  1. Waterside corrosion of zirconium alloys in nuclear power plants

    International Nuclear Information System (INIS)

    1998-01-01

    Technically the study of corrosion of zirconium alloys in nuclear power reactors is a very active field and both experimental work and understanding of the mechanisms involved are going through rapid changes. As a result, the lifetime of any publication in this area is short. Because of this it has been decided to revise IAEA-TECDOC-684 - Corrosion of Zirconium Alloys in Nuclear Power Plants - published in 1993. This updated, revised and enlarged version includes major changes to incorporate some of the comments received about the first version. Since this review deals exclusively with the corrosion of zirconium and zirconium based alloys in water, and another separate publication is planned to deal with the fuel-side corrosion of zirconium based fuel cladding alloys, i.e. stress corrosion cracking, it was decided to change the original title to Waterside Corrosion of Zirconium Alloys in Nuclear Power Plants. The rapid changes in the field have again necessitated a cut-off date for incorporating new data. This edition incorporates data up to the end of 1995; including results presented at the 11 International Symposium on Zirconium in the Nuclear Industry held in Garmisch-Partenkirchen, Germany, in September 1995. The revised format of the review now includes: Introductory chapters on basic zirconium metallurgy and oxidation theory; A revised chapter discussing the present extent of our knowledge of the corrosion mechanism based on laboratory experiments; a separate and revised chapter discussing hydrogen uptake; a completely reorganized chapter summarizing the phenomenological observations of zirconium alloy corrosion in reactors; a new chapter on modelling in-reactor corrosion; a revised chapter devoted exclusively to the manner in which irradiation might influence the corrosion process; finally, a summary of our present understanding of the corrosion mechanisms operating in reactor

  2. Corrosion of Zircaloy-clad fuel rods in high-temperature PWRs: Measurement of waterside corrosion in North Anna Unit 1

    International Nuclear Information System (INIS)

    Balfour, M.G.; Kilp, G.R.; Comstock, R.J.; McAtee, K.R.; Thornburg, D.R.

    1992-03-01

    Twenty-four peripheral rods and two interior rods from North Anna Unit 1, End-of-Cycle 7, were measured at poolside for waterside corrosion on four-cycle Region 6 assemblies F35 and F66, with rod average burnups of 60 GWD/MTU. Similar measurements were obtained on 24 two-cycle fuel rods from Region 8A assemblies H02 and H10 with average burnups of about 40 GWD/MTU. The Region 6 peripheral rods had been corrosion measured previously after three cycles, at 45 GWD/MTU average burnup. The four-cycle Region 6 fuel rods showed high corrosion, compared to only intermediate corrosion level after three cycles. The accelerated corrosion rate in the fourth cycle was accompanied by extensive laminar cracking and spalling of the oxide film in the thickest regions. The peak corrosion of the two-cycle region 8A rods was 32 μm to 53 μm, with some isolated incipient oxide spalling. In conjunction with the in-reactor corrosion measurements, extensive characterization tests plus long-term autoclave corrosion tests were performed on archive samples of the three major tubing lots represented in the North Anna measurements. The autoclave tests generally showed the same ordering of corrosion by tubing lot as in the reactor; the chief difference between the archive tubing samples was a lower tin content (1.38 percent) for the lot with the lowest corrosion rate compared with a higher tin content (1.58) for the lot with the highest corrosion rate. There was no indication in the autoclave tests of an accelerated rate of corrosion as observed in the reactor

  3. FORMATION OF WATERSIDES ON THE BOSPORUS AND SPATIAL DEVELOPMENT OF BOSPORUS WATERSIDE GARDENS

    Directory of Open Access Journals (Sweden)

    Petek JAWDET ABDULLA

    2014-01-01

    Full Text Available As one of the unique beauties of Bosporus, Bosporus watersides have been composed and formed through long ages along the Bosporus. Not only an architectural form and a residential type, the Bosporus watersides also were being a part of the culture in which they were built. They project the life traditions of the ages in which they were built. Their users were using those buildings as summer resorts, comprised of a hall, wide rooms, kitchen and other components. The gardens of the watersides also have had their own characteristics, and they were setting out unique beauties. The gardens of the watersides in Bosporus were beyond comparison by their organizational schemes and landscape designs. The watersides were designed with a garden within the bounds of spatial possibilities. The gardens were decorated with colorful flowery plants. Many watersides, which were built in Bosporus, have reached until today. As a type of residences, these buildings are among the most important buildings of Bosporus. The Bosporus watersides have unique architectural samples and features and they need to be well preserved. However, it has been identified that some of those structures have disappeared in time. There are many causes for such a removal. By analyzing these causes, we need to preserve these buildings better nowadays. Bosporus watersides and their gardens today need a better protection by effective policies to be produced. Having unique architectural features and styles, those buildings also are a part of our culture. We must better protect our historical and cultural patterns. This is a must to respect our history and culture too.

  4. Correlation of waterside corrosion and cladding microstructure in high-burnup fuel and gadolinia rods

    International Nuclear Information System (INIS)

    Chung, H.M.

    1989-09-01

    Waterside corrosion of the Zircaloy cladding has been examined in high-burnup fuel rods from several BWRs and PWRs, as well as in 3 wt % gadolinia burnable poison rods obtained from a BWR. The corrosion behavior of the high-burnup rods was then correlated with results from a microstructural characterization of the cladding by optical, scanning-electron, and transmission-electron microscopy (OM, SEM, and TEM). OM and SEM examination of the BWR fuel cladding showed both uniform and nodular oxide layers 2 to 45 μm in thickness after burnups of 11 to 30 MWd/kgU. For one of the BWRs, which was operated at 307 degree C rather than the normal 288 degree C, a relatively thick (50 to 70 μm) uniform oxide, rather than nodular oxides, was observed after a burnup of 27 to 30 MWd/kgU. TEM characterization revealed a number of microstructural features that occurred in association with the intermetallic precipitates in the cladding metal, apparently as a result of irradiation-induced or -enhanced processes. The BWR rods that exhibited white nodular oxides contained large precipitates (300 to 700 nm in size) that were partially amorphized during service, indicating that a distribution of the large intermetallic precipitates is conductive to nodular oxidation. 23 refs., 9 figs

  5. An assessment of the waterside corrosion and hydrogen pick-up in the zircaloy-2 pressure tubes of PHWR

    International Nuclear Information System (INIS)

    Sah, D.N.

    1992-01-01

    In view of the deleterious effect of hydriding on the operating life of zircaloy-2 pressure tubes in PHWRs there is an urgent need for the assessment of the status of the pressure tubes with respect to corrosion and hydrogen pick-up in the operating PHWRs. A model has been developed for analysing the waterside corrosion and hydrogen pick-up in the zircaloy-2 pressure tubes under reactor operating conditions. This model predicts the axial profiles of oxide layer thickness and hydrogen pick-up in the pressure tubes as a function of the operating time of the reactor. The prediction of hydrogen pick-up by the model in the F-10 pressure tube of RAPS-I have been found to be in good agreement with the measured value of hydrogen content. This report gives a brief description of the model and its predictions on the present status of hydrogen pick-up in the pressure tubes of lead reactor RAPS-II. (author). 6 refs., 5 figs., 2 tabs

  6. Zircaloy-4 corrosion in PWR's

    International Nuclear Information System (INIS)

    Fyfitch, S.; Smalley, W.R.; Roberts, E.

    1985-01-01

    Zircaloy-4 waterside corrosion has been studied extensively in the nuclear industry for a number of years. Following the early crud-related corrosion failures in the Saxton test reactor, Westinghouse undertook numerous programs to minimize crud deposition on fuel rods in power reactors through primary coolant chemistry control. Modern plants today are operating with improved coolant chemistry guidelines, and crud deposition levels are very low in proportion to earlier experience. Zircaloy-4 corrosion under a variety of coolant chemistry, heat flux and exposure conditions has been studied extensively. Experience to date, even in relatively high coolant temperature plants, has indicated that -for both fuel cladding and structural components- Zircaloy-4 waterside corrosion performance has been excellent. Recognizing future industry trends, however, which will result in Zircaloy-4 being subjected to ever increasing corrosion duties, Westinghouse will continue accumulating Zircaloy-4 corrosion experience in large power plants. 13 refs.

  7. Study on the behavior of waterside corroded PWR fuel rods under reactivity initiated accident conditions

    International Nuclear Information System (INIS)

    Sasajima, Hideo

    1989-06-01

    One of the highlighted problems from the fuel reliability point of view is a waterside corrosion of fuel cladding which becomes more significant at extended burnup stages. To date, at highly burned fuel, waterside corrosion was recognized as important because cladding oxidation increased with increasing burn-up. In experiments, as the basic research for the study of high burn-up fuel, the test fuel rods were prepressurized to ranges from 3.47 to 3.55 MPa, oxidized artificially to both 10 and 20 μm in thickness. Regarding fabricated oxide thickness of 10 μm, it is corresponded to be transition point from cubic law to linear law as a function of burn-up. Pulse irradiation experiments by NSRR were carried out to study the behavior of waterside corroded PWR type fuels under RIA conditions. Obtained results are: (1) The failure threshold of tested fuels was 110 cal/g·fuel (0.46 KJ/g·fuel) in enthalpy. This showed that the failure threshold of tested fuels was same as that of the past NSRR experimental data. (2) The failure mechanisms of the tested fuel rods was cladding rupture induced by ballooning. No differences in failure mechanisms existed between the past NSRR prepressurized standard fuel and the tested fuels. (3) Cracks were existed without propagating into cladding matrix, so that it was judged that these were not initiation of failure. (4) Whithin this experimental condition, reduction of cladding thickness being attributed to the increase of oxidation did not failure threshold. (author)

  8. Experience of decontaminating of the ventilation system electric motors and main circulation and waterside pump drive electric motors in conditions of the Chernobyl' NPP

    International Nuclear Information System (INIS)

    Denisov, V.I.; Karataev, B.A.; Platonov, A.I.; Potekhin, V.B.; Ryumin, G.V.; Sorokin, N.M.; Fenogenov, V.A.; Cheremshin, P.I.

    1989-01-01

    The ventilation system electric motor decontamination is described. In decontaminating waterside pump rotors and stators with high level of contamination was developed a procedure, eliminating corrosion action and damage of electric isolation coatings

  9. Influence of alkali metal oxides and alkaline earth metal oxides on the mitigation of stress corrosion cracking in CANDU fuel sheathing

    Energy Technology Data Exchange (ETDEWEB)

    Metzler, J.; Ferrier, G.A.; Farahani, M.; Chan, P.K.; Corcoran, E.C., E-mail: Joseph.Metzler@rmc.ca [Royal Military College of Canada, Kingston, ON (Canada)

    2015-07-01

    Stress corrosion cracking (SCC)can cause failures of CANDU Zircaloy-4 fuel sheathing. The process occurs when a corrosive element (i.e.,iodine) interacts with a susceptible material that is under sufficient strain at a high temperature. Currently, there is an ongoing effort to improve SCC mitigation strategies for future iterations of CANDU reactors. A potential mechanism for SCC mitigation involves utilizing alkali metal oxides and alkaline earth metal oxides that will sequester corrosive iodine while actively repairing a protective oxide layer on the sheath. SCC tests performed with sodium oxide (Na{sub 2}O) and calcium oxide (CaO) have shown to decrease significantly the sheath degradation. (author)

  10. Influence of alkali metal oxides and alkaline earth metal oxides on the mitigation of stress corrosion cracking in CANDU fuel sheathing

    Energy Technology Data Exchange (ETDEWEB)

    Metzler, J.; Ferrier, G.A.; Farahani, M.; Chan, P.K.; Corcoran, E.C., E-mail: Joseph.Metzler@rmc.ca [Royal Military College of Canada, Kingston, ON (Canada)

    2015-07-01

    This work investigates strategies to mitigate stress corrosion cracking (SCC) in Zircaloy-4 sheathing materials. The CANLUB coatings currently used in CANDU reactors contain both alkali metal and alkaline earth metal impurities, which can exist as oxides (e.g., Na{sub 2}O and CaO). It is believed that when the corrosive fission product iodine reacts with these oxides, the iodine can be sequestered through the formation of an iodide (e.g.,NaI and CaI{sub 2}). The subsequent O{sub 2} release may repair cracks in the protective ZrO{sub 2} layer on the sheathing, shielding the Zircaloy-4 sheathing from further corrosive fission product attack. For this investigation, O{sub 2} gas, Na{sub 2}O, and CaO were separately introduced into an environment wherein slotted Zircaloy-4 rings endure mechanical stresses in iodine vapour at high temperatures. Controlled additions of O{sub 2} gas created a slight reduction in the corrosive attack on Zircaloy-4 sheathing, while the inclusion of Na{sub 2}O and CaO lead to greater reductions. (author)

  11. Modelling the waterside corrosion of PWR fuel rods

    International Nuclear Information System (INIS)

    Abram, T.J.

    1997-01-01

    The mechanism of zirconium alloy cladding corrosion in PWRs is briefly reviewed, and an engineering corrosion model is proposed. The basic model is intended to produce a best-estimate fit to circumferentially-average oxide thickness measurements obtained from inter-span positions, way from the effects of structural or flow mixing grids. The model comprises an initial pre-transition weight gain expression which follows cubic rate kinetics. On reaching a critical oxide thickness, a transition to linear rate kinetics occurs. The post-transition corrosion rate includes a term which is dependent on fast neutron flux, and an Arrhenius thermal corrosion rate which has been fitted to isothermal ex-reactor data. This thermal corrosion rate is enhanced by the presence of lithium in the coolant, and by the concentration of hydrogen in the cladding. Different cladding materials are accounted for in the selection of the model constants, and results for standard Zircaloy-4, low tin (or ''optimized'') Zircaloy-4, and the Westinghouse advanced alloy ZIRLO TM are presented. A method of accounting for the effects of grids is described, and the application of the model within the ENIGMA-B and ZROX codes is discussed. (author). 35 refs, 6 figs, 3 tabs

  12. Waterside corrosion of zirconium alloys in nuclear power plants

    International Nuclear Information System (INIS)

    Jeong, Yong Hwan; Baek, B. J.; Park, S. Y. and others

    1999-08-01

    The overview of corrosion and hydriding behaviors of Zr-based alloy under the conditions of the in-reactor service and in the absence of irradiation is introduced in this report. The metallurgical characteristics of Zr-based alloys and the thermo-mechanical treatments on the microstructures and the textures in the manufacturing process for fuel cladding are also introduced. The factors affecting the corrosion of Zr alloy in reactor are summarized. And the corrosion mechanism and hydrogen up-take are discussed based on the laboratory and in-reactor results. The phenomenological observations of zirconium alloy corrosion in reactors are summarized and the models of in-reactor corrosion are exclusively discussed. Finally, the effects of irradiation on the corrosion process in Zr alloy were investigated mainly based on the literature data. (author). 538 refs., 26 tabs., 105 figs

  13. Modelling the waterside corrosion of PWR fuel rods

    Energy Technology Data Exchange (ETDEWEB)

    Abram, T J [Fuel Engineering Dept., British Nuclear Fuels plc, Salwick, Preston (United Kingdom)

    1997-08-01

    The mechanism of zirconium alloy cladding corrosion in PWRs is briefly reviewed, and an engineering corrosion model is proposed. The basic model is intended to produce a best-estimate fit to circumferentially-average oxide thickness measurements obtained from inter-span positions, way from the effects of structural or flow mixing grids. The model comprises an initial pre-transition weight gain expression which follows cubic rate kinetics. On reaching a critical oxide thickness, a transition to linear rate kinetics occurs. The post-transition corrosion rate includes a term which is dependent on fast neutron flux, and an Arrhenius thermal corrosion rate which has been fitted to isothermal ex-reactor data. This thermal corrosion rate is enhanced by the presence of lithium in the coolant, and by the concentration of hydrogen in the cladding. Different cladding materials are accounted for in the selection of the model constants, and results for standard Zircaloy-4, low tin (or ``optimized``) Zircaloy-4, and the Westinghouse advanced alloy ZIRLO{sup TM} are presented. A method of accounting for the effects of grids is described, and the application of the model within the ENIGMA-B and ZROX codes is discussed. (author). 35 refs, 6 figs, 3 tabs.

  14. A state-of-the art report on the investigation of the various corrosion models for zirconium-based alloy

    International Nuclear Information System (INIS)

    Kim, S. J.; Kim, K. H.; Baek, J. H.; Choi, B. K.; Jeong, Y. H.

    1999-02-01

    The desire to increase uranium utilization and to minimize spent fuel storage requirements provides an incentive to extend the average fuel rod discharge burnup to about 70,000MWd/MTU. For these higher burnups data are needed to determine if waterside corrosion of the cladding may be a life-limiting feature of fuel rod design. It is apparent that many factors can influence waterside corrosion, and these need to be better understood in order to minimize corrosion at these higher target burnups. The objective of this report is to review published data relevant to the corrosion of Zircaloy under PWR operating conditions. (author). 100 refs., 4 tabs., 21 figs

  15. Study on the Folk Costume Symbolization in Waterside Villages of Southern Yangtze in China

    Institute of Scientific and Technical Information of China (English)

    CUI Rong-rong; TAO Hui; SHEN Lin-lin

    2007-01-01

    The folk costume in waterside villages of Southern Yangtze in China was notonly daily consumer goods, but also a symbol system of foR-custom culture. This symbol system was directly conveyed by a series medley shape signs, many-faceted color signs and decorated craft signs of pleated skirt. Its origination, accumulation, continual process and development were greatly associated with the life style and paddy culture of waterside villages, such as the folk religion, social life, artistic philosophy, regional culture, the landform of waterside villages and the humanity environment. So the folk costume was the significant sign of practical function and also the significative sign of folk traditional culture, both of which composed the costume cultural symbol system of waterside villages of Southern Yangtze called " integration of aesthetic and practical function".

  16. Corrosion products in power generating systems

    International Nuclear Information System (INIS)

    Lister, D.H.

    1980-06-01

    The important mechanisms of corrosion and corrosion product movement and fouling in the heat transport systems of thermal electric generating stations are reviewed. Oil- and coal-fired boilers are considered, along with nuclear power systems - both direct and indirect cycle. Thus, the fireside and waterside in conventional plants, and the primary coolant and steam-raising circuits in water-cooled reactors, are discussed. Corrosion products in organic- and liquid-metal-cooled reactors also are shown to cause problems if not controlled, while their beneficial effects on the cooling water side of condensers are described. (auth)

  17. Swamp Rice Production in Ogun Waterside Local Government Area ...

    African Journals Online (AJOL)

    This study examined the economics of swamp rice production among peasant farmers in the Waterside Local Government Area of Ogun State for 2001 cropping year. A total of 50 swamp rice farmers were randomly selected from 5 villages using multistage sampling technique. The data collected, with the aid of ...

  18. 草坪汀步石间距初探%On exploration for waterside stone distance of lawns

    Institute of Scientific and Technical Information of China (English)

    夏卿; 周海萍

    2012-01-01

    From the distance and pace distance of the common waterside stone of lawns,the paper explores the way of adopting the proper modified measures for the waterside stone distance of lawns by investigation and feedback,so as to improve the application of the waterside stone in lawns and make it more comfortable and humanistic.%从常见的草坪汀步石的间距与步距关系着手,通过调查反馈,初步探究如何在汀步石间距方面采取适当的修改措施,以完善汀步在草坪中的使用,使其更加舒适和人性化。

  19. U.S. LMFBR steam generators materials considerations and waterside chemistry issues

    Energy Technology Data Exchange (ETDEWEB)

    Spalaris, C N

    1975-07-01

    This report describes the materials and waterside chemistry topics most relevant to the steam generator system for the Clinch River Breeder Reactor Plant. Development programs necessary to support or confirm design and plant operating conditions are summarized, together with selected test results obtained to date. (author)

  20. U.S. LMFBR steam generators materials considerations and waterside chemistry issues

    International Nuclear Information System (INIS)

    Spalaris, C.N.

    1975-01-01

    This report describes the materials and waterside chemistry topics most relevant to the steam generator system for the Clinch River Breeder Reactor Plant. Development programs necessary to support or confirm design and plant operating conditions are summarized, together with selected test results obtained to date. (author)

  1. Zircaloy sheathed thermocouples for PWR fuel rod temperature measurements

    International Nuclear Information System (INIS)

    Anderson, J.V.; Wesley, R.D.; Wilkins, S.C.

    1979-01-01

    Small diameter zircaloy sheathed thermocouples have been developed by EG and G Idaho, Inc., at the Idaho National Engineering Laboratory. Surface mounted thermocouples were developed to measure the temperature of zircaloy clad fuel rods used in the Thermal Fuels Behavior Program (TFBP), and embedded thermocouples were developed for use by the Loss-of-Fluid Test (LOFT) Program for support tests using zircaloy clad electrically heated nuclear fuel rod simulators. The first objective of this developmental effort was to produce zircaloy sheathed thermocouples to replace titanium sheathed thermocouples and thereby eliminate the long-term corrosion of the titanium-to-zircaloy attachment weld. The second objective was to reduce the sheath diameter to obtain faster thermal response and minimize cladding temperature disturbance due to thermocouple attachment

  2. Aluminum Corrosion and Turbidity

    International Nuclear Information System (INIS)

    Longtin, F.B.

    2003-01-01

    Aluminum corrosion and turbidity formation in reactors correlate with fuel sheath temperature. To further substantiate this correlation, discharged fuel elements from R-3, P-2 and K-2 cycles were examined for extent of corrosion and evidence of breaking off of the oxide film. This report discusses this study

  3. Effect of reactor chemistry and operating variables on fuel cladding corrosion in PWRs

    International Nuclear Information System (INIS)

    Park, Moon Ghu; Lee, Sang Hee

    1997-01-01

    As the nuclear industry extends the fuel cycle length, waterside corrosion of zircaloy cladding has become a limiting factor in PWR fuel design. Many plant chemistry factors such as, higher lithium/boron concentration in the primary coolant can influence the corrosion behavior of zircaloy cladding. The chemistry effect can be amplified in higher duty fuel, particularlywhen surface boiling occurs. Local boiling can result in increased crud deposition on fuel cladding which may induce axial power offset anomalies (AOA), recently reported in several PWR units. In this study, the effect of reactor chemistry and operating variables on Zircaloy cladding corrosion is investigated and simulation studies are performed to evaluate the optimal primary chemistry condition for extended cycle operation. (author). 8 refs., 3 tabs., 16 figs

  4. ELESTRES: performance of nuclear fuel, circumferential ridging, and multiaxial elastic-plastic stresses in sheaths

    International Nuclear Information System (INIS)

    Tayal, M.

    1986-10-01

    The finite element code ELESTRES models the two-dimensional axisymmetric behaviour of a CANDU fuel element during normal operation. The main focus of the code is to estimate temperatures, fission gas release, and axial variations of deformation/stresses in the pellet and in the sheath. Thus the code is able to predict details like stresses/strains at circumferential ridges. This paper describes the current version of ELESTRES. The emphasis is on a recent addition: multiaxial stresses in the sheath near circumferential ridges. For accuracy in the critical region, a fine mesh is used near the ridge. To keep computing costs low, a coarse mesh is used near the midplane of the pellet. Predictions of ELESTRES show good agreement with abouth 80 measurements of fission-gas-release. In this paper, we also present ELESTRES predictions of hoop strains in sheaths, for two irradiations: element ABS and bundle GB. For both irradiations, predictions, compare favourably with measurements. An illustrative example shows that near circumferential ridges, bending contributes to multiaxial stresses in the sheath. This can have a significant effect on sheath integrity, such as during stress-corrosion-cracking due to power-increases, or during corrosion-assisted-fatigue due to power cycling

  5. Effect of elevated lithium on the waterside corrosion of zircaloy-4: Experimental and predictive studies

    International Nuclear Information System (INIS)

    Pecheur, D.; Giordano, A.; Picard, E.; Billot, P.; Thomazet, J.

    1997-01-01

    Lithium and boron content in the coolant are known to influence the oxidation behaviour of the fuel cladding. Since new PWR operating conditions could consist in an increase of the lithium and the boron concentration in the coolant early in the cycle, a specific study has been conducted to analyze and to predict the effect of such new water chemistry conditions on the oxidation kinetics of the Zircaloy-4 material. Experimental studies have been performed in out-of-pile loop tests, under one and two phase flow heat transfer in various water chemistry conditions (0≤Li≤350 ppm, 0≤B≤1000 ppm, 0≤K≤56 ppm). A simulation of the effect of elevated lithium on the corrosion has been made using the semi-empirical COCHISE corrosion code. Under one phase flow heat transfer conditions, the addition of lithium hydroxide in the coolant increases the oxidation rate, essentially in the post-transition regime for low lithium levels (≤ 75 ppm) and immediately in the pre-transition phase for very high lithium level (350 ppm). Under two phase flow heat transfer, an enhancement of the corrosion is observed in the area of the rod submitted to boiling. Based on the out-of-pile loop test performed in presence of KOH instead of LiOH, such an enhancement of the corrosion appears to be due to a lithium enrichment in the oxide layer induced by boiling and not to a pH effect. The simulation of the increase of lithium content in the coolant from 2.2 to 3.5 ppm leads to an enhancement in corrosion rates which becomes only significant at high burn up. This predictive result of elevated lithium effect on corrosion is then compared with oxidation data derived from reactors operating under an elevated lithium regime. (author). 14 refs, 9 figs, 3 tabs

  6. Effect of elevated lithium on the waterside corrosion of zircaloy-4: Experimental and predictive studies

    Energy Technology Data Exchange (ETDEWEB)

    Pecheur, D; Giordano, A; Picard, E; Billot, P [CEA Centre d` Etudes de Cadarache, 13 - Saint-Paul-lez-Durance (France); Thomazet, J [FRAMATOME, Nuclear Fuel Div., Lyon (France)

    1997-02-01

    Lithium and boron content in the coolant are known to influence the oxidation behaviour of the fuel cladding. Since new PWR operating conditions could consist in an increase of the lithium and the boron concentration in the coolant early in the cycle, a specific study has been conducted to analyze and to predict the effect of such new water chemistry conditions on the oxidation kinetics of the Zircaloy-4 material. Experimental studies have been performed in out-of-pile loop tests, under one and two phase flow heat transfer in various water chemistry conditions (0{<=}Li{<=}350 ppm, 0{<=}B{<=}1000 ppm, 0{<=}K{<=}56 ppm). A simulation of the effect of elevated lithium on the corrosion has been made using the semi-empirical COCHISE corrosion code. Under one phase flow heat transfer conditions, the addition of lithium hydroxide in the coolant increases the oxidation rate, essentially in the post-transition regime for low lithium levels ({<=} 75 ppm) and immediately in the pre-transition phase for very high lithium level (350 ppm). Under two phase flow heat transfer, an enhancement of the corrosion is observed in the area of the rod submitted to boiling. Based on the out-of-pile loop test performed in presence of KOH instead of LiOH, such an enhancement of the corrosion appears to be due to a lithium enrichment in the oxide layer induced by boiling and not to a pH effect. The simulation of the increase of lithium content in the coolant from 2.2 to 3.5 ppm leads to an enhancement in corrosion rates which becomes only significant at high burn up. This predictive result of elevated lithium effect on corrosion is then compared with oxidation data derived from reactors operating under an elevated lithium regime. (author). 14 refs, 9 figs, 3 tabs.

  7. Atomistic studies of cation transport in tetragonal ZrO2 during zirconium corrosion

    International Nuclear Information System (INIS)

    Bai, Xian-Ming; Zhang, Yongfeng; Tonks, Michael R.

    2015-01-01

    Zirconium alloys are the major fuel cladding materials in current reactors. The water-side corrosion is a significant degradation mechanism of these alloys. During corrosion, the transport of oxidizing species in zirconium dioxide (ZrO 2 ) determines the corrosion kinetics. Previously, it has been argued that the outward diffusion of cations is important for forming protective oxides. In this work, the migration of Zr defects in tetragonal ZrO 2 is studied with temperature accelerated dynamics and molecular dynamics simulations. The results show that Zr interstitials have anisotropic diffusion and migrate preferentially along the [001] or c direction in tetragonal ZrO 2 . The compressive stresses can increase the Zr interstitial migration barrier significantly. The migration of Zr interstitials at a grain boundary is much slower than in a bulk oxide. The implications of these atomistic simulation results in the Zr corrosion are discussed. (authors)

  8. Deposition of corrosion products in-core

    International Nuclear Information System (INIS)

    Burrill, K.A.

    1994-11-01

    Data on corrosion product deposits on fuel sheaths are presented for a variety of operating conditions and water chemistries: boiling and non-boiling water; surface heat flux; pH, dissolved hydrogen concentration. Corrosion product behaviour in-core may be interpreted in terms of the solubility of magnetite and how it changes with water chemistry and temperature. A hypothesis of the deposition and release mechanisms was proposed in the 1970s in which particles deposited onto the sheath and subsequently dissolved in the heated water while being irradiated. Some of the deposition data may be interpreted using a model of these mechanisms. (author). 5 refs., 6 tabs., 8 figs

  9. Evaluation of materials' corrosion and chemistry issues for advanced gas cooled reactor steam generators using full scale plant simulations

    International Nuclear Information System (INIS)

    Woolsey, I.S.; Rudge, A.J.; Vincent, D.J.

    1998-01-01

    Advanced Gas Cooled Reactors (AGRS) employ once-through steam Generators of unique design to provide steam at approximately 530 degrees C and 155 bar to steam turbines of similar design to those of fossil plants. The steam generators are highly compact, and have either a serpentine or helical tube geometry. The tubes are heated on the outside by hot C0 2 gas, and steam is generated on the inside of the tubes. Each individual steam generator tube consists of a carbon steel feed and primary economiser section, a 9%Cr steel secondary economiser, evaporator and primary superheater, and a Type 316L austenitic stainless steel secondary superheater, all within a single tube pass. The multi-material nature of the individual tube passes, the need to maintain specific thermohydraulic conditions within the different material sections, and the difficulties of steam generator inspection and repair, have required extensive corrosion-chemistry test programmes to ensure waterside corrosion does not present a challenge to their integrity. A major part of these programmes has been the use of a full scale steam generator test facility capable of simulating all aspects of the waterside conditions which exist in the plant. This facility has been used to address a wide variety of possible plant drainage/degradation processes. These include; single- and two-phase flow accelerated corrosion of carbon steel, superheat margins requirements and the stress-corrosion behaviour of the austenitic superheaters, on-load corrosion of the evaporator materials, and iron transport and oxide deposition behaviour. The paper outlines a number of these, and indicates how they have been of value in helping to maintain reliable operation of the plant. (author)

  10. Stress-Assisted Corrosion in Boiler Tubes

    Energy Technology Data Exchange (ETDEWEB)

    Preet M Singh; Steven J Pawel

    2006-05-27

    A number of industrial boilers, including in the pulp and paper industry, needed to replace their lower furnace tubes or decommission many recovery boilers due to stress-assisted corrosion (SAC) on the waterside of boiler tubes. More than half of the power and recovery boilers that have been inspected reveal SAC damage, which portends significant energy and economic impacts. The goal of this project was to clarify the mechanism of stress-assisted corrosion (SAC) of boiler tubes for the purpose of determining key parameters in its mitigation and control. To accomplish this in-situ strain measurements on boiler tubes were made. Boiler water environment was simulated in the laboratory and effects of water chemistry on SAC initiation and growth were evaluated in terms of industrial operations. Results from this project have shown that the dissolved oxygen is single most important factor in SAC initiation on carbon steel samples. Control of dissolved oxygen can be used to mitigate SAC in industrial boilers. Results have also shown that sharp corrosion fatigue and bulbous SAC cracks have similar mechanism but the morphology is different due to availability of oxygen during boiler shutdown conditions. Results are described in the final technical report.

  11. Coating of Zircaloy sheaths with silica glass using the Sol-Gel technique for protection against oxidation

    International Nuclear Information System (INIS)

    De Sanctis, O.; Pellegri, N.; Gomez, L.

    1990-01-01

    With the aim of improving corrosion resistance of Zircaloy, a few Zircaloy sheaths were covered with vitreous silica. Deposition was made by dip coating in tetraetilortosilicate (TEOS) solutions and later densification treatment at 500 degrees C. Oxidation tests were performed and compared with sheaths not covered with silica. As a result, an effective increase in the resistance to dry oxidation was found in sheaths which had been protected. The coating-Zircaloy interface was studied using XPS (scanner). (Author). 6 refs., 3 figs

  12. Unirradiated UO2 in irradiated zirconium alloy sheathing

    International Nuclear Information System (INIS)

    MacDonald, R.D.; Hardy, D.G.; Hunt, C.E.L.; Scoberg, J.A.

    1979-07-01

    Zircaloy-clad UO 2 fuel elements have defected in power reactors when element power outputs were raised significantly after a long irradiation at low power. We have irradiated fuel elements fabricated from fresh UO 2 pellets and zirconium alloy sheaths previously irradiated without fuel. This gave a fuel element with radiation-damaged low-ductility sheathing but with no fission products in the fuel. The elements were power boosted in-reactor to linear power outputs up to 84 kW/m for two five-day periods. No elements defected despite sheath strains of 0.82 percent at circumferential ridge postions. Half of these elements were subsequently soaked at low power to build up the fission product inventory in the fuel and then power boosted to 63 kW/m for a third time. Two elements defected on this final boost. We conclude that these defects were caused by fission product induced stress-corrosion cracking and that this mechanism plays an importent role in power reactor fuel defects. (auth)

  13. Corrosion testing of uranium silicide fuel specimens

    International Nuclear Information System (INIS)

    Bourns, W.T.

    1968-09-01

    U 3 Si is the most promising high density natural uranium fuel for water-cooled power reactors. Power reactors fuelled with this material are expected to produce cheaper electricity than those fuelled with uranium dioxide. Corrosion tests in 300 o C water preceded extensive in-reactor performance tests of fuel elements and bundles. Proper heat-treatment of U-3.9 wt% Si gives a U 3 5i specimen which corrodes at less than 2 mg/cm 2 h in 300 o C water. This is an order of magnitude lower than the maximum corrosion rate tolerable in a water-cooled reactor. U 3 Si in a defected unbonded Zircaloy-2 sheath showed only a slow uniform sheath expansion in 300 o C water. All tests were done under isothermal conditions in an out-reactor loop. (author)

  14. Corrosion testing of uranium silicide fuel specimens

    Energy Technology Data Exchange (ETDEWEB)

    Bourns, W T

    1968-09-15

    U{sub 3}Si is the most promising high density natural uranium fuel for water-cooled power reactors. Power reactors fuelled with this material are expected to produce cheaper electricity than those fuelled with uranium dioxide. Corrosion tests in 300{sup o}C water preceded extensive in-reactor performance tests of fuel elements and bundles. Proper heat-treatment of U-3.9 wt% Si gives a U{sub 3}5i specimen which corrodes at less than 2 mg/cm{sup 2} h in 300{sup o}C water. This is an order of magnitude lower than the maximum corrosion rate tolerable in a water-cooled reactor. U{sub 3}Si in a defected unbonded Zircaloy-2 sheath showed only a slow uniform sheath expansion in 300{sup o}C water. All tests were done under isothermal conditions in an out-reactor loop. (author)

  15. Detrimental role of hydrogen on the corrosion rate of zirconium alloys

    International Nuclear Information System (INIS)

    Blat, M.; Noel, D.

    1996-01-01

    Recent studies have suggested that hydride precipitation at the metal/oxide interface could play a detrimental role on the waterside corrosion rate. Nevertheless, the mechanism of that detrimental role is not completely understood, and two hypotheses were investigated to understand the mechanism that controls the role of the hydrides. The first hypothesis is based on a mechanical effect: the hydrides precipitate at the metal/oxide interface and destroy the physical integrity of the barrier oxide layer. The second hypothesis is a modification of the transport properties of the oxide grown on the hydrided metal. The detrimental role of hydrides on the corrosion rate was studied by charging unirradiated Zircaloy-4 cladding material with hydrogen to a level higher than the limit of solubility at 400 C. Both gaseous and cathodic charging techniques were used. Static corrosion tests were carried out in autoclave with steam at 400 C on an as-received and hydrided sample. The detrimental role of hydrides is confirmed from the post-transition corrosion rate, and that effect is more significant for high cathodic charging. The results of the metallurgical examinations are discussed to provide an understanding of the mechanism. No relationship between hydrides, physical defects in the oxide, and local corrosion rate enhancement was found. Therefore, the results do not support the hypothesis of a mechanical effect at the scale of the performed examinations, but more detailed work is required to confirm this

  16. CANDU fuel sheath integrity and oxide layer thickness determination by Eddy current technique

    International Nuclear Information System (INIS)

    Gheorghe, Gabriela; Man, Ion; Parvan, Marcel; Valeca, Serban

    2010-01-01

    This paper presents results concerning the integrity assessment of the fuel elements cladding and measurements of the oxide layer on sheaths, using the eddy current technique. Flaw detection using eddy current provides information about the integrity of fuel element sheath or presence of defects in the sheath produced by irradiation. The control equipment consists of a flaw detector with eddy currents, operable in the frequency range 10 Hz to 10 MHz, and a differential probe. The calibration of the flaw detector is done using artificial defects (longitudinal, transversal, external and internal notches, bored and unbored holes) obtained on Zircaloy-4 tubes identical to those out of which the sheath of the CANDU fuel element is manufactured (having a diameter of 13.08 mm and a wall thickness of 0.4 mm). When analyzing the behavior of the fuel elements' cladding facing the corrosion is important to know the thickness of the zirconium oxide layer. The calibration of the device measuring the thickness of the oxide layer is done using a Zircaloy-4 tube identical to that which the cladding of the CANDU fuel element is manufactured of, and calibration foils, as well. (authors)

  17. Contribution to the physical study of sheath failure detections

    International Nuclear Information System (INIS)

    Mangin, Jean-Paul

    1968-11-01

    As the study of an installation aimed at the detection of sheath failure requires the knowledge of a great number of data related to all the fields of nuclear technology (fission mechanisms, sheath failure mechanisms, recoil of fission products, distribution of the heat transfer fluid in the reactor, techniques of measurement of beta and gamma neutrons, nuclear safety, and so on), this report aims at highlighting some specific issues, more particularly those related to sensors based on delayed neutrons. After having recalled the principles of sheath failure detection, the author presents the various aspects of the study of the formation of fission products and of their passage into the heat transfer fluid: detection by using delayed neutrons, detection by electrostatic collection, passage of fuel fission products into the coolant (recoil, corrosion, gaseous diffusion in the fuel), formation of fission products in the fuel (fission product efficiency). He reports the study of the transport of fission products by the coolant from their place of birth to the place of measurement. He presents the system of measurement by detection of delayed neutrons and by electrostatic collection, reports a sensitivity calculation, a background noise assessment, the determination of detection threshold, and the application of sensitivity and detection thresholds calculations [fr

  18. Factors affecting stress assisted corrosion cracking of carbon steel under industrial boiler conditions

    Science.gov (United States)

    Yang, Dong

    Failure of carbon steel boiler tubes from waterside has been reported in the utility boilers and industrial boilers for a long time. In industrial boilers, most waterside tube cracks are found near heavy attachment welds on the outer surface and are typically blunt, with multiple bulbous features indicating a discontinuous growth. These types of tube failures are typically referred to as stress assisted corrosion (SAC). For recovery boilers in the pulp and paper industry, these failures are particularly important as any water leak inside the furnace can potentially lead to smelt-water explosion. Metal properties, environmental variables, and stress conditions are the major factors influencing SAC crack initation and propagation in carbon steel boiler tubes. Slow strain rate tests (SSRT) were conducted under boiler water conditions to study the effect of temperature, oxygen level, and stress conditions on crack initation and propagation on SA-210 carbon steel samples machined out of boiler tubes. Heat treatments were also performed to develop various grain size and carbon content on carbon steel samples, and SSRTs were conducted on these samples to examine the effect of microstructure features on SAC cracking. Mechanisms of SAC crack initation and propagation were proposed and validated based on interrupted slow strain tests (ISSRT). Water chemistry guidelines are provided to prevent SAC and fracture mechanics model is developed to predict SAC failure on industrial boiler tubes.

  19. A technique for measuring hydrogen and water in inert gases and the hydrogen concentration in liquid sodium

    International Nuclear Information System (INIS)

    Smith, C.A.

    1978-04-01

    A method is described of measuring the hydrogen and water content of an inert gas. It is based upon the use of an electrochemical oxygen cell and has a high sensitivity at low hydrogen and water levels. The following possible applications of the method are described together with supporting experimental measurements: improving the sensitivity and range of the present PFR secondary circuit hydrogen detection instruments; the measurement of hydrogen diffusion coefficients in steels; the measurement of waterside corrosion rates of boiler steels; on-line monitoring of waterside boiler corrosion. Attention is given to the characteristics of diffusion barriers in relation to the first and last of these. (author)

  20. Modelling of iodine-induced stress corrosion cracking in CANDU fuel

    International Nuclear Information System (INIS)

    Lewis, B.J.; Thompson, W.T.; Kleczek, M.R.; Shaheen, K.; Juhas, M.; Iglesias, F.C.

    2011-01-01

    Iodine-induced stress corrosion cracking (I-SCC) is a recognized factor for fuel-element failure in the operation of nuclear reactors requiring the implementation of mitigation measures. I-SCC is believed to depend on certain factors such as iodine concentration, oxide layer type and thickness on the fuel sheath, irradiation history, metallurgical parameters related to sheath like texture and microstructure, and the mechanical properties of zirconium alloys. This work details the development of a thermodynamics and mechanistic treatment accounting for the iodine chemistry and kinetics in the fuel-to-sheath gap and its influence on I-SCC phenomena. The governing transport equations for the model are solved with a finite-element technique using the COMSOL Multiphysics (registered) commercial software platform. Based on this analysis, this study also proposes potential remedies for I-SCC.

  1. Communication through plasma sheaths

    International Nuclear Information System (INIS)

    Korotkevich, A. O.; Newell, A. C.; Zakharov, V. E.

    2007-01-01

    We wish to transmit messages to and from a hypersonic vehicle around which a plasma sheath has formed. For long distance transmission, the signal carrying these messages must be necessarily low frequency, typically 2 GHz, to which the plasma sheath is opaque. The idea is to use the plasma properties to make the plasma sheath appear transparent

  2. The electrostatic cylindrical sheath in a plasma

    International Nuclear Information System (INIS)

    Wang Chunhua; Sun Xiaoxia; Bai Dongxue

    2004-01-01

    The electrostatic sheath with a cylindrical geometry in an ion-electron plasma is investigated. Assuming a Boltzmann response to electrons and cold ions with bulk flow, it is shown that the radius of the cylindrical geometry do not affect the sheath potential significantly. The authors also found that the sheath potential profile is steeper in the cylindrical sheath compared to the slab sheath. The distinct feature of the cylindrical sheath is that the ion density distribution is not monotonous. The sheath region can be divided into three regions, two ascendant regions and one descendant region. (author)

  3. RF sheaths for arbitrary B field angles

    Science.gov (United States)

    D'Ippolito, Daniel; Myra, James

    2014-10-01

    RF sheaths occur in tokamaks when ICRF waves encounter conducting boundaries and accelerate electrons out of the plasma. Sheath effects reduce the efficiency of ICRF heating, cause RF-specific impurity influxes from the edge plasma, and increase the plasma-facing component damage. The rf sheath potential is sensitive to the angle between the B field and the wall, the ion mobility and the ion magnetization. Here, we obtain a numerical solution of the non-neutral rf sheath and magnetic pre-sheath equations (for arbitrary values of these parameters) and attempt to infer the parametric dependences of the Child-Langmuir law. This extends previous work on the magnetized, immobile ion regime. An important question is how the rf sheath voltage distributes itself between sheath and pre-sheath for various B field angles. This will show how generally previous estimates of the rf sheath voltage and capacitance were reasonable, and to improve the RF sheath BC. Work supported by US DOE grants DE-FC02-05ER54823 and DE-FG02-97ER54392.

  4. Tendon sheath fibroma in the thigh.

    Science.gov (United States)

    Moretti, Vincent M; Ashana, Adedayo O; de la Cruz, Michael; Lackman, Richard D

    2012-04-01

    Tendon sheath fibromas are rare, benign soft tissue tumors that are predominantly found in the fingers, hands, and wrists of young adult men. This article describes a tendon sheath fibroma that developed in the thigh of a 70-year-old man, the only known tendon sheath fibroma to form in this location. Similar to tendon sheath fibromas that develop elsewhere, our patient's lesion presented as a painless, slow-growing soft tissue nodule. Physical examination revealed a firm, nontender mass with no other associated signs or symptoms. Although the imaging appearance of tendon sheath fibromas varies, our patient's lesion appeared dark on T1- and bright on T2-weighted magnetic resonance imaging. It was well marginated and enhanced with contrast.Histologically, tendon sheath fibromas are composed of dense fibrocollagenous stromas with scattered spindle-shaped fibroblasts and narrow slit-like vascular spaces. Most tendon sheath fibromas can be successfully removed by marginal excision, although 24% of lesions recur. No lesions have metastasized. Our patient's tendon sheath fibroma was removed by marginal excision, and the patient remained disease free 35 months postoperatively. Despite its rarity, tendon sheath fibroma should be included in the differential diagnosis of a thigh mass on physical examination or imaging, especially if it is painless, nontender, benign appearing, and present in men. Copyright 2012, SLACK Incorporated.

