WorldWideScience

Sample records for soluble corrosion products

  1. Solubility of corrosion products in high temperature water

    International Nuclear Information System (INIS)

    Srinivasan, M.P.; Narasimhan, S.V.

    1995-01-01

    A short review of solubility of corrosion products at high temperature in either neutral or alkaline water as encountered in BWR, PHWR and PWR primary coolant reactor circuits is presented in this report. Based on the available literature, various experimental techniques involved in the study of the solubility, theory for fitting the solubility data to the thermodynamic model and discussion of the published results with a scope for future work have been brought out. (author). 17 refs., 7 figs

  2. Solubility of simulated PWR primary circuit corrosion products

    International Nuclear Information System (INIS)

    Kunig, R.H.; Sandler, Y.L.

    1986-08-01

    The solubility behavior of non-stoichiometric nickel ferrites, nickel-cobalt ferrites, and magnetite, as model substances for the corrosion products (''crud'') formed in nuclear pressurized water reactors, was studied in a flow system in aqueous solutions of lithium hydroxide, boric acid, and hydrogen with pH, temperature, and hydrogen concentrations as parameters. Below the temperature region of 300 to 330 0 C, at hydrogen concentrations of 25 to 40 cm 3 /kg H 2 O as used during reactor operation, the solubility of nickel-cobalt ferrite is the same as that of Ni and Co/sub x/Fe/sub 3-x/O 4 (x 3 /kg of hydrogen, the equilibrium iron and nickel solubilities increase congruently down to about 100 0 C, in a manner consistent with the solubility of Fe 3 O 4 , but sharply decline at lower temperatures, apparently due to formation of a borated layer. A cooldown experiment on a time scale of a typical Westinghouse reactor shutdown, as well as static experiments carried out on various ferrite samples at 60 0 C show that after addition of oxygen or peroxide evolution of nickel (and possibly cobalt) above the equilibrium solubility in hydrogen depends on the presence of dissociation products prior to oxidation. Thermodynamic calculations of various reduction and oxidative decomposition reactions for stoichiometric and non-stoichiometric nickel ferrite and cobalt ferrite are presented. Their significance to evolutions of nickel and cobalt on reactor shutdown is discussed. 30 refs., 38 figs., 34 tabs

  3. Solubility of corrosion products of plain steel in oxygen-containing water solutions at high parameters

    International Nuclear Information System (INIS)

    Martynova, O.I.; Samojlov, Yu.F.; Petrova, T.I.; Kharitonova, N.L.

    1983-01-01

    Technique for calculation of solubility of iron corrosion products in oxygen-containing aqueous solutions in the 298-573 K temperature range is presented. Solubility of corrosion products of plain steel in deeply-desalinizated water in the presence of oxygen for the such range of the temperatures is experimentally determined. Rather good convergence between calculated and experimental data is noted

  4. Steel corrosion products solubility under conditions simulating various water chemistry parameters in power plants

    International Nuclear Information System (INIS)

    Slobodov, A.A.; Kritskij, V.G.; Zarembo, V.I.; Puchkov, L.V.

    1988-01-01

    To simulate construction material corrosion product mass transfer model in power plant circuits calculation of iron oxide and hydroxide solubility, depending on water chemistry parameters: temperature, pH-value, content of dissolved in water hydrogen and oxygen, is carried out

  5. Predicting corrosion product transport in nuclear power stations using a solubility-based model for flow-accelerated corrosion

    International Nuclear Information System (INIS)

    Burrill, K.A.; Cheluget, E.L.

    1995-01-01

    A general model of solubility-driven flow-accelerated corrosion of carbon steel was derived based on the assumption that the solubilities of ferric oxyhydroxide and magnetite control the rate of film dissolution. This process involves the dissolution of an oxide film due to fast-flowing coolant unsaturated in iron. The soluble iron is produced by (i) the corrosion of base metal under a porous oxide film and (ii) the dissolution of the oxide film at the fluid-oxide film interface. The iron released at the pipe wall is transferred into the bulk flow by turbulent mass transfer. The model is suitable for calculating concentrations of dissolved iron in feedtrain lines. These iron levels were used to calculate sludge transport rates around the feedtrain. The model was used to predict sludge transport rates due to flow accelerated corrosion of major feedtrain piping in a CANDU reactor. The predictions of the model compare well with plant measurements

  6. A review of pH calculation and corrosion product solubilities under PWR primary coolant chemistry conditions

    International Nuclear Information System (INIS)

    Thornton, E.W.; Polley, M.V.

    1986-12-01

    The calculation of high temperature pH in boric acid solutions is discussed and various relationships for the ionisation constant Ksub(w) or ion product Qsub(w) for water are reviewed. It is shown that the boric acid equilibria of Mesmer, Baes and Sweeton remain virtually unaltered when Marshall and Franck's relationship for Ksub(w) is substituted in a re-analysis of Mesmer, Baes and Sweeton's original experimental data. Magnetite solubility data and Westinghouse's studies of iron, nickel and cobalt solubility from mixed ferrites are collated and consideration is given to experimental difficulties which could have contributed to the variability in the data. Thermodynamic model fits have been computerised and used to compare different studies and to determine pH values at which the temperature dependence of solubility is predicted to be zero. Consideration is given to the differing dependences of solubility on dissolved hydrogen concentration in the three model fits. Two models for predicting iron and nickel solubility with respect to non-stoichiometric nickel ferrites are briefly discussed showing that only one of these is likely to be credible. (author)

  7. Behaviour of steel corrosion products under neutral-oxidizing water conditions

    International Nuclear Information System (INIS)

    Martynova, O.I.; Petrova, T.I.; Samojlov, Yu.F.; Kharitonova, N.L.

    1985-01-01

    Results of laboratory experiments on studying the solubility of iron and cobalt corrosion products are given. It is established that oxygen dosage doesn't influence practically on the iron corrosion product solubility but cobalt corrosion product solubility decreases, the presence of hydrogen peroxide in an initial solution leads to increase of the iron corrosion product solubility especially at 125 deg C. It is shown that hydrogen peroxide affects unambiguously the cobalt corrosion product solubility: at hydrogen peroxide concentration of about 400 μg/l at 50-275 deg C temperature their solubility is minimum

  8. Correlation of flow accelerated corrosion rate with iron solubility

    International Nuclear Information System (INIS)

    Fujiwara, K.; Domae, M.; Yoneda, K.; Inada, F.; Ohira, T.; Hisamune, K.; Takiguchi, H.

    2009-01-01

    Flow Accelerated Corrosion (FAC) of carbon steel is one of the most important subjects in coolant systems of power plants. FAC is influenced by material, flow condition, temperature, and water chemistry. It is considered that solubility is the most important factor to determine the effect of water chemistry on FAC. In the present study, effect of specific oxide on FAC rate was studied from the thermodynamic solubility of iron. The effects of temperature and pH on the iron solubility were evaluated by taking into consideration hydrolysis reactions of ferrous iron, dissolution equilibria of Fe 3 O 4 , FeO, and Fe(OH) 2 , and charge balance. The correlation between the iron solubility and FAC behavior was evaluated by using the normalized mass transfer coefficient. It is clarified that the product of iron solubility equilibrated with Fe 3 O 4 and normalized mass transfer coefficient can explain the temperature and pH dependence of FAC. These results indicate presence of magnetite on the surface of carbon steel. Diffusion of iron from the saturated layer determines the FAC rate from water chemistry aspect. (author)

  9. Correlation of flow accelerated corrosion rate with iron solubility

    International Nuclear Information System (INIS)

    Fujiwara, K.; Domae, M.; Yoneda, K.; Inada, F.; Ohira, T.; Hisamune, K.

    2011-01-01

    Flow accelerated corrosion (FAC) of the carbon steel is one of the most important subjects in the coolant systems of the power plants. FAC is influenced by the composition of the material, the flow condition, temperature, and the water chemistry conditions. It is considered that the solubility of iron (Fe) is the most important factor in the water chemistry parameters affecting FAC. In the present study, the effects of temperature and pH on the Fe solubility were evaluated in consideration of the hydrolysis reactions of the ferrous iron, the dissolution equilibria of Fe 3 O 4 , FeO, and Fe(OH) 2 , and the charge balance. The correlation between the Fe solubility and the FAC behavior was discussed. It has been suggested that the product of the Fe solubility equilibrated with Fe 3 O 4 and the mass transfer coefficient can explain the temperature and pH dependence of FAC. These results indicate the presence of the magnetite on the surface of the carbon steel. Diffusion of the Fe from the saturated layer to the bulk solution determines the FAC rate from the water chemistry aspect.

  10. Aluminum corrosion product release kinetics

    Energy Technology Data Exchange (ETDEWEB)

    Edwards, Matt, E-mail: Matthew.Edwards@cnl.ca; Semmler, Jaleh; Guzonas, Dave; Chen, Hui Qun; Toor, Arshad; Hoendermis, Seanna

    2015-07-15

    Highlights: • Release of Al corrosion product was measured in simulated post-LOCA sump solutions. • Increased boron was found to enhance Al release kinetics at similar pH. • Models of Al release as functions of time, temperature, and pH were developed. - Abstract: The kinetics of aluminum corrosion product release was examined in solutions representative of post-LOCA sump water for both pressurized water and pressurized heavy-water reactors. Coupons of AA 6061 T6 were exposed to solutions in the pH 7–11 range at 40, 60, 90 and 130 °C. Solution samples were analyzed by inductively coupled plasma atomic emission spectroscopy, and coupon samples were analyzed by secondary ion mass spectrometry. The results show a distinct “boron effect” on the release kinetics, expected to be caused by an increase in the solubility of the aluminum corrosion products. New models were developed to describe both sets of data as functions of temperature, time, and pH (where applicable)

  11. Deposition of corrosion products in-core

    International Nuclear Information System (INIS)

    Burrill, K.A.

    1994-11-01

    Data on corrosion product deposits on fuel sheaths are presented for a variety of operating conditions and water chemistries: boiling and non-boiling water; surface heat flux; pH, dissolved hydrogen concentration. Corrosion product behaviour in-core may be interpreted in terms of the solubility of magnetite and how it changes with water chemistry and temperature. A hypothesis of the deposition and release mechanisms was proposed in the 1970s in which particles deposited onto the sheath and subsequently dissolved in the heated water while being irradiated. Some of the deposition data may be interpreted using a model of these mechanisms. (author). 5 refs., 6 tabs., 8 figs

  12. IN DRIFT CORROSION PRODUCTS

    Energy Technology Data Exchange (ETDEWEB)

    D.M. Jolley

    1999-12-02

    As directed by a written development plan (CRWMS M&O 1999a), a conceptual model for steel and corrosion products in the engineered barrier system (EBS) is to be developed. The purpose of this conceptual model is to assist Performance Assessment Operations (PAO) and its Engineered Barrier Performance Department in modeling the geochemical environment within a repository drift, thus allowing PAO to provide a more detailed and complete in-drift geochemical model abstraction and to answer the key technical issues (KTI) raised in the NRC Issue Resolution Status Report (IRSR) for the Evolution of the Near-Field Environment (NFE) Revision 2 (NRC 1999). This document provides the conceptual framework for the in-drift corrosion products sub-model to be used in subsequent PAO analyses including the EBS physical and chemical model abstraction effort. This model has been developed to serve as a basis for the in-drift geochemical analyses performed by PAO. However, the concepts discussed within this report may also apply to some near and far-field geochemical processes and may have conceptual application within the unsaturated zone (UZ) and saturated zone (SZ) transport modeling efforts.

  13. Corrosion mechanisms of containment glasses for fission products

    International Nuclear Information System (INIS)

    Nogues, J.L.

    1984-01-01

    After a review of nuclear energy production and waste vitrification principles, the aqueous corrosion mechanisms of the containment glasses and the various parameters affecting the corrosion are studied: effects of glass composition, temperature, lixiviation agent pH, lixiviation duration and mode. Conventional mass loss measurement and solution analyses are coupled to sophisticated surface analysis techniques. The hydrolyzed layer formation and the solubility limits are discussed. 87 figs., 30 tabs., 144 refs

  14. Understanding corrosion via corrosion product characterization: II. Role of alloying elements in improving the corrosion resistance of Zn-Al-Mg coatings on steel

    International Nuclear Information System (INIS)

    Volovitch, P.; Vu, T.N.; Allely, C.; Abdel Aal, A.; Ogle, K.

    2011-01-01

    Highlights: → Origins of better corrosion resistance of ZnAlMg coatings than galvanized steel. → Comparative study of corrosion products formed on ZnAlMg, ZnMg and Zn coatings. → Modeling of dissolution and precipitation stages of corrosion. → At early stages Mg stabilizes protective zinc basic salts during dry-wet cycling. → At later stages Al dissolves at high pH forming protective layered double hydroxides. - Abstract: Corrosion products are identified on Zn, ZnMg and ZnAlMg coatings in cyclic corrosion tests with NaCl or Na 2 SO 4 containing atmospheres. For Mg-containing alloys the improved corrosion resistance is achieved by stabilization of protective simonkolleite and zinc hydroxysulfate. At later stages, the formation of layered double hydroxides (LDH) is observed for ZnAlMg. According to thermodynamic modeling, Mg 2+ ions bind the excess of carbonate or sulfate anions preventing the formation of soluble or less-protective products. A preferential dissolution of Zn and Mg at initial stages of corrosion is confirmed by in situ dissolution measurement. The physicochemical properties of different corrosion products are compared.

  15. Corrosion products in the primary circuits of PWRs

    International Nuclear Information System (INIS)

    Darras, R.

    1983-01-01

    The characteristics of PWR primary circuits are recalled, particularly the chemical specifications of the medium and the various materials used (austenitic steel, nickel alloys, cobalt-based alloys and zirconium alloys). The behaviour of these materials as regards general corrosion in nominal and transient conditions is then outlined briefly, special emphasis being laid on the effect of the determining parameters on the quantity of corrosion products formed. The release of the latter into the primary coolant is caused by two main processes: solubilization and erosion. Particular attention was given therefore to the laws governing the solubility of the oxides involved, especially as a function of temperature and pH. Erosion, or release in the form of solid particles, is relatively severe during transient events. As these corrosion products are then carried through all circuits, they cause deposits to form in favourable places on the walls as a result either of precipitation of soluble species or of sedimentation followed by consolidation of suspended particles. The presence of corrosion products in the primary circuits creates a particular impact since they become radioactive as they pass through the core and especially when they remain in it in the form of deposits; as a result, the products are capable of contaminating the entire system. Finally, although long-term reliability is obviously an essential condition for materials developed, attention must also be given to problems associated with a build-up of corrosion products in the cooling circuits and efforts made to minimize them. To that end, a number of precautions are recommended, and various remedies can be applied: selecting materials which are not readily activated, keeping structures clean, purifying fluids properly, restricting solubilization and precipitation, and perhaps, periodic decontamination. (author)

  16. Device of capturing for radioactive corrosion products

    International Nuclear Information System (INIS)

    Ohara, Atsushi; Fukushima, Kimichika.

    1984-01-01

    Purpose: To increase the area of contact between the capturing materials for the radioactive corrosion products contained in the coolants and the coolants by producing stirred turbulent flows in the coolant flow channel of LMFBR type reactors. Constitution: Constituent materials for the nuclear fuel elements or the reactor core structures are activated under the neutron irradiation, corroded and transferred into the coolants. While capturing devices made of pure metal nickel are used for the elimination of the corrosion products, since the coolants form laminar flows due to the viscosity thereof near the surface of the capturing materials, the probability that the corrosion products in the coolants flowing through the middle portion of the channel contact the capturing materials is reduced. In this invention, rotating rolls and flow channels in which the balls are rotated are disposed at the upstream of the capturing device to forcively disturb the flow of the liquid sodium, whereby the radioactive corrosion products can effectively be captured. (Kamimura, M.)

  17. Techniques for the identification of corrosion products

    International Nuclear Information System (INIS)

    Ramanathan, L.V.

    1988-12-01

    This paper presents the different techniques that can be used to identify corrosion/oxidation products through determination of either their composition or their structure, chemical analysis and spectrochemical analysis are commonly used to determine the composition of gross corrosion products. Surface anaLysis techniques such as electron microprobe, AES, ESCA, SIMS, ISS, neutron activation analysis, etc., can be used not only to detect the concentration of the various elements present, but also to obtain the concentration profiles of these elements through the corrosion products. The structure of corrosion products is normally determined with the aid of either X-ray or electron diffraction techniques. This paper describes the basic principles, typical characteristics, limitations and the types of information that can be obtained from each of the techniques along with some typical examples. (author) [pt

  18. Corrosion products in power generating systems

    International Nuclear Information System (INIS)

    Lister, D.H.

    1980-06-01

    The important mechanisms of corrosion and corrosion product movement and fouling in the heat transport systems of thermal electric generating stations are reviewed. Oil- and coal-fired boilers are considered, along with nuclear power systems - both direct and indirect cycle. Thus, the fireside and waterside in conventional plants, and the primary coolant and steam-raising circuits in water-cooled reactors, are discussed. Corrosion products in organic- and liquid-metal-cooled reactors also are shown to cause problems if not controlled, while their beneficial effects on the cooling water side of condensers are described. (auth)

  19. Corrosion products behaviour under VVER primary coolant conditions

    International Nuclear Information System (INIS)

    Grygar, T.; Zmitko, M.

    2002-01-01

    The aim of this work was to collect data on thermodynamic stability of Cr, Fe, and Ni oxides, mechanisms of hydrothermal corrosion of stainless steels and to compare the real observation with the theory. We found that the electrochemical potential and pH in PWR and VVER are close to the thermodynamic boundary between two fields of stable spinel type oxides. The ways of degradation of the passivating layers due to changes in water chemistry were considered and PWR and VVER systems were found to be potentially endangered by reductive attack. In certain VVER systems the characteristics of the passivating layer on steels and also concentration of soluble corrosion products seem to be in contradiction with the theoretical expectations. (author)

  20. Corrosion and solubility in a TSP-buffered chemical environment following a loss of coolant accident: Part 2 – Zinc

    International Nuclear Information System (INIS)

    Pease, David; LaBrier, Daniel; Ali, Amir; Blandford, Edward D.; Howe, Kerry J.

    2016-01-01

    Highlights: • Zinc release is limited to less than 1 mg/L in TSP-buffered solution under a variety of conditions (pH, temperature, zinc source). • Zinc release in high-temperature non-TSP-buffered environment is approximately 25 mg/L. • Long-term zinc release is controlled by passivation (without TSP) and zinc solubility (with TSP). • Precipitation and solubility of zinc phosphate limit the release of zinc. - Abstract: Bench experiments were conducted to investigate the effect of the presence of trisodium phosphate (TSP) on the corrosion and release of zinc from metallic zinc-bearing surfaces under conditions representative of the containment pool following a postulated loss of coolant accident (LOCA) at a nuclear power generating facility. The experiments showed that in non-buffered (acidic) environments, measurable quantities of zinc are released from zinc-bearing surfaces. Precipitation and solubility of phosphate-based corrosion products, such as zinc phosphate, limit the release of zinc from zinc-bearing surfaces. These experiments have found that under a variety of conditions, including variations of temperature, pH, and across different zinc-bearing surfaces, the release of zinc into solution is limited to <1 mg/L when phosphate is present. When phosphate is not present, zinc release is instead bounded by a markedly higher saturation limit which is a strong function of the solution temperature.

  1. Capturing device for radioactive corrosion products

    International Nuclear Information System (INIS)

    Ono, Kiyoshi.

    1987-01-01

    Purpose: To render the flow channel area uniform for each of coolants over the entire capturing device and reduce the corrosion of capturing materials due to coolants. Constitution: Most of radioactivity caused by radioactive corrosion products are due to Mn-54 radioactive nuclides and it has been known that the nuclides are readily deposited to the surface of nickel material in sodium at high temperature. It is difficult in a conventional capturing device constituted by winding a nickel plate fabricated with protrusions in a multiple-coaxial configuration, that the flow channel area is reduced in a portion of the flow channel and it is difficult to make the flow of the coolants uniform. In view of the above, by winding a nickel plate having a plurality of protrusions at the surface formed integrally by way of an electrolytic process into a multiple-coaxial or spiral shape, those having high resistance to the coolant corrosion can be obtained. (Takahashi, M.)

  2. A computer code PACTOLE to predict activation and transport of corrosion products in a PWR

    International Nuclear Information System (INIS)

    Beslu, P.; Frejaville, G.; Lalet, A.

    1978-01-01

    Theoretical studies on activation and transport of corrosion products in a PWR primary circuit have been concentrated, at CEA on the development of a computer code : PACTOLE. This code takes into account the major phenomena which govern corrosion products transport: 1. Ion solubility is obtained by usual thermodynamics laws in function of water chemistry: pH at operating temperature is calculated by the code. 2. Release rates of base metals, dissolution rates of deposits, precipitation rates of soluble products are derived from solubility variations. 3. Deposition of solid particles is treated by a model taking into account particle size, brownian and turbulent diffusion and inertial effect. Erosion of deposits is accounted for by a semi-empirical model. After a review of calculational models, an application of PACTOLE is presented in view of analyzing the distribution of in core. (author)

  3. High Temperature Corrosion under Laboratory Conditions Simulating Biomass-Firing: A Comprehensive Characterization of Corrosion Products

    DEFF Research Database (Denmark)

    Okoro, Sunday Chukwudi; Montgomery, Melanie; Jappe Frandsen, Flemming

    2014-01-01

    characterization of the corrosion products. The corrosion products consisted of three layers: i) the outermost layer consisting of a mixed layer of K2SO4 and FexOy on a partly molten layer of the initial deposit, ii) the middle layer consists of spinel (FeCr2O4) and Fe2O3, and iii) the innermost layer is a sponge......-like Ni3S2 containing layer. At the corrosion front, Cl-rich protrusions were observed. Results indicate that selective corrosion of Fe and Cr by Cl, active oxidation and sulphidation attack of Ni are possible corrosion mechanisms....

  4. Study on corrosion products from ear piercing studs

    International Nuclear Information System (INIS)

    Rogero, Sizue O.; Costa, Isolda; Saiki, Mitiko

    2000-01-01

    In this work instrumental neutron activation analysis was applied to analyse elemental composition of commercial gold coated ear piercing substrate and metals present in their corrosion products. The cytotoxic effect was also verified in these corrosion product extracts, probably, due to the lixiviation of Ni present in high quantity in their substrates. The analysis of gold coated ear piercing surfaces by scanning electron microscopy before and after the corrosion test showed coating defects and the occurrence of corrosion process. (author)

  5. Mitigation of corrosion product ingress into SG's

    International Nuclear Information System (INIS)

    Han, S.H.

    1988-01-01

    Design and operation experiences to mitigate corrosion product ingress into SGs in Korea nuclear power plants are briefly reviewed. Maintaining the feedwater pH above 9.6 with morpholine seems to contribute significantly to reduction of iron transport to SGs. Measured iron transport rates were 4.8 g/hr/100 MWe at pH 9.8 and 2.8 g/hr/100 MWe at 9.3, respectively. Removal of corrosion products through SG blowdown is very limited. Its removal efficiency at the higher pH plant was in the neighborhood of 10 %. In one of the Korea Nuclear Units, a large amount of sludge piles were found in the middle of tube bundles especially on the cold leg side. Damaged tubes were identified by the multi-frequency eddy current tests and plugged later during the refueling period. Intermittent blowdown-rate increase was tried to enhance ionic impurity removal through SG blowdown. Even though it was not effective against Na, removal other impurity was improved, resulting in prolonged condensate polisher operation periods by 1 - 2 days. Two-bed polisher design, a cation bed followed by a mixed bed, was chosen for future PWR plants to enhance corrosion product filtering capability of the polishers. Condensate pump discharge polishing and divided hot well polishing methods are currently in consideration. (Nogami, K.)

  6. Drying characteristics of thorium fuel corrosion products

    Energy Technology Data Exchange (ETDEWEB)

    Smith, R.-E. E-mail: rzl@inel.gov

    2004-07-01

    The open literature and accessible US Department of Energy-sponsored reports were reviewed for the dehydration and rehydration characteristics of potential corrosion products from thorium metal and thorium oxide nuclear fuels. Mixed oxides were not specifically examined unless data were given for performance of mixed thorium-uranium fuels. Thorium metal generally corrodes to thorium oxide. Physisorbed water is readily removed by heating to approximately 200 deg. C. Complete removal of chemisorbed water requires heating above 1000 deg. C. Thorium oxide adsorbs water well in excess of the amount needed to cover the oxide surface by chemisorption. The adsorption of water appears to be a surface phenomenon; it does not lead to bulk conversion of the solid oxide to the hydroxide. Adsorptive capacity depends on both the specific surface area and the porosity of the thorium oxide. Heat treatment by calcination or sintering reduces the adsorption capacity substantially from the thorium oxide produced by metal corrosion.

  7. Characterization of Corrosion Products on Carbon Steel Exposed to Natural Weathering and to Accelerated Corrosion Tests

    Directory of Open Access Journals (Sweden)

    Renato Altobelli Antunes

    2014-01-01

    Full Text Available The aim of this work was to compare the corrosion products formed on carbon steel plates submitted to atmospheric corrosion in urban and industrial atmospheres with those formed after accelerated corrosion tests. The corrosion products were characterized by X-ray diffraction, Mössbauer spectroscopy, and Raman spectroscopy. The specimens were exposed to natural weathering in both atmospheres for nine months. The morphologies of the corrosion products were evaluated using scanning electron microscopy. The main product found was lepidocrocite. Goethite and magnetite were also found on the corroded specimens but in lower concentrations. The results showed that the accelerated test based on the ASTM B117 procedure presented poor correlation with the atmospheric corrosion tests whereas an alternated fog/dry cycle combined with UV radiation exposure provided better correlation.

  8. Solubility of oxygen in liquid sodium: effect on interpretation of corrosion data

    International Nuclear Information System (INIS)

    Claxton, K.T.

    1976-01-01

    No solubility correlation relating the equilibrium oxygen concentration with the sodium saturation temperature has yet been derived which has gained general acceptance. A statistical analysis of all the available data which directly or indirectly may be taken as representing a measurement of solubility has been made. The results indicate that a real and seemingly permanent difference is apparent between the assumed equilibrium levels of oxygen measured at different saturation temperatures as reported by UK and US workers. Data analysis procedures producing sub-sets of culled data which are then used to derive a compromise solubility function are considered less than adequate. It is considered preferable and more realistic to distinguish data sub-sets by the analytical technique employed. The established vacuum distillation method is shown to yield results differing among themselves by up to a factor of four at cold trap temperatures of relevance to fast reactor operation. The vanadium wire and electrochemical cell techniques are shown to give the lowest solubility values. Appropriate factors relating UK oxygen levels to values derived from alternative methods are presented. The divergent positions prevailing for oxygen-in-sodium analysis can lead to apparent anomalies when comparisons of corrosion rates from different sources have to be made. It is shown that this situation is, in part, apparently resolved by effecting comparisons at the equivalent cold trap temperature instead of the equivalent oxygen level. It is recognised that the approach presumes equilibrium of the oxygen in the sodium with the cold trap and reference is made to alternative ''sinks'' for oxygen. It is demonstrated, by comparison of a number of recommended and observed corrosion rates from US and European sources, that, in spite of the above and other qualifications, the approach is reasonable

  9. Exposure testing of fasteners in preservative treated wood: Gravimetric corrosion rates and corrosion product analyses

    Energy Technology Data Exchange (ETDEWEB)

    Zelinka, Samuel L., E-mail: szelinka@fs.fed.u [USDA Forest Products Laboratory, One Gifford Pinchot Drive, Madison, WI 53726 (United States); Sichel, Rebecca J. [College of Engineering, University of Wisconsin, Madison, WI 53706 (United States); Stone, Donald S. [Department of Materials Science and Engineering, College of Engineering, University of Wisconsin, Madison, WI 53706 (United States)

    2010-12-15

    Research highlights: {yields} The composition of the corrosion products was similar for the nail head and shank. {yields} Reduced copper was not detected on any of the fasteners. {yields} Measured corrosion rates were between 1 and 35 {mu}m year{sup -1}. - Abstract: Research was conducted to determine the corrosion rates of metals in preservative treated wood and also understand the mechanism of metal corrosion in treated wood. Steel and hot-dip galvanized steel fasteners were embedded in wood treated with one of six preservative treatments and exposed to 27 {sup o}C at 100% relative humidity for 1 year. The corrosion rate was determined gravimetrically and the corrosion products were analyzed with scanning electron microscopy, energy dispersive X-ray spectroscopy, and X-ray diffraction. Although the accepted mechanism of corrosion in treated wood involves the reduction of cupric ions from the wood preservative, no reduced copper was found on the corrosion surfaces. The galvanized corrosion products contained sulfates, whereas the steel corrosion products consisted of iron oxides and hydroxides. The possible implications and limitations of this research on fasteners used in building applications are discussed.

  10. Regularities of transition of steel corrosion products into aqueous medium

    International Nuclear Information System (INIS)

    Nikitin, V.I.; Gvozd', A.M.; Karpova, T.Ya.

    1981-01-01

    Effect of different factors on a degree of steel corrosion product transition to a water medium has been studied. Ratio of a specific masm qsub(c) of the corrosion products transferring to the water and a specific masm q of all the steel corrosion products produced under the given conditions was used as a criterium characterizing a degree of corrosion product transition from steel surfaces to water. The transition degree to water at a high temperature of different kind steel corrosion products differs relatively few (qsub(c)/q=0.5-0.7) in the water containing oxygen and different salts on increasing temperature, the corrosion process is characterized with continuous decrease of a relative amount of the corrosion products transferring to the medium. On the contrary, in the deaerated water the transition degree of perlite steel corrosion products to water remains constant in a wide temperature range (100-320 deg C). Besides chromium, nickel being a part of austenitic steel composition affects positively decrease of the transition degree of the corrosion products to water as well as q and qsub(c) reduction. The most difference in corrosion characteristics and the transition degree to water is observed when affecting colant steels in the low-temperature zone of the steam generator [ru

  11. Radiochemical studies on corrosion products of oral biomaterials

    International Nuclear Information System (INIS)

    Madbouly, H.A.Abdallah

    1998-01-01

    The work given in this thesis deals with a radioactive tracer study of the sorption of the corrosion products of dental amalgams and antimony on human teeth, porcelain and acrylic materials, used as dental restorative material. Sorption was investigated in presence of water and liquids commonly intaken by man; namely tea with or without sugar, soluble coffee ( Nescaffee) with or without sugar and/or milk, red tea (karkadeh or hibiscus) with or without sugar and chicken soup. The radioactive isotopes of Ag, Sn, Zn (amalgam components) and antimony were prepared by their irradiation in the nuclear reactor; 110m Ag, 113 Sn, 65 Zn and 124 Sb were thereby produced. The percent uptake of each studied element was evaluated from the depletion of radioactivity of the corresponding radioactive tracer in the given medium containing a tooth (human or artificial)

  12. Removal of corrosion products of construction materials in heat carrier

    International Nuclear Information System (INIS)

    1975-01-01

    A review of reported data has been made on the removal of structural material corrosion products into the heat-carrying agent of power reactors. The corrosion rate, and at the same time, removal of corrosion products into the heat-carrying agent (water) decreases with time. Thus, for example, the corrosion rate of carbon steel in boiling water at 250 deg C and O 2 concentration of 0.1 mg/1 after 3000 hr is 0.083 g/m 2 . day; after 9000 hr the corrosion rate has been reduced 2.5 times. Under static conditions the transfer rate of corrosion products into water has been smaller than in the stream and also depends on time. The corrosion rate of carbon steel under nuclear plant operating conditions is almost an order higher over that of steel Kh18N10T

  13. Analysis of corrosion product transport in PWR primary system under non-convective condition

    International Nuclear Information System (INIS)

    Han, Byoung Sub

    1992-02-01

    The increase of occupational radiation exposure (ORE) due to the increase of the operational period at existing nuclear power plant and also the publication of the new version of ICRP recommendation (ICRP publication No. 60) for radiological protection require much more strict reduction of radiation buildup in the nuclear power plant. The major sources of the radiation, i.e. the radioactive corrosion-products, are generated by the neutron activation of the corrosion products at the reactor core, and then the radioactive corrosion products are transported to the outside of the core, and accumulated near the steam generator side at PWR. Major radioactive corrosion-products of interest in PWR are Cr 51 ,: Mn 54 ,: Co 58 ,: Fe 59 and Co 60 . Among them Co 58 and Co 60 are known to contribute approximately more than 70% of the total ORE. Thus our main concerns are focused on predicting the transport and deposition of the Co radionuclides and suggesting the optimizing method which can minimize and control the ORE of the nuclear power plant. It is well known that Co-source is most effectively controlled by pH-solubility radiation control, and also some complex computer codes such as CORA and PACTOLE have been developed and revised to predict the corrosion product behavior. However these codes still imply some intrisic problems in simulating the real behavior of corrosion products in the reactor because of 1) the lack of important experimental data, coefficients and parameters of the transport and reactions under actual high temperature and pressure conditions, 2) no general theoretical modelling which can describe such many different mechanisms involved in the corrosion product movements, 3) the newly developed and measured behavior of the corrosion product transport mechanism. Since no sufficient and detailed information is available from the above-mentioned codes (also due to propriority problems), we concentrate on developing a new computer code, CP-TRAN (Corrosion

  14. Development of Copper Corrosion Products and Relation between Surface Appearance and Corrosion Rate

    International Nuclear Information System (INIS)

    Lan, Tran Thi Ngoc; Binh, Nguyen Thi Thanh; Tru, Nguyen Nhi; Yoshino, Tsujino; Yasuki, Maeda

    2008-01-01

    Copper was exposed unsheltered and sheltered in four humid tropical sites, representing urban, urban-industrial, urban-marine and rural environments. The corrosion rates and the sequence of corrosion product formation are presented and discussed in relation with climatic and atmospheric pollution parameters. Chemical compositions of corrosion products were found to depend on environments and duration of exposure. In all environments, cuprite was the predominating corrosion product that formed first and continuously increased during the exposure. Among the sulphur-containing corrosion products, posnjakite and brochantite were more frequently found and the first formed earlier. Nantokite was the most common chlorine-containing products for most cases, except the high-chloride environment, where atacamite was detected instead. The corrosion rate of copper was well indicated by the colour of patina. The red-purple colour corresponded to the high corrosion rate and the greenish grey colour corresponded to the low corrosion rate. Corrosion rate of sheltered copper in urban-marine environment increased with the exposure time

  15. Corrosion and solubility in a TSP-buffered chemical environment following a loss of coolant accident: Part 1 – Aluminum

    Energy Technology Data Exchange (ETDEWEB)

    Howe, Kerry J., E-mail: howe@unm.edu [University of New Mexico, 210 University Blvd., Albuquerque, NM 87131 (United States); Mitchell, Lana, E-mail: lmitchell@alionscience.com [University of New Mexico, 210 University Blvd., Albuquerque, NM 87131 (United States); Kim, Seung-Jun, E-mail: skim@lanl.gov [University of New Mexico, 210 University Blvd., Albuquerque, NM 87131 (United States); Blandford, Edward D., E-mail: edb@unm.edu [University of New Mexico, 210 University Blvd., Albuquerque, NM 87131 (United States); Kee, Ernest J., E-mail: erniekee@gmail.com [South Texas Project Nuclear Operating Company, P.O. Box 270, Wadsworth, TX 77483 (United States)

    2015-10-15

    Highlights: • Trisodium phosphate (TSP) causes aluminum corrosion to cease after 24 h of exposure. • Chloride, iron, and copper have a minimal effect on the rate of aluminum corrosion when TSP is present. • Zinc can reduce the rate of aluminum corrosion when TSP is present. • Aluminum occasionally precipitates at concentrations lower than the calculated solubility for Al(OH){sub 3}. • Corrosion and solubility equations can be used to calculate the solids generated during a LOCA. - Abstract: Bench experiments were conducted to investigate the effect of the presence of trisodium phosphate (TSP) on the corrosion and release of aluminum from metallic aluminum surfaces under conditions representative of the containment pool following a postulated loss of coolant accident at a nuclear power generating facility. The experiments showed that TSP is capable of passivating the aluminum surface and preventing continued corrosion after about 24 h at the conditions tested. A correlation that describes the rate of corrosion including the passivation effect was developed from the bench experiments and validated with a separate set of experiments from a different test system. The saturation concentration of aluminum was shown to be well described by the solubility of amorphous aluminum hydroxide for the majority of cases, but instances have been observed when aluminum precipitates at concentrations lower than the calculated aluminum hydroxide solubility. Based on the experimental data and previous literature, an equation was developed to calculate the saturation concentration of aluminum as a function of pH and temperature under conditions representative of a loss of coolant accident (LOCA) in a TSP-buffered pressurized water reactor (PWR) containment. The corrosion equation and precipitation equation can be used in concert with each other to calculate the quantity of solids that would form as a function of time during a LOCA if the temperature and pH profiles were known.

  16. Corrosion and solubility in a TSP-buffered chemical environment following a loss of coolant accident: Part 1 – Aluminum

    International Nuclear Information System (INIS)

    Howe, Kerry J.; Mitchell, Lana; Kim, Seung-Jun; Blandford, Edward D.; Kee, Ernest J.

    2015-01-01

    Highlights: • Trisodium phosphate (TSP) causes aluminum corrosion to cease after 24 h of exposure. • Chloride, iron, and copper have a minimal effect on the rate of aluminum corrosion when TSP is present. • Zinc can reduce the rate of aluminum corrosion when TSP is present. • Aluminum occasionally precipitates at concentrations lower than the calculated solubility for Al(OH) 3 . • Corrosion and solubility equations can be used to calculate the solids generated during a LOCA. - Abstract: Bench experiments were conducted to investigate the effect of the presence of trisodium phosphate (TSP) on the corrosion and release of aluminum from metallic aluminum surfaces under conditions representative of the containment pool following a postulated loss of coolant accident at a nuclear power generating facility. The experiments showed that TSP is capable of passivating the aluminum surface and preventing continued corrosion after about 24 h at the conditions tested. A correlation that describes the rate of corrosion including the passivation effect was developed from the bench experiments and validated with a separate set of experiments from a different test system. The saturation concentration of aluminum was shown to be well described by the solubility of amorphous aluminum hydroxide for the majority of cases, but instances have been observed when aluminum precipitates at concentrations lower than the calculated aluminum hydroxide solubility. Based on the experimental data and previous literature, an equation was developed to calculate the saturation concentration of aluminum as a function of pH and temperature under conditions representative of a loss of coolant accident (LOCA) in a TSP-buffered pressurized water reactor (PWR) containment. The corrosion equation and precipitation equation can be used in concert with each other to calculate the quantity of solids that would form as a function of time during a LOCA if the temperature and pH profiles were known

  17. Issues concerning the determination of solubility products of sparingly soluble crystalline solids. Solubility of HfO2(cr)

    International Nuclear Information System (INIS)

    Rai, Dhanpat; Kitamura, Akira; Rosso, Kevin M.; Sasaki, Takayuki; Kobayashi, Taishi

    2016-01-01

    Solubility studies were conducted with HfO 2 (cr) solid as a function HCl and ionic strength ranging from 2.0 to 0.004 mol kg -1 . These studies involved (1) using two different amounts of the solid phase, (2) acid washing the bulk solid phase, (3) preheating the solid phase to 1400 C, and (4) heating amorphous HfO 2 (am) suspensions to 90 C to ascertain whether the HfO 2 (am) converts to HfO 2 (cr) and to determine the solubility from the oversaturation direction. Based on the results of these treatments it is concluded that the HfO 2 (cr) contains a small fraction of less crystalline, but not amorphous, material [HfO 2 (lcr)] and this, rather than the HfO 2 (cr), is the solubility-controlling phase in the range of experimental variables investigated in this study. The solubility data are interpreted using both the Pitzer and SIT models and they provide log 10 K 0 values of -(59.75±0.35) and -(59.48±0.41), respectively, for the solubility product of HfO 2 (lcr)[HfO 2 (lcr) + 2H 2 O ↔ Hf 4+ + 4OH - ]. The log 10 of the solubility product of HfO 2 (cr) is estimated to be < -63. The observation of a small fraction of less crystalline higher solubility material is consistent with the general picture that mineral surfaces are often structurally and/or compositionally imperfect leading to a higher solubility than the bulk crystalline solid. This study stresses the urgent need, during interpretation of solubility data, of taking precautions to make certain that the observed solubility behavior for sparingly-soluble solids is assigned to the proper solid phase.

  18. Issues concerning the determination of solubility products of sparingly soluble crystalline solids. Solubility of HfO{sub 2}(cr)

    Energy Technology Data Exchange (ETDEWEB)

    Rai, Dhanpat [Rai Enviro-Chem, LLC, Yachats, OR (United States); Kitamura, Akira [Japan Atomic Energy Agency, Ibaraki (Japan); Rosso, Kevin M. [Pacific Northwest National Laboratory, Richland, WA (United States); Sasaki, Takayuki; Kobayashi, Taishi [Kyoto Univ. (Japan)

    2016-11-01

    Solubility studies were conducted with HfO{sub 2}(cr) solid as a function HCl and ionic strength ranging from 2.0 to 0.004 mol kg{sup -1}. These studies involved (1) using two different amounts of the solid phase, (2) acid washing the bulk solid phase, (3) preheating the solid phase to 1400 C, and (4) heating amorphous HfO{sub 2}(am) suspensions to 90 C to ascertain whether the HfO{sub 2}(am) converts to HfO{sub 2}(cr) and to determine the solubility from the oversaturation direction. Based on the results of these treatments it is concluded that the HfO{sub 2}(cr) contains a small fraction of less crystalline, but not amorphous, material [HfO{sub 2}(lcr)] and this, rather than the HfO{sub 2}(cr), is the solubility-controlling phase in the range of experimental variables investigated in this study. The solubility data are interpreted using both the Pitzer and SIT models and they provide log{sub 10} K{sup 0} values of -(59.75±0.35) and -(59.48±0.41), respectively, for the solubility product of HfO{sub 2}(lcr)[HfO{sub 2}(lcr) + 2H{sub 2}O ↔ Hf{sup 4+} + 4OH{sup -}]. The log{sub 10} of the solubility product of HfO{sub 2}(cr) is estimated to be < -63. The observation of a small fraction of less crystalline higher solubility material is consistent with the general picture that mineral surfaces are often structurally and/or compositionally imperfect leading to a higher solubility than the bulk crystalline solid. This study stresses the urgent need, during interpretation of solubility data, of taking precautions to make certain that the observed solubility behavior for sparingly-soluble solids is assigned to the proper solid phase.

  19. Corrosion-product transport, oxidation state and remedial measures

    International Nuclear Information System (INIS)

    Sawicki, J.A.; Brett, M.E.; Tapping, R.L.

    1998-01-01

    The issues associated with monitoring and controlling corrosion-product transport (CPT) in the balance-of-plant (BOP) and steam generators (SG) of CANDU stations are briefly reviewed. The efforts are focused on minimizing corrosion of carbon steel, which is used extensively in the CANDU primary and secondary systems. Emphasis is placed on the corrosion-product oxidation state as a monitor of water chemistry effectiveness, and as a monitor of system corrosion effects. The discussion is based mostly on the results and observations from Ontario Hydro plants, and their comparisons with PWRs. The effects of low oxygen and elevated hydrazine chemistry are reviewed, as well as the effects of lay-up and various start-up conditions. Progress in monitoring electrochemical potential (ECP) at Ontario Hydro plants and its relationship to the oxidation state of corrosion products is reviewed. Observations on corrosion-product transport on the primary side of steam generators are also discussed. (author)

  20. Production of soluble Neprilysin by endothelial cells

    International Nuclear Information System (INIS)

    Kuruppu, Sanjaya; Rajapakse, Niwanthi W.; Minond, Dmitriy; Smith, A. Ian

    2014-01-01

    Highlights: • A soluble full-length form of Neprilysin exists in media of endothelial cells. • Exosomal release is the key mechanism for the production of soluble Neprilysin. • Inhibition of ADAM-17 by specific inhibitors reduce Neprilysin release. • Exosome mediated release of Neprilysin is dependent on ADAM-17 activity. - Abstract: A non-membrane bound form of Neprilysin (NEP) with catalytic activity has the potential to cleave substrates throughout the circulation, thus leading to systemic effects of NEP. We used the endothelial cell line Ea.hy926 to identify the possible role of exosomes and A Disintegrin and Metalloprotease 17 (ADAM-17) in the production of non-membrane bound NEP. Using a bradykinin based quenched fluorescent substrate (40 μM) assay, we determined the activity of recombinant human NEP (rhNEP; 12 ng), and NEP in the media of endothelial cells (10% v/v; after 24 h incubation with cells) to be 9.35 ± 0.70 and 6.54 ± 0.41 μmols of substrate cleaved over 3 h, respectively. The presence of NEP in the media was also confirmed by Western blotting. At present there are no commercially available inhibitors specific for ADAM-17. We therefore synthesised two inhibitors TPI2155-14 and TPI2155-17, specific for ADAM-17 with IC 50 values of 5.36 and 4.32 μM, respectively. Treatment of cells with TPI2155-14 (15 μM) and TPI2155-17 (4.3 μM) resulted in a significant decrease in NEP activity in media (62.37 ± 1.43 and 38.30 ± 4.70, respectively as a % of control; P < 0.0001), implicating a possible role for ADAM-17 in NEP release. However, centrifuging media (100,000g for 1 h at 4 °C) removed all NEP activity from the supernatant indicating the likely role of exosomes in the release of NEP. Our data therefore indicated for the first time that NEP is released from endothelial cells via exosomes, and that this process is dependent on ADAM-17

  1. Solubility Products of M(II) - Carbonates

    International Nuclear Information System (INIS)

    Grauer, Rolf; Berner, Urs

    1999-01-01

    Many solubility data for M(II) carbonates commonly compiled in tables are contradictory and sometimes obviously wrong. The quality of such data has been evaluated based on the original publications and reliable solubility constants have been selected for the carbonates of Mn, Fe, Co, Ni, Cu, Zn, Cd and Pb with the help of cross-comparisons. (author)

  2. Preparations and properties of anti-corrosion additives of water-soluble metal working fluids for aluminum alloy materials.

    Science.gov (United States)

    Watanabe, Shoji

    2008-01-01

    This short review describes various types of anti-corrosion additives of water-soluble metal working fluids for aluminum alloy materials. It is concerned with synthetic additives classified according to their functional groups; silicone compounds, carboxylic acids and dibasic acids, esters, Diels-Alder adducts, various polymers, nitrogen compounds, phosphoric esters, phosphonic acids, and others. Testing methods for water-soluble metal working fluids for aluminum alloy materials are described for a practical application in a laboratory.

  3. Study on influence of native oxide and corrosion products on atmospheric corrosion of pure Al

    International Nuclear Information System (INIS)

    Liu, Yanjie; Wang, Zhenyao; Ke, Wei

    2014-01-01

    Highlights: •Corrosion products layer is only formed in coastal atmosphere. •In coastal atmosphere, rate controlling step is diffusion process. •In rural atmosphere, rate controlling step is charge transfer process. •Pitting area increases greatly in coastal site, but slightly in rural site. -- Abstract: Effects of native oxide and corrosion products on atmospheric corrosion of aluminium in rural and coastal sites were studied by electrochemical impedance spectroscopy (EIS), open-circuit potential (OCP) and scanning electron microscope (SEM) techniques after outdoor exposure. In the rural atmosphere, only the compact, adhesive native oxide layer exists, and the rate controlling step is diffusion process, while in the coastal atmosphere, another loose, inadhesive corrosion products layer exists, and a charge transfer process controls the corrosion process. The pitting area in the coastal atmosphere increases over time more obviously than that in the rural atmosphere

  4. Corrosion-product inventory: the Bruce-B secondary system

    International Nuclear Information System (INIS)

    Sawicki, J.A.; Price, J.; Brett, M.E.

    1995-01-01

    Corrosion inspection and corrosion-product characterization in water and steam systems are important for component and systems maintenance in nuclear power stations. Corrosion products are produced, released and redeposited at various sites in the secondary system. Depending on the alloys used in the condenser and feedwater heaters, particulate iron oxides and hydroxides can account for about 95-99% of the total corrosion-product transport. Where brass or cupro-nickel alloys are present, copper and zinc contribute significantly to the total transport and deposition. Particulates are transported by the feedwater to the steam generators, where they accumulate and can cause a variety of problems, such as loss of heat transfer capability through deposition on boiler tubes, blockage of flow through boiler-tube support plates and accelerated corrosion in crevices, either in deep sludge piles or at blocked tube supports. The influx of oxidized corrosion products may have a particularly adverse effect on the redox environment of steam generator tubing, thereby increasing the probability of localized corrosion and other degradation mechanisms. In this paper, there is a description of a survey of general corrosion deposits in Bruce-B, Units 5-8, which helps to identify the origin, evolution and inventory of corrosion products along the secondary system of Candu reactors

  5. Thermodynamics and the transport of corrosion products in PWR primary circuits

    International Nuclear Information System (INIS)

    Turner, D.J.

    1992-01-01

    It is argued that practically useful models for the activation, transport and deposition of corrosion products in PWR primary circuits can only be produced on the basis of an improved understanding of the chemical processes which control them. In particular, if a model is to make reliable predictions it is essential that its thermodynamic basis be sound. This is not the case with most current models which employ the erroneous concept of a corrosion product 'solubility'. In addition to the misuse of this term, other complications are discussed. These include the need to take account of the consequences of Gibbs' phase rule and the fact that, for mixed spinels, neither the concept of a thermodynamic solubility nor of a solubility product is valid. There is no reason to believe that measured apparent solubilities of nickel ferrites or spinel mixtures containing cobalt can give any direct guidance on the direction of transport of Ni or Co in PWR primary circuits. This is more likely to be determined by the distribution of stable and unstable ferrites and chromites than by any temperature coefficient of apparent solubility. Most of the transport of Ni and Co into and out of the core probably occurs as a consequence of either chemical or mechanical transients. Most important is likely to be the oxidative destruction and subsequent re-precipitation of chromites which occurs as a consequence of the oxygenated conditions employed during plant shutdown. (author)

  6. Treatment of coaly substances. [production of soluble products

    Energy Technology Data Exchange (ETDEWEB)

    Janner, J; Gonre, O

    1928-05-01

    A process is described for the production of soluble products from coaly substances. The process consists of heating coal or the like under pressure, and if desired with the addition of gases or vapors which do not react to a substantial extent with the coaly matter under the conditions of working. The product may be treated with a solvent at an elevated temperature and under pressure, with or without the addition of said gases or vapors. The products obtained by the above process may be subjected to a further treatment, in particular a cracking process and/or a destructive hydrogenation. The products may also be separated by the aid of suitable solvents into resins, waxes, and other substances.

  7. Solubility Products of M(II) - Carbonates

    Energy Technology Data Exchange (ETDEWEB)

    Grauer, Rolf; Berner, Urs [ed.

    1999-01-01

    Many solubility data for M(II) carbonates commonly compiled in tables are contradictory and sometimes obviously wrong. The quality of such data has been evaluated based on the original publications and reliable solubility constants have been selected for the carbonates of Mn, Fe, Co, Ni, Cu, Zn, Cd and Pb with the help of cross-comparisons. (author) translated from a PSI internal report written in German in 1994 (TM-44-94-05). 5 figs., 1 tab., 68 refs.

  8. High temperature corrosion during biomass firing: improved understanding by depth resolved characterisation of corrosion products

    DEFF Research Database (Denmark)

    Okoro, Sunday Chukwudi; Montgomery, Melanie; Jappe Frandsen, Flemming

    2015-01-01

    changes within the near surface region (covering both the deposit and the steel surface). Such cross-section analysis was further complemented by plan view investigations (additionally involving X-ray diffraction) combined with removal of the corrosion products. Improved insights into the nature......The high temperature corrosion of an austenitic stainless steel (TP 347H FG), widely utilised as a superheater tube material in Danish power stations, was investigated to verify the corrosion mechanisms related to biomass firing. KCl coated samples were exposed isothermally to 560 degrees C...... of the corrosion products as a function of distance from the deposit surface were revealed through this comprehensive characterisation. Corrosion attack during simulated straw-firing conditions was observed to occur through both active oxidation and sulphidation mechanisms....

  9. Oxidation kinetics of reaction products formed in uranium metal corrosion

    International Nuclear Information System (INIS)

    Totemeier, T. C.

    1998-01-01

    The oxidation behavior of uranium metal ZPPR fuel corrosion products in environments of Ar-4%O 2 and Ar-20%O 2 were studied using thermo-gravimetric analysis (TGA). These tests were performed to extend earlier work in this area specifically, to assess plate-to-plate variations in corrosion product properties and the effect of oxygen concentration on oxidation behavior. The corrosion products from two relatively severely corroded plates were similar, while the products from a relatively intact plate were not reactive. Oxygen concentration strongly affected the burning rate of reactive products, but had little effect on low-temperature oxidation rates

  10. Oxidation kinetics of reaction products formed in uranium metal corrosion.

    Energy Technology Data Exchange (ETDEWEB)

    Totemeier, T. C.

    1998-04-22

    The oxidation behavior of uranium metal ZPPR fuel corrosion products in environments of Ar-4%O{sub 2} and Ar-20%O{sub 2} were studied using thermo-gravimetric analysis (TGA). These tests were performed to extend earlier work in this area specifically, to assess plate-to-plate variations in corrosion product properties and the effect of oxygen concentration on oxidation behavior. The corrosion products from two relatively severely corroded plates were similar, while the products from a relatively intact plate were not reactive. Oxygen concentration strongly affected the burning rate of reactive products, but had little effect on low-temperature oxidation rates.

  11. Corrosion products study of alcohol by Mossbauer spectroscopy

    International Nuclear Information System (INIS)

    Velazquez, R.; Gil de Larre, M.

    1995-01-01

    Simulated corrosion essays in alcohol is presented and corrosion products of storage tanks (CAPASA) were analyzed. The analysis by Mossbauer absortion and transmission spectroscopy shows the formation of hematite substratum in the rust of the storage tanks of carburetant and burning alcohol. In the sample of corrosion with strong rum shows the formation of lepidocrocite and with destilled water besides of lepidocrocite, magnetite (Fe3 O4) is detected

  12. Kinetics of Corrosion Inhibition of Aluminum in Acidic Media by Water-Soluble Natural Polymeric Pectates as Anionic Polyelectrolyte Inhibitors.

    Science.gov (United States)

    Hassan, Refat M; Zaafarany, Ishaq A

    2013-06-17

    Corrosion inhibition of aluminum (Al) in hydrochloric acid by anionic polyeletrolyte pectates (PEC) as a water-soluble natural polymer polysaccharide has been studied using both gasometric and weight loss techniques. The results drawn from these two techniques are comparable and exhibit negligible differences. The inhibition efficiency was found to increase with increasing inhibitor concentration and decrease with increasing temperature. The inhibition action of PEC on Al metal surface was found to obey the Freundlich isotherm. Factors such as the concentration and geometrical structure of the inhibitor, concentration of the corrosive medium, and temperature affecting the corrosion rates were examined. The kinetic parameters were evaluated and a suitable corrosion mechanism consistent with the kinetic results is discussed in the paper.

  13. Kinetics of Corrosion Inhibition of Aluminum in Acidic Media by Water-Soluble Natural Polymeric Pectates as Anionic Polyelectrolyte Inhibitors

    Directory of Open Access Journals (Sweden)

    Refat M. Hassan

    2013-06-01

    Full Text Available Corrosion inhibition of aluminum (Al in hydrochloric acid by anionic polyeletrolyte pectates (PEC as a water-soluble natural polymer polysaccharide has been studied using both gasometric and weight loss techniques. The results drawn from these two techniques are comparable and exhibit negligible differences. The inhibition efficiency was found to increase with increasing inhibitor concentration and decrease with increasing temperature. The inhibition action of PEC on Al metal surface was found to obey the Freundlich isotherm. Factors such as the concentration and geometrical structure of the inhibitor, concentration of the corrosive medium, and temperature affecting the corrosion rates were examined. The kinetic parameters were evaluated and a suitable corrosion mechanism consistent with the kinetic results is discussed in the paper.

  14. Corrosion-product transport, oxidation state and remedial measures

    International Nuclear Information System (INIS)

    Sawicki, J.A.; Brett, M.E.; Tapping, R.L.

    1998-10-01

    The issues associated with monitoring and controlling corrosion-product transport (CPT) in the balance-of-plant (BOP) and steam generators (SG) of CANDU stations are briefly reviewed. Efforts are focused on minimizing corrosion of carbon steel, which is used extensively in the CANDU primary and secondary systems. Emphasis is placed on the corrosion-product oxidation state as a monitor of water chemistry effectiveness and as a monitor of system corrosion effects. The discussion is based mostly on the results of observations from Ontario Hydro plants, and their comparisons with pressurized-water reactors. The effects of low oxygen and elevated hydrazine chemistry are reviewed, as well as the effects of layup and various startup conditions. Progress in monitoring electrochemical potential (ECP) at Ontario Hydro plants and its relationship to the oxidation state of corrosion products is reviewed. Observations on CPT on the primary side of SGs are also discussed. (author)

  15. Penetration of corrosion products and corrosion-induced cracking in reinforced cementitious materials

    DEFF Research Database (Denmark)

    Michel, Alexander; Pease, Brad J.; Peterova, Adela

    2014-01-01

    This paper describes experimental investigations on corrosion-induced deterioration in reinforced cementitious materials and the subsequent development and implementation of a novel conceptual model. Rejnforced mortar specimens of varying water-to-cement ratios were subjected to current-induced c......This paper describes experimental investigations on corrosion-induced deterioration in reinforced cementitious materials and the subsequent development and implementation of a novel conceptual model. Rejnforced mortar specimens of varying water-to-cement ratios were subjected to current......-dependent concentrations of corrosion products averaged through the specimen thickness. Digital image correlation (DIC) was used to measure corrosion-induced deformations including deformations between steel and cementitious matrix as well as formation and propagation of corrosion-induced cracks. Based on experimental...... observations, a conceptual model was developed to describe the penetration of solid corrosion products into capillary pores of the cementitious matrix. Only capillary pores within a corrosion accommodating region (CAR), i.e. in close proximity of the steel reinforcement, were considered accessible...

  16. A non-destructive test method to monitor corrosion products and corrosion-induced cracking in reinforced cement based materials

    DEFF Research Database (Denmark)

    Michel, Alexander; Pease, Bradley Justin; Peterova, Adela

    2011-01-01

    ) was conducted to describe the impact of water-to-cement ratio and corrosion current density (i.e., corrosion rate) on the reinforcement corrosion process. Focus was placed, in particular on the determination of the corrosion accommodating region (CAR) and time to corrosion-induced cracking. Experimental results...... showed that x-ray attenuation measurements allow determination of the actual concentrations of corrosion products averaged through the specimen thickness. The total mass loss of steel measured by x-ray attenuation was found to be in very good agreement with the calculated mass loss obtained by Faraday......’s law. Furthermore, experimental results demonstrated that the depth of penetration of corrosion products as well as time to corrosion-induced cracking is varying for the different water-to-cement ratios and applied corrosion current densities....

  17. Spatial distribution of crystalline corrosion products formed during corrosion of stainless steel in concrete

    Energy Technology Data Exchange (ETDEWEB)

    Serdar, Marijana [Department of Materials, Faculty of Civil Engineering, University of Zagreb, 10000 Zagreb (Croatia); Meral, Cagla [Middle East Technical University, Department of Civil Engineering, Ankara (Turkey); Kunz, Martin [Lawrence Berkeley National Laboratory, 1 Cyclotron Road, Berkeley, CA 94720 (United States); Bjegovic, Dubravka [Department of Materials, Faculty of Civil Engineering, University of Zagreb, 10000 Zagreb (Croatia); Wenk, Hans-Rudolf [Department of Earth and Planetary Science, University of California, Berkeley, CA 94720 (United States); Monteiro, Paulo J.M., E-mail: monteiro@ce.berkeley.edu [Department of Civil and Environmental Engineering, University of California, Berkeley, CA 94720 (United States)

    2015-05-15

    The mineralogy and spatial distribution of nano-crystalline corrosion products that form in the steel/concrete interface were characterized using synchrotron X-ray micro-diffraction (μ-XRD). Two types of low-nickel high-chromium reinforcing steels embedded into mortar and exposed to NaCl solution were investigated. Corrosion in the samples was confirmed by electrochemical impedance spectroscopy (EIS). μ-XRD revealed that goethite (α-FeOOH) and akaganeite (β-FeOOH) are the main iron oxide–hydroxides formed during the chloride-induced corrosion of stainless steel in concrete. Goethite is formed closer to the surface of the steel due to the presence of chromium in the steel, while akaganeite is formed further away from the surface due to the presence of chloride ions. Detailed microstructural analysis is shown and discussed on one sample of each type of steel. - Highlights: • Synchrotron micro-diffraction used to map the distribution of crystalline phases. • Goethite and akaganeite are the main corrosion products during chloride induced corrosion in mortar. • Layers of goethite and akaganeite are negatively correlated. • EDS showed Cr present in corrosion products identified by SEM.

  18. Spatial distribution of crystalline corrosion products formed during corrosion of stainless steel in concrete

    International Nuclear Information System (INIS)

    Serdar, Marijana; Meral, Cagla; Kunz, Martin; Bjegovic, Dubravka; Wenk, Hans-Rudolf; Monteiro, Paulo J.M.

    2015-01-01

    The mineralogy and spatial distribution of nano-crystalline corrosion products that form in the steel/concrete interface were characterized using synchrotron X-ray micro-diffraction (μ-XRD). Two types of low-nickel high-chromium reinforcing steels embedded into mortar and exposed to NaCl solution were investigated. Corrosion in the samples was confirmed by electrochemical impedance spectroscopy (EIS). μ-XRD revealed that goethite (α-FeOOH) and akaganeite (β-FeOOH) are the main iron oxide–hydroxides formed during the chloride-induced corrosion of stainless steel in concrete. Goethite is formed closer to the surface of the steel due to the presence of chromium in the steel, while akaganeite is formed further away from the surface due to the presence of chloride ions. Detailed microstructural analysis is shown and discussed on one sample of each type of steel. - Highlights: • Synchrotron micro-diffraction used to map the distribution of crystalline phases. • Goethite and akaganeite are the main corrosion products during chloride induced corrosion in mortar. • Layers of goethite and akaganeite are negatively correlated. • EDS showed Cr present in corrosion products identified by SEM

  19. Properties of Douglas Point Generating Station heat transport corrosion products

    International Nuclear Information System (INIS)

    Montford, B.; Rummery, T.E.

    1975-09-01

    Chemical, radiochemical and structural properties of circulating and fixed corrosion products from the Douglas Point Generating Station are documented. Interaction of Monel-400 and carbon steel corrosion products is described, and the mechanisms of Monel-400 surface deposit release, and activity buildup in the coolant system, are briefly discussed. Efficiencies of filters and ion-exchangers for the removal of released radionuclides are given. (author)

  20. Corrosion

    Science.gov (United States)

    Slabaugh, W. H.

    1974-01-01

    Presents some materials for use in demonstration and experimentation of corrosion processes, including corrosion stimulation and inhibition. Indicates that basic concepts of electrochemistry, crystal structure, and kinetics can be extended to practical chemistry through corrosion explanation. (CC)

  1. Effect of water chemistry on corrosion of stainless steel and deposition of corrosion products in high temperature pressurised water

    International Nuclear Information System (INIS)

    Morrison, Jonathan; Cooper, Christopher; Ponton, Clive; Connolly, Brian; Banks, Andrew

    2012-09-01

    In any water-cooled nuclear reactor, the corrosion of the structural materials in contact with the coolant and the deposition of the resulting oxidised species has long been an operational concern within the power generation industry. Corrosion of the structural materials at all points in the reactor leads to low concentrations of oxidised metal species in the coolant water. The oxidised metal species can subsequently be deposited out as CRUD deposits at various points around the reactor's primary and secondary loops. The deposition of soluble oxidised material at any location in the reactor cooling system is undesirable due to several effects; deposits have a porous structure, capable of incorporating radiologically active material (forming out of core radiation fields) and concentrating aggressively corrosive chemicals, which exacerbate environmental degradation of structural and fuel-cladding materials. Deposits on heat transfer surfaces also limit efficiency of the system as a whole. The work in this programme is an attempt to determine and understand the fundamental corrosion and deposition behaviour under controlled, simulated reactor conditions. The rates of corrosion of structural materials within pressurised water reactors are heavily dependent on the condition of the exposed surface. The effect of mechanical grinding and of electropolishing on the corrosion rate and structure of the resultant oxide film formed on grade 316L stainless steel exposed to high purity water, modified to pH 9.5 and 10.5 at temperatures between 200 and 300 deg. C and pressures of up to 100 bar will be investigated. The corrosion of stainless steel in water via electrochemical oxidation leads to the formation of surface iron, nickel and chromium based spinels. Low concentrations of these spinels can be found dissolved in the coolant water. The solubility of magnetite, stainless steels' major corrosion product, in high purity water will be studied at pH 9.5 to 10.5 at

  2. Corrosion of aluminum and zinc in containment following a LOCA and potential for precipitation of corrosion products in the sump

    International Nuclear Information System (INIS)

    Niyogi, K.K.; Lunt, R.R.; Mackenzie, J.S.

    1982-01-01

    Following a loss-of-coolant accident (LOCA) in a LWR containment, certain materials in the containment come in contact with alkaline emergency cooling and containment spray solutions and may corrode yielding hydrogen gas. The problems associated with the production of hydrogen gas and the control of combustible gas concentration have been extensively explored in recent years. However, the phenomenon of corrosion and its consequences in the long term cooling of the reactor and the containment have drawn very little attention. United Engineers and Constructors Inc. has made an extensive effort to study through literature survey the solubility of the corrosion products from aluminum and zinc in order to assess the potential for precipitation in the containment sump. The analysis presented in this article is based on parameters for a typical large dry reactor containment with caustic/boric acid buffered spray solution. Parameters used in this study may vary from one plant to another. However, they are not expected to affect the overall conclusions

  3. Analysis of corrosion products of carbon steel in wet bentonite

    International Nuclear Information System (INIS)

    Osada, Kazuo; Nagano, Tetsushi; Nakayama, Shinichi; Muraoka, Susumu

    1992-02-01

    As a part of evaluation of the long-term durability for the overpack containers for high-level radioactive waste, we have conducted corrosion tests for carbon steel in wet bentonite, a candidate buffer material. The corrosion rates were evaluated by weight difference of carbon steel and corrosion products were analyzed by Fourier transform infrared spectroscopy (FT-IR) and colorimetry. At 40degC, the corrosion rate of carbon steel in wet bentonite was smaller than that in pure water. At 95degC, however, the corrosion rate in wet bentonite was much higher than that in pure water. This high corrosion rate in wet bentonite at 95degC was considered to result from evaporation of moisture in bentonite in contact with the metal. This evaporation led to dryness and then to shrinkage of the bentonite, which generated ununiform contact of the metal with bentonite. Probably, this ununiform contact promoted the local corrosion. The locally corroded parts of specimen in wet bentonite at 95degC were analyzed by Fourier transform infrared microspectroscopy (micro-FT-IR), and lepidocrocite γ-FeO(OH) was found as well as goethite α-FeO(OH). In wet bentonite at 95degC, hematite α-Fe 2 O 3 was identified by means of colorimetry. (author)

  4. Characterisation of corrosion products on pipeline steel under cathodic protection

    Energy Technology Data Exchange (ETDEWEB)

    Lanarde, Lise [Gaz de France Research and Development Division, 361 avenue du President Wilson, BP33, 93211 Saint Denis La Plaine (France)]|[UPR15 du CNRS, Laboratoire des Interfaces et Systemes Electrochimiques, Universite Pierre et Marie Curie, C.P. 133, 4 Place Jussieu, 75252 Paris Cedex 05 (France); Campaignolle, Xavier; Karcher, Sebastien; Meyer, Michel [Gaz de France Research and Development Division, 361 avenue du President Wilson, BP33, 93211 Saint Denis La Plaine (France); Joiret, Suzanne [UPR15 du CNRS, Laboratoire des Interfaces et Systemes Electrochimiques, Universite Pierre et Marie Curie, C.P. 133, 4 Place Jussieu 75252 Paris Cedex 05 (France)

    2004-07-01

    Onshore gas transmission lines are conjointly protected against external corrosion by cathodic protection (CP) and organic coatings. If both protection systems are simultaneously faulty, the pipe may be subjected to local loss of protection criteria. Consequently, the development of a corrosion due to the ground intrinsic corrosiveness may occur. To guarantee an optimal and safe use of its 31000 km buried gas transmission network, Gaz de France regularly inspects its pipelines. When indications of metal damage are suspected, excavations are realized to carry out a finer diagnosis and, if necessary, to repair. Whenever, corrosions are encountered, although it occurs very scarcely, it is necessary to evaluate its degree of gravity: activity, mechanism, and kinetics. Among corrosion defects, it is indeed essential to differentiate those active, from those older inactive at the time of excavation, since those last ones may possibly have been annihilated, by a PC reinforcement for instance. Eventually, the identification of the corrosion mechanism and its associated rate will provide an assessment of the risks encountered by other sections of the pipeline similar to that excavated. This study investigates to what extent the degree of gravity (activity, kinetics) of a corrosion can be determined by the characterization and identification of its associated corrosion products. Moreover, it will attempt to relate it to the close environment features as well as to the operating conditions of the pipe. The preliminary results presented in this paper consist in a laboratory study of the time evolution of corrosion products formed on the surface of ordinary low carbon steel samples. The specimens have been previously subjected to various polarization conditions in various aqueous media. The selected solutions are characteristic of ground waters. The main parameters considered for the definition of the media were its initial chemical composition, pH and dissolved gas composition

  5. Corrosion in systems for storage and transportation of petroleum products and biofuels identification, monitoring and solutions

    CERN Document Server

    Groysman, Alec

    2014-01-01

    This book treats corrosion as it occurs and affects processes in real-world situations, and thus points the way to practical solutions. Topics described include the conditions in which petroleum products are corrosive to metals; corrosion mechanisms of petroleum products; which parts of storage tanks containing crude oils and petroleum products undergo corrosion; dependence of corrosion in tanks on type of petroleum products; aggressiveness of petroleum products to polymeric material; how microorganisms take part in corrosion of tanks and pipes containing petroleum products; which corrosion monitoring methods are used in systems for storage and transportation of petroleum products; what corrosion control measures should be chosen; how to choose coatings for inner and outer surfaces of tanks containing petroleum products; and how different additives (oxygenates, aromatic solvents) to petroleum products and biofuels influence metallic and polymeric materials. The book is of interest to corrosion engineers, mat...

