WorldWideScience

Sample records for steel-kh25

  1. On the corrosion resistance of 01Kh25 ferritic steel

    International Nuclear Information System (INIS)

    Eremeeva, R.A.; Koval', E.K.

    1989-01-01

    Effect of non-ferrous metal ions on corrosion behaviour of 01Kh25 specific low carbon steel as compared to austenitic 12Kh18N10T and 06KhN28MDT steels in boiling solutions of sulfuric and nitric acids and their mixture is studied. Compositions initating commercial ones are chosen the media. It is shown that trough corrosion resistance of 01Kh25 steel in 10% H 2 SO 4 is two order below 06KhN28MDT austenitic steel in presence of Cu 2+ ions as a result of the surface passivation corrosion resistance of ferritic steel is an order higher the austenitic ones. Ferrite steel resistance in the nitric acid and its mixture with sulfuric acid is five timesas much as in 12Kh18N10T austenitic steel

  2. Nitrogen-containing superlow-carbon austenitic steel 02Kh25N22AM2

    Science.gov (United States)

    Fe'ldgandler, É. G.; Svistunova, T. V.; Savkina, L. Ya.; Lapshina, O. B.

    1996-02-01

    At present the equipment for manufacturing carbamide mineral fertilizers is produced from domestic steel 03Kh17N14M3 having "carbamide quality." Imported equipment also used in the industry is produced from steel of the 25-22-2 (Cr -Ni-Mo) type shipped by various firms, namely, 2RE69 (Sandvik, Sweden), 254SFER (Avesta, Sweden), 2522LCN (VDM, Germany), DM 1.4466 (Germany), and X2CrNiMo 25-22-2 (Dalmine, Italy). The imported steels are used because in some units steel 03Khl7Nl4M3 does not provide the requisite corrosion resistance in an intensified process of carbamide manufacturing. We currently possess domestic high-alloyed steel for producing new and repairing imported equipment operating under the severe conditions of carbamide synthesis. The present paper concerns the structure, mechanical properties, and corrosion resistance of industrially produced steel 02Kh25N22AM2 (ChS-108) and the recommended range of its application.

  3. Mechanical properties and kinetics of bainite transformation in the 35KhN3MFA and 25KhN3MFA steels

    International Nuclear Information System (INIS)

    Korotushenko, G.V.; Grigorkin, V.I.; Kozlov, V.I.; Sandomirskij, M.M.; Krivonosova, L.F.

    1978-01-01

    The mechanical properties and phase composition of the 25KhN3M A and 25KhN3M A bainitic steels have been investigated under austenization temperature varying from 870 to 1180 deg C and quenching cooling rate varying from 1 to 18x10 3 deg/min. Roentgen and quantitative phase analyses were employed. When bainitic steels are subjected to quenching by cooling with slow rate, their structure reveals b.c.c.-bainite with carbon content below the steel average, tetragonal martensite with a higher carbon content, carbon-rich residual austenite and carbides. Decreasing quenching cooling rates increase the concentration of tetragonal martensite and residual austenite and correspondingly reduce the concentration of b.c.c.-bainite. This tends to degrade the structural strength of bainitic steels in cores of large-size forged products

  4. Heat affected zone structure in welded joints of 15Kh1M1FL, 25Kh2NMFA and 20KhN2MFA steels

    International Nuclear Information System (INIS)

    Levenberg, N.E.; German, S.I.; Fomina, O.P.; Netesa, E.M.; Tsaryuk, A.K.; Kornienko, T.A.

    1983-01-01

    Heat affected zone (HAZ) structure of thick-walled, nature joints of 15Kh1M1FL steel for block structure of power reactors and 25Kh2NMFA and 20KhN2MFA steels for rotors - is investigated. Multi-layer arc welding is performed under conditions being created for standard components of turbines. Thermokinetics diagrams of austenite decomposition are built, phase composition and character of the structure forming at HAZ in the process of welding with preheating are studied. It is shown that at HAZ in joints of the steels under consideration in the process of welding with preheating is formed a structure of a grained bainite which is uniform in its structure and phase composition. Small volumes of round and elongated forms consisting of martensite and residual austenite are distributed in α-solid solution of the bainite. The bainite of the HAZ in welded joints possesses high hardness and great stability in the process of tempering

  5. Influence of sulphur and phosphorus impurities on ductility of 25Kh2NMFA steel during forging

    International Nuclear Information System (INIS)

    Onishchenko, A.K.

    1989-01-01

    Using cylindrical samples of the 25Kh2NMFA steel with sulfur and phosphorus content in the range of 0.001-0.030%, tensile test with the rate of deformation 10 -3 s -1 at the temperatures of 800-1200 deg C has been conducted. Analysis of fracture foci and plasticity diagrams has shown, that to ensure ductility during forging and high mechanical properties, the content of sulfur and phosphorus impurities in the 25Kh2NMFA steel must not exceed 0.015%

  6. Heat treatment effect on impact strength of 40Kh steel

    International Nuclear Information System (INIS)

    Golubev, V.K.; Novikov, S.A.; Sobolev, Yu.S.; Yukina, N.A.

    1984-01-01

    The paper presents results of studies on the effect of heat treatment on strength and pattern of 40Kh steel impact failure. Loading levels corresponding to macroscopic spalling microdamage initiation in the material are determined for three initial states. Metallographic study on the spalling failure pattern for 40Kh steel in different initial states and data on microhardness measurement are presented

  7. Corrosion failure of a bolt made of the 25Kh1MF material

    International Nuclear Information System (INIS)

    Liska, V.; Cechova, D.; Velkoborsky, J.

    1989-01-01

    M36x4 bolts, of which there are 222 at each nuclear power plant unit, are made of the 25Kh1MF or 38KhN3MFA steel. They are located in an environment with elevated temperature, with damp air and with boric acid. Corrosion of these bolts is due to the rather poor metallurgical quality of the steel. No inadmissible inhomogeneities of the type of lines of inclusions occur in the bolt material produced by cold rolling but defects of the type of laps were found on the threads. It is suggested that if the cold rolling technology were obviated, corrosion failure of the bolts might not occur. (M.D.). 7 figs., 3 refs

  8. Investigation of intergranular corrosion resistance of Cr16Ni25NMo6 steel

    International Nuclear Information System (INIS)

    Kamenev, Yu.B.; Nazarov, A.A.; Kuusk, L.V.; Majdeburova, T.F.

    1990-01-01

    The effect of 08Kh16N25AM6 steel susceptibility to intergranular corrosion on its intergranular cracking resistance in high-temperature water is investigated. In addition, the performed tests point to the susceptibility of sensibilized Kh16N25AM6 steel to intergranular corrosion in media simulating an agressive environment of power generation equipment; the latter requires a strict control over the resistance of weld joints of the above steel to intergranular corrosion. It is shown that Kh16N25AM6 type steel in sensibilized state is susceptible to intercrystalline corrosion cracking in high-temperature water which correlates with its susceptibility to intergranular corrosion established by AM GOST 6032-84 and potentiodynamic reactivation methods

  9. Corrosion resistance of welded joints in 08Kh22N6T and 08Kh21N6M2T steels made with new electrodes

    International Nuclear Information System (INIS)

    Sidorkina, Y.S.; Leibzon, V.M.; Mankevich, T.V.; Sidlin, E.A.; Zheltova, G.A.

    1986-01-01

    This paper examines the corrosion resistance of 08Kh22N6T and 08Kh21N6M2T steels which would make it possible to ensure equal properties of all the zones of the welded joints. The investigations were carried out on the welded joints in the steels produced with new OZL-40 and OZL-41 electrodes and with standard TsL-11 and EA-400/10u electrodes. The chemical compositions of the steels and deposited metal are presented. The tests of the intercrystalline corrosion resistances of the welded joints in the steels in the as-welded condition and after heat treatment showed that the weld metal is not attacked by intercrystalline corrosion. The tests also showed that the welded joints in 08Kh22N6T steel made with the OZL-40 and TsL-11 electrodes are resistant to corrosion in 55% phosphoric acid at 90 C in 1% sulfuric acid, and in 25% formic acid at 80 C. The investigated steels made with the OZL-40 and OZL-41 electrode respectively show that the welded joints are resistant to intercrystalline and general corrosion, have high mechanical and processing properties and the electrodes, and can be used for welding equipment designed for service in alkaline, neutral, and slightly acid media

  10. Development of production technology and investigation of quality for forged-welded turbine rotors of steel 25Kh2NVFA

    International Nuclear Information System (INIS)

    Borisov, I.A.; Merinov, G.N.; Slezkina, E.V.

    1997-01-01

    A study was made into mechanical properties and microstructure of turbine rotor components manufactured by forging and heat treated under various conditions. It is revealed that the optimal heat treatment of forgings must include double quenching with subsequent tempering at 630-640 deg C for 10-20 h. Forged and welded rotors should be tempered at 620-630 deg C for 50-100 h. Microscopic examination and mechanical tests showed that low alloy steel 25Kh2NMF can be successfully used for manufacturing rotors of high-, medium-and low-heat turbines

  11. Welding of heterogeneous 12Kh2MFSR steels with the Mn-Cr-Si-Ni system

    International Nuclear Information System (INIS)

    Smirnov, A.N.; Belogolov, E.I.

    1978-01-01

    The process of welding pipes of the 12Kh2MFSR pearlitic steels and austenitic steels of the Mn-Cr-Si-Ni system was studied. The filler materials were selected, and the working capacity of welded joints was examined in ageing and cyclic heatings. The microhardness of steels was measured, and the ultimate strength of welded joints was determined. The following has been established: the composite joints of steels of the Mn-Cr-Si-Ni system and 12Kh2MFSR steel are advisable to be welded on a coating layer welded by the EhA395/9 electrodes on the surface of a pipe of the 12Kh2MFSR pearlitic steel; this guarantees the sufficient working capacity of welded joints

  12. Hardening and stress relaxation during repeated heating of 15Kh2MFA and 15Kh2NMFA steels welded joints

    International Nuclear Information System (INIS)

    Zubchenko, A.S.; Suslova, E.A.

    1986-01-01

    Results of investigation of temperature-time conditions of hardening of welded joints of 15Kh2MFA and 15Kh2NMFA steels and their relaxation resistance, effect of metal structure of imitated heat affected zone (HAZ) on intensity of precipitation hardening at repeated heating are presented as well as the results of the process of relaxation of residual stresses at welded joints samples heating carried out by automatic welding under the flux with the use of adding materials and technology of manufacturing of vessels of WWER-440 and WWER-1000 reactors. Peculiarities of the hardening at repeated heating of the HAZ metal imitated at these steels. Precipitation hardening of overheated 15Kh2MFA steel is connected with precipitations at repeated heating of carbides of the M 7 C 3 , M 3 C and VC type. Stress relaxation in welded joints runs more intensively at the initial stage of repeated heating, i.e. during the same period of the process of dispersed carbide precipitations

  13. Structure, mechanical and corrosion properties of powdered stainless steel Kh13

    International Nuclear Information System (INIS)

    Radomysel'skij, I.D.; Napara-Volgina, S.G.; Orlova, L.N.; Apininskaya, L.M.

    1982-01-01

    Structure, mechanical and corrosion properties are studied for compact powdered stainless steel, Grade Kh13, produced from prealloyed powder and a mixture of chromium and iron powders by hot vacuum pressing (HVP) following four schemes: HVP of unsintered billets; HVP of presintered billets; HVP of unsintered billets followed by diffusion annealing; HVP of sintered billets followed by diffusion annealing. Analysis of the structure, mechanical and corrosion properties of Kh13 steel produced according to the four schemes confirmed that production of this steel by the HVP method without presintering of porous billets and diffusion annealing of compact stampings is possible only when prealloyed powder of particular composition is used as a starting material

  14. Structural inheritance in cast 30KhGNM-type steel

    International Nuclear Information System (INIS)

    Sadovskij, V.D.; Bershtejn, L.I.; Mel'nikova, A.A.; Polyakova, A.M.; Schastlivtsev, V.M.

    1980-01-01

    Structural inheritance in the cast 30KhGNM-type steel depending on the heating rate and the temperature of preliminary tempering is investigated. When eating the cast steel with a beinite structure at the rate of 1-150 deg/min, the restoration of austenite grain and the following recrystallization due to the phase cold work, are observed. Slow heating from room temperature or preliminary tempering hinder grain restoration during heating. A non-monotonous effect of tempering temperature on the structural inheritance is established which can be connected with the kinetics of decomposition of residual austenite in steel

  15. The Kinetics of Bainitic Transformation of Roll Steel 75Kh3MF

    Science.gov (United States)

    Kletsova, O. A.; Krylova, S. E.; Priymak, E. Yu.; Gryzunov, V. I.; Kamantsev, S. V.

    2018-01-01

    The critical points of steel 75Kh3MF and the temperature of the start of martensitic transformation are determined by a dilatometric method. The thermokinetic and isothermal diagrams of decomposition of supercooled austenite are plotted. The microstructure and microhardness of steel specimens cooled at different rates are studied. The kinetics of the occurrence of bainitic transformation in the steel is calculated using the Austin-Ricket equation.

  16. Preliminary heat treatment of 4KhM2Fch die steel

    International Nuclear Information System (INIS)

    Leonidov, V.M.; Berezkin, Y.A.; Nikitenko, E.V.

    1986-01-01

    To improve the machinability and preparation of the structure for hardening, die steels are given a preliminary treatment which provides a reduction in hardness as a result of separation in the structure of the carbide and ferrite phases, coagulation of the carbides, and acquisition by them of a granular form and also the obtaining of fine grains and a uniform distribution of the structural constituents. The microstructure was evaluated after etching in 4% nital on an MIM-8M microscope. The 4KhM2Fch steel was given a preliminary heat treatment of normalize and anneal. It was concluded that for 4KhM2Fch steel a preliminary heat treatment of normalizing from 950 0 C with a hold of 1.5-2 h, annealing at 750-760 0 C with a hold of 2-3 h, cooling to the isothermal temperature of 670-680 0 C with a hold of 3-4 h, and further air cooling is recommended. The structure after such a heat is granular pearlite with a rating 1-2 and a hardness of 220-250 HB

  17. Successive carbon- and boron saturation of KhVG steel in powder mixtures

    Energy Technology Data Exchange (ETDEWEB)

    Alimov, Yu A; Gordienko, S I

    1975-01-01

    Method of successive saturation of KhVG steel with carbon and boron in powder mixtures is described. After carbonization of steel in a charcoal carburator at 930 deg C during 3 hrs a domain of equiaxial large grains is formed there the latter representing carbides of Fe/sub 3/C and (Fe, M)/sub 3/C. The increase of duration of carbonization up to 5 hrs and above results in formation of a cement grid greatly impairing the mechanical properties of the metal. Carbonization is followed by borating in powdered technical boron carbide at 900 deg C for 4 hrs which ensures formation on the sample surface of a borated layer with depth up to 65 mkm covering the carbonized zone. As followed from metallographic and x-ray structural analysis, the borated layer consists of boride needles with complex composition (Fe, Cr, Mn)B. Oil hardening of carbonized KhVG steel from 850 deg C and low-temperature tempering at 180 deg C for 1 hr results in formation in the main metal of martensite-carbide structure and, respectively, in the decrease of the microhardness gradient between the diffusion layers, as compared with borated KhVG steel. Operation tests of strengthened matrices of preforming machines under the conditions of application of dynamic pressing forces up to 1500 kg Fce/cm/sup 2/ demonstrated that the cyclical strength of carboborated coverings is 2.0-3.0 times higher than that of borated ones. The method of carboborating is recommended for strengthening the details of stamp and press tools.

  18. Effect of zirconium on the structure and phase composition of steel 03Kh8SYu

    International Nuclear Information System (INIS)

    Tarzhumanova, V.A.; Ryabchenkov, A.V.; Shatunova, A.V.; Yoganova, S.A.

    1986-01-01

    Previously, the authors determined the optimum zirconium content providing retention of a fine-grained structure for steel 03Kh8SYu during high-temperature heating. It was suggested that this was caused by separation in the steel of intermetallic phase Fe 3 Zr. This paper presents results of further studies in this direction. X-ray analysis results for the anodic residues of the steels are presented. It can be seen that in steel without zirconium, carbides of the type M 23 C 6 and M 7 C 3 and aluminum nitride are present. On adding 0.05% Zr, zirconium nitride forms in addition to the existing aluminum nitride and carbides of the type M 7 C 3 . The authors also investigated the effect of zirconium on the tendency of the steel toward grain growth at higher temperature; they studied the structure of steel 03Kh8SYu with 0.61% Zr after soaking specimens for 100 h at 950-1100 C. Results are presented

  19. Effect of rolling temperature on 12Kh18N10T steel tube hardening

    International Nuclear Information System (INIS)

    Yushkevich, P.M.; Stepanovich, V.E.; Manankova, L.V.; Usenko, V.N.; Semenov, I.A.

    1984-01-01

    Mechanical properties and substructure of tubes at the constant reduction degree k(the ratio of deformation over wall thickness to deformation over diameter), depending on strain degree during cold and hot tube rolling, have been studied. The investigations are carried out using hot-rolled tubes with the dimensions 88x8 mm of 12Kh1hN10T steel. With the decrease of strain over the wall of the tube, produced of 12Kh18N10T steel as to strain over diameter the values of yield strength and ultimate strength increase with simultaneous decrease in ductility during warm rolling and yield strength and ultimate strength decrease with the increase in ductility-during cold rolling. During warm rolling of the tubes at 250 deg C the hardening of 12Kh18N10T steel is higher, than at the rolling temperature 150 deg C. The optimum temperature range of warm rolling is 120-150 deg C. Grain orientation in the metal of the tubes and degree of texture perfection increase with the temperature increase of the tube warm drolling as compared with col rolli

  20. Welding procedure for 06Kh13N7D2 steel

    International Nuclear Information System (INIS)

    Muromtsev, B.I.; Turkov, I.I.

    1990-01-01

    Based on the results of investigations into the process strength, mechanical and corrosion properties of 08Kh13N7D2 steel welded joints, the optimal method of its welding and a possibility of applying it for high-strength mounting in nuclear power plants are determined

  1. Hydrogen effect on mechanical properties and flake formation in the 10KhSND steel rolled plates

    Energy Technology Data Exchange (ETDEWEB)

    Muradova, R G; Zakharov, V A; Kuzin, A P; Gol' tsov, V A; Podgajskij, M S [Donetskij Politekhnicheskij Inst. (Ukrainian SSR); Donetskij Nauchno-Issledovatel' skij Inst. Chernoj Metallurgii (Ukrainian SSR))

    1982-01-01

    The effect of hydrogen on mechanical properties of the 10KhSND steel rolled plates during natural aging is studied. Optimum period of metal acceptance tests, which are advisable to conduct after 5-7 day natural aging of finished products, are found out. The technique is worked out and a safe hydrogen content to prevent flake formation in the 10KhSND steel is determined. It is shown that a safe hydrogen content is dependent on the experiment conditions (sample dimensions, conditions of cooling, and prehistory).

  2. Hydrogen effect on mechanical properties and flake formation in the 10KhSND steel rolled plates

    International Nuclear Information System (INIS)

    Muradova, R.G.; Zakharov, V.A.; Kuzin, A.P.; Gol'tsov, V.A.; Podgajskij, M.S.

    1982-01-01

    The effect of hydrogen on mechanical properties of the 10KhSND steel rolled plates during natural aging is studied. Optimum period of metal acceptance tests, which are advisable to conduct after 5-7 day natural aging of finished products, are found out. The technique is worked out and a safe hydrogen content to prevent flake formation in the 10KhSND steel is determined. It is shown that a safe hydrogen content is dependent on the experiment conditions (sample dimensions, conditions of cooling, and prehistory)

  3. Study of 16KhSN high strength steel in different structural states and under working conditions

    International Nuclear Information System (INIS)

    Skudnov, V.A.; Vorob'ev, I.A.; Kutyajkin, V.G.; Bugrov, Yu.V.

    1985-01-01

    A study was made on the effect of deformation degree (up to 60%) during reducing, drawing and heat treatment (annealing at 750 deg C), quenching from 930 deg C and tempering at 350 deg C) on strength, plasticity, hardening degree, notch sensitivity, density and elasticity characteristics of the steel. The effect of test temperature (from-196 up to 1000 deg C) on tensile strength and plasticity was studied as well. It was established that drawing and reducing of 16KhSN steel in annealed state with strain degrees of up to 60% results to increase of strength characteristics 1.7...2.3 times and decrease of plasticity characteristics by 15...23%, strain hardening coefficient - 2.2 times and the maximum strain energy - by 80 MJ/m 3 . Hardening heat treatment (quenching from 930 deg C+temperating at 350 deg C) affects on mechanical properties of 16KhSN steel in much the same way as cold working, but strength characteristics of heat-treated steel increase 2.6...3.6 times and the maximum strain energy grows by 640 MJ/m 3 . Systematic data on the effect of temperature (-196...1000 deg C) and tensile rate (4 mm/min...5m/s) on strength and plasticity of 16KhSN steel in annealed state were obtained

  4. Protective effect of KhOSP-10 inhibitor during corrosion, hydrogenadsorption and corrosion cracking of a steel in sulfuric acid

    Energy Technology Data Exchange (ETDEWEB)

    Mindyuk, A K; Svist, E I; Savitskaya, O P; Goyan, E B; Gopanenko, A N [AN Ukrainskoj SSR, Lvov. Fiziko-Mekhanicheskij Inst.

    1975-01-01

    The protective propeties of inhibitor KhOSP-10 in the time of corrosion and corrosive cracking of steel 40Kh are higher then those of inhibitors KPI-1, KI-1, I-I-V etc. Its ability to reduce steel hydrogenation is the same as in the case of KPI-1 inhibitor i.e. below that of KI-1. HCl additives enhance the efficiency of inhibitors KPI-1, KI-1, I-1-V etc. up to the protective ability of KhOSP-10. Kinetics of the electrode processes was estimated from polarization curves.

  5. Cooling rate and microstructure of surface layers of 5KhNM steel, machined by electroerosion method

    International Nuclear Information System (INIS)

    Foteev, N.K.; Ploshkin, V.V.; Lyakishev, V.A.; Shirokov, S.V.

    1982-01-01

    The cooling rate and microstructure of surface layers of steel 5KhNM machined by electroerosion method have been studied. It is shown that the difference in heating rate of the surface layers with electric discharge over the 5KhNM steel samples depth results in the intensive size reduction of the microstructure. In the surface layer alongside with martensite residual austenite is present, the lattice period of which increases with the increase of pulse duration, carbide phase of complex composition appears, and concentrational heterogeneity in alloying elements (except carbon) is absent

  6. Cooling rate and microstructure of surface layers of 5KhNM steel, machined by electroerosion method

    Energy Technology Data Exchange (ETDEWEB)

    Foteev, N.K.; Ploshkin, V.V.; Lyakishev, V.A.; Shirokov, S.V.

    1982-01-01

    The cooling rate and microstructure of surface layers of steel 5KhNM machined by electroerosion method have been studied. It is shown that the difference in heating rate of the surface layers with electric discharge over the 5KhNM steel samples depth results in the intensive size reduction of the microstructure. In the surface layer alongside with martensite residual austenite is present, the lattice period of which increases with the increase of pulse duration, carbide phase of complex composition appears, and concentrational heterogeneity in alloying elements (except carbon) is absent.

  7. Ultrasound surface treatment of Kh18N10T steel with different structural state. Ul'trazvukovaya poverkhnostnaya obrabotka stali Kh18N10T s razlichnym strukturnym sostoyaniem

    Energy Technology Data Exchange (ETDEWEB)

    Aksenov, V K; Danilov, P A; Mats, A V; Netesov, V M; Yaes, A A [AN Ukrainskoj SSR, Kharkov (Ukrainian SSR). Fiziko-Tekhnicheskij Inst.

    1989-09-01

    Ultrasound surface treatment (USST) is studied for its effect on the structure and mechanical-and-physical properties of Kh18N10T steel with different prehistory. It is shown that surface treatment may both increase and decrease steel microhardness.

  8. Welding of high-strength stainless steel 03Kh12N10MT for cryogenic engineering

    International Nuclear Information System (INIS)

    Pustovit, A.I.

    1989-01-01

    Consideration is being given to weld resistance to cold and hot cracking at 93 and 77K and to mechanical properties of welded joints of high-strength stainless steel 03Kh12N10MT, produced under the fluxes AN-17M, AN-18, AN-26, AN-45, ANF-5, 48-OF-6, ANK-45 and ANK-49 in combination with various welding wires. It is shown that welds on 03Kh12N10MT steel meet the requirements only when using 48-OF-6 or ANK-49 flux. It is noted that impact strength of welds at 77K is sufficiently affected by the volume fraction of non-metallic inclusions in weld metal

  9. Development of plastic deformations in 12Kh18N10T steel under cyclic symmetrical bending of specimens of various length

    Energy Technology Data Exchange (ETDEWEB)

    Pisarenko, G.S.; Leonets, V.A.; Bega, N.D. (AN Ukrainskoj SSR, Kiev. Inst. Problem Prochnosti)

    1983-08-01

    Effect of specimen length on intensity of plastic deformation development and cyclic strength is studied for annealed 12Kh18N10T steel under cyclic symmetrical bending. The intensity of microplastic deformations and cyclic strength of annealed 12Kh18N10T steel in the considered case is due to self-heating.

  10. On the protective effect of KhOSP-10 inhibitor during corrosion, hydrogenadsorption and corrosion cracking of a steel in sulfuric acid

    International Nuclear Information System (INIS)

    Mindyuk, A.K.; Svist, E.I.; Savitskaya, O.P.; Goyan, E.B.; Gopanenko, A.N.

    1975-01-01

    The protective propeties of inhibitor KhOSP-10 in the time of corrosion and corrosive cracking of steel 40Kh are higher then those of inhibitors KPI-1, KI-1, I-I-V etc. Its ability to reduce steel hydrogenation is the same as in the case of KPI-1 inhibitor i.e. below that of KI-1. HCl additives enhance the efficiency of inhibitors KPI-1, KI-1, I-1-V etc. up to the protective ability of KhOSP-10. Kinetics of the electrode processes was estimated from polarization curves

  11. Influence of local microplastic strains on stress corrosion of 08Kh18N10T steel

    International Nuclear Information System (INIS)

    Moskvin, L.N.; Efimov, A.A.; Sherman, Ya.I.; Fedorova, T.I.

    1987-01-01

    Study on specific features of microhomogeneous strain in the process of plastic strain development and their role in stress corrosion of 08Kh18N10T steel sheet specimens subject to preliminary strain by 1, 3, 6, 16 and 23% and subsequent tests of stress corrosion in magnesium chloride solution at 150 deg C 140 MPa has been carried out. Analysis of test results has shown that microplastic strain is distributed over a specimen nonuniformly and is accompanied with the slip bands formation which are sources of corrosion crack origination and development. 08Kh18N10T steel manifests the highest trend to stress corrosion under 1% microplastic strain

  12. Long-term strength and allowable stresses of grade 10Kh9MFB and X10CrMoVNb9-1 (T91/P91) chromium heat-resistant steels

    Science.gov (United States)

    Skorobogatykh, V. N.; Danyushevskiy, I. A.; Schenkova, I. A.; Prudnikov, D. A.

    2015-04-01

    Currently, grade X10CrMoVNb9-1 (T91, P91) and 10Kh9MFB (10Kh9MFB-Sh) chromium steels are widely applied in equipment manufacturing for thermal power plants in Russia and abroad. Compilation and comparison of tensile, impact, and long-term strength tests results accumulated for many years of investigations of foreign grade X10CrMoVNb9-1, T91, P91, and domestic grade 10Kh9MFB (10Kh9MFB-Sh) steels is carried out. The property identity of metals investigated is established. High strength and plastic properties of steels, from which pipes and other products are made, for operation under creep conditions are confirmed. Design characteristics of long-term strength on the basis of tests with more than one million of hour-samples are determined ( and at temperatures of 500-650°C). The table of recommended allowable stresses for grade 10Kh9MFB, 10Kh9MFB-SH, X10CrMoVNb9-1, T91, and P91 steels is developed. The long-time properties of pipe welded joints of grade 10Kh9MFB+10Kh9MFB, 10Kh9MFB-Sh+10Kh9MFB-Sh, X10CrMoVNb9-1+X10CrMoVNb9-1, P91+P91, T91+T91, 10Kh9MFB (10Kh9MFB-Sh)+X10CrMoVNb9-1(T/P91) steels is researched. The welded joint reduction factor is experimentally determined.

  13. Effect of the isothermal transformation temperature on the fine structure of steel-12Kh1MF

    International Nuclear Information System (INIS)

    Mints, I.I.; Berezina, T.G.; Lanskaya, K.A.

    1976-01-01

    For detailed analysis of bainite and pearlite in steel 12Kh1MF, homogeneous structures were obtained by isothermal annealing at 350, 450, 500, and 650 0 for 1 h. Isothermal transformation of austenite leads to the formation of bainite at 350-500 0 and pearlite at 650 0 . The austenitizing temperature was 980 0 for both types of samples, with holding for 20 min. For comparison, the plates were quenched from 980 0 and 1050 0 in ice-cold brine. The investigation was conducted with use of light and electron microscopes and x-ray analysis. The long-term strength was also determined. Isothermal treatment of steel 12Kh1MF at 350-500 0 C leads to the formation of a structure consisting of upper and lower bainite. At 500 0 the structure consists primarily of upper bainite, and at 350 0 of lower bainite. With tempering of the steel with a structure of upper and lower bainite at 730 0 for 3 h the dislocations undergo redistribution of the polygonization type within ferrite needles, with development of a cellular substructure. The acicular structure of the matrix is retained in this case. The density and evenness of the distribution of carbides is higher in upper bainite than in lower bainite. Steel 12Kh1MF with a structure of upper bainite is more susceptible to recrystallization as compared with a structure of lower bainite, which is responsible for the higher heat resistance of the latter

  14. Pipes out of the chromium-molybdenum 12Kh2M1 steel intended for power units

    International Nuclear Information System (INIS)

    Saf'yanov, A.V.; Plyatskovskij, O.A.; Khokhlov-Nekrasov, O.G.; Palatnikova, E.S.; Karpenko, N.P.

    1977-01-01

    Vanadiumless steel 12Kh2M1 (2.25%Cr, 1%Mo) known to be applied abroad has been used for production of 325x60 mm tubes. The technology involves heating of the blanks to 1270-1300 deg C, their piercing in a double-roller mill, rolling on a pilger mill 8-16'' in thick wall caliber rolls, thermal treatment (normalizing at 930-960 deg C for 1 hour and tempering at 730+-10 deg C for 4 hours and etching (12-22% H 2 SO 4 and up to 143 g/l FeSO 4 ) for 3-4 hours at 55-65 deg C. Good technological properties of the steel and its capacity of working at 540-580 deg C are confirmed. Vanadium alloying of boiler steels does not provide for essential improvement of oxydation resistance and long term strength, but decreases the workability and enhances scatter of working parameters on account of minor variations of chemical composition

  15. Defect accumulation in welded joints of 12Kh1MF steel steam pipelines during creep

    International Nuclear Information System (INIS)

    Anokhov, A.E.; Alekhova, I.A.

    1982-01-01

    Technique for investigation of micropore accumulation in 12Kh1MF steel welded joints is proposed. The micropore density in different zones of welded joints in non-uniform. It is shown that failure localization in welded joint in the softening zone during the creep takes place due to the micropore priority accumulation in this zone. It is found out that accumulation of residual deformations in different zones of 12Kh1MF welded joints under creep runs more uniformly as the level of working stresses decreases and test duration increases

  16. On change of vanadium carbide state during 20Kh3MVF steel heat treatment

    International Nuclear Information System (INIS)

    Gitgarts, M.I.; Maksimenko, V.N.

    1975-01-01

    The Xray diffraction study of vanadium carbide MC has been made in the steel-20KH3MVF quenched from 970 and 1040 deg and tempered at 660 deg for 210 hrs. It has been found that the constant of the MC crystal lattice regularly varies with the temperature of isothermal hold-up. In the steel tempered after quenching two vanadium carbides of different content could co-exist simultaneously: carbide formed in the quenching process and carbide formed during tempering. The discovered effect of the temperature dependence of the MC content is, evidently, inherent also to other steels containing vanadium

  17. Heating temperature effect on ferritic grain size of rotor steel

    International Nuclear Information System (INIS)

    Cheremnykh, V.G.; Derevyankin, E.V.; Sakulin, A.A.

    1983-01-01

    The heating temperature effect on ferritic grain size of two steels 13Kh1M1FA and 25Kh1M1FA is evaluated. It is shown that exposure time increase at heating temperatures below 1000 deg C up to 10h changes but slightly the size of the Cr-Mo-V ferritic grain of rotor steel cooled with 25 deg C/h rate. Heating up to 1000 deg C and above leads to substantial ferritic grain growth. The kinetics of ferritic grain growth is determined by the behaviour of phases controlling the austenitic grain growth, such as carbonitrides VCsub(0.14)Nsub(0.78) in 13Kh1M1FA steel and VCsub(0.18)Nsub(0.72) in 25Kh1M1FA steel. Reduction of carbon and alloying elements content in steel composition observed at the liquation over rotor length leads to a certain decrease of ferritic grain resistance to super heating

  18. Peculiarities of welding procedure for the 05Kh12K14N5M5T-VD maraging stainless steel with strength higher 1500 MPa

    International Nuclear Information System (INIS)

    Pustovit, A.I.

    1980-01-01

    The effect of welding procedure of 05Kh12K14N5M5T-VD stainless steel on the properties of its welded joints is investigated. A new procedure of welding for pressure vessels made of this steel using Sv-03Kh15K14N5M3T-EL welding wire is suggested [ru

  19. Structural changes in surface layer of steel 08Kh18N10T during machining

    International Nuclear Information System (INIS)

    Palenik, J.; Vodarek, V.

    1989-01-01

    The results are reported of a study of the surface layer of steel 08Kh18N10T affected by machining. Structural changes were studied caused by finish turning and by additional roller burnishing. Multiple deformation bands were observed to occur under the given cutting conditions; they mainly consisted of deformation doublets and only in isolated cases of ε-martensite. The presence of α'-martensite was not shown in the specimen surface layer following finish turning. The deformation shear bands in the roller-burnished specimen consisted of both ε-martensite and of deformation doublets. The amount of ε-martensite in the structure was significantly higher than in the specimen worked by turning. Local presence of α'-martensite formations was observed inside the deformation bands. It thus follows that roller burnishing is unsuitable as part of the manufacture of components from steel 08Kh18N10T. (J.B.). 5 figs., 1 tab., 9 refs

  20. Study of surface layer on 08Kh15N5D2T steel

    International Nuclear Information System (INIS)

    Tyurin, A.G.; Povolotskij, V.D.; Zhivotovskij, Eh.A.; Berg, B.N.

    1986-01-01

    08Kh15N5D2T steel phase composition is investigated. Its surface layer was determined by X-ray diffraction analysis method. It is shown, that a subscale appears to be the reason for corrosion of products, made of EhP410 steel. Under the existing smelling technology the carbon content in it is ≥ 0.05%. Therefore to avoid the metal surface depletion with chromium, one must provide for titanium relation to carbon of not less than 4.5 and carry out the rolled product thermal treatment in a protective atmosphere; otherwise, the technology must include not only the removal of scale from steel but the metal subscale layer as well

  1. Properties of structural steels melted out of high-purity charge

    International Nuclear Information System (INIS)

    Marchenko, V.N.; Sergeeva, T.K.; Kondakova, N.K.; Morozov, V.P.; Madorskij, L.L.

    1993-01-01

    A comparative evaluation has been made of impurities, mechanical properties and hydrogen embirittlement parameters for steels type 40Kh and 40KhS produced by electrometallurgical method with the use of direct reduced charge (DR-steels) and melted in an open-hearth furnace. Investigation results have shown that 40Kh and 40KhS Dr-steels have more coarse austenitic grains and experience more complete transformation of martensite into ferritic-pearlitic mixture on tempering. Threshold stresses increase 2.5 times due to purity enhancement at the expense of application of direct reduced charge

  2. Ductile fracture of two-phase welds under 77K. [Steel-EhP810, steel-EhP666, steel-08Kh18N10T, steel-EhP659-VI, steel-chP810

    Energy Technology Data Exchange (ETDEWEB)

    Yushchenko, K.A.; Voronin, S.A.; Pustovit, A.I.; Shavel' , A.V.

    The effect of the type of welding and fillers on crack resistance of welded joints high-strength steel EhP810 and its various compounds with steels EhP666, 08Kh18N10T has been studied. For the welding of steel EhP810 with steels EhP810, EhP666, 08Kh18N10T electron-beam, automatic, argon tungsten arc with non-consumable electrode with various fillers, as well as argon metal-arc welding with consumable electrode, were used. It is shown, that for a joint, made by electron-beam welding, parameters sigmasub(u), Ksub(IcJ), KCV are higher than for a joint of a similar phase structure made using filler wire EhP659-VI. It is explained by the fact, that during electron-beam welding joint metal refining takes place, which removes gases. In welded joints of chP810 steel, having joints with austenitic structure, characteristic of crack resistance Ssub(c) increases by more than 0.2 mm in contrast to two-phase joints, which conventional yield strength at 77 K exceeds 1000 MPa. It is worth mentioning, that for other classes of steels formation of two-phase structure of joint increases welded joint resistance to brittle fracture. It is possible to obtain the required structure of joint with assigned level of resistance to brittle fracture by means of the use of different fillers, optimum and welding procedure, regulating the part of the basic metal in joint content.

  3. Strain ageing of the 15Kh2MFA steel at 500 and 550 deg C

    International Nuclear Information System (INIS)

    Maksimovich, G.G.; Azbukin, V.G.; Krylova, R.P.; Tretyak, I.Yu.; Bardachevskaya, T.V.

    1978-01-01

    The effect of ageing at high temperatures and under high stresses on strength and plasticity of the 15Kh2MFA steel has been studied. The steel was kept at 500 and at 550 deg C for 100, 1000 and 2500 hours without stress and under stress of 0.5 and 0.9 of the long-term strength limit (sigmasub(ls)). Ageing at 500 deg C without stress and under 0.5 sigmasub(ls) changed neither strength nor plasticity of the steel; under 0.9 sigmasub(ls) the strength somewhat decreased. Ageing at 550 deg C for 1000 hours resulted in an appreciable stress drop

  4. Neutron diffraction study of a nitrogen martensitic steel 0Kh16N4AB under load

    Czech Academy of Sciences Publication Activity Database

    Sumin, V. V.; Papushkin, I.V.; Bannykh, O.A.; Blinov, V.M.; Lukáš, Petr

    2008-01-01

    Roč. 105, č. 1 (2008), s. 88-91 ISSN 0031-918X Institutional research plan: CEZ:AV0Z10480505 Keywords : steel 0Kh16N4AB * neutron diffraction * FSD Subject RIV: BG - Nuclear, Atomic and Molecular Physics , Colliders Impact factor: 0.412, year: 2008

  5. Simulation of Microdamage and Evaluation of Remaining Life of Steam Conduit Components from New-Generation Refractory Steel 10Kh9MF-Sh

    Science.gov (United States)

    Gladshtein, V. I.

    2018-03-01

    The effects of microdamage on the remaining life of high-temperature components of steam conduits from high-chromium steel 10Kh9MF-Sh and low-alloy steel 12Kh1M1F are compared. To simulate the microdamage, specimens with a circular notch and different relative diameters are fabricated. Specimens with a notch simulating the highest degree of microdamage and smooth specimens are tested for long-term strength. The coefficient of the remaining life of a conduit is computed for the range of relative damage presenting practical interest.

  6. Effect of melting technique on grain size and heat resistance of the 12Kh1MF steel

    International Nuclear Information System (INIS)

    Lanskaya, K.A.; Kulikova, L.V.; Butneva, N.I.

    1978-01-01

    Investigated are the 12Kh1MF steel melted in open-hearth and arc furnaces (deoxidation by aluminium in 1.0 kg/t quantity) and then subjected to electroslag melting. The size of an austenitic grain depends on the residual contents of nitrogen and aluminium in steel. The open-hearth metal subjected to electroslag melting and containing a small quantity of nitrogen (0.006%) and aluminium (0.013%) has coarse austenitic grains and higher heat resistance compared to the steel melted in an arc furnace and also sub ected to electroslag melting. The nitride analysis of steel is carried out

  7. Preliminary tension effect on low-cycle fatigue of 40Kh13 steel in gaseous hydrogen

    International Nuclear Information System (INIS)

    Romaniv, A.N.

    1984-01-01

    Comparative bending tests of specimens deformed by tension at 65, 18 and 30% in hydrogen and vacuum were accomplished to reveal the effect of preliminary tension on low-cycle fatigue strength of 40Kh13 martensitic steel. It was found that small amounts of preliminary strains induced a considerable decrease in low-cycle durability in vacuum and hydrogen which was connected with developing defects arising at the early stages of plastic deformation. A rather high degree of preliminary tension promoted steel homogenization, hydrogen embrittlement decrease and service behaviour improvement

  8. Effect of heat treatment and rotor steels composition on hydrogen solubility

    International Nuclear Information System (INIS)

    Ivanov, A.I.; Samojlenko, L.V.; Gorovaya, O.N.; Najdovskij, A.G.; Bilik, I.; Kret, Ya.

    1988-01-01

    Measurements of equilibrium hydrogen adsorption in samples of 27KhN3MFA and 25Kh2NMFA steels were conducted. Carbide inclusions and doping additions, typical for rotor steels, don't produce noticeable effect on hydrogen solubility in

  9. Estimation of structural strength of 38KhN3MFA steel, melted using different methods

    International Nuclear Information System (INIS)

    Kudrya, A.V.; Mochalov, B.V.; Fadeev, Yu.I.

    1982-01-01

    Quantity of steel melted by different methods using criteria of fracture mechanics is evaluated. Three technological variants of the 38KhN3MFA steel melting: acid Martin steel prepared by the duplex-process (melt 1); the main Martin steel melting with deoxidation and alloying in a ladle by liquid alloy and treatment with synthetic slag with argon purging after production (melt 2) and its electroslag remelt - ESP process (melt 3) are investigated. The analysis of the investigated melts has revealed that crack resistances of the acid Martin steel is higher than that of other melts at practically similar standard mechanical properties with 0.35 probability at 0.05 significance level in the low-tempered state; in the tempered state the best crack resistance is observed in the ESP main Martin steel. Metal of the main Martin melting has lower crack resistance as compared with other meltings at both strength levels. The results of the work point out the necessity of applying the criteria of fracture mechanics for obtaining an objective evaluation of the steel quality

  10. Effect of Heat Treatment on the Structure and Properties of Die Steel 70Kh3G2FTR

    Science.gov (United States)

    Krylova, S. E.; Kletsova, O. A.; Gryzunov, V. I.; Fot, A. P.; Tavtilov, I. Sh.

    2018-01-01

    The effect of heat treatment parameters on the properties and structural and phase composition of a promising die steel 70Kh3G2FTR for hot deformation is studied. The temperature-and-stress state of a hammer die under a heat treatment is simulated.

  11. Ductility of high chromium stainless steels

    International Nuclear Information System (INIS)

    Peretyat'ko, V.N.; Kazantsev, A.A.

    1997-01-01

    Aimed to optimize the hot working conditions for high chromium stainless steels the experiments were carried in the temperature range of 800-1300 deg C using hot torsion tests and cylindrical specimens of ferritic and ferritic-martensitic steels 08Kh13, 12Kh13, 20Kh13, 30Kh13 and 40Kh13. Testing results showed that steel plasticity varies in a wide range depending on carbon content. Steels of lesser carbon concentration (08Kh13 and 12Kh13) exhibit a sharp increase in plasticity with a temperature rise, especially in the interval of 1200-1250 deg C. Steels 20Kh13 and 30Kh13 display insignificant plasticity increasing, whereas plastic properties of steel 40Kh13 increase noticeably in the range of 1000-1300 deg C. It is shown that optimal hot working conditions for specific steel must be selected with account of steel phase composition at high temperatures

  12. Irradiation and annealing behavior of 15Kh2MFA reactor pressure vessel steel

    International Nuclear Information System (INIS)

    Popp, K.; Bergmann, U.; Bergner, F.; Hampe, E.; Leonhardt, W.D.; Schuetzler, H.P.; Viehrig, H.W.

    1992-01-01

    This work deals with the mechanical properties of RPV steels used WWER-440. The materials under investigation were a forging (base metal 15Kh2MFA) and the corresponding weld. Charpy V-notch specimens and tensile test specimens were irradiated in the WWER-2 Rheinsberg at about 270 C up to the two neutron fluence levels of 4 x 10 18 and 5 x 10 19 n/cm 2 (E>1MeV). Post-irradiation annealing heat treatments were performed, among others a 475 C/152 h treatment of technical interest. (orig.)

  13. Effect of nonmetallic inclusions on anisotropy of ductility in 35KhN3MFA steel forgings

    International Nuclear Information System (INIS)

    Shtremel', M.A.; Yavojskij, V.I.; Volkov, V.A.; Chursin, G.M.; Chukhlov, V.I.; Fetisov, G.I.; Mochalin, N.K.; Smol'yaninov, L.V.

    1980-01-01

    Characteristics of nonmetaltic inclusions and anizotropy of ductility and of impuct strength of forgings of the 35KhN3MFA steel are compared at different variants of melting and outer-furnace treatment. It is shown that method of melting rugulates anisotropy of ductility primarily through deformability of large inclusions during forging. Deformability of inclusions considerably changes due to introduction of silicocalcium in iron mold [ru

  14. Investigation of 12Kh1MF steel resistance to brittle fractures

    International Nuclear Information System (INIS)

    Bologov, G.A.; Rushchits, T.Yu.

    1977-01-01

    The metal of hot-rolled steam pipe made of 12Kh1MF steel, which has been subjected to thermal treatment under laboratory conditions, and metal samples from acting steam pipes after different exploitation periods at 510-565 deg C have been investigated. The dependence of impact viscosity and its constituents on conditions of thermal treatment has been established. The energy consumed by the developing crack has been used as an impact viscosity criterion. Appropriate thermal treatment is capable of rehabilitating the impact viscosity of embrittled metal. Cold plastic deformation increases crack propagation rate in the initial metal and promotes embrittlement during exploitation. Ageing of the working metal reduces its capacity of stopping the developing crack and shifts the temperature threshold of brittleness towards positive temperature

  15. Effect of partial oxygen pressure on physicochemical properties of Kh18N10T steel at isothermal oxidation

    International Nuclear Information System (INIS)

    Alekseev, V.N.; Oshe, E.K.; Fokin, M.N.; Bogdanova, S.V.; Loskutov, A.I.

    1990-01-01

    Auger-electron spectroscopy, photoelectric polarization, conductometry methods have been used to analyze chemical and defect composition of surface oxide layers, formed on stainless steel Kh18N10T in vacuum (10 -9 - 10 -2 torr) and at temperatures 593-673 K. The boundary conditions of manifestation of extermal behaviour of the dependence of the surface oxide growth rate at isothermal oxidation of this steel are determined. The relation between passivation properties of the surface oxide and the magnitude of the edge angle of the surface wetting with molten tin is revealed

  16. Cyclic crack resistance of anticorrosion cladding-15Kh2MFA steel joint

    International Nuclear Information System (INIS)

    Zvezdin, Yu.I.; Nikiforchin, G.N.; Timofeev, B.T.; Zima, Yu.V.; Andrusiv, B.N.

    1985-01-01

    Cyclie crack resistance of transition zone in austenitic cladding steel 15Kh2MFA joint is studied, taking into account the geometry of fatigue cracks, fracture micromechanism and crack closure effect. Kinetics of crack development from the cladding to the basic metal and vice versa is considered. Microstructure of transition zone is investigated. The results obtained are considered as applied to WWER. It is emphasized, that the braking of fatigue cracks is observed at low asymmetry of loading cycle. Increased loading asymmetry accelerates sharply the alloy fracture due to the growth of subcladding crack, at that, the direction of crack propagation and the structure of transition zone are not of great importance

  17. Investigation into the Cyclic Strength of the Bodies of Steam Shutoff Valves from 10Kh9MFB-Sh Steel

    Science.gov (United States)

    Skorobogatykh, V. N.; Kunavin, S. A.; Prudnikov, D. A.; Shchenkova, I. A.; Bazhenov, A. M.; Zadoinyi, V. A.; Starkovskii, G. L.

    2018-02-01

    Steam shutoff valves are operated under complex loading conditions at thermal and nuclear power stations. In addition to exposure to high temperature and stresses resulting in fatigue, these valves are subjected to cyclic loads in heating-up-cooling down, opening-closing, etc. cycles. The number of these cycles to be specified in designing the valves should not exceed the maximum allowable value. Hence, the problem of cyclic failure rate of steam shutoff valve bodies is critical. This paper continues the previous publications about properties of the construction material for steam shutoff valve bodies (grade 10Kh9MFB-Sh steel) produced by electroslag melting and gives the results of investigation into the cyclic strength of this material. Fatigue curves for the steal used for manufacturing steam shutoff valve bodies are presented. The experimental data are compared with the calculated fatigue curves plotted using the procedures outlined in PNAE G-002-986 and RD 10-249-98. It is confirmed that these procedures may be used in designing valve bodies from 10Kh9MFB-Sh steel. The effect of the cyclic damage after preliminary cyclic loading of the specimens according to the prescribed load conditions on the high-temperature strength of the steel is examined. The influence of cyclic failure rate on the long-term strength was investigated using cylindrical specimens with a smooth working section in the as-made conditions and after two regimes of preliminary cyclic loading (training) at a working temperature of 570°C and the number of load cycles exceeding the design value, which was 2 × 103 cycles. The experiments corroborated that the material (10Kh9MFB-Sh steel) of the body manufactured by the method of electroslag melting had high resistance to cyclic failure rate. No effect of cyclic damages in the metal of the investigated specimens on the high-temperature strength has been found.

  18. Metallographical procedure for detecting carburized layer in the 12Kh18N10T steel tubes

    International Nuclear Information System (INIS)

    Najmark, S.I.; Shmalenyuk, R.P.

    1977-01-01

    The various causes of the tendency to intercrystalline corrosion of stainless steel tubing were studied. 12Kh18N10T steel tube specimens were metallographically investigated to reveal the presence and depth of the carburized layer. Unlubricated specimens and specimens with the graphite-saltpeter lubrication applied on them were austenized in the temperature range from 950 to 1250 deg C and then exposed to a provoking anneal at 650 deg C for 24 h. All the lubricated specimens showed a carbide network along grain boundaries and intercrystalline cracks. The specimens treated without lubrication had no cracks. The method offered can differentiate poor tube cleaning and the undesirable effect of other processing steps on the tubes

  19. The effect of thermal treatment on corrosion properties of 0Kh15N16M3B stainless steel tested in the N2O4 boiling medium

    International Nuclear Information System (INIS)

    Kamenev, A.Ya.; Kopets, Z.V.; Mel'nikova, N.N.; Dergaj, A.M.; Fedyushin, E.E.

    1985-01-01

    The experimental data on the effect of thermal treatment on corrosion properties of stainless steel 00Kh16n15m3b tested in the N 2 O 4 boiling medium at 8.0 MPa and 433 K are presented. The electron microscope data on steel microstructure after different heat treatments and phase composition of oxide films emerging at corrosion test are given. It is shown, that the rise of the heat treatment temperature from 823 up to 1023 K increases total corrosion of 00Kh16n15m3b steel under given test conditions and practically does't affect intercrystalline corrosion. Developed oxide layers are of deposited nature and doesn't affect markedly the rate of progress of the corrosive processes. Taking into account high chromium volatility in vacuum one can assume that at the initial stages of the coolant effect, the process of depletion of steel surface by chromium durng heat treatment affects markedly steel corrosion stability

  20. Features of argon-arc welding of aluminium alloy AD1 to stainless steel 12Kh18N10T

    International Nuclear Information System (INIS)

    Sadov, I.I.

    1982-01-01

    Welding of pipes made of the 12Kh18N10T stainless steel and the AD1 aluminium alloy is proposed to perform using one-sided aluminizing. It is recommended to use shields in order to protect internal and external surfaces of pipes, aluminizing of which is impossible. It is shown that developed technological process for welded joints made of aluminium and stainless steel for cryogenic apparatus permits to create light-duty cryostat assembly using aluminium alloys instead of copper alloys, to increase reliability of apparatus (usage of welded joints instead of soldered ones), and to improve labour conditions

  1. Effect of heat treatment and plastic deformation on the structure and the mechanical properties of nitrogen-bearing 04N9Kh2A steel

    Science.gov (United States)

    Blinov, V. M.; Bannykh, O. A.; Lukin, E. I.; Kostina, M. V.; Blinov, E. V.

    2014-11-01

    The effect of the conditions of heat treatment and plastic deformation on the structure and the mechanical properties of low-carbon martensitic nickel steel (9 wt % Ni) with an overequilibrium nitrogen content is studied. The limiting strain to failure of 04N9Kh2A steel is found to be 40% at a rolling temperature of 20°C and 80% at a rolling temperature of 900°C. Significant strengthening of the steel (σ0.2 = 1089 MPa) is obtained after rolling at a reduction of 40% at 20°C. The start and final temperatures of the α → γ transformation on heating and those of the γ → α transformation on cooling are determined by dilatometry. The specific features of the formation of the steel structure have been revealed as functions of the annealing and tempering temperatures. Electron-microscopic studies show that, after quenching from 850°C and tempering at 600°C for 1 h, the structure contains packet martensite with thin interlayers of retained austenite between martensite crystals. The strength of the nitrogen-bearing 04N9Kh2A steel after quenching from 850 and 900°C, cooling in water, and subsequent tempering at 500°C for 1 h is significantly higher than that of carboncontaining 0H9 steel used in cryogenic engineering.

  2. Effect of hydrostatic pressure on phase transformations in Kh17N8 steel during deformation

    International Nuclear Information System (INIS)

    Eshchenko, R.N.; Teplov, V.A.

    1984-01-01

    The phase composition and structure of Kh17N8 steel strained to different degrees under atmospheric pressure and 1700 MPa are investigated. It has been found that deformation at 1700 MPa causes α and epsilon-martensite formation, the same deformation under atmospheric pressure - only α-martensite formation. The amount of the formed α-martensite is not changed with application of hydrostatic pressure. Electron-microscopic observations have shown that the dispersion of α-martensite formed under pressure is higher than in the absence of pressure; no interconnection in formation of α and epsilon-martensite in samples strained under pressure has been observed

  3. Additional materials for welding of the EP99 heat resisting alloy with the EI868 alloy and 12Kh18N9T steel

    International Nuclear Information System (INIS)

    Sorokin, L.I.; Filippova, S.P.; Petrova, L.A.

    1978-01-01

    Presented are the results of the studies aimed at selecting an additive material for argon-arc welding process involving heat-resistant nickel EP99 alloy to be welded to the EI868 alloy and 12Kh18N9T steel. As the additive material use was made of wire made of nickel-chromium alloys and covered electrodes made of the EP367 alloy with additions of tungsten. It has been established that in order to improve the resistance of metal to hot-crack formation during argon arc welding of the EP99 alloy with the EI868 alloy, it is advisable to use an additive material of the EP533 alloy, and while welding the same alloy with the 12Kh18N9T steel, filler wire of the EP367 alloy is recommended

  4. Effect of silicon on the structure, tribological behaviour, and mechanical properties of nitrogen-containing chromium-manganese austenitic steels

    International Nuclear Information System (INIS)

    Korshunov, L.G.; Chernenko, N.L.; Gojkhenberg, Yu.N.

    2003-01-01

    The effect of silicon in quantity of 3.5-4.5 mass. % on tribological behaviour is studied for nitrogen-bearing (0.20-0.52 mass. % of nitrogen) chromium-manganese austenitic steels (10Kh15G23S4A0.20, 10Kh16G17N3S4A0.30, 10Kh19G20NS4A0.50, 12Kh19G19NS2A0.50, 10Kh18G19A0.50, 08Kh16G8N10S4A0.18). Mechanical properties and corrosion resistance of the steels are determined. Using metallographic, x-ray diffraction and electron microscopical methods a study is made into structural transformations running in the steels considered under friction and static tension. It is shown that additional silicon alloying of nitrogen-bearing chromium-manganese austenitic steels results in an essential increase of adhesion wear resistance of the materials on retention of low friction coefficient (f=0.25-0.33). A strong silicon effect on steel tribological behaviour is related with planar slip activation and with an increase of austenite strength and heat resistance [ru

  5. Effect of agressive medium movement of local corrosion of the steel - 12Kh18N10T

    International Nuclear Information System (INIS)

    Makartsev, V.V.; Pakhomov, V.S.; Abramova, I.M.

    1980-01-01

    The effect of agressive medium movement on the formation of pitting corrosion of the 12Kh18N10T stainless steel in the acidic chloride-nitrate solution at room temperature is studied. It is established that the agressive medium movement hinders the formation of pitting corrosion at potentials more negative than +0.4 V and practically does not affect it at more positive potentials. The investigations have been carried out on a disc electrode rotating at a speed from 0 to 2000 rot./min

  6. Effect of partial oxygen pressure on physicochemical properties of Kh18N10T steel at isothermal oxidation. Vliyanie partsial'nogo davleniya kisloroda na fiziko-khimicheskie svojstva poverkhnosti stali Kh18N10T pri izotermicheskom okislenii

    Energy Technology Data Exchange (ETDEWEB)

    Alekseev, V N; Oshe, E K; Fokin, M N; Bogdanova, S V; Loskutov, A I [AN SSSR, Moscow (USSR). Inst. Fizicheskoj Khimii

    1990-10-01

    Auger-electron spectroscopy, photoelectric polarization, conductometry methods have been used to analyze chemical and defect composition of surface oxide layers, formed on stainless steel Kh18N10T in vacuum (10{sup -9} - 10{sup -2} torr) and at temperatures 593-673 K. The boundary conditions of manifestation of extermal behaviour of the dependence of the surface oxide growth rate at isothermal oxidation of this steel are determined. The relation between passivation properties of the surface oxide and the magnitude of the edge angle of the surface wetting with molten tin is revealed.

  7. Quality of austenite chrome-nickel steel made by gas-oxygen refining

    International Nuclear Information System (INIS)

    Fel'dgandler, Eh.G.; Levin, F.L.; Moshkevich, E.A.; Shifrin, Eh.V.; Movshovich, V.S.; Pargamonov, E.A.

    1991-01-01

    Properties and structure were investigated of austenitic 03Kh18N11 and 08KhN10T steels melted at gas oxygen refining aggregates. It was established that mechanical and corrosion properties of rolling of such steels were in agreement with standard properties of metal of open melting. Sheet 08Kh18N10T steel has the level of strength and plasticity regulated for 12Kh18N10T steel. As steel of 08Kh18N10T holds the complex of high mechanical and corrosion properties, 08Kh18N10T is recommended to be replace by 12Kh18N10T with the aim of decrease of titanium usage and increase of process efficiency

  8. Effect of boron control of environment on corrosion and resistance to low-cycle corrosion fatigue in structural steels

    International Nuclear Information System (INIS)

    Babej, Yu.I.; Zhitkov, V.V.; Zvezdin, Yu.I.; Liskevich, I.Yu.; Nazarov, A.A.

    1982-01-01

    Tests of the specimens on total, contact and crevice corrosion, corrosion cracking and low-cycle fatigue are conducted for determination of corrosion and corrosion-fatigue characteristics in the 15Kh3NMFA, 10N3MFA, 10Kh16N4B, 05Kh13N6M2 structural steels, used in energetics. The environment is subjected to boron control and contacting with atmosphere for simulation of stop and operation modes of the facility. The experiments are carried out in the distilled water with 12g/l H 3 BO 3 and 10 mg/l Cl' at 25, 60, 100 deg C under contacting with atmosphere. It is established, that the pearlitic steels 15Kh3NMFA, 10N3MFA, as well as transition and martensitic 05Kh13N6M2 and 10Kh16N4B steels are highly stable to total, crevice and contact corrosion at the high parameters of aqueous boron-containing medium. Steel resistance to low-cycle fracture decreases slightly under the conditions similar to the operation ones, in the water with 12 g/l H 3 BO 3 . Durability of the pearlitic steels at the simulation of stop conditions decreases more noticeably, crack formation as a rule, initiating from corrosion spots

  9. On choice of tempered steels

    International Nuclear Information System (INIS)

    Govorov, A.A.; Pan'shin, I.F.; Rakhmanov, V.I.

    1978-01-01

    For the purpose of developing a graphical method for choosing structural steels, a change in the propagation work of a crack and in the critical temperature of brittleness of 40, 40Kh, 40KhN, and 40KhNM steels, was examined depending on the hardness after hardening and tempering. A diagram enabling to choose the grade of steel for making an article of known dimensions according to the preset values of its mechanical properties has been plotted. The developed selection scheme takes into account the hardenability of steels and the influence of the hardness after thermal treatment on the cold-shortness of steel

  10. Radiation embrittlement of WWER 440 pressure vessel steel and of some improved steels by western producers

    International Nuclear Information System (INIS)

    Koutsky, J.; Vacek, M.; Stoces, B.; Pav, T.; Otruba, J.; Novosad, P.; Brumovsky, M.

    1982-01-01

    The resistance was studied of Cr-Mo-V type steel 15Kh2MFA to radiation embrittlement at an irradiation temperature of around 288 degC. Studied was the steel used for the manufacture of the pressure vessel of the Paks nuclear reactor in Hungary. The obtained results of radiation embrittlement and hardening of steel 15Kh2MFA were compared with similar values of Mn-Ni-Mo type steels A 533-B and A 508 manufactured by leading western manufacturers within the international research programme coordinated by the IAEA. It was found that the resistance of steel 15Kh2MFA to radiation embrittlement is comparable with steels A 533-B and A 508 by western manufacturers. (author)

  11. Low-temperature cyclic cracking resistance of Fe-Cr-Ni and Fe-Cr-Mn steels welded joints

    International Nuclear Information System (INIS)

    Ostash, O.P.; Zhmur-Klimenko, V.T.; Yarema, S.Ya.; Yushchenko, K.A.; Strok, L.P.; Belotserkovets, V.I.

    1983-01-01

    Results of further investigations into regularities of development of low-temperature fatigue fracture of welded oints in 07Kh13G20AN4 steel are presented, they are compared with analogous data traditional cryogenic 0Kh18N10T and 03Kh13AG19 steels. Welded joints have been prepared by means of automatic V-like level arc Welding of plates; 0Kh18N10T and 07Kh13G20AN4 steels have been welded by means of sv-04Kh19N9 wire, 03Kh13AG19 steel-by means of sv-07Kh13AG19 wire. Tests at almost zero (asymmetry coefficient R=0.05) cycle of extension at 15-20 Hz frequency have been conducted on 5 mm thick disk samples at 20 deg C and - 160 deg C according to the given methods. It is shown that by cyclic crack resistance of welded joint zones of 0Kh18N10T steel and chromium-manganese steels at normal temperature the 07Kh13G20AN4 steel exceeds 0Kh18N10T steel, at low temperature it yields to 0Kh18N10T only by fracture toughness of heat affected zones HAZ and weld metal (ne). 07Kh13G20AN4 steel and its welded joints as most hardened and cheap may be a good substituent for 0Kh18N10T steel. Optimization of WM alloying for increase of its cyclic fracture toughness at cryogenic temperatures is necessary

  12. Effect of metal properties of casts of steel-15Kh1M1FL on the crack resistance at 565 deg C

    International Nuclear Information System (INIS)

    Gladshtejn, V.I.; Sheshenev, M.F.