  5. An analysis of static loading results on slotted ring samples to allow for further investigation of stress corrosion cracking

    Energy Technology Data Exchange (ETDEWEB)

    Metzler, J.; Ferrier, G.A.; Farahani, M.; Chan, P.K.; Corcoran, E.C., E-mail: Joseph.Metzler@rmc.ca [Royal Military College of Canada, Kingston, ON (Canada)

    2014-07-01

    Stress corrosion cracking can cause failures of CANDU Zircaloy-4 fuel sheathing. A series of static loading tests were performed on slotted ring samples in support of ongoing efforts to analyze the effects of iodine concentration, temperature, and stress levels on the corrosion of Zircaloy-4. The corrosive degradation of Zircaloy-4 was evaluated using deflection measurements. A regression analysis determined that iodine concentration and temperature have had a linear effect on deflection results thus far, while the stress level has not. (author)

  6. A Study on Afforestation on the Waterside and Its Management

    Energy Technology Data Exchange (ETDEWEB)

    Choi, J.Y.; Lee, J.H. [Korea Environment Institute, Seoul (Korea)

    2001-12-01

    The important task of preserving and protecting water quality in water supply areas is best facilitated through environmental-friendly management. systems in adjacent waterzones, particularly through the formation of riparian buffers. Urban areas are of particular interest because their high contributions of pollution loading conflict with their low covering percentage in the watershed. This feature of the urban landscape requires that certain areas to be converted into riparian buffers in order to restrict pollution sources and purify non-point sources. The various functions of the riparian buffer in water supply areas include reducing non-point sources, assuaging the public's peace of mind, and improving the environment's esthetics. To be effective, any damaged riparian buffers in urban areas should be recovered and the existing ones maintained. The following policies are recommended in order to achieve such ends: l. To form operative riparian buffers, designated areas in fixed distances from bodies of water or areas that affect water quality, or absolute protection zones, need to be established. The absolute protecting zone is to be determined by factors of slope, soil, vegetation, pollutant source, and proximity. However, if taking account of flood water levels, surrounding areas within 30m of important water supply areas and urban areas, which are exclusive riparian buffer areas, should also be included. 2. Priority in terms of water quality should be established for each land segment in order to promote efficient land acquisition within the riparian buffer and for nation of vegetation. High priority areas should be dealt with preferentially and environment-friendly land management should be considered. 3. To establish legal bases for waterside zone management, independent laws and amendments to existing laws, such as 'Urban Planning Act' or 'River Act', that are related to the formation of riparian buffers should be introduced

  7. Chemical cleaning's role in tube failure prevention and correction

    International Nuclear Information System (INIS)

    Shields, K.J.; Dooley, R.B.

    2002-01-01

    Properly applied, chemical cleaning is a valuable tool used to prevent tube failures involving overheating and corrosion due to waterside deposits. In many cases, however, cleaning becomes yet an additional cost associated with correction of tube failure incidents. Discussion is focused on approaches taken to appraise tube waterside cleanliness and determine the need to clean, as typically practiced in conventional fossil plants. Also presented is an assessment of the suitability and limitations of these approaches to plants with heat recovery steam generator (HRSG) units. (orig.)

  8. Corrosion control in CANDU nuclear power reactors

    International Nuclear Information System (INIS)

    Lesurf, J.E.

    1974-01-01

    Corrosion control in CANDU reactors which use pressurized heavy water (PHW) and boiling light water (BLW) coolants is discussed. Discussions are included on pressure tubes, primary water chemistry, fuel sheath oxidation and hydriding, and crud transport. It is noted that corrosion has not been a significant problem in CANDU nuclear power reactors which is a tribute to design, material selection, and chemistry control. This is particularly notable at the Pickering Nuclear Generating Station which will have four CANDU-PHW reactors of 540 MWe each. The net capacity factor for Pickering-I from first full power (May 1971) to March 1972 was 79.5 percent, and for Pickering II (first full power November 1971) to March 1972 was 83.5 percent. Pickering III has just reached full power operation (May 1972) and Pickering IV is still under construction. Gentilly CANDU-BLW reached full power operation in May 1972 after extensive commissioning tests at lower power levels with no major corrosion or chemistry problems appearing. Experience and operating data confirm that the value of careful attention to all aspects of corrosion control and augur well for future CANDU reactors. (U.S.)

  9. Three-dimensional analysis of antenna sheaths

    International Nuclear Information System (INIS)

    Myra, J.R.; D'Ippolito, D.A.; Ho, Y.L.

    1996-01-01

    The present work is motivated by the importance of r.f. sheaths in determining the antenna-plasma interaction and the sensitivity of the sheaths to the complicated three-dimensional structure of modern ion cyclotron range of frequency (ICRF) antennas. To analyze r.f. sheaths on the plasma facing regions of the launcher, we first calculate the contact points of the tokamak magnetic field lines on the surface of the antenna Faraday screen and nearby limiters for realistic three-dimensional magnetic flux surface and antenna geometries. Next, the r.f. voltage that can drive sheaths at the contact points is determined and used to assess the resulting sheath power dissipation, r.f.-driven sputtering, and r.f.-induced convective cells (which produce edge profile modification). The calculations are embodied in a computer code, ANSAT (antenna sheath analysis tool), and sample ANSAT runs are shown to highlight the physics- and geometry-dependent characteristics of the r.f. sheaths and their relationship to the antenna design. One use of ANSAT is therefore as a design tool, to assess the strengths and weaknesses of a given design with respect to critical voltage handling and edge plasma interaction issues. Additionally, examples are presented where ANSAT has been useful in the analysis and interpretation of ICRF experiments (orig.)

  10. Barrier cell sheath formation

    International Nuclear Information System (INIS)

    Kesner, J.

    1980-04-01

    The solution for electrostatic potential within a simply modeled tandem mirror thermal barrier is seen to exhibit a sheath at each edge of the cell. The formation of the sheath requires ion collisionality and the analysis assmes that the collisional trapping rate into the barrier is considerably slower than the barrier pump rate

  11. Co-electrospinning fabrication and photocatalytic performance of TiO2/SiO2 core/sheath nanofibers with tunable sheath thickness

    International Nuclear Information System (INIS)

    Cao, Houbao; Du, Pingfan; Song, Lixin; Xiong, Jie; Yang, Junjie; Xing, Tonghai; Liu, Xin; Wu, Rongrong; Wang, Minchao; Shao, Xiaoli

    2013-01-01

    Graphical abstract: - Highlights: • The core–sheath TiO 2 /SiO 2 nanofibers were fabricated by co-electrospinning technique. • The catalytic property of nanofibers with different sheath thickness was studied. • The potential methods of improving catalytic efficiency are suggested. - Abstract: In this paper, core/sheath TiO 2 /SiO 2 nanofibers with tunable sheath thickness were directly fabricated via a facile co-electrospinning technique with subsequent calcination at 500 °C. The morphologies and structures of core/sheath TiO 2 /SiO 2 nanofibers were characterized by TGA, FESEM, TEM, FTIR, XPS and BET. It was found that the 1D core/sheath nanofibers are made up of anatase–rutile TiO 2 core and amorphous SiO 2 sheath. The influences of SiO 2 sheath and its thickness on the photoreactivity were evaluated by observing photo-degradation of methylene blue aqueous solution under the irradiation of UV light. Compared with pure TiO 2 nanofibers, the core/sheath TiO 2 /SiO 2 nanofibers performed a better catalytic performance. That was attributed to not only efficient separation of hole–electron pairs resulting from the formation of heterojunction but also larger surface area and surface silanol group which will be useful to provide higher capacity for oxygen adsorption to generate more hydroxyl radicals. And the optimized core/sheath TiO 2 /SiO 2 nanofibers with a sheath thickness of 37 nm exhibited the best photocatalytic performance

  12. Radio frequency sheaths in an oblique magnetic field

    International Nuclear Information System (INIS)

    Myra, J. R.; D'Ippolito, D. A.

    2015-01-01

    The physics of radio-frequency (rf) sheaths near a conducting surface is studied for plasmas immersed in a magnetic field that makes an oblique angle θ with the surface. A set of one-dimensional equations is developed that describes the dynamics of the time-dependent magnetic presheath and non-neutral Debye sheath. The model employs Maxwell-Boltzmann electrons, and the magnetization and mobility of the ions is determined by the magnetic field strength, and wave frequency, respectively. The angle θ, assumed to be large enough to insure an electron-poor sheath, is otherwise arbitrary. Concentrating on the ion-cyclotron range of frequencies, the equations are solved numerically to obtain the rectified (dc) voltage, the rf voltage across the sheath, and the rf current flowing through the sheath. As an application of this model, the sheath voltage-current relation is used to obtain the rf sheath impedance, which in turn gives an rf sheath boundary condition for the electric field at the sheath-plasma interface that can be used in rf wave codes. In general, the impedance has both resistive and capacitive contributions, and generalizes previous sheath boundary condition models. The resistive part contributes to parasitic power dissipation at the wall

  13. Sheath waves, non collisional dampings

    International Nuclear Information System (INIS)

    Marec, Jean Lucien Ernest

    1974-01-01

    When a metallic conductor is inserted into an ionised gas, an area of electron depletion is formed between the conductor and the plasma: the ionic sheath. Moreover, if the conductor is excited by an electric field, this ionic sheath plays an important role with respect to microwave properties. In this research thesis, the author addresses the range of frequencies smaller than the plasma frequency, and reports the study of resonance phenomena. After a presentation of the problem through a bibliographical study, the author recalls general characteristics of sheath wave propagation and of sheath resonances, and discusses the validity of different hypotheses (for example and among others, electrostatic approximations, cold plasma). Then, the author more particularly addresses theoretical problems related to non collisional dampings: brief bibliographical study, detailed presentation and description of the theoretical model, damping calculation methods. The author then justifies the design and performance of an experiment, indicates measurement methods used to determine plasma characteristics as well as other magnitudes which allow the description of mechanisms of propagation and damping of sheath waves. Experimental results are finally presented with respect to various parameters. The author discusses to which extent the chosen theoretical model is satisfying [fr

  14. Ion acceleration in the plasma source sheath

    International Nuclear Information System (INIS)

    Birdsall, C.K.

    1986-01-01

    This note is a calculation of the potential drop for a planar plasma source, across the source sheath, into a uniform plasma region defined by vector E = 0 and/or perhaps ∂ 2 PHI/∂ x 2 = 0. The calculation complements that of Bohm who obtained the potential drop at the other end of a plasma, at a planar collector sheath. The result is a relation between the source ion flux and the source sheath potential drop and the accompanying ion acceleration. This planar source sheath ion acceleration mechanism (or that from a distributed source) can provide the pre-collector-sheath ion acceleration as found necessary by Bohm. 3 refs

  15. Self-consistent radial sheath

    International Nuclear Information System (INIS)

    Hazeltine, R.D.

    1988-12-01

    The boundary layer arising in the radial vicinity of a tokamak limiter is examined, with special reference to the TEXT tokamak. It is shown that sheath structure depends upon the self-consistent effects of ion guiding-center orbit modification, as well as the radial variation of E /times/ B-induced toroidal rotation. Reasonable agreement with experiment is obtained from an idealized model which, however simplified, preserves such self-consistent effects. It is argued that the radial sheath, which occurs whenever confining magnetic field-lines lie in the plasma boundary surface, is an object of some intrinsic interest. It differs from the more familiar axial sheath because magnetized charges respond very differently to parallel and perpendicular electric fields. 11 refs., 1 fig

  16. Ultrasound diagnosis of rectus sheath hematoma

    International Nuclear Information System (INIS)

    Hwang, M. S.; Chang, J. C.; Rhee, C. B.

    1984-01-01

    6 cases of rectus sheath hematoma were correctly diagnosed by ultrasound. 2 cases had bilateral rectus sheath hematoma and 4 cases were unilateral. On ultrasound finding, relatively well defined oval or spindle like cystic mass situated in the area of rectus muscle on all cases. Ultrasound examination may give more definite diagnosis and extension rectus sheath hematoma and also helpful to follow up study of hematoma

  17. Sheath insulator final test report, TFE Verification Program

    Energy Technology Data Exchange (ETDEWEB)

    1994-07-01

    The sheath insulator in a thermionic cell has two functions. First, the sheath insulator must electrically isolate the collector form the outer containment sheath tube that is in contact with the reactor liquid metal coolant. Second, The sheath insulator must provide for high uniform thermal conductance between the collector and the reactor coolant to remove away waste heat. The goals of the sheath insulator test program were to demonstrate that suitable ceramic materials and fabrication processes were available, and to validate the performance of the sheath insulator for TFE-VP requirements. This report discusses the objectives of the test program, fabrication development, ex-reactor test program, in-reactor test program, and the insulator seal specifications.

  18. Sheath insulator final test report, TFE Verification Program

    International Nuclear Information System (INIS)

    1994-07-01

    The sheath insulator in a thermionic cell has two functions. First, the sheath insulator must electrically isolate the collector form the outer containment sheath tube that is in contact with the reactor liquid metal coolant. Second, The sheath insulator must provide for high uniform thermal conductance between the collector and the reactor coolant to remove away waste heat. The goals of the sheath insulator test program were to demonstrate that suitable ceramic materials and fabrication processes were available, and to validate the performance of the sheath insulator for TFE-VP requirements. This report discusses the objectives of the test program, fabrication development, ex-reactor test program, in-reactor test program, and the insulator seal specifications

  19. Plasma sheath criterion in thermal electronegative plasmas

    International Nuclear Information System (INIS)

    Ghomi, Hamid; Khoramabadi, Mansour; Ghorannevis, Mahmod; Shukla, Padma Kant

    2010-01-01

    The sheath formation criterion in electronegative plasma is examined. By using a multifluid model, it is shown that in a collisional sheath there will be upper as well as lower limits for the sheath velocity criterion. However, the parameters of the negative ions only affect the lower limit.

  20. Water chemistry and corrosion control of cladding and primary circuit components. Proceedings of a technical committee meeting

    International Nuclear Information System (INIS)

    1999-12-01

    Corrosion is the principal life limiting degradation mechanism in nuclear steam supply systems, especially taking into account the trends to increase fuel burnup, thermal rate and cycle length. Primary circuit components of water cooled power reactors have an impact on Zr-based alloys behaviour due to crud (primary circuit corrosion products) formation, transport and deposition on heat transfer surfaces. Crud deposits influence water chemistry, radiation and thermal hydraulic conditions near cladding surface, and by this way-Zr-based alloy corrosion. During the last decade, significant improvements were achieved in the reduction of the corrosion and dose rates by changing the cladding material for one more resistant to corrosion or by the improvement of water chemistry conditions. However, taking into account the above mentioned tendency for heavier fuel duties, corrosion and water chemistry, control will remain a serious task to work with for nuclear power plant operators and scientists, as well as development of generally accepted corrosion model of Zr-based alloys in a water environment in a new millennium. Upon the recommendation of the International Working Group on Water Reactor Fuel Performance and Technology, water chemistry and corrosion of cladding and primary circuit components are in the focus of the IAEA activities in the area of fuel technology and performance. At present the IAEA performs two co-ordinated research projects (CRPs): on On-line High Temperature Monitoring of Water Chemistry and Corrosion (WACOL) and on Activity Transport in Primary Circuits. Two CRPs deal with hydrogen and hydride degradation of the Zr-based alloys. A state-of-the-art review entitled: 'Waterside Corrosion of Zirconium Alloys in Nuclear Power Plants' was published in 1998. Technical Committee meetings on the subject were held in 1985 (Cadarache, France), 1989 (Portland, USA), 1993 (Rez, Czech Republic). During the last few years extensive exchange of experience in

  1. Stability of the plasma sheath

    International Nuclear Information System (INIS)

    Franklin, R.N.

    1979-12-01

    The stability of a collisionless sheath joined to a plasma in the presence of secondary emission of electrons from the sheath boundary is examined in the fluid approximation. Instability is unlikely to occur under floating conditions but if significant currents flow corresponding to increased wall-plasma potentials the system can go unstable. (author)

  2. Simulation study on insoluble granular corrosion products deposited in PWR core

    International Nuclear Information System (INIS)

    Yang Xu; Zhou Tao; Ru Xiaolong; Lin Daping; Fang Xiaolu

    2014-01-01

    In the operation of reactor, such as fuel rods, reactor vessel internals etc. will be affected by corrosion erosion of high pressure coolant. It will produce many insoluble corrosion products. The FLUENT software is adopted to simulate insoluble granular corrosion products deposit distribution in the reactor core. The fluid phase uses the standard model to predict the flow field in the channel and forecast turbulence variation in the near-wall region. The insoluble granular corrosion products use DPM (Discrete Phase Model) to track the trajectory of the particles. The discrete phase model in FLUENT follows the Euler-Lagrange approach. The fluid phase is treated as a continuum by solving the Navier-Stokes equations, while the dispersed phase is solved by tracking a large number of particles through the calculated flow field. Through the study found, Corrosion products particles form high concentration area near the symmetry, and the entrance section of the corrosion products particles concentration is higher than export section. Corrosion products particles deposition attached on large area for the entrance of the cladding, this will change the core neutron flux distribution and the thermal conductivity of cladding material, and cause core axial offset anomaly (AOA). Corrosion products particles dot deposit in the outlet of cladding, which can lead to pitting phenomenon in a sheath. Pitting area will cause deterioration of heat transfer, destroy the cladding integrity. In view of the law of corrosion products deposition and corrosion characteristics of components in the reactor core. this paper proposes regular targeted local cleanup and other mitigation measures. (authors)

  3. Rectus sheath abscess after laparoscopic appendicectomy

    Directory of Open Access Journals (Sweden)

    Golash Vishwanath

    2007-01-01

    Full Text Available Port site wound infection, abdominal wall hematoma and intraabdominal abscess formation has been reported after laparoscopic appendicectomy. We describe here a rectus sheath abscess which occurred three weeks after the laparoscopic appendicectomy. It was most likely the result of secondary infection of the rectus sheath hematoma due to bleeding into the rectus sheath from damage to the inferior epigastric arteries or a direct tear of the rectus muscle. As far as we are aware this complication has not been reported after laparoscopic appendicectomy.

  4. A sheath model for arbitrary radiofrequency waveforms

    Science.gov (United States)

    Turner, M. M.; Chabert, Pascal

    2012-10-01

    The sheath is often the most important region of a rf plasma, because discharge impedance, power absorption and ion acceleration are critically affected by the behaviour of the sheath. Consequently, models of the sheath are central to any understanding of the physics of rf plasmas. Lieberman has supplied an analytical model for a radio-frequency sheath driven by a single frequency, but in recent years interest has been increasing in radio-frequency discharges excited by increasingly complex wave forms. There has been limited success in generalizing the Lieberman model in this direction, because of mathematical complexities. So there is essentially no sheath model available to describe many modern experiments. In this paper we present a new analytical sheath model, based on a simpler mathematical framework than that of Lieberman. For the single frequency case, this model yields scaling laws that are identical in form to those of Lieberman, differing only by numerical coefficients close to one. However, the new model may be straightforwardly solved for arbitrary current waveforms, and may be used to derive scaling laws for such complex waveforms. In this paper, we will describe the model and present some illustrative examples.

  5. The characteristics of RF modulated plasma boundary sheaths: An analysis of the standard sheath model

    Science.gov (United States)

    Naggary, Schabnam; Brinkmann, Ralf Peter

    2015-09-01

    The characteristics of radio frequency (RF) modulated plasma boundary sheaths are studied on the basis of the so-called ``standard sheath model.'' This model assumes that the applied radio frequency ωRF is larger than the plasma frequency of the ions but smaller than that of the electrons. It comprises a phase-averaged ion model - consisting of an equation of continuity (with ionization neglected) and an equation of motion (with collisional ion-neutral interaction taken into account) - a phase-resolved electron model - consisting of an equation of continuity and the assumption of Boltzmann equilibrium -, and Poisson's equation for the electrical field. Previous investigations have studied the standard sheath model under additional approximations, most notably the assumption of a step-like electron front. This contribution presents an investigation and parameter study of the standard sheath model which avoids any further assumptions. The resulting density profiles and overall charge-voltage characteristics are compared with those of the step-model based theories. The authors gratefully acknowledge Efe Kemaneci for helpful comments and fruitful discussions.

  6. Sheath heating in low-pressure capacitive radio frequency discharges

    International Nuclear Information System (INIS)

    Wood, B.P.

    1991-01-01

    Capacitively coupled, parallel plate, r.f. discharges are commonly used for materials processing. The electrons in such a discharge gain and lose energy by reflection from the oscillating sheaths which form at the electrodes. Previous models of the electron heating by this mechanism have assumed that the sheath motion is slow compared to the electron thermal velocity, so that the electron energy change from each reflection is small. Here, the heating rate, density, and sheath width relations are derived analytically in the limit of very fast sheath motion. Numerical results are presented spanning the slow and fast limits. Results from particle-in-cell simulations show that in the large-energy-change regime, an electron beam is produced on each sheath expansion. At low pressure, this beam can traverse the plasma and interact with the sheath at the opposite electrode, producing a beam energy and density dependence on the length of the discharge. The beam produces a time and space varying warm tail on the electron energy distribution. Two revised heating models are derived, assuming power-law and two-temperature electron energy distributions, with temporal variation in electron temperature. These revised models yield new predictions for the variation of the power, density, and sheath thickness with applied r.f. voltage. These predictions are compared with simulation results and laboratory experiment. The electron sheath motion is investigated experimentally by observing the signal on a floating probe in the sheath region. This is compared to the signal product by a non-linear circuit model which accounts for the perturbation of the sheath potential by the probe and includes various forms of sheath motion. The experimental observations are consistent with the analytical predictions. Experimental observations of plasma-sheath resonance oscillations are presented which agree with analytical predictions

  7. Rectus sheath hematoma: three case reports

    Directory of Open Access Journals (Sweden)

    Kapan Selin

    2008-01-01

    Full Text Available Abstract Introduction Rectus sheath hematoma is an uncommon cause of acute abdominal pain. It is an accumulation of blood in the sheath of the rectus abdominis, secondary to rupture of an epigastric vessel or muscle tear. It could occur spontaneously or after trauma. They are usually located infraumblically and often misdiagnosed as acute abdomen, inflammatory diseases or tumours of the abdomen. Case presentation We reported three cases of rectus sheath hematoma presenting with a mass in the abdomen and diagnosed by computerized tomography. The patients recovered uneventfully after bed rest, intravenous fluid replacement, blood transfusion and analgesic treatment. Conclusion Rectus sheath hematoma is a rarely seen pathology often misdiagnosed as acute abdomen that may lead to unnecessary laparotomies. Computerized tomography must be chosen for definitive diagnosis since ultrasonography is subject to error due to misinterpretation of the images. Main therapy is conservative management.

  8. Corrosion and alteration of materials from the nuclear industry; La Corrosion et l'alteration des materiaux du nucleaire

    Energy Technology Data Exchange (ETDEWEB)

    Beauvy, M.; Berthoud, G.; Defranceschi, M.; Ducros, G.; Feron, D.; Guerin, Y.; Latge, C.; Limoge, Y.; Madic, C.; Santarini, G.; Seiler, J.M.; Vernaz, E.; Richet, C.

    2010-07-01

    , testing means, experimental techniques, internal corrosion of zircaloy sheath - the iodine effect, stress corrosion of nickel alloys - hydrogen influence, stress corrosion of stainless steels; C - wear corrosion: a coupled phenomenon, research in the framework of service life extension of the French electronuclear park; 3 - Corrosion in future reactors: A - corrosion in gas reactors: corrosion by helium impurities, oxidation resistance of silicon carbide, corrosion of graphite and carbon-carbon composites; B - corrosion in liquid metal reactors: sodium FBRs, lead and lead alloys reactors; C- corrosion in molten salt reactors: corrosion of Hastelloy N-type nickel alloys by molten fluorides, mass transfer in aniso-thermal fluoride systems, tellurium embrittlement, electrochemical study of pure metals corrosion in molten fluorides; 4 - Materials corrosion and alteration in the back-end of the fuel cycle: A - corrosion in concentrated nitric environment: materials behaviour, self-catalytic mechanism of nitric acid reduction; B - corrosion in unsaturated aqueous environment: metallic corrosion in unsaturated environment - application to the storage of waste containers, bitumens alteration, reinforced concrete behaviour and iron framework corrosion, concrete behaviour in severe thermal environment; C - Corrosion in saturated aqueous environment: metals corrosion in clayey environment, long-term behaviour of glasses, ceramics alteration, underwater concrete durability, clays transformation; D - materials biodegradation: microorganisms and nuclear wastes, biodegradation of bitumen, concretes and steels; 5 - Conclusion, glossary

  9. Sheath structure transition controlled by secondary electron emission

    Science.gov (United States)

    Schweigert, I. V.; Langendorf, S. J.; Walker, M. L. R.; Keidar, M.

    2015-04-01

    In particle-in-cell Monte Carlo collision (PIC MCC) simulations and in an experiment we study sheath formation over an emissive floating Al2O3 plate in a direct current discharge plasma at argon gas pressure 10-4 Torr. The discharge glow is maintained by the beam electrons emitted from a negatively biased hot cathode. We observe three types of sheaths near the floating emissive plate and the transition between them is driven by changing the negative bias. The Debye sheath appears at lower voltages, when secondary electron emission is negligible. With increasing applied voltage, secondary electron emission switches on and a first transition to a new sheath type, beam electron emission (BEE), takes place. For the first time we find this specific regime of sheath operation near the floating emissive surface. In this regime, the potential drop over the plate sheath is about four times larger than the temperature of plasma electrons. The virtual cathode appears near the emissive plate and its modification helps to maintain the BEE regime within some voltage range. Further increase of the applied voltage U initiates the second smooth transition to the plasma electron emission sheath regime and the ratio Δφs/Te tends to unity with increasing U. The oscillatory behavior of the emissive sheath is analyzed in PIC MCC simulations. A plasmoid of slow electrons is formed near the plate and transported to the bulk plasma periodically with a frequency of about 25 kHz.

  10. Performance of high burned PWR fuel during transient

    International Nuclear Information System (INIS)

    Yanagisawa, Kazuaki; Fujishiro, Toshio

    1992-01-01

    In a majority of Japanese light water type commercial powder reactors (LWRs), UO 2 pellet sheathed by zircaloy cladding is used. Licensed discharged burn-up of the PWR fuel rod is going to be increased from 39 MWd/kgU to 48 MWd/kgU. This requests the increased reliability of cladding material as a strong barrier against fission product (FP). A long time usage in the neutron field and in the high temperature coolant will cause the zircaloy hardening and embrittlement. The cladding material is also degraded by waterside corrosion. These degradations are enhanced much by increased burn-up. A increased magnitude of the pellet-cladding mechanical interaction (PCMI) is of importance for increasing the stress of cladding material. In addition, aggressive FPs released from the fuel tends to attack the cladding material to cause stress corrosion cracking (SCC). At the Nuclear Safety Research Reactor (NSRR) in JAERI, 14 x 14 PWR type fuel rods preirradiation up to 42 MWd/kgU was prepared for the transient pulse irradiation under the simulated reactivity initiated accident (RIA) conditions. This will cause a prompt increase of the fuel temperature and stress on the highly burned cladding material. In the present paper, steady-state and transient behavior observed from the tested PWR fuel rod and calculational results obtained from the computer code FPRETAIN will be described. (author)

  11. Clad-coolant chemical interaction

    International Nuclear Information System (INIS)

    Iglesias, F.C.; Lewis, B.J.; Desgranges, C.; Toffolon, C.

    2015-01-01

    This paper provides an overview of the kinetics for zircaloy clad oxidation behaviour in steam and air during reactor accident conditions. The generation of chemical heat from metal/water reaction is considered. Low-temperature oxidation of zircaloy due to water-side corrosion is further described. (authors)

  12. Composition of the sheath produced by the green alga Chlorella sorokiniana.

    Science.gov (United States)

    Watanabe, K; Imase, M; Sasaki, K; Ohmura, N; Saiki, H; Tanaka, H

    2006-05-01

    To investigate the chemical characterization of the mucilage sheath produced by Chlorella sorokiniana. Algal mucilage sheath was hydrolysed with NaOH, containing EDTA. The purity of the hydrolysed sheath was determined by an ATP assay. The composition of polysaccharide in the sheath was investigated by high-performance anion-exchange chromatography with pulsed amperometric detection. Sucrose, galacturonic acid, xylitol, inositol, ribose, mannose, arabinose, galactose, rhamnose and fructose were detected in the sheath as sugar components. Magnesium was detected in the sheath as a divalent cation using inductively coupled argon plasma. The sheath matrix also contained protein. It appears that the sheath is composed of sugars and metals. Mucilage sheath contains many kinds of saccharides that are produced as photosynthetic metabolites and divalent cations that are contained in the culture medium. This is the first report on chemical characterization of the sheath matrix produced by C. sorokiniana.

  13. Studies of irradiated zircaloy fuel sheathing using XPS

    Energy Technology Data Exchange (ETDEWEB)

    Chan, P K; Irving, K G [Atomic Energy of Canada Ltd., Chalk River, ON (Canada); Hocking, W H; Duclos, A M; Gerwing, A F [Atomic Energy of Canada Ltd., Pinawa, MB (Canada). Whiteshell Labs.

    1996-12-31

    The preliminary results reported here support the hypothesis that CANLUB graphite coating reduces the rate at which oxygen can react with fuel sheathing. X-ray photoelectron spectroscopic (XPS) characterization of Zircaloy sheathing obtained from extended-burnup Bruce-type elements (BDL-406-XY (555 MW.h/kgU) and BDL-406-AAH (731 MW.h/kgU)) irradiated in NRU indicates that CANLUB may reduce fuel sheath oxidation, and hence that fission-liberated oxygen may remain in the fuel. Chemical shifts in the Zr 3d spectra suggest that a stoichiometric (ZrO{sub 2}) oxide film was formed only on Zircaloy in direct contact with fuel. Particulate fuel adhering to the sheath was also determined to be systematically more oxidized on surfaces with CANLUB than on those without it. The unique association of tin on sheathing specimens with the non-CANLUB-coated specimens might also suggest that the tin had segregated from the sheathing. It must be emphasized that further experiments are required to better define the effect of CANLUB on fuel oxidation. (author). 14 refs., 1 tab., 3 figs.

  14. Studies of irradiated zircaloy fuel sheathing using XPS

    International Nuclear Information System (INIS)

    Chan, P.K.; Irving, K.G.; Hocking, W.H.; Duclos, A.M.; Gerwing, A.F.

    1995-01-01

    The preliminary results reported here support the hypothesis that CANLUB graphite coating reduces the rate at which oxygen can react with fuel sheathing. X-ray photoelectron spectroscopic (XPS) characterization of Zircaloy sheathing obtained from extended-burnup Bruce-type elements (BDL-406-XY (555 MW.h/kgU) and BDL-406-AAH (731 MW.h/kgU)) irradiated in NRU indicates that CANLUB may reduce fuel sheath oxidation, and hence that fission-liberated oxygen may remain in the fuel. Chemical shifts in the Zr 3d spectra suggest that a stoichiometric (ZrO 2 ) oxide film was formed only on Zircaloy in direct contact with fuel. Particulate fuel adhering to the sheath was also determined to be systematically more oxidized on surfaces with CANLUB than on those without it. The unique association of tin on sheathing specimens with the non-CANLUB-coated specimens might also suggest that the tin had segregated from the sheathing. It must be emphasized that further experiments are required to better define the effect of CANLUB on fuel oxidation. (author). 14 refs., 1 tab., 3 figs

  15. Dynamic sheath studies in plasma source ion implantation

    International Nuclear Information System (INIS)

    Schever, J.T.; Shamim, M.; Conrad, J.R.

    1990-01-01

    Plasma Source Ion Implantation (PSII) is a non-line-of-sight method for materials processing in which a target is immersed in a plasma and pulse biased to a high negative voltage (∼ 50 kV). A model of the dynamic sheath which forms under these conditions has been developed and applied to planar, cylindrical and spherical geometries. This model assumes that the transient sheath obeys the Child-Langmuir law for space charge limited emission at each instant during the propagation. Ions uncovered by the propagating sheath edge supply the space charge limited current. This yields an equation relating sheath edge velocity to position, which can be integrated to obtain the sheath edge position as a function of time. The same procedure used in cylindrical and spherical geometry results in a similar equation which must be integrated numerically. Comparison of results of experimental measurements, our model and simulation will be presented for the dynamic sheath edge position and target current waveform. Measurements of implanted dose uniformity of wedge shaped targets are also presented

  16. Analytical expression for sheath edge around corner cathodes

    International Nuclear Information System (INIS)

    Sheridan, T E

    2009-01-01

    A simple analytical expression for the position of the sheath edge around a two-dimensional corner cathode with included angle θ c has been discovered. This expression is valid for weakly collisional sheaths in the Child-Langmuir regime φ c >> kT e /e, where -φ c e is the electron temperature. In polar coordinates (r, θ), the sheath edge is given by (r/s 0 )sin[πθ/(2π - θ c )] = [π/(2π - θ c )] where s 0 is the planar sheath width far from the vertex of the corner. This result is verified by comparison with previous numerical solutions (Watterson P A 1989 J. Phys. D: Appl. Phys. 22 1300) for the knife edge (θ c = 0) and convex square corner (θ c = π/2). The observed agreement suggests that this expression gives the sheath edge for all corner angles, both concave and convex. The utility of this result is demonstrated by computing the full sheath solution for a knife-edge cathode with φ c = 100kT e /e.

  17. Non-Maxwellian plasma sheaths

    International Nuclear Information System (INIS)

    Haines, M.G.

    1998-01-01

    There is much experimental evidence that heat flux to divertor plates or to limiters is very asymmetric. For example, Lowry made measurements on poloidal limiters in JET, Stangeby and McCracken reported asymmetries in several experiments. In 1991 Haines considered the effects on the Child-Langmuir sheaths of having a net current flow. It was found that a sheath that receives more ions than electrons receives more energy flux than a sheath that receives more electrons than ions. We now extend the model to include for the electrons departures from a Maxwellian distribution arising from a net current flow, heat flow and thermoelectric effects in the scrape-off layer (SOL). It is envisaged that a net current flows in the SOL due to applied or induced electric fields, and is of a magnitude similar to that in the adjacent bulk plasma, though reduced due to the lower temperature in the SOL. We employ conventional linear transport theory eg. Braginskii, Epperlein and Haines in which the ions are a stationary Maxwellian. (orig.)

  18. What can be done about corrosion in submersible pumps?

    Energy Technology Data Exchange (ETDEWEB)

    Minett, S.

    2000-09-01

    Useful advice and a survey of materials and techniques which can help counter corrosion risks in submersible pumps are provided. The greatest risk of corrosion is caused by sea water, hydrochloric acid, certain types of solvents, hydrogen sulphide, liquids with a high copper content, bases with a high pH value and certain liquids containing a mixture of acids. Counteractive strategies suggested include using a corrosion resistant material such as stainless steel, or other resistant coatings and materials for particular components that are exposed to high corrosion risks. Most submersible pumps are made of cast iron which should present no corrosion problems in normal domestic use. In mining and construction applications aluminum submersibles are common, which is resistant to a pH value of about 8. The use of stainless steel is recommended as the main material in submersible pumps when used for pumping acidic liquids, and when purity of the liquid pumped is of prime consideration. Coatings and anodes on conventional cast iron pumps are a less expensive and more flexible alternative against salt water corrosion. Among coatings epoxy coating is the most widely used. Zinc anodes are used in conjunction with epoxy coatings, which by setting up a micro current by contact with the cast iron prevent corrosion of areas of the cast iron that may be exposed as a result of post-production scratching. By being sacrificially corroded, the zinc anodes thus significantly extend the life of a coated pump. Impressed current from an external power source, is an effective, but more expensive alternative to the implanted anode method. Using resistant materials such as nitrile rubber, fluoro-carbon rubber, corrosion resistant cemented carbide, or chlorinated rubber for various components (rotating shaft seals, rubber 'O' rings, cable sheathing, etc) are other alternatives that may be depending on the application and the degree of exposure.

  19. How to Patch Active Plasma and Collisionless Sheath: Practical Guide

    International Nuclear Information System (INIS)

    Kaganovich, Igor D.

    2002-01-01

    Most plasmas have a very thin sheath compared with the plasma dimension. This necessitates separate calculations of the plasma and sheath. The Bohm criterion provides the boundary condition for calculation of plasma profiles. To calculate sheath properties, a value of electric field at the plasma-sheath interface has to be specified in addition to the Bohm criterion. The value of the boundary electric field and robust procedure to approximately patch plasma and collisionless sheath with a very good accuracy are reported

  20. Plasma sheath in non-Maxwellian plasma

    International Nuclear Information System (INIS)

    Shimizu, Takuo; Horigome, Takashi

    1992-01-01

    Reviewing many theoretical and experimental works on the electron-energy distributions (EEDF) of various plasmas, we point out that many plasmas have EEDF of non-Maxwellian in shape. Therefore, the recent treatment of plasma sheath using the Maxwell-Boltzmann distribution approximation should be improved. To do this, we have adopted Rutcher's standard distribution as a generalized form in place of the traditional Maxwellian, and found that the minimum energy of ions entering the sheath edge (Bohm's criterion) varies largely, and have also shown the variation of Debye length with the shape of EEDF. The length is the most important parameter to proceed with more detailed analysis on plasma-sheaths, and also to control them in the future. (author)

  1. Theory of the Electron Sheath and Presheath

    Science.gov (United States)

    Scheiner, Brett; Baalrud, Scott; Yee, Benjamin; Hopkins, Matthew; Barnat, Edward

    2015-09-01

    Electron sheaths are commonly found near Langmuir probes collecting the electron saturation current. The common assumption is that the probe collects the random flux of electrons incident on the sheath, which tacitly implies that there is no electron presheath and that the flux collected is due to a velocity space truncation of the velocity distribution function (VDF). This work provides a dedicated theory of electron sheaths, which suggests that electron sheaths are not so simple. Motivated by VDFs observed in recent Particle-In-Cell (PIC) simulations, we develop a 1D model for the electron sheath and presheath. In the model, under low temperature plasma conditions, an electron pressure gradient accelerates electrons in the presheath to a flow velocity that exceeds the electron thermal speed at the sheath edge. This pressure gradient allows the generation of large flows compared to those that would be generated by the electric field alone. It is due to this pressure gradient that the electron presheath extends much further into the plasma (nominally by a factor of √{mi /me }) than an analogous ion presheath. Results of the model are compared with PIC simulations. This work was supported by the Office of Fusion Energy Science at the U.S. Department of Energy under contract DE-AC04-94SL85000 and by the Office of Science Graduate Student Research (SCGSR) program under Contract Number DE-AC05-06OR23100.

  2. Anode sheath in Hall thrusters

    International Nuclear Information System (INIS)

    Dorf, L.; Semenov, V.; Raitses, Y.

    2003-01-01

    A set of hydrodynamic equations is used to describe quasineutral plasma in ionization and acceleration regions of a Hall thruster. The electron distribution function and Poisson equation are invoked for description of a near-anode region. Numerical solutions suggest that steady-state operation of a Hall thruster can be achieved at different anode sheath regimes. It is shown that the anode sheath depends on the thruster operating conditions, namely the discharge voltage and the mass flow rate

  3. Abiotic Deposition of Fe Complexes onto Leptothrix Sheaths

    Science.gov (United States)

    Kunoh, Tatsuki; Hashimoto, Hideki; McFarlane, Ian R.; Hayashi, Naoaki; Suzuki, Tomoko; Taketa, Eisuke; Tamura, Katsunori; Takano, Mikio; El-Naggar, Mohamed Y.; Kunoh, Hitoshi; Takada, Jun

    2016-01-01

    Bacteria classified in species of the genus Leptothrix produce extracellular, microtubular, Fe-encrusted sheaths. The encrustation has been previously linked to bacterial Fe oxidases, which oxidize Fe(II) to Fe(III) and/or active groups of bacterial exopolymers within sheaths to attract and bind aqueous-phase inorganics. When L. cholodnii SP-6 cells were cultured in media amended with high Fe(II) concentrations, Fe(III) precipitates visibly formed immediately after addition of Fe(II) to the medium, suggesting prompt abiotic oxidation of Fe(II) to Fe(III). Intriguingly, these precipitates were deposited onto the sheath surface of bacterial cells as the population was actively growing. When Fe(III) was added to the medium, similar precipitates formed in the medium first and were abiotically deposited onto the sheath surfaces. The precipitates in the Fe(II) medium were composed of assemblies of globular, amorphous particles (ca. 50 nm diameter), while those in the Fe(III) medium were composed of large, aggregated particles (≥3 µm diameter) with a similar amorphous structure. These precipitates also adhered to cell-free sheaths. We thus concluded that direct abiotic deposition of Fe complexes onto the sheath surface occurs independently of cellular activity in liquid media containing Fe salts, although it remains unclear how this deposition is associated with the previously proposed mechanisms (oxidation enzyme- and/or active group of organic components-involved) of Fe encrustation of the Leptothrix sheaths. PMID:27271677

  4. Abiotic Deposition of Fe Complexes onto Leptothrix Sheaths

    Directory of Open Access Journals (Sweden)

    Tatsuki Kunoh

    2016-06-01

    Full Text Available Bacteria classified in species of the genus Leptothrix produce extracellular, microtubular, Fe-encrusted sheaths. The encrustation has been previously linked to bacterial Fe oxidases, which oxidize Fe(II to Fe(III and/or active groups of bacterial exopolymers within sheaths to attract and bind aqueous-phase inorganics. When L. cholodnii SP-6 cells were cultured in media amended with high Fe(II concentrations, Fe(III precipitates visibly formed immediately after addition of Fe(II to the medium, suggesting prompt abiotic oxidation of Fe(II to Fe(III. Intriguingly, these precipitates were deposited onto the sheath surface of bacterial cells as the population was actively growing. When Fe(III was added to the medium, similar precipitates formed in the medium first and were abiotically deposited onto the sheath surfaces. The precipitates in the Fe(II medium were composed of assemblies of globular, amorphous particles (ca. 50 nm diameter, while those in the Fe(III medium were composed of large, aggregated particles (≥3 µm diameter with a similar amorphous structure. These precipitates also adhered to cell-free sheaths. We thus concluded that direct abiotic deposition of Fe complexes onto the sheath surface occurs independently of cellular activity in liquid media containing Fe salts, although it remains unclear how this deposition is associated with the previously proposed mechanisms (oxidation enzyme- and/or active group of organic components-involved of Fe encrustation of the Leptothrix sheaths.

  5. Farris-Tang retractor in optic nerve sheath decompression surgery.

    Science.gov (United States)

    Spiegel, Jennifer A; Sokol, Jason A; Whittaker, Thomas J; Bernard, Benjamin; Farris, Bradley K

    2016-01-01

    Our purpose is to introduce the use of the Farris-Tang retractor in optic nerve sheath decompression surgery. The procedure of optic nerve sheath fenestration was reviewed at our tertiary care teaching hospital, including the use of the Farris-Tang retractor. Pseudotumor cerebri is a syndrome of increased intracranial pressure without a clear cause. Surgical treatment can be effective in cases in which medical therapy has failed and disc swelling with visual field loss progresses. Optic nerve sheath decompression surgery (ONDS) involves cutting slits or windows in the optic nerve sheath to allow cerebrospinal fluid to escape, reducing the pressure around the optic nerve. We introduce the Farris-Tang retractor, a retractor that allows for excellent visualization of the optic nerve sheath during this surgery, facilitating the fenestration of the sheath and visualization of the subsequent cerebrospinal fluid egress. Utilizing a medial conjunctival approach, the Farris-Tang retractor allows for easy retraction of the medial orbital tissue and reduces the incidence of orbital fat protrusion through Tenon's capsule. The Farris-Tang retractor allows safe, easy, and effective access to the optic nerve with good visualization in optic nerve sheath decompression surgery. This, in turn, allows for greater surgical efficiency and positive patient outcomes.

  6. Effect of collisions on photoelectron sheath in a gas

    Science.gov (United States)

    Sodha, Mahendra Singh; Mishra, S. K.

    2016-02-01

    This paper presents a study of the effect of the collision of electrons with atoms/molecules on the structure of a photoelectron sheath. Considering the half Fermi-Dirac distribution of photo-emitted electrons, an expression for the electron density in the sheath has been derived in terms of the electric potential and the structure of the sheath has been investigated by incorporating Poisson's equation in the analysis. The method of successive approximations has been used to solve Poisson's equation with the solution for the electric potential in the case of vacuum, obtained earlier [Sodha and Mishra, Phys. Plasmas 21, 093704 (2014)], being used as the zeroth order solution for the present analysis. The inclusion of collisions influences the photoelectron sheath structure significantly; a reduction in the sheath width with increasing collisions is obtained.

  7. Effect of two-temperature electrons distribution on an electrostatic plasma sheath

    International Nuclear Information System (INIS)

    Ou, Jing; Xiang, Nong; Gan, Chunyun; Yang, Jinhong

    2013-01-01

    A magnetized collisionless plasma sheath containing two-temperature electrons is studied using a one-dimensional model in which the low-temperature electrons are described by Maxwellian distribution (MD) and high-temperature electrons are described by truncated Maxwellian distribution (TMD). Based on the ion wave approach, a modified sheath criterion including effect of TMD caused by high-temperature electrons energy above the sheath potential energy is established theoretically. The model is also used to investigate numerically the sheath structure and energy flux to the wall for plasmas parameters of an open divertor tokamak-like. Our results show that the profiles of the sheath potential, two-temperature electrons and ions densities, high-temperature electrons and ions velocities as well as the energy flux to the wall depend on the high-temperature electrons concentration, temperature, and velocity distribution function associated with sheath potential. In addition, the results obtained in the high-temperature electrons with TMD as well as with MD sheaths are compared for the different sheath potential

  8. A suitable boundary condition for bounded plasma simulation without sheath resolution

    International Nuclear Information System (INIS)

    Parker, S.E.; Procassini, R.J.; Birdsall, C.K.; Cohen, B.I.

    1993-01-01

    We have developed a technique that allows for a sheath boundary layer without having to resolve the inherently small space and time scales of the sheath region. We refer to this technique as the logical sheath boundary condition. This boundary condition, when incorporated into a direct-implicit particle code, permits large space- and time-scale simulations of bounded systems, which would otherwise be impractical on current supercomputers. The lack of resolution of the collector sheath potential drop obtained from conventional implicit simulations at moderate values of ω pe Δt and Δz/λ De provides the motivation for the development of the logical sheath boundary condition. The algorithm for use of the logical sheath boundary condition in a particle simulation is presented. Results from simulations which use the logical sheath boundary condition are shown to compare reasonably well with those from an analytic theory and simulations in which the sheath is resolved

  9. Electrospinning jet behaviors under the constraints of a sheath gas

    Directory of Open Access Journals (Sweden)

    Yang Zhao

    2016-11-01

    Full Text Available Increasing the ejection efficiency and uniformity of nanofibers is the key to applications of electrospinning technology. In this work, a novel electrospinning spinneret with a sheath gas passageway is designed. The frictional resistance that stems from the sheath gas provides additional stretching and restriction forces on the jet. The sheath gas also reduces interference and enhances the stability of the charged jet. A bead-on-strain simulation model is built up to determine the constraint effects of the sheath gas. Simulation results show that the sheath gas decreases the motion area and increases the stretching ratio of the liquid jet. The stretching force from the sheath gas decreases the diameter and increases the uniformity of the nanofiber. As the gas pressure increases from 0 kPa to 50 kPa, the critical voltage of the jet ejection decreases from 8.4 kV to 2.5 kV, the diameter of the nanofiber deposition zone decreases from 40 cm to 10 cm, and the diameter of the nanofibers decreases from 557.97 nm to 277.73 nm. The uniformity of nanofibers can be improved significantly using a sheath gas. The sheath gas contributes to the rapid deposition of a uniform nanofibrous membrane and the industrial applications of electrospinning.