  6. Corrosion behaviors and effects of corrosion products of plasma electrolytic oxidation coated AZ31 magnesium alloy under the salt spray corrosion test

    Science.gov (United States)

    Wang, Yan; Huang, Zhiquan; Yan, Qin; Liu, Chen; Liu, Peng; Zhang, Yi; Guo, Changhong; Jiang, Guirong; Shen, Dejiu

    2016-08-01

    The effects of corrosion products on corrosion behaviors of AZ31 magnesium alloy with a plasma electrolytic oxidation (PEO) coating were investigated under the salt spray corrosion test (SSCT). The surface morphology, cross-sectional microstructure, chemical and phase compositions of the PEO coating were determined using scanning electron microscopy (SEM) equipped with energy dispersive X-ray spectroscopy (EDS) and X-ray diffraction analysis (XRD), respectively. Further, the corrosion process of the samples under the SSCT was examined in a non-aqueous electrolyte (methanol) using electrochemical impedance spectroscopy (EIS) coupled with equivalent circuit. The results show that the inner layer of the coating was destroyed firstly and the corrosion products have significant effects on the corrosion behaviors of the coating. The results above are discussed and an electrochemical corrosion model is proposed in the paper.

  7. Corrosion behaviors and effects of corrosion products of plasma electrolytic oxidation coated AZ31 magnesium alloy under the salt spray corrosion test

    International Nuclear Information System (INIS)

    Wang, Yan; Huang, Zhiquan; Yan, Qin; Liu, Chen; Liu, Peng; Zhang, Yi; Guo, Changhong; Jiang, Guirong; Shen, Dejiu

    2016-01-01

    Highlights: • Corrosion behaviors of a PEO coating was investigated after the salt spray test. • Corrosion products have significant effects on corrosion behaviors of the coating. • An electrochemical corrosion model is proposed. - Abstract: The effects of corrosion products on corrosion behaviors of AZ31 magnesium alloy with a plasma electrolytic oxidation (PEO) coating were investigated under the salt spray corrosion test (SSCT). The surface morphology, cross-sectional microstructure, chemical and phase compositions of the PEO coating were determined using scanning electron microscopy (SEM) equipped with energy dispersive X-ray spectroscopy (EDS) and X-ray diffraction analysis (XRD), respectively. Further, the corrosion process of the samples under the SSCT was examined in a non-aqueous electrolyte (methanol) using electrochemical impedance spectroscopy (EIS) coupled with equivalent circuit. The results show that the inner layer of the coating was destroyed firstly and the corrosion products have significant effects on the corrosion behaviors of the coating. The results above are discussed and an electrochemical corrosion model is proposed in the paper.

  8. Corrosion behaviors and effects of corrosion products of plasma electrolytic oxidation coated AZ31 magnesium alloy under the salt spray corrosion test

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Yan; Huang, Zhiquan; Yan, Qin; Liu, Chen; Liu, Peng; Zhang, Yi [State Key Laboratory of Metastable Materials Science and Technology, College of Materials Science and Engineering, Yanshan University, Qinhuangdao 066004 (China); Guo, Changhong; Jiang, Guirong [College of Mechanical Engineering, Yanshan University, Qinhuangdao 066004 (China); Shen, Dejiu, E-mail: DejiuShen@163.com [State Key Laboratory of Metastable Materials Science and Technology, College of Materials Science and Engineering, Yanshan University, Qinhuangdao 066004 (China)

    2016-08-15

    Highlights: • Corrosion behaviors of a PEO coating was investigated after the salt spray test. • Corrosion products have significant effects on corrosion behaviors of the coating. • An electrochemical corrosion model is proposed. - Abstract: The effects of corrosion products on corrosion behaviors of AZ31 magnesium alloy with a plasma electrolytic oxidation (PEO) coating were investigated under the salt spray corrosion test (SSCT). The surface morphology, cross-sectional microstructure, chemical and phase compositions of the PEO coating were determined using scanning electron microscopy (SEM) equipped with energy dispersive X-ray spectroscopy (EDS) and X-ray diffraction analysis (XRD), respectively. Further, the corrosion process of the samples under the SSCT was examined in a non-aqueous electrolyte (methanol) using electrochemical impedance spectroscopy (EIS) coupled with equivalent circuit. The results show that the inner layer of the coating was destroyed firstly and the corrosion products have significant effects on the corrosion behaviors of the coating. The results above are discussed and an electrochemical corrosion model is proposed in the paper.

  9. A computer simulation of iron corrosion in a sodium loop using the Fleitman-Isaacs' solubility relationship

    International Nuclear Information System (INIS)

    Polley, M.V.; Skyrme, G.

    1975-11-01

    At the present time, no theoretical treatment of mass transfer in sodium loops has been able to reconcile the low observed corrosion rates with values of iron solubility recommended in the literature. Although measured values of the solubility of iron in sodium have varied very widely, one recent determination by Fleitman and Isaacs gave low values at low oxygen activities. These values were used in the present work for predicting, by conventional mass transfer theory, corrosion in a non-isothermal loop. The method was to simulate mass transfer using a computer program while following the sodium around the loop until equilibrium was established. The advantages of this method are that the concentration driving force is predicted for all parts of the loop and that changes in mass transfer rates with change in temperature distribution and geometry can be easily investigated. The predicted variation of corrosion rate in the hot isothermal region is reported as a function of sodium velocity, downstream position, temperature, temperature differential, oxygen concentration and loop geometry. Both surface controlled and diffusion controlled mass transfer were investigated and the results were compared with the data of Thorley and Tyzack reported in the literature. (author)

  10. Spatial distribution of crystalline corrosion products formed during corrosion of stainless steel in concrete

    KAUST Repository

    Serdar, Marijana

    2015-05-01

    © 2015 Elsevier Ltd All rights reserved. The mineralogy and spatial distribution of nano-crystalline corrosion products that form in the steel/concrete interface were characterized using synchrotron X-ray micro-diffraction (μ-XRD). Two types of low-nickel high-chromium reinforcing steels embedded into mortar and exposed to NaCl solution were investigated. Corrosion in the samples was confirmed by electrochemical impedance spectroscopy (EIS). μ-XRD revealed that goethite (α-FeOOH) and akaganeite (β-FeOOH) are the main iron oxide-hydroxides formed during the chloride-induced corrosion of stainless steel in concrete. Goethite is formed closer to the surface of the steel due to the presence of chromium in the steel, while akaganeite is formed further away from the surface due to the presence of chloride ions. Detailed microstructural analysis is shown and discussed on one sample of each type of steel.

  11. Spatial distribution of crystalline corrosion products formed during corrosion of stainless steel in concrete

    KAUST Repository

    Serdar, Marijana; Meral, Cagla; Kunz, Martin; Bjegovic, Dubravka; Wenk, Hans-Rudolf; Monteiro, Paulo J.M.

    2015-01-01

    © 2015 Elsevier Ltd All rights reserved. The mineralogy and spatial distribution of nano-crystalline corrosion products that form in the steel/concrete interface were characterized using synchrotron X-ray micro-diffraction (μ-XRD). Two types of low-nickel high-chromium reinforcing steels embedded into mortar and exposed to NaCl solution were investigated. Corrosion in the samples was confirmed by electrochemical impedance spectroscopy (EIS). μ-XRD revealed that goethite (α-FeOOH) and akaganeite (β-FeOOH) are the main iron oxide-hydroxides formed during the chloride-induced corrosion of stainless steel in concrete. Goethite is formed closer to the surface of the steel due to the presence of chromium in the steel, while akaganeite is formed further away from the surface due to the presence of chloride ions. Detailed microstructural analysis is shown and discussed on one sample of each type of steel.

  12. Process for radiation cocrosslinking water soluble polymers and products thereof

    International Nuclear Information System (INIS)

    Assarsson, P.G.; King, P.A.

    1976-01-01

    Poly(ethylene oxide) and at least one other water soluble polymer are conveniently cocrosslinked by exposing aqueous systems of the polymers to high energy irradiation. The resulting products are insoluble hydrophilic gels which can contain or when dried absorb large quantities of aqueous fluids and hence are useful as absorbing media for disposable absorbent articles, agricultural applications and the like

  13. Purification, product characterization and kinetic properties of soluble tomato lipoxygenase

    NARCIS (Netherlands)

    Vliegenthart, J.F.G.; Suurmeijer, C.N.S.P.; Pérez-Gilabert, M.; Hijden, H.T.W.M. van der; Veldink, G.A.

    1998-01-01

    Soluble lipoxygenase (EC 1.13.11.12) from tomato fruits (Lycopersicon esculentum, var. Trust) was purified to apparent homogeneity as judged by SDS-PAGE, and the products and kinetics of the enzyme were studied in order to clarify the contradictory results that were obtained with a less purified

  14. Influence of temperature on corrosion rate and porosity of corrosion products of carbon steel in anoxic bentonite environment

    International Nuclear Information System (INIS)

    Stoulil, J.; Kaňok, J.; Kouřil, M.; Parschová, H.; Novák, P.

    2013-01-01

    Highlights: •The corrosion rate is not significantly dependent on temperature. •Corrosion products at higher temperatures have different color. •Corrosion products at higher temperatures are more compact. •The change in corrosion products nature is reversible. -- Abstract: The study focuses on the porosity of layers of corrosion products and its impact on corrosion rate of carbon steel in moist bentonite. Measurements were performed in an aggressive Czech type of bentonite – Rokle B75 at temperatures of 90 and 40 °C. Aggressiveness of B75 bentonite consists in low content of chlorides. Presence of chlorides in pore solution allows formation of more protective magnetite. The evaluation was made by electrochemical techniques (red/ox potential, open circuit potential, linear polarization resistance, impedance spectroscopy) and resistometric sensor measurements. The result imply that the higher the temperature the more compact is the layer of corrosion products that slightly decelerates corrosion rate compared to the state at 40 °C. The state of corrosion products at both temperatures is reversible

  15. Influence of temperature on corrosion rate and porosity of corrosion products of carbon steel in anoxic bentonite environment

    Energy Technology Data Exchange (ETDEWEB)

    Stoulil, J., E-mail: jan.stoulil@vscht.cz [Department of Metals and Corrosion Engineering, Institute of Chemical Technology, Prague (Czech Republic); Kaňok, J.; Kouřil, M. [Department of Metals and Corrosion Engineering, Institute of Chemical Technology, Prague (Czech Republic); Parschová, H. [Department of Power Engineering, Institute of Chemical Technology, Prague (Czech Republic); Novák, P. [Department of Metals and Corrosion Engineering, Institute of Chemical Technology, Prague (Czech Republic)

    2013-11-15

    Highlights: •The corrosion rate is not significantly dependent on temperature. •Corrosion products at higher temperatures have different color. •Corrosion products at higher temperatures are more compact. •The change in corrosion products nature is reversible. -- Abstract: The study focuses on the porosity of layers of corrosion products and its impact on corrosion rate of carbon steel in moist bentonite. Measurements were performed in an aggressive Czech type of bentonite – Rokle B75 at temperatures of 90 and 40 °C. Aggressiveness of B75 bentonite consists in low content of chlorides. Presence of chlorides in pore solution allows formation of more protective magnetite. The evaluation was made by electrochemical techniques (red/ox potential, open circuit potential, linear polarization resistance, impedance spectroscopy) and resistometric sensor measurements. The result imply that the higher the temperature the more compact is the layer of corrosion products that slightly decelerates corrosion rate compared to the state at 40 °C. The state of corrosion products at both temperatures is reversible.

  16. Application of Moessbauer spectroscopy on corrosion products of NPP

    Energy Technology Data Exchange (ETDEWEB)

    Dekan, J., E-mail: julius.dekan@stuba.sk; Lipka, J.; Slugen, V. [Institute of Nuclear and Physical Engineering, Faculty of Electrical Engineering and Information Technology, SUT (Slovakia)

    2013-04-15

    Steam generator (SG) is generally one of the most important components at all nuclear power plants (NPP) with close impact to safe and long-term operation. Material degradation and corrosion/erosion processes are serious risks for long-term reliable operation. Steam generators of four VVER-440 units at nuclear power plants V-1 and V-2 in Jaslovske Bohunice (Slovakia) were gradually changed by new original 'Bohunice' design in period 1994-1998, in order to improve corrosion resistance of SGs. Corrosion processes before and after these design and material changes in Bohunice secondary circuit were studied using Moessbauer spectroscopy during last 25 years. Innovations in the feed water pipeline design as well as material composition improvements were evaluated positively. Moessbauer spectroscopy studies of phase composition of corrosion products were performed on real specimens scrapped from water pipelines or in form of filters deposits. Newest results in our long-term corrosion study confirm good operational experiences and suitable chemical regimes (reduction environment) which results mostly in creation of magnetite (on the level 70 % or higher) and small portions of hematite, goethite or hydrooxides. Regular observation of corrosion/erosion processes is essential for keeping NPP operation on high safety level. The output from performed material analyses influences the optimisation of operating chemical regimes and it can be used in optimisation of regimes at decontamination and passivation of pipelines or secondary circuit components. It can be concluded that a longer passivation time leads more to magnetite fraction in the corrosion products composition.

  17. The Moessbauer spectroscopy in the characterization of atmospheric corrosion products

    International Nuclear Information System (INIS)

    Hernandez Torres, D.; Leiva Ronda, P.; Gomez, J.; Ronda, M.

    1996-01-01

    A study of corrosion products on mild steel formed after 1 and 5 years exposure in two industrial coastal weathering stations in the Bay from Matanzas City, Cuba, has been carried out. Structural analysis was conducted using mainly transmission Moessbauer Spectroscopy and the X-ray diffraction as complementary technique. The main phases found in the specimen exposed to high chloride containing environment were: lepidocrocite (γ- FeOOH), goethite (α- FeOOH) and magnetite concentration was the lowest, the phases found were γ- FeOOH and α- FeOOH, and the phase transformation proposed was γ- FeOOh -> α- Fe-OOH. In this station were found also amorphous corrosion products. There amorphous phases could be responsible for the lowest levels of corrosion on steel in this station

  18. The use of water-soluble hydrazones as inhibitors for the corrosion of C-steel in acidic medium

    International Nuclear Information System (INIS)

    Moussa, M.N.H.; El-Far, A.A.; El-Shafei, A.A.

    2007-01-01

    Inhibition efficiency of some water-soluble hydrazones for C-steel corrosion in hydrochloric acid has been tested by weight loss, polarisation measurements and open circuit technique. The inhibition effect was attributed to the adsorption of the additives on the C-steel surface as supported by adsorption measurements at Pt electrode using cyclic voltammetry. Electrochemical measurements indicated that all the additives behave as cathodic-type inhibitors. The data obtained fit well to both the Temkin adsorption isotherm and the kinetic-thermodynamic model. The inhibition behaviour and its order were explained with the help of the proposed skeletal representation

  19. The use of water-soluble hydrazones as inhibitors for the corrosion of C-steel in acidic medium

    Energy Technology Data Exchange (ETDEWEB)

    Moussa, M.N.H.; El-Far, A.A. [Department of Chemistry, Faculty of Science, Mansoura University, ET-35516 Mansoura (Egypt); El-Shafei, A.A. [Department of Chemistry, Faculty of Science, Mansoura University, ET-35516 Mansoura (Egypt)], E-mail: ashafei@mans.edu.eg

    2007-09-15

    Inhibition efficiency of some water-soluble hydrazones for C-steel corrosion in hydrochloric acid has been tested by weight loss, polarisation measurements and open circuit technique. The inhibition effect was attributed to the adsorption of the additives on the C-steel surface as supported by adsorption measurements at Pt electrode using cyclic voltammetry. Electrochemical measurements indicated that all the additives behave as cathodic-type inhibitors. The data obtained fit well to both the Temkin adsorption isotherm and the kinetic-thermodynamic model. The inhibition behaviour and its order were explained with the help of the proposed skeletal representation.

  20. Iron Drinking Water Pipe Corrosion Products: Concentrators of Toxic Metals

    Science.gov (United States)

    2013-01-01

    health risk. In addition Pb corrosion products may be sinks for other metals such as chromium (Cr), copper (Cu), manganese (Mn), and zinc (Zn). These...Vanadium K-Edge X-ray Absorption Near-Edge Structure Interpretation: Application to the Speciation of Vanadium in Oxide Phases from Steel Slag ’, Journal

  1. Material selection and corrosion control practices in petroleum production

    International Nuclear Information System (INIS)

    Tuttle, R.N.

    1980-01-01

    The intent of this paper is to review briefly the current state of the art and to discuss some of the anticipated future oil and gas drilling and production activities which may challenge the materials selection and corrosion technologies. The current state of art discussions in this paper have been augmented by providing a list of references so that interested engineers may delve into each subject in more detail as desired. The technological areas which appear to require additional input to meet future needs include high strength tubular goods for sour gas service, corrosion resistant high strength alloys, definition of the effects of pressure, temperature, and fluid composition on corrosion behavior, and fatigue properties of various steels in seawater

  2. Rhenium Uptake as Analogue 96Tc by Steel Corrosion Products

    International Nuclear Information System (INIS)

    K.M. Krupka; C.F. Brown; H. Todd Schaef; S. M. Heald; M. M. Valenta; B. W. Arey

    2006-01-01

    Static batch experiments were used to examine the sorption of dissolved perrhenate [Re(VII)], as a surrogate for pertechnetate [Tc(VII)], on corrosion products of A-516 carbon steel coupons contacted with synthetic groundwater or dilute water. After 109 days of contact time, the concentration of dissolved Re(VII) in the synthetic groundwater matrix decreased by approximately 26%; the dilute water matrix experienced a 99% decrease in dissolved Re(VII) over the same time period. Bulk x-ray diffraction (XRD) results for the corroded steel coupons showed that the corrosion products consisted primarily of maghemite, lepidocrocite, and goethite. Analyses of the coupons by scanning electron microscopy/energy dispersive spectroscopy (SEM/EDS) indicated that Re was present with the morphologically complex assemblages of Fe oxide/hydroxide corrosion products for samples spiked with the highest dissolved Re(VII) concentration (1.0 mmol/L) used for these experiments. Analyses of corroded steel coupons contacted with solutions containing 1.0 mmol/L Re(VII) by synchrotron-based methods confirmed the presence of Re sorbed with the corrosion product on the steel coupons. Analyses showed that the Re sorbed on these corroded coupons was in the +7 oxidation state, suggesting that the Re(VII) uptake mechanism did not involve reduction of Re to a lower oxidation state, such as +4. The results of our studies using Re(VII) as an analogue for 99 Tc(VII) suggest that 99 Tc(VII) would also be sorbed with steel corrosion products and that the inventory of 99 Tc(VII) released from breached waste packages would be lower than what is now conservatively estimated

  3. Nuclear reactor structural material forming less radioactive corrosion product

    International Nuclear Information System (INIS)

    Nakazawa, Hiroshi.

    1988-01-01

    Purpose: To provide nuclear reactor structural materials forming less radioactive corrosion products. Constitution: Ni-based alloys such as inconel alloy 718, 600 or inconel alloy 750 and 690 having excellent corrosion resistance and mechanical property even in coolants at high temperature and high pressure have generally been used as nuclear reactor structural materials. However, even such materials yield corrosion products being attacked by coolants circulating in the nuclear reactor, which produce by neutron irradiation radioactive corrosion products, that are deposited in primary circuit pipeways to constitute exposure sources. The present invention dissolves dissolves this problems by providing less activating nuclear reactor structural materials. That is, taking notice on the fact that Ni-58 contained generally by 68 % in Ni changes into Co-58 under irradiation of neutron thereby causing activation, the surface of nuclear reactor structural materials is applied with Ni plating by using Ni with a reduced content of Ni-58 isotopes. Accordingly, increase in the radiation level of the nuclear reactor structural materials can be inhibited. (K.M.)

  4. Chemical and mechanical control of corrosion product transport

    Energy Technology Data Exchange (ETDEWEB)

    Hede Larsen, O; Blum, R [I/S Fynsvaerket, Faelleskemikerne, Odense (Denmark); Daucik, K [I/S Skaerbaekvaerket, Faelleskemikerne, Fredericia (Denmark)

    1996-12-01

    The corrosion products formed in the condensate and feedwater system of once-through boilers are precipitated and deposited inside the evaporator tubes mainly in the burner zone at the highest heat flux. Depositions lead to increased oxidation rate and increased metal temperature of the evaporator tubes, hereby decreasing tube lifetime. This effect is more important in the new high efficiency USC boilers due to increased feedwater temperature and hence higher thermal load on the evaporator tubes. The only way to reduce the load on the evaporator tubes is to minimise corrosion product transport to the boiler. Two general methods for minimising corrosion product transport to the boiler have been evaluated through measurement campaigns for Fe in the water/steam cycle in supercritical boilers within the ELSAM area. One method is to reduce corrosion in the low temperature condensate system by changing conditioning mode from alkaline volatile treatment (AVT) to oxygenated treatment (OT). The other method is to filtrate part of the condensate with a mechanical filter at the deaerator. The results show, that both methods are effective at minimising Fe-transport to the boiler, but changing to OT has the highest effect and should always be used, whenever high purity condensate is maintained. Whether mechanical filtration also is required, depends on the boiler, specifically the load on the evaporator. A simplified calculation model for lifetime evaluation of evaporator tubes has been developed. This model has been used for evaluating the effect of corrosion product transport to the boiler on evaporator tube lifetime. Conventional supercritical boilers generally can achieve sufficient lifetime by AVT and even better by OT, whereas all measures to reduce Fe-content of feedwater, including OT and mechanical filtration, should be taken, to ensure sufficient lifetime for the new boilers with advanced steam data - 290 bar/580 deg. C and above. (au)

  5. Characterization of the corrosion products formed on mild steel in acidic medium with N-octadecylpyridinium bromide as corrosion inhibitor

    Energy Technology Data Exchange (ETDEWEB)

    Nava, N., E-mail: tnava@imp.mx; Likhanova, N. V. [Direccion de Investigacion y Posgrado, Instituto Mexicano del Petroleo (Mexico); Olivares-Xometl, O. [Benemerita Universidad Autonoma de Puebla, Facultad de Ingenieria Quimica (Mexico); Flores, E. A. [Direccion de Investigacion y Posgrado, Instituto Mexicano del Petroleo (Mexico); Lijanova, I. V. [CIITEC, Instituto Politecnico Nacional (Mexico)

    2011-11-15

    The characterization of the corrosion products formed on mild steel SAE 1018 after 2 months exposure in aqueous sulfuric acid with and without corrosion inhibitor N-octadecylpyridinium bromide has been carried out by means of transmission {sup 57}Fe Moessbauer spectroscopy and X-ray powder diffraction (XRD). The major constituent of the rust formed in this environment without corrosion inhibitor is goethite ({alpha}-FeOOH). The samples with N-octadecylpyridinium bromide contain rozenite and large amounts of melanterite in the corrosion layers.

  6. Characterization of corrosion products formed on steels in the first months of atmospheric exposure

    OpenAIRE

    Antunes Renato Altobelli; Costa Isolda; Faria Dalva Lúcia Araújo de

    2003-01-01

    The corrosion products of carbon steel and weathering steel exposed to three different types of atmospheres, at times ranging from one to three months, have been identified. The steels were exposed in an industrial site, an urban site (São Paulo City, Brazil), and a humid site. The effect of the steel type on the corrosion products formed in the early stages of atmospheric corrosion has been evaluated. The corrosion products formed at the various exposure locations were characterized by Raman...

  7. Evaluation of corrosion products formed by sulfidation as inhibitors of the naphthenic corrosion of AISI-316 steel

    Science.gov (United States)

    Sanabria-Cala, J. A.; Montañez, N. D.; Laverde Cataño, D.; Y Peña Ballesteros, D.; Mejía, C. A.

    2017-12-01

    Naphthenic acids present in oil from most regions worldwide currently stand as the main responsible for the naphthenic corrosion problems, affecting the oil-refining industry. The phenomenon of sulfidation, accompanying corrosion processes brought about by naphthenic acids in high-temperature refining plant applications, takes place when the combination of sulfidic acid (H2S) with Fe forms layers of iron sulphide (FeS) on the material surface, layers with the potential to protect the material from attack by other corrosive species like naphthenic acids. This work assessed corrosion products formed by sulfidation as inhibitors of naphthenic corrosion rate in AISI-316 steel exposed to processing conditions of simulated crude oil in a dynamic autoclave. Calculation of the sulfidation and naphthenic corrosion rates were determined by gravimetry. The surfaces of the AISI-316 gravimetric coupons exposed to acid systems; were characterized morphologically by X-Ray Diffraction (XRD) and X-ray Fluorescence by Energy Dispersive Spectroscopy (EDS) combined with Scanning Electron Microscopy (SEM). One of the results obtained was the determination of an inhibiting effect of corrosion products at 250 and 300°C, where lower corrosion rate levels were detected. For the temperature of 350°C, naphthenic corrosion rates increased due to deposition of naphthenic acids on the areas where corrosion products formed by sulfidation have lower homogeneity and stability on the surface, thus accelerating the destruction of AISI-316 steel. The above provides an initial contribution to oil industry in search of new alternatives to corrosion control by the attack of naphthenic acids, from the formation of FeS layers on exposed materials in the processing of heavy crude oils with high sulphur content.

  8. Behavior of copper corrosion products in water loops of heat-exchange units

    International Nuclear Information System (INIS)

    Zarembo, V.I.; Kritskii, V.G.; Slobodov, A.A.; Puchkov, L.V.

    1989-01-01

    This communication is dedicated to an examination of copper corrosion products (CP) in the conditions of real aqueous-chemical regime (ACR) parameters. The deposition of these CP in steam-generating zones (up to 85% of their total amount) stimulate local types of corrosion. The solubility in Cu CP (Cu 2 O, CuO, Cu(OH) 2 )-water (H 2 O)-gas (H 2 , O 2 )-conditioning additives (HCl, KOH) systems was determined by computer modeling according to the minimum Gibbs energy criterion on the basis of selected and matched thermodynamic constants for various chemical forms of copper under standard conditions. As a result of the authors' calculations they obtained the solubilities in water of CuO, Cu 2 O and Cu(OH) 2 when changing the dosage of active gases from 0 to 10 -2 mole/kg of water, of acid or equal to that of saturated vapor of pure water. Thus, they were able to monitor the behavior of copper CP in conditions modeling those of real ACR in operating heat exchange units, including in conditions deviating from the standard

  9. An X-ray diffraction study of corrosion products from low carbon steel

    International Nuclear Information System (INIS)

    Morales, A. L.

    2003-01-01

    It was found in earlier work a decrease in the corrosion rate from low carbon steel when it was subjected to the action of a combined pollutant concentration (SO 4 ''2-=10''-4 M+Cl=1.5x 10''-3 M). It was also found that large magnetic content of the rust was related to higher corrosion rates. In the present study corrosion products are further analyzed by means of X-ray diffraction to account for composition changes during the corrosion process. it is found that lepidocrocite and goethite are the dominant components for the short-term corrosion in all batches considered while for log-term corrosion lepidocrite and goethite dominates if the corrosion rates is low and magnetite dominates if the corrosion rate is high. The mechanism for decreasing the corrosion rate is related to the inhibition of magnetite production at this particular concentration. (Author) 15 refs

  10. Analysis of corrosion products of carbon steel in wet bentonite

    International Nuclear Information System (INIS)

    Osada, K.; Nagano, T.; Kozai, N.; Nakashima, S.; Nakayama, S.; Muraoka, S.

    1991-01-01

    The following conclusions were obtained; (1) At 40degC, the average corrosion rate of SS41 carbon steel in wet bentonite was 0.025 mm/y. This is smaller than the value of 0.042 mm/y obtained in pure water at 40degC. However, at 95degC, the corrosion rate of SS41 carbon steel in wet bentonite was 0.27 mm/y, which is much larger than that in pure water at 95degC. (2) At 95degC, γ-FeO(OH) (lepidocrocite) was formed only in wet bentonite, and it was absent in pure water. Evaporation of moisture resulted in the formation of partial covering of bentonite, which promoted local corrosion. Consequently, γ-FeO(OH) was considered to be formed. (3) In wet bentonite at 95degC, α-Fe 2 O 3 (hematite) can be identified by means of colorimetry. The color of corrosion products is orangish, indicating the contribution of α-Fe 2 O 3 in iron hydroxides. (author)

  11. Analysis Science Process Skills Content in Chemistry Textbooks Grade XI at Solubility and Solubility Product Concept

    Directory of Open Access Journals (Sweden)

    Bayu Antrakusuma

    2017-12-01

    Full Text Available The aim of this research was to determine the analysis of science process skills in textbooks of chemistry grade XI in SMA N 1 Teras, Boyolali. This research used the descriptive method. The instruments were developed based on 10 indicators of science process skills (observing, classifying, finding a conclusion, predicting, raising the question, hypothesizing, planning an experiment, manipulating materials, and equipment, Applying, and communicating. We analyzed 3 different chemistry textbooks that often used by teachers in teaching. The material analyzed in the book was solubility and solubility product concept in terms of concept explanation and student activity. The results of this research showed different science process skill criteria in 3 different chemistry textbooks. Book A appeared 50% of all aspects of science process skills, in Book B appeared 80% of all aspects of science process skills, and in Book C there was 40% of all aspects of the science process skills. The most common indicator in all books was observing (33.3%, followed by prediction (19.05%, classifying (11.90%, Applying (11.90% , planning experiments (9.52%, manipulating materials and equipment (7.14%, finding conclusion (4.76%, communicating (2.38%. Asking the question and hypothesizing did not appear in textbooks.

  12. The effects of corrosion product colloids on actinide transport

    International Nuclear Information System (INIS)

    Gardiner, M.P.; Smith, A.J.; Williams, S.J.

    1991-11-01

    This report assesses the possible effects of colloidal corrosion products on the transport of actinides from the near field of radioactive waste repositories. The desorption of plutonium and americium from colloidal corrosion products of iron and zirconium was studied under conditions simulating a transition from near-field to far-field environmental conditions. Desorption of actinides occurred slowly from the colloids under far-field conditions. Measurements of particle stability showed all the colloids to be unstable in the near field. Stability increased under far-field conditions or as a result of the evolution of the near field. Migration of colloids from the near field is unlikely except in the presence of organic materials. (Author)

  13. Phase Analysis of Corrosion Products from Nuclear Power Plants

    International Nuclear Information System (INIS)

    Lipka, J.; Slugen, V.; Toth, I.; Hascik, J.; Lehota, M.

    2002-01-01

    The variability of the properties and the composition of the corrosion products of the stainless CrNi and mild steels in dependence on the conditions (temperature, acidity, etc.) is of such a range that, in practice, it is impossible to determine the properties of the corrosion products for an actual case from the theoretical data only. Since the decontamination processes for the materials of the water-cooled reactor (VVER-440) secondary circuits are in a process of development, it is necessary to draw the needed information by the measurement and analysis of the real specimens. The corrosion layer was separated by scraping the rust off the surface and the powder samples were studied by transmission Moessbauer spectroscopy. It should be noted that the gamma spectroscopic measurements give no evidence of the presence of low-energy gamma radiation emitted from the samples. The scrapped specimen powder was homogenised (using the 50 μm sieve) and fixed into the special holder. The 57 Co in Rh matrix was used as the radioactive Moessbauer source. Measured spectra were fitted using program NORMOS SITE. According to the results obtained from Moessbauer spectra, it is possible to establish that the main component of secondary circuit's corrosion products is magnetite Fe 3 O 4 . Next components are hematite α-Fe 2 O 3 and hydroxide akagenite β-FeOOH, which is characterised by a significant paramagnetic doublet in the middle of the spectra. The sextets corresponding to base materials (martensite and austenite steels) were identified in all measured spectra.

  14. Enzymatic Production of FAME Biodiesel with Soluble Lipases

    DEFF Research Database (Denmark)

    T. Gundersen, Maria; Heltborg, Carsten Kirstejn; Yang, V

    Biodiesel is a viable alternative to fossil fuels, and biocatalysis is gaining interest as a greener process. We focus on converting oils to Fatty Acid Methyl Ester (FAME) using soluble lipases, which offer an advantage compared to immobilized enzymes by cost efficiency and ease of implementation...... the defined operating space concerning: temperature, water content, initial methanol concentration and enzyme content. The identified optimum range was experimentally evaluated, and model findings were confirmed. Another barrier in lipase use in biodiesel production is the higher melting point (m...

  15. Quantifying movements of corrosion products in reinforced concrete using x-ray attenuation measurements

    DEFF Research Database (Denmark)

    Pease, Bradley Justin; Michel, Alexander; Stang, Henrik

    2011-01-01

    Corrosion of steel reinforcement, embedded in concrete, may substantially degrade concrete structures due to the expansive nature of corrosion products. Expansion of corrosion products cause tensile stresses to develop and cracks to form in concrete. Extensive research has focused on corrosion...... of corrosion products move into the concrete without generating tensile stresses and cracks in the concrete. Typically, corrosion products are thought to occupy pores, interfacial defects, and/or air voids located near the concrete-steel interface and stresses develop only after filling of these pores. Further....... X-ray attenuation measurements are also capable of detecting cracks. Therefore, this approach provides a direct measurement of the amount and location of reinforcement corrosion products required to induce cracking. Results of a parametric investigation on the impact of water-to-cement ratio (0...

  16. Effects of amalgam corrosion products on human cells

    Energy Technology Data Exchange (ETDEWEB)

    Goldschmidt, P R; Cogen, R B; Taubman, S B [Departments of Periodontics and Pathology, University of Connecticut Health Center, Farmington, Connecticut, U.S.A.

    1976-01-01

    Using three independent criteria, we have found that 10/sup -4/,10/sup -6/M concentrations of ions presumably liberated from the corrosion of dental amalgam produce injurious effects on either human gingival fibroblasts or HeLa cells when the cells are grown in culture. Release of /sup 51/Cr and uptake of trypan blue dye were seen with 10/sup -5/M Hg/sup + +/ and Ag/sup +/. Inhibition of amino acid incorporation into protein-like material was seen with eluates of amalgam and with ionic solutions of most metals comprising dental amalgam. Stannous ion showed little if any cytotoxic potential. These results suggest that corrosion products of amalgam are capable of causing cellular injury or destruction.

  17. Evaluation of CRUDTRAN code to predict transport of corrosion products and radioactivity in the PWR primary coolant system

    International Nuclear Information System (INIS)

    Lee, C.B.

    2002-01-01

    CRUDTRAN code is to predict transport of the corrosion products and their radio-activated nuclides such as cobalt-58 and cobalt-60 in the PWR primary coolant system. In CRUDTRAN code the PWR primary circuit is divided into three principal sections such as the core, the coolant and the steam generator. The main driving force for corrosion product transport in the PWR primary coolant comes from coolant temperature change throughout the system and a subsequent change in corrosion product solubility. As the coolant temperature changes around the PWR primary circuit, saturation status of the corrosion products in the coolant also changes such that under-saturation in steam generator and super-saturation in the core. CRUDTRAN code was evaluated by comparison with the results of the in-reactor loop tests simulating the PWR primary coolant system and PWR plant data. It showed that CRUDTRAN could predict variations of cobalt-58 and cobalt-60 radioactivity with time, plant cycle and coolant chemistry in the PWR plant. (author)

  18. Fission and corrosion products behavior in primary circuits of LMFBR's

    International Nuclear Information System (INIS)

    Feuerstein, H.; Thorley, A.W.

    1987-08-01

    Most of the 20 presented papers report items belonging to more than one session. The equipment results of primary circuits of LMFBR's relative to corrosion and fission products, release and chemistry of fuel, measurement techniques and analytical procedures of sodium sampling, difficulties with radionuclides and particles, reactor experiences with EBR-II, FFTF, BR10, BOR60, BN350, BN600, JOYO, and KNK-II, DFR, PFR, RAPSODIE, PHENIX, and SUPERPHENIX, and at least the verification of codes for calculation models of radioactive products accumulation and distribution are described. All 20 papers presented at the meeting are separately indexed in the database. (DG)

  19. The water soluble composite poly(vinylpyrrolidone–methylaniline: A new class of corrosion inhibitors of mild steel in hydrochloric acid media

    Directory of Open Access Journals (Sweden)

    R. Karthikaiselvi

    2017-02-01

    Full Text Available In recent years poly methyl aniline has been reported as one of the efficient corrosion inhibitors of mild steel in acidic media. In view of the major limitation of the insolubility of polymethyl aniline PMA, we propose to convert PMA into a water soluble composite using supporting polymer polyvinylpyrrolidone to get higher solubility and corrosion inhibition efficiency. The water soluble composite poly(vinylpyrrolidone-methyl aniline was synthesized by chemical oxidative polymerization and its inhibitive effect on mild steel in 1 M HCl has been investigated using weight loss and electrochemical techniques (potentiodynamic polarization studies and impedance spectroscopy. SEM and EDX analyses are carried out to establish a protective film formation on the metal surface.

  20. The development of an adsorbent for corrosion products in high-temperature water

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Yong Ik; Sung, Ki Woung; Kim, Kwang Rag; Kim, Yu Hwan; Koo, Jae Hyoo [Korea Atomic Energy Research Institute, Taejon (Korea, Republic of)

    1996-08-01

    In order to use as adsorbent for removal of the soluble corrosion products, mainly Co{sup 60} under PWR reactor coolant conditions (300 deg C, 160 kg/cm{sup 2}), stable ZrO{sub 2} adsorbent was prepared using sol-gel process from zirconyl nitrate, AlO adsorbent was prepared by hydrolysis of aluminum isopropoxide, and titanium tetraisopropoxide, respectively. The prepared adsorbents were calcined at various temperature and analyzed by physical properties and the Co{sup 2+} adsorption capacity. And it was shown that the Co{sup 2+} adsorption capacity of the TiO{sub 2}-Al{sub 2}O{sub 3} adsorbents were found to have larger than that of ZrO{sub 2} and Al{sub 2}O{sub 3} adsorbents in high-temperature water. ZrO{sub 2}, Al{sub 2}O{sub 3} and TiO{sub 2}-Al{sub 2}O{sub 3} adsorbents were found to be suitable high-temperature adsorbents for the removal of dissolved corrosion products, mainly Co in PWR reactor coolant conditions. 15 tabs., 51 figs., 55 refs. (Author).

  1. The development of an adsorbent for corrosion products in high-temperature water

    International Nuclear Information System (INIS)

    Kim, Yong Ik; Sung, Ki Woung; Kim, Kwang Rag; Kim, Yu Hwan; Koo, Jae Hyoo

    1996-08-01

    In order to use as adsorbent for removal of the soluble corrosion products, mainly Co 60 under PWR reactor coolant conditions (300 deg C, 160 kg/cm 2 ), stable ZrO 2 adsorbent was prepared using sol-gel process from zirconyl nitrate, AlO adsorbent was prepared by hydrolysis of aluminum isopropoxide, and titanium tetraisopropoxide, respectively. The prepared adsorbents were calcined at various temperature and analyzed by physical properties and the Co 2+ adsorption capacity. And it was shown that the Co 2+ adsorption capacity of the TiO 2 -Al 2 O 3 adsorbents were found to have larger than that of ZrO 2 and Al 2 O 3 adsorbents in high-temperature water. ZrO 2 , Al 2 O 3 and TiO 2 -Al 2 O 3 adsorbents were found to be suitable high-temperature adsorbents for the removal of dissolved corrosion products, mainly Co in PWR reactor coolant conditions. 15 tabs., 51 figs., 55 refs. (Author)

  2. Characterization of uranium corrosion products involved in the March 13, 1998 fuel manufacturing facility pyrophoric event

    International Nuclear Information System (INIS)

    Totemeier, T.C.

    1999-01-01

    Uranium metal corrosion products from ZPPR fuel plates involved in the March 13, 1998 pyrophoric event in the Fuel Manufacturing Facility at Argonne National Laboratory-West were characterized using thermo-gravimetric analysis, X-ray diffraction, and BET gas sorption techniques. Characterization was performed on corrosion products in several different conditions: immediately after separation from the source metal, after low-temperature passivation, after passivation and extended vault storage, and after burning in the pyrophoric event. The ignition temperatures and hydride fractions of the corrosion product were strongly dependent on corrosion extent. Corrosion products from plates with corrosion extents less than 0.7% did not ignite in TGA testing, while products from plates with corrosion extents greater than 1.2% consistently ignited. Corrosion extent is defined as mass of corrosion products divided by the total mass of uranium. The hydride fraction increased with corrosion extent. There was little change in corrosion product properties after low-temperature passivation or vault storage. The burned products were not reactive and contained no hydride; the principal constituents were UO 2 and U 3 O 7 . The source of the event was a considerable quantity of reactive hydride present in the corrosion products. No specific ignition mechanism could be conclusively identified. The most likely initiator was a static discharge in the corrosion product from the 14th can as it was poured into the consolidation can. The available evidence does not support scenarios in which the powder in the consolidation can slowly self-heated to the ignition point, or in which the powder in the 14th can was improperly passivated

  3. Characterization of uranium corrosion products involved in the March 13, 1998 fuel manufacturing facility pyrophoric event.

    Energy Technology Data Exchange (ETDEWEB)

    Totemeier, T.C.

    1999-04-26

    Uranium metal corrosion products from ZPPR fuel plates involved in the March 13, 1998 pyrophoric event in the Fuel Manufacturing Facility at Argonne National Laboratory-West were characterized using thermo-gravimetric analysis, X-ray diffraction, and BET gas sorption techniques. Characterization was performed on corrosion products in several different conditions: immediately after separation from the source metal, after low-temperature passivation, after passivation and extended vault storage, and after burning in the pyrophoric event. The ignition temperatures and hydride fractions of the corrosion product were strongly dependent on corrosion extent. Corrosion products from plates with corrosion extents less than 0.7% did not ignite in TGA testing, while products from plates with corrosion extents greater than 1.2% consistently ignited. Corrosion extent is defined as mass of corrosion products divided by the total mass of uranium. The hydride fraction increased with corrosion extent. There was little change in corrosion product properties after low-temperature passivation or vault storage. The burned products were not reactive and contained no hydride; the principal constituents were UO{sub 2} and U{sub 3}O{sub 7}. The source of the event was a considerable quantity of reactive hydride present in the corrosion products. No specific ignition mechanism could be conclusively identified. The most likely initiator was a static discharge in the corrosion product from the 14th can as it was poured into the consolidation can. The available evidence does not support scenarios in which the powder in the consolidation can slowly self-heated to the ignition point, or in which the powder in the 14th can was improperly passivated.

  4. Activation of the IFMIF Lithium Loop Corrosion Products

    Energy Technology Data Exchange (ETDEWEB)

    Cambi, G [Department of Physics, Bologna University, Via Irnerio 46, 40126 Bologna (Italy); Cepraga, D G [ENEA FIS-MET, Via Don Fiammelli 2, 40128 Bologna (Italy); Frisoni, M [Athena s.a.s., Via del Battiferro 3, 40129 Bologna (Italy); Pinna, T [Associazione EURATOM- ENEA sulla Fusione, Via Enrico Fermi 45, I-00044 Frascati (RM), (Italy)

    2006-07-01

    The assessment of the activation of steel corrosion products generated in one year of IFMIF lithium loop operation due to the interaction between lithium and Stainless Steel SS-304 has been performed. This paper is mainly focused on the neutron activation and it describes the approach used for and present the results obtained. A preliminary estimate of the accelerator deuteron beam contribute to the activation is also presented. The study was accomplished through the following phases: 1) neutron spectrum calculation in the lithium target via MCNP-4C2 with McEnea neutron source model based on the measurements of neutron emission spectra produced in Li(d,n) reactions for a thick lithium target performed at the '' Cyclotron and Radioisotope Center (CYRIC) '', Tohoku University, Japan; 2) inventories calculations and decay gamma sources production via ANITA-IEAF activation code package; the calculations were performed by considering a lithium mix composition containing lithium impurities and corrosion products referred to 200 wppm of Steel SS-304 corresponding to a corrosion rate of 0.2 {mu}m/y and a SS-304 wetted surface of 572 m{sup 2} ; an irradiation scenario reproducing the integrated (in eleven months of operation) neutron flux responsible for the activation of the circulating corrosion products facing the deuteron beam was considered; 3) decay gamma transport analysis for dose rate evaluations via both VITENEA-IEF/SCALENEA-1 and MCNP-4C2 systems for the Longest Pipe of the Lithium loop. The following conclusions can be drawn by the results analysis: {center_dot} dose rates at 50 cm from the Longest Pipe are 198 {mu}Sv/h and 85{mu}Sv/h at 1 day and 1 week from the plant shutdown, respectively {center_dot} considering the average 20 mSv/a regulatory limit in Europe for '' Radiation Worker '' and the four-week period of annual maintenance activities in Li loop, the zone around the piping, exceeding 125 mSv/h, has to be declared '' Restricted Access Area '' {center

  5. Activation of the IFMIF Lithium Loop Corrosion Products

    International Nuclear Information System (INIS)

    Cambi, G.; Cepraga, D.G.; Frisoni, M.; Pinna, T.

    2006-01-01

    The assessment of the activation of steel corrosion products generated in one year of IFMIF lithium loop operation due to the interaction between lithium and Stainless Steel SS-304 has been performed. This paper is mainly focused on the neutron activation and it describes the approach used for and present the results obtained. A preliminary estimate of the accelerator deuteron beam contribute to the activation is also presented. The study was accomplished through the following phases: 1) neutron spectrum calculation in the lithium target via MCNP-4C2 with McEnea neutron source model based on the measurements of neutron emission spectra produced in Li(d,n) reactions for a thick lithium target performed at the '' Cyclotron and Radioisotope Center (CYRIC) '', Tohoku University, Japan; 2) inventories calculations and decay gamma sources production via ANITA-IEAF activation code package; the calculations were performed by considering a lithium mix composition containing lithium impurities and corrosion products referred to 200 wppm of Steel SS-304 corresponding to a corrosion rate of 0.2 μm/y and a SS-304 wetted surface of 572 m 2 ; an irradiation scenario reproducing the integrated (in eleven months of operation) neutron flux responsible for the activation of the circulating corrosion products facing the deuteron beam was considered; 3) decay gamma transport analysis for dose rate evaluations via both VITENEA-IEF/SCALENEA-1 and MCNP-4C2 systems for the Longest Pipe of the Lithium loop. The following conclusions can be drawn by the results analysis: · dose rates at 50 cm from the Longest Pipe are 198 μSv/h and 85μSv/h at 1 day and 1 week from the plant shutdown, respectively · considering the average 20 mSv/a regulatory limit in Europe for '' Radiation Worker '' and the four-week period of annual maintenance activities in Li loop, the zone around the piping, exceeding 125 mSv/h, has to be declared '' Restricted Access Area '' · the worker radiation protection

  6. Technical investigation of a pyrophoric event involving corrosion products from HEU ZPPR fuel plates

    International Nuclear Information System (INIS)

    Totemeier, T. C.

    2000-01-01

    A pyrophoric event recently occurred which involved corrosion products collected from highly-enriched uranium (HEU) fuel plates used in the Zero Power Physics Reactor (ZPPR). This paper summarizes the event and its background, and presents the results of an investigation into its source and mechanism. The investigation focused on characterization of corrosion product samples similar to those involved in the event using thermo-gravimetric analysis (TGA). Burning curve TGA tests were performed to measure the ignition temperature and hydride fractions of corrosion products in several different conditions to assess the effects of passivation treatment and long-term storage on chemical reactivity. The hydride fraction and ignition temperature of the corrosion products were found to be strongly dependent on the corrosion extent of the source metal. The results indicate that the energy source for the event was a considerable quantity of uranium hydride present in the corrosion products, but the specific ignition mechanism could not be identified

  7. Diesel-soluble lignin oils and methods of their production

    DEFF Research Database (Denmark)

    2016-01-01

    Solvent consumption in supercritical ethanol, propanol or butanol treatment of either refined pre-extracted lignin or comparatively impure lignin-rich solid residual from hydrothermally pretreated lignocellulosic biomass can be minimized by conducting the reaction at very high loading of lignin...... to solvent. Comparatively impure, crude lignin- rich solid residual can be directly converted by supercritical alcohol treatment to significantly diesel-soluble lignin oil without requirement for pre-extraction or pre- solubilisation of lignin or for added reaction promoters such as catalysts, hydrogen donor...... co-solvents, acids, based or H2 gas. O:C ratio of product oil can readily be obtained using crude lignin residual in such a process at levels 0.20 or lower....

  8. Experimental Study of Removing Surface Corrosion Products from Archaeological Iron Objects and Alternating Iron Corrosion Products by Nd:YAG Laser Cleaning System

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Hye Youn; Cho, Nam Chul [Kongju National University, Daejeon (Korea, Republic of); Lee, Jong Myoung [IMT co. Ltd, Suwon (Korea, Republic of); Yu, Jae Eun [National Research Institute of Cultural Heritage, Daejeon (Korea, Republic of)

    2012-05-15

    The corrosion product of archaeological iron objects is supposed to be removed because it causes re-corrosion. So far it is removed by scapel and sand blaster but they depend on the skill and experience of a conservator and the glass-dust of the sand blaster is harmful to humans. Therefore this study applies a laser cleaning system which is used in various industrial cleaning processes, to remove corrosion product from archaeological iron objects. In addition, this work studies the alternation of corrosion product after laser irradiation, which evaluates the reliability of the laser cleaning system. Optical microscopy, SEM-EDS, XRD, Raman have been used to observe and analyse the surface of the objects. The results show the capacity of laser cleaning some corrosion product, but blackening appears with increasing pulses and laser energy, and some corrosion products, goethite and hematite, are partially altered to magnetite. These problems, blackening and alternation of corrosion product, should be solved by further studies which find the optimal laser irradiation condition and use a wetting agent.

  9. The effect of corrosion product colloids on actinide transport

    International Nuclear Information System (INIS)

    Gardiner, M.P.; Smith, A.J.; Williams, S.J.

    1992-01-01

    The near field of the proposed UK repository for ILW/LLW will contain containers of conditioned waste in contact with a cementious backfill. It will contain significant quantities of iron and steel, Magnox and Zircaloy. Colloids deriving from their corrosion products may possess significant sorption capacity for radioelements. If the colloids are mobile in the groundwater flow, they could act as a significant vector for activity transport into the far field. The desorption of plutonium and americium from colloidal corrosion products of iron and zirconium has been studied under chemical conditions representing the transition from the near field to the far field. Desorption R d values of ≥ 5 x 10 6 ml g -1 were measured for both actinides on these oxides and hydroxides when actinide sorption took place under the near-field conditions and desorption took place under the far-field conditions. Desorption of the actinides occurred slowly from the colloids under far-field conditions when the colloids had low loadings of actinide and more quickly at high loadings of actinide. Desorbed actinide was lost to the walls of the experimental vessel. (author)

  10. Corrosion-product filtration in PWRs: Topical report

    International Nuclear Information System (INIS)

    Balakrishnan, P.V.; Buckley, L.P.

    1988-04-01

    As part of a programme on the optimization of pressurized water reactor (PWR) secondary side water treatment, laboratory-scale studies on filtration of the feedwater using materials having chemically active adsorbing surfaces were carried out. Graphite, zirconia and titania were identified, from a review of existing literature, as suitable filtration media, the last two because of their ion-exchange capability. The efficiency of filters packed with granular graphite for filtration of simulated feed train corrosion products and the pressure drop across the filters were determined as functions of filter dimensions and operating parameters at room temperature. A rough sizing of a full-flow feedwater filter using granular graphite was done on the basis of observations from the room temperature tests. Further studies are suggested at low concentrations of the corrosion product and at high temperature typical of steam generator feedwater after the high pressure heaters to derive realistic design parameters for a filter for installation in the PWR secondary circuit. Zirconia was produced in the form of spherical particles using a sol-gel process. The zirconia behaved as an anion exchanger at low pH and as a cation exchanger at high pH. Its suitability for purification of water at high temperature should be determined by futher studies. 30 refs., 16 figs., 8 tabs

  11. Oxidation kinetics of hydride-bearing uranium metal corrosion products

    Science.gov (United States)

    Totemeier, Terry C.; Pahl, Robert G.; Frank, Steven M.

    The oxidation behavior of hydride-bearing uranium metal corrosion products from Zero Power Physics Reactor (ZPPR) fuel plates was studied using thermo-gravimetric analysis (TGA) in environments of Ar-4%O 2, Ar-9%O 2, and Ar-20%O 2. Ignition of corrosion product samples from two moderately corroded plates was observed between 125°C and 150°C in all environments. The rate of oxidation above the ignition temperature was found to be dependent only on the net flow rate of oxygen in the reacting gas. Due to the higher net oxygen flow rate, burning rates increased with increasing oxygen concentration. Oxidation rates below the ignition temperature were much slower and decreased with increasing test time. The hydride contents of the TGA samples from the two moderately corroded plates, determined from the total weight gain achieved during burning, were 47-61 wt% and 29-39 wt%. Samples from a lightly corroded plate were not reactive; X-ray diffraction (XRD) confirmed that they contained little hydride.

  12. Oxidation kinetics of hydride-bearing uranium metal corrosion products

    International Nuclear Information System (INIS)

    Totemeier, T.C.; Pahl, R.G.; Frank, S.M.

    1998-01-01

    The oxidation behavior of hydride-bearing uranium metal corrosion products from zero power physics reactor (ZPPR) fuel plates was studied using thermo-gravimetric analysis (TGA) in environments of Ar-4%O 2 , Ar-9%O 2 , and Ar-20%O 2 . Ignition of corrosion product samples from two moderately corroded plates was observed between 125 C and 150 C in all environments. The rate of oxidation above the ignition temperature was found to be dependent only on the net flow rate of oxygen in the reacting gas. Due to the higher net oxygen flow rate, burning rates increased with increasing oxygen concentration. Oxidation rates below the ignition temperature were much slower and decreased with increasing test time. The hydride contents of the TGA samples from the two moderately corroded plates, determined from the total weight gain achieved during burning, were 47-61 wt% and 29-39 wt%. Samples from a lightly corroded plate were not reactive; X-ray diffraction (XRD) confirmed that they contained little hydride. (orig.)

  13. Biohydrogen production from soluble condensed molasses fermentation using anaerobic fermentation

    Energy Technology Data Exchange (ETDEWEB)

    Lay, Chyi-How; Lin, Chiu-Yue [Department of Environmental Engineering and Science, Feng Chia University, Taichung 40724 (China); Wu, Jou-Hsien; Hsiao, Chin-Lang [Department of Water Resource Engineering, Feng Chia University (China); Chang, Jui-Jen [Department of Life Sciences, National Chung Hsing University (China); Chen, Chin-Chao [Environmental Resources Laboratory, Department of Landscape Architecture, Chungchou Institute of Technology (China)

    2010-12-15

    Using anaerobic micro-organisms to convert organic waste to produce hydrogen gas gives the benefits of energy recovery and environmental protection. The objective of this study was to develop a biohydrogen production technology from food wastewater focusing on hydrogen production efficiency and micro-flora community at different hydraulic retention times. Soluble condensed molasses fermentation (CMS) was used as the substrate because it is sacchariferous and ideal for hydrogen production. CMS contains nutrient components that are necessary for bacterial growth: microbial protein, amino acids, organic acids, vitamins and coenzymes. The seed sludge was obtained from the waste activated sludge from a municipal sewage treatment plant in Central Taiwan. This seed sludge was rich in Clostridium sp. A CSTR (continuously stirred tank reactor) lab-scale hydrogen fermentor (working volume, 4.0 L) was operated at a hydraulic retention time (HRT) of 3-24 h with an influent CMS concentration of 40 g COD/L. The results showed that the peak hydrogen production rate of 390 mmol H{sub 2}/L-d occurred at an organic loading rate (OLR) of 320 g COD/L-d at a HRT of 3 h. The peak hydrogen yield was obtained at an OLR of 80 g COD/L-d at a HRT of 12 h. At HRT 8 h, all hydrogenase mRNA detected were from Clostridium acetobutylicum-like and Clostridium pasteurianum-like hydrogen-producing bacteria by RT-PCR analysis. RNA based hydrogenase gene and 16S rRNA gene analysis suggests that Clostridium exists in the fermentative hydrogen-producing system and might be the dominant hydrogen-producing bacteria at tested HRTs (except 3 h). The hydrogen production feedstock from CMS is lower than that of sucrose and starch because CMS is a waste and has zero cost, requiring no added nutrients. Therefore, producing hydrogen from food wastewater is a more commercially feasible bioprocess. (author)

  14. Electrochemical Characterisation of Filiform Corrosion on Aluminium Rolled Products

    NARCIS (Netherlands)

    Huisert, M.

    2001-01-01

    When aluminium is protected by an organic coating a special form of corrosion can occur underneath the organic coating; filiform corrosion. This form of corrosion manifests itself as threadlike filaments under the coating, it causes local delamination of the coating and the coating cannot protect

  15. The effect of zinc addition on PWR corrosion product deposition on zircaloy-4

    International Nuclear Information System (INIS)

    Walters, W.S.; Page, J.D.; Gaffka, A.P.; Kingsbury, A.F.; Foster, J.; Anderson, A.; Wickenden, D.; Henshaw, J.; Zmitko, M.; Masarik, V.; Svarc, V.

    2002-01-01

    During the period 1995 to 2001 a programme of loop irradiation tests have been performed to confirm the effectiveness of zinc additions on PWR circuit chemistry and corrosion. The programme included two loop irradiation experiments, and subsequent PIE; the experiments were a baseline test (no added zinc) and a test with added zinc (10 ppb). This paper addresses the findings regarding corrosion product deposition and activation on irradiated Zircaloy-4 surfaces. The findings are relevant to overall corrosion of the reactor primary circuit, the use of zinc as a corrosion inhibitor, and activation and transport of corrosion products. The irradiation experience provides information on the equilibration of the loop chemistry, with deliberate injection of zinc. The PIE used novel and innovative techniques (described below) to obtain samples of the oxide from the irradiated Zircaloy. The results of the PIE, under normal chemistry and zinc chemistry, indicate the effect of zinc on the deposition and activation of corrosion products on Zircaloy. It was found that corrosion product deposition on Zircaloy is enhanced by the addition of zinc (but corrosion product deposition on other materials was reduced in the presence of zinc). Chemical analysis and radioisotope gamma counting results are presented, to interpret the findings. A computer model has also been used to simulate the corrosion product deposition and activation, to assist in the interpretation of the results. (authors)

  16. The effect of zinc injection into PWR primary coolant on the reduction of radiation buildup and corrosion control. The solubilities of zinc, nickel and cobalt spinel oxides

    International Nuclear Information System (INIS)

    Miyajima, Kaori; Hirano, Hideo

    1999-01-01

    The use of zinc injection into PWR primary coolant to reduce radiation buildup has been widely studied, and te reduction effect has been experimentally confirmed. However, some items, such as the optimal concentration of zinc required to reduce radiation buildup, the corrosion control effect of zinc injection, and the influence of zinc injection on the integrity of fuel cladding, have not been clarified yet. In particular, the corrosion suppression effect of zinc remains unconfirmed. Therefore, it is necessary to measure and calculate the solubilities of zinc and nickel spinel oxides, which are formed on the surface of Ni-based alloys in PWR primary systems. In this study, in order to assess the effectiveness of zinc injection in the reduction of radiation buildup and the corrosion control of Ni-based alloy, the potential-pH diagrams for Zn-Cr-H 2 O, Ni-Cr-H 2 O, and Co-Cr-H 2 O systems at 300degC were constructed and the solubilities of Zn-Cr, Ni-Cr, and Co-Cr spinel oxides were calculated. It is concluded that under pH conditions for which NiCr 2 O 4 is stable, zinc injection is effective in corrosion control as well as in reducing radiation buildup. (author)

  17. Exposure testing of fasteners in preservative treated wood : gravimetric corrosion rates and corrosion product analyses

    Science.gov (United States)

    Samuel L. Zelinka; Rebecca J. Sichel; Donald S. Stone

    2010-01-01

    Research was conducted to determine the corrosion rates of metals in preservative treated wood and also understand the mechanism of metal corrosion in treated wood. Steel and hot-dip galvanized steel fasteners were embedded in wood treated with one of six preservative treatments and exposed to 27oC at 100% relative humidity for 1 year. The...

  18. Corrosion products in the coolant circuits of PWR nuclear power plants

    International Nuclear Information System (INIS)

    Darras, R.

    1984-01-01

    The characteristics of corrosion products formed in the primary and secondary circuits of pressurized light water nuclear power plants are first briefly recalled. The problem set by the pollution of coolants and metallic surfaces is then examined. Finally, the measures of precaution to take and the possible solutions to minimize the disturbing effects of this pollution by corrosion products are presented [fr

  19. The corrosion products in the coolant circuits of pressurized water nuclear power plants

    International Nuclear Information System (INIS)

    Darras, R.

    1983-01-01

    The characteristics of the corrosion products formed in the primary and secondary coolant circuits of light-water pressurized reactors are reviewed. The problem induced by the pollution of coolants and metallic surface are examined. Then, the recommendations to follow to minimize the disturbing effects of this pollution by the corrosion products are indicated [fr

  20. Test Production of Anti-Corrosive Paint in Laboratory Scale

    International Nuclear Information System (INIS)

    Thein Thein Win, Daw; Khin Aye Tint, Daw; Wai Min Than, Daw

    2003-02-01

    The main purpose of this project is to produce the anti-corrosive paint in laboratory scale. In these experiments, local raw materials, natural resin (shellac), pine oil, turpentine and ethyl alcohol wer applied basically. Laboratory trials were undrtaken to determine the suitablity of raw materials ane their composition for anti-corrosive paint manufacture.The results obtained show that the anti-corrosive paint from experiment No.(30) is suitable for steel plate and this is also considered commercially economics

  1. Simulation study on insoluble granular corrosion products deposited in PWR core

    International Nuclear Information System (INIS)

    Yang Xu; Zhou Tao; Ru Xiaolong; Lin Daping; Fang Xiaolu

    2014-01-01

    In the operation of reactor, such as fuel rods, reactor vessel internals etc. will be affected by corrosion erosion of high pressure coolant. It will produce many insoluble corrosion products. The FLUENT software is adopted to simulate insoluble granular corrosion products deposit distribution in the reactor core. The fluid phase uses the standard model to predict the flow field in the channel and forecast turbulence variation in the near-wall region. The insoluble granular corrosion products use DPM (Discrete Phase Model) to track the trajectory of the particles. The discrete phase model in FLUENT follows the Euler-Lagrange approach. The fluid phase is treated as a continuum by solving the Navier-Stokes equations, while the dispersed phase is solved by tracking a large number of particles through the calculated flow field. Through the study found, Corrosion products particles form high concentration area near the symmetry, and the entrance section of the corrosion products particles concentration is higher than export section. Corrosion products particles deposition attached on large area for the entrance of the cladding, this will change the core neutron flux distribution and the thermal conductivity of cladding material, and cause core axial offset anomaly (AOA). Corrosion products particles dot deposit in the outlet of cladding, which can lead to pitting phenomenon in a sheath. Pitting area will cause deterioration of heat transfer, destroy the cladding integrity. In view of the law of corrosion products deposition and corrosion characteristics of components in the reactor core. this paper proposes regular targeted local cleanup and other mitigation measures. (authors)

  2. 75 FR 55745 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Preliminary Results...

    Science.gov (United States)

    2010-09-14

    ... Products covered by this order are certain corrosion-resistant carbon steel flat products from Korea. These... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon... review of the countervailing duty (CVD) order on corrosion-resistant carbon steel flat products (CORE...

  3. Design considerations of fission and corrosion product in primary system of MONJU

    International Nuclear Information System (INIS)

    Yanagisawa, T.; Akagane, K.; Yamamoto, K.; Kawashima, K.

    1976-01-01

    General influence of fission and corrosion products in primary system on MONJU plant design is reviewed. Various research and development works are now in progress to decrease the generation rate, to remove the products more effectively and to develop the methods of evaluation the behaviour of radioactive products. The inventory and distribution of fission and corrosion products in the primary circuit of MONJU are given. The radiation levels on the primary components are estimated to be several roentgens per hour. (author)

  4. Evaluation of hydrogen production from CO2 corrosion of steel drums in SFR, Part 2

    International Nuclear Information System (INIS)

    Dugstad, A.; Videm, K.

    1987-06-01

    An experimental program has been carried out for the investigation of the hydrogen formation due to corrosion of steel by water containing CO 2 produced by microbiologic decomposition of paper in waste drums. The hydrogen production will be limited by a limited rate of CO 2 production, as CO 2 is consumed by corrosive reactions producing carbonate containing corrosion products. Experiments indicated that also iron oxide and hydroxides were formed together with FeCO 3 at low CO 2 partial pressures but at a rate which leads to a rather slow increase in hydrogen production. Hydrogen evaluation has been overestimated in previous reports on this subject. (authors)

  5. Barley Distillers Dried Grains with Solubles (DDGS) as Feedstock for Production of Acetone, Butanol and Ethanol

    NARCIS (Netherlands)

    Houweling-Tan, G.B.N.; Sperber, B.L.H.M.; Wal, van der H.; Bakker, R.R.C.; Lopez Contreras, A.M.

    2016-01-01

    Distillers dried grains with solubles (DDGS) represent important co-product from commercial yeast fermentations, including bioethanol, from grains. In view of the current expansion of the bioethanol fermentation process, with the concomitant increase in production of DDGS, alternative applications

  6. Study on Increasing High Temperature pH(t) to Reduce Iron Corrosion Products

    International Nuclear Information System (INIS)

    Shin, Dong Man; Hur, Nam Yong; Kim, Waang Bae

    2011-01-01

    The transportation and deposition of iron corrosion products are important elements that affect both the steam generator (SG) integrity and secondary system in pressurized water reactor (PWR) nuclear power plants. Most of iron corrosion products are generated on carbon steel materials due to flow accelerated corrosion (FAC). The several parameters like water chemistry, temperature, hydrodynamic, and steel composition affect FAC. It is well established that the at-temperature pH of the deaerated water system has a first order effect on the FAC rate of carbon steels through nuclear industry researches. In order to reduce transportation and deposition of iron corrosion products, increasing pH(t) tests were applied on secondary system of A, B units. Increasing pH(t) successfully reduced flow accelerated corrosion. The effect of increasing pH(t) to inhibit FAC was identified through the experiment and pH(t) evaluation in this paper

  7. Corrosion and corrosion control

    International Nuclear Information System (INIS)

    Khanna, A.S.; Totlani, M.K.