    1976-01-01

    Results are given of prolonged tests of the metal of industrial casts with various fluidity limits. It has been shown experimentally that a quite satisfactory crack resistance is characteristic of a metal with a fluidity limit in the range 30-50 kgf/mm 2 . Metallographic studies have been conducted. Upon variation of the structure and properties of the 15Kh1M1FL steel during operation, the rate of growth of small cracks (up to 2.0 mm) decreases almost by 3 orders of ten (from 1.4x10 -4 to 2.0x10 -7 mm/hour). Subsequent structural changes during prolonged operation (over 50000 hours) result in a gradual increase in the rate of crack growth. At the same time resistance towards appearance of the impermissible high rate of the crack growth, Ksub(10sup(-3)), diminishes monotonically with the operation time. The metal of industrial 15Kh1M1FL steel casts has good crack resistance (Ksub(10sup(-3)) =30-70 kgf/mmsup(3/2) and Vsub(ef) =) kgf/mm 2 ) and a satisfactory local plasticity (critical opening being no more than 0.20 mm for 10 3 hours)

  13. KH in Paraffin - KH(P): A Useful Base for Organic Synthesis

    Science.gov (United States)

    Taber, Douglass F.; Nelson, Christopher G.

    2011-01-01

    The preparation of KH as a one:one homogenate with paraffin, termed KH(P), is reported. KH(P), a solid at room temperature, is stable without special handling. On suspension in THF with a phosphonium salt, KH(P) rapidly generates the ylide. Wittig condensation with aromatic, aliphatic and α, β-unsaturated aldehydes proceeds with high Z-selectivity. KH(P) should be a generally useful base for organic synthesis. PMID:17081034

  14. Superheat effect on bainite steel hardenability

    International Nuclear Information System (INIS)

    Kubachek, V.V.; Sklyuev, P.V.

    1978-01-01

    The bainite hardenability of 34KhN1M and 35 KhN1M2Ph steels has been investigated by the end-face hardening technique. It is established that, as the temperature of austenitization rises from 900 to 1280 deg C, the temperature of bainite transformation increases and bainite hardenability of the steels falls off. A repeated slow heating to 900 deg C of previously overheated 34KhN1M steel breaks up grain, lowers the temperature of the bainite transformation and raises the hardenability to values obtained with ordinary hardening from 900 deg C. A similar heating of previously overheated 35KhN1M2Ph steel is accompanied by restoration of initial coarse grains and maintenance of both the elevated bainite transformation temperature and to lower hardenability corresponding to hardening from the temperature of previous overheating

  15. Electron beam welding of flanges with tubular shafts of steel 40KhNMA

    International Nuclear Information System (INIS)

    Leskov, G.I.; Zhivaga, L.I.; Shipitsyn, B.N.; Savichev, R.V.

    1975-01-01

    The results are presented of elaborating the technological process for the electron beam welding of flanges with a tube of the 40KhNMA steel and of investigation into the quality of the welded joints. A welded piece has been fabricated conforming to the technology suggested observing the parameters worked-out in the following sequence: assembling the piece; pre-welding of the edges in some points; welding; high tempering; welds quality control; removal of the seam reinforcement inside of the tube and the weld root to the depth of 2 mm; quenching; tempering; welds quality control; finishing. The welds quality control consists in visual inspection, ultrasonic testing, magnetic flaw detection, as well as X-ray and metallographic analyses. The mechanical properties are studied on notched samples cut out of the welded joints. The test results have shown that the mechanical properties of the welded joints meet the requirements on the same level with the base metal

  16. Experience manufacturing and properties of the high-strength corrosion-resistant magnetic 03Kh12K12D2 steel

    International Nuclear Information System (INIS)

    Fel'dgandler, Eh.G.; Moshkevich, E.I.; Bakuma, S.F.; Bulat, S.I.; Tikhonenko, V.D.

    1976-01-01

    In industrial conditions, steel 03Kh12K12D2 (DI48-VD) was melted in a 7-tinduction furnace with subsequent vacuum arc remelting. Ingots of dia 500 and 630 mm were forged into slabs and forgings. The slabs were rolled into sheets, 40 mm thick, and the forgings were rolled into sectional shapes. To obtain the optimum mechanical, corrosion, and magnetic properties, the metal was annealed at 600 deg C (10 hr) and 650 deg C (5 and 10 hr). The developed melting and remelting process enabled to obtain steel meeting all the requirements as for the chemical composition, workability, and mechanical magnetic properties. On testing in water with high parameters (200 deg C, 16 kgf/cm 2 ) and in synthetic sea water (70-90 deg C) the corrosion rate did not exceed 1 μm per year

  17. Effect of Cr, Ni, and Mo additions on the susceptibility of the 0Kh6n7m7c steel to hot cracking

    International Nuclear Information System (INIS)

    Tolstykh, L.G.; Pryakhin, A.V.; Popov, A.N.; Usynin, V.F.

    1977-01-01

    The effect of chromium, molybdenum, and nickel on the tendency of surfacing materials to form hot cracks (Vsub(kp) was studied using the mathematical statistics method. The St3 steel and 38KhN3MFA steel were used in the study. A device facilitating the hot cracking tendency test procedure was developed. It was found that, in the concentration range involved, Ni and Mo produce no effect on Vsub(kp), and Cr enhances it. A new powder wire, PP-OKh7N8M6S, capable of increasing surface material resistance by 1.5-2 times, has been developed

  18. Effect of hot rolling on the structure and the mechanical properties of nitrogen-bearing austenitic-martensitic 14Kh15AN4M steel

    Science.gov (United States)

    Bannykh, O. A.; Betsofen, S. Ya.; Lukin, E. I.; Blinov, V. M.; Voznesenskaya, N. M.; Tonysheva, O. A.; Blinov, E. V.

    2016-04-01

    The effect of the rolling temperature and strain on the structure and the properties of corrosionresistant austenitic-martensitic 14Kh15AN4M steel is studied. The steel is shown to exhibit high ductility: upon rolling in the temperature range 700-1100°C at a reduction per pass up to 80%, wedge steel specimens are uniformly deformed along and across the rolling direction without cracking and other surface defects. Subsequent cold treatment and low-temperature tempering ensure a high hardness of the steel (50-56 HRC). Austenite mainly contributes to the hardening upon rolling in the temperature range 700-800°C at a reduction of 50-70%, and martensite makes the main contribution at higher temperatures and lower strains. Texture does not form under the chosen deformation conditions, which indicates dynamic recrystallization with the nucleation and growth of grains having no preferential orientation.

  19. Fatigue resistance of Cr-Ni-Mo-V steel

    International Nuclear Information System (INIS)

    Naumchenkov, N.E.; Filimonova, O.V.; Borisov, I.A.

    1985-01-01

    A study was made on the effect of additional alloying (Ni, Ni+Co), stress concentration, surface plastic strain on fatigue resistance of rotor steel of Cr-Ni-Mo-V-composition. It is shown that the steel with decreased carbon content possesses high complex of mechanical properties. Fatigue characteristics are not inferior to similar characteristics of steels of 25KhN3MFA type. Additional alloying of the steel containing 0.11...0.17% C and 4.5...4.7% N:, with niobium separately or niobium and cobalt in combination enabled to improve fatigue resistance of samles up to 25%. Strengthening of stress concentration zones by surface plastic strain is recommended for improving rotor suppporting 'nower under cyclic loading

  20. Steel corrosion in tributyl phosphate in the presence of water and ethyl mercaptan

    International Nuclear Information System (INIS)

    Pischik, L.M.; Tsinman, A.I.

    1979-01-01

    Studied is the corrosion of steels St3, 15Kh5M, 08Kh13, 10Kh14G14N4T, 08Kh18G8N2T, 10Kh17N13M2T in TBP, in mixtures of TBP with ethyl mercaptan (EM) and two-phase systems TBP-water and TBP-water-EM at 50-150 deg. In pure TBP St3 corrosion rate is low even at 150 deg. In the presence of water St 3 strongly corrodes at above 50 deg temperature in organic and water layers and also in gas phase. The steel-08Kh18G8N2T at 90 deg in acid TBP is passive and its corrosion rate is lower than 0.01 mm/year. In identical conditions the resistance of stainless steels increases together with chromium content but in TBP with acid number 100 and above at 150 deg all tested steels including steel-10Kh17N13M2T are slightly resistant. Thus, even in absence of corrosion active additions of EM the mixture of TBP-water at higher temperature is agressive in relation not only to carbon steel but also to stainless steels

  1. Changes in structure and phase composition of chromium diffusion layer on stainless steels after long annealing

    International Nuclear Information System (INIS)

    Knyazev, E.V.; Voshedchenko, B.M.; Voskresenskij, Yu.A.

    1985-01-01

    A study was made on the effect of elevated temperatures UU and long holdings at heat on structure, phase composition and properties of chromium diffusion layer on austenitic chromium-nickel stainless steels 10Kh18N10TVD, 10Kh15N30M4B, 10Kh11N23T3MR, 10Kh21N28V6M3. The following mechanism of processes taking place in diffusion chromium layer is presented. The steady drop of chromium concentrations is observed after diffusion saturation. Chromium redistribution related with system transformation to more equilibrium state and simultaneous decarburization of steel surfaces takes place in diffusion layers of 10Kh15N30M4B and 10Kh21N28V6M3 steels after annealing at different temperatures and holdings at heat. Decarburization of steel surface layers is practically excluded in diffusion layers of 10Kh18N10T-VD and 10Kh11N23T3MR steels. Diffusion chromium-saturated layer stays effective only on 10Kh18N10T-VD and 10Kh11N23T3MR steels on heating up to 1000 deq C with holding up to 250 h

  2. The effect of thermoplastic treatment regimes on the microplastic strain of nitrogen-containing steel Kh21G10N7MBF

    International Nuclear Information System (INIS)

    Bannykh, O.A.; Blinov, V.M.; Kostina, M.V.; Grachev, S.V.; Mal'tseva, L.A.

    2005-01-01

    A study is made into the influence of a percentage reduction during cold rolling and subsequent holdings at heat on development of microplastic deformation when bending sheet specimens of stainless austenitic high-nitrogen steel Kh21G10N7MBF. It is revealed that a maximum value of apparent limit of elasticity (∼1800 MPa) is attained due to plastic deformation by rolling at 20 Deg C with a total percentage reduction of 60 % and subsequent aging at 500 Deg C for 1-4 h [ru

  3. Effect of austenitization conditions on kinetics of isothermal transformation of austenite of structural steels

    International Nuclear Information System (INIS)

    Konopleva, E.V.; Bayazitov, V.M.; Abramov, O.V.; Kozlova, A.G.

    1987-01-01

    Effect of austenization of kinetics of pearlite and bainite transformations for steels with different carbon content differing by alloying character and degree has been investigated. Austenization temperature increase is shown to leads to retardation of ferrite-pearlite transformation in low- and medium-carbon alloyed steels. Step-like holding in the region of austenite stable state (850, 950 deg) after high-temperature heating (1100 deg C) increases the rate of transformation partially recovering its kinetics and decomposition velocity after low-temperature heating in steels alloyed advantageously with carbide-forming elements (08Kh2G2F, 30Kh3) and does not affect kinetics in the 35Kh, 30KhGSN2A, 45N5 steels. Increase of heating temperature and growth of an austenite grain cause considerable acceleration of bainite transformation, increase of the temperaure of bainite transformation beginning and increase of the transformation amplitude in the 08Kh2G2F, 30Kh3 steels and affect weakly kinetics in steels with mixed alloying (30KhGSN2A) or low-alloy one (35Kh). The bainite transformation rate in the 45N5 steelite does not depend on austenization. The effect of additional acceleration of bainite transformation as a result holding after high-temperature heating in those steels, where activation of transformation occurs with increase of heating temperature

  4. Investigation of Creep Processes and Microdamages in 10Kh9V2MFBR-Sh High-Chromium Steel

    Science.gov (United States)

    Grin', E. A.; Pchelintsev, A. V.

    2018-01-01

    During the modernization and the new construction of power units at TPPs in Russia, high-chromium martensitic steels with higher heat-resistant properties than the traditional perlite steels are increasingly used as structural materials. High-chromium steels have a necessary regulatory support for their use in domestic power engineering. However, up to the present time, the issue of assessing the quality of these steels at the analysis of their state during long-term operation remains open. The article proposed is one of the first attempts to create a system of quality criteria for martensitic steels based on their microdamage parameters. Tests were carried out on the long-term strength and creep of samples from 10Kh9V2MFBR-Sh steel at high temperatures with the construction of creep curves in relative coordinates "deformation related to the deformation of fracture, current time related to time to failure." For some samples, the tests were interrupted and the metal was subjected to metallographic studies consisting of the analysis of microdamage with reference to the accumulated creep strain. It has been shown experimentally that the deformation curve of high-chromium steel differs from the analogous curve of pearlitic steel by a longer and flat section of steady creep and by a sharper transition to the third accelerated creep stage, which has a very short time period (approximately 10% of the total durability). The tendency to the increase in the microdamage of the structure of steel as the accumulated creep strain increases with time was confirmed. The beginning of transition to the final creep phase is characterized by the formation of contours of future pore chains and by the appearance of individual large pores of up to 6 μm in size, the presence of which in the microstructure of the martensitic steel indicates a very significant accumulation of creep strain, and corresponds to the predestruction stage of metal. It is necessary to continue the research to

  5. Development and industrial mastering hot rolling procedure for low-ductile steels and alloys

    International Nuclear Information System (INIS)

    Degterenko, V.K.; Sokolov, V.A.

    1980-01-01

    The technique for the development of the sheet hot rolling procedure for low-ductile steels and alloys (0Kh17N14M2, 12Kh21N5T, 20Kh25N20C2,40Kh13, 36NKhTYu etc.) is proposed, using plastometer which permits to obtain the data on the deformation resistance in the wide range of temperatures (800-1300 deg C), of deformation degrees (0.1-0.3) and deformation rates (0.001-300 c -1 ). With the help of the plastometric data processed on the computer the calculation of the rolling regimes for the sheet with improved surface quality is carried out at the more uniform loading on the mill stands

  6. Reliability and durability of the 12Kh1MF steel tubes of electroslag remelting and their welded joints

    International Nuclear Information System (INIS)

    Lanskaya, K.A.; Kulikova, L.V.; Mazel', R.E.; Khromchenko, F.A.; Strizhenova, V.F.

    1978-01-01

    Results of investigating the positive effect of electrolag remelting (ESR) on the properties of the base metal and welded joint of the 12Kh1MF steel steam pipes with the aim of increasing their durability up to 20,000 hrs, are presented. To estimate the quality and properties of tube billet metal, microstructure, content and nature of nonmetallic inclusions, content of gases, austenite grain size, austenite transformations during continuous cooling, metal ductility, mechanical properties at different temperatures and heat resisting properties, have been investigated. It is established, that the base metal in tubes of electroslag remelting possess higher heat resistance, while welded joints besides, have high deformability and resistance to brittle fracture

  7. Strength of low-carbon rotor steel

    International Nuclear Information System (INIS)

    Voropaev, V.I.; Filimonov, O.V.; Borisov, I.A.

    1988-01-01

    The results of studying the effect of chemical composition and thermal treatment regimes on the structural strength of steels of the 25KhN3MFA type are presented. It is shown that alloying with niobium from 0.01 to 0.08% steels with the increased nickel content (4.2-4.5%) contributes to the increase of structural strength and reduction of semibrittleness temperature. To obtain high values of strength and plastic properties cooling with the rate of 10 3 -10 5 K/hr is recommended

  8. Influence of quantity of non-martensite products of transformation on resistance to fracture of improving structural steel

    International Nuclear Information System (INIS)

    Gulyaev, A.P.; Golovanenko, Yu.S.; Zikeev, V.N.

    1978-01-01

    18KhNMFA, low-carbon, alloyed steel and 42KhMFA medium-carbon, alloyed steel have been examined. For the purpose of obtaining different structures in hardening the steel, different cooling rates, different temperatures and isothermal holding times are applied. The following has been shown: on tempering to the same hardness (HV 300), the presence of non-martensite structures in hardened state does not practically influence the standard mechanical properties of steel (sigmasub(B), sigmasub(0.2), delta, PSI). The resistance of steel to the brittle failure is enhanced by the uniform, fine-disperse distribution of the carbide phase in the structure of lower bainite (up to 80 % bainite in martensite for 42KhMF steel to be improved), as well as strongly fragmented packages of rack martensite-bainite (up to 50 % lower bainite in martensite of 18KhNMFA steel). The formation of the upper bainite in the structure of the hardened steels 18KhNMFA and 42KhMF results on tempering in the formation of coarse, non-uniform, branched carbide inclusions, and this, in its turn, leads to raising the cold-shortness threshold and to lowering the amount of work as required for propagation of a crack. The presence of ferritic-pearlitic structures in the structural steels hardened to martensite and bainite results in reducing the resistance of steel to the brittle failure; the presence of every 10 % ferritic-pearlitic component in martensite of the structural steels 18KhNMFA and 42KhMFA to be thermally improved, raises T 50 by 8 deg and 20 deg C, respectively

  9. Study of cast and thermo-mechanically strengthened chromium-nickel nitrogen-containing steel

    International Nuclear Information System (INIS)

    Prokoshkina, V.G.; Kaputkina, L.M.; Svyazhin, A.G.

    2000-01-01

    The effect of nitrogen on the structure and strength of corrosion-resistant chromium-nickel steels after thermal and thermomechanical treatment is studied. The 06Kh15N7AD and 07Kh15N7DAMB steels alloying by nitrogen was accomplished through the basic composition steels remelting in the molecular nitrogen atmosphere under the pressure of 0.1-2.5 MPa. The 02Kh15N5DAF and 05Kh15N5DAM steels ingots were obtained through melting in a plasma furnace under the nitrogen pressure of 0.4MPA. The high-temperature thermomechanical treatment (HTMT) was performed by rolling with preliminary blanks heating up to 1050 deg C and the rolling end temperature not below 950 deg C. It is shown, that the HTMT of the nitrogen-containing steels makes it possible to obtain strength characteristics by 1.5 times exceeding the properties of traditionally applicable corrosion-resistant steels, whereby sufficiently high plasticity of the nitrogen-containing steel is retained [ru

  10. The effect of chromium diffusion redistribution on wear resistance of carburized 3Kh13 steel

    International Nuclear Information System (INIS)

    Shcherbedinskij, G.V.; Shumakov, A.I.; Zemskij, S.V.; Pereverzev, V.M.

    1977-01-01

    The redistribution of chromium in steel 3Kh13 on carburization in a high-activity carburizer and the wear-resistance of the steel have been investigated. Surface layers with an increased chromium concentration show the highest wear-resistance. The chromium content in the surface layer increases due to its diffusion from the interior. The distribution of carbon and chromium in the carburized layers has been studied with the aid of the radioactive isotope 14 C by the method of layer-by-layer spectral analysis on a vacuum quantometer, layer-by-layer chemical and X-ray structure analysis. The composition of the carbides has been determined by physicochemical analysis. It has been established that the carburized layer can be divided into four zones with respect to its phase composition: first zone - hematite and spinal with 0.5-2.0% C; second zone - solid carbides (Fe,Cr) 7 C 3 ; up to 5% C; third zone - globular carbides in a troostite matrix (Cr,Fe) 7 C 3 and Cr 23 C 6 ; up to 3.5% C; fourth, transitional, zone - troostite carbide mixture Cr 23 C 6 ; up to 1% C. The chromium diffusion in the carburized layer is faster than in the initial austenite. The chromium counterdiffusion is due to the development of a zone of solid carbides M 7 C 3

  11. Effect of neutron irradiation on the properties of the repair welds of the 15Kh2MFA steel

    International Nuclear Information System (INIS)

    Morozov, A.M.; Khachaturyants, L.V.

    1986-01-01

    The authors studied the effect of neutron irradiation on the tendency of the metal belonging to the heat affected zone of the weld toward brittle fracture (an increase in the critical temperature of brittleness). For comparison, the authors studied the radiation embrittlement of the original base metal (steel 15Kh2MFA) subjected to the conventional heat treatment of the reactor frames consisting of hardening and high-temperature tempering. Along with these materials, the radiational embrittlement of the base metal in the rehardened condition without tempering was studied. It was concluded that the presence of the regions repaired according to this technology and located in the frame at the level of the reactor core does not pose the problem of decreased resistance to brittle fracture

  12. Coarsening of (Fe, Cr)23C6 carbide phase on the tempering of 14Kh17N2 chromium-nickel steel

    International Nuclear Information System (INIS)

    Psarev, V.I.

    2002-01-01

    Paper lists the results of computer analysis of distribution according to sizes (Fe, Cr) 23 C 6 microparticles resulting from 14Kh17N2 steel tempering under 700 Deg C. Data were obtained at the maximum beneficial magnification of a light microscope. The mentioned curves of distribution densities are characterized by more reliable run from most permissible sizes of dispersed particles. Application of general rules of distributions and of previously elaborated procedure to identify experimental histograms with theoretical distributions enables to derive valuable information on dynamics of coarsening of a disperse phase in this case, as well [ru

  13. Effect of nickel and MnS inclusions in the metal on the pitting corrosion of low-carbon stainless steels

    International Nuclear Information System (INIS)

    Frejman, L.I.; Nguen, The Dong; Volkov, D.E.; Konnov, Yu.P.

    1986-01-01

    The resistance to pitting corrosion of steels on the 03Kh17-03Kh18 base containing up to 20 % Ni at different levels of S and Mn impurities contamination is investigated. It is shown that up to 50 % of nickel introduced into ordinary steels with 5-6 % Ni is spent to compensate the resistance decrease caused by MnS inclusions. Full compensation is not attained even in the 10-20 %. Ni range in which nickel practically does not affect the resistance of neither ordinary, nor pure (without MnS) steels. Titanium introduction into ordinary steel on the Kh22N6 base permits to surpass the level of 03Kh17N3 pure steel resistance and attain the level of 03Kh17N6 pure steel almost by all characteristics (including passivated characteristics in sulfuric acid) besides pitting repassivity. In this property pure steels with Ni >or approx. 3 % surpass even the molybdenum containing 03Kh21NbM2T ordinary steel though they by far concede by passivation in sulfuric acid

  14. Stationary potentials and corrosion of metals and steels in sodium and potassium chloride eutectic melts saturated with hydrogen chloride

    International Nuclear Information System (INIS)

    Belov, V.N.; Ershova, T.K.; Kochergin, V.P.

    1978-01-01

    Stationary potentials have been measured at 850 deg C and corrosion rates found gravimetrically for a number of metals and steels in the eutectic NaCl-KCl melt saturated with HCl. Periodic shifts of the stationary potentials towards positive values have been established in the Ti-V-Cr-Fe-Ni, Cu-Zr-Nb-Mo, Ag-Ta-W-Pt systems, with the corrosion rate of metals decreasing in them. The stationary potentials are shown to shift towards positive values in the series: st.08 KP, st.3, Kh17N2, Kh22N6T, Kh13NChG9, 1Kh18N10T, Kh17N13M2T, OKh17N16M3T, Kh23N18, Kh25N16G7, Kh23N28M3D3T, with corrosive resistance in this series increasing

  15. On the adsorption-induced fatigue of structural steels in the presence of alcohols

    International Nuclear Information System (INIS)

    Loboiko, V.I.; Karpenko, G.V.; Vasilenko, I.I.

    1976-01-01

    The purpose of the work was to study he effect of anhydrous alcohols on the cyclic fatigue of steels in the absence of contact of the alcohol with atmospheric moisture during the testing process. A vacuum was created in the operating space and then the vacuum annealing was carried out in a bath with the sample and through metal vacuum connection the bath was filled with anhydrous alcohol. Studies were made on several construction steels (20Kh, 40Kh, 50Kh, and ShKh15); steels 40Kh, 50Kh, and ShKh15 were quenched from 840-860 0 C in oil and then tempered at 200 0 C (2 h), steel 20Kh was studied in the as-received state. It was shown that with increase in the carbon content of steel with a martensite structure, the decrease in strength in the presence of anhydrous alcohol was greater than in dry air. Experiments showed that anhydrous alcohol causes an adsorption decrease in the strength both of samples with preliminarily formed cracks and V-shaped stress concentrators and of smooth samples. The greatest adsorption effect of alcohols in our case, as in static fatigue, was observed in samples with cracks. A dependence was shown between the length of the carbon chain and the fatigue limit. This dependence indicates the monotone nature of the decrease in the fatigue limit with transfer from methyl to butyl and then to octyl alcohol

  16. Annealing effect on restoration of irradiation steel properties

    International Nuclear Information System (INIS)

    Vishkarev, O.M.; Kolesova, T.N.; Myasnikova, K.P.; Pecherin, A.M.; Shamardin, V.K.

    1986-01-01

    The effect of temperature and annealing time on the restoration of properties of the 15Kh2NMFAA and 15Kh2MFA steels after irradiation at 285 deg with the fluence of 6x10 23 neutr/m 2 (E>0.5 MeV) is studied. Microhardness (H μ ) restoration in the irradiated 15Kh2NMFAA steel is shown to start from 350 deg C annealing temperature. The complete microhardness restoration is observed at the annealing temperature of 500 deg C for 10 hours

  17. Influence of isothermal thermomechanical treatment on structure and properties of structural steels

    International Nuclear Information System (INIS)

    Smirnov, M.A.; Kaletin, A.Yu.; Schastlivthev, V.M.; Kaletina, Yu.V.

    1997-01-01

    A study is made into the structure and mechanical properties of steel 35KhGSA and 37KhN3A after isothermal hardening resulting in bainitic structure formation as well as after low-temperature thermomechanical treatment (LTTMT) combining the plastic deformation at the temperature of bainitic transformation and subsequent isothermal hardening. It is shown that LTTMT permits and essential enhancement of strength properties in steel 35KhGSA, high plasticity and impact strength being reserved. This is associated with bainitic structure refinement. In steel 37KhN3A the process of carbide formation takes place along with bainitic transformation, and LTTMT results in lesser strengthening. LTTMT is fount to not practically affect the tendency of structural steels to bainitic brittleness. This treatment promotes some shift of brittleness manifestation to lower temperatures

  18. Increasing the brittle fracture resistance in manual arc welding and heat treatment of type 12KhM steels

    International Nuclear Information System (INIS)

    Tikhonov, V.P.; Bychenkova, G.A.; Gordeev, Y.V.; Ilyuhov, C.V.

    1984-01-01

    The extensive application of heat-resisting steels is delayed by their poor weldability. Optimum technology has been developed for manual arc welding and heat treatment of structures of type 12KhM steels resulting in high cracking resistance. Trials were conducted to evaluate the efficiency of removing the structural stresses in tempering the structures. On the basis of the experimental results, it may be assumed that the toughness properties of the welded joints produced by manual arc welding can be improved by optimizing the alloying system of the weld metal, with the parent metal treated in the optimum heat treatment conditions. The aim of subsequent investigations was to assess the properties of the weld metal made with vanadium-free electrodes. It was found that the impact toughness increased two to three times; the mean hardness and the maximum hardness were both less than 220. The reduction in hardness and increase of the toughness properties of the metal are caused by the lower degree of hardening of the bulk of the grain and, consequently, by the lower concentration of plastic strain at the grain boundaries

  19. Rupture of the steel-12KH1MF under creep at temperatures close to 0,5 Tsub(melt)

    International Nuclear Information System (INIS)

    Berezina, T.G.; Ashikhmina, L.A.; Karasev, V.V.

    1976-01-01

    Optical and transmission microscopy and fractography techniques have been employed in studying the peculiarities of nucleation and growth of micropores in steel 12Kh1MF at creep. The nucleation of micropores occurs at the initial stages of creep at stress concentration points, predominantly following the retarded shear mechanism. Micropores grow by the way of diffusion, as well as following the deslocation mechanism. An important role in the process of micropore growth is played by pore opening through grain-boundary slip. Pores of 1 to 5 microns in size can be formed along grain boundaries both due to the growth of individual micropores and by coalescence of micropores at points of their concentration. Transition of the creep to the critical phase coincides with the process of the pores blending together to

  20. Fracture of ledeburitic steel during hot plastic deformation

    International Nuclear Information System (INIS)

    Nikitin, V.P.; Borisov, Yu.A.; Bulat, S.I.; Zajtsev, V.V.

    1977-01-01

    The mechanisms of the high-temperature failure of high-carbon chromium Kh6F1, Kh6T2 and Kh6VF steels and a possibility to avoid their overheating have been investigated. At 1190 deg C and over the failure occurs along boundaries of grains at points of formation of the initial portions of the liquid phase as carbides are dissolved. If after a holding at 1190-1210 deg C the steels are cooled to 1120-1150 deg C and held for a sufficiently long time, secondary carbides are formed in the eutectic areas and, if the steels are deformed, the discontinuities present a rounded shape. Holding of an overheated steel at 1120-1150 deg C ensures its satisfactory workability in rolling. By choosing adequate overheating and subsequent slight cooling conditions, it is possible not only to retain, but even to improve the plasticity of carbide high-carbon steels. The results of laboratory tests have been confirmed under industrial conditions

  1. Effect of smelt aluminium on mechanical properties of steels

    International Nuclear Information System (INIS)

    Ryabov, V.R.; Dykhno, I.S.; Deev, G.F.; Karikh, V.V.

    1987-01-01

    Effect of smelt aluminium on mechanical properties of armco-iron and 12 Kh18N10T steel is studied. It is stated that in smelt aluminium and aluminium alloy contact with armco-iron the sample ductility is decreased. Corrosion effect of smelt alluminium on (18Kh15N5AM3) steel in the form of reinforced wire in aluminium-steel KAS-1A composite material is investigted. It is stated in experiment that during smelt alluminium-steel contact interaction of heterogeneous phases takes place

  2. Local corrosion of high alloy steels under biodeposits

    International Nuclear Information System (INIS)

    Korovyakova, M.D.; Nikitin, V.M.; Speshneva, N.V.

    1999-01-01

    Impact of the bacteriozenosis different structural-functional state under biodeposits on corrosion resistance of the 12Kh18N10T and Kh18N10T high-alloy steels in the natural seawater is studied. It is shown that saturation of natural micro communities by separate aerobic and facultative-anaerobic bacterial monocultures increases corrosion resistance of these steels by their overgrow with biodeposits [ru

  3. Structural features and properties of the laser-deposited nickel alloy layer on a KhV4F tool steel after heat treatment

    Science.gov (United States)

    Shcherbakov, V. S.; Dikova, Ts. D.; Stavrev, D. S.

    2017-07-01

    The study and application of the materials that are stable in the temperature range up to 1000°C are necessary to repair forming dies operating in this range. Nickel-based alloys can be used for this purpose. The structural state of a nickel alloy layer deposited onto a KhV4F tool steel and then heat treated is investigated. KhV4F tool steel (RF GOST) samples are subjected to laser deposition using a pulsed Nd:YAG laser. A nickel-based material (0.02C-73.8Ni-2.5Nb-19.5Cr-1.9Fe-2.8Mn) is employed for laser deposition. After laser deposition, the samples are subjected to heat treatment at 400°C for 5 h, 600°C for 1 h, 800°C for 1 h, and 1000°C for 1 h. The microstructure, the phase composition, and the microhardness of the deposited layer are studied. The structure of the initial deposited layer has relatively large grains (20-40 μm in size). The morphology is characterized by a cellular-dendritic structure in the transition zone. The following two structural constituents with a characteristic dendritic structure are revealed: a supersaturated nickel-based γ solid solution and a chromium-based bcc α solid solution. In the initial state and after heat treatment, the hardness of the deposited material (210-240 HV 0.1) is lower than the hardness of the base material (400-440 HV 0.1). Only after heat treatment at 600°C for 1 h, the hardness increases to 240-250 HV0.1. Structure heredity in the form of a dendritic morphology is observed at temperatures of 400, 600, and 800°C. The following sharp change in the structural state is detected upon heat treatment at 1000°C for 1 h: the dendritic morphology changes into a typical α + γ crystalline structure. The hardness of the base material decreases significantly to 160-180 HV 0.1. The low hardness of the deposited layer implies the use of the layer material in limited volume to repair the forming surfaces of dies and molds for die casting. However, the high ductility of the deposited layer of the nickel

  4. SCC growth behavior of cast stainless steels in high-temperature water. Influences of corrosion potential, steel type, thermal aging and cold-work

    International Nuclear Information System (INIS)

    Yamada, Takuyo; Terachi, Takumi; Miyamoto, Tomoki; Arioka, Koji

    2011-01-01

    Recent studies on crack growth rate (CGR) measurement in oxygenated high-temperature pure water conditions, such as normal water chemistry (NWC) in BWRs, using compact tension (CT) type specimens have shown that stainless steel weld metal are susceptible to stress corrosion cracking (SCC). On the other hand, the authors reported that no significant SCC growth was observed on stainless steel weld metals in PWR primary water at temperatures from 250degC to 340degC. Cast austenitic stainless steels are widely used in light water reactors, and there is a similarity between welded and cast stainless steels in terms of the microstructure of the ferrite/austenite duplex structure. However, there are a few reports giving CGR data on cast stainless steels in the BWRs and PWRs. The principal purpose of this study was to examine the SCC growth behavior of cast stainless steels in simulated PWR primary water. A second objective was to examine the effects on SCC growth in hydrogenated and oxygenated water environments at 320degC of: (1) corrosion potential; (2) steels type (Mo in alloy); (3) thermal-aging (up to 400degC x 40 kh); and (4) cold-working (10%). The results were as follows: (1) No significant SCC growth was observed on all types of cast stainless steels: aged (400degC x 40 kh) of SCS14A and SCS13A and 10% cold-working, in hydrogenated (low-potential) water at 320degC. (2) Aging at 400degC x 40 kh SCS14A (10%CW) markedly accelerated the SCC growth of cast material in high-potential water at 320degC, but no significant SCC growth was observed in the hydrogenated water, even after long-term thermal aging (400degC x 40 kh). (3) Thus, cast stainless steels have excellent SCC resistance in PWR primary water. (4) On the other hand, significant SCC growth was observed on all types of cast stainless steels: 10%CW SCS14A and SCS13A, in 8 ppm-oxygenated (high-potential) water at 320degC. (5) No large difference in SCC growth was observed between SCS14A (Mo) and SCS13A. (6) No

  5. Nitrogen effect on the tendency of Cr-Ni-MN steels to delayed fracture under stress and hydrogen effects

    International Nuclear Information System (INIS)

    Suvorova, S.O.; Fillipov, G.A.

    1996-01-01

    Austenitic steels types 03Kh17N16G10AM5, 03Kh6N12G10AM5 and 07Kh13AG20 with various nitrogen contents were studied for their tendency to delayed fracture using mechanical tests, fractography and X ray diffraction analysis. The steel type 07Kh13G20 exhibited the highest strength in the initial state but showed an increase tendency to delayed fracture after hydrogenation. It is underlined that nitrogen additions essentially intensify the tendency of cold worked steels to delayed fracture. This fact should be taken into account when using nitrogen-containing Cr-Ni-Mn steels under severe operational conditions. 4 refs., 2 tabs

  6. Hot working effect on austenite transformations in structural steel in continuous cooling

    International Nuclear Information System (INIS)

    Zajmovskij, V.A.; Kisteh, N.V.; Samedov, O.V.

    1979-01-01

    Austenite transformations in 40, 40Kh, 40KhN and 40KhNMA steels under hot working at 900 deg C with 20% reduction degree and continuous cooling with 1,7-16 0 /s are investigated. Changing of cooling rate in various ways affects the temperature range of austenite transformation in pearlite and bainite regions. Regulating the cooling rate after hot working one can essentially change the impact strength and steel ductility as a result of high temperature thermomechanical treatment effect

  7. Corrosion of austenitic steels and their components in vanadium-containing chloride melts

    Science.gov (United States)

    Abramov, A. V.; Polovov, I. B.; Rebrin, O. I.; Lisienko, D. G.

    2014-08-01

    The corrosion of austenitic 12Kh18N10T, 10Kh17N13M2T, and 03Kh17N14M3 steels and their components (Cr, Fe, Ni, Mo) in NaCl-KCl-VCl2 melts with 5 wt % V at 750°C is studied. The rates and mechanisms of corrosion of the materials under these conditions are determined. The processes that occur during contact of the metals and steels with vanadium-containing chloride electrolytes are investigated.

  8. Damping capacity of unstable steels on chromium-nickel-manganese base

    Energy Technology Data Exchange (ETDEWEB)

    Kochkin, L.I.; Rudakov, A.A. (Kirovskij Politekhnicheskij Inst. (USSR))

    1982-02-01

    The paper deals with results of a study on the energy scattering in OKh13N3G8, 20Kh13N3G4 and 30Kh13N3G4 unstable steels. It is shown that the development of microplastic strains most easily occurs in low-carbon steel having a two-phase structure in the initial state. The proceeding of microplastic deformations in carbon unstable steels is limited by the interstitial atom effect on the dislocation movement. It is established that in OKh13N3G8 steel the martensite ..cap alpha --> gamma..- transformation begins under the cyclic stress amplitudes below the yield point of this steel. The steels studied possess a high vibrostrength.

  9. The effect of laser treatment on the wear resistance of steel in corrosive media

    International Nuclear Information System (INIS)

    Plyatsko, G.V.; Porter, A.I.; Prejs, G.A.; Mojsa, M.I.

    1975-01-01

    The corrosion mechanical wearing properties of steel 45 treated with a laser beam (H 100 =7800 Mn/sq.m) under friction with nitrated steel 40KhNMA (HV=7000 Mn/sq.m), chrome cast iron Kh15M (hardened and low-temperature tempered, modified), perlite cast iron and bronze are studied. The aqueous buffers with pH=6 and 11 are used as a corrosion active media. In a weakly acid medium the most intensive wearing of steel 40KhNMA is observed at P=8 Mn/sq.m. Its wearing reduces due to increase of pressure to 12 Mn/sq.m. Extent of steel 45 wearing increases with pressure increase from 8 to 12 Mn/sg.m. Friction coefficient of this pair changes by jumps at an increase of normal pressure and its variation range is smaller than that observed in an alkaline medium. The maximum value of friction coefficient is shifted to the higher pressure. The wearing of cast iron Kh15M-steel 45 pair has an alternative pattern. In an alkaline medium the cast iron wearing intensity shows a linear increase with the normal contact pressure but that of the steel changes jumpwise attaining extreme at 8 and 12 Mn/sq.m. In a weak acid medium the intensity of grasping and graphitization at the friction surface of cast iron Kh15M-steel 45 pair is higher than that in the alkaline medium. Experiments demonstrate an effectiveness of the laser beam treatment of steel 45 for its friction in the alkaline medium with nitrated steel 40KhNMA and with hardened low-temperature tempered cast iron 45 under friction contact pressure as high as 8 Mn/sq.m, and in acid medium at 12 and 8 Mn/sq.m respectively. The laser treatment provides high corrosion-mechanical stability of steel 45 and the counterbodies described, as well as the low friction coefficient of these pairs

  10. Welding wires for high-tensile steels

    International Nuclear Information System (INIS)

    Laz'ko, V.E.; Starova, L.L.; Koval'chuk, V.G.; Maksimovich, T.L.; Labzina, I.E.; Yadrov, V.M.

    1993-01-01

    Strength of welded joints in arc welding of high-tensile steels of mean and high thickness by welding wires is equal to approximately 1300 MPa in thermohardened state and approximately 600 MPa without heat treatment. Sv-15Kh2NMTsRA-VI (EhK44-VI) -Sv-30Kh2NMTsRA-VI (EkK47-VI) welding wires are suggested for welding of medium-carbon alloyed steels. These wires provide monotonous growth of ultimate strength of weld metal in 1250-1900 MPa range with increase of C content in heat-treated state

  11. Effect of preliminary heat treatment on phase transformations and properties of the Kh15N5D2T (VNS-2) steel

    International Nuclear Information System (INIS)

    Madyanov, S.A.; Voronenko, B.I.; Makhnev, E.S.

    1978-01-01

    It is shown that preliminary heat treatment has a significant effect on the α→γ transformation kinetics, the quantity of residual austenite, the grain size and mechanical properties of the Kh15N5D2T steel after final heat treatment. The preliminary heat treatment regimes leading to the increase of the quantity of residual austenite and to grain refining increase the work of crack propagation in the finally strengthened state. The optimum properties were obtained after threefold preliminary tempering for 1h at 650 deg C. An approximately constant relation of α- and γ-phases (approximately 50%) is observed at 625 deg C irrespective of the investigated regimes of preliminary heat treatment

  12. Wear resistance and structural changes in nitrogen-containing high-chromium martensitic steels under conditions of abrasive wear and sliding friction

    International Nuclear Information System (INIS)

    Makarov, A.V.; Korshunov, L.G.; Schastlivtsev, V.M.; Chernenko, N.L.

    1998-01-01

    Martensitic nitrogen-containing steels Kh17N2A0.14, Kh13A0.14, Kh14G4A0.22 as well as steel 20Kh13 were studied for their wear resistance under conditions of friction and abrasion. Metallography, X ray diffraction analysis and electron microscopy were used to investigate the structural changes taking place in a thin surface layer on wearing. It is shown that an increase of nitrogen content of 0.14 to 0.22% promotes an enhancement of steel resistance to abrasive and adhesive wear, especially after tempering in the range of 500-550 deg C. Typically, the nitrogen-containing steels exhibit lower resistance to various types of wear in comparison with the steels with high-carbon martensite due to their lower deformability under conditions of friction loading

  13. Damping capacity of unstable steels on chromium-nickel-manganese base

    International Nuclear Information System (INIS)

    Kochkin, L.I.; Rudakov, A.A.

    1982-01-01

    The paper deals with results of a study on the energy scattering in OKh13N3G8, 20Kh13N3G4 and 30Kh13N3G4 unstable steels. It is shown that the development of microplastic strains most easily occurs in low-carbon steel having a two-phase structure in the initial state. The proceeding of microplastic deformations in carbon unstable steels is limited by the interstitial atom effect on the dislocation movement. It is established that in OKh13N3G8 steel the martensite α→γ- transformation begins under the cyclic stress amplitudes below the yield point of this steel. The steels studied possess a high vibrostrength [ru

  14. Influence of structure and properties of tubular billets of the 12 Kh 18N10T steel on deformability of tubes at cold-rolling mills

    International Nuclear Information System (INIS)

    Vil'yams, O.S.; Bol'shova, N.M.; Olejnik, O.V.; Velikotnaya, E.S.

    1979-01-01

    Metallographic analysis of the defects of the ''oblique cracks'' type on the surface of hot-rolled tubes of the 12Kh18N10T steel has been carried out. Recommended is the complex of mechanical properties and the structure factors (grain size) of conversion hot-rolled tubes, providing the combination of ductility and high rapture strength during rolling at pilger mills. At a grain size not coarser than number 5, a billet must have σsub(T) 5 >=40 %. Hot-rolled coarse-grained billet is not recommended for warm rolng because of high strain hardening

  15. Corrosion behavior of austenitic steels and their components in niobium-containing chloride melts

    Science.gov (United States)

    Abramov, A. V.; Polovov, I. B.; Rebrin, O. I.; Volkovich, V. A.; Lisienko, D. G.

    2014-02-01

    The mechanism of corrosion of austenitic steels 12Kh18N10T, 10Kh17N13M2T, and 03Kh17N14M3 and metals Cr, Fe, Ni, and Mo in a NaCl-KCl-NbCl n ( n = 3.5, Nb content is 5 ± 0.1 wt %) melt at 750°C is studied. The metal and steel corrosion rates under these conditions are determined. The character of material fracture and the mechanisms of material corrosion are found.

  16. Chemical heat treatment of low alloyed maraging steels

    Energy Technology Data Exchange (ETDEWEB)

    Malinov, L S; Korotich, I K [Zhdanovskij Metallurgicheskij Inst. (Ukrainian SSR)

    1979-09-01

    The investigation concerned the nitriding, cementation, chromizing, borating of economically alloyed maraging grade 04Kh2N5MFYu steel. The investigated methods of chemothermal treatment were found to considerably increase the hardness of the surface layer of the maraging steel. The high tempering of the grade 04Kh2N5MFYu cemented and hardened steel was found to produce secondary hardening. On chromizing, the diffusion layer is an alloyed ferrite which strengthens because of the dispersion hardening on ageing. The formation of the plastic low-carbon martensite at relatively small cooling rates greatly decreases the tendency of the boride layer to cracking.

  17. Plasticity of low carbon stainless steels

    International Nuclear Information System (INIS)

    Bulat, S.I.; Fel'dgandler, Eh.G.; Kareva, E.N.

    1975-01-01

    In the temperature range 800-1200 0 C and with strain rates of from 10 -3 to 3 s -1 , austenitic (000Kh18N12) and austenitic-ferrite (000Kh26N6) very low carbon stainless steels containing 0.02-0.03% C exhibit no higher resilience than corresponding ordinary steels containing 0.10-0.12% C. However, the plasticity of such steels (particularly two-phase steels) at 900-1100 0 C is appreciably inferior owing to the development of intergranular brittle fracture. Pressure treatment preceded by partial cooling of the surface to 850 0 C yields rolled and forged products with acceptable indices but is inconvenient technically. At the Zlatoustovsk and Ashin metallurgical plants successful tests have been performed involving the forging and rolling of such steels heated to 1280-1300 0 C without partial cooling; it was necessary to improve the killing conditions, correct the chemical composition (increasing the proportion of ferrite) and take measures against heat loss. (author)

  18. 46 CFR 54.25-25 - Welding of quenched and tempered steels (modifies UHT-82).

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 2 2010-10-01 2010-10-01 false Welding of quenched and tempered steels (modifies UHT-82... ENGINEERING PRESSURE VESSELS Construction With Carbon, Alloy, and Heat Treated Steels § 54.25-25 Welding of quenched and tempered steels (modifies UHT-82). (a) The qualification of welding procedures, welders, and...

  19. Mechanical and fracture properties at impact loading of selected steels for nuclear power engineering

    International Nuclear Information System (INIS)

    Buchar, J.; Bilek, Z.

    1988-01-01

    The possibilities are briefly characterized of experimental research of mechanical and fracture properties of steels used in nuclear power engineering. Attention is paid to plastic deformation and the assessment of fracture formation during impact loading. The results are reported for steels 15Kh2MFA and 10GN2MFA. For steel 15Kh2MFA the effect was also studied of neutron radiation at different temperatures. From the theory developed for non-irradiated material 10GN2MFA, a prediction is made within the original model of the fracture stress value for steel 15Kh2MFA in both non-irradiated and irradiated states. The conclusion is arrived at that the existing methods of assessing steel properties at impact load allow obtaining knowledge of all significant effects during actual stress, this using only small specimens of the materials. (Z.M.). 4 figs., 8 refs

  20. Analysis of ductile-brittle transition shifts for standard and miniature bending specimens of irradiated steel

    International Nuclear Information System (INIS)

    Korshunov, M.E.; Korolev, Yu.N.; Krasikov, E.A.; Gabuev, N.N.; Tykhmeev, D.Yu.

    1996-01-01

    A study is made to reveal if there is a correlation between shifts in temperature curves obtained when testing thin plates and standard specimens on impact bending and fracture toughness. The tests were carried out using steel 25Kh3NM specimens irradiated by 6 x 10 19 cm -2 neutron fluence. A conclusion is made about the possibility to evaluate the degree of radiation-induced embrittlement of reactor steels on the basis of thin plate testing under quasistatic loads [ru

  1. Unit rupture work as a criterion for quantitative estimation of hardenability in steel

    International Nuclear Information System (INIS)

    Kramarov, M.A.; Orlov, E.D.; Rybakov, A.B.

    1980-01-01

    Shown is possible utilization of high sensitivity of resistance to fracture of structural steel to the hardenability degree in the course of hardening to find the quantitative estimation of the latter one. Proposed is a criterion kappa, the ratio of the unit rupture work in the case of incomplete hardenability (asub(Tsub(ih))) under investigation, and the analoguc value obtained in the case of complete hardenability Asub(Tsub(Ch)) at the testing temperature corresponding to the critical temperature Tsub(100(M). Confirmed is high criterion sensitivity of the hardened steel structure on the basis of experimental investigation of the 40Kh, 38KhNM and 38KhNMFA steels after isothermal hold-up at different temperatures, corresponding to production of various products of austenite decomposition

  2. Low-temperature nitriding of austenitic steel in a vibrofluidized bed

    Science.gov (United States)

    Baraz, V. R.; Grachev, S. V.

    1999-11-01

    The prospects for use of a vibrofluidized bed (VFB) for low-temperature nitrogen saturation of high-strength austenitic steel based on Cr-Ni-Mn (12Kh17N8G2S2MF) are considered. The positive effect of preliminary plastic deformation on the intensity of nitriding is described. The temperature and time parameters of nitriding in a VFB for strain-aging austenitic steel 12Kh17N8G2S2MF are shown to be adequate for the regimes of the final heat-treatment operation of aging. This creates the possibility of combining the operations of surface alloying and strain aging into a single cycle. This combined treatment increases substantially the resistance of the steel to cyclic loads while preserving the strength parameters. It is shown that the presented method of low-temperature nitriding in a VFB is expedient for improving the service characteristics of austenitic steel 12Kh17N8G2S2MF used for production of force springs of automobile brake systems.

  3. Structural steels for power generating equipment and heat and chemical heat treatments

    International Nuclear Information System (INIS)

    Astaf'ev, A.A.

    1979-01-01

    Development of structural steels for power generating equipment and for reactor engineering, in particular, is elucidated. Noted is utilization of the 15Kh2NMFA steels for the WWER-1000 reactor vessels, the 10GN2MFA steels for steam generators, pressurizers, vessels of the automatic emergency shut down and safety system; the 00Kh12N3DL steel for cast pump vessels and main locking bars. The recommendations on heat treatment of big forgings, for instance, ensuring the necessary complex of mechanical properties are given. Diffusion chromizing with subsequent nitriding of austenitic steels which increase durability of the components in BN reactors more than 4 times, is practised on a large scale

  4. Chromium surface alloying of structural steels during laser treatment

    International Nuclear Information System (INIS)

    Kurov, I.E.; Nagornykh, S.N.; Sivukhin, G.A.; Solenov, S.V.

    1987-01-01

    Results of matrix alloying from the surface layer and creation of considerably increased chromium concentration in the depth which permits to increase the efficiency of laser treatment of steels (12Kh18N10T and 38KhN3M) in the process of their further mechanical polishing, are presented. The treatment was realized by continuous CO 2 -laser at different power densities and scanning rates are presented. A model describing the creation of anomalous distributions of the alloying element in steels is plotted

  5. Parametrical limits of SCC-susceptibility of austenitic and austenitic-ferritic Cr-Ni steels

    International Nuclear Information System (INIS)

    Starosvetskij, D.I.; Baru, R.L.; Bondarenko, A.I.; Bogoyavlenskij, V.L.; Timonin, V.A.

    1990-01-01

    Comparative investigations into corrosion cracking (CC) of austenitic (12Kh18N10T) and austenitic-ferritic (08Kh22N6T) chromium-nickel steels are performed for various chloride media in a wide range of chloride concentrations and temperatures. It is shown that the ratio between steels in terms of their CC-susceptibility is not definite and can undergo a reversal depending on parameters of medium, level and conditions of loading. Differences in mechanisms of corrosion cracking of austenitic and austenitic-ferritic steels are established

  6. Close toleranoe forging of chromium steel blades for powerful steam turbines

    International Nuclear Information System (INIS)

    Shastin, Eh.G.; Kositskij, Yu.N.; Lyubchits, G.A.

    1989-01-01

    Work on simulating technological process on die-forging hammer was performed in order to reduce the preparation period bringing technology of close tolerance forging of turbine blades to a commercial level. A special attention was paid to development of accurate forming of forgings of 20Kh13Sh, 12Kh13 and 15Kh11MFSh steels on screw presses with nominal effort equal to 80 and 144 MN

  7. Manufacture of rings of 08Kh18N10T sheet for internal structures of WWER type reactors

    International Nuclear Information System (INIS)

    Fojta, A.; Nitka, B.

    1984-01-01

    Technology is presented of the manufacture of rings for the jacket, shaft, core catcher and shaft bottom of WWER-440 reactors produced by Vitkovice Steel Works. The rings are manufactured from sheets of austenitic steel 08Kh18N10T. The materials and technology problems are discussed of sheet production, ring welding technology and annealing following welding. The plastic properties are assessed of the welded joints and problems are outlined of ring production for WWER-1000 reactors. (B.S.)

  8. Surface finishing and levelling of thermomechanically hardened rolled steel

    International Nuclear Information System (INIS)

    Grosval'd, V.G.; Bashchenko, A.P.; Grishkov, A.I.; Gutnik, M.V.; Kanevskij, B.L.; Nikozov, A.I.; Sedov, N.D.; Prosin, K.A.; Safonov, L.I.

    1975-01-01

    The finishing of high-strength merchant shapes from alloy steel was tried out under industrial conditions with the equipment of metallurgical plants. After thermomechanical hardening in the production line of the rolling mill, 30KhGSN2A and 40Kh1NVA steel rounds 32 and 31 mm in diameter were straightened on a two-roller straightening machine designed by the All-Union Scientific Research Institute for Metallurgical Machinery (VNII Metmash). This made possible subsequent turning and grinding of the rods. The conditions of straightening, turning and grinding have been worked so as to obtain thermomechanically strengthened and ground rolled products approximating the gauged and ground metal in shape geometry and surface finish. It is shown that the labour-consuming operation of turning can be eliminated by reducing the machining pass of the rolled product, and this lowers the labour required for the finishing operations by 75%. After grinding with 40- and 25-grain abrasive wheels, high strength rolled shapes were obtained with a diameter of 30-0.20 mm and a surface finish of class 6-5 satisfying the technical specifications. (author)

  9. Influence of crystallization conditions on formation and distribution of nonmetallic inclusions in steels

    International Nuclear Information System (INIS)

    Efimov, V.A.

    1977-01-01

    The processes were studied of the formation and the distribution of nonmetallic inclusions and the chemical inhomogeneity formation during the solidification of h steel. The variation of the character of oxides and sulfides across ingots was shown by considering st 25 and 20 Kh steels. To improve the distribution of inclusions and the stability of properties throughout the body of ingots, it is recommended to throughly deoxidize the metal, to raise the rate of solidification, to reduce the temperature gradient, to employ powder cooling agents, to use casting under a blanket of slag, to modify steel by active elements (r.e.e., Ca, Ba, Zr, B) which affect favourably the nature and the shape of the nonmetallic phase

  10. Parameter optimization for steel quenching by C02-laser irradiation

    International Nuclear Information System (INIS)

    Moryashchev, S.F.; Kislitsyn, A.A.; Kosyrev, F.K.

    1984-01-01

    The dependence of average absorption factor on maximal temperature of the article surface during quenching by CO 2 -laser irradiation was determined empirically. The calculations of depth of a hardening zone and process productivity in 40 Kh, 4Kh13 steels and Armco-iron with regard to this dependence were conducted

  11. Effect of heat treatment regime on structural lamination in ferritic-austenitic steels

    International Nuclear Information System (INIS)

    Sizov, R.A.; Zakharova, M.I.; Novikov, I.I.; Bannykh, O.A.

    1983-01-01

    The effect of preliminary thermal treatment on lamination and viscosity of EhP-53 and KO-3 steels after durable aging at the temperature of 350 is studied. It is shown that preliminary heat treatment considerably affects lamination processes in the result of aging of 0Kh18G8N2T steel. The lowest rate of lamination and higher impact strength after aging at 350 deg C for 4500 hours corresponds to the following heat treatment: 10 hour aging at 650 deg C with cooling in the air, then quenching in water from 950 deg C after aging for 30 min and the following tempering (650 deg C, 5 hours). Unlike the 0Kh18G8N2T steel, lamination parameters of steel 0Kh22N6T practically do not change after the application of heat treatment. Nevertherless, taking into account results of impact strength, it is advisable to have thermal treatment according to the regime: quenching in water at 950 deg C after aging for 30 min

  12. Quality of structural steel melted by single-slag process

    International Nuclear Information System (INIS)

    Levin, A.M.; Andreev, V.I.; Monastyrskij, A.V.; Drozdova, M.F.; Pashchenko, V.E.; Orzhekh, M.B.

    1982-01-01

    The 40Kh and 12KhN3A steels were used to compare the quality of the metal manufactured according to several variants of a single-slag process with the metal of a conventional melting technology. Investigation results show, that a single-slag process metal has higher sulfides and oxides contents as well as an increased anisotropy of mechanical properties while its tendency to flake formation is weaker due to a less degree of gas saturation. It is marked that anisotropy in the properties and a sulfide content may be decreased by out-of-furnace treatment of steels

  13. Determination of constant of chemical reaction rate in the process of steel treatment in the endothermal atmosphere

    International Nuclear Information System (INIS)

    Gyulikhandanov, E.L.; Kislenkov, V.V.

    1978-01-01

    The high-temperature method was applied to measuring a relative variation in the electrical resistance of a thin steel foil prepared from the 12KhN3A, 18Kh2N4VA, 20KhGNR, and 20Kh3MVF steels during its carburization and decarburization, and determined was the temperature dependence of the reaction rate of the interaction of the endothermal atmosphere of different compositions with the analloyed γ-Fe. A connection has been established between the reaction rate constant and the thermodynamic activity of carbon in the alloyed austenite at the temperature of about 925 deg C, corresponding to the cementation temperature. This provides the quantitative estimation of the above value for any alloyed steels and with the presence of numerical values of diffusion coefficients; this also enables one to carry out an accurate calculation of the distribution of carbon throughout the depth of a layer when effecting the cementation in the endothermal atmosphere

  14. Estimation of the Ultimate Tensile Strength of Steel from Its HB and HV Hardness Numbers and Coercive Force

    Science.gov (United States)

    Sandomirskii, S. G.

    2017-11-01

    A formula is derived to accurately describe the tabulated relation between the Brinell ( HB) and Vickers ( HV) hardnesses of steel over the entire range of their possible variation. This formula and the formulas describing the relation between the HB hardness of chromium-molybdenum and chromium-nickel steels and their ultimate tensile strength σu are used to analyze the change in σu of 38KhNM steel upon quenching and tempering. The data that reveal a relation between σu of 38KhNM steel and its coercive force are obtained.

  15. Structural changes in complex steels with 12 % Cr during welding thermal cycle

    International Nuclear Information System (INIS)

    Ul'yanova, N.V.; Kurnosova, N.D.

    1981-01-01

    The structural changes in the heat affected zones of welded steam tubes of the 12Kh11V2MF and 18Kh12VMBFR steels, are investigated. A short-time heating of thin samples up to 1300-900 deg C with the aim of imitating the thermal welding cycle permits to determine temperatures of specific region formation in heat affeced zones of 12% Cr steels. The difference in the amounts and structure of σ-ferrite and γ-phase in these regions is established. A ''tongue'' nature of γ-phase grain growth is found in the temperature range of 1150-1100 deg C, while at 1300-1250 deg C σ-ferrite growth with the formation of saw-shape boundaries is observed. It is shown that tensile properties of imitated heat affected zone of 12Kh12VMBFP steel increase with heating temperature with the insignificant plasticity decrease. Impact strength on longitudinal samples decreases but remains higher than that determined by specifications [ru

  16. Quality of the KhN73MBTYu alloy after electroslag remelting and vacuum arc remelting

    International Nuclear Information System (INIS)

    Shelgaeva, A.V.; Krichevets, M.I.; Shinkina, N.S.; Komissarov, A.I.

    1978-01-01

    The structure and properties of the heat-resisting KhN73MBTYu alloy are investigated after electroslag remelting (ESR) and vacuum arc (VAR) remelting in commercial furnaces. The complex investigations of the casted metal were carried out by modern methods along with the standard acceptance tests, and a number of service properties were determined. It is established that the ESR metal contains magnesium and has the reduced sulphur concentration; the alloy has more fine-grained structure at high isotropy of the properties at room and operating temperatures; higher endurance is achieved under reversal rotational bending; no laminated fractures are observed. According to the basic quality factors the ESR metal satisfies all requirements for the VAR metal. Due to exclusion of strippling of ESR electrodes and ingots the yield of steel forgings increases by 20-25% and the prime cost decreases in comparison with the industrial production of VAR metal

  17. Tendency of the 18-8 type corrosion-resistant steel to cracking in automatic building-up of copper and copper base alloys in argon

    International Nuclear Information System (INIS)

    Abramovich, V.R.; Andronik, V.A.

    1978-01-01

    Studied was the tendency of the 18-8 type corrosion-resistant steel to cracking during automatic building-up of copper and bronze in argon. The investigation was carried out on the 0kh18n10t steel in argon. It had been established, that the degree of copper penetration into the steel inceases with the increase in the time of the 0Kh18n10t steel contact with liquid copper. Liquid copper and copper base alloys have a detrimental effect on mechanical properties of the steel under external tensile load during intercontant. It is shown that in building-up of copper base alloys on the steel-0Kh18n10t, tendency of the steel to cracking decreases with increase in stiffness of a surfaced weld metal plate and with decrease in building-up energy per unit length. The causes of macrocracking in steel at building-up non-ferrous metals are explained. The technological procedures to avoid cracking are suggested

  18. Evolution of secondary-phase precipitates during annealing of the 12Kh18N9T steel irradiated with neutrons to a dose of 5 DPA

    Science.gov (United States)

    Tsai, K. V.; Maksimkin, O. P.; Turubarova, L. G.

    2007-03-01

    The formation and evolution of thermally-induced secondary precipitates in an austenitic stainless steel 12Kh18N9T irradiated in the core of a laboratory reactor VVR-K to a dose of 5 dpa and subjected to post-radiation isochronous annealings for 1 h in a temperature range from 450 to 1050°C have been studied using transmission electron microscopy (TEM) and microhardness measurements. It has been shown that the formation of stitch (secondary) titanium carbides and M 23C6 carbides at grain and twin boundaries after annealing at 1050°C is preceded by a complex evolution of fineparticles of secondary phases (titanium carbides and nitrides) precipitated at dislocation loops and dislocations during annealing at temperatures above 750°C.

  19. Design of the WWER-440 pressurizer

    International Nuclear Information System (INIS)

    Bednarek, L.

    1978-01-01

    The main specifications are presented of a pressurizer for the WWER-440 reactor as are factors securing operating reliability and the required life of the equipment. Ferritic-pearlite steel 22K is the basic material for the manufacture of the shell, support and couplings. The internal parts and the heads are manufactured from the 08KH18N10T chromium-nickel austenitic steel, the bolts and nuts of manholes from chromium-molybdenum steels 25KH1MF and 25KH2MFA. Quality testing of basic materials and quality control during the process of manufacture are briefly described. (Z.M.)