  10. Use of guiding sheaths in peroral fluoroscopic gastroduodenal stent placement

    International Nuclear Information System (INIS)

    Bae, Jae-Ik; Shin, Ji Hoon; Song, Ho-Young; Yoon, Chang Jin; Nam, Deok Ho; Choi, Won-Chan; Lim, Jin-Oh

    2005-01-01

    Our purpose was to assess the safety and usefulness of guiding sheaths in peroral fluoroscopic gastroduodenal stent placement. Two types of guiding sheath were made from straight polytetrafluoroethylene tubes. Type A was 80 cm in length, 4 mm in outer diameter and 3 mm in inner diameter. Type B was 70 cm in length, 6 mm in outer diameter and 5 mm in inner diameter. The type A sheath was used in 18 patients in whom a catheter-guide wire combination failed to pass through a stricture. The type B sheath was used in 22 patients in whom a stent delivery system failed to pass through the stricture due to loop formation within the gastric lumen. The overall success rate for guiding a catheter-guide wire through a stricture after using the type A sheath was 89%. The overall success rate for passing a stent delivery system through a stricture after using the type B sheath was 100%. All procedures were tolerated by the patients without any significant complications. The guiding sheaths were safe and useful in peroral fluoroscopic gastroduodenal stent placement. (orig.)

  11. Experimental investigation of plasma sheaths in magnetic mirror and cusp configurations

    Science.gov (United States)

    Jiang, Zhengqi; Wei, Zi-an; Ma, J. X.

    2017-11-01

    Sheath structures near a metal plate in a magnetized plasma were experimentally investigated in magnetic mirror and cusp configurations. Plasma parameters and the sheath potential distributions were probed by a planar and an emissive probe, respectively. The measured sheath profiles in the mirror configuration show that the sheath thickness first decreases and then increases when the magnetic strength is raised. A magnetic flux-tube model was used to explain this result. In the cusp configuration, the measured sheath thickness decreases with the increase of the coil current creating the magnetic cusp. However, when normalized by the electron Debye length, the dependence of the sheath thickness on the coil current is reversed.

  12. Behavior of collisional sheath in electronegative plasma with q-nonextensive electron distribution

    Science.gov (United States)

    Borgohain, Dima Rani; Saharia, K.

    2018-03-01

    Electronegative plasma sheath is addressed in a collisional unmagnetized plasma consisting of q-nonextensive electrons, Boltzmann distributed negative ions and cold fluid positive ions. Considering the positive ion-neutral collisions and ignoring the effects of ionization and collisions between negative species and positive ions (neutrals), a modified Bohm sheath criterion and hence floating potential are derived by using multifluid model. Using the modified Bohm sheath criterion, the sheath characteristics such as spatial profiles of density, potential and net space charge density have been numerically investigated. It is found that increasing values of q-nonextensivity, electronegativity and collisionality lead to a decrease of the sheath thickness and an increase of the sheath potential and the net space charge density. With increasing values of the electron temperature to negative ion temperature ratio, the sheath thickness increases and the sheath potential as well as the net space charge density in the sheath region decreases.

  13. Corrosion and alteration of materials from the nuclear industry

    International Nuclear Information System (INIS)

    Beauvy, M.; Berthoud, G.; Defranceschi, M.; Ducros, G.; Feron, D.; Guerin, Y.; Latge, C.; Limoge, Y.; Madic, C.; Santarini, G.; Seiler, J.M.; Vernaz, E.; Richet, C.

    2010-01-01

    , testing means, experimental techniques, internal corrosion of zircaloy sheath - the iodine effect, stress corrosion of nickel alloys - hydrogen influence, stress corrosion of stainless steels; C - wear corrosion: a coupled phenomenon, research in the framework of service life extension of the French electronuclear park; 3 - Corrosion in future reactors: A - corrosion in gas reactors: corrosion by helium impurities, oxidation resistance of silicon carbide, corrosion of graphite and carbon-carbon composites; B - corrosion in liquid metal reactors: sodium FBRs, lead and lead alloys reactors; C- corrosion in molten salt reactors: corrosion of Hastelloy N-type nickel alloys by molten fluorides, mass transfer in aniso-thermal fluoride systems, tellurium embrittlement, electrochemical study of pure metals corrosion in molten fluorides; 4 - Materials corrosion and alteration in the back-end of the fuel cycle: A - corrosion in concentrated nitric environment: materials behaviour, self-catalytic mechanism of nitric acid reduction; B - corrosion in unsaturated aqueous environment: metallic corrosion in unsaturated environment - application to the storage of waste containers, bitumens alteration, reinforced concrete behaviour and iron framework corrosion, concrete behaviour in severe thermal environment; C - Corrosion in saturated aqueous environment: metals corrosion in clayey environment, long-term behaviour of glasses, ceramics alteration, underwater concrete durability, clays transformation; D - materials biodegradation: microorganisms and nuclear wastes, biodegradation of bitumen, concretes and steels; 5 - Conclusion, glossary

  14. ALINE: A device dedicated to understanding radio-frequency sheaths

    Directory of Open Access Journals (Sweden)

    S. Devaux

    2017-08-01

    Full Text Available In fusion devices, radiofrequency (RF antennas are used for heating the plasma. Those antennas and the plasma interact with each other through the so-called RF sheaths, layers of plasma where the quasi-neutrality breaks down and large electric fields arise. Among the effects of RF sheaths, there is the enhancement of the particles and energy fluxes toward the surface of the antenna, which in turn generate hot spots and release impurities, which are both deleterious for plasma operations. RF sheaths comprehension stumbles on the difficulty to achieve in situ measurements of the sheath properties, as scrape-off layer plasmas are a harsh environment. The very goal of the ALINE device is to tackle this issue and to fulfil the blank between numerical simulations and full-scale experiment by providing measurements within the RF sheaths in a controlled environment. In this paper we report on the latest experimental results from ALINE, in which a cylindrical Langmuir probe mounted on a remotely controlled and programmable arm allows for plasma characterizations in the three dimensions of space around the stainless steel antenna, including the sheath. We present a series of density and potential profiles and three dimension (3D maps in the plasma surrounding a stainless-steel RF antenna as well as in the sheath itself, for unmagnetized and magnetized plasmas.

  15. In vivo engineering of a functional tendon sheath in a hen model.

    Science.gov (United States)

    Xu, Liang; Cao, Dejun; Liu, Wei; Zhou, Guangdong; Zhang, Wen Jie; Cao, Yilin

    2010-05-01

    Repair of injured tendon sheath remains a major challenge and this study explored the possibility of in vivo reconstruction of a tendon sheath with tendon sheath derived cells and polyglycolic acid (PGA) fibers in a Leghorn hen model. Total 55 Leghorn hens with a 1cm tendon sheath defect created in the left middle toe of each animal were randomly assigned into: (1) experimental group (n=19) that received a cell-PGA construct; (2) scaffold control group (n=18) that received a cell-free PGA scaffold; (3) blank control group (n=18) with the defect untreated. Tendon sheath cells were isolated, in vitro expanded, and seeded onto PGA scaffolds. After in vitro culture for 7 days, the constructs were in vivo implanted to repair the sheath defects. Alcian blue staining confirmed the ability of cultured cells to produce specific matrices containing acidic carboxyl mucopolysaccharide (mainly hyaluronic acid). In addition, the engineered sheath formed a relatively mature structure at 12 weeks post-surgery, which was similar to that of native counterpart, including a smooth inner surface, a well-developed sheath histological structure with a clear space between the tendon and the engineered sheath. More importantly, Work of Flexion assay revealed that the tendons needed less power consumption to glide inside the engineered sheath when compared to the tendons which were surrounded by scar-repaired tissues, indicating that the engineered sheaths had gained the function to a certain extent of preventing tendon adhesion. Taken together, these results suggest that tendon sheaths that are functionally and structurally similar to native sheaths are possible to be engineered in vivo using tendon sheath cells and PGA scaffolds. Copyright 2010 Elsevier Ltd. All rights reserved.

  16. Smart pigging - a contribution to the monitoring of the anti-corrosion protection systems on pig-inspectable high-pressure gas transmission pipelines; Intelligente Molchung - ein Beitrag zur Ueberwachung des Korrosionsschutzes molchbarer Gashochdruckleitungen

    Energy Technology Data Exchange (ETDEWEB)

    Ahlers, M.; Schoeneich, H.G. [Ruhrgas AG, Essen (Germany). Kompetenz-Center Korrosionsschutz

    2000-07-01

    High-pressure gas transmission pipelines installed underground are exposed to the risk of external corrosion. The application of a sheathing (passive protection) and, since the 1950s, the installation of a cathodic anti-corrosion protection system, provide pipelines with effective protection against this danger. In the past, the effectiveness of cathodic anti-corrosion protection systems was verified by means of intensive measuring and re-measuring cycles. It became apparent that points of damage to the sheathing were protected in the majority of cases against corrosion by the cathodic anti-corrosion protection system. There are, however, particular design circumstances and ambient conditions which can make this anti-corrosion protection concept either partially or completely ineffective. The use of smart pigs for inspection of pig-inspectable gas transmission pipelines makes it possible to detect and eliminate these weak points. (orig.) [German] Gashochdruckleitungen, die im Erdboden verlegt werden, unterliegen einer Gefaehrdung durch Aussenkorrosion. Durch eine Umhuellung (passiver Schutz) und seit den 50er Jahren durch die Einrichtung des kathodischen Korrosionsschutzes (aktiver Schutz) sind die Leitungen gegen diese Gefaehrdung wirkungsvoll geschuetzt. In der Vergangenheit wurde die Ueberpruefung der Wirksamkeit des kathodischen Korrosionsschutzes durch Intensivmessungen und Nachmessungen sichergestellt. Dabei zeigte sich, dass in der ueberwiegenden Zahl Umhuellungsbeschaedigungen durch den kathodischen Korrosionsschutz gegen Korrosion geschuetzt sind. Es gibt jedoch besondere konstruktive oder Umgebungsbedingungen, die dieses Korrosionsschuzkonzept teilweise oder vollstaendig unwirksam werden lassen. Mit dem Einsatz von intelligenten Molchen zur Inspektion molchbarer Gastransportleitungen koennen diese Schwachstellen erkannt und beseitigt werden. (orig.)

  17. Intrapontine malignant nerve sheath tumor

    DEFF Research Database (Denmark)

    Kozić, Dusko; Nagulić, Mirjana; Samardzić, Miroslav

    2008-01-01

    . On pathological examination, the neoplasm appeared to be an intrapontine nerve sheath tumor originating most likely from the intrapontine segment of one of the cranial nerve fibres. The tumor showed exophytic growth, with consequent spread to adjacent subaracnoid space. MR spectroscopy revealed the presence......The primary source of malignant intracerebral nerve sheath tumors is still unclear We report the imaging and MR spectroscopic findings in a 39-year-old man with a very rare brain stem tumor MR examination revealed the presence of intraaxial brain stem tumor with a partial exophytic growth...

  18. The Child-Langmuir law and analytical theory of collisionless to collision-dominated sheaths

    International Nuclear Information System (INIS)

    Benilov, M S

    2009-01-01

    This paper is concerned with summarizing simple analytical models of space-charge sheaths and tracing their relation to the Child-Langmuir model of an ion sheath. The topics discussed include the Child-Langmuir law and model of a collisionless ion sheath, the Mott-Gurney law and model of a collision-dominated ion sheath, the Bohm model of a collisionless ion-electron sheath, the Su-Lam-Cohen model of a collision-dominated ion-electron sheath, ion sheaths with arbitrary collisionality, high-accuracy boundary conditions for the Child-Langmuir and Mott-Gurney models of an ion sheath and the mathematical sense of Child-Langmuir type models of an ion sheath from the point of view of modern theoretical physics.

  19. What is the size of a floating sheath? An answer

    Science.gov (United States)

    Voigt, Farina; Naggary, Schabnam; Brinkmann, Ralf Peter

    2016-09-01

    The formation of a non-neutral boundary sheath in front of material surfaces is universal plasma phenomenon. Despite several decades of research, however, not all related issues are fully clarified. In a recent paper, Chabert pointed out that this lack of clarity applies even to the seemingly innocuous question ``What the size of a floating sheath?'' This contribution attempts to provide an answer that is not arbitrary: The size of a floating sheath is defined as the plate separation of an equivalent parallel plate capacitor. The consequences of the definition are explored with the help of a self-consistent sheath model, and a comparison is made with other sheath size definitions. Deutsche Forschungsgemeinschaft within SFB TR 87.

  20. Effects of emitted electron temperature on the plasma sheath

    International Nuclear Information System (INIS)

    Sheehan, J. P.; Kaganovich, I. D.; Wang, H.; Raitses, Y.; Sydorenko, D.; Hershkowitz, N.

    2014-01-01

    It has long been known that electron emission from a surface significantly affects the sheath surrounding that surface. Typical fluid theory of a planar sheath with emitted electrons assumes that the plasma electrons follow the Boltzmann relation and the emitted electrons are emitted with zero energy and predicts a potential drop of 1.03T e /e across the sheath in the floating condition. By considering the modified velocity distribution function caused by plasma electrons lost to the wall and the half-Maxwellian distribution of the emitted electrons, it is shown that ratio of plasma electron temperature to emitted electron temperature significantly affects the sheath potential when the plasma electron temperature is within an order of magnitude of the emitted electron temperature. When the plasma electron temperature equals the emitted electron temperature the emissive sheath potential goes to zero. One dimensional particle-in-cell simulations corroborate the predictions made by this theory. The effects of the addition of a monoenergetic electron beam to the Maxwellian plasma electrons were explored, showing that the emissive sheath potential is close to the beam energy only when the emitted electron flux is less than the beam flux

  1. Sheath impedance effects in very high frequency plasma experiments

    International Nuclear Information System (INIS)

    Schwarzenbach, W.; Howling, A.A.; Fivaz, M.; Brunner, S.; Hollenstein, C.

    1995-05-01

    The frequency dependence (13.56 MHz to 70 MHz) of the ion energy distribution at the ground electrode was measured by mass spectrometry in a symmetrical capacitive argon discharge. Reduced sheath impedance at Very High Frequency allows high levels of plasma power and substrate ion flux whilst maintaining low levels of ion energy and electrode voltage. The lower limit of ion bombardment energy is fixed by the sheath floating potential at high frequency, in contrast to low frequencies where only the rf voltage amplitude is determinant. The capacitive sheaths are thinner at high frequencies which accentuates the high frequency reduction in sheath impedance. It is argued that the frequency dependence of sheath impedance is responsible for the principal characteristics of Very High Frequency plasmas. The measurements are summarised by simple physical descriptions and compared with a Particle-In-Cell simulation. (author) figs., tabs., refs

  2. Genomic and Expression Profiling of Benign and Malignant Nerve Sheath Profiling of Benign and Malignant Nerve Sheath

    Science.gov (United States)

    2007-05-01

    Benign and Malignant Nerve Sheath Tumors in Neurofibromatosis Patients PRINCIPAL INVESTIGATOR: Matt van de Rijn, M.D., Ph.D. Torsten...Annual 3. DATES COVERED 1 May 2006 –30 Apr 2007 4. TITLE AND SUBTITLE 5a. CONTRACT NUMBER Genomic and Expression Profiling of Benign and Malignant Nerve...Award Number: DAMD17-03-1-0297 Title: Genomic and Expression Profiling of Benign and Malignant Nerve Sheath Tumors in Neurofibromatosis

  3. Nondestructive testing of metallic sheath for internally cooled superconductor

    International Nuclear Information System (INIS)

    McClung, R.W.; Cook, K.V.; Dodd, C.V.; Smith, J.H.

    1983-01-01

    For quality assurance in the Oak Ridge National Laboratory Large Coil Program, we developed ultrasonic and eddy-current techniques to examine the JBK-75 alloy sheath for superconducting cable for a large magnet. Ultrasound was used to examine the strip before forming into the sheath, and eddy currents were used to examine the seam weld after the sheath had been formed around the cable

  4. Dynamic thermo-chemo-mechanical strain of Zircaloy-4 slotted rings for evaluating strategies that mitigate stress corrosion cracking

    Energy Technology Data Exchange (ETDEWEB)

    Ferrier, G.A.; Metzler, J.; Farahani, M.; Chan, P.K.; Corcoran, E.C. [Royal Military College of Canada, Kingston, ON (Canada)

    2014-07-01

    Stress corrosion cracking (SCC) in Zircaloy-4 fuel sheaths has been investigated by static loading of slotted ring samples under hot and corrosive conditions. However, in nuclear reactors, power ramps can have short (e.g., 10-20 minutes) and recurring time frames due to dynamic processes such as on-power refuelling, adjuster rod manoeuvres, and load following. Therefore, to enable out-reactor dynamic testing, an apparatus was designed to dynamically strain slotted ring samples under SCC conditions. This apparatus can additionally be used to test fatigue properties. Unique capabilities of this apparatus and preliminary results obtained from static and dynamic tests are presented. (author)

  5. Plasma Sheath Behavior in a Coaxial Discharge Device

    International Nuclear Information System (INIS)

    EL-Aragi, G.; Soliman, H.M.; Masoud, M.M.

    2001-01-01

    The behavior of the plasma sheath has been studied experimentally and theoretically for 3 kJ coaxial discharge device. The discharge takes place in argon gas with pressure of 0.8 mbar. The experiments are conducted with a 10 kV bank charging voltage, which corresponds to 110 kA peak discharge current with time period of 34 μs. The experimental investigations have been studied using a magnetic probes and a miniature Rogowsky coil. A snowplough model is used to drive an analytical solution of the plasma sheath behavior in axial direction. Measurements of radial distribution of plasma sheath current density J r at the muzzle, show that J r has the following relation, J r is proportional to r -1.1 . From the experimental results and theoretical calculations of axial distribution of azimuthal magnetic field induction and plasma sheath velocity, the inclination angle between the normal of the plasma sheath with the axial distance at any axial position is evaluated and it has approximately a constant value for most axial distances. Also, the axial motion of plasma sheath acceleration is estimated experimentally a max = 0.13 x 10 12 ' cm / s 2 at z = 11 cm and from theoretical calculations a max = 0.15 x 10 12 cm/ s 2 at max z = 1.6 cm. A comparison of the experimental results with the theoretical calculations, under the assumption of the snowplough model are not in agreement. (author)

  6. Stability of the Tonks–Langmuir discharge pre-sheath

    Energy Technology Data Exchange (ETDEWEB)

    Tskhakaya, D. D. [Fusion@ÖAW, Institute of Applied Physics, TU Wien, Wiedner Hauptstraße 8-10, 1040 Vienna (Austria); Kos, L. [LECAD Laboratory, Faculty of Mechanical Engineering, University of Ljubljana, SI-1000 Ljubljana (Slovenia); Tskhakaya, D. [Fusion@ÖAW, Institute of Applied Physics, TU Wien, Wiedner Hauptstraße 8-10, 1040 Vienna (Austria); Institute for Theoretical Physics, University of Innsbruck, A-6020 Innsbruck (Austria)

    2016-03-15

    The article formulates the stability problem of the plasma sheath in the Tonks–Langmuir discharge. Using the kinetic description of the ion gas, i.e., the stability of the potential shape in the quasi-neutral pre-sheath regarding the high and low frequency, the perturbations are investigated. The electrons are assumed to be Maxwell–Boltzmann distributed. Regarding high-frequency perturbations, the pre-sheath is shown to be stable. The stability problem regarding low-frequency perturbations can be reduced to an analysis of the “diffusion like” equation, which results in the instability of the potential distribution in the pre-sheath. By means of the Particle in Cell simulations, also the nonlinear stage of low frequency oscillations is investigated. Comparing the figure obtained with the figure for linear stage, one can find obvious similarity in the spatial-temporal behavior of the potential.

  7. The magnetized sheath of a dusty plasma with grains size distribution

    International Nuclear Information System (INIS)

    Ou, Jing; Gan, Chunyun; Lin, Binbin; Yang, Jinhong

    2015-01-01

    The structure of a plasma sheath in the presence of dust grains size distribution (DGSD) is investigated in the multi-fluid framework. It is shown that effect of the dust grains with different sizes on the sheath structure is a collective behavior. The spatial distributions of electric potential, the electron and ion densities and velocities, and the dust grains surface potential are strongly affected by DGSD. The dynamics of dust grains with different sizes in the sheath depend on not only DGSD but also their radius. By comparison of the sheath structure, it is found that under the same expected value of DGSD condition, the sheath length is longer in the case of lognormal distribution than that in the case of uniform distribution. In two cases of normal and lognormal distributions, the sheath length is almost equal for the small variance of DGSD, and then the difference of sheath length increases gradually with increase in the variance

  8. An analytical investigation: Effect of solar wind on lunar photoelectron sheath

    Science.gov (United States)

    Mishra, S. K.; Misra, Shikha

    2018-02-01

    The formation of a photoelectron sheath over the lunar surface and subsequent dust levitation, under the influence of solar wind plasma and continuous solar radiation, has been analytically investigated. The photoelectron sheath characteristics have been evaluated using the Poisson equation configured with population density contributions from half Fermi-Dirac distribution of the photoemitted electrons and simplified Maxwellian statistics of solar wind plasma; as a consequence, altitude profiles for electric potential, electric field, and population density within the photoelectron sheath have been derived. The expression for the accretion rate of sheath electrons over the levitated spherical particles using anisotropic photoelectron flux has been derived, which has been further utilized to characterize the charging of levitating fine particles in the lunar sheath along with other constituent photoemission and solar wind fluxes. This estimate of particle charge has been further manifested with lunar sheath characteristics to evaluate the altitude profile of the particle size exhibiting levitation. The inclusion of solar wind flux into analysis is noticed to reduce the sheath span and altitude of the particle levitation; the dependence of the sheath structure and particle levitation on the solar wind plasma parameters has been discussed and graphically presented.

  9. Simulations of rf-driven sheath formation in two dimensions

    International Nuclear Information System (INIS)

    Riyopoulos, S.; Grossmann, W.; Drobot, A.; Kress, M.

    1992-01-01

    The results from two-dimensional particle simulations of sheath formation around periodic metal arrays placed inside magnetized plasmas and driven by oscillating voltages are reported. The main goal is the modeling of the plasma interaction with the Faraday bars surrounding the antennas during ion cyclotron tokamak heating. The study of the time-averaged potentials shows that the two-dimensional sheath structure depends on both the sheath length-to-thickness ratio and the inclination of the magnetic lines. The equipotential surfaces form closed, nested cells between adjacent bars. When the magnetic lines are nearly perpendicular to the potential gradients, the ion motion is dominated by the ExB drift, and ion streamlines form vortices around the equipotentials. At larger inclinations of the magnetic lines, the flow decouples from the equipotentials and ion transport is mainly along the potential gradients. The critical angle for the transition from vortex circulation to field aligned flow is computed. The effects of the cross-field ion transport on the sheath properties are discussed. It is shown that the sheath length and the magnetic line inclination affect the sheath scaling in the two-dimensional case. The one-dimensional theory results are recovered in the limit of high length-to-thickness ratio and large inclination of the magnetic lines

  10. The Tubular Sheaths Encasing Methanosaeta thermophila Filaments Are Functional Amyloids.

    Science.gov (United States)

    Dueholm, Morten S; Larsen, Poul; Finster, Kai; Stenvang, Marcel R; Christiansen, Gunna; Vad, Brian S; Bøggild, Andreas; Otzen, Daniel E; Nielsen, Per Halkjær

    2015-08-14

    Archaea are renowned for their ability to thrive in extreme environments, although they can be found in virtually all habitats. Their adaptive success is linked to their unique cell envelopes that are extremely resistant to chemical and thermal denaturation and that resist proteolysis by common proteases. Here we employ amyloid-specific conformation antibodies and biophysical techniques to show that the extracellular cell wall sheaths encasing the methanogenic archaea Methanosaeta thermophila PT are functional amyloids. Depolymerization of sheaths and subsequent MS/MS analyses revealed that the sheaths are composed of a single major sheath protein (MspA). The amyloidogenic nature of MspA was confirmed by in vitro amyloid formation of recombinant MspA under a wide range of environmental conditions. This is the first report of a functional amyloid from the archaeal domain of life. The amyloid nature explains the extreme resistance of the sheath, the elastic properties that allow diffusible substrates to penetrate through expandable hoop boundaries, and how the sheaths are able to split and elongate outside the cell. The archaeal sheath amyloids do not share homology with any of the currently known functional amyloids and clearly represent a new function of the amyloid protein fold. © 2015 by The American Society for Biochemistry and Molecular Biology, Inc.

  11. Corrosion and biofouling resistance evaluation of 90-10 copper-nickel

    Energy Technology Data Exchange (ETDEWEB)

    Powell, Carol [Consultant to Copper Development Association, UK, Square Covert, Caynham, Ludlow, Shropshire (United Kingdom)

    2004-07-01

    Copper-nickel alloys for marine use were developed for naval applications in the early part of the 20. century with a view to improving the corrosion resistance of condenser tubes and seawater piping. They still enjoy widespread use today not only for many navies but also in commercial shipping, floating production, storage and off loading vessels (FPSOs), and in multistage flash desalination. The two popular alloys contain 90% or 70% copper and differ in strength and maximum sea water velocity levels they can handle but it is the 90-10 copper-nickel (CuNi10Fe1Mn) which is the more economic and extensively used. An additional benefit of this alloy is its high resistance to biofouling: in recent years this has led to sheathing developments particularly for structures and boat hulls. This paper provides a review of the corrosion and biofouling resistance of 90-10 copper-nickel based on laboratory test data and documented experience of the alloy in marine environments. Particular attention is given to exposure trials over 8 years in Langstone Harbour, UK, which have recently been completed by Portsmouth University on behalf of the Nickel Institute. These examined four sheathing products; plate and foil as well as two composite products with rubber backing. The latter involved copper-nickel granules and slit sheet. The trial results are consistent with the behaviour of the alloy in the overall review. There is an inherent high resistance to marine biofouling when freely exposed. Prolonged exposure to quiet conditions can result in some growth of marine organisms but this is loosely attached and can readily be removed by wiping or a light scraping. The good corrosion resistance of 90-10 copper-nickel in sea water is also confirmed and associated with the formation of a thin, complex, protective and predominantly cuprous oxide surface film, which forms and matures naturally on exposure to seawater. Sound initial oxide film formation is also known to help protect against

  12. Malignant Peripheral Nerve Sheath Tumour of the Maxilla

    Directory of Open Access Journals (Sweden)

    Puja Sahai

    2014-01-01

    Full Text Available A 38-year-old man was diagnosed with malignant peripheral nerve sheath tumour of the maxilla. He was treated with total maxillectomy. Histopathological examination of the resected specimen revealed a close resection margin. The tumour was of high grade with an MIB-1 labelling index of almost 60%. At six weeks following the surgery, he developed local tumour relapse. The patient succumbed to the disease at five months from the time of diagnosis. The present report underlines the locally aggressive nature of malignant peripheral nerve sheath tumour of the maxilla which necessitates an early therapeutic intervention. A complete resection with clear margins is the most important prognostic factor for malignant peripheral nerve sheath tumour in the head and neck region. Adjuvant radiotherapy may be considered to improve the local control. Future research may demarcate the role of targeted therapy for patients with malignant peripheral nerve sheath tumour.

  13. Significance of rice sheath photosynthesis: Yield determination by ...

    African Journals Online (AJOL)

    Using high-yielding hybrid rice Liangyopeijiu (LYP9), its male parent 9311 and hybrid rice Shanyou 63 (SY63) as the experimental materials, the photosynthesis of rice sheath was studied by 14C radio-autography. The results showed that rice sheath could trap sunlight and produce photosynthates, and these ...

  14. Nuclear technology and materials science

    International Nuclear Information System (INIS)

    Olander, D.R.

    1992-01-01

    Current and expected problems in the materials of nuclear technology are reviewed. In the fuel elements of LWRs, cladding waterside corrosion, secondary hydriding and pellet-cladding interaction may be significant impediments to extended burnup. In the fuel, fission gas release remains a key issue. Materials issues in the structural alloys of the primary system include stress-corrosion cracking of steel, corrosion of steam generator tubing and pressurized thermal shock of the reactor vessel. Prediction of core behavior in severe accidents requires basic data and models for fuel liquefaction, aerosol formation, fission product transport and core-concrete interaction. Materials questions in nuclear waste management and fusion technology are briefly reviewed. (author)

  15. Revisiting the plasma sheath—dust in plasma sheath

    Energy Technology Data Exchange (ETDEWEB)

    Das, G. C. [Mathematical Science Division, IASST, Guwahati 781014 (India); Deka, R.; Bora, M. P., E-mail: mpbora@gauhati.ac.in [Physics Department, Gauhati University, Guwahati 781014 (India)

    2016-04-15

    In this work, we have considered the formation of warm plasma sheath in the vicinity of a wall in a plasma with considerable presence of dust particles. As an example, we have used the parameters relevant in case of plasma sheath formed around surfaces of various solid bodies in space, though the results obtained in this work can be applied to any other physical situation such as laboratory plasma. In the ion-acoustic time scale, we neglect the dust dynamics. The dust particles affect the sheath dynamics by affecting the Poisson equation which determines the plasma potential in the sheath region. It is important to note that our calculations are valid only when the amount of dust particles is not sufficient so as to affect the plasma dynamics in the dust-acoustic time scale, but enough to affect the plasma sheath. We have assumed the current to a dust particle to be balanced throughout the analysis. This makes the grain potential dependent on plasma potential, which is then incorporated into the Poisson equation. The resultant numerical model becomes an initial value problem, which is described by a 1-D integro-differential equation, which is then solved self-consistently by incorporating the change in plasma potential caused by inclusion of the dust potential in the Poisson equation.

  16. Sheath-accumulating Propagation of Interplanetary Coronal Mass Ejection

    Energy Technology Data Exchange (ETDEWEB)

    Takahashi, Takuya; Shibata, Kazunari, E-mail: takahasi@kusastro.kyoto-u.ac.jp [Kwasan and Hida Observatories, Kyoto University, Yamashina, Kyoto 607–8471 (Japan)

    2017-03-10

    Fast interplanetary coronal mass ejections (ICMEs) are the drivers of strong space weather storms such as solar energetic particle events and geomagnetic storms. The connection between the space-weather-impacting solar wind disturbances associated with fast ICMEs at Earth and the characteristics of causative energetic CMEs observed near the Sun is a key question in the study of space weather storms, as well as in the development of practical space weather prediction. Such shock-driving fast ICMEs usually expand at supersonic speeds during the propagation, resulting in the continuous accumulation of shocked sheath plasma ahead. In this paper, we propose a “sheath-accumulating propagation” (SAP) model that describes the coevolution of the interplanetary sheath and decelerating ICME ejecta by taking into account the process of upstream solar wind plasma accumulation within the sheath region. Based on the SAP model, we discuss (1) ICME deceleration characteristics; (2) the fundamental condition for fast ICMEs at Earth; (3) the thickness of interplanetary sheaths; (4) arrival time prediction; and (5) the super-intense geomagnetic storms associated with huge solar flares. We quantitatively show that not only the speed but also the mass of the CME are crucial for discussing the above five points. The similarities and differences between the SAP model, the drag-based model, and the“snow-plow” model proposed by Tappin are also discussed.

  17. Sheath-accumulating Propagation of Interplanetary Coronal Mass Ejection

    International Nuclear Information System (INIS)

    Takahashi, Takuya; Shibata, Kazunari

    2017-01-01

    Fast interplanetary coronal mass ejections (ICMEs) are the drivers of strong space weather storms such as solar energetic particle events and geomagnetic storms. The connection between the space-weather-impacting solar wind disturbances associated with fast ICMEs at Earth and the characteristics of causative energetic CMEs observed near the Sun is a key question in the study of space weather storms, as well as in the development of practical space weather prediction. Such shock-driving fast ICMEs usually expand at supersonic speeds during the propagation, resulting in the continuous accumulation of shocked sheath plasma ahead. In this paper, we propose a “sheath-accumulating propagation” (SAP) model that describes the coevolution of the interplanetary sheath and decelerating ICME ejecta by taking into account the process of upstream solar wind plasma accumulation within the sheath region. Based on the SAP model, we discuss (1) ICME deceleration characteristics; (2) the fundamental condition for fast ICMEs at Earth; (3) the thickness of interplanetary sheaths; (4) arrival time prediction; and (5) the super-intense geomagnetic storms associated with huge solar flares. We quantitatively show that not only the speed but also the mass of the CME are crucial for discussing the above five points. The similarities and differences between the SAP model, the drag-based model, and the“snow-plow” model proposed by Tappin are also discussed.

  18. Experimental test of models of radio-frequency plasma sheaths

    International Nuclear Information System (INIS)

    Sobolewski, M.A.

    1997-01-01

    The ion current and sheath impedance were measured at the radio-frequency-powered electrode of an asymmetric, capacitively coupled plasma reactor, for discharges in argon at 1.33 endash 133 Pa. The measurements were used to test the models of the radio frequency sheath derived by Lieberman [IEEE Trans. Plasma Sci. 17, 338 (1989)] and Godyak and Sternberg [Phys. Rev. A 42, 2299 (1990)], and establish the range of pressure and sheath voltage in which they are valid. copyright 1997 American Institute of Physics

  19. Development of laser welded appendages to Zircaloy-4 fuel tubing (sheath/cladding)

    Energy Technology Data Exchange (ETDEWEB)

    Livingstone, S., E-mail: steve.livingstone@cnl.ca [Canadian Nuclear Laboratories Limited, Chalk River, ON, Canada K0J 1J0 (Canada); Xiao, L. [Canadian Nuclear Laboratories Limited, Chalk River, ON, Canada K0J 1J0 (Canada); Corcoran, E.C.; Ferrier, G.A.; Potter, K.N. [Department of Chemistry and Chemical Engineering, Royal Military College of Canada, Kingston, ON, Canada K7K 7B4 (Canada)

    2015-04-01

    Highlights: • Examines feasibility of laser welding appendages to Zr-4 tubing. • Laser welding minimizes the HAZ and removes toxic Be. • Mechanical properties of laser welds appear competitive with induction brazed joints. • Work appears promising and lays the foundation for further investigations. - Abstract: Laser welding is a potential alternative to the induction brazing process commonly used for appendage attachment in CANDU{sup ®} fuel fabrication that uses toxic Be as a filler metal, and creates multiple large heat affected zones in the sheath. For this work, several appendages were laser welded to tubing using different laser heat input settings and then examined with a variety of techniques: visual examination, metallography, shear strength testing, impact testing, and fracture surface analysis. Where possible, the examination results are contrasted against production induction brazed joints. The work to date looks promising for laser welded appendages. Further work on joint optimization, corrosion testing, irradiation testing, and post-irradiation examination will be performed in the future.

  20. Studies on the transmission of sub-THz waves in magnetized inhomogeneous plasma sheath

    Science.gov (United States)

    Yuan, Kai; Shen, Linfang; Yao, Ming; Deng, Xiaohua; Chen, Zhou; Hong, Lujun

    2018-01-01

    There have been many studies on the sub-terahertz (sub-THz) wave transmission in reentry plasma sheaths. However, only some of them have paid attention to the transmission of sub-THz waves in magnetized plasma sheaths. In this paper, the transmission of sub-THz waves in both unmagnetized and magnetized reentry plasma sheaths was investigated. The impacts of temporal evolution of the plasma sheath on the wave transmission were studied. The transmission of "atmospheric window" frequencies in a magnetized plasma sheath was discussed in detail. According to the study, the power transmission rates (Tp) for the left hand circular (LHC) and the right hand circular modes in the magnetized plasma sheath are obviously higher and lower than those in the unmagnetized plasma sheath, respectively. The Tp of LHC mode increases with both wave frequency and external magnetic field strength. Also, the Tp of LHC mode in both magnetized and unmagnetized plasma sheaths varies with time due to the temporal evolution of the plasma sheath. Moreover, the performance of sub-THz waves in magnetized plasma sheath hints at a new approach to the "blackout" problem. The new approach, which is in the capability of modern technology, is to utilize the communication system operating at 140 GHz with an onboard magnet installed near the antenna.

  1. The dust motion inside the magnetized sheath - The effect of drag forces

    International Nuclear Information System (INIS)

    Pandey, B. P.; Samarian, A.; Vladimirov, S. V.

    2010-01-01

    The isolated charged dust inside the magnetized plasma sheath moves under the influence of the electron and ion drag force and the sheath electrostatic field. The charge on the dust is a function of its radius as well as the value of the ambient sheath potential. It is shown that the charge on the dust determines its trajectory and dust performs the spiraling motion inside the sheath. The location of the turning spiral is determined by the number of negative charge on the dust, which in turn is a function of the dust radius. The back and forth spiraling motion finally causes the dust to move in a small, narrow region of the sheath. For a bigger dust particle, the dust moves closer to the sheath presheath boundary suggesting that the bigger grains, owing to the strong repulsion between the wall and dust, will be unable to travel inside the sheath. Only small, micron-sized grains can travel closer to the wall before repulsion pushes it back toward the plasma-sheath boundary. The temporal behavior of the spiraling dust motion appears like a damped harmonic oscillation, suggesting that the plasma drag force causes dissipation of the electrostatic energy. However, after initial damping, the grain keeps oscillating although with much smaller amplitude. The possible application of the present results to the ongoing sheath experiments is discussed.

  2. Fabrication and use of zircaloy/tantalum-sheathed cladding thermocouples and molybdenum/rhenium-sheathed fuel centerline thermocouples

    International Nuclear Information System (INIS)

    Wilkins, S.C.; Sepold, L.K.

    1985-01-01

    The thermocouples described in this report are zircaloy/tantalum-sheathed and molybdenum/rhenium alloy-sheathed instruments intended for fuel rod cladding and fuel centerline temperature measurements, respectively. Both types incorporate beryllium oxide insulation and tungsten/rhenium alloy thermoelements. These thermocouples, operated at temperatures of 2000 0 C and above, were developed for use in the internationally sponsored Severe Fuel Damage test series in the Power Burst Facility. The fabrication steps for both thermocouple types are described in detail. A laser-welding attachment technique for the cladding-type thermocouple is presented, and experience with alternate materials for cladding and fuel therocouples is discussed

  3. An investigation of tendon sheathing filler migration into concrete

    International Nuclear Information System (INIS)

    Naus, D.J.; Oland, C.B.

    1998-03-01

    During some of the inspections at nuclear power plants with prestressed concrete containments, it was observed that the containments has experienced leakage of the tendon sheathing filler (i.e., streaks). The objective of this activity was to provide an indication of the extent of tendon sheathing filler leakage into the concrete and its affects on concrete properties. Literature was reviewed and concrete core samples were obtained from the Trojan Nuclear Plant and tested. The literature primarily addressed effects of crude or lubricating oils that are known to cause concrete damage. However, these materials have significantly different characteristics relative to the materials used as tendon sheathing fillers. Examination and testing of the concrete cores indicated that the appearance of tendon sheathing filler on the concrete surface was due to leakage from the conduits and its subsequent migration through cracks that were present. Migration of the tendon sheathing filler was confined to the cracks and there was no perceptible movement into the concrete. Results of compressive strength testing indicated that the concrete quality was consistent in the containment and that the strength had increased over 40% in 25.4 years relative to the average compressive strength at 28-days age

  4. Structural Conservation of the Myoviridae Phage Tail Sheath Protein Fold

    Energy Technology Data Exchange (ETDEWEB)

    Aksyuk, Anastasia A.; Kurochkina, Lidia P.; Fokine, Andrei; Forouhar, Farhad; Mesyanzhinov, Vadim V.; Tong, Liang; Rossmann, Michael G. (SOIBC); (Purdue); (Columbia)

    2012-02-21

    Bacteriophage phiKZ is a giant phage that infects Pseudomonas aeruginosa, a human pathogen. The phiKZ virion consists of a 1450 {angstrom} diameter icosahedral head and a 2000 {angstrom}-long contractile tail. The structure of the whole virus was previously reported, showing that its tail organization in the extended state is similar to the well-studied Myovirus bacteriophage T4 tail. The crystal structure of a tail sheath protein fragment of phiKZ was determined to 2.4 {angstrom} resolution. Furthermore, crystal structures of two prophage tail sheath proteins were determined to 1.9 and 3.3 {angstrom} resolution. Despite low sequence identity between these proteins, all of these structures have a similar fold. The crystal structure of the phiKZ tail sheath protein has been fitted into cryo-electron-microscopy reconstructions of the extended tail sheath and of a polysheath. The structural rearrangement of the phiKZ tail sheath contraction was found to be similar to that of phage T4.

  5. ICME-driven sheath regions deplete the outer radiation belt electrons

    Science.gov (United States)

    Hietala, H.; Kilpua, E. K.; Turner, D. L.

    2013-12-01

    It is an outstanding question in space weather and solar wind-magnetosphere interaction studies, why some storms result in an increase of the outer radiation belt electron fluxes, while others deplete them or produce no change. One approach to this problem is to look at differences in the storm drivers. Traditionally drivers have been classified to Stream Interaction Regions (SIRs) and Interplanetary Coronal Mass Ejections (ICMEs). However, an 'ICME event' is a complex structure: The core is a magnetic cloud (MC; a clear flux rope structure). If the mass ejection is fast enough, it can drive a shock in front of it. This leads to the formation of a sheath region between the interplanetary shock and the leading edge of the MC. While both the sheath and the MC feature elevated solar wind speed, their other properties are very different. For instance, the sheath region has typically a much higher dynamic pressure than the magnetic cloud. Moreover, the sheath region has a high power in magnetic field and dynamic pressure Ultra Low Frequency (ULF) range fluctuations, while the MC is characterised by an extremely smooth magnetic field. Magnetic clouds have been recognised as important drivers magnetospheric activity since they can comprise long periods of very large southward Interplanetary Magnetic Field (IMF). Nevertheless, previous studies have shown that sheath regions can also act as storm drivers. In this study, we analyse the effects of ICME-driven sheath regions on the relativistic electron fluxes observed by GOES satellites on the geostationary orbit. We perform a superposed epoch analysis of 31 sheath regions from solar cycle 23. Our results show that the sheaths cause an approximately one order of magnitude decrease in the 24h-averaged electron fluxes. Typically the fluxes also stay below the pre-event level for more than two days. Further analysis reveals that the decrease does not depend on, e.g., whether the sheath interval contains predominantly northward

  6. Electric sheath and presheath in a collisionless, finite ion temperature plasma

    International Nuclear Information System (INIS)

    Emmert, G.A.; Wieland, R.M.; Mense, A.T.; Davidson, J.N.

    1980-01-01

    The plasma-sheath equation for a collisionless plasma with arbitrary ion temperature in plane geometry is formulated. Outside the sheath, this equation is approximated by the plasma equation, for which an analytic solution for the electrostatic potential is obtained. In addition, the ion distribution function, the wall potential, and the ion energy and particle flux into the sheath are explicitly calculated. The plasma-sheath equation is also solved numerically with no approximation of the Debye length. The numerical results compare well with the analytical results when the Debye length is small

  7. Atomic Structure of Type VI Contractile Sheath from Pseudomonas aeruginosa.

    Science.gov (United States)

    Salih, Osman; He, Shaoda; Planamente, Sara; Stach, Lasse; MacDonald, James T; Manoli, Eleni; Scheres, Sjors H W; Filloux, Alain; Freemont, Paul S

    2018-02-06

    Pseudomonas aeruginosa has three type VI secretion systems (T6SSs), H1-, H2-, and H3-T6SS, each belonging to a distinct group. The two T6SS components, TssB/VipA and TssC/VipB, assemble to form tubules that conserve structural/functional homology with tail sheaths of contractile bacteriophages and pyocins. Here, we used cryoelectron microscopy to solve the structure of the H1-T6SS P. aeruginosa TssB1C1 sheath at 3.3 Å resolution. Our structure allowed us to resolve some features of the T6SS sheath that were not resolved in the Vibrio cholerae VipAB and Francisella tularensis IglAB structures. Comparison with sheath structures from other contractile machines, including T4 phage and R-type pyocins, provides a better understanding of how these systems have conserved similar functions/mechanisms despite evolution. We used the P. aeruginosa R2 pyocin as a structural template to build an atomic model of the TssB1C1 sheath in its extended conformation, allowing us to propose a coiled-spring-like mechanism for T6SS sheath contraction. Copyright © 2017 The Authors. Published by Elsevier Ltd.. All rights reserved.

  8. SHEATHING URANIUM

    Science.gov (United States)

    Colbeck, E.W.

    1959-02-01

    A method is deseribed for forming a conveniently handled corrosion resistant U articlc comprising pouring molten U into an open-ended corrosion resistant metal eontainer such as Cu and its alloys, Al, or austenitic Ni stainless steel. The exposed surface of the cast U is covered with a metallic packing material such as a brazing flux consisting of Al-Si alloy. The container is sealed iii contact with substantially the entire exposed surface of the packing material. The article is then worked mechanically to reduce the cross section. l3651 A thorium--carbon alloy containing 0.1 to 0.5% by weight carbon, whieh is more resistant to water corrosion than pure thorium metal is presented. The alloy is prepared by fusing thorium metal with the desired amount of carbon at a temperature of about 1850 C. It is found that the carbon is present in the alloy as thorium monocarbide

  9. Review of zircaloy oxidation

    Energy Technology Data Exchange (ETDEWEB)

    Iglesias, F.C. [Royal Military College of Canada, Kingston, Ontario (Canada); Lewis, B.J. [Univ. of Ontario Inst. of Technology, Faculty of Energy Systems and Nuclear Science, Oshawa, Ontario (Canada)

    2013-07-01

    This paper provides an overview of the kinetics for Zircaloy clad oxidation behaviour in steam and air during reactor accident conditions. The generation of chemical heat from metal/water reaction is considered. The effect of internal clad oxidation due to Zircaloy/UO{sub 2} interaction is also discussed. Low-temperature oxidation of Zircaloy due to water-side corrosion is further described. (author)

  10. Gene Expression Profiling of the Intact Dermal Sheath Cup of Human Hair Follicles.

    Science.gov (United States)

    Niiyama, Shiro; Ishimatsu-Tsuji, Yumiko; Nakazawa, Yosuke; Yoshida, Yuzo; Soma, Tsutomu; Ideta, Ritsuro; Mukai, Hideki; Kishimoto, Jiro

    2018-04-24

    Cells that constitute the dermal papillae of hair follicles might be derived from the dermal sheath, the peribulbar component of which is the dermal sheath cup. The dermal sheath cup is thought to include the progenitor cells of the dermal papillae and possesses hair inductive potential; however, it has not yet been well characterized. This study investigated the gene expression profile of the intact dermal sheath cup, and identified dermal sheath cup signature genes, including extracellular matrix components and BMP-binding molecules, as well as TGF-b1 as an upstream regulator. Among these, GREM2, a member of the BMP antagonists, was found by in situ hybridization to be highly specific to the dermal sheath cup, implying that GREM2 is a key molecule contributing to maintenance of the properties of the dermal sheath cup.