    1995-01-01

    Corrosion has always been associated with structures, plants, installations and equipment exposed to aggressive environments. It effects economy, safety and product reliability. Monitoring of component corrosion has thus become an essential requirement for the plant health and safety. Protection methods such as appropriate coatings, cathodic protection and use of inhibitors have become essential design parameters. High temperature corrosion, especially hot corrosion, is still a difficult concept to accommodate in corrosion allowance; there is a lack of harmonized system of performance testing of materials at high temperatures. In order to discuss and deliberate on these aspects, National Association for Corrosion Engineers International organised a National Conference on Corrosion and its Control in Bombay during November 28-30, 1995. This volume contains papers presented at the symposium. Paper relevant to INIS is indexed separately. refs., figs., tabs

  8. Concrete Cracking Prediction Including the Filling Proportion of Strand Corrosion Products

    Science.gov (United States)

    Wang, Lei; Dai, Lizhao; Zhang, Xuhui; Zhang, Jianren

    2016-01-01

    The filling of strand corrosion products during concrete crack propagation is investigated experimentally in the present paper. The effects of stirrups on the filling of corrosion products and concrete cracking are clarified. A prediction model of crack width is developed incorporating the filling proportion of corrosion products and the twisting shape of the strand. Experimental data on cracking angle, crack width, and corrosion loss obtained from accelerated corrosion tests of concrete beams are presented. The proposed model is verified by experimental data. Results show that the filling extent of corrosion products varies with crack propagation. The rust filling extent increases with the propagating crack until a critical width. Beyond the critical width, the rust-filling extent remains stable. Using stirrups can decrease the critical crack width. Stirrups can restrict crack propagation and reduce the rust filling. The tangent of the cracking angle increases with increasing corrosion loss. The prediction of corrosion-induced crack is sensitive to the rust-filling extent. PMID:28772367

  9. Quantitative assessment of the effect of corrosion product buildup on occupational exposure

    International Nuclear Information System (INIS)

    Divine, J.R.

    1982-10-01

    The program was developed to provide a method for predicting occupational exposures caused by the deposition of radioactive corrosion products outside the core of the primary system of an operating power reactor. This predictive capability will be useful in forecasting total occupational doses during maintenance, inspection, decontamination, waste treatment, and disposal. In developing a reliable predictive model, a better understanding of the parameters important to corrosion product film formation, corrosion product transport, and corrosion product film removal will be developed. This understanding can lead to new concepts in reactor design to minimize the buildup and transport of radioactive corrosion products or to improve methods of operation. To achieve this goal, three objectives were established to provide: (1) criteria for acceptable coolant sampling procedures and sampling equipment that will provide data which will be used in the model development; (2) a quantitative assessment of the effect of corrosion product deposits on occupational exposure; and (3) a model which describes the influence of flow, temperature, coolant chemistry, construction materials, radiation, and other operating parameters on the transport and buildup of corrosion products

  10. Chapter 23: Corrosion of Metals in Wood Products

    Science.gov (United States)

    Samuel L. Zelinka

    2014-01-01

    The corrosion of metals in contact with wood has been studied for over 80 years, and in most situations wood is not corrosive [1]. Recently, however, the durability of fasteners in preservative--treated wood has become a concern. Changes in legislation and certification in the United States, the European Union, and Australasia have restricted the use of chromated...

  11. TEM characterization of corrosion products formed on a SS-15ZR alloy

    International Nuclear Information System (INIS)

    Luo, J. S.; Abraham, D. P.

    2000-01-01

    The corrosion products formed on a stainless steel-15Zr (SS-15Zr) alloy have been characterized by transmission electron microscopy (TEM) and energy dispersive x-ray spectroscopy (EDS). Examination of alloy particles that were immersed in 90 C deionized water for two years revealed that different corrosion products were formed on the stainless steel and intermetallic phases. Two corrosion products were identified on an austenite particle: trevorite (NiFe 2 O 4 ) in the layer close to the metal and maghemite (Fe 2 O 3 ) in the outer layer. The corrosion layer formed on the intermetallic was uniform, adherent, and amorphous. The EDS analysis indicated that the layer was enriched in zirconium when compared with the intermetallic composition. High-resolution TEM images of the intermetallic-corrosion layer interface show an interlocking metal-oxide interface which may explain the relatively strong adherence of the corrosion layer to the intermetallic surface. These results will be used to evaluate corrosion mechanisms and predict long-term corrosion behavior of the alloy waste form

  12. Theoretical approach to description of some corrosion product transport processes in PWRs primary circuit

    International Nuclear Information System (INIS)

    Zmitko, M.

    1990-10-01

    The behavior and mass transport of corrosion products in primary circuits of PWR type reactors are described assuming that the products occur in ionic form, in colloidal form (about 0.01-0.6 μm in size) and in particulate form. The transport of the soluble form is treated as a diffusion process. For the colloidal form, allowance is made for its Van der Waals attraction and repulsion interaction with the surfaces. For particles and their agglomerates, the hydrodynamical effects of the flowing liquid on the agglomerate breakdown and re-formation of the particle suspension are taken into account. Efforts were made to employ theoretical relations rather than particular experimental data, for the conclusions to be applicable to different facilities. It is believed that the complex approach to the problem can contribute to gaining insight into the role of the individual factors and processes involved, particularly as regards colloidal particles whose effect on the formation of radiation fields is not yet fully understood. (author). 3 figs., 10 refs

  13. Bioaccumulation and food chain transfer of corrosion products from radioactive stainless steel

    International Nuclear Information System (INIS)

    Young, J.S.

    1986-07-01

    Two sets of experiments were conducted to determine if corrosion products from radioactive Type 347 stainless steel could be biologically transferred from sediment through a marine food chain, and whether corrosion products dissolved in seawater could be bioaccumulated and then eliminated. Corrosion products containing 60 Co and 63 Ni from the radioactive stainless steel were introduced into marine sediments. Infaunal polychaete worms exposed to these sediments bioaccumulated the radionuclides. The feeding of these worms to shrimp and fish resulted in a trophic transfer of the radioactive products across a one-step food chain. The magnitude of the transfers are described in terms of transfer factors. Dissolved corrosion products as measured by the radionuclides were also bioaccumulated by shrimp and fish concentrating more than fish. Concentration factors were calculated

  14. 77 FR 31877 - Corrosion-Resistant Carbon Steel Flat Products From Germany and Korea; Scheduling of Full Five...

    Science.gov (United States)

    2012-05-30

    ... INTERNATIONAL TRADE COMMISSION [Investigation Nos. 701-TA-350 and 731-TA-616 and 618 (Third Review)] Corrosion-Resistant Carbon Steel Flat Products From Germany and Korea; Scheduling of Full Five-Year Reviews... corrosion-resistant carbon steel flat products from Korea and the antidumping duty orders on corrosion...

  15. 78 FR 19210 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Final Results of...

    Science.gov (United States)

    2013-03-29

    .... Scope of the Order Products covered by this order are certain corrosion-resistant carbon steel flat... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon... countervailing duty (CVD) order on corrosion-resistant carbon steel flat products from the Republic of Korea for...

  16. 78 FR 55241 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Preliminary Results of...

    Science.gov (United States)

    2013-09-10

    ... merchandise covered by this Order \\2\\ is certain corrosion- resistant carbon steel flat products from Korea... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon... the countervailing duty (CVD) order on corrosion-resistant carbon steel flat products (CORE) from the...

  17. 78 FR 16832 - Corrosion-Resistant Carbon Steel Flat Products From Germany and the Republic of Korea: Revocation...

    Science.gov (United States)

    2013-03-19

    ...] Corrosion-Resistant Carbon Steel Flat Products From Germany and the Republic of Korea: Revocation of... ``ITC'') that revocation of the antidumping duty (``AD'') orders on corrosion-resistant carbon steel... (``Sunset'') Review, 77 FR 85 (January 3, 2012). \\2\\ See Corrosion-Resistant Carbon Steel Flat Products From...

  18. Corrosion products of reinforcement in concrete in marine and industrial environments

    International Nuclear Information System (INIS)

    Vera, R.; Villarroel, M.; Carvajal, A.M.; Vera, E.; Ortiz, C.

    2009-01-01

    The corrosion products formed on embedded steel in concrete under simulated marine and industrial conditions and natural marine environment were studied. A 0.50 water/cement ratio concrete was used and 3.5% NaCl and 180 g L -1 of H 2 SO 4 with 70 ppm of chloride ions solutions were used to simulate the synthetic medium. The initial electrochemical variables of the steel and pH, chlorides and sulfates profiles were measured according to the concrete depth. The morphology of the corrosive attack was determined via scanning electron microscopy (SEM), and the composition of the corrosion products was determined using an X-ray analyzer and an X-ray diffractometer (XRD). The protective power of the corrosion products was evaluated through anodic polarization curves in a saturated Ca(OH) 2 solution. The results from XRD and SEM show that all the resulting corrosion products correspond to lepidocrocite, goethite and magnetite mixtures; moreover, akaganeite was also identified under natural and simulated marine environments. Siderite was only detected in samples exposed to a natural marine environment. Concerning the protective nature of the corrosion products, these show lower performance in a simulated industrial environment, where the corrosion rate of the steel is up to 1.48 μm year -1

  19. Corrosion products of reinforcement in concrete in marine and industrial environments

    Energy Technology Data Exchange (ETDEWEB)

    Vera, R. [Instituto de Quimica, Facultad de Ciencias, Pontificia Universidad Catolica de Valparaiso, Avenida Brasil 2950, Casilla 4059, Valparaiso (Chile)], E-mail: rvera@ucv.cl; Villarroel, M. [Instituto de Quimica, Facultad de Ciencias, Pontificia Universidad Catolica de Valparaiso, Avenida Brasil 2950, Casilla 4059, Valparaiso (Chile); Carvajal, A.M. [Facultad de Ingenieria, Escuela de Construccion Civil, Pontificia Universidad Catolica de Chile, Av. Vicuna Mackenna 4860, Macul, Santiago (Chile); Vera, E.; Ortiz, C. [Universidad Pedagogica y Tecnologica de Colombia, Avenida Central Norte, Km 2, Tunja (Colombia)

    2009-03-15

    The corrosion products formed on embedded steel in concrete under simulated marine and industrial conditions and natural marine environment were studied. A 0.50 water/cement ratio concrete was used and 3.5% NaCl and 180 g L{sup -1} of H{sub 2}SO{sub 4} with 70 ppm of chloride ions solutions were used to simulate the synthetic medium. The initial electrochemical variables of the steel and pH, chlorides and sulfates profiles were measured according to the concrete depth. The morphology of the corrosive attack was determined via scanning electron microscopy (SEM), and the composition of the corrosion products was determined using an X-ray analyzer and an X-ray diffractometer (XRD). The protective power of the corrosion products was evaluated through anodic polarization curves in a saturated Ca(OH){sub 2} solution. The results from XRD and SEM show that all the resulting corrosion products correspond to lepidocrocite, goethite and magnetite mixtures; moreover, akaganeite was also identified under natural and simulated marine environments. Siderite was only detected in samples exposed to a natural marine environment. Concerning the protective nature of the corrosion products, these show lower performance in a simulated industrial environment, where the corrosion rate of the steel is up to 1.48 {mu}m year{sup -1}.

  20. Application of electromagnetic fields to improve the removal rate of radioactive corrosion products

    International Nuclear Information System (INIS)

    Kong, Tae Young; Lee, Kun Jai; Song, Min Chul

    2004-01-01

    To comply with increasingly strict regulations for protection against radiation exposure, many nuclear power plants have been working ceaselessly to reduce and control both the radiation sources within power plants and the radiation exposure experienced by operational and maintenance personnel. Many research studies have shown that deposits of irradiated corrosion products on the surfaces of coolant systems are the main cause of occupational radiation exposure in nuclear power plants. These corrosion product deposits on the fuel-clad surface are also known to be main factors in the onset of Axial Offset Anomaly (AOA). Hence, there is a great deal of ongoing research on water chemistry and corrosion processes. In this study, a magnetic filter with permanent magnets was devised to remove the corrosion products in the coolant stream by taking advantage of the magnetic properties of the corrosion particles. Experiments using permanent magnets to filter the corrosion products demonstrated a removal efficiency of over 90% for particles above 5 μm. This finding led to the construction of an electromagnetic device that causes the metallic particulates to flocculate into larger aggregates of about 5 μm in diameter by using a novel application of electromagnetic flocculation on radioactive corrosion products

  1. Process for the production of furfural from pentoses and/or water soluble pentosans

    NARCIS (Netherlands)

    De Jong, W.; Marcotullio, G.

    2012-01-01

    The invention is directed to a process for the production of furfural from pentoses and/or water soluble pentosans, said process comprising converting the said pentoses and/or water soluble pentosans in aqueous solution in a first step to furfural and in a second step feeding the aqueous solution

  2. POTENTIAL EFFECTS OF PHOSPHATE PRODUCTS ON LEAD SOLUBILITY IN PLUMBING SYSTEMS

    Science.gov (United States)

    Lead concentrations in drinking water can be minimized by adjusting the pH and alkalinity. Such lead solubility controls, however, may be offset by other water treatment measures that inadvertently increase lead solubility, e.g., the adding of polyphosphate-containing products. ...

  3. Spectral Analysis of CO2 Corrosion Product Scales on 13Cr Tubing Steel

    International Nuclear Information System (INIS)

    Guan-fa, Lin; Zhen-quan, Bai; Yao-rong, Feng; Xun-yuan, Xu

    2008-01-01

    CO 2 corrosion product scales formed on 13 Cr tubing steel in autoclave and in the simulated corrosion environment of oil field are investigated in the paper. The surface and cross-section profiles of the scales were observed by scanning electron microscopy (SEM), the chemical compositions of the scales were analyzed using energy dispersion analyzer of X-ray (EDAX), X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS) to confirm the corrosion mechanism of the 13 Cr steel in the simulated CO 2 corrosion environment. The results show that the corrosion scales are formed by the way of fashion corrosion, consist mainly of four elements, i.e. Fe, Cr, C and O, and with a double-layer structure, in which the surface layer is constituted of bulky and incompact crystals of FeCO 3 , and the inner layer is composed of compact fine FeCO 3 crystals and amorphous Cr(OH) 3 . Because of the characteristics of compactness and ionic permeating selectivity of the inner layer of the corrosion product scales, 13 Cr steel is more resistant in CO 2 corrosion environment

  4. Modeling of corrosion product migration in the secondary circuit of nuclear power plants with WWER-1200

    Science.gov (United States)

    Kritskii, V. G.; Berezina, I. G.; Gavrilov, A. V.; Motkova, E. A.; Zelenina, E. V.; Prokhorov, N. A.; Gorbatenko, S. P.; Tsitser, A. A.

    2016-04-01

    Models of corrosion and mass transfer of corrosion products in the pipes of the condensate-feeding and steam paths of the secondary circuit of NPPs with WWER-1200 are presented. The mass transfer and distribution of corrosion products over the currents of the working medium of the secondary circuit were calculated using the physicochemical model of mass transfer of corrosion products in which the secondary circuit is regarded as a cyclic system consisting of a number of interrelated elements. The circuit was divided into calculated regions in which the change in the parameters (flow rate, temperature, and pressure) was traced and the rates of corrosion and corrosion products entrainment, high-temperature pH, and iron concentration were calculated. The models were verified according to the results of chemical analyses at Kalinin NPP and iron corrosion product concentrations in the feed water at different NPPs depending on pH at 25°C (pH25) for service times τ ≥ 5000 h. The calculated pH values at a coolant temperature t (pH t ) in the secondary circuit of NPPs with WWER-1200 were presented. The calculation of the distribution of pH t and ethanolamine and ammonia concentrations over the condensate feed (CFC) and steam circuits is given. The models are designed for developing the calculation codes. The project solutions of ATOMPROEKT satisfy the safety and reliability requirements for power plants with WWER-1200. The calculated corrosion and corrosion product mass transfer parameters showed that the model allows the designer to choose between the increase of the correcting reagent concentration, the use of steel with higher chromium contents, and intermittent washing of the steam generator from sediments as the best solution for definite regions of the circuit.

  5. Effect of high temperature filtration on out-core corrosion product activity

    International Nuclear Information System (INIS)

    Horvath, G.L.; Bogancs, J.

    1983-01-01

    Investigation of the effect of high temperature filtration on corrosion product transport and out-core corrosion product activity has been carried out for VVER-440 plants. In the physico-chemical model applied particulate and dissolved corrosion products were taken into account. We supposed 100% effectivity for the particulate filter. It was found that about 0,5% 160 t/h/ of the main flow would result in an approx.50% reduction of the out-core corrosion product activity. Investigation of the details of the physico-chemical model in Nuclear Power Plant Paks showed a particle deposition rate measured during power transients fairly agreeing with other measurements and data used in the calculations. (author)

  6. Some in-reactor loop experiments on corrosion product transport and water chemistry

    International Nuclear Information System (INIS)

    Balakrishnan, P.V.; Allison, G.M.

    1978-01-01

    A study of the transport of activated corrosion products in the heat transport circuit of pressurized water-cooled nuclear reactors using an in-reactor loop showed that the concentration of particulate and dissolved corrosion products in the high-temperature water depends on such chemical parameters as pH and dissolved hydrogen concentration. Transients in these parameters, as well as in temperature, generally increase the concentration of suspended corrosion products. The maximum concentration of particles observed is much reduced when high-flow, high-temperature filtration is used. Filtration also reduces the steady-state concentration of particles. Dissolved corrosion products are mainly responsible for activity accumulation on surfaces. The data obtained from this study were used to estimate the rate constants for some of the transfer processes involved in the contamination of the primary heat transport circuit in water-cooled nuclear power reactors

  7. Production, solubility and antioxidant activity of curcumin nanosuspension

    Directory of Open Access Journals (Sweden)

    Deivis de Moraes Carvalho

    2015-03-01

    Full Text Available Curcumin is a powerful bioactive agent and natural antioxidant, but it is practically water-insoluble and has low bioavailability; a possible solution to this obstacle would be formulations of curcumin nanoparticles. Surfactants such as tween 80 can be used to stabilize low-solubility molecules preventing particle aggregation. The objectives of this study were the preparation of a suspension with curcumin nanoparticles in tween 80, the testing of pure curcumin solubility and of a simple mixture of curcumin with tween 80 and nanosuspension in water and ethanol as solvents, and finally the assessment of the antioxidant activity. We prepared the nanosuspension by injecting a curcumin solution in dichloromethane at low flow in water with tween 80 under heating and ultrasound. The analysis of particles size was conducted through dynamic light scattering; the non-degradation of curcumin was verified through thin-layer chromatography. The analyses of antioxidant activity were carried out according to the DPPH method. The method applied to reduce the particles size was efficient. Both the curcumin suspension and nanosuspension in tween 80 increased its solubility. Curcumin and the formulations presented antioxidant activity.

  8. The solubilities and solubility products of zirconium hydroxide and oxide after aging at 278, 313, and 333 K

    Energy Technology Data Exchange (ETDEWEB)

    Kobayashi, Taishi; Uemura, Takuya; Sasaki, Takayuki; Takagi, Ikuji [Kyoto Univ. (Japan). Dept. of Nuclear Engineering; Moriyama, Hirotake [Kyoto Univ. (Japan). Research Reactor Inst.

    2016-07-01

    The solubilities of zirconium hydroxide and oxide after aging at 278, 313, and 333 K were measured at 278, 298, 313, and 333 K in the pH{sub c} range of 0.3-7 in a 0.5 M ionic strength solution of NaClO{sub 4} and HClO{sub 4}. Size distributions of the colloidal species were investigated by ultrafiltration using membranes with different pore sizes, and the solid phases were examined by X-ray diffraction. The apparent solubility of zirconium amorphous hydroxide (Zr(OH){sub 4}(am)), prepared by the oversaturation method, decreased with increasing aging temperature (T{sub a}), and the size distributions obtained after aging at elevated temperatures indicated the growth of the colloidal species. We, therefore, suggested that agglomeration of the colloidal species and dehydration and crystallization of Zr(OH){sub 4}(am) as the solubility-limiting solid phase occurred over the course of aging at elevated temperatures. For sample solutions of the crystalline oxide (ZrO{sub 2}(cr)), the aging temperature had no significant effect on the solubility, but the solubility data at lower temperatures were found to be slightly higher than those at higher temperatures, implying a small fraction of the amorphous components. In the analysis of different solid phases (Zr(OH){sub 4}(s,T{sub a}), T{sub a} = 278, 313, and 333 K) depending on the aging temperatures, the solubility products (K{sub sp}, T{sub a}) were determined at different measurement temperatures, and the enthalpy change (Δ{sub r}H {sup circle}) for Zr{sup 4+} 4OH{sup -} <=> Zr(OH){sub 4}(s,T{sub a}) was calculated using the van't Hoff equation. The solid-phase-transformation process at elevated temperatures was also analyzed based on the obtained K{sub sp}, T{sub a} and Δ{sub r}H {sup circle} values.

  9. A mini-catalogue of metal corrosion products studied by Raman microscopy

    International Nuclear Information System (INIS)

    Bouchard, M.; Smith, D.C.

    2000-01-01

    Full text.The extensive development of physical methods of analysis since the beginning of this century has revolutionised the classical observation techniques most frequently used by the archaeologist. Raman Microscopy (RM) appears to be one of the most promising tools due to the many advantages that it offers: e.g. non-destructive, in situ, micro-analysis. RM is being applied to many archaeological fields as well as to industrial or environmental sectors. In relation with parallel studies made on the identification of corrosion products on archaeological materials, and according to the principal condition for the RM characterisation of an unknown product being the comparison of its Raman spectrum with known standard spectra, the essential aim of this study is to build a mini-catalogue of standard corrosion products susceptible to be found on metallic objects; these could be from archaeological as well as from modern contexts. However, it is noted that the identification of a corrosion product may suggest either an urgent intervention from the restoration team (in the case of active corrosion products), or a stabilisation of the corrosion layer if this is considered to be a protective layer. All the standard samples are natural minerals coming from the Museum National d'Histoire Naturelle in Paris (France) and correspond to the corrosion products most frequently found on metals such copper, zinc, lead or tin. These samples have been analyzed by RM and also confirmed by powder x-ray diffraction analysis. This catalogue, including more than 30 standard species corresponding to the most common metal corrosion products, is very useful for the different studies in progress in collaboration with different archaeological metal restoration teams. The near future will probably see a mobile Raman Microprobe (MRM) equipped with many different mini-catalogues on the site of a corroded mettalic bridge, a corroded canalisation or under the sea to rapidly identify the different

  10. Mössbauer effect study of corrosion products from a Brazilian oil refinery

    Science.gov (United States)

    da Costa, M. I.; Kunrath, J. I.; Moro, J. T.; da Cunha, J. B. M.; Englert, G.; Comparsi, L. U.; Muller, I. L.

    1993-04-01

    Corrosion of an oil refining plant in southern Brazil is controlled by placing metallic coupons in strategic places of the unit. The amount of the corrosion products formed after two months of exposure of the coupons is then obtained by weight loss measurements. To have a better insight of these products an analysis by Conversion Electron and transmission Mössbauer spectroscopies was done on some of the coupons. This paper reports some of the findings.

  11. Influence of phosphorus precipitation on permeability and soluble microbial product concentration in a membrane bioreactor

    Czech Academy of Sciences Publication Activity Database

    Gómez, M.; Dvořák, L.; Růžičková, I.; Wanner, J.; Holba, Marek; Sýkorová, E.

    2013-01-01

    Roč. 129, Feb 2013 (2013), s. 164-169 ISSN 0960-8524 Institutional support: RVO:67985939 Keywords : membrane bioreactor * coagulant adition * soluble microbial products Subject RIV: EF - Botanics Impact factor: 5.039, year: 2013

  12. Corrosion product layers on magnesium alloys AZ31 and AZ61: Surface chemistry and protective ability

    Science.gov (United States)

    Feliu, S.; Llorente, I.

    2015-08-01

    This paper studies the chemical composition of the corrosion product layers formed on magnesium alloys AZ31 and AZ61 following immersion in 0.6 M NaCl, with a view to better understanding their protective action. Relative differences in the chemical nature of the layers were quantified by X-ray photoelectron spectroscopy (XPS), scanning electron microscopy (SEM), energy dispersive analysis of X-ray (EDX) and low-angle X-ray diffraction (XRD). Corrosion behavior was investigated by Electrochemical Impedance Spectroscopy (EIS) and hydrogen evolution measurement. An inhibitive effect from the corrosion product layers was observed from EIS, principally in the case of AZ31, as confirmed by hydrogen evolution tests. A link was found between carbonate enrichment observed by XPS in the surface of the corrosion product layer, concomitant with the increase in the protective properties observed by EIS.

  13. Studies on dissolution characteristics of simulated corrosion products on pressurized water reactor primary coolant loops. Pt.2: Cobalt simulated corrosion product

    International Nuclear Information System (INIS)

    Li Shan; Zhou Xianyu

    1997-01-01

    The studies on the dissolution characteristics of simulated corrosion product of cobalt on pressurized water reactor primary coolant loops in aqueous solution of citric acid, hydrogen peroxide and citric acid-hydrogen peroxide have been performed. The results show that the portion of the dissolved simulated corrosion product of cobalt in citric acid aqueous solution clearly increases with a rise in citric acid concentration and is ten times above the corresponding value of iron. The portion of the products that dissolve is the largest at pH 3.00 in the pH range of 2.33∼4.50 and at 70 degree C in the range of 60∼80 degree C. It is shown that the portion of the dissolved simulated corrosion product of cobalt in hydrogen peroxide aqueous solution is smaller than the corresponding value in citric acid, and that the portion of the dissolved simulated corrosion product of cobalt in aqueous solution of hydrogen peroxide-citric acid is larger than the corresponding value in single citric acid aqueous solution

  14. Estimation of elastic modulus of reinforcement corrosion products using inverse analysis of digital image correlation measurements for input in corrosion-induced cracking model

    DEFF Research Database (Denmark)

    Pease, Bradley Justin; Michel, Alexander; Thybo, Anna Emilie A.

    2012-01-01

    A combined experimental and numerical approach for estimating the elastic modulus of reinforcement corrosion products is presented. Deformations between steel and mortar were measured using digital image correlation during accelerated corrosion testing at 100 μA/cm2 (~1.16 mm/year). Measured defo...

  15. Activity of corrosion products in pool type reactors with ascending flow in the core

    International Nuclear Information System (INIS)

    Andrade e Silva, Graciete S. de; Queiroz Bogado Leite, Sergio de

    1995-01-01

    A model for the activity of corrosion products in the water of a pool type reactor with ascending flow is presented. The problem is described by a set of coupled differential equations relating the radioisotope concentrations in the core and pool circuits and taking into account two types of radioactive sources: i) those from radioactive species formed in the fuel cladding, control elements, reflector, etc, and afterwards released to the primary stream by corrosion (named reactor sources) and ii) those formed from non radioactive isotopes entering the primary stream by corrosion of the circuit components and being activated when passing through the core (named circuit sources). (author). 6 refs, 3 figs, 4 tabs

  16. Simulations of corrosion product transfer with the OSCAR V1.2 code

    International Nuclear Information System (INIS)

    Dacquait, F.; Francescatto, J.; Broutin, F.; Genin, J.B.; Benier, G.; Girard, M.; You, D.; Ranchoux, G.; Bonnefon, J.; Bachet, M.; Riot, G.

    2012-09-01

    Activated Corrosion Products (ACPs) generate a radiation field in PWRs, which is the major contributor to the dose absorbed by nuclear power plant staff working during shutdown operations and maintenance. Therefore, a thorough understanding of the mechanisms that control the corrosion product transfer is of the highest importance. Since the 1970's, the R and D strategy in France has been based on experiments in test loops representative of PWR conditions, on in-situ gamma spectrometry measurements of the PWR primary system contamination and on simulation code development. The simulation of corrosion product transfers in PWR primary circuits is a major challenge since it involves many physical and chemical phenomena including: corrosion, dissolution, precipitation, erosion, deposition, convection, activation... In addition to the intrinsic difficulty of multi-physics modelling, the primary systems present severe operating conditions (300 deg. C, 150 bar, neutron flux, fluid velocity up to 15 m.s -1 and very low corrosion product concentrations). The purpose of the OSCAR code, developed by the CEA in cooperation with EDF and AREVA NP, is to predict the PWR primary system contamination by corrosion and fission products. The OSCAR code is considered to be not only a tool for numerical simulations and predictions (operational practices improvements and new-built PWRs design) but also one that might combine and organise all new knowledge useful to progress on contamination. The OSCAR code for Products of Corrosion, OSCAR PC, allows researchers to analyse the corrosion product behaviour and to calculate the ACP volume and surface activities of the primary and auxiliary systems. In the new version, OSCAR PC V1.2, the corrosion product transfer in the particulate form is enhanced and a new feature is the possibility to simulate cold shutdowns. In order to validate this version, the contamination transfer has been simulated in 5 French PWRs with different operating and

  17. Characterization of corrosion products from Nd-Fe-B magnets used in dental prostheses

    Energy Technology Data Exchange (ETDEWEB)

    Saiki, Mitiko; Rogero, Sizue O.; Costa, Isolda; Dantas, Elisabeth; Oliveira, Mara C.L. [Instituto de Pesquisas Energeticas e Nucleares (IPEN), Sao Paulo, SP (Brazil)

    2002-07-01

    A special group of magnets composed mainly by Nd-Fe-B has been widely used in dental applications as retentive devices for overdentures, due to their strong force and compactness. Dental materials should present high corrosion resistance and be innocuous to human tissues, however, Nd-Fe-B magnets are highly susceptible to corrosion. This work presents results obtained in the elemental analysis of Nd-Fe-B magnets and their corrosion products. The corrosion products were analyzed in the extracts of culture medium where the magnets had been immersed for 10 days at 37 deg C. Elements B, Co, Fe, La, Nd, Dy, Pr, Sm, Ho, Yb and Lu were found in the magnet and the analysis of extract indicated that Co, Fe and Nd are released from the magnet to the extract. Toxicity was also investigated in this extract using the neutral red uptake cytotoxicity assay. Acknowledgements: To FAPESP and CNPq for financial support. (author)

  18. Characterization of corrosion products from Nd-Fe-B magnets used in dental prostheses

    International Nuclear Information System (INIS)

    Saiki, Mitiko; Rogero, Sizue O.; Costa, Isolda; Dantas, Elisabeth; Oliveira, Mara C.L.

    2002-01-01

    A special group of magnets composed mainly by Nd-Fe-B has been widely used in dental applications as retentive devices for overdentures, due to their strong force and compactness. Dental materials should present high corrosion resistance and be innocuous to human tissues, however, Nd-Fe-B magnets are highly susceptible to corrosion. This work presents results obtained in the elemental analysis of Nd-Fe-B magnets and their corrosion products. The corrosion products were analyzed in the extracts of culture medium where the magnets had been immersed for 10 days at 37 deg C. Elements B, Co, Fe, La, Nd, Dy, Pr, Sm, Ho, Yb and Lu were found in the magnet and the analysis of extract indicated that Co, Fe and Nd are released from the magnet to the extract. Toxicity was also investigated in this extract using the neutral red uptake cytotoxicity assay. Acknowledgements: To FAPESP and CNPq for financial support. (author)

  19. Impact of β- radiolysis and transient products on irradiation-enhanced corrosion of zirconium alloys

    International Nuclear Information System (INIS)

    Lemaignan, C.

    1992-01-01

    An analysis has been undertaken of the various cases of local enhancement of the corrosion rate of zirconium alloys under irradiation. It is observed that in most cases a strong emission of energetic β - is present leading to a local energy desorption rate higher than the core average. This suggests that the local transient radiolytic oxidising species produced in the coolant by the β - particles could contribute to corrosion enhancement, by increasing the local corrosion potential. This process is applicable to the local enhanced corrosion found in front of stainless steels structural parts, due to the contribution of Mn, in front of Pt inserts and Cu-rich cruds. It explains also the irradiation corrosion enhancement of Cu-rich Zr alloys. Enhanced corrosion around neutron absorbing material is explained similarly by pair production from conversion of high energy capture photons in the cladding, leading to energetic electrons. The same process was found to be active with other highly ionising species like α in Ni-rich alloys and fission products in homogeneous reactors. This mechanism, applicable for an explanation of localised irradiation-enhanced corrosion, is proposed to be extended to the reactor core, where the general enhancement of Zr-alloy corrosion under irradiation would be due to the general radiolysis. It suggests that care should be taken to avoid any source of β - emission or other ionising species in the reactor core that could give an increase of energy deposition rate for radiolysis. Also the corrosion testing conditions for the materials to be used in reactors have to be relevant to the radiolytic environments found in the reactor cores. (orig.)

  20. Coupled modelling of convergence, steel corrosion, gas production and brine flow in a rock salt repository

    International Nuclear Information System (INIS)

    Becker, D.A.; Hirsekorn, R.P.

    2013-01-01

    This poster presents the global simulation of the behaviour of thick-walled steel containers piled up in a borehole in a rock salt repository. The simulation takes into account: the convergence by the creeping of rock salt, the backfill and waste compaction, the porosity dependent flow resistance, the anaerobic corrosion (iron to magnetite transformation, gas production, brine consumption, water consumption and salt precipitation) and pressure development. Mechanical influence of corrosion has not yet been taken into account in the integrated code LOPOS

  1. Surface area and chemical reactivity characteristics of uranium metal corrosion products.

    Energy Technology Data Exchange (ETDEWEB)

    Totemeier, T. C.

    1998-02-17

    The results of an initial characterization of hydride-containing corrosion products from uranium metal Zero Power Physics Reactor (ZPPR) fuel plates are presented. Sorption analyses using the BET method with a Kr adsorbate were performed to measure the specific areas of corrosion product samples. The specific surface areas of the corrosion products varied from 0.66 to 1.01 m{sup 2}/g. The reactivity of the products in Ar-9%O{sub 2} and Ar-20%O{sub 2} were measured at temperatures between 35 C and 150 C using a thermo-gravimetric analyzer. Ignition of the products occurred at temperatures of 150 C and above. The oxidation rates below ignition were comparable to rates observed for uranium metal.

  2. Surface area and chemical reactivity characteristics of uranium metal corrosion products

    International Nuclear Information System (INIS)

    Totemeier, T. C.

    1998-01-01

    The results of an initial characterization of hydride-containing corrosion products from uranium metal Zero Power Physics Reactor (ZPPR) fuel plates are presented. Sorption analyses using the BET method with a Kr adsorbate were performed to measure the specific areas of corrosion product samples. The specific surface areas of the corrosion products varied from 0.66 to 1.01 m 2 /g. The reactivity of the products in Ar-9%O 2 and Ar-20%O 2 were measured at temperatures between 35 C and 150 C using a thermo-gravimetric analyzer. Ignition of the products occurred at temperatures of 150 C and above. The oxidation rates below ignition were comparable to rates observed for uranium metal

  3. Preparation, characterization and solubility product constant of AmOHCO3

    International Nuclear Information System (INIS)

    Silva, R.J.

    1985-01-01

    An investigation into the nature and solubility of a stable solid phase formed by a trivalent actinide, 243 Am 3+ , in dilute aqueous carbonate solutions was conducted. The compound exhibited an x-ray powder diffraction pattern which was nearly identical to that reported for NdOHCO 3 - type A. The pattern could be indexed in the orthorhombic system with unit cell parameters a = 4.958, b = 8.487, and c = 7.215 A. The steady-state solubility of the compound was determined from the results of both dissolution and precipitation experiments. The average solubility product quotient for 0.1M ionic strength, 25 +- 1 0 C and 1 atmosphere pressure was found to be 583 +- 206. The solubility product constant for zero ionic strength was estimated to be 335 +- 120. 22 references, 3 tables

  4. Preparation, characterization and solubility product constant of AmOHCO/sub 3/

    Energy Technology Data Exchange (ETDEWEB)

    Silva, R.J.

    1985-01-12

    An investigation into the nature and solubility of a stable solid phase formed by a trivalent actinide, /sup 243/Am/sup 3 +/, in dilute aqueous carbonate solutions was conducted. The compound exhibited an x-ray powder diffraction pattern which was nearly identical to that reported for NdOHCO/sub 3/ - type A. The pattern could be indexed in the orthorhombic system with unit cell parameters a = 4.958, b = 8.487, and c = 7.215 A. The steady-state solubility of the compound was determined from the results of both dissolution and precipitation experiments. The average solubility product quotient for 0.1M ionic strength, 25 +- 1/sup 0/C and 1 atmosphere pressure was found to be 583 +- 206. The solubility product constant for zero ionic strength was estimated to be 335 +- 120. 22 references, 3 tables.

  5. Modelling and numerical simulation of the corrosion product transport in the pressurised water reactor primary circuit

    International Nuclear Information System (INIS)

    Marchetto, C.

    2002-05-01

    During operation of pressurised water reactor, corrosion of the primary circuit alloys leads to the release of metallic species such as iron, nickel and cobalt in the primary fluid. These corrosion products are implicated in different transport phenomena and are activated in the reactor core where they are submitted to neutron flux. The radioactive corrosion products are afterwards present in the out of flux parts of primary circuit where they generate a radiation field. The first part of this study deals with the modelling of the corrosion: product transport phenomena. In particular, considering the current state of the art, corrosion and release mechanisms are described empirically, which allows to take into account the material surface properties. New mass balance equations describing the corrosion product behaviour are thus obtained. The numerical resolution of these equations is implemented in the second part of this work. In order to obtain large time steps, we choose an implicit time scheme. The associated system is linearized from the Newton method and is solved by a preconditioned GMRES method. Moreover, a time step auto-adaptive management based on Newton iterations is performed. Consequently, an efficient resolution has been implemented, allowing to describe not only the quasi-steady evolutions but also the fast transients. In a last step, numerical simulations are carried out in order to validate the new corrosion product transport modelling and to illustrate the capabilities of this modelling. Notably, the numerical results obtained indicate that the code allows to restore the on-site observations underlining the influence of material surface properties on reactor contamination. (author)

  6. Morphology of the ash corrosion products on the P92 steel

    International Nuclear Information System (INIS)

    Hernas, A.; Imosa, M.

    2004-01-01

    The P92 steel, owing to its high mechanical strength at an elevated temperature, is one of the new steel types intended for the components of modern boilers in the power engineering industry. Currently, attempts are being undertaken to use the P92 steel for the components of boiler units in municipal waste incineration plants. Therefore, it is important that an analysis be made of the P92 steel resistance to the high-temperature chlorine - sulfur corrosion impact, the latter being the main factor which limits durability of boilers in waste incineration plants. The present article presents the investigation of P92 steel corrosion resistance under the conditions of high-temperature chlorine- sulfur corrosion in an atmosphere of flue gas with ashes. The analyses were conducted by means of laboratory tests in an atmosphere containing sulfur and chlorine compounds. The morphology of corrosion products was determined by scanning microscopy and X-ray analysis methods. (author)

  7. Guidelines for prediction of CO{sub 2} corrosion in oil and gas production systems

    Energy Technology Data Exchange (ETDEWEB)

    Nyborg, Rolf

    2009-09-15

    A group of corrosion experts from different oil companies has prepared guidelines for use of CO{sub 2} corrosion prediction tools. The guidelines are intended for use in design and engineering practice applied by companies operating oil and gas production facilities. This document attempts to set minimum guidelines that should be common to most companies. The document is sufficiently flexible to allow individual companies to adapt the information set forth in this document to their own environment and requirements. A methodology for defining the Iikelihood of corrosion and the impact on CO{sub 2} prediction is developed. The CO{sub 2} prediction is based on existing tools. An overview of available CO{sub 2} corrosion prediction models evaluated by the participants is given. It is the responsibility of the operator to select which model to use. (Author)

  8. Processes controlling the production of aromatic water-soluble organic matter during litter decomposition

    NARCIS (Netherlands)

    Klotzbücher, T.; Kaiser, K.; Filley, T.R.; Kalbitz, K.

    2013-01-01

    Dissolved organic matter (DOM) plays a fundamental role for many soil processes. For instance, production, transport, and retention of DOM control properties and long-term storage of organic matter in mineral soils. Production of water-soluble compounds during the decomposition of plant litter is a

  9. Corrosion product layers on magnesium alloys AZ31 and AZ61: Surface chemistry and protective ability

    International Nuclear Information System (INIS)

    Feliu, S.; Llorente, I.

    2015-01-01

    Highlights: • Surface chemistry of the corrosion product layers on magnesium alloys. • Influence of the type of alloy on the carbonate surface enrichment. • Relation between surface composition and protection properties. - Abstract: This paper studies the chemical composition of the corrosion product layers formed on magnesium alloys AZ31 and AZ61 following immersion in 0.6 M NaCl, with a view to better understanding their protective action. Relative differences in the chemical nature of the layers were quantified by X-ray photoelectron spectroscopy (XPS), scanning electron microscopy (SEM), energy dispersive analysis of X-ray (EDX) and low-angle X-ray diffraction (XRD). Corrosion behavior was investigated by Electrochemical Impedance Spectroscopy (EIS) and hydrogen evolution measurement. An inhibitive effect from the corrosion product layers was observed from EIS, principally in the case of AZ31, as confirmed by hydrogen evolution tests. A link was found between carbonate enrichment observed by XPS in the surface of the corrosion product layer, concomitant with the increase in the protective properties observed by EIS

  10. Corrosion product layers on magnesium alloys AZ31 and AZ61: Surface chemistry and protective ability

    Energy Technology Data Exchange (ETDEWEB)

    Feliu, S., E-mail: sfeliu@cenim.csic.es; Llorente, I.

    2015-08-30

    Highlights: • Surface chemistry of the corrosion product layers on magnesium alloys. • Influence of the type of alloy on the carbonate surface enrichment. • Relation between surface composition and protection properties. - Abstract: This paper studies the chemical composition of the corrosion product layers formed on magnesium alloys AZ31 and AZ61 following immersion in 0.6 M NaCl, with a view to better understanding their protective action. Relative differences in the chemical nature of the layers were quantified by X-ray photoelectron spectroscopy (XPS), scanning electron microscopy (SEM), energy dispersive analysis of X-ray (EDX) and low-angle X-ray diffraction (XRD). Corrosion behavior was investigated by Electrochemical Impedance Spectroscopy (EIS) and hydrogen evolution measurement. An inhibitive effect from the corrosion product layers was observed from EIS, principally in the case of AZ31, as confirmed by hydrogen evolution tests. A link was found between carbonate enrichment observed by XPS in the surface of the corrosion product layer, concomitant with the increase in the protective properties observed by EIS.

  11. The formation, composition and structure of corrosion products in CANDU nuclear power reactors

    International Nuclear Information System (INIS)

    Rummery, T.E.

    1978-01-01

    To gain a better understanding of the formation and transport of corrosion products in CANDU-PHW power reactors, and the role played by these products in the generation and subsequent fixation of radioactive species, we have examined in detail several surfaces removed from the Douglas Point Generating Station (Douglas Point, Ontario). Results are given for the surface of the primary-side of a Monel-400 boiler tube, and surfaces of carbon steel piping at the inlet and outlet of the boiler. The experimental techniques that were used included sequential acid stripping, X-ray diffractometry, scanning electron microscopy and energy dispersive X-ray spectrometry. The corrosion products on the Monel-400 were mainly nickel, copper, nickel oxide and nickel-deficient nickel ferrite and varied in composition and quantity as a function of both distance from the boiler inlet, and depth in the corrosion layer. The radioactive cobalt ( 60 Co) content was localized in 'streaks' deposited in the straight sections of the boiler tube, but distributed uniformly over the whole surface in the downstream bend section. The material covering the carbon steel surface comprised three phases: magnetite, aluminosilicate particles at the outermost surface, and a mixed cation spinel phase uniformly distributed over the surface at the corrosion film-water interface. The formation, composition and structure of the corrosion products are discussed. (author)

  12. Method of separation of fission and corrosion products and of corresponding isotopes from liquid waste

    International Nuclear Information System (INIS)

    Prochazka, H.; Stamberg, K.; Jilek, R.; Hulak, P.; Katzer, J.

    1976-01-01

    A method of separating fission and corrosion products and corresponding stable isotopes from liquid waste is described. Mycelia of fungi are used as sorbents for retaining these products on their surface and within their pores. Methods of activation or regeneration of the sorbent are outlined. 11 claims

  13. Corrosion of ferritic steels by molten lithium: Influence of competing thermal gradient mass transfer and surface product reactions

    International Nuclear Information System (INIS)

    Tortorelli, P.F.

    1987-10-01

    An Fe-12Cr-1MoVW steel was exposed to thermally convective lithium for 6962 h. Results showed that the weight change profile of Fe-12Cr-1MoVW steel changed substantially as the maximum loop temperature was raised from 500 to 600 0 C. Furthermore, for a particular loop experiment, changes in the structure and composition of the exposed surfaces did not reflect typical thermal gradient mass transfer effects for all elements: the surface concentration of chromium was often a maximum at intermediate temperatures, while nickel (present at low concentrations in the starting material) tended to be transported to the coldest part of the loop. Such data were interpreted in terms of a qualitative model in which there are different dominant reactions or the various constituents of the ferritic steels (surface product formation involving nitrogen and/or carbon and solubility-driven elemental transport). This competition among different reactions is important in evaluating overall corrosion behavior and the effects of temperature. The overall corrosion rate of the 12Cr-1MoVW steel was relatively low when compared to that for austenitic stainless steel exposed under similar conditions

  14. Corrosion products, activity transport and deposition in boiling water reactor recirculation systems

    International Nuclear Information System (INIS)

    Alder, H.P.; Buckley, D.; Grauer, R.; Wiedemann, K.H.

    1992-01-01

    The deposition of activated corrosion products in the recirculation loops of Boiling Water Reactors produces increased radiation levels which lead to a corresponding increase in personnel radiation dose during shut down and maintenance. The major part of this dose rate is due to cobalt-60. Based on a comprehensive literature study concerning this theme, it has been attempted to identify the individual stages of the activity build-up and to classify their importance. The following areas are discussed in detail: The origins of the corrosion products and of cobalt-59 in the reactor feedwaters; the consolidation of the cobalt in the fuel pins deposits (activation); the release and transport of cobalt-60; the build-up of cobalt-60 in the corrosion products in the recirculation loops. Existing models of the build-up of circuit radioactivity are discussed and the operating experiences from selected reactors are summarized. 90 refs, figs and tabs

  15. Modelling the behaviour of corrosion products in the primary heat transfer circuits of pressurised water reactors

    International Nuclear Information System (INIS)

    Rodliffe, R.S.; Polley, M.V.; Thornton, E.W.

    1985-05-01

    The redistribution of corrosion products from the primary circuit surfaces of a water reactor can result in increased flow resistance, poorer heat transfer performance, fuel failure and radioactive contamination of circuit surfaces. The environment is generally sufficiently well controlled to ensure that the first three effects are not limiting. The last effect is of particular importance since radioactive corrosion products are major contributors to shutdown fields and since it is necessary to ensure that the radiation exposure of personnel is as low as reasonably achievable. This review focusses attention on the principles which must form the basis for any mechanistic model describing the formation, transport and deposition of radioactive corrosion products. It is relevant to all water reactors in which the primary heat transfer medium is predominantly single-phase water and in which steam is generated in a secondary circuit, i.e. including CANDU pressurised heavy water reactors, Sovient VVERs, etc. (author)

  16. The effect of organic matter associated with the corrosion products on the corrosion of mild steel in the Arabian Sea

    Digital Repository Service at National Institute of Oceanography (India)

    Bhosle, N.B.; Wagh, A.B.

    The corrosion of mild steel immersed at various depths (0-100 m) from three stations of the Arabian Sea was investigated. The corrosion of mild steel decreased with increasing immersion depth. Significant positive relationships were observed between...

  17. Strontium Concentrations in Corrosion Products from Residential Drinking Water Distribution Systems

    Science.gov (United States)

    2013-04-22

    compounds are Sr2+SO4 (celestite) and Sr 2+ CO3 (strontianite). Naturally occurring Sr2+ compounds are highly soluble in water; consequently, Sr2+ is readily...and one from Utility C (UC) were collected from single 30 cm long sections of 15 cm id unlined cast iron residential mains. Two iron corrosion...in top-up mode at 7 GeV and a ring current of 101 mA. A 0.5 mm premonochromator slit width and a Si(111) double crystal monochromator detuned by 10

  18. Hydrogen Production by a Hyperthermophilic Membrane-Bound Hydrogenase in Soluble Nanolipoprotein Particles

    Energy Technology Data Exchange (ETDEWEB)

    Baker, S E; Hopkins, R C; Blanchette, C; Walsworth, V; Sumbad, R; Fischer, N; Kuhn, E; Coleman, M; Chromy, B; Letant, S; Hoeprich, P; Adams, M W; Henderson, P T

    2008-10-22

    Hydrogenases constitute a promising class of enzymes for ex vivo hydrogen production. Implementation of such applications is currently hindered by oxygen sensitivity and, in the case of membrane-bound hydrogenases (MBH), poor water solubility. Nanolipoprotein particles (NLPs), formed from apolipoproteins and phospholipids, offer a novel means to incorporate MBH into in a well-defined water-soluble matrix that maintains the enzymatic activity and is amenable to incorporation into more complex architectures. We report the synthesis, hydrogen-evolving activity and physical characterization of the first MBH-NLP assembly. This may ultimately lead to the development of biomimetic hydrogen production devices.

  19. The Influence of Pseudomonas fluorescens on Corrosion Products of Archaeological Tin-Bronze Analogues

    Science.gov (United States)

    Ghiara, G.; Grande, C.; Ferrando, S.; Piccardo, P.

    2018-01-01

    In this study, tin-bronze analogues of archaeological objects were investigated in the presence of an aerobic Pseudomonas fluorescens strain in a solution, containing chlorides, sulfates, carbonates and nitrates according to a previous archaeological characterization. Classical fixation protocols were employed in order to verify the attachment capacity of such bacteria. In addition, classical metallurgical analytical techniques were used to detect the effect of bacteria on the formation of uncommon corrosion products in such an environment. Results indicate quite a good attachment capacity of the bacteria to the metallic surface and the formation of the uncommon corrosion products sulfates and sulfides is probably connected to the bacterial metabolism.

  20. XPS response in the corrosion products analysis for copper exposed at clean air environment

    International Nuclear Information System (INIS)

    Mariaca, L.; Morcillo, M.; Feliu Jr, S.; Gonzalez, J.A.

    1998-01-01

    In this work is presented the obtained response for superficial analysis technique by X-ray photoelectron spectroscopy (XPS or ESCA), to determine the corrosion products formed during the copper exposure at environment without pollutants (clean air) at 50, 70 and 90 % of relative humidity at 35 Centigrade. One of the copper corrosion products most knew is Cu 2 O. This oxide is formed instantly to be exposed the copper at air. However in function of the exposure time and the relative humidity at it is exposed, the Cu 2 O oxide is transformed at Cu O and Cu(OH) 2 (Author)

  1. Treating thin stillage or condensed distillers solubles with phytase for production of low phytate co-products

    Science.gov (United States)

    Fuel ethanol production from grains is mainly based on dry grind processing, during which phytate is concentrated about three fold in distillers dried grains with solubles (DDGS), a major co-product. For reducing phyate in DDGS, two industrial phytase preparations (Natuphos and Ronozyme) were used ...

  2. Investigations of the diverse corrosion products on steel in a hydrogen sulfide environment

    International Nuclear Information System (INIS)

    Bai, Pengpeng; Zheng, Shuqi; Zhao, Hui; Ding, Yu; Wu, Jian; Chen, Changfeng

    2014-01-01

    Highlights: • Diverse corrosion products on steel are investigated in H 2 S environment. • The sequence of the main corrosion products is mackinawite + cubic FeS → troilite. • The large single beam-shaped troilite has a growth pattern along the c axis. • The flower-like troilite develops from beam- or hexagonal wire-shaped grains. • The corresponding crystal structure and morphology of the products are provided. - Abstract: The corrosion products of carbon steel in aqueous H 2 S environment are investigated. The products, which include mackinawite, cubic FeS, troilite, and pyrite, are characterized through their shapes, chemical compositions and crystal structures. Mackinawite appears with a flake shape. Cubic FeS has a perfect/truncated octahedral shape, and pyrite is framboid-shaped. Flower-shaped troilite is developed from beam- or hexagonal wire-shaped grains by electrostatic interactions along a certain lattice plane. The large single beam-shaped troilite has a growth pattern along the c axis. The corresponding crystal structure and micro-morphology of the corrosion products are provided, and the three-dimensional models of them are generated

  3. In situ Raman identification of corrosion products on galvanized steel sheets

    International Nuclear Information System (INIS)

    Bernard, M.C.; Hugot le Goff, A.; Massinon, D.; Phillips, N.; Thierry, D.

    1992-01-01

    In situ Raman spectroscopy was used to identify corrosion products on zinc immersed in chloride solutions. In aerated 0,03 M NaCl solution, zinc carbonate was identified as the main corrosion product. Even with higher chloride concentrations, for which zinc hydroxychloride was also detected, the carbon dioxide concentration is likely to be the rate controlling factor of the corrosion process. In a confinement experiment, Raman analysis revealed that the upper face of the sample was covered with zinc carbonate, whereas hydroxychlorides were identified on the confined face. This result confirmed the hypothesis of a differential aeration mechanism responsible for the formation of zinc hydroxychloride. This is in good agreement with Raman spectroscopy results obtained in the case of painted galvanized steel

  4. Simulation of corrosion product activity in ion- exchanger of PWR under acceleration of corrosion and flow rate perturbations

    International Nuclear Information System (INIS)

    Mirza, N.M.; Mirza, S.M.; Rafique, M.

    2005-01-01

    In this paper computer code developed earlier by the authors (CPAIR-P) has been employed to compute corrosion product activity in PWRs for flow rate perturbations. The values of radioactivity in ion exchanger of Pressurized Water Reactor (PWR) under normal and flow rate perturbation conditions have been calculated. For linearly accelerating corrosion rates, activity saturates for removal rate of 600 cm/sup 3// s in primary coolant of PWR. A higher removal rate of 750 cm/sup 3// s was selected for which the saturation value is sufficiently low (0. 28 micro Ci/cm/sup 3/). Simulation results shows that the Fe/sup 59/ Na/sup 24/, Mo/sup 99/, Mn/sup 56/ reaches saturation values with in about 700 hours of reactor operation. However, Co/sup 58/ and Co/sup 60/ keep on accumulating and do not saturate with in 2000 hours of these simulation time. When flow rate is decreased by 10% of rated flow rate after 500 hours of reactor operation, a dip in activity is seen, which reaches to the value of 0.00138 micro Ci cm/sup -3/ then again it begins to rise and reaches saturation value of 0.00147 cm/sup 3//s. (author)

  5. Production of water-soluble sago waste - HAMPAS

    International Nuclear Information System (INIS)

    Norhazlin Zainuddin; Kamaruddin Hashim; Kamaruddin Bahari; Mansor Ahmad; Wan Md Zin Wan Yunus

    2002-01-01

    Carboxylmethyl sago waste (CMSW) was prepared in completely heterogeneous conditions as a product of the reaction of sago waste and sodium monochloroacetate (MCA) in mixed solution of isopropanol and sodium hydroxide (NaOH). The results showed that the DS values depend on the concentration of NaOH, ratio of MCA to anhydroglucose unit (AGU), (MCA:AGU), and also time and temperature of the reaction. DS value increased with increasing the concentration of NaOH and reaction temperature, but further increase will reduce the value of DS. Increasing the reaction time will increase the DS value and achieve a constant value after 2 hours. The study showed that the highest value of DS i.e. 1.04, could be achieved at 2:1 of MCA:AGU ratio, NaOh concentration of 25% and 2 hours reaction time at 55 degree C. (Author)

  6. Solubility is the most important mass transfer factor

    International Nuclear Information System (INIS)

    Slobodov, A.A.; Zarembo, V.I.

    1992-01-01

    The existence of the quantitative correlation between mass transfer and equilibrium solubility of corrosion products of construction materials in water circuits of power plants is shown. Thermodynamic and mathematical methods of modeling and calculating for these processes are developed. The results for iron based materials - aqueous solution systems in a wide range of temperature, pH, oxygen-hydrogen concentrations are presented. The optimization conditions for mass transfer, sedimentation of corrosion products for BWR, PWR reactors, etc. have been obtained

  7. Underground pipeline corrosion

    CERN Document Server

    Orazem, Mark

    2014-01-01

    Underground pipelines transporting liquid petroleum products and natural gas are critical components of civil infrastructure, making corrosion prevention an essential part of asset-protection strategy. Underground Pipeline Corrosion provides a basic understanding of the problems associated with corrosion detection and mitigation, and of the state of the art in corrosion prevention. The topics covered in part one include: basic principles for corrosion in underground pipelines, AC-induced corrosion of underground pipelines, significance of corrosion in onshore oil and gas pipelines, n

  8. 75 FR 18153 - Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2010-04-09

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Extension of Time Limit for Preliminary Results of... countervailing duty order on corrosion-resistant carbon steel flat products (CORE) from Korea. See Countervailing...

  9. 77 FR 16810 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2012-03-22

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limit for Preliminary Results of... Register the countervailing duty order on corrosion-resistant carbon steel flat products (CORE) from Korea...

  10. 76 FR 20954 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2011-04-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limit for Preliminary Results of... Register the countervailing duty order on corrosion-resistant carbon steel flat products (CORE) from Korea...

  11. 77 FR 25405 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2012-04-30

    ... antidumping duty order on corrosion-resistant carbon steel flat products from the Republic of Korea, covering... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limit for the Preliminary Results of...

  12. 76 FR 21332 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2011-04-15

    ... antidumping duty order on corrosion-resistant carbon steel flat products from the Republic of Korea, covering... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limits for the Preliminary Results of...

  13. 75 FR 25841 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2010-05-10

    ... antidumping duty order on corrosion-resistant carbon steel flat products from the Republic of Korea, covering... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limits for the Preliminary Results of...

  14. 77 FR 27438 - Certain Corrosion-Resistant Carbon Steel Flat Products From Korea: Final Results of Expedited...

    Science.gov (United States)

    2012-05-10

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Certain Corrosion-Resistant... order on certain corrosion-resistant carbon steel flat products (``CORE'') from the Republic of Korea.... Scope of the Order The merchandise covered by the order includes flat-rolled carbon steel products, of...

  15. Sulphide production and corrosion in seawaters during exposure to FAME diesel.

    Science.gov (United States)

    Lee, Jason S; Ray, Richard I; Little, Brenda J; Duncan, Kathleen E; Oldham, Athenia L; Davidova, Irene A; Suflita, Joseph M

    2012-01-01

    Experiments were designed to evaluate the corrosion-related consequences of storing/transporting fatty acid methyl ester (FAME) alternative diesel fuel in contact with natural seawater. Coastal Key West, FL (KW), and Persian Gulf (PG) seawaters, representing an oligotrophic and a more organic- and inorganic mineral-rich environment, respectively, were used in 60 day incubations with unprotected carbon steel. The original microflora of the two seawaters were similar with respect to major taxonomic groups but with markedly different species. After exposure to FAME diesel, the microflora of the waters changed substantially, with Clostridiales (Firmicutes) becoming dominant in both. Despite low numbers of sulphate-reducing bacteria in the original waters and after FAME diesel exposure, sulphide levels and corrosion increased markedly due to microbial sulphide production. Corrosion morphology was in the form of isolated pits surrounded by an intact, passive surface with the deepest pits associated with the fuel/seawater interface in the KW exposure. In the presence of FAME diesel, the highest corrosion rates measured by linear polarization occurred in the KW exposure correlating with significantly higher concentrations of sulphur and chlorine (presumed sulphide and chloride, respectively) in the corrosion products.

  16. Positive aspects issued from bio corrosion studies: from hydrogen production to biofuel cells

    International Nuclear Information System (INIS)

    Silva Munoz, L. de

    2007-12-01

    Microbially influenced corrosion or bio corrosion is a problem that generates heavy global economic losses (several billion euros per year). In spite of the progress made on the understanding of the underlying mechanisms, the complexity of the phenomenon has prevented finding definitive solutions to the problem and continues to inspire many research works. The participation in bio corrosion of catalytic mechanisms induced by weak acids was studied in this work. Another objective of the thesis has been to take advantage from catalytic phenomena found in bio corrosion research to apply them in other areas: energy production with biofuel cells or electrochemical hydrogen production in mild conditions. This work has shown that the presence of weak acids and amino acids inside bio-films could play a major role in steel bio corrosion accelerating the phenomenon through the catalysis of the water reduction reaction. The reversibility of this mechanism, discerned and proved here, could explain the corrosion increase when hydrogen is removed (bacterial consumption, agitation...). In addition, phosphates allow the production of hydrogen by electrolysis in mild pH conditions (pH 4.0 - 8.0) with an equal or better performance than those found in alkaline electrolysis. Finally, industrial materials like stainless steel and titanium could be used in the fabrication of enzymatic electrodes for biosensors or microsystems. The use of the glucose oxidase/glucose system in an aqueous fuel cell with a stainless steel cathode, allows the improvement of the cell performance thanks to the production of hydrogen peroxide that is easily reduced. Moreover, the use of materials with micro-structured surfaces like sandblasted steels deserve to be studied in detail to exploit the remarkable reactivity they present compared to smooth electrodes. (author)

  17. Positive aspects issued from bio-corrosion studies: from hydrogen production to biofuel cells

    International Nuclear Information System (INIS)

    De Silva Munoz, Leonardo

    2007-01-01

    Microbially influenced corrosion or bio-corrosion is a problem that generates heavy global economic losses (several billion euros per year). In spite of the progress made on the understanding of the underlying mechanisms, the complexity of the phenomenon has prevented finding definitive solutions to the problem and continues to inspire many research works. The participation in bio-corrosion of catalytic mechanisms induced by weak acids was studied in this work. Another objective of the thesis has been to take advantage from catalytic phenomena found in bio corrosion research to apply them in other areas: energy production with biofuel cells or electrochemical hydrogen production in mild conditions. This work has shown that the presence of weak acids and amino acids inside bio films could play a major role in steel bio-corrosion accelerating the phenomenon through the catalysis of the water reduction reaction. The reversibility of this mechanism, discerned and proved here, could explain the corrosion increase when hydrogen is removed (bacterial consumption, agitation...). In addition, phosphates allow the production of hydrogen by electrolysis in mild ph conditions (pH 4.0 - 8.0) with an equal or better performance than those found in alkaline electrolysis. Finally, industrial materials like stainless steel and titanium could be used in the fabrication of enzymatic electrodes for biosensors or microsystems. The use of the glucose oxidase / glucose system in an aqueous fuel cell with a stainless steel cathode, allows the improvement of the cell performance thanks to the production of hydrogen peroxide that is easily reduced. Moreover, the use of materials with micro-structured surfaces like sandblasted steels deserve to be studied in detail to exploit the remarkable reactivity they present compared to smooth electrodes. (author) [fr

  18. High temperature corrosion in the thermochemical hydrogen production from nuclear heat

    International Nuclear Information System (INIS)

    Coen-Porisini, F.; Imarisio, G.

    1976-01-01

    In the production of hydrogen by water decomposition utilizing nuclear heat, a multistep process has to be employed. Water and the intermediate chemical products reach in chemical cycles giving hydrogen and oxygen with regeneration of the primary products used. Three cycles are examined, characterized by the presence of halide compounds and particularly hydracids at temperatures up to 800 0 C. Corrosion tests were carried out in hydrobromic acid, hydrochloric acid, ferric chloride solutions, and hydriodic acid

  19. Solubility classification of airborne products from uranium ores and tailings piles

    International Nuclear Information System (INIS)

    Kalkwarf, D.R.

    1979-01-01

    Airborne products generated at uranium mills were assigned solubility classifications for use in the ICRP Task Group Lung Model. No significant difference was seen between the dissolution behavior of airborne samples and sieved ground samples of the same product. If the product contained radionuclides that dissolved at different rates, composite classifications were assigned to show the solubility class of each component. If the dissolution data indicated that a radionuclide was present in two chemical forms that dissolved at different rates, a mixed classification was assigned to show the percentage of radionuclide in each solubility class. Uranium-ore dust was assigned the composite classification: ( 235 U, 238 U) W; ( 226 Ra) 10% D, 90% Y; ( 230 Th, 210 Pb, 210 Po) Y. Tailings-pile dust was classified: ( 226 Ra) 10% D, 90% Y; ( 230 Th, 210 Pb, 210 Po) Y. Uranium octoxide was classified Y, uranium tetrafluoride was also classified Y, ammonium diuranate was classified D, and yellow-cake dust was classified ( 235 U, 238 U) 60% D, 40% W. The term yellow cake, however, covers a variety of materials which differ significantly in dissolution rate. Solubility classifications based on the dissolution half-times of particular yellow-cake products should, thus, be used when available. The D, W, and Y classifications refer to biological half-times for clearance from the human respiratory tract of 0 to 10 days, 11 to 100 days, and > 100 days, respectively

  20. Corrosion/95 conference papers

    International Nuclear Information System (INIS)

    Anon.

    1995-01-01

    The papers in this conference represent the latest technological advances in corrosion control and prevention. The following subject areas are covered: cathodic protection in natural waters; materials for fossil fuel combustion and conversion systems; modern problems in atmospheric corrosion; innovative ideas for controlling the decaying infrastructure; deposits and their effects on corrosion in industry; volatile high temperature and non aqueous corrosion inhibitors; corrosion of light-weight and precoated metals for automotive application; refining industry corrosion; corrosion in pulp and paper industry; arctic/cold weather corrosion; materials selection for waste incinerators and associated equipment; corrosion measurement technology; environmental cracking of materials; advancing technology in the coating industry; corrosion in gas treating; green inhibition; recent advances in corrosion control of rail equipment; velocity effects and erosion corrosion in oil and gas production; marine corrosion; corrosion of materials in nuclear systems; underground corrosion control; corrosion in potable and industrial water systems in buildings and its impact on environmental compliance; deposit related boiler tube failures; boiler systems monitoring and control; recent developments and experiences in reactive metals; microbiologically influenced corrosion; corrosion and corrosion control for steel reinforced concrete; international symposium on the use of 12 and 13 Cr stainless steels in oil and gas production environments; subsea corrosion /erosion monitoring in production facilities; fiberglass reinforced pipe and tubulars in oilfield service; corrosion control technology in power transmission and distribution; mechanisms and methods of scale and deposit control; closing the loop -- results oriented cooling system monitoring and control; and minimization of aqueous discharge

  1. PRODUCTION OF POROUS POWDER MATERIALS OF SPHERICAL POWDERS OF CORROSION-RESISTANT STEEL

    Directory of Open Access Journals (Sweden)

    V. N. Kovalevskij

    2012-01-01

    Full Text Available Production of porous powder materials from spherical powders of corrosion-resistant steel 12Х18н10Т with formation at low pressures 120–140 mpa in the mold with the subsequent activated sintering became possible due to increase of duration of process of spattering and formation of condensate particles (Si–C or (Mo–Si on surface.

  2. Siderite as a Corrosion Product on Archaeological Iron from a Waterlogged Environment

    DEFF Research Database (Denmark)

    Matthiesen, H.; Hilbert, Lisbeth Rischel; Gregory, D.J.

    2003-01-01

    This paper discusses the occurrence of siderite (FeCO3) on iron artifacts excavated from the waterlogged peat and gyttja sediment of the Danish Iron Age site Nydam Mose. Siderite was identified by means of X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR) and scanning electron...... microscopy with energy-dispersive spectrometry (SEM-EDS), which showed only minor contents of other minerals in the corrosion scales. The implications of the formation of siderite as a corrosion product are discussed in terms of its possible passivating properties and thermodynamic stability in situ...

  3. Study of the formation and transport of corrosion products in PWR primary circuit simulators

    International Nuclear Information System (INIS)

    Noe, M.; Frejaville, G.; Camp, J.J.

    1983-01-01

    The formation, migration and deposition of corrosion products in PWR primary circuits are studied in out-of-reactor loops. The aim of these studies is to limit the build-up of the radiation fields impinging on out-of-flux walls and to reduce the danger of rapid corrosion of fuel cans, taking into account the tougher conditions imposed on current trends in the operation of such industrial plants. Four simulator loops and their respective possibilities and research methods are described. (author)

  4. Analysis of chemical concepts as the basic of virtual laboratory development and process science skills in solubility and solubility product subject

    Science.gov (United States)

    Syafrina, R.; Rohman, I.; Yuliani, G.