  20. Corrosion behaviour of stainless steels by internal friction method

    International Nuclear Information System (INIS)

    Postnikov, V.S.; Kovalevskij, V.I.

    1987-01-01

    Corrosion of austenite chromium-nickel stainless steels 12 Kh18N9, 12Kh18N9T, 12Kh18N10 and 12Kh18N10T is investigated. Wire samples 0.7...0.8 mm in diameter before tests were subjected to quenching in water from the temperature of 1050...1100 deg C and part of them - to tempering at 650 deg C for 2 h. Pitting corrosion was brought about by different concentration of iron chloride solutions (C FeCl 3 ). Total corrosion has a slight effect on the character of IF (internal friction) variation that increases without the whole test period up to the moment when mechanical strength of the sample

  1. Corrosion of chromium, nickel, titanium and steels in solutions of sodium and ammonium thiosulfates

    International Nuclear Information System (INIS)

    Grebenshchikova, S.V.; Kochergin, V.P.; Doronina, I.V.

    1983-01-01

    Results of gravimetric determinatiion of average rate of chromium, nickel, titatnium and steels 12Kh18N10T and VSt.3 corrosion rate in solutions 50 mass.% (NH 4 ) 2 S 2 O 3 and Na 2 S 2 O 3 in the air and nitrogen atmosphere at 333 K have been generalized. Anodic polarization curves are recorded and stationary potentials of metals and steels under the conditions are measured. It is shown that in (NH 4 ) 2 S 2 O 3 solution the rate of metal and steels corrosion is higher than in Na 2 S 2 O 3 solution indepenent of the nature of gaseous medium contacting with solution. In the series Ni → VSt.3 → 12Kh18N10T → VT1 → chromium in (NH 4 ) 2 S 2 O 3 and Na 2 S 2 O 3 solutions at 333 K corrosion resistance increases. Chromium, titanium and chromium-nickel steel 12Kh18N10T possess a high corrosion resistance

  2. Electroplastic drawing of stainless steels

    International Nuclear Information System (INIS)

    Troitskij, O.A.; Spitsyn, V.I.; Sokolov, N.V.; Ryzhkov, V.G.

    1977-01-01

    Effect of electroplastic drawing on mechanical, magnetic and electrical properties of wire of 12Kh18N10T and Kh13N13M2 steels was studied. Pulse, direct and alternating currents were used. Direct and alternating current densities were 400 A/mm 2 , mean density of pulse current was 200 A/mm 2 . The investigations have shown that the current density increase results in decreasing the wire strengthening intensity though in increasing plastic properties. As a result of electroplastic drawing the growth of magnetic characteristics of wire occurs

  3. PENDIDIKAN KARAKTER MENURUT KH. WAHID HASYIM

    Directory of Open Access Journals (Sweden)

    Rangga Sa’adillah S. A. P.

    2015-11-01

    Full Text Available This library research examined two research questions. They are what thoughts of KH. Wahid Hasyim about the character education are and how the concept of character education by KH. Wahid Hasyim is relevant to the current condition of education in Indonesia. This study reveals two findings through an inductive analysis. The chief finding of this study is that there are eight characteristic values taught by KH.Wahid Hasyim including religious, tolerant, independent, democratic, patriotic, nasionalist, communicative, and keen on reading. Second, this study disclosed that the thought of character education by KH. Wahid Hasyim is in line with the goal of character education. He strove to build a multicultural national life, educate an intelligent civilization, build a noble character, encourage people to contribute to the development of human life, and develop the potential of having kind hearts, positive thoughts and good behavior as well as exemplary models. He also sought to generate enthusiasm of citizens to keep the peace, creativity, independence, and to be able to coexist with other nations in a harmony.

  4. Optimal control of conditions of deformation during rolling the bar alloy from alloy steel

    International Nuclear Information System (INIS)

    Inatovich, Yu.V.; Shilov, V.A.; Shvarts, D.L.; Kudelin, S.P.

    2001-01-01

    A complex of programs for determining the optimal gaps between rollers during rolling of simple merchant sections of alloy steels of a wide brand assortment (12KhN3A, Kh17N2, Kh18N10T) was elaborated. Experience in calculations made according to the programs suggests advisability of their use in the automated design systems for roller calibration and for adjustment of section mills [ru

  5. Effect of helium ion bombardment on hydrogen behaviour in stainless steel

    International Nuclear Information System (INIS)

    Guseva, M.I.; Stolyarova, V.G.; Gorbatov, E.A.

    1987-01-01

    The effect of helium ion bombardment on hydrogen behaviour in 12Kh18N10T stainless steel is investigated. Helium and hydrogen ion bombardment was conducted in the ILU-3 ion accelerator; the fluence and energy made up 10 16 -5x10 17 cm -2 , 30 keV and 10 16 -5x10 18 cm -2 , 10 keV respectively. The method of recoil nuclei was used for determination of helium and hydrogen content. Successive implantation of helium and hydrogen ions into 12Kh18N10T stainless steel results in hydrogen capture by defects formed by helium ions

  6. Specific features of precipitation hardening of austenitic steels with various base. 2. Kinetics and mechanism of carbide precipitation

    International Nuclear Information System (INIS)

    Kositsyna, I.I.; Sagaradze, V.V.; Khakimova, O.N.

    1997-01-01

    Electron microscopic studies were carried out to determine the kinetics and mechanisms of precipitation hardening in Fe-Mn, Fe-Mn-Cr, Fe-Cr-Mn-N, Fe-Cr-Ni and Fe-Ni base stainless steels (45G20M2F2, 50Kh16G15N6M2F2, 45Kh18N10G10M2F2, 40Kh18Ni18M2F2, 45N26M2F2). The steels were heat treated under various conditions. It is revealed that in manganese steels the particles of vanadium carbide nucleate according to homogeneous mechanism at all aging temperatures (600-750 deg C). The presence of chromium in the matrix promotes the transition to heterogeneous mechanism of carbide nucleation and growth. With nickel content increasing the plasticity of precipitation hardened steels gets better due to more intense diffusion of atoms and vacancies to grain boundaries and, hence, the widening of near-boundary zones free of carbide particles

  7. Investigation of thermal fatigue of chromium-molybdenum steels, used for calcining and agglomeration constructions

    International Nuclear Information System (INIS)

    Sinyavskij, D.P.; Gorkalo, A.P.

    1979-01-01

    The technique for investigating thermal fatigue of materials is described. The data on sample stress deformed state and current temperature values are taken from the local volume of the material studied. Results of investigating thermal fatigue of the 15KhMl and 20KhMl steels are presented

  8. Topic 1. Steels for light water reactor pressure vessels

    International Nuclear Information System (INIS)

    Brumovsky, M.; Brynda, J.; Kepka, M.; Barackova, L.; Vacek, M.; Havel, S.; Cukr, B.; Protiva, K.; Petrman, I.; Tvrdy, M.; Hyspecka, L.; Mazanec, K.; Kupca, L.; Brezina, M.

    1980-01-01

    Part 1 of the Proceedings consists of papers on the criteria for the selection and comparison of the properties of steel for pressure vessels and on the metallurgy of the said steels, the selection of suitable material for internal tubing systems, the manufacture of high-alloy steels for WWER components, the mechanical and metallurgical properties of steel 22K for WWER 440 pressure components, and of steel 10MnNi2Mo for the WWER primary coolant circuit, and the metallographic assessment of steel 0Kh18N10T. (J.P.)

  9. Relationships of quenching stresses to structural transformations in steel

    International Nuclear Information System (INIS)

    Loshkarev, V.E.

    1985-01-01

    Technique for accountancy of the effect of stresses on structural transformations in steel when solving problems of thermoplasticity is suggested. It is revealed on the basis of the conducted calculations that accountancy of interrelation of stressed and structural states of 20Kh2MF steel essentially affects forecasting of results of quenching

  10. Influence of chemical heterogeneity of solid solutions on brittleness in chromium steels

    International Nuclear Information System (INIS)

    Madyanov, S.A.; Sedov, V.K.; Apaev, B.A.

    1985-01-01

    The role of chemical heterogeneity of solid solutions in formation of mechanical properties of Kh09, Kh15, Kh20, Kh19N2G5T chromium steels has been investigated. It is established that besides the known regioA of chemical heterogeneity in the vicinity of 475 deg C exists a high-temperature region (1000-1050 deg C), where maximum heteroge=- neity of chromium distribution in solid solution, is observed. Both types of chemical heterogeneity cause essential hardening of alloys, which becomes apparent in abrupt change of capability to microplastic deformation The mechanism of occurrence of the given temper brittleness consists in carbon diffusion into microvolunes enriched in carbide-forming elements

  11. Improving composition of protective coatings for steel casting

    International Nuclear Information System (INIS)

    Kuz'kina, N.N.; Pegov, V.G.; Bogatenkov, V.F.; Shub, L.G.; Raspopova, N.A.

    1983-01-01

    A radically new fuel-free slag-forming mixture used as protective coating for steel casting is introduced. The lack of combustible powders precludes explosion and fire Lazard in mixture preparation. Usage of the new mixture in stainless steel casting of Kh18N10T type permitted to improve the ingot surface quality and reduce spoilage from 1.16 to 0.66%

  12. Long-term behaviour of heat-resistant steels and high-temperature materials

    International Nuclear Information System (INIS)

    1987-01-01

    This book contains 10 lectures with the following subjects: On the effect of thermal pretreatment on the structure and creep behaviour of the alloy 800 H (V. Guttmann, J. Timm); Material properties of heat resistant ferritic and austenitic steels after cold forming (W. Bendick, H. Weber); Investigations for judging the working behaviour of components made of alloy 800 and alloy 617 under creep stress (H.J. Penkalla, F. Schubert); Creep behaviour of gas turbine materials in hot gas (K.H. Kloos et al.); Effect of small cold forming on the creep beahviour of gas turbine blades made of Nimonic 90 (K.H. Keienburg et al.); Investigations on creep fatigue alternating load strength of nickel alloys (G. Raule); Change of structure, creep fatigue behaviour and life of X20 Cr Mo V 12 1 (by G. Eggeler et al.); Investigations on thermal fatigue behaviour (K.H. Mayer et al.); Creep behaviour of similar welds of the steels 13 Cr Mo 4 4, 14 MoV 6 3, 10 Cr Mo 910 and GS-17 Cr Mo V 5 11 (K. Niel et al.); Determining the creep crack behaviour of heat resistant steels with samples of different geometry (K. Maile, R. Tscheuschner). (orig.,/MM) [de

  13. Toughness of 2,25Cr-1Mo steel and weld metal

    Science.gov (United States)

    Acarer, Mustafa; Arici, Gökhan; Acar, Filiz Kumdali; Keskinkilic, Selcuk; Kabakci, Fikret

    2017-09-01

    2,25Cr-1Mo steel is extensively used at elevated temperature structural applications in fossil fire power plants for steam pipes, nozzle chambers and petrochemical industry for hydrocracking unit due to its excellent creep resistance and good redundant to oxidation. Also they should have acceptable weldability and toughness. The steels are supplied in quenched and tempered condition and their welded components are subjected to post-weld heat treatment (PWHT). Tempering process is carried out at 690-710°C to improve toughness properties. However they are sensitive to reheat cracking and temper embrittlement. To measure temper embrittlement of the steels and their weld metal, temper embrittlement factor and formula (J factor - Watanabe and X formula- Bruscato) are used. Step cooling heat treatment is also applied to determine temper embrittlement. In this study, toughness properties of Cr Mo (W) steels were reviewed. Also transition temperature curves of 2,25Cr-1Mo steel and its weld metal were constructed before and after step cool heat treatment as experimental study. While 2,25Cr-1Mo steel as base metal was supplied, all weld metal samples were produced in Gedik Welding Company. Hardness measurements and microstructure evaluation were also carried out.

  14. Stainless austenitic steels strengthened due to reversible phase transformations and by ageing

    International Nuclear Information System (INIS)

    Sagaradze, V.V.; Kositsyna, I.I.; Ozhiganov, A.V.

    1981-01-01

    The effect of the reversible phase transformations, consisting in the conduction of the direct and reverse martensite transformations and aging, during which the intermetallide γ'-phase of the composition Ni 3 Ti is formed, on the streng-thening of alloys in the Fe-Cr-Ni-Ti system is considered. Stainless austenitic steels Kh12N12T3 and Kh12N14T3, which acquire high mechanical properties: σsub(0.2)=685-785 MPa, σsub(B)=1275 MPa, delta >= 20%, as a result of reversible phase transformations and aging, are suggested. After the reversible phase transformations and ageing the steels possess a high resistance to γ-α-transformation during cold treatment [ru

  15. Effect of elevated temperature on the composition, structure, and mechanical properties of diffusion chromized steel

    International Nuclear Information System (INIS)

    Osintsev, V.D.

    1986-01-01

    The author studies the effect of operating temperature for equipment in contact sections of sulfuric acid workshops on the structure and mechanical properties of the chromized coatings and core of chromized articles. The ferrite lattice spacing was determined in a DRON-0.5 diffractometer according to the line in copper K /sub alpha/ radiation exposure was carried out after layer-by-layer anodic etching of the coating in an aqueous solution. It was shown that diffusion chromizing may lead to a reduction in strength properties compared with those of unchromized steel. As a base for chromized articles intended for operation at temperatures up to 475 0 C it is desirable to use steels 09G2 or 09G25, or for operation at temperatures up to 540 0 C, steels 12KhM and 12MKh

  16. Effect of niobium on the embrittlement of 2.25 Cr and 2.25 Cr-1Mo steels by phosphous

    International Nuclear Information System (INIS)

    Antunes, J.L.B.

    1985-01-01

    The influence of niobium on the temper embrittlement of 2.25Cr and 2.25 Cr-1Mo steels doped with phosphorus is evaluated. The transition temperatures of the samples tempered at 650 0 C and aged at different temperatures for niobium steels. (M.J.C.) [pt

  17. Fouling and biocorrosion of a high-alloy steel in the Golden Horn bay

    International Nuclear Information System (INIS)

    Koryakova, M.D.; Nikitin, V.M.; Suponina, A.P.; Kharchenko, U.V.; Zvyagintsev, A.Yu.

    2002-01-01

    The studies on the effect of contamination of the Golden Horn bay waters (the Peter the Great Bay in the Japanese Sea) on formation of the community of the bacterio- and macrofouling and corrosion resistance of the Kh18N10T high-alloy steel are continued. The dissolved and chemically absorbed oxygen, pH, saprophytes, oil-oxidizing, sulfate-reducing bacteria and heavy metals are among the medium indicators, characterizing the level of pollution of the regions of the samples testing. It is shown, that the obtained experimental data extend our understanding of the dependent effect of three factors: the sea medium → fouling → corrosion resistance of the Kh18N10T high-alloy steel [ru

  18. On the low-cycle fracture of chromium-nickel-molybdenum structural steels in seawater

    International Nuclear Information System (INIS)

    Karpenko, G.V.; Kobzaruk, A.V.; Malyshevskij, V.A.; Shul'te, A.Yu.; Rybin, V.V.; Silaev, I.I.

    1977-01-01

    The processes of low-cycle fracture of the chrome-nickel-molybdenum steels 15KhN5MF, 12KhN4MF and 15KhN3M in air, and in sea water have been investigated by the optical microscopy method, and electron microscopic examination of thin films. Bringing no change in the fracture character, sea water produces a speeding-up effect on the low-cycle fatigue fracture process. During long-time corrosion fatigue testing considerable importance lies with the electrochemical corrosion factor expediting the occurrence of corrosive pits acting as crack-initiation nuclei, fatigue crack attack, accumulation of corrosion products in fatigue cracks, etc

  19. Influence of prolonged service of steam turbines on the properties of materials of rotor and vessel components

    International Nuclear Information System (INIS)

    Anfimov, V.M.; Artamonov, V.V.; Chizhik, T.A.

    1984-01-01

    The structure and mechanical properties of steam turbine elements of 25Kh1MF, 25Kh1M1FA (rotors), 15Kh1M1FL (vessel components) steels have been investigated both in initial state and after 200 000 h operation. The structure stability and phase composition of rotor steels providing conservation of heat resistance at a required level was established. Examination of vessel components showed a decrease in the yield strength by 15-20% and durability - by 10% as compared to initial ones. The conclusion on a possible prolongation of the steam turbine service life to 200 000 h is drawn. The nominal service life equals 100 000 h

  20. Methods for protection of high-strength welded stainless steel from corrosion cracking

    International Nuclear Information System (INIS)

    Lashchevskij, V.B.; Gurvich, L.Ya.; Batrakov, V.P.; Kozheurova, N.S.; Molotova, V.A.; Shvarts, M.M.

    1978-01-01

    The efficiency of protection from corrosion cracking under a bending stress of 100 kgf/mm 2 in a salt mist and in a sulphur dioxide atmosphere, of welded joints of steel 08Kh15N5D2T with metallizing, galvanic and varnish coatings and lubricants, and of steel 1Kh15N4AM3 with sealing compounds has been investigated. Metallization of welded joints with aluminium and zinc efficiently increases corrosion resistance in a salt mist. Galvanic coatings of Cd, Zn, and Cr increase the time to cracking in a salt mist from 2-3 to 60-80 days. The protective properties of varnishes under the effect of a salt mist decrease in the following sequence: epoxy-polyamide enamel EP-140, acrylic enamel C-38, silicone enamels KO-834, KO-811, and KO-814. In an atmosphere containing SO 2 0.15 vol.% at 100% relative humidity, the varnishes investigated, with the exception of the inhibited coating XC-596, show lower protective properties than in a salt mist. The high efficiency of protection from corrosion cracking in a salt mist of slots of steel 1Kh15N4AM3 when using organic sealing compounds U4-21 and U5-21, and also slushing lubricants and oils PVK, TsIATIM-201, K17, and AMS3 was established

  1. X-ray diffraction study of slags forming during corrosion resistant steel production

    International Nuclear Information System (INIS)

    Slavov, V.I.; Zadorozhnaya, V.N.; Shurygina, A.V.

    1990-01-01

    Using X-ray diffraction analysis slags, forming during corrosion-resistant 12Kh18N10T grade steel production by two flowsheets, are studied. Standard two-slag technology of steel production does not provide efficient disintegration of chromospinelides in slags, gives high steel contamination with respect to nonmetallic impurities, coarse structure and, as a consequence, presence of macrodefects on rolled products surface. One-slag steel melting technology with titanium alloying of the steel at vacuum causes fast removal of chromospinelides at the beginning of reduction period, promotes titanium absorption by the steel, refines nonmetallic inclusions, provides more fine structure and steel plasticity, removes surface defects

  2. Boron effect on fabrication properties and service behaviour of complex corrosion-resistant steels

    International Nuclear Information System (INIS)

    Gol'dshtejn, Ya.E.; Piskunova, A.I.; Shmatko, M.N.

    1978-01-01

    In order to determine the optimum boron admixtures for the improvement of the technological plasticity without the considerable reduction in the corrosion resistance of the complex alloy Cr-Ni-Mo steels, industrial heats of the 03KH16N15M3, 03KH17N14M3 and other steels, containing 0.0005-0.003% boron, have been researched. The plasticity, corrosion resistance and microstructure of certain steels have been determined. It is shown that small additions of boron enhance the technological plasticity during the ingot rolling. In order to prevent a sharp reduction in the corrosion resistance, the boron content should be confined to 0.0015% and the quenching temperature raised to 1,120-1,150 deg C. The positive effect of the quenching temperature increase is accounted for by the solution of the excess phases and by the reduction of the dislocation density in the near-the-boundary zones

  3. Optimum conditions for aging of stainless maraging steels

    International Nuclear Information System (INIS)

    Mironenko, P.A.; Krasnikova, S.I.; Drobot, A.V.

    1980-01-01

    Aging kinetics of two 0Kh11N10M2T type steels in which 3 % Mo (steel 1), and 3 % Mo and 11 % Co (steel 2) had been additionally introduced instead of titanium were investigated. Electron microscopy and X-ray methods were used. It was ascertained that the process of steel aging proceeded in 3 stages. Steel 2 was hardened more intensively during the aging, had a higher degree of hardness and strength after the aging, weakened more slowly if overaged than steel 1. The intermetallide hcp-phase Fe 2 Mo was the hardening phase on steels extended aging. Optimum combination of impact strength and strength was was achieved using two-stage aging: the first stage - maximum strength aging was achieved, the second stage - aging at minimum temperatures of two-phase α+γ region

  4. Effect of smelting method on the austenite grain size and properties of heat-resisting pearlitic steel

    International Nuclear Information System (INIS)

    Balakhovskaya, M.B.; Khusainova, N.A.; Davlyatova, L.N.

    1975-01-01

    Influence of smelting method on austenite grain size and properties of refractory perlite steel were studied. An opportunity was found to increase the steel refractoriness without deteriorating its other properties. The steel 12Kh1MF of electric or common open-hearth smelting was used. The dependence of kinetics of austenite grain growth on the smelting method was studied in the temperature range 950 deg - 1200 deg C with 1 hour exposure. The grain size of austenite in steel is supposedly determined by aluminium nitrides and vanadium carbides. In tests of normalized (kept for 20 minutes at 950-980 deg C) and tempered (kept for 3 hours at 730 deg C) transverse (tangential) pipe cross-section samples the electric steel had higher impact viscosity than the open-hearth metal. At working temperatures (540 deg -580 deg C) the difference in viscosity has its minimum. Viscosity of both steels 12Kh1MF begins to sharply decrease from 20 deg C. However, electric steel has rather high viscosity even at - 40 deg C, while the open-hearth one becomes brittle as early as at - 20 deg C. Long-term strength tests at 580 deg C under stresses 10-14 kG/mm 2 show that the coarse-grain steel is more refractory, i.e. time till fracture of open-hearth steel samples is twice as long as that of electric steel samples

  5. Creep rupture properties of oxidised 20%Cr austenitic stainless steels

    International Nuclear Information System (INIS)

    Lobb, R.C.; Ecob, R.C.

    1989-02-01

    Sheet specimens of stabilised 20%Cr/25%Ni/Nb and nitrided 20%Cr/25%Ni/Ti stainless steels, both used as fuel cladding materials in CAGRs, have been oxidised in simulated reactor gas (Co 2 /1-2%CO) for up to l.9kh at 850 0 C, including intermediate thermal cycles to room temperature. The oxidised specimens have been creep tested subsequently at 750 0 C, under conditions of constant stress. The creep rupture properties are affected differently for the two materials. For 20%Cr/25%Ni/Nb stainless steel, there was no effect of oxidation on the intrinsic microstructure, when compared with thermally aged, non-oxidised material. Any differences in creep ductility were ascribed to geometric effects in specimens of this alloy. Lower ductilities were associated with an increased incidence of pitting attack (higher oxide spallation) and it was concluded that the extent of local, rather than general, loss of section controlled the ductility. For nitrided 20%Cr/25%Ni/Ti stainless steel, the intrinsic microstructure was affected by oxidation, such that increased grain boundary precipitation of M 23 C 6 occurred. The resultant effect was for a greater tendency for intergranular failure at lower ductility than for the thermally aged material. The magnitude of this reduction could not be quantified because the specimen geometry was also changed by oxidation. In this instance, the oxidation mode that produced the most severe loss of section was grain boundary, rather than pitting, attack. This mode of attack was not linked directly to oxide fracture/spallation, but to the period of oxidation. (author)

  6. Influence of heating temperature on bainite transformation proceeding in chromium-nickel-molybdenum steels

    International Nuclear Information System (INIS)

    Kaletin, Yu.M.; Kaletin, A.Yu.

    1983-01-01

    The purpose of the present paper is to investigate the effect of heating and cooling from austenization temperature on development of bainite transformation in 37KhN3MFA and 18Kh2N4MA structural alloyed steels. The metallographical analysis of specimens has revealed that first crystals of bainite under slow heating up to 770-790 deg C appear at the temperature of about 500 deg C and at 475 deg C there has been much bainite over the whole cross section of the specimen. It is revealed that an increase of heating temperature and cooling rate replace the starting point of bainite transformation upwards. The strongest displacement of the point Bsub(S) into hogh-temperature range takes place after heating steel with the initial bainite structure in intercritical temperature range

  7. Crustal Structure of Khövsgöl, Mongolia

    Science.gov (United States)

    Scott, A. M.; Meltzer, A.; Stachnik, J.; Russo, R.; Munkhuu, U.; Tsagaan, B.

    2017-12-01

    Mongolia is part of the Central Asian Orogenic Belt, an accretionary event that spanned 800 million years from the mid-Proterozoic to mid-Phanerozoic. As a result of the past collisional and rifting events, the modern Khövsgöl rift system of northern Mongolia contains a heterogeneous lithospheric structure. The current rift system has three parallel N-S trending basins that roughly align with terrane boundaries. Structures inherited during the accretionary events may be a factor influencing regional deformation. The forces that drive local deformation are not well understood, but varying processes have been proposed: far-field effects of India-Eurasian plate convergence, westward subduction of the Pacific plate, magmatic underplating at the base of the crust, mantle plume activity, and asthenospheric mantle convection. Determining the nature of crustal features within this poorly understood region may illuminate processes that control rifting within intracontinental settings. A network of 26 broadband seismic stations encompassing 200 square kilometers of the Khövsgöl rift system were deployed from August 2014 to June 2016. More than 2100 events were detected, and most earthquakes were concentrated near rift structures. Events between Busiin-Gol and Darkhad, the westernmost and central basins of the Khövsgöl rift system, are distributed within the crust. An active fault is outlined along the eastern border of the Darkhad basin. Khövsgöl earthquakes bound both sides of the rift. Along the northern border of Lake Khövsgöl, seismic events define a shallow active fault orthogonal to the basin. The largest event recorded within the network was a magnitude ml=5.2 located near the northeastern border of Lake Khövsgöl on 12-05-2014. The focal mechanism of this earthquake is predominantly strike-slip, but also includes an extensional component. This work focuses on earthquake relocation and calculating moment tensors and focal mechanisms of larger regional

  8. The influence of heating rate on reheat-cracking in a commercial 2 1/4Cr1Mo steel

    International Nuclear Information System (INIS)

    Hippsley, C.A.

    1983-03-01

    The effects of elevated heating rate on stress-relief cracking in a commercial 2 1/4 Cr1Mo steel have been investigated. A SEN bend-specimen stress-relaxation test was used to assess reheat cracking susceptibility and fracture mechanisms for an initial post-weld heating rate of 1000 Kh - 1 . Two factors controlling the influence of heating rate on the final severity of cracking were identified, i.e. the rate of stress-relaxation with respect to temperature, and the time available for crack-growth. The factors were found to counteract each other, but in the case of commercial 2 1/4 Cr1Mo steel, the crack-growth factor outweighed the relaxation factor, resulting in a reduction in the propensity to stress-relief cracking at the elevated heating rate. However, by reference to the results of a separate investigation concerning A508/2 MnMoNiCr steel it was demonstrated that the balance between these two factors may be reversed in other alloy systems, with the consequence that reheat cracking is exacerbated by increasing the initial heating rate. A computer model was addressed to the stress-relaxation test conditions using data from the commercial 2 1/4 Cr1Mo steel. The model predictions exhibited reasonable agreement with experimental test results for both 100 Kh - 1 and 1000 Kh - 1 heating rates. (author)

  9. Application of experiment planning during investigation of cementation process in solid carburizers

    International Nuclear Information System (INIS)

    Lisenkov, A.N.; Denisov, V.M.; Prigozhina, E.L.

    1981-01-01

    A mathematical model of cementation process in solid carburizirs is obtained, the most effective contents of carburizers are chosen. Specimens are produced out of St20, 12KhN3A, 40Kh13, KhVG steels. It is shown that specimens of St20 and 12KhN3A steels have the higher depth of cementated layer, specimens made of 40Kh13 and KhVG steels-the lower depth. It is shown that the quality of cementated layer structure at recommended regimes improved, cementated layer depth for low-carbon steels changed a little and for tool steels increased infficiently: for KhVG steel in 2-3 times for 40Kh13 steel in 1.5-2.5 times

  10. Hydrogen induced plastic damage in pressure vessel steel of 2.25Cr-1Mo

    International Nuclear Information System (INIS)

    Han, G.W.; Song, Y.J.

    1995-01-01

    2.25Cr-1Mo steel is generally employed as a hydrogenation reaction vessel material used at elevated temperature and in a hydrogen containing environment. During service of the reaction vessel, a large number of hydrogen atoms would enter its wall. When the reaction vessel is shutdown and the temperature reduces to about ambient temperature, the hydrogen atoms remaining in the wall would induce plastic damage in the steel. The mechanism of hydrogen induced plastic damage is different for various materials with different microstructures. Investigations have demonstrated that the hydrogen induced plastic damage in carbide annealed carbon steels is caused by hydrogen accelerating the initiating and growing of microvoids from the carbide particles. However, SEM examination on the fracture surface of hydrogen charged tensile specimen of 2.25Cr-1Mo steel show that a large number of fisheyes appear on the fracture surface. This indicates that hydrogen induced plastic damage in 2.25Cr-1Mo steel is related to the occurrence of fisheye cracks during plastic deformation. By means of micro-fracture mechanics to analyze fisheye crack occurrence from the first generation microvoid, the mechanism of hydrogen induced plastic damage in the pressure vessel steel is investigated

  11. Influences of silicon on the work hardening behavior and hot deformation behavior of Fe–25 wt%Mn–(Si, Al) TWIP steel

    International Nuclear Information System (INIS)

    Li, Dejun; Feng, Yaorong; Song, Shengyin; Liu, Qiang; Bai, Qiang; Ren, Fengzhang; Shangguan, Fengshou

    2015-01-01

    Highlights: • Influence of Si on work hardening behavior of Fe–25 wt%Mn TWIP steel was investigated. • Influence of Si on hot deformation behavior of Fe–25 wt%Mn TWIP steel was studied. • Si blocks dislocation glide and favors mechanical twinning in Fe–25 wt%Mn TWIP steel. • The addition of Si increases the hot deformation activation energy of Fe–25 wt%Mn TWIP steel. • The addition of Si retards the nucleation and growth of DRX grains of Fe–25 wt%Mn TWIP steel. - Abstract: The influence of silicon on mechanical properties and hot deformation behavior of austenitic Fe–25 wt%Mn TWIP steel was investigated by means of the comparison research between 25Mn3Al and 25Mn3Si3Al steel. The results show that the 25Mn3Si3Al steel has higher yield strength and higher hardness than that of 25Mn3Al steel because of the solution strengthening caused by Si atoms and possesses higher uniform deformation ability and tensile strength than that of 25Mn3Al steel due to the higher work hardening ability of 25Mn3Si3Al steel. 25Mn3Si3Al steel presents a clear four-stage curve of work hardening rate in course of cold compression. Quite the opposite, the 25Mn3Al steel presents a monotonic decline curve of work hardening rate. The difference of the work hardening behavior between 25Mn3Al and 25Mn3Si3Al steel can be attributed to the decline of stacking fault energy (SFE) caused by the addition of 3 wt% Si. The dislocation glide plays an important role in the plastic deformation of 25Mn3Al steel even though the mechanical twinning is still one of the main deformation mechanisms. The 3 wt% Si added into the 25Mn3Al steel blocks the dislocation glide and promotes the mechanical twinning, and then the dislocation glide characteristics cannot be observed in cold deformed microstructure of 25Mn3Si3Al steel. The hot compression tests reveal that the hot deformation resistance of the 25Mn3Si3Al steel is significantly higher than that of the 25Mn3Al steel due to the solid

  12. Specific features of the occurrence, development, and re-compaction of spall and shear fractures in spherically-convergent shells made of unalloyed iron and some steels under their spherical explosive loading

    International Nuclear Information System (INIS)

    Kozlov, E.A.; Brichikov, S.A.; Gorbachev, D.M.; Brodova, I.G.; Yablonskikh, T.I.

    2007-01-01

    Results of comparative metallographic examination of recovered shells exposed to explosive loading in two modes (with and without a heavy casing confining explosion products scatter) are presented. The shells were made of high-purity and technical-grade unalloyed iron with the initial grain size 250 and 125 μm, steel 30KhGSA in delivery state and quenched up to HR C 35...40, austenitic stainless steel 12Kh18N10T. The heavy casing used in experiments is demonstrated to ensure a rather compact convergence of shells destroyed at high radii. In the described comparative experiments, one managed to compile the 12Kh18N10T steel shell, after it was spalled at high radii and exposed to shear fracture and spallation layer fragmentation at medium radii, into a compact sphere but failed to do the same with the 30KhGSA quenched steel shell after it was fractured according to spall and shear mechanisms at high and medium radii. Polar zones of this steel shell have obvious undercompressed areas due to significant dissipative losses to overcome the shear strength. Occurrence, development, and re-compaction of spall and shear fractures in spherically-convergent shells made of materials, which were already carefully investigated in 1D- and 2D-geometry experiments, were systematically studied in order to verify and validate new physical models of dynamic fractures, as well as up-to-date used in 1D-, 2D- and 3D-numerical algorithms [ru

  13. Investigation of fretting corrosion of vacuum-chrome-plated vt3-1 titanium alloy in pair with unprotected vt3-1 alloy and 40khnma steel

    International Nuclear Information System (INIS)

    Rojkh, I.L.; Koltunova, L.N.; Vejtsman, M.G.; Birman, Ya.N.; Skosarev, A.V.; Kogan, I.S.

    1978-01-01

    The character of destruction of contacting surfaces in the process of fretting corrosion of titanium alloy VT3-1 chromized in vacuum in pair with unprotected alloy VT3-1 and steel 40KhNMA has been studied by scanning electron microscopy, electronography, and recording the surface profile. The specific load was 200 kg/cm 2 , vibration amplitude 50 mkm and frequency 500 Hz. It has been established that pairs unprotected with coating are subjected to intensive fretting corrosion especially when they are made of titanium alloy. For the pair chromized alloy VT3-1 - unprotected alloy VT3-1 no destruction of a chromized surface is observed. Vacuum chromium coating in the pair with steel 40KhNMA reveals similar properties as in pair with a titanium alloy. The surface of a steel sample is destroyed because of fretting corrosion, though the intensity of corrosion is lower than in the case of unprotected pairs. Vacuum chromium coating is recommended for protection of titanium alloy VT3-1 from fretting corrosion in pair with steel 40KhNMA or an alloy VT3-1 especially in those cases when various organic coatings are unsuitable

  14. Joint formation of dissimilar steels in pressure welding with superposition of ultrasonic oscillations

    Energy Technology Data Exchange (ETDEWEB)

    Surovtsev, A P; Golovanenko, S A; Sukhanov, V E; Kazantsev, V F

    1983-12-01

    Investigation results of kinetics and quality of carbon steel joints with the steel 12Kh18N10T, obtained by pressure welding with superposition of ultrasonic oscillations with the frequency 16.5-18.0 kHz are given. The effect of ultrasonic oscillations on the process of physical contact development of the surfaces welded, formation of microstructure and impact viscosity of the compound, is shown.

  15. Effect of smelting method on the austenite grain size and properties of heat-resisting pearlitic steel

    Energy Technology Data Exchange (ETDEWEB)

    Balakhovskaya, M B; Khusainova, N A; Davlyatova, L N [Vsesoyuznyj Nauchno-Issledovatel' skij Teplotekhnicheskij Inst., Moscow (USSR)

    1975-12-01

    Influence of smelting method on austenite grain size and properties of refractory perlite steel were studied. An opportunity was found to increase the steel refractoriness without deteriorating its other properties. The steel 12Kh1MF of electric or common open-hearth smelting was used. The dependence of kinetics of austenite grain growth on the smelting method was studied in the temperature range 950 deg - 1200 deg C with 1 hour exposure. The grain size of austenite in steel is supposedly determined by aluminium nitrides and vanadium carbides. In tests of normalized (kept for 20 minutes at 950-980 deg C) and tempered (kept for 3 hours at 730 deg C) transverse (tangential) pipe cross-section samples the electric steel had higher impact viscosity than the open-hearth metal. At working temperatures (540 deg -580 deg C) the difference in viscosity has its minimum. Viscosity of both steels 12Kh1MF begins to sharply decrease from 20 deg C. However, electric steel has rather high viscosity even at /sup -/40 deg C, while the open-hearth one becomes brittle as early as at /sup -/20 deg C. Long-term strength tests at 580 deg C under stresses 10-14 kG/mm/sup 2/ show that the coarse-grain steel is more refractory, i.e. time till fracture of open-hearth steel samples is twice as long as that of electric steel samples.

  16. Certain peculiarities of structural inheritance in phase recrystallization of steel

    International Nuclear Information System (INIS)

    Mukhamedov, A.A.

    1978-01-01

    The structural inheritance in phase recrystallization of previously overheated to various temperatures industrially melted 40Kh steel and of Armco-iron has been investigated. The steels have been heated to 100O, 11O0, 1200 and 1260 deg C and cooled in the air, and in some instances, hardened (quenched) in water. The physical broadening of X-ray lines points to a nonmonotonous variation of fine structure parameters as a function of the temperature and the heating time. The inheritance effect of fine structure defects affects the steel properties obtained in a final heat treatment. The structural inheritance effect has an important bearing upon the wear resistance of steel. A purpose-oriented use of the structural inheritance effect can enhance service properties of steel parts

  17. Comparative estimation of weld-ability of medium-alloy steels

    International Nuclear Information System (INIS)

    Makarov, Eh.L.; Laz'ko, V.E.

    1977-01-01

    Weldability of various industrial steels has been investigated as affected by mutual presence of carbon and alloying elements in a wide range of concentrations. Mechanical properties and technological strength of medium alloyed steel welded joints have been compared. Technological strength parameters have been found to sharply decrease with increasing carbon content, the decrease depending on the alloying system. Resistance to hot and cold cracking is somewhat decreased by nickel and increased by molibdenum and tungsten. The best mechanical properties are displayed by steels of the Kh2GSNVM type. Industrial evidence on argon arc welding of different constructions made of steels 1.5-20 mm thick is compared to laboratory results. Accordingly, the high strength steels are divided into three groups, i.e. those manifesting good, satisfactory and poor weldability

  18. On the ways of improving mechanical properties of boiler steels subject to hydrogen effect

    International Nuclear Information System (INIS)

    Tkachev, V.I.; Litvin, A.K.; Zvezdin, Yu.I.

    1975-01-01

    The effect of oxygen on the strength properties of boiler steels Kh15M2 and 48TS subjected to heat treatment and preliminary plastic deformation has been studied. It is shown that changes in the strength properties of the steel are determined by the heterogeneity of its structure. Treatment which contributes to homogenization of the metal structure increases the resistance of the steel to detrimental effect of hydrogen. Absorption of hydrogen during cathode polarization at various current densities is shown

  19. Special Features of Induction Annealing of Friction Stir Welded Joints of Medium-Alloy Steels

    Science.gov (United States)

    Priymak, E. Yu.; Stepanchukova, A. V.; Bashirova, E. V.; Fot, A. P.; Firsova, N. V.

    2018-01-01

    Welded joints of medium-alloy steels XJY750 and 40KhN2MA are studied in the initial condition and after different variants of annealing. Special features of the phase transformations occurring in the welded steels are determined. Optimum modes of annealing are recommended for the studied welded joints of drill pipes, which provide a high level of mechanical properties including the case of impact loading.

  20. Positron annihilation and Moessbauer studies of neutron irradiated reactor pressure vessel steels

    International Nuclear Information System (INIS)

    Brauer, G.; Matz, W.; Liszkay, L.; Molnar, B.

    1990-11-01

    Positron annihilation (lifetime, Doppler broadening) and Moessbauer studies on unirradiated, neutron irradiated and neutron irradiated plus annealed reactor pressure vessel steels (Soviet type 15Kh2NMFA) are presented. The role of microstructural properties and the formation of irradiation-induced precipitates is discussed. (orig.) [de

  1. Solidification Segregation and Homogenization Behavior of 1Cr-1.25Mo-0.25V Steel Ingot

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Dong-Bae [Dae-gu Mechatronics and Materials Institute, Daegu (Korea, Republic of); Na, Young-Sang; Seo, Seong-Moon [Korea Institute of Materials Science, Changwon (Korea, Republic of); Lee, Je-Hyun [Changwon National University, Changwon (Korea, Republic of)

    2016-09-15

    As a first step to optimizing the homogenization heat treatment following high temperature upset forging, the solidification segregation and the homogenization behaviors of solute elements were quantitatively analyzed for 1Cr-1.25Mo-0.25V steel ingot by electron probe micro-analysis (EPMA). The random sampling approach, which was designed to generate continuous compositional profiles of each solute element, was employed to clarify the segregation and homogenization behaviors. In addition, ingot castings of lab-scale and a 16-ton-sized 1Cr-1.25Mo-0.25V steel were simulated using the finite element method in three dimensions to understand the size effect of the ingot on the microsegregation and its reduction during the homogenization heat treatment. It was found that the microsegregation in a large-sized ingot was significantly reduced by the promotion of solid state diffusion due to the extremely low cooling rate. On the other hand, from the homogenization point of view, increasing the ingot size causes a dramatic increase in the dendrite arm spacing, and hence the homogenization of microsegregation in a large-sized ingot appears to be practically difficult.

  2. Characteristics of centrifugally cast GX25CrNiSi18-9 steel

    Directory of Open Access Journals (Sweden)

    R. Zapała

    2011-07-01

    Full Text Available The paper presents the results of microstructural examinations of the industrial heat-resistant centrifugally cast GX25CrNiSi18-9 steel characterised by increased content of Cu. The study included changes in the microstructure of base cast steel respective of the steel held at a temperature of 900 and 950°C for 48 hours. Based on the results obtained, an increase in microhardness of the examined cast steel matrix with increasing temperature was stated, which was probably caused by fine precipitates enriched in Cr, Mo, and C forming inside the matrix grains.The layer of scale formed on the tested cast steel oxidised in the atmosphere of air at 900 and 950°C was characterised by an increased tendency to degradation with increasing temperature of the conducted tests.

  3. Phosphorus effect on fracture properties of structural steels

    International Nuclear Information System (INIS)

    Goritskij, V.M.; Guseva, I.A.

    1985-01-01

    Phosphorus content is studied for its effect on fracture peculiarities and fracture toughness. It is supposed that the phosphorus effect on ductile fractures is associated with phosphorus segregation on the ferrite-carbide interfaces. An increase of the phosphorus content in heat-treated 10KhSND steel from 0.020 up to 0.043 wt.% results in a decrease of the pore size and asub(p) value. Close linear correlation is established between critical temperature of embrittlement T 50 and √ asub(p) or √ KC values for a number of structural steels with different phosphorus content

  4. Role of grain refinement in hardening of structural steels at preliminary thermomechanical treatment

    International Nuclear Information System (INIS)

    Bukhvalov, A.B.; Grigor'eva, E.V.; Davydova, L.S.; Degtyarev, M.V.; Levit, V.I.; Smirnova, N.A.; Smirnov, L.V.

    1981-01-01

    The hardening mechanism during preliminary thermomechanical treatment with deformation by cold rolling or hydroextrusion is studied on structural 37KhN3M1 and 38KhN3MFA steels. Specimens have been tested on static tension, impact strength and fracture toughness. It is shown that hydroextrusion application instead of rolling does not change the hardening effect of preliminary thermomechanical treatment (PTMT). It is established that the increase of preliminary deformation degree and the use of accelerated short term hardening heating provides a bett er grain refinement and the increase of PTMT hardening effect [ru

  5. [Effects of different amounts of phosphate fertilizers on copper, zinc transfer in red soil under the application of KH2PO4].

    Science.gov (United States)

    Guo, Liang; Li, Zhong-wu; Huang, Bin; Wang, Yan; Zhang, Yan

    2014-09-01

    In order to study the effects of different phosphate addition amounts on migration and transformation of heavy metals (Cu, Zn) in soil, an indoor leaching experiment using soil columns was carry out to study the leaching behavior of Cu and Zn. The KH2PO4 was chosen as the fertilizer application at the doses of 5 mg.kg-1, 15 mg.kg-1 and 25 mg.kg-1. The results showed that KH2PO4, could reduce the leachate pH, but different phosphate amounts had little effect on leachate pH, pH in leachate kept rising in the whole leaching process. With the application of KH2PO4, Cu migration was mainly in the surface layer while Zn migrated into deeper soil. Concentrations of Cu, Zn in deep soil leachate were low indicating that it was harmless to the shallow groundwater. After leaching, heavy metals mainly existed in the residual form in soil, the proportion of residual form of Cu was around 60% and the proportion of residual form of Zn was around 40%. High concentration of KH2PO4 helps the transformation of Zn from residual organic combination state to exchange state.

  6. Fatigue fracture of steel after mechanical and ultrasonic strengthening

    International Nuclear Information System (INIS)

    Stotskij, I.M.

    1978-01-01

    Fatigue fracture surfaces of samples after mechanical and ultrasonic strengthening have been studied metallographically and by electron fractography. Studied was the 40Kh steel hardened from 850 deg and then tempered at 180 deg or at 550 deg C. The ultrasound power was 25 kWt, the frequency was 20 kHz, the sample rotation velocity was 39.5 m/min. Mechanical and ultrasonic treatment was found to cause structural changes (formation of a white layer) and deformation of the material under the layer. The fatigue cracks were extending beyond the white layer; their propagation involved generation and coalescence of microcracks on account of segregation of carbides. It is concluded that mechanical and ultrasonic treatment should be used for increasing the fatigue strength of low and average strength materials rather than hardened or low-tempered ones

  7. Effect of operational conditions of electroerosion machining on the surface microgeometry parameters of steels and alloys

    International Nuclear Information System (INIS)

    Foteev, N.K.

    1976-01-01

    Studies the influence of pulse duration and a series of operating conditions of a ShGI-40-440 spark-machining generator on changes in the basic surface microgeometry characteristics of components of stainless steel 1Kh18N10T, steel St 45 and hard alloy T14K8. The microgeometry characteristics of spark-machined surfaces differ significantly from the corresponding characteristics of surfaces machined by cutting and vibro-rolling

  8. Corrosion resistance of chromium-nickel steel containing rare earths

    International Nuclear Information System (INIS)

    Asatiani, G.N.; Mandzhgaladze, S.N.; Tavadze, L.F.; Chuvatina, S.N.; Saginadze, D.I.

    1983-01-01

    Effect of additional out-of-furnace treatment with complex alloy (foundry alloy) calcite-silicon-magnesium-rare earth metal on corrosion resistance of the 03Kh18N20M3D3C3B steel has been studied. It is shown that introduction of low additions of rare earths improves its corrosion resistance improves its corrosion resistance in agressive media (in 70% - sulfuric acid) in the range of transition from active to passive state. Effect of additional introduction of rare earth metals is not considerable, if potential of steel corrosion is in the range of stable passive state (32% - sulfuric acid). Additional out-of-furnace treatment with complex foundry alloy, containing rare earth metals, provides a possibility to use a steel with a lower content of Cr, Ni, Mo, than in conventional acid-resistant steels in highly agressive media

  9. Thermomechanical fatigue and damage mechanisms in Sanicro 25 steel

    Czech Academy of Sciences Publication Activity Database

    Petráš, Roman; Škorík, Viktor; Polák, Jaroslav

    2016-01-01

    Roč. 650, JAN (2016), s. 52-62 ISSN 0921-5093 R&D Projects: GA MŠk(CZ) EE2.3.30.0063; GA ČR(CZ) GA13-23652S Institutional support: RVO:68081723 Keywords : thermomechanical fatigue * Sanicro 25 steel * damage mechanism * FIB cutting * localized oxidation-cracking Subject RIV: JL - Materials Fatigue, Friction Mechanics Impact factor: 3.094, year: 2016

  10. X-ray spectrum microanalysis of copper and stainless steel surface layer after electroerosion machining

    International Nuclear Information System (INIS)

    Abdukarimov, Eh.T.; Saidinov, S.Ya.

    1989-01-01

    The results of experimental investigations of the surface layer of copper and steel 12Kh18N10T after electroerrosion treatment by a rotating tungsten electrode in natural and distilled water are presented. It is established that the quantity of electrode material transferred to the surface of the steel treated grows with the spark discharge energy increase. Tungsten concentration in the surface layer reaches 5-10% with the average depth of penetration 40-50 μm

  11. Non-destructive automated express method for determining the inclination of chromium-nickel steels IGC

    International Nuclear Information System (INIS)

    Nazarov, A.A.; Kamenev, Yu.B.; Kuusk, L.V.; Kormin, E.G.; Vasil'ev, A.N.; Sumbaeva, T.E.

    1986-01-01

    Methods of automated control of 18-10-type steel inclination to IGC are developed and a corresponding automated testing complex (ATS) is created. 08Kh18N10T steel samples had two variants of thermal treatment: 1) 1200 deg (5 h), 600 deg (50 h); 2) 1200 deg (5 h). Methods of non-destructive automated control of 18-10-type steel inclination to IGC are developed on the basis of potentiodynamic reactivation (PR) principle. Automated testing complex is developed, which has undergone experimental running and demonstrated a high confidence of results, reliability and easy operation

  12. Behaviour of glass and thermal protective coatings on stainless steels in the nitrogen tetroxide based coolant

    International Nuclear Information System (INIS)

    Bakalin, Yu.I.; Dobrunova, V.M.; Doroshkevich, V.N.; Nesterenko, V.B.; Trubnikov, V.P.

    1985-01-01

    The technology of application of glass and enamel protective coatings on stainless steel has been examined, their testing in the medium of nitrogen tetroxide based coolant with different content of nitric acid has been carried out, the basic characteristics of the coatings after testing have been defined. Chromium-nickel austenitic 12kh18n10t steel, widely used in the nuclear power, have been chosen as a basic object of examination. The coatings have been tested in nitrogen oxide at P=12.0 MPa, temperature 310 deg C and 0.1% HNO 3 , and also in the medium of vat residue of the rectifying tower with nitric acid content up to 25 mass %. Tests of the coatings have demonstrated their sufficiently high stability, especially of those based on enamels A-20 and BK-5. These coatings are characterised by satisfactory performance and can be used for corrosion protection of the materials used in nuclear power

  13. Nitrogen ion implantation effect on friction coefficient of tool steel

    International Nuclear Information System (INIS)

    Velichko, N.I.; Udovenko, V.F.; Markus, A.M.; Presnyakova, G.N.; Gamulya, G.D.

    1988-01-01

    Effect of nitrogen molecular ion implantation into KhVSG steel on the friction coefficient in the air and vacuum is investigated. Irradiation is carried out by the N 2 + beam with energy 120 keV and flux density 5 μ/cm 2 at room temperature in vacuum 5x10 -4 Pa. The integral dose of irradiation is 10 17 particle/cm 2 . Nitrogen ion implantation is shown to provide the formation of the modified layer changing friction properties of steel. The friction coefficient can either increase or decrease depending on implantation and test conditions. 4 refs.; 2 figs

  14. Welded joint properties of steel 2.25Cr1MoNiNb

    International Nuclear Information System (INIS)

    Gladis, R.; Ivanek, J.; Gottwald, M.

    1981-01-01

    Welded joints of steel 08Cr2.25Mo1NiNb for fast reactor steam generators made using manual arc welding with electrodes of identical compositions attain short-term mechanical properties and times to fracture when creep tested that match those of the base material. The reduction of the carbidic phase content in the steel and the welded joint metal did not adversely affect the tensile properties of the welded joint while increasing notch toughness of the heat-affected zone. Reduced carbon and niobium contents in the steel and the welded joint resulted in significant reduction in the proportion of carbidic eutectic particles in both the heat-affected zone and the weld metal. (Ha)

  15. Analytical description of changes in the magnetic states of chromium-nickel steel under uniaxial elastic deformation

    Science.gov (United States)

    Gorkunov, E. S.; Yakushenko, E. I.; Zadvorkin, S. M.; Mushnikov, A. N.

    2017-12-01

    Dependences of magnetization and magnetic permeability of the 15KhN4D structural steel on the value of uniaxial stresses and magnetic field strength are obtained. A polynomial approximation fairly accurately describing the observed changes is proposed on the basis of experimental data.

  16. The inhibitory effect of different concentrations of KH902 eye drops on corneal neovascularization induced by alkali burn

    Directory of Open Access Journals (Sweden)

    Yan Wu

    2017-01-01

    Full Text Available Purpose: The aim of this study was to evaluate the inhibitory effect of different concentrations of KH902 eye drops on rabbit corneal neovascularization (CNV induced by alkali burn. Methods: Forty-eight adult rabbits were randomized into four groups after alkali burning: Group A (2.5 mg/ml, Group B (5 mg/ml, and Group C (10 mg/ml by different concentrations of KH902 eye drops and Group D by saline solution as control with three times a day for 2 weeks. At days 7, 14, and 28, the anterior segment photographs, confocal microscopy, and histopathology were performed to evaluate corneal opacity, neovascularization, inflammatory cell density, vessel size, and edema. Immunohistochemistry was applied to analyze the vascular endothelial growth factor (VEGF level. Results: (1 The CNV in the medicine-treated groups showed a reduction without obvious corneal side effects histologically. (2 Compared to the control group, the three medicine-treated groups showed a reduction in the VEGF levels and CNV areas on days 7, 14, and 28 and in the inflammatory cell density on days 14 and 28 (P 0.05. Conclusion: KH902 eye drops in lower concentration showed an obvious reduction of the CNV growing for rabbit corneal alkali burn without side effects.

  17. Konsep Pendidikan Akhlak dan Dakwah dalam Perspektif Dr. KH. Zakky Mubarak, MA

    Directory of Open Access Journals (Sweden)

    Muchtar Muchtar

    2017-09-01

    Full Text Available Research aims to understand role, and the concept of education and dakwah in perspective Dr. KH. Zakky Mubarak, MA. This research departs from looking at the phenomenon of human life is increasingly complex, entered the modern life and globalization present and the future, wich is characterized by technical and professional paced lives, is forecast to many people ignore the moral and religious in individual and social life. The concept of moral education in the perspective of Dr. KH. Zakky Mubarak, MA that establishes the character of the learners, provide good role models, develop the moral high level, and then apply the knowledge of good character and exemplary in real life so it can become an ingrained habit. The concept of dakwah in perspective Dr. KH. Zakky Mubarak, MA at least two steps that need to be understood by a preacher, first that of bringing the wisdom, it means explaining the wisdoms contained in worship and other Islamic activities without patronizing impression, meaning a preacher should put the words and appropriate sentence appropriate to the circumstances . The second is to mau'idlah hasanah , means giving advice that touch the heart so that the message can be embedded in the memories of audience. Dr. KH. Zakky Mubarak, MA is one of the Nahdlatul Ulama cleric who spend their time preaching, either through a lecture or through scientific papers, scientific papers written contains a lot of moral education that can be used as a reference.  Keywords: Concept of Education and Dakwah, Zakky Mubarak, Nahdlatul Ulama Abstrak Penelitian ini bertujuan untuk mengetahui peran, serta konsep pendidikan akhlak dan dakwah dalam perspektif Dr. KH. Zakky Mubarak, MA. Kesimpulan penelitian ini bahwa Konsep pendidikan akhlak dalam perspektif Dr. KH. Zakky Mubarak, MA yaitu menanamkan pemahaman tentang akhlak terhadap peserta didik, memberikan keteladanan yang baik, mengembangkan pada akhlak tingkat tinggi, dan kemudian mengaplikasikan

  18. Influence of creep ductility on creep-fatigue behaviour of 20%Cr/25%Ni/Nb stainless steel

    International Nuclear Information System (INIS)

    Gladwin, D.; Miller, D.A.

    1985-01-01

    The influence of creep ductility on creep-fatigue endurance of 20%Cr/25%Ni/Nb stainless steel has been examined. In order to induce different creep ductilities in the 20/25/Nb stainless steel, three different thermo-mechanical routes were employed. These resulted in a range of ductilities (3-36%) being obtained at the strain rates of interest. Strain controlled slow-fast creep-fatigue cycles were used with strain rates of 10 -6 s -1 , 10 -7 s -1 in tension and 10 -3 s -1 in compression. It was found that creep ductility strongly influenced the creep-fatigue endurance of the 20/25/Nb stainless steel. When failure was creep dominated endurance was found to be directly proportional to the creep ductility. A ductility exhaustion model has been used to successfully predict creep-fatigue endurance when failure was creep dominated. (author)

  19. Effect of aging on the tribological and mechanical properties of a high-nitrogen stainless austenitic steel

    International Nuclear Information System (INIS)

    Korshunov, L.G.; Chernenko, N.L.; Tereshchenko, N.A.; Uvarov, A.I.

    2005-01-01

    The effect of aging, associated with predominant precipitation of vanadium nitrides (VN), on tribological and mechanical properties of austenitic steel 10Kh18AG18N5MF hardened from 1100 Deg C is studied. Metallographic, X-ray diffraction and electron microscopical methods are used to study structural transformations proceeding in the steel on aging as well as on friction loading under conditions of dry slipping friction in steel-abrasive and steel-steel pairs. It is shown that the aging at temperatures of 600-700 Deg C resulting in a considerable increase of strength properties of the steel demonstrates a relatively weak positive effect on steel resistance to abrasive and adhesive wear. It is stated that the use of aging by continuous mechanism permits attaining favourable mechanical and tribological properties in vanadium-alloying nitrogen-bearing austenitic steels [ru

  20. Safety conditions of using structural steels under high temperature and pressures in hydrogen containing environment

    International Nuclear Information System (INIS)

    Asviyan, M.B.

    1984-01-01

    The method for establishing full-strength conditions was suggested on the base of results of creep-rupture test of tube samples under hydrogen pressure and according to permissible stresses in neutral medium. Applicability of the method was considered taking St3 and 12KhM steels as examples. It was shown that the use of suggested dependences and special efficiency factors enables to forecast endurance limit for the given steel grade and assigned partial hydrogen pressure without labour-intensive test conducting

  1. Experimental verification of the statistical theories of scaling factor effect in fatigue fracture of steel

    International Nuclear Information System (INIS)

    Svistun, R.P.; Babej, Yu.I.; Tkachenko, N.N.

    1976-01-01

    Statistical theories of the scale effect in the fatigue failure of 40KH18N9T, 10 and 20 steels have been verified. The theories are shown to be not invariably suitable for a satisfactory exlanation of the fatigue strength of the samples with respect to their dimensions. One of the main reasons for displaying the scale effect in the process of steel fatigue is the sample self-heating, i.e. a temperature factor which in many cases overlaps a statistical one

  2. Experimental verification of the statistical theories of scaling factor effect in fatigue fracture of steel

    Energy Technology Data Exchange (ETDEWEB)

    Svistun, R P; Babei, Yu I; Tkachenko, N N [AN Ukrainskoj SSR, Lvov. Fiziko-Mekhanicheskij Inst.; L' vovskij Lesotekhnicheskij Inst. (Ukrainian SSR))

    1976-01-01

    Statistical theories of the scale effect in the fatigue failure of 40KH18N9T, 10 and 20 steels have been verified. The theories are shown to be not invariably suitable for a satisfactory exlanation of the fatigue strength of the samples with respect to their dimensions. One of the main reasons for displaying the scale effect in the process of steel fatigue is the sample self-heating, i.e. a temperature factor which in many cases overlaps a statistical one.

  3. Study of the 1.25Cr-1Mo-0.25V steel microstructure after a carburization phenomenon

    Energy Technology Data Exchange (ETDEWEB)

    Simonetti, S., E-mail: ssimonet@uns.edu.ar [Departamento de Fisica, Universidad Nacional del Sur, Av. Alem 1253, 8000 Bahia Blanca (Argentina); Departamentos de Ciencias Basicas e Ingenieria Mecanica, Universidad Tecnologica Nacional, 11 de Abril 461, 8000 Bahia Blanca (Argentina); Lanz, C. [Departamento de Ingenieria, Universidad Nacional del Sur, Av. Alem 1253, 8000 Bahia Blanca (Argentina); Brizuela, G.; Juan, A. [Departamento de Fisica, Universidad Nacional del Sur, Av. Alem 1253, 8000 Bahia Blanca (Argentina)

    2010-08-20

    We studied the changes in the structure and carbide particle size in 1.25Cr-1Mo-0.25V steel under 600 deg. C and 168 MPa, after 4000 h service. We used microscopy and microanalysis techniques to analyze the carbide particles. We performed a complementary theoretical study on the chemical bonding and electronic structure of the carbide-Fe matrix interaction. The results contribute to the understanding of the changes in the alloy microstructure caused by the carburization phenomenon.

  4. Corrosion-electrochemical behavior of metals in alkali solutions

    International Nuclear Information System (INIS)

    Levin, V.A.; Levina, E.Eh.

    1995-01-01

    Results of an investigation into corrosion-electrochemical behaviour of 12Kh18N10T, 10Kh17N13M2T, 08Kh21N6M2T and 15Kh25T steels, 06KhN28MDT and KhN78T alloys as well as NP-2 nickel in sodium, potassium and lithium hydroxide solutions at 95-180 deg C temperatures are considered. It is ascertained, that anode polarization curves of all metals irrespective of hydroxide nature, concentration, temperature, presence of chloride and chlorate additions, are of identic character. The movement of anode polarization curves in the direction of lower current of hydroxide type in NaOH-KOH-LiOH series, temperature and solution concentration reduction at other equal terms. 12 refs.; 6 figs

  5. TRANSFORMASI KURIKULUM PESANTREN: Telaah Pemikiran KH. MA. Sahal Mahfudh dan Nurcholish Madjid

    OpenAIRE

    Mukhlison Effendi; Suradi Suradi

    2016-01-01

    Abstract; Islamic boarding school is an indigenous Indonesia. Some contribution that given in the Islamization process, create a good community literacy and culture are very large. One reason, because there are Islamic boarding school curriculum transformation. Most influential enticement are KH. MA. Sahal Mahfudh and Nurcholish Madjid enticement. To knowing and determine the transformation both of those figures, the researcher take focus of study as: 1) the speculation of KH. MA. Sahal Mahfu...

  6. Enhancement of strength properties of hot rolled 10KHSND steel

    International Nuclear Information System (INIS)

    Nasibov, A.G.; Popova, L.V.; Pikulin, S.A.; Globa, N.I.