  11. Compression test of cold-formedsteel perforated profile with steel sheathing

    Directory of Open Access Journals (Sweden)

    Shamanin Aleksandr Yur’evich

    2015-05-01

    Full Text Available The subject of this paper is the stability and strength of cold-formed and perforated steel sigma-section columns with steel sheathing of different thickness. Ceilings with and without steel sheathing of different thickness are tested to failure in compression on a laboratory machine, which was based on a manual hydraulic jack. Series of 4 experiments with full-scale walls (2.5 m height were carried out. Also, for examination of the role of boundary conditions, the sheet in a ceiling is either left free or connected to base with screws.In civil engineering there are many experiments and methodologies for calculating the strength and buckling of ceiling with the sheathing of various materials, such as oriented strand board and gypsum board. However, for producing superstructures of ships the materials with high plastic properties and strength characteristics are required. For example steel possesses such properties. It was the main reason for conducting a series of experiments and studying the behavior of cold-formed steel columns with steel sheathing. During the experiments the deformation of the cross-section of three equally spaced cross sections was determined, as well as the axial deformation of the central column in the ceiling with steel sheathing.The test results showed the influence of the thickness of sheathing and boundary condition of a sheet on the strength and buckling of ceiling. According to the results of the tests it is necessary to evaluate the impact of the sheathing made of different materials and if necessary to carry out further tests.

  12. Dictionary corrosion and corrosion control

    International Nuclear Information System (INIS)

    1985-01-01

    This dictionary has 13000 entries in both languages. Keywords and extensive accompanying information simplify the choice of word for the user. The following topics are covered: Theoretical principles of corrosion; Corrosion of the metals and alloys most frequently used in engineering. Types of corrosion - (chemical-, electro-chemical, biological corrosion); forms of corrosion (superficial, pitting, selective, intercrystalline and stress corrosion; vibrational corrosion cracking); erosion and cavitation. Methods of corrosion control (material selection, temporary corrosion protection media, paint and plastics coatings, electro-chemical coatings, corrosion prevention by treatment of the corrosive media); Corrosion testing methods. (orig./HP) [de

  13. Hot temperature corrosion of a zircon-1%niobium alloy

    International Nuclear Information System (INIS)

    Muller, Sebastian; Lanzani, Liliana

    2010-01-01

    The reaction of the Zr-1%Niobium alloy to corrosion is studied in this work, which is used as fuel elements sheath material in Russian VVER reactors. For comparative purposes, the conventional alloys Zircaloy-4 y Zr-2.5%Nb have been tested as well. Autoclave tests were carried out in water and in solutions of LiOH with concentrations of 0-1 to 1M at 343 o C and in water vapor at 400 o C (following ASTM G2/G2M-06). The gain in weight/unit of area of the autoclaved samples was determined in order to evaluate the corrosion, and metallographics were performed to characterize the oxides and hydrides that formed. The results show that for tests of 16 hours, a minimum concentration of 0.65M LiOH is needed to accelerate corrosion in Zr-1%Nb and Zr-2.5%Nb, while acceleration occurs in Zircaloy-4 at a concentration of 0.45M. In solutions of LiOH 1M the hydrogen 'uptake' in Zr-1Nb and Zr-2,5Nb is considerably lower in Zircaloy-4. The lesser amount of β-Zr phase present in the Zr-1Nb alloy produces thinner and more compact oxides, with better visual characteristics than for those formed in Zr-2.5Nb

  14. Sheath rendezvous method: a novel distal protection technique during endovascular treatment of subclavian artery occlusions.

    Science.gov (United States)

    Haraguchi, Takuya; Urasawa, Kazushi; Nakama, Tatsuya; Nakagawa, Yuya; Tan, Michinao; Koshida, Ryoji; Sato, Katsuhiko

    2016-10-01

    To describe an innovative distal protection technique, "sheath rendezvous method", during endovascular treatment for subclavian arterial occlusions. 4.5F and 6F guiding sheath were inserted from left brachial and common femoral artery, respectively. 0.014″ guidewire retrogradely passed through occlusion and into antegrade sheath to establish a pull-through system. 3.0 mm balloon was used to expand occlusion and anchor to deliver retrograde sheath into antegrade one. Both sheaths locked by balloon dilatation crossed occlusion until antegrade sheath passed over lesion. Balloon expandable stent was delivered within antegrade sheath. Sheath was removed, and stent was implanted. We obtained an excellent outcome without complications.

  15. Ultrasonographic findings of pilar sheath acanthoma: A case report

    Energy Technology Data Exchange (ETDEWEB)

    Kang, Dong Joo; Lee, Sun Joo; Kim, Seong Jin [Inje University College of Medicine, Busan Paik Hospital, Busan (Korea, Republic of)

    2017-08-15

    Pilar sheath acanthoma is a rare benign follicular hamartoma that presents with a central sinus containing keratinous material and is lined by epithelium. It typically occurs on the face, especially on the upper lip and forehead. In our case, the ultrasound (US) feature of pilar sheath acanthoma revealed a well-defined, oval hypoechoic nodule with hypoechoic capping within the dermis over the medial aspect of the calf. To the best of our knowledge, despite many reports on the clinicopathological aspects of pilar sheath acanthoma, this entity has not been well described in the radiologic literature, and US findings have not been documented.

  16. Benign and malignant neurogenic tumors of nerve sheath origin on FDG PET

    International Nuclear Information System (INIS)

    Yun, M. J.; Go, D. H.; Yoo, Y. H.; Shin, K. H.; Lee, J. D

    2004-01-01

    The differentiation between benign and malignant nerve sheath tumors is difficult based on conventional radiological imaging. This study was undertaken to investigate the value of FDG PET in distinguishing benign from malignant neurogenic tumors of nerve sheath origin. We performed a retrospective review of the medical record to select patients with nerve sheath tumors who had underdone FDG PET imaging. Fifteen patients (7F: 8M) with benign or malignant nerve sheath tumors were included in this study. Of the 15 patients, 9 were diagnosed with the known neurofibromatosis type I. A total of 19 nerve sheath tumors were included from the 15 patients. All patients had undergone FDG PET to evaluate for malignant potential of the known lesions. Images of FDG PET were semi-quantitatively analyzed and a region of interest (ROI) was placed over the area of the maximum FDG uptake and an average standardized uptake value was taken for final analysis. There were 5 malignant peripheral nerve sheath tumors, 5 schwannomas, and 9 neurofibromas. The mean SUV was 2 (ranged from 1.6 to 3.3) for schwannomas, 1.3 (0.7 to 2.5) for neurofibromas, and 8.4 (4.6 to 12.2) for malignant peripheral nerve sheath tumors. Of 14 benign tumors, all except one schwannoma showed a SUV less than 3. When a cutoff SUV of 4 was used to differentiate the nerve sheath tumors, all tumors were correctly classified as benign or malignant, respectively. Among the 9 patients diagnosed with neurofibromatosis type I. 4 had malignant peripheral nerve sheath tumors and FDG PET accurately detected all the 4 lesions with malignant transformation. According to our results, FDG PET seems to have a great potential for accurately characterizing benign versus malignant nerve sheath tumors. It appears to be extremely useful for patients with neurofibromatosis to localize the lesion with malignant transformation

  17. Bilateral giant cell tumor of tendon sheath of tendoachilles

    Directory of Open Access Journals (Sweden)

    Soma Datta

    2014-01-01

    Full Text Available Giant cell tumor of tendon sheath arises from the synovium of tendon sheaths, joints, or bursae, mostly affects adults between 30 and 50 years of age, and is slightly more common in females. We report the case of a 32-years-old male presenting with pain in both ankles without any history of trauma. On clinical examination, tenderness on both tendoachilles and local thickening were observed. Ultrasonography showed thickening of local tendinous area with increase in anteroposterior diameter, and Doppler demonstrated increased flow in peritendinous area. MRI findings showed that most of the tumor had intermediate signal intensity and portions of the tumor had low signal intensity. Fine needle aspiration cytology confirmed the diagnosis of giant cell tumor of tendon sheath. Excision biopsy was done with no recurrence on five month follow-up. Review of literature did not reveal any similar result; so, bilateral giant cell tumor of tendon sheath of tendoachilles is a rare presentation.

  18. Measure Guideline: Guidance on Taped Insulating Sheathing Drainage Planes

    Energy Technology Data Exchange (ETDEWEB)

    Grin, A. [Building Science Corporation, Somerville, MA (United States); Lstiburek, J. [Building Science Corporation, Somerville, MA (United States)

    2014-09-01

    The goal of this research is to provide durable and long-term water management solutions using exterior insulating sheathing as part of the water management system. It is possible to tape or seal the joints in insulating sheathing to create a drainage plane and even an air control layer. There exists the material durability component of the tape as well as the system durability component being the taped insulating sheathing as the drainage plane. This measure guideline provides best practice and product recommendations from the interviewed contractors and homebuilders who collectively have a vast amount of experience. Three significant issues were discussed with the group, which are required to make taped insulating sheathing a simple, long-term, and durable drainage plane: horizontal joints should be limited or eliminated wherever possible; where a horizontal joint exists use superior materials; and frequent installation inspection and regular trade training are required to maintain proper installation.

  19. Synovial sarcoma mimicking benign peripheral nerve sheath tumor

    Energy Technology Data Exchange (ETDEWEB)

    Larque, Ana B.; Nielsen, G.P.; Chebib, Ivan [Massachusetts General Hospital and Harvard Medical School, Department of Pathology, Boston, MA (United States); Bredella, Miriam A. [Massachusetts General Hospital and Harvard Medical School, Department of Radiology, Boston, MA (United States)

    2017-11-15

    To assess the radiographic and clinicopathologic features of synovial sarcoma of the nerve that were clinically or radiologically interpreted as benign peripheral nerve sheath tumor. Five patients with synovial sarcoma arising from the peripheral nerve and interpreted clinically and radiologically as peripheral nerve sheath tumors were identified. Clinicopathologic and imaging features were evaluated. There were three females and two males, ranging in age from 28 to 50 (mean 35.8) years. Most patients (4/5) complained of a mass, discomfort or pain. MR images demonstrated a heterogeneous, enhancing, soft tissue mass contiguous with the neurovascular bundle. On histologic examination, most tumors were monophasic synovial sarcoma (4/5). At the time of surgery, all tumors were noted to arise along or within a peripheral nerve. All patients were alive with no evidence of disease with median follow-up of 44 (range 32-237) months. For comparison, approximately 775 benign peripheral nerve sheath tumors of the extremities were identified during the same time period. Primary synovial sarcoma of the nerve can mimic peripheral nerve sheath tumors clinically and on imaging and should be included in the differential diagnosis for tumors arising from peripheral nerves. (orig.)

  20. Properties of plasma sheath with ion temperature in magnetic fusion devices

    International Nuclear Information System (INIS)

    Liu Jinyuan; Wang Feng; Sun Jizhong

    2011-01-01

    The plasma sheath properties in a strong magnetic field are investigated in this work using a steady state two-fluid model. The motion of ions is affected heavily by the strong magnetic field in fusion devices; meanwhile, the effect of ion temperature cannot be neglected for the plasma in such devices. A criterion for the plasma sheath in a strong magnetic field, which differs from the well-known Bohm criterion for low temperature plasma sheath, is established theoretically with a fluid model. The fluid model is then solved numerically to obtain detailed sheath information under different ion temperatures, plasma densities, and magnetic field strengths.

  1. Plasma sheath axial phase dynamics in coaxial device

    Energy Technology Data Exchange (ETDEWEB)

    Soliman, H.M. (Plasma Physics Dept., NRC, Atomic Energy Authority, Cairo (Egypt)); Masoud, M.M. (Plasma Physics Dept., NRC, Atomic Energy Authority, Cairo (Egypt))

    1994-10-01

    The study of the plasma sheath dynamics in the axial phase has been carried out in a 3 kJ coaxial system of Mather type for two different inner electrode (IE) lengths, 20 cm and 31.5 cm. For both lengths, measurements showed that the plasma sheath is splitted into two layers at the breech, which is referred to as a shock front and its magnetic piston. It has been found that the two layers of the plasma current sheath rotate around the inner electrode. At the muzzle the back layer reverse its rotation direction due to the magnetic field structure of the system. Results showed that the axial velocity of the first layer is greater than the second one all over the axial phase within the range between 1.4 and 1.7. (orig.).

  2. Plasma sheath axial phase dynamics in coaxial device

    International Nuclear Information System (INIS)

    Soliman, H.M.; Masoud, M.M.

    1994-01-01

    The study of the plasma sheath dynamics in the axial phase has been carried out in a 3 kJ coaxial system of Mather type for two different inner electrode (IE) lengths, 20 cm and 31.5 cm. For both lengths, measurements showed that the plasma sheath is splitted into two layers at the breech, which is referred to as a shock front and its magnetic piston. It has been found that the two layers of the plasma current sheath rotate around the inner electrode. At the muzzle the back layer reverse its rotation direction due to the magnetic field structure of the system. Results showed that the axial velocity of the first layer is greater than the second one all over the axial phase within the range between 1.4 and 1.7. (orig.)

  3. Optic Nerve Sheath Mechanics in VIIP Syndrome

    Science.gov (United States)

    Raykin, Julia; Forte, Taylor E.; Wang, Roy; Feola, Andrew; Samuels, Brian; Myers, Jerry; Nelson, Emily; Gleason, Rudy; Ethier, C. Ross

    2016-01-01

    Visual Impairment Intracranial Pressure (VIIP) syndrome is a major concern in current space medicine research. While the exact pathology of VIIP is not yet known, it is hypothesized that the microgravity-induced cephalad fluid shift increases intracranial pressure (ICP) and drives remodeling of the optic nerve sheath. To investigate this possibility, we are culturing optic nerve sheath dura mater samples under different pressures and investigating changes in tissue composition. To interpret results from this work, it is essential to first understand the biomechanical response of the optic nerve sheath dura mater to loading. Here, we investigated the effects of mechanical loading on the porcine optic nerve sheath.Porcine optic nerves (number: 6) were obtained immediately after death from a local abattoir. The optic nerve sheath (dura mater) was isolated from the optic nerve proper, leaving a hollow cylinder of connective tissue that was used for biomechanical characterization. We developed a custom mechanical testing system that allowed for unconfined lengthening, twisting, and circumferential distension of the dura mater during inflation and under fixed axial loading. To determine the effects of variations in ICP, the sample was inflated (0-60 millimeters Hg) and circumferential distension was simultaneously recorded. These tests were performed under variable axial loads (0.6 grams - 5.6 grams at increments of 1 gram) by attaching different weights to one end of the dura mater. Results and Conclusions: The samples demonstrated nonlinear behavior, similar to other soft connective tissue (Figure 1). Large increases in diameter were observed at lower transmural pressures (approximately 0 to 5 millimeters Hg), whereas only small diameter changes were observed at higher pressures. Particularly interesting was the existence of a cross-over point at a pressure of approximately 11 millimeters Hg. At this pressure, the same diameter is obtained for all axial loads applied

  4. Malignant peripheral nerve sheath tumour of the bladder associated with neurofibromatosis I.

    LENUS (Irish Health Repository)

    O'Brien, Julie

    2008-12-01

    Neurofibromatosis is a hamartomatous disorder of autonomic peripheral nerve sheaths associated with peripheral nerve sheath tumours. Most tumours are neurofibromas; however, the genitourinary system is rarely involved. We present a rare case of a nerve sheath tumour of the bladder in a young patient, which was discovered to be malignant.

  5. Review of power ramp irradiations with different pellet L/D ratios and thicknesses of CANLUB layers

    International Nuclear Information System (INIS)

    2009-01-01

    Power ramps in fuel during normal operation can result in Stress Corrosion Cracking (SCC) failures. Experimental evidence shows that pellets with smaller L/D ratios produce smaller circumferential ridges at pellet interface, the location where power ramps failures commonly occur. This may reduce the power ramp damage to the sheath, thereby improving the ability of the fuel sheath to withstand SCC. CANLUB coatings have demonstrated beneficial effects with respect to SCC. It is speculated that the coating acts as a chemical barrier by interacts with the corrosive fission products reducing the amount of corrosive species to reach susceptible areas of the sheath surface. This reduced concentration of corrosive products may enable the sheath to resist higher levels of incremental stresses/strains and therefore survive severe power-ramps. This work focuses on the review of experimental information that substantiates the effect of pellets with lower L/D ratios and thicker CANLUB layers on SCC sheath failures. (author)

  6. AC losses of single-core MgB{sub 2} wires with different metallic sheaths

    Energy Technology Data Exchange (ETDEWEB)

    Kováč, J., E-mail: elekjkov@savba.sk; Šouc, J.; Kováč, P.; Hušek, I.

    2015-12-15

    Highlights: • AC losses in single-core MgB{sub 2} wires with different metallic sheaths have been measured. • It has been shown that metallic sheath can affect the measured AC loss considerably. • GlidCop and Stainless Steel have negligible effect to the overall loss. • Strong contribution of eddy currents has been found in the wire with well conductive copper sheath. • Due to Monel sheath AC loss of MgB{sub 2} core is not visible. - Abstract: AC losses of single-core MgB{sub 2} superconductors with different metallic sheaths (Cu, GlidCop, stainless steel and Monel) have been measured and analyzed. These wires were exposed to external magnetic field with frequencies 72 and 144 Hz and amplitudes up to 0.1 T at temperatures ranged from 18 to 40 K. The obtained results have shown that applied metallic sheath can affect the measured AC loss considerably. In the case of GlidCop and Stainless Steel a negligible small effect of metallic sheath was observed. Strong contribution of eddy currents has been found in the wire with well conductive copper sheath. In the case of Monel sheath, the hysteresis loss of magnetic sheath is dominated and AC loss of MgB{sub 2} core is practically not visible.

  7. Multimodal imaging in neurofibromatosis type 1-associated nerve sheath tumors

    International Nuclear Information System (INIS)

    Salamon, J.; Adam, G.; Mautner, V.F.; Derlin, T.

    2015-01-01

    Neurofibromatosis type 1 (NF1) is a neurogenetic disorder. Individuals with NF1 may develop a variety of benign and malignant tumors of which peripheral nerve sheath tumors represent the most frequent entity. Plexiform neurofibromas may demonstrate a locally destructive growth pattern, may cause severe symptoms and may undergo malignant transformation into malignant peripheral nerve sheath tumors (MPNSTs). Whole-body magnetic resonance imaging (MRI) represents the reference standard for detection of soft tissue tumors in NF1. It allows for identification of individuals with plexiform neurofibromas, for assessment of local tumor extent, and for evaluation of whole-body tumor burden on T2-weighted imaging. Multiparametric MRI may provide a comprehensive characterization of different tissue properties of peripheral nerve sheath tumors, and may identify parameters associated with malignant transformation. Due to the absence of any radiation exposure, whole-body MRI may be used for serial follow-up of individuals with plexiform neurofibromas. 18 F-fluorodeoxyglucose positron-emission-tomography (FDG PET/CT) allows a highly sensitive and specific detection of MPNST, and should be used in case of potential malignant transformation of a peripheral nerve sheath tumor. PET/CT provides a sensitive whole-body tumor staging. The use of contrast-enhanced CT for diagnosis of peripheral nerve sheath tumors is limited to special indications. To obtain the most precise readings, optimized examination protocols and dedicated radiologists and nuclear medicine physicians familiar with the complex and variable morphologies of peripheral nerve sheath tumors are required.

  8. File list: His.Neu.50.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available His.Neu.50.AllAg.Nerve_Sheath_Neoplasms mm9 Histone Neural Nerve Sheath Neoplasms h...ttp://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/His.Neu.50.AllAg.Nerve_Sheath_Neoplasms.bed ...

  9. File list: His.Neu.05.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available His.Neu.05.AllAg.Nerve_Sheath_Neoplasms mm9 Histone Neural Nerve Sheath Neoplasms h...ttp://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/His.Neu.05.AllAg.Nerve_Sheath_Neoplasms.bed ...

  10. File list: DNS.Neu.10.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available DNS.Neu.10.AllAg.Nerve_Sheath_Neoplasms mm9 DNase-seq Neural Nerve Sheath Neoplasms... http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/DNS.Neu.10.AllAg.Nerve_Sheath_Neoplasms.bed ...

  11. File list: Unc.Neu.50.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Unc.Neu.50.AllAg.Nerve_Sheath_Neoplasms mm9 Unclassified Neural Nerve Sheath Neopla...sms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Unc.Neu.50.AllAg.Nerve_Sheath_Neoplasms.bed ...

  12. File list: DNS.Neu.05.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available DNS.Neu.05.AllAg.Nerve_Sheath_Neoplasms mm9 DNase-seq Neural Nerve Sheath Neoplasms... http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/DNS.Neu.05.AllAg.Nerve_Sheath_Neoplasms.bed ...

  13. File list: Unc.Neu.05.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Unc.Neu.05.AllAg.Nerve_Sheath_Neoplasms mm9 Unclassified Neural Nerve Sheath Neopla...sms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Unc.Neu.05.AllAg.Nerve_Sheath_Neoplasms.bed ...

  14. File list: DNS.Neu.50.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available DNS.Neu.50.AllAg.Nerve_Sheath_Neoplasms mm9 DNase-seq Neural Nerve Sheath Neoplasms... http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/DNS.Neu.50.AllAg.Nerve_Sheath_Neoplasms.bed ...

  15. File list: DNS.Neu.20.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available DNS.Neu.20.AllAg.Nerve_Sheath_Neoplasms mm9 DNase-seq Neural Nerve Sheath Neoplasms... http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/DNS.Neu.20.AllAg.Nerve_Sheath_Neoplasms.bed ...

  16. File list: His.Neu.20.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available His.Neu.20.AllAg.Nerve_Sheath_Neoplasms mm9 Histone Neural Nerve Sheath Neoplasms h...ttp://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/His.Neu.20.AllAg.Nerve_Sheath_Neoplasms.bed ...

  17. File list: Unc.Neu.20.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Unc.Neu.20.AllAg.Nerve_Sheath_Neoplasms mm9 Unclassified Neural Nerve Sheath Neopla...sms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Unc.Neu.20.AllAg.Nerve_Sheath_Neoplasms.bed ...

  18. File list: His.Neu.10.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available His.Neu.10.AllAg.Nerve_Sheath_Neoplasms mm9 Histone Neural Nerve Sheath Neoplasms h...ttp://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/His.Neu.10.AllAg.Nerve_Sheath_Neoplasms.bed ...

  19. Contrast material filling of the peroneal tendon sheath

    International Nuclear Information System (INIS)

    Zadravecz, Gy.; Grexa, E.

    1981-01-01

    In case of complaints after fracture of the calcaneus the common sheath of the peroneus tendons was filled up with contrast material. The tendon sheath was punctured Oehind the external ankle. The three-directional radiograms clearly showed the dislocation and compression of the tendons, caused by the exostosis of the calcaneus. The concomitant tendovaginitis caused the complaints. This alteration was observed in 11% of all the calcaneus fractures. (L.E.)

  20. File list: Pol.Neu.50.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Pol.Neu.50.AllAg.Nerve_Sheath_Neoplasms mm9 RNA polymerase Neural Nerve Sheath Neop...lasms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Pol.Neu.50.AllAg.Nerve_Sheath_Neoplasms.bed ...

  1. File list: Pol.Neu.20.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Pol.Neu.20.AllAg.Nerve_Sheath_Neoplasms mm9 RNA polymerase Neural Nerve Sheath Neop...lasms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Pol.Neu.20.AllAg.Nerve_Sheath_Neoplasms.bed ...

  2. File list: Pol.Neu.10.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Pol.Neu.10.AllAg.Nerve_Sheath_Neoplasms mm9 RNA polymerase Neural Nerve Sheath Neop...lasms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Pol.Neu.10.AllAg.Nerve_Sheath_Neoplasms.bed ...

  3. File list: Pol.Neu.05.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Pol.Neu.05.AllAg.Nerve_Sheath_Neoplasms mm9 RNA polymerase Neural Nerve Sheath Neop...lasms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Pol.Neu.05.AllAg.Nerve_Sheath_Neoplasms.bed ...

  4. Verification of high voltage rf capacitive sheath models with particle-in-cell simulations

    Science.gov (United States)

    Wang, Ying; Lieberman, Michael; Verboncoeur, John

    2009-10-01

    Collisionless and collisional high voltage rf capacitive sheath models were developed in the late 1980's [1]. Given the external parameters of a single-frequency capacitively coupled discharge, plasma parameters including sheath width, electron and ion temperature, plasma density, power, and ion bombarding energy can be estimated. One-dimensional electrostatic PIC codes XPDP1 [2] and OOPD1 [3] are used to investigate plasma behaviors within rf sheaths and bulk plasma. Electron-neutral collisions only are considered for collisionless sheaths, while ion-neutral collisions are taken into account for collisional sheaths. The collisionless sheath model is verified very well by PIC simulations for the rf current-driven and voltage-driven cases. Results will be reported for collisional sheaths also. [1] M. A. Lieberman, IEEE Trans. Plasma Sci. 16 (1988) 638; 17 (1989) 338 [2] J. P. Verboncoeur, M. V. Alves, V. Vahedi, and C. K. Birdsall, J. Comp. Phys. 104 (1993) 321 [3] J. P. Verboncoeur, A. B. Langdon and N. T. Gladd, Comp. Phys. Comm. 87 (1995) 199

  5. Evaluation of the Effusion within Biceps Long Head Tendon Sheath Using Ultrasonography

    Science.gov (United States)

    Park, In; Lee, Hyo-Jin; Kim, Sung-Eun; Bae, Sung-Ho; Lee, Kwang-Yeol; Park, Kwang-Sun

    2015-01-01

    Background Many shoulder diseases are related to glenohumeral joint synovitis and effusion. The purpose of the present study is to detect effusion within the biceps long head tendon sheath as the sign of glenohumeral joint synovitis using ultrasonography, and to evaluate the clinical meaning of effusion within the biceps long head tendon sheath. Methods A consecutive series of 569 patients who underwent ultrasonography for shoulder pain were reviewed retrospectively and ultimately, 303 patients were included. The authors evaluated the incidence and amount of the effusion within the biceps long head tendon sheath on the ultrasonographic short axis view. Furthermore, the authors evaluated the correlation between the amount of effusion within the biceps long head tendon sheath and the range of motion and the functional score. Results The effusion within the biceps long head tendon sheath was detected in 58.42% of the patients studied: 69.23% in adhesive capsulitis, 56.69% in rotator cuff tear, 41.03% in calcific tendinitis, and 33.33% in biceps tendinitis. The average amount of the effusion within the biceps long head tendon sheath was 1.7 ± 1.6 mm, and it was measured to be the largest in adhesive capsulitis. The amount of effusion within biceps long head tendon sheath showed a moderate to high degree of correlation with the range of motion, and a low degree of correlation with the functional score and visual analogue scale for pain in each type of shoulder disease. Conclusions The effusion within the biceps long head tendon sheath is closely related to the range of motion and clinical scores in patients with painful shoulders. Ultrasonographic detection of the effusion within the biceps long head tendon sheath might be a simple and easy method to evaluate shoulder function. PMID:26330958

  6. Design of Cold-Formed Steel Screw Connections with Gypsum Sheathing at Ambient and Elevated Temperatures

    Directory of Open Access Journals (Sweden)

    Wei Chen

    2016-09-01

    Full Text Available Load-bearing cold-formed steel (CFS walls sheathed with double layers of gypsum plasterboard on both sides have demonstrated good fire resistance and attracted increasing interest for use in mid-rise CFS structures. As the main connection method, screw connections between CFS and gypsum sheathing play an important role in both the structural design and fire resistance of this wall system. However, studies on the mechanical behavior of screw connections with double-layer gypsum sheathing are still limited. In this study, 200 monotonic tests of screw connections with single- or double-layer gypsum sheathing at both ambient and elevated temperatures were conducted. The failure of screw connections with double-layer gypsum sheathing in shear was different from that of single-layer gypsum sheathing connections at ambient temperature, and it could be described as the breaking of the loaded sheathing edge combined with significant screw tilting and the loaded sheathing edge flexing fracture. However, the screw tilting and flexing fracture of the loaded sheathing edge gradually disappear at elevated temperatures. In addition, the influence of the loaded edge distance, double-layer sheathing and elevated temperatures is discussed in detail with clear conclusions. A unified design formula for the shear strength of screw connections with gypsum sheathing is proposed for ambient and elevated temperatures with adequate accuracy. A simplified load–displacement model with the post-peak branch is developed to evaluate the load–displacement response of screw connections with gypsum sheathing at ambient and elevated temperatures.

  7. Embedded cladding surface thermocouples on Zircaloy-sheathed heater rods

    International Nuclear Information System (INIS)

    Wilkins, S.C.

    1977-06-01

    Titanium-sheathed Type K thermocouples embedded in the cladding wall of zircaloy-sheathed heater rods are described. These thermocouples constitute part of a program intended to characterize the uncertainty of measurements made by surface-mounted cladding thermocouples on nuclear fuel rods. Fabrication and installation detail, and laboratory testing of sample thermocouple installations are included

  8. File list: ALL.Neu.50.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available ALL.Neu.50.AllAg.Nerve_Sheath_Neoplasms mm9 All antigens Neural Nerve Sheath Neopla...sms SRX337965 http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/ALL.Neu.50.AllAg.Nerve_Sheath_Neoplasms.bed ...

  9. File list: Oth.Neu.05.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Oth.Neu.05.AllAg.Nerve_Sheath_Neoplasms mm9 TFs and others Neural Nerve Sheath Neop...lasms SRX337965 http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Oth.Neu.05.AllAg.Nerve_Sheath_Neoplasms.bed ...

  10. File list: Oth.Neu.50.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Oth.Neu.50.AllAg.Nerve_Sheath_Neoplasms mm9 TFs and others Neural Nerve Sheath Neop...lasms SRX337965 http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Oth.Neu.50.AllAg.Nerve_Sheath_Neoplasms.bed ...

  11. File list: Oth.Neu.20.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Oth.Neu.20.AllAg.Nerve_Sheath_Neoplasms mm9 TFs and others Neural Nerve Sheath Neop...lasms SRX337965 http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Oth.Neu.20.AllAg.Nerve_Sheath_Neoplasms.bed ...

  12. File list: ALL.Neu.20.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available ALL.Neu.20.AllAg.Nerve_Sheath_Neoplasms mm9 All antigens Neural Nerve Sheath Neopla...sms SRX337965 http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/ALL.Neu.20.AllAg.Nerve_Sheath_Neoplasms.bed ...

  13. File list: Oth.Neu.10.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available Oth.Neu.10.AllAg.Nerve_Sheath_Neoplasms mm9 TFs and others Neural Nerve Sheath Neop...lasms SRX337965 http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/Oth.Neu.10.AllAg.Nerve_Sheath_Neoplasms.bed ...

  14. File list: ALL.Neu.10.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available ALL.Neu.10.AllAg.Nerve_Sheath_Neoplasms mm9 All antigens Neural Nerve Sheath Neopla...sms SRX337965 http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/ALL.Neu.10.AllAg.Nerve_Sheath_Neoplasms.bed ...

  15. File list: ALL.Neu.05.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available ALL.Neu.05.AllAg.Nerve_Sheath_Neoplasms mm9 All antigens Neural Nerve Sheath Neopla...sms SRX337965 http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/ALL.Neu.05.AllAg.Nerve_Sheath_Neoplasms.bed ...

  16. On the upper bound in the Bohm sheath criterion

    Energy Technology Data Exchange (ETDEWEB)

    Kotelnikov, I. A., E-mail: I.A.Kotelnikov@inp.nsk.su; Skovorodin, D. I., E-mail: D.I.Skovorodin@inp.nsk.su [Russian Academy of Sciences, Budker Institute of Nuclear Physics, Siberian Branch (Russian Federation)

    2016-02-15

    The question is discussed about the existence of an upper bound in the Bohm sheath criterion, according to which the Debye sheath at the interface between plasma and a negatively charged electrode is stable only if the ion flow velocity in plasma exceeds the ion sound velocity. It is stated that, with an exception of some artificial ionization models, the Bohm sheath criterion is satisfied as an equality at the lower bound and the ion flow velocity is equal to the speed of sound. In the one-dimensional theory, a supersonic flow appears in an unrealistic model of a localized ion source the size of which is less than the Debye length; however, supersonic flows seem to be possible in the two- and three-dimensional cases. In the available numerical codes used to simulate charged particle sources with a plasma emitter, the presence of the upper bound in the Bohm sheath criterion is not supposed; however, the correspondence with experimental data is usually achieved if the ion flow velocity in plasma is close to the ion sound velocity.

  17. Spontaneous rectus sheath hematoma: The utility of CT angiography

    Directory of Open Access Journals (Sweden)

    Antonio Pierro, MD

    2018-04-01

    Full Text Available We described the utility of computed tomography (CT angiography in detection of bleeding vessels for a rapid percutaneous arterial embolization of the spontaneous rectus sheath hematoma. A 70-year-old woman comes to our attention with acute abdominal pain and a low hemoglobin level. An unenhanced CT was performed demonstrating a large rectus sheath hematoma. A conservative management was initially established. Despite this therapy, the abdominal pain increased together with a further decrease of hemoglobin values. A CT angiography was then performed, demonstrating an active bleeding within the hematoma and addressing the patient to a rapid percutaneous arterial embolization. Keywords: Rectus sheath hematoma, Acute abdomen, Arterial embolization, CT angiography, Active bleeding

  18. Slow-wave propagation and sheath interaction in the ion-cyclotron frequency range

    International Nuclear Information System (INIS)

    Myra, J R; D'Ippolito, D A

    2010-01-01

    In previous work (Myra J R and D'Ippolito D A 2008 Phys. Rev. Lett. 101 195004) we studied the propagation of slow-wave (SW) resonance cones launched parasitically by a fast-wave antenna into a tenuous magnetized plasma. Here we extend the treatment of SW propagation and sheath interaction to 'dense' scrape-off-layer plasmas where the usual cold-plasma SW is evanescent. Using the sheath boundary condition, it is shown that for sufficiently close limiters, the SW couples to a sheath-plasma wave and is no longer evanescent, but radially propagating. A self-consistent calculation of the rf-sheath width yields the resulting sheath voltage in terms of the amplitude of the launched SW, plasma parameters and connection length. The conditions for avoiding potentially deleterious rf-wall interactions in tokamak rf heating experiments are summarized.

  19. Comparison of a fuel sheath failure model with published experimental data

    International Nuclear Information System (INIS)

    Varty, R.L.; Rosinger, H.E.

    1982-01-01

    A fuel sheath failure model has been compared with the published results of experiments in which a Zircaloy-4 fuel sheath was subjected to a temperature ramp and a differential pressure until failure occurred. The model assumes that the deformation of the sheath is controlled by steady-state creep and that there is a relationship between tangential stress and temperature at the instant of failure. The sheath failure model predictions agree reasonably well with the experimental data. The burst temperature is slightly overpredicted by the model. The burst strain is overpredicted for small experimental burst strains but is underpredicted otherwise. The reasons for these trends are discussed and the extremely wide variation in burst strain reported in the literature is explained using the model

  20. The collisional capacitive RF sheath and the assumption of a sharp electron edge

    Science.gov (United States)

    Brinkmann, Ralf Peter

    2008-10-01

    The transition from quasi-neutrality to charge depletion is one of the characteristic features of the plasma boundary sheath. It is often described in terms of the so-called step model which assumes a transition point (electron step) where the electron density drops from a value equal to the ion density (in the bulk) to a value of zero (in the sheath). Inserted into Poisson's equation, the step model yields an expression for the field which is realistic deep in the sheath but fails to merge correctly into the ambipolar field of the bulk. This work studies the consequences of that approximation for the example of the collision-dominated, capacitive RF sheath by Lieberman [1]. First, the model is solved exactly, using a relaxation scheme. Then, the step approximation is applied which recovers Lieberman's semi-analytical solution. It is demonstrated that the step approximation induces a spurious divergence of the ion density at the sheath edge and prevents a matching of the sheath model to a bulk model. Integral sheath quantities, on the other hand, like the capacitance or the overall voltage drop, are faithfully reproduced. [1] M. A. Lieberman, IEEE Trans. Plasma Sci. 16, pp. 638-644 (1988).

  1. Theoretical and computational studies of the sheath of a planar wall

    Science.gov (United States)

    Giraudo, Martina; Camporeale, Enrico; Delzanno, Gian Luca; Lapenta, Giovanni

    2012-03-01

    We present an investigation of the stability and nonlinear evolution of the sheath of a planar wall. We focus on the electrostatic limit. The stability analysis is conducted with a fluid model where continuity and momentum equations for the electrons and ions are coupled through Poisson's equation. The effect of electron emission from the wall is studied parametrically. Our results show that a sheath instability associated with the emitted electrons can exist. Following Ref. [1], it is interpreted as a Rayleigh-Taylor instability driven by the favorable combination of the sheath electron density gradient and electric field. Fully kinetic Particle-In-Cell (PIC) simulations will also be presented to investigate whether this instability indeed exists and to study the nonlinear effect of electron emission on the sheath profiles. The simulations will be conducted with CPIC, a new electrostatic PIC code that couples the standard PIC algorithm with strategies for generation and adaptation of the computational grid. [4pt] [1] G.L. Delzanno, ``A paradigm for the stability of the plasma sheath against fluid perturbations,'' Phys. Plasmas 18, 103508 (2011).

  2. Dynamics of Dust in a Plasma Sheath with Magnetic Field

    International Nuclear Information System (INIS)

    Duan Ping; Liu Jinyuan; Gon Ye; Liu Yue; Wang Xiaogang

    2007-01-01

    Dynamics of dust in a plasma sheath with a magnetic field was investigated using a single particle model. The result shows that the radius, initial position, initial velocity of the dust particles and the magnetic field do effect their movement and equilibrium position in the plasma sheath. Generally, the dust particles with the same size, whatever original velocity and position they have, will locate at the same position in the end under the net actions of electrostatic, gravitational, neutral collisional, and Lorentz forces. But the dust particles will not locate in the plasma sheath if their radius is beyond a certain value

  3. Coronal mass ejections and their sheath regions in interplanetary space

    Science.gov (United States)

    Kilpua, Emilia; Koskinen, Hannu E. J.; Pulkkinen, Tuija I.

    2017-11-01

    Interplanetary coronal mass ejections (ICMEs) are large-scale heliospheric transients that originate from the Sun. When an ICME is sufficiently faster than the preceding solar wind, a shock wave develops ahead of the ICME. The turbulent region between the shock and the ICME is called the sheath region. ICMEs and their sheaths and shocks are all interesting structures from the fundamental plasma physics viewpoint. They are also key drivers of space weather disturbances in the heliosphere and planetary environments. ICME-driven shock waves can accelerate charged particles to high energies. Sheaths and ICMEs drive practically all intense geospace storms at the Earth, and they can also affect dramatically the planetary radiation environments and atmospheres. This review focuses on the current understanding of observational signatures and properties of ICMEs and the associated sheath regions based on five decades of studies. In addition, we discuss modelling of ICMEs and many fundamental outstanding questions on their origin, evolution and effects, largely due to the limitations of single spacecraft observations of these macro-scale structures. We also present current understanding of space weather consequences of these large-scale solar wind structures, including effects at the other Solar System planets and exoplanets. We specially emphasize the different origin, properties and consequences of the sheaths and ICMEs.

  4. Coronal mass ejections and their sheath regions in interplanetary space

    Directory of Open Access Journals (Sweden)

    Emilia Kilpua

    2017-11-01

    Full Text Available Abstract Interplanetary coronal mass ejections (ICMEs are large-scale heliospheric transients that originate from the Sun. When an ICME is sufficiently faster than the preceding solar wind, a shock wave develops ahead of the ICME. The turbulent region between the shock and the ICME is called the sheath region. ICMEs and their sheaths and shocks are all interesting structures from the fundamental plasma physics viewpoint. They are also key drivers of space weather disturbances in the heliosphere and planetary environments. ICME-driven shock waves can accelerate charged particles to high energies. Sheaths and ICMEs drive practically all intense geospace storms at the Earth, and they can also affect dramatically the planetary radiation environments and atmospheres. This review focuses on the current understanding of observational signatures and properties of ICMEs and the associated sheath regions based on five decades of studies. In addition, we discuss modelling of ICMEs and many fundamental outstanding questions on their origin, evolution and effects, largely due to the limitations of single spacecraft observations of these macro-scale structures. We also present current understanding of space weather consequences of these large-scale solar wind structures, including effects at the other Solar System planets and exoplanets. We specially emphasize the different origin, properties and consequences of the sheaths and ICMEs.

  5. Anode Sheath Switching in a Carbon Nanotube Arc Plasma

    International Nuclear Information System (INIS)

    Fetterman, Abe; Raitses, Yevgeny; Keidar, Michael

    2008-01-01

    The anode ablation rate is investigated as a function of anode diameter for a carbon nanotube arc plasma. It is found that anomalously high ablation occurs for small anode diameters. This result is explained by the formation of a positive anode sheath. The increased ablation rate due to this positive anode sheath could imply greater production rate for carbon nanotubes.

  6. Hot corrosion of the steel SA213-T22 and SA213-TP347H in 80% V2O5-20%Na2SO4 mixture

    International Nuclear Information System (INIS)

    Almeraya, F.; Martinez-Villafane, A.; Gaona, C.; Romero, M.A.; Malo, J.M.

    1998-01-01

    Many hot corrosion problems in industrial and utility boilers are caused by molten salts. The corrosion processes which occur in salts are of an electrochemical nature, and so they can be studied using electrochemical test methods. In this research, electrochemical techniques in molten salt systems have been used for the measurements of molten corrosion processes. Electrochemical test methods are described here for a salt mixture of 80%V 2 O 5 -20%NaSO 4 at 540-680 degree centigrade. To establish better the electrochemical corrosion rate measurements for molten salt systems, information from electrochemical potentiodynamic polarization curves, such as polarization resistance and Tafeol slopes were used in this study to generate corrosion rate data. The salt was contained in a quartz crucible inside a stainless retort. The atmosphere used was air. A thermocouple sheathed with quartz glass was introduced into the molten salt for temperature monitoring and control. Two materials were tested in the molten mixture: SA213-T22 and SA213-TP347H steels. The corrosion rates values obtained using electrochemical methods were around 0.58-7.14 mm/yr (22.9-281 mpy). The corrosion rate increase with time. (Author) 7 refs

  7. Corrosion and corrosion control

    International Nuclear Information System (INIS)

    Khanna, A.S.; Totlani, M.K.

    1995-01-01

    Corrosion has always been associated with structures, plants, installations and equipment exposed to aggressive environments. It effects economy, safety and product reliability. Monitoring of component corrosion has thus become an essential requirement for the plant health and safety. Protection methods such as appropriate coatings, cathodic protection and use of inhibitors have become essential design parameters. High temperature corrosion, especially hot corrosion, is still a difficult concept to accommodate in corrosion allowance; there is a lack of harmonized system of performance testing of materials at high temperatures. In order to discuss and deliberate on these aspects, National Association for Corrosion Engineers International organised a National Conference on Corrosion and its Control in Bombay during November 28-30, 1995. This volume contains papers presented at the symposium. Paper relevant to INIS is indexed separately. refs., figs., tabs

  8. Fibroma of the tendon sheath of the long head of the biceps tendon

    International Nuclear Information System (INIS)

    Maeseneer, Michel de; Shahabpour, Maryam; Isacker, Tom van; Lenchik, Leon; Caillie, Marie-Astrid van

    2014-01-01

    Fibroma of the tendon sheath is a benign tumor that is less common than giant cell tumor of the tendon sheath. Both tumors may present as a painless, slowly enlarging mass. Radiological findings may be similar for both tumors. Histologically, fibroma of the tendon sheath lacks the hemosiderin-laden macrophages that are typical for giant cell tumor of the tendon sheath. We report on a 49-year-old woman with fibroma of the tendon sheath of the long head of the biceps tendon. In our case, on MR images, we observed band-like hypointense areas centrally in the tumor, mild patchy contrast enhancement, and most importantly, no decrease of signal intensity on gradient echo images. These characteristics reflected histological findings. (orig.)

  9. The anatomy of the first sacral nerve root sheath shown by computed tomography.

    Science.gov (United States)

    Moore, N R; Dixon, A K; Freer, C E

    1989-08-01

    Analysis of 25 patients with normal computed tomographic appearances at the lumbosacral junction revealed wide variation in the anatomical level at which the first sacral nerve root sheaths were seen emerging from the theca. In nine patients (36%), the S1 nerve root sheaths were first recognized at the level of the lumbosacral disc. In 14 patients (56%), the sheaths emerged cranial to the disc; it is possible that these patients may be more prone to neurological complications related to disc or facet joint disease, especially if the sheath is laterally sited within the lateral recess. Conversely, that minority of patients (two, 8%) in whom the root sheaths emerge caudal to the disc level may be relatively protected from neurological complications.

  10. Effects of Reentry Plasma Sheath on GPS Patch Antenna Polarization Property

    Directory of Open Access Journals (Sweden)

    L. Zhao

    2013-01-01

    Full Text Available A plasma sheath enveloping a reentry vehicle would affect performances of on-board antenna greatly, especially the navigation antennas. This paper studies the effects of reentry plasma sheath on a GPS right-hand circularly polarized (RHCP patch antenna polarization property during a typical reentry process. Utilizing the algorithm of finite integration technique, the polarization characteristic of a GPS antenna coated by a plasma sheath is obtained. Results show that the GPS RHCP patch antenna radiation pattern distortions as well as polarization deteriorations exist during the entire reentry process, and the worst polarization mismatch loss between a GPS antenna and RHCP GPS signal is nearly 3 dB. This paper also indicates that measures should be taken to alleviate the plasma sheath for maintaining the GPS communication during the reentry process.

  11. Internal pressure effects in the AIRCO-LCT conductor sheath

    International Nuclear Information System (INIS)

    Luton, J.N.; Clinard, J.A.; Lue, J.W.; Gray, W.H.; Summers, L.T.; Kershaw, R.