    2018-05-01

    This study aims to analyze the concept characteristics of solubility and solubility products that will serve as the basis for the development of virtual laboratory and students' science process skills. Characteristics of the analyzed concepts include concept definitions, concept attributes, and types of concepts. The concept analysis method uses concept analysis according to Herron. The results of the concept analysis show that there are twelve chemical concepts that become the prerequisite concept before studying the solubility and solubility and five core concepts that students must understand in the solubility and Solubility product. As many as 58.3% of the definitions of the concepts contained in high school textbooks support students' science process skills, the rest of the definition of the concept is memorized. Concept attributes that meet three levels of chemical representation and can be poured into a virtual laboratory have a percentage of 66.6%. Type of concept, 83.3% is a concept based on principle; and 16.6% concepts that state the process. Meanwhile, the science process skills that can be developed based on concept analysis are the ability to observe, calculate, measure, predict, interpret, hypothesize, apply, classify, and inference.

  5. Semiquantitative analysis of corrosion products in iron channel by the X-ray diffraction technique

    International Nuclear Information System (INIS)

    Bueno, C.R.E.; Varela, J.A.

    1995-01-01

    The corrosion in the us very important in the slag line region, but in others regions over and above this line there is a corrosion process still important. We have made a detailed mapping of phases present in seven different regions in the iron channel in three distinct positions. After the phases identifications, it was made a deconvolution of the diffractograms using Gaussian functions. The analysis of the relative intensity of each phase gave an idea for a semi-quantitative analysis and we have proposed a mechanism of the refractory corrosion. It was observed that the calcium oxide migrates by diffusion to different regions originating low melting point products like pseudo-wolastonite, anorthite and guelenite. (author)

  6. Radioactive corrosion products in circuit of fast reactor loop with dissociating coolant

    International Nuclear Information System (INIS)

    Dolgov, V.M.; Katanaev, A.O.

    1982-01-01

    The results of experimental investigation into depositions of radionuclides of corrosion origin on the surfaces of a reactor-in-pile loop facility with a dissociating coolant are presented. It is stated that the ratio of radionuclides in fixed depositions linearly decreases with decrease of the coolant temperature at the core-condenser section. The element composition of non-fixed compositions quantitatively and qualitatively differs from the composition of structural material, and it is more vividly displayed for the core-condenser section. The main mechanism of circuit contamination with radioactive corrosion products is substantiated: material corrosion in the zones of coolant phase transfer, their remove by the coolant in the core, deposition, activation and wash-out by the coolant from the core surfaces

  7. Kinetics of radiolysis of irradiated ligno celluloses into soluble products in water and rumen liquid

    International Nuclear Information System (INIS)

    Tukenmez, I.; Bakioglu, A.T.; Ersen, M.S.

    1997-01-01

    In order to increase the low bio hydrolysis of ligno celluloses in biotechnological and biological processes where these materials are used as raw materials and ruminant feed, the substrates were pretreated with irradiation to induce radiolytic depolymerisation and then kinetics of their radiolysis into soluble products in water and rumen liquid were analyzed. Wheat straw used as a representative lignocellulose substrate was irradiated at 0-2.5 MGy doses at 20''o''C with an optimum equilibrium humidity of 6.6% in Cs-137 gamma irradiator with a dose rate of 1.8 kGy/h, and soluablefractions in water and in situ rumen liquid were determined gravimetrically. Based on these data, a reaction mechanism was proposed for the radiolysis of ligno celluloses into soluble fractions. From the corresponding reaction rate equations with this mechanism a dose dependent kinetics was derived for the radiolysis of ligno celluloses into water/rumen liquid-soluble products. Defined by this kinetics, the threshold doses for the radiolysis of the substrate into water/rumen liquid-soluble products were respectively found 80.6 kGy and 186.0 kGy, and fractional radiolytic decomposition yields 0.193 MGy''-1''.It was emphasized that developed kinetic models may be used for the process design of irradiation pretreatments to improve the bio hydrolysis of ligno celluloses.(2figs. and 17 refs.)

  8. Refuse derived soluble bio-organics enhancing tomato plant growth and productivity

    Energy Technology Data Exchange (ETDEWEB)

    Sortino, Orazio [Dipartimento di Scienze Agronomiche Agrochimiche e delle Produzioni Animali, Universita degli Studi di Catania, Via Valdisavoia 5, 95123 Catania (Italy); Dipasquale, Mauro [Dipartimento di Chimica, Universita di Torino, Via P. Giuria 7, 10125 Torino (Italy); Montoneri, Enzo, E-mail: enzo.montoneri@unito.it [Dipartimento di Chimica, Universita di Torino, Via P. Giuria 7, 10125 Torino (Italy); Tomasso, Lorenzo; Perrone, Daniele G. [Dipartimento di Chimica, Universita di Torino, Via P. Giuria 7, 10125 Torino (Italy); Vindrola, Daniela; Negre, Michele; Piccone, Giuseppe [Dipartimento di Valorizzazione e Protezione delle Risorse Agroforestali, Universita di Torino, Via L. da Vinci 44, 10095 Grugliasco (Italy)

    2012-10-15

    Highlights: Black-Right-Pointing-Pointer Municipal bio-wastes are a sustainable source of bio-based products. Black-Right-Pointing-Pointer Refuse derived soluble bio-organics promote chlorophyll synthesis. Black-Right-Pointing-Pointer Refuse derived soluble bio-organics enhance plant growth and fruit ripening rate. Black-Right-Pointing-Pointer Sustainable chemistry exploiting urban refuse allows sustainable development. Black-Right-Pointing-Pointer Chemistry, agriculture and the environment benefit from biowaste technology. - Abstract: Municipal bio-refuse (CVD), containing kitchen wastes, home gardening residues and public park trimmings, was treated with alkali to yield a soluble bio-organic fraction (SBO) and an insoluble residue. These materials were characterized using elemental analysis, potentiometric titration, and 13C NMR spectroscopy, and then applied as organic fertilizers to soil for tomato greenhouse cultivation. Their performance was compared with a commercial product obtained from animal residues. Plant growth, fruit yield and quality, and soil and leaf chemical composition were the selected performance indicators. The SBO exhibited the best performance by enhancing leaf chlorophyll content, improving plant growth and fruit ripening rate and yield. No product performance-chemical composition relationship could be assessed. Solubility could be one reason for the superior performance of SBO as a tomato growth promoter. The enhancement of leaf chlorophyll content is discussed to identify a possible link with the SBO photosensitizing properties that have been demonstrated in other work, and thus with photosynthetic performance.

  9. Nanocrystals of medium soluble actives--novel concept for improved dermal delivery and production strategy.

    Science.gov (United States)

    Zhai, Xuezhen; Lademann, Jürgen; Keck, Cornelia M; Müller, Rainer H

    2014-08-15

    After use in oral pharmaceutical products, nanocrystals are meanwhile applied to improve the dermal penetration of cosmetic actives (e.g. rutin, hesperidin) and of drugs. By now, nanocrystals are only dermally applied made from poorly soluble actives. The novel concept is to formulate nanocrystals also from medium soluble actives, and to apply a dermal formulation containing additionally nanocrystals. The nanocrystals should act as fast dissolving depot, increase saturation solubility and especially accumulate in the hair follicles, to further increase skin penetration. Caffeine was used as model compound with relevance to market products, and a particular process was developed for the production of caffeine nanocrystals to overcome the supersaturation related effect of crystal growth and fiber formation - typical with medium soluble compounds. It is based on low energy milling (pearl milling) in combination with low dielectric constant dispersion media (water-ethanol or ethanol-propylene glycol mixtures) and optimal stabilizers. Most successful was Carbopol(®) 981 (e.g. 20% caffeine in ethanol-propylene glycol 3:7 with 2% Carbopol, w/w). Nanocrystals with varied sizes can now be produced in a controlled process e.g. 660 nm (optimal for hair follicle accumulation) to 250 nm (optimal for fast dissolution). The short term test proved stability over 2 months of the present formulation being sufficient to perform in vivo testing of the novel concept. Copyright © 2014 Elsevier B.V. All rights reserved.

  10. Refuse derived soluble bio-organics enhancing tomato plant growth and productivity

    International Nuclear Information System (INIS)

    Sortino, Orazio; Dipasquale, Mauro; Montoneri, Enzo; Tomasso, Lorenzo; Perrone, Daniele G.; Vindrola, Daniela; Negre, Michele; Piccone, Giuseppe

    2012-01-01

    Highlights: ► Municipal bio-wastes are a sustainable source of bio-based products. ► Refuse derived soluble bio-organics promote chlorophyll synthesis. ► Refuse derived soluble bio-organics enhance plant growth and fruit ripening rate. ► Sustainable chemistry exploiting urban refuse allows sustainable development. ► Chemistry, agriculture and the environment benefit from biowaste technology. - Abstract: Municipal bio-refuse (CVD), containing kitchen wastes, home gardening residues and public park trimmings, was treated with alkali to yield a soluble bio-organic fraction (SBO) and an insoluble residue. These materials were characterized using elemental analysis, potentiometric titration, and 13C NMR spectroscopy, and then applied as organic fertilizers to soil for tomato greenhouse cultivation. Their performance was compared with a commercial product obtained from animal residues. Plant growth, fruit yield and quality, and soil and leaf chemical composition were the selected performance indicators. The SBO exhibited the best performance by enhancing leaf chlorophyll content, improving plant growth and fruit ripening rate and yield. No product performance-chemical composition relationship could be assessed. Solubility could be one reason for the superior performance of SBO as a tomato growth promoter. The enhancement of leaf chlorophyll content is discussed to identify a possible link with the SBO photosensitizing properties that have been demonstrated in other work, and thus with photosynthetic performance.

  11. Characterization of corrosion products of Zn and Zn–Mg–Al coated steel in a marine atmosphere

    International Nuclear Information System (INIS)

    Diler, E.; Rouvellou, B.; Rioual, S.; Lescop, B.; Nguyen Vien, G.; Thierry, D.

    2014-01-01

    Highlights: • The corrosion behaviour of Zn–Mg–Al alloy in marine environment is characterized. • Zn–Mg–Al alloy shows a better corrosion resistance than Zn. • Strong enhancement of NaZn 4 Cl(OH) 6 SO 4 ·6H 2 O in the corrosion products is observed. • Al 3+ and Mg 2+ induced quenching effects in corrosion activity are described. - Abstract: The corrosion behaviour of pure zinc and zinc–magnesium–aluminium alloy (ZMA) has been studied during 6 months of exposure in marine environment (Brest, France). The composition of corrosion products is analysed using infrared spectroscopy (FTIR), X-ray diffraction (XRD), and X-ray photoelectron spectroscopy (XPS). An improved corrosion resistance of ZMA is observed. This improvement is found to be connected to Mg 2+ and Al 3+ induced quenching of corrosion activity and to the enhancement of NaZn 4 Cl(OH) 6 SO 4 ·6H 2 O in the formed corrosion product

  12. Brief description of out-of-pile test facilities for study in corrosion and fission product behaviour in flowing sodium

    International Nuclear Information System (INIS)

    Iizawa, K.; Sekiguchi, N.; Atsumo, H.

    1976-01-01

    The experimental methods to perform tests for study in corrosion and fission products behaviour in flowing sodium are outlined. Flow diagrams for the activated materials and fission products behaviour test loop are given

  13. Extractive biotransformation for production of metabolites of poorly soluble compounds: synthesis of 32-hydroxy-rifalazil.

    Science.gov (United States)

    Mozhaev, Vadim V; Mozhaeva, Lyudmila V; Michels, Peter C; Khmelnitsky, Yuri L

    2008-10-01

    A novel reaction system was developed for the production of metabolites of poorly water-soluble parent compounds using mammalian liver microsomes. The system includes the selection and use of an appropriate hydrophobic polymeric resin as a reservoir for the hydrophobic parent compounds and its metabolites. The utility of the extractive biotransformation approach was shown for the production of a low-yielding, synthetically challenging 32-hydroxylated metabolite of the antibiotic rifalazil using mouse liver microsomes. To address the low solubility and reactivity of rifalazil in the predominantly aqueous microsomal catalytic system, a variety of strategies were tested for the enhanced delivery of hydrophobic substrates, including the addition of mild detergents, polyvinylpyrrolidone, glycerol, bovine serum albumin, and hydrophobic polymeric resins. The latter strategy was identified as the most suitable for the production of 32-hydroxy-rifalazil, resulting in up to 13-fold enhancement of the volumetric productivity compared with the standard aqueous system operating at the solubility limit of rifalazil. The production process was optimized for a wide range of reaction parameters; the most important for improving volumetric productivity included the type and amount of the polymeric resin, cofactor recycling system, concentrations of the biocatalyst and rifalazil, reaction temperature, and agitation rate. The optimized extractive biotransformation system was used to synthesize 32-hydroxy-rifalazil on a multimilligram scale.

  14. Complementary Methods for the Characterization of Corrosion Products on a Plant-Exposed Superheater Tube

    DEFF Research Database (Denmark)

    Okoro, Sunday Chukwudi; Nießen, Frank; Villa, Matteo

    2017-01-01

    In this work, complex corrosion products on a superheater tube exposed to biomass firing were characterized by the complementary use of energy-dispersive synchrotron diffraction, electron microscopy, and energy-dispersive X-ray spectroscopy. Non-destructive synchrotron diffraction in transmission......-rich austenite phase to selective removal of Fe and Cr from the alloy, via a KCl-induced corrosion mechanism. Compositional variations were related to diffraction results and revealed a qualitative influence of the spinel cation concentration on the observed diffraction lines.......In this work, complex corrosion products on a superheater tube exposed to biomass firing were characterized by the complementary use of energy-dispersive synchrotron diffraction, electron microscopy, and energy-dispersive X-ray spectroscopy. Non-destructive synchrotron diffraction in transmission...... geometry measuring with a small gauge volume from the sample surface through the corrosion product allowed depth-resolved phase identification and revealed the presence of (Fe,Cr)2O3 and FeCr2O4. This was supplemented by microstructural and elemental analysis correlating the additional presence of a Ni...

  15. Corrosion products, activity transport and deposition in boiling water reactor recirculation systems

    International Nuclear Information System (INIS)

    Alder, H.P.; Buckley, D.; Grauer, R.; Wiedemann, K.H.

    1989-09-01

    The deposition of activated corrosion products in the recirculation loops of Boiling Water Reactors produces increased radiation levels which lead to a corresponding increase in personnel radiation dose during shut down and maintenance. The major part of this dose rate is due to cobalt-60. The following areas are discussed in detail: - the origins of the corrosion products and of cobalt-59 in the reactor feedwaters, - the consolidation of the cobalt in the fuel pin deposits (activation), - the release and transport of cobalt-60, - the build-up of cobalt-60 in the corrosion products in the recirculation loops. Existing models of the build-up of circuit radioactivity are discussed and the operating experiences from selected reactors are summarised. Corrosion chemistry aspects of the cobalt build-up in the primary circuit have already been studied on a broad basis and are continuing to be researched in a number of centers. The crystal chemistry of chromium-nickel steel corrosion products poses a number of yet unanswered questions. There are major loopholes associated with the understanding of activation processes of cobalt deposited on the fuel pins and in the mass transfer of cobalt-60. For these processes, the most important influence stems from factors associated with colloid chemistry. Accumulation of data from different BWRs contributes little to the understanding of the activity build-up. However, there are examples that the problem of activity build-up can be kept under control. Although many details for a quantitative understanding are still missing, the most important correlations are visible. The activity build-up in the BWR recirculation systems cannot be kept low by a single measure. Rather a whole series of measures is necessary, which influences not only cobalt-60 deposition but also plant and operation costs. (author) 26 figs., 13 tabs., 90 refs

  16. Catalysis of copper corrosion products on chlorine decay and HAA formation in simulated distribution systems.

    Science.gov (United States)

    Zhang, Hong; Andrews, Susan A

    2012-05-15

    This study investigated the effect of copper corrosion products, including Cu(II), Cu(2)O, CuO and Cu(2)(OH)(2)CO(3), on chlorine degradation, HAA formation, and HAA speciation under controlled experimental conditions. Chlorine decay and HAA formation were significantly enhanced in the presence of copper with the extent of copper catalysis being affected by the solution pH and the concentration of copper corrosion products. Accelerated chlorine decay and increased HAA formation were observed at pH 8.6 in the presence of 1.0 mg/L Cu(II) compared with that observed at pH 6.6 and pH 7.6. Further investigation of chlorine decay in the presence of both Suwannee River NOM and Cu(II) indicated that an increased reactivity of NOM with dissolved and/or solid surface-associated Cu(II), rather than chlorine auto-decomposition, was a primary reason for the observed rapid chlorine decay. Copper corrosion solids [Cu(2)O, CuO, Cu(2)(OH)(2)CO(3)] exhibited catalytic effects on both chlorine decay and HAA formation. Contrary to the results observed when in the absence of copper corrosion products, DCAA formation was consistently predominant over other HAA species in the presence of copper corrosion products, especially at neutral and high pH. This study improves the understanding for water utilities and households regarding chlorine residuals and HAA concentrations in distribution systems, in particular once the water reaches domestic plumbing where copper is widely used. Copyright © 2012 Elsevier Ltd. All rights reserved.

  17. 75 FR 55769 - Certain Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of...

    Science.gov (United States)

    2010-09-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant...) is conducting the sixteenth administrative review of the antidumping order on corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea (Korea).\\1\\ This review covers eight...

  18. 78 FR 59652 - Certain Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of...

    Science.gov (United States)

    2013-09-27

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant... corrosion-resistant carbon steel flat products (``CORE'') from the Republic of Korea (``Korea''), pursuant... administrative review of the antidumping duty order on CORE from Korea covering the period of review (``POR'') of...

  19. 78 FR 55057 - Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Preliminary Results of...

    Science.gov (United States)

    2013-09-09

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon... Department) is conducting an administrative review of the antidumping duty order on corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea (Korea), covering the period [[Page 55058...

  20. 78 FR 16247 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea; Final Results of...

    Science.gov (United States)

    2013-03-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon... preliminary results of the administrative review of the antidumping duty order on corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea (Korea).\\1\\ This review covers seven manufacturers...

  1. 76 FR 69703 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of Extension of...

    Science.gov (United States)

    2011-11-09

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon... administrative review of the antidumping duty order on corrosion-resistant carbon steel flat products from Korea, covering the period August 1, 2009, to July 31, 2010. See Initiation of Antidumping and Countervailing Duty...

  2. 77 FR 14501 - Certain Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of...

    Science.gov (United States)

    2012-03-12

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant... the preliminary results of the antidumping duty administrative review for certain corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea (Korea).\\1\\ This review covers eight...

  3. 76 FR 77775 - Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2011-12-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon... results of the administrative review of the countervailing duty order on corrosion-resistant carbon steel flat products from the Republic of Korea covering the period January 1, 2009, through December 31, 2009...

  4. 77 FR 54891 - Certain Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Preliminary...

    Science.gov (United States)

    2012-09-06

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant...) is conducting the 18th administrative review of the antidumping order on corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea \\1\\ (Korea). This review covers seven...

  5. 76 FR 4291 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Partial Rescission of...

    Science.gov (United States)

    2011-01-25

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon... Commerce (the Department) initiated an administrative review of the countervailing duty order on corrosion- resistant carbon steel flat products from the Republic of Korea covering the period January 1, 2009, through...

  6. 78 FR 59651 - Certain Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of...

    Science.gov (United States)

    2013-09-27

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant... duty order on certain corrosion-resistant carbon steel flat products (``CORE'') from the Republic of... covering the period of review (``POR'') of August 1, 2006 through July 31, 2007, with respect to the...

  7. 76 FR 55004 - Certain Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Preliminary...

    Science.gov (United States)

    2011-09-06

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant...) is conducting the seventeenth administrative review of the antidumping order on corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea \\1\\ (Korea). This review covers eight...

  8. 75 FR 77615 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of Extension of...

    Science.gov (United States)

    2010-12-13

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon... administrative review of the antidumping duty order on corrosion-resistant carbon steel flat products from Korea, covering the period August 1, 2008, to July 31, 2009. See Initiation of Antidumping and Countervailing Duty...

  9. The external beam facility used to characterize corrosion products in metallic statuettes

    International Nuclear Information System (INIS)

    Rizzutto, M.A.; Tabacniks, M.H.; Added, N.; Barbosa, M.D.L.; Curado, J.F.; Santos, W.A.; Lima, S.C.; Melo, H.G.; Neiva, A.C.

    2005-01-01

    To open new possibilities in nuclear applied physics research, mainly for the analysis of art objects in air, an external beam facility was installed at LAMFI (Laboratorio de Analise de Materiais por Feixes Ionicos) of University of Sao Paulo. PIXE measurements were made using an XR-100CR (Si-PIN) X-ray detector pointed to the sample mounted after an approximate 11 mm air path, hence with effective beam energy of 0.9 MeV. This setup was used to characterize the corrosion products of two ethnological metallic statuettes from the African collection of the Museum of Archaeology and Etnology. PIXE analysis of the corrosion free base of one statuette showed that Cu and Zn are the main components of the alloy, while Pb is present in smaller amount. The analysis of some corrosion products showed a Zn:Cu relationship higher than that of the base, evidencing selective corrosion. The main components of the other statuette were Cu and Pb, while S and Zn were found in smaller amounts

  10. A family of E. coli expression vectors for laboratory scale and high throughput soluble protein production

    Directory of Open Access Journals (Sweden)

    Bottomley Stephen P

    2006-03-01

    Full Text Available Abstract Background In the past few years, both automated and manual high-throughput protein expression and purification has become an accessible means to rapidly screen and produce soluble proteins for structural and functional studies. However, many of the commercial vectors encoding different solubility tags require different cloning and purification steps for each vector, considerably slowing down expression screening. We have developed a set of E. coli expression vectors with different solubility tags that allow for parallel cloning from a single PCR product and can be purified using the same protocol. Results The set of E. coli expression vectors, encode for either a hexa-histidine tag or the three most commonly used solubility tags (GST, MBP, NusA and all with an N-terminal hexa-histidine sequence. The result is two-fold: the His-tag facilitates purification by immobilised metal affinity chromatography, whilst the fusion domains act primarily as solubility aids during expression, in addition to providing an optional purification step. We have also incorporated a TEV recognition sequence following the solubility tag domain, which allows for highly specific cleavage (using TEV protease of the fusion protein to yield native protein. These vectors are also designed for ligation-independent cloning and they possess a high-level expressing T7 promoter, which is suitable for auto-induction. To validate our vector system, we have cloned four different genes and also one gene into all four vectors and used small-scale expression and purification techniques. We demonstrate that the vectors are capable of high levels of expression and that efficient screening of new proteins can be readily achieved at the laboratory level. Conclusion The result is a set of four rationally designed vectors, which can be used for streamlined cloning, expression and purification of target proteins in the laboratory and have the potential for being adaptable to a high

  11. REACTION PRODUCTS AND CORROSION OF MOLYBDENUM ELECTRODE IN GLASS MELT CONTAINING ANTIMONY OXIDES AND SODIUM SULFATE

    Directory of Open Access Journals (Sweden)

    JIŘÍ MATĚJ

    2012-09-01

    Full Text Available The products on the interface of a molybdenum electrode and glass melt were investigated primarily at 1400°C in three model glass melts without ingredients, with 1 % Sb2O3 and with 1 % Sb2O3 and 0.5 % SO3 (wt. %, both under and without load by alternating current. Corrosion of the molybdenum electrode in glass melt without AC load is higher by one order of magnitude if antimony oxides are present. The corrosion continues to increase if sulfate is present in addition to antimony oxides. Isolated antimony droplets largely occur on the electrode-glass melt interface, and numerous droplets are also dissipated in the surrounding glass if only antimony oxides are present in the glass melt. A comparatively continuous layer of antimony occurs on the interface if SO3 is also present, antimony being always in contact with molybdenum sulfide. Almost no antimony droplets are dissipated in the glass melt. The total amount of precipitated antimony also increases. The presence of sulfide on the interface likely facilitates antimony precipitation. The reaction of molybdenum with antimony oxides is inhibited in sites covered by an antimony layer. The composition of sulfide layers formed at 1400°C approximates that of Mo2S3. At 1100°C, the sulfide composition approximates that of MoS4. Corrosion multiplies in the glass melt without additions through the effect of AC current, most molybdenum being separated in the form of metallic particles. Corrosion also increases in the glass melt containing antimony oxides. This is due to increased corrosion in the neighborhood of the separated antimony droplets. This mechanism also results in the loosening of molybdenum particles. The amount of precipitated antimony also increases through the effect of the AC current. AC exerts no appreciable effect on either corrosion, the character of the electrode-glass interface, or antimony precipitation in the glass melt containing SO3.

  12. Solubility product of tetravalent neptunium hydrous oxide and its ionic strength dependence

    Energy Technology Data Exchange (ETDEWEB)

    Fujiwara, K.; Mori, T. [Japan Nuclear Cycle Development Institute (JNC), 4-33, Muramatsu, Tokai-mura, Naka-gun, Ibaraki-ken, 319-1194 (Japan); Kohara, Y. [Inspection and Development Company, 4-33, Muramatsu, Tokaimura, Naka-gun, Ibaraki-ken, 319-1112 (Japan)

    2005-07-01

    Full text of publication follows: Solubility products (K{sub sp}) are key parameters in the context of reliable assessment of actinides migration in the repository conditions of high level radioactive waste. Neptunium (Np(IV)) is one of the most important actinide elements in the assessment, because of its inventory and the long half-life. A few previous data for Np(IV) solubility are varied widely due to experimental difficulties related to the extremely low solubility. We carried out batch-type experiments under nitrogen atmosphere using a glovebox. Np(V) was reduced to Np(III) by bubbling 0.5 ppm H{sub 2} / N{sub 2} gas through the solution for 30 days in the presence of platinum black as catalyst. After reducing treatment, the Np(III) converted to Np(IV) by auto-oxidation within approximately three days. The solubilities of the Np(IV) were measured in the pHc ranging from 2 to 4, at room temperature (23 {+-} 2 deg. C), in ionic strength(I) = 0.1, 0.5, 1.0 and 2.0 M NaClO{sub 4}. The equilibrium condition was confirmed by over-saturation and under-saturation method. After the equilibrium, the pH{sub c} and the E{sub h} value of the suspension were measured. The suspension was then filtered using a filter with a NMWL of 3000 (less than 2 nm{phi}). The Np radio activity in the filtrate was determined by alpha spectrometry and absorption spectra of Np(IV). The solubility decreased with increasing pHc and the hydrolysis species are predominantly formed. From the obtained results, the solubility products (K{sub sp}) of Np hydroxide, for the reaction, NpO{sub 2} . xH{sub 2}O {r_reversible} Np{sup 4+} + 4OH{sup -} + (x-2)H{sub 2}O, at I = 0.1, 0.5, 1.0 and 2.0 were determined by using formation constants ({beta}{sub n}(I)), which were determined for the reaction, Np{sup 4+} + nOH{sup -} {r_reversible} Np(OH){sub n}{sup (4-n)+}. By using the specific interaction theory (SIT), the solubility product of tetravalent Np hydrous oxide is calculated to be log K{sub sp}{sup 0

  13. Release of corrosion products from construction materials containing cobalt. Pt.2: Inconel X750

    International Nuclear Information System (INIS)

    Falk, I.

    1978-02-01

    This report describes experimental work aimed at determining the release rate for corrosion products from 18Cr8Ni steel and Inconel X750 in BWR environments. For test purposes these environments were simulated in a high pressure loop, where irradiated samples of the materials were exposed for 720 hours. The amounts of released products were determined using gamma spectrometric analysis. The results show that the release from Inconel X750 is higher than that from 18Cr8Ni steel. The release calculated from Co58 measurements is 7 times higher and from Co60 measurements it is 1.5 times higher. Both the filtered and the deposited fractions of the released corrosion products exhibit the same relative concentrations of Co58 and Co60. (author)

  14. The Moessbauer spectroscopy in the characterization of atmospheric corrosion products; La espectroscopia Moessbauer en la caracterizacion de productos de corrosion atmosferica

    Energy Technology Data Exchange (ETDEWEB)

    Hernandez Torres, D; Leiva Ronda, P [Centro de Estudios Aplicados al Desarrollo Nuclear (CEADEN), La Habana (Cuba); Gomez, J; Ronda, M [Centro de Investigaciones del Petroleo, La Habana (Cuba)

    1996-07-01

    A study of corrosion products on mild steel formed after 1 and 5 years exposure in two industrial coastal weathering stations in the Bay from Matanzas City, Cuba, has been carried out. Structural analysis was conducted using mainly transmission Moessbauer Spectroscopy and the X-ray diffraction as complementary technique. The main phases found in the specimen exposed to high chloride containing environment were: lepidocrocite ({gamma}- FeOOH), goethite ({alpha}- FeOOH) and magnetite concentration was the lowest, the phases found were {gamma}- FeOOH and {alpha}- FeOOH, and the phase transformation proposed was {gamma}- FeOOh -> {alpha}- Fe-OOH. In this station were found also amorphous corrosion products. There amorphous phases could be responsible for the lowest levels of corrosion on steel in this station.

  15. Mechanical properties of layers of corrosion products at steel / concrete interface

    International Nuclear Information System (INIS)

    Dehoux, Anita

    2012-01-01

    To take account of the development of corrosion products layers in residual lifetime calculations of reinforced concrete structures requires a good knowledge of the mechanical properties of these products. Our study aims to determine the mechanical properties of layers of corrosion products. The approach consists of an identification of the microstructure properties complemented by homogenization calculations to calculate a mesoscopic behavior in linear elasticity of layers of corrosion products. The study includes a series of experimental campaigns at the microscopic scale. Vickers micro indentation tests analyzed by a Gaussian mixture model approach allowed the acquisition of hardness and elastic moduli at the microscale. An identification of the microstructure products is performed by Raman microspectrometry. The microstructure's characterization brings valuable information for homogenization calculations. The first approach has consisted of calculations of random media homogenization by self-consistent and generalized self-consistent schemes. In the second approach, effective modulus calculations were performed using numerical microstructures resulting from 2D images taken with an optical microscope. The corpus is composed of samples of different ages and origins, their microstructures were compared. (author) [fr

  16. Changing oxidoreduction potential to improve water-soluble yellow pigment production with Monascus ruber CGMCC 10910.

    Science.gov (United States)

    Huang, Tao; Tan, Hailing; Lu, Fangju; Chen, Gong; Wu, Zhenqiang

    2017-11-21

    Monascus pigments are widely used in the food and pharmaceutical industries due to their safety to human health. Our previous study found that glucose concentration induced extracellular oxidoreduction potential (ORP) changes could influence extracellular water-soluble yellow pigment production by Monascus ruber CGMCC 10910 in submerged fermentation. In this study, H 2 O 2 and dithiothreitol (DTT) were used to change the oxidoreduction potential for investigating the effects of oxidative or reductive substances on Monascus yellow pigment production by Monascus ruber CGMCC 10910. The extracellular ORP could be controlled by H 2 O 2 and DTT. Both cell growth and extracellular water-soluble yellow pigment production were enhanced under H 2 O 2 -induced oxidative (HIO) conditions and were inhibited under dithiothreitol-induced reductive conditions. By optimizing the amount of H 2 O 2 added and the timing of the addition, the yield of extracellular water-soluble yellow pigments significantly increased and reached a maximum of 209 AU, when 10 mM H 2 O 2 was added on the 3rd day of fermentation with M. ruber CGMCC 10910. Under HIO conditions, the ratio of NADH/NAD+ was much lower than that in the control group, and the expression levels of relative pigment biosynthesis genes were up-regulated; moreover, the activity of glucose-6-phosphate dehydrogenase (G6PDH) was increased while 6-phosphofructokinase (PFK) activity was inhibited. Oxidative conditions induced by H 2 O 2 increased water-soluble yellow pigment accumulation via up-regulation of the expression levels of relative genes and by increasing the precursors of pigment biosynthesis through redirection of metabolic flux. In contrast, reductive conditions induced by dithiothreitol inhibited yellow pigment accumulation. This experiment provides a potential strategy for improving the production of Monascus yellow pigments.

  17. Fate of corrosion products released from stainless steel in marine sediments and seawater. Part 4: Hatteras abyssal red clay

    International Nuclear Information System (INIS)

    Schmidt, R.L.

    1982-07-01

    A study in which neutron-activated 347 stainless steel was exposed to surficial sediment from a site in the Hatteras Abyssal Plain of the Northwest Atlantic Ocean is described. This sediment consists of approx. 20% CaCO 3 , which could lead to the formation of calcareous scale on the metal surface and reduce the corrosion rate. The distribution of indigenous metals among different chemical fractions shows that extractable Cr, Mn, Fe, Co, and Zn were associated with amorphous Mn and Fe oxides. Most of the remaining extractable Cr, and about a third of the extractable Cu appear to have been weakly complexed. Major fractions (25 to 36%) of extractable Mn, Co and Ni were present as adsorbed cations. Organic complexation appears to account for a large amount of extractable Fe, Ni, Cu and Zn. Neutron-activated 347 stainless steel specimens were exposed to sediment slurry under aerobic and non-oxygenated conditions for a period of 94 days. The redox potential measurements for air-sparged and N 2 , CO 2 -sparged sediment slurries were +410 and +60 mv, respectively. The presence of 0 2 produced increased amounts of corrosion products. Chemical extraction showed that relatively labile substances constituted about 84% of the 60 Co activity released in aerated sediment. Relatively labile substances constitute about 82% of the total 60 Co activity released under non-oxygenated conditions. A large fraction of 60 Co which was in the soluble or easily dissolved forms under non-oxygenated conditions appears to have been more strongly adsorbed to the sediment under aerated conditions

  18. Fate of corrosion products released from stainless steel in marine sediments and seawater. Part 4: Hatteras abyssal red clay

    Energy Technology Data Exchange (ETDEWEB)

    Schmidt, R.L.

    1982-07-01

    A study in which neutron-activated 347 stainless steel was exposed to surficial sediment from a site in the Hatteras Abyssal Plain of the Northwest Atlantic Ocean is described. This sediment consists of approx. 20% CaCO/sub 3/, which could lead to the formation of calcareous scale on the metal surface and reduce the corrosion rate. The distribution of indigenous metals among different chemical fractions shows that extractable Cr, Mn, Fe, Co, and Zn were associated with amorphous Mn and Fe oxides. Most of the remaining extractable Cr, and about a third of the extractable Cu appear to have been weakly complexed. Major fractions (25 to 36%) of extractable Mn, Co and Ni were present as adsorbed cations. Organic complexation appears to account for a large amount of extractable Fe, Ni, Cu and Zn. Neutron-activated 347 stainless steel specimens were exposed to sediment slurry under aerobic and non-oxygenated conditions for a period of 94 days. The redox potential measurements for air-sparged and N/sub 2/, CO/sub 2/-sparged sediment slurries were +410 and +60 mv, respectively. The presence of 0/sub 2/ produced increased amounts of corrosion products. Chemical extraction showed that relatively labile substances constituted about 84% of the /sup 60/Co activity released in aerated sediment. Relatively labile substances constitute about 82% of the total /sup 60/Co activity released under non-oxygenated conditions. A large fraction of /sup 60/Co which was in the soluble or easily dissolved forms under non-oxygenated conditions appears to have been more strongly adsorbed to the sediment under aerated conditions.

  19. Major activated corrosion products cobalt, silver and antimony in the primary coolant of PWR power plants

    International Nuclear Information System (INIS)

    Xu Mingxia

    2012-01-01

    The production of the major activated corrosion products such as cobalt, silver and antimony in the primary coolant of PWR power plants and the impacts on the increase of the dose rates caused by these corrosion products during the shutdown are described in the paper. Investigating the corrosion product behavior during the operation and shutdown periods aims at detecting the appearance of these radiological pollutants in the early time and searching relevant solutions that may enable eventually to decrease the dose rate. The solutions may include: Replacing critical material in the primary system's equipment and components, which contact with primary coolant circuit to possibly limit the source term, Elaborating strictly the specific chemical and shutdown procedure to optimize the purification capacity and to minimize the over-contaminations; Improving purification techniques according to the real operation circumstance, and limiting the impacts of these pollutants. It is obvious in the real practices that implementing appropriate solution will be benefit to decrease or limit the pollutants species like cobalt, silver and antimony. (author)

  20. Simulation of corrosion product activity in pressurized water reactors under flow rate transients

    International Nuclear Information System (INIS)

    Mirza, Anwar M.; Mirza, Nasir M.; Mir, Imran

    1998-01-01

    Simulation of coolant activation due to corrosion products and impurities in a typical pressurized water reactor has been done under flow rate transients. Employing time dependent production and losses of corrosion products in the primary coolant path an approach has been developed to calculate the coolant specific activity. Results for 24 Na, 56 Mn, 59 Fe, 60 Co and 99Mo show that the specific activity in primary loop approaches equilibrium value under normal operating conditions fairly rapidly. Predominant corrosion product activity is due to Mn-56. Parametric studies at full power for various ramp decreases in flow rate show initial decline in the activity and then a gradual rise to relatively higher saturation values. The minimum value and the time taken to reach the minima are strong functions of the slope of linear decrease in flow rate. In the second part flow rate coastdown was allowed to occur at different flow half-times. The reactor scram was initiated at 90% of the normal flow rate. The results show that the specific activity decreases and the rate of decrease depends on pump half time and the reactor scram conditions

  1. Storage of spent fuels: implementation of a research program on the risk of waste container rupture due to stress corrosion induced by fission products

    International Nuclear Information System (INIS)

    Parise, M.; Walle, E.; Foct, J.

    2001-01-01

    The following topics were dealt with: research programm on stress corrosion of spent fuel casks materials due to fission products, such as iodine, chemical interactions with zirconium, chemical aspects of stress corrosion, rupture risk assessment

  2. Analysis of corrosion-product transport using nondestructive XRF and MS techniques

    International Nuclear Information System (INIS)

    Sawicka, B.D.; Sawicki, J.A.

    1998-01-01

    This paper describes the application of X-ray fluorescence (XRF) and Moessbauer spectroscopy (MS) techniques to monitor corrosion-product transport (CPT) in water circuits of nuclear reactors. The combination of XRF and MS techniques was applied in studies of CPT crud filters from both primary- and secondary-side water circuits (i.e., radioactive and nonradioactive specimens) of CANDU reactors. The XRF-MS method allows nondestructive analysis of species collected on filters and provides more complete information about corrosion products than commonly used digestive methods of chemical analysis. Recent analyses of CPT specimens from the Darlington Nuclear Generating Station (NGS) primary side and the Bruce B NGS feedwater system are shown as examples. Some characteristics of primary and secondary water circuits are discussed using these new data. (author)

  3. Mass transfer of corrosion products in high temperature, high pressure water circuits

    International Nuclear Information System (INIS)

    Rodd, J.T.; Nicholson, F.D.

    1976-01-01

    The CWL-3 loop is used to study the mass transfer of corrosion products in water at 270 0 C for pressures up to 6.9 MPa. Two parallel Zircaloy-2 test sections are heated directly by a low voltage a.c. electrical current to give a heat flux up to 500 W cm -2 and a heat rating up to 1500 W cm -1 . Coolant flow rates can be varied up to 0.4 kg cm -2 s -1 with or without boiling. A tracer technique has been developed to monitor continuously the deposition of corrosion products in the test sections during operation of the loop. Magnetite deposits 2.6 nm thick can be readily detected. (author)

  4. The Behavior of Corrosion Products in Sampling Systems under Boiling Water Reactor Conditions

    Energy Technology Data Exchange (ETDEWEB)

    Hermansson, Hans-Peter

    1977-08-15

    A high pressure loop has been used to simulate sampling systems employed under BWR conditions. The reliability of the sampling method was studied in a series of six test runs. A variety of parameters that are thought to influence the reliability of the sampling was investigated. These included piping geometry, water oxygen content, flow, temperature and temperature gradients. Amongst other things the results indicate that the loss by deposition of iron containing corrosion products does not exceed 50 %; this figure is only influenced to a minor extent by the above mentioned parameters. The major part of the corrosion products thus deposited is found along the first few meters of the piping and cooler coil. A moderate prolongation of a pipe which is already relatively long should thus be incapable of producing a major influence on the sampling error

  5. Corrosion of metal iron in contact with anoxic clay at 90 °C: Characterization of the corrosion products after two years of interaction

    International Nuclear Information System (INIS)

    Schlegel, Michel L.; Bataillon, Christian; Brucker, Florence; Blanc, Cécile; Prêt, Dimitri; Foy, Eddy; Chorro, Matthieu

    2014-01-01

    Highlights: • Generalized, heterogeneous corrosion is observed. • The corrosion interface is made of several layers with distinct mineralogy. • Magnetite, chukanovite, Fe-phyllosilicate, ankerite are identified from metal to clay. • The estimated corrosion damage (15 μm in two years) supports surface passivation. • The corrosion products contain only half of oxidized Fe. - Abstract: Chemical and mineralogical properties of solids formed upon free corrosion of two iron probes (one massive iron rod, and one model overpack made by two pipes covering the ends of a glass rod) in saturated clay rock (Callovo-Oxfordian formation, East of Paris Basin, France) at 90 °C over two years were investigated by microscopic and spectroscopic techniques (X-ray tomography, scanning electron microscopy coupled with energy-dispersive X-ray analysis, Raman microspectroscopy, micro-X-ray diffraction, and micro-X-ray Absorption Fine Structure spectroscopy). The corrosion rate of the massive rod was monitored in situ by electrochemical impedance spectrometry, and found to decrease from about 90 μm/year during the first month of reaction, to less than 1 μm/year after two years. X-ray tomography revealed the presence of several fractures suggesting the presence of preferential flow and diffusion pathways along the iron samples. Microscopic observations revealed similar corrosion interfaces for both samples. Corrosion heterogeneously affected the interface, with damaged thickness from ∼0 to 80 μm. In extensively damaged areas, an inner discontinuous layer of magnetite in contact with metal, an intermediate chukanovite (Fe 2 CO 3 (OH) 2 ) layer (only when magnetite is present, and only for the overpack), and an outer layer of poorly ordered Fe phyllosilicate were observed. In areas with little damage, only the Fe-silicate solids are observed. The clay transformation layer is predominantly made of ankerite ((Fe,Ca,Mg)CO 3 ) forming a massive unit near the trace of the original

  6. Enhanced corrosion resistance of stainless steel type 316 in sulphuric acid solution using eco-friendly waste product

    Science.gov (United States)

    Sanni, O.; Popoola, A. P. I.; Fayomi, O. S. I.

    2018-06-01

    Literature has shown that different organic compounds are effective corrosion inhibitors for metal in acidic environments. Such compounds usually contain oxygen, nitrogen or sulphur and function through adsorption on the metal surface, thereby creating a barrier for corrosion attack. Unfortunately, these organic compounds are toxic, scarce and expensive. Therefore, plants, natural product and natural oils have been posed as cheap, environmentally acceptable, abundant, readily available and effective molecules having low environmental impact. The corrosion resistance of austenitic stainless steel Type 316 in the presence of eco-friendly waste product was studied using weight loss and potentiodynamic polarization techniques in 0.5 M H2SO4. The corrosion rate and corrosion potential of the steel was significantly altered by the studied inhibitor. Results show that increase in concentration of the inhibitor hinders the formation of the passive film. Experimental observation shows that its pitting potential depends on the concentration of the inhibitor in the acid solution due to adsorption of anions at the metal film interface. The presence of egg shell powder had a strong influence on the corrosion resistance of stainless steel Type 316 with highest inhibition efficiency of 94.74% from weight loss analysis, this is as a result of electrochemical action and inhibition of the steel by the ionized molecules of the inhibiting compound which influenced the mechanism of the redox reactions responsible for corrosion and surface deterioration. Inhibitor adsorption fits the Langmuir isotherm model. The two methods employed for the corrosion assessment were in good agreement.

  7. Mini-review: The Morphology, Mineralogy and Microbiology of Accumulated Iron Corrosion Products

    Science.gov (United States)

    2014-03-11

    including the morphology, mineralogy , microbiology and the mecha- nisms for formation. Use of descriptive terms to denote specific iron corrosion product...RESPONSIBLE PERSON 19b. TELEPHONE NUMBER (Include area code) 11-03-2014 Journal Article Mini-review: the morphology, mineralogy and microbiology of...oxides/ hydroxides with a preponderance of α-FeOOH (goethite) and accumulation of metals. Bacteria, particularly iron-oxidizing and sulfatereducing

  8. Production of a highly active, soluble form of the cytochrome P450 reductase (CPR A) from Candida tropicalis

    Science.gov (United States)

    Donnelly, Mark

    2006-08-01

    The present invention provides soluble cytochrome p450 reductase (CPR) proteins from Candida sp. having an altered N-terminal region which results in reduced hydrophobicity of the N-terminal region. Also provided are host cells comprising the subject soluble CPR proteins. In addition, the present invention provides nucleotide and corresponding amino acid sequences for soluble CPR proteins and vectors comprising the nucleotide sequences. Methods for producing a soluble CPR, for increasing production of a dicarboxylic acid, and for detecting a cytochrome P450 are also provided.

  9. X-ray diffraction study of slags forming during corrosion resistant steel production

    International Nuclear Information System (INIS)

    Slavov, V.I.; Zadorozhnaya, V.N.; Shurygina, A.V.

    1990-01-01

    Using X-ray diffraction analysis slags, forming during corrosion-resistant 12Kh18N10T grade steel production by two flowsheets, are studied. Standard two-slag technology of steel production does not provide efficient disintegration of chromospinelides in slags, gives high steel contamination with respect to nonmetallic impurities, coarse structure and, as a consequence, presence of macrodefects on rolled products surface. One-slag steel melting technology with titanium alloying of the steel at vacuum causes fast removal of chromospinelides at the beginning of reduction period, promotes titanium absorption by the steel, refines nonmetallic inclusions, provides more fine structure and steel plasticity, removes surface defects

  10. Strontium concentrations in corrosion products from residential drinking water distribution systems.

    Science.gov (United States)

    Gerke, Tammie L; Little, Brenda J; Luxton, Todd P; Scheckel, Kirk G; Maynard, J Barry

    2013-05-21

    The United States Environmental Protection Agency (US EPA) will require some U.S. drinking water distribution systems (DWDS) to monitor nonradioactive strontium (Sr(2+)) in drinking water in 2013. Iron corrosion products from four DWDS were examined to assess the potential for Sr(2+) binding and release. Average Sr(2+) concentrations in the outermost layer of the corrosion products ranged from 3 to 54 mg kg(-1) and the Sr(2+) drinking water concentrations were all ≤0.3 mg L(-1). Micro-X-ray adsorption near edge structure spectroscopy and linear combination fitting determined that Sr(2+) was principally associated with CaCO3. Sr(2+) was also detected as a surface complex associated with α-FeOOH. Iron particulates deposited on a filter inside a home had an average Sr(2+) concentration of 40.3 mg kg(-1) and the associated drinking water at a tap was 210 μg L(-1). The data suggest that elevated Sr(2+) concentrations may be associated with iron corrosion products that, if disturbed, could increase Sr(2+) concentrations above the 0.3 μg L(-1) US EPA reporting threshold. Disassociation of very small particulates could result in drinking water Sr(2+) concentrations that exceed the US EPA health reference limit (4.20 mg kg(-1) body weight).

  11. Deposition and incorporation of corrosion product to primary coolant suppressing method

    International Nuclear Information System (INIS)

    Tsuzuki, Yasuo; Hasegawa, Naoyoshi; Fujioka, Tsunaaki.

    1992-01-01

    In a PWR type nuclear power plant, the concentration of dissolved nitrogen in primary coolants is increased by controlling the nitrogen partial pressure in a volume controlling tank gas phase portion or addition of water in a primary system water supply tank containing dissolved nitrogen to a primary system. Then ammonium is formed by a reaction with hydrogen dissolved in the primary coolants in the field of radiation rays, to control the concentration of ammonium in the coolants within a range from 0.5 to 3.5 ppm, and operate the power plant. As a result, deposition and incorporation of corrosion products to the structural materials of the primary system equipments during plant operation (pH 6.8 to 8.0) are suppressed. In other words, deposition of particulate corrosion products on the surface of fuel cladding tubes and the inner surface of pipelines in the primary system main equipments is prevented and incorporation of ionic radioactive corrosion products to the oxide membranes on the inner surface of the pipelines of the primary system main equipments is suppressed, to greatly reduce the radiation dose rate of the primary system pipelines. Thus, operator's radiation exposure can be decreased upon shut down of the plant. (N.H.)

  12. A Moessbauer and Electrochemical Characterization of the Corrosion Products Formed from Marine and Marine-Antartic Environments

    Energy Technology Data Exchange (ETDEWEB)

    Ohanian, M.; Caraballo, R.; Dalchiele, E. A.; Quagliata, E. [Instituto de Ingenieria Quimica, Facultad de Ingenieria (Uruguay)

    2003-06-15

    Corrosion products formed on low alloy steel under two marine environments are characterised. Both environments are classified as C4 according to the ISO 9223 Standard. The corrosion products are identified and their relative proportion is determined by Moessbauer spectroscopy (transmission geometry). Free potentials of corrosion are measured to evaluate the activity of their surfaces. Structural characterisation by XRD were performed on selected samples. It is concluded that the principal phases are goethite, lepidocrocite, ferrihidrite and maghemite. The relative amount of each of them changes with time and with the atmospheric dynamics of each environment.

  13. A Moessbauer and Electrochemical Characterization of the Corrosion Products Formed from Marine and Marine-Antartic Environments

    International Nuclear Information System (INIS)

    Ohanian, M.; Caraballo, R.; Dalchiele, E. A.; Quagliata, E.

    2003-01-01

    Corrosion products formed on low alloy steel under two marine environments are characterised. Both environments are classified as C4 according to the ISO 9223 Standard. The corrosion products are identified and their relative proportion is determined by Moessbauer spectroscopy (transmission geometry). Free potentials of corrosion are measured to evaluate the activity of their surfaces. Structural characterisation by XRD were performed on selected samples. It is concluded that the principal phases are goethite, lepidocrocite, ferrihidrite and maghemite. The relative amount of each of them changes with time and with the atmospheric dynamics of each environment.

  14. Development of experimental method to simulate the corrosion products in the primary system of nuclear power plant

    International Nuclear Information System (INIS)

    Kim, Sang Hyun; Kim, In Sup; Jang, Chang Heui

    2005-01-01

    Corrosion products are recognized as one of the major sources of occupational radiation exposure for nuclear power plant workers. Numerous studies have been conducted on the primary water chemistry to reduce the amount of crud in the primary circuit to avoid the radioactivity build-up in the plant. However, experiments with crud are restricted in laboratory because the crud is highly radioactive material. The objective of this study is to develop the simulating method of corrosion product in nuclear power plant

  15. Fate of corrosion products released from stainless steel in marine sediments and seawater. Part 2. Sequim Bay clayey silt

    International Nuclear Information System (INIS)

    Schmidt, R.L.

    1982-04-01

    This report describes laboratory experiments in which neutron-activated 347 stainless steel specimens were exposed to clayey silt from Sequim Bay, Washington. The properties and trace metal geochemistry of the sediment and the amounts of corrosion products that were released under oxic and reduced conditions and their distribution among different chemical fractions of the sediment are discussed. The distributions of Cr, Mn, Fe, Ni and Cu among different chemical forms in the Sequim Bay sediment show that DTPA removed <10% of extractable Cr, Fe and Mn, approx. 20% of extractable Ni and approx. 30% of extractable Cu. The inorganic fraction (material soluble in 2.5% acetic acid) accounted for approx. 30% of total extractable Mn and approx. 10% or less of Cr, Fe, Ni and Cu. Major portions of Cr and Cu, and a large amount of Fe were in the organic fraction. Extractable Mn, Fe and Ni were associated with hydrous oxides likely as coatings on the mineral substrate of the sediment. No Co was detectable in any of the extracts

  16. Testing and prediction of erosion-corrosion for corrosion resistant alloys used in the oil and gas production industry

    Science.gov (United States)

    Rincon, Hernan E.

    The corrosion behavior of CRAs has been thoroughly investigated and documented in the public literature by many researchers; however, little work has been done to investigate erosion-corrosion of such alloys. When sand particles are entrained in the flow, the degradation mechanism is different from that observed for sand-free corrosive environment. There is a need in the oil and gas industry to define safe service limits for utilization of such materials. The effects of flow conditions, sand rate, pH and temperature on the erosion-corrosion of CRAs were widely studied. An extensive experimental work was conducted using scratch tests and flow loop tests using several experimental techniques. At high erosivity conditions, a synergistic effect between erosion and corrosion was observed. Under the high sand rate conditions tested, erosivity is severe enough to damage the passive layer protecting the CRA thereby enhancing the corrosion rate. In most cases there is likely a competition between the rates of protective film removal due to mechanical erosion and protective film healing. Synergism occurs for each of the three alloys examined (13Cr and Super13Cr and 22Cr); however, the degree of synergism is quite different for the three alloys and may not be significant for 22Cr for field conditions where erosivities are typically much lower that those occurring in the small bore loop used in this research. Predictions of the corrosion component of erosion-corrosion based on scratch test data compared reasonably well to test results from flow loops for the three CRAs at high erosivity conditions. Second order behavior appears to be an appropriate and useful model for representing the repassivation process of CRAs. A framework for a procedure to predict penetration rates for erosion-corrosion conditions was developed based on the second order model behavior observed for the re-healing process of the passive film of CRAs and on computational fluid dynamics (CFD) simulations

  17. Corrosion Product Measurements to ensure integrity of the Steam Generators in Beznau NPP

    International Nuclear Information System (INIS)

    Mailand, Irene; Franz, Patrick; Venz, Hartmut

    2012-09-01

    The Nuclear Power Plant Beznau comprises two identical 380 MWe PWR units with two loops each, commissioned in 1969 and 1971. Westinghouse was responsible for the primary part of the plant and BBC/ABB for the secondary circuit. The original materials used in the secondary systems were made of several copper-based alloys, such as for the Condensers, the Low Pressure Pre-heaters and the Moisture Separator Re-heater. The original Steam Generator Tubes were made of Inconel 600 MA. Regarding its age, the NPP Beznau has to be qualified as an old plant. However, in fact particularly in the last 20 years the plant has undergone an extensive modernisation programme in which about 1.5 billion Swiss Francs have been invested. Important measures were the replacements of the Steam Generators with tubes comprising Inconel 690 TT which was realized at unit 1 in 1993 and at unit 2 in 1999. Copper was completely banished from the secondary system and replaced by stainless and chromium steel. The Condensers were fitted with titanium tubes. The secondary water chemistry had to be changed by these replacements and moved step by step from Low-AVT with a pH of about 9.3 to High-AVT with a pH of 9.8 to 9.9, currently. To ensure the integrity of the new Steam Generators as well as of the whole Secondary System a corrosion product programme was introduced at the end of the Nineties. Several investigations which are performed periodically are represented by analyses of corrosion products, measurements of sludge mass and composition in the Steam Generators, Hide-Out-Return- and mass balance measurements of corrosion products in the whole circuit. Objectives of these investigations are assessments of the efficiency of the water chemistry and trend considerations regarding to the transport of corrosion products and pollutants into the Steam Generator, as well as of the potential danger of deposits and stored or absorbed pollutants. The main target of all measures is to avoid any chemical

  18. The study of the corrosion protection of the low-carbon steel using film-products

    International Nuclear Information System (INIS)

    Aiancului, L.; Millet, Jean-Pierre

    2001-01-01

    The paper reports studies on the efficiency of the film-inhibitors that covered low-carbon steel placed in a humid medium, and also, the optimization of the working conditions to improve the resistance to corrosion. The analyzes were done in the Industrial Physical - Chemical Laboratories of INSA - Lyon by electrochemical stationary techniques. The experimental device was a potentiometer of type EGG PAR (Princeton Applied Research). It was connected with a computer and three potential electrodes introduced in a cell with NaCl 30 g/l solution to acquire the data and to process the information. The film-products used were organic hydrosoluble polymers with diphosphonic 'heads' that permit a very good absorption at the metallic surface. This research is used to protect the installations of low-carbon steel against the atmospheric and high temperature corrosion. (authors)

  19. Soluble suppressor supernatants elaborated by concanavalin A-activated human mononuclear cells. Characterization of a soluble suppressor of B cell immunoglobulin production

    International Nuclear Information System (INIS)

    Fleisher, T.A.; Greene, W.C.; Blaese, R.M.; Waldmann, T.A.

    1981-01-01

    Human peripheral blood mononuclear cells (PBMC) activated with the mitogenic lectin concanavalin A (Con A) elaborate a soluble immune suppressor supernatant (SISS) that contains at least 2 distinct suppressor factors. One of these, SISS-B, inhibits polyclonal B cell immunoglobulin production, whereas the other, SISS-T, suppresses T cell proliferation to both mitogens and antigens. The latter mediator is discussed in the companion paper. Characteristics of the human soluble suppressor of B cell immunoglobulin production (SISS-B) include: 1) inhibition by a noncytotoxic mechanism, 2) loss of activity in the presence of the monosaccharide L-rhamnose, 3) appearance within 8 to 16 hr after the addition of Con A, 4) elaboration by cells irradiated with 500 or 2000 rads, 5) production by highly purified T cells, 6) stability at pH 2.5 but instability at 56/sup o/C, and 7) m.w. of 60 to 80,000. These data indicate that after Con A activation, selected T cells not only become potent suppressor cells, but also generate a soluble saccharide-specific factor(s) that inhibits polyclonal immunoglobulin production by human B cells

  20. Efficient protein production method for NMR using soluble protein tags with cold shock expression vector

    International Nuclear Information System (INIS)

    Hayashi, Kokoro; Kojima, Chojiro

    2010-01-01

    The E. coli protein expression system is one of the most useful methods employed for NMR sample preparation. However, the production of some recombinant proteins in E. coli is often hampered by difficulties such as low expression level and low solubility. To address these problems, a modified cold-shock expression system containing a glutathione S-transferase (GST) tag, the pCold-GST system, was investigated. The pCold-GST system successfully expressed 9 out of 10 proteins that otherwise could not be expressed using a conventional E. coli expression system. Here, we applied the pCold-GST system to 84 proteins and 78 proteins were successfully expressed in the soluble fraction. Three other cold-shock expression systems containing a maltose binding protein tag (pCold-MBP), protein G B1 domain tag (pCold-GB1) or thioredoxin tag (pCold-Trx) were also developed to improve the yield. Additionally, we show that a C-terminal proline tag, which is invisible in 1 H- 15 N HSQC spectra, inhibits protein degradation and increases the final yield of unstable proteins. The purified proteins were amenable to NMR analyses. These data suggest that pCold expression systems combined with soluble protein tags can be utilized to improve the expression and purification of various proteins for NMR analysis.

  1. Efficient protein production method for NMR using soluble protein tags with cold shock expression vector

    Energy Technology Data Exchange (ETDEWEB)

    Hayashi, Kokoro [Fujifilm Corporation, Analysis Technology Center (Japan); Kojima, Chojiro, E-mail: kojima@protein.osaka-u.ac.j [Nara Institute of Science and Technology (NAIST), Graduate School of Biological Sciences (Japan)

    2010-11-15

    The E. coli protein expression system is one of the most useful methods employed for NMR sample preparation. However, the production of some recombinant proteins in E. coli is often hampered by difficulties such as low expression level and low solubility. To address these problems, a modified cold-shock expression system containing a glutathione S-transferase (GST) tag, the pCold-GST system, was investigated. The pCold-GST system successfully expressed 9 out of 10 proteins that otherwise could not be expressed using a conventional E. coli expression system. Here, we applied the pCold-GST system to 84 proteins and 78 proteins were successfully expressed in the soluble fraction. Three other cold-shock expression systems containing a maltose binding protein tag (pCold-MBP), protein G B1 domain tag (pCold-GB1) or thioredoxin tag (pCold-Trx) were also developed to improve the yield. Additionally, we show that a C-terminal proline tag, which is invisible in {sup 1}H-{sup 15}N HSQC spectra, inhibits protein degradation and increases the final yield of unstable proteins. The purified proteins were amenable to NMR analyses. These data suggest that pCold expression systems combined with soluble protein tags can be utilized to improve the expression and purification of various proteins for NMR analysis.

  2. Kinetics of corrosion products release from nickel-base alloys corroding in primary water conditions. A new modeling of release

    International Nuclear Information System (INIS)

    Carrette, F.; Guinard, L.; Pieraggi, B.

    2002-01-01

    The radioactivity in the primary circuit arises mainly from the activation of corrosion products in the core of pressurised water reactors; corrosion products dissolve from the oxide scales developed on steam generator tubes of alloy 690. The controlling and modelling of this process require a detailed knowledge of the microstructure and chemical composition of oxide scales as well as the kinetics of their corrosion and dissolution. Alloy 690 was studied as tubes and sheets, with three various surface states (as-received, cold-worked, electropolished). Corrosion tests were performed at 325 C and 155 bar in primary water conditions (B/Li - 1000/2 ppm, [H 2 ] 30 cm 3 .kg -1 TPN, [O 2 ] < 5 ppb); test durations ranged between 24 and 2160 hours. Corrosion tests in the TITANE loop provided mainly corrosion and oxidation kinetics, and tests in the BOREAL loop yielded release kinetics. This study revealed asymptotic type kinetics. Characterisation of the oxide scales grown in representative conditions of the primary circuit was performed by several techniques (SEM, TEM, SIMS, XPS, GIXRD). These analyses revealed the essential role of the fine grained cold-worked scale present on as-received and cold-worked materials. This scale controls the corrosion and release phenomena. The kinetic study and the characterisation of the oxide scales contributed to the modelling of the corrosion/release process. A growth/dissolution model was proposed for corrosion product scales grown in non-saturated dynamic fluid. This model provided the temporal evolution of oxide scales and release kinetics for different species (Fe, Ni, Cr). The model was validated for several surface states and several alloys. (authors)

  3. Reduction of corrosion products in water coolant - basic way of increase in efficiency and improvement of ecological safety of NPU

    International Nuclear Information System (INIS)

    Prozorov, V.V.

    2004-01-01

    Corrosion of oxidated steel in water with additives of inhibitors or oxygen was considered. It is shown that preliminary oxidation of steel makes possible declining concentration of inhibitors or oxygen. Experiments demonstrate possibilities of the neutral-oxygen water regime for supply of the effective protection. Corrosion resistance of steel may be increased in many times through correct aqua-chemical regimes. Also concentration of corrosion products may be decreased in many times in coolant and their activation in neutron flux of nuclear reactor, amount of radioisotopes [ru

  4. Development of corrosion models to ensure reliable performance of nuclear power plants

    International Nuclear Information System (INIS)

    Kritzky, V.G.; Stjazhkin, P.S.

    1993-01-01

    The safety and reliability of the coolant circuits in nuclear power plants depend much on corrosion and corrosion products transfer processes. Various empirical models have been developed which are applicable to particular sets of operational conditions. In our laboratory a corrosion model has been worked out, which is based on the thermodynamic properties of the compounds, participating in corrosion process and on the assumption, that the corrosion process is controlled by the solubilities of the corrosion products forming the surface oxide layer. The validity of the model has been verified by use of retrospective experimental data, which have been obtained for a series of structural materials such as e.g., carbon and stainless steels, Cu-, Al-, and Zr alloys. With regard for hydriding the model satisfactorily describes stress corrosion cracking process in water-salt environments. This report describes a model based on the thermodynamic properties of the compounds participating in the corrosion process, and on the assumption that the corrosion process is controlled by the solubilities of the corrosion products forming the surface oxide layer

  5. A Revisit to the Corrosion Inhibition of Aluminum in Aqueous Alkaline Solutions by Water-Soluble Alginates and Pectates as Anionic Polyelectrolyte Inhibitors

    Directory of Open Access Journals (Sweden)

    Refat Hassan

    2013-01-01

    Full Text Available The corrosion behavior of aluminum (Al in alkaline media in presence of some natural polymer inhibitors has been reinvestigated. The inhibition action of the tested inhibitors was found to obey both Langmuir and Freundlich isotherms models. The inhibition efficiency was found to increase with increasing the inhibitors concentration and decrease with increasing the temperature, suggesting physical adsorption mechanism. Factors such as the concentration and geometrical structure of the inhibitor, concentration of the corrosive medium, and temperature affecting the corrosion rates were examined. The kinetic parameters were evaluated, and a suitable corrosion mechanism consistent with the kinetic results obtained is suggested and discussed.

  6. Corrosion testing on crude oil tankers and other product carriers by means of acoustic emission (AE)

    Energy Technology Data Exchange (ETDEWEB)

    Lackner, Gerald [TUV Austria, Deutschstrasse 10, 1230 Wien (Austria); Tscheliesnig, Peter [TUV Austria, Deutschstrasse 10, 1230 Wien (Austria)

    2004-07-01

    In the last decades a lot of maritime disasters with crude oil tankers occurred (e.g. Exxon- Valdez, Erika, Prestige). Every accident led to extreme pollution with horrible consequences not only for the environment but also for the life of the inhabitants of the affected coasts. Although most of these accidents were caused by human errors, the material degradation of the ship hull due to corrosion played an important role. Acoustic emission (AE) is already used to detect and discriminate the stage of corrosion of structures located on land. A consortium consisting of experienced partners from the fields of ship building and classification as well as from AE testing and equipment manufacturing started to investigate the feasibility of this testing technique for its application on oil tankers. The aim of the research project funded by the European Commission is to develop an on-line corrosion monitoring technique based on a permanent installation of AE sensors as well as a spot testing technique during stops in harbors or at anchorages using mobile equipment. Since the project was started, a lot of lab tests as well as background measurements were done on different types of tankers up to a size of 35.000 dead weight tons (DWT). The gathered data were evaluated with a frequency domain based pattern recognition system and it was possible to distinguish the AE signals related to corrosion from those signals, which were emitted by the structure due to the harsh environment on sea (background noise). Together with the oncoming developments of the AE equipment and the improvement of the data base, this project will lead to an important breakthrough for the safe shipping of hazardous products like crude oil. (authors)

  7. Phase analysis of corrosion products of carbon steel in sea water

    International Nuclear Information System (INIS)

    Garcia R, J.; Yee M, H.; Maldonado M, H.; Nunez, L.; Reguera, E.

    1998-01-01

    Nowadays carbon steel continues being the most widely used metallic material in marine and coastal buildings. The economic losses, due to corrosion processes, of those countries with important industrial and social activities in coastal regions are highly significant. In this sense the evaluation of the corrosion process of carbon steel and other materials in seawater or in coastal zones is a primary task for protection methods or to predict the hfe of an specific installation. In this communication we present the phases analysis, using XRD and Moessbauer techniques, of corrosion products of a carbon steel (CT3, equivalent to AISI C1020) exposed in two natural corrosion stations in the Caribbean sea (Cuba). The exposition time run from days to 36 months and the evaluated rust are characteristic of samples totally immersed in seawater, from the splash zone and form coastal zones at different distance from the shoreline. Quantitative phase analysis shown presence of magnetite (Fe 3 O 4 ), maghemite (y-Fe 2 O 3 ), akaganeite (B-FeOOH), lepidocrocite (y-FeOOH) and goethite (a-FeOOH) as iron bearing phases, and CaCO 3 (Calcite and aragonite), these last ones mainly in the immersed samples. Quantitative phase analysis by XRD was implemented as a linear combination of the patterns characteristic of all the detected phases and an appropriate model for the background. The quantitative results were used in kinetic models to understand the phase transformation between the iron oxides and oxy hydroxides in the studied conditions. The XRD qualitative and quantitative results were corroborated by Moessbauer spectroscopy in the temperature range of 20 to 300 K. (Author)

  8. Method of inhibiting concentration of radioactive corrosion products in cooling water or nuclear power plants

    International Nuclear Information System (INIS)

    Takabayashi, Jun-ichi; Hishida, Mamoru; Ishikura, Takeshi.

    1979-01-01

    Purpose: To suppress the increase in the concentration of the radioactive corrosion products in cooling water, which increase is accompanied by the transference of the corrosion products activated and accumulated in the core due to dissolution and exfoliation into the core water, and inhibit the flowing of said products out of the core and the diffusion thereof into the cooling system, thereby to prevent the accumulation of said products in the cooling system and prevent radioactive contaminations. Method: In a nuclear power plant of a BWR type light water reactor, when the temperature of the pile water is t 0 C, hydrogen is injected in cooling water in a period of time from immediately before starting of the drive stopping operation of the nuclear power plant to immediately after the termination of restarting operation, whereby the concentration of hydrogen in the reactor water through said period is maintained at a value more than 2exp (0.013 t) cm 3 N.T.P./kg H 2 O. (Aizawa, K.)