    1989-01-01

    To find out the reasons of low hot rolling yield for 10KhSND steel sheets in mechanical properties, titanium effect in the range of 0.008-0.03% concentrations is studied. It is established that the titanium content in a solid solution is conserved within 0.003-0.005%, the rest of titanium is bound to carbonitrides Ti(C, N). It is shown that alloys with 0.025-0.03% titanium content possess the increased values of ultimate and yield strength the necessary level of impact strength and good wealdability. The good steel yield, when the titanium content is sustained at the given level, increases from 40 to 85%

  7. Praktik Pemikiran Inklusif-Sosial KH M Sholeh Bahruddin Ngalah sebagai Manifestasi Pendidikan Multikultural Pesantren

    Directory of Open Access Journals (Sweden)

    M Anang Sholikhudin

    2016-12-01

    Full Text Available Dalam sejarah hidupnya, praktik pemikiran inklusif-sosial Kiai Sholeh sangat dipengaruhi oleh beberapa hal. Pertama, atas perintah ayahanda dengan pesan seperti berikut: “sak temene dek pasar, dek masjid, dek dalan, kabeh iku dulurmu (sesungguhnya baik di pasar, di masjid, maupun di jalanan, di seluruh tempat itu ada saudaramu.” Kedua, penerapan teori Abraham, yakni mencontoh perilaku ayahanda KH M Bahruddin Kalam (almarhum dan juga perilaku kakek KH M Kalam (almarhum. Ketiga, praktik dari rukun Tarekat Naqshabandiyah pada poin kelima dan keenam, yakni “ambugusi kabeh konco, cilik gede, lanang wadon, enom tuo, lan ambagusi kabeh makhluk (bergaul secara baik dengan semua teman, baik kecil maupun besar, laki-laki maupun perempuan, muda maupun tua, dan bergaul secara baik dengan semua makhluk.” Penelitian ini memfokuskan pada praktik pemikiran inklusif-sosial KH M Sholeh Bahruddin dengan model studi kasus, pendekatan yang dipakai adalah expose facto. Data diambil melalui observasi, wawancara serta dokumentasi. Penelitian menyimpulkan bahwa praktik pemikiran inklusif-sosial KH.. M. Sholeh Bahruddin sebenarnya mempertemukan misi perintah masing-masing agama (Islam, Kristen, Katolik, Budha dan Konghucu untuk membangun perdamaian, keamanan dan memelihara kasih sayang bersama-sama dan meminimalisir terjadinya konflik agama. || In the history of his life, the practice of inclusive social thought by Kiai Sholeh greatly influenced by several things. First, on the orders of his father with the following message: “In the markets, in the mosques, as well as on the streets, all over the places there are your brothers.” Secondly, the application of Abraham’s theory, which was practiced by KH M Bahruddin Kalam, the father (deceased of Kiai Sholeh, as well as KH M Kalam, the grandfather (deceased of Kiai Sholeh. Third, the practice of the Naqshabandi pillars that say: “being good with all friends, both small and great, both men and women, young

  8. On superplasticity of corrosion resistant ferritic-austenitic chromium-nickel steels

    Energy Technology Data Exchange (ETDEWEB)

    Surovtsev, A P; Sukhanov, V E

    1988-01-01

    The deformability of corrosion resistant chromium-nickel ferritic austenitic steel type O8Kh22N6T under tension, upsetting and torsion in the 600-1200 deg C temperature range is studied. For the deformation rate of the order of 10/sup -3/ s/sup -1/ the effect of superelasticity reveals itself at 850 deg C in the process of ferrite dynamic polymerization, in the 925-950 deg C range, at initial stages of dynamic recrystallization - the dynamic polygonization controlled by chromium carbide dissolving in steel and maximum at 1050 deg C in the process of development of austenite dynamic recrystallization with grain refinement with F/A ratio equalling 1. After upsetting in the elasticity mode at 1050 deg C the impact strength of the above steel is maximum.

  9. Creep and long-term strength of heat-resistant steels with different structures with the account taken of the type of stress deviator

    International Nuclear Information System (INIS)

    Giginyak, F.F.; Dragunov, Yu.G.; Mozharovskaya, T.N.; Titov, V.F.

    1993-01-01

    The results of the experimental investigations into creep and long-term strength of heat-resistant steels 15Kh2MFA and 15Kh2NMFA in the initial state and after heat-treatment simulating the metal irradiation embrittlement at the end of the product service date under static loading at the complex stress state and at high temperatures are presented. The experimentally substantiated equations of state describing creep and long-term stability of materials taking into account the type of the stress state are derived. (author)

  10. Interaction of steel, titanium and zirconium with melted chlorides containing copper and zinc

    International Nuclear Information System (INIS)

    Ozeryanaya, I.N.; Manukhina, T.I.; Shibanov, B.S.

    1976-01-01

    Cu and Zn coatings were obtained by contact displacement of their molten chlorides. Cu was deposited on Kh18N10T stainless steel, and Zn was deposited on Ti or Zr at 400-550 0 . Cu was displaced from the electrolyte by all components in the steel. A smooth coating exhibited high adhesion. According to metallography there was a transition layer of a Ni-Cr solid solution between the surface Cu layer and steel. With electronegetiol Ti and Zr, contact deposition of Zn or Cu from chloride melts was possible. The coatings were multilayer and exhibited adequate adhesion. The coating consisted of an intermetallic compound of Ti or Zr with Zn

  11. Killing Effects of an Isolated Serratia marcescens KH-001 on Diaphorina citri via Lowering the Endosymbiont Numbers

    Directory of Open Access Journals (Sweden)

    Wei Hu

    2018-05-01

    Full Text Available Huanglongbing (HLB is the most devastating citrus disease worldwide, and suppression of the Asian citrus psyllid (Diaphorina citri is regarded as an effective method to inhibit the spread of HLB. In this study, we isolated a strain named as Serratia marcescens KH-001 from D. citri nymphs suffering from disease, and evaluated its killing effect on D. citri via toxicity test and effect on microbial community in D. citri using high-throughput sequencing. Our results indicated that S. marcescens KH-001 could effectively kill 83% of D. citri nymphs, while the fermentation products of S. marcescens KH-001 only killed 40% of the D. citrinymphs. High-throughput sequencing results indicated that the S. marcescens KH-001 increased the OTU numbers from 62.5 (PBS buffer to 81.5, while significantly lowered the Shannon index compared with Escherichia coli DH5α (group E (p < 0.05. OTU analysis showed that the S. marcescens KH-001 had significantly reduced the relative abundance of endosymbionts Wolbachia, Profftella, and Carsonella in group S compared with that in other groups (p < 0.05. Therefore, the direct killing effect of the fermentation products of S. marcescens KH-001 and the indirect effect via reducing the numbers of endosymbionts (Wolbachia, Profftella, and Carsonella of D. citri endow S. marcescens KH-001 a sound killing effect on D. citri. Further work need to do before this strain is used as a sound biological control agents.

  12. Study of effect of austenite prehistory of 03Ch20N16AG6 steel on it structure and properties

    Energy Technology Data Exchange (ETDEWEB)

    Demchuk, I S; Krakhmalev, V I; Manninen, A I [Leningradskij Politekhnicheskij Inst. (USSR)

    1981-01-01

    Effect of preliminary cold working and different procedures of thermal treatment on structure and mechanical properties of stable austenite of 03Kh20N16AG6 steel is found out. It is shown that the degree of defectability of initial austenite structure predetermines the further deformation behaviour of the steel (level of strength characteristics, plasticity storage, hardening degree etc.) in the wide temperature range. Close connection of structural changes with properties should determine the choice of preliminary treatment of stable austenitic steel as applied to concrete condition of operation.

  13. Corrosion resistance of heat exchange equipment in hydrotreating Orenburg Condensate

    International Nuclear Information System (INIS)

    Teslya, B.M.; Burlov, V.V.; Parputs, I.V.; Parputs, T.P.

    1986-01-01

    The authors study the corrosion resistance of materials of construction and select appropriate materials for the fabrication of heat exchange equipment that will be serviceable under hydrotreating conditions. This paper discusses the Orenburg condensate hydrotreating unit which has been shut down repeatedly for repair because of corrosion damage to components of heat exchangers in the reactor section: tube bundles (08Kh18N10T steel), corrugated compensators (12Kh18N10T steel), and pins of the floating heads (37Kh13N8G8MFB steel). The authors recommend that the tube bundles and the compensators in heat exchangers in the reaction section should be fabricated of 08Kh21N6M2T or 10Kh17N13M2T steel. The pins have been replaced by new pins made of 10Kh17N13 X M2T steel, increasing the service life from 6-12 months to 2 years

  14. SCC growth behavior of stainless steel weld metals in high-temperature water. Influence of corrosion potential, weld type, thermal aging, cold-work and temperature

    International Nuclear Information System (INIS)

    Yamada, Takuyo; Terachi, Takumi; Miyamoto, Tomoki; Arioka, Koji

    2009-01-01

    Recent studies on crack growth rate measurement in oxygenated high-temperature pure water conditions, such as normal water chemistry in boiling water reactors, using compact tension type specimens have shown that weld stainless steels are susceptible to stress corrosion cracking. However, to our knowledge, there is no crack growth data of weld stainless steels in pressurized water reactor primary water. The principal purpose of this study was to examine the SCC growth behavior of stainless steel weld metals in simulated PWR primary water. A second objective was to examine the effect of (1) corrosion potential, (2) thermal-aging, (3) Mo in alloy and (4) cold-working on SCC growth in hydrogenated and oxygenated water environments at 320degC. In addition, the temperature dependence of SCC growth in simulated PWR primary water was also studied. The results were as follows: (1) No significant SCC growth was observed on all types of stainless steel weld metals: as-welded, aged (400degC x 10 kh) 308L and 316L, in 2.7 ppm-hydrogenated (low-potential) water at 320degC. (2) 20% cold-working markedly accelerated the SCC growth of weld metals in high-potential water at 320degC, but no significant SCC growth was observed in the hydrogenated water, even after 20% cold-working. (3) No significant SCC growth was observed on stainless steel weld metals in low-potential water at 250degC and 340degC. Thus, stainless steel weld metals have excellent SCC resistance in PWR primary water. On the other hand, (4) significant SCC growth was observed on all types of stainless steel weld metals: as-weld, aged (400degC x 10 kh) and 20% cold-worked 308L and 316L, in 8 ppm-oxygenated (high-potential) water at 320degC. (5) No large difference in SCC growth was observed between 316L (Mo) and 308L. (6) No large effect on SCC growth was observed between before and after aging up to 400degC for 10 kh. (7) 20% cold-working markedly accelerated the SCC growth of stainless steel weld metals. (author)

  15. Killing Effects of an Isolated Serratia marcescens KH-001 on Diaphorina citri via Lowering the Endosymbiont Numbers.

    Science.gov (United States)

    Hu, Wei; Kuang, Fan; Lu, Zhanjun; Zhang, Ning; Chen, Tingtao

    2018-01-01

    Huanglongbing (HLB) is the most devastating citrus disease worldwide, and suppression of the Asian citrus psyllid ( Diaphorina citri ) is regarded as an effective method to inhibit the spread of HLB. In this study, we isolated a strain named as Serratia marcescens KH-001 from D. citri nymphs suffering from disease, and evaluated its killing effect on D. citri via toxicity test and effect on microbial community in D. citri using high-throughput sequencing. Our results indicated that S. marcescens KH-001 could effectively kill 83% of D. citri nymphs, while the fermentation products of S. marcescens KH-001 only killed 40% of the D. citri nymphs. High-throughput sequencing results indicated that the S. marcescens KH-001 increased the OTU numbers from 62.5 (PBS buffer) to 81.5, while significantly lowered the Shannon index compared with Escherichia coli DH5α (group E) ( p citri endow S. marcescens KH-001 a sound killing effect on D. citri . Further work need to do before this strain is used as a sound biological control agents.

  16. Creep Rupture Analysis and Life Estimation of 1.25Cr-0.5Mo, 2.25Cr-1Mo and Modified 9Cr-1Mo Steel: A Comparative Study

    Science.gov (United States)

    Roy, Prabir Kumar

    2018-04-01

    This paper highlights a comparative assessment of creep life of 1.25Cr-0.5Mo, 2.25Cr-1Mo and modified 9Cr-1Mo steels based on accelerated creep rupture tests. Creep rupture test data have been analysed and creep life of the above mentioned materials have been assessed using Larson Miller parameter at the stress levels of 60 and 42 MPa for different temperatures. Limiting steam temperatures for minimum design life of 105 h at 42 and 60 MPa for the above mentioned steels have also been calculated. Microstructural studies for the three above mentioned steels are also done.

  17. A prominent figure in tatar dryhaeology. A. Kh. Khalikov’S 85th birthday anniversary

    Directory of Open Access Journals (Sweden)

    Khuzin Fayaz Sh.

    2014-06-01

    Full Text Available The article is devoted to scientific activity of Alfred Khasanovich Khalikov (May 30, 1929–July 24, 1994, an outstanding scholar, Dr. habil. (History, Professor, corresponding member of the Academy of Sciences of Tatarstan, a renowned specialist in archaeology and ancient history of the Turkic and Finno-Ugric peoples of the Volga-Ural region. A.Kh. Khalikov was a pioneer discoverer of hundreds of monuments referring to different archaeological periods, from the Paleolithic to modern times. However, the principal sphere of his scientific interests was medieval archaeology and history of the Volga region peoples. As head of major archaeological expeditions, such as the Mari, Tatar, Bilyar, “The Kazan Kremlin”, etc. ones, A.Kh. Khalikov had emerged as organizer of large-scale research in the territory of Tatarstan and other republics and regions of the Middle Volga region for 40 years,. A.Kh. Khalikov created an extensive cultural-chronological scheme of the Stone, the Chalcolithic, the Bronze and Early Iron ages in the Volga region, offered his own concept of ethnogenesis of the Finno-Ugric and Turkic peoples of the region. A.Kh. Khalikov authored over 400 articles and 20 books covering the origin and early history of the peoples of the Middle Volga and Ural regions. On his initiative, a complete list of archaeological monuments of Tatarstan in 6 volumes was created. Preservation of monuments of history and culture was an important direction of his activities. Professor A.Kh. Khalikov was engaged in fruitful teaching process at Kazan State University and created his own scientific school.

  18. The Historiography of Islamic Law: The Case of Tārīkh al-Tashrī‘ Literature

    Directory of Open Access Journals (Sweden)

    Arif Maftuhin

    2016-12-01

    Full Text Available Tārīkh al-Tashrī‘ (the history of sharia affairs is a relatively new genre of Islamic historiography and very popular among students of Islamic Law. Despite its popularity, academics of Islamic historiography seem not interested in studying it. There is hardly any academic paper seriously studied the literature. This paper is a first effort to explore the Tārīkhu’t-tashrī‘ literature through a historiographical analysis. As an initial exploration, it argues that Tārīkh al-Tashrī‘ is the latest development of Islamic historiography, developed in the 19th century, but it is a genre of the old Islamic historiography with some new elements. The new elements are influenced by both modern Western historiography and the need to re-open the supposedly closed gate of ijtihād. The paper studied books of Tārīkh al-Tashrī‘ available during the research between 2013-2015. [Tārīkh al-Tashrī‘ adalah genre yang relatif ‘baru’ dalam matarantai perkembangan historiografi Islam­. Literatur ini sangat popular dan menjadi mata kuliah wajib di fakultas-fakultas Syariah di Indonesia maupun Timur Tengah. Hanya saja, meskipun ia sangat populer sebagai mata pelajaran, Tārīkh al-Tashrī‘ belum banyak menarik minat para peneliti historiografi. Makalah in berusaha mengeksplorasi literatur Tārīkh al-Tashrī‘ dengan pendekatan historiografi. Makalah ini berpendapat bahwa Tārīkh al-Tashrī‘, meski terlihat ‘modern’ dari segi kelahirannya, tidak banyak berbeda dengan literatur historiografi klasik. Perbedaan terjadi karena adanya pengaruh historiografi Barat dalam model penulisannya dan karena kebutuhan untuk membuka kembali pintu ijtihad yang tertutup. Kajian dilakukan terhadap kitab-kitab Tārīkh al-Tashrī‘ yang dapat ditemukan selama riset antara 2013-2015 

  19. Mitigating Localized Corrosion Using Thermally Sprayed Aluminum (TSA) Coatings on Welded 25% Cr Superduplex Stainless Steel

    Science.gov (United States)

    Paul, S.; Lu, Q.; Harvey, M. D. F.

    2015-04-01

    Thermally sprayed aluminum (TSA) coating has been increasingly used for the protection of carbon steel offshore structures, topside equipment, and flowlines/pipelines exposed to both marine atmospheres and seawater immersion conditions. In this paper, the effectiveness of TSA coatings in preventing localized corrosion, such as pitting and crevice corrosion of 25% Cr superduplex stainless steel (SDSS) in subsea applications, has been investigated. Welded 25% Cr SDSS (coated and uncoated) with and without defects, and surfaces coated with epoxy paint were also examined. Pitting and crevice corrosion tests, on welded 25% Cr SDSS specimens with and without TSA/epoxy coatings, were conducted in recirculated, aerated, and synthetic seawater at 90 °C for 90 days. The tests were carried out at both the free corrosion potentials and an applied cathodic potential of -1100 mV saturated calomel electrode. The acidity (pH) of the test solution was monitored daily and adjusted to between pH 7.5 and 8.1, using dilute HCl solution or dilute NaOH, depending on the pH of the solution measured during the test. The test results demonstrated that TSA prevented pitting and crevice corrosion of 25% Cr SDSS in artificial seawater at 90 °C, even when 10-mm-diameter coating defect exposing the underlying steel was present.

  20. Observations on thermally cycled 20% Cr/25% Ni/Nb stabilised stainless steel

    International Nuclear Information System (INIS)

    Lobb, R.C.

    1984-06-01

    A variety of optical and electron techniques, such as optical metallography, scanning electron microscopy and electron probe microanalysis, have been used to study the morphology and composition of oxides formed on 20 Cr/25 Ni/Nb stainless steel during oxidation at 850 0 C and subsequent thermal cycling in simulated reactor gas. (author)

  1. High-cycle fatigue characteristics of weldable steel for light-water reactors

    International Nuclear Information System (INIS)

    Klesnil, M.; Polak, J.; Obrtlik, K.; Troshchenko, V.T.; Mishchenko, Yu.I.; Khamaza, L.A.

    1982-01-01

    Czechoslovak and Soviet 15Kh2NMFA steel was used for running fatigue tests at temperatures of 20, 350 and 400 degC in the high-cycle range with various loading regimes. The results show that at the given temperatures in this type of steel a cyclic softening occurs. The fatigue characteristics were measured with great dispersion of results, but within this dispersion they are almost identical for various steels at the same temperature. Increased temperature results in the decrease in the amplitude of cyclic deformation stress and in the increase in the amplitude of plastic deformation. The diversity in the values of cyclic plasticity and stress response measured in the given mode may be explained by the lower level of softening and the non-homogeneous cyclic plastic deformation of material under the given constant conditions. (J.B.)

  2. Specific electrical conductivity in molten potassium dihydrogen phosphate KH2PO4 - An electrolyte for water electrolysis at ∼300°C

    DEFF Research Database (Denmark)

    Nikiforov, Aleksey Valerievich; Berg, Rolf W.; Petrushina, Irina

    2016-01-01

    The conductivity of pure molten KH2PO4 salt and four mixtures with more or less water (KH2PO4-H2O and KH2PO4-KPO3 systems, respectively) were measured at temperatures of 240-320°C and under their own water vapor pressures. Molten KH2PO4 has been proven to be a promising electrolyte for an elevated...

  3. Cooling intensification during quenching of power plant components - the way to increase reliability

    International Nuclear Information System (INIS)

    Borisov, I.A.

    1989-01-01

    To enchance the complex of mechanical properties and to increase operation time of large components of power facilities, regimes of accelerated cooling are developed. Results of heat treatment with accelerated cooling of turbine rotor of steel 26KhN3M2FAA, disks of turbine welded rotor of steel 20KhN2MFAA, components of steel 35KhN3MFA, are given. Special steels with carbon content less than 0.30% for details of power machine-building are developed

  4. Effect of cold work on decarburization of 2.25Cr-1Mo steel in high temperature sodium

    International Nuclear Information System (INIS)

    Aoki, Norichika; Yoshida, Eiichi; Wada, Yusaku.

    1994-01-01

    It is known that the mechanical properties of a 2.25Cr-1Mo steel deteriorated due to the decarburization during immersion in the melt sodium at high temperatures. In low-alloy steel as well as a 2.25Cr-1Mo steel, precipitation reactions of carbides are known to be accelerated by cold working and aging. Thus, it may be expected that cold working and aging effectively suppress the decarburization of the mechanical properties of a 2.25Cr-1Mo steel because the decarburization will be restrained owing to fixation of carbon as precipitates of the carbides. In the present article, effects of cold-working and heat treatments on the kinetics of the decarburization of a 2.25Cr-1Mo steel has been studied experimentally. The annealed, cold-rolled, and normalized and tempered specimens were immersed in the melt of sodium at 500, 600 and 700degC for 425, 437 and 432h, respectively. On the basis of the observations obtained from these specimens, the experiment was also carried out at 450, 500 and 550degC for 2270 and 5465h. The microstructures before and after the immersion were observed with optical and scanning electron microscopes. An average concentration of carbon in each specimen was analyzed by an inert gas fusion method. The carbides extracted from the specimens were identified by X-ray diffraction. At immersion temperatures of 450 and 500degC, a 10% reduction of the decarburization in thickness by cold-working is sufficiently effective for retardation of the decarburization at both 2270 and 5465h. Whereas, at 550degC, more than 30% reduction in thickness by cold-working is needed for it at 2270h but even 80% reduction in thickness by cold-working causes merely slight retardation of the decarburization at 5465h. (author)

  5. Study of radiation damage of steels for light water pressure vessels at UJV

    International Nuclear Information System (INIS)

    Vacek, N.; Stoces, B.

    1980-01-01

    Preoperational determination of radiation resistance of pressure vessel steels is performed at accelerated neutron exposure in a test or materials research reactor. The results obtained at accelerated and operating exposure are not fully identical and surveillance bodies are therefore used manufactured from the pressure vessel material. Currently, the following steels are used for the manufacture of light water reactor pressure vessels: Mn-Mo-Ni (ASTM-A533-B, ASTM-A508), Cr-Mo-V (15Kh2M1FA). At UJV Rez, for irradiation Chanca-M probes imported from France are used featuring electric temperature control. Almost identical radiation embrittlement was measured for all three steels after irradiation with a neutron fluence of 3x10 23 n.m -2 at a temperature of 290 degC. (H.S.)

  6. The effects of minor alloy modifications and heat treatment on the microstructure and creep rupture behavior of 2.25Cr-1Mo Steel

    International Nuclear Information System (INIS)

    Todd, J.A.; Chung, D.W.; Parker, E.R.

    1983-01-01

    The effects of alloy additions on the microstructure of simulated cooled and tempered 2.25Cr-1Mo steels have been studied using transmission electron microscopy. Carbide precipitation sequences have been identified in the modification 3Cr-1Mo-1Mn-1Ni and compared to those in 2.25Cr-1Mo steels modified with Mn and Ni and also with Ti, V and B. The influence of minor compositional changes on the creep rupture behavior of 2.25Cr-1Mo steel has been studied at 500 C, 560 C, and 600 C. The most significant effect of alloy modifications on creep properties resulted from additions of Mn and Cr. Preliminary studies show that 1% Mn and 0.5Mn + 1Ni + 0.75Cr additions significantly reduce creep strength at all three temperatures for tests up to 2000 hours duration. The 3Cr-1Mo-1Mn-1Ni steel showed improvements in rupture ductility at all temperatures when compared with the base 2.25Cr-1Mo steel and the manganese-nickel modifications. Plots of the Larson-Miller parameter for both these modifications lay within the scatter band for commercial 2.25Cr-1Mo steels

  7. KOMPARASI PENDIDIKAN ISLAM K.H. AHMAD DAHLAN DAN MUHAMMAD FETHULLAH GÜLEN

    Directory of Open Access Journals (Sweden)

    Mohamad Ali

    2016-05-01

    Full Text Available Islamic education is considered only oriented to the hereafter alone, teach rituals and develop a defensive posture and formisme paradigm. On the other hand, Islamic education is faced with the phenomenon of discontinuity which marked the waning value of respect for the basic values and ethics, such as honesty, discipline, tolerance. This Problem is what ignited K.H. Ahmad Dahlan (1868-1923 and Muhammad Fethullah Gülen (1838 - ... strengthening Islamic education. This study aims to understand the concepts, practices, and comparative Islamic education K.H. Ahmad Dahlan and Muhammad Fethullah Gülen. This type of research is the study of literature  with historical and philosophical approach. The results show: first, the concept of Islamic education K.H. Ahmad Dahlan stressed intregration of religious sciences and the modern sciences, tolerance, open to modernity and perfection of mind (intellect; for Fethullah Gülen education is a manifestation of Allah, which emphasizes ethics, science, and theology. Secondly, the common the sharing concept between the two are at: ideas, foundation, educational goals and teaching methods. Third, while the point of difference lies in the educational materials, dormitory educational models (boarding school and implementing a system of moving class.

  8. Study of nitrogen solubility in multicomponent iron alloys at its pressure in gaseous phase up to 1000kPa

    International Nuclear Information System (INIS)

    Pomarin, Yu.M.; Grigorenko, G.M.; Latash, Yu.V.; Kanibolotskij, S.A.

    1983-01-01

    A facility in which metal is melted in a weighed state and nitrogen partical pressure during relting may be charge from 0 to 1000 kPa is developed to investigate nitrogen solubility is liquim metals and alloys. Investigation of nitrogen solubility was performed using samples of 03Kh25N5AM3 steel and Kh20N5, Kh20N10, Kh40N10, Kh40N20 alloys. Positive deflection of [N]=f(√Psub(Nsub(2))) dependence from the Henry law is shown to be observed in the Kh40N10 alloy in the 100-1000 kPa pressure range. In this case the vatue of positive deflection decreases with temperature growth and at T=2273 K nitrogen solubility in the alloy submits to the law of square root. An equation permitting to calculate nitrogen solubility in alloys of Fe-Cr-Ni and Fe-Cr-Mn systems in the 0 to 1000 kPa range of nitrogen partial pressures is obtained

  9. A Page and Its Politics: Situating Kullinā Khālid Saʿīd in Egypt’s Ideological Landscape at the Time of Revolution

    NARCIS (Netherlands)

    Woltering, R.; Abdulla, R.; Poell, T.; Rieder, B.; Zack, L.

    2015-01-01

    In discussions concerning the importance of social media in the 25January revolution, a central role is given to the "Kullinā Khālid Saʿīd" [We’re all Khaled Said] Facebook page. Using an advanced data collection and extraction application called Netvizz, a research team consisting of Arabists and

  10. REVIVALISME PENDIDIKAN ISLAM AWAL ABAD 20 (STUDI KRITIS PEMBARUAN PENDIDIKAN ISLAM PERSPEKTIF KH. AHMAD DAHLAN

    Directory of Open Access Journals (Sweden)

    Zetty Azizatun Ni'mah

    2016-05-01

    Full Text Available The idea of Islamic educational reform in Indonesia began in the early twentieth century. This was caused by out of concerns Muslim intellectual leaders of the secular education system which implemented the Dutch East Indies and then has a negative impact on the condition of Islamic education in Indonesia. KH. Ahmad Dahlan is pioneer figure of Islamic educational reform in Indonesia. He is of leaders respond to the condition of Islamic education in Indonesia needs to be updated in terms of objectives, materials, methods and management. This article aims to analyze thoughts KH. Ahmad Dahlan. KH. Ahmad Dahlan reform of Islamic education as well as his correlation with the current education system. This issues is examined using research methods “library research” using written materials in the form of books, magazines, journals, articles and other literatures relevant to the discussion. For data analysis the authors use the approach of history, sociology and anthropology. The results of the research that has been conducted by the author suggests that the concept of Islamic education reform in perspective KH. Ahmad: the aim of Islamic education leads to increased economic, politic, social race with modernism education, the Qur’an and Hadits are direct material examined by leaving the classic are often assessed the traditionalists, Islamic education methods abandon traditional methods, the Islamic educational institutions organized under auspices of the Muhammadiyah organization with a model of organizational leadership. Educational issues such as character building, problem solving, integration of scientific and educational innovation are concepts of education offered by KH.Ahmad Dahlan which it is an attempt to anticipate the renewal of the times and the situation in the subsequent periods.

  11. Properties of cast Ti-stabilised stainless steel after long-term ageing

    International Nuclear Information System (INIS)

    Ehrnsten, U.; Karjalainen-Roikonen, P.; Nenonen, P.; Ahlstrand, R.; Hietanen, O.; Timofeev, B.T.; Bloomin, A.A.

    2000-01-01

    Mechanical properties and microstructure are studied and compared for two kinds of specimens of cast Ti-stabilized stainless steel 08Kh18N10T used for manufacturing of valves and pumps in nuclear power plants. One set of specimens represents the main gate valve material after 106000 h (∼ 12 years) operation at 270 deg C. The comparison is made with reference specimens in as-fabricated state. The results of impact tests, hardness measurements and microscopic examination show that 12 year operation gives rise to the shift of ductile-brittle transition temperature to higher values (from - 68 deg C - 103 deg C). The microstructure of both materials is similar. The microhardness of δ-ferrite in the steel after long-term operation is slightly higher [ru

  12. Automation of ultrasonic testing of turbine disk billets

    International Nuclear Information System (INIS)

    Gorodkov, V.E.; Domashevskij, B.N.; Pron', N.I.; Tkachenko, V.A.

    1984-01-01

    cations of ultrasonic facility for automation of testing turbine disk billets of 25Kh2PMFA and 34KhM1A steels are considered. The operating principle and the design of ''Disk-1'' facility are described, its test results are presented. It is shown that the facility increases the test efficiency five times, enables to estimate dimensions of revealed defect with regard to the quality of acoustic contact, thus facilitating the work of personnel and improving the test quality

  13. A theory of piezoelectric, elastic, and dielectric properties of the KH2PO4 family crystals under the strain u6. Phase transition and the piezoelectric effect in the KH2PO4 crystal

    International Nuclear Information System (INIS)

    Levits'kij, R.R.; Lyisnij, B.M.

    2003-01-01

    In order to study the dielectric, piezoelectric and elastic properties of ferroelectrics and antiferroelectrics of the KH 2 PO 4 family, we consider an extended proton tunneling model that takes into account the shear strain u 6 . In the four-particle cluster approximation for the short-range interactions and the mean field approximation for the long-range interaction we calculate the transverse components of the dielectric susceptibility tensor of the KH 2 PO 4 family ferroelectrics

  14. Water vapor pressure over molten KH_2PO_4 and demonstration of water electrolysis at ∼300 °C

    International Nuclear Information System (INIS)

    Berg, R.W.; Nikiforov, A.V.; Petrushina, I.M.; Bjerrum, N.J.

    2016-01-01

    Highlights: • The vapor pressure over molten KH_2PO_4 was measured by Raman spectroscopy to be about 8 bars at ∼300 °C. • Raman spectroscopy shows that molten KH_2PO_4 under its own vapor pressure contains much dissolved water. • It is demonstrated spectroscopically that water electrolysis is possible in KH_2PO_4 electrolyte forming H_2 and O_2 at 300 °C. • Molten KH_2PO_4 is a possible electrolyte for water electrolysis. - Abstract: A new potentially high-efficiency electrolyte for water electrolysis: molten monobasic potassium phosphate, KH_2PO_4 or KDP has been investigated at temperatures ∼275–325 °C. At these temperatures, KH_2PO_4 was found to dissociate into H_2O gas in equilibrium with a melt mixture of KH_2PO_4−K_2H_2P_2O_7−KPO_3−H_2O. The water vapor pressure above the melt, when contained in a closed ampoule, was determined quantitatively vs. temperature by use of Raman spectroscopy with methane or hydrogen gas as an internal calibration standard, using newly established relative ratios of Raman scattering cross sections of water and methane or hydrogen to be 0.40 ± 0.02 or 1.2 ± 0.03. At equilibrium the vapor pressure was much lower than the vapor pressure above liquid water at the same temperature. Electrolysis was realized by passing current through closed ampoules (vacuum sealed quartz glass electrolysis cells with platinum electrodes and the electrolyte melt). The formation of mixtures of hydrogen and oxygen gases as well as the water vapor was detected by Raman spectroscopy. In this way it was demonstrated that water is present in the new electrolyte: molten KH_2PO_4 can be split by electrolysis via the reaction 2H_2O → 2H_2 + O_2 at temperatures ∼275–325 °C. At these temperatures, before the start of the electrolysis, the KH_2PO_4 melt gives off H_2O gas that pressurizes the cell according to the following dissociations: 2KH_2PO_4 ↔ K_2H_2P_2O_7 + H_2O ↔ 2KPO_3 + 2H_2O. The spectra show however that the water by

  15. Effect of boron on the hot ductility of 2.25Cr1Mo steel

    International Nuclear Information System (INIS)

    Song, S.-H.; Guo, A.-M.; Shen, D.-D.; Yuan, Z.-X.; Liu, J.; Xu, T.-D.

    2003-01-01

    The effect of boron on the hot ductility of 2.25Cr1Mo steel is investigated by means of a Gleeble 2000 thermomechanical simulator. There is a trough in the hot ductility-temperature curve, which is located between 1000 and 700 deg. C. The ductility trough shifts to lower temperatures with increasing boron content and the hot brittle range becomes shallow and narrow. In general, boron may improve the steel hot ductility in that it may retard the formation of pro-eutectoid ferrite and increase grain boundary cohesion. These effects may be related to the segregation of boron to austenite grain boundaries

  16. Relationship of acoustic emission to the kinetics and micromechanism of fatigue failure of high-strength steel with a martensitic structure

    International Nuclear Information System (INIS)

    Romaniv, O.N.; Kirillov, K.I.; Zima, Yu.V.; Nikiforchin, G.N.

    1987-01-01

    Techniques and results are presented for the rules of change in acoustic emission in fatigue crack propagation in hardened and low-temperature tempered 40Kh steel intended, in this study, for use as a reactor material. The results of the acoustic measurements are compared with data of quantitative aimed microfractography conducted during mechanical fracture tests

  17. Operational reliability of high pressure steam lines of pearlitic steels after 150-200 thousand h service

    International Nuclear Information System (INIS)

    Veksler, E.Ya.; Chajkovskij, V.M.; Osasyuk, V.V.

    1980-01-01

    Usage of both calculational and physical methods is recommended to estimate a service operating life of long-term working steam line materials. Application of these methods is demonstrated when studying steam line bends made of 12MKh and 12Kh1MF pearlitic steels. Good coincidence of results for the determination of residual durability of steam lines is obtained using these two methods [ru

  18. Influence of corrosion environment composition on crack propagation in high-strength martensitic steel

    International Nuclear Information System (INIS)

    Romaniv, O.N.; Nikiforchin, G.N.; Tsirul'nik, A.T.

    1984-01-01

    The 40 Kh steel is taken as an example to investigate the dependence of electrochemical parameters in the crack tip and characteristics of corrosion static cracking resistance of martensitic steel on the composition of environment. The tests are performed in acidic and alkaline solutions prepared by adding HC or NaOH in distilled water. It is established that growth of pH value of initial solutions trom 0 to 13 brings about linear increase of a threshold stress intensity factor. It is found that acidic medium in the crack tip preserves up to pH 13 of initial medium. The possibility of corrosion crack propagation in alkaline solutions according to the mechanism of hydrogen embrittlement is proved

  19. Smelting of high-quality boiler steel in large-load arc furnaces

    Energy Technology Data Exchange (ETDEWEB)

    Kablukovskij, A F; Breus, V M; Tyurin, E I; Khristich, V D; Dumchev, Ya P [Tsentral' nyj Nauchno-Issledovatel' skij Inst. Chernoj Metallurgii, Moscow (USSR)

    1975-02-01

    High-grade steel can be obtained in large-capacity furnaces if the smelting technology used takes account of the size of the aggregates, the course of the metal fusion process, interaction with slag, furnace atmosphere, reducing agents, and other process characteristics. 12Kh1MF boiler steel smelted in a 100-ton electric arc furnace by an oxidizing process with oxygen bath blow and cast by the siphon method into 6.5-ton ingots using a slag-forming mixture (240 mm diameter billets and 219 to 245 mm diameter tubes) is satisfactory with regard to macro and microstructure, oxygen and nonmetallic oxide inclusion content, and mechanical properties. The stress rupture strength of 10/sup 5/ h at 570/sup 0/C is similar to that of open-hearth steel. Sulfides larger than a 3.5 spheroid have been detected in it. The nitrogen content of the electric steel is 0.0090 to 0.0120%, which is somewhat greater than usual in open-hearth metal. Of the oxygen inclusions in the steel, spinel-alumina predominates. Large inclusions were represented mainly by brittle silicates which appeared to be of exogenous origin.

  20. Boron content effect on the high-temperature plasticity of corrosion resistant low-carbon austenite type steels

    International Nuclear Information System (INIS)

    Gol'dshtejn, Ya.E.; Shmatko, M.N.; Chuvatina, S.N.

    1976-01-01

    With the concept that the state of grain and subgrain boundaries influences the hot plasticity of corrosion resistant steel as a starting point, the study was undertaken of the effect of boron microalloying up on the intergranular strength and of the action boron exerts upon the distribution (redistribution) of other phases present in austenitic 03Kh16N14M3 steels. An electron microscope study of the composition of redundant phases and that of the fine structure of steel have shown the effect of small additions of boron upon the hot plasticity of steel to be linked directly to its influence upon austenite disintegration and the precipitation along the boundaries of crystals of redundant phases in the course of hot plastic deformation. The action of boron upon the process plasticity of steel depends on the temperature and the rate of deformation which govern the kinetics of the precipitation of the redundant phases

  1. [Effect of KH2PO4 on the odonto- and osteogenic differentiation potential of human stem cells from apical papillae].

    Science.gov (United States)

    Wang, Yan-ping; Wu, Jin-tao; Wang, Zi-lu; Zheng, Yang-yu; Zhang, Guang-dong; Yu, Jin-hua

    2013-01-01

    To determine the effects of KH2PO4 on the odonto- and osteogenic differentiation potential of human stem cells from apical papillae (SCAP) in vitro. SCAP were isolated and cultured respectively in alpha minimum essential medium (α-MEM) or α-MEM containing 1.8 mmol/L KH2PO4. Alkaline phosphatase (ALP) activity, alizarin red staining, real-time reverse transcription polymerase chain reaction (RT-PCR) and Western blotting were used to examine the odonto and osteogenic potential of SCAP in the two media. SCAP cultured in α-MEM containing 1.8 mmol/L KH2PO4 exhibited a higher ALP activity [(0.370 ± 0.013) Sigma unit×min(-1)×mg(-1)] at day 3 than control group [(0.285 ± 0.008) Sigma unit×min(-1)×mg(-1)] and KH2PO4-treated SCAP formed more calcified nodules at day 5 [(0.539 ± 0.007) µg/g] and day 7 [(1.617 ± 0.042) µg/g] than those in normal medium [(0.138 ± 0.037) µg/g, P odonto- and osteogenic markers were significantly up-regulated after the stimulation of KH2PO4 at day 3 and 7 respectively, as compared with control group. 1.8 mmol/L KH2PO4 can promote the odonto and osteogenic differentiation potential of human SCAP.

  2. Mutation and crystallization of the first KH domain of human polycytosine-binding protein 1 (PCBP1) in complex with DNA

    International Nuclear Information System (INIS)

    Yoga, Yano M. K.; Traore, Daouda A. K.; Wilce, Jacqueline A.; Wilce, Matthew C. J.

    2011-01-01

    The successful preparation of a mutant KH domain representing the first KH domain of PCBP1 and its crystallization in complex with a C-rich DNA are reported. This structure is anticipated to provide high-resolution information that will allow better understanding of the basis of cytosine specificity by PCBPs. Polycytosine-binding proteins (PCBPs) are triple KH-domain proteins that play an important role in the regulation of translation of eukaryotic mRNA. They are also utilized by viral RNA and have been shown to interact with ssDNA. Underlying their function is the specific recognition of C-rich nucleotides by their KH domains. However, the structural basis of this recognition is only partially understood. Here, the preparation of a His-tagged KH domain is described, representing the first domain of PCBP1 that incorporates a C54S mutation as well as the addition of a C-terminal tryptophan. This construct has facilitated the preparation of highly diffracting crystals in complex with C-rich DNA (sequence ACCCCA). Crystals of the KH1–DNA complex were grown using the hanging-drop vapour-diffusion method in 0.1 M phosphate–citrate pH 4.2, 40%(v/v) PEG 300. X-ray diffraction data were collected to 1.77 Å resolution and the diffraction was consistent with space group P2 1 , with unit-cell parameters a = 38.59, b = 111.88, c = 43.42 Å, α = γ = 90.0, β = 93.37°. The structure of the KH1–DNA complex will further our insight into the basis of cytosine specificity by PCBPs

  3. Evolution of the structure and the phase composition of a bainitic structural steel during plastic deformation

    Science.gov (United States)

    Nikitina, E. N.; Glezer, A. M.; Ivanov, Yu. F.; Aksenova, K. V.; Gromov, V. E.; Kazimirov, S. A.

    2017-10-01

    The evolution of the phase composition and the imperfect substructure of the 30Kh2N2MFA bainitic structural steel subjected to compressive deformation by 36% is quantitatively analyzed. It is shown that deformation is accompanied by an increase in the scalar dislocation density, a decrease in the longitudinal fragment sizes, an increase in the number of stress concentrators, the dissolution of cementite particles, and the transformation of retained austenite.

  4. Reflection of K.H. Ahmad Dahlan’s educational ideas for school development

    Directory of Open Access Journals (Sweden)

    S. Suripto

    2017-09-01

    Full Text Available This research was aimed to reflect the form of K.H. Ahmad Dahlan’s educational ideas in schools. The kind of this research was qualitative with multi sites approach.  The research was conducted at MTs Muhammadiyah 2 and Muhammadiyah 1 Vocational School – Trenggalek.The object of this research was the form of K.H. Ahmad Dahlan’s educational ideas whereas the subject was all the school's administrators. Data were collected through deep interview, documentation and observation techniques. Data validity was tested with; credibility, transferability, and confirmability. Data analysis model was interractionally each other; data reduction, data presentation, conclusion withdrawal, and verification. The research result were; first, at MTs Muhammadiyah 2, the form of K.H. Ahmad Dahlan’s educational ideas covered: Muhammadiyah values, such as a. TBC eradication, worry attitude towards the improvement of fundamentalist religious culture in the society (LDII, b. Willingness to sacrifice attitude grown by the school founders’ core team, organizers, and administrators; c. The spirit of dakwah and dedication for the nation and the religion. Second, at Muhammadiyah 1 Vocational School, it covered a. Charity effort movement for all (rahmatan lilalamin; b. Amar maruf nahy munkar was formed in the construction of all field of life, c. Working was the spirit of movement organization. Keywords: educational ideas, school development

  5. Specific Features of Structural-Phase State and Properties of Reactor Pressure Vessel Steel at Elevated Irradiation Temperature

    Directory of Open Access Journals (Sweden)

    E. A. Kuleshova

    2017-01-01

    Full Text Available This paper considers influence of elevated irradiation temperature on structure and properties of 15Kh2NMFAA reactor pressure vessel (RPV steel. The steel is investigated after accelerated irradiation at 300°C (operating temperature of VVER-1000-type RPV and 400°C supposed to be the operating temperature of advanced RPVs. Irradiation at 300°C leads to formation of radiation-induced precipitates and radiation defects-dislocation loops, while no carbide phase transformation is observed. Irradiation at a higher temperature (400°C neither causes formation of radiation-induced precipitates nor provides formation of dislocation loops, but it does increase the number density of the main initial hardening phase—of the carbonitrides. Increase of phosphorus concentration in grain boundaries is more pronounced for irradiation at 400°C as compared to irradiation at 300°C due to influence of thermally enhanced diffusion at a higher temperature. The structural-phase changes determine the changes of mechanical properties: at both irradiation temperatures irradiation embrittlement is mainly due to the hardening mechanism with some contribution of the nonhardening one for irradiation at 400°C. Lack of formation of radiation-induced precipitates at T = 400°C provides a small ΔTK shift (17°C. The obtained results demonstrate that the investigated 15Kh2NMFAA steel may be a promising material for advanced reactors with an elevated operating temperature.

  6. A luminary of tatar archaeology. To the 85th anniversary of the birth of A.Kh. Khalikov

    Directory of Open Access Journals (Sweden)

    Khuzin Fayaz Sh.

    2014-06-01

    Full Text Available The article is devoted to scientific activity of Alfred Khasanovich Khalikov (May 30, 1929–July 24, 1994, an outstanding scholar, Dr. habil. (History, Professor, corresponding member of the Academy of Sciences of Tatarstan, a renowned specialist in archaeology and ancient history of the Turkic and Finno-Ugric peoples of the Volga-Ural region. A.Kh. Khalikov was a pioneer discoverer of hundreds of monuments referring to different archaeological periods, from the Paleolithic to modern times. However, the principal sphere of his scientific interests was medieval archaeology and history of the Volga region peoples. As head of major archaeological expeditions, such as the Mari, Tatar, Bilyar, “The Kazan Kremlin”, etc. ones, A.Kh. Khalikov had emerged as organizer of large-scale research in the territory of Tatarstan and other republics and regions of the Middle Volga region for 40 years,. A.Kh. Khalikov created an extensive cultural-chronological scheme of the Stone, the Chalcolithic, the Bronze and Early Iron ages in the Volga region, offered his own concept of ethnogenesis of the Finno-Ugric and Turkic peoples of the region. A.Kh. Khalikov authored over 400 articles and 20 books covering the origin and early history of the peoples of the Middle Volga and Ural regions. On his initiative, a complete list of archaeological monuments of Tatarstan in 6 volumes was created. Preservation of monuments of history and culture was an important direction of his activities. Professor A.Kh. Khalikov was engaged in fruitful teaching process at Kazan State University and created his own scientific school.

  7. Properties of welded joints of 2,25Cr-1Mo steel with various carbon content

    International Nuclear Information System (INIS)

    Vornovitskij, I.N.; Brodetskaya, E.Z.; Pozdnyakova, A.S.

    1980-01-01

    Properties of welded joints of 2,25 Cr - 1 Mo steel pipelines with different carbon content are considered. It is shown that application of electrodes developed in some countries for welding permits in many cases to exclude heat treatment of welded joints owing to high ductility of weld deposited metal. To improve the ductility, it is necessary to limit both carbon content down to 0,03-0,06% and detrimental elements (sulfur, phosphorus). Heat affected zone hardness may be increased at the expense of carbon. Weld deposited metal possesses the highest long-term strength at the given test temperature; in this case long-term strength of welded joints and base metal is practically the same. The long-term strength of high-carbon steel is higher at the test temperature of 565 deg C as compared to mean-carbon and low-carbon steels, whose long-term strength is practically equal at this temperature. The long-term strength of high-carbon and mean-carbon steels is practically the same and higher as compared with low-carbon one at the test temperature of 510 deg C

  8. Low cycle fatigue behavior of Sanicro25 steel at room and at elevated temperature

    Czech Academy of Sciences Publication Activity Database

    Polák, Jaroslav; Petráš, Roman; Heczko, Milan; Kuběna, Ivo; Kruml, Tomáš; Chai, G.

    2014-01-01

    Roč. 615, OKT (2014), s. 175-182 ISSN 0921-5093 R&D Projects: GA ČR(CZ) GA13-23652S Institutional support: RVO:68081723 Keywords : Sanicro 25 steel * Cyclic plasticity * Dislocation structure * Fatigue life * Effect of temperature Subject RIV: JL - Materials Fatigue, Friction Mechanics Impact factor: 2.567, year: 2014

  9. Hot deformation effect on the kinetics of austenite transformation under continuous cooling conditions

    International Nuclear Information System (INIS)

    Bernshtejn, M.L.; Zajmovskij, V.A.; Kisteh, N.V.; Samedov, O.V.; Faldin, S.A.

    1979-01-01

    The effect of hot deformation on the kinetics of austenite transformations in the commercial 4040Kh 40KhN, and 40KhNMA steels on continuous cooling was studied. The transformations were studied using a dilatometer of a special design which permits a specimen to be fixed quickly in holders after hot deformation. It is stated that in hot-deformed austenite the pearlite transformation proceeds at higher temperatures and in a narrower temperature range. Austenite deformation provides an opportunity to obtain a more fine ferrite-pearlite structure and ensures a uniform distribution of a structurally free ferrite in the steel bulk. The effect of hot deformation on the structure of ferrite decomposition products in the 40KhN and 40KhNMA steels is more complicated, which is connected with a substantial change in the kinetics of pearlite and intermediate transformations

  10. Effect of cyclic electron irradiation on mechanical properties of austenite steel

    International Nuclear Information System (INIS)

    Tsepelev, A.B.; Sadykhov, S.I.O.; Chernov, A.I.; Sevost'yanov, M.A.

    2006-01-01

    To check the supposition on the possibility of radiation-stimulated process enhancement under cyclic irradiation conditions an experimental investigation is carried out to elucidate the effect of the mode of irradiation (continuous or cyclic) on mechanical properties of chromium-manganese austenitic stainless steel type 10Kh12G20V. The effect of some radiation hardening is observed under cyclic irradiation, however, the data obtained cannot be considered as good evidence for the validity of proposed model of dynamic preference if the scatter in experimental data is taken into account [ru

  11. Thermal fatigue strength estimation of 2.25Cr-1Mo steel under creep-fatigue interaction

    International Nuclear Information System (INIS)

    Kuwahara, Kazuo; Nitta, Akihito; Kitamura, Takayuki

    1980-01-01

    A 2-1/4Cr-1Mo steel is one of principal materials for high temperature equipments in nuclear and thermal power plants. The authors experimentally analyzed the high temperature fatigue strength and creep strength of a 2-1/4 Cr-1Mo steel main steam pipe which had been used in a thermal plant for operation up to 130,000 hours, and pointed out that the strain-range vs. life curves crossed each other due to the difference of temperature-strain phase in thermal fatigue. This suggests that it is difficult to estimate thermal fatigue life of steel materials having been subjected to different temperature-strain phase on the basis of isothermal low-cycle fatigue life at the upper limit temperature of thermal fatigue, and that it is urgently required to establish an appropriate method of evaluating thermal fatigue life. The authors attempted to prove that the strain range partitioning method used for the evaluation of thermal fatigue life in SUS 304 steels is applicable to this 2-1/4Cr-1Mo steel. Consequently, it was found that the thermal fatigue life could be estimated within a factor of 2.5 by the application of this method. (author)

  12. Specific electrical conductivity in molten potassium dihydrogen phosphate KH2PO4 - An electrolyte for water electrolysis at ∼300°C

    DEFF Research Database (Denmark)

    Nikiforov, Aleksey Valerievich; Berg, Rolf W.; Petrushina, Irina

    2016-01-01

    The conductivity of pure molten KH2PO4 salt and four mixtures with more or less water (KH2PO4-H2O and KH2PO4-KPO3 systems, respectively) were measured at temperatures of 240-320°C and under their own water vapor pressures. Molten KH2PO4 has been proven to be a promising electrolyte for an elevated...... temperature pressurized water electrolyzer demonstrating high conductivity of ∼0.30Scm-1 at 300°C. The conductivity data are given as polynomial functions of temperature and composition. The melting point of the pure salt under its own water vapor pressure was determined to be ∼272°C....

  13. Aging behaviour of 25Cr-17Mn high nitrogen duplex stainless steel

    OpenAIRE

    Machado, I. F.; Padilha, A. F.

    2000-01-01

    The precipitation behaviour of a nickel free stainless steel containing 25% chromium, 17% manganese and 0.54% nitrogen, with duplex ferritic-austenitic microstructure, was studied using several complementary techniques of microstructural analysis after aging heat treatments between 600 and 1 000 degrees C for periods of lime between 15 and 6 000 min. During aging heat treatments, ferrite was decomposed into sigma phase and austenite by a eutectoid reaction, like in the Fe-Cr-Ni duplex stainle...

  14. AERODYNAMIC IMPROVEMENT OF KhADI 33 RACING CAR RADIATOR COMPARTMENT

    Directory of Open Access Journals (Sweden)

    A. Avershyn

    2011-01-01

    Full Text Available Aerodynamic characteristics of radiator compartment of KhADI 33 racing car on the basis of the decision of the interfaced problem of internal and external aerodynamics are numerically investigated. The rational variant of radiator compartment which is characterized by high throughput and low level of non-uniformity of speed field at the input is offered.

  15. Corrosion resistance of metals and alloys in molten alkalies

    International Nuclear Information System (INIS)

    Zarubitskij, O.G.; Dmitruk, B.F.; Minets, L.A.

    1979-01-01

    Literature data on the corrosion of non-ferrous and noble metals, iron and steels in the molten alkalis and mixtures of their base are presented. It is shown that zirconium, niobium and tantalum are characterized by high corrosion stability in the molten NaOH. Additions of NaOH and KOH to the alkali chloride melts result in a 1000 time decrease of zirconium corrosion rate at 850 deg. The data testify to the characteristic passivating properties of OH - ions; Mo and W do not possess an ability to selfpassivation in hydroxide melts. Corrosion resistance of carbon and chromium-nickel steels in hydroxide melts depends considerably on the temperature, electrolyte composition and atmosphere over them. At the temperatures up to 600 deg C chromium-nickel steel is corrosion resistant in the molten alkali only in the inert atmosphere. Corrosion rate of chromium-nickel alloy is the lower the less chromium and the more nickel it contains. For the small installations the 4Kh18N25S2 and Kh23N28M3D3T steels can be recommended

  16. On abnormal decomposition of supercooled austenite in carbon and alloy steels

    International Nuclear Information System (INIS)

    Parusov, V.V.; Dolzhenkov, I.I.; Podobedov, L.V.; Vakulenko, I.A.

    1980-01-01

    Residual stresses which appear as a result of thermal cycling in the temperature range of 300-700 deg C are investigated in an austenitic class steel (03Kh18N11) to ground the assumption on the effect of plastic deformation, appearing due to thermal stresses, on the mechanism of supercooled austenite decomposition. The determination of residual stresses is carried out with the help of X-ray diffraction analysis. It is established that the deformation brings about an increase in density of dislocation the interaction of which leads to the formation of a typical austenite substructure which conditions the proceeding of the eutectoid transformation according to an abnormal mechanism. It is noted, that the grain pearlite formation due to plastic and microplastic deformation of supercooled austenite induced by thermal stresses should be taken into account when developing steel heat treatment shedules [ru

  17. Water vapor pressure over molten KH2PO4 and demonstration of water electrolysis at ∼300ºC

    DEFF Research Database (Denmark)

    Berg, Rolf W.; Nikiforov, Aleksey Valerievich; Petrushina, Irina

    2016-01-01

    A new potentially high-efficiency electrolyte for water electrolysis: molten monobasic potassium phosphate, KH2PO4 or KDP has been investigated at temperatures ∼275–325 °C. At these temperatures, KH2PO4 was found to dissociate into H2O gas in equilibrium with a melt mixture of KH2PO4—K2H2P2O7—KPO3...... of water and methane or hydrogen to be 0.40 ± 0.02 or 1.2 ± 0.03. At equilibrium the vapor pressure was much lower than the vapor pressure above liquid water at the same temperature. Electrolysis was realized by passing current through closed ampoules (vacuum sealed quartz glass electrolysis cells...... with platinum electrodes and the electrolyte melt). The formation of mixtures of hydrogen and oxygen gases as well as the water vapor was detected by Raman spectroscopy. In this way it was demonstrated that water is present in the new electrolyte: molten KH2PO4 can be split by electrolysis via the reaction 2H2O...

  18. New 1H-pyrrole-2,5-dione derivatives as efficient organic inhibitors of carbon steel corrosion in hydrochloric acid medium: Electrochemical, XPS and DFT studies

    International Nuclear Information System (INIS)

    Zarrouk, A.; Hammouti, B.; Lakhlifi, T.; Traisnel, M.; Vezin, H.; Bentiss, F.

    2015-01-01

    Highlights: • 1H-pyrrole derivatives act as good corrosion inhibitors for carbon steel in 1 M HCl. • Adsorption of the inhibitors on carbon steel surface obeys Langmuir’s isotherm. • XPS showed that the inhibitors are chemisorbed on the metal surface. • Quantum chemical parameters were correlated with experimental results. - Abstract: New 1H-pyrrole-2,5-dione derivatives, namely 1-phenyl-1H-pyrrole-2,5-dione (PPD) and 1-(4-methylphenyl)-1H-pyrrole-2,5-dione (MPPD) were synthesised and their inhibitive action against the corrosion of carbon steel in 1 M HCl solution were investigated at 308 K by weight loss, potentiodynamic polarization curves, and electrochemical impedance spectroscopy (EIS) methods. The results showed that the investigated 1H-pyrrole-2,5-dione derivatives are good corrosion inhibitors for carbon steel in 1 M HCl medium, their inhibition efficiency increased with inhibitor concentration, and MPPD is slightly more effective than PPD. Potentiostatic polarization study showed that PPD and MPPD are mixed-type inhibitors in 1 M HCl. Impedance experimental data revealed a frequency distribution of the capacitance, simulated as constant phase element. The results obtained from electrochemical and weight loss studies were in reasonable agreement. The adsorption of MPPD and PPD on steel surface obeyed Langmuir’s adsorption isotherm. Thermodynamic data and XPS analysis clearly indicated that the adsorption mechanism of 1H-pyrrole-2,5-dione derivatives on carbon steel surface in 1 M HCl solution is mainly controlled by a chemisorption process. Quantum chemical calculations using the Density Functional Theory (DFT) were performed on 1H-pyrrole-2,5-dione derivatives to determine the relationship between molecular structures and their inhibition efficiencies

  19. Influence of ion implanted helium on deuterium trapping in Kh18N10T stainless steel

    International Nuclear Information System (INIS)

    Tolstolutskaya, G.D.; Ruzhitskij, V.V.; Kopanets, I.E.

    2004-01-01

    The results are presented on evolution of distribution profiles and helium and deuterium thermal desorption ion implanted in steel 18Cr10NiTi. Accumulation, trapping, retention and microstructure evolution are studied; effect helium and hydrogen simultaneous implantation on these processes is also studied

  20. Structural sensitivity of cyclic crack resistance of rotor steel in gaseous hydrogen

    International Nuclear Information System (INIS)

    Romaniv, O.N.; Nikiforchin, G.N.; Kozak, L.Yu.

    1984-01-01

    Comparative evaluation of cyclic crack resistance of hardened rotor set steel 35KhN3MFA in different cstructural states during tesis in agea geseous hydrogen, in the air and in vacuum, has been mde made. It is shown, that structural sensitivity of near-threshold crack resistance of the studied rotor steel in gaseous hydrogen is to a high extent determined by the closing and morphology of fatigue crack. The decrease in crack closing (CC) observed during tests in hydrogen in low-strenght and crack branching in high-strength steels results in the fact, that in contrast to well-known notions on a higher sensitivity to hydrogen embrittlement of high-strenght alloys the negative effect of hydrogen on the near-threshold cyclic crack resistance is manifested only in steel in low-strenght state. The considered regularities in crack growth in low-alloyed steel under the effect of gaseous hydrogen are just only for high-frequency loading. In all probability in the case of fatigue crack growth (GCG) at low frequencies of loading not only the medium activity, but also the role o, closing and crack geometty in the kinetics of fatigue fracture, the clarifying of which requires further studieds, will change

  1. Numerical and experimental study of creep of grade 91 steel at high temperature

    International Nuclear Information System (INIS)

    Lim, R.

    2011-01-01

    Grade 91 steel is a suitable candidate for structural components of the secondary and the vapour of the generation IV nuclear reactors. Their in-service lifetime will be extended to 60 years. It is necessary to consider the mechanisms involved-term during long creep to propose more reliable predictions of creep lifetimes. Necking is the main failure mechanism for creep lifetimes up to 160 kh at 500 C and 94 kh at 600 C. Necking modelling including the material creep softening leads to two bound laws including experimental lifetimes of a large number of tempered martensitic steels loaded up to 200 kh at temperature 500-700 C. The observed creep intergranular cavities are shown to affect very weekly creep strain rate. The prediction of the cavity evolution will allow estimating creep lifetimes out of experimental data domain. Their nucleation and growth, supposed to be associated to vacancy diffusion, are modelled using two classical models. The first one considers instantaneous nucleation (Raj and Ashby) and the second one continuous nucleation obeying the Dyson law (Riedel). The second one leads to two bound laws, more stable with respect to the parameter values. It allows predicting final sizes of cavities in reasonable agreement with the measured ones. Nevertheless, nucleation rate should be estimated from measured cavity densities. Nucleation of cavities by diffusion is simulated using the Raj model. This model does not allow predicted final cavity densities in agreement with the measured ones, even by considering cavity nucleation at precipitates/Laves interfaces experimentally observed and the maximum local stress concentration of a factor 2 computed using finite element calculation in a 2D plane strain hypothesis based on either simulated or real microstructures containing triple points or precipitates/Laves phases. The use of the Dyson law allows us to propose predictions of long-term creep lifetimes. Lifetime predicted using the diffusion-induced growth

  2. Choice of corrosion-resistant metal for fluotitanic acid

    International Nuclear Information System (INIS)

    Reingeverts, M.D.; Lapchenko, E.P.; Semenyuk, E.Y.

    1986-01-01

    The authors investigate the corrosion and anodic behavior of steels 12Kh18N10T, 08Kh21N6M2T, and 06KhN28MDT, nickel, and molybdenum in 10-40% naturally aerated solutions of H 2 TiF 6 at 20 and 50 degrees C. The authors found that in solutions of fluotitanic acid, as also in tetrafluoroboric and hydrofluoric acids, the most stable alloys are chromium-nickel-molybdenum alloy of type 06KhN28MDT and (for acid concentrations above 20%) copper-nickel-alloys of the monel metal type. Steels 12Kh18N10T and 08Kh21N6M2T can be used in acid concentrations of less than 10% and temperatures up to 20 degrees C with anodic protection

  3. The effect of alloying and treatment on martensite transformation during deformation in Fe-Cr-Mn steels with unstable austenite

    International Nuclear Information System (INIS)

    Malinov, L.S.; Konop, V.I.; Sokolov, K.N.

    1977-01-01

    The effect is studied of alloying with chromium (6-10%), silicon (1-2%), molybdenum (1-3%), and copper (2%), the heat treatment conditions, and the deformation conditions, or the martensitic transformation and mechanical properties of Fe-Cr-Mn steels of the transitional class based on 0G8AM2S. It is shown that appropriate alloying and treatment, taking into account the degree of stability of the austenite, can ensure a complex of high mechanical properties of the steels investigated. For instance, the treatment of steel 0Kh10AG8MD2S by the technique: hardening+ 40% deformation at 400 deg C + 10% deformation at room temperature has yielded the following mechanical properties: sigmasub(B)=150 kgf/mm 2 , sigmasub(T)=110 kgf/mm 2 , sigma=18%, psi=32%

  4. About Moral Ideals of Turkic Philosopher M.Kh. Dulaty

    Directory of Open Access Journals (Sweden)

    Botagoz S.Asankulova

    2015-04-01

    Full Text Available The ideas of moral upbringing during the period of Kazakh kingdom on the example of M.Kh.Dulaty ҆s work «Tarikh-i-Rashidi» are given in the article. The main idea is historical-pedagogical aspect of investigation of moral upbringing problems. Genesis of progressive ideas in this direction is the basis of historical experience, which allows to define the dynamics of upbringing process contributing to the moral perfection of personality.