    1985-01-01

    The large Nb 3 Sn superconducting test coil produced by Westinghouse Electric Corporation for the international Large Coil Task (LCT) utilizes a conductor composed of cabled multifilamentary strands immersed in flowing supercritical helium contained by a square structural sheath made of the high-strength stainless alloy JBX-75. Peak pressures of a few hundred atmospheres are predicted to occur during quench, and measurement of these pressures seems feasible only through penetrations of the sheath wall. Fully processed short lengths of conductor were taken from production ends, fitted with pressure taps and strain gauges, and pressurized with helium gas. Failure, at 1000 atm at liquid nitrogen temperature, was by a catastrophic splitting of the sheath at a corner. Strain measurements and burst pressure agreed with elastic-plastic finite element stress calculations made for the sheath alone. Neither the production seam weld nor the pressure tap penetrations or their fillet welds contributed to the failure, although the finite element calculations show that these areas were also highly stressed, and examination of the failed sample showed that the finite welds were of poor quality. Failure was by tensile overload, with no evidence of fatigue

  12. Hertwig’s Epithelial Root Sheath Fate during Initial Cellular Cementogenesis in Rat Molars

    International Nuclear Information System (INIS)

    Yamamoto, Tsuneyuki; Yamada, Tamaki; Yamamoto, Tomomaya; Hasegawa, Tomoka; Hongo, Hiromi; Oda, Kimimitsu; Amizuka, Norio

    2015-01-01

    To elucidate the fate of the epithelial root sheath during initial cellular cementogenesis, we examined developing maxillary first molars of rats by immunohistochemistry for keratin, vimentin, and tissue non-specific alkaline phosphatase (TNALP) and by TdT-mediated dUTP nick end labeling (TUNEL). The advancing root end was divided into three sections, which follow three distinct stages of initial cellular cementogenesis: section 1, where the epithelial sheath is intact; section 2, where the epithelial sheath becomes fragmented; and section 3, where initial cellular cementogenesis begins. After fragmentation of the epithelial sheath, many keratin-positive epithelial sheath cells were embedded in the rapidly growing cellular cementum. A few unembedded epithelial cells located on the cementum surface. Dental follicle cells, precementoblasts, and cementoblasts showed immunoreactivity for vimentin and TNALP. In all three sections, there were virtually no cells possessing double immunoreactivity for vimentin-keratin or TNALP-keratin and only embedded epithelial cells showed TUNEL reactivity. Taken together, these findings suggest that: (1) epithelial sheath cells divide into two groups; one group is embedded in the cementum and thereafter dies by apoptosis, and the other survives on the cementum surface as epithelial cell rests of Malassez; and (2) epithelial sheath cells do not undergo epithelial-mesenchymal transition during initial cellular cementogenesis

  13. Balloon sheaths for gastrointestinal guidance and access: a preliminary phantom study

    International Nuclear Information System (INIS)

    He, Xu; Shin, Ji Hoon; Kim, Hyo Cheol; Woo, Cheol Woong; Woo, Sung Ha; Choi, Won Chan; Kim, Jong Gyu; Lim, Jin Oh; Kim, Tae Hyung; Yoon, Chang Jin; Song, Ho Young; Kang, Wee Chang

    2005-01-01

    We wanted to evaluate the feasibility and usefulness of a newly designed balloon sheath for gastrointestinal guidance and access by conducting a phantom study. The newly designed balloon sheath consisted of an introducer sheath and a supporting balloon. A coil catheter was advanced over a guide wire into two gastroduodenal phantoms (one was with stricture and one was without stricture); group I was without a balloon sheath, group II was with a deflated balloon sheath, and groups III and IV were with an inflated balloon and with the balloon in the fundus and body, respectively. Each test was performed for 2 minutes and it was repeated 10 times in each group by two researchers, and the positions reached by the catheter tip were recorded. Both researchers had better performances with both phantoms in order of group IV, III, II and I. In group IV, both researchers advanced the catheter tip through the fourth duodenal segment in both the phantoms. In group I, however, the catheter tip never reached the third duodenal segment in both the phantoms by both the researchers. The numeric values for the four study groups were significantly different for both the phantoms (ρ < 0.001). A significant difference was also found between group III and IV for both phantoms (ρ < 0.001). The balloon sheath seems to be feasible for clinical use, and it has good clinical potential for gastrointestinal guidance and access, particularly when the inflated balloon is placed in the gastric body

  14. Ontogeny of the sheathing leaf base in maize (Zea mays).

    Science.gov (United States)

    Johnston, Robyn; Leiboff, Samuel; Scanlon, Michael J

    2015-01-01

    Leaves develop from the shoot apical meristem (SAM) via recruitment of leaf founder cells. Unlike eudicots, most monocot leaves display parallel venation and sheathing bases wherein the margins overlap the stem. Here we utilized computed tomography (CT) imaging, localization of PIN-FORMED1 (PIN1) auxin transport proteins, and in situ hybridization of leaf developmental transcripts to analyze the ontogeny of monocot leaf morphology in maize (Zea mays). CT imaging of whole-mounted shoot apices illustrates the plastochron-specific stages during initiation of the basal sheath margins from the tubular disc of insertion (DOI). PIN1 localizations identify basipetal auxin transport in the SAM L1 layer at the site of leaf initiation, a process that continues reiteratively during later recruitment of lateral leaf domains. Refinement of these auxin transport domains results in multiple, parallel provascular strands within the initiating primordium. By contrast, auxin is transported from the L2 toward the L1 at the developing margins of the leaf sheath. Transcripts involved in organ boundary formation and dorsiventral patterning accumulate within the DOI, preceding the outgrowth of the overlapping margins of the sheathing leaf base. We suggest a model wherein sheathing bases and parallel veins are both patterned via the extended recruitment of lateral maize leaf domains from the SAM. © 2014 The Authors. New Phytologist © 2014 New Phytologist Trust.

  15. File list: NoD.Neu.05.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available NoD.Neu.05.AllAg.Nerve_Sheath_Neoplasms mm9 No description Neural Nerve Sheath Neop...lasms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/NoD.Neu.05.AllAg.Nerve_Sheath_Neoplasms.bed ...

  16. File list: InP.Neu.10.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available InP.Neu.10.AllAg.Nerve_Sheath_Neoplasms mm9 Input control Neural Nerve Sheath Neopl...asms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/InP.Neu.10.AllAg.Nerve_Sheath_Neoplasms.bed ...

  17. File list: NoD.Neu.50.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available NoD.Neu.50.AllAg.Nerve_Sheath_Neoplasms mm9 No description Neural Nerve Sheath Neop...lasms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/NoD.Neu.50.AllAg.Nerve_Sheath_Neoplasms.bed ...

  18. File list: InP.Neu.05.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available InP.Neu.05.AllAg.Nerve_Sheath_Neoplasms mm9 Input control Neural Nerve Sheath Neopl...asms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/InP.Neu.05.AllAg.Nerve_Sheath_Neoplasms.bed ...

  19. File list: InP.Neu.20.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available InP.Neu.20.AllAg.Nerve_Sheath_Neoplasms mm9 Input control Neural Nerve Sheath Neopl...asms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/InP.Neu.20.AllAg.Nerve_Sheath_Neoplasms.bed ...

  20. File list: NoD.Neu.10.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available NoD.Neu.10.AllAg.Nerve_Sheath_Neoplasms mm9 No description Neural Nerve Sheath Neop...lasms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/NoD.Neu.10.AllAg.Nerve_Sheath_Neoplasms.bed ...

  1. File list: InP.Neu.50.AllAg.Nerve_Sheath_Neoplasms [Chip-atlas[Archive

    Lifescience Database Archive (English)

    Full Text Available InP.Neu.50.AllAg.Nerve_Sheath_Neoplasms mm9 Input control Neural Nerve Sheath Neopl...asms http://dbarchive.biosciencedbc.jp/kyushu-u/mm9/assembled/InP.Neu.50.AllAg.Nerve_Sheath_Neoplasms.bed ...

  2. The Tubular Sheaths Encasing Methanosaeta and Methanospirillum Filaments are Functional Amyloids

    DEFF Research Database (Denmark)

    Dueholm, Morten Simonsen; Larsen, Poul; Nielsen, Per Halkjær

    Archaea are well-recognized for their ability to thrive in extreme environments, although they can be found in virtually all habitats. Their adaptive success is linked to their unique cell envelopes, which often display extremely resistant to chemical and thermal denaturation and resist proteolysis...... techniques to show that the extracellular cell wall sheaths of the methanogenic archaea Methanosaeta and Methanospirillum are functional amyloid structures. Depolymerization of sheaths with formic acid and reducing agents and subsequent MS/MS analysis revealed that the sheaths are composed of a single major...... sheath protein (MspA). The amyloidogenic nature of MspA was confirmed by in vitro amyloid formation of recombinant MspA under a wide range of environmental conditions. This is the first report of a functional amyloid from the archaeal domain of life. The amyloid properties explain the extreme resistance...

  3. Selective pH-Responsive Core-Sheath Nanofiber Membranes for Chem/Bio/Med Applications: Targeted Delivery of Functional Molecules.

    Science.gov (United States)

    Han, Daewoo; Steckl, Andrew J

    2017-12-13

    Core-sheath fibers using different Eudragit materials were successfully produced, and their controlled multi-pH responses have been demonstrated. Core-sheath fibers made of Eudragit L 100 (EL100) core and Eudragit S 100 (ES100) sheath provide protection and/or controlled release of core material at pH 6 by adjusting the sheath thickness (controlled by the flow rate of source polymer solution). The thickest sheath (∼250 nm) provides the least core release ∼1.25%/h, while the thinnest sheath (∼140 nm) provides much quicker release ∼16.75%/h. Furthermore, switching core and sheath material dramatically altered the pH response. Core-sheath fibers made of ES100 core and EL100 sheath can provide a consistent core release rate, while the sheath release rate becomes higher as the sheath layer becomes thinner. For example, the thinnest sheath (∼120 nm) provides a core and sheath release ratio of 1:2.5, while the thickest sheath (∼200 nm) shows only a ratio of 1:1.7. All core-sheath Eudragit fibers show no noticeable release at pH 5, while they are completely dissolved at pH 7. Extremely high surface area in the porous network of the fiber membranes provides much faster (>30 times) response to external pH changes as compared to that of equivalent cast films.

  4. Effects of an anode sheath on energy and momentum transfer in vacuum arcs

    International Nuclear Information System (INIS)

    Wang, Zhenxing; Zhou, Zhipeng; Tian, Yunbo; Wang, Haoran; Wang, Jianhua; Geng, Yingsan; Liu, Zhiyuan

    2017-01-01

    Anode phenomena under high-current vacuum arcs have a significant impact on the interrupting capacity of vacuum interrupters. However, the vacuum arc energy flux and momentum flux on the anode—which are necessary boundary conditions for simulations—are either set to an imaginary distribution or calculated using simple formulas without considering anode sheath regulatory effects. The objective of this paper is to reveal the anode sheath effects on regulating the energy and momentum transfer from the arc column to the anode surface in vacuum arcs. A particle-in-cell model for the anode sheath is developed. The required input parameters are obtained from a magnetohydrodynamic model for the arc column. From the results, there exists a sheath near the anode with a negative voltage drop. Both the electron density and the ion density significantly decline in the anode sheath region. The kinetic energy of the ions absorbed by the anode consists of directed kinetic energy, random kinetic energy, and sheath acceleration energy. The sheath acceleration energy contribution is the largest, and the random kinetic energy also accounts for a large part that cannot be ignored. The arc pressure on the anode surface is mainly caused by ion impact, and the accelerating effect of the anode sheath on the ions cannot be neglected in pressure calculations. In addition, in the case of an arc current at 15 kA, the input energy and momentum upon the anode surface is not obviously affected by the evaporated atoms at surface temperatures of 1600 K and 2000 K. (paper)

  5. Can using a peel-away sheath in shunt implantation prevent ventricular catheter obstruction?

    Science.gov (United States)

    Camlar, Mahmut; Ersahin, Yusuf; Ozer, Fusun Demirçivi; Sen, Fatih; Orman, Mehmet

    2011-02-01

    Shunt obstruction is the most common shunt complication. In 2003, Kehler et al. used peel-away sheath while implanting the ventricular catheter in 20 patients. They found less revision rate in the peel-away sheath group. We aimed to test the efficacy of this technique in cadavers. We used 100 fresh brains obtained from medicolegal autopsies. Posterior parietal and frontal approaches were used to puncture the lateral ventricle in each cerebral hemisphere. The ventricle is punctured with a peel-away sheath system. After the ventricle is reached, the mandarin is retracted and the ventricular catheter is introduced through the opening. The ventricular catheter was removed from the ventricle, the opening at the tip of the ventricular catheter was checked out for obstruction, and the number of patent and plugged openings was recorded. This procedure was repeated four times for each location with and without using peel-away sheath. The control group consisted of the procedures done without using peel-away sheath. The number of the plugged openings in the peel-away sheath group was significantly smaller than the control group. There was no significant difference between the two groups in terms of gender and left and right cerebral hemispheres. The obstruction rate was significantly lower in the posterior parietal approach. Pearson's correlation showed that increasing age was associated with less obstruction rate. Peel-away sheath decreases the number of plugged openings of the ventricular catheter. A clinical cooperative study is needed to prove that a peel-away sheath should be included in the ventricular shunt systems in the market.

  6. Slow Wave Propagation and Sheath Interaction for ICRF Waves in the Tokamak SOL

    International Nuclear Information System (INIS)

    Myra, J. R.; D'Ippolito, D. A.

    2009-01-01

    In previous work we studied the propagation of slow-wave resonance cones launched parasitically by a fast-wave antenna into a tenuous magnetized plasma. Here we extend the previous calculation to ''dense'' scrape-off-layer (SOL) plasmas where the usual slow wave is evanescent. Using the sheath boundary condition, it is shown that for sufficiently close limiters, the slow wave couples to a sheath plasma wave and is no longer evanescent, but radially propagating. A self-consistent calculation of the rf-sheath width yields the resulting sheath voltage in terms of the amplitude of the launched SW, plasma parameters and connection length.

  7. Optic Nerve Sheath Meningocele: A Case Report

    Science.gov (United States)

    Halimi, E.; Wavreille, O.; Rosenberg, R.; Bouacha, I.; Lejeune, J.-P.; Defoort-Dhellemmes, S.

    2013-01-01

    Abstract Isolated optic nerve sheath meningocele is a rare affection defined as the cystic enlargement of the optic nerve sheath filled with cerebrospinal fluid. We report the case of a 39-year-old woman presenting with bilateral meningocele uncovered during a routine examination for headache complaints. A 5-year follow-up validated the lesion’s clinical and imaging stability. Magnetic resonance imaging (MRI) is an essential tool in the diagnosis of this pathology, alongside characteristic symptoms indicating that the meningocele might have progressively expanded into the orbit. In this case we present a therapeutic approach based on pathophysiological hypotheses and review of the literature. PMID:28163760

  8. Corrosion of metallic materials. Dry corrosion, aqueous corrosion and corrosion by liquid metal, methods of protection

    International Nuclear Information System (INIS)

    Helie, Max

    2015-01-01

    This book is based on a course on materials given in an engineering school. The author first gives an overview of metallurgy issues: metallic materials (pure metals, metallic alloys), defects of crystal lattices (point defects, linear defects or dislocations), equilibrium diagrams, steels and cast, thermal processing of steels, stainless steels, aluminium and its alloys, copper and its alloys. The second part addresses the properties and characterization of surfaces and interfaces: singularity of a metal surface, surface energy of a metal, energy of grain boundaries, adsorption at a material surface, metal-electrolyte interface, surface oxide-electrolyte interface, techniques of surface analysis. The third chapter addresses the electrochemical aspects of corrosion: description of the corrosion phenomenon, free enthalpy of a compound and free enthalpy of a reaction, case of dry corrosion (thermodynamic aspect, Ellingham diagram, oxidation mechanisms, experimental study, macroscopic modelling), case of aqueous corrosion (electrochemical thermodynamics and kinetics, experimental determination of corrosion rate). The fourth part addresses the different forms of aqueous corrosion: generalized corrosion (atmospheric corrosion, mechanisms and tests), localized corrosion (galvanic, pitting, cracking, intergranular, erosion and cavitation), particular cases of stress cracking (stress corrosion, fatigue-corrosion, embrittlement by hydrogen), and bi-corrosion (of non alloyed steels, of stainless steels, and of aluminium and copper alloys). The sixth chapter addresses the struggle and the protection against aqueous corrosion: methods of prevention, scope of use of main alloys, geometry-based protection of pieces, use of corrosion inhibitors, use of organic or metallic coatings, electrochemical protection. The last chapter proposes an overview of corrosion types in industrial practices: in the automotive industry, in the oil industry, in the aircraft industry, and in the

  9. The relative axial expansions under irradiation of stacks of UO{sub 2} pellets in zircaloy sheaths

    Energy Technology Data Exchange (ETDEWEB)

    Notley, M. J.F.

    1962-08-15

    An experiment was performed to measure the relative axial movement of UO{sub 2} fuel pellets inside a Zircaloy sheath. Although the results must be treated with some reservation, the inferences are that there is very little relative movement between the fuel and the sheath when the two are in firm pressure contact. Relative movement was in the range 0.075 {+-} 0.03 cm for a 30 cm fuel length, and was not greatly affected by the power output, profile of the pellet end-faces or the diametral clearance left between the fuel and the sheath on assembly. However in two elements that had thick sheaths to withstand the coolant pressure and that were assembled with large diametral clearances (2% of the diameter) the available axial clearance for relative fuel/ sheath movement (1%) was fully taken up. The thin sheathed elements showed residual axial expansions of up to 0.17 cm, indicating that the pellets move relative to the sheath only until frictional forces are sufficient for the sheath to grip the fuel; thereafter the sheath is extended. The measurements also indicate that sheath elongation is governed by the temperature at the contact points between adjacent pellets, eg. at the inner edge of a pellet shoulder, as long as that temperature is below approximately 1000{sup o}C. At higher temperatures, the UO{sub 2} is too plastic to exert sufficient force to strain the sheath. (author)

  10. The endomembrane sheath: a key structure for understanding the plant cell?

    Science.gov (United States)

    Reuzeau, C.; McNally, J. G.; Pickard, B. G.

    1997-01-01

    Recent evidence suggests that integrin is abundant in endomembranes of plant cells, and the endomembranes are clad by a sheath of cytoskeleton including F-actin. A role for endomembrane integrin and the endomembrane sheath is proposed: this system might orchestrate metabolic regulation by providing and modulating loci for channelling, and might accelerate channeling as needed by dragging the endoplasmic reticulum (ER) and organelles through the cytoplasm. To accomplish this "streaming", F-actin might lever against the rest of the endomembrane sheath and the ER might also lever against adhesion sites (i.e., plasmodesmata and plasmalemmal control centers). As an important agent in the control of cellular activities, according to this model, the endomembrane sheath would play a major part in responses to diverse signals and stresses, and under extreme stress cell survival would depend on the ability of the system to maintain enough integrity to direct critical syntheses and degradations.

  11. Dust crystal in the electrode sheath of a gaseous discharge

    International Nuclear Information System (INIS)

    Schweigert, I.V.; Schweigert, V.A.

    2002-01-01

    The phenomena observed in strongly coupled dusty plasmas in the electrode sheath of gas discharge clearly indicate that the screened Coulomb potential is not valid for inter-particle interaction. The reason why the conventional model breaks down is clear now. The strong electric field, accelerating ions toward the cathode, leads to an asymmetrical particle shielding and the appearance of an attractive component in the inter-particle force. The sheath plasma with micro-particles is non Hamiltonian system because of input of energy from ion flux from the bulk plasma. The models of interaction potential of microparticles in sheath are proposed. The first is the linear effective positive charge (EPC). On the basis of this model the stability of the dust crystal in the sheath is analyzed both analytically and in MD simulations. The scenario of crystal melting is described. The role of different types of defects in the local heating of the crystal is considered. The next non-linear model of sheath plasma with micro-particles allows to find all parameter of plasma crystal: particle charge, inter-particle distance and study the structural transition. We constructed the analytical expression for inter-particle potential and have found the mechanism acceleration of extra particle beneath the monolayer. Recently new more simple analytical kinetic approach, accounting for ion collisions, have been developed. The structural transition in the dust molecular was obtained in simulation with multipole expansion model interaction potential

  12. Dissociation and Re-Aggregation of Multicell-Ensheathed Fragments Responsible for Rapid Production of Massive Clumps of Leptothrix Sheaths

    Science.gov (United States)

    Kunoh, Tatsuki; Nagaoka, Noriyuki; McFarlane, Ian R.; Tamura, Katsunori; El-Naggar, Mohamed Y.; Kunoh, Hitoshi; Takada, Jun

    2016-01-01

    Species of the Fe/Mn-oxidizing bacteria Leptothrix produce tremendous amounts of microtubular, Fe/Mn-encrusted sheaths within a few days in outwells of groundwater that can rapidly clog water systems. To understand this mode of rapid sheath production and define the timescales involved, behaviors of sheath-forming Leptothrix sp. strain OUMS1 were examined using time-lapse video at the initial stage of sheath formation. OUMS1 formed clumps of tangled sheaths. Electron microscopy confirmed the presence of a thin layer of bacterial exopolymer fibrils around catenulate cells (corresponding to the immature sheath). In time-lapse videos, numerous sheath filaments that extended from the periphery of sheath clumps repeatedly fragmented at the apex of the same fragment, the fragments then aggregated and again elongated, eventually forming a large sheath clump comprising tangled sheaths within two days. In this study, we found that fast microscopic fragmentation, dissociation, re-aggregation and re-elongation events are the basis of the rapid, massive production of Leptothrix sheaths typically observed at macroscopic scales. PMID:27490579

  13. Floating fat in the wrist joint and in the tendon sheaths

    Energy Technology Data Exchange (ETDEWEB)

    Le Corroller, Thomas; Zink, Jean-Vincent; Champsaur, Pierre [Hopital Sainte-Marguerite, Radiology Department, Marseille (France); Parratte, Sebastien; Argenson, Jean-Noel [Hopital Sainte-Marguerite, Orthopaedic Surgery Department, Marseille (France)

    2010-09-15

    A traumatic fat effusion in a tendon sheath is an unreported entity. We report on the clinical and imaging features, including radiography and computed tomography (CT), of a fat-density effusion in the wrist joint and tendon sheaths of the extensor pollicis longus, extensor carpi radialis longus, and extensor carpi radialis brevis in a 28-year-old patient after a roller-skating accident. Radiographs showed a fracture of the distal radius and a wrist joint effusion. Preoperative CT examination exhibited two distinct layers resulting in a fat-fluid level pathognomonic of lipohemarthrosis in the radiocarpal joint. In addition, a fat-density effusion was noted in the sheaths of the second and third compartment extensor tendons. The lipohemarthrosis depicted on imaging classically results from the extrusion of fat from bone marrow into the joint space after an intraarticular fracture. Similarly, a traumatic fat effusion in a tendon sheath presents characteristic imaging features that may help to diagnose a potentially overlooked fracture. (orig.)

  14. Floating fat in the wrist joint and in the tendon sheaths

    International Nuclear Information System (INIS)

    Le Corroller, Thomas; Zink, Jean-Vincent; Champsaur, Pierre; Parratte, Sebastien; Argenson, Jean-Noel

    2010-01-01

    A traumatic fat effusion in a tendon sheath is an unreported entity. We report on the clinical and imaging features, including radiography and computed tomography (CT), of a fat-density effusion in the wrist joint and tendon sheaths of the extensor pollicis longus, extensor carpi radialis longus, and extensor carpi radialis brevis in a 28-year-old patient after a roller-skating accident. Radiographs showed a fracture of the distal radius and a wrist joint effusion. Preoperative CT examination exhibited two distinct layers resulting in a fat-fluid level pathognomonic of lipohemarthrosis in the radiocarpal joint. In addition, a fat-density effusion was noted in the sheaths of the second and third compartment extensor tendons. The lipohemarthrosis depicted on imaging classically results from the extrusion of fat from bone marrow into the joint space after an intraarticular fracture. Similarly, a traumatic fat effusion in a tendon sheath presents characteristic imaging features that may help to diagnose a potentially overlooked fracture. (orig.)

  15. Experimental Studies of Anode Sheath Phenomena in a Hall Thruster Discharge

    International Nuclear Information System (INIS)

    Dorf, L.; Raitses, Y.; Fisch, N.J.

    2004-01-01

    Both electron-repelling and electron-attracting anode sheaths in a Hall thruster were characterized by measuring the plasma potential with biased and emissive probes [L. Dorf, Y. Raitses, V. Semenov, and N.J. Fisch, Appl. Phys. Let. 84 (2004) 1070]. In the present work, two-dimensional structures of the plasma potential, electron temperature, and plasma density in the near-anode region of a Hall thruster with clean and dielectrically coated anodes are identified. Possible mechanisms of anode sheath formation in a Hall thruster are analyzed. The path for current closure to the anode appears to be the determining factor in the anode sheath formation process. The main conclusion of this work is that the anode sheath formation in Hall thrusters differs essentially from that in the other gas discharge devices, like a glow discharge or a hollow anode, because the Hall thruster utilizes long electron residence times to ionize rather than high neutral pressures

  16. Anomalous Capacitive Sheath with Deep Radio Frequency Electric Field Penetration

    International Nuclear Information System (INIS)

    Kaganovich, Igor D.

    2002-01-01

    A novel nonlinear effect of anomalously deep penetration of an external radio-frequency electric field into a plasma is described. A self-consistent kinetic treatment reveals a transition region between the sheath and the plasma. Because of the electron velocity modulation in the sheath, bunches in the energetic electron density are formed in the transition region adjusted to the sheath. The width of the region is of order V(subscript T)/omega, where V(subscript T) is the electron thermal velocity, and w is frequency of the electric field. The presence of the electric field in the transition region results in a cooling of the energetic electrons and an additional heating of the cold electrons in comparison with the case when the transition region is neglected

  17. Electric fields in the sheath formed in a 300 mm, dual frequency capacitive argon discharge

    International Nuclear Information System (INIS)

    Barnat, E V; Miller, P A; Hebner, G A; Paterson, A M; Panagopoulos, T; Hammond, E; Holland, J

    2007-01-01

    The spatial structure and temporal evolution of the electric fields in a sheath formed in a dual frequency, 300 mm capacitive argon discharge are measured as functions of relative mixing between a low frequency current and a high frequency current. It is found that the overall structure of the sheath (potential across the sheath and the thickness of the sheath) are dominated by the lower frequency component while (smaller) oscillations in these quantities are dictated by the higher frequency component. Comparisons of the measured spatial and temporal profiles are made for Lieberman's and Robiche et al sheath model and with a particle in a cell calculation

  18. 30 CFR 15.32 - Tolerances for weight of explosive, sheath, wrapper, and specific gravity.

    Science.gov (United States)

    2010-07-01

    ..., wrapper, and specific gravity. 15.32 Section 15.32 Mineral Resources MINE SAFETY AND HEALTH ADMINISTRATION... explosive, sheath, wrapper, and specific gravity. (a) The weight of the explosive, the sheath, and the outer.... (c) The specific gravity of the explosive and sheath shall be within ±7.5 percent of that specified...

  19. Effect of electron emission on an ion sheath structure

    International Nuclear Information System (INIS)

    Mishra, M K; Phukan, A; Chakraborty, M

    2014-01-01

    This article reports on the variations of ion sheath structures due to the emission of both hot and cold electrons in the target plasma region of a double plasma device. The ion sheath is produced in front of a negatively biased plate. The plasma is produced by hot filament discharge in the source region, and no discharge is created in the target region of the device. The plate is placed in the target (diffused plasma) region where cold electron emitting filaments are present. These cold electrons are free from maintenance of discharge, which is sustained in the source region. The hot ionizing electrons are present in the source region. Three important parameters are changed by both hot and cold electrons i.e. plasma density, plasma potential and electron temperature. The decrease in plasma potential and the increase in plasma density lead to the contraction of the sheath. (paper)

  20. Accounting for Debye sheath expansion for proud Langmuir probes in magnetic confinement fusion plasmas.

    Science.gov (United States)

    Tsui, C K; Boedo, J A; Stangeby, P C

    2018-01-01

    A Child-Langmuir law-based method for accounting for Debye sheath expansion while fitting the current-voltage I-V characteristic of proud Langmuir probes (electrodes that extend into the volume of the plasma) is described. For Langmuir probes of a typical size used in tokamak plasmas, these new estimates of electron temperature and ion saturation current density values decreased by up to 60% compared to methods that did not account for sheath expansion. Changes to the collection area are modeled using the Child-Langmuir law and effective expansion perimeter l p , and the model is thus referred to as the "perimeter sheath expansion method." l p is determined solely from electrode geometry, so the method may be employed without prior measurement of the magnitude of the sheath expansion effects for a given Langmuir probe and can be used for electrodes of different geometries. This method correctly predicts the non-saturating ΔI/ΔV slope for cold, low-density plasmas where sheath-expansion effects are strong, as well as for hot plasmas where ΔI/ΔV ∼ 0, though it is shown that the sheath can still significantly affect the collection area in these hot conditions. The perimeter sheath expansion method has several advantages compared to methods where the non-saturating current is fitted: (1) It is more resilient to scatter in the I-V characteristics observed in turbulent plasmas. (2) It is able to separate the contributions to the ΔI/ΔV slope from sheath expansion to that of the high energy electron tail in high Te conditions. (3) It calculates the change in the collection area due to the Debye sheath for conditions where ΔI/ΔV ∼ 0 and for V = V f .

  1. Soil sheaths, photosynthate distribution to roots, and rhizosphere water relations for Opuntia ficus-indica

    Energy Technology Data Exchange (ETDEWEB)

    Huang, B.; North, G.B.; Nobel, P.S. (Univ. of California, Los Angeles, CA (United States))

    1993-09-01

    Soil sheaths incorporating aggregated soil particles surround young roots of many species, but the effects of such sheaths on water movement between roots and the soil are largely unknown. The quantity and location of root exudates associated with soil sheath along the entire length of its young roots, except within 1.4 cm of the tip. The soil sheaths, which average 0.7 mm in thickness, were composed of soil particles and root hairs, both of which were covered with exuded mucilaginous material. As determined with a [sup 14]C pulse-labeling technique, 2% of newly fixed [sup 14]C-photosynthate was translocated into the roots at 3d, 6% at 9 d, and 8% at 15 d after labeling. The fraction of insoluble [sup 14]C in the roots increased twofold from 3 d to 15 d. Over the same time period, 6%-9% of the [sup 14]C translocated to the roots was exuded into the soil. The soluble [sup 14]C compounds exuded into the soil were greater in the 3-cm segment at the root tip than elsewhere along the root, whereas mucilage was exuded relatively uniformly along roots 15 cm in length. The volumetric efflux of water increase for both sheathed and unsheathed roots as the soil water potential decreased form -0.1 MPa to -1.0 MPa. The efflux rate was greater for unsheathed roots than for sheathed roots, which were more turgid and had a higher water potential, especially at lower soil water potentials. During drying, soil particles in the sheaths aggregate more tightly, making the sheaths less permeable to water and possibly creating air gaps. The soil sheaths of O. ficus-indica thus reduce water loss from the roots to a drying soil. 34 refs., 6 figs., 1 tab.

  2. Ion clusters, REB, and current sheath characteristics in focused discharges

    International Nuclear Information System (INIS)

    Bortolotti, A.; Brzosko, J.; DeChiara, P.; Kilic, H.; Mezzetti, F.; Nardi, V.; Powell, C.; Zeng, D.

    1990-01-01

    Small fluctuations in the current sheath characteristics (peak current density, FWHM of leading sheath, control parameters of sheath internal structure) are linked to wide fluctuations of ion and ion cluster emission from the pinch. Magnetic probe data are used for correlating variations of current sheath parameters with particle emission intensity, Z/M composition, particle energy spectrum. The emission of ion and ion clusters at 90 degrees from the axis of a plasma focus discharge is monitored simultaneously with the 0 degrees emission. The particle energy spectrum is analyzed with a Thomson (parabola) spectrometer (time resolution ∼ 1 nanosec). The cross-sectional structure of the REB at 180 degrees along the discharge axis is monitored via the deposition of collective-field accelerated ions on a target in the REB direction. Etched tracks of ion and ion clusters are in all cases recorded on CR-39 plates. Sharp peaks of the D + -ion spectrum at 90 degrees are found for E > 200 keV/unit charge in all focused discharges. These peaks are due to ion crossing of the azimuthal magnetic field of the pinch region, in a predominant ion cluster structure

  3. Influence of vacuum space on formation of potential sheath in plasmas

    International Nuclear Information System (INIS)

    Uhm, H.S.

    1997-01-01

    Properties of potential sheaths developed in plasmas are investigated in terms of the plasma Debye length and the dimension of vacuum space. Biased plasma potential and the potential profile depend very sensitively on the geometrical configuration of plasma and vacuum space. The potential sheath is never developed near electrodes in high-density plasmas where the Debye length is much less than the dimension of the vacuum space. In this case, most of the potential drops occur in the vacuum space and almost no electric field exists inside the plasma. Parametric investigation of the potential sheath in terms of the vacuum-space and plasma dimensions is carried out. (orig.)

  4. Photovoltaic building sheathing element with anti-slide features

    Science.gov (United States)

    Keenihan, James R.; Langmaid, Joseph A.; Lopez, Leonardo C.

    2015-09-08

    The present invention is premised` upon an assembly that includes at least a photovoltaic building sheathing element capable of being affixed on a building structure, the photovoltaic building sheathing element. The element including a photovoltaic cell assembly, a body portion attached to one or more portions of the photovoltaic cell assembly; and at feast a first and a second connector assembly capable of directly or indirectly electrically connecting the photovoltaic cell assembly to one or more adjoining devices; wherein the body portion includes one or more geometric features adapted to engage a vertically adjoining device before installation.

  5. Sheathed electrical resistance heaters for nuclear or other specialized service - approved 1973

    International Nuclear Information System (INIS)

    Anon.

    1976-01-01

    This specification presents the requirements for cylindrical metal-sheathed, electrical resistance heaters with compacted mineral-oxide insulation for nuclear or other specialized service. The intended use of a sheathed heater in a specific nuclear or general application will require an evaluation by the purchaser of the compatibility of the heater assembly in the proposed application including the effects of the integrated proposed application including the effects of the integrated neutron flux, temperature, and atmosphere on the properties of the materials of construction. This specification does not include all possible specifications, standards, etc. for materials that may be used in sheathing, insulation, resistance wire, or conductors wire in nuclear environments. The requirements of this specification include only the austenitic stainless steels and nickel-based alloys for sheathing; magnesium oxide, aluminum oxide, beryllium oxide for insulation; and nickel-chromium or iron-chromium-aluminum heater elements with or without low-resistance connecting wires. The intent of this specification is to present the requirements for heaters capable of operating at sheath temperatures and heat fluxes that will limit the maximum internal heater-element temperature to 1050 0 C

  6. RF-sheath assessment of ICRF antenna geometry for long pulses

    International Nuclear Information System (INIS)

    Colas, L.; Bremond, S.

    2003-01-01

    Monitoring powered ion cyclotron resonance frequency (ICRF) antennas in magnetic fusion devices has revealed localized modifications of the plasma edge in the antenna shadow, most of them probably related to an enhanced polarization of the scrape-off layer (SOL) through radio-frequency (RF) sheath rectification. Although tolerable on present short RF pulses, sheaths should be minimized, as they may hinder proper operation of steady-state antennas and other subsystems connected magnetically to them, such as lower hybrid grills. As a first step towards mitigating RF sheaths in the design of future antennas, the present paper analyses the spatial structure of sheath potential maps in their vicinity, in relation with the 3D topology of RF near fields and the geometry of antenna front faces. Various combinations of poloidal radiating straps are first considered, and results are confronted to those inferred from transmission line theory. The dependence of sheath potentials on RF voltages or RF currents is studied. The role of RF near-field symmetries along tilted field lines is stressed to interpret such effects as that of strap phasing. A generalization of the 'dipole effect' is proposed. With similar arguments, the behavior of Faraday screen corners, where hot spots concentrate on Tore-Supra (TS), is then studied. The merits of aligning the antenna structure with the tilted magnetic field are thus discussed. The effect of switching from TS (high RF voltage near corners) to ITER-like electrical configurations of the straps (high voltage near equatorial plane) is also analyzed. (authors)

  7. Levitation and dynamics of a collection of dust particles in a fully ionized plasma sheath

    International Nuclear Information System (INIS)

    Nitter, T.; Aslaksen, T.K.; Melandsoe, F.; Havnes, O.

    1994-01-01

    The authors have examined the dynamics of a collection of charged dust particles in the plasma sheath above a large body in a fully ionized space plasma when the radius of the large body is much larger than the sheath thickness. The dust particles are charged by the plasma, and the forces on the dust particles are assumed to be from the electric field in the sheath and from gravitation only. These forces will often act in opposite direction and may balance, making dust suspension and collection possible. The dust particles are supplied by injection or by electrostatic levitation. The ability of the sheath to collect dust particles, will be optimal for a certain combination of gravitation and plasma and dust particle parameters. In a dense dust sheath, the charges on the dust particles contribute significantly to the total space charge, and collective effects become important. These effects will reduce the magnitude of the sheath electric field strength and the charge on the dust particles. As dust particles are collected, the dust sheath is stretched and the largest dust particles may drop out, because the sheath is no longer able to suspend them. In a tenuous dust sheath, the inner layer, from the surface and about one Debye length thick, will be unstable for dust particle motion, and dust will not collect there. In a dense dust sheath, collective effects will decrease the thickness of this inner dust-free layer, making dust collection closer to the surface possible. By linearization of the force and current equations, they find the necessary and sufficient conditions which resemble those of planetary system bodies, but the results may also be of relevance to some laboratory plasmas

  8. Benign Peripheral Nerve Sheath Tumor in a Wild Toco Toucan ( Ramphastos toco ).

    Science.gov (United States)

    Carvalho, Marcelo P N; Fernandes, Natalia C C A; Nemer, Viviane C; Neto, Ramiro N Dias; Teixeira, Rodrigo H F; Miranda, Bruna S; Mamprim, Maria J; Catão-Dias, José L; Réssio, Rodrigo A

    2016-09-01

    Peripheral nerve sheath tumors are a heterogeneous group of neoplasms that comprise neurofibromas, schwannomas, neurilemmomas, and perineuromas. In animals, peripheral nerve sheath neoplasms are most commonly diagnosed in dogs and cattle, followed by horses, goats, and cats, but their occurrence is uncommon in birds. An adult, free-living, male toco (common) toucan ( Ramphastos toco ) was admitted to the zoo animal clinic with weight loss, dehydration, and presence of a soft nodule adhered to the medial portion of the left pectoral muscle. Clinical, cytologic, and computed tomography scan results were indicative of a neoplasm. The toucan died during surgical resection of the mass. Necropsy, histopathologic, and immunohistochemical findings confirmed the diagnosis of benign peripheral nerve sheath tumor. To our knowledge, benign peripheral nerve sheath tumor has not previously been reported in a toucan or any other species in the order Piciformes.

  9. Anode sheath transition in an anodic arc for synthesis of nanomaterials

    Science.gov (United States)

    Nemchinsky, V. A.; Raitses, Y.

    2016-06-01

    The arc discharge with ablating anode or so-called anodic arc is widely used for synthesis of nanomaterials, including carbon nanotubes and fullerens, metal nanoparticles etc. We present the model of this arc, which confirms the existence of the two different modes of the arc operation with two different anode sheath regimes, namely, with negative anode sheath and with positive anode sheath. It was previously suggested that these regimes are associated with two different anode ablating modes—low ablation mode with constant ablation rate and the enhanced ablation mode (Fetterman et al 2008 Carbon 46 1322). The transition of the arc operation from low ablation mode to high ablation mode is determined by the current density at the anode. The model can be used to self-consistently determine the distribution of the electric field, electron density and electron temperature in the near-anode region of the arc discharge. Simulations of the carbon arc predict that for low arc ablating modes, the current is driven mainly by the electron diffusion to the anode. For positive anode sheath, the anode voltage is close to the ionization potential of anode material, while for negative anode sheath, the anode voltage is an order of magnitude smaller. It is also shown that the near-anode plasma, is far from the ionization equilibrium.

  10. Anode sheath transition in an anodic arc for synthesis of nanomaterials

    International Nuclear Information System (INIS)

    Nemchinsky, V A; Raitses, Y

    2016-01-01

    The arc discharge with ablating anode or so-called anodic arc is widely used for synthesis of nanomaterials, including carbon nanotubes and fullerens, metal nanoparticles etc. We present the model of this arc, which confirms the existence of the two different modes of the arc operation with two different anode sheath regimes, namely, with negative anode sheath and with positive anode sheath. It was previously suggested that these regimes are associated with two different anode ablating modes—low ablation mode with constant ablation rate and the enhanced ablation mode (Fetterman et al 2008 Carbon 46 1322). The transition of the arc operation from low ablation mode to high ablation mode is determined by the current density at the anode. The model can be used to self-consistently determine the distribution of the electric field, electron density and electron temperature in the near-anode region of the arc discharge. Simulations of the carbon arc predict that for low arc ablating modes, the current is driven mainly by the electron diffusion to the anode. For positive anode sheath, the anode voltage is close to the ionization potential of anode material, while for negative anode sheath, the anode voltage is an order of magnitude smaller. It is also shown that the near-anode plasma, is far from the ionization equilibrium. (paper)

  11. The plasma-sheath boundary region

    International Nuclear Information System (INIS)

    Franklin, R N

    2003-01-01

    In this review an attempt is made to give a broad coverage of the problem of joining plasma and sheath over a wide range of physical conditions. We go back to the earliest works quoting them, where appropriate, to understand what those who introduced the various terms associated with the structure of the plasma-sheath had in mind. We try to bring out the essence of the insights that have been gained subsequently, by quoting from the literature selectively, indicating how misunderstandings have arisen. In order to make it accessible to the generality of those currently working in low temperature plasmas we have sought to avoid mathematical complexity but retain physical insight, quoting from published work where appropriate. Nevertheless, in clarifying my own ideas I have found it necessary to do additional original work in order to give a consistent picture. In this way I have sought to bring together work in the late 1920s, the 1960s, and now mindful of the commercial importance of plasma processing, work over the past 15 years that adds to the general understanding. (topical review)

  12. Measurement of sheath thickness by lining out grooves in the Hall-type stationary plasma thrusters

    International Nuclear Information System (INIS)

    Yu Daren; Wu Zhiwen; Ning Zhongxi; Wang Xiaogang

    2007-01-01

    Using grooves created along the axial direction of the discharge channel, a method for measuring sheath thickness in Hall-type stationary plasma thrusters has been developed. By distorting the wall surface using these grooves, it is possible to numerically study the effect of the wall surface on the sheath and near wall conductivity. Monte Carlo method is applied to calculate the electron temperature variation with different groove depths. The electron dynamic process in the plasma is described by a test particle method with the electron randomly entering the sheath from the discharge channel and being reflected back. Numerical results show that the reflected electron temperature is hardly affected by the wall surface if the groove depth is much less than the sheath thickness. On the other hand, the reflected electron temperature increases if the groove depth is much greater than the sheath thickness. The reflected electron temperature has a sharp jump when the depth of groove is on the order of the sheath thickness. The simulation is repeated with different sheath thicknesses and the results are the same. Therefore, a diagnosis mean of the sheath thickness can be developed based on the method. Also the simulation results are in accord with the experimental data. Besides, the measurement method may be applicable to other plasma device with similar orthogonal steady state electrical and magnetic fields

  13. Mitigating the Risk of Stress Corrosion of Austenitic Stainless Steels in Advanced Gas Cooled Reactor Boilers

    International Nuclear Information System (INIS)

    Bull, A.; Owen, J.; Quirk, G.; G, Lewis; Rudge, A.; Woolsey, I.S.

    2012-09-01

    Advanced Gas-Cooled Reactors (AGRs) operated in the UK by EDF Energy have once-through boilers, which deliver superheated steam at high temperature (∼500 deg. C) and pressure (∼150 bar) to the HP turbine. The boilers have either a serpentine or helical geometry for the tubing of the main heat transfer sections of the boiler and each individual tube is fabricated from mild steel, 9%Cr1%Mo and Type 316 austenitic stainless steel tubing. Type 316 austenitic stainless steel is used for the secondary (final) superheater and steam tailpipe sections of the boiler, which, during normal operation, should operate under dry, superheated steam conditions. This is achieved by maintaining a specified margin of superheat at the upper transition joint (UTJ) between the 9%Cr1%Mo primary superheater and the Type 316 secondary superheater sections of the boiler. Operating in this mode should eliminate the possibility of stress corrosion cracking of the Type 316 tube material on-load. In recent years, however, AGRs have suffered a variety of operational problems with their boilers that have made it difficult to maintain the specified superheat margin at the UTJ. In the case of helical boilers, the combined effects of carbon deposition on the gas side and oxide deposition on the waterside of the tubing have resulted in an increasing number of austenitic tubes operating with less than the specified superheat margin at the UTJ and hence the possibility of wetting the austenitic section of the boiler. Some units with serpentine boilers have suffered creep-fatigue damage of the high temperature sections of the boiler, which currently necessitates capping the steam outlet temperature to prevent further damage. The reduction in steam outlet temperature has meant that there is an increased risk of operation with less than the specified superheat margin at the UTJ and hence stress corrosion cracking of the austenitic sections of the boiler. In order to establish the risk of stress

  14. Statistical analysis of mirror mode waves in sheath regions driven by interplanetary coronal mass ejection

    Science.gov (United States)

    Ala-Lahti, Matti M.; Kilpua, Emilia K. J.; Dimmock, Andrew P.; Osmane, Adnane; Pulkkinen, Tuija; Souček, Jan

    2018-05-01

    We present a comprehensive statistical analysis of mirror mode waves and the properties of their plasma surroundings in sheath regions driven by interplanetary coronal mass ejection (ICME). We have constructed a semi-automated method to identify mirror modes from the magnetic field data. We analyze 91 ICME sheath regions from January 1997 to April 2015 using data from the Wind spacecraft. The results imply that similarly to planetary magnetosheaths, mirror modes are also common structures in ICME sheaths. However, they occur almost exclusively as dip-like structures and in mirror stable plasma. We observe mirror modes throughout the sheath, from the bow shock to the ICME leading edge, but their amplitudes are largest closest to the shock. We also find that the shock strength (measured by Alfvén Mach number) is the most important parameter in controlling the occurrence of mirror modes. Our findings suggest that in ICME sheaths the dominant source of free energy for mirror mode generation is the shock compression. We also suggest that mirror modes that are found deeper in the sheath are remnants from earlier times of the sheath evolution, generated also in the vicinity of the shock.