  9. Filterability of corrosion products formed between carbon steel and water. Influence of temperature and oxygen content

    International Nuclear Information System (INIS)

    Kelen, T.; Falk, I.

    1975-09-01

    A laboratory investigation has been made for the purpose of studying the influence of temperature and oxygen content on the filterability of corrosion products formed between carbon-steel and water. The experiments were performed in a high temperature loop where the water is initially heated in a pre-heater, then cooled and finally filtered. The corrosion products were transferred to thewater from a carbon-steel surface that had previously been neutron activated and the amount of iron present was determined from measurements of the γ-radiation emitted by Fe-59. Filterability was then computed as the ratio between the total amount of iron in the water phase and the amount of iron retained on the filter. The investigation covers a series of experiments at filtering temperatures of 20, 90 and 160 dec G, pre-heater temperatures up to 300 deg C and oxygen contents of 10 and 300 ppb O 2 . In addition the extent of iron deposition in the pre-heater and heat regulator has been determined after each series of experiments. Filterability exhibited a pronounced dependence upon both the filter and pre-heater temperatures and also upon the oxygen content. Among the conclusions to which the results lead is the observation that a strict comparison of filterability values for the fraction of corrosion products in cooled water samples is impossible when these are taken from 1) different sections of a high temperature system 2) a single sampling point while the system is being run up 3) two separate systems (e.g. steam boilers) operated at different temperatures 4) two separate systems operated at different oxygen contents. It accordingly appears advizable to restrict the use of cold-filtered samples from conventional steam-raising plants to the comparison of values relating to a single sampling point under constant operating conditions. (author)

  10. Zinc corrosion after loss-of-coolant accidents in pressurized water reactors – Physicochemical effects

    Energy Technology Data Exchange (ETDEWEB)

    Kryk, Holger, E-mail: h.kryk@hzdr.de [Helmholtz-Zentrum Dresden-Rossendorf, Institute of Fluid Dynamics, P.O. Box 510119, D-01314 Dresden (Germany); Hoffmann, Wolfgang [Helmholtz-Zentrum Dresden-Rossendorf, Institute of Fluid Dynamics, P.O. Box 510119, D-01314 Dresden (Germany); Kästner, Wolfgang; Alt, Sören; Seeliger, André; Renger, Stefan [Hochschule Zittau/Görlitz, Institute of Process Technology, Process Automation and Measuring Technology, Theodor-Körner-Allee 16, D-02763 Zittau (Germany)

    2014-12-15

    Highlights: • Physicochemical effects due to post-LOCA zinc corrosion in PWR were elucidated. • Decreasing solubility of corrosion products with increasing temperature was found. • Solid corrosion products may be deposited on hot surfaces and/or within hot-spots. • Corrosion products precipitating from coolant were identified as zinc borates. • Depending on coolant temperature, different types of zinc borate are formed. - Abstract: Within the framework of the reactor safety research, generic experimental investigations were carried out aiming at the physicochemical background of possible zinc corrosion product formation, which may occur inside the reactor pressure vessel during the sump circulation operation after loss-of-coolant accidents in pressurized water reactors. The contact of the boric acid containing coolant with hot-dip galvanized steel containment internals causes corrosion of the corresponding materials resulting in dissolution of the zinc coat. A retrograde solubility of zinc corrosion products with increasing temperature was observed during batch experiments of zinc corrosion in boric acid containing coolants. Thus, the formation and deposition of solid corrosion products cannot be ruled out if the coolant containing dissolved zinc is heated up during its recirculation into hot regions within the emergency cooling circuit (e.g. hot-spots in the core). Corrosion experiments at a lab-scale test facility, which included formation of corrosion products at a single heated cladding tube, proved that dissolved zinc, formed at low temperatures in boric acid solution by zinc corrosion, turns into solid deposits of zinc borates when contacting heated zircaloy surfaces during the heating of the coolant. Moreover, the temperature of formation influences the chemical composition of the zinc borates and thus the deposition and mobilization behavior of the products.

  11. Zinc corrosion after loss-of-coolant accidents in pressurized water reactors – Physicochemical effects

    International Nuclear Information System (INIS)

    Kryk, Holger; Hoffmann, Wolfgang; Kästner, Wolfgang; Alt, Sören; Seeliger, André; Renger, Stefan

    2014-01-01

    Highlights: • Physicochemical effects due to post-LOCA zinc corrosion in PWR were elucidated. • Decreasing solubility of corrosion products with increasing temperature was found. • Solid corrosion products may be deposited on hot surfaces and/or within hot-spots. • Corrosion products precipitating from coolant were identified as zinc borates. • Depending on coolant temperature, different types of zinc borate are formed. - Abstract: Within the framework of the reactor safety research, generic experimental investigations were carried out aiming at the physicochemical background of possible zinc corrosion product formation, which may occur inside the reactor pressure vessel during the sump circulation operation after loss-of-coolant accidents in pressurized water reactors. The contact of the boric acid containing coolant with hot-dip galvanized steel containment internals causes corrosion of the corresponding materials resulting in dissolution of the zinc coat. A retrograde solubility of zinc corrosion products with increasing temperature was observed during batch experiments of zinc corrosion in boric acid containing coolants. Thus, the formation and deposition of solid corrosion products cannot be ruled out if the coolant containing dissolved zinc is heated up during its recirculation into hot regions within the emergency cooling circuit (e.g. hot-spots in the core). Corrosion experiments at a lab-scale test facility, which included formation of corrosion products at a single heated cladding tube, proved that dissolved zinc, formed at low temperatures in boric acid solution by zinc corrosion, turns into solid deposits of zinc borates when contacting heated zircaloy surfaces during the heating of the coolant. Moreover, the temperature of formation influences the chemical composition of the zinc borates and thus the deposition and mobilization behavior of the products

  12. Corrosion protection products as a source of bisphenol A and toxicity to the aquatic environment.

    Science.gov (United States)

    Vermeirssen, Etiënne L M; Dietschweiler, Conrad; Werner, Inge; Burkhardt, Michael

    2017-10-15

    Steel components are typically treated with anti-corrosion coatings like epoxy or polyurethane resins to protect the integrity and functioning of steel. Such resins may contain substances, such as bisphenol A (BPA), that have caused concern in a human and environmental toxicological context. We investigated the release of toxicity from four anti-corrosion coatings used in hydraulic and civil engineering. Resins were applied onto glass plates and leachate samples produced by horizontally shaking the plates in water for 7 days. Two experiments were conducted, one with a 1 day and one with a 7 day curing period. Using a suite of bioassays, we tested samples for: agonistic and antagonistic effects on various mammalian nuclear receptors; inhibition of photosynthesis and growth in algae; inhibition of bacterial bioluminescence; and inhibition of water flea reproduction. Concentrations of BPA, bisphenol F and various BPA transformation products were determined by chemical analysis (LC-MS/MS). Bioassay results were evaluated using a scheme developed by DIBt (Centre of Competence for Construction, Berlin, Germany). Three products induced responses in one or more of the measured endpoints and toxicity profiles varied markedly in intensity across products. One product released high amounts of BPA which was associated with effects on nuclear receptor transactivation, requiring a more than 700-fold dilution for effect induction to fall below 20%. The same product was also the most toxic to water flea reproduction, requiring ca. 70-fold dilution for effects to fall below 20%. Another product was highly toxic in terms of bacterial bioluminescence, particularly after a shorter curing time, requiring a ca. 1'300-fold dilution for effects to fall below 20%. The third product required a 22-fold dilution for inhibition of water flea reproduction to drop below 20%. Results show that anti-corrosion coatings based on epoxy resins can be a source of toxicity to the aquatic environment

  13. Electrochemical corrosion studies on a selected carbon steel for application in nuclear waste disposal containers: Influence of radiolytic products on corrosion in brines

    International Nuclear Information System (INIS)

    Farvaque-Bera, A.M.; Smailos, E.

    1994-07-01

    In previous corrosion studies, carbon steels were identified as promising materials for the manufacturing of long-lived high-level waste containers that could act as a radionuclide barrier in a rock-salt repository. In the present work, the influence of some important oxidizing radiolytic products generated in gamma irradiated brines on the electrochemical corrosion behaviour of the preselected fine-grained steel TStE 355 was studied. The steel was examined by potentiodynamic and potentiostatic polarization methods at 90 C in a disposal relevant NaCl-rich brine containing radiolytic products such as H 2 O 2 , ClO - , ClO 3 - and ClO 4 - at concentrations between 10 -4 and 10 -2 M/l. The significance of the radiolytic products to steel corrosion depends on their concentration at the metal-brine interface, which in turn, depends on many factors such as the dose rate, the amount of water present in the disposal area, the escape of gases (e.g. H 2 )

  14. Preliminary study of radionuclide corrosion products in primary cooling water at RSG-GAS

    International Nuclear Information System (INIS)

    Lestari, D.E.; Pudjojanto, M.S.; Subiharto; Budi, S.

    1998-01-01

    Analysis of radionuclides emitting gamma rays at the primary cooling water at RSG-GAS has been carried out. The water coolant samples was performed using a low level background gamma spectrometer unit, including of high resolution of gamma detector HP-Ge Tennelec and Multichannel Analyzer (MCA) ADCAM 100 ORTEC. The result indicated Na-24 and Mn-56 radionuclides that may be as corrosion product and should studied deeply in the future. The expected activity concentration radionuclide for Mn-56 is lower than those written in the Safety Analysis Report (SAR), while for Na-24 is in agreement

  15. Modeling how soluble microbial products (SMP) support heterotrophic bacteria in autotroph-based biofilms

    DEFF Research Database (Denmark)

    Merkey, Brian; Rittmann, Bruce E.; Chopp, David L.

    2009-01-01

    . In this paper, we develop and use a mathematical model to describe a model biofilm system that includes autotrophic and heterotrophic bacteria and the key products produced by the bacteria. The model combines the methods of earlier multi-species models with a multi-component biofilm model in order to explore...... the interaction between species via exchange of soluble microbial products (SMP). We show that multiple parameter sets are able to describe the findings of experimental studies, and that heterotrophs growing on autotrophically produced SMP may pursue either r- or K-strategies to sustain themselves when SMP...... is their only substrate. We also show that heterotrophs can colonize some distance from the autotrophs and still be sustained by autotrophically produced SMP. This work defines the feasible range of parameters for utilization of SMP by heterotrophs and the nature of the interactions between autotrophs...

  16. Characterization of soluble microbial products as precursors of disinfection byproducts in drinking water supply.

    Science.gov (United States)

    Liu, Jin-Lin; Li, Xiao-Yan; Xie, Yue-Feng; Tang, Hao

    2014-02-15

    Water pollution by wastewater discharge can cause the problem of disinfection byproducts (DBPs) in drinking water supply. In this study, DBP formation characteristics of soluble microbial products (SMPs) as the main products of wastewater organic biodegradation were investigated. The results show that SMPs can act as DBP precursors in simulated wastewater biodegradation process. Under the experimental conditions, stabilized SMPs had DBPFP (DBP formation potential) yield of around 5.6 μmol mmol(-1)-DOC (dissolved organic carbon) and DBP speciation profile different from that of the conventional precursor, natural organic matter (NOM). SMPs contained polysaccharides, proteins, and humic-like substances, and the latter two groups can act as reactive DBP precursors. SMP fraction with molecular weight of water treatment processes, more efforts are needed to control wastewater-derived DBP problem in water resource management. Copyright © 2013 Elsevier B.V. All rights reserved.

  17. Soluble Receptor for Advanced Glycation End Product: A Biomarker for Acute Coronary Syndrome

    Directory of Open Access Journals (Sweden)

    Louise J. N. Jensen

    2015-01-01

    Full Text Available The receptor of advanced glycation end products (RAGE and its ligands are linked to the pathogenesis of coronary artery disease (CAD, and circulating soluble receptor of advanced glycation end products (sRAGE, reflecting the RAGE activity, is suggested as a potential biomarker. Elevated sRAGE levels are reported in relation to acute ischemia and this review focuses on the role of sRAGE as a biomarker for the acute coronary syndrome (ACS. The current studies demonstrated that sRAGE levels are elevated in relation to ACS, however during a very narrow time period, indicating that the time of sampling needs attention. Interestingly, activation of RAGE may influence the pathogenesis and reflection in sRAGE levels in acute and stable CAD differently.

  18. Factors affecting the corrosion of SiC layer by fission product palladium

    International Nuclear Information System (INIS)

    Dewita, E.

    2000-01-01

    HTR is one of the advanced nuclear reactors which has inherent safety system, graphite moderated and helium gas cooled. In general, these reactors are designed with the TRISO coated particle consist of four coating layers that are porous pyrolytic carbon (PyC). inner dense PyC (IPyC), silicon carbide (SiC), and outer dense PyC (OPyC). Among the four coating layers, the SiC plays an important role beside in retaining metallic fission products, it also provides mechanical strength to fuel particle. However, results of post irradiation examination indicate that fission product palladium can react with and corrode SiC layer, This assessment is conducted to get the comprehension about resistance of SiC layer on irradiation effects, especially in order to increase the fuel bum-up. The result of this shows that the corrosion of SiC layer by fission product palladium is beside depend on the material characteristics of SiC, and also there are other factors that affect on the SiC layer corrosion. Fuel enrichment, bum-up, and irradiation time effect on the palladium flux in fuel kernel. While, the fuel density, vapour pressure of palladium (the degree depend on the irradiation temperature and kernel composition) effect on palladium migration in fuel particle. (author)

  19. COPPER CORROSION AND SOLUBILITY RESEARCH

    Science.gov (United States)

    This poster provides a very cursory summary of TTEB in-house copper research experimental systems, and extramural research projects. The field studies summarized are the Indian Hill (OH) study of the use of orthophosphate for reducing cuprosolvency in a high alkalinity water, an...

  20. The solubility of inorganic compounds in water and steam with particular reference to silica and iron oxides and its deposits in power plant cycles

    International Nuclear Information System (INIS)

    Heitmann, H.G.

    1975-01-01

    The presence of silica in the water-steam cycle can be extremely detrimental to the operation of a high pressure power station. The solubility diagram of silica in water and steam obtained from numerous measurements is presented. The solubility and deposition of corrosion products, particularly iron oxyde, were investigated together with the effect on heat transfer in heated steam generator tubes. The remove corrosion products from feedwater, electromagnetic filters may be employed and their installation in the primary circuits of the PWR type reactors leads to a considerable reduction of the corrosion products and activity levels

  1. Magnesium microelectrode corrosion product transport modelling in relation to chloride induced pitting

    International Nuclear Information System (INIS)

    Burrows, R.; Cook, A.; Stevens, N.P.C.

    2012-09-01

    The high magnesium alloy Magnox is used as a fuel clad for the UK gas cooled, graphite moderated reactors of the same name. The fuel is metallic uranium (typically natural enrichment), so a low neutron absorption cross-section clad is required. Following discharge from reactor, spent fuel is stored in water, which acts as an effective heat transfer medium and biological shield. The chemistry of these ponds is carefully controlled to ensure that the Magnox clad remains in a passive state. This is primarily through the maintenance of a high pH and very low anion concentration. Of particular concern is the presence of chloride ions as even very low levels may allow localised corrosion to initiate. Although extensive work has been undertaken historically considering the behaviour of Magnox clad and the acceptable storage envelopes, the challenges of ageing plant and aspirations for accelerated decommissioning give value to further understanding of the corrosion mechanisms of this material. Recently, electrochemical techniques have been employed to characterise performance in a variety of chemistries and microelectrodes have been produced which have shown characteristics of salt film corrosion at moderate chloride concentrations under polarisation. A characteristic of the electrochemical response observed during the mass transport limited (potential independent) salt film regime has been periodic transients which correspond to emission of microscopic hydrogen bubbles from the microelectrode cavity. A simple finite element multi-physics model has been employed to assist in understanding the dominant processes of corrosion product transport away from a magnesium electrode surface which is dissolving under a salt film and this shows that characteristic transients observed in electrochemical tests may be simulated with reasonable agreement by consideration of convection from laminar flow around hydrogen micro-bubbles in the pit cavity combined with aqueous diffusion in the

  2. Effect of Rare Earth on Corrosion Products and Impedance Behavior of AZ91 Magnesium Alloy Under Dry-wet Cycles

    Directory of Open Access Journals (Sweden)

    ZHAO Xi

    2017-04-01

    Full Text Available The effect of mischmetal of lanthanum and cerium on the composition and structure of the corrosion products on the surface of AZ91 Mg alloy in deicing salt solution under dry-wet cycles was investigated by scanning electron microscopy (SEM, X-ray diffraction (XRD and energy dispersive spectrometer (EDS. The results show that the corrosion products of AZ91 Mg alloy without mischmetal addition (La,Ce are mainly composed of Mg(OH2, MgO, CaCO3 and Mg6Al2CO3(OH16·4H2O; and (La,CeAlO3 can be found in the products of AZ91 with mischmetal addition, meanwhile dense layer occurs in the corrosion products. Electrochemical impedance spectroscopy (EIS measurements show that the charge transfer resistance of AZ91 alloy with mischmetal addition tested in the same dry-wet cycles is much higher than that of AZ91 alloy, the addition of mischmetal helps to reduce the dispersing effect of impedance spectroscopy, indicating that the corrosion resistance of AZ91 Mg alloy and the stability of corrosion product films can be improved by mischmetal of La and Ce.

  3. Analysis of Gamma Dose Rate Caused by Corrosion Products inside the Containment Building of Yonngwang Nuclear Power Plant Unit 3 During Shutdown Period

    Energy Technology Data Exchange (ETDEWEB)

    Ha, Wi Ho; Kim, Jae Cheon; Kim, Soon Young; Kim, Jong Kyung [Hanyang Univ., Seoul (Korea, Republic of)

    2005-07-01

    Occupational radiation exposure(ORE) of nuclear power plant(NPP) workers mainly occurs during the shutdown period. Major radioactive sources are the corrosion products released from the reactor coolant system(RCS). The corrosion products consist of circulating crud and deposited crud. Major radioactive corrosion products, {sup 58}Co and {sup 60}Co, are known to contribute approximately more than 70% of the total ORE. In this study, the corrosion products regarding cobalt were evaluated during the shutdown period, and gamma dose rates caused by them were calculated at the main working area inside the containment building of the Yonggwang NPP Unit 3.

  4. Study of the corrosion products formed on carbon steels in the tropical atmosphere of Panama

    Directory of Open Access Journals (Sweden)

    Jaén, J. A.

    2003-12-01

    Full Text Available Mössbauer spectroscopy and X-ray powder diffraction (in selected samples have been used to characterize corrosion products on carbon steels after atmospheric exposure to the tropical Panamanian locations of Panama and Colon, classified according to ISO 9223 as C3 and C5, respectively. Goethite (α-FeOOH of intermediate particle size (20-100 nm, lepidocrocite (γ-FeOOH, a spinel phase consisting of non-stoichiometric magnetite (Fe3-xO4 and/or maghemite (γ-Fe2O3 and nano-sized particles were identified in the corrosion products. The spinel phase is related to short term atmospheric exposure transforms in time to other corrosion products. The corrosion resistance increased with fraction of goethite following a saturation-type behavior.

    Se caracterizaron los productos de corrosión de aceros al carbono expuestos a las atmósferas tropicales panameñas localizadas en Panamá y Colón, mediante el uso de la espectroscopia Mössbauer y difracción de rayos-X (en muestras seleccionadas. Las atmósferas se clasifican como C3 y C5, respectivamente, de acuerdo a la norma ISO 9223. Se lograron identificar los compuestos goethita (α-FeOOH de tamaño de partícula intermedio (20-100 nm, lepidocrocita (γ-FeOOH, una fase de espinela consistente en magnetita no estequiométrica (Fe3-xO4 y/o maghemita (γ-Fe2O3, y nanopartículas. La fase de espinela se puede correlacionar con exposiciones cortas a la atmósfera, transformándose en el tiempo en otros productos de corrosión. La resistencia a la corrosión se incrementa con la cantidad de goethita siguiendo una conducta de saturación.

  5. On iron radionuclide interactions and in situ measurement of iron corrosion products

    International Nuclear Information System (INIS)

    Puranen, A.; Jonsson, M.; Cui, D.; Scheidegger, A.M.; Wersin, P.; Spahiu, K.

    2005-01-01

    Full text of publication follows: In performance assessments of hard rock repositories, it is conservatively assumed that waste canisters are breached and that the spent fuel will get into contact with groundwater after 1000 years. When the canister eventually fails to protect HLW from groundwater, dissolved radionuclides from HLW will react with iron canister materials. The reactivity will depend on the conditions in solution and at the iron-water interface. To improve our understanding on the redox chemistry at near field conditions, batch experiments are conducted by contacting polished iron foils with a synthetic groundwater solution containing 10 mM NaCl, 2 mM NaHCO 3 and 5 ppm Se(IV), Se(VI), Tc(VII) and U(VI) in a glove box filled with Ar + 0.03% CO 2 gas mixture. The reaction rates are measured by analysing Se, Tc and U concentrations by ICP-MS. Iron corrosion products formed during the reaction(s) is monitored in-situ by a Layer Raman spectrometer through an optical window. The corrosion potential of the iron foil as well as the Eh and pH values of the bulk solution are recorded continuously during the experiment. The reacted iron foil is embedded with EPOXY resin, and the cross section will be analysed by SEM-EDS and XAS. The preliminary experimental results shows that with the formation of iron green rust FeII 4 FeIII 2 (OH) 12 CO 3 on iron foil, the rates of redox reactions between iron and the negatively charged radionuclides species are increased. The observation is explained by the fact that radionuclide anionic species can be first adsorbed then reduced on the positively charged outer surface of iron green rust. The positive charge is a result of the electrical balance of the negative charges of carbonate contained between the layered iron hydroxides in the green rust. Reduced forms of radionuclides are identified in the iron corrosion products. The results suggest that the formation of iron green rust as a corrosion product on the surface of iron

  6. RAPK-7. code for calculating mass transfer and corrosion products activation in the circulation loops of water-cooled reactors

    International Nuclear Information System (INIS)

    Mikhaylov, A.V.; Moryakov, A.V.; Nikitin, A.V.

    2012-09-01

    . This mode makes it possible to simulate partial core refueling and reactor operation during several campaigns. With this done, the code will calculate the pHt and the solubility of spinel in the form of Fe 3-x Ni x O 4 . The next step is to solve the system of differential equations describing mass-transfer of non-irradiated and radioactive corrosion products. The total number of differential equations in the system can come to about a million, which leads to tougher requirements imposed on the hardware and more complicated input data setting. These difficulties are overcome with the help of the user-friendly interface and by the availability of two code versions - one designed for use at the IBM PC-compatible computer and the other for multiprocessor computer applications. While running, the code checks on the correctness of numerical computation and visualises the results as: - 3-D graphs in the axes of 'computation area - time - functional value'; - 2-D graphs (with the axes set by the user at will) and tables. (authors)

  7. Corrosion product identification and relative rates of corrosion of candidate metals in an irradiated air-steam environment

    International Nuclear Information System (INIS)

    Reed, D.T.; Swayambunathan, V.; Tani, B.S.; Van Konynenburg, R.A.

    1989-01-01

    Previously reported work by others indicates that dicopper trihydroxide nitrate, Cu 2 NO 3 (OH) 3 , forms on copper and copper alloys subjected to irradiated moist air near room temperature. We have performed experiments over a range of temperature and humidity, and have found that this species is formed at temperatures up to at least 150 degree C if low to intermediate relative humidities are present. At 150 degree C and 100% relative humidity, only Cu 2 O and CuO were observed. The relative general corrosion rates of the copper materials tested in 1-month experiments at dose rates of 0.7 and 2.0 kGy/h were Cu > 70/30 Cu--Ni > Al-bronze. High-nickel alloy 825 showed no observable corrosion. 29 refs., 4 tabs

  8. Study of MHD Corrosion and Transport of Corrosion Products of Ferritic/Martensitic Steels in the Flowing PbLi and its Application to Fusion Blanket

    Science.gov (United States)

    Saeidi, Sheida

    Two important components of a liquid breeder blanket of a fusion power reactor are the liquid breeder/coolant and the steel structure that the liquid is enclosed in. One candidate combination for such components is Lead-Lithium (PbLi) eutectic alloy and advanced Reduced Activation Ferritic/Martensitic (RAFM) steel. The research performed here is aimed at: (1) better understanding of corrosion processes in the system including RAFM steel and flowing PbLi in the presence of a strong magnetic field and (2) prediction of corrosion losses in conditions of a Dual Coolant Lead Lithium (DCLL) blanket, which is at present the key liquid metal blanket concept in the US. To do this, numerical and analytical tools have been developed and then applied to the analysis of corrosion processes. First, efforts were taken to develop a computational suite called TRANSMAG (Transport phenomena in Magnetohydrodynamic Flows) as an analysis tool for corrosion processes in the PbLi/RAFM system, including transport of corrosion products in MHD laminar and turbulent flows. The computational approach in TRANSMAG is based on simultaneous solution of flow, energy and mass transfer equations with or without a magnetic field, assuming mass transfer controlled corrosion and uniform dissolution of iron in the flowing PbLi. Then, the new computational tool was used to solve an inverse mass transfer problem where the saturation concentration of iron in PbLi was reconstructed from the experimental data resulting in the following correlation: CS = e 13.604--12975/T, where T is the temperature of PbLi in K and CS is in wppm. The new correlation for saturation concentration was then used in the analysis of corrosion processes in laminar flows in a rectangular duct in the presence of a strong transverse magnetic field. As shown in this study, the mass loss increases with the magnetic field such that the corrosion rate in the presence of a magnetic field can be a few times higher compared to purely

  9. Soluble microbial products (SMPs release in activated sludge systems: a review

    Directory of Open Access Journals (Sweden)

    Azami Hamed

    2012-12-01

    Full Text Available Abstract This review discusses the characterization, production and implications of soluble microbial products (SMPs in biological wastewater treatment. The precise definition of SMPs is open to talk about, but is currently regarded as “the pool of organic compounds that are released into solution from substrate metabolism and biomass decay”'. Some of the SMPs have been identified as humic acids, polysaccharides, proteins, amino acids, antibiotics, extracellular enzymes and structural components of cells and products of energy metabolism. They adversely affect the kinetic activity, flocculating and settling properties of sludge. This review outlines some important findings with regard to biodegradability and treatability of SMPs and also the effect of process parameters on their production. As SMPs are produced during biological treatment process, their trace amounts normally remain in the effluent that defines the highest COD removal efficiency. Their presence in effluent represents a high potential risk of toxic by-product formation during chlorine disinfection. Studies have indicated that among all wastewater post-treatment processes, the adsorption by granular activated carbon combined with biologically induced degradation is the most effective method for removal of SMPs. However, it may be concludes that the knowledge regarding SMPs is still under progress and more work is required to fully understand their contribution to the treatment process.

  10. Soluble Microbial Products (SMPs Release in Activated Sludge Systems: a Review

    Directory of Open Access Journals (Sweden)

    Hamed Azami

    2012-12-01

    Full Text Available This review discusses the characterization, production and implications of soluble microbial products (SMPs in biological wastewater treatment. The precise definition of SMPs is open to talk about, but is currently regarded as “the pool of organic compounds that are released into solution from substrate metabolism and biomass decay”'.Some of the SMPs have been identified as humic acids, olysaccharides, proteins, amino acids, antibiotics,extracellular enzymes and structural components of cells and products of energy metabolism. They adversely affect the kinetic activity, flocculating and settling properties of sludge. This review outlines some important findings with regard to biodegradability and treatability of SMPs and also the effect of process parameters on their production.As SMPs are produced during biological treatment process, their trace amounts normally remain in the effluent that defines the highest COD removal efficiency. Their presence in effluent represents a high potential risk of toxic by-product formation during chlorine disinfection. Studies have indicated that among all wastewaterpost-treatment processes, the adsorption by granular activated carbon combined with biologically induced degradation is the most effective method for removal of SMPs. However, it may be concludes that the knowledge regarding SMPs is still under progress and more work is required to fully understand their contribution to the treatment process.

  11. Corrosion in the oil industry

    Energy Technology Data Exchange (ETDEWEB)

    Brondel, D [Sedco Forex, Montrouge (France); Edwards, R [Schlumberger Well Services, Columbus, OH (United States); Hayman, A [Etudes et Productions Schlumberger, Clamart (France); Hill, D [Schlumberger Dowell, Tulsa, OK (United States); Mehta, S [Schlumberger Dowell, St. Austell (United Kingdom); Semerad, T [Mobil Oil Indonesia, Inc., Sumatra (Indonesia)

    1994-04-01

    Corrosion costs the oil industry billions of dollars a year, a fact that makes the role of the corrosion engineer an increasingly important one. Attention is paid to how corrosion affects every aspect of exploration and production, from offshore rigs to casing. Also the role of corrosion agents such as drilling and production fluids is reviewed. Methods of control and techniques to monitor corrosion are discussed, along with an explanation of the chemical causes of corrosion. 21 figs., 32 refs.

  12. Salt Solubility Products of Diprenorphine Hydrochloride, Codeine and Lidocaine Hydrochlorides and Phosphates – Novel Method of Data Analysis Not Dependent on Explicit Solubility Equations

    Directory of Open Access Journals (Sweden)

    Gergely Völgyi

    2013-12-01

    Full Text Available A novel general approach was described to address many of the challenges of salt solubility determination of drug substances, with data processing and refinement of equilibrium constants encoded in the computer program pDISOL-XTM. The new approach was illustrated by the determinations of the solubility products of diprenorphine hydrochloride, codeine hydrochloride and phosphate, lidocaine hydrochloride and phosphate at 25 oC, using a recently-optimized saturation shake-flask protocol.  The effects of different buffers (Britton-Robinson universal and Sörensen phosphate were compared. Lidocaine precipitates were characterized by X-ray powder diffraction (XRPD and polarization light microscopy. The ionic strength in the studied systems ranged from 0.25 to 4.3 M. Codeine (and possibly diprenorphine chloride were less soluble than the phosphates for pH > 2. The reverse trend was evident with lidocaine.  Diprenorphine saturated solutions showed departure from the predictions of the Henderson-Hasselbalch equation in alkaline (pH > 9 solutions, consistent with the formation of a mixed-charge anionic dimer.

  13. Performance of surrogate high-level waste glass in the presence of iron corrosion products

    International Nuclear Information System (INIS)

    Jain, V.; Pan, Y.M.

    2004-01-01

    Radionuclide release from a waste package (WP) is a series of processes that depend upon the composition and flux of groundwater contacting the waste-forms (WF); the corrosion rate of WP containers and internal components made of Alloy 22, 316L SS, 304L SS and carbon steel; the dissolution rate of high-level radioactive waste (HLW) glass and spent nuclear fuel (SNF); the solubility of radionuclides; and the retention of radionuclides in secondary mineral phases. In this study, forward reaction rate measurements were made on a surrogate HLW glass in the presence of FeCl 3 species. Results indicate that the forward reaction rate increases with an increase in the FeCl 3 concentration. The addition of FeCl 3 causes the drop in the pH due to hydrolysis of Fe 3+ ions in the solution. Results based on the radionuclide concentrations and dissolution rates for HLW glass and SNF indicate that the contribution from glass is similar to SNF at 75 deg C. (authors)

  14. X-rays diffraction characterization of corrosion products transported by secondary side of a CANDU NPP

    International Nuclear Information System (INIS)

    Dinu, A.; Tunaru, M.; Velciu, L.

    2016-01-01

    To verify the chemistry of secondary side of CANDU steam generators, Millipore filters are used to sampling from condensing extraction pump, from feed water header and blow down of steam generator. These filters retain the corrosion products as very fine particles and are used as samples in chemistry water control. X-Ray diffraction technique is the able to distinguish the different crystallographic compounds present in oxide films deposited on the Millipore filters and gives information referring to the nature of corrosion products transported in secondary side. The XRD analysis has identified the following substance in deposited layer: magnetite (Fe_3O_4), hematite (Fe_2O_3), and iron oxide hydroxide (FeOOH). By optical microscopy it was observed a brown-reddish background specific to hematite and iron oxide hydroxide, especially for filters extracted from condensing extraction pump. The black colour of crud present on filters extracted from feed water header and blow down of steam generator shows the presence of magnetite. (authors)

  15. Detection of boron in simulated corrosion products by using a laser induced breakdown spectroscopy

    International Nuclear Information System (INIS)

    Song, K.; Yeon, J-W.; Jung, S-H.; Hwang, J.; Jung, E-C.

    2010-01-01

    In nuclear power plants, many methods for detection of coolant leakage have been developed and employed for the safe operation. However, these methods have many limitations for analyzing and dealing with the corrosion products due to the high radioactivity. LIBS (Laser-induced breakdown spectroscopy) offer a remote and on-site elemental analysis including the boron in the corrosion products with no sample preparation. In this study, we investigated the feasibility of detecting boron and analyzing an elemental composition of boron-containing iron oxides with the LIBS, in order to develop a coolant leakage detection system. First, we prepared five different boron-containing iron oxides and the element ratios were determined by using ICP-AES (inductive coupled plasma-atomic emission spectrometer). After this, the laser induced emission spectra of these iron oxides were obtained by using a 266 nm Nd:YAG laser. The B/Fe ratios of the oxides were determined by comparing the intensities of the B emission peak at 249.844 nm with those of the Fe peak at 250.217 nm as an internal reference. It was confirmed that the B contents in the oxides could be analyzed over 0.1 wt% by the laser induced breakdown spectroscopic technique. (author)

  16. Factors governing particulate corrosion product adhesion to surfaces in water reactor coolant circuits

    International Nuclear Information System (INIS)

    1979-03-01

    Gravity, van der Waals, magnetic, electrical double layer and hydrodynamic forces are considered as potential contributors to the adhesion of particulate corrosion products to surfaces in water reactor coolant circuits. These forces are renewed and evaluated, and the following are amongst the conclusions drawn; adequate theories are available to estimate the forces governing corrosion product particle adhesion to surfaces in single phase flow in water reactor coolant circuits. Some uncertainty is introduced by the geometry of real particle-surface systems. The major uncertainties are due to inadequate data on the Hamaker constant and the zeta potential for the relevant materials, water chemistry and radiation chemistry at 300 0 C; van der Waals force is dominant over the effect of gravity for particles smaller than about 100 m; quite modest zeta potentials, approximately 50mV, are capable of inhibiting particle deposition throughout the size range relevant to water reactors; for surfaces exposed to typical water reactor flow conditions, particles smaller than approximately 1 m will be stable against resuspension in the absence of electrical double layer repulsion; and the magnitude of the electrical double layer repulsion for a given potential depends on whether the interaction is assumed to occur at constant potential or constant change. (author)

  17. High temperature filtration of radioactivable corrosion products in the primary circuit of PWR type reactors

    International Nuclear Information System (INIS)

    Dolle, L.

    1976-01-01

    A effective limitation to the deposition of radioactive corrosion products in the core of a reactor at power operation, is to be obtained by filtering the water of the primary circuit at a flow rate upper than 1% of the coolant flow rate. However, in view of accounting for more important release of corrosion products during the reactor start-up and also for some possible variations in the efficiency of the system, it is better that the flow rate to be treated by the cleaning circuit is stated at 5%. Filtration must be effected at the temperature of the primary circuit and preferably on each loop. To this end, the feasibility of electromagnetic filtration or filtration through a deep bed of granulated graphite has been studied. The on-loop tests effected on each filter gave efficiencies and yields respectively upper than 90% and 99% for magnetite and ferrite particles in suspension in water at 250 deg C. Such results confirm the interest lying in high temperature filtration and lead to envisage its application to reactors [fr

  18. 77 FR 25141 - Corrosion-Resistant Carbon Steel Flat Products From Germany and South Korea: Extension of Time...

    Science.gov (United States)

    2012-04-27

    ...-Resistant Carbon Steel Flat Products From Germany and South Korea: Extension of Time Limits for Preliminary...) orders on corrosion-resistant carbon steel flat products (CORE) from Germany and South Korea (Korea... from Germany and South Korea: Adequacy Redetermination Memorandum,'' (April 20, 2012). The preliminary...

  19. Enhancing production and cytotoxic activity of polymeric soluble FasL-based chimeric proteins by concomitant expression of soluble FasL.

    Directory of Open Access Journals (Sweden)

    Aurore Morello

    Full Text Available Membrane FasL is the natural trigger of Fas-mediated apoptosis. A soluble homotrimeric counterpart (sFasL also exists which is very weakly active, and needs oligomerization beyond its trimeric state to induce apoptosis. We recently generated a soluble FasL chimera by fusing the immunoglobulin-like domain of the leukemia inhibitory factor receptor gp190 to the extracellular region of human FasL, which enabled spontaneous dodecameric homotypic polymerization of FasL. This polymeric soluble human FasL (pFasL displayed anti-tumoral activity in vitro and in vivo without systemic cytotoxicity in mouse. In the present work, we focused on the improvement of pFasL, with two complementary objectives. First, we developed more complex pFasL-based chimeras that contained a cell-targeting module. Secondly, we attempted to improve the production and/or the specific activity of pFasL and of the cell-targeting chimeras. We designed two chimeras by fusing to pFasL the extracellular portions of the HLA-A2 molecule or of a human gamma-delta TCR, and analyzed the consequences of co-expressing these molecules or pFasL together with sFasL on their heterotopic cell production. This strategy significantly enhanced the production of pFasL and of the two chimeras, as well as the cytotoxic activity of the two chimeras but not of pFasL. These results provide the proof of concept for an optimization of FasL-based chimeric proteins for a therapeutic use.

  20. The Kinetics of Fission Products Release from Microfuel Taking into Account the Trapped Fraction and Limited Solubility Effects

    International Nuclear Information System (INIS)

    Ivanov, A.S.; Rusinkevich, A.A.

    2014-01-01

    In this paper the effect of the oxygen getter on fission products release from the coated particle was studied by the “FP Kinetics” code. Trapped fraction and limited solubility effects taken into consideration. It was shown that these effects have a significant impact on the concentration profile and integral release of fission products. (author)

  1. Design of containment system of nuclear fuel attacked by corrosion with leaking fission products

    International Nuclear Information System (INIS)

    Poblete Maturana, Tomas

    2015-01-01

    The following report presents the design of an innovative confinement system for the nuclear fuel attacked by corrosion, with leakage of fission products to be used in the RECH-1 nuclear experimental reactor of the Chilean Nuclear Energy Commission, is currently within the framework of the international nuclear waste management program developed by the member countries of the IAEA, including Chile. The main objective of this project is the development of a system that is capable of containing, in the smallest possible volume, the fission products that are released to the reactor coolant medium from the nuclear fuel that are attacked by corrosion. Among the tasks carried out for the development of the project are: the compilation of the necessary bibliography for the selection of the most suitable technology for the retention of the fission products, the calculation of the most important parameters to ensure that the system will operate within ranges that do not compromise the radiological safety, and the design of the hydraulic circuit of the system. The results obtained from the calculations showed that the fuel element confinement system is stable from a thermal point of view since the refrigerant does not under any circumstances reach the saturation temperature and, in addition, from a hydraulic point of view, since the rate at which the refrigerant flows through the hydraulic circuit is low enough so that the deformation of the fuel plates forming the nuclear fuel does not occur. The most appropriate technology for the extraction of fission products according to the literature consulted is by ion exchange. The calculations developed showed that with a very small volume of resins, it is possible to capture all of the non-volatile fission products of a nuclear fuel

  2. Identification of microorganisms associated with corrosion of offshore oil production systems

    Science.gov (United States)

    Sørensen, Ketil; Grigoryan, Aleksandr; Holmkvist, Lars; Skovhus, Torben; Thomsen, Uffe; Lundgaard, Thomas

    2010-05-01

    Microbiologically influenced corrosion (MIC) poses a major challenge to oil producers and distributors. The annual cost associated with MIC-related pipeline failures and general maintenance and surveillance of installations amounts to several billion dollar in the oil production sector alone. Hence, large efforts are undertaken by some producers to control and monitor microbial growth in pipelines and other installations, and extensive surveillance programs are carried out in order to detect and quantify potential MIC-promoting microorganisms. Traditionally, efforts to mitigate and survey microbial growth in oil production systems have focused on sulfate-reducing Bacteria (SRB), and microorganisms have usually been enumerated by the culture-dependent MPN (most probable number) -technique. Culture-independent molecular tools yielding much more detailed information about the microbial communities have now been implemented as a reliable tool for routine surveillance of oil production systems in the North Sea. This has resulted in new and hitherto unattainable information regarding the distribution of different microorganisms in hot reservoirs and associated oil production systems. This presentation will provide a review of recent insights regarding thermophilic microbial communities and their implication for steel corrosion in offshore oil production systems. Data collected from solids and biofilms in different corroded pipelines and tubes indicate that in addition to SRB, other groups such as methanogens and sulfate-reducing Archaea (SRA) are also involved in MIC. In the hot parts of the system where the temperature approaches 80 ⁰C, SRA closely related to Archaeoglobus fulgidus outnumber SRB by several orders of magnitude. Methanogens affiliated with the genus Methanothermococcus were shown to completely dominate the microbial community at the metal surface in a sample of highly corroded piping. Thus, the microbial communities associated with MIC appear to be more

  3. The effect of nickel as a nickel chromium restoration corrosion product on gingival fibroblast through analysis of BCl-2

    Directory of Open Access Journals (Sweden)

    FX Ady Soesetijo

    2012-12-01

    Full Text Available Background: Restoration of NiCr may undergo corrosion process in artificial saliva. Corrosion product is soluble Ni substances in salivary electrolytes. Ni2+ may freely enter the cells through passive transport DMT-1. Ni2+ in the cell causes initiation of the ROS formation,which subsequently can conduct the redoxs reactions leading to DNA damage. The damage DNA affects the genetic expression, especially bcl-2, and even triggers apoptosis. Purpose: The aim of this study was to reveal the mechanism of Ni toxicity as a corrosion product of NiCr restoration on gingival fibroblasts through expression analysis of Bcl-2. Methods: Cells with a density of 105 planted on each coverslip in 72 wells to the treatment group and 24 wells to the control group (24 hours incubation. In the treatment groups, each well exposed with 20 μL artificial saliva containing Ni concentration results immerse each restoration, whereas the control group was exposed to 20 μL artificial saliva (incubation 1, 3, and 7 days. The data collected were subsequently analyzed using two-ways ANOVA, followed by one-way ANOVA. Comparing between experimental groups after one-way ANOVA was conducted using Fisher’s LSD. Whereas, the calculation and documentation of Bcl-2 expression was performed camera of Olympus Microscope BX-50 Japan. Results: Statistical analysis of two-ways ANOVA showed the presence of interaction between the increasing Ni concentration and exposure duration on the expression of Bcl-2 gingival fibroblasts (p=0.021

  4. Modeling the formation of soluble microbial products (SMP in drinking water biofiltration

    Directory of Open Access Journals (Sweden)

    Yu Xin

    2008-09-01

    Full Text Available Both a theoretical and an empirical model were developed for predicting the formation of soluble microbial products (SMP during drinking water biofiltration. Four pilot-scale biofilters with ceramsite as the medium were fed with different acetate loadings for the determination of SMP formation. Using numerically simulated and measured parameters, the theoretical model was developed according to the substrate and biomass balance. The results of this model matched the measured data better for higher SMP formation but did not fit well when SMP formation was lower. In order to better simulate the reality and overcome the difficulties of measuring the kinetic parameters, a simpler empirical model was also developed. In this model, SMP formation was expressed as a function of fed organic loadings and the depth of the medium, and a much better fit was obtained.

  5. Effect of the ion force on the hydrolysis constants and of the solubility product of Europium

    International Nuclear Information System (INIS)

    Jimenez R, M.; Ramirez G, J.J.; Solache R, M.; Rojas H, A.

    2003-01-01

    A study on the behavior of the first hydrolysis constant β Eu,H l-0 and the constant of the solubility product Kps of the europium in front of the changes of the ion force: 0. 02 M, 0.1 M, 0.7M, 2M, 3M and 4M of sodium perchlorate, at 303 K. Experimentally the potentiometry and also radioactivity measures its were used. The specific interaction of ions theory (SIT) of Bronsted-Guggenheim-Scatchard allows the extrapolation of the values to infinite dilution and the results were: log β Eu,H l-0 = -7 36 and log K sp l-0 = -24. 68. A discussion of the group of results with the data of the literature is presented. (Author)

  6. Corrosion product balances for the Ringhals PWR plants based on extensive fuel crud and water chemistry measurements

    International Nuclear Information System (INIS)

    Lundgren, K.; Wikmark, G.; Bengtsson, B.

    2010-01-01

    The corrosion product balance in a PWR plant is of great importance for the fuel performance as well as for the radiation field buildup. This balance is of special concern in connection to steam generator replacement (SGR) and power uprate projects. The Ringhals PWRs are all of Westinghouse design. Two of the plants have performed Steam Generator Replacement (SGR) to I-690 SG tubes and such a replacement is being planned in the third and last unit in 2011. Two of the units are in different phases of power uprate projects. The plants are all on 10-14-months cycles operating with medium to high fuel duty. Water chemistry is controlled by a pH300 in the range ∼7.2 to 7.4 from beginning of cycle to end of cycle (BOC-EOC) in the units with new SGs while kept at a coordinated pH of 7.2 in the one still using I-600. The maximum Li content has recently been increased to about 4.5 to 5 ppm in all units. In order to be able to improve the assessment of corrosion product balances in the plants, comprehensive fuel crud measurements were performed in 2007. Improved integrated reactor water sampling techniques have also been introduced in order to make accurate mass balances possible. The corrosion products covered in the study are the main constituents, Ni, Fe and Cr in the primary circuit Inconel and stainless steel, together with Co. The activated corrosion products, Co-58, Co-60, Cr-51, Fe-59 and Mn-54, are all mainly produced through neutron irradiation of the covered corrosion products. The main results of the corrosion product balances are presented. Observed differences between the plants, indicating significant impact of pH control and SG tube materials, are presented and discussed. The importance of accurate sampling techniques is especially addressed in this paper. (author)

  7. Kinetics of corrosion inhibition of aluminum in acidic media by water-soluble natural polymeric chondroitin-4-sulfate as anionic polyelectrolyte inhibitor.

    Science.gov (United States)

    Hassan, Refat M; Ibrahim, Samia M; Takagi, Hideo D; Sayed, Suzan A

    2018-07-15

    Corrosion inhibition of aluminum (Al) in hydrochloric acid by anionic polyelectrolyte chondroitin-4-sulfate (CS) polysaccharide has been studied using both gasometrical and weight-loss techniques. The results drawn from these two techniques are comparable and exhibit negligible differences. The inhibition efficiency was found to increase with increasing the inhibitor concentration and decreased with increasing temperature. The inhibition action of CS on Al metal surface was found to obey both of Langmuir and Freundlich isotherms. The factors affecting the corrosion rates such as the concentration and geometrical structure of the inhibitor, concentration of the corrosive medium, and the temperature were examined. The kinetic parameters were evaluated and a suitable corrosion mechanism consistent with the results obtained is discussed. Copyright © 2018. Published by Elsevier Ltd.

  8. Dual effect of soluble materials in pretreated lignocellulose on simultaneous saccharification and co-fermentation process for the bioethanol production.

    Science.gov (United States)

    Qin, Lei; Li, Xia; Liu, Li; Zhu, Jia-Qing; Guan, Qi-Man; Zhang, Man-Tong; Li, Wen-Chao; Li, Bing-Zhi; Yuan, Ying-Jin

    2017-01-01

    In this study, wash liquors isolated from ethylenediamine and dry dilute acid pretreated corn stover were used to evaluate the effect of soluble materials in pretreated biomass on simultaneous saccharification and co-fermentation (SSCF) for ethanol production, respectively. Both of the wash liquors had different impacts on enzymatic hydrolysis and fermentation. Enzymatic conversions of glucan and xylan monotonically decreased as wash liquor concentration increased. Whereas, with low wash liquor concentrations, xylose consumption rate, cell viability and ethanol yield were maximally stimulated in fermentation without nutrient supplementary. Soluble lignins were found as the key composition which promoted sugars utilization and cell viability without nutrient supplementary. The dual effects of soluble materials on enzymatic hydrolysis and fermentation resulted in the reduction of ethanol yield as soluble materials increased in SSCF. Copyright © 2016 Elsevier Ltd. All rights reserved.

  9. Impact of feed carbohydrates and nitrogen source on the production of soluble microbial products (SMPs) in anaerobic digestion.

    Science.gov (United States)

    Le, Chencheng; Stuckey, David C

    2017-10-01

    Six stirred fill-and-draw batch reactors with a range of carbohydrate feeds (glucose, fructose and sucrose), and nitrogen sources (NH 4 Cl, urea) at various concentrations were used to investigate the effect of feed composition on the production of soluble microbial products (SMPs) during anaerobic digestion (AD). To gain greater insights into the SMPs produced, the composition of various fractions was analyzed, while the low molecular weight (MW) SMPs generated with different feeds and nutrients were collected and chemically analyzed using GC-MS. Other organic solutes such as free amino acids were determined using HPLC, and this level of chemical analysis has never been carried out in past work because of analytical limitations. It was found that the presence of ammonium salts rather than urea at 200 mg/L stimulated the production of not only volatile fatty acids, but also SMPs of different MW fractions, and reduced the production of biogas significantly. The study also revealed that the type of SMP that dominates in a particular system depends on the chemical characteristics of the feed, and this insight has implications on the composition of the effluent from anaerobic digesters (and their potential chlorination by-products), and membrane fouling in membrane bioreactors. Copyright © 2017 Elsevier Ltd. All rights reserved.

  10. Effect of corrosion product layer on SCC susceptibility of copper containing type 304 stainless steel in 1 M H2SO4

    International Nuclear Information System (INIS)

    Asawa, M.; Devasenapathi, A.; Fujisawa, M.

    2004-01-01

    The effect of surface corrosion product layer on the stress corrosion cracking (SCC) susceptibility of type 304 stainless steel with Cu was studied in 1 kmol/m 3 (1 M) sulfuric acid at 353 K temperature. Studies based on the intermittent removal of surface corrosion product layer indicated that the surface film governs the SCC behavior of the alloy by accelerating both the crack initiation and propagation stages. The electrochemical impedance and polarization studies showed the surface layer to be promoting SCC initiation by lowering the uniform corrosion rate and the propagation by shifting the surface corrosion potential to a more noble direction. The elemental analysis of the corrosion product both by the energy dispersive X-ray (EDX) spectroscopy and by X-ray diffraction (XRD) analysis along with the thermodynamic calculations showed the layer to be constituted mainly of metallic copper (Cu) and the mono-hydrated iron sulfate which acts as cathode promoting SCC

  11. Characterization of soluble microbial products and their fouling impacts in membrane bioreactors

    KAUST Repository

    Jiang, Tao; Kennedy, Maria Dolores; Schepper, Veerle D.; Nam, Seongnam; Nopens, Ingmar; Vanrolleghem, Peter A.; Amy, Gary L.

    2010-01-01

    Membrane bioreactor (MBR) fouling is not only influenced by the soluble microbial products (SMP) concentration but by their characteristics. Experiments of separate producing biomass associated products (BAP) and utilization associated products (UAP) allowed the separation of BAP and UAP effects from sludge water (SW). Thus, filtration of individual SMP components and further characterization becomes possible. Unstirred cell filtration was used to study fouling mechanisms and liquid chromatography-organic carbon detection (LC-OCD) and fluorescence excitation-emission matrix (EEM) were used to characterize the foulant. Generally, the SMP exhibiting characteristics of higher molecular weight, greater hydrophilicity and a more reduced state showed a higher retention percentage. However, the higher retention does not always yield higher fouling effects. The UAP filtration showed the highest specific cake resistance and pore blocking resistance attributed to their higher percentage of low molecular weight molecules, although their retention percentage was lower than the SW and BAP filtration. The UAP produced in the cell proliferation phase appeared to have the highest fouling potential. © 2010 American Chemical Society.

  12. Characterization of soluble microbial products and their fouling impacts in membrane bioreactors

    KAUST Repository

    Jiang, Tao

    2010-09-01

    Membrane bioreactor (MBR) fouling is not only influenced by the soluble microbial products (SMP) concentration but by their characteristics. Experiments of separate producing biomass associated products (BAP) and utilization associated products (UAP) allowed the separation of BAP and UAP effects from sludge water (SW). Thus, filtration of individual SMP components and further characterization becomes possible. Unstirred cell filtration was used to study fouling mechanisms and liquid chromatography-organic carbon detection (LC-OCD) and fluorescence excitation-emission matrix (EEM) were used to characterize the foulant. Generally, the SMP exhibiting characteristics of higher molecular weight, greater hydrophilicity and a more reduced state showed a higher retention percentage. However, the higher retention does not always yield higher fouling effects. The UAP filtration showed the highest specific cake resistance and pore blocking resistance attributed to their higher percentage of low molecular weight molecules, although their retention percentage was lower than the SW and BAP filtration. The UAP produced in the cell proliferation phase appeared to have the highest fouling potential. © 2010 American Chemical Society.

  13. Corrosion of stainless and carbon steels in molten mixtures of industrial nitrates

    Energy Technology Data Exchange (ETDEWEB)

    Goods, S.H.; Bradshaw, R.W. [Sandia National Labs., Livermore, CA (United States); Prairie, M.R.; Chavez, J.M. [Sandia National Labs., Albuquerque, NM (United States)

    1994-03-01

    Corrosion behavior of two stainless steels and carbon steel in mixtures of NaNO{sub 3} and KNO{sub 3} was evaluated to determine if impurities found in commodity grades of alkali nitrates aggravate corrosivity as applicable to an advanced solar thermal energy system. Corrosion tests were conducted for 7000 hours with Types 304 and 316 stainless steels at 570C and A36 carbon steel at 316C in seven mixtures of NaNO{sub 3} and KNO{sub 3} containing variations in impurity concentrations. Corrosion tests were also conducted in a ternary mixture of NaNO{sub 3}, KNO{sub 3}, and Ca(NO{sub 3}){sub 2}. Corrosion rates were determined by descaled weight losses while oxidation products were examined by scanning electron microscopy, electron microprobe analysis, and X-ray diffraction. The nitrate mixtures were periodically analyzed for changes in impurity concentrations and for soluble corrosion products.

  14. Measurement of fuel corrosion products using planar laser-induced fluorescence

    International Nuclear Information System (INIS)

    Wantuck, P.J.; Sappey, A.D.; Butt, D.P.

    1993-01-01

    Characterizing the corrosion behavior of nuclear fuel material in a high-temperature hydrogen environment is critical for ascertaining the operational performance of proposed nuclear thermal propulsion (NTP) concepts. In this paper, we describe an experimental study undertaken to develop and test non-intrusive, laser-based diagnostics for ultimately measuring the distribution of key gas-phase corrosion products expected to evolve during the exposure of NTP fuel to hydrogen. A laser ablation technique is used to produce high temperature, vapor plumes from uranium-free zirconium carbide (ZrC) and niobium carbide (NbC) forms for probing by various optical diagnostics including planar laser-induced fluorescence (PLIF). We discuss the laser ablation technique, results of plume emission measurements, and we describe both the actual and proposed planar LIF schemes for imaging constituents of the ablated ZrC and NbC plumes. Envisioned testing of the laser technique in rf-heated, high temperature gas streams is also discussed

  15. Deposition of corrosion products from dowels on human dental root surfaces measured with proton microprobe technique

    International Nuclear Information System (INIS)

    Brune, D.; Brunell, G.; Lindh, U.

    1982-01-01

    Distribution of copper, mercury and zinc on human teeth root surfaces adjacent to dowels of gold alloy or brass as well as dowels of brass in conjunction with an amalgam crown has been measured with a proton microprobe using PIXE techniques. Upper limits of the contents of gold and silver on the root surfaces were established. Pronounced concentration profiles of copper and zinc were observed on the root surfaces of teeth prepared with dowels of brass. The dowel of gold alloy revealed only zinc deposition. The major part of copper on the root surfaces is assumed to arise from corrosion of the dowels, and has been transported to the surface by diffusion through the dential tubuli. Zinc in the volume analysed is a constituent of dentin tissue as well as a corrosion product of the brass dowel. Part of the zinc level could also be ascribed to erosion of the zinc phosphate cement matrix. The volumes analysed were (25 x 25 x 25)μm 3 . The levels of copper, mercury and zinc on the tooth root surfaces attained values up to about 200, 20 and 600 ppm, respectively. (orig.)

  16. Deposition of corrosion products from dowels on human dental root surfaces measured with proton microprobe technique

    Science.gov (United States)

    Brune, D.; Brunell, G.; Lindh, U.

    1982-06-01

    Distribution of copper, mercury and zinc on human teeth root surfaces adjacent to dowels of gold alloy or brass as well as dowels of brass in conjunction with an amalgam crown has been measured with a proton microprobe using PIXE techniques. Upper limits of the contents of gold and silver on the root surfaces were established. Pronounced concentration profiles of copper and zinc were observed on the root surfaces of teeth prepared with dowels of brass. The dowel of gold alloy revealed only zinc deposition. The major part of copper on the root surfaces is assumed to arise from corrosion of the dowels, and has been transported to the surface by diffusion through the dential tubuli. Zinc in the volume analysed is a constituent of dentin tissue as well as a corrosion product of the brass dowel. Part of the zinc level could also be ascribed to erosion of the zinc phosphate cement matrix. The volumes analysed were (25×25×25)μm 3. The levels of copper, mercury and zinc on the tooth root surfaces attained values up to about 200, 20 and 600 ppm, respectively.

  17. corrosion problems and their relationship with the environment in the Colombian productive system

    International Nuclear Information System (INIS)

    Arroyave P, Carlos E; Herrera B, Francisco J; Delgado L, Juan; Cuervo T, Joaquin

    1999-01-01

    As a part of a broad study on the corrosion problems in the Colombian industry, it was included an assessment of the effect of the main corrosive environments (atmosphere, soil, salad and drinking water, and chemicals), on materials stability. On the other hand, the impact of the corrosion processes on the environmental constituents (live species, atmosphere, soil, materials, and water) was also assessed. Main conclusions are: Atmosphere is the more extensively corrosive environment, and, all the environmental constituents are affected by corrosion without significant differences

  18. Hydrogen and methane production from condensed molasses fermentation soluble by a two-stage anaerobic process

    Energy Technology Data Exchange (ETDEWEB)

    Lin, Chiu-Yue; Liang, You-Chyuan; Lay, Chyi-How [Feng Chia Univ., Taichung, Taiwan (China). Dept. of Environmental Engineering and Science; Chen, Chin-Chao [Chungchou Institute of Technology, Taiwan (China). Environmental Resources Lab.; Chang, Feng-Yuan [Feng Chia Univ., Taichung, Taiwan (China). Research Center for Energy and Resources

    2010-07-01

    The treatment of condensed molasses fermentation soluble (CMS) is a troublesome problem for glutamate manufacturing factory. However, CMS contains high carbohydrate and nutrient contents and is an attractive and commercially potential feedstock for bioenergy production. The aim of this paper is to produce hydrogen and methane by two-stage anaerobic fermentation process. The fermentative hydrogen production from CMS was conducted in a continuously-stirred tank bioreactor (working volume 4 L) which was operated at a hydraulic retention time (HRT) of 8 h, organic loading rate (OLR) of 120 kg COD/m{sup 3}-d, temperature of 35 C, pH 5.5 and sewage sludge as seed. The anaerobic methane production was conducted in an up-flow bioreactor (working volume 11 L) which was operated at a HRT of 24 -60 hrs, OLR of 4.0-10 kg COD/m{sup 3}-d, temperature of 35 C, pH 7.0 with using anaerobic granule sludge from fructose manufacturing factory as the seed and the effluent from hydrogen production process as the substrate. These two reactors have been operated successfully for more than 400 days. The steady-state hydrogen content, hydrogen production rate and hydrogen production yield in the hydrogen fermentation system were 37%, 169 mmol-H{sub 2}/L-d and 93 mmol-H{sub 2}/g carbohydrate{sub removed}, respectively. In the methane fermentation system, the peak methane content and methane production rate were 66.5 and 86.8 mmol-CH{sub 4}/L-d with methane production yield of 189.3 mmol-CH{sub 4}/g COD{sub removed} at an OLR 10 kg/m{sup 3}-d. The energy production rate was used to elucidate the energy efficiency for this two-stage process. The total energy production rate of 133.3 kJ/L/d was obtained with 5.5 kJ/L/d from hydrogen fermentation and 127.8 kJ/L/d from methane fermentation. (orig.)

  19. Corrosion product deposition on fuel element surfaces of a boiling water reactor

    International Nuclear Information System (INIS)

    Orlov, A.

    2011-01-01

    Over the last decade the problem of corrosion products deposition on light water reactor fuel elements has been extensively investigated in relation to the possibility of failures caused by them. The goal of the present study is to understand in a quantitative way the formation of such kind of deposits and to analytically understand the mechanism of formation and deposition with help of the quasi-steady state concentrations of a number of 3d metals in reactor water. Recent investigations on the complex corrosion product deposits on a Boiling Water Reactor (BWR) fuel cladding have shown that the observed layer locally presents unexpected magnetic properties. The buildup of magnetic corrosion product deposits (crud) on the fuel cladding of the BWR, Kernkraftwerk Leibstadt (KKL) Switzerland has hampered the Eddy-current based measurements of ZrO 2 layer thickness. The magnetic behavior of this layer and its axial variation on BWR fuel cladding is of interest with respect to non-destructive cladding characterization. Consequently, a cladding from a BWR was cut at elevations of 810 mm, where the layer was observed to be magnetic, and of 1810 mm where it was less magnetic. The samples were subsequently analyzed using electron probe microanalysis (EPMA), magnetic analysis and X-ray techniques (μXRF, μXRD and μXAFS). Both EPMA and μXRF have shown that the observed corrosion deposit layer which is situated on the Zircaloy corrosion layer consists mostly of 3-d elements’ oxides (Fe, Zn, Ni and Mn). The distribution of these elements within the investigated layer is rather complex and not homogeneous. The main components identified by 2D μXRD mapping inside the layer were hematite and spinel phases with the common formula (M x Fe y )[M (1-x) Fe (2-y) ]O 4 , where M = Zn, Ni, Mn. With μXRD it was clearly shown that the cell parameter of analyzed spinel is different from the one of the pure endmembers (ZnFe 2 O 4 , NiFe 2 O 4 and MnFe 2 O 4 ) proving the existence of

  20. Study of the corrosion products in the primary system of PWR plants as the source of radiation fields build-up

    International Nuclear Information System (INIS)

    Brabant, R. van; Regge, P. de.

    1982-01-01

    In the first part the behaviour of the corrosion products in the primary system of PWR plants is depicted on the basis of a literature review of the field. Water chemistry, corrosion processes and activation of corrosion products are the main topics. In the second part the results of the characterization of corrosion particles in the primary coolant circuit of the Doel 1 and 2 reactors are described, during steady state operation and transient phases. In the third part the possibilities for radiation control at nuclear power plants are outlined. The filtration possibilities for the reactor coolant are explored in detail. (author)

  1. Galvanic corrosion between carbon steel 1018 and Alloy 600 in crevice with boric acid solution

    International Nuclear Information System (INIS)

    Kim, Dong Jin; Kim, Hong Pyo; Kim, Joung Soo; Machonald, Digby D.

    2005-01-01

    This work dealt with the evaluation of galvanic corrosion rate in a corrosion cell having annular gap of 0.5 mm between carbon steel 1018 and alloy 600 as a function of temperature and boron concentration. Temperature and boron concentration were ranged from 110 to 300 .deg. C and 2000∼10000 ppm, respectively. After the operating temperature of the corrosion cell where the electrolyte was injected was attained at setting temperature, galvanic coupling was made and at the same time galvanic current was measured. The galvanic corrosion rate decreased with time, which was described by corrosion product such as protective film as well as boric acid deposit formed on the carbon steel with time. From the galvanic current obtained as a function of temperature and boron concentration, it was found that the galvanic corrosion rate decreased with temperature while the corrosion rate increased with boron concentration. The experimental results obtained from galvanic corrosion measurement were explained by adhesive property of corrosion product such as protective film, boric acid deposit formed on the carbon steel wall and dehydration of boric acid to be slightly soluble boric acid phase. Moreover the galvanic corrosion rate calculated using initial galvanic coupling current instead of steady state coupling current was remarked, which could give us relatively closer galvanic corrosion rate to real pressurized water reactor

  2. Measurement and evaluation of radioactive corrosion product behaviour in primary sodium circuits of JOYO

    International Nuclear Information System (INIS)

    Ito, K.; Iizawa, K.; Takahashi, K.; Zulquarnain, M.A.; Suzuki, S.; Kinjo, K.

    1992-01-01

    In the experimental fast reactor JOYO, the radioactive corrosion product (CP) measurement has been conducted in the primary sodium circuits during each annual inspection. The measured data has been analyzed by the computer code 'PSYCHE', which has been developed by PNC. Main results obtained from the measurements and/or calculations are as follows; (1) The dominant CP nuclide is 54 Mn followed by 60 Co and 58 Co. (2) Average surface gamma dose rate around the primary piping system at the 8th annual inspection is 0.96 mSv/h. The increasing rate of this value is 0.25 (mSv/h)/EFPY. (3) The calculated deposition densities of 54 Mn and 60 Co agree with measured ones within factor of 0.7 ∼ 1.7. (author)

  3. Transport of radioactive corrosion products in primary system of sodium-cooled fast breeder reactor 'MONJU'

    International Nuclear Information System (INIS)

    Matuo, Youichirou; Hasegawa, Masanori; Maegawa, Yoshiharu; Miyahara, Shinya

    2011-01-01

    Radioactive corrosion products (CP) are primary cause of personal radiation exposure during maintenance work at FBR plants with no breached fuel. The PSYCHE code has been developed based on the Solution-Precipitation model for analysis of CP transfer behavior. We predicted and analyzed the CP solution and precipitation behavior of MONJU to evaluate the applicability of the PSYCHE code to MONJU, using the parameters verified in the calculations for JOYO. From the calculation result pertaining to the MONJU system, distribution of 54 Mn deposited in the primary cooling system over 20 years of operation is predicted to be approximately 7 times larger than that of 60 Co. In particular, predictions show a notable tendency for 54 Mn precipitation to be distributed in the primary pump and cold-leg. The calculated distribution of 54 Mn and 60 Co in the primary cooling system of MONJU agreed with tendencies of measured distribution of JOYO. (author)

  4. Effect of fission product interactions on the corrosion and mechanical properties of HTGR alloys

    International Nuclear Information System (INIS)

    Aronson, S.; Chow, J.G.Y.; Soo, P.; Friedlander, M.

    1978-01-01

    Preliminary experiments have been carried out to determine how fission product interactions may influence the mechanical integrity of reference HTGR structural metals. In this work Type 304 stainless steel, Incoloy 800 and Hastelloy X were heated to 550 to 650 0 C in the presence of CsI. It was found that no corrosion of the alloys occurred unless air or oxygen was also present. A mechanism for the observed behavior is proposed. A description is also given of some long term exposures of HTGR materials to more prototypic, low concentrations of I 2 , Te 2 and CsI in the presence of low partial pressures of O 2 . These samples are scheduled for mechanical bend tests after exposure to determine the degree of embrittlement

  5. Prevention of Acid Mine Drainage Through Complexation of Ferric Iron by Soluble Microbial Growth Products

    Science.gov (United States)

    Pandey, S.; Yacob, T. W.; Silverstein, J.; Rajaram, H.; Minchow, K.; Basta, J.