  5. Thermodynamics of complex structures formed between single-stranded DNA oligomers and the KH domains of the far upstream element binding protein

    Energy Technology Data Exchange (ETDEWEB)

    Chakraborty, Kaushik; Sinha, Sudipta Kumar; Bandyopadhyay, Sanjoy, E-mail: sanjoy@chem.iitkgp.ernet.in [Molecular Modeling Laboratory, Department of Chemistry, Indian Institute of Technology, Kharagpur 721302 (India)

    2016-05-28

    The noncovalent interaction between protein and DNA is responsible for regulating the genetic activities in living organisms. The most critical issue in this problem is to understand the underlying driving force for the formation and stability of the complex. To address this issue, we have performed atomistic molecular dynamics simulations of two DNA binding K homology (KH) domains (KH3 and KH4) of the far upstream element binding protein (FBP) complexed with two single-stranded DNA (ss-DNA) oligomers in aqueous media. Attempts have been made to calculate the individual components of the net entropy change for the complexation process by adopting suitable statistical mechanical approaches. Our calculations reveal that translational, rotational, and configurational entropy changes of the protein and the DNA components have unfavourable contributions for this protein-DNA association process and such entropy lost is compensated by the entropy gained due to the release of hydration layer water molecules. The free energy change corresponding to the association process has also been calculated using the Free Energy Perturbation (FEP) method. The free energy gain associated with the KH4–DNA complex formation has been found to be noticeably higher than that involving the formation of the KH3–DNA complex.

  6. Innovative Education and Science in Information Technologies: Experience of M.Ye. Zhukovsky National Aerospace University «KhAI»

    Directory of Open Access Journals (Sweden)

    Kryvtsov, V.S.

    2015-05-01

    Full Text Available Information technologies are among the most promising and fastest growing sectors in the world and Ukrainian industry. In the paper the authors share the experience of National Aerospace University «KhAI» in personnel education and training for the IT industry and the results of successful cooperation with IT companies. Innovative education programs, scientific and practical researches in information technologies, which are implementing in KhAI are also discussed.

  7. Lattice defect inheritance during γ-α-γ transformation in steel having no ''reverse'' (martensite) transition during austenization

    International Nuclear Information System (INIS)

    Bernshtejn, M.L.; Zajmovskij, V.A.; Kozlova, A.G.; Kolupaeva, T.L.

    1979-01-01

    An investigation was carried out, using an electron microscope technique, of the substructure of austenite in the 120Kh3G steel. It was shown that the austenite substructure, resulting from high-temperature mechanical working, is inherited on deep cooling by the low-temperature phase (martensite), and in subsequent heating is again inherited by austenite. If the disintegration of the hot-deformed austenite takes place in the pearlite phase, reheating gives rise to an austenite free from the substructure

  8. Austenite strengthening and softening during hot deformation

    International Nuclear Information System (INIS)

    Tushinskij, L.I.; Vlasov, V.S.; Kazimirova, I.E.; Tokarev, A.O.

    1981-01-01

    Processes of formation of austenite structure of 20 and 12Kh18N10T steels during hot deformation and postdeformation isothermal holdings have been investigated by the methods of analysis of curves of hot deformation, high-temperature metallography and light microscopy. Deformation has been exercised by extention in vacuum with average 4x10 -2 s -1 rate. Deformation temperatures of steel 20 are 930 and 1000 deg C, of steel 12Kh18N10T - 1100 deg C. It is stated that dynamic recrystallization takes place in both investigated steels during hot deformation. In the carbonic steel it is developed by shifting sections of high-angular boundaries, flow stress in this case remains constant. Recrystallization is developed by subgrain coalescence in austenite steel, that brings about preservation of increased defect density in recrystallized volumes. As a result strengthening of steel is continued up to fracture during the increase of the deformation degree. Postdeformation weakening of 12Kh18N10T steel is slowed down as compared with weakening of carbonic steel [ru

  9. Surface profile evolution and fatigue crack initiation in Sanicro 25 steel at room temperature

    Czech Academy of Sciences Publication Activity Database

    Polák, Jaroslav; Petráš, Roman; Chai, G.; Škorík, Viktor

    2016-01-01

    Roč. 658, MAR (2016), s. 221-228 ISSN 0921-5093 R&D Projects: GA MŠk(CZ) ED1.1.00/02.0068; GA MŠk(CZ) EE2.3.30.0063; GA ČR(CZ) GA13-23652S Institutional support: RVO:68081723 Keywords : Sanicro 25 steel * Fatigue crack initiation * Persistent slip markings * Extrusions * Intrusions Subject RIV: JL - Materials Fatigue, Friction Mechanics Impact factor: 3.094, year: 2016

  10. Estimation of work capacity of welded mounting joints of pipelines of heat resisting steel

    International Nuclear Information System (INIS)

    Gorynin, I.V.; Ignatov, V.A.; Timofeev, B.T.; Blyumin, A.A.

    1982-01-01

    The analysis of a work capacity of circular welds made for the Dsub(y)850 pipeline connection with high pressure vessels of heat resisting steel of the 15Kh1NMFA type has been carried out on the base of test results with small samples and real units. Welds were performed using the manual electric arc welding without the following heat treatment. It has been shown that residual stresses in such welds do not produce an essential effect on the resistance of weld metal and heat affected zone on the formation and developments of cracks

  11. Development of ferritic steels for fusion reactor applications

    Energy Technology Data Exchange (ETDEWEB)

    Klueh, R.L.; Maziasz, P.J.; Corwin, W.R.

    1988-08-01

    Chromium-molybdenum ferritic (martensitic) steels are leading candidates for the structural components for future fusion reactors. However, irradiation of such steels in a fusion environment will produce long-lived radioactive isotopes that will lead to difficult waste-disposal problems. Such problems could be reduced by replacing the elements in the steels (i.e., Mo, Nb, Ni, N, and Cu) that lead to long-lived radioactive isotopes. We have proposed the development of ferritic steels analogous to conventional Cr-Mo steels, which contain molybdenum and niobium. It is proposed that molybdenum be replaced by tungsten and niobium be replaced by tantalum. Eight experimental steels were produced. Chromium concentrations of 2.25, 5, 9, and 12% were used (all concentrations are in wt %). Steels with these chromium compositions, each containing 2% W and 0.25% V, were produced. To determine the effect of tungsten and vanadium, 2.25 Cr steels were produced with 2% W and no vanadium and with 0.25% V and O and 1% W. A 9Cr steel containing 2% W, 0.25 V, and 0.07% Ta was also studied. For all alloys, carbon was maintained at 0.1%. Tempering studies on the normalized steels indicated that the tempering behavior of the new Cr-W steels was similar to that of the analogous Cr-Mo steels. Microscopy studies indicated that 2% tungsten was required in the 2.25 Cr steels to produce 100% bainite in 15.9-mm-thick plate during normalization. The 5Cr and 9Cr steels were 100% martensite, but the 12 Cr steel contained about 75% martensite with the balance delta-ferrite. 33 refs., 35 figs., 5 tabs.

  12. Development of ferritic steels for fusion reactor applications

    International Nuclear Information System (INIS)

    Klueh, R.L.; Maziasz, P.J.; Corwin, W.R.

    1988-08-01

    Chromium-molybdenum ferritic (martensitic) steels are leading candidates for the structural components for future fusion reactors. However, irradiation of such steels in a fusion environment will produce long-lived radioactive isotopes that will lead to difficult waste-disposal problems. Such problems could be reduced by replacing the elements in the steels (i.e., Mo, Nb, Ni, N, and Cu) that lead to long-lived radioactive isotopes. We have proposed the development of ferritic steels analogous to conventional Cr-Mo steels, which contain molybdenum and niobium. It is proposed that molybdenum be replaced by tungsten and niobium be replaced by tantalum. Eight experimental steels were produced. Chromium concentrations of 2.25, 5, 9, and 12% were used (all concentrations are in wt %). Steels with these chromium compositions, each containing 2% W and 0.25% V, were produced. To determine the effect of tungsten and vanadium, 2.25 Cr steels were produced with 2% W and no vanadium and with 0.25% V and O and 1% W. A 9Cr steel containing 2% W, 0.25 V, and 0.07% Ta was also studied. For all alloys, carbon was maintained at 0.1%. Tempering studies on the normalized steels indicated that the tempering behavior of the new Cr-W steels was similar to that of the analogous Cr-Mo steels. Microscopy studies indicated that 2% tungsten was required in the 2.25 Cr steels to produce 100% bainite in 15.9-mm-thick plate during normalization. The 5Cr and 9Cr steels were 100% martensite, but the 12 Cr steel contained about 75% martensite with the balance delta-ferrite. 33 refs., 35 figs., 5 tabs

  13. Alloy spreading and filling of gaps in brazing of VDU-2 and KhN50VMTYuB heat resistant nickel alloys with VPr3K and VPr10 alloys

    International Nuclear Information System (INIS)

    Shapiro, A.E.; Podol'skij, B.A.; Lepisko, M.R.; Borzyak, A.G.; Moryakov, V.F.; Rostislavskaya, T.T.

    1984-01-01

    A study was made on contact interaction of VDU-2 and KhN50VMTYuB alloys with VPr3K and VPr10 alloys at 1325 and 1220 deg C in argon and industrial vacuum. The contact angles and wettability indexes were determined. The solders fill the vertical gaps of up to 0.25 mm width through 80 mm height. Spreading and filling of gaps proceeds better during soldering in argon with boron trifluoride addition as compared to soldering in industrial vacuum. VPr10 alloy is divided into two phases when wetting KhN50VMTYuB alloy: fusible one on the base of nickel-chromium-manganese solution and infusible one on the base of nickel-niobium eutectics. The square of fusible phase spreading is 2.5...3 times larger as compared to infusible one

  14. Paramagnetic defects in KH{sub 2}PO{sub 4} crystals with high concentration of embedded TiO{sub 2} nanoparticles

    Energy Technology Data Exchange (ETDEWEB)

    Grachev, Valentin G., E-mail: grachev@physics.montana.edu; Tse, Romand; Malovichko, Galina I. [Physics Department, Montana State University, Bozeman, Montana 59717 (United States); Pritula, Igor M.; Bezkrovnaya, Olga N.; Kosinova, Anna V. [Institute for Single Crystals, NAS of Ukraine, Kharkiv (Ukraine)

    2016-01-21

    Qualitative transformations of spectra of Electron Paramagnetic Resonance, EPR, were found in KH{sub 2}PO{sub 4} crystals grown from liquor with 10{sup −5}–10{sup −1 }wt. % of anatase TiO{sub 2} nanoparticles in comparison with nominally pure KH{sub 2}PO{sub 4}. The nanoparticles have larger segregation coefficient for prismatic parts of the crystals than for pyramidal ones. Significant decrease in resonance absorption, complete disappearance of EPR lines of Fe{sup 3+} and Cr{sup 3+} centers, and appearance of four weak lines of equal intensities together with broad asymmetric lines with g-factors about 2.07–2.5 was observed in pyramidal parts grown with concentration of TiO{sub 2} nanoparticles larger than the threshold value 10{sup −2 }wt. %. The four lines were attributed to non-controlled impurity As substituted for P. In the presence of TiO{sub 2} nanoparticles, non-paramagnetic AsO{sub 4}{sup 3−} clusters trap electrons becoming AsO{sub 4}{sup 4−}. Disappearance of Fe{sup 3+} and Cr{sup 3+} centers was explained by their recharge to “EPR-silent” states and/or pairing at the surface of TiO{sub 2} nanoparticles.

  15. Kankaan tuotekehittäminen erikoisolosuhteisiin K&H Annala Oy:lle

    OpenAIRE

    Koski, Marjo

    2017-01-01

    Opinnäytetyö tehtiin yhteistyössä Suomen ainoan huonekalukankaita valmistavan yrityksen K&H Annala Oy:n kanssa. Työn aiheena oli suunnitella ja tuotteistaa kangasmallisto erikoisolosuhteisiin innovatiivisesta, Italiassa valmistettavasta Flyer-langasta. Projektin lähtökohtana oli opinnäytetyöntekijän kasvava kiinnostuneisuus kudottuja tekstiilejä kohtaan ja kankaan suunnitteluprosessin vieminen teollisen tuotannon puolelle. Projektissa tähdättiin uudentyyppiseen kankaaseen ilmeen ja materiaali...

  16. Fabrication of welded pipes of the KhN45Yu alloy

    International Nuclear Information System (INIS)

    Lyapunov, A.I.; Krichevskij, E.M.; L'vov, V.N.; Kozlov, N.N.; Kireeva, T.S.

    1977-01-01

    A highly heat-resistant KhN45Yu (EP 747) alloy has been developed; the alloy is designed to withstand prolonged service in the temperature range of 1000-1300 deg C, or short-term service at 1300-1400 deg C. The satisfactory ductility and good weldability of the alloy have made it possible to obtain sheets and pipes (32 x 2.0 mm) by argon arc welding. The ductility of pipes from EP 747 alloy exceeds that of pipes from KhN78T (EI 435) alloy by 5.10%, the strength being approximately equal. In regard to strength the welded joint differs little from the base metal. The ductility characteristics up to 900 deg C are also equal, since failure occurs in the base metal. At higher temperatures the welded joint fails in the metal of the weld, and its ductility drops sharply. The grain size of the base metal corresponds to No. 3-4. The welded joint has a cast structure with a grain size larger than No. 1, but its ductility characteristics are satisfactory. This structure ensures an increased long-term strength of the material at 1000-1200 deg C

  17. Metodologi Fatwa K.H. Muhammad Syaf’i Hadzami

    Directory of Open Access Journals (Sweden)

    Muhammad Ardiansyah

    2018-01-01

    Full Text Available Fatwa is one of the heavy mandates on the shoulders of Moslem scholars. There are some conditions that must be fulflled before the fatwa could be used to solve the problems of the people. Basically, the fatwa replaces the task of the Prophet in conveying the shari’a law, then the scholars did not dare to be reckless in declaring any fatwa. Therefore, being a mufti is not only required by reading the translation of al-Qur’an or Hadith, or by searching on the google, or by copying broadcasts in social media. According to al-Shirazi, the intellectual condition that must be required to be a mufti is deep understanding toward al-Qur’an and Hadith, also understanding sources of speech such as ḥaqîqah-majâz, ‘âmm-khâṣṣ, Arabic language, nâsikh-mansûkh, ijmâ’, ikhtilaf, and tartîb al-adillah. While the moral requirements to be a mufti according to Imam Ahmad bin Hanbal are having pure intention, having broad knowledge, patience, and soul, having strong mentality to fulfl the task, having suffciency of life to avoid being influenced by others, and understanding the condition of society. This paper attempts to examine the fatwas of a mufti from Betawi who had lived in the modern era known as Mu’allim Syaf’i Hadzami. The fatwas were collected in a work entitled Tawḍîḥ al-Adillah. In this article, the author has concluded that Mu’allim uses eight complementary and relevant fatwa methodologies to solve today’s problems

  18. Effect of tensile deformation on micromagnetic parameters in 0.2% carbon steel and 2.25Cr-1Mo steel

    Energy Technology Data Exchange (ETDEWEB)

    Moorthy, V.; Vaidyanathan, S.; Jayakumar, T.; Raj, B. [Indira Gandhi Centre for Atomic Research, Kalpakkam (India). Metallurgy and Materials Group; Kashyap, B.P. [Indian Inst. of Tech., Bombay (India). Dept. of Metallurgical Engineering and Materials Science

    1999-04-23

    The influence of prior tensile deformation on the magnetic Barkhausen emission (MBE) and the hysteresis (B-H) curve has been studied in 0.2% carbon steel and 2.25Cr-1Mo steel under different tempered conditions. This study shows that the micromagnetic parameters can be used to identify the four stages of deformation, namely (1) perfectly elastic, (2) microplastic yielding, (3) macroyielding and (4) progressive plastic deformation. However, it is observed that the MBE profile shows more distinct changes at different stages of tensile deformation than the hysteresis curve. It has been established that the beginning of microplastic yielding and macroyielding can be identified from the MBE profile which is not possible from the stress-strain plot. The onset of microplastic yielding can be identified from the decrease in the MBE peak height. The macroyielding can be identified from the merging of the initially present two-peak MBE profile into a single central peak with relatively higher peak height and narrow profile width. The difference between the variation of MBE and hysteresis curve parameters with strain beyond macroyielding indicates the difference in the deformation state of the surface and bulk of the sample.

  19. Effect of preliminary neutron irradiation on helium blistering of 0Kh16N15M3B steel

    International Nuclear Information System (INIS)

    Chernov, I.I.; Kalin, B.A.; Skorov, D.M.; Shishkin, G.N.; Ivanov, M.V.

    1982-01-01

    The method of electron microscopy has been applied to investigate the effect of preliminary neutron irradiation on the OKh16N15M3B steel blistering under irradiation by 20 keV helium ions with (1-10)x10 21 ion/m 2 doses at the temperature below 373 K. It is shown that neutron irradiation shifts critical doses of blister formation and intense scaling towards higher doses. But after the incubation period the erosion of steel preliminary neutron irradiated grows with the increase of helium ion dose above 7x10 21 ion/m 2 . Short-term heating of neutron irradiated samples during 15 min at 1173 K does not practically affect the beginning of intense scaling of the surface

  20. MTS-MD of Biomolecules Steered with 3D-RISM-KH Mean Solvation Forces Accelerated with Generalized Solvation Force Extrapolation.

    Science.gov (United States)

    Omelyan, Igor; Kovalenko, Andriy

    2015-04-14

    We developed a generalized solvation force extrapolation (GSFE) approach to speed up multiple time step molecular dynamics (MTS-MD) of biomolecules steered with mean solvation forces obtained from the 3D-RISM-KH molecular theory of solvation (three-dimensional reference interaction site model with the Kovalenko-Hirata closure). GSFE is based on a set of techniques including the non-Eckart-like transformation of coordinate space separately for each solute atom, extension of the force-coordinate pair basis set followed by selection of the best subset, balancing the normal equations by modified least-squares minimization of deviations, and incremental increase of outer time step in motion integration. Mean solvation forces acting on the biomolecule atoms in conformations at successive inner time steps are extrapolated using a relatively small number of best (closest) solute atomic coordinates and corresponding mean solvation forces obtained at previous outer time steps by converging the 3D-RISM-KH integral equations. The MTS-MD evolution steered with GSFE of 3D-RISM-KH mean solvation forces is efficiently stabilized with our optimized isokinetic Nosé-Hoover chain (OIN) thermostat. We validated the hybrid MTS-MD/OIN/GSFE/3D-RISM-KH integrator on solvated organic and biomolecules of different stiffness and complexity: asphaltene dimer in toluene solvent, hydrated alanine dipeptide, miniprotein 1L2Y, and protein G. The GSFE accuracy and the OIN efficiency allowed us to enlarge outer time steps up to huge values of 1-4 ps while accurately reproducing conformational properties. Quasidynamics steered with 3D-RISM-KH mean solvation forces achieves time scale compression of conformational changes coupled with solvent exchange, resulting in further significant acceleration of protein conformational sampling with respect to real time dynamics. Overall, this provided a 50- to 1000-fold effective speedup of conformational sampling for these systems, compared to conventional MD

  1. Heat treatment effect on the properties of the EhP767 maraging steel welded joints

    International Nuclear Information System (INIS)

    Taver, E.I.; Piskarev, M.N.; Yushchenko, K.A.; Pustovit, A.I.; Anisimova, M.S.

    1977-01-01

    Heat treatment effect on properties of welded joints of maraging 03Kh13N4K13M3T (EhP767) steel with yield strength over 150 kgs/mm 2 has been investigated. It is shown, that change in impact strength of aged joints at - 196 deg C depends on the amount of residual austenite and grain size. To stabilize 20-40 % residual austenite heat treatment regimes have been developed. Recommended are quenching at 1030-1050 deg C, sub-zero treatment and aging at 520 deg C for 16 hrs

  2. Fabrication and characterization of microstructure of stainless steel matrix composites containing up to 25 vol% NbC

    Energy Technology Data Exchange (ETDEWEB)

    Kan, Wen Hao, E-mail: wkan6795@uni.sydney.edu.au [School of Civil Engineering, The University of Sydney, NSW 2006 (Australia); Ye, Zi Jie; Zhu, Yue [School of Civil Engineering, The University of Sydney, NSW 2006 (Australia); Bhatia, Vijay Kumar [School of Aerospace, Mechanical and Mechatronic Engineering, The University of Sydney, NSW 2006 (Australia); Australian Centre for Microscopy and Microanalysis, The University of Sydney, NSW 2006 (Australia); Dolman, Kevin; Lucey, Timothy; Tang, Xinhu [Weir Minerals Australia, Artarmon, NSW 2064 (Australia); Proust, Gwénaëlle [School of Civil Engineering, The University of Sydney, NSW 2006 (Australia); Cairney, Julie [School of Aerospace, Mechanical and Mechatronic Engineering, The University of Sydney, NSW 2006 (Australia); Australian Centre for Microscopy and Microanalysis, The University of Sydney, NSW 2006 (Australia)

    2016-09-15

    AISI 440 stainless steels reinforced with various volume fractions of niobium carbide (NbC) particles of up to 25 vol% were fabricated in-situ using an argon arc furnace and then heat-treated to produce a martensitic matrix. Optical and scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS) and electron back-scatter diffraction (EBSD) techniques were used to analyze the microstructure, phases and composition of these composites. Interestingly, it was found that Chinese-script NbC could nucleate on existing primary NbC particles creating NbC clusters with complex microstructures. Additionally, hardness tests were used to evaluate viability in mining and mineral processing applications. The increase in NbC content resulted in an overall increase in the hardness of the composites while causing a marginal decrease in the amount of Cr in solid solution with the matrix, which could be a concern for corrosion resistance. The latter was due to the fact that the NbC lattice could dissolve a minor amount of Cr. Thermodynamic simulations also attributed this to a slight increase in M{sub 7}C{sub 3} precipitation. Nonetheless, these novel composites show great promise for applications in wear and corrosive environments. - Highlights: •Stainless steels reinforced with NbC particles of up to 25 vol% were fabricated. •NbC was formed in-situ in the steels using an arc melter. •Martensitic transformation of the matrix of each sample was achieved. •NbC reinforcements increased the bulk hardness values of the steels. •Dissolved Cr in the matrix of each sample was sufficient for passivity in theory.

  3. Kinetics and mechanism of oxidation of carbidized electrolytic chromium coatings

    International Nuclear Information System (INIS)

    Arkharov, V.I.; Yar-Mukhamedov, Sh.Kh.

    1978-01-01

    Thermal stability carbidized electrolytic chromium coatings has been studied depending on the conditions of their formation; the specific features of the mechanism of oxidation at 1200 deg in an air atmosphere have been elucidated. It has been established that kinetics of high temperature oxidation of the coatings depends essentially on the conditions of their formation and on the composition of steel to which the coating is applied. It has been shown that two oxidation mechanisms are possible: by diffusion of the residual chromium through a carbide layer along the carbide grain boundaries outwards or, when there is no residual chromium, by chemical reaction of carbon combustion and oxidation of the liberated chromium. The comparison of oxidation kinetic curves of the samples of 38KhMYuA, 35KhGSA, and DI-22 steels with and without coating has shown that the coatings under study have a better protective effect on 38KhMYuA steel than on 35KhGSA, although without coating oxidability of the first steel is higher than that of the second

  4. Cold-rolled sheets production of stainless martensite-ageing steel smelted by vacuum arc and electroslag techniques

    Energy Technology Data Exchange (ETDEWEB)

    Rivkin, A A; Grishkov, A I; Suslin, A P; Nesterenko, A A; Lola, V N [Tsentral' nyj Nauchno-Issledovatel' skij Inst. Chernoj Metallurgii, Moscow (USSR)

    1975-05-01

    In cooperation with a number of metallurgical works the production of a high strength sheet stainless maraging steel EHP678 (000KH11N10M2T) has been tested by rolling cylindrical ingots of vacuum arc smelting at the blooming (the mass of rough ingots was 5.1 to 6.0 t, that of cleaned ingots - 3.8 to 5.1 t) or rectangular ingots of electroslag smelting (13 t) at the slabbing. The recommended regimes of heating and deformation are much similar to those used for the steel-KH18N10T. The output of valid cold-rolled sheets proved to be rather low (0.24 t/t for the vacuum arc smelting and 0.30 t/t for the electroslag smelting) mainly due to the losses on cleaning and a considerable portion of wrong-size slabs. The data are presented on the steel-EHP678 properties after various heat treatments. For the production of wide cold-rolled sheets of the steel EHP678 it is recommended to use steelmaking procedure with electroslag smelting including open-hearth melting in arc furnaces, rolling of ingots at the slabbing with heating up to 1260-1280 deg C (hold-up of 4.5 to 5 hrs); electroslag smelting for rectangular section slabs, rolling of ingots of electroslag smelting at the slabbing with their heating up to 1250 deg C (hold-up of 5.5 to 6 hrs), rolling at the 1680-type mill with heating up to 1250-1260 deg C (hold-up of 4 to 4.5 hrs ensuring the rolling temperature after a rough group not below 1100 deg C), quenching of hot-rolled sheets heating up to 920-940 deg C (hold-up of 3 to 3.5 min/mm), shot peening of sheets for descaling (provided the respective equipment is available) with a subsequent short-time pickling in an acid solution and cold rolling with a summary deformation of 35 to 45 %. The steelmaking with the electroslag smelting is much more profitable as regards to the fine technology of number of the main procedures, convenient cooperation of the works and a considerably greater output of the final products out of one ton of the steel produced.

  5. Octanol-Water Partition Coefficient from 3D-RISM-KH Molecular Theory of Solvation with Partial Molar Volume Correction.

    Science.gov (United States)

    Huang, WenJuan; Blinov, Nikolay; Kovalenko, Andriy

    2015-04-30

    The octanol-water partition coefficient is an important physical-chemical characteristic widely used to describe hydrophobic/hydrophilic properties of chemical compounds. The partition coefficient is related to the transfer free energy of a compound from water to octanol. Here, we introduce a new protocol for prediction of the partition coefficient based on the statistical-mechanical, 3D-RISM-KH molecular theory of solvation. It was shown recently that with the compound-solvent correlation functions obtained from the 3D-RISM-KH molecular theory of solvation, the free energy functional supplemented with the correction linearly related to the partial molar volume obtained from the Kirkwood-Buff/3D-RISM theory, also called the "universal correction" (UC), provides accurate prediction of the hydration free energy of small compounds, compared to explicit solvent molecular dynamics [ Palmer , D. S. ; J. Phys.: Condens. Matter 2010 , 22 , 492101 ]. Here we report that with the UC reparametrized accordingly this theory also provides an excellent agreement with the experimental data for the solvation free energy in nonpolar solvent (1-octanol) and so accurately predicts the octanol-water partition coefficient. The performance of the Kovalenko-Hirata (KH) and Gaussian fluctuation (GF) functionals of the solvation free energy, with and without UC, is tested on a large library of small compounds with diverse functional groups. The best agreement with the experimental data for octanol-water partition coefficients is obtained with the KH-UC solvation free energy functional.

  6. Inhibitor effect on corrosion of titanium alloys in muriatic solutions of titanium-magnesium production

    International Nuclear Information System (INIS)

    Dobrunov, Yu.V.; Volynskij, V.V.; Kolobov, G.A.; Kuznetsov, S.I.

    1977-01-01

    Corrosion tests of titanium alloys VTI-0, OT4, VT5-1 and steel Kh18N1OT in 10% and 18% HCl with additions of carnallite at 40 deg C have been carried out. It has been established that titanium alloys in 10% and 18% HCl containing 5 and 10% carnallite are sufficiently corrosion resistant in the presence of 0.1-1% FeCl or HNO 3 and can be used for manufacturing the equipment of recirculation gas scrubbers. Steel Kh18N10T is unstable in all the media tested. It is subjected to intensive pitting. Specimens of steel Kh18N10T have also revealed edge cracking

  7. Effect of heating and deformation conditions on the depth of surface defects in alloyed steel rolling

    International Nuclear Information System (INIS)

    Malygin, R.Z.; Karyakin, B.P.; Grosman, A.B.; Simovskikh, V.N.; Storozhev, V.I.

    1978-01-01

    The effect of heating and deformation conditions on the depth change of artificial defects in the 50 KhFA alloyed steel rolling on the 850 blooming and 450 section mill was studied. Quite a definite regularity in the arrangement of defects (cracks and hairlines) along the circumference of the round steel bar and obvious relation with the defect distribution on the bloom faces are established. Oxidation is shown to diminish defect depth while ingot and billet heating especially on the faces under direct firing. Blooms should be placed in the furnace with 90 deg canting in relation to the faces position while ingot heating. Round rolling must be performed with one or several 45 deg strip cantings. The defect depth for the ingots to be rolled without chipping is set up

  8. On effect of some thermodeformation parameters of welding cycle on tendency of pearlitic heat-resisting steels to fracture in reheating

    International Nuclear Information System (INIS)

    Prokhorov, N.N.; Bardokin, E.V.

    1979-01-01

    Studied is the inclination of the 12Kh1MF, 15Kh3M1F and N18K9M5T steels subject to thermodeformation cycle imitating a welding one, to fracture in reheating. A hot-rolled metal then subject to the same thermal treatment was used. The imitation of thermodeformation cycle of the welding permitted to vary maximum heating temperatures, the period during which the metal is kept at temperatures higher than 1100 deg C, and the cooling rate of ajacent zone metal. It is shown that the curve of the dependence of deformation ability and the tendency to fracture at the reheating of adjacent zone metal on the rate of its cooling at welding is U-shaped. Deformation ability has its maximum value at the cooling rate of 30 deg c/s in the range 1300 to 1000 deg C

  9. Relaxation response of A533B steel from 25 to 600/degree/C

    International Nuclear Information System (INIS)

    Swindeman, R.W.; Bolling, E.

    1989-01-01

    Relaxation tests were performed on A533B steel over the range 25 to 600/degree/C in order to examine the general features of time- dependent deformation. It was found that the relaxation strength increased with the flow stress at low temperatures and was relatively independent of history at high temperatures. In the temperature range 400 to 600/degree/C the inelastic strain rates calculated from the relaxation rates followed stress dependencies that were consistent with expectations based on a model proposed by Hart and coworkers for matrix deformation. 21 refs., 10 figs

  10. Development of low-chromium, chromium-tungsten steels for fusion

    International Nuclear Information System (INIS)

    Klueh, R.L.; Alexander, D.J.; Kenik, E.A.

    1995-01-01

    High-chromium (9-12% Cr) Cr-Mo and Cr-W ferritic steels are favored as candidates for fusion applications. In early work to develop reduced-activation steels, an Fe-2.25Cr-2W-0.25V-0.1C steel (designated 2.25Cr-2WV) had better strength than an Fe-9Cr-2W-0.25V-0.07Ta-0.1C (9Cr-2WVTa) steel (compositions are in weight percent). However, the 2.25Cr-2WV had poor impact properties, as determined by the ductile-brittle transition temperature and upper-shelf energy of subsize Charpy impact specimens. Because low-chromium steels have some advantages over high-chromium steels, a program to develop low-chromium steels is in progress. Microstructural analysis indicated that the reason for the inferior impact toughness of the 2.25Cr-2WV was the granular bainite obtained when the steel was normalized. Properties can be improved by developing an acicular bainite microstructure by increasing the cooling rate after austenitization. Alternatively, acicular bainite can be promoted by increasing the hardenability. Hardenability was changed by adding small amounts of boron and additional chromium to the 2.25Cr-2WV composition. A combination of B, Cr, and Ta additions resulted in low-chromium reduced-activation steels with mechanical properties comparable to those of 9Cr-2WVTa. (orig.)

  11. On the hypothesis of agressive environment effect evaluation on the cyclic cracking resistance in metals and alloys

    International Nuclear Information System (INIS)

    Romaniv, O.N.; Gladkij, Ya.N.; Nikiforchin, G.N.

    1978-01-01

    Experimental data on studying static and cyclic cracking resistances of steels in water and inert gaseous media are given. Presented are experimental values of threshold coefficients of stress intensities for a series of the systems: metal (the 4340 steel of the 45KhN2MFA type, 12Ni-5Cr-3Mo steel, 9Ni-4Co-0.25C steel and others)-medium. On the base of the above data analysis and representations on the mechanism of crack growth under conditions of permanent and variable load effects the conclusion is drawn on the groundlessness of the hypothesis of contribution superposition resulted from pure fatigue and corrosion-static factors when estimating cracking resistance of metals and alloys

  12. LOCATING THE TRAILING EDGE OF THE CIRCUMBINARY RING IN THE KH 15D SYSTEM

    International Nuclear Information System (INIS)

    Capelo, Holly L.; Herbst, William; Leggett, S. K.; Hamilton, Catrina M.; Johnson, John A.

    2012-01-01

    Following two years of complete occultation of both stars in the binary T Tauri star KH 15D by its opaque circumbinary ring, KH 15D has abruptly brightened again during apastron phases, reaching I = 15 mag. Here, we show that the brightening is accompanied by a change in spectral class from K6/K7 (the spectral class of star A) to ∼K1, and a bluing of the system in V – I by about 0.3 mag. A radial velocity measurement confirms that, at apastron, we are now seeing direct light from star B, which is more luminous and of earlier spectral class than star A. Evidently, the trailing edge of the occulting screen has just become tangent to one anse of star B's projected orbit. This confirms a prediction of the precession models, supports the view that the tilted ring is self-gravitating, and ushers in a new era of the system's evolution that should be accompanied by the same kind of dramatic phenomena observed from 1995 to 2009. It also promotes KH 15D from a single-lined to a double-lined eclipsing binary, greatly enhancing its value for testing pre-main-sequence models. The results of our study strengthen the case for truncation of the outer ring at around 4 AU by a sub-stellar object such as an extremely young giant planet. The system is currently at an optimal configuration for detecting the putative planet and we urge expedient follow-up observations.

  13. Electrochemical machining of internal built-up surfaces of large-sized vessels for nuclear power plants

    Energy Technology Data Exchange (ETDEWEB)

    Ryabchenko, N N; Pulin, V Ya [Vsesoyuznyj Proektno-Tekhnologicheskij Inst. Atomnogo Mashinostroeniya i Kotlostroeniya, Rostov-na-Donu (USSR)

    1977-01-01

    Electrochemical machining (ECM) has been employed for finishing of mechanically processed inner surfaces of large lateral parts of construction bodies with welded 0Kh18N10T steel overlayer. The finishing technology developed reduces the surface roughness from 10 mcm to the standard 2.5 mcm at the efficiency of machining of 2-4 m/sup 2/ per hour.

  14. The influence of cerium and yttrium ion implantation upon the oxidation behaviour of a 20% Cr/25% Ni/Nb stabilised stainless steel, in carbon dioxide, at 8250C

    International Nuclear Information System (INIS)

    Bennett, M.J.; Dearnaley, G.; Houlton, M.R.; Hawes, R.W.M.

    1982-01-01

    The influence of cerium and yttrium ion implantation upon the oxidation behaviour of a 20% Cr/25% Ni niobium stabilised stainless steel during up to 7 157h exposure to carbon dioxide, at 825 0 C has been examined. The doses ranged between 5 x 10 14 and 10 17 ions cm -2 . Above thresholds of between 5 x 10 14 and 5 x 10 15 yttrium and between 5 x 10 15 and 10 16 cerium ions cm -2 the implantation of both elements improved the oxidation resistance of the 20/25/Nb steel. Yttrium exerted the greater influence, reducing by a factor of two the attack after 7 157h. Up to 80% of the oxide formed on the 20/25/Nb steel spalled, particularly on thermal cycling. Cerium and yttrium implantation improved oxide adhesion by similar extents, which increased with ion dose such that with the highest doses, no spallation was measurable. The effect of the implanted elements derived from their incorporation within the oxide film. It was initiated by their promotion of the formation of an initial chromium-rich oxide layer, which had a finer grain size than that formed on the 20/25/Nb steel. Reduction in continuing attack was associated in part, with improved oxide adhesion, as this decreased the significant contribution to the attack of the 20/25/Nb steel from the reoxidation of spalled areas. (author)

  15. Effect of KH2PO4 on gene expression, morphological and biochemical characteristics of stevia rebaudiana Bertoni under in vitro conditions.

    Science.gov (United States)

    Kahrizi, D; Ghari, S M; Ghaheri, M; Fallah, F; Ghorbani, T; Beheshti Ale Agha, A; Kazemi, E; Ansarypour, Z

    2017-08-15

    Stevia rebaudiana is one of the most important biologically sourced and low-calorie sweeteners Bertoni that has a lot of steviol glycosides. Tissue culture is the best for propagation of stevia and micro nutrients can affect both morphological traits and steviol glycosides production. Therefore, the effect of different concentrations of KH2PO4on stevia growth factors and gene expression had been studied by tissue culture methods, RT-PCR and HPLC. According the results, bud numbers had increased significantly in MS + 0.034 mMKH2PO4 media and the highest measured length was seen in plants grown under MS + 0.034 mM KH2PO4 treatment. Also, the highest growth rate (1.396 mm/d) was observed in MS + 0.034 mMKH2PO4.The best concentration of KH2PO4 for expression of UGT74G1 was 0.00425mMand the best one for UGT76G1 expression was 0.017mM. Interestingly, the best media for both stevioside and rebaudioside A accumulation was 0.017mM KH2PO4containing media. There was positive correlation between the best media for gene expression and the best one for steviol glycosides production.

  16. Observations of copper clustering in a 25Cr-7Ni super duplex stainless steel during low-temperature aging under load

    Science.gov (United States)

    Thuvander, M.; Zhou, J.; Odqvist, J.; Hertzman, S.; Hedström, P.

    2012-07-01

    Atom-probe tomography was used to investigate phase separation and copper (Cu) clustering in the ferrite phase of a 25Cr-7Ni super duplex stainless steel. The steel was subjected to a tensile load during aging at 325°C for 5800 h. The degree of phase separation into α (Fe-rich) and α‧ (Cr-rich) was small, but still, it was the highest in the steel subjected to the highest load. Cu was found to cluster, and the number density of clusters increased with increasing load. In the material subjected to the highest load, Cu was enriched in regions that were neither Fe-rich nor Cr-rich. These regions also had the highest number density of Cu clusters.

  17. Cyclic and isothermal oxidation behavior of 2.25Cr-1Mo steel

    International Nuclear Information System (INIS)

    Proy, M.; Utrilla, M. v.; Otero, E.

    2014-01-01

    Cyclic and isothermal oxidation of chromium-molybdenum steel 2.25Cr-1Mo were analyzed at 550 degree centigrade and 650 degree centigrade during 360 hours in air atmospheres. The cycles were performed with two stages; one of heating in furnace during 90 minutes and then the sample were cooled to 50 degree centigrade by air flow. Thermogravimetric analyses were performed to obtain high temperature corrosion kinetics. Several characterization techniques have been used to identify the corrosion mechanism, as X-Ray Diffraction (XRD), Optical Microscopy (OM) and Scanning Electron Microscopy (SEM). Thermal cycling tests can changes the corrosion mechanism, due cracks propagation in oxide scale, that witch can favors the access of oxidant agent to the substrate. (Author)

  18. Bulgarian ethnos according to A.Kh. Khalikov’ works: scientific concept and its theoretical bases

    Directory of Open Access Journals (Sweden)

    Izmaylov Iskander L.

    2017-02-01

    Full Text Available The article is devoted to the problems of Bulgar and Tatar ethnogenesis studied in the works of the prominent Kazan archaeologist A.Kh. Khalikov. His concept was based on the fact that a number of ethnic groups (Turkic, Finno-Ugric, and East Slavic participated in the formation of these peoples and that the key role in these processes was played by their mutual cultural influence. The concept of ethnogenesis and ethnic history of the Tatar people offered by A.Kh. Khalikov was a serious theoretical breakthrough against the background of both ideology-biased historical schemes of the Soviet era and the various nationalist ideas, differing from them by a comprehensive, integral scientific analysis of predominantly archaeological data. At present, however, when theoretical and factual bases of historical and ethnological research have considerably expanded, a number of conflicting issues have arisen in the framework of this concept, which, therefore, require new approaches to their solution.

  19. Hot ductility of structural steels melted with the use of direct reduction charge

    International Nuclear Information System (INIS)

    Marchenko, V.N.; Bulat, S.I.; Litvinenko, D.A.

    1982-01-01

    A possibility of the use of direct reduction charge during the open arc melting of the 40Kh2N2MA steel with the subsequent electroslag remelting was investigated. It is shown that the use of such charge free from non-ferrous metal admixtures permits to increase an alloy hot ductility in the hot-brittleness range from 900 up to 1500 deg C. An increase of the deformation rate from 0.1 up to 1 s - 1 increases 1.5-3 times a level of minimum ductility within this temperature range. It is established that antimony and bismuth impurities considerably decrease hot ductility

  20. Organizational and technological compatibility of the technological processes of second and third line maintenance of KhTZ-3522 tractors

    Directory of Open Access Journals (Sweden)

    Kyzminskyj Roman

    2018-01-01

    Full Text Available The work is devoted to systematic substantiation of productivity, production structure and specialization of service stations of KhTZ-3522 tractors. Based on the technical and economic comparative analysis of the results of the technological processes modeling of the second and third line maintenance of KhTZ-3522 tractors, the parametrical series of production structures of service stations both mono- and polytechnological specialization, which can work effectively in a wide range of the general annual program of orders, and in the conditions of seasonal fluctuations of orders for the maintenance of these tractors, are found. The results of calculations of the indicators system for organizational and technological compatibility of technological processes of the second and third line maintenance of KhTZ-3522 tractors in the joint technological flow are presented. The dependencies of these indicators on the total annual program of orders for service stations of different productivity are analyzed. According to the results of the analysis, the polytechnological specialization of such service stations is substantiated.

  1. Multiaxial creep of fine grained 0.5Cr-0.5Mo-0.25V and coarse grained 1Cr-0.5Mo steels

    International Nuclear Information System (INIS)

    Browne, R.J.; Flewitt, P.E.J.; Lonsdale, D.

    1991-01-01

    To explore the multiaxial creep response of materials used for electrical power generating plant, two steels, a fine grained 0.5Cr-0.5Mo-0.25V steel in a normalised and tempered condition with high creep ductility and a coarse grained 1Cr-0.5Mo steel in a quenched and tempered condition with low uniaxial creep ductility, have been selected. A range of multiaxial stress testing techniques which span the stress states that would allow identification of any technique dependent variables has been used. The deformation and failure of the normalised and tempered 0.5Cr-0.5Mo-0.25V steel for a range of multiaxial test techniques and, therefore, stress states may be described by an equivalent stress criterion. The results from the multiaxial tests carried out on the fully bainitic 1Cr-0.5Mo steel show that the multiaxial stress rupture criterion (MSRC) varies with stress state; at high triaxiality (notch), it is controlled by the maximum principal stress, whereas at low triaxiality (shear) it is dependent on both maximum principal stress and equivalent stress. Furthermore, a simple description of stress state based on maximum principal and equivalent stress does not define this uniquely, since the MSRC derived from uniaxial and torsion testing does not describe the failure of notch, tube, or double shear tests. (author)

  2. PENDIDIKAN KARAKTER MENURUT K.H. HASYIM ASY’ARI DALAM KITAB ADÂB AL-‘ÂLIM WA AL-MUTA‘ALLIM

    OpenAIRE

    Sholikah Sholikah

    2015-01-01

    The article deals with K.H. Hasyim Asy’ari’s thought of character education. The result of the study indicates that according to K.H. Hasyim Asy’ari the characters of teachers and students in his work Adab al-‘Âlim wa al-Muta’allim can be classified into three parts, are mentality or character, which should be possessed by teachers and learners: attempts to be done in order to become characterized teachers and learners, and: teaching strategies employed by educators and learning strategies us...

  3. Corrosion cracking of 03N18K1M3TYu and 02N12Kh5M3 maraging steels in chloride solutions

    Energy Technology Data Exchange (ETDEWEB)

    Pavlov, V.N.; Chumalo, G.V.; Vereshchagin, A.N.; Melekhov, R.K.

    1987-07-01

    The authors investigate the electrochemical behavior in 0.5% NaCl solution and 42% MgCl/sub 2/ solution and the tendency toward corrosion cracking was determined in boiling 0.5% chloride solution of the cobalt-containing maraging steels in the title. Weld specimens and specimens of the base metal of 03N18K1M3TYu steel were tested in 3% NaCl solution for resistance to corrosion cracking. Additional investigations were made of specimens of that steel with previously created fatigue cracks of the base metal and the weld specimens in 3% NaCl solutions, since that steel is a promising material for structures operating in sea water and low concentration chloride solutions.

  4. Experimental verification of lifetime of bolting joints for WWER reactor pressure vessels

    International Nuclear Information System (INIS)

    Brumovsky, M.; Polachova, H.

    1992-01-01

    This paper presents results from experimental verification of cyclic lifetime of bolting joints of M 140x6 mm type used for WWER-440 MW reactor pressure vessels. Bolting joints or real dimensions were tested in a special testing equipment ZS 1000 in Skoda Concern. Stud bolts are made from 25Kh1MF or 38KhN3MFA type of steels. Tests were carried out at operating as well as at room temperatures with coefficient of asymmetry equal to 0.1; one tests was realized with given bending moment. Experimental results have been compared with calculated lifetimes according to ASME, Soviet and CMEA Codes. In all cases calculations give conservative assessments. (orig.)

  5. Hot rolling of chromium - nickel - manganese stainless steel containing nitrogen and boron

    International Nuclear Information System (INIS)

    Khorosh, V.A.; Bulat, S.I.; Mukhina, M.A.; Sorokina, N.A.; Yushchenko, K.A.; Tsentral'nyj Nauchno-Issledovatel'skij Inst. Chernoj Metallurgii, Moscow; AN Ukrainskoj SSR, Kiev. Inst. Ehlektrosvarki)

    1976-01-01

    The strength of stainless steel of the 03Kh2ON16AG6 type increases perceptibly with an increase in the nitrogen content from 0.11 to 0.37%. At the same time, however, its ductility in the region of hot deformation temperatures (red brittleness range of 800 to 1,000 deg C) decreases. Microalloying with boron (0.002 to 0.005% by calculation) permits enhancing the hot ductility to an acceptable level without adversely affecting the working properties. The mechaniusm of boron effect is analyzed. The temperature at which ingots are heated prior to rolling to achieve the desired effect must be sufficiently low. Optimum condition for two stage heating of 6.2-ton ingots are recommeded

  6. Stahlschüssel key to steel

    CERN Document Server

    Wegst, W S

    2016-01-01

    The Key to Steel (Stahlschlüssel/Stahlschluessel) cross reference book will help you to decode / decipher steel designations and find equivalent materials worldwide. The 2016 edition includes more than 70,000 standard designations and trade names from approximately 300 steelmakers and suppliers. Presentation is trilingual: English, French, and German. Materials covered include structural steels, tool steels, valve steels, high temperature steels and alloys, stainless and heat-resisting steels, and more. Standards and designations from 25 countries are cross-referenced.

  7. Effect of microplastic strain on hydrogen behaviour in steel and resistance to hydrogen embrittlement

    Energy Technology Data Exchange (ETDEWEB)

    Gribanova, L.I.; Sarrak, V.I.; Filippov, G.A.; Shlyafirner, A.M. (Tsentral' nyj Nauchno-Issledovatel' skij Inst. Chernoj Metallurgii, Moscow (USSR))

    1981-01-01

    A connection between the tendency to delayed fracture and resistance to microplastic deformation is studied in the presence of hydrogen on smooth samples of the 40Kh steel. Tests for delayed fracture have been carried out at the ''Instron'' machine. Two critical levels of strains during delayed fracture in the hydridation process are found out (sigmasub(cr1)=0.3sigmasub(0.2) and sigmasub(cr2)=0.5sigmasub(0.2)). At stresses below the sigmasub(cr1) hydrogen does not influence on the resistance to microplastic deformation of steel and does not cause delayed fracture. Propagation of cracks arising from defects occurring as a result of mutual effect of hydrogen and elastic stresses runs in the stress range from sigmasub(cr1) up to sigmasub(cr2). At stresses higher than sigmasub(cr2) the crack propagates from defects existing in the moment of hydridation process beginning.

  8. Constructing kinetics fatigue diagrams using testing results obtained on a machine with rigid loading for specimens of various thickness

    International Nuclear Information System (INIS)

    Simin'kovich, V.N.; Gladkij, Ya.N.; Deev, N.A.

    1981-01-01

    Bending tests of 40KhS steel specimens, tempered at 200 and 500 deg C, are conducted to investigate the possible effects of specimen thickness on fatigue crack growth. Kinetic fatigue diagrams are constructed using the investigation results. An increase in crack growth with thickness is observed only in high-tempered specimens. Changes in specimen thickness do not affect crack growth in 40KhS low-tempered steel [ru

  9. Structure and phase composition of titanium nitride coating on austenitic steel

    International Nuclear Information System (INIS)

    Dubovitskaya, N.V.; Kolenchenko, L.D.; Larikov, L.N.

    1989-01-01

    Structure and phase composition of titanium nitride coating deposited on 08Kh18N10T steel substrate using ''Bulat'' device are studied. Use of complex investigation methods permitted despite small coating thickness (1μm) to aquire information on hardness, porosity, to study phase composition in all coating thickness. The surface layer (∼0.1 μm) consists of ε-Ti 2 N, TiN 0.6 , TiC 0.35 , that is formed with carbon participation from oil vacuum. In more deeper layers beside ε-Ti 2 N TiC 0.14 N 0.77 is present. Effect of carbon diffusion from substrate to forming coating is stated. Gradient of element concentrations in the substrate-coating interface causes recrystallization of austenite

  10. Pendidikan Karakter Menurut K.H. Hasyim Asy'ari Dalam Kitab Adâb Al-‘Âlim Wa Al-Muta‘Allim

    OpenAIRE

    Sholikah, Sholikah

    2015-01-01

    The article deals with K.H. Hasyim Asy'ari's thought of character education. The result of the study indicates that according to K.H. Hasyim Asy'ari the characters of teachers and students in his work Adab al-‘Âlim wa al-Muta'allim can be classified into three parts, are mentality or character, which should be possessed by teachers and learners: attempts to be done in order to become characterized teachers and learners, and: teaching strategies employed by educators and learning strategies us...

  11. Corrosion inhibition performance of 2,5-bis(4-dimethylaminophenyl)-1,3,4-oxadiazole for carbon steel in HCl solution: Gravimetric, electrochemical and XPS studies

    Energy Technology Data Exchange (ETDEWEB)

    Bouanis, M.; Tourabi, M.; Nyassi, A. [Laboratoire de Catalyse et de Corrosion des Matériaux (LCCM), Faculté des Sciences, Université Chouaib Doukkali, B.P. 20, M-24000 El Jadida (Morocco); Zarrouk, A. [LCAE-URAC 18, Faculty of Science, First Mohammed University, PO Box 717, M-60 000 Oujda (Morocco); Jama, C. [UMET-ISP, CNRS UMR 8207, ENSCL, Université Lille Nord de France, CS 90108, F-59652 Villeneuve d' Ascq Cedex (France); Bentiss, F., E-mail: fbentiss@gmail.com [Laboratoire de Catalyse et de Corrosion des Matériaux (LCCM), Faculté des Sciences, Université Chouaib Doukkali, B.P. 20, M-24000 El Jadida (Morocco); UMET-ISP, CNRS UMR 8207, ENSCL, Université Lille Nord de France, CS 90108, F-59652 Villeneuve d' Ascq Cedex (France)

    2016-12-15

    Highlights: • 2,5-Bis(4-dimethylaminophenyl)-1,3,4-oxadiazole is good corrosion inhibitor for carbon steel in 1 M HCl. • XPS analysis has provided the composition of adsorbed protective layer on the steel surface. • The adsorption of the investigated 1,3,4-oxadiazole is mainly due to chemisorption. - Abstract: Corrosion inhibition of carbon steel in normal hydrochloric acid solution at 30 °C by 2,5-bis(4-dimethylaminophenyl)-1,3,4-oxadiazole (DAPO) has been studied by weight loss measurements and electrochemical techniques (polarization and AC impedance). The experimental results showed that DAPO acted as an efficient inhibitor against the carbon steel corrosion in 1 M HCl, and its inhibition efficiency increased with the inhibitor concentration reaching a value up to 93% at 1 mM. Polarization studies showed that the DAPO was a mixed-type inhibitor. The adsorption of this 1,3,4-oxadiazole derivative on the carbon steel surface in 1 M HCl solution followed the Langmuir adsorption isotherm and the corresponding value of the standard Gibbs free energy of adsorption (ΔG°{sub ads}) is associated to a chemisorption mechanism. Scanning Electron Microscopy (SEM) and X-Ray Photoelectron Spectroscopy (XPS) analyses were carried out to characterize the chemical composition of the inhibitive film formed on the steel surface. The surfaces studies showed that the inhibitive layer is composed of an iron oxide/hydroxide mixture where DAPO molecules are incorporated. The cytotoxicity of DAPO was also determined using cell culture system.

  12. Comparison of the tribological properties at 25 C of seven different polyimide films bonded to 301 stainless steel

    Science.gov (United States)

    Fusaro, R. L.

    1980-01-01

    A pin-on-disk type of friction and wear apparatus was used to study the tribological properties of seven different polyimide films bonded to AISI 301 stainless steel disks at 25 C. It was found that the substrate material was extremely influential in determining the lubricating ability of the polyimide films. All seven films spalled in less than 1000 cycles of sliding. This was believed to be caused by poor adherence to the 301 stainless steel or the inability of the films to withstand the high localized tensile stresses imparted by the deformation of the soft substrate under sliding conditions. The friction coefficients obtained for six of the polyimides varied between 0.21 to 0.32 while one varied between 0.32 to 0.39.

  13. Study of regularities in propagation of thermal fatigue cracks

    International Nuclear Information System (INIS)

    Tachkova, N.G.; Sobolev, N.D.; Egorov, V.I.; Rostovtsev, Yu.V.; Ivanov, Yu.S.; Sirotin, V.L.

    1978-01-01

    Regularities in the propagation of thermal fatigue cracks in the Cr-Ni steels of the austenite class depending upon deformation conditions in the crack zone, have been considered. Thin-walled tube samples of the Kh16N40, Kh18N20 and Kh16N15 steels have been tested in the 10O reversible 400 deg C and 100 reversible 500 deg C regimes. The samples have possessed a slot-shaped stress concentrator. Stress intensity pseudocoefficient has been calculated for the correlation of experimental data. The formula for determining crack propagation rate has been obtained. The experiments permit to conclude that propagation rate of thermal fatigue cracks in the above steels depends upon the scope of plastic deformation during a cycle and stress intensity pseudocoefficient, and is determined by plastic deformation resistance during thermal cyclic loading

  14. Inhibition of salt precipitation, corrosion and corrosion fatigue of steel in neutral environments

    International Nuclear Information System (INIS)

    Mikhajlovskij, V.Ya.; Slobodyan, Z.V.; Soprunyuk, N.G.; Ivanov, A.M.

    1983-01-01

    Processes of salt precipitation, corrosion under dynamic and static conditions, are studied as well as corrosion fatigue of 20 and 40Kh steels in neutral aqueous media without and with the addition of compounds of several classes. The solution of calcium bicarbonate with the initial concentration [Ca(HCO 3 ) 2 ]=1.3 g/l and 3% NaCl solution in distilled water are used for investigation. The effectiveness index of salt precipitation inhibitor is determined by the change in the rate of calcium bicarbonate transformation into carbonate. The combination of results obtained permits to make the conclusion that tripolyphosphate and pyrophosphoric acid are rather perspective inhibitors of complex effect with low protective concentrations

  15. Combined equilibrium and non-equilibrium phosphorus segregation to grain boundaries in a 2.25Cr1Mo steel

    International Nuclear Information System (INIS)

    Song, S.-H.; Shen, D.-D.; Yuan, Z.-X.; Liu, J.; Xu, T.-D.; Weng, L.-Q.

    2003-01-01

    Grain boundary segregation of phosphorus in a P-doped 2.25Cr1Mo steel during ageing at 540 deg. C after quenching from 980 deg. C is examined by Auger electron spectroscopy. The segregation is a combined effect of equilibrium segregation and non-equilibrium segregation. The effect of phosphorus non-equilibrium segregation is to enhance the kinetics of its equilibrium segregation

  16. Effect of rhenium and osmium on mechanical properties of a 9Cr-2W-0.25V-0.07Ta-0.1C steel

    International Nuclear Information System (INIS)

    Klueh, R.L.; Alexander, D.J.; Sokolov, M.A.

    2000-01-01

    The nuclear transmutation of tungsten to rhenium and osmium in a tungsten-containing steel irradiated in a fission or fusion reactor will change the chemical composition of the steel. To determine the possible consequences of such compositional changes on the mechanical properties, tensile and Charpy impact properties were measured on five 9Cr-2W-0.25V-0.07Ta-0.1C steels that contained different amounts of rhenium, osmium, and tungsten. The mechanical properties changes caused by these changes in composition were minor. Observations were also made on the effect of carbon concentration. The effect of carbon on tensile behavior was minor, but there was a large effect on Charpy properties. Several of the steels showed little effect of tempering temperature on the Charpy transition temperature, a behavior that was tentatively attributed to the low silicon and/or manganese concentration of the experimental steels

  17. Radiation-induced sensitisation of stainless steels

    International Nuclear Information System (INIS)

    Norris, D.I.R.

    1987-01-01

    The book contains the proceedings of a symposium on radiation-induced sensitization of stainless steels, which took place at Berkeley, United Kingdom, 1986. The purpose of the symposium was to examine the mechanism leading to inter-granular corrosion of 20%Cr/25% Ni/Nb stainless steel cladding of AGR fuel following irradiation. Nine papers are presented, of which three are theoretical, two papers are based upon corrosion studies of 20%Cr/25%Ni/Nb steel, and the remaining are concerned with compositional redistribution and its measurement. (U.K.)

  18. Effects of multi-pass arc welding on mechanical properties of carbon steel C25 plate

    International Nuclear Information System (INIS)

    Adedayo, S.M.; Babatunde, A.S.

    2013-01-01

    The effects of multi-pass welding on mechanical properties of C25 carbon steel plate were examined. Mild steel plate workpieces of 90 x 55 mm 2 area and 10 mm thickness with a 30 degrees vee weld-grooves were subjected to single and multi-pass welding. Toughness, hardness and tensile tests of single and multi-pass welds were conducted. Toughness values of the welds under double pass welds were higher than both single pass and unwelded alloy, at respective maximum values of 2464, 2342 and 2170 kN/m. Hardness values were reduced under double pass relative to single pass welding with both being lower than the value for unwelded alloy; the values were 40.5, 43.2 and 48.5 Rs respectively at 12 mm from the weld line. The tensile strength of 347 N/mm 2 under multi-pass weld was higher than single pass weld with value of 314 N/mm 2 . Therefore, the temperature distribution and apparent pre-heating during multi-pass welding increased the toughness and tensile strength of the weldments, but reduced the hardness. (au)

  19. Superprotonic KH(PO3H)-SiO2 composite electrolyte for intermediate temperature fuel cells

    NARCIS (Netherlands)

    Bandarenka, A.; Bondarenko, Alexander S.; Zhou, W.; Bouwmeester, Henricus J.M.

    2009-01-01

    Novel thin film composite electrolyte membranes, prepared by dispersion of nano-sized SiO2 particles in the solid acid compound KH(PO3H), can be operated under both oxidizing and reducing conditions. Long-term stable proton conductivity is observed at not, vert, similar140 °C, i.e., slightly above

  20. Structure and properties of joints of two-ply steel using ''elastic'' explosives

    International Nuclear Information System (INIS)

    Gel'man, A.S.; Savel'ev, S.A.; Kulakevich, Ya.S.; Sharypov, N.A.; Drogovejko, I.Z.; Domolego, I.E.

    1980-01-01

    Some experimental data on structure and properties of compounds during cladding of sheets made of St3 with sheets of nichrome and steel 12Kh18N10T with the use of ''elastic'' explosives are presented. It is shown that the use of ''elastic'' explosives permits to decrease r parameter sufficiently, (where r - is the ratio of explosive mass to the mass of throwen phate) that reduces considerably the specific consumption explosives in comparison with the consumption conventional mixture explosives. Peculiarities of tested ''elastic'' explosives make their application perspective in two cases - at cladding of complex curved surfaces (drums, tube blanks etc.), as sell as at applications of burst chambers, where explosive mass limits dimensions of cladding blanks and details [ru

  1. PENDIDIKAN KARAKTER MENURUT K.H. HASYIM ASY’ARI DALAM KITAB ADÂB AL-‘ÂLIM WA AL-MUTA‘ALLIM

    Directory of Open Access Journals (Sweden)

    Sholikah Sholikah

    2015-09-01

    Full Text Available The article deals with K.H. Hasyim Asy’ari’s thought of character education. The result of the study indicates that according to K.H. Hasyim Asy’ari the characters of teachers and students in his work Adab al-‘Âlim wa al-Muta’allim can be classified into three parts, are mentality or character, which should be possessed by teachers and learners: attempts to be done in order to become characterized teachers and learners, and: teaching strategies employed by educators and learning strategies used by learners. These three parts have compatible indicators with the competence of educators stated in UU Sisdiknas (The Legislation of National Educational System year 2003 along with 18 values of character promulgated by Pusat Kurikulum Pengembangan dan Pendidikan Budaya dan Karakter Bangsa. Moreover, according to K.H. Hasyim Asy’ari, the relevance of character education with the context of character education in Indonesia consists of a number of character education elements, namely the meaning and goal of character education, the values of character for both teachers and students, the rationale of character education, the method of character education, the media of character education, and the evaluation of character education

  2. Study on the process of calibration and deep centring of blanks

    International Nuclear Information System (INIS)

    Potapov, I.N.; Romantsev, B.A.; Popov, V.A.; Volodin, V.V.; Goncharuk, A.V.

    1985-01-01

    Process of calibration and deep centring of blanks before broaching is developed and studied. Investigations are performed at a semi-industrial screw rolling mill MISiS-100 T. Blanks made of 40Kh, 60, 50, 45KhN2MFA, 30KhGSNA steels 80, 85, and 90 mm in diameter and 300 mm long were calibrated and centered after heating in a furnace to a depth of 200 mm at shafts and faces with different calibration. 30KhN2MFA steel is chosen for face material; heat treatment is conducted under the following conditions: heating up to 950-1000 deg C and hold-up during 30-35 min with the following cooling in the air. The above experimental investigations reveal that the process of calibration and deep centring accomplished at a three-shaft screw rolling mill is rather stable and provides a high accuracy of centering hollow marking

  3. Structure and delayed failure behaviour of 0.25C-Ni-Cr-Mo-V steel

    International Nuclear Information System (INIS)

    Kang, C.H.; Maeng, S.C.