  15. Mitigating impact of thermal and rectified radio-frequency sheath potentials on edge localized modes

    Energy Technology Data Exchange (ETDEWEB)

    Gui, B. [Institute of Plasma Physics Chinese Academy of Sciences, Hefei (China); Lawerence Livermore National Lab, Livermore, California 94550 (United States); Xu, X. Q. [Lawerence Livermore National Lab, Livermore, California 94550 (United States); Myra, J. R.; D' Ippolito, D. A. [Lodestar Research Corporation, Boulder, Colorado 80301 (United States)

    2014-11-15

    The mitigating impact of thermal and rectified radio frequency (RF) sheath potentials on the peeling-ballooning modes is studied non-linearly by employing a two-fluid three-field simulation model based on the BOUT++ framework. Additional shear flow and the Kelvin-Helmholtz effect due to the thermal and rectified RF sheath potential are induced. It is found that the shear flow increases the growth rate while the K-H effect decreases the growth rate slightly when there is a density gradient, but the energy loss of these cases is suppressed in the nonlinear phase. The stronger external electrostatic field due to the sheaths has a more significant effect on the energy loss suppression. From this study, it is found the growth rate in the linear phase mainly determines the onset of edge-localized modes, while the mode spectrum width in the nonlinear phase has an important impact on the turbulent transport. The wider mode spectrum leads to weaker turbulent transport and results in a smaller energy loss. Due to the thermal sheath and rectified RF sheath potential in the scrape-off-layer, the modified shear flow tears apart the peeling-ballooning filament and makes the mode spectrum wider, resulting in less energy loss. The perturbed electric potential and the parallel current near the sheath region is also suppressed locally due to the sheath boundary condition.

  16. Moisture Durability with Vapor-Permeable Insulating Sheathing

    Energy Technology Data Exchange (ETDEWEB)

    Lepage, R. [Building Science Corporation, Somerville, MA (United States); Lstiburek, J. [Building Science Corporation, Somerville, MA (United States)

    2013-09-01

    Exterior sheathing insulation is an effective strategy in increasing the overall R-value of wall assemblies; other benefits include decreasing the effects of thermal bridging and increasing the moisture durability of the built assembly. Vapor-permeable exterior insulation, such as mineral board or expanded polystyrene foam, are one such product that may be used to achieve these benefits. However, uncertainty exists on the effects of inward driven moisture and the interaction of increased sheathing temperatures on the moisture durability of the edifice. To address these concerns, Building Science Corporation (BSC) conducted a series of hygrothermal models for cities representing a range of different climate zones. This report describes the research project, key research questions, and the procedures utilized to analyse the problems.

  17. Moisture Durability with Vapor-Permeable Insulating Sheathing

    Energy Technology Data Exchange (ETDEWEB)

    Lepage, R. [Building Science Corporation, Somerville, MA (United States); Lstiburek, J. [Building Science Corporation, Somerville, MA (United States)

    2013-09-01

    Exterior sheathing insulation is an effective strategy in increasing the overall R-value of wall assemblies; other benefits include decreasing the effects of thermal bridging and increasing the moisture durability of the built assembly. Vapor-permeable exterior insulation, such as mineral board or expanded polystyrene foam, are one such product that may be used to achieve these benefits. However,uncertainty exists on the effects of inward driven moisture and the interaction of increased sheathing temperatures on the moisture durability of the edifice. To address these concerns, Building Science Corporation (BSC) conducted a series of hygrothermal models for cities representing a range of different climate zones. This report describes the research project, key research questions, and theprocedures utilized to analyse the problems.

  18. Cell Based Meniscal Repair Using an Aligned Bioactive Nanofibrous Sheath

    Science.gov (United States)

    2017-07-01

    to subsequently guide tissue regeneration , for example, by seeded tissue progenitor cells . To achieve this objective, the first step is to develop...AWARD NUMBER: W81XWH-15-1-0104 TITLE: Cell -Based Meniscal Repair Using an Aligned Bioactive Nanofibrous Sheath PRINCIPAL INVESTIGATOR...SUBTITLE 5a. CONTRACT NUMBER Cell -Based Meniscal Repair Using an Aligned Bioactive Nanofibrous Sheath 5b. GRANT NUMBER W81XWH-15-1-0104 5c. PROGRAM

  19. The ion polytropic coefficient in a collisionless sheath containing hot ions

    Energy Technology Data Exchange (ETDEWEB)

    Lin, Binbin; Xiang, Nong, E-mail: xiangn@ipp.ac.cn; Ou, Jing [Institute of Plasma Physics, Chinese Academy of Sciences, Hefei 230031 (China); Center for Magnetic Fusion Theory, Chinese Academy of Sciences, Hefei 230031 (China)

    2016-08-15

    The fluid approach has been widely used to study plasma sheath dynamics. For a sheath containing hot ions whose temperature is greater than the electron's, how to truncate the fluid hierarchy chain equations while retaining to the fullest extent of the kinetic effects is always a difficult problem. In this paper, a one-dimensional, collisionless sheath containing hot ions is studied via particle-in-cell simulations. By analyzing the ion energy equation and taking the kinetic effects into account, we have shown that the ion polytropic coefficient in the vicinity of the sheath edge is approximately constant so that the state equation with the modified polytropic coefficient can be used to close the hierarchy chain of the ion fluid equations. The value of the polytropic coefficient strongly depends on the hot ion temperature and its concentration in the plasma. The semi-analytical model is given to interpret the simulation results. As an application, the kinetic effects on the ion saturation current density in the probe theory are discussed.

  20. Rectus sheath haematoma or leaking aortic aneurysm - a diagnostic challenge: a case report

    Directory of Open Access Journals (Sweden)

    Shaw Aidan G

    2009-11-01

    Full Text Available Abstract Introduction A rectus sheath haematoma is a rare condition that arises from the accumulation of blood within the rectus sheath from either muscular tear or rupture of the epigastric vessels. It is a known complication of either blunt abdominal trauma, anticoagulation therapy or the repetitive contraction of the rectus muscle such as paroxysms of coughing. It remains an uncommon and elusive entity and is often clinically misdiagnosed. Case presentation An 80-year-old British man with a known aortic aneurysm was admitted with sudden onset of right iliac fossa pain. The patient was hemodynamically stable and underwent a computed tomography scan which revealed an intact aorta and an acute rectus sheath hematoma. Conclusion To the best of our knowledge, no case has previously been reported involving the diagnostic challenge of a rectus sheath hematoma in a patient with a known aortic aneurysm. Here we discuss the symptoms and signs of a rectus sheath hematoma, as well as the radiological modalities that could be utilized to reach the diagnosis.

  1. Study of the behavior to corrosion of samples of nuclear grade aluminium sheathed in nickel-phosphorous alloys obtained autocatalytically

    International Nuclear Information System (INIS)

    Castro, Maria Eugenia; Barbero, Jose Alfredo; Bubach, Ernesto

    2006-01-01

    One of the ways to protect an industrially important metallic material against corrosion is by covering the piece with an approximately 1 μm layer of a material whose resistance to corrosion is greater than the element being protected. The mechanism by which the anticorrosive protection is obtained is with the formation of a pore free physical barrier without defects that impedes the arrival of the agents responsible for the electrochemical attack. Other sacrifice anodes such as aluminum or zinc have protective forms based on their dissolution as a consequence of their less electrochemically noble behavior to preserve the material. This work studies the resistance to the corrosion of metallic coatings on nuclear grade aluminum substrates. The focus is on coating nickel-phosphorous (ni-P) alloys obtained autocatalytically from aluminum 6061. A comparative study is carried out of a series of electroless nickel coatings containing different amounts of the latter element, but without surpassing the threshold of 12%. The work includes the study of another nickel coating, Vitrovac 0080 (without phosphorous content) in order to compare structures and anticorrosive properties. These materials are also compared with the Al6061 substrate without any kind of coating. The study is carried out with surface characterization of each one of the samples with or without coating using a series of complementary techniques, such as chemical and electrochemical techniques (linear-sweep voltammetry, cyclic voltammetry, determination of the polarization resistance) and physical techniques (SEM microscopy, determination of micro-hardness). The correlation of variables is carried out later as a function of the phosphorous content of the test samples. The structures obtained from the coatings are amorphous. They have no pores or faults and have high hardness values. The electrochemical study proves that the anticorrosive protection capacity of the Ni-P alloy increases along with the

  2. Development of Ti-sheathed MgB2 wires with high critical current density

    International Nuclear Information System (INIS)

    Liang, G; Fang, H; Hanna, M; Yen, F; Lv, B; Alessandrini, M; Keith, S; Hoyt, C; Tang, Z; Salama, K

    2006-01-01

    Working towards developing lightweight superconducting magnets for future space and other applications, we have successfully fabricated mono-core Ti-sheathed MgB 2 wires by the powder-in-tube method. The wires were characterized by magnetization, electrical resistivity, x-ray diffraction, scanning electron microscopy, and energy dispersive spectrometry measurements. The results indicate that the Ti sheath does not react with the magnesium and boron, and the present wire rolling process can produce MgB 2 wires with a superconducting volume fraction of at least 64% in the core. Using the Bean model, it was found that at 5 K, the magnetic critical current densities, J c , measured in magnetic fields of 0, 5, and 8 T are about 4.2 x 10 5 , 3.6 x 10 4 , and 1.4 x 10 4 A cm -2 , respectively. At 20 K and 0 T, the magnetic J c is about 2.4 x 10 5 A cm -2 . These results show that at zero and low fields, the values of the magnetic J c for Ti-sheathed MgB 2 wires are comparable with the best results available for the Fe-sheathed MgB 2 wires. At high fields, however, the J c for Ti-sheathed MgB 2 wires appears higher than that for the Fe-sheathed MgB 2 wires

  3. Research on stress distribution regularity of cement sheaths of radial well based on ABAQUS

    Science.gov (United States)

    Shi, Jihui; Cheng, Yuanfang; Li, Xiaolong; Xiao, Wen; Li, Menglai

    2017-12-01

    To ensure desirable outcome of hydraulic fracturing based on ultra-short radius radial systems, it is required to investigate the stress distribution regularity and stability of the cement sheath. On the basis of the theoretical model of the cement sheath stress distribution, a reservoir mechanical model was built using the finite element software, ABAQUS, according to the physical property of a certain oil reservoir of the Shengli oilfield. The stress distribution of the casing-cement-sheath-formation system under the practical condition was simulated, based on which analyses were conducted from multiple points of view. Results show that the stress on the internal interface of the cement sheath exceeds that on the external interface, and fluctuates with higher amplitudes, which means that the internal interface is the most failure-prone. The unevenness of the cement sheath stress distribution grows with the increasing horizontal principal stress ratio, and so does the variation magnitude. This indicates that higher horizontal principal stress ratios are unfavourable for the structural stability of the cement sheath. Both the wellbore quantity of the URRS and the physical property of the material can affect the cement sheath distribution. It is suggested to optimize the quantity of the radial wellbore and use cement with a lower elastic modulus and higher Poisson’s ratio. At last, the impact level of the above factor was analysed, with the help of the grey correlation analysis.

  4. Hot corrosion of the steel SA213-T22 and SA213-TP347H in 80% V{sub 2}O{sub 5}-20%Na{sub 2}SO{sub 4} mixture; Corrosion por depositos salinos de los aceros SA213-T22 y SA213-TP347H en presencia de una mezcal 80%V{sub 2} O{sub 5}-20%Na{sub 2}SO{sub 4}

    Energy Technology Data Exchange (ETDEWEB)

    Almeraya, F; Martinez-Villafane, A; Gaona, C; Romero, M A; Malo, J M

    1998-06-01

    Many hot corrosion problems in industrial and utility boilers are caused by molten salts. The corrosion processes which occur in salts are of an electrochemical nature, and so they can be studied using electrochemical test methods. In this research, electrochemical techniques in molten salt systems have been used for the measurements of molten corrosion processes. Electrochemical test methods are described here for a salt mixture of 80%V{sub 2}O{sub 5}-20%NaSO{sub 4} at 540-680 degree centigree. To establish better the electrochemical corrosion rate measurements for molten salt systems, information from electrochemical potentiodynamic polarization curves, such as polarization resistance and Tafeol slopes were used in this study to generate corrosion rate data. The salt was contained in a quartz crucible inside a stainless retort. The atmosphere used was air. A thermocouple sheathed with quartz glass was introduced into the molten salt for temperature monitoring and control. Two materials were tested in the molten mixture: SA213-T22 and SA213-TP347H steels. The corrosion rates values obtained using electrochemical methods were around 0.58-7.14 mm/yr (22.9-281 mpy). The corrosion rate increase with time. (Author) 7 refs.

  5. Child-Langmuir law for cathode sheath of glow discharge in CO2

    International Nuclear Information System (INIS)

    Lisovskiy, V.A.; Krol, H.H.; Osmayev, R.O.; Yegorenkov, V.D.

    2016-01-01

    This work is devoted to the determination of the law that may be applicable to the description of the cathode sheath in CO 2 . To this end three versions of the Child-Langmuir law have been considered - a collision free one (for the ions moving through a cathode sheath without collisions with gas molecules) as well as two collision- related versions - one for a constant mean free path of positive ions and one for a constant mobility of positive ions. The current-voltage characteristics and the cathode sheath thickness of the glow discharge in CO 2 have been simultaneously measured in the pressure range from 0.05 to 1 Torr and with the discharge current values up to 80 mA. In the whole range of the discharge conditions we have studied the cathode sheath characteristics are found to obey correctly only to the Child-Langmuir law version with a constant ion mobility.

  6. Effects of neutral gas collisions on the power transmission factor at the divertor sheath

    International Nuclear Information System (INIS)

    Futch, A.H.; Matthews, G.F.; Buchenauer, D.; Hill, D.N.; Jong, R.A.; Porter, G.D.

    1992-01-01

    We show that charge-exchange and other ion-neutral collision can reduce the power transmission factor of the plasma sheath, thereby lowering the ion impact energy and target plate sputtering. The power transmission factor relates the heat flux reaching the divertor target to the plasma density and temperature just in front of the surface: δ=Q surf /J ew k T e . Experimental data from the DIII-D tokamak suggests that δ could be as low as 2-3 near the region of peak divertor particle flux, instead of the 7-8 expected from usual sheath theory. Several effects combine to allow ion-neutral interactions to be important in the divertor plasma sheath. The shallow angle of incidence of the magnetic field (1-3deg in DIII-D) leads to the spatial extension of the sheath from approximately ρ i ∝1 mm normal to the plate to several centimeters along the field lines. Ionization reduces the sheath potential, and collisions reduce the ion impact energy. (orig.)

  7. Effect of rise-time patterns on dynamics of sheath expansion during plasma immersion ion implantation

    International Nuclear Information System (INIS)

    Huang Yongxian; Tian Xiubo; Yang Shiqin; Fu Ricky; Paul, C.K.

    2007-01-01

    Plasma immersion ion implantation (PIII) has been developed as a low-cost and efficient surface modification technique of irregularly-shaped objects. The effect of six pulse waves with different rise-time patterns on the spatio-temporal evolution of plasma sheath,energy and dose of ion implantation has been simulated by particle-in-cell modeling. Statistical results may be obtained through assuming the Boltzmann distribution of electrons, and solving Poisson and Newton equations for tracing each ion in the plasma sheath. The results show that rise-time pattern has a critical influence on the evolution of plasma sheath. There exists maximum thickness difference of plasma sheath for different waveforms. The acceleration of ions is non-uniform due to the non-uniformity of electrical field strength. The maximum gradient of electrical field appears near the edge of plasma sheath. The results also show that optimization of dose and energy of incident ions may be achieved through modification of rise-time pattern. The numerical simulation of sheath expansion can be effectively used to provide a scientific basis for optimizing the PIII process. (authors)

  8. Qualification of Alloy 800 for sodium heated steam generators

    International Nuclear Information System (INIS)

    Duke, J.M.; Sessions, C.E.; Ray, W.E.

    1976-01-01

    A reference specification of Alloy 800 for use in LMFBR steam generators is defined considering waterside corrosion, weldability and mechanical properties. Additional mechanical test data are being generated to support ASME Code acceptance. Candidate weld filler metals were assessed for use in subsequent weld process development. Progress on resolving technical concerns related to the role of tertiary creep identified the impact of test conditions and gamma prime strengthening in determining the creep behavior of Alloy 800

  9. Dusty Plasma Modeling of the Fusion Reactor Sheath Including Collisional-Radiative Effects

    International Nuclear Information System (INIS)

    Dezairi, Aouatif; Samir, Mhamed; Eddahby, Mohamed; Saifaoui, Dennoun; Katsonis, Konstantinos; Berenguer, Chloe

    2008-01-01

    The structure and the behavior of the sheath in Tokamak collisional plasmas has been studied. The sheath is modeled taking into account the presence of the dust 2 and the effects of the charged particle collisions and radiative processes. The latter may allow for optical diagnostics of the plasma.

  10. Fibrin Sheath Angioplasty: A Technique to Prevent Superior Vena Cava Stenosis Secondary to Dialysis Catheters

    Science.gov (United States)

    Hacker, Robert I.; Garcia, Lorena De Marco; Chawla, Ankur; Panetta, Thomas F.

    2012-01-01

    Fibrin sheaths are a heterogeneous matrix of cells and debris that form around catheters and are a known cause of central venous stenosis and catheter failure. A total of 50 cases of central venous catheter fibrin sheath angioplasty (FSA) after catheter removal or exchange are presented. A retrospective review of an outpatient office database identified 70 eligible patients over a 19-month period. After informed consent was obtained, the dialysis catheter exiting the skin was clamped, amputated, and a wire was inserted. The catheter was then removed and a 9-French sheath was inserted into the superior vena cava, a venogram was performed. If a fibrin sheath was present, angioplasty was performed using an 8 × 4 or 10 × 4 balloon along the entire length of the fibrin sheath. A completion venogram was performed to document obliteration of the sheath. During the study, 50 patients were diagnosed with a fibrin sheath, and 43 had no pre-existing central venous stenosis. After FSA, 39 of the 43 patient's (91%) central systems remained patent without the need for subsequent interventions; 3 patients (7%) developed subclavian stenoses requiring repeat angioplasty and stenting; 1 patent (2.3%) developed an occlusion requiring a reintervention. Seven patients with prior central stenosis required multiple angioplasties; five required stenting of their central lesions. Every patient had follow-up fistulograms to document long-term patency. We propose that FSA is a prudent and safe procedure that may help reduce the risk of central venous stenosis from fibrin sheaths due to central venous catheters. PMID:23997555

  11. Arthroscopic sheath design and technical evaluation

    NARCIS (Netherlands)

    Tuijthof, Gabriëlle J. M.; Blankevoort, Leendert; Herder, Just L.; van Dijk, C. Niek

    2009-01-01

    The maintenance of a clear view on the operation area is essential to perform a minimally invasive procedure In arthroscopy, this is achieved by irrigating the Joint with a saline fluid that is pumped through the joint At present the arthroscopic sheaths are not designed for optimal irrigation,

  12. Community structure of filamentous, sheath-building sulfur bacteria, Thioploca spp, off the coast of Chile

    DEFF Research Database (Denmark)

    Schulz, HN; Jørgensen, BB; Fossing, HA

    1996-01-01

    of Concepcion was investigated,vith respect to biomass, species distribution, and three-dimensional orientation of the sheaths, Thioploca sheaths and filaments were found across the whole shelf area within the oxygen minimum zone, The maximum wet weight of sheaths, 800 g m(-2), was found at a depth of 90 m......The filamentous sulfur bacteria Thioploca spp, produce dense bacterial mats in the shelf area off the coast of Chile and Peru. The mat consists of common sheaths, shared by many filaments, that reach 5 to 10 cm dean into the sediment, The structure of the Thioploca communities off the Bay...

  13. Application of Spray Foam Insulation Under Plywood and Oriented Strand Board Roof Sheathing

    Energy Technology Data Exchange (ETDEWEB)

    Grin, A. [Building Science Corporation, Somerville, MA (United States); Smegal, J. [Building Science Corporation, Somerville, MA (United States); Lstiburek, J. [Building Science Corporation, Somerville, MA (United States)

    2013-10-01

    Unvented roof strategies with open cell and closed cell spray polyurethane foam insulation sprayed to the underside of roof sheathing have been used since the mid-1990's to provide durable and efficient building enclosures. However, there have been isolated moisture related incidents reported anecdotally that raise potential concerns about the overall hygrothermal performance of these systems. This project involved hygrothermal modeling of a range of rainwater leakage and field evaluations of in-service residential roofs using spray foam insulation. All of the roof assemblies modeled exhibited drying capacity to handle minor rainwater leakage. All field evaluation locations of in-service residential roofs had moisture contents well within the safe range for wood-based sheathing. Explorations of eleven in-service roof systems were completed. The exploration involved taking a sample of spray foam from the underside of the roof sheathing, exposing the sheathing, then taking a moisture content reading. All locations had moisture contents well within the safe range for wood-based sheathing. One full-roof failure was reviewed, as an industry partner was involved with replacing structurally failed roof sheathing. In this case the manufacturer's investigation report concluded that the spray foam was installed on wet OSB based on the observation that the spray foam did not adhere well to the substrate and the pore structure of the closed cell spray foam at the ccSPF/OSB interface was indicative of a wet substrate.

  14. Modelling of the dual frequency capacitive sheath in the intermediate pressure range

    International Nuclear Information System (INIS)

    Boyle, P C; Robiche, J; Turner, M M

    2004-01-01

    The nonlinearity of the plasma sheath in dual frequency capacitively coupled reactors is investigated for frequencies well above the ion plasma frequency. This work focuses on the behaviour of the voltage and the sheath width with respect to the driving current source and the collisionality regime. For typical plasma processing applications, the gas pressure ranges from a few milliTorrs to hundreds of milliTorrs, and the ion dynamics span different collisional regimes. To describe these different ion dynamics, we have used a collisionless model and a variable mobility model. The sheath widths and the voltages obtained from these two models have then been compared

  15. Corrosion and hydriding behaviour of some Zr 2.5 wt% Nb alloys in water, steam and various gases at high temperature

    Energy Technology Data Exchange (ETDEWEB)

    Dalgaard, S. B.

    1962-05-15

    Fuel sheaths and pressure tubes in Canadian power reactors are at present made from Zircaloy-2. Mechanical properties of a suitably heat treated Zr 2.5 wt% Nb alloy are superior to those of Zircaloy-2, but any new alloy must have resistance to corrosion and hydriding by the coolant and by the gas that insulates the pressure tube from the cold moderator. Exposed to water at temperatures up to 325{sup o}C, the Zr 2.5 wt% Nb alloy has corrosion resistance acceptable for power reactors. Resistance to air and carbon dioxide is less favourable. Addition of tin, or iron and chromium, to the base alloy have little effect on the corrosion resistance, but the addition of copper reduces corrosion in water and steam to some extent and in air and carbon dioxide to a greater extent. Studies of the effect of heat treatment suggest that the amount of niobium in a solid-solution controls the rate of oxidation and hydriding and that concentration, size and distribution of second phase is of little importance. Initial results obtained in NRX indicate that a thermal flux of 3-7 x 10{sup 13} n/cm{sup 2}/sec has little or no effect on oxidation and hydriding in high temperature water. (author)

  16. Studies of RF sheaths and diagnostics on IShTAR

    Energy Technology Data Exchange (ETDEWEB)

    Crombé, K., E-mail: Kristel.Crombe@UGent.be [Department of Applied Physics, Ghent University, Ghent (Belgium); LPP-ERM/KMS, Royal Military Academy, Brussels (Belgium); Devaux, S.; Faudot, E.; Heuraux, S.; Moritz, J. [YIJL, UMR7198 CNRS-Université de Lorraine, Nancy (France); D’Inca, R.; Faugel, H.; Fünfgelder, H.; Jacquot, J.; Ochoukov, R. [Max-Planck-Institut für Plasmaphysik, Garching (Germany); Louche, F.; Tripsky, M.; Van Eester, D.; Wauters, T. [LPP-ERM/KMS, Royal Military Academy, Brussels (Belgium); Noterdaeme, J.-M. [Department of Applied Physics, Ghent University, Ghent (Belgium); Max-Planck-Institut für Plasmaphysik, Garching (Germany)

    2015-12-10

    IShTAR (Ion cyclotron Sheath Test ARrangement) is a linear magnetised plasma test facility for RF sheaths studies at the Max-Planck-Institut für Plasmaphysik in Garching. In contrast to a tokamak, a test stand provides more liberty to impose the parameters and gives better access for the instrumentation and antennas. The project will support the development of diagnostic methods for characterising RF sheaths and validate and improve theoretical predictions. The cylindrical vacuum vessel has a diameter of 1 m and is 1.1 m long. The plasma is created by an external cylindrical plasma source equipped with a helical antenna that has been designed to excite the m=1 helicon mode. In inductive mode, plasma densities and electron temperatures have been characterised with a planar Langmuir probe as a function of gas pressure and input RF power. A 2D array of RF compensated Langmuir probes and a spectrometer are planned. A single strap RF antenna has been designed; the plasma-facing surface is aligned to the cylindrical plasma to ease the modelling. The probes will allow direct measurements of plasma density profiles in front of the RF antenna, and thus a detailed study of the density modifications induced by RF sheaths, which influences the coupling. The RF antenna frequency has been chosen to study different plasma wave interactions: the accessible plasma density range includes an evanescent and propagative behaviour of slow or fast waves, and allows the study of the effect of the lower hybrid resonance layer.

  17. Use of a hot sheath Tormac for advance fuels

    International Nuclear Information System (INIS)

    Levine, M.A.

    1977-01-01

    The use of hot electrons in a Tormac sheath is predicted to improve stability and increase ntau by an order of magnitude. An effective ntau for energy containment is derived and system parameters for several advance fuels are shown. In none of the advance fuels cases considered is a reactor with fields greater than 10 Wb or major plasma radius of more than 3 m required for ignition. Minimum systems have power output of under 100 MW thermal. System parameters for a hot sheath Tormac have a wide latitude. Sizes, magnetic fields, operating temperatures can be chosen to optimize engineering and economic considerations

  18. Application of CdZnTe Gamma-Ray Detector for Imaging Corrosion under Insulation

    International Nuclear Information System (INIS)

    Abdullah, J.; Yahya, R.

    2007-01-01

    Corrosion under insulation (CUI) on the external wall of steel pipes is a common problem in many types of industrial plants. This is mainly due to the presence of moisture or water in the insulation materials. This type of corrosion can cause failures in areas that are not normally of a primary concern to an inspection program. The failures are often the result of localised corrosion and not general wasting over a large area. These failures can tee catastrophic in nature or at least have an adverse economic effect in terms of downtime and repairs. There are a number of techniques used today for CUI investigations. The main ones are profile radiography, pulse eddy current, ultrasonic spot readings and insulation removal. A new system now available is portable Pipe-CUI-Profiler. The nucleonic system is based on dual-beam gamma-ray absorption technique using Cadmium Zinc Telluride (CdZnTe) semiconductor detectors. The Pipe-CUI-Profiler is designed to inspect pipes of internal diameter 50, 65, 80, 90, 100, 125 and 150 mm. Pipeline of these sizes with aluminium or thin steel sheathing, containing fibreglass or calcium silicate insulation to thickness of 25, 40 and 50 mm can be inspected. The system has proven to be a safe, fast and effective method of inspecting pipe in industrial plant operations. This paper describes the application of gamma-ray techniques and CdZnTe semiconductor detectors in the development of Pipe-CUI-Profiler for non-destructive imaging of corrosion under insulation of steel pipes. Some results of actual pipe testing in large-scale industrial plant will be presented

  19. Application of CdZnTe Gamma-Ray Detector for Imaging Corrosion under Insulation

    Science.gov (United States)

    Abdullah, J.; Yahya, R.

    2007-05-01

    Corrosion under insulation (CUI) on the external wall of steel pipes is a common problem in many types of industrial plants. This is mainly due to the presence of moisture or water in the insulation materials. This type of corrosion can cause failures in areas that are not normally of a primary concern to an inspection program. The failures are often the result of localised corrosion and not general wasting over a large area. These failures can tee catastrophic in nature or at least have an adverse economic effect in terms of downtime and repairs. There are a number of techniques used today for CUI investigations. The main ones are profile radiography, pulse eddy current, ultrasonic spot readings and insulation removal. A new system now available is portable Pipe-CUI-Profiler. The nucleonic system is based on dual-beam gamma-ray absorption technique using Cadmium Zinc Telluride (CdZnTe) semiconductor detectors. The Pipe-CUI-Profiler is designed to inspect pipes of internal diameter 50, 65, 80, 90, 100, 125 and 150 mm. Pipeline of these sizes with aluminium or thin steel sheathing, containing fibreglass or calcium silicate insulation to thickness of 25, 40 and 50 mm can be inspected. The system has proven to be a safe, fast and effective method of inspecting pipe in industrial plant operations. This paper describes the application of gamma-ray techniques and CdZnTe semiconductor detectors in the development of Pipe-CUI-Profiler for non-destructive imaging of corrosion under insulation of steel pipes. Some results of actual pipe testing in large-scale industrial plant will be presented.

  20. Stress/strain characteristics of Cu alloy sheath in situ processed MgB2 superconducting wires

    International Nuclear Information System (INIS)

    Katagiri, Kazumune; Kasaba, Koichi; Shoji, Yoshitaka

    2005-01-01

    The mechanical properties of copper and copper alloy (Cu-Zr, Cu-Be and Cu-Cr) sheath in situ PIT-processed MgB 2 superconducting wires were studied at room temperature (RT) and 4.2 K. The effects of stress-strain on the critical current (I c ) of the wires have also been studied at 4.2 K and in magnetic fields up to 5 T. It has been clarified that alloying the Cu sheath significantly increases the yield and flow stresses of the wires at both RT and 4.2 K. The 0.5% flow stresses of the Cu alloy sheath wire were 147-237 MPa, whereas that of Cu was 55 MPa. At RT, serration corresponding to multiple cracking was observed around a strain of 0.4% and the stress-strain curves saturated beyond that point. The strain dependence of I c prior to the critical strain (ε irr ) was different depending on the magnetic field; being almost constant at 2 T and increasing with strain at 5 T. The I c decreased beyond ε irr , which is much larger for Cu alloy sheath wires as compared to Cu sheath wire. This is due to the difference in the residual compressive strain in the MgB 2 core during cooling from the heat-treatment temperature to 4.2 K, which is determined through relaxation by yielding in the sheath materials. The transverse compression tests revealed that the I c of the Cu alloy sheath wire did not degrade up to 314 MPa, which is also higher than that of Cu sheath wire. (author)

  1. Synthesis of sheath voltage drops in asymmetric radio-frequency discharges

    International Nuclear Information System (INIS)

    Yonemura, Shigeru; Nanbu, Kenichi; Iwata, Naoaki

    2004-01-01

    A sheath voltage drop in asymmetric discharges is one of the most important parameters of radio-frequency capacitively coupled plasmas because it determines the kinetic energy of the ions incident on the target or substrate. In this study, we developed a numerical simulation code to estimate the sheath voltage drops and, consequently, the self-bias voltage. We roughly approximated general asymmetric rf discharges to one-dimensional spherical ones. The results obtained by using our simulation code are consistent with measurements and Lieberman's theory

  2. Effect of composition on the fabrication and properties of Ag-Cu alloy sheathed (Bi,Pb)2223 tapes

    International Nuclear Information System (INIS)

    Nakamura, Yuichi; Nakashima, Sohei; Inada, Ryoji; Oota, Akio

    2004-01-01

    To achieve high J c values as well as high mechanical strength, the effects of Ag-Cu alloy sheath and initial composition of precursor on the microstructure and J c properties of Ag-Cu alloy sheathed tapes were investigated. The alkaline-earth cuprate particles were found to form preferentially near the interface between superconducting core and sheath. Although the worse (Bi,Pb)2223 purity and microstructure of alloy sheathed tapes, the reduction of J c values of the tapes was small especially in 7-filaments tapes. This might be explained by the well grain alignment of (Bi,Pb)2223 into the middle region of the filament due to the high strength of alloy sheath. The usage of the Cu deficient composition was effective to reduce the total amount of 14:24 particle while the filament thickness should be thin to maintain J c values for Ag-Cu alloy sheathed tapes due to the lack of Cu diffusion from the sheath to convert 2212 into (Bi,Pb) in the middle region of the filament

  3. On the biogenesis of the myelin sheath : Cognate polarized trafficking pathways in oligodendrocytes

    NARCIS (Netherlands)

    de Vries, H; Hoekstra, D

    2000-01-01

    Oligodendrocytes, the myelinating cells of the central nervous system, are capable of transporting vast quantities of proteins and of lipids, In particular galactosphingolipids, to the myelin sheath. The sheath is continuous with the plasma membrane of the oligodendrocyte, but the composition of

  4. Effects of Fast-Ion Injection on a Magnetized Sheath near a Floating Wall

    International Nuclear Information System (INIS)

    Li Jiajia; Hu Zhanghu; Song Yuanhong; Wang Younian

    2013-01-01

    A fully kinetic particle-in-cell/Monte Carlo model is employed to self-consistently study the effects of fast-ion injection on sheath potential and electric field profile in collisional magnetized plasma with a floating absorbing wall. The influences of the fast-ion injection velocity and density, the magnetic field and angle θ 0 formed by the magnetic field and the x-axis on the sheath potential and electric field are discussed in detail. Numerical results show that increasing fast-ion injection density or decreasing injection velocity can enhance the potential drop and electric field in the sheath. Also, increasing the magnetic field strength can weaken the loss of charged particles to the wall and thus decrease the potential and electric field in the sheath. The time evolution of ion flux and velocity distribution on the wall is found to be significantly affected by the magnetic field.

  5. Effects of Reentry Plasma Sheath on Mutual-Coupling Property of Array Antenna

    Directory of Open Access Journals (Sweden)

    B. W. Bai

    2015-01-01

    Full Text Available A plasma sheath enveloping a reentry vehicle would cause the failure of on-board antennas, which is an important effect that contributes to the “blackout” problem. The method of replacing the on-board single antenna with the array antennas and using beamforming technology has been proposed to mitigate “blackout” problem by many other researchers. Because the plasma sheath is a reflective medium, plasma will alter the mutual coupling between array elements and degrade the beamforming performance of array antenna. In this paper, the effects of the plasma sheath on the mutual coupling properties between adjacent array elements are studied utilizing the algorithm of finite integration technique. Results show that mutual coupling coefficients of array elements are deteriorating more seriously with the decrease of collision frequency. Moreover, when electron density and collision frequency are both large, plasma sheath improves the mutual coupling property of array elements; this conclusion suggests that replacing the on-board single antenna with the array antennas and using beamforming technology can be adopted to mitigate the blackout problem in this condition.

  6. CT saber-sheath trachea. Correlation with clinical, chest radiographic and functional findings

    International Nuclear Information System (INIS)

    Trigaux, J.P.; Hermes, G.; Dubois, P.; Beers, B. van; Delaunois, L.; Jamart, J.

    1994-01-01

    The diagnosis of saber-sheath trachea is easy at CT due to its cross-sectional imaging, but the significance of this CT sign has not been evaluated in the diagnosis of chronic obstructive pulmonary disease (COPD). Various signs of COPD were compared between a series of 20 patients with a saber-sheath trachea at CT (tracheal index ≤66%) and a group of 20 pneumologic control patients without saber-sheath trachea (tracheal index ≥70%). These signs include clinical and standard radiographic indices of COPD, sternum-spine distance and 3 functional tests of COPD: forced expiratory volume in one second, carbon monoxide diffusing lung capacity, and funtional residual capacity (FRC). A significant difference was found between the 2 groups, concerning the values of FRC and of sternum-spine distance (p -2 ). The tracheal index was significantly correlated with the FRC values and with the sternum-spine distance. No other significant difference was observed. It is concluded that saber-sheath trachea is basically a sign of hyperinflation. (orig./MG)

  7. Experimental investigations on waterside corrosion problems of sodium-heated steam generators

    International Nuclear Information System (INIS)

    Buescher, E.; Haubold, W.; Jansing, W.; Vinzens, K.

    1975-01-01

    Based on experimental results, it is shown that the formation of a protective magnetite layer in sodium-heated steam generators - operated with neutral demineralized water - proceeds very fast. The stability of the magnetite layer is excellent even at sudden load changes and at the start-up or shut-down operation. (author)

  8. Experimental investigations on waterside corrosion problems of sodium-heated steam generators

    Energy Technology Data Exchange (ETDEWEB)

    Buescher, E; Haubold, W; Jansing, W; Vinzens, K

    1975-07-01

    Based on experimental results, it is shown that the formation of a protective magnetite layer in sodium-heated steam generators - operated with neutral demineralized water - proceeds very fast. The stability of the magnetite layer is excellent even at sudden load changes and at the start-up or shut-down operation. (author)

  9. Core-Sheath Paraffin-Wax-Loaded Nanofibers by Electrospinning for Heat Storage.

    Science.gov (United States)

    Lu, Yuan; Xiao, Xiudi; Zhan, Yongjun; Huan, Changmeng; Qi, Shuai; Cheng, Haoliang; Xu, Gang

    2018-04-18

    Paraffin wax (PW) is widely used for smart thermoregulation materials due to its good thermal performance. However, the leakage and low thermal conductivity of PW hinder its application in the heat storage field. Accordingly, developing effective methods to address these issues is of great importance. In this study, we explored a facile approach to obtain PW-loaded core-sheath structured flexible nanofibers films via coaxial electrospinning technique. The PW as the core layer was successfully encapsulated by the sheath-layer poly(methyl methacrylate). The diameter of the fiber core increased from 395 to 848 nm as the core solution speed rate increased from 0.1 to 0.5 mL/h. In addition, it can be seen that higher core solution speed rate could lead to higher PW encapsulation efficiency according to the transmission electron microscopy results. The core-sheath nanofiber films, moreover, possessed the highest latent heat of 58.25 J/g and solidifying enthalpy of -56.49 J/g. In addition, we found that after 200 thermal cycles, there was little change in latent heat, which demonstrated that it is beneficial for the PW-loaded core-sheath structure to overcome the leakage issue and enhance thermal stability properties for the thermoregulation film.

  10. Physical models for the description of an electrodynamically accelerated plasma sheath

    International Nuclear Information System (INIS)

    Zambreanu, V.

    1977-01-01

    An analysis of the models proposed for the description of the plasma sheath dynamics in a coaxial system (of the same type as that operating at the Bucharest Institute of Physics) is presented. A particular attention is paid to the physical structure of the accelerated plasma. It has been shown that a self-consistent model could be derived from a phenomenological description of the sheath structure. The physical models presented so far in the literature have been classified into three groups: the hydrodynamic models, the plasma sheet models and the shock wave models. Each of these models is briefly described. The simplifying assumptions used in the construction of these models have been pointed out. The final conclusion has been that, under these assumptions, none of these models taken separately could completely and correctly describe the dynamical state of the plasma sheath. (author)

  11. Measurements of the sheath potential in low density plasmas

    International Nuclear Information System (INIS)

    Bradley, J.W.; Khamis, R.A.; Sanduk, M.I.; Elliott, J.A.; Rusbridge, M.G.

    1992-01-01

    We have measured the sheath potential around a probe in a range of different plasma conditions in the UMIST, University of Manchester Institute of Science and Technology, quadrupole GOLUX and in a related experiment in which the plasma expands freely to supersonic velocity. In the latter case, the sheath potential agrees well with an appropriately modified form of the usual expression for a field-free plasma, for both hydrogen and argon plasmas. In GOLUX, however, the sheath potential is found to be significantly less than the accepted value, even when the magnetic field is taken into account. For the slow moving plasma in the outer part of the quadrupole confining field, we present both theoretical and experimental results showing that the reduction is due to truncation of the electron velocity distribution as the probe drains electrons from a closed flux tube faster than they can be replaced. In the central hot plasma, however, this explanation cannot apply. Here, the plasma is moving at about sonic speed and magnetic effects are weak. Nevertheless, the results are significantly different from both in the field free experiment. (author)

  12. Double polymer sheathed carbon nanotube supercapacitors show enhanced cycling stability

    Science.gov (United States)

    Zhao, Wenqi; Wang, Shanshan; Wang, Chunhui; Wu, Shiting; Xu, Wenjing; Zou, Mingchu; Ouyang, An; Cao, Anyuan; Li, Yibin

    2015-12-01

    Pseudo-materials are effective in boosting the specific capacitance of supercapacitors, but during service their degradation may also be very strong, causing reduced cycling stability. Here, we show that a carbon nanotube sponge grafted by two conventional pseudo-polymer layers in sequence can serve as a porous supercapacitor electrode with significantly enhanced cycling stability compared with single polymer grafting. Creating conformal polymer coatings on the nanotube surface and the resulting double-sheath configuration are important structural factors leading to the enhanced performance. Combining different polymers as double sheaths as reported here might be a potential route to circumvent the dilemma of pseudo-materials, and to simultaneously improve the capacitance and stability for various energy storage devices.Pseudo-materials are effective in boosting the specific capacitance of supercapacitors, but during service their degradation may also be very strong, causing reduced cycling stability. Here, we show that a carbon nanotube sponge grafted by two conventional pseudo-polymer layers in sequence can serve as a porous supercapacitor electrode with significantly enhanced cycling stability compared with single polymer grafting. Creating conformal polymer coatings on the nanotube surface and the resulting double-sheath configuration are important structural factors leading to the enhanced performance. Combining different polymers as double sheaths as reported here might be a potential route to circumvent the dilemma of pseudo-materials, and to simultaneously improve the capacitance and stability for various energy storage devices. Electronic supplementary information (ESI) available. See DOI: 10.1039/c5nr05978j

  13. Sheath and arc-column voltages in high-pressure arc discharges

    International Nuclear Information System (INIS)

    Benilov, M S; Benilova, L G; Li Heping; Wu Guiqing

    2012-01-01

    Electrical characteristics of a 1 cm-long free-burning atmospheric-pressure argon arc are calculated by means of a model taking into account the existence of a near-cathode space-charge sheath and the discrepancy between the electron and heavy-particle temperatures in the arc column. The computed arc voltage exhibits a variation with the arc current I similar to the one revealed by the experiment and exceeds experimental values by no more than approximately 2 V in the current range 20-175 A. The sheath contributes about two-thirds or more of the arc voltage. The LTE model predicts a different variation of the arc voltage with I and underestimates the experimental values appreciably for low currents but by no more than approximately 2 V for I ≳ 120 A. However, the latter can hardly be considered as a proof of unimportance of the space-charge sheath at high currents: the LTE model overestimates both the resistance of the bulk of the arc column and the resistance of the part of the column that is adjacent to the cathode, and this overestimation to a certain extent compensates for the neglect of the voltage drop in the sheath. Furthermore, if the latter resistance were evaluated in the framework of the LTE model in an accurate way, then the overestimation would be still much stronger and the obtained voltage would significantly exceed those observed in the experiment.

  14. Dengue fever with rectus sheath hematoma: A case report

    Directory of Open Access Journals (Sweden)

    Anurag Sharma

    2014-01-01

    Full Text Available Dengue fever, also known as breakbone fever, is an infectious tropical disease caused by the Dengue virus. It is associated with a number of complications, which are well documented. However, Dengue fever associated with rectus sheath hematoma (RSH is a very rare complication. Only one case report has been published prior supporting the association of Dengue fever with RSH. We report a case of Dengue fever who presented with RSH and was successfully treated conservatively. RSH is also an uncommon cause of acute abdominal pain. It is accumulation of blood in the sheath of the rectus abdominis, secondary to rupture of an epigastric vessel or muscle tear.

  15. Evaluation of the equine digital flexor tendon sheath using diagnostic ultrasound and contrast radiography

    International Nuclear Information System (INIS)

    Redding, W.R.

    1994-01-01

    This study was designed to evaluate the normal anatomy of the digital flexor tendon sheath using contrast radiography and diagnostic ultrasound. Iodinated contrast medium was injected into eight cadaver limbs and the limbs immediately frozen. Lateromedial and dorsopalmar/plantar radiographs were made. These limps were then cut transversely and proximal to distal radiographs of each slab were made. This cross sectional contrast methodology allowed the visualization of the relative size and shape of the superficial and deep digital flexor tendons as well as the potential space taken by effusions of the digital flexor tendon sheath. The second part of the study used twelve live animals with normal digital flexor tendon sheaths. Ultrasonographic measurement of the structures of the digital flexor tendon sheath at each level were compiled. This documented the ability of diagnostic ultrasound to image: 1) the superficial and deep digital flexor tendons, 2) the proximal and distal ring of the manica flexoria, 3) the straight and oblique sesamoidean ligaments, and 4) the mesotendinous attachments to the superficial and deep flexor tendons. Iodinated contrast medium was then injected into the digital flexor tendon sheath and the ultrasonography repeated. These images were compared with those obtained from contrast radiography and prosections of twenty normal limbs. The iodinated contrast medium enhanced sonographic imaging of the structures of the digital tendon sheath, particularly the abaxial borders of the superficial digital flexor tendon branches and the mesotendinous attachments to the superficial and deep digital flexor tendons

  16. Redefinition of the self-bias voltage in a dielectrically shielded thin sheath RF discharge

    Science.gov (United States)

    Ho, Teck Seng; Charles, Christine; Boswell, Rod

    2018-05-01

    In a geometrically asymmetric capacitively coupled discharge where the powered electrode is shielded from the plasma by a layer of dielectric material, the self-bias manifests as a nonuniform negative charging in the dielectric rather than on the blocking capacitor. In the thin sheath regime where the ion transit time across the powered sheath is on the order of or less than the Radiofrequency (RF) period, the plasma potential is observed to respond asymmetrically to extraneous impedances in the RF circuit. Consequently, the RF waveform on the plasma-facing surface of the dielectric is unknown, and the behaviour of the powered sheath is not easily predictable. Sheath circuit models become inadequate for describing this class of discharges, and a comprehensive fluid, electrical, and plasma numerical model is employed to accurately quantify this behaviour. The traditional definition of the self-bias voltage as the mean of the RF waveform is shown to be erroneous in this regime. Instead, using the maxima of the RF waveform provides a more rigorous definition given its correlation with the ion dynamics in the powered sheath. This is supported by a RF circuit model derived from the computational fluid dynamics and plasma simulations.

  17. The role of the sheath in magnetized plasma turbulence and flows

    International Nuclear Information System (INIS)

    Loizu, J.