    2011-12-01

    Acid mine drainage (AMD) is a widespread environmental problem with deleterious impacts on water quality in streams and watersheds. AMD is generated largely by the oxidation of metal sulfides (i.e. pyrite) by ferric iron. This abiotic reaction is catalyzed by conversion of ferrous to ferric iron by iron and sulfur oxidizing microorganisms. Biostimulation is currently being investigated as an attempt to inhibit the oxidation of pyrite and growth of iron oxidizing bacteria through addition of organic carbon. This may stimulate growth of indigenous communities of acidophilic heterotrophic bacteria to compete for oxygen. The goal of this research is to investigate a secondary mechanism associated with carbon addition: complexation of free Fe(III) by soluble microbial growth products (SMPs) produced by microorganisms growing in waste rock. Exploratory research at the laboratory scale examined the effect of soluble microbial products (SMPs) on the kinetics of oxidation of pure pyrite during shaker flask experiments. The results confirmed a decrease in the rate of pyrite oxidation that was dependent upon the concentration of SMPs in solution. We are using these data to verify results from a pyrite oxidation model that accounts for SMPs. This reactor model involves differential-algebraic equations incorporating total component mass balances and mass action laws for equilibrium reactions. Species concentrations determined in each time step are applied to abiotic pyrite oxidation rate expressions from the literature to determine the evolution of total component concentrations. The model was embedded in a parameter estimation algorithm to determine the reactive surface area of pyrite in an abiotic control experiment, yielding an optimized value of 0.0037 m2. The optimized model exhibited similar behavior to the experiment for this case; the root mean squared of residuals for Fe(III) was calculated to be 7.58 x 10-4 M, which is several orders of magnitude less than the actual

  6. Corrosion/96 conference papers

    International Nuclear Information System (INIS)

    Anon.

    1996-01-01

    Topics covered by this conference include: cathodic protection in natural waters; cleaning and repassivation of building HVAC systems; worldwide opportunities in flue gas desulfurization; advancements in materials technology for use in oil and gas service; fossil fuel combustion and conversion; technology of corrosion inhibitors; computers in corrosion control--modeling and information processing; recent experiences and advances of austenitic alloys; managing corrosion with plastics; corrosion measurement technology; corrosion inhibitors for concrete; refining industry; advances in corrosion control for rail and tank trailer equipment; CO 2 corrosion--mechanisms and control; microbiologically influenced corrosion; corrosion in nuclear systems; role of corrosion in boiler failures; effects of water reuse on monitoring and control technology in cooling water applications; methods and mechanisms of scale and deposit control; corrosion detection in petroleum production lines; underground corrosion control; environmental cracking--relating laboratory results and field behavior; corrosion control in reinforced concrete structures; corrosion and its control in aerospace and military hardware; injection and process addition facilities; progress reports on the results of reinspection of deaerators inspected or repaired per RP0590 criteria; near 100% volume solids coating technology and application methods; materials performance in high temperature environments containing halides; impact of toxicity studies on use of corrosion/scale inhibitors; mineral scale deposit control in oilfield related operations; corrosion in gas treating; marine corrosion; cold climate corrosion; corrosion in the pulp and paper industry; gaseous chlorine alternatives in cooling water systems; practical applications of ozone in recirculating cooling water systems; and water reuse in industry. Over 400 papers from this conference have been processed separately for inclusion on the data base

  7. 77 FR 67395 - Corrosion-Resistant Carbon Steel Flat Products From Germany and Korea; Revised Schedule for the...

    Science.gov (United States)

    2012-11-09

    ... INTERNATIONAL TRADE COMMISSION [Investigation Nos. 701-TA-350 and 731-TA-616 and 618 (Third Review)] Corrosion-Resistant Carbon Steel Flat Products From Germany and Korea; Revised Schedule for the Subject Reviews AGENCY: United States International Trade Commission. ACTION: Notice. DATES: Effective Date...

  8. Characterisation of the corrosion products of non-irradiated material test reactors fuel elements (MTR-FE)

    Energy Technology Data Exchange (ETDEWEB)

    Mazeina, L.; Curtius, H.; Fachinger, J. [Inst. for Safety Research and Reactor Technology, Research Centre Juelich (Germany)

    2003-07-01

    In a high concentrated Mg-rich brine a non-irradiated MTR-FE corroded. The formed corrosion products consists of an amorphous part and of hydrotalcites, which were identified as Mg-Al-hydrotalcites with chloride anions in the interlayer. (orig.)

  9. A process for the production of a scale-proof and corrosion-resistant coating on graphite and carbon bodies

    Science.gov (United States)

    Fitzer, E.

    1981-01-01

    A process for the production of a corrosion resistant coating on graphite and carbon bodies is described. The carbon or graphite body is coated or impregnated with titanium silicide under the addition of a metal containing wetting agent in a nitrogen free atmosphere, so that a tight coating is formed.

  10. Synchrotron based x-ray fluorescence microscopy confirms copper in the corrosion products of metals in contact with treated wood

    Science.gov (United States)

    Samuel L. Zelinka; Joseph E. Jakes; Grant T. Kirker; David Vine; Stefan Vogt

    2017-01-01

    Copper based waterborne wood preservatives are frequently used to extend the service life of wood products when subjected to frequent moisture exposure. While these copper based treatments protect the wood from fungal decay and insect attack, they increase the corrosion of metals embedded or in contact with the treated wood. Previous research has shown the most...

  11. The role of fission products (noble metal particles) in spent fuel corrosion process in a failed container

    Energy Technology Data Exchange (ETDEWEB)

    Wu, L., E-mail: lwu59@uwo.ca [Univ. of Western Ontario, Dept. of Chemistry, London, Ontario (Canada); Shoesmith, D.W. [Univ. of Western Ontario, Dept. of Chemistry, London, Ontario (Canada); Univ. of Western Ontario, Surface Science Western, London, Ontario (Canada)

    2013-07-01

    The corrosion/dissolution of simulated spent fuel has been studied electrochemically. Fission products within the UO{sub 2} matrix are found to have significant effect on the anodic dissolution behaviour of the fuel. It is observed that H{sub 2}O{sub 2}oxidation is accelerated on the surfaces of doped noble metal (ε) particles existing in the fuel matrix. It is concluded that H{sub 2}O{sub 2} decomposition rather than UO{sub 2} corrosion should be the dominant reaction under high H{sub 2}O{sub 2} concentrations. (author)

  12. Properties of colloidal corrosion products and their effects on nuclear plants. Volume 1. Executive summary. Final report

    International Nuclear Information System (INIS)

    Matijevic, E.

    1982-10-01

    The properties of aqueous dispersions of finely divided oxides of iron, nickel, cobalt, chromium, and copper are described in overview fashion. More detailed aspects of this work will be found in a separate, larger report, NP-2606, Volume 2. The properties of these oxide corrosion products of importance to nuclear reactor water system technology are emphasized: adhesion, desorption, dissolution, transformation, and adsorption of dissolved species such as Co 60 ions. The work is fundamental to many LWR problems - radiation transport to piping surfaces, avoidance of crud buildup on nuclear fuel rods, decontamination and chemical cleaning of heat exchangers, and control of corrosion of piping

  13. Solubility of Oxygen in Liquid Sodium and the Interpretation of Predictions for the Corrosion Rate of Stainless Steels in Liquid Sodium

    International Nuclear Information System (INIS)

    Claxton, K. T.

    1979-01-01

    A statistical analysis of all oxygen in sodium solubility data has been made. The results indicate a real difference. between levels of oxygen reported by UK und US workers. Analysis using sub-sets of culled data to derive a compromise solubility function are considered less than adequate. It is considered preferable and more realistic to distinguish data sub-sets by the analytical technique employed. The vacuum distillation method yields results differing amongst them selves by up to a factor of five at cold trap temperatures of relevance to fast reactor operation. The vanadium wire and electrochemical cell techniques give the lowest solubility values. (Author) 51 refs

  14. Determining a Solubility Product Constant by Potentiometric Titration to Increase Students' Conceptual Understanding of Potentiometry and Titrations

    Science.gov (United States)

    Grabowski, Lauren E.; Goode, Scott R.

    2017-01-01

    Potentiometric titrations are widely taught in first-year undergraduate courses to connect electrochemistry, stoichiometry, and equilibria and to reinforce acid-base titrations. Students perform a potentiometric titration that is then analyzed to determine analyte concentrations and the solubility product constant of the solid species.

  15. Co-expression of sulphydryl oxidase and protein disulphide isomerase in Escherichia coli allows for production of soluble CRM197

    CSIR Research Space (South Africa)

    Roth, Robyn L

    2017-04-01

    Full Text Available The aim of this article is to investigate the production of soluble cross-reacting material 197 (CRM(sub197)) in Escherichia coli, a safe and effective T-cell-dependent protein carrier for polysaccharides used in the manufacture and application...

  16. Analysis of vanadium slags, roasted and leached products. Determination of contents of total vanadium, chromium, sodium, and soluble vanadium

    International Nuclear Information System (INIS)

    Hasek, Z.

    1975-01-01

    Accurate, rapid and simple methods were elaborated of determining total vanadium, chromium, and sodium in vanadium slags, and in roasted and leached products in one sample batch. The analysis was conducted in a teflon vial using inorganic acids. A method od determining soluble vanadium in similar materials was also elaborated and verified. (B.S.)

  17. The mechanisms underlying corrosion product formation and deposition in nuclear power plant circuits through the action of galvanic and thermal electromotive forces

    International Nuclear Information System (INIS)

    Brusakov, V.P.; Sedov, V.M.; Khitrov, Yu.A.; Brusov, K.N.; Razmashkin, N.V.; Versin, V.V.; Rybalchenko, I.L.

    1983-01-01

    From a theoretical standpoint, the processes of formation of corrosion products in nuclear power plant circuits, deposition of corrosion products on the circuit surfaces, formation of an equilibrium concentration of corrosion products in the coolant, and distribution of radionuclides resulting from corrosion in different parts of the circuit are considered. It is shown that the main driving forces for the mass-transfer processes in the circuits are the thermal and galvanic electromotive forces (EMF) of the microcouples. On the basis of the theoretical concepts developed the authors have obtained analytical dependences for calculating the individual stages of the process of corrosion product transfer in the circuits. The mechanisms underlying the processes which occur as a result of thermal and galvanic EMFs are considered, together with the factors influencing these processes. The results of verification of the dependences by computational methods are given and they are compared with operational data from nuclear and conventional thermal power plants and with experimental data. (author)

  18. Characteristics and fates of soluble microbial products in ceramic membrane bioreactor at various sludge retention times.

    Science.gov (United States)

    Shin, Hang-Sik; Kang, Seok-Tae

    2003-01-01

    The formation and fate of soluble microbial products (SMP) in membrane bioreactor (MBR) was investigated at various sludge retention times (SRT) for 170 days. The SMP concentration was estimated by feeding glucose, which could be completely degraded, and by measuring the dissolved organic carbon (DOC) of the effluent from MBR. Under the conditions of SRT of 20 days, influent DOC of 112 mg/l and HRT of 6 h, the produced SMP was 4.7 mg DOC/l of which 57% was removed or retained by the membrane. DOC of MBR supernatant increased during 100 days and then gradually decreased. Specific UV absorbance showed that the accumulated compounds had a portion of larger, more aromatic, more hydrophobic and double-bond-rich organics, which originated from the decayed biomass. Molecular weight distributions of SMP in MBR supernatant showed that the acclimated microorganisms in a long SRT could decompose high molecular weight organics, it caused the shift of molecular weight distributions of SMP to a lower range. During the operation period, enumeration of active cells in the MBR showed that microbial inhibitions by accumulated SMP was not observed.

  19. Removal of anaerobic soluble microbial products in a biological activated carbon reactor.

    Science.gov (United States)

    Dong, Xiaojing; Zhou, Weili; He, Shengbing

    2013-09-01

    The soluble microbial products (SMP) in the biological treatment effluent are generally of great amount and are poorly biodegradable. Focusing on the biodegradation of anaerobic SMP, the biological activated carbon (BAC) was introduced into the anaerobic system. The experiments were conducted in two identical lab-scale up-flow anaerobic sludge blanket (UASB) reactors. The high strength organics were degraded in the first UASB reactor (UASB1) and the second UASB (UASB2, i.e., BAC) functioned as a polishing step to remove SMP produced in UASB1. The results showed that 90% of the SMP could be removed before granular activated carbon was saturated. After the saturation, the SMP removal decreased to 60% on the average. Analysis of granular activated carbon adsorption revealed that the main role of SMP removal in BAC reactor was biodegradation. A strain of SMP-degrading bacteria, which was found highly similar to Klebsiella sp., was isolated, enriched and inoculated back to the BAC reactor. When the influent chemical oxygen demand (COD) was 10,000 mg/L and the organic loading rate achieved 10 kg COD/(m3 x day), the effluent from the BAC reactor could meet the discharge standard without further treatment. Anaerobic BAC reactor inoculated with the isolated Klebsiella was proved to be an effective, cheap and easy technical treatment approach for the removal of SMP in the treatment of easily-degradable wastewater with COD lower than 10,000 mg/L.

  20. Hydration interactions and stability of soluble microbial products in aqueous solutions.

    Science.gov (United States)

    Wang, Ling-Ling; Wang, Long-Fei; Ye, Xiao-Dong; Yu, Han-Qing

    2013-10-01

    Soluble microbial products (SMP) are organic compounds excreted by microorganisms in their metabolism and decay and the main constituents in effluent from biological wastewater treatment systems. They also have an important contribution to the dissolved organic matters in natural aqueous systems. So far the interactions between SMP colloids have not been well explored. In this work, the interactions between SMP colloids in water and salt solutions were studied by using a combination of static and dynamic light scattering, Fourier transform infrared spectra, Zeta potential and acid-base titration techniques. The second osmotic virial coefficient had a larger value in a 750-mM salt solution than that in a 50-mM solution, indicating that repulsion between SMP colloids increased with an increase in salt concentration, which is contrary with the classic Derjaguin, Landau, Verwey, and Overbeek (DLVO) theory. Such a repulsion was attributed to water structuring and enhanced by the accumulation of hydrophilic counter ions around SMP colloids and the formed hydration force. The repulsion and hydration effect led to the dispersing and deeper draining structure, accompanied by a decreased hydrodynamic radius and increased diffusion coefficient. This hydration force was related to so-called ion specific effect, and electrolyte sodium chloride had a more substantial effect on hydration force than KCl, CsCl, NaBr and NaI. Our results provide an experimental approach to explore the SMP structures, inter-colloid interactions and confirm the non-DLVO forces. Copyright © 2013 Elsevier Ltd. All rights reserved.

  1. A novel biological function of soluble biglycan: Induction of erythropoietin production and polycythemia.

    Science.gov (United States)

    Frey, Helena; Moreth, Kristin; Hsieh, Louise Tzung-Harn; Zeng-Brouwers, Jinyang; Rathkolb, Birgit; Fuchs, Helmut; Gailus-Durner, Valérie; Iozzo, Renato V; de Angelis, Martin Hrabě; Schaefer, Liliana

    2017-06-01

    Secondary polycythemia, a disease characterized by a selective increase in circulating mature erythrocytes, is caused by enhanced erythropoietin (Epo) concentrations triggered by hypoxia-inducible factor-2α (HIF-2α). While mechanisms of hypoxia-dependent stabilization of HIF-2α protein are well established, data regarding oxygen-independent regulation of HIF-2α are sparse. In this study, we generated a novel transgenic mouse model, in which biglycan was constitutively overexpressed and secreted by hepatocytes (BGN Tg ), thereby providing a constant source of biglycan released into the blood stream. We discovered that although the mice were apparently normal, they harbored an increase in mature circulating erythrocytes. In addition to erythrocytosis, the BGN Tg mice showed elevated hemoglobin concentrations, hematocrit values and enhanced total iron binding capacity, revealing a clinical picture of polycythemia. In BGN Tg mice markedly enhanced Epo mRNA expression was observed in the liver and kidney, while elevated Epo protein levels were found in liver, kidney and blood. Mechanistically, we showed that the transgenic animals had an abundance of HIF-2α protein in the liver and kidney. Finally, by transiently overexpressing circulating biglycan in mice deficient in various Toll-like receptors (TLRs), we determined that this novel function of biglycan to promote Epo synthesis was specifically mediated by a selective interaction with TLR2. Thus, we discovered a novel biological pathway of soluble biglycan inducing HIF-2α protein stabilization and Epo production presumably in an oxygen-independent manner, ultimately giving rise to secondary polycythemia.

  2. Thermodynamics of soluble fission products cesium and iodine in the Molten Salt Reactor

    Science.gov (United States)

    Capelli, E.; Beneš, O.; Konings, R. J. M.

    2018-04-01

    The present study describes the full thermodynamic assessment of the Li,Cs,Th//F,I system. The existing database for the relevant fluoride salts considered as fuel for the Molten Salt Reactor (MSR) has been extended with two key fission products, cesium and iodine. A complete evaluation of all the common-ion binary and ternary sub-systems of the LiF-ThF4-CsF-LiI-ThI4-CsI system has been performed and the optimized parameters are presented in this work. New equilibrium data have been measured using Differential Scanning Calorimetry and were used to assess the reciprocal ternary systems and confirm the extrapolated phase diagrams. The developed database significantly contributes to the understanding of the behaviour of cesium and iodine in the MSR, which strongly depends on their concentration and chemical form. Cesium bonded with fluorine is well retained in the fuel mixture while in the form of CsI the solubility of these elements is very limited. Finally, the influence of CsI and CsF on the physico-chemical properties of the fuel mixture was calculated as function of composition.

  3. Photoautotrophic Production of Biomass, Laurate, and Soluble Organics by Synechocystis sp. PCC 6803

    Science.gov (United States)

    Nguyen, Binh Thanh

    Photosynthesis converts sunlight to biomass at a global scale. Among the photosynthetic organisms, cyanobacteria provide an excellent model to study how photosynthesis can become a practical platform of large-scale biotechnology. One novel approach involves metabolically engineering the cyanobacterium Synechocystis sp. PCC 6803 to excrete laurate, which is harvested directly. This work begins by defining a working window of light intensity (LI). Wild-type and laurate-excreting Synechocystis required an LI of at least 5 muE/m2-s to sustain themselves, but are photo-inhibited by LI of 346 to 598 muE/m2-s. Fixing electrons into valuable organic products, e.g., biomass and excreted laurate, is critical to success. Wild-type Synechocystis channeled 75% to 84% of its fixed electrons to biomass; laurate-excreting Synechocystis fixed 64 to 69% as biomass and 6.6% to 10% as laurate. This means that 16 to 30% of the electrons were diverted to non-valuable soluble products, and the trend was accentuated with higher LI. How the Ci concentration depended on the pH and the nitrogen source was quantified by the proton condition and experimentally validated. Nitrate increased, ammonium decreased, but ammonium nitrate stabilized alkalinity and Ci. This finding provides a mechanistically sound tool to manage Ci and pH independently. Independent evaluation pH and Ci on the growth kinetics of Synechocystis showed that pH 8.5 supported the fastest maximum specific growth rate (mumax): 2.4/day and 1.7/day, respectively, for the wild type and modified strains with LI of 202 muE/m2-s. Half-maximum-rate concentrations (KCi) were less than 0.1 mM, meaning that Synechocystis should attain its mumax with a modest Ci concentration (≥1.0 mM). Biomass grown with day-night cycles had a night endogenous decay rate of 0.05-1.0/day, with decay being faster with higher LI and the beginning of dark periods. Supplying light at a fraction of daylight reduced dark decay rate and improved overall

  4. Removal of soluble microbial products as the precursors of disinfection by-products in drinking water supplies.

    Science.gov (United States)

    Liu, Jin-Lin; Li, Xiao-Yan

    2015-01-01

    Water pollution worsens the problem of disinfection by-products (DBPs) in drinking water supply. Biodegradation of wastewater organics produces soluble microbial products (SMPs), which can be important DBP precursors. In this laboratory study, a number of enhanced water treatment methods for DBP control, including enhanced coagulation, ozonation, and activated carbon adsorption, were evaluated for their effectiveness in treating SMP-containing water for the DBP reduction purpose. The results show that enhanced coagulation with alum could remove SMPs only marginally and decrease the DBP formation potential (DBPFP) of the water by less than 20%. Although ozone could cause destruction of SMPs in water, the overall DBPFP of the water did not decrease but increased after ozonation. In contrast, adsorption by granular activated carbon could remove the SMP organics from water by more than 60% and reduce the DBPFP by more than 70%. It is apparent that enhanced coagulation and ozonation are not suitable for the removal of SMPs as DBP precursors from polluted water, although enhanced coagulation has been commonly used to reduce the DBP formation caused by natural organic matter. In comparison, activated carbon adsorption is shown as a more effective means to remove the SMP content from water and hence to control the wastewater-derived DBP problem in water supply.

  5. Inhibitory effects of soluble algae products (SAP) released by Scenedesmus sp. LX1 on its growth and lipid production.

    Science.gov (United States)

    Zhang, Tian-Yuan; Yu, Yin; Wu, Yin-Hu; Hu, Hong-Ying

    2013-10-01

    Soluble algal products (SAP) accumulated in culture medium via water reuse may affect the growth of microalga during the cultivation. Scenedesmus sp. LX1, a freshwater microalga, was used in this study to investigate the effect of SAP on growth and lipid production of microalga. Under the SAP concentrations of 6.4-25.8 mg L(-1), maximum algal density (K) and maximum growth rate (Rmax) of Scenedesmus sp. LX1 were decreased by 50-80% and 35-70% compared with the control group, respectively. The effect of SAP on lipid accumulation of Scenedesmus sp. LX1 was non-significant. According to hydrophilic-hydrophobic and acid-base properties, SAP was fractionized into six fractions. All of the fractions could inhibit the growth of Scenedesmus sp. LX1. Organic bases (HIB, HOB) and hydrophilic acids (HIA) showed the strongest inhibition. HIA could also decrease the lipid content of Scenedesmus sp. LX1 by 59.2%. As the inhibitory effect, SAP should be seriously treated before water reuse. Copyright © 2013 Elsevier Ltd. All rights reserved.

  6. Use of a free-jet expansion, molecular beam mass spectrometer to understand processes involving volatile corrosion products

    International Nuclear Information System (INIS)

    Jacobson, N.S.

    1997-01-01

    Many high-temperature corrosion processes generate volatile products in addition to condensed phase products. Examples of these volatile products are chlorides, oxychlorides, and certain oxides and hydroxyl species. One of the best techniques to identify high temperature vapor molecules is mass spectrometry. Most mass spectrometers operate in high vacuum and are generally used to examine processes ocurring at greatly reduced pressures. However, a free-jet expansion, molecular beam mass spectrometer system allows direct sampling of volatile corrosion products. This instrument is described. Several examples from our studies on chlorination/oxidation of metals and ceramics are discussed. In addition, reactions of Cr 2 O 3 , SiO 2 , and Al 2 O 3 with water vapor, which produce volatile hydroxyl species are discussed. (orig.)

  7. Soluble Microbial Product Characterization of Biofilm Formation in Bench-Scale

    KAUST Repository

    Mines, Paul

    2012-12-01

    The biological process known as activated sludge (AS) in conjunction with membrane separation technology for the treatment of wastewater has been employed for over four decades. While, membrane biological reactors (MBR) are now widely employed, the phenomenon of membrane fouling is still the most significant factor leading to performance decline of MBRs. Although much research has been done on the subject of MBR fouling over the past two decades, many questions remain unanswered, and consensus within the scientific community is rare. However, research has led to one system parameter generally being regarded as a contributor to membrane fouling, extracellular polymeric compounds (EPS). EPS, and more specifically, the soluble fraction of EPS known as soluble microbial products (SMP), must be further investigated in order to better understand membrane fouling. The biological activity and performance of the MBR is affected by myriad operational parameters, which in turn affects the SMP generated. A commonly varied operational parameter is, depending on the specific treatment needs of a MBR, the sludge retention time (SRT). This study aims to characterize the SMP in three bench-scale MBRs as the SRT is gradually lowered. By studying how the SMP change as the operation of the system is altered, greater understanding of how SMP are related to fouling can be achieved. At the onset of the study, a steady state was established in the system with a SRT of 20 days. Upon stabilization of a 20 day SRT, the system was gradually transitioned to a five and a half day SRT, in stepwise adjustments. Initially, both the trans-membrane pressure (TMP) and the SMP concentrations were at relatively low values, indicating the presence of minimal amounts of biofilm on the membrane surfaces. As the system was altered and more activated sludge was wasted from the reactors, the SRT inherently decreased. As the lower SRT was transitioned and established, the data from TMP measurements, as well

  8. Solubilities of iron and nickel oxides under high temperature and high pressure conditions

    International Nuclear Information System (INIS)

    Choi, Ke-Chon; Jung, Yong-Ju; Yeon, Jei-Won; Jee, Kwang-Yong

    2007-01-01

    The purposes of primary coolant chemistry are to assure fuel and material integrity and to minimize out of core radiation fields. During the PWR operation, crud deposits are expected on the cladding, leading to cladding failure and raising the radioactivity. Such deposits come from the corrosion products of system surface. To achieve optimal conditions for primary coolant, basic researches on mass transfer, deposition and solubility of corrosion products are needed. The initial stage of crud formation could be the studies on the solubility of a structural material. It has been known that the solubility of metal oxides in boric acid under high temperature and high pressure condition depends on the pH and dissolved hydrogen. Thus, the effect of various pH on the solubility of metal oxide in boric acid solution was investigated in this work

  9. Solid solubility of fission product and other transition elements in carbides and nitrides of uranium and plutonium

    International Nuclear Information System (INIS)

    Benedict, U.

    1979-01-01

    Solubility studies were made in some MX-Me systems (M:U or Pu; X: C or N; Me: fission product or other transition element) by X-ray diffraction and partly by microprobe determination of solute concentrations. Up to 23 m/o ZrC and 17 m/o TaC dissolved in the PuC phases of sintered PuC-ZrC and PuC-TaC samples; the lattice parameter/concentration relationships were derived. The relative lattice parameter difference (RLPD) between MXy and MeXy (y: ratio X/(M+Me)) was used as a solubility criterion. NaCl type monocarbides with RLPD's from -10.2% to +7.8% are completely miscible with UC and PuC. NaCl type mononitrides with RLPD's from -7.5% to 8.5% are completely miscible with UN and PuN. The solubility in the sesquicarbides increases with decreasing RLPD and becomes complete in Pu 2 C 3 at RLPD =+4%, and in U 2 C 3 at RLPD ca. +1.5%. Solubilities are predicted on the basis of these rules for the cases where no experimental results are available. A general review on the experimental and predicted solubilities is given. (orig.) [de

  10. Composition and Morphology of Product Layers in the Steel/Cement Paste Interface in Conditions of Corrosion and Cathodic Protection in Reinforced Concrete

    NARCIS (Netherlands)

    Koleva, D.A.; Van Breugel, K.; De Wit, J.H.W.; Fraaij, A.L.A.; Boshkov, N.

    2007-01-01

    The present study explores the formation of corrosion products on the steel surface in reinforced concrete in conditions of corrosion and subsequent transformation of these layers in conditions of cathodic protection (CP). Of particular interest was to investigate if the introduced pulse CP (as

  11. Electrochemical properties of corrosion products formed on Zn-Mg, Zn-Al and Zn-Al-Mg coatings in model atmospheric conditions

    Czech Academy of Sciences Publication Activity Database

    Stoulil, J.; Prošek, T.; Nazarov, A.; Oswald, Jiří; Kříž, P.; Thierry, D.

    2015-01-01

    Roč. 66, č. 8 (2015), s. 777-782 ISSN 0947-5117 Institutional support: RVO:68378271 Keywords : corrosion products * electrochemical properties * zinc coating Subject RIV: JK - Corrosion ; Surface Treatment of Materials Impact factor: 1.450, year: 2015

  12. Corrosion resistance of zinc-magnesium coated steel

    International Nuclear Information System (INIS)

    Hosking, N.C.; Stroem, M.A.; Shipway, P.H.; Rudd, C.D.

    2007-01-01

    A significant body of work exists in the literature concerning the corrosion behaviour of zinc-magnesium coated steel (ZMG), describing its enhanced corrosion resistance when compared to conventional zinc-coated steel. This paper begins with a review of the literature and identifies key themes in the reported mechanisms for the attractive properties of this material. This is followed by an experimental programme where ZMG was subjected to an automotive laboratory corrosion test using acidified NaCl solution. A 3-fold increase in time to red rust compared to conventional zinc coatings was measured. X-ray diffraction, X-ray photoelectron spectroscopy and scanning electron microscopy were used to characterize the corrosion products formed. The corrosion products detected on ZMG included simonkolleite (Zn 5 Cl 2 (OH) 8 . H 2 O), possibly modified by magnesium uptake, magnesium hydroxide (Mg(OH) 2 ) and a hydroxy carbonate species. It is proposed that the oxygen reduction activity at the (zinc) cathodes is reduced by precipitation of alkali-resistant Mg(OH) 2 , which is gradually converted to more soluble hydroxy carbonates by uptake of atmospheric carbon dioxide. This lowers the surface pH sufficiently to allow thermodynamically for general precipitation of insoluble simonkolleite over the corroding surface thereby retarding the overall corrosion reactions, leaving only small traces of magnesium corrosion products behind. Such a mechanism is consistent with the experimental findings reported in the literature

  13. Dictionary corrosion and corrosion control

    International Nuclear Information System (INIS)

    1985-01-01

    This dictionary has 13000 entries in both languages. Keywords and extensive accompanying information simplify the choice of word for the user. The following topics are covered: Theoretical principles of corrosion; Corrosion of the metals and alloys most frequently used in engineering. Types of corrosion - (chemical-, electro-chemical, biological corrosion); forms of corrosion (superficial, pitting, selective, intercrystalline and stress corrosion; vibrational corrosion cracking); erosion and cavitation. Methods of corrosion control (material selection, temporary corrosion protection media, paint and plastics coatings, electro-chemical coatings, corrosion prevention by treatment of the corrosive media); Corrosion testing methods. (orig./HP) [de

  14. Corrosion product behaviour in the primary circuit of the KNK nuclear reactor facility

    International Nuclear Information System (INIS)

    Stamm, H.H.; Stade, K.Ch.

    1976-01-01

    During nuclear operation of the KNK facility from 1972 until September 1974 the composition and behaviour of radionuclides occuring in the primary circuit were investigated. Besides traces of 140 Ba/ 140 La, no fission product activity was detectable in the KNK primary circuit. The fuel element purification from sodium deposits (prior to transport to the reprocessing plant) did not yield any indication of a fuel element failure during KNK-I operation. The activity inventory of the primary loop was exclusively made up of activated corrosion products and 22 Na. The main activity was due to 65 Zn, followed by 54 Mn, 22 Na, sup(110m)Ag, 182 Ta, 60 Co and 124 Sb. It was found that the sorption of 65 Zn and 54 Mn on crucibles made from nickel was condiserably higher than on vessels made from other materials. This observation was confirmed both in tests with material samples from the primary circuit and for disks of gate valves of the primary circuit. sup(110m)Ag did hardly exhibit any sorption effects and had been dissolved largely homogeneously in the hot primary coolant. In the first primary cold trap which was removed from the circuit after some 20,000 hours of operation, only 65 Zn and 54 Mn were detected in addition to traces of 60 Co and 182 Ta. (author)

  15. A computer analysis code of radioactive corrosion product behaviour in primary circuits of LMFBRs (PSYCHE)

    International Nuclear Information System (INIS)

    Iizawa, Katsuyuki; Seki, Seiichi; Kawasaki, Yuji; Kano, Shigeki; Nihei, Isao

    1986-01-01

    Recently it has become an important subject to reduce exposure to radiation from radioactive corrosion products (CPs) during maintenance and repair works in reactor plants. Metallic sodium is used as cooling material in fast reactor plants, leading to different CP behaviours compared to light water reactors. In the present study, a computer code for analyzing behaviours of CPs in fast reactor plants is developed. The analysis code, called PSYCHE, makes it possible to perform consistent analysis of production, migration and deposition of CPs in primary circuits together with dose rate around piping of apparatus in cooling systems. An analysis model is developed based on test results on CP behaviour in out-pile sodium. The model, called the ''dissolution-deposition model'', can reproduce atom-selective behaviour, transient phenomenon and downstream effect of CPs, which represent mass transfer phenomena in sodium. Verification of this code is carried out on the basis of CP measurements made in ''Joyo''. The calculation vs. measurement ratio is found to be 0.5 - 2 for CP deposition density in piping for cooling systems and 0.7 - 1.3 for dose rate, demonstrating that this code can give reasonable results. Analysis is also made to predict future changes in total amount of deposited CP in ''Joyo''. (Nogami, K.)

  16. Corrosion of carbon steel in contact with bentonite

    International Nuclear Information System (INIS)

    Dobrev, D.; Vokal, A.; Bruha, P.

    2010-01-01

    of approximately 2-3 mm/yr in bentonite pore water solution. No significant pressure increase was observed due to generation of hydrogen. The results of surprising behaviour of carbon steels in bentonite could be explained by the different composition of solution after granitic water flow through bentonite or by hypothesis based on our modelling experiments that corrosion rate increase is caused by so called pumping effect of bentonite which is in turn caused by different solubilities of corrosion products in the corrosion layer and bentonite. Influence of corrosion products on bentonite is another important question. It was clearly visible that the transport of corrosion products into Volclay bentonite is approximately 1 mm after 30 days of corrosion at 70 deg. C. The reason why no pressure increase was observed due to hydrogen evolution could be explained by higher rate of hydrogen transport in bubbles than is its evolution rate. But these hydrogen bubbles might be also accumulated between carbon steel layer and bentonite what results in inhomogeneity of corrosion layer. The results achieved significantly affect performance assessment of concept of disposal with carbon steel and bentonite. Only rather short term (30 days) experiments were carried out. In the next period longer experiments will have to give answer if the increase of corrosion rate of carbon steel in contact with bentonite is transient or will last for long time. (authors)

  17. Soluble products of Escherichia coli induce mitochondrial dysfunction-related sperm membrane lipid peroxidation which is prevented by lactobacilli.

    Directory of Open Access Journals (Sweden)

    Arcangelo Barbonetti

    Full Text Available Unidentified soluble factors secreted by E. coli, a frequently isolated microorganism in genitourinary infections, have been reported to inhibit mitochondrial membrane potential (ΔΨm, motility and vitality of human spermatozoa. Here we explore the mechanisms involved in the adverse impact of E. coli on sperm motility, focusing mainly on sperm mitochondrial function and possible membrane damage induced by mitochondrial-generated reactive oxygen species (ROS. Furthermore, as lactobacilli, which dominate the vaginal ecosystem of healthy women, have been shown to exert anti-oxidant protective effects on spermatozoa, we also evaluated whether soluble products from these microorganisms could protect spermatozoa against the effects of E. coli. We assessed motility (by computer-aided semen analysis, ΔΨm (with JC-1 dye by flow cytometry, mitochondrial ROS generation (with MitoSOX red dye by flow cytometry and membrane lipid-peroxidation (with the fluorophore BODIPY C11 by flow cytometry of sperm suspensions exposed to E. coli in the presence and in the absence of a combination of 3 selected strains of lactobacilli (L. brevis, L. salivarius, L. plantarum. A Transwell system was used to avoid direct contact between spermatozoa and microorganisms. Soluble products of E. coli induced ΔΨm loss, mitochondrial generation of ROS and membrane lipid-peroxidation, resulting in motility loss. Soluble factors of lactobacilli prevented membrane lipid-peroxidation of E. coli-exposed spermatozoa, thus preserving their motility. In conclusion, sperm motility loss by soluble products of E. coli reflects a mitochondrial dysfunction-related membrane lipid-peroxidation. Lactobacilli could protect spermatozoa in the presence of vaginal disorders, by preventing ROS-induced membrane damage.

  18. Fermentation of calcium-fortified soymilk with Lactobacillus: effects on calcium solubility, isoflavone conversion, and production of organic acids.

    Science.gov (United States)

    Tang, A L; Shah, N P; Wilcox, G; Walker, K Z; Stojanovska, L

    2007-11-01

    The objective of this study was to enhance calcium solubility and bioavailability from calcium-fortified soymilk by fermentation with 7 strains of Lactobacillus, namely, L. acidophilus ATCC 4962, ATCC33200, ATCC 4356, ATCC 4461, L. casei ASCC 290, L. plantarum ASCC 276, and L. fermentum VRI-003. The parameters that were used are viability, pH, calcium solubility, organic acid, and biologically active isoflavone aglycone content. Calcium-fortified soymilk made from soy protein isolate was inoculated with these probiotic strains, incubated for 24 h at 37 degrees C, then stored for 14 d at 4 degrees C. Soluble calcium was measured using atomic absorption spectrophotometry (AA). Organic acids and bioactive isoflavone aglycones, including diadzein, genistein, and glycetein, were measured using HPLC. Viability of the strains in the fermented calcium-fortified soymilk was > 8.5 log(10) CFU/g after 24 h fermentation and this was maintained for 14-d storage at 4 degrees C. After 24 h, there was a significant increase (P casei ASCC 290 demonstrated the highest increase with 89.3% and 87.0% soluble calcium after 24 h, respectively. The increase in calcium solubility observed was related to lowered pH associated with production of lactic and acetic acids. Fermentation significantly increased (P < 0.05) the level of conversion of isoflavones into biologically active aglycones, including diadzein, genistein, and glycetein. Our results show that fermenting calcium-fortified soymilk with the selected probiotics can potentially enhance the calcium bioavailability of calcium-fortified soymilk due to increased calcium solubility and bioactive isoflavone aglycone enrichment.

  19. Pipe Lines – External Corrosion

    Directory of Open Access Journals (Sweden)

    Dan Babor

    2008-01-01

    Full Text Available Two areas of corrosion occur in pipe lines: corrosion from the medium carried inside the pipes; corrosion attack upon the outside of the pipes (underground corrosion. Electrolytic processes are also involved in underground corrosion. Here the moisture content of the soil acts as an electrolyte, and the ions required to conduct the current are supplied by water-soluble salts (chlorides, sulfates, etc. present in the soil. The nature and amount of these soluble materials can vary within a wide range, which is seen from the varying electrical conductivity and pH (varies between 3 and 10. Therefore the characteristics of a soil will be an important factor in under-ground corrosion.

  20. Calculated model of radioactive fission and corrosion product accumulation and distribution in a fast reactor sodium coolant circuit

    International Nuclear Information System (INIS)

    Kizin, V.D.; Konyashov, V.V.

    1987-01-01

    A simple calculation procedure of radioactive products accumulation and distribution in a primary circuit has been developed on the basis of experimental investigations at the BOR-60 reactor. Common knowledge on the impurity products transfer at the liquid-solid and liquid-gas phase boundary is taken. Use is made of the typical in reactor physics relationships for the description of the products transition to the equipment surfaces, of fission products release, metal corrosion and others. Satisfactory agreement of the calculation data with the experimental ones has been obtained. (orig.)

  1. The growing rate and the type of corrosion products of aluminium alloy AA 5052 in deionized water at temperature up to 3000C

    International Nuclear Information System (INIS)

    Ferreira, E.G.

    1980-01-01

    The process of corrosion concerning the aluminum alloy AA5052 in deionized water at temperatures of 40 0 C, 80 0 C, 90 0 C, 140 0 C, 200 0 C and 280 0 C is studied. The following methods are used: periodic weighting of the test samples; analysis by neutronic activation of the corrosion products dissolved in water; thermogravimetric and thermodiferential analysis; analysis through X-ray diffraction and from metalografic observations of the crystals produced in the corrosion process; an optical microscope using polarized and normal light and a scanning electronic microscope. The activation energies are calculated for the corrosion film formation, and for the dissolution of the corrosion products in the deionized water. (ARHC) [pt

  2. Production and characterization of cowpea protein hydrolysate with optimum nitrogen solubility by enzymatic hydrolysis using pepsin.

    Science.gov (United States)

    Mune Mune, Martin Alain; Minka, Samuel René

    2017-06-01

    Cowpea is a source of low-cost and good nutritional quality protein for utilization in food formulations in replacement of animal proteins. Therefore it is necessary that cowpea protein exhibits good functionality, particularly protein solubility which affects the other functional properties. The objective of this study was to produce cowpea protein hydrolysate exhibiting optimum solubility by the adequate combination of hydrolysis parameters, namely time, solid/liquid ratio (SLR) and enzyme/substrate ratio (ESR), and to determine its functional properties and molecular characteristics. A Box-Behnken experimental design was used for the experiments, and a second-order polynomial to model the effects of hydrolysis time, SLR and ESR on the degree of hydrolysis and nitrogen solubility index. The optimum hydrolysis conditions of time 208.61 min, SLR 1/15 (w/w) and ESR 2.25% (w/w) yielded a nitrogen solubility of 75.71%. Protein breakdown and the peptide profile following enzymatic hydrolysis were evaluated by sodium dodecyl sulfate polyacrylamide gel electrophoresis and size exclusion chromatography. Cowpea protein hydrolysate showed higher oil absorption capacity, emulsifying activity and foaming ability compared with the concentrate. The solubility of cowpea protein hydrolysate was adequately optimized by response surface methodology, and the hydrolysate showed adequate functionality for use in food. © 2016 Society of Chemical Industry. © 2016 Society of Chemical Industry.

  3. Responses of Microbial Community Composition to Temperature Gradient and Carbon Steel Corrosion in Production Water of Petroleum Reservoir

    Directory of Open Access Journals (Sweden)

    Xiao-Xiao Li

    2017-12-01

    Full Text Available Oil reservoir production systems are usually associated with a temperature gradient and oil production facilities frequently suffer from pipeline corrosion failures. Both bacteria and archaea potentially contribute to biocorrosion of the oil production equipment. Here the response of microbial populations from the petroleum reservoir to temperature gradient and corrosion of carbon steel coupons were investigated under laboratory condition. Carbon steel coupons were exposed to production water from a depth of 1809 m of Jiangsu petroleum reservoir (China and incubated for periods of 160 and 300 days. The incubation temperatures were set at 37, 55, and 65°C to monitoring mesophilic, thermophilic and hyperthermophilic microorganisms associated with anaerobic carbon steel corrosion. The results showed that corrosion rate at 55°C (0.162 ± 0.013 mm year-1 and 37°C (0.138 ± 0.008 mm year-1 were higher than that at 65°C (0.105 ± 0.007 mm year-1, and a dense biofilm was observed on the surface of coupons under all biotic incubations. The microbial community analysis suggests a high frequency of bacterial taxa associated with families Porphyromonadaceae, Enterobacteriaceae, and Spirochaetaceae at all three temperatures. While the majority of known sulfate-reducing bacteria, in particular Desulfotignum, Desulfobulbus and Desulfovibrio spp., were predominantly observed at 37°C; Desulfotomaculum spp., Thermotoga spp. and Thermanaeromonas spp. as well as archaeal members closely related to Thermococcus and Archaeoglobus spp. were substantially enriched at 65°C. Hydrogenotrophic methanogens of the family Methanobacteriaceae were dominant at both 37 and 55°C; acetoclastic Methanosaeta spp. and methyltrophic Methanolobus spp. were enriched at 37°C. These observations show that temperature changes significantly alter the microbial community structure in production fluids and also affected the biocorrosion of carbon steel under anaerobic conditions.

  4. Production of soluble mammalian proteins in Escherichia coli: identification of protein features that correlate with successful expression

    Directory of Open Access Journals (Sweden)

    Perera Rajika L

    2004-12-01

    Full Text Available Abstract Background In the search for generic expression strategies for mammalian protein families several bacterial expression vectors were examined for their ability to promote high yields of soluble protein. Proteins studied included cell surface receptors (Ephrins and Eph receptors, CD44, kinases (EGFR-cytoplasmic domain, CDK2 and 4, proteases (MMP1, CASP2, signal transduction proteins (GRB2, RAF1, HRAS and transcription factors (GATA2, Fli1, Trp53, Mdm2, JUN, FOS, MAD, MAX. Over 400 experiments were performed where expression of 30 full-length proteins and protein domains were evaluated with 6 different N-terminal and 8 C-terminal fusion partners. Expression of an additional set of 95 mammalian proteins was also performed to test the conclusions of this study. Results Several protein features correlated with soluble protein expression yield including molecular weight and the number of contiguous hydrophobic residues and low complexity regions. There was no relationship between successful expression and protein pI, grand average of hydropathicity (GRAVY, or sub-cellular location. Only small globular cytoplasmic proteins with an average molecular weight of 23 kDa did not require a solubility enhancing tag for high level soluble expression. Thioredoxin (Trx and maltose binding protein (MBP were the best N-terminal protein fusions to promote soluble expression, but MBP was most effective as a C-terminal fusion. 63 of 95 mammalian proteins expressed at soluble levels of greater than 1 mg/l as N-terminal H10-MBP fusions and those that failed possessed, on average, a higher molecular weight and greater number of contiguous hydrophobic amino acids and low complexity regions. Conclusions By analysis of the protein features identified here, this study will help predict which mammalian proteins and domains can be successfully expressed in E. coli as soluble product and also which are best targeted for a eukaryotic expression system. In some cases

  5. Atmospheric corrosion in subtropical areas: XRD and electrochemical study of zinc atmospheric corrosion products in the province of Santa Cruz de Tenerife (Canary Islands, Spain)

    Energy Technology Data Exchange (ETDEWEB)

    Morales, J. [Departamento de Quimica Fisica, Universidad de La Laguna, 38071 La Laguna, Tenerife (Spain)]. E-mail: jmorales@ull.es; Diaz, F. [Departamento de Quimica Fisica, Universidad de La Laguna, 38071 La Laguna, Tenerife (Spain); Hernandez-Borges, J. [Departamento de Quimica Analitica, Nutricion y Bromatologia, Universidad de La Laguna, 38071 La Laguna, Tenerife (Spain); Gonzalez, S. [Departamento de Quimica Fisica, Universidad de La Laguna, 38071 La Laguna, Tenerife (Spain)

    2006-02-15

    In the present paper, zinc sheets have been exposed for 4 years to the action of different atmospheres in 35 test sites located in the province of Santa Cruz de Tenerife, Canary Islands, Spain. Corrosion products formed on the surface of the samples have been identified by means of X-ray diffraction (XRD) for the first and second year of exposure. Zincite, hydrozincite, simonkolleite, zinc chlorohydroxysulphate, zinc oxysulphate and zinc hydroxysulphate have been identified in the test sheets. Preliminary results of an electrochemical study of the breakdown potential of zinc samples are also presented in order to test the protective effect of the film formed on the surface of the samples. It was found that the protective effect of this film increases linearly with exposure time.

  6. A comparison of fingerprint sweat corrosion of different alloys of brass.

    Science.gov (United States)

    Sykes, Stephanie; Bond, John W

    2013-01-01

    Fingerprint sweat from 40 donors was deposited onto samples of five α and α + β phase brasses, comprising five alloys with different copper and zinc concentrations, two of which also had the addition of small concentrations of lead. Visual grading of the visibility of the corrosion revealed that brasses with the least amount of zinc produced the most visible and fully formed fingerprints from the most donors. Consideration of previously reported mechanisms for the corrosion of brass suggests red copper (I) oxide as a likely corrosion product for low zinc brasses, and a consideration of the color, composition, and solubility of fingerprint sweat corrosion products suggests that copper (I) oxide produces good contrast and visibility with the brass substrate. Scanning electron microscope images of the corrosion of all five alloys confirmed the enhanced contrast between corroded and uncorroded areas for low zinc alloys. © 2012 American Academy of Forensic Sciences.

  7. CO2 and O2 solubility and diffusivity data in food products stored in data warehouse structured by ontology.

    Science.gov (United States)

    Guillard, Valérie; Buche, Patrice; Dibie, Juliette; Dervaux, Stéphane; Acerbi, Filippo; Chaix, Estelle; Gontard, Nathalie; Guillaume, Carole

    2016-06-01

    This data article contains values of oxygen and carbon dioxide solubility and diffusivity measured in various model and real food products. These data are stored in a public repository structured by ontology. These data can be retrieved through the @Web tool, a user-friendly interface to capitalise and query data. The @Web tool is accessible online at http://pfl.grignon.inra.fr/atWeb/.

  8. Conformations and molecular interactions of poly-γ-glutamic acid as a soluble microbial product in aqueous solutions

    OpenAIRE

    Wang, Ling-Ling; Chen, Jian-Tao; Wang, Long-Fei; Wu, Sha; Zhang, Guang-zhao; Yu, Han-Qing; Ye, Xiao-dong; Shi, Qing-Shan

    2017-01-01

    Soluble microbial products (SMPs) are of significant concern in the natural environment and in engineered systems. In this work, poly-γ-glutamic acid (γ-PGA), which is predominantly produced by Bacillus sp., was investigated in terms of pH-induced conformational changes and molecular interactions in aqueous solutions; accordingly, its sedimentation coefficient distribution and viscosity were also elucidated. Experimental results indicate that pH has a significant impact on the structure and m...

  9. Phenomenology and modeling of particulate corrosion product behavior in Hanford N Reactor primary coolant

    International Nuclear Information System (INIS)

    Bechtold, D.B.

    1983-01-01

    The levels and composition of filterable corrosion products in the Hanford N Reactor Primary Loop are measurable by filtration. The suspended crud level has ranged from 0.0005 ppM to 6.482 ppM with a median 0.050 ppM. The composition approximates magnetite. The particle size distribution has been found in 31 cases to be uniformly a log normal distribution with a count median ranging from 1.10 to 2.31 microns with a median of 1.81 microns, and the geometric standard deviation ranging from 1.60 to 2.34 with a median of 1.84. An auto-correcting inline turbidimeter was found to respond to linearly to suspended crud levels over a range 0.05 to at least 6.5 ppM by direct comparison with filter sample weights. Cause of crud bursts in the primary loop were found to be power decreases. The crud transients associated with a reactor power drop, several reactor shutdowns, and several reactor startups could be modeled consistently with each other using a simple stirred-tank, first order exchange model of particulate between makeup, coolant, letdown, and loosely adherent crud on pipe walls. Over 3/10 of the average steady running particulate crud level could be accounted for by magnetically filterable particulate in the makeup feed. A simulation model of particulate transport has been coded in FORTRAN

  10. Inventory of radioactive corrosion products on the primary surfaces and release during shutdown in Ringhals 2

    International Nuclear Information System (INIS)

    Aronsson, O.

    1994-01-01

    In Ringhals 2 a retrospective study using gamma scans of system surfaces, fuel crud sampling and reactor coolant analyses during operation and shutdown has been done. The data have been used to prepare a balance of activity inventory. The inventory has been fairly stable from 1986 to 1993, expressed as a gamma source term. The steam generator replacement in 1989 removed some 40-50% of the Co-60 inventory in the reactor system. After the steam generator replacement, the gamma source term has got an increasing contribution from Co-58, absolutely as well as relatively. The reason for this is probably the switch from high pH operation to modified pH operation. Corrosion from fresh alloy 690 surfaces in the new steam generators is probably another contributing factor. The inventory and production rate of Co-60 is decreasing over the years. It has also been found that clean-up of the reactor coolant during start-up, operation, and shutdown as well as the fuel pool during refuelling removes about the same amounts of Co-60. (author). 11 figs., 15 refs

  11. Eh and fission product solubilities: two factors in the leaching of UO2

    International Nuclear Information System (INIS)

    Ogard, A.E.; Duffy, C.J.

    1981-01-01

    Eh was found to have a large effect on the dissolution of UO 2 in water at pH 4. As was estimated from thermodynamic data, the solubility was found to decrease as the oxygen fugacity, and therefore the Eh of the water, was decreased. Some of the rare earths and other actinides such as europium, cerium, americium, and plutonium released during the leaching of a spent fuel element behaved differently. These elements were not affected to any large extent by the variation in Eh of these experiments. It has been postulated that these elements reached their solubility limits and precipitated as the spent fuel was leached. 2 figures, 2 tables

  12. Design of Fusion Proteins for Efficient and Soluble Production of Immunogenic Ebola Virus Glycoprotein in Escherichia coli.

    Science.gov (United States)

    Ji, Yang; Lu, Yuan; Yan, Yishu; Liu, Xinxin; Su, Nan; Zhang, Chong; Bi, Shengli; Xing, Xin-Hui

    2018-03-03

    The Ebola hemorrhagic fever caused by Ebola virus is an extremely dangerous disease, and effective therapeutic agents are still lacking. Platforms for the efficient production of vaccines are crucial to ensure quick response against an Ebola virus outbreak. Ebola virus glycoprotein (EbolaGP) on the virion surface is responsible for membrane binding and virus entry, thus becoming the key target for vaccine development. However, heterologous expression of this protein still faces engineering challenges such as low production levels and insoluble aggregation. Here, the authors design and compare various fusion strategies, attaching great importance to the solubility-enhancing effect, and tag removal process. It is found that a C-terminal intein-based tag greatly enhances the solubility of EbolaGP and allows one-step chromatographic purification of the untagged EbolaGP through thiol-catalyzed self-cleavage. The purified untagged EbolaGP alone or with Freund's adjuvant are highly immunogenic, as confirmed in a mouse model. Consequently, the present study puts forward a new strategy for the efficient and soluble expression of untagged immunogenic EbolaGP. The intein-based protein fusion approach may be of importance for the large-scale production of Ebola virus subunit vaccine. © 2018 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

  13. Analysis on the gamma dose distribution by major corrosion products during preventive maintenance period in nuclear power plant

    International Nuclear Information System (INIS)

    Ha, Wi Ho

    2006-02-01

    The information on dose distribution inside the containment building is an essential requirement to make a reduction of radiation exposure as well as effective operation and design of nuclear power plant. After reactor shutdown, radiation exposure to workers mainly occurs during preventive maintenance period due to inspection or repair works of major components. During that period, gamma doses are induced by major corrosion products in the primary coolant system. The radiation exposure to workers has been assessed by using the measurements. The measurements are, of course, a basic and reliable assessment. But the measurement has defect such as limitation of detecting area. In order to improve the defect of the measurements, system for assessment of gamma dose distribution during preventive maintenance period by using computational code was suggested in this study. First, activity of major corrosion products was calculated by using modified CRUDSIM code. Original CRUDSIM code was modified to add evaluation of other major corrosion products besides cobalt isotopes. Modeling of containment building for YGN Unit 3 was then performed. Gamma dose distribution by major corrosion products inside the containment building was calculated by using MCNPX code. Finally, the calculations were mapped for whole space inside the containment building and were compared with the measurements. As a result of this study, the defect of the measurement are supplemented by using computational calculation system, and it is expected that workers can make an effective work plan through providing dose distribution inside the containment building in advance. In addition, this study can be applied to technology development to make an effective containment shielding design of the next generation reactor as well as an improvement of the safety for workers in nuclear power plant

  14. Review of available data on the release, transport and deposition of corrosion products in PWR, BWR and SGHWR systems

    International Nuclear Information System (INIS)

    Taylor, N.K.

    1976-03-01

    A survey has been carried out of data which are relevant to the theoretical and experimental aspects of corrosion product release, transport, activation and deposition and which were available from operational experience of water reactors and associated experiments. The data have been assessed in connection with commercial SGHWR systems with regard to construction, commissioning and operational procedures. A few areas of work where the existing evidence is inconclusive or incomplete are listed. (author)

  15. Corrosion inhibitors for neutral aqueous media based on the products on sugar cane processing. 1.Furfural derivatives as inhibitors

    International Nuclear Information System (INIS)

    Ledovskikh, V.M.; Kamekho Khinnebra, Kh.Kh.

    1993-01-01

    A series of carboxy-, nitrogen- and nitroderivaties of furfural - the main product of sugar cane processing (furancasboxylic acid, 5-nitrofurancarboxylic acid and its salts, furfurine, furfurylamine) was studied as inhibitors of iron and copper, corrosion in aqueous-salt media. Nitrofuroates of sodium and ammonium, which decelerate anode process, intensity cathode one and provide the stable passive state, are considered to be the most effective

  16. High Temperature Corrosion of Superheater Materials for Power Production through Biomass

    DEFF Research Database (Denmark)

    Montgomery, Melanie; Maahn, Ernst emanuel; Nielsen, Karsten agersted

    The aim of the present study has been to establish a fundamental knowledge of the corrosion mechanisms acting on materials for use in biomass fired power plants. The knowledge is created based on laboratory exposures on selected materials in well-defined corrosive gas environments. An experimental...... facility has been established wherein the planned exposures are completed. Specimens were exposed in combined synthetic flue gas at temperatures up to 900C. The specimens could be cooled to 300C below the gas temperature. Gas flow and gas mixture can be varied according to the conditions found in a power......) on the corrosion progress has been investigated.In addition the corrosion behaviour of the same materials was investigated after having been exposed under a cover of ash in air in a furnace at temperatures of 525C, 600C and 700C. The ashes utilised are from a straw-fired power plant and a synthetic ash composed...

  17. CORROSION AND WEAR PROPERTIES OF MATERIALS USED FOR MINCED MEAT PRODUCTION

    DEFF Research Database (Denmark)

    Jellesen, Morten Stendahl; Hansen, Martin Otto Laver; Hilbert, Lisbeth Rischel

    2009-01-01

    measurements. Combined sliding wear and corrosion conditions have been simulated in laboratory using a block-on-ring setup allowing for electrochemical measurements. Detailed information concerning the mechanism of possible material degradation is provided by these results, together with microstructural...

  18. A mechanism for corrosion product deposition on the carbon steel piping in the residual heat removal system of BWRs

    International Nuclear Information System (INIS)

    Aizawa, Motohiro; Chiba, Yoshinori; Hosokawa, Hideyuki; Ohsumi, Katsumi; Uchida, Shunsuke; Ishizawa, Noboru

    2002-01-01

    The dose rate of the residual heat removal (RHR) piping has been considered to be caused by accumulation of insoluble (crud) radioactive corrosion products on carbon steel surfaces. Soft shutdown procedures (i.e., plant shutdown with moderate coolant temperature reduction rate) used to be applied to reduce crud radioactivity release from the fuel surface, but these are no longer used because of the need for shorter plant shutdown times. In order to apply other suitable countermeasures to reduce RHR dose rate, assessment of plant data, experiments on deposition of crud and ion species on carbon steel, and mass balance evaluation of radioactive corrosion products based on plant and laboratory data were carried out and the following findings were made. (1) Deposits of ion species on carbon steel surfaces of the RHR piping was much more numerous than for crud. (2) Ion species accumulation behavior on RHR piping, which is temperature dependent, can be evaluated with the calculation model used for the dehydration reaction of corrosion products generated during the wet lay-up period. (3) Deposition amounts could be reduced to 1/2.5 when the starting RHR system operation temperature was lowered from 155degC to 120degC. (author)

  19. X-ray diffraction phase analysis of crystalline copper corrosion products after treatment in different chloride solutions

    International Nuclear Information System (INIS)

    Chmielova, M.; Seidlerova, J.; Weiss, Z.

    2003-01-01

    The corrosion products Cu 2 (OH) 3 Cl, Cu 2 O, and CuCl 2 were identified on the surface of copper plates after their four days treating in three different sodium chloride, sodium/magnesium, and sodium/calcium chloride solutions using X-ray diffraction powder analysis. However, the quantitative proportions of individual corrosion products differ and depend on the type of chloride solution used. Treating of copper plates only in the sodium chloride solution produced the mixture of corrosion products where Cu 2 O is prevailing over the Cu 2 (OH) 3 Cl and CuCl 2 was not identified. The sample developed after treating of the cooper surface in the sodium/magnesium chloride solution contains Cu 2 (OH) 3 Cl and CuCl 2 prevailing over the Cu 2 O, while the sample developed after treatment of copper in sodium/calcium chloride solution contains Cu 2 (OH) 3 Cl prevailing over CuCl 2 and Cu 2 O was not identified

  20. Surface analysis and depth profiling of corrosion products formed in lead pipes used to supply low alkalinity drinking water.

    Science.gov (United States)

    Davidson, C M; Peters, N J; Britton, A; Brady, L; Gardiner, P H E; Lewis, B D

    2004-01-01

    Modern analytical techniques have been applied to investigate the nature of lead pipe corrosion products formed in pH adjusted, orthophosphate-treated, low alkalinity water, under supply conditions. Depth profiling and surface analysis have been carried out on pipe samples obtained from the water distribution system in Glasgow, Scotland, UK. X-ray diffraction spectrometry identified basic lead carbonate, lead oxide and lead phosphate as the principal components. Scanning electron microscopy/energy-dispersive x-ray spectrometry revealed the crystalline structure within the corrosion product and also showed spatial correlations existed between calcium, iron, lead, oxygen and phosphorus. Elemental profiling, conducted by means of secondary ion mass spectrometry (SIMS) and secondary neutrals mass spectrometry (SNMS) indicated that the corrosion product was not uniform with depth. However, no clear stratification was apparent. Indeed, counts obtained for carbonate, phosphate and oxide were well correlated within the depth range probed by SIMS. SNMS showed relationships existed between carbon, calcium, iron, and phosphorus within the bulk of the scale, as well as at the surface. SIMS imaging confirmed the relationship between calcium and lead and suggested there might also be an association between chloride and phosphorus.

  1. Apparent Solubility of Natural Products Extracted with Near-Critical Carbon Dioxide

    Czech Academy of Sciences Publication Activity Database

    Sovová, Helena

    2012-01-01

    Roč. 3, 12A (2012), s. 958-965 ISSN 2156-8251 R&D Projects: GA TA ČR TA01010578 Institutional support: RVO:67985858 Keywords : supercritical fluid extraction * solubility * adsorption isotherm Subject RIV: CI - Industrial Chemistry, Chemical Engineering http://www.scirp.org/journal/ajac/

  2. High temperature salt corrosion cracking of intermediate products of titanium alloys

    International Nuclear Information System (INIS)

    Sinyavskij, V.S.; Usova, V.V.; Lunina, S.I.; Kushakevich, S.A.; Makhmutova, E.A.; Khanina, Z.K.

    1982-01-01

    The high temperature salt corrosion cracking (HTSCC) of intermediate products from titanium base alloys in the form of hot rolled plates and rods has been studied. The investigated materials are as follows: VT20 pseudo-α-alloy, VT6 and VT14 α+β alloys; the comparison has been carried out with commercial titanium and low-alloyed OT4-1 α-alloy. The experiments have been held at 400 and 500 deg C, defining different stress levels: 0.4; 0.5; 0.75 and 0.9 tausub(0.2). The test basis - not less than 100 h. Standard tensile samples of circular cross section with NaCl (approximately 0.2-0.3 mg/cm 2 ) salt coatings, cut off from hot-rolled rods along the direction of rolling and hot-rolled plates along and across the direction of rolling have been tested. It has been extablished before hand that the notch doesn't affect the resistance of titanium alloys to HTSCC. The sensitivity of titanium alloy subproducts to HTSCC is estimated as to the time until the failure of the sample with salt coatings and without them. It is shown that salt coating practically doesn't affect the behaviour of titanium, that allows to consider it to be resistant to HTSCC. Titanium alloys alloying with β-isomorphous stabilizing additions increases it's HTSCC resistance. Vanadium alloying of the alloy (VT6 alloy of Ti-Al-V system) produces a favourable effect; intermediate products of VT14 (α+β) alloy (Ti-Al-V-Mo system), containing two β-stabilizing additions-vanadium and molybdenum, have satisfactory HTSCC resistance. It is shown that by changes is mechanical properties of alloys during HTSCC one can indirectly judge about their HTSCC sensitivity

  3. The enhancing power of iodide on corrosion prevention of mild steel in the presence of a synthetic-soluble Schiff-base: Electrochemical and surface analyses

    International Nuclear Information System (INIS)

    Lashgari, Mohsen; Arshadi, Mohammad-Reza; Miandari, Somaieh

    2010-01-01

    The inhibitory action of N,N'-1,3-propylen-bis(3-methoxysalicylidenimine) {PMSI} on mild steel corrosion in sulfuric acid medium was investigated through electrochemical methods and evaluations based on infrared spectroscopy and scanning electron micrographs. The studies revealed that the molecule is a good mixed-type inhibitor (mostly anodic), acts as a multi-dentate ligand and repels the corrosive agents by hydrophobic forces. Its adsorption on metal surface has a physicochemical nature and obeys the Langmuir isotherm. At a critical (optimum) concentration, an anomalous inhibitory behavior was observed and interpreted at microscopic level by means of desorption/adsorption process and horizontal ↔vertical hypothesis. The addition of iodide into acid moreover causes a synergistic influence, a substantial enhancement on inhibitory performance. Finally, using isolated inhibitor calculations at B3LYP/6-31G + (d,p) level of theory, the equilibrium geometry of PMSI was determined and the energy required for hindrance avoidance was predicted.

  4. Basic aspects of the carbon dioxide corrosion in oil and gas production; Aspectos basicos de la corrosion por dioxido de carbono en la produccion de petroleo y gas

    Energy Technology Data Exchange (ETDEWEB)

    Angulo Macias, J.

    2010-07-01

    Carbon dioxide (CO{sub 2}) is a non-corrosive gas within the driven conditions in the oil and gas industry, but the presence of water converts it, maybe, in the most important component in the corrosive processes in this industry. Corrosion has an important impact inside the oil and gas companies, no only in economics but also in safety, environmental and social aspects. After several decades of investigation of these corrosion processes, there are still several mechanisms not fully understood. (Author) 19 refs.

  5. In vitro solubility of calcium, iron and zinc in relation to phytic acid levels in rice-based consumer products in China

    NARCIS (Netherlands)

    Liang, J.; Han, B.Z.; Nout, M.J.R.; Hamer, R.J.

    2010-01-01

    In vitro solubility of calcium, iron and zinc in relation to phytic acid (PA) levels in 30 commercial rice-based foods from China was studied. Solubility of minerals and molar ratios of PA to minerals varied with degrees of processing. In primary products, [PA]/[Ca] values were less than 5 and

  6. Fighting corrosion in India

    Energy Technology Data Exchange (ETDEWEB)

    Rajagopalan, K S; Rangaswamy, N S

    1979-03-01

    A survey covers the cost of corrosion in India; methods of preventing corrosion in industrial plants; some case histories, including the prevention of corrosion in pipes through which fuels are pumped to storage and the stress-corrosion cracking of evaporators in fertilizer plants; estimates of the increase in demand in 1979-89 for anticorrosion products and processes developed by the Central Electrochemical Research Institute (CECRI) at Karaikudi, India; industries that may face corrosion problems requiring assistance from CECRI, including the light and heavy engineering structural, and transport industries and the chemical industry; and some areas identified for major efforts, including the establishment of a Corrosion Advisory Board with regional centers and the expansion of the Tropical Corrosion Testing Station at Mandapam Camp, Tamil Nadu.

  7. High temperature corrosion of superheater materials for power production through biomass

    Energy Technology Data Exchange (ETDEWEB)

    Gotthjaelp, K.; Broendsted, P. [Forskningscenter Risoe (Denmark); Jansen, P. [FORCE Institute (Denmark); Montgomery, M.; Nielsen, K.; Maahn, E. [Technical Univ. of Denmark, Corrosion and Surface Techn. Inst. of Manufacturing Engineering (Denmark)

    1996-08-01

    The aim of the present study has been to establish a fundamental knowledge of the corrosion mechanisms acting on materials for use in biomass fired power plants. The knowledge is created based on laboratory exposures of selected materials in well-defined corrosive gas environments. The experiments using this facility includes corrosion studies of two types of high temperature resistant steels, Sanvik 8LR30 (18Cr 10Ni Ti) and Sanicro 28 (27Cr 31Ni 4Mo), investigated at 600 deg. C in time intervals up to 300 hours. The influence of HCl (200 ppm) and of SO{sub 2} (300 ppm) on the corrosion progress has been investigated. In addition the corrosion behaviour of the same materials was investigated after having been exposed under a cover of ash in air in a furnace at temperatures of 525 deg. C, 600 deg. C, and 700 deg. C. The ashes utilised are from a straw fired power plant and a synthetic ash composed of potassium chloride (KCl) and potassium sulphate (K{sub 2}SO{sub 4}). Different analysis techniques to characterise the composition of the ash coatings have been investigated in order to judge the reliability and accuracy of the SEM-EDX method. The results are considered as an important step towards a better understanding of the high temperature corrosion under the conditions found in biomass fired power plants. One of the problems to solve in a suggested subsequent project is to combine the effect of the aggressive gases (SO{sub 2} and HCl) and the active ash coatings on high temperature corrosion of materials. (EG) 20 refs.

  8. Standard test method for determining susceptibility to stress-corrosion cracking of 2XXX and 7XXX Aluminum alloy products

    CERN Document Server

    American Society for Testing and Materials. Philadelphia

    1998-01-01

    1.1 This test method covers a uniform procedure for characterizing the resistance to stress-corrosion cracking (SCC) of high-strength aluminum alloy wrought products for the guidance of those who perform stress-corrosion tests, for those who prepare stress-corrosion specifications, and for materials engineers. 1.2 This test method covers method of sampling, type of specimen, specimen preparation, test environment, and method of exposure for determining the susceptibility to SCC of 2XXX (with 1.8 to 7.0 % copper) and 7XXX (with 0.4 to 2.8 % copper) aluminum alloy products, particularly when stressed in the short-transverse direction relative to the grain structure. 1.3 The values stated in SI units are to be regarded as standard. The inch-pound units in parentheses are provided for information. This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and de...