    1980-01-01

    Delayed failure behaviour of the different transformation structures of 0.25C-2.5Ni-2.5Cr-0.5Mo-0.1V low alloy steel has been studied. The studied microstructures are martensite, lower bainite, and mixed structure of 50% martensite and 50% lower bainite. All these structures have been tempered at 450 deg C for 40 min to have the same tensile strength level of 143 kg/mm 2 . Delayed failure testing has been carried out with cantilever bend tester, in distilled water at 25 deg C. By comparing K 1 sub(scc) values, lower bainitic structure has shown the highest value, although it is only slightly higher than that of the martensitic structure. Mixed structure has the lowest resistance to delayed failure. The fracture modes of both martensitic and mixed structures have been observed as intergranular. In the martensitic structure, however, it is noticeable that there is a larger amount of ductile tearing between intergranular facets. The fracture mode of lower bainitic structure is the mixed topography of microplastic tearing and microvoid coalescence. The above experimental results are discussed in terms of Oriani's decohesion theory of hydrogen embrittlement. The lowest resistance of the mixed structure to delayed failure may be due to the enhanced decohesion by hydrogen at the phase boundaries of martensite and lower bainite. (author)

  4. Polarization mechanism and ferroelectric instability in KH2PO4

    International Nuclear Information System (INIS)

    Koval, S.; Migoni, R.L.; Kohanoff, J.; Bussmann-Holder, A.

    2000-11-01

    The polarization mechanism and the origin of ferroelectricity in KH 2 PO 4 (KDP) are studied by first-principles electronic structure calculations. In the low-temperature phase, the collective off-center ordering of the protons is accompanied by an electronic charge delocalization from the near and localization at the far oxygen within the O-H...0 bonds. Electrostatic forces, then, push the K + ions towards off-center positions, and induce a macroscopic polarization. The analysis of the correlation between different geometrical and electronic quantities, in connection with experimental data, supports the idea that the role of tunnelling in isotopic effects is irrelevant. Instead, geometrical quantum effects appear to play a central role. (author)

  5. Radiation damage structure in irradiated and annealed 440 WWER-Type reactor pressure vessel steels

    International Nuclear Information System (INIS)

    Kocik, J.; Keilova, E.

    1993-01-01

    A review of irradiation damages in WWER-type RPV steels based on conventional Transmission Electron Microscopy investigations in a power reactor and a research reactor, is presented; the samples consist in Cr-Mo-V ferritic steel (15Kh2MFA type). The visible part of radiation-induced defects consists of very fine vanadium carbide precipitates, small dislocation loops and black dots (presumably corresponding to clusters and particle embryos formed from vacancies and solute-atoms (vanadium, copper, phosphorus) and carbon associated with vanadium. Radiation-induced defects are concentrated at dislocation substructure during irradiation in a power reactor, revealing the role of radiation-enhanced diffusion in damage structure forming process. Contrarily, the distribution of defects resulting from annealing of specimens irradiated in the research reactor is pre-determined by an homogenous distribution of radiation-induced defects prior to annealing. Increasing the number of re-irradiation and annealing cycles, the amount of dislocation loops among all defects seems to be growing. Simultaneously, the dislocation substructure recovers considerably. (authors). 14 refs., 11 figs., 3 tabs

  6. Radiation damage structure in irradiated and annealed 440 WWER-Type reactor pressure vessel steels

    Energy Technology Data Exchange (ETDEWEB)

    Kocik, J; Keilova, E [Czech Nuclear Society, Prague (Czech Republic)

    1994-12-31

    A review of irradiation damages in WWER-type RPV steels based on conventional Transmission Electron Microscopy investigations in a power reactor and a research reactor, is presented; the samples consist in Cr-Mo-V ferritic steel (15Kh2MFA type). The visible part of radiation-induced defects consists of very fine vanadium carbide precipitates, small dislocation loops and black dots (presumably corresponding) to clusters and particle embryos formed from vacancies and solute-atoms (vanadium, copper, phosphorus) and carbon associated with vanadium. Radiation-induced defects are concentrated at dislocation substructure during irradiation in a power reactor, revealing the role of radiation-enhanced diffusion in damage structure forming process. Contrarily, the distribution of defects resulting from annealing of specimens irradiated in the research reactor is pre-determined by an homogenous distribution of radiation-induced defects prior to annealing. Increasing the number of re-irradiation and annealing cycles, the amount of dislocation loops among all defects seems to be growing. Simultaneously, the dislocation substructure recovers considerably. (authors). 14 refs., 11 figs., 3 tabs.

  7. KH 2PO4 as a novel catalyst for regioselective monobromination of aralkyl ketones using N-bromosuccinimide: a green methodology

    Directory of Open Access Journals (Sweden)

    P. Md. Khaja Mohinuddin

    2015-08-01

    Full Text Available A simple, regioselective and green method has been developed for the preparation of monobrominated ketones from various aralkyl ketones by using N-bromosuccinimide in presence of KH 2PO 4 in EtOH at reflux temperature. The present method is of short reaction time and simple with excellent isolated yields of products. The use of eco-friendly solvent, reuse of organic waste (succinimide and recyclable catalyst used for 4 times without loss of activity are advantageous. This is the first example of the use of KH 2PO 4 as a useful catalyst in organohalogen chemistry and the present method meets reduce-reuse-recycle (RRR principle towards development of green protocol.

  8. The steel scrap age.

    Science.gov (United States)

    Pauliuk, Stefan; Milford, Rachel L; Müller, Daniel B; Allwood, Julian M

    2013-04-02

    Steel production accounts for 25% of industrial carbon emissions. Long-term forecasts of steel demand and scrap supply are needed to develop strategies for how the steel industry could respond to industrialization and urbanization in the developing world while simultaneously reducing its environmental impact, and in particular, its carbon footprint. We developed a dynamic stock model to estimate future final demand for steel and the available scrap for 10 world regions. Based on evidence from developed countries, we assumed that per capita in-use stocks will saturate eventually. We determined the response of the entire steel cycle to stock saturation, in particular the future split between primary and secondary steel production. During the 21st century, steel demand may peak in the developed world, China, the Middle East, Latin America, and India. As China completes its industrialization, global primary steel production may peak between 2020 and 2030 and decline thereafter. We developed a capacity model to show how extensive trade of finished steel could prolong the lifetime of the Chinese steelmaking assets. Secondary steel production will more than double by 2050, and it may surpass primary production between 2050 and 2060: the late 21st century can become the steel scrap age.

  9. Microstructural characterization of 5-9% chromium reduced-activation steels

    International Nuclear Information System (INIS)

    Jayaram, R.; Klueh, R.L.

    1997-01-01

    The microstructures of a 9Cr-2W-0.25-0.1C (9Cr-2WV), a 9Cr-2W-0.25V-0.07Ta-0.1C (9Cr-2WVTa), a 7Cr-2W-0.25V-0.07Ta-0.1C (7Cr-2WVTa), and a 5Cr-2W-0.25V-0.07Ta-0.1C (5Cr-2WVTa) steel (all compositions are in weight percent) have been characterized by Analytical Electron Microscopy (AEM) and Atom Probe Field Ion Microscopy (APFIM). The matrix in all four reduced-activation steels was 100% martensite. In the two 9Cr steels, the stable precipitates were blocky M 23 C 6 and small spherical MC. The two lower-chromium steels contained blocky M 7 C 3 and small needle-shaped carbonitrides in addition to M 23 C 6 . AEM and APFIM analysis revealed that in the steels containing tantalum, the majority of the tantalum was in solid solution. The experimental observations were in good agreement with phases and compositions predicted by phase equilibria calculations

  10. Measurement of trace elements in KH2PO4 crystals by x-ray fluorescence spectrometry

    International Nuclear Information System (INIS)

    Ryon, R.W.; Duewer, T.I.

    1981-02-01

    A non-destructive method is described for the quantitative measurement of impurities in KDP (KH 2 PO 4 ) crystals. Part per million concentrations of impurities can be determined with good accuracy in about one hour of instrument time. An energy dispersive x-ray spectrometer is used. Both the crystals and the solutions from which they are grown may be analyzed

  11. ESF GROUND SUPPORT - STRUCTURAL STEEL ANALYSIS

    Energy Technology Data Exchange (ETDEWEB)

    T. Misiak

    1996-06-26

    The purpose and objective of this analysis are to expand the level of detail and confirm member sizes for steel sets included in the Ground Support Design Analysis, Reference 5.20. This analysis also provides bounding values and details and defines critical design attributes for alternative configurations of the steel set. One possible configuration for the steel set is presented. This analysis covers the steel set design for the Exploratory Studies Facility (ESF) entire Main Loop 25-foot diameter tunnel.

  12. Elevated temperature creep and fatigue damage of a 2.25 Cr--1 Mo steel weldment

    International Nuclear Information System (INIS)

    Van Den Avyle, J.A.

    1978-01-01

    In weldments between dissimilar metals wide variations occur in metallurgical structure and mechanical properties, so that for good structural design it is necessary to understand the mechanical response of individual microstructural segments of the weld. This study investigates elevated temperature properties of a 2.25 Cr--1 Mo ferritic steel base metal welded with Chromenar 382V (Inconel 82) filler metal. Creep and low-cycle fatigue tests at 866 0 K (1100 0 F) show the filler metal and heat affected zone to be much stronger than the base metal. Optical microscopy does not show significant aging effects in the short-term fatigue tests or creep tests of 1180 hour duration

  13. Investigation programme and procedure for creep and long-term rupture strength in materials with accounting for stress deviator and loading history

    International Nuclear Information System (INIS)

    Mozharovskaya, T.N.

    1984-01-01

    A programme and procedure are given to study 08Kh18N9 steel at 600 deg C and 15Kh2MFA steel at 550 deg C for creep and long-term strength at different parameters of proportional loading as well as at different parameters under loading in two-link irregular trajectories. This makes it possible to estimate the effect of the kind of a stress deviator, history and prehistory of loading on plastic deformation in creep and on failure under long-term loading

  14. Investigation programme and procedure for creep and long-term rupture strength in materials with accounting for stress deviator and loading history

    Energy Technology Data Exchange (ETDEWEB)

    Mozharovskaya, T N [AN Ukrainskoj SSR, Kiev. Inst. Problem Prochnosti

    1984-11-01

    A programme and procedure are given to study 08Kh18N9 steel at 600 deg C and 15Kh2MFA steel at 550 deg C for creep and long-term strength at different parameters of proportional loading as well as at different parameters under loading in two-link irregular trajectories. This makes it possible to estimate the effect of the kind of a stress deviator, history and prehistory of loading on plastic deformation in creep and on failure under long-term loading.

  15. Microstructural evolution in austenitic heat-resistant cast steel 35Cr25Ni12NNbRE during long-term service

    International Nuclear Information System (INIS)

    Liu Jiangwen; Jiao Dongling; Luo Chengping

    2010-01-01

    The microstructural evolution of austenitic heat-resistant cast steel 35Cr25Ni12NNbRE during aging and long-term service was investigated using optical microscope (OM), X-ray diffraction (XRD), scanning electron microscope (SEM) and transmission electron microscope (TEM). The microstructure of the as cast steel consists of the dendritic austenite, the block-like eutectic carbide M 7 C 3 spreaded among austenitic dendrite, and a small quantity of M 23 C 6 carbide. The microstructure of the steel aged at 600 deg. C consists of eutectic carbide M 23 C 6 transformed from eutectic carbide M 7 C 3 and dendritic austenite in which fine secondary carbide particles M 23 C 6 precipitated. The precipitated carbide M 23 C 6 kept a cubic-cubic orientation relationship (OR) with austenite matrix. There existed a carbide precipitation free zone (PFZ) around the eutectic carbide. For the long-term serviced samples, the secondary carbide precipitated in the austenite strikingly increased and the PFZ disappeared. Part of the M 23 C 6 transformed into M 6 C, which always kept a twin OR, [114] M 6 C //[110] A //[110] M 23 C 6 , with the austenite and the M 23 C 6 secondary carbide. In addition, a small quantity of σ phase FeCr and ε-Cr 2 N were also identified. The effects of alloy composition and service condition on the microstructural evolution of the steel were discussed.

  16. Microstructural evaluation and non-destructive examination of 2.25 Cr--1 Mo steel

    International Nuclear Information System (INIS)

    Van Den Avyle, J.A.; Jones, W.B.; Gieske, J.H.

    1978-07-01

    Specimens of 2.25 Cr-1 Mo steel were damaged to various levels by creep and combined creep-fatigue cycling at 886 0 K (1100 0 F) with hold periods. Ultrasonic shear wave velocity measurements were performed and showed small changes with large amounts of creep or fatigue damage; these changes were deemed too small for practical application. Measurements of magnetic properties were unsuccessful in following damage. Optical and transmission electron microscopy (TEM) were performed on the samples. TEM observations showed that microstructural changes which occurred at 886 0 K (1100 0 F) did not occur homogeneously throughout the matrix; during creep, carbide spheroidization and coarsening began in widely separated regions, with an increasing fraction of the material undergoing the process with time. A precipitate was observed to form during fatigue which did not occur during simple aging or creep

  17. Composition of the spheroidal objects in KhN77TYuR-VD alloy

    International Nuclear Information System (INIS)

    Kotkis, M.A.; Nabutovskii, L.S.; Ostrov, A.E.; Zil'berman, A.G.

    1986-01-01

    The authors make an element analysis of the spheroidal objects in KhN77TYuR-VD alloy with the use of the energy dispersion microanalyzer with which the Stereoscan S-180 scanning electron microscope is equipped. Examples of the qualitative element analysis are shown. The results of the investigations show that the composition of the spheroidal inclusions includes nickel, chromium, titanium, iron, and also silicon and sulfur. The information obtained makes it possible to make an assumption on the mechanism of origin of these objects

  18. Microstructural characterization of 5-9% chromium reduced-activation steels

    Energy Technology Data Exchange (ETDEWEB)

    Jayaram, R. [Univ. of Pittsburgh, PA (United States); Klueh, R.L. [Oak Ridge National Lab., TN (United States)

    1997-08-01

    The microstructures of a 9Cr-2W-0.25-0.1C (9Cr-2WV), a 9Cr-2W-0.25V-0.07Ta-0.1C (9Cr-2WVTa), a 7Cr-2W-0.25V-0.07Ta-0.1C (7Cr-2WVTa), and a 5Cr-2W-0.25V-0.07Ta-0.1C (5Cr-2WVTa) steel (all compositions are in weight percent) have been characterized by Analytical Electron Microscopy (AEM) and Atom Probe Field Ion Microscopy (APFIM). The matrix in all four reduced-activation steels was 100% martensite. In the two 9Cr steels, the stable precipitates were blocky M{sub 23}C{sub 6} and small spherical MC. The two lower-chromium steels contained blocky M{sub 7}C{sub 3} and small needle-shaped carbonitrides in addition to M{sub 23}C{sub 6}. AEM and APFIM analysis revealed that in the steels containing tantalum, the majority of the tantalum was in solid solution. The experimental observations were in good agreement with phases and compositions predicted by phase equilibria calculations.

  19. Effect of reactor irradiation on long-term strength and creep of 0Kh16N15M3B steel under plane stressed state

    International Nuclear Information System (INIS)

    Khristov, G.P.; Kosov, B.D.

    1982-01-01

    The paper deals with analysis of results of experimental studies in creep of the austenitic OKh16n15m3b steel with various size of initial-structure grain under conditions of high-intensity reactor irradiation and control tests. It is suggested to consider the material initial structure effect on intensity of minimum creep rates both under ordinary and intrareactor conditions of loading by means of the function grain size effect on the equivalent stress. It is shown that the criterial expression previously suggested by the authors is invariant to the type of stressed and structural states and relative to intensity of minimal creep rates. It is established that the creep rate of the irradiated steel may be calculated from dependence for nonirradiated steel using as an argument a certain reduced equivalent stress which is a function of the acting stress and irradiation parameter

  20. Auburn Steel Company radioactive contamination incident

    International Nuclear Information System (INIS)

    Bradley, F.J.; Cabasino, L.; Kelly, R.; Awai, A.; Kasyk, G.

    1986-04-01

    On February 21, 1983, workers at the Auburn Steel Company, Auburn, New York discovered that about 120 tons of steel poured that day had become contaminated with 60 Co. In addition to the steel, the air cleaning system and portions of the mill used in casting the steel were contaminated. Approximately 25 curies of 60 Co were involved. Decontamination and disposal of the contamination cost in excess of $2,200,000. This report details the discovery of the contamination, decontamination of the plant and disposal of the contamination

  1. Study of radiation-thermal effect of electron beam on steel and cast iron

    International Nuclear Information System (INIS)

    Machurin, E.S.; Lonchin, G.M.

    1980-01-01

    Studied is the influence of radiation-heat treatment by high energy (3-4.5 MeV) electron beam on the structure and properties of carbon steels (65G, 90KhF) and cast iron. Metallography and electron microscopy methods are used to study microstructure. It is shown that after the treatment by the electron beam there is observed noticeable structure grinding, sample fracture viscosity (even in a quenched state), increase of hardness and impact strength. The mechanism of metal heating process by electron beam is calculated and temperature field is defined in a heating region accounting for electron beam characteristics, medium and geometric factor. Theoretical data are close to experimental ones obtained in a course of determining the microhardness of irradiated samples for the cases of electron treatment duration up to 10 s

  2. Structural changes IN THE Kh20N45M4B nickel alloys and THE Kh16N15M3B steel due to helium ion bombardment

    International Nuclear Information System (INIS)

    Kalin, B.A.; Chernikov, U.N.; Chernov, I.I.; Kozhevnikov, O.A.; Shishkin, G.N.; Yakushin, V.L.

    1986-01-01

    Using transmission electron microscopy, x-ray structural analysis, and the thermal desorption techniques, the authors carried out a detailed study of the structural and phase changes, defect formation, and helium accumulation in the He + -bombarded 16-15 austenitic steels and 20-45 nickel alloys. Microstructure of the bombarded specimens was studied using the methods of transmission electron microscopy of thin foils in the EVM-100, and EM-301G electron microscopes. Results of x-ray studies on the bombarded specimens are presented. The conducted studies show that bombardment of structural materials with light ions can lead to significant structural damages and changes in the chemical and phase composition of the surface layer. The possible mechanisms of the changes in the chemical and phase composition include selective sputtering and radiation-induced accelerated diffusion of elements in the field of internal lateral stresses developing during the He + implantation process

  3. Weldability of Stainless Steels

    International Nuclear Information System (INIS)

    Saida, Kazuyoshi

    2010-01-01

    It gives an outline of metallographic properties of welding zone of stainless steels, generation and mechanisms of welding crack and decreasing of corrosion resistance of welding zone. It consists of seven chapters such as introduction, some kinds of stainless steels and properties, metallographic properties of welding zone, weld crack, toughness of welding zone, corrosion resistance and summary. The solidification modes of stainless steels, each solidification mode on the cross section of Fe-Cr-Ni alloy phase diagram, each solidification mode of weld stainless steels metal by electron beam welding, segregation state of alloy elements at each solidification mode, Schaeffler diagram, Delong diagram, effects of (P + S) mass content in % and Cr/Ni equivalent on solidification cracking of weld stainless steels metal, solidification crack susceptibility of weld high purity stainless steels metal, effects of trace impurity elements on solidification crack susceptibility of weld high purity stainless steels metal, ductile fracture susceptibility of weld austenitic stainless steels metal, effects of H2 and ferrite content on generation of crack of weld 25Cr-5N duplex stainless steels, effects of O and N content on toughness of weld SUS 447J1 metals, effect of ferrite content on aging toughness of weld austenitic stainless steel metal, corrosion morphology of welding zone of stainless steels, generation mechanism of knife line attack phenomenon, and corrosion potential of some kinds of metals in seawater at room temperature are illustrated. (S.Y.)

  4. Technical Note: Calibration device for the krypton hygrometer KH20

    Directory of Open Access Journals (Sweden)

    T. Foken

    2012-08-01

    Full Text Available A calibration device for krypton hygrometers (KH20, Campbell Scientific, Inc. with variable path length is presented. This unit allows for in-situ calibrations of the krypton hygrometer, which is typically not very stable over time, during measuring campaigns. It was constructed mainly for application at high altitudes and low temperatures, where further improvements are needed to the IR-hygrometers which are normally used. The changing path length requires that a changing concentration of the absorber be simulated. Because oxygen absorbs more strongly than water vapour, the calibration is made against oxygen and transferred to water vapour. The design of the calibration instrument is made as one unit containing a stepper motor system, PC and humidity sensor. For the calibration, it is necessary to install the krypton hygrometer on this unit.

  5. Active and passive fire protection system in academic building KH. Mas Mansur, Islamic University of Indonesia

    Directory of Open Access Journals (Sweden)

    Suryoputro M. Ragil

    2018-01-01

    Full Text Available According to the theory of fire triangle, the existence of combustible materials, heat, and oxygen can cause fire disaster. KH. Mas Mansur building, Islamic University of Indonesia has a fire protection, but rarely to be checked regularly and the number of equipment is less standard as well as the lack of an evacuation route map to facilitate the evacuation process. Inside the building also does not provide safety signs such as the evacuation directions, exit, and warning in case of fire. Therefore, researchers analysed the infrastructure of prevention and control in the building KH. Mas Mansur. Researchers used the method of observation, interviews, and checklist to know the condition directly, and compare with the standard regulations. Results concordance rate of existing infrastructure is 67% fire extinguisher, hydrant box 56%, 71% alarms, sprinkler 0%, 40% detectors, emergency doors 71%, 50% emergency stairs, assembly point 0% and directions 0%. The current results were below the standard of at least 80%. As for recommendations, researchers create a new evacuation map then put the existing infrastructure according to standard regulations, and it had consulted with the specialist of Occupational Safety and Health in the field of fire.

  6. Metastable structure formation during high velocity grinding

    International Nuclear Information System (INIS)

    Samarin, A.N.; Klyuev, M.M.

    1984-01-01

    Metastable structures in surface layers of samples are; investigated during force high-velocity abrasive grinding. Samples of martensitic (40Kh13), austenitic (12Kh18N10T), ferritic (05Kh23Yu5) steels and some alloys, in particular KhN77TYuR (EhI437B), were grinded for one pass at treatment depth from 0.17 up to 2.6 mm. It is established that processes of homogenizing, recrystallization and coagulation are; developed during force high-velocity grinding along with polymorphic transformations in the zone of thermomechanical effect, that leads to changes of physical and mechanical properties of the surface

  7. Ferritic steels for French LMFBR steam generators

    International Nuclear Information System (INIS)

    Aubert, M.; Mathieu, B.; Petrequin, P.

    1983-06-01

    Austenitic stainless steels have been widely used in many components of the French LMFBR. Up to now, ferritic steels have not been considered for these components, mainly due to their relatively low creep properties. Some ferritic steels are usable when the maximum temperatures in service do not exceed about 530 0 C. It is the case of the steam generators of the Phenix plant, where the exchange tubes of the evaporator are made of 2,25% Cr-1% Mo steel, stabilized or not by addition of niobium. These ferritic alloys have worked successfully since the first steam production in October 1973. For the SuperPhenix power plant, an ''all austenitic stainless alloy'' apparatus has been chosen. However, for the future, ferritic alloys offer potential for use as alternative materials in the evaporators: low alloys steels type 2,25% Cr-1% Mo (exchange tubes, tube-sheets, shells), or at higher chromium content type 9% Cr-2% Mo NbV (exchange tubes) or 12M Cr-1% Mo-V (tube-sheets). Most of these steels have already an industrial background, and are widely used in similar applications. The various potential applications of these steels are reviewed with regards to the French LMFBR steam generators, indicating that some points need an effort of clarification, for instance the properties of the heterogeneous ferritic/austenitic weldments

  8. Low cycle fatigue behavior of Sanicro25 steel at room and at elevated temperature

    Energy Technology Data Exchange (ETDEWEB)

    Polák, Jaroslav, E-mail: polak@ipm.cz [Institute of Physics of Materials, Academy of Sciences of the Czech Republic, Žižkova 22, 616 62 Brno (Czech Republic); CEITEC, Institute of Physics of Materials Academy of Sciences of the Czech Republic, Žižkova 22, Brno (Czech Republic); Petráš, Roman; Heczko, Milan; Kuběna, Ivo [Institute of Physics of Materials, Academy of Sciences of the Czech Republic, Žižkova 22, 616 62 Brno (Czech Republic); Kruml, Tomáš [Institute of Physics of Materials, Academy of Sciences of the Czech Republic, Žižkova 22, 616 62 Brno (Czech Republic); CEITEC, Institute of Physics of Materials Academy of Sciences of the Czech Republic, Žižkova 22, Brno (Czech Republic); Chai, Guocai [Sandvik Materials Technology, SE-811 81 Sandviken (Sweden); Linköping University, Engineering Materials, SE-581 83 Linköping (Sweden)

    2014-10-06

    Austenitic heat resistant Sanicro 25 steel developed for high temperature applications in power generation industry has been subjected to strain controlled low cycle fatigue tests at ambient and at elevated temperature in a wide interval of strain amplitudes. Fatigue hardening/softening curves, cyclic stress–strain curves and fatigue life curves were evaluated at room temperature and at 700 °C. The internal dislocation structures of the material at room and at elevated temperature were studied using transmission electron microscopy. High resolution surface observations and FIB cuts revealed early damage at room temperature in the form of persistent slip bands and at elevated temperature as oxidized grain boundary cracks. Dislocation arrangement study and surface observations were used to identify the cyclic slip localization and to discuss the fatigue softening/hardening behavior and the temperature dependence of the fatigue life.

  9. Development and use of data base on mechanical properties of materials in power engineering

    International Nuclear Information System (INIS)

    Popov, A.A.; Shchukina, E.G.; Karaev, A.B.

    1987-01-01

    The structure of a data base on the properties of materials used in reactor engineering is considered. The data base presents a factographic automated data retrieval system, containing test results on the 15Kh2NMFA, 15Kh2NMFA-A, 15Kh2MFA, 10GN2MFA, 22K reactor vessel steels and also the data on the A533, A508 and A304 steels taken from literature. The system is realized using the VAN6 minicomputer and operates in a dialogue mode. Software of the system is arranged by module scheme and realized using the BASIC language. Results of tensile, impact, hardness, fatigue, brittle hardness, radiation resistance, high-temperature strength and heat-resistance tests and data on the thermal properties of the alloys are introduced into the system. Prior to the input in the system the information is subjected to additional expert analysis for completeness and authenticity. The main function of the data base considered consists in the systematization of a large volume of experimental data, which envisages arbitrary retrieval and subsequent analysis using statistical methods. The system contains approximately 15 thousand records on magnetic discs. The total volume of the store is 20 M byte. The system capabilities are demonstrated when analyzing the effects of aalloying additions on mechanical properties of the 15Kh2NMFA steel

  10. Electric dipole moment in KH{sub 2}PO{sub 4} systematically modified by proton irradiation

    Energy Technology Data Exchange (ETDEWEB)

    Jin Kweon, Jung; Lee, Cheol Eui [Department of Physics and Institute for Nano Science, Korea University, Seoul 136-713 (Korea, Republic of); Noh, S. J.; Kim, H. S. [Department of Applied Physics, Dankook University, Yongin 448-701 (Korea, Republic of)

    2012-01-01

    We have carried out an impedance spectroscopy study on a series of proton-irradiated KH{sub 2}PO{sub 4} (KDP) systems. A systematic modification was observed in the transverse dipole moment of the proton-irradiated KDP systems, associated with hydrogen-ion displacements, as obtained from dielectric constant measurements by using a mean-field approximation. Besides, intercorrelation of the charge transport with the dielectric properties was revealed, both having closely to do with the hydrogen-bond modification.

  11. Precipitation in 20 Cr-25 Ni type stainless steel irradiated at low temperatures in a thermal reactor (AGR)

    International Nuclear Information System (INIS)

    Taylor, C.

    1983-01-01

    The effects of irradiation on the microstructure of AGR fuel rod cladding have been studied by analytical electron microscopy. Two alloys were investigated, the standard 20 Cr-25 Ni steel stabilised with Nb and a variant containing less Nb but strengthened with a dispersion of TiN precipitates. Irradiation at 360 deg C to 480 deg C produced (Ni, Si)-rich precipitates in both alloys; additionally the standard alloy contained (Ni, Nb, Si)-rich precipitates when irradiated at 440 deg C to 640 deg C. While similar features have been observed in other austenitic stainless steels irradiated in fast reactors, where the lattice-damage rate is greater than in a thermal reactor, their formation is not predicted by isothermal equilibrium diagrams. It is suggested here that the phases are irradiation-induced and that the total displacement damage is the controlling factor. Cladding solution-treated above 1050 deg C then irradiated at 2 -based reactor coolant occurred in cladding with low levels of cold-work at the outer surface, also resulting in Cr-rich carbide formation. (author)

  12. Bubble formation upon crystallization of high nitrogen iron base alloys

    International Nuclear Information System (INIS)

    Svyazhin, A.G.; Sivka, E.; Skuza, Z.

    2000-01-01

    A study is made into the conditions of nitrogen bubble formation during crystallization of unalloyed iron, alloys of Fe-O, Fe-O-S systems, steels 1Kh13, 0Kh18N9 and a two-phase Fe-11%Cr-1%Mo-0.2%V steel. It is revealed that the amount of bubbles in a high nitrogen steel casting increases with a degree of nitrogen supersaturation and decreases with a cooling rate growth and with a rise of surfactant concentration in the metal. In sound castings a nitrogen content can be increased due to a cooling rate growth, nitrogen dilution with inert gas, an increase of nitrogen pressure during crystallization as well as due to the introduction of such surfactants as sulphur, selenium, tellurium, tin [ru

  13. Dynamics of water around the complex structures formed between the KH domains of far upstream element binding protein and single-stranded DNA molecules

    Energy Technology Data Exchange (ETDEWEB)

    Chakraborty, Kaushik; Bandyopadhyay, Sanjoy, E-mail: sanjoy@chem.iitkgp.ernet.in [Molecular Modeling Laboratory, Department of Chemistry, Indian Institute of Technology, Kharagpur 721302 (India)

    2015-07-28

    Single-stranded DNA (ss-DNA) binding proteins specifically bind to the single-stranded regions of the DNA and protect it from premature annealing, thereby stabilizing the DNA structure. We have carried out atomistic molecular dynamics simulations of the aqueous solutions of two DNA binding K homology (KH) domains (KH3 and KH4) of the far upstream element binding protein complexed with two short ss-DNA segments. Attempts have been made to explore the influence of the formation of such complex structures on the microscopic dynamics and hydrogen bond properties of the interfacial water molecules. It is found that the water molecules involved in bridging the ss-DNA segments and the protein domains form a highly constrained thin layer with extremely retarded mobility. These water molecules play important roles in freezing the conformational oscillations of the ss-DNA oligomers and thereby forming rigid complex structures. Further, it is demonstrated that the effect of complexation on the slow long-time relaxations of hydrogen bonds at the interface is correlated with hindered motions of the surrounding water molecules. Importantly, it is observed that the highly restricted motions of the water molecules bridging the protein and the DNA components in the complexed forms originate from more frequent hydrogen bond reformations.

  14. Mechanical properties of low alloy high phosphorus weathering steel

    Directory of Open Access Journals (Sweden)

    Jena B.K.

    2015-01-01

    Full Text Available Mechanical behaviour of two low alloy steels (G11 and G12 was studied with respect to different phosphorus contents. Tensile strength and yield strength increased while percentage elongation at fracture decreased on increasing phosphorus content. The SEM and light optical photomicrograph of low phosphorus steel (G11 revealed ferrite and pearlite microstructure. On increasing phosphorus content from 0.25 wt.% to 0.42 wt.%, the morphology of grain changed from equiaxed shape to pan-cake shape and grain size also increased. The Charpy V notch (CVN impact energy of G11 and G12 steel at room temperature was 32 J and 4 J respectively and their fractographs revealed brittle rupture with cleavage facets for both the steels. However, the fractograph of G11 steel after tensile test exhibited ductile mode of fracture with conical equiaxed dimple while that of G12 steel containing 0.42 wt. % P exhibited transgranular cleavage fracture. Based on this study, G11 steel containing 0.25 wt. % P could be explored as a candidate material for weathering application purpose where the 20°C toughness requirement is 27 J as per CSN EN10025-2:2004 specification.

  15. Sàng khôn as A Theorizing Tool in Mobility Education

    Directory of Open Access Journals (Sweden)

    Ngoc Ba Doan

    2017-02-01

    Full Text Available The current virtual and physical mobility of humans, ideas, knowledge and epistemologies has major implications for education, especially in settings where English is seen as the default medium of instruction. While diversity is inherent in mobility, English-only pedagogy is a denial of the richness and potential of diverse resources learners bring with them through their mobility. This paper reports a philosophical stance and pedagogical practices employed by a lecturer in English language education at an Australian university. It argues that students’ full linguistic resources and epistemologies, known as sàng khôn, contribute to their agency and can be used as tools to theorise new knowledge in the context of their mobility education.

  16. Thermal stability of manganese-stabilized stainless steels

    International Nuclear Information System (INIS)

    Klueh, R.L.; Kenik, E.A.

    1993-01-01

    Previous work on a series of experimental high-manganese reduced-activation austenitic stainless steels demonstrated that they have improved tensile properties relative to type 316 stainless steel in both the annealed and 20% cold-worked conditions. Steels were tested with an Fe-20Mn-12Cr-0.25C (in weight percent) base composition, to which various combinations of Ti, W, V, P, and B were added. Tensile tests have now been completed on these steels after thermal aging at 600 degrees C. Thermal stability varied with composition, but the alloys were as stable or more stable than type 316 stainless steel. the strength of the annealed steels increased slightly after aging to 5000 h, while a strength decrease occurred for the cold worked steel. In both conditions, a steel containing a combination of all the alloying elements was most stable and had the best strength after thermal aging 5000 h at 600 degrees C. Despite having much higher strength than 316 stainless steel after aging, the ductility of the strongest experimental alloy was still as good as that of 316 stainless steel

  17. Removal of corrosion products of construction materials in heat carrier

    International Nuclear Information System (INIS)

    1975-01-01

    A review of reported data has been made on the removal of structural material corrosion products into the heat-carrying agent of power reactors. The corrosion rate, and at the same time, removal of corrosion products into the heat-carrying agent (water) decreases with time. Thus, for example, the corrosion rate of carbon steel in boiling water at 250 deg C and O 2 concentration of 0.1 mg/1 after 3000 hr is 0.083 g/m 2 . day; after 9000 hr the corrosion rate has been reduced 2.5 times. Under static conditions the transfer rate of corrosion products into water has been smaller than in the stream and also depends on time. The corrosion rate of carbon steel under nuclear plant operating conditions is almost an order higher over that of steel Kh18N10T

  18. Tribological properties at 25 C of seven polyimide films bonded to 440 C high-temperature stainless steel

    Science.gov (United States)

    Fusaro, R. L.

    1982-01-01

    The tribological properties of seven polyimide films applied to 440 C high temperature stainless steel substrates were studied at 25 C with a pin-on-disk type of friction and were apparatus. The polyimides fell into two groups according to friction and wear properties. Group I polyimides had slightly lower friction but much higher wear than group II polyimides. The wear mechanism was predominately adhesion, but the wear particles were larger for group I polyimides. For most of the polyimides the transfer films consisted of clumps of compacted wear particles. One polyimide composition produced a very thin transfer film that sheared plastically in the contact area.

  19. Microstructural evolution in 13Cr-8Ni-2.5Mo-2Al martensitic precipitation-hardened stainless steel

    International Nuclear Information System (INIS)

    Ping, D.H.; Ohnuma, M.; Hirakawa, Y.; Kadoya, Y.; Hono, K.

    2005-01-01

    The microstructure of 13Cr-8Ni-2.5Mo-2Al martensitic precipitation-hardened (PH) stainless steel has been investigated using transmission electron microscopy, three-dimensional atom probe and small-angle X-ray scattering. A high number density (∼10 23-25 m -3 ) of ultra-fine (1-6 nm) β-NiAl precipitates are formed during aging at 450-620 deg. C, which are spherical in shape and dispersed uniformly with perfect coherency with the matrix. As the annealing temperature increases, the size and concentration of the precipitates increase concurrently while the number density decreases. The Mo and Cr segregation to the precipitate-matrix interface has been detected and is suggested to suppress precipitate coarsening. In the sample aged for 500 h at 450 deg. C, the matrix decomposes into Cr-rich (α') and Cr-poor (α) regions. The decrease in the strength at higher temperature (above 550 deg. C) is attributed to the formation of larger carbides and reverted austenite

  20. Nickel and its alloys as perspective materials for intermediate temperature steam electrolysers operating on proton conducting solid acids as electrolyte

    DEFF Research Database (Denmark)

    Nikiforov, Aleksey; Petrushina, Irina; Jensen, Jens Oluf

    2012-01-01

    Several stainless steels, nickel-based alloys, Ta-coated stainless steel, niobium, nickel, platinum and gold were evaluated as possible materials for use in the intermediate temperature water electrolysers. The corrosion resistance was measured in molten KH2PO4 as simulated conditions corresponding...

  1. Sources of optical distortion in rapidly grown crystals of KH2PO4

    International Nuclear Information System (INIS)

    De Yoreo, J.J.; Zaitseva, N.P.; Woods, B.W.; Land, T.A.; Rek, Z.U.

    1995-01-01

    We report results of x-ray topographic and optical measurements on KH 2 PO 4 crystals grown at rates of 5 to 30mm/day. We show that optical distortion in these crystals is caused primarily by 3 sources: dislocations, differences in composition between adjacent growth sectors of the crystal, and differences in composition between adjacent sectors of vicinal growth hillocks within a single growth sector of the crystal. We find that the compositional heterogeneities cause spatial variations in the refractive index and induced distortion of the transmitted wave front while large groups of dislocations are responsible for strain induced birefringence which leads to beam depolarization

  2. Study of strength of Dsub(y)150 gate valve case, manufactured by centrifugal casting

    International Nuclear Information System (INIS)

    Umanskaya, L.G.; Semenov, P.V.; Tinyakov, V.G.; Babkina, R.I.; Khatuntsev, Eh.V.

    1982-01-01

    A process for manufacturing centrifugal-cast gate valve body is developed. Structural strength of such items, homogeneity, ductile and strength properties over the cross section as well as the metal susceptibility to embrittlement have been investigated. Three cast gate valve bodies have been taken: one - of 20GSL steel - for hydraulic testing, and two - of 15Kh1MFL steel - for investigation into the metal properties across the valve thickness. The strength properties of the centrifugal-cast gate valve body of 15Kh1M1FL steel are stated to meet the specifications. The gate valve metal ductility (delta and PSI) is twice as high as that of a sand-cast valve. The microstructure, strength and ductility are uniform both over wall thickness and over different body cross sections

  3. The Mechanical Behavior of a 25Cr Super Duplex Stainless Steel at Elevated Temperature

    Science.gov (United States)

    Lasebikan, B. A.; Akisanya, A. R.; Deans, W. F.

    2013-02-01

    Super duplex stainless steel (SDSS) is a candidate material for production tubing in oil and gas wells and subsea pipelines used to transport corrosive hydrocarbon fluids. The suitability of this material for high temperature applications is examined in this article. The uniaxial tensile properties are determined for a 25Cr SDSS over a range of temperature relevant to high pressure-high temperature oil and gas wells. It is shown that there is a significant effect of temperature on the uniaxial tensile properties. Elevated temperature was shown to reduce the Young's modulus and increase the strain hardening index; temperature effects on these two parameters are usually neglected in the design of subsea pipelines and oil well tubulars, and this could lead to wrong predictions of the collapse pressure. The manufacturing process of the super duplex tubular did not lead to significant anisotropy in the hardness and the ultimate tensile and uniaxial yield strengths.

  4. Development of x-ray computed tomographic scanner for iron and steel

    International Nuclear Information System (INIS)

    Taguchi, Isamu; Nakamura, Shigeo.

    1985-01-01

    X-ray computed tomography is extensively used in medicine, but has rarely been applied to non-medical purposes. Steel specimens pose particularly difficult problems-very poor transmission of X-rays and the need for high resolving capability. There has thus been no effective tomographic method of examining steel specimens. Due to the growing need for non-destructive, non-contact methods for observing and analyzing the internal conditions of steel microscopically, however, we have developed an X-ray Computed Tomographic Scanner for Steel (CTS) system, specifically for examination of steel specimens. Its major specifications and functions are as follows. Type: the second-generation CT, 8-channels, Scanning method: 6 0 revolution, 30-times traversing, Slice width: 0.5 mm, Resolving capability: 0.25 x 0.25 mm, X-ray source: 420 kV, 3 mA, X-ray detector: BGO scintillator, Standard specimen shape: 50 mm dia., 100 mm high, Measuring time: 10.5 min. Porosity of a stainless steel (SUS 304) bloom was examined three-dimensionally by the CTS system. Corrosion procedure of a steel slab was also examined. (author)

  5. The effect of hydrostatic pressure on the creep life of a 2.25% Cr1% Mo Steel

    International Nuclear Information System (INIS)

    Lonsdale, D.; Flewitt, P.E.J.

    1979-01-01

    The effect of superimposed hydrostatic pressures on the creep life of a 2.25% Cr 1% Mo steel, with a bainitic microstructure, is examined. Creep tests have been carried out at 923K with uniaxial stresses in the range 55 to 80 MPa and superimposed hydrostatic pressures up to 35 MPa. Optical and scanning electron microscopy have been used to evaluate the contribution of the hydrostatic stress to grain boundary cavitation. Increasing the hydrostatic pressure for a given uniaxial stress suppresses cavitation, but little changes the secondary creep rate, thereby excending the creep life. Furthermore, the time to failure depends on both the applied uniaxial stress and the hydrostatic pressure and not simply the principal stress. (orig.) [de

  6. Microstructure of laser cladded martensitic stainless steel

    CSIR Research Space (South Africa)

    Van Rooyen, C

    2006-08-01

    Full Text Available and martensite with 10% ferrite for Material B. Table 7 - Proposed martensitic stainless steel alloys for laser cladding Material C* Cr Ni Mn Si Mo Co Ms (ºC)* Cr eq Ni eq Material A 0.4 13 - 1 0.5 2.5 5.5 120 16.5 12.5 Material B 0.2 15 2 1 0.7 2.5 5.5 117... dilution, low heat input, less distortion, increased mechanical and corrosion properties excellent repeatability and control of process parameters. Solidification of laser cladded martensitic stainless steel is primarily austenitic. Microstructures...

  7. Forms of Pilgrimage at the Shrine of Khāled Nabi, Northeastern Iran

    Directory of Open Access Journals (Sweden)

    Mehdi Ebadi

    2015-07-01

    Full Text Available Pilgrimage (religious tourism is one of the fastest growing forms of tourism. Nevertheless, there is still a gap between abstract theory and empirical research about this form of tourism in the literature. This dearth of tourism studies is even more glaring in the field of Ziyārat or pilgrimage in Islam which in spite of its importance and wide extended practice have been mostly ignored in tourism and geographic literature. The present study features one such area that is (almost unknown within the community of tourism and geography researchers. In Iran, religious pilgrimage has a long tradition. Numerous sacred places with varieties of rituals and traditions, which practice among the pilgrims all around the country, indicate on its antiquity (before Islamic periods. Among the most practiced forms of religious pilgrimage are the visits to several thousands of shrines, which are known in Iran as Ziyāratgah (lit. place of visit or Imāmzādeh. One of these Ziyāratgah is the pre-Islamic shrine of Khāled Nabi (also known as Halat Nabi, which belong to a legendary Christian holy man of the 6th A.D. The shrine lies in the northeastern Iranian province of Golestan, in a region called Turkmen-Sahra. Despite its relative remote setting, every year more than 90,000 travellers do visit this shrine. This article seeks to consider varieties of pilgrimage forms at the shrine. The results of the study shows that the travelers of Khāled Nabi shrine are not homogenous and comprise of different types of visitors. In addition to secular motivations, based on the visitors’ inventives, three zones/forms of pilgrimage, namely, ‘‘religious pilgrims’’, ‘‘cultural pilgrims’’, ‘‘nostalgic pilgrims’’have been recognized.

  8. Nano-composite stainless steel

    Science.gov (United States)

    Dehoff, Ryan R.; Blue, Craig A.; Peter, William H.; Chen, Wei; Aprigliano, Louis F.

    2015-07-14

    A composite stainless steel composition is composed essentially of, in terms of wt. % ranges: 25 to 28 Cr; 11 to 13 Ni; 7 to 8 W; 3.5 to 4 Mo; 3 to 3.5 B; 2 to 2.5 Mn; 1 to 1.5 Si; 0.3 to 1.7 C; up to 2 O; balance Fe. The composition has an austenitic matrix phase and a particulate, crystalline dispersed phase.

  9. On the nature of anomalies in temperature dependence of the OKh18N1OT steel yield strength after thermal cycling in the low temperature range

    International Nuclear Information System (INIS)

    Medvedev, E.M.; Lavrent'ev, F.F.; Kurmanova, T.N.

    1978-01-01

    Investigated were structural transformations in 0Kh18N10T steel as a result of heating and cooling and of deformation within the range of temperatures between 300 and 77 K, the quantity relationships between the said transformations and the variation of the yield limit with the temperature. The studies were conducted by metallography and mechanical test methods. It was shown that an increase in the number of heating and cooling cycles correlates with a loss in strength of the steel while deformation at 77 K. This anomaly in the temperature relationship of the yield limit is related to the appearance in the course of deformation of α-martensite with a BCC lattice. Deformation at 300 K increases the amount ea of epsilon-martensite, a decrses the effectve size of grain and, in consequence, increases the yield limit. The relationship between the yield limit and the grain size at the temperature of 300 K is described adequately by the Hall-Petch equation

  10. Mechanical properties and microstructure changes of low-activation 3Cr-2W-V-Ti ferritic steels developed for nuclear applications

    International Nuclear Information System (INIS)

    Asakura, Kentaro; Kohyama, Akira; Yamada, Takemi.

    1990-01-01

    The effects of alloying elements such as Cr, W, V and Mn on tensile strength at elevated temperatures, creep-rupture properties and toughness of low activation (2.25-3)Cr-(2-2.5)W-V-Ti steels were investigated together with their microstructure change during high temperature exposure. These steels were normalized to produce bainitic structures in the same manner as that for a conventional 2.25Cr-1Mo steel. They presented superior tensile strength at elevated temperatures and creep-rupture strength in comparison with a conventional 2.25Cr-1Mo steel. The creep-rupture strength of the steels at 500degC for 100 000 h demonstrated about twice that of the conventional 2.25Cr-1Mo steel. The 3Cr-2.5W-0.2V-0.01Ti steel is recommended as a potential low activation ferritic steel for nuclear applications with well optimized mechanical properties, such as tensile strength at elevated temperatures, creep-rupture strength and toughness. The effects of alloying elements were discussed with correlating microstructural and mechanical aspects. (author)

  11. TiC reinforced cast Cr steels

    Energy Technology Data Exchange (ETDEWEB)

    Dogan, O.N.; Hawk, J.A.; Schrems, K.K.

    2006-06-01

    A new class of materials, namely TiC-reinforced cast chromium (Cr) steels, was developed for applications requiring high abrasion resistance and good fracture toughness. The research approach was to modify the carbide structure of commercial AISI 440C steel for better fracture resistance while maintaining the already high abrasion resistance. The new alloys contained 12Cr, 2.5–4.5Ti, and 1–1.5C (wt.%) and were melted in a vacuum induction furnace. Their microstructure was composed primarily of a martensitic matrix with a dispersion of TiC precipitates. Modification of TiC morphology was accomplished through changing the cooling rate during solidification. Wear rates of the TiC-reinforced Cr steels were comparable to that of AISI 440C steel, but the impact resistance was much improved.

  12. Biological Background of Kh.DIC Mice and Their Learning and Memory Defects

    Institute of Scientific and Technical Information of China (English)

    潘卫松; 邢东明; 秦川; 孙虹; 高虹; 金文; 杜力军

    2003-01-01

    The learning ability of the Kh.DIC mice, a mutant of the Kunming mice, was studied to analyze its memory development.The mice's brain function was evaluated using a water maze with the amount of monoamines measured by fluorospectrophotometry and enzyme activities detected by ultraviolet spectrophotometry.The mice were found to have spacial learning and memory defects at the age of 1 month in both ordinary animals and in special pathogen free (SPF) animals.At the same time, the amount of monoamines and the activities of monoamine oxidase-B and dopamine-β-hydroxylase differed from those of the Kunming mice.The defects might be related to the differences in the monoamine neurotransmitter system.The results suggest that the DIC mice may be useful economic animal models for the study of brain defects.

  13. Secondary recrystallisation in 20 w/o Cr-25 w/o Ni-Nb stabilised stainless steel

    International Nuclear Information System (INIS)

    Healey, T.; Brown, A.F.; Speight, M.V.

    1976-11-01

    The fuel cladding material for the Commercial Advanced Gas Reactor is a fine grain 20 w/o Cr-25 w/o Ni niobium stabilised stainless steel. The grain structure stability of this alloy has been investigated as a function of carbon content over the temperature range 930 - 990 0 C. It is demonstrated that the primary grain structure is susceptible to abnormal growth due to secondary recrystallisation of the initial fine grain structure after a composition and temperature dependent incubation period. The magnitude of the incubation period is analysed on the basis that secondary recrystallisation commences when randomly dispersed niobium carbide particles have coarsened to a critical size. The validity of the analysis is tested by comparing the predictions with experimental observation. The model is subsequently used to evaluate the incubation period for conditions of temperature, composition and microstructure which differ from those defined in the experimental studies. (author)

  14. Quality control of chemical heat treatment by the fractography method

    International Nuclear Information System (INIS)

    Tamarina, A.M.; Parygin, V.A.; Karpov, V.N.

    1978-01-01

    A fractographic investigation is carried out of fracture of a nitrided layer of 38KhMYuA steel and of cemented and cyanided layers of 12KhM3A steel. It is established that a fracture of the nitrided layer consists of three zones of crystalline facets: 1) a surface zone of fine crystalline facets located in a single plane and having the appearance of a white band (Σ-phase zone); 2) zone of acicular facets whose presence is due to the break-down of the carbonitride phase; 3) zone of large facets of boundary breakdown. The fractures of cemented and cyanided samples consist of multiple fine facets of multi-face shapes. It has been found that the depth and the microstructure of a diffusion layer in steel after chemothermal processing can be most rapidly and objectively evaluated by the fractographic method

  15. A comparison of low-chromium and high-chromium reduced-activation steels for fusion applications

    International Nuclear Information System (INIS)

    Klueh, R.L.; Maziasz, P.J.; Alexander, D.J.

    1996-01-01

    Ferritic steels have been considered candidate structural materials for first wall and blanket structures for fusion power plants since the late 1970s. The first steels considered in the United States were the conventional Cr-Mo steels Sandvik HT9 (nominally 12Cr-1Mo-0.25V-0.5W-0.5Ni-0.2C, here designated l2Cr-1MoVW), modified 9Cr-1Mo steel (9Cr-1Mo-0.2V-0.06Nb-0. IC, designated 9Cr-1MoVNb) and, to a lesser extent, 2 1/4Cr-1Mo steel (2.25Cr-Mo-0.1C). All compositions are in wt. %. The normalized-and-tempered 9 and 12Cr steels had a tempered martensite microstructure, and the normalized-and-tempered 2 1/4 Cr steel had a tempered bainite microstructure. This report describes chromium steels tested in normalized and tempered conditions. Miniature tensile and Charpy specimens were tested

  16. The History Of Muhammadiyahs Thought And Movement Study On Personality And Idea Of The Founding Figure KH. Ahmad Dahlan

    Directory of Open Access Journals (Sweden)

    Fauji Koda

    2017-08-01

    Full Text Available Muhammadiyah is one of the pioneers of religious renewal in Indonesia. As a religious reformist Muhammadiyah has contributed greatly in the development of the majority of Indonesias people are Muslims. This research is a study of the thought and movement of Muhammadiyah in Indonesia aims to conduct a study in order to understand the history and ideas of the Muhammadiyah movement focused on the personality of the founder KH. Ahmad Dahlan and the idea of social renewal Muhammadiyah movement. Study of this scientific work using qualitative paradigm with historical-phenomenological approach which examines the history and phenomenon of Muhammadiyah from aspects of personality and thoughts and ideas of KH. Ahmad Dahlan revealed in external actions words and deeds in developing Muhammadiyah in Indonesia. The results of this study indicate that the birth of Muhammadiyah in Indonesia is strongly influenced by the Islamic reform movement in the world the basic idea of thinking founder of Muhammadiyah is the unity of humanity which has implications for the doctrine to achieve welfare and peace of all mankind the idea of social reform Muahmmadiyah refers to movement Tajdid which includes purification and renewal modernization.

  17. Changes of structure and properties of cast steels GX10NiCrNb32-20 and GX10NiCrNb3-25 after long-term tempering at 600-1000 C

    International Nuclear Information System (INIS)

    Gommans, R.; Schrijen, H.; Sundermann, J.; Steinkusch, W.; Hering, W.

    2001-01-01

    Low-alloy cast steels of type GX 10NiCrNb 32.20 are commonly used for the outlet section of reformer and cracker tubes for the temperature range of 600-1000 C. There was a lack of data on the ductility of the 25%Cr alloyed cast steel GX10NiCrNb 35.25 at room temperature after tempering, which was investigated in a joint project of Pose-Marre and DSM. Mechanical tests were carried out at room temperature and at elevated temperatures. Apart from light microscopy, also SEM/EDX, SAM and TEM analyses were carried out. The 25% alloy has lower ductility than the 20% alloy, owing primarily to the more pronounced development of M 6 C carbide from primary NbC carbide, which takes up Ni and Si during tempering. The microstructure and composition of the M 6 C carbide wre not fully clarified. Information is presented on the potential application of low-carbon materials of the type GX10NiCrNb35.25 [de

  18. Stereofractographic investigation of static start and dynamic jump of a fatigue crack in pressure vessel steel

    International Nuclear Information System (INIS)

    Stepanenko, V.A.; Shtukaturova, A.S.; Yasnij, P.V.; AN Ukrainskoj SSR, Kiev. Inst. Problem Prochnosti)

    1983-01-01

    Results of investigaytion have been discussed ipto the effect of certain temperature-force factors on regularities in the formation of stretch zones during the crack initiation static and transition zones at crack jumps in the process of cyclic loading. The 15Kh2NMFA pressure vessel steel has been investigated. The steel fracture toughnesKub(Ic) has been determined testing s the specimens for excentric stretching or a bending through an angle. It has been shown that transition zones in a front of fatique cracks at the jump beginning and end are formed through the shift mechanism owing to the material separation along the maximum failure zone contour, i.e. along the plastic zone contour in a crack vertex. This is the mait difference of regularities in the formation of the transition zones during fatique crack jumps from stretching zones formed through the break-away mechanism of crack vertex bluntness during its static move. It is noted that a final conclusion on the mechanism of transition zone formation during fartique crack jumps allows one to perform systematic investigation into the plastic zone configuration in a fatique crack verteX and stereofractographic measurement of two identically conjugate jump surfaces on opposite fractures of the same samples

  19. 46 CFR 54.25-5 - Corrosion allowance.

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 2 2010-10-01 2010-10-01 false Corrosion allowance. 54.25-5 Section 54.25-5 Shipping COAST GUARD, DEPARTMENT OF HOMELAND SECURITY (CONTINUED) MARINE ENGINEERING PRESSURE VESSELS Construction With Carbon, Alloy, and Heat Treated Steels § 54.25-5 Corrosion allowance. The corrosion allowance...

  20. Influence of chromium and vanadium in the mechanical resistance of steels

    International Nuclear Information System (INIS)

    Moro, L.; Gonzalez, G.; Brizuela, G.; Juan, A.; Simonetti, S.

    2008-01-01

    Steel exposed to high temperatures and stress in a corrosive environment suffers detriment in the mechanical properties and finally embrittlement. The objective of this work is to study the mechanical properties of steels of different chemical compositions under hydrogen attack (HA). The influence of chromium and vanadium in the mechanical resistance was analyzed. The 1.25Cr1Mo0.25V and 2.25Cr1Mo ferritic steels previously hydrogenated are studied at different temperatures and loads. The temperature, electric charge density and electrolyte concentration were modified during the electrochemical charge in order to find the optimum hydrogen income to the material. The metal test conditions were characterized by scanning electron microscopy. The material remains in stationary state for a period of time and the residual damage was evaluated. The steels were subject to torsion creep tests while the temperature and the load were maintained constant along the experience. We studied the relationship between the strain rate at the secondary stage and both the stress and temperature. The stress exponent and the activation energy were also determined. A comparison with the same steel samples without hydrogen charge was also performed. The microstructural mechanics during the tests and the embrittlement degree were also discussed

  1. Effect of heat treatment and irradiation temperature on impact behavior of irradiated reduced-activation ferritic steels

    International Nuclear Information System (INIS)

    Klueh, R.L.; Alexander, D.J.

    1998-01-01

    Charpy tests were conducted on eight normalized-and-tempered reduced-activation ferritic steels irradiated in two different normalized conditions. Irradiation was conducted in the Fast Flux Test Facility at 393 C to ∼14 dpa on steels with 2.25, 5, 9, and 12% Cr (0.1% C) with varying amounts of W, V, and Ta. The different normalization treatments involved changing the cooling rate after austenitization. The faster cooling rate produced 100% bainite in the 2.25 Cr steels, compared to duplex structures of bainite and polygonal ferrite for the slower cooling rate. For both cooling rates, martensite formed in the 5 and 9% Cr steels, and martensite with ∼25% δ-ferrite formed in the 12% Cr steel. Irradiation caused an increase in the ductile-brittle transition temperature (DBTT) and a decrease in the upper-shelf energy. The difference in microstructure in the low-chromium steels due to the different heat treatments had little effect on properties. For the high-chromium martensitic steels, only the 5 Cr steel was affected by heat treatment. When the results at 393 C were compared with previous results at 365 C, all but a 5 Cr and a 9 Cr steel showed the expected decrease in the shift in DBTT with increasing temperature

  2. The development of EUROFER reduced activation steel

    Energy Technology Data Exchange (ETDEWEB)

    Schaaf, B. van der E-mail: vanderschaaf@nrg-nl.com; Tavassoli, F.; Fazio, C.; Rigal, E.; Diegele, E.; Lindau, R.; LeMarois, G

    2003-09-01

    Ferritic martensitic steels show limited swelling and susceptibility to helium effects and can be made with low activation chemical compositions. These properties make them the reference steel for the development of breeding blankets in fusion power plants. EUROFER97 is the European implementation of such a steel, where experience gained from an IEA co-operation with Japan and the US is also implemented. Results obtained so far show that EUROFER steel has attractive mechanical properties even after long ageing times. Compatibility tests in water and PbLi17 are in progress. Oxidised aluminium is the most effective protective layer in PbLi17. The displacement damage and helium formation strongly influence the hydrogen transport in the steel. Present experiments should be backed by tests in a more fusion relevant environment, e.g. IFMIF. The 2.5 dpa neutron irradiations at low temperatures result in a higher DBTT. High dose irradiations, up to 80 dpa, are underway. The early results of ODS grades with EUROFER steel composition show potential of these grades for increasing the operating temperature with 100-150 K.

  3. Effect of combined addition of N and Nb on the high temperature behavior of a 25Cr-20Ni stainless steel

    International Nuclear Information System (INIS)

    Park, In Duck; Nam, Ki Woo

    2002-01-01

    In order to clarify the effect of precipitates on creep strength at high temperature in 25Cr-20Ni stainless steels, threshold stress and void-hardening stress have been measured and compared each others. The value of threshold stress for high temperature, measured by stress abruptly loading test, is about 130 MPa. Threshold stress must be measured by the function of stress loading time in the combination hardening steel of solution hardening and precipitate hardening. Average diameter and inter-partial distance of precipitates from TEM microstructure can determine void-hardening stress. The value of void-hardening stress, evaluated by using Scattergood and Bacon's equation, was from 101 to 130 MPa. The ratio of average void hardening to threshold stress is 1.13 and both values are not equal. The result from analyzing the electron diffraction pattern shows that the dispersed precipitates in SUS310J1TB is NbCrN nitrides. Mechanism of the interaction between dislocations and precipitate particles in SUS310J1TB is Srolovitz mechanism, which is a gravitation-type interaction

  4. Corrosion resistance testing of high-boron-content stainless steels

    International Nuclear Information System (INIS)

    Petrman, I.; Safek, V.

    1994-01-01

    Boron steels, i.e. stainless steels with boron contents of 0.2 to 2.25 wt.%, are employed in nuclear engineering for the manufacture of baskets or wells in which radioactive fissile materials are stored, mostly spent nuclear fuel elements. The resistance of such steels to intergranular corrosion and uniform corrosion was examined in the Strauss solution and in boric acid; the dependence of the corrosion rate of the steels on their chemical composition was investigated, and their resistance was compared with that of AISI 304 type steel. Corrosion resistance tests in actual conditions of ''wet'' compact storage (demineralized water or a weak boric acid solution) gave evidence that boron steels undergo nearly no uniform corrosion and, as electrochemical measurements indicated, match standard corrosion-resistant steels. Corrosion resistance was confirmed to decrease slightly with increasing boron content and to increase somewhat with increasing molybdenum content. (Z.S.). 3 tabs., 4 figs., 7 refs

  5. Study of electric arc welding of castings for nuclear power machine-building

    International Nuclear Information System (INIS)

    Rymkevich, A.I.; Korsunov, P.M.

    1977-01-01

    Mechanical and corrosion-resistance properties are studied of the welded joints of cast billets from steel 00Kh12N3DL by automatic submerged arc welding. It is shown by testing the joints made with preheating up to 100 deg C and subsequent tempering (620 deg C for 25 h + 640 deg C for 16 h) that in the temperature range of 20-350 deg C they possess fairly good strength, ductility, impact viscosity, and corrosion-resistance properties approximating the corresponding characteristics of the base metal. The welding technology developed can be used to make pump casings for atomic power equipment

  6. Combating Wear of ASTM A36 Steel by Surface Modification Using Thermally Sprayed Cermet Coatings

    Directory of Open Access Journals (Sweden)

    Vineet Shibe

    2016-01-01

    Full Text Available Thermal spray coatings can be applied economically on machine parts to enhance their requisite surface properties like wear, corrosion, erosion resistance, and so forth. Detonation gun (D-Gun thermal spray coatings can be applied on the surface of carbon steels to improve their wear resistance. In the present study, alloy powder cermet coatings WC-12% Co and Cr3C2-25% NiCr have been deposited on ASTM A36 steel with D-Gun thermal spray technique. Sliding wear behavior of uncoated ASTM A36 steel and D-Gun sprayed WC-12% Co and Cr3C2-25% NiCr coatings on base material is observed on a Pin-On-Disc Wear Tester. Sliding wear performance of WC-12% Co coating is found to be better than the Cr3C2-25% NiCr coating. Wear performance of both these cermet coatings is found to be better than uncoated ASTM A36 steel. Thermally sprayed WC-12% Co and Cr3C2-25% NiCr cermet coatings using D-Gun thermal spray technique is found to be very useful in improving the sliding wear resistance of ASTM A36 steel.

  7. Experimental assessment of welded joints brittle fracture on the crack arrest criterion for WWER-1000 RPV

    International Nuclear Information System (INIS)

    Blumin, A.A.; Timofeev, B.T.