    2013-01-01

    Controlled nuclear fusion could provide our society with a clean, safe, and virtually inexhaustible source of electric power production. The tokamak has proven to be capable of producing large amounts of fusion reactions by conning magnetically the fusion fuel at sufficiently high density and temperature, thus in the plasma state. Because of turbulence, however, high temperature plasma reaches the outermost region of the tokamak, the Scrape-Off Layer (SOL), which features open magnetic field lines that channel particles and heat into a dedicated region of the vacuum vessel. The plasma dynamics in the SOL is crucial in determining the performance of tokamak devices, and constitutes one of the greatest uncertainties in the success of the fusion program. In the last few years, the development of numerical codes based on reduced fluid models has provided a tool to study turbulence in open field line configurations. In particular, the GBS (Global Braginskii Solver) code has been developed at CRPP and is used to perform global, three-dimensional, full-n, flux-driven simulations of plasma turbulence in open field lines. Reaching predictive capabilities is an outstanding challenge that involves a proper treatment of the plasma-wall interactions at the end of the field lines, to well describe the particle and energy losses. This involves the study of plasma sheaths, namely the layers forming at the interface between plasmas and solid surfaces, where the drift and quasi neutrality approximations break down. This is an investigation of general interest, as sheaths are present in all laboratory plasmas. This thesis presents progress in the understanding of plasma sheaths and their coupling with the turbulence in the main plasma. A kinetic code is developed to study the magnetized plasma-wall transition region and derive a complete set of analytical boundary conditions that supply the sheath physics to fluid codes. These boundary conditions are implemented in the GBS code and

  18. Corrosion

    Science.gov (United States)

    Slabaugh, W. H.

    1974-01-01

    Presents some materials for use in demonstration and experimentation of corrosion processes, including corrosion stimulation and inhibition. Indicates that basic concepts of electrochemistry, crystal structure, and kinetics can be extended to practical chemistry through corrosion explanation. (CC)

  19. Sheath formation of a plasma containing multiply charged ions, cold and hot electrons, and emitted electrons

    International Nuclear Information System (INIS)

    You, H.J.

    2012-01-01

    It is quite well known that ion confinement is an important factor in an electron cyclotron resonance ion source (ECRIS) as it is closely related to the plasma potential. A model of sheath formation was extended to a plasma containing multiply charged ions (MCIs), cold and hot electrons, and secondary electrons emitted either by MCIs or hot electrons. In the model, a modification of the 'Bohm criterion' was given, the sheath potential drop and the critical emission condition were also analyzed. It appears that the presence of hot electrons and emitted electrons strongly affects the sheath formation so that smaller hot electrons and larger emission current result in reduced sheath potential (or floating potential). However the sheath potential was found to become independent of the emission current J when J > J c , (where J c is the critical emission current. The paper is followed by the associated poster

  20. Integrity: A semi-mechanistic model for stress corrosion cracking of fuel

    Energy Technology Data Exchange (ETDEWEB)

    Tayal, M; Hallgrimson, K; Macquarrie, J; Alavi, P [Atomic Energy of Canada Ltd., Mississauga, ON (Canada); Sato, S; Kinoshita, Y; Nishimura, T [Electric Power Development Co. Ltd., Tokyo (Japan)

    1997-08-01

    In this paper we describe the features, validation, and illustrative applications of a semi-mechanistic model, INTEGRITY, which calculates the probability of fuel defects due to stress corrosion cracking. The model expresses the defect probability in terms of fundamental parameters such as local stresses, local strains, and fission product concentration. The assessments of defect probability continue to reflect the influence of conventional parameters like ramped power, power-ramp, burnup and Canlub coating. In addition, the INTEGRITY model provides a mechanism to account for the impacts of additional factors involving detailed fuel design and reactor operation. Some examples of the latter include pellet density, pellet shape and size, sheath diameter and thickness, pellet/sheath clearance, coolant temperature and pressure, etc. The model has been fitted to a database of 554 power-ramp irradiations of CANDU fuel with and without Canlub. For this database the INTEGRITY model calculates 75 defects vs 75 actual defects. Similarly good agreements were noted in the different sub-groups of the data involving non-Canlub, thin-Canlub, and thick-Canlub fuel. Moreover, the shapes and the locations of the defect thresholds were consistent with all the above defects as well as with additional 14 ripple defects that were not in the above database. Two illustrative examples demonstrate how the defect thresholds are influenced by changes in the internal design of the fuel element and by extended burnup. (author). 19 refs, 7 figs.

  1. Integrity: A semi-mechanistic model for stress corrosion cracking of fuel

    International Nuclear Information System (INIS)

    Tayal, M.; Hallgrimson, K.; Macquarrie, J.; Alavi, P.; Sato, S.; Kinoshita, Y.; Nishimura, T.

    1997-01-01

    In this paper we describe the features, validation, and illustrative applications of a semi-mechanistic model, INTEGRITY, which calculates the probability of fuel defects due to stress corrosion cracking. The model expresses the defect probability in terms of fundamental parameters such as local stresses, local strains, and fission product concentration. The assessments of defect probability continue to reflect the influence of conventional parameters like ramped power, power-ramp, burnup and Canlub coating. In addition, the INTEGRITY model provides a mechanism to account for the impacts of additional factors involving detailed fuel design and reactor operation. Some examples of the latter include pellet density, pellet shape and size, sheath diameter and thickness, pellet/sheath clearance, coolant temperature and pressure, etc. The model has been fitted to a database of 554 power-ramp irradiations of CANDU fuel with and without Canlub. For this database the INTEGRITY model calculates 75 defects vs 75 actual defects. Similarly good agreements were noted in the different sub-groups of the data involving non-Canlub, thin-Canlub, and thick-Canlub fuel. Moreover, the shapes and the locations of the defect thresholds were consistent with all the above defects as well as with additional 14 ripple defects that were not in the above database. Two illustrative examples demonstrate how the defect thresholds are influenced by changes in the internal design of the fuel element and by extended burnup. (author). 19 refs, 7 figs

  2. Corrosion in airframes

    OpenAIRE

    PETROVIC ZORAN C.

    2016-01-01

    The introductory chapter provides a brief reference to the issue of corrosion and corrosion damage to aircraft structures. Depending on the nature and dimensions of this non uniformity, three different categories of corrosion are defined: uniform, selective and localized corrosion. The following chapters present the forms of corrosion that can occur in three defined categories of corrosion. Conditions that cause certain types of corrosion in various corrosive environments are discussed. Examp...

  3. Sheath structure in negative ion sources for fusion (invited)

    International Nuclear Information System (INIS)

    McAdams, R.; King, D. B.; Surrey, E.; Holmes, A. J. T.

    2012-01-01

    In fusion negative ion sources, the negative ions are formed on the caesiated plasma grid predominantly by hydrogen atoms from the plasma. The space charge of the negative ions leaving the wall is not fully compensated by incoming positive ions and at high enough emission a virtual cathode is formed. This virtual cathode limits the flux of negative ions transported across the sheath to the plasma. A 1D collisionless model of the sheath is presented taking into account the virtual cathode. The model will be applied to examples of the ion source operation. Extension of the model to the bulk plasma shows good agreement with experimental data. A possible role for fast ions is discussed.

  4. Corrosion engineering

    Energy Technology Data Exchange (ETDEWEB)

    Fontana, M.G.

    1986-01-01

    This book emphasizes the engineering approach to handling corrosion. It presents corrosion data by corrosives or environments rather than by materials. It discusses the corrosion engineering of noble metals, ''exotic'' metals, non-metallics, coatings, mechanical properties, and corrosion testing, as well as modern concepts. New sections have been added on fracture mechanics, laser alloying, nuclear waste isolation, solar energy, geothermal energy, and the Statue of Liberty. Special isocorrosion charts, developed by the author, are introduced as a quick way to look at candidates for a particular corrosive.

  5. Magnetic sheath effect on the gross and net erosion rates due to impurities

    Science.gov (United States)

    Mellet, N.; Pégourié, B.; Martin, C.; Gunn, J. P.; Bufferand, H.; Roubin, P.

    2016-02-01

    Simulations of impurity trajectories in deuterium plasmas in the vicinity of the surface are performed by taking into account the magnetic sheath in conditions relevant for ITER and WEST. We show that the magnetic sheath has a strong effect on the average impact angle of impurities in divertor conditions and that it can lead to an increase of ≈ 60% at the gross erosion maximum for neon (Ne+4) compared to the case when only the cyclotron motion is considered. The evaluation of the net erosion has been undertaken by retaining local redeposition of tungsten (W). We investigate how it is affected by the sheath magnetic potential profile. The largest effect is however observed when an energy distribution is considered. In this case the number of particles that manage to exit the sheath is larger as it is dominated by the more energetic particles. The comparison with other work is also discussed. The application to a scenario of the WEST project is finally performed, which exhibits a moderate, however non negligible, erosion of the plasma facing components.

  6. A smart core-sheath nanofiber that captures and releases red blood cells from the blood

    Science.gov (United States)

    Shi, Q.; Hou, J.; Zhao, C.; Xin, Z.; Jin, J.; Li, C.; Wong, S.-C.; Yin, J.

    2016-01-01

    A smart core-sheath nanofiber for non-adherent cell capture and release is demonstrated. The nanofibers are fabricated by single-spinneret electrospinning of poly(N-isopropylacrylamide) (PNIPAAm), polycaprolactone (PCL) and nattokinase (NK) solution blends. The self-assembly of PNIPAAm and PCL blends during the electrospinning generates the core-sheath PCL/PNIPAAm nanofibers with PNIPAAm as the sheath. The PNIPAAm-based core-sheath nanofibers are switchable between hydrophobicity and hydrophilicity with temperature change and enhance stability in the blood. When the nanofibers come in contact with blood, the NK is released from the nanofibers to resist platelet adhesion on the nanofiber surface, facilitating the direct capture and isolation of red blood cells (RBCs) from the blood above phase-transition temperature of PNIPAAm. Meanwhile, the captured RBCs are readily released from the nanofibers with temperature stimuli in an undamaged manner. The release efficiency of up to 100% is obtained while maintaining cellular integrity and function. This work presents promising nanofibers to effectively capture non-adherent cells and release for subsequent molecular analysis and diagnosis of single cells.A smart core-sheath nanofiber for non-adherent cell capture and release is demonstrated. The nanofibers are fabricated by single-spinneret electrospinning of poly(N-isopropylacrylamide) (PNIPAAm), polycaprolactone (PCL) and nattokinase (NK) solution blends. The self-assembly of PNIPAAm and PCL blends during the electrospinning generates the core-sheath PCL/PNIPAAm nanofibers with PNIPAAm as the sheath. The PNIPAAm-based core-sheath nanofibers are switchable between hydrophobicity and hydrophilicity with temperature change and enhance stability in the blood. When the nanofibers come in contact with blood, the NK is released from the nanofibers to resist platelet adhesion on the nanofiber surface, facilitating the direct capture and isolation of red blood cells (RBCs) from

  7. Sheath-lens probe for negative ion detection in reactive plasmas

    International Nuclear Information System (INIS)

    Stamate, E.; Sugai, H.; Takai, O.; Ohe, K.

    2004-01-01

    A method that allows easy and inexpensive detection of negative ions is introduced. The method is based upon the electrostatic lens effect of the sheath layer evolving to a positively biased planar probe that focuses the negative charges to distinct regions on the surface. Trajectories of negative ions inside the sheath are obtained after computing the potential and electric field distribution by solving in three dimensions the nonlinear Poisson equation. The negative ions' flux to square and disk probes is developed in Ar/SF 6 and O 2 plasmas. The method allows negative ion detection with sensitivity higher than that of Langmuir probes

  8. Achievments of corrosion science and corrosion protection technology

    International Nuclear Information System (INIS)

    Fontana, M.; Stehjl, R.

    1985-01-01

    Problems of corrosion-mechanical strength of metals, effect of corrosive media on creep characteristics are presented. New concepts of the mechanism of corrosion cracking and its relation to hydrogen embrittlement are described. Kinetics and mechanism of hydrogen embrittlement effect on the process of corrosion cracking of different steels and alloys are considered. The dependence of such types of failure on various structural factors is shown. Data on corrosion cracking of high-strength aluminium and titanium alloys, mechanism of the processes and protective methods are given

  9. An integrative time-varying frequency detection and channel sounding method for dynamic plasma sheath

    Science.gov (United States)

    Shi, Lei; Yao, Bo; Zhao, Lei; Liu, Xiaotong; Yang, Min; Liu, Yanming

    2018-01-01

    The plasma sheath-surrounded hypersonic vehicle is a dynamic and time-varying medium and it is almost impossible to calculate time-varying physical parameters directly. The in-fight detection of the time-varying degree is important to understand the dynamic nature of the physical parameters and their effect on re-entry communication. In this paper, a constant envelope zero autocorrelation (CAZAC) sequence based on time-varying frequency detection and channel sounding method is proposed to detect the plasma sheath electronic density time-varying property and wireless channel characteristic. The proposed method utilizes the CAZAC sequence, which has excellent autocorrelation and spread gain characteristics, to realize dynamic time-varying detection/channel sounding under low signal-to-noise ratio in the plasma sheath environment. Theoretical simulation under a typical time-varying radio channel shows that the proposed method is capable of detecting time-variation frequency up to 200 kHz and can trace the channel amplitude and phase in the time domain well under -10 dB. Experimental results conducted in the RF modulation discharge plasma device verified the time variation detection ability in practical dynamic plasma sheath. Meanwhile, nonlinear phenomenon of dynamic plasma sheath on communication signal is observed thorough channel sounding result.

  10. Tunneled dialysis catheter exchange with fibrin sheath disruption is not associated with increased rate of bacteremia.

    Science.gov (United States)

    Valliant, Amanda M; Chaudhry, Muhammad K; Yevzlin, Alexander S; Astor, Brad; Chan, Micah R

    2015-01-01

    Tunneled dialysis catheters are the most common form of vascular access among incident dialysis patients in the United States. Fibrin sheath formation is a frequent cause of late catheter dysfunction requiring an exchange procedure with balloon disruption of the fibrin sheath. It is unknown whether fibrin sheath disruption is associated with increased incidence of bacteremia or catheter failure. We reviewed all tunneled dialysis catheter exchange procedures at the University of Wisconsin between January 2008 and December 2011. The primary outcome was incidence of bacteremia, defined as positive blood cultures within 2 weeks of the procedure. Catheter failure, requiring intervention or replacement, was examined as a secondary outcome. Baseline characteristics examined included diabetic status, gender, race and age. A total of 163 procedures were reviewed; 67 (41.1%) had fibrin sheath disruption and 96 did not. Bacteremia occurred in 4.5% (3/67) of those with and 3.1% (3/97) of those without fibrin sheath disruption (p=0.65). Fibrin sheath disruption was not significantly associated with the risk of catheter failure (adjusted hazard ratio [aHR]=1.34; 95% confidence interval [CI]: 0.87-2.10; p=0.18). Diabetes was associated with greater risk of catheter failure (aHR=1.88; 95% CI: 1.19-2.95; p=0.006), whereas higher age was associated with a lower risk of catheter failure (aHR per 10 years=0.83; 95% CI: 0.72-0.96; p=0.01). This study demonstrates that there is no significant increase in bacteremia and subsequent catheter dysfunction rates after fibrin sheath disruption compared to simple over the wire exchange. These results are encouraging given the large numbers of patients utilizing tunneled catheters for initial hemodialysis access and the known rates of fibrin sheath formation leading to catheter failure.

  11. Erosion–corrosion and corrosion properties of DLC coated low temperature Erosion–corrosion and corrosion properties of DLC coated low temperature

    DEFF Research Database (Denmark)

    Jellesen, Morten Stendahl; Christiansen, Thomas; Hilbert, Lisbeth Rischel

    2009-01-01

    of AISI 316 as substrate for DLC coatings are investigated. Corrosion and erosion–corrosion measurements were carried out on low temperature nitrided stainless steel AISI 316 and on low temperature nitrided stainless steel AISI 316 with a top layer of DLC. The combination of DLC and low temperature...... nitriding dramatically reduces the amount of erosion–corrosion of stainless steel under impingement of particles in a corrosive medium....

  12. The effect of oxygen on the failure of reactor fuel sheaths during a postulated loss-of-coolant accident

    International Nuclear Information System (INIS)

    Ferner, J.; Rosinger, H.E.

    1983-09-01

    The failure model for Zircaloy-4 reactor fuel sheaths was used to study the effect of steam oxidation on sheath burst strain. The model, in the form of a computer program called BURST-3, was used to calculate burst strain for a Zircaloy-4 sheath under arbitrary pressure and temperature sequences in an oxidizing (steam) atmosphere. In particular, BURST-3 was used in a parametric study to predict the sheath behaviour in steam as compared to an inert atmosphere, the effect of heating rate, and the effect of circumferential temperature variations on burst strain. It was found that fuel sheath oxidation, which decreases burst strain, becomes increasingly important with increasing temperature and/or time. An effective oxygen concentration of greater than 0.27 wt. percent will cause the sheath to fail with a negligible strain. The hottest region of a sheath will have the highest oxygen concentration, the largest localized strain, and will be the site of failure. The model predictions were compared to experimental data in the range 900 to 1600 K. Agreement between theory and experiment for all three heating rates (5, 25, and 100 K.s -1 ) was very good

  13. Corrosion Evaluation and Corrosion Control of Steam Generators

    International Nuclear Information System (INIS)

    Maeng, W. Y.; Kim, U. C.; Sung, K. W.; Na, J. W.; Lee, Y. H.; Lee, D. H.; Kim, K. M.

    2008-06-01

    Corrosion damage significantly influences the integrity and efficiency of steam generator. Corrosion problems of steam generator are unsolved issues until now even though much effort is made around world. Especially the stress corrosion cracking of heat exchange materials is the first issue to be solved. The corrosion protection method of steam generator is important and urgent for the guarantee of nuclear plant's integrity. The objectives of this study are 1) to evaluate the corrosion properties of steam generator materials, 2) to optimize the water chemistry of steam generator and 3) to develop the corrosion protection method of primary and secondary sides of steam generator. The results will be reflected to the water chemistry guideline for improving the integrity and efficiency of steam generator in domestic power plants

  14. Transport of negative ions across a double sheath with a virtual cathode

    International Nuclear Information System (INIS)

    McAdams, R; King, D B; Surrey, E; Holmes, A J T

    2011-01-01

    A one-dimensional analytical model of the sheath in a negative ion source, such as those proposed for heating and diagnostic beams on present and future fusion devices, has been developed. The model, which is collisionless, describes the transport of surface produced negative ions from a cathode, across the sheath to a plasma containing electrons, positive ions and negative ions. It accounts for the situation where the emitted flux of negative ions is greater than the space charge limit, where the electric field at the cathode is negative, and a virtual cathode is formed. It is shown that, in the presence of a virtual cathode, there is a maximum current density of negative ions that can be transported across the sheath into the plasma. Furthermore, for high rates of surface production the virtual cathode persists regardless of the negative bias applied to the cathode, so that the current density transported across the sheath is limited. This is a significant observation and implies that present negative ion sources may not be exploiting all of the surface production available. The model is used to calculate the transported negative ion flux in a number of examples. The limitations of the model and proposed future work are also discussed.

  15. FEAST 3.1: finite-element modeling of sheath deformation such as longitudinal ridging and collapse into axial gap

    Energy Technology Data Exchange (ETDEWEB)

    Wang, X.; Xu, Z.; Kim, Y-S.; Lai, L.; Cheng, G.; Xu, S. [Atomic Energy of Canada Limited, Mississauga, Ontario (Canada)

    2010-07-01

    During normal operation, the collapsible CANDU® fuel sheath deforms, especially, it may deform into longitudinal ridges or collapse instantaneously into the axial gaps between the end pellet and endcap or between two neighbouring pellets. These phenomena occur under certain conditions, such as the coolant pressure exceeding critical pressures for longitudinal ridging or axial collapse. Both longitudinal ridging and axial collapse phenomena result from plastic instability in the sheath under coolant pressure. Longitudinal ridging features one or multiple lobes or 'ridges' (outward from the sheath surface) formed along the sheath in the longitudinal direction. Axial collapse features a 'valley' around the sheath circumference. Both phenomena can lead to sheath overstrain, which in turn potentially leads to sheath failure. The LONGER code, which contains empirical correlations, has been used to predict the critical pressures for these two sheath deformation phenomena. To study fuel behaviour outside of the application ranges of the LONGER empirical correlations, a mechanistic model is needed. FEAST (Finite Element Analysis for Stresses) is an AECL computer code used to assess the structural integrity of the CANDU fuel element. The FEAST code has recently been developed (to Version 3.1) to model processes occurring during longitudinal ridge formation and instantaneous collapse into the axial gap. The new models include those for geometric non-linearity (large deformation, large material rotation), non-linear stress-strain curve for plastic deformation, Zr-4 sheath creep law, and variable Young’s Modulus etc. This paper describes the mechanistic model (FEAST 3.1) development for analyses of longitudinal ridging and instantaneous collapse into axial gap, and the comparison with the results from empirical correlations in LONGER. (author)

  16. FEAST 3.1: finite-element modeling of sheath deformation such as longitudinal ridging and collapse into axial gap

    International Nuclear Information System (INIS)

    Wang, X.; Xu, Z.; Kim, Y-S.; Lai, L.; Cheng, G.; Xu, S.

    2010-01-01

    During normal operation, the collapsible CANDU® fuel sheath deforms, especially, it may deform into longitudinal ridges or collapse instantaneously into the axial gaps between the end pellet and endcap or between two neighbouring pellets. These phenomena occur under certain conditions, such as the coolant pressure exceeding critical pressures for longitudinal ridging or axial collapse. Both longitudinal ridging and axial collapse phenomena result from plastic instability in the sheath under coolant pressure. Longitudinal ridging features one or multiple lobes or 'ridges' (outward from the sheath surface) formed along the sheath in the longitudinal direction. Axial collapse features a 'valley' around the sheath circumference. Both phenomena can lead to sheath overstrain, which in turn potentially leads to sheath failure. The LONGER code, which contains empirical correlations, has been used to predict the critical pressures for these two sheath deformation phenomena. To study fuel behaviour outside of the application ranges of the LONGER empirical correlations, a mechanistic model is needed. FEAST (Finite Element Analysis for Stresses) is an AECL computer code used to assess the structural integrity of the CANDU fuel element. The FEAST code has recently been developed (to Version 3.1) to model processes occurring during longitudinal ridge formation and instantaneous collapse into the axial gap. The new models include those for geometric non-linearity (large deformation, large material rotation), non-linear stress-strain curve for plastic deformation, Zr-4 sheath creep law, and variable Young’s Modulus etc. This paper describes the mechanistic model (FEAST 3.1) development for analyses of longitudinal ridging and instantaneous collapse into axial gap, and the comparison with the results from empirical correlations in LONGER. (author)

  17. Corrosion-Activated Micro-Containers for Environmentally Friendly Corrosion Protective Coatings

    Science.gov (United States)

    Li, Wenyan; Buhrow, J. W.; Zhang, X.; Johnsey, M. N.; Pearman, B. P.; Jolley, S. T.; Calle, L. M.

    2016-01-01

    This work concerns the development of environmentally friendly encapsulation technology, specifically designed to incorporate corrosion indicators, inhibitors, and self-healing agents into a coating, in such a way that the delivery of the indicators and inhibitors is triggered by the corrosion process, and the delivery of self-healing agents is triggered by mechanical damage to the coating. Encapsulation of the active corrosion control ingredients allows the incorporation of desired autonomous corrosion control functions such as: early corrosion detection, hidden corrosion detection, corrosion inhibition, and self-healing of mechanical damage into a coating. The technology offers the versatility needed to include one or several corrosion control functions into the same coating.The development of the encapsulation technology has progressed from the initial proof-of-concept work, in which a corrosion indicator was encapsulated into an oil-core (hydrophobic) microcapsule and shown to be delivered autonomously, under simulated corrosion conditions, to a sophisticated portfolio of micro carriers (organic, inorganic, and hybrid) that can be used to deliver a wide range of active corrosion ingredients at a rate that can be adjusted to offer immediate as well as long-term corrosion control. The micro carriers have been incorporated into different coating formulas to test and optimize the autonomous corrosion detection, inhibition, and self-healing functions of the coatings. This paper provides an overview of progress made to date and highlights recent technical developments, such as improved corrosion detection sensitivity, inhibitor test results in various types of coatings, and highly effective self-healing coatings based on green chemistry. The NASA Kennedy Space Centers Corrosion Technology Lab at the Kennedy Space Center in Florida, U.S.A. has been developing multifunctional smart coatings based on the microencapsulation of environmentally friendly corrosion

  18. Magnetically modified sheaths of Leptothrix sp. as an adsorbent for Amido black 10B removal

    International Nuclear Information System (INIS)

    Angelova, Ralitsa; Baldikova, Eva; Pospiskova, Kristyna; Safarikova, Mirka; Safarik, Ivo

    2017-01-01

    The goal of this study was to assess the biosorption of Amido black 10B dye from aqueous solutions on magnetically modified sheaths of Leptothrix sp. in a batch system. The magnetic modification of the sheaths was performed using both microwave synthesized iron oxide nano- and microparticles and perchloric acid stabilized ferrofluid. The native and both magnetically modified sheaths were characterized by SEM. Various parameters significantly affecting the adsorption process, such as pH, contact time, temperature and initial concentration, were studied in detail using the adsorbent magnetized by both methods. The highest adsorption efficiency was achieved at pH 2. The maximum adsorption capacities of both types of magnetized material at room temperature were found to be 339.2 and 286.1 mg of dye per 1 g of ferrofluid modified and microwave synthesized particles modified adsorbent, respectively. Thermodynamic study of dye adsorption revealed a spontaneous and endothermic process in the temperature range between 279.15 and 313.15 K. The data were fitted to various equilibrium and kinetic models. Experimental data matched well with the pseudo-second-order kinetics and Freundlich isotherm model. The Leptothrix sheaths have excellent efficacy for dye adsorption. This material can be used as an effective, low-cost adsorbent. - Highlights: • Magnetic modification of Leptothrix sheaths using two methods is proposed. • Such magnetic material is an excellent adsorbent for Amido black 10B. • The magnetically modified sheaths can be easily separated by magnets.

  19. Magnetically modified sheaths of Leptothrix sp. as an adsorbent for Amido black 10B removal

    Energy Technology Data Exchange (ETDEWEB)

    Angelova, Ralitsa [Department of Nanobiotechnology, Biology Centre, ISB, CAS, Na Sadkach 7, 370 05 Ceske Budejovice (Czech Republic); Department of General and Industrial Microbiology, Faculty of Biology, Sofia University “St. Kliment Ohridski”, 8 Dragan Tsankov Blvd, 1164 Sofia (Bulgaria); Laboratory Microwave Magnetics, Institute of Electronics, Bulgarian Academy of Sciences, 72 Tzarigradsko Chaussee Blvd, 1784 Sofia (Bulgaria); Baldikova, Eva [Global Change Research Institute, CAS, Na Sadkach 7, 370 05 Ceske Budejovice (Czech Republic); Department of Applied Chemistry, Faculty of Agriculture, University of South Bohemia, Branisovska 1457, 370 05 Ceske Budejovice (Czech Republic); Pospiskova, Kristyna [Regional Centre of Advanced Technologies and Materials, Palacky University, Slechtitelu 27, 783 71 Olomouc (Czech Republic); Safarikova, Mirka [Department of Nanobiotechnology, Biology Centre, ISB, CAS, Na Sadkach 7, 370 05 Ceske Budejovice (Czech Republic); Global Change Research Institute, CAS, Na Sadkach 7, 370 05 Ceske Budejovice (Czech Republic); Safarik, Ivo, E-mail: ivosaf@yahoo.com [Department of Nanobiotechnology, Biology Centre, ISB, CAS, Na Sadkach 7, 370 05 Ceske Budejovice (Czech Republic); Global Change Research Institute, CAS, Na Sadkach 7, 370 05 Ceske Budejovice (Czech Republic); Regional Centre of Advanced Technologies and Materials, Palacky University, Slechtitelu 27, 783 71 Olomouc (Czech Republic)

    2017-04-01

    The goal of this study was to assess the biosorption of Amido black 10B dye from aqueous solutions on magnetically modified sheaths of Leptothrix sp. in a batch system. The magnetic modification of the sheaths was performed using both microwave synthesized iron oxide nano- and microparticles and perchloric acid stabilized ferrofluid. The native and both magnetically modified sheaths were characterized by SEM. Various parameters significantly affecting the adsorption process, such as pH, contact time, temperature and initial concentration, were studied in detail using the adsorbent magnetized by both methods. The highest adsorption efficiency was achieved at pH 2. The maximum adsorption capacities of both types of magnetized material at room temperature were found to be 339.2 and 286.1 mg of dye per 1 g of ferrofluid modified and microwave synthesized particles modified adsorbent, respectively. Thermodynamic study of dye adsorption revealed a spontaneous and endothermic process in the temperature range between 279.15 and 313.15 K. The data were fitted to various equilibrium and kinetic models. Experimental data matched well with the pseudo-second-order kinetics and Freundlich isotherm model. The Leptothrix sheaths have excellent efficacy for dye adsorption. This material can be used as an effective, low-cost adsorbent. - Highlights: • Magnetic modification of Leptothrix sheaths using two methods is proposed. • Such magnetic material is an excellent adsorbent for Amido black 10B. • The magnetically modified sheaths can be easily separated by magnets.

  20. Modeling of Sheath Ion-Molecule Reactions in Plasma Enhanced Chemical Vapor Deposition of Carbon Nanotubes

    Science.gov (United States)

    Hash, David B.; Govindan, T. R.; Meyyappan, M.

    2004-01-01

    In many plasma simulations, ion-molecule reactions are modeled using ion energy independent reaction rate coefficients that are taken from low temperature selected-ion flow tube experiments. Only exothermic or nearly thermoneutral reactions are considered. This is appropriate for plasma applications such as high-density plasma sources in which sheaths are collisionless and ion temperatures 111 the bulk p!asma do not deviate significantly from the gas temperature. However, for applications at high pressure and large sheath voltages, this assumption does not hold as the sheaths are collisional and ions gain significant energy in the sheaths from Joule heating. Ion temperatures and thus reaction rates vary significantly across the discharge, and endothermic reactions become important in the sheaths. One such application is plasma enhanced chemical vapor deposition of carbon nanotubes in which dc discharges are struck at pressures between 1-20 Torr with applied voltages in the range of 500-700 V. The present work investigates The importance of the inclusion of ion energy dependent ion-molecule reaction rates and the role of collision induced dissociation in generating radicals from the feedstock used in carbon nanotube growth.

  1. Structural analysis of sheath folds in the Sylacauga Marble Group, Talladega slate belt, southern Appalachians

    Science.gov (United States)

    Mies, J.W.

    1993-01-01

    Remnant blocks of marble from the Moretti-Harrah dimension-stone quarry provide excellent exposure of meter-scale sheath folds. Tubular structures with elliptical cross-sections (4 ???Ryz ??? 5) are the most common expression of the folds. The tubes are elongate subparallel to stretching lineation and are defined by centimeter-scale layers of schist. Eccentrically nested elliptical patterns and opposing asymmetry of folds ('S' and 'Z') are consistent with the sheath-fold interpretation. Sheath folds are locally numerous in the Moretti-Harrah quarry but are not widely distributed in the Sylacauga Marble Group; reconnaissance in neighboring quarries provided no additional observations. The presence of sheath folds in part of the Talladega slate belt indicates a local history of plastic, non-coaxial deformation. Such a history of deformation is substantiated by petrographic study of an extracted hinge from the Moretti-Harrah quarry. The sheath folds are modeled as due to passive amplification of initial structures during simple shear, using both analytic geometry and graphic simulation. As indicated by these models, relatively large shear strains (y ??? 9) and longitudinal initial structures are required. The shear strain presumably relates to NW-directed displacement of overlying crystalline rocks during late Paleozoic orogeny. ?? 1993.

  2. Oxide thickness measurement technique for duplex-layer Zircaloy-4 cladding

    International Nuclear Information System (INIS)

    McClelland, R.G.; O'Leary, P.M.

    1992-01-01

    Siemens Nuclear Power Corporation (SNP) is investigating the use of duplex-layer Zircaloy-4 tubing to improve the waterside corrosion resistance of cladding for high-burnup pressurized water reactor (PWR) fuel designs. Standard SNP PWR cladding is typically 0.762-mm (0.030-in.)-thick Zircaloy-4. The SNP duplex cladding is nominally 0.660-mm (0.026-in.)-thick Zircalloy-4 with an ∼0.102-mm (0.004-in.) outer layer of another, more corrosion-resistant, zirconium-based alloy. It is common industry practice to monitor the in-reactor corrosion behavior of Zircaloy cladding by using an eddy-current 'lift-off' technique to measure the oxide thickness on the outer surface of the fuel cladding. The test program evaluated three different cladding samples, all with the same outer diameter and wall thickness: Zircaloy-4 and duplex clad types D2 and D4

  3. Correlation of the SLAP lesion with lesions of the medial sheath of the biceps tendon and intra-articular subscapularis tendon

    Directory of Open Access Journals (Sweden)

    Bennett William

    2009-01-01

    Full Text Available Background: Superior labral anterior to posterior (SLAP lesions have been well described in the literature and are thought to be secondary to traction injuries to the biceps anchor and/or falls on the outstretched arm. The pulley has recently been described as a structure that aids in the prevention of biceps instability. The intra-articular subscapularis insertion (IASS has been noted to contribute to the robust nature of the medial sheath. The purpose of the study was to determine a potential correlation of SLAP lesions and pulley lesions with/without IASS lesions, (hereafter referred to as medial sheath as forces that can disrupt the biceps anchor and may also disrupt structures of the medial sheath or vice-versa. Materials and Methods: Three hundred and sixteen consecutive shoulder arthroscopies performed by one surgeon were reviewed retrospectively. Operative reports and arthroscopic pictures were carefully reviewed with particular attention paid to the labral and pulley pathology. Selection bias was noted as the author had never operated primarily for a Type 1 SLAP lesion. Following, however, and as such, the exclusion criteria, was a Type 1 SLAP. Results: There were a total of 30 SLAP lesions and a total of 126 medial sheath lesions. There were 13 patients who had both SLAP and medial sheath lesions. There were 17 patients who had a SLAP lesion without a medial sheath lesion. There were 96 medial sheath lesions without a SLAP. A comparison of rates between patients who had a medial sheath lesion with a SLAP and those who had a medial sheath lesion without a SLAP, for the 316 patients, and when tested with a Fisher exact test revealed that there was no statistical significance, P = 0.673. The prevalence of SLAP lesions in this population of 316 patients was 9.4%, Buford 1%, medial sheath lesions 39%, and SLAP and medial sheath lesions 4%. Interestingly, there were three Buford complexes, all associated with a SLAP and one Buford complex

  4. Review on stress corrosion and corrosion fatigue failure of centrifugal compressor impeller

    Science.gov (United States)

    Sun, Jiao; Chen, Songying; Qu, Yanpeng; Li, Jianfeng

    2015-03-01

    Corrosion failure, especially stress corrosion cracking and corrosion fatigue, is the main cause of centrifugal compressor impeller failure. And it is concealed and destructive. This paper summarizes the main theories of stress corrosion cracking and corrosion fatigue and its latest developments, and it also points out that existing stress corrosion cracking theories can be reduced to the anodic dissolution (AD), the hydrogen-induced cracking (HIC), and the combined AD and HIC mechanisms. The corrosion behavior and the mechanism of corrosion fatigue in the crack propagation stage are similar to stress corrosion cracking. The effects of stress ratio, loading frequency, and corrosive medium on the corrosion fatigue crack propagation rate are analyzed and summarized. The corrosion behavior and the mechanism of stress corrosion cracking and corrosion fatigue in corrosive environments, which contain sulfide, chlorides, and carbonate, are analyzed. The working environments of the centrifugal compressor impeller show the behavior and the mechanism of stress corrosion cracking and corrosion fatigue in different corrosive environments. The current research methods for centrifugal compressor impeller corrosion failure are analyzed. Physical analysis, numerical simulation, and the fluid-structure interaction method play an increasingly important role in the research on impeller deformation and stress distribution caused by the joint action of aerodynamic load and centrifugal load.

  5. Abduction of Arm Facilitates Correction of Kinked Peel-Away Sheath During Subclavian Central Line Placement.

    Science.gov (United States)

    Kim, Sunghoon

    2015-12-01

    A tunneled central line catheter placement using a subclavian vein approach can be complicated by an occurrence of peel-away sheath kink which prevents the advancement of the catheter through the sheath. The kink is created due to the angular junction of subclavian and brachiocephalic veins which meet at 90 degree angle. A technique is described which corrects the peel-away sheath kink by extending the subclavian/brachiocephalic vein angle to greater than 90 degrees by abducting the patient's arm. Copyright © 2015 Elsevier Inc. All rights reserved.

  6. Tumor targeted delivery of doxorubicin in malignant peripheral nerve sheath tumors.

    Directory of Open Access Journals (Sweden)

    A B Madhankumar

    Full Text Available Peripheral nerve sheath tumors are benign tumors that have the potential to transform into malignant peripheral nerve sheath tumors (MPNSTs. Interleukin-13 receptor alpha 2 (IL13Rα2 is a cancer associated receptor expressed in glioblastoma and other invasive cancers. We analyzed IL13Rα2 expression in several MPNST cell lines including the STS26T cell line, as well as in several peripheral nerve sheath tumors to utilize the IL13Rα2 receptor as a target for therapy. In our studies, we demonstrated the selective expression of IL13Rα2 in several peripheral nerve sheath tumors by immunohistochemistry (IHC and immunoblots. We established a sciatic nerve MPNST mouse model in NIH III nude mice using a luciferase transfected STS26T MPNST cell line. Similarly, analysis of the mouse sciatic nerves after tumor induction revealed significant expression of IL13Rα2 by IHC when compared to a normal sciatic nerve. IL13 conjugated liposomal doxorubicin was formulated and shown to bind and internalized in the MPNST cell culture model demonstrating cytotoxic effect. Our subsequent in vivo investigation in the STS26T MPNST sciatic nerve tumor model indicated that IL13 conjugated liposomal doxorubicin (IL13LIPDXR was more effective in inhibiting tumor progression compared to unconjugated liposomal doxorubicin (LIPDXR. This further supports that IL13 receptor targeted nanoliposomes is a potential approach for treating MPNSTs.

  7. Corrosion Evaluation and Corrosion Control of Steam Generators

    Energy Technology Data Exchange (ETDEWEB)

    Maeng, W. Y.; Kim, U. C.; Sung, K. W.; Na, J. W.; Lee, Y. H.; Lee, D. H.; Kim, K. M

    2008-06-15

    Corrosion damage significantly influences the integrity and efficiency of steam generator. Corrosion problems of steam generator are unsolved issues until now even though much effort is made around world. Especially the stress corrosion cracking of heat exchange materials is the first issue to be solved. The corrosion protection method of steam generator is important and urgent for the guarantee of nuclear plant's integrity. The objectives of this study are 1) to evaluate the corrosion properties of steam generator materials, 2) to optimize the water chemistry of steam generator and 3) to develop the corrosion protection method of primary and secondary sides of steam generator. The results will be reflected to the water chemistry guideline for improving the integrity and efficiency of steam generator in domestic power plants.

  8. Sheath and heat flow of a two-electron-temperature plasma in the presence of electron emission

    International Nuclear Information System (INIS)

    Sato, Kunihiro; Miyawaki, Fujio

    1992-01-01

    The electrostatic sheath and the heat flow of a two-electron-temperature plasma in the presence of electron emission are investigated analytically. It is shown that the energy flux is markedly enhanced to a value near the electron free-flow energy flux as a result of considerable reduction of the sheath potential due to electron emission if the fraction of hot electrons at the sheath edge is much smaller than one. If the hot- to cold-electron temperature ratio is of the order of ten and the hot electron density is comparable to the cold electron density, the action of the sheath as a thermal insulator is improved as a result of suppression of electron emission due to the space-charge effect of hot electrons. (author)

  9. Acute optic nerve sheath fenestration with the free-electron laser

    Science.gov (United States)

    Shen, Jin-Hui; Casagrande, Vivien A.; Joos, Karen M.; Shetlar, Debra J.; Robinson, Richard D.; Head, William S.; Mavity-Hudson, Julia A.; Nunnally, Amy H.

    1999-06-01

    Purpose: To determine if the free electron laser (FEL) energy can be delivered to a small space to perform optic nerve sheath fenestration with minimal acute nerve damage. Methods: A 530 mm hollow waveguide probe was designed. Optic nerve sheath fenestration (1.0 mm diameter) was performed in 8 rabbits using either the FEL (4 eyes, 6.45mm, 10 Hz, 2 mJ) or a knife (4 eyes). Within 2 hours following surgery, the animals were perfused with aldehyde fixative. The integrity of the optic nerve and glial response at the site of fenestration were evaluated on tissue selections with H&E, and antibodies to S100β or GFAP. Results: Surgery using the FEL probe was found to be technically superior to the knife. The glial reaction was limited to a zone adjacent to the fenestration and was similar in both the FEL and knife incisions. Conclusions: The FEL appears capable of efficiently performing an optic nerve sheath fenestration in a small space with minimal acute damage. Both the FEL and knife incisions result in a rapid glial response at the site of fenestration even when optic nerve integrity is not compromised.

  10. Corrosion cracking

    International Nuclear Information System (INIS)

    Goel, V.S.

    1985-01-01

    This book presents the papers given at a conference on alloy corrosion cracking. Topics considered at the conference included the effect of niobium addition on intergranular stress corrosion cracking, corrosion-fatigue cracking in fossil-fueled-boilers, fracture toughness, fracture modes, hydrogen-induced thresholds, electrochemical and hydrogen permeation studies, the effect of seawater on fatigue crack propagation of wells for offshore structures, the corrosion fatigue of carbon steels in seawater, and stress corrosion cracking and the mechanical strength of alloy 600

  11. Osteocalcin expressing cells from tendon sheaths in mice contribute to tendon repair by activating Hedgehog signaling

    OpenAIRE

    Wang, Yi; Zhang, Xu; Huang, Huihui; Xia, Yin; Yao, YiFei; Mak, Arthur Fuk-Tat; Yung, Patrick Shu-Hang; Chan, Kai-Ming; Wang, Li; Zhang, Chenglin; Huang, Yu; Mak, Kingston King-Lun

    2017-01-01

    Both extrinsic and intrinsic tissues contribute to tendon repair, but the origin and molecular functions of extrinsic tissues in tendon repair are not fully understood. Here we show that tendon sheath cells harbor stem/progenitor cell properties and contribute to tendon repair by activating Hedgehog signaling. We found that Osteocalcin (Bglap) can be used as an adult tendon-sheath-specific marker in mice. Lineage tracing experiments show that Bglap-expressing cells in adult sheath tissues pos...

  12. Optic nerve sheath diameter: A novel way to monitor the brain

    Directory of Open Access Journals (Sweden)

    Seelora Sahu

    2017-01-01

    Full Text Available Measurement and monitoring of intracranial pressure is pivotal in management of brain injured patients. As a rapid and easily done bed side measurement, ultrasonography of the optic nerve sheath diameter presents itself as a possible replacement of the conventional invasive methods of intracranial pressure management. In this review we go through the evolution of optic nerve sheath diameter measurement as a novel marker of predicting raised intracranial pressure, the modalities by which it can be measured as well as its correlation with the invasive methods of intracranial pressure monitoring.

  13. Pipeline corrosion prevention by pH stabilization or corrosion inhibitors

    Energy Technology Data Exchange (ETDEWEB)

    Nyborg, Rolf [Institute for Energy Technology, Oslo (Norway)

    2009-07-01

    In many offshore oil and gas projects the pipeline costs are a considerable part of the investment and can become prohibitively high if the corrosivity of the fluid necessitates the use of corrosion resistant alloys instead of carbon steel. Development of more robust and reliable methods for internal corrosion control can increase the application range of carbon steel and therefore have a large economic impact. Corrosion control of carbon steel pipelines has traditionally often been managed by the use of corrosion inhibitors. The pH stabilization technique has been successfully used for corrosion control of several large wet gas pipelines in the last years. This method has advantages over film forming corrosion inhibitors when no or little formation water is produced. The use of corrosion inhibitors in multiphase pipelines implies several challenges which are not fully accounted for in traditional corrosion inhibitor testing procedures. Specialized test procedures have been developed to take account for the presence of emulsions dispersions and sand and clay particles in corrosion inhibitor testing. (author)

  14. Underground pipeline corrosion

    CERN Document Server

    Orazem, Mark

    2014-01-01

    Underground pipelines transporting liquid petroleum products and natural gas are critical components of civil infrastructure, making corrosion prevention an essential part of asset-protection strategy. Underground Pipeline Corrosion provides a basic understanding of the problems associated with corrosion detection and mitigation, and of the state of the art in corrosion prevention. The topics covered in part one include: basic principles for corrosion in underground pipelines, AC-induced corrosion of underground pipelines, significance of corrosion in onshore oil and gas pipelines, n

  15. Zircaloy-sheathed element rods fitted with thermo-couples

    International Nuclear Information System (INIS)

    Bernardy de Sigoyer, B.; Jacques, F.; Thome, P.

    1963-01-01

    In order to carry out thermal conductivity measurements on UO 2 in conditions similar to those under which fuel rods are used, it was necessary to measure the temperature at the interior of a fuel element sheathed in zircaloy. The temperatures are taken with Thermocoax type thermocouples, that is to say fitted with a very thin sheath of stainless steel or Inconel. It is known also that fusion welding of zircaloy onto stainless steel is impossible and that high temperature welded joints are very difficult because of their aggressiveness. The technique used consists in brazing the thermocouples to relatively large stainless steel parts and then joining these plugs by electron bombardment welding to diffused stainless steel-zircaloy couplings. The properties of these diffused couplings and of the brazed joints were studied; the various stages in the fabrication of the containers are also described. (authors) [fr

  16. The Presence of Turbulent and Ordered Local Structure within the ICME Shock-sheath and Its Contribution to Forbush Decrease

    Energy Technology Data Exchange (ETDEWEB)

    Shaikh, Zubair; Bhaskar, Ankush [Indian Institute of Geomagnetism (IIG), New Panvel, Navi Mumbai-410218 (India); Raghav, Anil, E-mail: raghavanil1984@gmail.com [University Department of Physics, University of Mumbai, Vidyanagari, Santacruz (E), Mumbai-400098 (India)

    2017-08-01

    The transient interplanetary disturbances evoke short-time cosmic-ray flux decrease, which is known as Forbush decrease. The traditional model and understanding of Forbush decrease suggest that the sub-structure of an interplanetary counterpart of coronal mass ejection (ICME) independently contributes to cosmic-ray flux decrease. These sub-structures, shock-sheath, and magnetic cloud (MC) manifest as classical two-step Forbush decrease. The recent work by Raghav et al. has shown multi-step decreases and recoveries within the shock-sheath. However, this cannot be explained by the ideal shock-sheath barrier model. Furthermore, they suggested that local structures within the ICME’s sub-structure (MC and shock-sheath) could explain this deviation of the FD profile from the classical FD. Therefore, the present study attempts to investigate the cause of multi-step cosmic-ray flux decrease and respective recovery within the shock-sheath in detail. A 3D-hodogram method is utilized to obtain more details regarding the local structures within the shock-sheath. This method unambiguously suggests the formation of small-scale local structures within the ICME (shock-sheath and even in MC). Moreover, the method could differentiate the turbulent and ordered interplanetary magnetic field (IMF) regions within the sub-structures of ICME. The study explicitly suggests that the turbulent and ordered IMF regions within the shock-sheath do influence cosmic-ray variations differently.