  9. Ab Initio investigation of chloroaqualead (II) complexes as possible corrosion products in Super Critical Water Cooled Reactor (SCWR)

    Energy Technology Data Exchange (ETDEWEB)

    Anzelj, D.; Pye, C.C., E-mail: diki1979@hotmail.com, E-mail: cory.pye@smu.ca [Saint Mary' s University, Halifax, NS (Canada)

    2015-07-01

    One of the undesirable processes hindering development of Generation IV SCWR is the possibility of corrosion of construction material. Formation of corrosion products such as metal-ligand complexes is poorly understood both experimentally and computationally. It is essential to predict and control its water chemistry to ensure sustainability of SCWR. Pressurized and heated solutions are challenging for experimental research; computational method becomes an important research tool. A series of ab initio calculations of chloroaqualead (II) complexes have been performed at HF, MP2 and B3LYP levels of theory with CEP-121G, LANL2DZ, SDD basis sets for Pb and 6-31G*, 6-31+G*, 6-311+G* for water. (author)

  10. Corrosion behavior of stainless steel in bio diesel production; Comportamento quanto a corrosao de acos inoxidaveis na producao do biodiesel

    Energy Technology Data Exchange (ETDEWEB)

    Miranda, E.F. de [ArcelorMittal Sao Paulo Servicos, SP (Brazil); Moreira, M.C.; Lebrao, S.M.G. [Centro Universitario do Instituto Maua de Tecnologia, Sao Paulo, SP (Brazil)], e-mail: susana.lebrao@maua.br

    2010-07-01

    Biodiesel has become more attractive due to the benefits to the environment, mainly because it is a renewable resource. However, the main barrier to biodiesel is it cost. One factor which is charged to marketing is the use of stainless steel throughout the production line, the most used is AISI 304. To evaluate more economical stainless steels, weight loss and stress corrosion tests were performed on samples of AISI 304 and 439 in methanol PS X30% sodium methylate solution, crude soybean oil, glycerol and biodiesel for about two hundred and fifty days. The mass loss was negligible, and there was complete absence of pitting and stress corrosion cracking in all media studied, showing that both alloys are suitable for the manufacture of such equipment. (author)

  11. Ab Initio investigation of chloroaqualead (II) complexes as possible corrosion products in Super Critical Water Cooled Reactor (SCWR)

    International Nuclear Information System (INIS)

    Anzelj, D.; Pye, C.C.

    2015-01-01

    One of the undesirable processes hindering development of Generation IV SCWR is the possibility of corrosion of construction material. Formation of corrosion products such as metal-ligand complexes is poorly understood both experimentally and computationally. It is essential to predict and control its water chemistry to ensure sustainability of SCWR. Pressurized and heated solutions are challenging for experimental research; computational method becomes an important research tool. A series of ab initio calculations of chloroaqualead (II) complexes have been performed at HF, MP2 and B3LYP levels of theory with CEP-121G, LANL2DZ, SDD basis sets for Pb and 6-31G*, 6-31+G*, 6-311+G* for water. (author)

  12. Corrosion and solubility in a TSP-buffered chemical environment following a loss of coolant accident: Part 4 – Integrated chemical effects testing

    Energy Technology Data Exchange (ETDEWEB)

    Ali, Amir; LaBrier, Daniel [Department of Nuclear Engineering, University of New Mexico (United States); Blandford, Edward, E-mail: edb@unm.edu [Department of Nuclear Engineering, University of New Mexico (United States); Howe, Kerry [Department of Civil Engineering, University of New Mexico (United States)

    2016-04-15

    Highlights: • Integrated test explored the material release of a postulated large break LOCA. • Aluminum concentration was very low (<0.1 mg/L) throughout the test duration. • Zinc concentration was low (<1 mg/L) in TSP-buffered system. • Calcium release showed two distinguished release zones: prompt and meta-stable. • Copper and iron has no distinguishable concentration up to first 24 h of testing. - Abstract: This paper presents the results of an integrated chemical effects experiment executed under conditions representative of the containment pool following a postulated loss of coolant accident (LOCA) at the Vogtle nuclear power plant, operated by the Southern Nuclear Operating Company (SNOC). This test was conducted for closure of a series of bench scale experiments conducted to investigate the effect of the presence of trisodium phosphate (TSP) on the corrosion and release of aluminum (Howe et al., 2015) and zinc (Pease et al., 2015) from metallic surfaces, and calcium from NUKON fiberglass insulation (Olson et al., 2015) . The integrated test was performed in the Corrosion/Chemical Head Loss Experimental (CHLE) facility with representative amounts of zinc, aluminum, carbon steel, copper, NUKON fiberglass, and latent debris. The test was conducted using borated TSP-buffered solution under a post-LOCA prototypical temperature profile lasting for 30 days. The results presented in this article demonstrate trends for zinc, aluminum, and calcium release that are consistent with separate bench scale testing and previous integrated tests under TSP conditions. The release rate and maximum concentrations of the released materials were slightly different than the separate effect testing as a result of different experimental conditions (temperature, surface area-to-water volume ratio) and/or the presence of other metals and chemicals in the integrated test. Samples of metal coupons and fiberglass were selected for analysis using Scanning Electron Microscopy

  13. Corrosion and solubility in a TSP-buffered chemical environment following a loss of coolant accident: Part 4 – Integrated chemical effects testing

    International Nuclear Information System (INIS)

    Ali, Amir; LaBrier, Daniel; Blandford, Edward; Howe, Kerry

    2016-01-01

    Highlights: • Integrated test explored the material release of a postulated large break LOCA. • Aluminum concentration was very low (<0.1 mg/L) throughout the test duration. • Zinc concentration was low (<1 mg/L) in TSP-buffered system. • Calcium release showed two distinguished release zones: prompt and meta-stable. • Copper and iron has no distinguishable concentration up to first 24 h of testing. - Abstract: This paper presents the results of an integrated chemical effects experiment executed under conditions representative of the containment pool following a postulated loss of coolant accident (LOCA) at the Vogtle nuclear power plant, operated by the Southern Nuclear Operating Company (SNOC). This test was conducted for closure of a series of bench scale experiments conducted to investigate the effect of the presence of trisodium phosphate (TSP) on the corrosion and release of aluminum (Howe et al., 2015) and zinc (Pease et al., 2015) from metallic surfaces, and calcium from NUKON fiberglass insulation (Olson et al., 2015) . The integrated test was performed in the Corrosion/Chemical Head Loss Experimental (CHLE) facility with representative amounts of zinc, aluminum, carbon steel, copper, NUKON fiberglass, and latent debris. The test was conducted using borated TSP-buffered solution under a post-LOCA prototypical temperature profile lasting for 30 days. The results presented in this article demonstrate trends for zinc, aluminum, and calcium release that are consistent with separate bench scale testing and previous integrated tests under TSP conditions. The release rate and maximum concentrations of the released materials were slightly different than the separate effect testing as a result of different experimental conditions (temperature, surface area-to-water volume ratio) and/or the presence of other metals and chemicals in the integrated test. Samples of metal coupons and fiberglass were selected for analysis using Scanning Electron Microscopy

  14. Cesium release from ceramic waste form materials in simulated canister corrosion product containing solutions

    Energy Technology Data Exchange (ETDEWEB)

    Vittorio, Luca; Drabarek, Elizabeth; Chronis, Harriet; Griffith, Christopher S

    2004-07-01

    It has previously been demonstrated that immobilization of Cs{sup +} and/or Sr{sup 2+} sorbed on hexagonal tungsten oxide bronze (HTB) adsorbent materials can be achieved by heating the materials in air at temperatures in the range 500 - 1300 deg C. Highly crystalline powdered HTB materials formed by heating at 800 deg C show leach characteristics comparable to Cs-containing hot-pressed hollandites in the pH range from 0 to 12. As a very harsh leaching test, and also to model in a basic manner, leaching in the presence of canister corrosion products in oxidising environments, leaching of the bronzoid phases has been undertaken in Fe(NO{sub 3}){sub 3} solutions of increasing concentration. This is done in comparison with Cs -hollandite materials in order to compare the leaching characteristics of these two materials under such conditions. Both the Cs-loaded bronze and hollandite materials leach severely in Fe(NO{sub 3}){sub 3} losing virtually all of the immobilized Cs in a period of four days at 150 deg C. Total release of Cs and conversion of hollandite to titanium and iron titanium oxides begins to be observed at relatively low concentrations and is virtually complete after four days reaction in 0.5 mol/L Fe(NO{sub 3}){sub 3}. In the case of the bronze, all of the Cs is also extracted but the HTB structure is preserved. The reaction presumably involves an ion-exchange mechanism and iron oxide with a spinel structure is also observed at high Fe concentrations. (authors)

  15. Cesium release from ceramic waste form materials in simulated canister corrosion product containing solutions

    International Nuclear Information System (INIS)

    Vittorio, Luca; Drabarek, Elizabeth; Chronis, Harriet; Griffith, Christopher S.

    2004-01-01

    It has previously been demonstrated that immobilization of Cs + and/or Sr 2+ sorbed on hexagonal tungsten oxide bronze (HTB) adsorbent materials can be achieved by heating the materials in air at temperatures in the range 500 - 1300 deg C. Highly crystalline powdered HTB materials formed by heating at 800 deg C show leach characteristics comparable to Cs-containing hot-pressed hollandites in the pH range from 0 to 12. As a very harsh leaching test, and also to model in a basic manner, leaching in the presence of canister corrosion products in oxidising environments, leaching of the bronzoid phases has been undertaken in Fe(NO 3 ) 3 solutions of increasing concentration. This is done in comparison with Cs -hollandite materials in order to compare the leaching characteristics of these two materials under such conditions. Both the Cs-loaded bronze and hollandite materials leach severely in Fe(NO 3 ) 3 losing virtually all of the immobilized Cs in a period of four days at 150 deg C. Total release of Cs and conversion of hollandite to titanium and iron titanium oxides begins to be observed at relatively low concentrations and is virtually complete after four days reaction in 0.5 mol/L Fe(NO 3 ) 3 . In the case of the bronze, all of the Cs is also extracted but the HTB structure is preserved. The reaction presumably involves an ion-exchange mechanism and iron oxide with a spinel structure is also observed at high Fe concentrations. (authors)

  16. Electrochemical formation of carbonated corrosion products on carbon steel in deaerated solutions

    International Nuclear Information System (INIS)

    Refait, Ph.; Bourdoiseau, J.A.; Jeannin, M.; Nguyen, D.D.

    2012-01-01

    Highlights: ► Green rust is electro-generated at low NaHCO 3 concentration (0.003 mol dm −3 ). ► Chukanovite and carbonated green rust are obtained in NaHCO 3 + Na 2 SO 4 deaerated electrolytes. ► The mechanisms of formation of carbonated corrosion products of carbon steel are specified. - Abstract: To investigate the nature and properties of carbonated rust layers, carbon steel electrodes were polarised anodically at a potential ∼100–200 mV higher than the open circuit potential in NaHCO 3 solutions (0.003, 0.1 and 1 mol dm −3 ) continuously deaerated by an argon flow. X-ray diffraction and μ-Raman spectroscopy were used to identify the electro-generated compounds. GR(CO 3 2− ) (=Fe II 4 Fe III 2 (OH) 12 CO 3 ·4H 2 O) is observed at 0.003 and 0.1 mol dm −3 NaHCO 3 whereas FeCO 3 is obtained at the largest concentration (1 mol dm −3 ). GR(CO 3 2− ) is accompanied by magnetite Fe 3 O 4 at the lowest NaHCO 3 concentration. The current density decreases to negligible values in each case, indicating that a passive film also forms independently of the nature of the carbonated compound. Experiments were performed similarly in solutions of NaHCO 3 and Na 2 SO 4 . Chukanovite Fe 2 (OH) 2 CO 3 could be obtained in solutions containing 0.03 mol dm −3 of each salt. In contrast with the results obtained in the solutions free of sulphate, the current density remains important during the formation of the rust layer

  17. Research and development on is process components for hydrogen production. (2) Corrosion resistance of glass lining in high temperature sulfuric acid

    International Nuclear Information System (INIS)

    Tanaka, Nobuyuki; Iwatsuki, Jin; Kubo, Shinji; Terada, Atsuhiko; Onuki, Kaoru

    2009-01-01

    Japan Atomic Energy Agency has been conducting a research and development on hydrogen production system using High Temperature Gas-Cooled Reactor. As a part of this effort, thermochemical water-splitting cycle featuring iodine- and sulfur-compounds (IS process) is under development considering its potential of large-scale economical hydrogen production. The IS process constitutes very severe environments on the materials of construction because of the corrosive nature of process chemicals, especially of the high temperature acidic solution of sulfuric acid and hydriodic acid dissolving iodine. Therefore, selection of the corrosion-resistant materials and development of the components has been studied as a crucial subject of the process development. This paper discusses corrosion resistance of commercially available glass-lining material in high temperature sulfuric acid. Corrosion resistance of a soda glass used for glass-lining was examined by immersion tests. The experiments were performed in 47-90wt% sulfuric acids at temperatures of up to 400degC and for the maximum immersion time of 100 hours using an autoclave designed for the concerned tests. In every condition tested, no indication of localized corrosion such as defect formation or pitting corrosion was observed. Also, the corrosion rates decreased with the progress of immersion, and were low enough (≅0.1 mm/year) after 60-90 hours of immersion probably due to formation of a silica rich surface. (author)

  18. Production of a soluble recombinant prion protein fused to blue fluorescent protein without refolding or detergents in Escherichia coli cells.

    Science.gov (United States)

    Arii, Yasuhiro; Yamaguchi, Hidenori; Fukuoka, Shin-Ichi

    2007-10-01

    The physiological function of prion proteins (PrP) remains unclear. To investigate the physiological relevance of PrP, we constructed a fusion protein of PrP with enhanced blue fluorescent protein (PrP-EBFP) to quantify the interaction of PrP with other molecules. Production of soluble PrP-EBFP was achieved by lowering the expression temperature in Escherichia coli (E. coli) cells to 15 degrees C. Soluble PrP-EBFP was purified on cation exchange and heparin-affinity columns to yield high purity protein. This is the first report of the preparation of soluble recombinant PrP without refolding following solubilization using denaturants or disruption using detergents. To confirm the integrity of PrP-EBFP, anisotropy was estimated under physiological conditions in the presence of heparin, which interacts with PrP. The dissociation constant was determined to be 0.88+/-0.07 microM. PrP-EBFP should be useful in the quantification of PrP interactions with other molecules.

  19. Analysis of corrosion products in some metallic statuettes of the Museum of Archaeology and Ethnology (MAE-USP)

    International Nuclear Information System (INIS)

    Rizzutto, Marcia A.; Tabacniks, Manfredo H.; Added, Nemitala; Barbosa, Marcel D.L.; Lima, Silvia Cunha; Melo, Hercilio G.; Neiva, Augusto C.

    2005-01-01

    The recent acquisition of a sealed chamber with controlled humidity by the Museum of Archaeology and Ethnology of the University of Sao Paulo (MAE-USP) requires new methods for conservation and restoration of metallic objects in its collection. To establish new procedures for the identification of corrosion mechanisms and agents in the exhibition environment, and to set up new standards for conservation of the museum's collection, Proton Induced X-Ray Emission (PIXE) elementary analysis of some metallic objects is in progress, using the external beam facility at LAMFI. The first analysis involved metallic objects from the collection of MAE, two African statuettes 'male Edans' from the Ogboni Secret Society, of the Ilobu-Ioruba ethnic group, one pectoral adornment from the Chimu culture, Peru and one anthropomorphic pendant from the Tairona culture, Colombia. The in air non destructive PIXE analysis allowed identifying major and some secondary components in the alloys and in the corrosion products on the samples, data that were used to identify the corrosion sources and to set up the exhibition environment. (author)

  20. The solubility of solid fission products in carbides and nitrides of uranium and plutonium: Pt.2. Solubility rules based on lattice parameter differences

    International Nuclear Information System (INIS)

    Benedict, U.

    1977-01-01

    The Relative Lattice Parameter Difference (RLPD) is defined for a solute element with respect to cubic carbides and nitrides of uranium and plutonium as solvents. Rules are given for the relationship between the solubility and the RLPD. NaCl type monocarbides with RLPD's from -10.2% to +7.8% are completely miscible with UC and PuC. NaCl type mononitrides with RLPD's from -7.5% to +8.5% are completely miscible with UN and PuN. The solubility in the sesquicarbides increases with decreasing RPLD and becomes complete in Pu 2 C 3 at RLPD = +4%, and in U 2 C 3 at RLPD approximately +1.5%. Solubilities are predicted on the basis of these rules for the cases where no experimental results are available

  1. Utilization of Condensed Distillers Solubles as Nutrient Supplement for Production of Nisin and Lactic Acid from Whey

    Science.gov (United States)

    Liu, Chuanbin; Hu, Bo; Chen, Shulin; Glass, Richard W.

    The major challenge associated with the rapid growth of the ethanol industry is the usage of the coproducts, i.e., condensed distillers solubles (CDS) and distillers dried grains, which are currently sold as animal feed supplements. As the growth of the livestock industries remains flat, alternative usage of these coproducts is urgently needed. CDS is obtained after the removal of ethanol by distillation from the yeast fermentation of a grain or a grain mixture by condensing the thin stillage fraction to semisolid. In this work, CDS was first characterized and yeast biomass was proven to be the major component of CDS. CDS contained 7.50% crude protein but with only 42% of that protein being water soluble. Then, CDS was applied as a nutrient supplement for simultaneous production of nisin and lactic acid by Lactococcus lactis subsp. lactis (ATCC 11454). Although CDS was able to support bacteria growth and nisin production, a strong inhibition was observed when CDS was overdosed. This may be caused by the existence of the major ethanol fermentation byproducts, especially lactate and acetate, in CDS. In the final step, the CDS based medium composition for nisin and lactic acid production was optimized using response surface methodology.

  2. Reduction transport of corrosion products through the secondary circuit by increasing the dosage of ammonia; Reduccion del transporte de productos de corrosion a traves del circuito secundario mediante el aumento de la dosificacion de amoniaco

    Energy Technology Data Exchange (ETDEWEB)

    Espanol, J.; Boronat, M.

    2015-07-01

    Reduce transport of corrosion products through the Secondary Circuit, mainly magnetite, by increasing the dosage of ammonia in order to reduce oxides accumulation in the Steam Generators top of tube sheet where become hard sludge, as one of the TTS denting mitigation actions. (Author)

  3. Reaction products and corrosion of molybdenum electrode in glass melt containing antimony oxides and sodium sulfate

    Czech Academy of Sciences Publication Activity Database

    Matěj, J.; Langrová, Anna

    2012-01-01

    Roč. 56, č. 3 (2012), s. 280-285 ISSN 0862-5468 Institutional support: RVO:67985831 Keywords : antimony oxides * corrosion * glass melt * Molybdenum electrode * sulfate Subject RIV: DD - Geochemistry Impact factor: 0.418, year: 2012 http://www.ceramics-silikaty.cz/2012/pdf/2012_03_280.pdf

  4. Spectroscopic study of the final protective corrosion product on weathering steel

    International Nuclear Information System (INIS)

    Yamashita, M.; Misawa, T.

    1998-01-01

    Recent progress in understanding the structure and properties of final protective rust layer on weathering steel and its application for structural steels is shown based on the data obtained mainly by spectroscopic characterization. The main constituent of the weathering steel rust layer is changed with exposure period from γ- FeOOH (less than a few years) via, amorphous substance (several years), to α-FeOOH goethite phase (decades). The corrosion rate of the weathering steel decreased with this phase transformation. The final protective rust layer possesses the structure of α- (Fe 1 - X p Cr x)O OH, Cr substitute goethite; the crystal size decreases with its Cr-content. It is shown that the Cr content in the Cr-substituted goethite increases gradiently with reaching the rust/steel interface. This increase in the Cr content and resultant aggregation of fine crystals lead a densely packed Cr-substituted goethite rust layers which provides higher protective ability for atmospheric corrosives. It is found that the Cr-substituted goethite possesses the cation selective ability at the vicinity of the rust/steel interface where the Cr content can be estimated approximately 5-10 mass %. Thus, the final protective rust layer of the Cr-substituted goethite impedes the penetration of aggressive corrosive anions such as Cl - and SO 4 2- , besides the physically prevention effect of its densely aggregated structure for corrosive penetration. It is found that Cr 2 (SO 4 ) 3 is effective for obtaining the final protective rust layer in a short period. SO 4 2 accelerates rust formation and Cr 3- substitutes goethite crystal lattice point at the initial stage of corrosion; resultantly the rust layer formed suppresses dissolution of the steel even in the severe environment. (Author)

  5. Deposition of radioactive corrosion products on the internal surfaces of tube elements in gaseous phase of dissociating system N2O4 reversible 2NO2 reversible 2NO+O2

    International Nuclear Information System (INIS)

    Gol'tsev, V.P.; Dolgov, V.M.; Katanaev, A.O.

    1979-01-01

    Analysis of experimental data, obtained as a result of γ-scanning of tube element samples of loop assembling with dissociating coolant contacting with N 2 O 4 gaseous phase is presented. Radioactive depositions are differentiated on fixed and unfixed ones by the method of radiochemical analysis. The data obtained have made it possible to establish the analytical form of radioactive element distribution functions along the piping length. It is noted, that relative quantities of radioactive isotopes, existing in fixed and unfixed depositions vary with temperature. The fraction of soluble forms of corrosion radioactive products in unfixed depositions increases both with the decrease of temperature and after passing of radioactive impurity through the zone of liquid coolant

  6. Iron corrosion inhibition by phosphonate complexes of rare earth metals

    International Nuclear Information System (INIS)

    Kuznetsov, Yu.I.; Raskol'nikov, A.F.; Starobinskaya, I.V.; Alekseev, V.N.

    1993-01-01

    Capability is shown of trivalent rare earth nitrilotrimethylphosphonates (R= Ce, Pr, Nd, Eu, Lu, Y) to retard steel corrosion in soft water due to the formation of slightly soluble hydroxides on steel surface. The protective film is produced as a result of electrophilic substitution of nascent iron cations for rare earth ions in near the surface layer. The introduction of rare earth cations into the protective film is ascertained by Auger spectroscopy in combination with the argon spraying. A quantitative interrelation between the protective effectiveness and solubility product of rare earth hydroxides is revealed

  7. Monitoring Microbially Influenced Corrosion

    DEFF Research Database (Denmark)

    Hilbert, Lisbeth Rischel

    and diffusional effects and unreliable corrosion rates, when biofilm and ferrous sulphide corrosion products cover the steel surface. Corrosion rates can be overestimated by a factor of 10 to 100 by electrochemical techniques. Weight loss coupons and ER are recommended as necessary basic monitoring techniques......Abstract Microbially influenced corrosion (MIC) of carbon steel may occur in media with microbiological activity of especially sulphate-reducing bacteria (SRB). The applicability and reliability of a number of corrosion monitoring techniques for monitoring MIC has been evaluated in experiments....... EIS might be used for detection of MIC as the appearance of very large capacitances can be attributed to the combined ferrous sulphide and biofilm formation. Capacitance correlates directly with sulphide concentration in sterile sulphide media. Keywords: Corrosion monitoring, carbon steel, MIC, SRB...

  8. SRB seawater corrosion project

    Science.gov (United States)

    Bozack, M. J.

    1991-01-01

    The corrosion behavior of 2219 aluminum when exposed to seawater was characterized. Controlled corrosion experiments at three different temperatures (30, 60 and 100 C) and two different environments (seawater and 3.5 percent salt solution) were designed to elucidate the initial stages in the corrosion process. It was found that 2219 aluminum is an active catalytic surface for growth of Al2O3, NaCl, and MgO. Formation of Al2O3 is favored at lower temperatures, while MgO is favored at higher temperatures. Visible corrosion products are formed within 30 minutes after seawater exposure. Corrosion characteristics in 3.5 percent salt solution are different than corrosion in seawater. Techniques utilized were: (1) scanning electron microscopy, (2) energy dispersive x-ray spectroscopy, and (3) Auger electron spectroscopy.

  9. The solubility of solid fission products in carbides and nitrides of uranium and plutonium. Part I: literature review on experimental results

    International Nuclear Information System (INIS)

    Benedict, U.

    1977-01-01

    This review compiles the available data on the solubility of the most important non-volatile fission products in the carbides, nitrides, and carbonitrides of uranium and plutonium. It includes some elements which are not fission products, but belong to a group of the Periodic Table which contains one or more fission products elements

  10. The study on the magnetic filter using the rotation of permanent magnets for separation of radioactive corrosion products

    International Nuclear Information System (INIS)

    Song, M.C.; Lee, K.J.

    2004-01-01

    Most of the insoluble radioactive corrosion products have the characteristic of showing strong ferrimagnetism. Along with the new development and production of permanent magnets which generate much stronger magnetic field than conventional permanent magnets, new type of magnetic filter that can separate radioactive corrosion products efficiently and eventually reduce the radiation exposure of the personnel at a nuclear power plant is suggested. This new type of separator with novel geometry consists of an inner and an outer magnet assembly, a coolant channel and a container surrounding the outer magnet assembly. The particulates are separated from the coolant by the alternating magnetic fields that are generated by shift arrangement of permanent magnets. This study describes of experimental results performed with the different flow rates, rotation velocities of magnet assemblies, particle size and various materials. The efficiency of magnetic filter tends to increase as the flow rate is lower, and particle size is bigger. The rotating velocity of magnet assembly has also some influences on the separation efficiency. This new magnetic filter shows good performance results in filtering magnetite, cobalt ferrite and nickel ferrite except hematite, which is a kind of anti-ferromagnetic material, from aqueous coolant simulation. At the above 5 μm of particle size, the separation efficiencies are over than 90%. (author)

  11. Development of moving alternating magnetic filter using permanent magnet for removal of radioactive corrosion product from nuclear power plant

    International Nuclear Information System (INIS)

    Song, M. C.; Kim, S. I.; Lee, K. J.

    2002-01-01

    Radioactive Corrosion Products (CRUD) which are generated by the neutron activation of general corrosion products at the nuclear power plant are the major source of occupational radiation exposure. Most of the CRUD has a characteristic of showing strong ferrimagnetisms. Along with the new development and production of permanent magnet (rare earth magnet) which generates much stronger magnetic field than the conventional magnet, new type of magnetic filter that can separate CRUD efficiently and eventually reduce radiation exposure of personnel at nuclear power plant is suggested. This separator consists of inner and outer magnet assemblies, coolant channel and container surrounding the outer magnet assembly. The rotational motion of the inner and outer permanent magnet assemblies surrounding the coolant channel by driving motor system produces moving alternating magnetic fields in the coolant channel. The CRUD can be separated from the coolant by the moving alternating magnetic field. This study describes the results of preliminary experiment performed with the different flow rates of coolant and rotation velocities of magnet assemblies. This new magnetic filter shows better performance results of filtering the magnetite at coolant (water). Flow rates, rotating velocities of magnet assemblies and particle sizes turn out to be very important design parameters

  12. Inhibitor effect on corrosion of titanium alloys in muriatic solutions of titanium-magnesium production

    International Nuclear Information System (INIS)

    Dobrunov, Yu.V.; Volynskij, V.V.; Kolobov, G.A.; Kuznetsov, S.I.

    1977-01-01

    Corrosion tests of titanium alloys VTI-0, OT4, VT5-1 and steel Kh18N1OT in 10% and 18% HCl with additions of carnallite at 40 deg C have been carried out. It has been established that titanium alloys in 10% and 18% HCl containing 5 and 10% carnallite are sufficiently corrosion resistant in the presence of 0.1-1% FeCl or HNO 3 and can be used for manufacturing the equipment of recirculation gas scrubbers. Steel Kh18N10T is unstable in all the media tested. It is subjected to intensive pitting. Specimens of steel Kh18N10T have also revealed edge cracking

  13. Components made of corrosion-resistent zirconium alloy and method for its production

    International Nuclear Information System (INIS)

    Hanneman, R.E.; Urquhart, A.W.; Vermilyea, D.A.

    1977-01-01

    The invention deals with a method to increase the resistance of zirconium alloys to blister corrosion which mainly occurs in boiling-water nuclear reactors. According to the method described, the surface of the alloy body is coated with a thin film of a suitable electronically conducting material. Gold, silver, platinum, nickel, chromium, iron and niobium are suitable as coating materials. The invention is more closely explained by means of examples. (GSC) [de

  14. Sulfide Production and Corrosion in Seawater During Exposure to FAME Alternative Fuel

    Science.gov (United States)

    2012-06-01

    transporting fatty acid methyl ester ( FAME ] alternative diesel fuel in contact with natural seawater under anaerobic conditions. Coastal Key West...Glycerol Fatty Acid Methyl Ester Exposure Chamber Anaerobic Chamber - bal. N2,10% H2, 0.1% C02 - maintain pH ~8 Polarization Resistance (Rp...and Corrosion in Seawater During Exposure to FAME Alternative Fuel Jason 5. Lee Richard I. Ray BrendaJ. Little Naval Research Laboratory Stennis

  15. Corrosion and anticorrosion. Industrial practice

    International Nuclear Information System (INIS)

    Beranger, G.; Mazille, H.

    2002-01-01

    This book comprises 14 chapters written with the collaboration of about 50 French experts of corrosion. It is complementary to another volume entitled 'corrosion of metals and alloys' and published by the same editor. This volume comprises two parts: part 1 presents the basic notions of corrosion phenomena, the properties of surfaces, the electrochemical properties of corrosion etc.. Part 2 describes the most frequent forms of corrosion encountered in industrial environments and corresponding to specific problems of protection: marine environment, atmospheric corrosion, galvanic corrosion, tribo-corrosion, stress corrosion etc.. The first 8 chapters (part 1) treat of the corrosion problems encountered in different industries and processes: oil and gas production, chemical industry, phosphoric acid industry, PWR-type power plants, corrosion of automobile vehicles, civil engineering and buildings, corrosion of biomaterials, non-destructive testing for the monitoring of corrosion. The other chapters (part 2) deal with anticorrosion and protective coatings and means: choice of materials, coatings and surface treatments, thick organic coatings and enamels, paints, corrosion inhibitors and cathodic protection. (J.S.)

  16. Characterization of corrosive bacterial consortia isolated from petroleum-product-transporting pipelines

    Energy Technology Data Exchange (ETDEWEB)

    Rajasekar, Aruliah; Ting, Yen-Peng [National Univ. of Singapore (Singapore). Dept. of Chemical and Biomolecular Engineering; Anandkumar, Balakrishnan [Sourashtra Coll., Madurai (India). Dept. of Biotechnology; Maruthamuthu, Sundaram [Central Electrochemical Research Inst., Karaikudi (India). Biocorrosion Group; Rahman, Pattanathu K.S.M. [Teesside Univ., Tees Valley (United Kingdom). Chemical and Bioprocess Engineering Group

    2010-01-15

    Microbiologically influenced corrosion is a problem commonly encountered in facilities in the oil and gas industries. The present study describes bacterial enumeration and identification in diesel and naphtha pipelines located in the northwest and southwest region in India, using traditional cultivation technique and 16S rDNA gene sequencing. Phylogenetic analysis of 16S rRNA sequences of the isolates was carried out, and the samples obtained from the diesel and naphtha-transporting pipelines showed the occurrence of 11 bacterial species namely Serratia marcescens ACE2, Bacillus subtilis AR12, Bacillus cereus ACE4, Pseudomonas aeruginosa AI1, Klebsiella oxytoca ACP, Pseudomonas stutzeri AP2, Bacillus litoralis AN1, Bacillus sp., Bacillus pumilus AR2, Bacillus carboniphilus AR3, and Bacillus megaterium AR4. Sulfate-reducing bacteria were not detected in samples from both pipelines. The dominant bacterial species identified in the petroleum pipeline samples were B. cereus and S. marcescens in the diesel and naphtha pipelines, respectively. Therefore, several types of bacteria may be involved in biocorrosion arising from natural biofilms that develop in industrial facilities. In addition, localized (pitting) corrosion of the pipeline steel in the presence of the consortia was observed by scanning electron microscopy analysis. The potential role of each species in biofilm formation and steel corrosion is discussed. (orig.)

  17. Degradation Mechanism of Poly(Ether-Urethane) Estane Induced by High Energy Radiation (III) : Radiolytic Gases and Water Soluble Products

    International Nuclear Information System (INIS)

    Dannoux, A.

    2006-01-01

    Within the framework of nuclear waste management, there is interest in the prediction of long-term behaviour of organic materials subjected to high energy radiation. Once organic waste has been stored, gases and low molecular products might be generated from materials irradiated by radionuclides. Long-term behaviour of organic material in nuclear waste has several common concerns with radiation ageing of polymers. But a more detailed description of the chemical evolution is needed for nuclear waste management. In a first approach, an extensive work on radiation ageing is used to identify the different processes encountered during the degradation of a polyurethane, including oxidation dose rate-effects and influence of dose on the oxidation mechanism. In a second approach, a study is performed to identify and quantify gases and possible production of water soluble chemical complexing agents which might enhance radionuclides migration away from the repository. In this work, we present results concerning the production of radiolytic gases and the formation of water soluble oligomers reached with leaching tests Films were made from a poly(ether-urethane) synthesized from methylene bis(p-phenyl isocyanate) (MDI) and poly(tetramethylene glycol) (PTMG) with 1,4 butanediol (BD) and were irradiated by high-energy electron beam to cover a wide doses range and by γ rays to determine the formation/consumption yields of gases. They were measured by mass spectrometry and gas-chromatography/mass spectrometry (GC/MS). The migration of water soluble oligomers in water was reached by measuring the weight loss versus leaching time. The identification of oligomers was performed by using a mass spectrometry with an electrospray ionisation interface (ESI-MS-MS). The analysis of radiolytic gases indicates the formation of H 2 , CO 2 and CO with respective radiolytic yields of 1, 0.5 and 0.3 molecule/100 eV. The consumption of O 2 is evaluated to 6 molecules/100 eV. For absorbed doses

  18. Recent improvements in the filtration of corrosion products in high temperature water and application to reactor circuits

    International Nuclear Information System (INIS)

    Darras, R.; Dolle, L.; Chenouard, J.; Laylavoix, F.

    1977-01-01

    The nature and physico-chemical behavior of corrosion products released by structural materials into high temperature water flowing in power reactor circuits have been investigated in test loops and different power plants. The results improve more particularly the knowledge of probable rate constants governing their disappearance through deposition of crud on the fuel cladding. It appears that a considerable limitation of radioactivity transportation in the primary circuit components of pressurized water reactors is in a general way only possible through extraction of the corrosion products by filtration at a rate adequate to minimize the amount of crud deposited in the core. This extraction rate has been estimated; its magnitude implicates a filtration operating on the high temperature water in the primary circuit which allows the necessary high flows. The application of magnetic and electromagnetic so as deep granular graphite bed filters has been studied. The results concerning efficiencies and limiting yields at high temperatures are given. Estimates concerning technological feasibility and corresponding investments are discussed

  19. Radiation hazards due to activated corrosion and neutron sputtering products in fusion reactor coolant and tritium breeding fluids

    International Nuclear Information System (INIS)

    Klein, A.C.; Vogelsang, W.F.

    1985-01-01

    The accumulation of radioactive corrosion and neutron sputtering products on the surfaces of components in fusion reactor coolant and tritium breeding systems can cause significant personnel access problems. Remote maintenance techniques or special treatment may be required to limit the amount of radiation exposure to plant operational and maintenance personnel. A computer code, RAPTOR, has been developed to estimate the transport of this activated material throughout a fusion heat transfer and/or tritium breeding material loop. A method is devised which treats the components of the loop individually and determines the source rates, deposition and erosion rates, decay rates, and purification rates of these radioactive materials. RAPTOR has been applied to the MARS and Starfire conceptual reactor designs to determine the degree of the possible radiation hazard due to these products. Due to the very high corrosion release rate by HT-9 when exposed to LiPb in the MARS reactor design, the radiation fields surrounding the primary system will preclude direct contact maintenance even after shutdown. Even the removal of the radioactive LiPb from the system will not decrease the radiation fields to reasonable levels. The Starfire primary system will exhibit radiation fields similar to those found in present pressurized water reactors. (orig.)

  20. Reliability and corrosion induced degradation of electronic system

    International Nuclear Information System (INIS)

    Tapas, V.K.; Varde, P.V.

    2014-01-01

    This paper describe the corrosion induced degradation of electronic system failures due to environmental conditions such as humidity, temperature, ionic or organic contaminants, residuals; etc. which can accelerates as electrochemical reaction and causes corrosion of electronic components, Corrosive gases and water vapours from humid condition come into contact with the base metal results in buildup of various chemical reaction products. Ionic contamination responsible for electrochemical reaction, forms soluble complexes with metals, it can degrade the protective oxide film that forms on the positively biased metallization and/or lead to change in the local pH. Deterioration of metal components or electronic circuitry due to electrochemical migration needs to be controlled in order to reduce the corrosion. With explosive increase in demand and miniaturization in electronic system resulted in smaller components, closer spacing and thinner metallic path, it is expected that the corrosion and deterioration of electronic components may become cause or concern. This paper summarises the current understanding of chemistry behind possible causes of corrosion of electronic devices and its failure mechanism. (author)

  1. Investigations on the determination of corrosion kinetics and the structure of corrosion products on high-temperature alloys under low oxygen partial pressures

    International Nuclear Information System (INIS)

    Poestges, A.; Naoumidis, A.; Nickel, H.

    1979-04-01

    On three nickel-base-alloys (NIMONIC 80A, INCONNEL 617 and ALLOY 713LC), which are planned as materials for components of the primary cooling circuit of high-temperature reactors, studies for the determination of the oxidation behaviour under reactor relevant conditions were performed. The test conditions were fixed at an oxygen partial pressure of 10 -16 bars with a total pressure of 0,2 bars and a temperature of 1080 0 C. The use of the X-ray diffraction analysis on the oxidised samples of type NIMONIC 80A showed the corrosion products Cr 2 O 3 , TiO 2 and Cr 2 Ti 2 O 7 in the outer oxide coating as well as Al 2 O 3 in the inner oxide zone. The samples of the alloy type INCOEL 617 showed the oxides Cr 2 O 3 and Cr 2 Ti 2 O 7 in the outer oxide coating. Samples of the alloy ALLOY 713LC showed Cr 2 O 3 and CrNbO 4 in the outer oxide coating and Al 2 O 3 in the zone of inner oxidation. Sufficient detection certainty was only ascertained by investigating samples with plane surface. For both alloys first mentioned, it was possible to prove the validity of the paralinear relationship W = k x t -1 / 2 - a x t for the increase in weight for the explanation of the time law of the oxidation. For the non-destructive determination of the oxide coating thickness on the alloys samples, the X-ray fluorescence analysis gave reproducible results of good precision. (orig.) [de

  2. Continuous production of bio-oil by catalytic liquefaction from wet distiller’s grain with solubles (WDGS) from bio-ethanol production

    International Nuclear Information System (INIS)

    Toor, Saqib Sohail; Rosendahl, Lasse; Nielsen, Mads Pagh; Glasius, Marianne; Rudolf, Andreas; Iversen, Steen Brummerstedt

    2012-01-01

    Bio-refinery concepts are currently receiving much attention due to the drive toward flexible, highly efficient systems for utilization of biomass for food, feed, fuel and bio-chemicals. One way of achieving this is through appropriate process integration, in this particular case combining enzymatic bio-ethanol production with catalytic liquefaction of the wet distillers grains with soluble, a byproduct from the bio-ethanol process. The catalytic liquefaction process is carried out at sub-critical conditions (280–370 °C and 25 MPa) in the presence of a homogeneous alkaline and a heterogeneous Zirconia catalyst, a process known as the Catliq ® process. In the current work, catalytic conversion of WDGS was performed in a continuous pilot plant with a maximum capacity of 30 dm 3 h −1 of wet biomass. In the process, WDGS was converted to bio-oil, gases and water-soluble organic compounds. The oil obtained was characterized using several analysis methods, among them elementary analysis and GC–MS. The study shows that WDGS can be converted to bio oil with high yields. The results also indicate that through the combination of bio-ethanol production and catalytic liquefaction, it is possible to significantly increase the liquid product yield and scope, opening up for a wider end use applicability. -- Highlights: ► Hydrothermal liquefaction of wet biomass. ► Product phase analysis: oil, acqeous, gas and mineral phase. ► Energy and mass balance evaluation.

  3. Natural products phytotoxicity A bioassay suitable for small quantities of slightly water-soluble compounds.

    Science.gov (United States)

    Dornbos, D L; Spencer, G F

    1990-02-01

    A large variety of secondary metabolites that can inhibit germination and/or seedling growth are produced by plants in low quantities. The objective of this study was to develop a bioassay capable of reliably assessing reductions in germination percentage and seedling length of small-seeded plant species caused by exposure to minute quantities of these compounds. The germination and growth of alfalfa (Medicago saliva), annual ryegrass (Lolium multiflorum), and velvetleaf (Abutilon theophrasti) were evaluated against six known phytotoxins from five chemical classes; cinmethylin (a herbicidal cineole derivative) was selected as a comparison standard. Each phytotoxin, dissolved in a suitable organic solvent, was placed on water-agar in small tissue culture wells. After the solvent evaporated, imbibed seeds were placed on the agar; after three days, germination percentages and seedling lengths were measured. Compared to a commonly used filter paper procedure, this modified agar bioassay required smaller quantities of compound per seed for comparable bioassay results. This bioassay also readily permitted the measurement of seedling length, a more sensitive indicator of phytotoxicity than germination. Seedling length decreased sigmoidally as the toxin concentration increased logarithmically. Phytotoxicity was a function of both compound and plant species. Cinmethylin, a grass herbicide, reduced the length of annual ryegrass seedlings by 90-100%, whereas that of alfalfa and velvetleaf was inhibited slightly. The agar bioassay facilitated the rapid and reliable testing of slightly water-soluble compounds, requiring only minute quantities of each compound to give reproducible results.

  4. Corrosion cracking

    International Nuclear Information System (INIS)

    Goel, V.S.

    1985-01-01

    This book presents the papers given at a conference on alloy corrosion cracking. Topics considered at the conference included the effect of niobium addition on intergranular stress corrosion cracking, corrosion-fatigue cracking in fossil-fueled-boilers, fracture toughness, fracture modes, hydrogen-induced thresholds, electrochemical and hydrogen permeation studies, the effect of seawater on fatigue crack propagation of wells for offshore structures, the corrosion fatigue of carbon steels in seawater, and stress corrosion cracking and the mechanical strength of alloy 600

  5. THE ROLE OF PIPE AGEING IN COPPER CORROSION BY-PRODUCT RELEASE

    Science.gov (United States)

    The presence of sulphate, bicarbonate and orthophosphate can change the type of solid present in systems containing cupric ion or cupric hydroxide solids. In some cases, a short-term reduction in copper solubility is realized, but over longer periods of time formation of basic c...

  6. Reduction of the interlocking potential of sump sieves by corrosion products as consequence of loss-of-coolant accidents; Verminderung des Verblockungspotenzials von Sumpfansaugsieben durch Korrosionsprodukte nach Kuehlmittelverluststoerfaellen

    Energy Technology Data Exchange (ETDEWEB)

    Hoffmann, Wolfgang; Kryk, Holger [Helmholtz-Zentrum Dresden-Rossendorf, Dresden (Germany). Inst. fuer Fluiddynamik

    2012-11-01

    In German nuclear power plants thermal insulation fragmentation as a consequence of loss-of-coolant accidents have not been identified, but recently significant pressure increase in the sump sieves due to corrosion products have been observed. The corrosion products are released from hot-galvanized steel grids by steam jet fragmentation. It was shown that critical deposition of corrosion products can occur in the long-term process of the accident. The hazard of sieve blocking could be reduced by zinc containing chemicals or an increase of the pH value (to about 6.7). The possibility of disadvantageous consequences of resulting chemical reactions has to be investigated in the future.

  7. First multi-scale investigation of an iron corrosion products/glass interface on an archaeological analogue

    Energy Technology Data Exchange (ETDEWEB)

    Michelin, A.; Neff, D.; Dillmann, Ph. [CEA Saclay, Lab. Pierre Sue, UMR 9956 CEA/CNRS, 91 - Gif-sur-Yvette (France); Michelin, A.; Gin, St. [CEA Marcoule, Lab. d' Etudes du Comportement a Long Terme des Materiaux de Conditionnement 30 (France); Robinet, L. [Synchrotron SOLEIL, IPANEMA, 91 - Gif-sur-Yvette (France)

    2009-07-01

    Full text of publication follows: In the context of nuclear waste storage, the French approach is to cast the high-level radioactive waste into a stable form and to bury them into a deep geological repository. This conditioning is based on a multi-barrier concept (glass matrix, steel container, overpack and geological barrier) and must ensure the durable confinement of radionuclides. But laboratory experiments do not permit to predict directly the behaviour of these materials over typically a million-year timescale and the extrapolation of short-term laboratory data to long time periods remains problematic. Part of the validation of the predictive models relies on natural and archaeological analogues. For that reason, blast furnace slags originating from a 16. century iron-making site (Glinet, Normandy) are studied. This material is composed of opaque glass containing cast iron balls. Thus, it represents a good analogue for long-term prediction of glass/iron alteration behaviour. Moreover, these artefacts were buried several centuries in a fine characterized anoxic environment which is the subject of field investigations. The aim of this study is to characterize interfacial zones using microbeam techniques (EDS/WDS for elemental information, EDS/TEM microanalysis, {mu}Raman, {mu}XAS under synchrotron radiation for structural analyses). First of all, corrosion products around cast iron balls have been identified as siderite (FeCO{sub 3}) and iron hydroxycarbonate (Fe{sub 2}(OH){sub 2}CO{sub 3}) using {mu}Raman and EDS microanalysis. Then the interface glass/corrosion products has been studied with the same techniques. A signal variation on Raman spectra is observed along the interface and EDS-SEM microanalysis points out a calcium depletion. It means that mass transfer exists between glass and iron-rich phases and this leads to the development of an altered zone of glass. However, this interface seems to be too thin for the resolution of these techniques. That

  8. Enzymatic production of dietary nucleotides from low-soluble purine bases by an efficient, thermostable and alkali-tolerant biocatalyst.

    Science.gov (United States)

    Del Arco, J; Cejudo-Sanches, J; Esteban, I; Clemente-Suárez, V J; Hormigo, D; Perona, A; Fernández-Lucas, J

    2017-12-15

    Traditionally, enzymatic synthesis of nucleoside-5'-monophosphates (5'-NMPs) using low water-soluble purine bases has been described as less efficient due to their low solubility in aqueous media. The use of enzymes from extremophiles, such as thermophiles or alkaliphiles, offers the potential to increase solubilisation of these bases by employing high temperatures or alkaline pH. This study describes the cloning, expression and purification of hypoxanthine-guanine-xanthine phosphoribosyltransferase from Thermus thermophilus (TtHGXPRT). Biochemical characterization indicates TtHGXPRT as a homotetramer with excellent activity and stability across a broad range of temperatures (50-90°C) and ionic strengths (0-500mMNaCl), but it also reveals an unusually high activity and stability under alkaline conditions (pH range 8-11). In order to explore the potential of TtHGXPRT as an industrial biocatalyst, enzymatic production of several dietary 5'-NMPs, such as 5'-GMP and 5'-IMP, was carried out at high concentrations of guanine and hypoxanthine. Copyright © 2017 Elsevier Ltd. All rights reserved.

  9. SITE-94. Radionuclide solubilities for SITE-94

    Energy Technology Data Exchange (ETDEWEB)

    Arthur, R.; Apted, M. [QuantiSci, Denver, CO (United States)

    1996-12-01

    In this report, solubility constraints are evaluated on radioelement source-term concentrations supporting the SITE-94 performance assessment. Solubility models are based on heterogeneous-equilibrium, mass- and charge-balance constraints incorporated into the EQ3/6 geochemical software package, which is used to calculate the aqueous speciation behavior and solubilities of U, Th, Pu, Np, Am, Ni, Ra, Se, Sn, Sr, Tc and Zr in site groundwaters and near-field solutions. The chemical evolution of the near field is approximated using EQ3/6 in terms of limiting conditions at equilibrium, or steady state, in three closed systems representing fully saturated bentonite, Fe{sup o} corrosion products of the canister, and spent fuel. The calculations consider both low-temperature (15 deg C) and high-temperature (80 deg C) conditions in the near field, and the existence of either reducing or strongly oxidizing conditions in each of the bentonite, canister, and spent-fuel barriers. Heterogeneities in site characteristics are evaluated through consideration of a range of initial groundwaters and their interactions with engineered barriers. Aqueous speciation models for many radioelements are constrained by thermodynamic data that are estimated with varying degrees of accuracy. An important question, however, is how accurate do these models need to be for purposes of estimating source-term concentrations? For example, it is unrealistic to expect a high degree of accuracy in speciation models if such models predict solubilities that are below the analytical detection limit for a given radioelement. From a practical standpoint, such models are irrelevant if calculated solubilities cannot be tested by direct comparison to experimental data. In the absence of models that are both accurate and relevant for conditions of interest, the detection limit could define a pragmatic upper limit on radioelement solubility 56 refs, 25 tabs, 10 figs

  10. SITE-94. Radionuclide solubilities for SITE-94

    International Nuclear Information System (INIS)

    Arthur, R.; Apted, M.

    1996-12-01

    In this report, solubility constraints are evaluated on radioelement source-term concentrations supporting the SITE-94 performance assessment. Solubility models are based on heterogeneous-equilibrium, mass- and charge-balance constraints incorporated into the EQ3/6 geochemical software package, which is used to calculate the aqueous speciation behavior and solubilities of U, Th, Pu, Np, Am, Ni, Ra, Se, Sn, Sr, Tc and Zr in site groundwaters and near-field solutions. The chemical evolution of the near field is approximated using EQ3/6 in terms of limiting conditions at equilibrium, or steady state, in three closed systems representing fully saturated bentonite, Fe o corrosion products of the canister, and spent fuel. The calculations consider both low-temperature (15 deg C) and high-temperature (80 deg C) conditions in the near field, and the existence of either reducing or strongly oxidizing conditions in each of the bentonite, canister, and spent-fuel barriers. Heterogeneities in site characteristics are evaluated through consideration of a range of initial groundwaters and their interactions with engineered barriers. Aqueous speciation models for many radioelements are constrained by thermodynamic data that are estimated with varying degrees of accuracy. An important question, however, is how accurate do these models need to be for purposes of estimating source-term concentrations? For example, it is unrealistic to expect a high degree of accuracy in speciation models if such models predict solubilities that are below the analytical detection limit for a given radioelement. From a practical standpoint, such models are irrelevant if calculated solubilities cannot be tested by direct comparison to experimental data. In the absence of models that are both accurate and relevant for conditions of interest, the detection limit could define a pragmatic upper limit on radioelement solubility

  11. Exploring fungal biodiversity for the production of water-soluble pigments as potential natural food colorants

    DEFF Research Database (Denmark)

    Mapari, Sameer Shamsuddin; Nielsen, Kristian Fog; Larsen, Thomas Ostenfeld

    2005-01-01

    The production of many currently authorized natural food colorants has a number of disadvantages, including a dependence on the supply of raw materials and variations in pigment extraction. Fungi provide a readily available alternative source of naturally derived food colorants that could easily...... be produced in high yields. The recent authorization of a fungal food colorant has fuelled research to explore the extraordinary chemical diversity and biodiversity of fungi for the biotechnological production of pigments as natural food colorants. These studies require an appropriate use of chernotaxonomic...... technology, in the future it should be possible to employ metabolic engineering to create microbial cell factories for the production of food colorants....

  12. Corrosion behavior of environmental assessment glass in product consistency tests of extended duration

    International Nuclear Information System (INIS)

    Bates, J.K.; Buck, E.C.; Ebert, W.L.; Luo, J.S.; Tam, S.W.

    1998-01-01

    We have conducted static dissolution tests to study the corrosion behavior of the Environmental Assessment (EA) glass, which is the benchmark glass for high-level waste glasses being produced at US Department of Energy facilities. These tests were conducted to evaluate the behavior of the EA glass under the same long-term and accelerated test conditions that are being used to evaluate the corrosion of waste glasses. Tests were conducted at 90 C in a tuff groundwater solution at glass surface area/solution volume (WV) ratios of about 2000 and 20,000 m -1 . The glass dissolved at three distinct dissolution rates in tests conducted at 2000 m -1 . Based on the release of boron, dissolution within the first seven days occurred at a rate of about 0.65 g/(m 2 · d). The rate between seven and 70 days decreased to 0.009 g/(m 2 · d). An increase in the dissolution rate occurred at longer times after the precipitation of zeolite phases analcime, gmelinite, and an aluminum silicate base. The dissolution rate after phase formation was about 0.18 g/(m 2 · d). The formation of the same zeolite alteration phases occurred after about 20 days in tests at 20,000 m - . The average dissolution rate over the first 20 days was 0.5 g/(m 2 · d) and the rate after phase formation was about 0.20 g/(m 2 · d). An intermediate stage with a lower rate was not observed in tests at 20,000 m -1 . The corrosion behavior of EA glass is similar to that observed for other high-level waste glasses reacted under the same test conditions. The dissolution rate of EA glass is higher than that of other high-level waste glasses both in 7-day tests and after alteration phases form

  13. Effect of Corn Dried Distiller Grains with Solubles (DDGS in Dairy Cow Diets on Manure Bioenergy Production Potential

    Directory of Open Access Journals (Sweden)

    Daniel I. Massé

    2014-03-01

    Full Text Available The main objective of this study was to obtain scientifically sound data on the bioenergy potential of dairy manures from cows fed different levels of corn dried distillers grains with solubles (DDGS. Three diets differing in corn DDGS content were formulated: 0% corn DDGS (DDGS0; control diet, 10% corn DDGS (DDGS10 and 30% corn DDGS (DDGS30. Bioenergy production was determined in psychrophilic (25 ± 1 °C sequencing batch reactors (SBRs fed 3 g COD L−1·day−1 during a two-week feeding period followed by a two-week react period. Compared to the control diet, adding DDGS10 and DDGS30 to the dairy cow diet increased the daily amount of fat excreted in slurry by 29% and 70%, respectively. The addition of DDGS30 increased the cows’ daily production of fresh feces and slurry by 15% and 11%, respectively. Furthermore, the incorporation of DDGS30 in the diet increased the daily amounts of dry matter (DM, volatile solids (VS, neutral detergent fiber (NDF, acid detergent fiber (ADF and hemicellulose by 18%, 18%, 30%, 15% and 53%, respectively, compared to the control diet. While the addition of DDGS did not significantly affect the specific CH4 production per kg VS compared to the control diet, DDGS30 increased the per cow daily CH4 production by 14% compared to the control diet.

  14. Effect of Corn Dried Distiller Grains with Solubles (DDGS) in Dairy Cow Diets on Manure Bioenergy Production Potential.

    Science.gov (United States)

    Massé, Daniel I; Jarret, Guillaume; Benchaar, Chaouki; Saady, Noori M Cata

    2014-03-05

    The main objective of this study was to obtain scientifically sound data on the bioenergy potential of dairy manures from cows fed different levels of corn dried distillers grains with solubles (DDGS). Three diets differing in corn DDGS content were formulated: 0% corn DDGS (DDGS0; control diet), 10% corn DDGS (DDGS10) and 30% corn DDGS (DDGS30). Bioenergy production was determined in psychrophilic (25 ± 1 °C) sequencing batch reactors (SBRs) fed 3 g COD L(-1)·day(-1) during a two-week feeding period followed by a two-week react period. Compared to the control diet, adding DDGS10 and DDGS30 to the dairy cow diet increased the daily amount of fat excreted in slurry by 29% and 70%, respectively. The addition of DDGS30 increased the cows' daily production of fresh feces and slurry by 15% and 11%, respectively. Furthermore, the incorporation of DDGS30 in the diet increased the daily amounts of dry matter (DM), volatile solids (VS), neutral detergent fiber (NDF), acid detergent fiber (ADF) and hemicellulose by 18%, 18%, 30%, 15% and 53%, respectively, compared to the control diet. While the addition of DDGS did not significantly affect the specific CH₄ production per kg VS compared to the control diet, DDGS30 increased the per cow daily CH₄ production by 14% compared to the control diet.

  15. Soluble receptor for advanced glycation end-product levels are related to albuminuria and arterial stiffness in essential hypertension.

    Science.gov (United States)

    Dimitriadis, K; Tsioufis, C; Kasiakogias, A; Miliou, A; Poulakis, M; Kintis, K; Bafakis, I; Benardis, E; Tousoulis, D; Stefanadis, C

    2013-04-01

    Emerging evidence suggests that the soluble receptor for advanced glycation end-products (sRAGE) is implicated in the development of vascular disease. We investigated the interrelationships of sRAGE with albumin to creatinine ratio (ACR) and arterial stiffness in essential hypertension. In 309 untreated non-diabetic hypertensives, ACR values were determined as the mean of three non-consecutive morning spot urine samples and aortic stiffness was evaluated on the basis of carotid to femoral pulse wave velocity (c-f PWV). In all subjects, venous blood sampling was performed for the estimation of sRAGE levels. Patients with low (n = 155) compared to those with high sRAGE values (n = 154) had greater 24-h systolic BP (140 ± 8 vs. 134 ± 7 mmHg, p involvement of sRAGE in the progression of hypertensive vascular damage. Copyright © 2011 Elsevier B.V. All rights reserved.

  16. The characteristics of extracellular polymeric substances and soluble microbial products in moving bed biofilm reactor-membrane bioreactor.

    Science.gov (United States)

    Duan, Liang; Jiang, Wei; Song, Yonghui; Xia, Siqing; Hermanowicz, Slawomir W

    2013-11-01

    The characteristics of extracellular polymeric substances (EPS) and soluble microbial products (SMP) in conventional membrane bioreactor (MBR) and in moving bed biofilm reactor-membrane bioreactors (MBBR-MBR) were investigated in long-term (170 days) experiments. The results showed that all reactors had high removal efficiency of ammonium and COD, despite very different fouling conditions. The MBBR-MBR with media fill ratio of 26.7% had much lower total membrane resistance and no obvious fouling were detected during the whole operation. In contrast, MBR and MBBR-MBR with lower and higher media fill experienced more significant fouling. Low fouling at optimum fill ratio may be due to the higher percentage of small molecular size (100 kDa) of EPS and SMP in the reactor. The composition of EPS and SMP affected fouling due to different O-H bonds in hydroxyl functional groups, and less polysaccharides and lipids. Copyright © 2013 Elsevier Ltd. All rights reserved.

  17. Influence of solids retention time on membrane fouling: characterization of extracellular polymeric substances and soluble microbial products.

    Science.gov (United States)

    Duan, Liang; Tian, Zhiyong; Song, Yonghui; Jiang, Wei; Tian, Yuan; Li, Shan

    2015-01-01

    The objective of this study was to investigate the influence of solids retention time (SRT) on membrane fouling and the characteristics of biomacromolecules. Four identical laboratory-scale membrane bioreactors (MBRs) were operated with SRTs for 10, 20, 40 and 80 days. The results indicated that membrane fouling occurred faster and more readily under short SRTs. Fouling resistance was the primary source of filtration resistance. The modified fouling index (MFI) results suggested that the more ready fouling at short SRTs could be attributed to higher concentrations of soluble microbial products (SMP). Fourier transform infrared (FTIR) spectra indicated that the SRT had a weak influence on the functional groups of the total extracellular polymeric substances (TEPS) and SMP. However, the MBR under a short SRT had more low-molecular-weight (MW) compounds (100 kDa). Aromatic protein and tryptophan protein-like substances were the dominant groups in the TEPS and SMP, respectively.

  18. Thermodynamics of Highly Supersaturated Aqueous Solutions of Poorly Water-Soluble Drugs-Impact of a Second Drug on the Solution Phase Behavior and Implications for Combination Products.

    Science.gov (United States)

    Trasi, Niraj S; Taylor, Lynne S

    2015-08-01

    There is increasing interest in formulating combination products that contain two or more drugs. Furthermore, it is also common for different drug products to be taken simultaneously. This raises the possibility of interactions between different drugs that may impact formulation performance. For poorly water-soluble compounds, the supersaturation behavior may be a critical factor in determining the extent of oral absorption. The goal of the current study was to evaluate the maximum achievable supersaturation for several poorly water-soluble compounds alone, and in combination. Model compounds included ritonavir, lopinavir, paclitaxel, felodipine, and diclofenac. The "amorphous solubility" for the pure drugs was determined using different techniques and the change in this solubility was then measured in the presence of differing amounts of a second drug. The results showed that "amorphous solubility" of each component in aqueous solution is substantially decreased by the second component, as long as the two drugs are miscible in the amorphous state. A simple thermodynamic model could be used to predict the changes in solubility as a function of composition. This information is of great value when developing co-amorphous or other supersaturating formulations and should contribute to a broader understanding of drug-drug physicochemical interactions in in vitro assays as well as in the gastrointestinal tract. © 2015 Wiley Periodicals, Inc. and the American Pharmacists Association.

  19. Proposed method of the modeling and simulation of corrosion product behavior in the primary cooling system of fast breeder reactors

    International Nuclear Information System (INIS)

    Matuo, Youichirou; Miyahara, Shinya; Izumi, Yoshinobu

    2011-01-01

    Radioactive corrosion products (CP) are main cause of personal radiation exposure during maintenance without fuel failure in FBR plants. In order to establish the techniques of radiation dose estimation for worker in radiation-controlled area, Program SYstem for Corrosion Hazard Evaluation code 'PSYCHE' has been developed. The PSYCHE is based on the Solution-Precipitation model. The CP transfer calculation using the Solution-Precipitation model needs a fitting factor for the calculation of the precipitation of CP. This fitting factor must be determined based on the measured values in reactors that have operating experience. For this reason, the inability to make accurate predictions for reactor without measured values is a major issue. In this study, in addition to existing Solution-Precipitation model in PSYCHE, a transfer-model of CP species in particle form was applied to calculations of CP behavior in the primary cooling system of fast breeder reactor MONJU. Based on the calculated results, we estimated the contribution of CP deposition in the particle-form. It was suggested that the improved model including transfer-model of CP species in particle-form could be used for evaluation of CP transfer and radiation-source distribution in place of conventional Solution-Precipitation model with fitting factor in the PSYCHE. Moreover, it was predicted that CP particles would tend to be deposited in region with high-flow rate of coolant. (author)

  20. Simulation of radioactive corrosion product in primary cooling system of Japanese sodium-cooled fast breeder reactor

    International Nuclear Information System (INIS)

    Matuo, Youichirou; Miyahara, Shinya; Izumi, Yoshinobu

    2012-01-01

    Radioactive Corrosion Product (CP) is a main cause of personal radiation exposure during maintenance with no breached fuel in fast breeder reactor (FBR) plants. The most important CP is 54 Mn and 60 Co. In order to establish techniques of radiation dose estimation for radiation workers in radiation-controlled areas of the FBR, the PSYCHE (Program SYstem for Corrosion Hazard Evaluation) code was developed. We add the Particle Model to the conventional PSYCHE analytical model. In this paper, we performed calculation of CP transfer in JOYO using an improved calculation code in which the Particle Model was added to the PSYCHE. The C/E (calculated / experimentally observed) value for CP deposition was improved through use of this improved PSYCHE incorporating the Particle Model. Moreover, among the percentage of total radioactive deposition accounted for by CP in particle form, 54 Mn was estimated to constitute approximately 20% and 60 Co approximately 40% in the cold-leg region. These calculation results are consistent with the measured results for the actual cold-leg piping in the JOYO. (author)

  1. Characterisation of the surface topography, tomography and chemistry of fretting corrosion product found on retrieved polished femoral stems.

    Science.gov (United States)

    Bryant, M; Ward, M; Farrar, R; Freeman, R; Brummitt, K; Nolan, J; Neville, A

    2014-04-01

    This study presents the characterisation of the surface topography, tomography and chemistry of fretting corrosion product found on retrieved polished femoral stems. Scanning Electron Microscopy (SEM), X-ray Photoelectron Spectroscopy (XPS), Transmission Electron Microscopy (TEM) and Fourier Transform Infrared Spectroscopy (FI-IR) were utilised in order to assess the surface morphology of retrieved Metal-on-Metal Total Hip Replacements and surface chemistry of the films found on the surface. Gross slip, plastic deformation and directionality of the surface were extensively seen on the proximal surfaces of the retrievals. A more corrosive phenomenon was observed in the distal regions of the stem, demonstrating a seemingly intergranular attack. Tribochemical reactions were seen to occur within the stem-cement interfaces with tribofilms being observed on the femoral stem and counterpart PMMA bone cement. XPS, TEM-EDX and FT-IR analyses demonstrated that the films present in the stem surfaces were a complex mixture of chromium oxide and amorphous organic material. A comparison between current experimental and clinical literature has been conducted and findings from this study demonstrate that the formation and chemistry of films are drastically influenced by the type of wear or degradation mechanism. Films formed in the stem-cement interface are thought to further influence the biological environment outside the stem-cement interface due to the formation of Cr and O rich films within the interface whilst Co is free to migrate away. © 2013 Elsevier Ltd. All rights reserved.

  2. Effect of air humidity on microstructure and phase composition of lithium deuteride corrosion products

    International Nuclear Information System (INIS)

    Liu, Xiaobo; Liu, Jiping

    2017-01-01

    Highlights: • Lithium deuteride samples are corroded by air with different relative humidity. • Show the structure and composition of fracture surface of corrosion particle. • The lithium carbonate formation is related to air humidity. • The lithium carbonate only exists in the surface of lithium hydroxide layer. • There is a concentration gradient of H 2 O across the lithium hydroxide layer. - Abstract: Lithium deuteride (LiD) was exposed to air for 600 min to determine the effect of air humidity on its microstructure and phase composition. XRD and XPS results revealed that LiOH and Li 2 CO 3 formed at relative humidity values of >30%, whereas only LiOH formed at values <20%. SEM and EDS images showed a clear LiOH layer; Li 2 CO 3 was confined to the surface of this layer. The schematic illustration revealed that the concentration gradient of H 2 O across the LiOH layer resulted in little Li 2 CO 3 formed in the layer. This work will contribute to increase understanding of LiD corrosion in air.

  3. Inspection indications, stress corrosion cracks and repair of process piping in nuclear materials production reactors

    International Nuclear Information System (INIS)

    Louthan, M.R. Jr.; West, S.L.; Nelson, D.Z.

    1991-01-01

    Ultrasonic inspection of Schedule 40 Type 304 stainless steel piping in the process water system of the Savannah River Site reactors has provided indications of discontinuities in less than 10% of the weld heat affected zones. Pipe sections containing significant indications are replaced with Type 304L components. Post removal metallurgical evaluation showed that the indications resulted from stress corrosion cracking in weld heat-affected zones and that the overall weld quality was excellent. The evaluation also revealed weld fusion zone discontinuities such as incomplete penetration, incomplete fusion, inclusions, underfill at weld roots and hot cracks. Service induced extension of these discontinuities was generally not significant although stress corrosion cracking in one weld fusion zone was noted. One set of UT indications was caused by metallurgical discontinuities at the fusion boundary of an extra weld. This extra weld, not apparent on the outer pipe surface, was slightly overlapping and approximately parallel to the weld being inspected. This extra weld was made during a pipe repair, probably associated with initial construction processes. The two nearly parallel welds made accurate assessment of the UT signal difficult. The implications of these observations to the inspection and repair of process water systems of nuclear reactors is discussed

  4. Corrosion engineering

    Energy Technology Data Exchange (ETDEWEB)

    Fontana, M.G.

    1986-01-01

    This book emphasizes the engineering approach to handling corrosion. It presents corrosion data by corrosives or environments rather than by materials. It discusses the corrosion engineering of noble metals, ''exotic'' metals, non-metallics, coatings, mechanical properties, and corrosion testing, as well as modern concepts. New sections have been added on fracture mechanics, laser alloying, nuclear waste isolation, solar energy, geothermal energy, and the Statue of Liberty. Special isocorrosion charts, developed by the author, are introduced as a quick way to look at candidates for a particular corrosive.