    2000-01-01

    The crack arrest fracture toughness in a vessel steel used in WWER-1000 reactor, namely in steel 15Kh2NMFA and its submerged arc welded joints, produced with Sv-08KhGNMTA, Sv-12 Kh2NMFA welding wires and NF-18 M, FZ-16 A welding fluxes, is under study. Experimental studies are carried out using three heats with the chemical composition meeting the specifications. Weld specimens 100-200 mm thick are subjected to tempering according various regimes to induce the embrittlement and simulate mechanical properties (yield strength and ductile-brittle transition temperature) corresponding to those at the end of service life under neutron radiation effect. Base metal and weld properties are compared. The wide scatter is noted for experimental data on fracture toughness temperature dependences. A possibility to use the dependence of K Ia = f (T-T k ) for determining the crack arrest fracture toughness is discussed taking in account that K Ia is a stress intensity factor calculated within the frame of static fracture mechanics [ru

  8. Use of microstructure control to toughen ferritic steels for cryogenic use. I. Fe--Ni steels

    International Nuclear Information System (INIS)

    Syn, C.K.; Jin, S.; Morris, J.W. Jr.

    1976-12-01

    Alternation of austenitization and austenite + ferrite two-phase decomposition treatment in a cyclic thermal treatment allows the achievement of ultra-fine grain size in steels containing 8-12% Ni. The grain refinement leads to a substantial improvement in cryogenic mechanical properties. The ductile-brittle transition temperature of a ferritic Fe-12Ni-0.25Ti alloy was suppressed to below liquid helium temperature by this grain refinement procedure; the transition temperature of commercial ''9Ni'' cryogenic steel was similarly reduced by combining the grain refinement with a final temper which introduces a small admixture of retained austenite

  9. Soft zone formation in dissimilar welds between two Cr-Mo steels

    International Nuclear Information System (INIS)

    Albert, S.K.; Gill, T.P.S.; Tyagi, A.K.; Mannan, S.L.; Rodriguez, P.; Kulkarni, S.D.

    1997-01-01

    Two dissimilar weldments between 9Cr-1Mo and 2.25Cr-1Mo ferritic steels have been characterized for their microstructural stability during various postweld heat treatments (PWHTs). The samples for the investigation were extracted from bead-on-plate weldments made by depositing 2.25Cr-1Mo weld metal on 9Cr-1Mo base plate and vice versa. Subsequent application of PWHT resulted in the formation of a soft zone in the low Cr ferritic steel weld or base plate. A carbide-rich hard zone, adjoining the soft zone, was also detected in the high Cr side of the weldment. Unmixed zones in the weld metal provided additional soft and hard zones in the weld metals. The migration of carbon from low-Cr steel to high-Cr steel, driven by the carbon activity gradient, has been shown to be responsible for the formation of soft and hard zones. A carbon activity diagram for 2.25Cr-1Mo/9Cr-1Mo weldments has been proposed to aid in the selection of welding consumables for reducing or preventing the soft zone formation

  10. Reduced-activation austenitic stainless steels: The Fe--Mn--Cr--C system

    International Nuclear Information System (INIS)

    Klueh, R.L.; Maziasz, P.J.

    1988-01-01

    Nickel-free manganese-stabilized steels are being developed for fusion-reactor applications. As the first part of this effort, the austenite-stable region in the Fe--Mn--Cr--C system was determined. Results indicated that the Schaeffler diagram developed for Fe--Ni--Cr--C alloys cannot be used to predict the constituents expected for high-manganese steels. This is true because manganese is not as strong an austenite stabilizer relative to δ-ferrite formation as predicted by the diagram, but it is a stronger austenite stabilizer relative to martensite than predicted. Therefore, the austenite-stable region for Ne--Mn--Cr--C alloys occurs at lower chromium and hugher combinations of manganese and carbon than predicted by the Schaeffler diagram. Development of a manganese-stabilized stainless steel should be possible in the composition range of 20 to 25% Mn, 10 to 15% Cr, and 0.01 to 0.25%C. Tensile behavior of an Fe--20%Mn--12%Cr--0.25%C alloy was determined. The strength and ductility of this possible base composition was comparable to type 316 stainless steel in both the solution-annealed and cold-worked condition

  11. Corrosion of stainless steel in alcohol solutions of the simplest carboxylic acids

    International Nuclear Information System (INIS)

    Vigdorovich, V.I.; Korneeva, T.V.; Tsygankova, L.E.

    1975-01-01

    The behaviour of stainless Kh18N10T steel is considered in the methanol and ethanol solutions of formic and acetic acids, respectively. Consideration is given to the effect of the concentration (C) of the acid (0.01-1.00 N), water (0.1-20.0 mass.%) and temperature (room temperature, 40 and 60 deg C). Curves of anodic polarization were plotted. In the course of time in 1.0 and 0.5 N anhydrous methanol solutions of HCOOH at room temperature in the absence of the external anode current one can observe an increase in the electrode potential. Continued reduction of the formic acid concentration results in an improvement on the initial potential (psi) and a practical constancy of psi in time. It is shown that depending on the acid concentration the additions of water are capable of producing both a passivating and an activating effect. It is assumed that the growth in the length of the hydrocarbon radical of carboxylic acid promotes the adsorption displacement of water and alcohols from the metal surface and enhancement of the corrosion rate

  12. Structure change in 25 Cr - 20 Ni steels as a function of their Cr, Ni, Si and W content

    International Nuclear Information System (INIS)

    Gribaudo, L.M.; Durand, F.; Durand-Charre, M.

    1983-01-01

    The influence of varying the Cr, Ni, Si and W concentrations on the type and composition of the carbides of solidification and on the phase shift temperature is studied with 18 alloys of composition close to stainless steel-25-20 (AISI 310) composition. Experimental techniques used are differential thermal analysis, microprobe and scanning electron microscope. Crystallization is interpreted with the equilibrium diagram Ni-Cr-C. The formation of the interdendritic σ phase for a chromium rich alloys is interpreted with the phase equilibrium diagram of Fe-Ni-Cr-C. Mechanical properties and corrosion resistance are dependent on the morphology of the carbides M 7 C 3 and M 23 C 6 [fr

  13. Peculiar features of determination of plastic properties in bimetals

    International Nuclear Information System (INIS)

    Voronin, A.V.; Zhadan, V.T.; Osadchij, V.A.; Rumyantsev, A.V.

    1993-01-01

    Method for calculating relative elongation of sheet bimetal on the basis of data of plastic characteristics of bimetal components has been developed. Results of calculation according to suggested method differ slightly from experimental values. It was shown analytically and supported by experiments (taking St3+12Kh18N10T samples, 45+Kh12 steel as examples), that the value of bimetal area reduction coincides with the value of area reduction of less plastic component

  14. Preliminary studies on steel slag as a substitute for coarse aggregate on concrete

    Directory of Open Access Journals (Sweden)

    Karolina Rahmi

    2017-01-01

    Full Text Available The development of science and technology in the field of construction that is rapidly increasing, is always followed by the growing community needs for infrastructure facilities, such as buildings, bridges and other construction. One of the key element in that development is concrete. Due to the rapid development of science and technology in the field of construction, it’s required a building material which has better advantage than the materials of the existing building. To obtain a better building materials, one alternative is the use of waste as aggregate in concrete mixture. In this study the authors using waste steel waste (steel slag as a substitute for coarse aggregate. Steel slag used is steel waste from PT. Growth Sumatra Industry. The gravel substitution variations is 0%, 15%, and 25% and the testing was done by the slump test, compressive strength and flexural strength of concrete. From the test results obtained optimum compressive strength variation occurs in 25% substitution of steel slag gravel amounted to 40.481 MPa, whereas for the optimum bending capacity contained in variations of 25% substitution of steel slag gravel amounted to 19.592 N / mm2. And for optimum slump value obtained on the variation of normal concrete. This shows the workability of the concrete normally higher than the other variation.

  15. Microstructure and mechanical properties of unirradiated low activation ferritic steel

    International Nuclear Information System (INIS)

    Hsu, C.Y.; Lechtenberg, T.A.

    1986-01-01

    Transmission electron micrographs of normalized and tempered 9Cr-2.5W-0.3V-0.15C low activation ferritic steel showed tempered lath-type martensite with precipitation of rod and plate-like carbides at lath and grain boundaries. X-ray diffraction analysis of the extracted replicas revealed nearly 100% M 23 C 6 carbides (a=1.064 nm), with no indication of Fe 2 W-type Laves phase even after thermal aging at 600 0 C/1000 h. Thermal aging increased the number density of rod-like M 23 C 6 along prior austenite grain boundaries and martensite lath boundaries. The elevated-temperature tensile strengths of this steel are about 10% higher than the average strengths of commercial heats of 9Cr-1Mo and modified 9Cr-1Mo steels up to 650 0 C, with equivalent uniform elongation and ∝50% decrease in total elongation. The DBTT was determined to be -25 0 C which is similar to other 9Cr-1Mo steels. Fractographic examination of tensile tested specimens shows a mixed mode of equiaxed and elongated dimples at test temperatures above 400 0 C. Modification of the Ga3X alloy composition for opimization of materials properties is discussed. However, the proposed low activation ferritic steel shows the promise of improved mechanical properties over 9Cr-1Mo steels. (orig.)

  16. National steel tries wheeling

    International Nuclear Information System (INIS)

    Dudak, J.R.

    1992-01-01

    In 1989, National Steel felt the need to take the next step to make its Detroit-based division, Great Lakes Steel, more competitive in the world flat-rolled steel market. In 1988, Great Lakes Steel started flowing natural gas through the first fully litigated bypass (Competitive Sourcing Option) of a local distribution company. In 1989, the second connection with the new supply route for gas transportation, Panhandle Eastern had started flowing and the LDC, Michigan Consolidated Gas Co. (MichCon) had pulled out their piping previously serving the plants. Since we had been able to structure a fully reliable supply route, storage and balancing program for gas in the face of such strong opposition by the LDC, the author felt it was time to attack the next singularly sourced major commodity, electricity. Electricity, at this major integrated steel plant, represented approximately 7% of plant cost yearly. Yet being monopolized, Great Lakes Division (GLD) could not multiple source this commodity like it does with its other 93% of costs, except for labor (25% of the 93%). Multiple sourcing is done to bring competitive pressure to suppliers and to diversify supplies and protect plant operation in the event of failure by one supplier. This paper describes National Steel's strategy to reduce the cost of power, at the minimum of capital costs, the most expedient way possible, that does not sacrifice any major long-term potential cost improvements. The results show that competitively priced power is available across the mid-west, at prices well below many state regulated electric utilities, for at least 5 to 15 years, but with major obstacles in obtaining transmission access

  17. Effect of room temperature prestrain on creep life of austenitic 25Cr-20Ni stainless steels

    International Nuclear Information System (INIS)

    Park, In Duck; Ahn, Seok Hwan; Nam, Ki Woo

    2004-01-01

    25Cr-20Ni series strainless steels have an excellent high temperature strength, high oxidation and high corrosion resistance. However, further improvement can be expected of creep strength by work hardening prior creep. In the present study, the effect of prestraining at room temperature on the creep behavior of a Class M(STS310S) and a Class A(STS310J1TB) alloy containing precipitates have been examined. Prestraining was carried out at room temperature and range of prestrain was 0.5∼2.5 % at STS310J1TB and 2.0∼7.0 % at STS310S. Creep behavior and creep rate of pre-strained specimens were compared with that of virgin specimens. Room temperature prestraining produced the creep life that is longer than that of a virgin specimen both for STS310J1TB and STS310S when creep test was carried out at the temperature lower than recrystallization temperature. The reason for this improvement of creep life was ascribable to the interaction between dislocations and precipitates in addition to the dislocation-dislocation interaction in STS310J1TB and the dislocation-dislocation interaction in STS310S. The beneficial effect of prestraining in STS310J1TB was larger than that of STS310S

  18. History of the formerly top secret KH-9 Hexagon spy satellite

    Science.gov (United States)

    Pressel, Phil

    2014-12-01

    This paper is about the development, design, fabrication and use of the KH-9 Hexagon spy in the sky satellite camera system that was finally declassified by the National Reconnaissance Office on September 17, 2011 twenty five years after the program ended. It was the last film based reconnaissance camera and was known by experts in the field as "the most complicated system ever put up in orbit." It provided important intelligence for the United States government and was the reason that President Nixon was able to sign the SALT treaty, and when President Reagan said "Trust but Verify" it provided the means of verification. Each satellite weighed 30,000 pounds and carried two cameras thereby permitting photographs of the entire landmass of the earth to be taken in stereo. Each camera carried up to 30 miles of film for a total of 60 miles of film. Ultra-complex mechanisms controlled the structurally "wimpy" film that traveled at speeds up to 204 inches per second at the focal plane and was perfectly synchronized to the optical image.

  19. Tensile and high cycle fatigue behaviors of high-Mn steels at 298 and 110 K

    Energy Technology Data Exchange (ETDEWEB)

    Seo, Wongyu; Jeong, Daeho; Sung, Hyokyung; Kim, Sangshik, E-mail: sang@gnu.ac.kr

    2017-02-15

    Tensile and high cycle fatigue behaviors of high-Mn austenitic steels, including 25Mn, 25Mn0.2Al, 25Mn0.5Cu, 24Mn4Cr, 22Mn3Cr and 16Mn2Al specimens, were investigated at 298 and 110 K. Depending on the alloying elements, tensile ductility of high-Mn steels either increased or decreased with decreasing temperature from 298 to 110 K. Reasonable correlation between the tendency for martensitic tranformation, the critical twinning stress and the percent change in tensile elongation suggested that tensile deformation of high-Mn steels was strongly influenced by SFE determining TRIP and TWIP effects. Tensile strength was the most important parameter in determining the resistance to high cycle fatigue of high-Mn steels with an exceptional work hardening capability at room and cryogenic temperatures. The fatigue crack nucleation mechanism in high-Mn steels did not vary with decreasing tempertature, except Cr-added specimens with grain boundary cracking at 298 K and slip band cracking at 110 K. The EBSD (electron backscatter diffraction) analyses suggested that the deformation mechanism under fatigue loading was significantly different from tensile deformation which could be affected by TRIP and TWIP effects. - Highlights: •The resistances to HCF of various high-Mn steels were measured. •The variables affecting tensile and HCF behaviors of high-Mn steels were assessed. •The relationship between tensile and the HCF behaviors of high-Mn steels was established.

  20. Mechanical properties of irradiated 9Cr-2WVTa steel

    International Nuclear Information System (INIS)

    Klueh, R.L.; Alexander, D.J.; Rieth, M.

    1998-01-01

    An Fe-9Cr-2W-0.25V-0.07Ta-0.1C (9Cr-2WVTa) steel has excellent strength and impact toughness before and after irradiation in the Fast Flux Test Facility and the High Flux Reactor (HFR). The ductile-brittle transition temperature (DBTT) increased only 32 C after 28 dpa at 365 C in FFTF, compared to a shift of ∼60 C for a 9Cr-2WV steel--the same as the 9Cr-2WVTa steel but without tantalum. This difference occurred despite the two steels having similar tensile but without tantalum. This difference occurred despite the two steels having similar tensile properties before and after irradiation. The 9Cr-2WVTa steel has a smaller prior-austenite grain size, but otherwise microstructures are similar before irradiation and show similar changes during irradiation. The irradiation behavior of the 9Cr-2WVTa steel differs from the 9Cr-2WV steel and other similar steels in two ways: (1) the shift in DBTT of the 9Cr-2WVTa steel irradiated in FFTF does not saturate with fluence by ∼28 dpa, whereas for the 9Cr-2WV steel and most similar steels, saturation occurs at <10 dpa, and (2) the shift in DBTT for 9Cr-2WVTa steel irradiated in FFTF and HFR increased with irradiation temperature, whereas it decreased for the 9Cr-2WV steel, as it does for most similar steels. The improved properties of the 9Cr-2WVTa steel and the differences with other steels were attributed to tantalum in solution

  1. Durability of bends in high-temperature steam lines under the conditions of long-term operation

    Science.gov (United States)

    Katanakha, N. A.; Semenov, A. S.; Getsov, L. B.

    2015-04-01

    The article presents the results of stress-strain state computations and durability of bent and steeply curved branches of high-temperature steam lines carried out on the basis of the finite element method using the modified Soderberg formula for describing unsteady creep processes with taking the accumulation of damage into account. The computations were carried out for bends made of steel grades that are most widely used for manufacturing steam lines (12Kh1MF, 15Kh1M1F, and 10Kh9MFB) and operating at different levels of inner pressure and temperature. The solutions obtained using the developed creep model are compared with those obtained using the models widely used in practice.

  2. Friction Welding of Titanium and Carbon Steel

    OpenAIRE

    Atsushi, HASUI; Yoichi, KIRA; Faculty of Science and Technology, Keio University; Ishikawajima-Harima Heavy Industries, Co., Ltd.

    1985-01-01

    Titanium-steel is a combination of dissimilar materials, which are difficult to weld in general, owing to inevitable formation of brittle intermetallic compounds. A prominent feature of friction welding process is ability to weld dissimilar materials in many kinds of combinations. This report deals with friction weldabilily of pure titanium and S25C steel, which are 12 mm in diameter. Main results are summarized as follows; (1) Suitable welding conditions to obtain a sound weld, which has a j...

  3. Long-term Stability of 9- to 12 % Cr Steels

    DEFF Research Database (Denmark)

    Hald, John

    2004-01-01

    In the recent 25 years creep rupture strength of 9- to 12 %Cr steels for steam pipes and turbines has been doubled by development of new alloys. This development has formed a basis for improved efficiency of fossil fired steam power plants by introduction of advanced steam temperatures...... and pressures. Newly developed steam pipe steels are based on modifications of well-established steels like the X 20CrMoV12 1. Balanced addition of V, Nb and N to a 9Cr 1 Mo steel led to the Modified 9 Cr steel P 91. Addition of 1% W to a 9Cr 1 MoVNbN base composition led to steel E 911 and partial replacement...... of Mo with 1.8 % W combined with a slight amount of Boron led to steel P 92. The creep rupture strength of these new alloys are now secured with long-term tests up to 100,000 hours, which demonstrate improvements of 50% (P 91), 75 % (E 911) and 100 % (P 92) in strength compared to X 20CrMoV12 1....

  4. Characterization on the Microstructure Evolution and Toughness of TIG Weld Metal of 25Cr2Ni2MoV Steel after Post Weld Heat Treatment

    Directory of Open Access Journals (Sweden)

    Xia Liu

    2018-03-01

    Full Text Available The microstructure and toughness of tungsten inert gas (TIG backing weld parts in low-pressure steam turbine welded rotors contribute significantly to the total toughness of the weld metal. In this study, the microstructure evolution and toughness of TIG weld metal of 25Cr2Ni2MoV steel low-pressure steam turbine welded rotor under different post-weld heat treatment (PWHT conditions are investigated. The fractography and microstructure of weld metal after PWHT are characterized by optical microscope, SEM, and TEM, respectively. The Charpy impact test is carried out to evaluate the toughness of the weld. The optical microscope and SEM results indicate that the as-welded sample is composed of granular bainite, acicular ferrite and blocky martensite/austenite (M-A constituent. After PWHT at 580 °C, the blocky M-A decomposes into ferrite and carbides. Both the number and size of precipitated carbides increase with holding time. The impact test results show that the toughness decreases dramatically after PWHT and further decreases with holding time at 580 °C. The precipitated carbides are identified as M23C6 carbides by TEM, which leads to the dramatic decrease in the toughness of TIG weld metal of 25Cr2Ni2MoV steel.

  5. HIGH TEMPERATURE TENSILE PROPERTIES OF NEW FE-CR-MN DEVELOPED STEEL

    Directory of Open Access Journals (Sweden)

    M. Mahmoudiniya

    2017-03-01

    Full Text Available Nowadays, Ni-free austenitic stainless steels are being developed rapidly and high price of nickel is one of the most important motivations for this development. At present research a new FeCrMn steel was designed and produced based on Fe-Cr-Mn-C system. Comparative studies on microstructure and high temperature mechanical properties of  new steel and AISI 316 steel were done. The results showed that new FeCrMn developed steel has single austenite phase microstructure, and its tensile strength and toughness were higher than those of 316 steel at 25, 200,350 and 500°C. In contrast with 316 steel, the new FeCrMn steel did not show strain induced transformation and dynamic strain aging phenomena during tensile tests that represented higher austenite stability of new developed steel. Lower density and higher strength of the new steel caused higher specific strength in comparison with the 316 one that can be considered as an important advantage in structural applications but in less corrosive environment

  6. Fabrication, testing and analysis of steel/composite DLS adhesive joints

    DEFF Research Database (Denmark)

    Nashim, S.; Nisar, J.; Tsouvalis, N.

    2009-01-01

    0/90 WR GFRP and 0/90 UD CFRP laminates and steel. The focus here is on CFRP/steel joint due to availability of test data. The thickness of the outer adherend varies from 3 mm to 6 mm. Shear overlaps of 25-200mm were considered. The overall objectives are (i) to assess the quality of the standard...

  7. Manufacture of tube billets for fuel cans by vacuum centrifugal casting

    International Nuclear Information System (INIS)

    Zelenskij, V.F.; Neklyudov, I.M.; Chernyj, B.P.

    1989-01-01

    Vacuum device for induction melting with centrifugal casting in the ingot mold with rotation vertical or horisontal axis is presented. Removing and grinding of nonmetallic inclusions are realized by selection of casting conditions and of chemically active reducer, sound metal with high ductility is obtained. Data on micro- and macrostructure of casted tube billets made of 08Kh18N10T and 06Kh16H15M3B stainless steels, designed for manufacture of fuel cans are presented

  8. Investigation into mechanical properties of joints of heterogeneous materials brazed with high-temperature solders

    International Nuclear Information System (INIS)

    Lomenko, V.I.; Merkushev, V.P.; Borodina, L.M.; Sycheva, T.S.; Tokhtina, O.A.; Frolov, N.N.

    1988-01-01

    Mechanical properties of copper joints with copper, 12Kh18M10T steel and KhD50 composite obtained by vacuum brazing by copper-titanium solder as compared with properties of joints brazed by PSr 72 and PMFOTsr 6-4-0.03 solders in hydrogen are studied. Dependences of joints strength on temperature of contact - reactive vacuum brazing are obtained. Possible applications of joints of dissimilar materials in electrovacuum devices subjected to the effect of dynamic loadings are established

  9. Microstructural evaluation and non-destructive examination of 2. 25 Cr--1 Mo steel. [886/sup 0/K

    Energy Technology Data Exchange (ETDEWEB)

    Van Den Avyle, J.A.; Jones, W.B.; Gieske, J.H.

    1978-07-01

    Specimens of 2.25 Cr-1 Mo steel were damaged to various levels by creep and combined creep-fatigue cycling at 886/sup 0/K (1100/sup 0/F) with hold periods. Ultrasonic shear wave velocity measurements were performed and showed small changes with large amounts of creep or fatigue damage; these changes were deemed too small for practical application. Measurements of magnetic properties were unsuccessful in following damage. Optical and transmission electron microscopy (TEM) were performed on the samples. TEM observations showed that microstructural changes which occurred at 886/sup 0/K (1100/sup 0/F) did not occur homogeneously throughout the matrix; during creep, carbide spheroidization and coarsening began in widely separated regions, with an increasing fraction of the material undergoing the process with time. A precipitate was observed to form during fatigue which did not occur during simple aging or creep.

  10. Influence of initial thermomechanical treatment on high temperature properties of laves phase strengthened ferritic steels

    International Nuclear Information System (INIS)

    Talik, Michal

    2016-01-01

    The aim of this work was to design 17 wt%Cr Laves phase strengthened HiperFer (High performance Ferrite) steels and evaluate their properties. This class of steel is supposed to be used in Advanced Ultra Super Critical power plants. Such cycles exhibit higher efficiency and are environmentally friendly, but improved materials with high resistance to reside/steam oxidation and sufficient creep strength are required. The work focused on the characterization of creep properties of 17Cr2.5W0.5Nb0.25Si heat resistant steel. Small batches of steels with nominal compositions of 17Cr3W0.5Nb0.25Si and 17Cr3W0.9Nb0.25Si were used to analyze the influence of chemical composition on the precipitation behaviour in comparison to 17Cr2.5W0.5Nb0.25Si steel. Creep strength of HiperFer steels is ensured by ne dispersion of thermodynamically stable Laves phase particles, while maintaining high corrosion resistance by a relatively high chromium content. Design of HiperFer steels was accomplished by thermodynamic modeling (Thermocalc) with the main tasks of elimination of the unwelcome brittle (Fe,Cr)-σ phase and maximization of the content of the strengthening C14 Fe_2Nb type Laves phase particles. Long term annealing experiments of all HiperFer steels were performed at 650 C in order to evaluate the role of chemical composition and initial thermo-mechanical treatment state on precipitation behaviour. Laves phase particles formed quickly after few hours and the size of precipitates did not change significantly within 1,000 hours. The observed development of Laves phase particles was compared with thermodynamical calculations (TC-Prisma). The creep properties of 17Cr2.5W0.5Nb0.25Si steel in different initial thermo-mechanical treatment states were tested at 650 C. The influence of different cold rolling procedures, and heat treatments was investigated. Increased cold rolling deformation had a positive effect resulting not only from work hardening, but from the acceleration of Laves

  11. Corrosion behavior of carbon steel in wet Na-bentonite medium

    International Nuclear Information System (INIS)

    Yeon, Jae-Won; Ha, Young-Kyoung; Choi, In-Kyu; Chun, Kwan-Sik

    1996-01-01

    Corrosion behaviors of carbon steel in wet Na-bentonite medium were studied. Corrosion rate of carbon steel in wet bentonite was measured to be 20 μm/yr at 25 deg C using the AC impedance technique. This value is agreed with that obtained by weight loss at 40 deg C for 1 year. The effect of bicarbonate ion on the corrosion of carbon steel in wet bentonite was also evaluated. The carbon steels in wet bentonite having 0.001, 0.01, and 0.1 M concentration of bicarbonate ion gave corrosion rates of 20, 8, and 0.2 μm/yr, respectively. Corrosion potentials of specimens were also measured and compared with the AC impedance results. Both results indicated that bicarbonate ion could effectively reduce the corrosion rate of carbon steels in bentonite due to the formation of protective layer on the carbon steel. (author)

  12. Experimental Study on the Utilization of Fine Steel Slag on Stabilizing High Plastic Subgrade Soil

    OpenAIRE

    Hussien Aldeeky; Omar Al Hattamleh

    2017-01-01

    The three major steel manufacturing factories in Jordan dump their byproduct, steel slag, randomly in open areas, which causes many environmental hazardous problems. This study intended to explore the effectiveness of using fine steel slag aggregate (FSSA) in improving the geotechnical properties of high plastic subgrade soil. First soil and fine steel slag mechanical and engineering properties were evaluating. Then 0%, 5%, 10%, 15%, 20%, and 25% dry weight of soil of fine steel slag (FSSA) w...

  13. High Temperature Performance Evaluation of As-serviced 25Cr35Ni Type Heat-resistant Steel Based on Stress Relaxation Tests

    Directory of Open Access Journals (Sweden)

    XU Jun

    2017-08-01

    Full Text Available Based on an as-serviced 25Cr35Ni type steel, the high temperature property evaluation using stress relaxation test(SRT method and residual life prediction were studied. The results show that creep rupture property decreases because of the formation of network carbides along grain boundaries and coarsening of secondary carbides in the austenitic matrix. Based on the relationship of stress relaxation strain rate curves obtained at different temperatures, and the extrapolation equation of stress relaxation rate-rupture time, it is capable to perform residual life evaluation by combining SRT data and a small amount of creep rupture test(CRT. Good agreement is observed for predicting results performed by current method and traditional method.

  14. Tribological and microstructural characteristics of ion-nitrided steels

    Science.gov (United States)

    Spalvins, T.

    1983-01-01

    Three steels AISI 4140, AISI 4340 and AISI 304 stainless steel were ion nitrided in a plasma consisting of a 75:25 mixture of H2:N2, sometimes with a trace of CH4. Their surface topography was characterized by SEM and two distinct compound phases were identified: the gamma and the epsilon. The core-case hardness profiles were also established. The low Cr alloy steels have an extended diffusion zone in contrast to the 3034 stainless steels which have a sharp interface. The depth of ion-nitriding is increased as the Cr content is decreased. Friction tests reveal that the gamma surface phase has a lower coefficient of friction than the epsilon phase. The lowest coefficient of friction is achieved when both the rider and the specimen surface are ion nitrided. Previously announced in STAR as N83-24635

  15. Account of internal friction when estimating recoverable creep strain

    International Nuclear Information System (INIS)

    Demidov, A.S.

    1986-01-01

    It is supposed that a difference of empirical and calculated data on the creep strain recovery for Kh18N10T steel under conditions of cyclic variations in stress is specified by the effect of internal friction. In the accepted model of creep β-flow is considered to be reversible and γ-flow- irreversible. Absorptivity is determined as a ratio of the difference between the expended work and work of strain recovery forces to the work expended in cycle. A notion of the equivalent stress acting in the period of the creep strain recovery is introduced. Results of the calculation according to the empirical formula where absorptivity was introduced into are compared with empirical data obtained for Kh18N10T steel at 750 deg C

  16. Roentgenoelectronic investigation into oxidation of iron-chromium and iron-chromium-nickel alloys

    International Nuclear Information System (INIS)

    Akimov, A.G.; Rozenfel'd, I.L.; Kazanskij, L.P.; Machavariani, G.V.

    1978-01-01

    Kinetics of iron-chromium and iron-chromium-nickel alloy oxidation (of the Kh13 and Kh18N10T steels) in oxygen was investigated using X-ray electron spectroscopy. It was found that according to X-ray electron spectra chromium oxidation kinetics in the iron-chromium alloy differs significantly from oxidation kinetics of chromium pattern. Layer by layer X-ray electron analysis showed that chromium is subjected to a deeper oxidation as compared to iron, and accordingly, Cr 2 O 3 layer with pure iron impregnations is placed between the layer of mixed oxide (Fe 3 O 4 +Cr 2 O 3 ) and metal. A model of the iron-chromium alloy surface is suggested. The mixed oxide composition on the steel surface is presented as spinel Fesub(2+x)Crsub(1-x)Osub(y)

  17. Ionic Liquids as Additives of Coffee Bean Oil in Steel-Steel Contacts

    Directory of Open Access Journals (Sweden)

    James Grace

    2015-10-01

    Full Text Available Environmental awareness and ever-growing restrictive regulations over contamination have increased the need for more environmentally-friendly lubricants. Due to their superior biodegradability and lower toxicity, vegetable oils are a good alternative to replace currently-used mineral oils. However, vegetable oils show low oxidation and thermal stability and poor anti-wear properties. Most of these drawbacks can be attenuated through the use of additives. In the last decade, ionic liquids have emerged as high-performance fluids and lubricant additives due to their unique characteristics. In this study, the tribological behavior of two phosphonium-based ionic liquids is investigated as additives of coffee bean oil in steel-steel contact. Coffee bean oil-ionic liquid blends containing 1, 2.5, and 5 wt% of each ionic liquid are studied using a block-on-flat reciprocating tribometer and the test results are compared to commercially-available, fully-formulated lubricant. Results showed that the addition of the ionic liquids to the coffee bean oil reduces wear volume of the steel disks, and wear values achieved are comparable to that obtained when the commercially-available lubricant is used.

  18. Cyclic and isothermal oxidation behavior of 2.25Cr-1Mo steel; Estudio del comportamiento del acero 2.25Cr-1Mo frente a los fenomenos de oxidacion ciclica e isoterma

    Energy Technology Data Exchange (ETDEWEB)

    Proy, M.; Utrilla, M. v.; Otero, E.

    2014-04-01

    Cyclic and isothermal oxidation of chromium-molybdenum steel 2.25Cr-1Mo were analyzed at 550 degree centigrade and 650 degree centigrade during 360 hours in air atmospheres. The cycles were performed with two stages; one of heating in furnace during 90 minutes and then the sample were cooled to 50 degree centigrade by air flow. Thermogravimetric analyses were performed to obtain high temperature corrosion kinetics. Several characterization techniques have been used to identify the corrosion mechanism, as X-Ray Diffraction (XRD), Optical Microscopy (OM) and Scanning Electron Microscopy (SEM). Thermal cycling tests can changes the corrosion mechanism, due cracks propagation in oxide scale, that witch can favors the access of oxidant agent to the substrate. (Author)

  19. Mechanical properties of steel/kenaf (hybrid) fibers added into concrete mixtures

    Science.gov (United States)

    Baarimah, A. O.; Syed Mohsin, S. M.

    2018-04-01

    This paper investigates the potential advantages of adding hybrid steel-kenaf fibers to concrete mixtures. Compression and flexural test were conducted on six concrete mixtures at 28 days to investigate the mechanical properties of the concrete. The experimental work consists of six concrete mixtures, in which the first mixture was a control mixture without adding any fiber. The following five concrete mixtures contain a total of 1% of volume fraction for steel, kenaf and a mixture of steel-kenaf (hybrid) fibers. Three ratios were considered for hybrid fibers with the ratios of 0.25/0.75, 0.5/0.5 and 0.75/0.25 for steel and kenaf fibers, respectively. From the investigation, it was observed that fibers have minimal effect on compressive strength of the concrete. However, the findings suggest promising improvement on the flexural strength of the concrete added with hybrid fiber (up to 86%) as well as manages to change the mode of failure of the beam from brittle to a more ductile manner.

  20. Prediction of long-term precipitate evolution in austenitic heat-resistant steels

    Energy Technology Data Exchange (ETDEWEB)

    Shim, Jae-Hyeok; Jung, Woo-Sang; Cho, Young Whan [Korea Institute of Science and Technology, Seoul (Korea, Republic of). Materials/Devices Div.; Kozeschnik, Ernst [Vienna Univ. of Technology (Austria). Inst. of Materials Science and Technology

    2010-07-01

    Numerical prediction of the long-term precipitate evolution in five different austenitic heat-resistant stainless steels, NF709, Super304H, Sanicro25, CF8C-PLUS and HTUPS has been carried out. MX and M{sub 23}C{sub 6} are predicted to remain as major precipitates during long-term aging in these steels. The addition of 3 wt% Cu produces very fine Cu-rich precipitates during aging in Super304H and Sanicro25. It is found that the amount of Z phase start to increase remarkably between 1,000 and 10,000 hours of aging at the expense of MX precipitates in the steels containing a high nitrogen content. However, the growth rate of Z phase is relatively slow and its average size reaches at most a few tens of nanometers after 100,000 hours of aging at 700 C, compared with 9-12% Cr ferritic/martensitic heat-resistant steels. The predicted precipitation sequence and precipitate size during aging are in general agreement with experimental observations. (orig.)

  1. Corrosion of carbon steel in neutral water

    International Nuclear Information System (INIS)

    Kawai, Noboru; Iwahori, Toru; Kurosawa, Tatsuo

    1983-01-01

    The initial corrosion behavior of materials used in the construction of heat exchanger and piping system of BWR nuclear power plants and thermal power plants have been examined in neutral water at 30, 50, 100, 160, 200, and 285 deg C with two concentrations of dissolved oxygen in the water. In air-saturated water, the corrosion rate of carbon steel was so higher than those in deaerated conditions and the maximum corrosion rate was observed at 200 deg C. The corrosion rate in deaerated water gradually increased with increasing the water temperature. Low alloy steel (2.25 Cr, 1Mo) exhibited good corrosion resistance compared with the corrosion of carbon steel under similar testing conditions. Oxide films grown on carbon steel in deaerated water at 50, 100, 160, 200, and 285 deg C for 48 and 240 hrs were attacked by dissolved oxygen in room temperature water respectively. However the oxide films formed higher than about 160 deg C showed more protective. The electrochemical behavior of carbon steel with oxide films was also similar to the effect of temperature on the stability of oxide films. (author)

  2. Carbide Precipitation in 2.25 Cr-1 Mo Bainitic Steel: Effect of Heating and Isothermal Tempering Conditions

    Science.gov (United States)

    Dépinoy, Sylvain; Toffolon-Masclet, Caroline; Urvoy, Stéphane; Roubaud, Justine; Marini, Bernard; Roch, François; Kozeschnik, Ernst; Gourgues-Lorenzon, Anne-Françoise

    2017-05-01

    The effect of the tempering heat treatment, including heating prior to the isothermal step, on carbide precipitation has been determined in a 2.25 Cr-1 Mo bainitic steel for thick-walled applications. The carbides were identified using their amount of metallic elements, morphology, nucleation sites, and diffraction patterns. The evolution of carbide phase fraction, morphology, and composition was investigated using transmission electron microscopy, X-ray diffraction, as well as thermodynamic calculations. Upon heating, retained austenite into the as-quenched material decomposes into ferrite and cementite. M7C3 carbides then nucleate at the interface between the cementite and the matrix, triggering the dissolution of cementite. M2C carbides precipitate separately within the bainitic laths during slow heating. M23C6 carbides precipitate at the interfaces (lath boundaries or prior austenite grain boundaries) and grow by attracting nearby chromium atoms, which results in the dissolution of M7C3 and, depending on the temperature, coarsening, or dissolution of M2C carbides, respectively.

  3. Evaluation of Creep Strength of Heterogeneous Welded Joint in HR6W Alloy and Sanicro 25 Steel

    Directory of Open Access Journals (Sweden)

    Zieliński A.

    2017-12-01

    Full Text Available This article presents the results of investigations on HR6W alloy and Sanicro 25 steel and the dissimilar welded joint made of them. The characteristic images of microstructure of the investigated materials in the as-received condition and following the creep test, observed with a scanning electron microscope (SEM, are shown. The X-ray analysis of phase composition of the existing precipitates was carried out. The method for evaluation of creep strength based on abridged creep tests carried out at a temperature higher than the design one is presented. The obtained results do not deviate from the values of creep strength determined in long-term creep tests. The maximum difference in creep strength of the investigated materials is ±20%, which is in compliance with the acceptable scatter band. The methodology presented can be used for verification of creep strength (life time of the material of finished components to be operated under creep conditions.

  4. Analysis of nature of brazed joints fracture under operating conditions

    International Nuclear Information System (INIS)

    Orlov, A.V.; Gura, P.M.

    1985-01-01

    Technique establishing causes leading to brazed joint fracture in pressure boundary components, operating under heavy conditions of high temperature and corrosive medium is described. Some cases of tube brazed joint fractures in a superheater of 12Kh1MF and 08Kh18N10T steels are considered. The attention is paid on using metallography for determination of mechanical or corrosion fracture properties. The diagram is developed permitting to take into account the interrelation between the fracture area in the given zone and its strength

  5. Introgression of Blast Resistance Genes (Putative Pi-b and Pi-kh) into Elite Rice Cultivar MR219 through Marker-Assisted Selection

    Science.gov (United States)

    Tanweer, Fatah A.; Rafii, Mohd Y.; Sijam, Kamaruzaman; Rahim, Harun A.; Ahmed, Fahim; Ashkani, Sadegh; Latif, Mohammad A.

    2015-01-01

    Blast is the most common biotic stress leading to the reduction of rice yield in many rice-growing areas of the world, including Malaysia. Improvement of blast resistance of rice varieties cultivated in blast endemic areas is one of the most important objectives of rice breeding programs. In this study, the marker-assisted backcrossing strategy was applied to improve the blast resistance of the most popular Malaysian rice variety MR219 by introgressing blast resistance genes from the Pongsu Seribu 2 variety. Two blast resistance genes, Pi-b and Pi-kh, were pyramided into MR219. Foreground selection coupled with stringent phenotypic selection identified 15 plants homozygous for the Pi-b and Pi-kh genes, and background selection revealed more than 95% genome recovery of MR219 in advanced blast resistant lines. Phenotypic screening against blast disease indicated that advanced homozygous blast resistant lines were strongly resistant against pathotype P7.2 in the blast disease endemic areas. The morphological, yield, grain quality, and yield-contributing characteristics were significantly similar to those of MR219. The newly developed blast resistant improved lines will retain the high adoptability of MR219 by farmers. The present results will also play an important role in sustaining the rice production of Malaysia. PMID:26734013

  6. Test Ability of Chiller Post Re-functioning at The Facility of KH-IPSB3

    International Nuclear Information System (INIS)

    Harahap, Sentot-Alibasya; M-Taufik-Arsyad; Djunaidi

    2006-01-01

    Chiller water unit (CWU) represent supplier of cool water for the system of ventilation, cooler of purification system irrigate canal (T.C) and pool (depository ponds) ex-fuel at facility of KH-IPSB3. Have been conducted by re-functioning of Chiller unit water by changing system conduct and control from electronic mode to mode of electric-mechanic and parts of damage other. A unit water chiller system have some component / appliance which way of its activity integrated one other, so that re-functioning of partial like in this time where some of component / appliance use old goods and some of using new material hence to get optimum activity at test ability of difficult chiller relative. At operation is old ones expected by optimum activity will be able to reach with an process which in phases and planed. (author)

  7. Functional characterization of a wheat NHX antiporter gene TaNHX2 that encodes a K(+/H(+ exchanger.

    Directory of Open Access Journals (Sweden)

    Yuanyuan Xu

    Full Text Available The subcellular localization of a wheat NHX antiporter, TaNHX2, was studied in Arabidopsis protoplasts, and its function was evaluated using Saccharomyces cerevisiae as a heterologous expression system. Fluorescence patterns of TaNHX2-GFP fusion protein in Arabidopsis cells indicated that TaNHX2 localized at endomembranes. TaNHX2 has significant sequence homology to NHX sodium exchangers from Arabidopsis, is abundant in roots and leaves and is induced by salt or dehydration treatments. Western blot analysis showed that TaNHX2 could be expressed in transgenic yeast cells. Expressed TaNHX2 protein suppressed the salt sensitivity of a yeast mutant strain by increasing its K(+ content when exposed to salt stress. TaNHX2 also increased the tolerance of the strain to potassium stress. However, the expression of TaNHX2 did not affect the sodium concentration in transgenic cells. Western blot analysis for tonoplast proteins indicated that the TaNHX2 protein localized at the tonoplast of transgenic yeast cells. The tonoplast vesicles from transgenic yeast cells displayed enhanced K(+/H(+ exchange activity but very little Na(+/H(+ exchange compared with controls transformed with the empty vector; Na(+/H(+ exchange was not detected with concentrations of less than 37.5 mM Na(+ in the reaction medium. Our data suggest that TaNHX2 is a endomembrane-bound protein and may primarily function as a K(+/H(+ antiporter, which is involved in cellular pH regulation and potassium nutrition under normal conditions. Under saline conditions, the protein mediates resistance to salt stress through the intracellular compartmentalization of potassium to regulate cellular pH and K(+ homeostasis.

  8. Quest for steel quality: the role of metallurgical chemistry

    Energy Technology Data Exchange (ETDEWEB)

    McLean, A. [Toronto Univ., ON (Canada). Dept. of Metallurgy and Materials Science

    2000-10-01

    Improvements in the quality of steels and the role played by metallurgical chemistry to bring about those improvements are discussed. The particular emphasis is on the chemical behaviour of solutes in molten steel and the reaction between steel, slag and refractory materials and the manner in which they influence the physical properties and performance of the steel product. As an illustration of the contribution of chemistry to steel making the case of the steel plates used in the construction of the Titanic is cited. In 1911 when the Titanic was constructed by Harland and Wolff at their Belfast shipyard, the steel plates used in the hull met all then current specifications. In 1992 when a number of steel samples recovered from the Titanic were examined, it was found that the hull of the vessel was constructed of low carbon, semi-killed steel, produced in the open-hearth process. Microstructural analysis showed extensive carbon banding, typical of hot rolled 0.2 per cent carbon steel. Also found were long manganese sulphide inclusions elongated in the rolling direction, some of which exceeded 25 mm in length. It was determined that as a consequence of these inclusions, at a seawater temperature of 0 degree C, the hull plates of the Titanic had essentially no resistance to fracture. Today's high quality steels used in applications such as Arctic pipelines, offshore platforms, icebreakers and ships for the transportation of natural gas, oxygen and sulphur concentrations are frequently less than 10 ppm. These elements have a profound influence of the quality of the final steel products by virtue of their effect of hindering the formation of inclusions. 2 refs., 3 figs.

  9. On phase equilibria in duplex stainless steels

    Energy Technology Data Exchange (ETDEWEB)

    Wessman, S. [Swerea KIMAB AB, Stockholm (Sweden); Pettersson, R. [Outokumpu Stainless AB, Avesta Research Centre, Avesta (Sweden); Hertzman, S. [Outokumpu Stainless Research Foundation, Stockholm (Sweden)

    2010-05-15

    The equilibrium conditions of four duplex stainless steels; Fe-23Cr-4.5Ni-0.1N, Fe-22Cr-5.5Ni-3Mo-0.17N, Fe-25Cr-7Ni-4Mo-0.27N and Fe-25Cr-7Ni-4Mo-1W-1.5Cu-0.27N were studied in the temperature region from 700 to 1000 C. Phase compositions were determined with SEM EDS and the phase fractions using image analysis on backscattered SEM images. The results showed that below 1000 C the steels develop an inverse duplex structure with austenite and sigma phase, of which the former is the matrix phase. With decreasing temperature, the microstructure will be more and more complex and finely dispersed. The ferrite is, for the higher alloyed steels, only stable above 1000 C and at lower temperatures disappears in favour of intermetallic phases. The major intermetallic phase is sigma phase with small amounts of chi phase, the latter primarily in high Mo and W grades. Nitrides, not a focus in this investigation, were present as rounded particles and acicular precipitates at lower temperatures. The results were compared to theoretical predictions using the TCFE5 and TCFE6 databases. (Abstract Copyright [2010], Wiley Periodicals, Inc.)

  10. Strength behaviour of 10CrMo9.10 steel in nonsteady-state applications

    International Nuclear Information System (INIS)

    Seidel, C.

    2 testing runs with cyclic temperature increase were conducted on steel 10CrMo9.10 samples, i.e., at 500 degC and cyclic increase by 10, 25 and 50 degC, and at 550 degC and cyclic increase by 50 degC. Long-term strength was studied under a strain of 6.1 to 25.6 kp/mm 2 for 22,000 hours and the effect of periodical unloading was investigated on long-term strength at 550 degC. Sample loading and unloading proceeded within the range of 8.8 to 24.7 kp/mm 2 at an unloading rate of 8 to 100 %/min. Steel lifetime was not affected by the number of cycles. The effect of the changing load and of constant temperature without load on the long-term strength of the steel at 550 degC is shown graphically. The results showed a clear dependence of steel life on dwell time at the given temperature without load. (J.P.)

  11. Sodium phthalamates as corrosion inhibitors for carbon steel in aqueous hydrochloric acid solution

    International Nuclear Information System (INIS)

    Flores, Eugenio A.; Olivares, Octavio; Likhanova, Natalya V.; Dominguez-Aguilar, Marco A.; Nava, Noel; Guzman-Lucero, Diego; Corrales, Monica

    2011-01-01

    Highlights: → N-Alkyl-sodium phthalamates as corrosion inhibitors for industry in acidic medium. → Compounds behaved as mixed type inhibitors and followed Langmuir adsorption isotherm. → Efficiencies were proportional to aliphatic chain length and inhibitor concentration. → Iron complexes and chelates with phthalamates contributed to carbon steel protection. - Abstract: Three compounds of N-alkyl-sodium phthalamates were synthesized and tested as corrosion inhibitors for carbon steel in 0.5 M aqueous hydrochloric acid. Tests showed that inhibitor efficiencies were related to aliphatic chain length and dependent on concentration. N-1-n-tetradecyl-sodium phthalamate displayed moderate efficiency against uniform corrosion, 42-86% at 25 deg. C and 25-60% at 40 o C. Tests indicated that compounds behave as mixed type inhibitors where molecular adsorption on steel followed Langmuir isotherm, whereas thermodynamic suggested that a physisorption process occurred. XPS analysis confirmed film formation on surface, where Fe +2 complexes and Fe +2 chelates with phthalamates prevented steel from further corrosion.

  12. Neutron irradiation creep in stainless steel alloys

    Energy Technology Data Exchange (ETDEWEB)

    Schuele, Wolfgang (Commission of the European Union, Institute for Advanced Materials, I-21020 Ispra (Vatican City State, Holy See) (Italy)); Hausen, Hermann (Commission of the European Union, Institute for Advanced Materials, I-21020 Ispra (Vatican City State, Holy See) (Italy))

    1994-09-01

    Irradiation creep elongations were measured in the HFR at Petten on AMCR steels, on 316 CE-reference steels, and on US-316 and US-PCA steels varying the irradiation temperature between 300 C and 500 C and the stress between 25 and 300 MPa. At the beginning of an irradiation a type of primary'' creep stage is observed for doses up to 3-5 dpa after which dose the secondary'' creep stage begins. The primary'' creep strain decreases in cold-worked steel materials with decreasing stress and decreasing irradiation temperature achieving also negative creep strains depending also on the pre-treatment of the materials. These primary'' creep strains are mainly attributed to volume changes due to the formation of radiation-induced phases, e.g. to the formation of [alpha]-ferrite below about 400 C and of carbides below about 700 C, and not to irradiation creep. The secondary'' creep stage is found for doses larger than 3 to 5 dpa and is attributed mainly to irradiation creep. The irradiation creep rate is almost independent of the irradiation temperature (Q[sub irr]=0.132 eV) and linearly dependent on the stress. The total creep elongations normalized to about 8 dpa are equal for almost every type of steel irradiated in the HFR at Petten or in ORR or in EBR II. The negative creep elongations are more pronounced in PCA- and in AMCR-steels and for this reason the total creep elongation is slightly smaller at 8 dpa for these two steels than for the other steels. ((orig.))

  13. Slag inclusions in vacuum-melted ingots of the KhN73MBTYu nickel base alloy

    International Nuclear Information System (INIS)

    Gorin, V.A.; Kleshchev, A.S.; Kazharskaya, L.P.

    1977-01-01

    Three types of slag inclusions in ingots of the vacuum-arc-remelted nickel alloy KhN73MBTYu are considered. Type 1 inclusions are those in the surface zone; type 2 inclusions are agglomerations of nitrides and oxides formed due to the fall of lining slag; type 3 inclusions consist of agglomerations of nitrides and oxides as a result of interaction of dissolved oxygen and nitrogen with melt components. The inclusions are removed by machining of the lateral surface. It should be noted that the presence of a large amount of slag on the surface of the molten pool adversely affects the stability of the electrical regime of melting. Strict adherence to the recommendations on the melting and pouring of the initial metal reduces the pollution of the consumable electrode with nonmetallic inclusions

  14. A study of enhanced diffusion during high dose high flux pulsed metal ion implantation into steel and aluminium

    International Nuclear Information System (INIS)

    Zhang Tonghe; Ji Chengzhou; Shen Jinghua; Chen Jun

    1992-01-01

    The depth profiles of metal ions implanted into steel and aluminium were measured by Rutherford backscattering (RBS). The ions of Mo, W and Y, produced by a metal vapour vacuum are ion source (MEVVA) were implanted at an energy range from 25 to 50 keV for doses of (2-5)x10 17 cm -2 into H13 steel and aluminium. Beam currents were from 0.5 to 1.0 A. The beam flux is in the range of 25 to 75 μAcm -2 . In order to simulate the profiles, a formula which includes the sputtering yield, diffusion coefficients and reaction rate was obtained. The results demonstrate that the penetration depth and retained dose increase with increasing beam flux for Mo implanted into aluminium. The peak concentration of Mo implanted H13 steel increases with increasing ion flux. In contrast to this for Y implantation into steel, the peak concentration of Y decreases with increasing ion flux. For an ion flux of 25 μAcm -2 for Mo, Y and W implantation into steel, the penetration depth and retained dose are 3-5 times greater than the theoretical values. The diffusion coefficients are about 10 -16 to 10 -15 s -1 . If the ion flux is greater than 47 μAcm -2 , the penetration depth and retained dose are 5 to 10 times greater than the theoretical values for Mo implanted aluminium. The diffusion coefficients increase with increasing ion flux for Mo implanted aluminium. The diffusion coefficients hardly change with increasing ion flux for Y and Mo implanted H13 steel. The retained dose increases 0.43 to 1.16 times for Y implanted steel for an ion flux of 25 μAcm -2 . Finally, the influence of phases precipitates, reaction rate and diffusion on retained dose, diffusion coefficient and penetration depth are discussed. (orig.)

  15. Precipitation-hardening stainless steels with a shape-memory effect

    Science.gov (United States)

    Sagaradze, V. V.; Afanasiev, S. V.; Volkova, E. G.; Zavalishin, V. A.

    2016-02-01

    The possibility of obtaining the shape-memory effect as a result of the γ → ɛ → γ transformations in aging stainless steels strengthened by VC carbides has been investigated. Regimes are given for strengthening aging (at 650 and 720°C) for stainless steels that predominantly contain (in wt %) 0.06-0.45C, 1-2V, 2-5Si, 9 and 13-14Cr. The values of reversible deformation e (amount of shape-memory effect) determined after heating to 400°C in samples preliminarily deformed to 3.5-4% vary from 0.15 to 2.7%, depending on the composition of the steels and regimes of stabilizing and destabilizing aging.

  16. Experimental investigation on temperature distribution of foamed concrete filled steel tube column under standard fire

    Science.gov (United States)

    Kado, B.; Mohammad, S.; Lee, Y. H.; Shek, P. N.; Kadir, M. A. A.

    2018-04-01

    Standard fire test was carried out on 3 hollow steel tube and 6 foamed concrete filled steel tube columns. Temperature distribution on the columns was investigated. 1500 kg/m3 and 1800 kg/m3 foamed concrete density at 15%, 20% and 25% load level are the parameters considered. The columns investigated were 2400 mm long, 139.7 mm outer diameter and 6 mm steel tube thickness. The result shows that foamed concrete filled steel tube columns has the highest fire resistance of 43 minutes at 15% load level and low critical temperature of 671 ºC at 25% load level using 1500 kg/m3 foamed concrete density. Fire resistance of foamed concrete filled column increases with lower foamed concrete strength. Foamed concrete can be used to provide more fire resistance to hollow steel column or to replace normal weight concrete in concrete filled columns. Since filling hollow steel with foamed concrete produce column with high fire resistance than unfilled hollow steel column. Therefore normal weight concrete can be substituted with foamed concrete in concrete filled column, it will reduces the self-weight of the structure because of its light weight at the same time providing the desired fire resistance.

  17. Tensile behavior of irradiated manganese-stabilized stainless steel

    Energy Technology Data Exchange (ETDEWEB)

    Klueh, R.L. [Oak Ridge National Lab., TN (United States)

    1996-10-01

    Tensile tests were conducted on seven experimental, high-manganese austenitic stainless steels after irradiation up to 44 dpa in the FFTF. An Fe-20Mn-12Cr-0.25C base composition was used, to which various combinations of Ti, W, V, B, and P were added to improve strength. Nominal amounts added were 0.1% Ti, 1% W, 0.1% V, 0.005% B, and 0.03% P. Irradiation was carried out at 420, 520, and 600{degrees}C on the steels in the solution-annealed and 20% cold-worked conditions. Tensile tests were conducted at the irradiation temperature. Results were compared with type 316 SS. Neutron irradiation hardened all of the solution-annealed steels at 420, 520, and 600{degrees}C, as measured by the increase in yield stress and ultimate tensile strength. The steel to which all five elements were added to the base composition showed the least amount of hardening. It also showed a smaller loss of ductility (uniform and total elongation) than the other steels. The total and uniform elongations of this steel after irradiation at 420{degrees}C was over four times that of the other manganese-stabilized steels and 316 SS. There was much less difference in strength and ductility at the two higher irradiation temperatures, where there was considerably less hardening, and thus, less loss of ductility. In the cold-worked condition, hardening occured only after irradiation at 420{degrees}C, and there was much less difference in the properties of the steels after irradiation. At the 420{degrees}C irradiation temperature, most of the manganese-stabilized steels maintained more ductility than the 316 SS. After irradiation at 420{degrees}C, the temperature of maximum hardening, the steel to which all five of the elements were added had the best uniform elongation.

  18. Neutron irradiation effects on the ductile-brittle transition of ferritic/martensitic steels

    Energy Technology Data Exchange (ETDEWEB)

    Klueh, R.L.; Alexander, D.J. [Oak Ridge National Lab., TN (United States)

    1997-08-01

    Ferritic/martensitic steels such as the conventional 9Cr-1MoVNb (Fe-9Cr-1Mo-0.25V-0.06Nb-0.1C) and 12Cr-1MoVW (Fe-12Cr-1Mo-0.25V-0.5W-0.5Ni-0.2C) steels have been considered potential structural materials for future fusion power plants. The major obstacle to their use is embrittlement caused by neutron irradiation. Observations on this irradiation embrittlement is reviewed. Below 425-450{degrees}C, neutron irradiation hardens the steels. Hardening reduces ductility, but the major effect is an increase in the ductile-brittle transition temperature (DBTT) and a decrease in the upper-shelf energy, as measured by a Charpy impact test. After irradiation, DBTT values can increase to well above room temperature, thus increasing the chances of brittle rather than ductile fracture.

  19. Development of Next Generation Heating System for Scale Free Steel Reheating

    Energy Technology Data Exchange (ETDEWEB)

    Dr. Arvind C. Thekdi

    2011-01-27

    The work carried out under this project includes development and design of components, controls, and economic modeling tools that would enable the steel industry to reduce energy intensity through reduction of scale formation during the steel reheating process. Application of scale free reheating offers savings in energy used for production of steel that is lost as scale, and increase in product yield for the global steel industry. The technology can be applied to a new furnace application as well as retrofit design for conversion of existing steel reheating furnaces. The development work has resulted in the knowledge base that will enable the steel industry and steel forging industry us to reheat steel with 75% to 95% reduction in scale formation and associated energy savings during the reheating process. Scale reduction also results in additional energy savings associated with higher yield from reheat furnaces. Energy used for steel production ranges from 9 MM Btu/ton to 16.6 MM Btu/ton or the industry average of approximately 13 MM Btu/ton. Hence, reduction in scale at reheating stage would represent a substantial energy reduction for the steel industry. Potential energy savings for the US steel industry could be in excess of 25 Trillion Btu/year when the technology is applied to all reheating processes. The development work has resulted in new design of reheating process and the required burners and control systems that would allow use of this technology for steel reheating in steel as well as steel forging industries.

  20. Surface Nb-ALLOYING on 0.4C-13Cr Stainless Steel: Microstructure and Tribological Behavior

    Science.gov (United States)

    Yu, Shengwang; You, Kai; Liu, Xiaozhen; Zhang, Yihui; Wang, Zhenxia; Liu, Xiaoping

    2016-02-01

    0.4C-13Cr stainless steel was alloyed with niobium using double glow plasma surface alloying and tribological properties of Nb-alloyed steel such as hardness, friction and wear were measured. Effects of the alloying temperature on microstructure and the tribological behavior of the alloyed steel were investigated compared with untreated steel. Formation mechanisms of Nb-alloyed layers and increased wear resistance were also studied. The result shows that after surface Nb-alloying treatment, the 0.4C-13Cr steel exhibits a diffusion adhesion at the alloyed layer/substrate interface and improved tribological property. The friction coefficient of Nb-alloyed steel is decreased by about 0.3-0.45 and the wear rate after Nb-alloying is only 2-5% of untreated steel.

  1. Inhibition performance of a gemini surfactant and its co-adsorption effect with halides on mild steel in 0.25 M H{sub 2}SO{sub 4} solution

    Energy Technology Data Exchange (ETDEWEB)

    Wang Xiumei [State Key Laboratory for Corrosion and Protection, Institute of Metal Research Chinese Academy of Sciences, Shenyang 110016 (China); School of Materials Science and Engineering, Shenyang Jianzhu University, Shenyang 110168 (China); Yang Huaiyu, E-mail: hyyang@imr.ac.cn [State Key Laboratory for Corrosion and Protection, Institute of Metal Research Chinese Academy of Sciences, Shenyang 110016 (China); Wang Fuhui [State Key Laboratory for Corrosion and Protection, Institute of Metal Research Chinese Academy of Sciences, Shenyang 110016 (China)

    2012-02-15

    Highlights: Black-Right-Pointing-Pointer 1,4-Bis (1-chlorobenzyl-benzimidazolyl)-butane has good inhibition effect for mild steel in H{sub 2}SO{sub 4}. Black-Right-Pointing-Pointer The compound acts as a mixed-type inhibitor and obeys Langmuir adsorption isotherm. Black-Right-Pointing-Pointer Halide ions can improve the inhibition property of compound via the co-adsorption effect. Black-Right-Pointing-Pointer The adsorbed halides play an important intermediate bridge role in co-adsorption process. Black-Right-Pointing-Pointer The obtained results can supply the bases for the future using of cationic inhibitor. - Abstract: The inhibition performance of a cationic gemini-surfactant (CBB) and its co-adsorption behavior with halides on mild steel in 0.25 M H{sub 2}SO{sub 4} solution was studied by weight loss and electrochemical techniques. Results showed that the compound could effectively inhibit the mild steel corrosion and acted as a mixed-type inhibitor by suppressing simultaneously anodic and cathodic reactions. Addition of the halides improve the inhibition efficiency of CBB and the synergistic effect increase in the order of I{sup -} > Br{sup -} > Cl{sup -}, revealing that halides radii and their electronegativity may play significant roles in co-adsorption with the cationic inhibitor.

  2. Account of low temperature hardening in calculation of permissible stresses

    International Nuclear Information System (INIS)

    Novikov, N.V.; Ul'yanenko, A.P.; Gorodyskij, N.I.

    1980-01-01

    Suggested is a calculation scheme of permissible stresses with the account of temperature hardening for steels and alloys, the dependences of strength, plasticity and rupture work of which on cooling temperature do not have threshold changes in a wide range of low temperatures (from 300 to 4.2 K). Application of the suggested scheme is considered on the example of 12Kh18N10T austenitic chromium-nickel steel

  3. Preparation of porous diatomite-templated carbons with large adsorption capacity and mesoporous zeolite K-H as a byproduct.

    Science.gov (United States)

    Liu, Dong; Yuan, Weiwei; Deng, Liangliang; Yu, Wenbin; Sun, Hongjuan; Yuan, Peng

    2014-06-15

    In this study, KOH activation was performed to enhance the porosity of the diatomite-templated carbon and to increase its adsorption capacity of methylene blue (MB). In addition to serving as the activation agent, KOH was also used as the etchant to remove the diatomite templates. Zeolite K-H was synthesized as a byproduct via utilization of the resultant silicon- and potassium-containing solutions created from the KOH etching of the diatomite templates. The obtained diatomite-based carbons were composed of macroporous carbon pillars and tubes, which were derived from the replication of the diatomite templates and were well preserved after KOH activation. The abundant micropores in the walls of the carbon pillars and tubes were derived from the break and reconfiguration of carbon films during both the removal of the diatomite templates and KOH activation. Compared with the original diatomite-templated carbons and CO2-activated carbons, the KOH-activated carbons had much higher specific surface areas (988 m(2)/g) and pore volumes (0.675 cm(3)/g). Moreover, the KOH-activated carbons possessed larger MB adsorption capacity (the maximum Langmuir adsorption capacity: 645.2 mg/g) than those of the original carbons and CO2-activated carbons. These results showed that KOH activation was a high effective activation method. The zeolite K-H byproduct was obtained by utilizing the silicon- and potassium-containing solution as the silicon and potassium sources. The zeolite exhibited a stick-like morphology and possessed nanosized particles with a mesopore-predominant porous structure which was observed by TEM for the first time. Copyright © 2014 Elsevier Inc. All rights reserved.

  4. Creep and microstructural processes in a low-alloy 2.25%Cr1.6%W steel (ASTM Grade 23)

    Czech Academy of Sciences Publication Activity Database

    Kuchařová, Květa; Sklenička, Václav; Kvapilová, Marie; Svoboda, Milan

    2015-01-01

    Roč. 109, NOV (2015), s. 1-8 ISSN 1044-5803 R&D Projects: GA TA ČR TA02010260; GA MŠk(CZ) ED1.1.00/02.0068 Institutional support: RVO:68081723 Keywords : Bainitic steel * Low-alloy steel * Creep strength * Microstructural changes * Carbide precipitation Subject RIV: JG - Metallurgy Impact factor: 2.383, year: 2015

  5. High temperature corrosion behavior of different grain size specimens of 2.25 Cr-1 Mo steel in SO2+O2 environment

    International Nuclear Information System (INIS)

    Ghosh, D.; Mitra, S.K.

    2011-01-01

    The investigation is primarily aimed at the high temperature corrosion behavior of different grain sizes of 2.25 Cr-1 Mo steel at SO 2 +O 2 (mixed oxidation and sulfidation). The various grain sizes (18 μm,26 μm, 48 μm, and 72 μm) are obtained by different annealing treatment. Isothermal corrosion studies are carried out in different grain size specimens at 973K for 8 hours. The corrosion growth rate and the reaction kinetics are studied by weight gain method. The external scales of the post corroded specimen are studied in Scanning Electron Microscope (SEM) to examine the corrosion products morphology on the scale. X-ray mapping analysis of the different elements (Fe, O, Cr and S) is carried out by Energy Dispersive Spectroscopy (EDS) attached with SEM. The X-ray Diffraction Analysis (XRD) is also carried out to identify the corrosion products in the external scale. Finally, it is concluded that that the corrosion rate of 2.25 Cr-1 Mo steel strongly depend on grain sizes of the specimens. The corrosion rate increases with the decreases of grain size. The finer grain (18 μm) show higher corrosion rate than the coarse grains (72 μm). The weight gain kinetics follows the parabolic growth rate which further indicates that the corrosion process is diffusion controlled. The scale analysis shows the thicker scale and extensive scale cracking and spallations in case of finer grain size specimen (18 μm), whereas the coarse grain specimen (72 μm) shows compact and adherent layer. The XRD analysis shows that the corrosion products consist of mixtures of iron oxides( Fe 3 O 4 and Fe 2 O 3 ) and iron sulfides (FeS). The details mechanism of the corrosion is discussed to explain the difference in corrosion rate for different grain sizes. (author)

  6. Draft genome sequence of Bacillus okhensis Kh10-101T, a halo-alkali tolerant bacterium from Indian saltpan

    Directory of Open Access Journals (Sweden)

    Pilla Sankara Krishna

    2015-12-01

    Full Text Available We report the 4.86-Mb draft genome sequence of Bacillus okhensis strain Kh10-101T, a halo-alkali tolerant rod shaped bacterium isolated from a salt pan near port of Okha, India. This bacterium is a potential model to study the molecular response of bacteria to salt as well as alkaline stress, as it thrives under both high salt and high pH conditions. The draft genome consist of 4,865,284 bp with 38.2% G + C, 4952 predicted CDS, 157 tRNAs and 8 rRNAs. Sequence was deposited at DDBJ/EMBL/GenBank under the project accession JRJU00000000.

  7. Heat treatment effects on structure and proerties of the alloy type KhN73MBNYu (EhJ 698)

    International Nuclear Information System (INIS)

    Maslenkov, S.B.; Maslenkova, E.A.; Solov'ev, Yu.V.; Zryumov, V.P.

    1994-01-01

    Influence of quenching temperature and various ageing conditions on tensile properties and impact strength of wrought alloy type KhN73MBTYu has been investigated at room temperature and in the range of 500-850 deg C. Two-step quenching followed by ageing at 700-750 deg C. Two-step quenching followed by ageing at 700-750 deg C is shown to assure needed heat resistance of the alloy. Due to the whole complex of structural changes during heat treatments mechanical properties of the alloy preserv high level up to 750 deg C. This temperature is limiting value in the case of long-term operation

  8. Microbial-Influenced Corrosion of Corten Steel Compared with Carbon Steel and Stainless Steel in Oily Wastewater by Pseudomonas aeruginosa

    Science.gov (United States)

    Mansouri, Hamidreza; Alavi, Seyed Abolhasan; Fotovat, Meysam

    2015-07-01

    The microbial corrosion behavior of three important steels (carbon steel, stainless steel, and Corten steel) was investigated in semi petroleum medium. This work was done in modified nutrient broth (2 g nutrient broth in 1 L oily wastewater) in the presence of Pseudomonas aeruginosa and mixed culture (as a biotic media) and an abiotic medium for 2 weeks. The behavior of corrosion was analyzed by spectrophotometric and electrochemical methods and at the end was confirmed by scanning electron microscopy. The results show that the degree of corrosion of Corten steel in mixed culture, unlike carbon steel and stainless steel, is less than P. aeruginosa inoculated medium because some bacteria affect Corten steel less than other steels. According to the experiments, carbon steel had less resistance than Corten steel and stainless steel. Furthermore, biofilm inhibits separated particles of those steels to spread to the medium; in other words, particles get trapped between biofilm and steel.

  9. Improved swelling resistance for PCA austenitic stainless steel under HFIR irradiation through microstructural control

    International Nuclear Information System (INIS)

    Maziasz, P.J.; Braski, D.N.

    1984-01-01

    Swelling evaluation of PCA variants and 20%-cold-worked (N-Lot) type 316 stainless steel (CW 316) at 300 to 600 0 C was extended to 44 dpa. Swelling was negligible in all the steels at 300 0 C after approx. 44 dpa. At 500 to 600 0 C 25%-cold-worked PCA showed better void swelling resistance than type 316 at approx. 44 dpa. There was less swelling variation among alloys at 400 0 C, but again 25%-cold-worked PCA was the best

  10. Testing of advanced chromium - iron based steel

    International Nuclear Information System (INIS)

    Simeg Veternikova, J.; Degmova, J.; Sabelova, V.; Sojak, S.; Petriska, M.; Slugen, V.; Simko, F.; Pekarcikova, M.

    2015-01-01

    Research and Development of advanced nuclear reactors in Generation IV (GEN IV) are limited by the selection of proper construction materials. Suitable candidate materials are still under extensive investigation, because their properties must be excellent to achieve high level of reactor system safety. NF 709 (Fe-20Cr-25Ni) is new austenitic steel with improved properties in compare to AISI steels; therefore it is also one of candidate materials. Our study is focused on investigation of radiation resistance as well as thermal stability of this steel - NF 709. New austenitic steel NF 709, candidate materials for construction of Generation IV reactors, was observed in term of its stability after an exposure to very high temperature and irradiation. The change of microstructure was observed by positron annihilation techniques which demonstrated the growth of vacancy defects from di-vacancies in as-received material to three-vacancies in material after the thermal and implantation treatments; although the total change of structure was very small. Thus, NF 709 showed good resistance to tested strains and according to our preliminary results. Therefore, this material could be used for high temperature applications and interchangeable components of Generation IV reactors. (authors)

  11. Aircraft Steels

    Science.gov (United States)

    2009-02-19

    component usage. PH 13-8Mo is a precipitation-hardenable martensitic stainless steel combining excellent corrosion resistance with strength. Custom 465 is...a martensitic , age-hardenable stainless steel capable of about 1,724 MPa (250 ksi) UTS when peak-aged (H900 condition). Especially, this steel can...NOTES 14. ABSTRACT Five high strength steels (4340, 300M, AerMet 100, Ferrium S53, and Hy-Tuf) and four stainless steels (High Nitrogen, 13

  12. Steel making

    CERN Document Server

    Chakrabarti, A K

    2014-01-01

    "Steel Making" is designed to give students a strong grounding in the theory and state-of-the-art practice of production of steels. This book is primarily focused to meet the needs of undergraduate metallurgical students and candidates for associate membership examinations of professional bodies (AMIIM, AMIE). Besides, for all engineering professionals working in steel plants who need to understand the basic principles of steel making, the text provides a sound introduction to the subject.Beginning with a brief introduction to the historical perspective and current status of steel making together with the reasons for obsolescence of Bessemer converter and open hearth processes, the book moves on to: elaborate the physiochemical principles involved in steel making; explain the operational principles and practices of the modern processes of primary steel making (LD converter, Q-BOP process, and electric furnace process); provide a summary of the developments in secondary refining of steels; discuss principles a...

  13. New method for NPP sodium coolant pipeline austenization

    International Nuclear Information System (INIS)

    Malashonok, V.A.; Rotshtejn, A.V.; Gotshalk, A.L.; Miryushchenko, E.F.

    1980-01-01

    Heat treatment technology is considered for pipelines intended for the NPP cooling systems employing sodium coolant. Various techniques are discussed which are used for protecting the pipeline internal surfaces against oxidation in the process of heat treatment. It is noted that the austenite formation of welded joints of steel 12Kh18N9 and steel Kh16N11M3 at temperatures of 1050 and 1100 deg C releases welding-induced stresses and reduces a possibility of local damages. Evacuation down to 1 mm Hg appears to be the most rational protective technique. The considered procedure of the pipeline heat treatment has been utilized for mounting the equipment of the BN-600 reactor at the Beloyarskaya NPP. The economic gain resulting from the use of the procedure, owing to decrease in argon consumption and reduction of labour input, makes up 150 000 roubles

  14. Alloys influence in ferritic steels with hydrogen attack

    International Nuclear Information System (INIS)

    Moro, L; Rey Saravia, D; Lombardich, J; Saggio, M; Juan, A; Blanco, J

    2003-01-01

    Materials exposed to a corrosive environment and high temperatures, are associated with a decrease of their mechanical properties and embitterment.At room temperatures atomic hydrogen diffuses easily through metals structure, it accumulates in lattice defects forming molecular hydrogen and generating cracking due to internal stresses.Under high temperatures the phenomenon is more complex.The steels in these conditions present different structures of precipitates, that the change under creep conditions period.In this work it is determined the influence of Cr and V alloys, the changes of ferritic steel resistance in a corrosive environment and high temperatures.1.25 Cr 1 Mo 0.25 V and 2.25Cr 1 Mo under different loads and temperatures previously attacked by hydrogen environment.The hydrogen is induced by the electrolytic technique, optimizing the choice of temperatures, current density, electrolyte, etc. In order to control an adequate cathode charge, a follow up procedure is carried out by electronic barrier microscopy.After the attack, the material is settled at room temperatures for certain period of time, to allow the hydrogen to leave and evaluate the residual damage.Creep by torsion assays, under constant load and temperature is used as an experimental technique.With the outcome data curves are drawn in order to study the secondary creep rate, with the applied load and temperature, determining the value of stress exponent n and the activation energy Q.Comparing to equal assays to the same ferritic steels but non attacked by hydrogen, these values allows the prediction of microstructure changes present during these tests

  15. The Microstructure Evolution of Dual-Phase Pipeline Steel with Plastic Deformation at Different Strain Rates

    Science.gov (United States)

    Ji, L. K.; Xu, T.; Zhang, J. M.; Wang, H. T.; Tong, M. X.; Zhu, R. H.; Zhou, G. S.

    2017-07-01

    Tensile properties of the high-deformability dual-phase ferrite-bainite X70 pipeline steel have been investigated at room temperature under the strain rates of 2.5 × 10-5, 1.25 × 10-4, 2.5 × 10-3, and 1.25 × 10-2 s-1. The microstructures at different amount of plastic deformation were examined by using scanning and transmission electron microscopy. Generally, the ductility of typical body-centered cubic steels is reduced when its stain rate increases. However, we observed a different ductility dependence on strain rates in the dual-phase X70 pipeline steel. The uniform elongation (UEL%) and elongation to fracture (EL%) at the strain rate of 2.5 × 10-3 s-1 increase about 54 and 74%, respectively, compared to those at 2.5 × 10-5 s-1. The UEL% and EL% reach to their maximum at the strain rate of 2.5 × 10-3 s-1. This phenomenon was explained by the observed grain structures and dislocation configurations. Whether or not the ductility can be enhanced with increasing strain rates depends on the competition between the homogenization of plastic deformation among the microconstituents (ultra-fine ferrite grains, relatively coarse ferrite grains as well as bainite) and the progress of cracks formed as a consequence of localized inconsistent plastic deformation.

  16. Wrought Cr--W--V bainitic/ferritic steel compositions

    Science.gov (United States)

    Klueh, Ronald L.; Maziasz, Philip J.; Sikka, Vinod Kumar; Santella, Michael L.; Babu, Sudarsanam Suresh; Jawad, Maan H.

    2006-07-11

    A high-strength, high-toughness steel alloy includes, generally, about 2.5% to about 4% chromium, about 1.5% to about 3.5% tungsten, about 0.1% to about 0.5% vanadium, and about 0.05% to 0.25% carbon with the balance iron, wherein the percentages are by total weight of the composition, wherein the alloy is heated to an austenitizing temperature and then cooled to produce an austenite transformation product.

  17. Surface deformation effects on stainless steel, Ni, Cu and Mo produced by medium energy He ions irradiation

    International Nuclear Information System (INIS)

    Constantinescu, B.; Florescu, V.; Sarbu, C.

    1993-01-01

    To investigate dose and energy dependence of surface deformation effects (blistering and flaking), different kinds of candidate CTR first wall materials as 12KH18N10T, W-4541, W-4016 and SS-304 stainless steels, Ni, Cu, Mo were irradiated at room temperature with 3.0, 4.7 and 6.8 MeV He + ions at IAP Cyclotron. The effects were investigated by means of a TEMSCAN 200 CX electron microscope and two metallographic Orthoplan Pol Leitz and Olympus microscopes. We observed two dose dependent main phenomena: blistering and flaking (craters). So, blisters occurrence on the irradiated surface is almost instantaneous when a critical dose (number of He ions accumulated in the region at the end of alpha particles range) is reached. Increasing irradiation dose, we reached flaking stage. So, isolated submicronic fissures along grain boundaries were observed on the blister skin, chronologically followed by large (5-20 μm) deep cracks of hundreds of microns in length, blisters opening and, finally, flaking appearance. (author) 8 figs., 1 tab

  18. Corrosion behavior of steels in liquid lead bismuth with low oxygen concentrations

    Science.gov (United States)

    Kurata, Yuji; Futakawa, Masatoshi; Saito, Shigeru

    2008-02-01

    Corrosion tests in pots were conducted to elucidate corrosion behavior of various steels in liquid lead-bismuth for 3000 h under the condition of an oxygen concentration of 5 × 10 -8 wt% at 450 °C and an oxygen concentration of 3 × 10 -9 wt% at 550 °C, respectively. Significant corrosion was not observed at 450 °C for ferritic/martensitic steels, F82H, Mod.9Cr-1Mo steel, 410SS, 430SS except 2.25Cr-1Mo steel. Pb-Bi penetration into steels and dissolution of elements into Pb-Bi were severe at 550 °C even for ferritic/martensitic steels. Typical dissolution attack occurred for pure iron both at 550 °C without surface Fe 3O 4 and at 450 °C with a thin Fe 3O 4 film. Ferritization due to dissolution of Ni and Cr, and Pb-Bi penetration were recognized for austenitic stainless steels, 316SS and 14Cr-16Ni-2Mo steel at both temperatures of 450 °C and 550 °C. The phenomena were mitigated for 18Cr-20Ni-5Si steel. In some cases oxide films could not be a corrosion barrier in liquid lead-bismuth.

  19. Effect of microstructure on the sulphide stress cracking susceptibility of a high strength pipeline steel

    Energy Technology Data Exchange (ETDEWEB)

    Ramirez, E. [Centro de Investigacion en Ingenieria y Ciencias Aplicadas-UAEM, Av. Universidad 1001, 62209-Cuernavaca, Mor. (Mexico); Gonzalez-Rodriguez, J.G. [Centro de Investigacion en Ingenieria y Ciencias Aplicadas-UAEM, Av. Universidad 1001, 62209-Cuernavaca, Mor. (Mexico)], E-mail: ggonzalez@uaem.mx; Torres-Islas, A.; Serna, S. [Centro de Investigacion en Ingenieria y Ciencias Aplicadas-UAEM, Av. Universidad 1001, 62209-Cuernavaca, Mor. (Mexico); Campillo, B. [Intituto de Ciencias Fisicas-Facultad de Quimicas-Universidad Nacional Autonoma de Mexico Cuernavaca, Mor. (Mexico); Dominguez-Patino, G. [Centro de Investigacion en Ingenieria y Ciencias Aplicadas-UAEM, Av. Universidad 1001, 62209-Cuernavaca, Mor. (Mexico); Juarez-Islas, J.A. [Instituto de Investigaciones en Materiales-Universidad Nacional Autonoma de Mexico, Circuito Exterior S/N, Cd. Universitaria, C.P. 04510, Mexico, D.F. (Mexico)

    2008-12-15

    The sulphide stress cracking (SSC) susceptibility of a newly developed high strength microalloyed steel with three different microstructures has been evaluated using the slow strain rate testing (SSRT) technique. Studies were complemented with potentiodynamic polarization curves and hydrogen permeation measurements. Material included a C-Mn steel having Ni, Cu, and Mo as main microalloying elements with three microstructures: martensitic, ferritic and ferritic + bainitic. Testing temperatures included 25, 50, 70 and 90 deg. C. Detailed SEM observations of the microstructure and fracture surfaces were done to identify possible degradation mechanisms. The results showed that in all cases, the corrosion rate, number of hydrogen atoms at the surface and the percentage reduction in area increased with temperature. The steel with a martensitic microstructure had the highest SSC susceptibility at all temperatures, whereas the ferritic steels were susceptible only at 25 deg. C, and the most likely mechanism is hydrogen embrittlement assisted by anodic dissolution.

  20. Ni-Flash-Coated Galvannealed Steel Sheet with Improved Properties

    Science.gov (United States)

    Pradhan, D.; Dutta, M.; Venugopalan, T.

    2016-11-01

    In the last several years, automobile industries have increasingly focused on galvannealed (GA) steel sheet due to their superior properties such as weldability, paintability and corrosion protection. To improve the properties further, different coatings on GA have been reported. In this context, an electroplating process (flash coating) of bright and adherent Ni plating was developed on GA steel sheet for covering the GA defects and enhancing the performances such as weldability, frictional behavior, corrosion resistance and phosphatability. For better illustration, a comparative study with bare GA steel sheet has also been carried out. The maximum electroplating current density of 700 A/m2 yielded higher cathode current efficiency of 95-98%. The performances showed that Ni-coated (coating time 5-7 s) GA steel sheet has better spot weldability, lower dynamic coefficient of friction (0.07 in lubrication) and three times more corrosion resistance compared to bare GA steel sheet. Plate-like crystal of phosphate coating with size of 10-25 µm was obtained on the Ni-coated GA. The main phase in the phosphate compound was identified as hopeite (63.4 wt.%) along with other phases such as spencerite (28.3 wt.%) and phosphophyllite (8.3 wt.%).

  1. Effect of intercritical heat treatment on mechanical properties of reinforcing steel bars

    International Nuclear Information System (INIS)

    Abro, M.I.; Memon, R.A.; Soomro, I.A.; Aftab, U.

    2017-01-01

    Intercritical heat treatments attempts were made to enhance the mechanical properties of reinforcing steel bars milled from scrap metal. For this, two grades of steel bars were obtained from different steel mills and their mechanical properties that include hardness, ultimate tensile strength, and percent elongation before and after intercritical heat treatment were determined. Results indicated that 25.5 and 17.6%, improvements in UTS (Ultimate Tensile Strength) and 18.8 and 14.3% improvement in percent elongation in two grades of reinforcing steel samples containing 0.17 and 0.24% carbon respectively was achieved while heating at 750 degree C for 2h. Appreciable improvement in the mechanical properties was noted due to birth of sufficient quantity of martensite along with ferrite. (author)

  2. Porous stainless steel for biomedical applications

    Directory of Open Access Journals (Sweden)

    Sabrina de Fátima Ferreira Mariotto

    2011-01-01

    Full Text Available Porous 316L austenitic stainless steel was synthesized by powder metallurgy with relative density of 0.50 and 0.30 using 15 and 30 wt. (% respectively of ammonium carbonate and ammonium bicarbonate as foaming agents. The powders were mixed in a planetary ball mill at 60 rpm for 10 minutes. The samples were uniaxially pressed at 287 MPa and subsequently vacuum heat treated in two stages, the first one at 200 ºC for 5 hours to decompose the carbonate and the second one at 1150 ºC for 2 hours to sinter the steel. The sintered samples had a close porous structure and a multimodal pore size distribution that varied with the foaming agent and its concentration. The samples obtained by addition of 30 wt. (% of foaming agents had a more homogeneous porous structure than that obtained with 15 wt. (%. The MTT cytotoxicity test (3-[4,5-dimethylthiazol]-2,5-diphenyltetrazolium bromide was used to evaluate the mitochondrial activity of L929 cells with samples for periods of 24, 48, and 72 hours. The cytotoxicity test showed that the steel foams were not toxic to fibroblast culture. The sample with the best cellular growth, therefore the most suitable for biomedical applications among those studied in this work, was produced with 30 wt. (% ammonium carbonate. In this sample, cell development was observed after 48 hours of incubation, and there was adhesion and spreading on the material after 72 hours. Electrochemical experiments using a chloride-containing medium were performed on steel foams and compared to massive steel. The massive steel had a better corrosion performance than the foams as the porosity contributes to increase the surface area exposed to the corrosive medium.

  3. Peculiar features in formation of diffusion layer properties during nitridation

    International Nuclear Information System (INIS)

    Gulyaev, A.P.; Konoval'tsev, V.I.; Nikitin, V.V.

    1983-01-01

    Peculiarities of the formation of multiphase nitridated layer at samples of commercial iron, 20, 40Kh and 38KhMYu6A steels are studied with the help of high-temperature methods of investigation (X-ray diffraction analysis, hardening and thickness measuring). It is found out that during the saturation the solid solution oversaturated with nitrogen is formed; some increase in hardness in the process is a result of solid solution hardening and the increase of thickness of nitride zone; however the main growth of the layer hardness is achieved during the cooling as a result of α phase precipitating hardening

  4. Gas Furnace with Pulsed Feeding of the Heating Agent for Volume Precision Heat Treatment of CCM Rolls

    Science.gov (United States)

    Moroz, V. I.; Egorova, V. M.; Gusev, S. V.

    2001-05-01

    A standard chamber batch furnace of the Severstal' plant has been modified for precision heat treatment of CCM rolls. The certification tests of a charge of rolls from steel 24KhM1F have shown the technical and economical advantages of the new design.

  5. Liquid steel analysis by laser-induced plasma spectroscopy

    International Nuclear Information System (INIS)

    Gruber, J.

    2002-11-01

    When a nanosecond pulsed laser is focused onto a sample and the intensity exceeds a certain threshold, material is vaporized and a plasma is formed above the sample surface. The laser-light becomes increasingly absorbed by inverse bremsstrahlung and by photo-excitation and photo-ionization of atoms and molecules. The positive feedback, by which the number of energetic electrons for ionization is increased in an avalanche-like manner under the influence of laser-light, is the so-called optical breakdown. Radiating excited atoms and ions within the expanding plasma plume produce a characteristic optical emission spectrum. A spectroscopic analysis of this optical emission of the laser-induced plasma permits a qualitative and quantitative chemical analysis of the investigated sample. This technique is therefore often called laser-induced plasma spectroscopy (LIPS) or laser-induced breakdown spectroscopy (LIBS). LIPS is a fast non-contact technique, by which solid, liquid or gaseous samples can be analyzed with respect to their chemical composition. Hence, it is an appropriate tool for the rapid in-situ analysis of not easily accessible surfaces for process control in industrial environments. In this work, LIPS was studied as a technique to determine the chemical composition of solid and liquid steel. A LIPS set-up was designed and built for the remote and continuous in-situ analysis of the steel melt. Calibration curves were prepared for the LIPS analysis of Cr, Mn, Ni and Cu in solid steel using reference samples with known composition. In laboratory experiments an induction furnace was used to melt steel samples in crucibles, which were placed at a working distance of 1.5 m away from the LIPS apparatus. The response of the LIPS system was monitored on-line during the addition of pure elements to the liquid steel bath within certain concentration ranges (Cr: 0.11 - 13.8 wt%, Cu: 0.044 - 0.54 wt%, Mn: 1.38 - 2.5 wt%, Ni: 0.049 - 5.92 wt%). The analysis of an element

  6. On the inhibition of mild steel corrosion by 4-amino-5-phenyl-4H-1, 2, 4-trizole-3-thiol

    International Nuclear Information System (INIS)

    Musa, Ahmed Y.; Kadhum, Abdul Amir H.; Mohamad, Abu Bakar; Takriff, Mohd Sobri; Daud, Abdul Razak; Kamarudin, Siti Kartom

    2010-01-01

    The corrosion inhibition of mild steel in a 2.5 M H 2 SO 4 solution by 4-amino-5-phenyl-4H-1, 2, 4-trizole-3-thiol (APTT) was studied at different temperatures, utilising open circuit potential, potentiodynamic and impedance measurements. The results indicate that APTT performed as an excellent mixed-type inhibitor for mild steel corrosion in a 2.5 M H 2 SO 4 solution and that the inhibition efficiencies increased with the inhibitor concentration but decreased proportionally with temperature. The kinetic and thermodynamic parameters for adsorption of APTT on the mild steel surface were calculated. A chemisorption mechanism of APTT molecules on the mild steel surface was proposed based on the thermodynamic adsorption parameters.

  7. Theoretical study of [Li(H2O)n]+ and [K(H2O)n]+ (n = 1-4) complexes

    International Nuclear Information System (INIS)

    Wojcik, M.J.; Mains, G.J.; Devlin, J.P.

    1995-01-01

    The geometries, successive binding energies, vibrational frequencies, and infrared intensities are calculated for the [Li(H 2 O) n ] + and [K(H 2 O) n ] + (n = 1-4) complexes. The basis sets used are 6-31G * and LANL1DZ (Los Alamos ECP+DZ) at the SCF and MP2 levels. There is an agreement for calculated structures and frequencies between the MP2/6-31G * and MP2/LANL1DZ basis sets, which indicates that the latter can be used for calculations of water complexes with heavier ions. Our results are in a reasonable agreement with available experimental data and facilitate experimental study of these complexes. 19 refs., 4 figs., 6 tabs

  8. Low cycle fatigue of 2.25Cr1Mo steel with tensile and compressed hold loading at elevated temperature

    Energy Technology Data Exchange (ETDEWEB)

    Zhang, Junfeng; Yu, Dunji; Zhao, Zizhen; Zhang, Zhe; Chen, Gang; Chen, Xu, E-mail: xchen@tju.edu.cn

    2016-06-14

    A series of uniaxial strain-controlled fatigue and creep-fatigue tests of the bainitic 2.25Cr1Mo steel forging were performed at 455 °C in air. Three different hold periods (30 s, 120 s, 300 s) were employed at maximum tensile strain and compressive strain under fully reversed strain cycling. Both tensile and compressive holds significantly reduce the fatigue life. Fatigue life with tensile hold is shorter than that with compressive hold. A close relationship is found between the reduction of fatigue life and the amount of stress relaxation. Microstructural examination by scanning electron microscope reveals that strain hold introduces more crack sources, which can be probably ascribed to the intensified oxidation and the peeling-off of oxide layers. A modified plastic strain energy approach considering stress relaxation effect is proposed to predict the creep-fatigue life, and the predicted lives are in superior agreement with the experimental results.

  9. Quaternary (liquid + liquid) equilibria of aqueous two-phase polyethylene glycol, poly-N-vinylcaprolactam, and KH{sub 2}PO{sub 4}: Experimental and the generalized Flory-Huggins theory

    Energy Technology Data Exchange (ETDEWEB)

    Foroutan, Masumeh [Department of Physical Chemistry, Faculty of Chemistry, College of Science, University of Tehran, Enghelab Ave., Tehran 14155-6455 (Iran, Islamic Republic of)], E-mail: foroutan@khayam.ut.ac.ir; Zarrabi, Mona [Department of Physical Chemistry, Faculty of Chemistry, College of Science, University of Tehran, Enghelab Ave., Tehran 14155-6455 (Iran, Islamic Republic of)

    2008-06-15

    A quaternary (liquid + liquid) equilibrium study was performed to focus attention on the interaction parameters between poly-N-vinylcaprolactam (PVCL) and poly-ethylene glycol (PEG) as well as between other species. At first, the new experimental data of (liquid + liquid) equilibria for aqueous two-phase systems containing PEG, KH{sub 2}PO{sub 4}, and PVCL at T = 303.15 K have been determined. Then the Flory-Huggins theory with two electrostatic terms (the Debye-Huckel and the Pitzer-Debye-Huckel equations) has been generalized to correlate the phase behavior of the quaternary system. Good agreement has been found between experimental and calculated data from both models especially from the Pitzer-Debye-Huckel equation. Also an effort was done to compare the effect of temperature as well as addition of PVCL on the binodal curves of PEG, KH{sub 2}PO{sub 4}, and water. The effect of the type of salt on the binodals has been also studied, and the salting out power of the salts has been determined.

  10. Relationship of bainitic microstructure to impact toughness in Cr-Mo and Cr-W steels

    International Nuclear Information System (INIS)

    Klueh, R.L.; Alexander, D.J.

    1992-01-01

    Non-classical bainite microstructures can develop during continuous cooling of low-carbon alloy steels. These differ from classical upper and lower bainite developed by isothermal transformation. Two non-classical bainite microstructures were produced in a 3Cr-1.5Mo0.25V-0.lC steel using different cooling rates after austenitizing--water quenching and air cooling. The carbide-free acicular bainite formed in the quenched steel had a lower ductile-brittle transition temperature (DBTT) than the granular bainite formed in the air-cooled steel. With increasing tempering parameter (defined bv tempering time and temperature), the DBTT of both decreased and approached a common value, although the final value occurred at a much lower tempering parameter for the quenched steel than for the air-cooled steel. The upper-shelf enery was similarly affected by microstructure. These observations along with similar observations in two Cr-W steels indicate that control of the bainite microstructure can be used to optimize strength and toughness

  11. Influence of continuous electron irradiation and different modes of mechanic-thermal treatment on structure-phase composition of alloys 36NKhTYu and 40KhNYu

    International Nuclear Information System (INIS)

    Alontseva, D.L.; Suslov, S.E.; Kupchishin, A.I.; Plotnikov, S.V.; Petrov, V.A.

    2002-01-01

    Principal regularities of structure formation in strongly deformed alloys 36NKhTYu and 40KhNYu under aging in certain temperature range and after electron irradiation are revealed. Morphological features of precipitating phases with purpose of development of methods for getting of optimal structural states providing essential properties rate were determined. Data of electron microscopic examinations of structure-phase composition are compared with data on mechanical properties

  12. The effect of strain rate and temperature on the elevated temperature tensile flow behavior of service-exposed 2.25Cr-1Mo steel

    International Nuclear Information System (INIS)

    Girish Shastry, C.; Parameswaran, P.; Mathew, M.D.; Bhanu Sankara Rao, K.; Mannan, S.L.

    2007-01-01

    The elevated temperature tensile flow behavior of service-exposed 2.25Cr-1Mo steel has been critically examined with respect to strain rate sensitivity (m) and apparent activation energy (Q) for tensile deformation. The predominant role of forest dislocations in determining the relative flow response at true plastic strains greater than 0.01 is inferred from the profile of 'm' against flow stress. The variation of 'm' with temperature and strain is discussed based on the kinetics of dislocation generation and recovery. The decrease in Q with the increase in strain rate or temperature is attributed to the increase in recovery processes like dislocation annihilation and subcell/subgrain formation. This suggestion has been supported by transmission electron microscopy

  13. The Khôra of the commons. The role of civil society in two productive landscapes of Llobregat River

    Directory of Open Access Journals (Sweden)

    Javier Rocamonde Lourido

    2018-03-01

    Full Text Available The starting point of this article is The Khôra of the commons metaphor. First of all, we’ll discuss the role of civil society in the design and preservation of two productive landscapes linked to the Llobregat River. In addition, we will analyse the relationship between agents and landscape that follows dynamics dependent of social, economic and urban context. We will compare two case studies in order to better understand those phenomena (Infanta canal and Can Batlló factory. In conclusion this paper synthetizes several periods common to both case studies that explain the changing relationship between actors and landscape.

  14. Interfacial interactions between some La-based perovskite thick films and ferritic steel substrate with regard to the operating conditions of SOFC

    International Nuclear Information System (INIS)

    Przybylski, K.; Brylewski, T.; Morgiel, J.

    2004-01-01

    An overview is presented on the oxidation kinetics, electrical properties and microstructure investigations of the oxide products formed on Fe-25 wt.-%Cr steel uncoated and coated with electrical conducting films of (La,Ca)CrO 3 or (La,Sr)CoO 3 in air and H 2 /H 2 O gas mixture at 1023-1173 K for up to 480 hrs with regard to their application as the SOFC metallic interconnect. The application of the Fe-25Cr steel in SOFC operating at 1073 K requires its surface modification to improve the electrical conductivity of chromia scale forming on the uncoated steel surface. The thick films of (La,Ca)CrO 3 and (La,Sr)CoO 3 with the thickness range of 20-100 μm, coated on the Fe-25Cr steel by screen-printing method helped solve this problem. TEM-SAD, SEM-EDS and impedance spectroscopy investigations have shown significant influence of the multilayer products formation at the substrate steel/coating films interfacial zone on the electrical properties of the metallic interconnect. (orig.)

  15. Microbial electrocatalysis with Geobacter sulfurreducens biofilm on stainless steel cathodes

    OpenAIRE

    Dumas, Claire; Basséguy, Régine; Bergel, Alain

    2008-01-01

    Stainless steel and graphite electrodes were individually addressed and polarized at−0.60V vs. Ag/AgCl in reactors filled with a growth medium that contained 25mM fumarate as the electron acceptor and no electron donor, in order to force the microbial cells to use the electrode as electron source. When the reactor was inoculated with Geobacter sulfurreducens, the current increased and stabilized at average values around 0.75Am−2 for graphite and 20.5Am−2 for stainless steel. Cyclic voltamm...

  16. Development oxide dispersion strengthened ferritic steels for fusion

    Energy Technology Data Exchange (ETDEWEB)

    Mukhopadhyay, D.K.; Froes, F.H.; Gelles, D.S. [Pacific Northwest National Lab., Richland, WA (United States)

    1997-04-01

    Uniaxial tension creep response is reported for an oxide dispersion strengthened (ODS) steel, Fe-13.5Cr-2W-0.5Ti-0.25 Y{sub 2}O{sub 3} (in weight percent) manufactured using the mechanical alloying process. Acceptable creep response is obtained at 900{degrees}C.

  17. Super-Hydrophobic Green Corrosion Inhibitor On Carbon Steel

    Science.gov (United States)

    Hassan, H.; Ismail, A.; Ahmad, S.; Soon, C. F.

    2017-06-01

    There are many examples of organic coatings used for corrosion protection. In particular, hydrophobic and super-hydrophobic coatings are shown to give good protection because of their enhanced ability to slow down transport of water and ions through the coating. The purpose of this research is to develop water repellent coating to avoid direct contact between metal and environment corrosive and mitigate corrosion attack at pipeline system. This water repellent characteristic on super-hydrophobic coating was coated by electrodeposition method. Wettability of carbon steel with super-hydrophobic coating (cerium chloride and myristic acid) and oxidized surface was investigated through contact angle and inhibitor performance test. The inhibitor performance was studied in 25% tannin acid corrosion test at 30°C and 3.5% sodium chloride (NaCl). The water contact angle test was determined by placing a 4-μL water droplet of distilled water. It shows that the wettability of contact angle super-hydrophobic with an angle of 151.60° at zero minute can be classified as super-hydrophobic characteristic. By added tannin acid as inhibitor the corrosion protection on carbon steel becomes more consistent. This reveals that the ability of the coating to withstand with the corrosion attack in the seawater at different period of immersions. The results elucidate that the weight loss increased as the time of exposure increased. However, the corrosion rates for uncoated carbon steel is high compared to coated carbon steel. As a conclusion, from both samples it can be seen that the coated carbon steel has less corrosion rated compared to uncoated carbon steel and addition of inhibitor to the seawater provides more protection to resist corrosion attack on carbon steel.

  18. Elevated-Temperature Ferritic and Martensitic Steels and Their Application to Future Nuclear Reactors

    Energy Technology Data Exchange (ETDEWEB)

    Klueh, RL

    2005-01-31

    In the 1970s, high-chromium (9-12% Cr) ferritic/martensitic steels became candidates for elevated-temperature applications in the core of fast reactors. Steels developed for conventional power plants, such as Sandvik HT9, a nominally Fe-12Cr-1Mo-0.5W-0.5Ni-0.25V-0.2C steel (composition in wt %), were considered in the United States, Europe, and Japan. Now, a new generation of fission reactors is in the planning stage, and ferritic, bainitic, and martensitic steels are again candidates for in-core and out-of-core applications. Since the 1970s, advances have been made in developing steels with 2-12% Cr for conventional power plants that are significant improvements over steels originally considered. This paper will review the development of the new steels to illustrate the advantages they offer for the new reactor concepts. Elevated-temperature mechanical properties will be emphasized. Effects of alloying additions on long-time thermal exposure with and without stress (creep) will be examined. Information on neutron radiation effects will be discussed as it applies to ferritic and martensitic steels.

  19. Stiff, light, strong and ductile: nano-structured High Modulus Steel.

    Science.gov (United States)

    Springer, H; Baron, C; Szczepaniak, A; Uhlenwinkel, V; Raabe, D

    2017-06-05

    Structural material development for lightweight applications aims at improving the key parameters strength, stiffness and ductility at low density, but these properties are typically mutually exclusive. Here we present how we overcome this trade-off with a new class of nano-structured steel - TiB 2 composites synthesised in-situ via bulk metallurgical spray-forming. Owing to the nano-sized dispersion of the TiB 2 particles of extreme stiffness and low density - obtained by the in-situ formation with rapid solidification kinetics - the new material has the mechanical performance of advanced high strength steels, and a 25% higher stiffness/density ratio than any of the currently used high strength steels, aluminium, magnesium and titanium alloys. This renders this High Modulus Steel the first density-reduced, high stiffness, high strength and yet ductile material which can be produced on an industrial scale. Also ideally suited for 3D printing technology, this material addresses all key requirements for high performance and cost effective lightweight design.

  20. The role of duplex stainless steels for downhole tubulars

    International Nuclear Information System (INIS)

    Francis, R.

    1993-01-01

    In sour conditions there is an increasing trend to turn to corrosion resistant alloys for downhole tubulars. The most commonly used CRA tubular is 13Cr, and there are thousands of feet in service. However, there are limits to the use of 13Cr, ie., the risk of sulphide stress corrosion cracking at high H 2 S levels, and the possibility of pitting or high corrosion rates in waters with high chloride contents. Where the service conditions are felt to be too severe for 13Cr alloys it has been traditional to switch to nickel base alloys such as alloys 825 and C-276 (UNS N08825 and N10276). The alloys are much more expensive than 13Cr, and in recent years the duplex stainless steels have been selected as alloys with superior corrosion and SSCC resistance compared with 13Cr, and having lower cost than nickel alloys. Originally the 22Cr duplex alloy (UNS 31803) was used, but more recently the 25Cr super duplex alloys (UNS S32760 and S32750) have become more available. The present paper reviews the data available for 13Cr and the limits of applicability. Data is also presented for laboratory tests for both the 22Cr and 25Cr super duplex alloys. There is extensive service experience with both 22Cr and 25Cr super duplex in the North Sea, covering both downhole tubulars, manifold and post wellhead equipment. Data is presented showing some of the sour condition being experienced in the North Sea by super duplex alloys. These results show that there is a substantial gap between the limits of use for 13Cr and the 25Cr super duplex stainless steel alloys. This means that in many sour environments super duplex stainless steel provides a cost effective alternative to nickel-base alloys

  1. Identification of electron and hole traps in KH2PO4 crystals

    International Nuclear Information System (INIS)

    Garces, N. Y.; Stevens, K. T.; Halliburton, L. E.; Demos, S. G.; Radousky, H. B.; Zaitseva, N. P.

    2001-01-01

    Electron paramagnetic resonance (EPR) has been used to characterize a hole trap and several electron traps in single crystals of potassium dihydrogen phosphate (KH 2 PO 4 or KDP). The paramagnetic charge states of these centers are produced by ionizing radiation (e.g., x rays or a 266 nm beam from a pulsed Nd:YAG laser) and are stable for days and even weeks at room temperature. One center consists of a hole trapped on an oxygen ion adjacent to a silicon impurity located on a phosphorus site. This defect has a small, but easily observed, hyperfine interaction with the adjacent substitutional proton. The other centers are formed when an electron is trapped at an oxygen vacancy. These latter defects are best described as (PO 3 ) 2- molecular ions, where the primary phosphorus nucleus is responsible for a large hyperfine splitting (500--800 G in magnitude). Five EPR spectra representing variations of these oxygen vacancy centers are observed, with the differences being attributed to the relative position of a nearby cation vacancy, either a missing proton or potassium. An angular study of the EPR spectra, conducted at room temperature, provided principal values and principal directions for the g matrices and hyperfine matrices for the hole center and two of the electron centers

  2. Ductile fracture of two-phase welds under 77K

    International Nuclear Information System (INIS)

    Yushchenko, K.A.; Voronin, S.A.; Pustovit, A.I.; Shavel', A.V.

    1984-01-01

    The effect of the type of welding and fillers on crack resistance of welded joints high-strength steel EhP810 and its various compounds with steels EhP666, 08Kh18N10T has been studied. For the welding of steel EhP810 with steels EhP810, EhP666, 08Kh18N10T electron-beam, automatic, argon tungsten arc with non-consumable electrode with various fillers, as well as argon metal-arc welding with consumable electrode, were used. It is shown, that for a joint, made by electron-beam welding, parameters σsub(u), Ksub(IcJ), KCV are higher than for a joint of a similar phase structure made using filler wire EhP659-VI. It is explained by the fact, that during electron-beam welding joint metal refining takes place, which removes gases. In welded joints of chP810 steel, having joints with austenitic structure, characteristic of crack resistance Ssub(c) increases by more than 0.2 mm in contrast to two-phase joints, which conventional yield strength at 77 K exceeds 1000 MPa. It is worth mentioning, that for other classes of steels formation of two-phase structure of joint increases welded joint resistance to brittle fracture. It is possible to obtain the required structure of joint with assigned level of resistance to brittle fracture by means of the use of different fillers, optimum and welding procedure, regulaing the part of the basic metal in joint content

  3. Study of corrosion resistance properties of nitrided carbon steel using radiofrequency N{sub 2}/H{sub 2} cold plasma process

    Energy Technology Data Exchange (ETDEWEB)

    Bouanis, F.Z. [Unite Materiaux et Transformations (UMET), Ingenierie des Systemes Polymeres, CNRS UMR 8207, ENSCL, BP 90108, F-59652 Villeneuve d' Ascq Cedex (France); Jama, C., E-mail: charafeddine.jama@ensc-lille.f [Unite Materiaux et Transformations (UMET), Ingenierie des Systemes Polymeres, CNRS UMR 8207, ENSCL, BP 90108, F-59652 Villeneuve d' Ascq Cedex (France); Traisnel, M. [Unite Materiaux et Transformations (UMET), Ingenierie des Systemes Polymeres, CNRS UMR 8207, ENSCL, BP 90108, F-59652 Villeneuve d' Ascq Cedex (France); Bentiss, F. [Laboratoire de Chimie de Coordination et d' Analytique, Faculte des Sciences, Universite Chouaib Doukkali, B.P. 20, M-24000 El Jadida (Morocco)

    2010-10-15

    C38 carbon steel have been plasma-nitrided using a radiofrequency cold plasma discharge treatment in order to investigate the influence of gas composition on corrosion behaviour of nitrided substrates. The investigated C38 steel was nitrided by a RF plasma discharge treatment using two different gas mixtures (75% N{sub 2}/25% H{sub 2} and 25% N{sub 2}/75% H{sub 2}) at different times of plasma-treatment on non-heated substrates. Electron Probe Microanalysis (EPMA) showed that the nitrided layer formed using 75% N{sub 2}/25% H{sub 2} gas mixture was thicker compared to those formed in the case of 25% N{sub 2}/75% H{sub 2} or pure N{sub 2}. The modifications of the corrosion resistance characteristics of plasma-nitrided C38 steel in 1 M HCl solution were investigated by weight loss measurements and ac impedance technique. The results obtained from these two evaluation methods were in good agreement. It was shown that the nitriding treatment in both cases (75% N{sub 2}/25% H{sub 2} and 25% N{sub 2}/75% H{sub 2}) improves the corrosion resistance of investigated carbon steel, while the better performance is obtained for the 75% N{sub 2}/25% H{sub 2} gas mixture. X-ray photoelectron spectroscopy (XPS) was carried out before and after immersion in corrosive medium in order to establish the mechanism of corrosion inhibition using N{sub 2}/H{sub 2} cold plasma nitriding process.

  4. Analysis of elevated temperature flow and work hardening behaviour of service-exposed 2.25Cr-1Mo steel using Voce equation

    International Nuclear Information System (INIS)

    Girish Shastry, C.; Mathew, M.D.; Bhanu Sankara Rao, K.; Mannan, S.L.

    2004-01-01

    The Voce equation was used to model the tensile flow and work-hardening behaviour of a service-exposed 2.25Cr-1Mo steel. The applicability of Voce parameters obtained from the fit to experimental true stress-true strain datasets for estimating the validity of the fit was examined. The Voce equation was found to model the stress-strain curve closely. The Voce parameter n v was correlated to the underlying dislocation activities. It was found that the values of Voce parameters at various temperatures and strain rates can be used to infer the operating recovery mechanism during stage III hardening. A low absolute value of n v is indicative of recovery by cross-slip, whereas the high temperature transition to climb or sub-boundary migration driven recovery is accompanied by an increase in the value of n v

  5. Long-Term Aging Diagnosis of Rotor Steel Using Acoustic Nonlinearity

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Chung Seok; Jhang, Kyung Young [Hanyang University, Seoul (Korea, Republic of); Park, Ik Keun; Hyun, Chang Yong [Seoul National University of Science and Tecnology, Seoul (Korea, Republic of)

    2011-12-15

    The long-term aging of ferritic 2.25CrMo steel was characterized using the acoustic nonlinear effect in order to apply to diagnose the degradation behavior of structural materials. We measured the acoustic nonlinearity parameter for each thermally aged specimen by the higher harmonic-generation technique. The acoustic nonlinearity parameter increased with aging time due to equilibrium M6C carbide precipitation, and has a favorable linear relation with Rockwell hardness. This study suggests that acoustic nonlinearity testing may be applicable to diagnostics on strength degradation in rotor steels.

  6. From aluminium pistons to steel pistons in trucks and ships; Von Aluminium- zum Stahlgrosskolben bei Nkw und Schiffen

    Energy Technology Data Exchange (ETDEWEB)

    Kortas, J. [Mahle GmbH, Markgroeningen (Germany). Produktkonstruktion Grossmotorenkomponenten

    2005-11-01

    This article is intended to show the development from one-piece aluminum pistons to composite pistons made from forged steel. With the Mahle pistons completely produced from forged steel, process-safe peak cylinder pressures of 25 MPa can be achieved. The steel piston development was initiated in the commercial vehicle sector and then extended to large engines with cylinder diameters up to 480 mm. (orig.)

  7. 46 CFR 56.25-20 - Bolting.

    Science.gov (United States)

    2010-10-01

    ..., Blanks, Flange Facings, Gaskets, and Bolting § 56.25-20 Bolting. (a) General. (1) Bolts, studs, nuts, and....01-2). (2) Bolts and studs must extend completely through the nuts. (3) See § 58.30-15(c) of this... steel stud bolts must be threaded full length or, if desired, may have reduced shanks of a diameter not...

  8. The Study on Weldability of Boron Steel and Hot-Stamped Steel by Using Laser Heat Source (Ⅲ) - Comparison on Laser Weldability of Boron Steel and Hot -Stamped Steel-

    Energy Technology Data Exchange (ETDEWEB)

    Choi, So Young; Kim, Jong Do [Korea Maritime and Ocean University, Busan (Korea, Republic of); Kim, Jong Su [Korea Institute of Machinery and Materials, Daejeon (Korea, Republic of)

    2015-01-15

    This study was conducted to compare the laser weldability of boron steel and hot-stamped steel. In general, boron steel is used in the hot-stamping process. Hot-stamping is a method for simultaneously forming and cooling boron steel in a press die after heating it to the austenitizing temperature. Hot-stamped steel has a strength of 1500 MPa or more. Thus, in this study, the laser weldability of boron steel and that of hot-stamped steel were investigated and compared. A continuous wave disk laser was used to produce butt and lap joints. In the butt welding, the critical cooling speed at which full penetration was obtained in the hot-stamped steel was lower than that of boron steel. In the lap welding, the joint widths were similar regardless of the welding speed when full penetration was obtained.

  9. The Study on Weldability of Boron Steel and Hot-Stamped Steel by Using Laser Heat Source (Ⅲ) - Comparison on Laser Weldability of Boron Steel and Hot -Stamped Steel-

    International Nuclear Information System (INIS)

    Choi, So Young; Kim, Jong Do; Kim, Jong Su

    2015-01-01

    This study was conducted to compare the laser weldability of boron steel and hot-stamped steel. In general, boron steel is used in the hot-stamping process. Hot-stamping is a method for simultaneously forming and cooling boron steel in a press die after heating it to the austenitizing temperature. Hot-stamped steel has a strength of 1500 MPa or more. Thus, in this study, the laser weldability of boron steel and that of hot-stamped steel were investigated and compared. A continuous wave disk laser was used to produce butt and lap joints. In the butt welding, the critical cooling speed at which full penetration was obtained in the hot-stamped steel was lower than that of boron steel. In the lap welding, the joint widths were similar regardless of the welding speed when full penetration was obtained

  10. Application of the radioisotope process when studying the decarbonization of low-alloy multicomponent steels in sodium

    International Nuclear Information System (INIS)

    Pavlinov, L.V.; Evstratov, V.D.

    1982-06-01

    By means of the radioisotope process and the method of a planning matrix for factor experiments quantitative values have been found for the influence of alloys of chromium molybdenum, niobium, vanadium, titanium on the decarbonization of low alloy pearlitic steels in sodium at temperatures of 500 to 800 0 C. It has been proved that of all alloys with a concentration of 1 to 3% Cr, 1 to 2% Mo, 0 to 1% Nb, 0 to 0.25% V, and 0 to 0.25% Ti, which had been studied, the alloys of iron with 1-3% Cr and 1% Mo showed the greatest tendency for decarbonization in sodium where the carbon concentration decreases from 0.01 to 0.02% at the surface. An increase of the concentration of molybdenum and especially of niobium and titanium leads to a decrease of the decarbonization tendency of steel because the surface concentration of carbon remains at the level of 0.08 to 0.09% in alloys which contain up to 1% niobium and in complex alloy steels with up to 1% niobium, 0.25% vanadium, and 0.25% titanium. (orig.) [de

  11. CEMS of Sb+ implanted stainless steels

    International Nuclear Information System (INIS)

    Roy-Poulsen, H.; Johnson, E.; Johansen, A.; Sarholt-Kristensen, L.; Hayashi, H.

    1986-01-01

    Martensitic transformations have been analyzed in a series of antimony implanted austenitic stainless steels using CEMS. The implanted samples contain about 70 vol% martensite, which is considerably more than can be formed conventionally by plastic deformation of cooling below the martensite start temperature. CEM spectra from implantation induced martensite and from martensite formed in conventional processes are virtually identical. In both cases the hyperfine field is ∼ 25T. (Auth.)

  12. CEMS of Sb+ implanted stainless steels

    International Nuclear Information System (INIS)

    Roy-Poulsen, H.; Copenhagen Univ.; Johnson, E.; Johansen, A.; Sarholt-Kristensen, L.; Hayashi, H.

    1985-01-01

    Martensitic transformations have been analyzed in a series of antimony implanted austenitic stainless steels using CEMS. The implanted samples contain about 70 vol% martensite, which is considerably more than can be formed conventionally by plastic deformation or cooling below the martensite start temperature. CEM spectra from implantation induced martensite and from martensite formed in conventional processes are virtually identical. In both cases the hyperfine field is ∝25 T. (orig.)

  13. Effect of Si and Mn additions on ferrite and austenite phase fractions in 25Cr-7Ni-1.5Mo-3W base super duplex stainless steels

    International Nuclear Information System (INIS)

    Jeong, S.W.; Lee, Z.-H.; Lee, H.M.

    2000-01-01

    The effect of heat treatment and Si and Mn additions on the ferrite and austenite phase fractions of the super duplex stainless steel (SDSS), Fe-25Cr-7Ni-1.5Mo-3W-Si-Mn-0.25N (numbers are all in wt.% unless specified otherwise), was investigated. The thermodynamic calculations of phase equilibria and phase fractions were performed using the Thermo-Calc program. Based on the calculated results, specific compositions of Si and Mn were selected and alloys with these compositions were analysed by Feritscope, X-ray diffractometry and scanning electron microscopy. The calculated phase fractions and experimentally analysed ones were compared and there was a good agreement between calculations and measurements. The optimum heat treatment condition for Fe-25Cr-7Ni-1.5Mo-3W-0.5Si-0.5Mn-0.25N is to hold at 1050 to 1100 C for 2 h in considering the ferrite to austenite ratio of 50:50 and to avoid second phase precipitation such as the σ phase. It was suggested that an excessive addition of more than 0.8Si and 1.0Mn may induce the σ phase precipitation. (orig.)

  14. Damage of target edges in brush-like geometry in the course of ELM-like plasma pulses in QSPA Kh-50

    Science.gov (United States)

    Makhlaj, V. A.; Garkusha, I. E.; Aksenov, N. N.; Bazylev, B.; Byrka, O. V.; Chebotarev, V. V.; Landman, I.; Herashchenko, S. S.; Staltsov, V. V.

    2015-08-01

    Castellated edges of macro-brush armour elements of ITER divertor can be a source of molten/solid dust particles which are injected into the plasma. The targets that combined in brush-like geometry have been irradiated under different inclination angles in QSPA Kh-50. The cubic brushes element has typical size of 1 cm. The titanium was used to investigate dynamics of mountains' formation. The onset of dust particles ejection from the exposed castellated targets has been studied. Formation of resolidified bridges through the gaps of brush-like targets due to the melt motion is studied in dynamics. With following plasma impacts such resolidified bridges became additional source of dust.

  15. Damage of target edges in brush-like geometry in the course of ELM-like plasma pulses in QSPA Kh-50

    International Nuclear Information System (INIS)

    Makhlaj, V.A.; Garkusha, I.E.; Aksenov, N.N.; Bazylev, B.; Byrka, O.V.; Chebotarev, V.V.; Landman, I.; Herashchenko, S.S.; Staltsov, V.V.

    2015-01-01

    Castellated edges of macro-brush armour elements of ITER divertor can be a source of molten/solid dust particles which are injected into the plasma. The targets that combined in brush-like geometry have been irradiated under different inclination angles in QSPA Kh-50. The cubic brushes element has typical size of 1 cm. The titanium was used to investigate dynamics of mountains’ formation. The onset of dust particles ejection from the exposed castellated targets has been studied. Formation of resolidified bridges through the gaps of brush-like targets due to the melt motion is studied in dynamics. With following plasma impacts such resolidified bridges became additional source of dust

  16. Damage of target edges in brush-like geometry in the course of ELM-like plasma pulses in QSPA Kh-50

    Energy Technology Data Exchange (ETDEWEB)

    Makhlaj, V.A., E-mail: makhlay@ipp.kharkov.ua [Institute of Plasma Physics of the NSC KIPT, 61108 Kharkov (Ukraine); Garkusha, I.E.; Aksenov, N.N. [Institute of Plasma Physics of the NSC KIPT, 61108 Kharkov (Ukraine); Bazylev, B. [Karlsruhe Institute of Technology (KIT), IHM, 76344 Karlsruhe (Germany); Byrka, O.V.; Chebotarev, V.V. [Institute of Plasma Physics of the NSC KIPT, 61108 Kharkov (Ukraine); Landman, I. [Karlsruhe Institute of Technology (KIT), IHM, 76344 Karlsruhe (Germany); Herashchenko, S.S.; Staltsov, V.V. [Institute of Plasma Physics of the NSC KIPT, 61108 Kharkov (Ukraine)

    2015-08-15

    Castellated edges of macro-brush armour elements of ITER divertor can be a source of molten/solid dust particles which are injected into the plasma. The targets that combined in brush-like geometry have been irradiated under different inclination angles in QSPA Kh-50. The cubic brushes element has typical size of 1 cm. The titanium was used to investigate dynamics of mountains’ formation. The onset of dust particles ejection from the exposed castellated targets has been studied. Formation of resolidified bridges through the gaps of brush-like targets due to the melt motion is studied in dynamics. With following plasma impacts such resolidified bridges became additional source of dust.

  17. Connections: Superplasticity, Damascus Steels, Laminated Steels, and Carbon Dating

    Science.gov (United States)

    Wadsworth, Jeffrey

    2016-12-01

    In this paper, a description is given of the connections that evolved from the initial development of a family of superplastic plain carbon steels that came to be known as Ultra-High Carbon Steels (UHCS). It was observed that their very high carbon contents were similar, if not identical, to those of Damascus steels. There followed a series of attempts to rediscover how the famous patterns found on Damascus steels blades were formed. At the same time, in order to improve the toughness at room temperature of the newly-developed UHCS, laminated composites were made of alternating layers of UHCS and mild steel (and subsequently other steels and other metals). This led to a study of ancient laminated composites, the motives for their manufacture, and the plausibility of some of the claims relating to the number of layers in the final blades. One apparently ancient laminated composite, recovered in 1837 from the great pyramid of Giza which was constructed in about 2750 B.C., stimulated a carbon dating study of ancient steels. The modern interest in "Bladesmithing" has connections back to many of these ancient weapons.

  18. Outlook of the world steel cycle based on the stock and flow dynamics.

    Science.gov (United States)

    Hatayama, Hiroki; Daigo, Ichiro; Matsuno, Yasunari; Adachi, Yoshihiro

    2010-08-15

    We present a comprehensive analysis of steel use in the future compiled using dynamic material flow analysis (MFA). A dynamic MFA for 42 countries depicted the global in-use stock and flow up to the end of 2005. On the basis of the transition of steel stock for 2005, the growth of future steel stock was then estimated considering the economic growth for every country. Future steel demand was estimated using dynamic analysis under the new concept of "stocks drive flows". The significant results follow. World steel stock reached 12.7 billion t in 2005, and has doubled in the last 25 years. The world stock in 2005 mainly consisted of construction (60%) and vehicles (10%). Stock in these end uses will reach 55 billion t in 2050, driven by a 10-fold increase in Asia. Steel demand will reach 1.8 billion t in 2025, then slightly decrease, and rise again by replacement of buildings. The forecast of demand clearly represents the industrial shift; at first the increase is dominated by construction, and then, after 2025, demand for construction decreases and demand for vehicles increases instead. This study thus provides the dynamic mechanism of steel stock and flow toward the future, which contributes to the design of sustainable steel use.

  19. Final Scientific Report - "Novel Steels for High Temperature Carburizing"

    Energy Technology Data Exchange (ETDEWEB)

    McKimpson, Marvin G.; Liu, Tianjun; Maniruzzaman, Md

    2012-07-27

    This program was undertaken to develop a microalloy-modified grade of standard carburizing steel that can successfully exploit the high temperature carburizing capabilities of current commercial low pressure (i.e. 'vacuum') carburizing systems. Such steels can lower the amount of energy required for commercial carburizing operations by reducing the time required for deep-case carburizing operations. The specific technical objective of the work was to demonstrate a carburizing steel composition capable of maintaining a prior austenite grain size no larger than ASTM grain size number 5 after exposure to simulated carburizing conditions of 1050 C for 8 hr. Such thermal exposure should be adequate for producing carburized case depths up to about 2 mm. Such carburizing steels are expected to be attractive for use across a wide range of industries, including the petroleum, chemical, forest products, automotive, mining and industrial equipment industries. They have potential for reducing energy usage during low pressure carburizing by more than 25%, as well as reducing cycle times and process costs substantially. They also have potential for reducing greenhouse gas emissions from existing low pressure carburizing furnaces by more than 25%. High temperature carburizing can be done in most modern low pressure carburizing systems with no additional capital investment. Accordingly, implementing this technology on carburizing furnaces will provide a return on investment significantly greater than 10%. If disseminated throughout the domestic carburizing community, the technology has potential for saving on the order of 23 to 34 trillion BTU/year in industrial energy usage. Under the program, two compositions of microalloyed, coarsening-resistant low alloy carburizing steels were developed, produced and evaluated. After vacuum annealing at 1050oC for 8 hrs and high pressure gas quenching, both steels exhibited a prior austenite ASTM grain size number of 5.0 or finer

  20. Evolution of dislocations and twins in a strong and ductile nanotwinned steel

    International Nuclear Information System (INIS)

    Zhou, P.; Liang, Z.Y.; Liu, R.D.; Huang, M.X.

    2016-01-01

    A twinning-induced plasticity (TWIP) steel was subjected to a simple processing route (i.e. cold rolling followed by a recovery heat treatment) suitable for large-scale industrial production, resulting in the production of a strong and ductile nanotwinned steel. This nanotwinned steel combines high yield strength (1450 MPa), high ultimate tensile strength (1600 MPa) and good ductility (25% total elongation). Detailed transmission electron microscopy observation reveals that the twin volume fraction of the nanotwinned steel remains constant during tensile deformation. This is different to the deformation behaviour of recrystallized TWIP steels whose twin volume fraction increase continuously with strain during tensile deformation. The constant twin volume fraction indicates that a maximum twin volume fraction has been reached during the cold rolling process. In contrast, the dislocation density of the nanotwinned steel increases with strain as measured by the synchrotron X-ray diffraction experiments. In other words, the plastic deformation of the nanotwinned steel is mainly accommodated by glide and multiplication of dislocations. Based on the experimental results, an analytical model was developed to capture the respective effects of dislocations and twins on the strength and ductility of the present nanotwinned steel. The modelling results indicate that the strength is contributed by both twins and dislocations while the ductility is mainly attributed to dislocation multiplication. -- Graphical abstract: (a) TEM bright field image showing intensive nanotwins in the nanotwinned steel. Selected area diffraction pattern obtained within the red circle. (b) The engineering stress–stain curve of the nanotwinned steel. Display Omitted