  5. Corrosion Resistance Properties of Aluminum Coating Applied by Arc Thermal Metal Spray in SAE J2334 Solution with Exposure Periods

    Directory of Open Access Journals (Sweden)

    Han-Seung Lee

    2016-03-01

    Full Text Available Arc thermal metal spray coating provides excellent corrosion, erosion and wear resistance to steel substrates. This paper incorporates some results of aluminum coating applied by this method on plain carbon steel. Thereafter, coated panels were exposed to an environment known to form stable corrosion products with aluminum. The coated panels were immersed in Society of Automotive Engineers (SAE J2334 for different periods of time. This solution consists of an aqueous solution of NaCl, CaCl2 and NaHCO3. Various electrochemical techniques, i.e., corrosion potential-time, electrochemical impedance spectroscopy (EIS and the potentiodynamic were used to determine the performance of stimulants in improving the properties of the coating. EIS studies revealed the kinetics and mechanism of corrosion and potentiodynamic attributed the formation of a passive film, which stifles the penetration of aggressive ions towards the substrate. The corrosion products that formed on the coating surface, identified using Raman spectroscopy, were Dawsonite (NaAlCO3(OH2 and Al(OH3. These compounds of aluminum are very sparingly soluble in aqueous solution and protect the substrate from pitting and uniform corrosion. The morphology and composition of corrosion products determined by scanning electron microscopy and energy dispersive X-ray analyses indicated that the environment plays a decisive role in improving the corrosion resistance of aluminum coating.

  6. Thermodynamics of soluble fission products cesium and iodine in the Molten Salt Reactor

    NARCIS (Netherlands)

    Capelli, E.; Beneš, O.; Konings, R.J.M.

    2018-01-01

    The present study describes the full thermodynamic assessment of the Li,Cs,Th//F,I system. The existing database for the relevant fluoride salts considered as fuel for the Molten Salt Reactor (MSR) has been extended with two key fission products, cesium and iodine. A complete evaluation of all

  7. High solubility pathway for the carbon dioxide free production of iron.

    Science.gov (United States)

    Licht, Stuart; Wang, Baohui

    2010-10-07

    We report a fundamental change in the understanding of iron oxide thermochemistry, opening a facile, new CO(2)-free route to iron production. The resultant process can eliminate a major global source of greenhouse gas emission, producing the staple iron in molten media at high rate and low electrolysis energy.

  8. Effect of fluid flow, pH and tobacco extracts concentration as organic inhibitors to corrosion characteristics of AISI 1045 steel in 3.5% NaCl environment containing CO2 gas

    Science.gov (United States)

    Kurniawan, Budi Agung; Pratiwi, Vania Mitha; Ahmadi, Nafi'ul Fikri

    2018-04-01

    Corrosion become major problem in most industries. In the oil and gas company, corrosion occurs because of reaction between steel and chemical species inside crude oil. Crude oil or nature gas provide corrosive species, such as CO2, O2, H2S and so on. Fluid containing CO2 gas causes CO2 corrosion which attack steel as well as other corrosion phenomena. This CO2 corrosion commonly called as sweet environment and produce FeCO3 as corrosion products. Fluid flow factor in pipelines during the oil and gas transportation might increase the rate of corrosion itself. Inhibitor commonly use used as corrosion protection because its simplicity in usage. Nowadays, organic inhibitor become main issue in corrosion protection because of biodegradable, low cost, and environmental friendly. This research tried to use tobacco leaf extract as organic inhibitor to control corrosion in CO2 environment. The electrolyte solution used was 3.5% NaCl at pH 4 and pH 7. Weight loss test results showed that the lowest corrosion rate was reach at 132.5 ppm inhibitor, pH 7 and rotational speed of 150 rpm with corrosion rate of 0.091 mm/y. While at pH 4, the lowest corrosion rate was found at rotational speed of 150 rpm with inhibitor concentration of 265 ppm and corrosion rate of 0.327 mm/y. FTIR results indicate the presence of nicotine functional groups on the steel surface. However, based on corrosion rate, it is believed that corrosion occurs, and FeCO3 was soluble in electrolyte. Tobacco leaf extract inhibitors worked by a physisorption mechanism, where tobacco inhibitors formed thin layer on the steel surface.

  9. Effects of soy-soluble fiber and flaxseed gum on the glycemic and insulinemic responses to glucose solutions and dairy products in healthy adult males.

    Science.gov (United States)

    Au, Marco M C; Goff, H Douglas; Kisch, Julie A; Coulson, Alex; Wright, Amanda J

    2013-01-01

    Soy-soluble polysaccharides and flaxseed gum are underutilized dietary fibers of interest to the food industry. However, because the ability of soluble fibers to modulate postprandial glucose and insulin metabolism has been related to their viscous effects, the utility of these and other low-viscosity soluble fibers remains unproven. The objective of this study was to examine the associations between soy-soluble polysaccharides and flaxseed gum concentration, product viscosity, and the postprandial glycemic and insulinemic responses in the context of glucose solutions as well as fluid and gelled dairy products. Twelve healthy males participated in a randomized crossover postprandial study in which they visited the laboratory following overnight fasts on 11 occasions to consume one of 11 study treatments, each consisting of 50 g available carbohydrates. The study treatments included a glucose reference (in duplicate), glucose solutions containing soy-soluble polysaccharides (6%), flaxseed gum (0.7%), or guar gum (0.23%), all matched for an apparent viscosity of 61 mPa·s at 50 s⁻¹, as well as dairy-based beverages and puddings with 0% or 1% soluble fiber added. Blood samples were collected at fasting and up to 2 hours postprandially for determination of glucose and insulin concentrations. Area under the curve (AUC), peak concentration, and time-to-peak values as well as glycemic index (GI) and insulinemic index (II) were calculated. Fiber fortification of a 50 g glucose solution had no effect on postprandial blood glucose or insulin levels, even at a high concentration (i.e., 6% soy-soluble polysaccharides). Glucose AUC and GI values for the dairy-based beverage (p glucose reference. Glucose AUC and GI values for the soy-soluble polysaccharide-fortified dairy products (p glucose reference. No significant differences were observed between the fiber-fortified fluid and gelled dairy-based study treatments and no significant differences were observed in terms of the

  10. Evaluating the influence of process parameters on soluble microbial products formation using response surface methodology coupled with grey relational analysis.

    Science.gov (United States)

    Xu, Juan; Sheng, Guo-Ping; Luo, Hong-Wei; Fang, Fang; Li, Wen-Wei; Zeng, Raymond J; Tong, Zhong-Hua; Yu, Han-Qing

    2011-01-01

    Soluble microbial products (SMPs) present a major part of residual chemical oxygen demand (COD) in the effluents from biological wastewater treatment systems, and the SMP formation is greatly influenced by a variety of process parameters. In this study, response surface methodology (RSM) coupled with grey relational analysis (GRA) method was used to evaluate the effects of substrate concentration, temperature, NH(4)(+)-N concentration and aeration rate on the SMP production in batch activated sludge reactors. Carbohydrates were found to be the major component of SMP, and the influential priorities of these factors were: temperature>substrate concentration > aeration rate > NH(4)(+)-N concentration. On the basis of the RSM results, the interactive effects of these factors on the SMP formation were evaluated, and the optimal operating conditions for a minimum SMP production in such a batch activated sludge system also were identified. These results provide useful information about how to control the SMP formation of activated sludge and ensure the bioreactor high-quality effluent. Copyright © 2010 Elsevier Ltd. All rights reserved.

  11. Higher plasma soluble Receptor for Advanced Glycation End Products (sRAGE) levels are associated with incident cardiovascular disease and all-cause mortality in type 1 diabetes

    DEFF Research Database (Denmark)

    Nin, Johanna W M; Jorsal, Anders; Ferreira, Isabel

    2010-01-01

    To investigate the associations of plasma levels of soluble receptor for advanced glycation end products (sRAGE) with incident cardiovascular disease (CVD) and all-cause mortality in type 1 diabetes and the extent to which any such associations could be explained by endothelial and renal dysfunct......To investigate the associations of plasma levels of soluble receptor for advanced glycation end products (sRAGE) with incident cardiovascular disease (CVD) and all-cause mortality in type 1 diabetes and the extent to which any such associations could be explained by endothelial and renal...

  12. The inclusión of distiller’s dried com grains with solubles in the feed of laying hens during the production stage

    OpenAIRE

    Rodríguez-Ríos, Hernán E; Campos-Parra, Jorge A; Williams-Salinas, Pamela A; Blanck-Heimann, Markus H; Astudillo-Neira, Rita G; Grande-Cano, Jesús D

    2015-01-01

    H.E. Rodríguez-Ríos, J.A. Campos-Parra, P.A. Williams-Salinas, M.H. Blanck-Heimann, R.G. Astudillo-Neira, and J.D. Grande-Cano. 2015. The inclusion of distiller’s dried corn grains with solubles in the feed of laying hens during the production stage. Cien. Inv. Agr. 42(3): 331-339. The aim of this study was to assess the effects of distiller’s dried corn grains with solubles (DDGS) in the diet of laying hens on their productive parameters (live weight, laying percentage, and feed intake) and ...

  13. Surface reactivity of colloidal corrosion product and alloys in PWR conditions

    International Nuclear Information System (INIS)

    Lefevre, Gregory; Leclercq, Stephanie; Cabanas, Bruna-Martin; Delaunay, Sophie; Mansour, Carine; Berger, Gilles

    2012-09-01

    The corrosion of metallic components of water circuits of Pressurized Water Reactors generates colloidal particles. These particles are transported in the circuits, they sorb dissolved species and they can deposit on alloys in given parts of the circuits. Sorption and deposition generate several technical drawbacks in both primary and secondary circuits. According to the DLVO theory, adhesion between two surfaces is controlled by electrostatic and Van der Waals forces. The latter are always attractive and does not depends on solution chemistry. On the contrary, electrostatic forces are connected to the surface charge and depend strongly on the chemical properties of the solids and on the chemistry of the solution. Depending on the relative charge of the surfaces, these forces are attractive or repulsive and can have a major effect on the deposition behavior of particles. According to the surface complexation theory, the surface charge of metallic oxides results from sorption or desorption of protons, leading to positive or negative surface sites, and thus, strongly depends on the solution pH. Dissolved species can sorb on the surface, depending on the ionic charge of these species and on the surface charge. Thus, the knowledge of the surface charge of corrosion particles and alloys, their affinity towards several ions as protons, nickel, cobalt, sulfate, or borate ions has been shown to be useful to predict the transport of the contamination in the primary circuit, or to understand the accumulation of impurities in the steam generator in the secondary circuit. At room temperature, these data can be easily measured, or found in literature. In PWR conditions (high temperature, high pressure), most of the usual protocols and commercial instruments cannot be used. For several years, collaboration between EDF R and D and CNRS has been developed to get information about the surface reactivity of iron oxides, ferrites, and alloys in such conditions. Some of the results

  14. In vitro solubility of calcium, iron and zinc in relation to phytic acid levels in rice-based consumer products in China.

    Science.gov (United States)

    Liang, Jianfen; Han, Bei-Zhong; Nout, M J Robert; Hamer, Robert J

    2010-02-01

    In vitro solubility of calcium, iron and zinc in relation to phytic acid (PA) levels in 30 commercial rice-based foods from China was studied. Solubility of minerals and molar ratios of PA to minerals varied with degrees of processing. In primary products, [PA]/[Ca] values were less than 5 and [PA]/[Fe] and [PA]/[Zn] similarly ranged between 5 and 74, with most values between 20 and 30. [PA]/[mineral] molar ratios in intensively processed products were lower. Solubility of calcium ranged from 0% to 87%, with the lowest in brown rice (12%) and the highest in infant foods (50%). Iron solubility in two-thirds of samples was lower than 30%, and that of zinc narrowly ranged from 6% to 30%. Solubility of minerals was not significantly affected by [PA]/[mineral]. At present, neither primary nor intensively processed rice-based products are good dietary sources of minerals. Improvements should be attempted by dephytinization, mineral fortification or, preferably, combination of both.

  15. Dissolution properties of cerium dibutylphosphate corrosion inhibitors

    NARCIS (Netherlands)

    Soestbergen, van M.; Erich, S.J.F.; Huinink, H.P.; Adan, O.C.G.

    2013-01-01

    The corrosion inhibitor cerium dibutylphosphate, Ce(dbp)3, prevents corrosion by cerium and dbp deposition at the alkaline cathode and acidic anode respectively. The pH dependent Ce(dbp)3 solubility seems to play an essential role in the inhibition degree. We found that Ce(dbp)3 scarcely dissolves

  16. The effect of corrosion product CrF3 on thermo-physical properties of FLiNaK

    International Nuclear Information System (INIS)

    Yin Huiqin; Zhang Peng; An Xuehui; Zhao Sufang; Xie Leidong; Wang Wenfeng

    2016-01-01

    FLiNaK (LiF–NaF–KF: 46.5–11.5–42 mol%) is a promising candidate as the secondary loop coolant in molten salt reactor. The thermo-physical properties of pure FLiNaK and FLiNaK containing up to 6000 ppm (equivalent to mg/kg) corrosion product CrF 3 were measured. The results indicate that the effects of CrF 3 on melting point, enthalpy, specific heat capacity, density and thermal diffusivity of FLiNaK in liquid state are negligible within the allowable error range, meanwhile the change of thermal diffusivity is significant for FLiNaK in solid state. This work provides fundamental knowledge for the thermo-physical properties of coolant in molten salt reactor. (author)

  17. Effects of organic matters coming from Chinese tea on soluble copper release from copper teapot

    International Nuclear Information System (INIS)

    Ni Lixiao; Li Shiyin

    2008-01-01

    The morphology and elemental composition of the corrosion products of copper teapot's inner-surface were characterized by the scanning electron microscopy and energy dispersive X-ray surface analysis (SEM/EDS), X-ray powder diffraction (XRD) and X-ray photon spectroscopy (XPS) analysis. It was revealed that Cu, Fe, Ca, P, Si and Al were the main elements of corrosion by-products, and the α-SiO 2 , Cu 2 O and CaCO 3 as the main mineral components on the inner-surface of copper teapot. The effects of organic matters coming from Chinese tea on soluble copper release from copper teapots in tap water were also investigated. The results showed that the doses of organic matter (as TOC), temperate and stagnation time have significant effects on the concentration of soluble copper released from copper teapots in tap water

  18. Production of ethanol in batch and fed-batch fermentation of soluble sugar

    International Nuclear Information System (INIS)

    Chaudhary, M.Y.; Shah, M.A.; Shah, F.H.

    1991-01-01

    Keeping in view of the demand and need for alternate energy source, especially liquid fuels and the availability of raw materials in Pakistan, we have carried out biochemical and technological studies for ethanol through fermentation of renewable substrates. Molasses and sugar cane have been used as substrate for yeast fermentation. Selected yeast were used in both batch and semi continuous fermentation of molasses. Clarified dilute molasses were fermented with different strains of Saccharomyces cerevisiae. Ethanol concentration after 64 hours batch fermentation reached 9.4% with 90% yield based on sugar content. During feed batch system similar results were obtained after a fermentation cycle of 48 hours resulting in higher productivity. Similarly carbohydrates in fruit juices and hydro lysates of biomass can be economically fermented to ethanol to be used as feed stock for other chemicals. (author)

  19. Moessbauer study of corrosion products formed on Fe80B20 and Fe40Ni40 (MoB)20 amorphous alloys in an SO2-polluted atmosphere

    International Nuclear Information System (INIS)

    Davalos, J.; Marco, J.F.; Gracia, M.; Gancedo, J.R.; Greneche, J.M.

    1990-01-01

    ICEMS, XPS, XRD, and AES have been used to study the corrosion layers formed on two metallic glasses, Fe 80 B 20 and Fe 40 Ni 40 (MoB) 20 (2605 and 2826 MB, Allied Company), exposed to an SO 2 -polluted humid atmosphere. The iron-containing corrosion products are the same found for pure iron in the same environment, but different relative concentrations were clearly evidenced by ICEMS results. Elemental sulphur, Ni(OH) 2 , and B(OH) 3 , the latter enriched at the surface, were found by XPS, XRD and AES. (orig.)

  20. Quantification of nitrous oxide (N2O) emissions and soluble microbial product (SMP) production by a modified AOB-NOB-N2O-SMP model.

    Science.gov (United States)

    Kim, MinJeong; Wu, Guangxue; Yoo, ChangKyoo

    2017-03-01

    A modified AOB-NOB-N 2 O-SMP model able to quantify nitrous oxide (N 2 O) emissions and soluble microbial product (SMP) production during wastewater treatment is proposed. The modified AOB-NOB-N 2 O-SMP model takes into account: (1) two-step nitrification by ammonia-oxidizing bacteria (AOB) and nitrite-oxidizing bacteria (NOB), (2) N 2 O production by AOB denitrification under oxygen-limited conditions and (3) SMP production by microbial growth and endogenous respiration. Validity of the modified model is demonstrated by comparing the simulation results with experimental data from lab-scale sequencing batch reactors (SBRs). To reliably implement the modified model, a model calibration that adjusts model parameters to fit the model outputs to the experimental data is conducted. The results of this study showed that the modeling accuracy of the modified AOB-NOB-N 2 O-SMP model increases by 19.7% (NH 4 ), 51.0% (NO 2 ), 57.8% (N 2 O) and 16.7% (SMP) compared to the conventional model which does not consider the two-step nitrification and SMP production by microbial endogenous respiration. Copyright © 2016 Elsevier Ltd. All rights reserved.

  1. The SKB spent fuel corrosion programme. Status report 1988

    International Nuclear Information System (INIS)

    Werme, L.O.; Forsyth, R.S.

    1989-05-01

    The results of the Swedish spent fuel corrosion programme from 1982 to 1988 are reviewed. Areas where additional research will be required are indentified. The major findings and conclusions after the first six years of the programme are that uranium attains relatively rapidly a constant solution concentration of about 1 mg/l. This is probably solubility controlled. Also plutonium, after initially higher concentration appear to reach a constant concentration of about 0.3 μg/l in groundwater. In DI water, the normalized Pu release is higher than the U release, indicating ongoing fuel oxidation/alteration after the leachant has been saturated with U. Under reducing conditions, the absence of fuel oxidation and the very low U solubility lead to a stronger tendency towards congruent releases, controlled by the solubility of the fuel matrix. The fission products Cs, Sb, Tc and Mo appear to selectively leached, probably from inclusions or from fuel cracks, fissures and grain boundaries. (authors)

  2. Pharmacological hypothesis: Nitric oxide-induced inhibition of ADAM-17 activity as well as vesicle release can in turn prevent the production of soluble endothelin-converting enzyme.

    Science.gov (United States)

    Kuruppu, Sanjaya; Rajapakse, Niwanthi W; Parkington, Helena C; Smith, Ian

    2017-10-01

    Endothelin-1 (ET-1) and nitric oxide (NO) are two highly potent vasoactive molecules with opposing effects on the vasculature. Endothelin-converting enzyme (ECE) and nitric oxide synthase (NOS) catalyse the production of ET-1 and NO, respectively. It is well established that these molecules play a crucial role in the initiation and progression of cardiovascular diseases and have therefore become targets of therapy. Many studies have examined the mechanism(s) by which NO regulates ET-1 production. Expression and localization of ECE-1 is a key factor that determines the rate of ET-1 production. ECE-1 can either be membrane bound or be released from the cell surface to produce a soluble form. NO has been shown to reduce the expression of both membrane-bound and soluble ECE-1. Several studies have examined the mechanism(s) behind NO-mediated inhibition of ECE expression on the cell membrane. However, the precise mechanism(s) behind NO-mediated inhibition of soluble ECE production are unknown. We hypothesize that both exogenous and endogenous NO, inhibits the production of soluble ECE-1 by preventing its release via extracellular vesicles (e.g., exosomes), and/or by inhibiting the activity of A Disintegrin and Metalloprotease-17 (ADAM17). If this hypothesis is proven correct in future studies, these pathways represent targets for the therapeutic manipulation of soluble ECE-1 production. © 2017 The Authors. Pharmacology Research & Perspectives published by John Wiley & Sons Ltd, British Pharmacological Society and American Society for Pharmacology and Experimental Therapeutics.

  3. Grazing behaviour, intake, rumen function and milk production of dairy cows offered Lolium perenne containing different levels of water-soluble carbohydrates

    NARCIS (Netherlands)

    Taweel, H.Z.; Tas, B.M.; Smit, H.J.; Elgersma, A.; Dijkstra, J.; Tamminga, S.

    2006-01-01

    The aim of this study was to assess grazing behaviour, intake, rumen function, milk production and composition of dairy cows grazing perennial ryegrass varieties that were morphologically and chemically similar, but differed in their water-soluble carbohydrate (WSC) concentration. Eight multiparous

  4. Effectivity of fluoride treatment on hydrogen and corrosion product generation in temporal implants for different magnesium alloys.

    Science.gov (United States)

    Trinidad, Javier; Arruebarrena, Gurutze; Marco, Iñigo; Hurtado, Iñaki; Sáenz de Argandoña, Eneko

    2013-12-01

    The increasing interest on magnesium alloys relies on their biocompatibility, bioabsorbility and especially on their mechanical properties. Due to these characteristics, magnesium alloys are becoming a promising solution to be used, as temporary implants. However, magnesium alloys must overcome their poor corrosion resistance. This article analyses the corrosion behaviour in phosphate-buffered saline solution of three commercial magnesium alloys (AZ31B, WE43 and ZM21) as well as the influence of fluoride treatment on their corrosion behaviour. It is shown that the corrosion rate of all the alloys is decreased by fluoride treatment. However, fluoride treatment affects each alloy differently.

  5. Calculational model and code for corrosion products transfer in sodium systems

    International Nuclear Information System (INIS)

    Iizawa, Katsuyuki; Kikuchi, Takao; Nihei, Isao; Horie, Junnosuke

    1987-01-01

    The parameters to predict LMFBR radioactive CP behaviour are obtained by fitting the model to the release rates and distribution of deposits in experimental sodium loops. Analysis of the downstream effect for Co-60 deposition confirms that the mechanism controlling Co-60 transfer is diffusion through the boundary sublayer in the flowing sodium. On the other hand, analysis of Mn-54 deposition suggests that the controlling mechanism for this nuclide is probably an intermediate case between diffusion-control in the liquid and reaction-control at steel surfaces. The super-stoichiometric release of Mn-54 and the sub-stoichiometric release of Co-60 are interpreted from their model parameters as being likely related to their solubilities in sodium. The computer code developed for this model is named PSYCHE. (orig./HP)

  6. Plutonium solubilities

    International Nuclear Information System (INIS)

    Puigdomnech, I.; Bruno, J.

    1991-02-01

    Thermochemical data has been selected for plutonium oxide, hydroxide, carbonate and phosphate equilibria. Equilibrium constants have been evaluated in the temperature range 0 to 300 degrees C at a pressure of 1 bar to T≤100 degrees C and at the steam saturated pressure at higher temperatures. Measured solubilities of plutonium that are reported in the literature for laboratory experiments have been collected. Solubility data on oxides, hydroxides, carbonates and phosphates have been selected. No solubility data were found at temperatures higher than 60 degrees C. The literature solubility data have been compared with plutonium solubilities calculated with the EQ3/6 geochemical modelling programs, using the selected thermodynamic data for plutonium. (authors)

  7. Increased bioclogging and corrosion risk by sulfate addition during iodine recovery at a natural gas production plant.

    Science.gov (United States)

    Lim, Choon-Ping; Zhao, Dan; Takase, Yuta; Miyanaga, Kazuhiko; Watanabe, Tomoko; Tomoe, Yasuyoshi; Tanji, Yasunori

    2011-02-01

    Iodine recovery at a natural gas production plant in Japan involved the addition of sulfuric acid for pH adjustment, resulting in an additional about 200 mg/L of sulfate in the waste brine after iodine recovery. Bioclogging occurred at the waste brine injection well, causing a decrease in well injectivity. To examine the factors that contribute to bioclogging, an on-site experiment was conducted by amending 10 L of brine with different conditions and then incubating the brine for 5 months under open air. The control case was exposed to open air but did not receive additional chemicals. When sulfate addition was coupled with low iodine, there was a drastic increase in the total amount of accumulated biomass (and subsequently the risk of bioclogging) that was nearly six times higher than the control. The bioclogging-associated corrosion rate of carbon steel was 84.5 μm/year, which is four times higher than that observed under other conditions. Analysis of the microbial communities by denaturing gradient gel electrophoresis revealed that the additional sulfate established a sulfur cycle and induced the growth of phototrophic bacteria, including cyanobacteria and purple bacteria. In the presence of sulfate and low iodine levels, cyanobacteria and purple bacteria bloomed, and the accumulation of abundant biomass may have created a more conducive environment for anaerobic sulfate-reducing bacteria. It is believed that the higher corrosion rate was caused by a differential aeration cell that was established by the heterogeneous distribution of the biomass that covered the surface of the test coupons.

  8. Vascular Canals in Permanent Hyaline Cartilage: Development, Corrosion of Nonmineralized Cartilage Matrix, and Removal of Matrix Degradation Products.

    Science.gov (United States)

    Gabner, Simone; Häusler, Gabriele; Böck, Peter

    2017-06-01

    Core areas in voluminous pieces of permanent cartilage are metabolically supplied via vascular canals (VCs). We studied cartilage corrosion and removal of matrix degradation products during the development of VCs in nose and rib cartilage of piglets. Conventional staining methods were used for glycosaminoglycans, immunohistochemistry was performed to demonstrate collagens types I and II, laminin, Ki-67, von Willebrand factor, VEGF, macrophage marker MAC387, S-100 protein, MMPs -2,-9,-13,-14, and their inhibitors TIMP1 and TIMP2. VCs derived from connective tissue buds that bulged into cartilage matrix ("perichondrial papillae", PPs). Matrix was corroded at the tips of PPs or resulting VCs. Connective tissue stromata in PPs and VCs comprised an axial afferent blood vessel, peripherally located wide capillaries, fibroblasts, newly synthesized matrix, and residues of corroded cartilage matrix (collagen type II, acidic proteoglycans). Multinucleated chondroclasts were absent, and monocytes/macrophages were not seen outside the blood vessels. Vanishing acidity characterized areas of extracellular matrix degradation ("preresorptive layers"), from where the dismantled matrix components diffused out. Leached-out material stained in an identical manner to intact cartilage matrix. It was detected in the stroma and inside capillaries and associated downstream veins. We conclude that the delicate VCs are excavated by endothelial sprouts and fibroblasts, whilst chondroclasts are specialized to remove high volumes of mineralized cartilage. VCs leading into permanent cartilage can be formed by corrosion or inclusion, but most VCs comprise segments that have developed in either of these ways. Anat Rec, 300:1067-1082, 2017. © 2016 Wiley Periodicals, Inc. © 2016 Wiley Periodicals, Inc.

  9. Process for dissolving the radioactive corrosion products from internal surfaces in nuclear reactors

    International Nuclear Information System (INIS)

    Brown, W.W.

    1976-01-01

    This invention concerns a process for dissolving in the coolant flowing in a reactor the radioactive substances from the corrosion of the internal surfaces of the reactor to which they cling. When a reactor is operating, the fission occurring in the fuel generates gases and fission substances, such as iodine 131 and 133, cesium 134 and 137, molybdenum 99, xenon 133 and activates the structural materials of the reactor such as nickel by giving off cobalt 58 and similar substances. Under this invention an oxygen rich solution is injected in the reactor coolant after the temperature and pressure reduction stage, during the preparation prior to refuelling and repairs. The oxygen in the solution speeds up the release of cobalt 58 and other radioactive substances from the internal surfaces of the reactor and their dissolving in the oxygenated cold coolant at the start of the cooling procedures of the installation. This allows them to be removed by an ion exchanger before the reactor is emptied. By utilising this process, about half a day may be gained in refuelling time when this has to be done once a week [fr

  10. Analysis of corrosions-products in tissue samples near surgical implants by means of LAMMA (Laser Microprobe Mass Analyzer) and ICP-MS (Inductively Coupled Plasma Mass Spectrometer)

    International Nuclear Information System (INIS)

    Schlagenhaufen, C.

    1996-08-01

    In this work corrosion products of surgical implants in tissue samples were identified. For the characterization of the corrosion products the LAMMA 500 (Laser Microprobe Mass Analyzer) was used. Additional analysis were made with the ICP-MS (Inductively Coupled Plasma Mass Spectrometer) to determine the concentration of chromium, cobalt, nickel, and molybdenum in the tissues. In the first part several synthetic chromium- and molybdenum compounds were investigated with LAMMA. With the anionic mass spectra of the chromium-compounds it is possible to the oxidation state of chromium. The mass spectra of the synthetic compounds were used to identify, the compounds in the corrosion products. In the second part thin sections prepared from the tissue samples from the surrounding of the implants were analyzed. Several embedding and cutting methods were tested. Histological staining methods and LAMMA spectra were used to characterize the deposits in the tissue. Three different deposits were found in the tissue. In all tissues metal splinters from the implant were found. In most of the tissues iron-rich deposits were found, that were identified as iron-phosphate. As definitive corrosion products of the implant mixtures of chromium(III)phosphate, calcium molybdate, calcium phosphate and chromium(III) molybdate were identified. The ICP-MS results show in comparison to normal values, very high concentrations for chromium, nickel, cobalt and molybdenum. These results support the conclusions based on LAMMA results. The results of these investigations clearly indicate, that stainless steel implants, are not corrosion-resistant in the body. Relatively high amounts of the constituents, of the implant dissolved, and are deposited as solid compounds in the tissue next to the implant. (author)

  11. Soluble CD163, a product of monocyte/macrophage activation, is inversely associated with haemoglobin levels in placental malaria.

    Directory of Open Access Journals (Sweden)

    Caroline Lin Lin Chua

    Full Text Available In Plasmodium falciparum malaria, activation of monocytes and macrophages (monocytes/macrophages can result in the production of various inflammatory mediators that contribute to immunopathology. Soluble CD163 (sCD163 is a specific marker of monocyte/macrophage activation typically found at increased levels during various inflammatory conditions and can be associated with poor clinical outcomes. To better understand the relationships between levels of sCD163 and clinical parameters in women with placental malaria, we measured plasma sCD163 levels in maternal peripheral and placental blood compartments at delivery and determined their correlations with birth weight and maternal haemoglobin concentrations. sCD163 levels were negatively correlated with birth weight only in the placental compartment (r = -0.145, p = 0.03 and were inversely correlated with maternal haemoglobin concentrations, both in peripheral blood (r = -0.238, p = 0.0004 and in placental blood (r = -0.259, p = 0.0001. These inverse relationships suggest a potential role for monocyte/macrophage activation in the pathogenesis of malaria in pregnancy, particularly in relation to malaria-associated anaemia.

  12. Organic Contaminants and Treatment Chemicals in Steam-Water Cycles : Thermal stability, decomposition products and flow-accelerated corrosion

    NARCIS (Netherlands)

    Moed, D.H.

    2015-01-01

    Boiler feedwater and steam have to be of high purity, because of the susceptibility of the steam-water cycle to corrosion. Organic contaminants break down in boilers by hydrothermolysis, leading to the formation of organic acid anions, which are suspected to cause corrosion of steam-water cycle

  13. Numerical simulation of the detection of crack in reinforced concrete structures of NPP due to expansion of reinforcing corrosive products using Impact-Echo method

    Directory of Open Access Journals (Sweden)

    Morávka Š.

    2008-12-01

    Full Text Available Nuclear energy boom is starting nowadays. But also current nuclear power plants (NPP are duty to certify their security for regular renewal of their operating licenses. NPP security can be significantly affected by defects of large amount of ageing reinforced concrete structures. Advanced Impact-Echo method seams to be very hopeful to cooperate at performing in-service inspections such structures. Just these in-service inspections are included in the first priority group of specific technical issues according to the recommendations of OECD-Nuclear Energy Agency, Commission on Safety of Nuclear Installation in the field of ageing management.This paper continues of extensive project dealing with Impact-Echo method application. It will present method description and main results of numerical modeling of detection and localization of crack caused by corrosive product expansion. Steel reinforcing rods are subjected to corrosion due to diffusion of corrosive agents from structure surface. Corrosive products have up to 7-times larger volume than pure steel. Raised strain can cad lead up to concrete failure and crack development. We investigate whether it is possible to detect these growing cracks by Impact-Echo method in time.Experimental verification of our numerical predictions is prepared on Civil Faculty in Brno.

  14. Characterization of soluble microbial products (SMPs) in a membrane bioreactor (MBR) treating synthetic wastewater containing pharmaceutical compounds.

    Science.gov (United States)

    Zhang, Dongqing; Trzcinski, Antoine Prandota; Kunacheva, Chinagarn; Stuckey, David C; Liu, Yu; Tan, Soon Keat; Ng, Wun Jern

    2016-10-01

    This study investigated the behaviour and characteristics of soluble microbial products (SMP) in two anoxic-aerobic membrane bioreactors (MBRs): MBRcontrol and MBRpharma, for treating municipal wastewater. Both protein and polysaccharides measured exhibited higher concentrations in the MBRpharma than the MBRcontrol. Molecular weight (MW) distribution analysis revealed that the presence of pharmaceuticals enhanced the accumulation of SMPs with macro- (13,091 kDa and 1587 kDa) and intermediate-MW (189 kDa) compounds in the anoxic MBRpharma, while a substantial decrease was observed in both MBR effluents. Excitation emission matrix (EEM) fluorescence contours indicated that the exposure to pharmaceuticals seemed to stimulate the production of aromatic proteins containing tyrosine (10.1-32.6%) and tryptophan (14.7-43.1%), compared to MBRcontrol (9.9-29.1% for tyrosine; 11.8-42.5% for tryptophan). Gas chromatography-mass spectrometry (GC-MS) analysis revealed aromatics, long-chain alkanes and esters were the predominant SMPs in the MBRs. More peaks were present in the aerobic MBRpharma (196) than anoxic MBRpharma (133). The SMPs identified exhibited both biodegradability and recalcitrance in the MBR treatment processes. Only 8 compounds in the MBRpharma were the same as in the MBRcontrol. Alkanes were the most dominant SMPs (51%) in the MBRcontrol, while aromatics were dominant (40%) in the MBRpharma. A significant decrease in aromatics (from 16 to 7) in the MBRpharma permeate was observed, compared to the aerobic MBRpharma. Approximately 21% of compounds in the aerobic MBRcontrol were rejected by membrane filtration, while this increased to 28% in the MBRpharma. Copyright © 2016 Elsevier Ltd. All rights reserved.

  15. Effect of Glycerol and Glucose on the Enhancement of Biomass, Lipid and Soluble Carbohydrate Production by Chlorella vulgaris in Mixotrophic Culture

    Directory of Open Access Journals (Sweden)

    Hong Yang

    2013-01-01

    Full Text Available Biodiesel-derived glycerol is a promising substrate for mixotrophic cultivation of oleaginous microalgae, which can also reduce the cost of microalgal biodiesel. The objective of this study is to investigate the potential of using glycerol and glucose as a complex carbon substrate to produce microalgal biomass and biochemical components, such as photosynthetic pigments, lipids, soluble carbohydrates and proteins by Chlorella vulgaris. The results show that C. vulgaris can utilize glycerol as a sole carbon substrate, but its effect is inferior to that of the mixture of glycerol and glucose. The effect of glycerol and glucose could enhance the algal cell growth rate, biomass content and volumetric productivity, and overcome the lower biomass production on glycerol as the sole organic carbon source in mixotrophic culture medium. The utilization of complex organic carbon substrate can stimulate the biosynthesis of lipids and soluble carbohydrates as the raw materials for biodiesel and bioethanol production, and reduce the anabolism of photosynthetic pigments and proteins. This study provides a promising niche for reducing the overall cost of biodiesel and bioethanol production from microalgae as it investigates the by-products of algal biodiesel production and algal cell hydrolysis as possible raw materials (lipids and carbohydrates and organic carbon substrates (soluble carbohydrates and glycerol for mixotrophic cultivation of microalgae.

  16. Near-field solubility studies

    International Nuclear Information System (INIS)

    Thomason, H.P.; Williams, S.J.

    1992-02-01

    Experimental determinations of the solubilities of americium, plutonium, neptunium, protactinium, thorium, radium, lead, tin, palladium and zirconium are reported. These elements have radioactive isotopes of concern in assessments of radioactive waste disposal. All measurements were made under the highly alkaline conditions typical of the near field of a radioactive waste repository which uses cementitious materials for many of the immobilisation matrices, the backfill and the engineered structures. Low redox potentials, typical of those resulting from the corrosion of iron and steel, were simulated for those elements having more than one accessible oxidation state. The dissolved concentrations of the elements were defined using ultrafiltration. In addition, the corrosion of iron and stainless steel was shown to generate low redox potentials in solution and the solubility of iron(II) at high pH was measured and found to be sufficient for it to act as a redox buffer with respect to neptunium and plutonium. (author)

  17. [Methods quantitative for determination of water-soluble vitamins in premixes and fortified food products by micellar electrokinetic chromatography on short end of the capillary].

    Science.gov (United States)

    Bogachuk, M N; Bessonov, V V; Perederiaev, O I

    2011-01-01

    It was purposed new technique by micellar electrokinetic chromatography on short end of the capillary (capillary electrophoresis system Agilent 3D CE, DAD, quartz capillary HPCE stndrd cap 56 cm, 50 microm, 50 mM borate buffer pH=9,3, 100 mM sodium dodecil sulfate) for simultaneous determination of water-soluble vitamins (B1, B2, B6, B12, PP, B5, B9, C, B8) in fortified food products and premixes. It was observed on 6 samples of vitamin premixes and 28 samples of fortified food products using this technique. Our findings are consistent with the results of research on certain vitamins, conducted by other methods. The developed technique can be used in analysis of water-soluble vitamins in premixes and fortified food products.

  18. Corrosion products behavior and source term reduction : guidelines and feedback for EDF PWRs, concerning the B/Li coordinations and steam generators replacement

    International Nuclear Information System (INIS)

    Taunier, S.; Wintergerst, M.; De Bouvier, O.; Pokor, C.; Carrette, F.; Toivonen, A.; Ranchoux, G.; Bretelle, J.L.

    2010-01-01

    The release of corrosion products by the various components of the primary system into the cooling water may induce some issues on reactor control and on radiation dose rates. Heavy crud deposits may occur on the fuel clad surface and lead to axial offset anomalies (AOA) and in extreme cases, to fuel failures. This deposition phenomenon is apparently associated with steam generator (SG) materials, water chemistry, thermal hydraulics, fuel cleaning or reactor operation history. Moreover, under intense neutron flux, these corrosion products are activated and their dissolution and deposition in the primary system may further increase the out-of-core radioactive contamination and result in radiation dose rates. Several ways are available to reduce the amount and transportation of corrosion products in the primary coolant. A first approach is related to the materials used in the primary system. As one of the main contributors to the release of corrosion products, the Ni-alloy used for the steam generators (SG) tubes has to be properly selected, manufactured and 'passivated'. The paper presents the recent feedback regarding the primary coolant chemistry and radiochemistry after Steam Generators Replacements (SGR). The modified startup procedure of the plant after SGR is also described, as well as its potential benefits on the primary coolant behavior. A second approach is to optimize the primary water chemistry to reduce the release and the transport of the corrosion products through the pH control. This kind of control is important, since higher fuel enrichments are currently used in our reactors, in order to get longer production cycles through higher burn-ups. To ensure the core reactivity control in the PWRs, the concentration of boric acid is increased in the primary water at the beginning of cycle (BOC). As a consequence, the resulting lower pH can induce a higher release of corrosion products from the steam generators. That is why, to keep an almost

  19. Carbon Dioxide Corrosion:

    DEFF Research Database (Denmark)

    Fosbøl, Philip Loldrup

    2008-01-01

    CO2 corrosion is a general problem in the industry and it is expensive. The focus of this study is an oil gas production related problem. CO2 corrosion is observed in offshore natural gas transportation pipelines. A general overview of the problem is presented in chapter 1. The chemical system...... with the basic thermodynamics of electrolytes in chapter 2, the extension and general description of electrolyte mass transport in chapter 3, and the electrochemical kinetics of corrosion in chapter 4. A literature overview of CO2 corrosion is shown in chapter 5 and possible extensions of the models...... and validated against heat capacity data. The model is also fitted to experimental data produced and shown in chapter 8 for SLE in the Na2CO3-NaHCO3-MEG-H2O system. The application of the above model is shown in chapter 9. Here the thermodynamic correction factors are calculated. These show how the diffusion...

  20. Production of a water-soluble fertilizer containing amino acids by solid-state fermentation of soybean meal and evaluation of its efficacy on the rapeseed growth.

    Science.gov (United States)

    Wang, Jianlei; Liu, Zhemin; Wang, Yue; Cheng, Wen; Mou, Haijin

    2014-10-10

    Soybean meal is a by-product of soybean oil extraction and contains approximately 44% protein. We performed solid-state fermentation by using Bacillus subtilis strain N-2 to produce a water-soluble fertilizer containing amino acids. Strain N-2 produced a high yield of protease, which transformed the proteins in soybean meal into peptide and free amino acids that were dissolved in the fermentation products. Based on the Plackett-Burman design, the initial pH of the fermentation substrate, number of days of fermentation, and the ratio of liquid to soybean meal exhibited significant effects on the recovery of proteins in the resulting water-soluble solution. According to the predicted results of the central composite design, the highest recovery of soluble proteins (99.072%) was achieved at the optimum conditions. Under these conditions, the resulting solution contained 50.42% small peptides and 7.9% poly-γ-glutamic acid (γ-PGA). The water-soluble fertilizer robustly increased the activity of the rapeseed root system, chlorophyll content, leaf area, shoot dry weight, root length, and root weight at a concentration of 0.25% (w/v). This methodology offers a value-added use of soybean meal. Copyright © 2014 Elsevier B.V. All rights reserved.

  1. Synergy effect of naphthenic acid corrosion and sulfur corrosion in crude oil distillation unit

    Science.gov (United States)

    Huang, B. S.; Yin, W. F.; Sang, D. H.; Jiang, Z. Y.

    2012-10-01

    The synergy effect of naphthenic acid corrosion and sulfur corrosion at high temperature in crude oil distillation unit was studied using Q235 carbon-manganese steel and 316 stainless steel. The corrosion of Q235 and 316 in corrosion media containing sulfur and/or naphthenic acid at 280 °C was investigated by weight loss, scanning electron microscope (SEM), EDS and X-ray diffractometer (XRD) analysis. The results showed that in corrosion media containing only sulfur, the corrosion rate of Q235 and 316 first increased and then decreased with the increase of sulfur content. In corrosion media containing naphthenic acid and sulfur, with the variations of acid value or sulfur content, the synergy effect of naphthenic acid corrosion and sulfur corrosion has a great influence on the corrosion rate of Q235 and 316. It was indicated that the sulfur accelerated naphthenic acid corrosion below a certain sulfur content but prevented naphthenic acid corrosion above that. The corrosion products on two steels after exposure to corrosion media were investigated. The stable Cr5S8 phases detected in the corrosion products film of 316 were considered as the reason why 316 has greater corrosion resistance to that of Q235.

  2. Positive aspects issued from bio corrosion studies: from hydrogen production to biofuel cells; Des aspects positifs issus des recherches en biocorrosion: de la production d'hydrogene aux biopiles a combustible

    Energy Technology Data Exchange (ETDEWEB)

    Silva Munoz, L. de

    2007-12-15

    Microbially influenced corrosion or bio corrosion is a problem that generates heavy global economic losses (several billion euros per year). In spite of the progress made on the understanding of the underlying mechanisms, the complexity of the phenomenon has prevented finding definitive solutions to the problem and continues to inspire many research works. The participation in bio corrosion of catalytic mechanisms induced by weak acids was studied in this work. Another objective of the thesis has been to take advantage from catalytic phenomena found in bio corrosion research to apply them in other areas: energy production with biofuel cells or electrochemical hydrogen production in mild conditions. This work has shown that the presence of weak acids and amino acids inside bio-films could play a major role in steel bio corrosion accelerating the phenomenon through the catalysis of the water reduction reaction. The reversibility of this mechanism, discerned and proved here, could explain the corrosion increase when hydrogen is removed (bacterial consumption, agitation...). In addition, phosphates allow the production of hydrogen by electrolysis in mild pH conditions (pH 4.0 - 8.0) with an equal or better performance than those found in alkaline electrolysis. Finally, industrial materials like stainless steel and titanium could be used in the fabrication of enzymatic electrodes for biosensors or microsystems. The use of the glucose oxidase/glucose system in an aqueous fuel cell with a stainless steel cathode, allows the improvement of the cell performance thanks to the production of hydrogen peroxide that is easily reduced. Moreover, the use of materials with micro-structured surfaces like sandblasted steels deserve to be studied in detail to exploit the remarkable reactivity they present compared to smooth electrodes. (author)

  3. Effects of COD/N ratio on soluble microbial products in effluent from sequencing batch reactors and subsequent membrane fouling.

    Science.gov (United States)

    Ly, Quang Viet; Nghiem, Long D; Sibag, Mark; Maqbool, Tahir; Hur, Jin

    2018-05-01

    The relative ratios of chemical oxygen demand (COD) to nitrogen (N) in wastewater are known to have profound effects on the characteristics of soluble microbial products (SMP) from activated sludge. In this study, the changes in the SMP characteristics upon different COD/N ratios and the subsequent effects on ultrafiltration (UF) membrane fouling potentials were examined in sequencing batch reactors (SBR) using excitation emission matrix-parallel factor analysis (EEM-PARAFAC) and size exclusion chromatography (SEC). Three unique fluorescent components were identified from the SMP samples in the bioreactors operated at the COD/N ratios of 100/10 (N rich), 100/5 (N medium), and 100/2 (N deficient). The tryptophan-like component (C1) was the most depleted at the N medium condition. Fulvic-like (C2) and humic-like (C3) components were more abundant with N rich wastewater. Greater abundances of large size biopolymer (BP) and low molecular weight neutrals (LMWN) were found under the N deficient and N rich conditions, respectively. SMPs from various COD/N exhibited a greater degree on membrane fouling following the order of 100/2 > 100/10 > 100/5. C1 and C2 had close associations with reversible and irreversible fouling, respectively, while the reversible fouling potential of C3 depended on the COD/N ratios. No significant impact of COD/N ratio was observed on the relative contributions of SMP size fractions to either reversible or irreversible fouling potential. However, the COD/N ratios likely altered the BP foulants' composition with greater contribution of proteinaceous substances to reversible fouling under the N deficient condition than at other N richer conditions. The opposite trend was observed for irreversible fouling. Our results provided further insight into changes in different SMP constitutes and their membrane fouling in response to microbial activities under different COD/N ratios. Copyright © 2018 Elsevier Ltd. All rights reserved.

  4. Soluble Receptor for Advanced Glycation End-Products Predicts Impaired Alveolar Fluid Clearance in Acute Respiratory Distress Syndrome.

    Science.gov (United States)

    Jabaudon, Matthieu; Blondonnet, Raiko; Roszyk, Laurence; Bouvier, Damien; Audard, Jules; Clairefond, Gael; Fournier, Mathilde; Marceau, Geoffroy; Déchelotte, Pierre; Pereira, Bruno; Sapin, Vincent; Constantin, Jean-Michel

    2015-07-15

    Levels of the soluble form of the receptor for advanced glycation end-products (sRAGE) are elevated during acute respiratory distress syndrome (ARDS) and correlate with severity and prognosis. Alveolar fluid clearance (AFC) is necessary for the resolution of lung edema but is impaired in most patients with ARDS. No reliable marker of this process has been investigated to date. To verify whether sRAGE could predict AFC during ARDS. Anesthetized CD-1 mice underwent orotracheal instillation of hydrochloric acid. At specified time points, lung injury was assessed by analysis of blood gases, alveolar permeability, lung histology, AFC, and plasma/bronchoalveolar fluid measurements of proinflammatory cytokines and sRAGE. Plasma sRAGE and AFC rates were also prospectively assessed in 30 patients with ARDS. The rate of AFC was inversely correlated with sRAGE levels in the plasma and the bronchoalveolar fluid of acid-injured mice (Spearman's ρ = -0.73 and -0.69, respectively; P < 10(-3)), and plasma sRAGE correlated with AFC in patients with ARDS (Spearman's ρ = -0.59; P < 10(-3)). Similarly, sRAGE levels were significantly associated with lung injury severity, and decreased over time in mice, whereas AFC was restored and lung injury resolved. Our results indicate that sRAGE levels could be a reliable predictor of impaired AFC during ARDS, and should stimulate further studies on the pathophysiologic implications of RAGE axis in the mechanisms leading to edema resolution. Clinical trial registered with www.clinicaltrials.gov (NCT 00811629).

  5. Skin Autofluorescence Relates to Soluble Receptor for Advanced Glycation End-Products and Albuminuria in Diabetes Mellitus

    Directory of Open Access Journals (Sweden)

    J. Škrha

    2013-01-01

    Full Text Available The aim of this study was to compare skin autofluorescence caused by advanced glycation end-products (AGEs with biochemical markers of endothelial dysfunction and soluble receptor for AGEs (sRAGE in patients with diabetes. Skin autofluorescence (AF assessed by AGE-Reader was evaluated with sRAGE and other biochemical parameters in 88 patients with diabetes (47 Type 1/T1DM/ and 41 Type 2/T2DM/ and 20 controls. Skin AF was significantly higher in T1DM and T2DM in comparison to controls (2.39 ± 0.54, 2.63 ± 0.73 versus 1.96 ± 0.33 AU; P<0.0001. Positive correlation of AF with sRAGE was detected in T1DM and T2DM (r=0.37, P<0.02 and r=0.60, P<0.0001, but not in controls. Significantly higher AF values were found in patients with positive albuminuria as compared to those with normal albuminuria. Similarly, higher AF was detected in patients with endothelial dysfunction expressed by vWF, ICAM-1, and VCAM-1. Multiple regression analysis revealed independent association of skin AF with age, sRAGE, and albumin-creatinine ratio in patients with diabetes (R2=0.38. Our study confirms that AF is elevated in patients with diabetes, especially with positive albuminuria and endothelial dysfunction. The strong and independent relationship between AF and sRAGE supports the idea that AF may reflect AGEs/RAGE interactions. The exact mechanism remains to be established.

  6. Corrosivity Index Copper and Steel at Two Locations in Villahermosa, Tabasco

    Directory of Open Access Journals (Sweden)

    Tejero-Rivas María Candelaria

    2015-03-01

    Full Text Available This paper presents a study of the atmospheric corrosion of copper and carbon steel made ​​in two environments Villahermosa, Tabasco for six months. The test site of the industrial zone started Villahermosa Institute of Technology (ITVH and rural-urban site at the Technological University of Tabasco (UTTAB. Aluminum in combination with a screw carbon steel provided the index marine corrosivity (MA, the brass screw gives the index of industrial corrosivity (IA; wire method of screw according to ASTM G116-93 was used and the plastic screw nylon gives the rate of rural-urban corrosivity (RUA. The determination of air pollutants (sulfur dioxide and chlorides, was with the methods of wet candle and sulfation plates according to ISO 9225. Morphology studies were performed on the corrosion products formed on the specimens screw, using scanning electron microscopy coupled with energy dispersive. The corrosion products that formed on the surface of copper and carbon steel, having a bulb-shaped morphology characteristic of the addition of soluble salts, particularly sulphates and chlorides, were identified in the two stations.

  7. Influence of hydrazine primary water chemistry on corrosion of fuel cladding and primary circuit components

    International Nuclear Information System (INIS)

    Iourmanov, V.; Pashevich, V.; Bogancs, J.; Tilky, P.; Schunk, J.; Pinter, T.

    1999-01-01

    Earlier at Paks 1-4 NPP standard ammonia chemistry was in use. The following station performance indicators were improved when hydrazine primary water chemistry was introduced: occupational radiation exposures of personnel; gamma-radiation dose rates near primary system components during refuelling and maintenance outages. The reduction of radiation exposures and radiation fields were achieved without significant expenses. Recent results of experimental studies allowed to explain the mechanism of hydrazine dosing influence on: corrosion rate of structure materials in primary coolant; behaviour of soluble and insoluble corrosion products including long-life corrosion-induced radionuclides in primary system during steady-state and transient operation modes; radiolytic generation of oxidising radiolytic products in core and its corrosion activity in primary system; radiation situation during refuelling and maintenance outages; foreign material degradation and removal (including corrosion active oxidant species) from primary system during abnormal events. Operational experience and experimental data have shown that hydrazine primary water chemistry allows to reduce corrosion wear and thereby makes it possible to extend the life-time of plant components in primary system. (author)

  8. Radiation effects in moist-air systems and the influence of radiolytic product formation on nuclear waste glass corrosion

    International Nuclear Information System (INIS)

    Wronkiewicz, D.J.; Bates, J.K.; Buck, E.C.; Hoh, J.C.; Emery, J.W.; Wang, L.M.

    1997-07-01

    Ionizing radiation may affect the performance of glass in an unsaturated repository site by interacting with air, water vapor, or liquid water to produce a variety of radiolytic products. Tests were conducted to examine the effects of radiolysis under high gas/liquid ratios. Results indicate that nitrate is the predominant radiolytic product produced following both gamma and alpha radiation exposure, with lesser amounts of nitrite and carboxylic acids. The formation of nitrogen acids during exposure to long-lived, alpha-particle-emitting transuranic elements indicates that these acids may play a role in influencing nuclear waste form reactions in a long-term unsaturated disposal scenario. Experiments were also conducted with samples that simulate the composition of Savannah River Plant nuclear waste glasses. Radiolytic product formation in batch tests (340 m -1 , 90 C) resulted in a small increase in the release rates of many glass components, such as alkali and alkaline earth elements, although silicon and uranium release rates were slightly reduced indicating an overall beneficial effect of radiation on waste form stability. The radiolytic acids increased the rate of ion exchange between the glass and the thin film of condensate, resulting in accelerated corrosion rates for the glass. The paragenetic sequence of alteration phases formed on both the irradiated and nonirradiated glass samples reacted in the vapor hydration tests matches closely with those developed during volcanic glass alteration in naturally occurring saline-alkaline lake systems. This correspondence suggests that the high temperatures used in these tests have not changed the underlying glass reaction mechanism relate to that which controls glass reactions under ambient surficial conditions

  9. Radiation effects in moist-air systems and the influence of radiolytic product formation on nuclear waste glass corrosion

    Energy Technology Data Exchange (ETDEWEB)

    Wronkiewicz, D.J.; Bates, J.K.; Buck, E.C.; Hoh, J.C.; Emery, J.W. [Argonne National Lab., IL (United States). Chemical Technology Div.; Wang, L.M. [Univ. of New Mexico, Albuquerque, NM (United States). Dept. of Geology

    1997-07-01

    Ionizing radiation may affect the performance of glass in an unsaturated repository site by interacting with air, water vapor, or liquid water to produce a variety of radiolytic products. Tests were conducted to examine the effects of radiolysis under high gas/liquid ratios. Results indicate that nitrate is the predominant radiolytic product produced following both gamma and alpha radiation exposure, with lesser amounts of nitrite and carboxylic acids. The formation of nitrogen acids during exposure to long-lived, alpha-particle-emitting transuranic elements indicates that these acids may play a role in influencing nuclear waste form reactions in a long-term unsaturated disposal scenario. Experiments were also conducted with samples that simulate the composition of Savannah River Plant nuclear waste glasses. Radiolytic product formation in batch tests (340 m{sup {minus}1}, 90 C) resulted in a small increase in the release rates of many glass components, such as alkali and alkaline earth elements, although silicon and uranium release rates were slightly reduced indicating an overall beneficial effect of radiation on waste form stability. The radiolytic acids increased the rate of ion exchange between the glass and the thin film of condensate, resulting in accelerated corrosion rates for the glass. The paragenetic sequence of alteration phases formed on both the irradiated and nonirradiated glass samples reacted in the vapor hydration tests matches closely with those developed during volcanic glass alteration in naturally occurring saline-alkaline lake systems. This correspondence suggests that the high temperatures used in these tests have not changed the underlying glass reaction mechanism relate to that which controls glass reactions under ambient surficial conditions.

  10. In vitro evaluation of iron solubility and dialyzability of various iron fortificants and of iron-fortified milk products targeted for infants and toddlers.

    Science.gov (United States)

    Kapsokefalou, Maria; Alexandropoulou, Isidora; Komaitis, Michail; Politis, Ioannis

    2005-06-01

    The objectives of the present study were: to compare the solubility and dialyzability of various iron fortificants (iron pyrophosphate, ferrous bis-glycinate, ferrous gluconate, ferrous lactate, ferrous sulfate) added, in the presence of ascorbic acid, to pasteurized milk samples produced under laboratory conditions; and to compare the solubility and dialyzability of iron in commercial pasteurized, UHT and condensed milk products available in the Greek market fortified with various vitamins and minerals including iron and targeted towards infants (6-12 months old) and toddlers. Iron solubility and dialyzability were determined using a simulated gastrointestinal digestive system. Ferrous dialyzable iron (molecular weight lower than 8000) was used as an index for prediction of iron bioavailability. Ferrous dialyzable iron in pasteurized milk samples fortified with iron pyrophosphate, ferrous lactate and ferrous bis-glycinate was higher (P iron in products fortified with ferrous lactate was not different (P > 0.05) from those fortified with ferrous sulfate. Ferrous dialyzable iron in four condensed commercial milk products was higher (P iron was higher (P iron source, milk processing and the overall product composition affect formation of ferrous dialyzable iron and may determine the success and effectiveness of iron fortification of milk.

  11. Application of CATE 2.0 code on evaluating activated corrosion products in a PWR cooling loop

    Energy Technology Data Exchange (ETDEWEB)

    Zhang, Jingyu; Li, Lu; Chen, Yixue [North China Electric Power Univ., Beijing (China). School of Nuclear Science and Engineering

    2017-03-15

    In PWR plants, most Occupational Radiation Exposure (ORE) for personnel results from Activated Corrosion Products (ACPs) in the cooling loop. In order to evaluate the ACPs in the cooling loop, a three-region transport model is built up based on the theory of driving force from the concentration difference in CATE 2.0 code. In order to analyze the nuclide composition of ACPs, the EAF-2007 nuclear database is embedded in CATE 2.0. The case of MIT PCCL test loop is simulated to test the availability of CATE 2.0 on PWR ACPs evaluation, and the activity of Co-58 and Co-60 after operation for 42 days calculated by CATE 2.0 is consistent with that from the code CRUDSIM adopted by MIT. Then, the nuclide composition of ACPs is analyzed in detail respectively for operation of 42 days and 12 months using CATE 2.0. The results show that the short-lived nuclides contribute a majority of the activity in the regions of in-flux wall and coolant, while the long-lived nuclides contribute most of the activity in the region of out-flux wall.

  12. Numerical simulation of heat-transfer and insoluble corrosion product deposition in lead-bismuth eutectic alloy

    International Nuclear Information System (INIS)

    Yang Xu; Zhou Tao; Fang Xiaolu; Lin Daping; Ru Xiaolong

    2015-01-01

    As the primary coolant of ADS (accelerator driven sub-critical system), the safety of reactor will be threatened and the lifetime of the reactor will be shortened by appearing of the tiny particles in LBE (lead-bismuth eutectic) alloy. To this end, numerical simulation with the code of FLUENT was used to research the deposition distribution of insoluble corrosion products in rectangular channel. The standard k-ε model was selected to predict the turbulence variation in the rectangular channel. The discrete phase model (DPM) was used to track the trajectory of the particles. It is found that the deposition efficiency is positively correlated with the temperature difference between the fluid and cold wall. The near wall region with a high concentration of particulate matter and low temperature is in favor of particulate matter deposition on the wall. At the same time, the high turbulence kinetic near wall region is not conducive to the deposition of particulate matter. A secondary flow phenomenon occurs under the influence of boundary wall, namely that there are eight symmetrical regions in the radial direction. (authors)

  13. Analysis of the corrosion products on galvanized steels by FTIR spectroscopy

    International Nuclear Information System (INIS)

    Kasperek, J.

    1998-01-01

    FTIR reflectance spectroscopy has been used for the characterization of products formed by an accelerated wet ageing test on industrial hot-dip galvanized steel. Several aluminium contents are selected. Various products have been detected in this study. The kind and amount vary with the substrate, the type of ageing test used, the relative humidity level and the temperature. The galvanized coatings studied show a mixed zinc-aluminium compound, Zn 6 Al 2 (OH) 16 CO 3 .4H 2O. This phase is observed from the first exposure time on all coatings regardless of the amount of aluminium. Contrary to zinc, no basic aluminium compound has been detected. (orig.)

  14. Effect of Soybean Meal and Soluble Starch on Biogenic Amine Production and Microbial Diversity Using Rumen Fermentation

    Directory of Open Access Journals (Sweden)

    Chang-Dae Jeong

    2015-01-01

    Full Text Available This study was conducted to investigate the effect of soybean meal (SM and soluble starch (SS on biogenic amine production and microbial diversity using in vitro ruminal fermentation. Treatments comprised of incubation of 2 g of mixture (expressed as 10 parts containing different ratios of SM to SS as: 0:0, 10:0, 7:3, 5:5, 3:7, or 0:10. In vitro ruminal fermentation parameters were determined at 0, 12, 24, and 48 h of incubation while the biogenic amine and microbial diversity were determined at 48 h of incubation. Treatment with highest proportion of SM had higher (p<0.05 gas production than those with higher proportions of SS. Samples with higher proportion of SS resulted in lower pH than those with higher proportion of SM after 48 h of incubation. The largest change in NH3-N concentration from 0 to 48 h was observed on all SM while the smallest was observed on exclusive SS. Similarly, exclusive SS had the lowest NH3-N concentration among all groups after 24 h of incubation. Increasing methane (CH4 concentrations were observed with time, and CH4 concentrations were higher (p<0.05 with greater proportions of SM than SS. Balanced proportion of SM and SS had the highest (p<0.05 total volatile fatty acid (TVFA while propionate was found highest in higher proportion of SS. Moreover, biogenic amine (BA was higher (p<0.05 in samples containing greater proportions of SM. Histamines, amine index and total amines were highest in exclusive SM followed in sequence mixtures with increasing proportion of SS (and lowered proportion of SM at 48 h of incubation. Nine dominant bands were identified by denaturing gradient gel electrophoresis (DGGE and their identity ranged from 87% to 100% which were mostly isolated from rumen and feces. Bands R2 (uncultured bacterium clone RB-5E1 and R4 (uncultured rumen bacterium clone L7A_C10 bands were found in samples with higher proportions of SM while R3 (uncultured Firmicutes bacterium clone NI_52, R7 (Selenomonas sp

  15. Prediction of crude protein digestibility of animal by-product meals for dogs by the protein solubility in pepsin method.

    Science.gov (United States)

    Kawauchi, Iris M; Sakomura, Nilva K; Pontieri, Cristiana F F; Rebelato, Aline; Putarov, Thaila C; Malheiros, Euclides B; Gomes, Márcia de O S; Castrillo, Carlos; Carciofi, Aulus C

    2014-01-01

    Animal by-product meals have large variability in crude protein (CP) content and digestibility. In vivo digestibility procedures are precise but laborious, and in vitro methods could be an alternative to evaluate and classify these ingredients. The present study reports prediction equations to estimate the CP digestibility of meat and bone meal (MBM) and poultry by-product meal (PM) using the protein solubility in pepsin method (PSP). Total tract CP digestibility of eight MBM and eight PM samples was determined in dogs by the substitution method. A basal diet was formulated for dog maintenance, and sixteen diets were produced by mixing 70 % of the basal diet and 30 % of each tested meal. Six dogs per diet were used to determine ingredient digestibility. In addition, PSP of the MBM and PM samples was determined using three pepsin concentrations: 0·02, 0·002 and 0·0002 %. The CP content of MBM and PM ranged from 39 to 46 % and 57 to 69 %, respectively, and their mean CP digestibility by dogs was 76 (2·4) and 85 (2·6) %, respectively. The pepsin concentration with higher Pearson correlation coefficients with the in vivo results were 0·0002 % for MBM (r 0·380; P = 0·008) and 0·02 % for PM (r 0·482; P = 0·005). The relationship between the in vivo and in vitro results was better explained by the following equations: CP digestibility of MBM = 61·7 + 0·2644 × PSP at 0·0002 % (P = 0·008; R (2) 0·126); and CP digestibility of PM = 54·1 + 0·3833 × PSP at 0·02 % (P = 0·005; R (2) 0·216). Although significant, the coefficients of determination were low, indicating that the models were weak and need to be used with caution.

  16. Corrosion control in nuclear fuel reprocessing

    International Nuclear Information System (INIS)

    Steele, D.F.

    1986-01-01

    This article looks in detail at tribology-related hazards of corrosion in irradiated fuel reprocessing plants and tries to identify and minimize problems which could contribute to disaster. First, the corrosion process is explained. Then the corrosion aspects at each of four stages in reprocessing are examined, with particular reference to oxide fuel reprocessing. The four stages are fuel receipt and storage, fuel breakdown and dissolution, solvent extraction and product concentration and waste management. Results from laboratory and plant corrosion trails are used at the plant design stage to prevent corrosion problems arising. Operational procedures which minimize corrosion if it cannot be prevented at the design stage, are used. (UK)

  17. Corrosion Engineering.

    Science.gov (United States)

    White, Charles V.

    A description is provided for a Corrosion and Corrosion Control course offered in the Continuing Engineering Education Program at the General Motors Institute (GMI). GMI is a small cooperative engineering school of approximately 2,000 students who alternate between six-week periods of academic study and six weeks of related work experience in…

  18. Evaluating energy efficient strategies and product quality for distillers' dried grains with solubles (DDGS) in dry-grind ethanol plants

    Science.gov (United States)

    Lan, Tian

    The drying of distillers dried grains with solubles (DDGS), a coproduct of dry-grind corn processing to ethanol utilizes about 30% of the total energy required for the production of a liter of fuel ethanol. Therefore, improving DDGS drying energy efficiency could have significant impact on the economics of the dry-grind corn-to-ethanol process. Drying process improvements must take account into the effects of various drying strategies on the final quality of DDGS which is primarily utilized as a feed ingredient. Previous studies in the literature have shown that physical and chemical properties of DDGS vary according to the ratio of the two primarily feed streams, wet distillers grains (WDG) and condensed distillers solubles (CDS) which make up DDGS. Extensive research using plant-scale and bench-scale experiments have been conducted on the effect of process variables (ratios of WDG, CDS and DDGS add-back) during drying on the physical and chemical properties of DDGS. However, these investigations did not correlate the product characteristics data to drying efficiency. Additionally, it cannot be clearly determined from the literature on DDGS drying that processes used in the industry are optimized for both product quality and energy efficiency. A bench-scale rotary drum dryer heated by an electrically powered heat gun was used to investigate the effects of WDG, CDS and add-back ratios on both energy efficiency, drying performance and DDGS physical and chemical properties. A two stage drying process with the bench-scale rotary dryer was used to simulate the drying of DDGS using ICM (ICM, Inc., Colwich, KS) dry-grind process technology for DDGS drying which uses two rotary drum dryers in series. Effects of drying process variables, CDS content (0, 10, 20 and 40% by mass) and percent DDGS add-back (0, 20, 40 and 60% by mass) on energy performance and product quality were determined. Sixteen different drying strategies based on drying process variable ratios were

  19. Use of a post-production fractionation process improves the nutritional value of wheat distillers grains with solubles for young broiler chicks

    OpenAIRE

    Thacker, Philip; Deep, Aman; Beltranena, Eduardo

    2013-01-01

    Background Post-production fractionation of wheat distillers grains with solubles (DDGS) increases their crude protein content and reduces their fiber content. This experiment was conducted to determine the effects of fractionation of wheat DDGS on apparent total tract digestibility (ATTD) and performance when fed to broiler chicks (0?21 d). Methods A total of 150, day-old, male broiler chicks (Ross-308 line; Lilydale Hatchery, Wynyard, Saskatchewan) weighing an average of 49.6 ? 0.8 g were a...

  20. Consequences of Ingestions of Potentially Corrosive Cleaning Products, One-Year Follow-Up

    Czech Academy of Sciences Publication Activity Database

    Mrázová, K.; Navrátil, Tomáš; Pelclová, D.

    2012-01-01

    Roč. 7, č. 3 (2012), s. 1734-1748 ISSN 1452-3981 R&D Projects: GA AV ČR IAA400400806 Institutional research plan: CEZ:AV0Z40400503 Keywords : Czech Toxicological Information Centre * cleaning products * consequences Subject RIV: CG - Electrochemistry Impact factor: 3.729, year: 2011 http://www.electrochemsci.org/papers/vol7/7031734.pdf