  17. Ratio of sheath thickness to Debye length for a slightly ionized continuum plasma

    International Nuclear Information System (INIS)

    Hamilton, J.

    1980-01-01

    The penetration of plasma sheaths for spherical probes in a slightly ionized continuum plasma has been computed for values of epsilon (the ratio of ion to electron temperature) of 0.01 and 1.0 with rhosub(p) (the ratio of probe radius to plasma Debye length) set at 5.10,20 and 30. Values of the potential drops at the sheath boundaries are presented

  18. Monitoring corrosion rates and localised corrosion in low conductivity water

    DEFF Research Database (Denmark)

    Hilbert, Lisbeth Rischel

    2006-01-01

    Monitoring of low corrosion rates and localised corrosion in a media with low conductivity is a challenge. In municipal district heating, quality control may be improved by implementing on-line corrosion monitoring if a suitable technique can be identified to measure both uniform and localised...... corrosion. Electrochemical techniques (LPR, EIS, crevice corrosion current) as well as direct measurement techniques (high-sensitive electrical resistance, weight loss) have been applied in operating plants. Changes in the corrosion processes are best monitored in non-aggressive, low conductivity media...

  19. The effect of an auxiliary discharge on anode sheath potentials in a transverse discharge

    International Nuclear Information System (INIS)

    Foster, J.E.; Gallimore, A.D.

    1997-01-01

    A novel scheme that employs the use of an auxiliary discharge has been shown to reduce markedly anode sheath potentials in a transverse discharge. An 8.8 A low-pressure argon discharge in the presence of a transverse magnetic field was used as the plasma source in this study. In such discharges, the transverse flux that is collected by the anode is severely limited due to marked reductions in the transverse diffusion coefficient. Findings of this study indicate that the local electron number density and the transverse flux increase when the auxiliary discharge is operated. Changes in these parameters are reflected in the measured anode sheath voltage. Anode sheath potentials, estimated by using Langmuir probes, were shown to be reduced by over 33% when the auxiliary discharge is operated. These reductions in anode sheath potentials translated into significant reductions in anode power flux as measured using water calorimeter techniques. The reductions in anode power flux also correlate well with changes in the electron transverse flux. Finally, techniques implementing these positive effects in real plasma accelerators are discussed. copyright 1997 American Institute of Physics

  20. Dust charging and charge fluctuations in a weakly collisional radio-frequency sheath at low pressure

    International Nuclear Information System (INIS)

    Piel, Alexander; Schmidt, Christian

    2015-01-01

    Models for the charging of dust particles in the bulk plasma and in the sheath region are discussed. A new model is proposed that describes collision-enhanced ion currents in the sheath. The collisions result in a substantial reduction of the negative charge of the dust. Experimental data for the dust charge in the sheath can be described by this model when a Bi-Maxwellian electron distribution is taken into account. Expressions for the dust charging rate for all considered models are presented and their influence on the rise of the kinetic dust temperature is discussed

  1. Normal tendon sheath of the second to fifth fingers as seen on oblique views

    Energy Technology Data Exchange (ETDEWEB)

    Fischer, E.

    1984-01-01

    Oblique views of the fingers, using a low kilovolt technique, show a portion of the tendon sheaths which can be regarded as representative of the entire sheath. Because of the varying obliquity of each finger, this proportion differs in the fingers. With increasing age the projected portion of the sheath becomes smaller because it is covered by increasing bone formation in the insertion of the tendon sheat. Normal values have been obtained for adults according to their decades; from these, quite minor degrees of tendon sheat thickening can be determined. In camptodactyly of the fifth finger, which is not uncommon, the tendon sheat may be widened in the absence of a tenosynovitis.

  2. Review of corrosion causes and corrosion control in a technical facility

    International Nuclear Information System (INIS)

    Charng, T.; Lansing, F.

    1982-06-01

    Causes of corrosion of metals and their alloys are reviewed. The corrosion mechanism is explained by electrochemical reaction theory. The causes and methods of controlling of both physiochemical corrosion and biological corrosion are presented. Factors which influence the rate of corrosion are also discussed

  3. Magneto-optical investigations of Ag-sheathed Bi-2223 tapes with ferromagnetic shielding

    International Nuclear Information System (INIS)

    Yurchenko, V.V.; Shantsev, D.V.; Galperin, Y.M.; Alamgir, A.K.M.; Han, Z.; Johansen, T.H.

    2007-01-01

    An increase in the critical current and suppression of AC losses in superconducting wires and tapes with soft magnetic sheath have been predicted theoretically and confirmed experimentally. In this work we present the results of magneto-optical investigations on a series of Ag-sheathed Bi-2223 tapes with Ni coating. We visualize distributions of magnetic field at increasing external field and different temperatures, demonstrating a difference between the flux propagation in the superconductor with Ni rims and a reference sample without Ni coating

  4. Magneto-optical investigations of Ag-sheathed Bi-2223 tapes with ferromagnetic shielding

    Energy Technology Data Exchange (ETDEWEB)

    Yurchenko, V.V.; Shantsev, D.V.; Galperin, Y.M. [University of Oslo, Department of Physics, P.O. Box 1048, Blindern, 0316 Oslo (Norway); Alamgir, A.K.M.; Han, Z. [Applied Superconductivity Research Center, Department of Physics, Tsinghua University, Beijing 100084 (China); Johansen, T.H. [University of Oslo, Department of Physics, P.O. Box 1048, Blindern, 0316 Oslo (Norway)], E-mail: tomhj@fys.uio.no

    2007-09-01

    An increase in the critical current and suppression of AC losses in superconducting wires and tapes with soft magnetic sheath have been predicted theoretically and confirmed experimentally. In this work we present the results of magneto-optical investigations on a series of Ag-sheathed Bi-2223 tapes with Ni coating. We visualize distributions of magnetic field at increasing external field and different temperatures, demonstrating a difference between the flux propagation in the superconductor with Ni rims and a reference sample without Ni coating.

  5. Factors in the selection of broiler tube materials for a civil fast reactor

    Energy Technology Data Exchange (ETDEWEB)

    Tyzack, C; Chitty, A

    1975-07-01

    This paper briefly considers some of the factors which must be balanced in the selection of a boiler tube material for a Civil Fast Reactor. The merits and possible demerits of low alloy ferritic steels and the austenitic Alloy 800 are compared with respect to waterside corrosion resistance, mechanical properties, fabrication and weldability and possible effects of exposure to the sodium environment under normal and fault conditions. It is pointed out that although there is operational experience of most of the materials in boiler superheater applications there is little or none in evaporative regimes. (author)

  6. Retroperitoneal and rectus sheath hematomas.

    Science.gov (United States)

    Kasotakis, George

    2014-02-01

    The retroperitoneum is rich in vascular structures and can harbor large hematomas, traumatic or spontaneous. The management of retroperitoneal hematomas depends on the mechanism of injury and whether they are pulsatile/expanding. Rectus sheath hematomas are uncommon abdominal wall hematomas secondary to trauma to the epigastric arteries of the rectus muscle. The common risk factors include anticoagulation, strenuous exercise, coughing, coagulation disorders, and invasive procedures on/through the abdominal wall. The management is largely supportive, with the reversal of anticoagulation and transfusions; angioembolization may be necessary. Copyright © 2014 Elsevier Inc. All rights reserved.

  7. Corrosion/95 conference papers

    International Nuclear Information System (INIS)

    Anon.

    1995-01-01

    The papers in this conference represent the latest technological advances in corrosion control and prevention. The following subject areas are covered: cathodic protection in natural waters; materials for fossil fuel combustion and conversion systems; modern problems in atmospheric corrosion; innovative ideas for controlling the decaying infrastructure; deposits and their effects on corrosion in industry; volatile high temperature and non aqueous corrosion inhibitors; corrosion of light-weight and precoated metals for automotive application; refining industry corrosion; corrosion in pulp and paper industry; arctic/cold weather corrosion; materials selection for waste incinerators and associated equipment; corrosion measurement technology; environmental cracking of materials; advancing technology in the coating industry; corrosion in gas treating; green inhibition; recent advances in corrosion control of rail equipment; velocity effects and erosion corrosion in oil and gas production; marine corrosion; corrosion of materials in nuclear systems; underground corrosion control; corrosion in potable and industrial water systems in buildings and its impact on environmental compliance; deposit related boiler tube failures; boiler systems monitoring and control; recent developments and experiences in reactive metals; microbiologically influenced corrosion; corrosion and corrosion control for steel reinforced concrete; international symposium on the use of 12 and 13 Cr stainless steels in oil and gas production environments; subsea corrosion /erosion monitoring in production facilities; fiberglass reinforced pipe and tubulars in oilfield service; corrosion control technology in power transmission and distribution; mechanisms and methods of scale and deposit control; closing the loop -- results oriented cooling system monitoring and control; and minimization of aqueous discharge

  8. Slit-surface electrospinning: a novel process developed for high-throughput fabrication of core-sheath fibers.

    Directory of Open Access Journals (Sweden)

    Xuri Yan

    Full Text Available In this work, we report on the development of slit-surface electrospinning--a process that co-localizes two solutions along a slit surface to spontaneously emit multiple core-sheath cone-jets at rates of up to 1 L/h. To the best of our knowledge, this is the first time that production of electrospun core-sheath fibers has been scaled to this magnitude. Fibers produced in this study were defect-free (i.e. non-beaded and core-sheath geometry was visually confirmed under scanning electron microscopy. The versatility of our system was demonstrated by fabrication of (1 fibers encapsulating a drug, (2 bicomponent fibers, (3 hollow fibers, and (4 fibers from a polymer that is not normally electrospinnable. Additionally, we demonstrate control of the process by modulating parameters such as flow rate, solution viscosity, and fixture design. The technological achievements demonstrated in this work significantly advance core-sheath electrospinning towards commercial and manufacturing viability.

  9. Formation of Stylet Sheaths in āere (in air from eight species of phytophagous hemipterans from six families (Suborders: Auchenorrhyncha and Sternorrhyncha.

    Directory of Open Access Journals (Sweden)

    J Kent Morgan

    Full Text Available Stylet sheath formation is a common feature among phytophagous hemipterans. These sheaths are considered essential to promote a successful feeding event. Stylet sheath compositions are largely unknown and their mode of solidification remains to be elucidated. This report demonstrates the formation and solidification of in āere (in air produced stylet sheaths by six hemipteran families: Diaphorina citri (Psyllidae, Asian citrus psyllid, Aphis nerii (Aphididae, oleander/milkweed aphid, Toxoptera citricida (Aphididae, brown citrus aphid, Aphis gossypii (Aphididae, cotton melon aphid, Bemisia tabaci biotype B (Aleyrodidae, whitefly, Homalodisca vitripennis (Cicadellidae, glassy-winged sharpshooter, Ferrisia virgata (Pseudococcidae, striped mealybug, and Protopulvinaria pyriformis (Coccidae, pyriform scale. Examination of in āere produced stylet sheaths by confocal and scanning electron microscopy shows a common morphology of an initial flange laid down on the surface of the membrane followed by continuous hollow core structures with sequentially stacked hardened bulbous droplets. Single and multi-branched sheaths were common, whereas mealybug and scale insects typically produced multi-branched sheaths. Micrographs of the in āere formed flanges indicate flange sealing upon stylet bundle extraction in D. citri and the aphids, while the B. tabaci whitefly and H. vitripennis glassy-winged sharpshooter flanges remain unsealed. Structural similarity of in āere sheaths are apparent in stylet sheaths formed in planta, in artificial diets, or in water. The use of 'Solvy', a dissolvable membrane, for intact stylet sheath isolation is reported. These observations illustrate for the first time this mode of stylet sheath synthesis adding to the understanding of stylet sheath formation in phytophagous hemipterans and providing tools for future use in structural and compositional analysis.

  10. EUROCORR 2007 - The European corrosion congress - Progress by corrosion control. Book of Abstracts

    International Nuclear Information System (INIS)

    2007-01-01

    This book of abstracts contains lectures, workshops and posters which were held on the European Corrosion Congress 2007 in Freiburg (Germany). The main topics of the sessions and posters are: 1. Corrosion and scale inhibition; 2. Corrosion by hot gases and combustion products; 3. Nuclear corrosion; 4. Environment sensitive fracture; 5. Surface Science; 6. Physico-chemical methods of corrosion testing; 7. Marine corrosion; 8. Microbial corrosion; 9. Corrosion of steel in concrete; 10. Corrosion in oil and gas production; 11. Coatings; 12. Corrosion in the refinery industry; 13. Cathodic protection; 14. Automotive Corrosion; 15. Corrosion of polymer materials. The main topics of the workshops are: 1. High temperature corrosion in the chemical, refinery and petrochemical industries; 2. Bio-Tribocorrosion; 3. Stress corrosion cracking in nuclear power plants; 4. Corrosion monitoring in nuclear systems; 5. Cathodic protection for marine and offshore environments; 6. Self-healing properties of new surface treatments; 7. Bio-Tribocorrosion - Cost 533/Eureka-ENIWEP-Meeting; 8. Drinking water systems; 9. Heat exchangers for seawater cooling

  11. significance of rice sheath photosynthesis: yield determination by c ...

    African Journals Online (AJOL)

    ACSS

    1State Key Laboratory of Hybrid Rice, Hunan Hybrid Rice Research Center, Changsha 410125, P.R. China. 2School of ... for contribution rates of sheath photosynthesis to economical yield. ..... related processes during ripening in rice plants.

  12. Addition of rectus sheath relaxation incisions to emergency midline laparotomy for peritonitis to prevent fascial dehiscence.

    Science.gov (United States)

    Marwah, Sanjay; Marwah, Nisha; Singh, Mandeep; Kapoor, Ajay; Karwasra, Rajender Kumar

    2005-02-01

    The incidence of fascial dehiscence and incisional hernia after two methods for abdominal wound closure (rectus sheath relaxation incisions and conventional mass closure) was studied in a randomized prospective clinical trial in a consecutive series of 100 patients undergoing midline laparotomy for peritonitis. The two groups were well matched for etiologies of peritonitis, the surgical procedures performed, and the presence of known risk factors for fascial dehiscence. Fifty patients each were randomized either to the conventional continuous mass closure procedure or the rectus sheath relaxation incision technique (designed to increase wound elasticity and decrease tension in the suture line) using identical polypropylene sutures. The incidence of postoperative complications such as duration of ileus, chest infection, and wound infection were not statistically different between the two groups. The intensity of postoperative pain in the rectus sheath relaxation incision group was significantly less. The incidence of wound hematoma was significantly increased in the rectus sheath relaxation incision group. The incidences of fascial dehiscence (16% vs,28%; p cases of peritonitis using the rectus sheath relaxation technique is safe and less painful, provides increased wound elasticity and decreased tension on the suture line, and significantly decreases the incidence of wound dehiscence.

  13. 63 the ethnic question and the challenge of development in nigeria

    African Journals Online (AJOL)

    social policy in effecting necessary attitudinal and behavioral change. .... we talk of real federal presence, one's mind runs to such areas as breaching .... waterside, Mango Estate, Elechi Beach Waterside, Afikpo Waterside, Eleme Close 2, and.

  14. Evaluation of Bcl-2, Bcl-x and Cleaved Caspase-3 in Malignant Peripheral Nerve Sheath Tumors and Neurofibromas

    Directory of Open Access Journals (Sweden)

    KARIN S. CUNHA

    2013-11-01

    Full Text Available AIMS: To study the expression of Bcl-2, Bcl-x, as well the presence of cleaved caspase-3 in neurofibromas and malignant peripheral nerve sheath tumors. The expression of Bcl-2 and Bcl-x and the presence of cleaved caspase 3 were compared to clinicopathological features of malignant peripheral nerve sheath tumors and their impact on survival rates were also investigated. MATERIALS AND METHODS: The evaluation of Bcl-2, Bcl-x and cleaved caspase-3 was performed by immunohistochemistry using tissue microarrays in 28 malignant peripheral nerve sheath tumors and 38 neurofibromas. Immunoquantification was performed by computerized digital image analysis. CONCLUSIONS: Apoptosis is altered in neurofibromas and mainly in malignant peripheral nerve sheath tumors. High levels of cleaved caspase-3 are more common in tumors with more aggressive histological features and it is associated with lower disease free survival of patients with malignant peripheral nerve sheath tumors.

  15. Saber-sheath trachea as a marker of severe airflow obstruction in chronic obstructive pulmonary disease.

    Science.gov (United States)

    Ciccarese, Federica; Poerio, Antonio; Stagni, Silvia; Attinà, Domenico; Fasano, Luca; Carbonara, Paolo; Bacchi Reggiani, Maria Letizia; Zompatori, Maurizio

    2014-02-01

    Saber-sheath trachea is a specific radiographic parameter for chronic obstructive pulmonary disease (COPD), which consists of marked coronal narrowing associated with sagittal widening (tracheal index saber-sheath trachea and clinical-radiological findings in a group of patients with COPD of varying severity. We evaluated the chest radiographs of 71 patients with COPD distributed as follows: GOLD class I, 8/71 (11.3 %); class II, 34/71 (47.9 %); class III, 16/71(22.5 %); class IV, 13/71 (18.3 %). In 52/71 (73.2 %) patients we also evaluated chest computed tomography (CT) scans. We analyzed the prevalence of saber-sheath trachea and its correlation with the Tiffenau index, GOLD stage and radiological signs of COPD. Moreover, we evaluated the sensitivity, specificity and accuracy of chest radiography as compared to CT taken as the gold standard, and the correlation between the radiographic and CT tracheal index. Saber-sheath trachea was found in 18/71 (25.4 %) patients, with a greater prevalence in patients with lower Tiffenau Index (p = 0.02), GOLD stages III-IV and visual severity score 3 (severe) on chest CT. Saber-sheath trachea was not found to be related to other radiological signs of COPD. The sensitivity, specificity and accuracy values of radiography were 72.2, 97.0 and 88.5 %, with perfect concordance between the radiographic and CT tracheal index (p Saber-sheath trachea is linked to the functional severity of airway obstruction, but not to other radiological signs of COPD. Thus, evaluation of the trachea at chest radiography is strongly recommended.

  16. A matching approach to communicate through the plasma sheath surrounding a hypersonic vehicle

    International Nuclear Information System (INIS)

    Gao, Xiaotian; Jiang, Binhao

    2015-01-01

    In order to overcome the communication blackout problem suffered by hypersonic vehicles, a matching approach has been proposed for the first time in this paper. It utilizes a double-positive (DPS) material layer surrounding a hypersonic vehicle antenna to match with the plasma sheath enclosing the vehicle. Analytical analysis and numerical results indicate a resonance between the matched layer and the plasma sheath will be formed to mitigate the blackout problem in some conditions. The calculated results present a perfect radiated performance of the antenna, when the match is exactly built between these two layers. The effects of the parameters of the plasma sheath have been researched by numerical methods. Based on these results, the proposed approach is easier to realize and more flexible to the varying radiated conditions in hypersonic flight comparing with other methods

  17. Corrosion and stress corrosion cracking in supercritical water

    Science.gov (United States)

    Was, G. S.; Ampornrat, P.; Gupta, G.; Teysseyre, S.; West, E. A.; Allen, T. R.; Sridharan, K.; Tan, L.; Chen, Y.; Ren, X.; Pister, C.

    2007-09-01

    Supercritical water (SCW) has attracted increasing attention since SCW boiler power plants were implemented to increase the efficiency of fossil-based power plants. The SCW reactor (SCWR) design has been selected as one of the Generation IV reactor concepts because of its higher thermal efficiency and plant simplification as compared to current light water reactors (LWRs). Reactor operating conditions call for a core coolant temperature between 280 °C and 620 °C at a pressure of 25 MPa and maximum expected neutron damage levels to any replaceable or permanent core component of 15 dpa (thermal reactor design) and 100 dpa (fast reactor design). Irradiation-induced changes in microstructure (swelling, radiation-induced segregation (RIS), hardening, phase stability) and mechanical properties (strength, thermal and irradiation-induced creep, fatigue) are also major concerns. Throughout the core, corrosion, stress corrosion cracking, and the effect of irradiation on these degradation modes are critical issues. This paper reviews the current understanding of the response of candidate materials for SCWR systems, focusing on the corrosion and stress corrosion cracking response, and highlights the design trade-offs associated with certain alloy systems. Ferritic-martensitic steels generally have the best resistance to stress corrosion cracking, but suffer from the worst oxidation. Austenitic stainless steels and Ni-base alloys have better oxidation resistance but are more susceptible to stress corrosion cracking. The promise of grain boundary engineering and surface modification in addressing corrosion and stress corrosion cracking performance is discussed.

  18. Magnetic storm generation by large-scale complex structure Sheath/ICME

    Science.gov (United States)

    Grigorenko, E. E.; Yermolaev, Y. I.; Lodkina, I. G.; Yermolaev, M. Y.; Riazantseva, M.; Borodkova, N. L.

    2017-12-01

    We study temporal profiles of interplanetary plasma and magnetic field parameters as well as magnetospheric indices. We use our catalog of large-scale solar wind phenomena for 1976-2000 interval (see the catalog for 1976-2016 in web-side ftp://ftp.iki.rssi.ru/pub/omni/ prepared on basis of OMNI database (Yermolaev et al., 2009)) and the double superposed epoch analysis method (Yermolaev et al., 2010). Our analysis showed (Yermolaev et al., 2015) that average profiles of Dst and Dst* indices decrease in Sheath interval (magnetic storm activity increases) and increase in ICME interval. This profile coincides with inverted distribution of storm numbers in both intervals (Yermolaev et al., 2017). This behavior is explained by following reasons. (1) IMF magnitude in Sheath is higher than in Ejecta and closed to value in MC. (2) Sheath has 1.5 higher efficiency of storm generation than ICME (Nikolaeva et al., 2015). The most part of so-called CME-induced storms are really Sheath-induced storms and this fact should be taken into account during Space Weather prediction. The work was in part supported by the Russian Science Foundation, grant 16-12-10062. References. 1. Nikolaeva N.S., Y. I. Yermolaev and I. G. Lodkina (2015), Modeling of the corrected Dst* index temporal profile on the main phase of the magnetic storms generated by different types of solar wind, Cosmic Res., 53(2), 119-127 2. Yermolaev Yu. I., N. S. Nikolaeva, I. G. Lodkina and M. Yu. Yermolaev (2009), Catalog of Large-Scale Solar Wind Phenomena during 1976-2000, Cosmic Res., , 47(2), 81-94 3. Yermolaev, Y. I., N. S. Nikolaeva, I. G. Lodkina, and M. Y. Yermolaev (2010), Specific interplanetary conditions for CIR-induced, Sheath-induced, and ICME-induced geomagnetic storms obtained by double superposed epoch analysis, Ann. Geophys., 28, 2177-2186 4. Yermolaev Yu. I., I. G. Lodkina, N. S. Nikolaeva and M. Yu. Yermolaev (2015), Dynamics of large-scale solar wind streams obtained by the double superposed epoch

  19. The Bohm criterion for a dusty plasma sheath

    Indian Academy of Sciences (India)

    undergo temperature fluctuations due to collision, the mean square fluctuation in their temperature is much less than the equilibrium temperature. The problem of sheath dynamics with the plasma–wall interactions is of great importance in a number of areas, viz., plasma ion implantation, high-density com- puter chip ...

  20. Corrosion/96 conference papers

    International Nuclear Information System (INIS)

    Anon.

    1996-01-01

    Topics covered by this conference include: cathodic protection in natural waters; cleaning and repassivation of building HVAC systems; worldwide opportunities in flue gas desulfurization; advancements in materials technology for use in oil and gas service; fossil fuel combustion and conversion; technology of corrosion inhibitors; computers in corrosion control--modeling and information processing; recent experiences and advances of austenitic alloys; managing corrosion with plastics; corrosion measurement technology; corrosion inhibitors for concrete; refining industry; advances in corrosion control for rail and tank trailer equipment; CO 2 corrosion--mechanisms and control; microbiologically influenced corrosion; corrosion in nuclear systems; role of corrosion in boiler failures; effects of water reuse on monitoring and control technology in cooling water applications; methods and mechanisms of scale and deposit control; corrosion detection in petroleum production lines; underground corrosion control; environmental cracking--relating laboratory results and field behavior; corrosion control in reinforced concrete structures; corrosion and its control in aerospace and military hardware; injection and process addition facilities; progress reports on the results of reinspection of deaerators inspected or repaired per RP0590 criteria; near 100% volume solids coating technology and application methods; materials performance in high temperature environments containing halides; impact of toxicity studies on use of corrosion/scale inhibitors; mineral scale deposit control in oilfield related operations; corrosion in gas treating; marine corrosion; cold climate corrosion; corrosion in the pulp and paper industry; gaseous chlorine alternatives in cooling water systems; practical applications of ozone in recirculating cooling water systems; and water reuse in industry. Over 400 papers from this conference have been processed separately for inclusion on the data base

  1. Scattering characteristics of electromagnetic waves in time and space inhomogeneous weakly ionized dusty plasma sheath

    Science.gov (United States)

    Guo, Li-xin; Chen, Wei; Li, Jiang-ting; Ren, Yi; Liu, Song-hua

    2018-05-01

    The dielectric coefficient of a weakly ionised dusty plasma is used to establish a three-dimensional time and space inhomogeneous dusty plasma sheath. The effects of scattering on electromagnetic (EM) waves in this dusty plasma sheath are investigated using the auxiliary differential equation finite-difference time-domain method. Backward radar cross-sectional values of various parameters, including the dust particle radius, charging frequency of dust particles, dust particle concentration, effective collision frequency, rate of the electron density variation with time, angle of EM wave incidence, and plasma frequency, are analysed within the time and space inhomogeneous plasma sheath. The results show the noticeable effects of dusty plasma parameters on EM waves.

  2. Corrosion/94 conference papers

    International Nuclear Information System (INIS)

    Anon.

    1994-01-01

    The approximately 500 papers from this conference are divided into the following sections: Rail transit systems--stray current corrosion problems and control; Total quality in the coatings industry; Deterioration mechanisms of alloys at high temperatures--prevention and remediation; Research needs and new developments in oxygen scavengers; Computers in corrosion control--knowledge based system; Corrosion and corrosivity sensors; Corrosion and corrosion control of steel reinforced concrete structures; Microbiologically influenced corrosion; Practical applications in mitigating CO 2 corrosion; Mineral scale deposit control in oilfield-related operations; Corrosion of materials in nuclear systems; Testing nonmetallics for life prediction; Refinery industry corrosion; Underground corrosion control; Mechanisms and applications of deposit and scale control additives; Corrosion in power transmission and distribution systems; Corrosion inhibitor testing and field application in oil and gas systems; Decontamination technology; Ozone in cooling water applications, testing, and mechanisms; Corrosion of water and sewage treatment, collection, and distribution systems; Environmental cracking of materials; Metallurgy of oil and gas field equipment; Corrosion measurement technology; Duplex stainless steels in the chemical process industries; Corrosion in the pulp and paper industry; Advances in cooling water treatment; Marine corrosion; Performance of materials in environments applicable to fossil energy systems; Environmental degradation of and methods of protection for military and aerospace materials; Rail equipment corrosion; Cathodic protection in natural waters; Characterization of air pollution control system environments; and Deposit-related problems in industrial boilers. Papers have been processed separately for inclusion on the data base

  3. An extension of a high temperature creep model to account for fuel sheath oxidation

    International Nuclear Information System (INIS)

    Boccolini, G.; Valli, G.

    1983-01-01

    Starting from the high-temperature creep model for Zircaloy fuel sheathing, the NIRVANA (developed by AECL), a multilayer model, is proposed in this paper: it includes the outer oxide plus alpha retained layers, and the inner core of beta or alpha plus beta material, all constrained to deform with the same creep rate. The model has been incorporated into the SPARA fuel computer code developed for the transient analysis of fuel rod behaviour in the CIRENE prototype reactor, but it is in principle valid for all Zircaloy fuel sheathings. Its predictions are compared with experimental results from burst tests on BWR and PWR type sheaths; the tests were carried out at CNEN under two research contracts with Ansaldo Meccanico Nucleare and Sigen-Sopren, respectively

  4. Applicability of the Child-Langmuir laws versions for describing the glow discharge cathode sheath in CO2

    Science.gov (United States)

    Lisovskiy, Valeriy; Krol, Hennadii; Osmayev, Ruslan; Yegorenkov, Vladimir

    2016-09-01

    This work is devoted to the determination of the law that may be applicable to the description of the cathode sheath in CO2. To this end three versions of the Child-Langmuir law have been considered - a collision free one (for the ions moving through a cathode sheath without collisions with gas molecules) as well as two collision- related versions- one for a constant mean free path of positive ions and one for a constant mobility of positive ions. The current-voltage characteristics and the cathode sheath thickness of the glow discharge in carbon oxide have been simultaneously measured in the pressure range from 0.05 to 1 Torr and with the discharge current values up to 80 mA. The inter-electrode distance has been chosen such that the discharge consists only of the cathode sheath and a small portion of the negative glow, i.e. the experiments have been performed in short tubes. In this case the voltage drop across the cathode sheath is equal approximately to the voltage drop across the electrodes. In the whole range of the discharge conditions we have studied the cathode sheath characteristics are found to obey correctly only to the Child-Langmuir law version with a constant ion mobility. The reason for this phenomenon may be related with a significant conversion of carbon dioxide molecules.

  5. X-band microwave generation caused by plasma-sheath instability

    International Nuclear Information System (INIS)

    Bliokh, Y.; Felsteiner, J.; Slutsker, Ya. Z.

    2012-01-01

    It is well known that oscillations at the electron plasma frequency may appear due to instability of the plasma sheath near a positively biased electrode immersed in plasma. This instability is caused by transit-time effects when electrons, collected by this electrode, pass through the sheath. Such oscillations appear as low-power short spikes due to additional ionization of a neutral gas in the electrode vicinity. Herein we present first results obtained when the additional ionization was eliminated. We succeeded in prolonging the oscillations during the whole time a positive bias was applied to the electrode. These oscillations could be obtained at much higher frequency than previously reported (tens of GHz compared to few hundreds of MHz) and power of tens of mW. These results in combination with presented theoretical estimations may be useful, e.g., for plasma diagnostics.

  6. Texture gradients in Fe-sheathed ex situ produced MgB2 tapes

    International Nuclear Information System (INIS)

    Lezza, P; Gladyshevskii, R; Abaecherli, V; Fluekiger, R

    2006-01-01

    Superconducting Fe-sheathed MgB 2 monofilamentary tapes have been fabricated by the powder-in-tube technique, varying the particle size of the starting MgB 2 powder and applying either cold or hot rolling during the last deformation process. Measurements of the critical current density J c with the magnetic field applied parallel or perpendicular to the tape surface revealed a pronounced anisotropy for the cold rolled tapes, which was found to increase with increasing particle size and magnetic field strength. The microstructural origin of the J c anisotropy was confirmed by means of x-ray diffraction performed on the filaments after mechanical removal of the sheath. The local texture was studied in a series of diffraction patterns collected at different distances from the filament centre, removing each time some 25 μm of the filament thickness. In the cold rolled tapes, the average orientation of the MgB 2 grains was found to approach a preferred orientation with the crystallographic c-axis perpendicular to the tape surface, near the interface with the sheath; however, the misalignment angle increased towards the centre of the tape. In the hot rolled tapes, for which no J c anisotropy was observed, the grains were found to be approximately randomly oriented. Roughness measurements performed on the side of the Fe sheath in contact with the MgB 2 filament are in agreement with the difference in texture observed for cold and hot rolled tapes

  7. Hyphenation of capillary high-performance ion-exchange chromatography with mass spectrometry using sheath-flow electrospray ionization.

    Science.gov (United States)

    Kochmann, Sven; Matysik, Frank-Michael

    2014-12-15

    Mass spectrometry (MS) is an attractive method for extending capillary-size ion chromatography (cHPIC) to create a valuable technique for speciation analysis. For hyphenation, the aqueous effluent of cHPIC has to be transformed into a volatile mixture for MS while preserving analytical concentrations as well as peak shapes during transfer from cHPIC to MS. Finally, the approach should technically be flexible and easy-to-use. A combination of cHPIC and sheath-flow electrospray ionization (ESI)-MS offers to solve all these challenges. cHPIC/sheath-flow-ESI-TOFMS was used in this study for the speciation analysis of various arsenic model compounds. These model compounds were analyzed with different hyphenation setups and configurations of cHPIC/MS and their respective assets and drawbacks were examined and discussed. The parameters (flow rate and composition of sheath liquid) of sheath-flow ESI and their influence on the performance of the spray and the sensitivity of the detector were investigated and compared with those of sheathless ESI. Using an injection valve to couple cHPIC and MS was found to be the best method for hyphenation, since it constitutes a flexible and dead-volume-free approach. The investigation of sheath-flow ESI revealed that the flow rate of the sheath liquid has to resemble the flow rate of the IC effluent to ensure a stable spray and that a composition of 2-propanol/water/ammonia at 50:50:0.2 (v/v/v) suits most applications without unilaterally promoting the sensitivity for either organic or inorganic compounds. The optimized setup and conditions were successfully applied to the analysis of a mixture of important arsenic species and used to determine limits of detection of organic and inorganic arsenic species (3.7 µg L(-1) elemental arsenic). A method for cHPIC/sheath-flow-ESI-MS was developed. The method was shown to be a valuable tool for speciation and trace analysis. It features no dead volume, fast transfer from IC to MS, only minimal

  8. Ultrastructure of the extracellular matrix of bovine dura mater, optic nerve sheath and sclera.

    Science.gov (United States)

    Raspanti, M; Marchini, M; Della Pasqua, V; Strocchi, R; Ruggeri, A

    1992-10-01

    The sclera, the outermost sheath of the optic nerve and the dura mater have been investigated histologically and ultrastructurally. Although these tissues appear very similar under the light microscope, being dense connective tissues mainly composed of collagen bundles and a limited amount of cells and elastic fibres, they exhibit subtle differences on electron microscopy. In the dura and sclera collagen appears in the form of large, nonuniform fibrils, similar to those commonly found in tendons, while in the optic nerve sheath the fibrils appear smaller and uniform, similar to those commonly observed in reticular tissues, vessel walls and skin. Freeze-fracture also reveals these fibrils to have different subfibrillar architectures, straight or helical, which correspond to 2 distinct forms of collagen fibril previously described (Raspanti et al. 1989). The other extracellular matrix components also vary with the particular collagen fibril structure. Despite their common embryological derivation, the dura mater, optic nerve sheath and sclera exhibit diversification of their extracellular matrix consistent with the mechanical loads to which these tissues are subjected. Our observations indicate that the outermost sheath of the optic nerve resembles the epineurium of peripheral nerves rather than the dura to which it is commonly likened.

  9. Corrosion technology. V. 1

    International Nuclear Information System (INIS)

    Khan, I.H.

    1989-01-01

    This book has been produced for dissemination of information on corrosion technology, corrosion hazards and its control. Chapter one of this book presents an overall view of the subject and chapter 2-5 deals with electrochemical basics, types of corrosion, pourbaix diagrams and form of corrosion. The author explains polarization/kinetics of corrosion, passivity, aqueous corrosion and corrosion testing and monitoring in 6-11 chapters. The author hopes it will provide incentive to all those interested in the corrosion technology. (A.B.)

  10. A Novel Technique Using a Protection Filter During Fibrin Sheath Removal for Implanted Venous Access Device Dysfunction

    Energy Technology Data Exchange (ETDEWEB)

    Sotiriadis, Charalampos; Hajdu, Steven David [University Hospital of Lausanne, Cardiothoracic and Vascular Unit, Department of Radiology (Switzerland); Degrauwe, Sophie [University Hospital of Lausanne, Department of Cardiology (Switzerland); Barras, Heloise; Qanadli, Salah Dine, E-mail: salah.qanadli@chuv.ch [University Hospital of Lausanne, Cardiothoracic and Vascular Unit, Department of Radiology (Switzerland)

    2016-08-15

    With the increased use of implanted venous access devices (IVADs) for continuous long-term venous access, several techniques such as percutaneous endovascular fibrin sheath removal, have been described, to maintain catheter function. Most standard techniques do not capture the stripped fibrin sheath, which is subsequently released in the pulmonary circulation and may lead to symptomatic pulmonary embolism. The presented case describes an endovascular technique which includes stripping, capture, and removal of fibrin sheath using a novel filter device. A 64-year-old woman presented with IVAD dysfunction. Stripping was performed using a co-axial snare to the filter to capture the fibrin sheath. The captured fragment was subsequently removed for visual and pathological verification. No immediate complication was observed and the patient was discharged the day of the procedure.

  11. Genomic and Expression Profiling of Benign and Malignant Nerve Sheath Tumors in Neurofibromatosis Patients

    Science.gov (United States)

    2008-05-01

    DAMD17-03-1-0297 Title: Genomic and Expression Pr ofiling of Benign and Malignant Nerve Sheath Tumors in Neurofibromatosis Patients...have determined the gene expression signature for benign and malignant peripheral nerve sheath tumors and found that the major trend in transformation...However, EGFR data in soft tissue neoplasms is limited. Using a variety of benign and malignant spindle cell neoplasms, we assessed EGFR status by

  12. Extraction of antioxidant pigments from dye sorghum leaf sheaths

    NARCIS (Netherlands)

    Kayode, A.P.P.; Bara, C.A.; Dalode-Vieira, G.; Linnemann, A.R.; Nout, M.J.R.

    2012-01-01

    Extraction of antioxidant biocolorant pigments from leaf sheaths of dye sorghum was optimized. Effects of temperature and ethanol concentration of the extraction solvent on the concentrations of the 3-deoxyanthocyanidins, total phenolics and total anthocyanins, and the colour parameters of the

  13. Ganglion of the Flexor Tendon Sheath at the A2 Pulley - Case Report

    Directory of Open Access Journals (Sweden)

    P Gunaseelan

    2015-03-01

    Full Text Available There are few reported cases of flexor tendon sheath ganglion arising from the A2 pulley. We report a case of a flexor tendon sheath ganglion in a 17-year old female who presented with pain, triggering and a swelling at the base of her right ring finger. During the excision biopsy, a ganglion measuring 0.5×0.8×0.4 cm in size was removed from the A2 pulley area.

  14. Physics of the intermediate layer between a plasma and a collisionless sheath and mathematical meaning of the Bohm criterion

    Energy Technology Data Exchange (ETDEWEB)

    Almeida, N. A.; Benilov, M. S. [Departamento de Fisica, CCCEE, Universidade da Madeira Largo do Municipio, 9000 Funchal (Portugal)

    2012-07-15

    A transformation of the ion momentum equation simplifies a mathematical description of the transition layer between a quasi-neutral plasma and a collisionless sheath and clearly reveals the physics involved. Balance of forces acting on the ion fluid is delicate in the vicinity of the sonic point and weak effects come into play. For this reason, the passage of the ion fluid through the sonic point, which occurs in the transition layer, is governed not only by inertia and electrostatic force but also by space charge and ion-atom collisions and/or ionization. Occurrence of different scenarios of asymptotic matching in the plasma-sheath transition is analyzed by means of simple mathematical examples, asymptotic estimates, and numerical calculations. In the case of a collisionless sheath, the ion speed distribution plotted on the logarithmic scale reveals a plateau in the intermediate region between the sheath and the presheath. The value corresponding to this plateau has the meaning of speed with which ions leave the presheath and enter the sheath; the Bohm speed. The plateau is pronounced reasonably well provided that the ratio of the Debye length to the ion mean free path is of the order of 10{sup -3} or smaller. There is no such plateau if the sheath is collisional and hence no sense in talking of a speed with which ions enter the sheath.

  15. STRETCHY ELECTRONICS. Hierarchically buckled sheath-core fibers for superelastic electronics, sensors, and muscles.

    Science.gov (United States)

    Liu, Z F; Fang, S; Moura, F A; Ding, J N; Jiang, N; Di, J; Zhang, M; Lepró, X; Galvão, D S; Haines, C S; Yuan, N Y; Yin, S G; Lee, D W; Wang, R; Wang, H Y; Lv, W; Dong, C; Zhang, R C; Chen, M J; Yin, Q; Chong, Y T; Zhang, R; Wang, X; Lima, M D; Ovalle-Robles, R; Qian, D; Lu, H; Baughman, R H

    2015-07-24

    Superelastic conducting fibers with improved properties and functionalities are needed for diverse applications. Here we report the fabrication of highly stretchable (up to 1320%) sheath-core conducting fibers created by wrapping carbon nanotube sheets oriented in the fiber direction on stretched rubber fiber cores. The resulting structure exhibited distinct short- and long-period sheath buckling that occurred reversibly out of phase in the axial and belt directions, enabling a resistance change of less than 5% for a 1000% stretch. By including other rubber and carbon nanotube sheath layers, we demonstrated strain sensors generating an 860% capacitance change and electrically powered torsional muscles operating reversibly by a coupled tension-to-torsion actuation mechanism. Using theory, we quantitatively explain the complementary effects of an increase in muscle length and a large positive Poisson's ratio on torsional actuation and electronic properties. Copyright © 2015, American Association for the Advancement of Science.

  16. Effects of a reentry plasma sheath on the beam pointing properties of an array antenna

    Directory of Open Access Journals (Sweden)

    Bowen Bai

    2018-03-01

    Full Text Available The reduction in the gain of an on-board antenna caused by a reentry plasma sheath is an important effect that contributes to the reentry “blackout” problem. Using phased array antenna and beamforming technology could provide higher gain and an increase in the communication signal intensity. The attenuation and phase delay of the electromagnetic (EM waves transmitting through the plasma sheath are direction-dependent, and the radiation pattern of the phased array antenna is affected, leading to a deviation in the beam pointing. In this paper, the far-field pattern of a planar array antenna covered by a plasma sheath is deduced analytically by considering both refraction and mutual coupling effects. A comparison between the analytic results and the results from an electromagnetic simulation is carried out. The effect of the plasma sheath on the radiation pattern and the beam pointing errors of the phased array antenna is studied systematically, and the derived results could provide useful information for the correction of pointing errors.

  17. A review on pipeline corrosion, in-line inspection (ILI), and corrosion growth rate models

    International Nuclear Information System (INIS)

    Vanaei, H.R.; Eslami, A.; Egbewande, A.

    2017-01-01

    Pipelines are the very important energy transmission systems. Over time, pipelines can corrode. While corrosion could be detected by in-line inspection (ILI) tools, corrosion growth rate prediction in pipelines is usually done through corrosion rate models. For pipeline integrity management and planning selecting the proper corrosion ILI tool and also corrosion growth rate model is important and can lead to significant savings and safer pipe operation. In this paper common forms of pipeline corrosion, state of the art ILI tools, and also corrosion growth rate models are reviewed. The common forms of pipeline corrosion introduced in this paper are Uniform/General Corrosion, Pitting Corrosion, Cavitation and Erosion Corrosion, Stray Current Corrosion, Micro-Bacterial Influenced Corrosion (MIC). The ILI corrosion detection tools assessed in this study are Magnetic Flux Leakage (MFL), Circumferential MFL, Tri-axial MFL, and Ultrasonic Wall Measurement (UT). The corrosion growth rate models considered in this study are single-value corrosion rate model, linear corrosion growth rate model, non-linear corrosion growth rate model, Monte-Carlo method, Markov model, TD-GEVD, TI-GEVD model, Gamma Process, and BMWD model. Strengths and limitations of ILI detection tools, and also corrosion predictive models with some practical examples are discussed. This paper could be useful for those whom are supporting pipeline integrity management and planning. - Highlights: • Different forms of pipeline corrosion are explained. • Common In-Line Inspection (ILI) tools and corrosion growth rate models are introduced. • Strength and limitations of corrosion growth rate models/ILI tools are discussed. • For pipeline integrity management programs using more than one corrosion growth rate model/ILI tool is suggested.

  18. Erosion and erosion-corrosion

    International Nuclear Information System (INIS)

    Isomoto, Yoshinori

    2008-01-01

    It is very difficult to interpret the technical term of erosion-corrosion' which is sometimes encountered in piping systems of power plants, because of complicated mechanisms and several confusing definitions of erosion-corrosion phenomena. 'FAC (flow accelerated corrosion)' is recently introduced as wall thinning of materials in power plant systems, as a representative of 'erosion-corrosion'. FAC is, however, not necessarily well understood and compared with erosion-corrosion. This paper describes firstly the origin, definition and fundamental understandings of erosion and erosion-corrosion, in order to reconsider and reconfirm the phenomena of erosion, erosion-corrosion and FAC. Next, typical mapping of erosion, corrosion, erosion-corrosion and FAC are introduced in flow velocity and environmental corrosiveness axes. The concept of damage rate in erosion-corrosion is finally discussed, connecting dissolution rate, mass transfer of metal ions in a metal oxide film and film growth. (author)

  19. The normal tendon sheath of the second to fifth fingers as seen on oblique views

    International Nuclear Information System (INIS)

    Fischer, E.

    1984-01-01

    Oblique views of the fingers, using a low kilovolt technique, show a portion of the tendon sheaths which can be regarded as representative of the entire sheath. Because of the varying obliquity of each finger, this proportion differs in the fingers. With increasing age the projected portion of the sheath becomes smaller because it is covered by increasing bone formation in the insertion of the tendon sheat. Normal values have been obtained for adults according to their decades; from these, quite minor degrees of tendon sheat thickening can be determined. In camptodactyly of the fifth finger, which is not uncommon, the tendon sheat may be widened in the absence of a tenosynovitis. (orig.) [de

  20. Accelerated Corrosion Testing

    Science.gov (United States)

    1982-12-01

    Treaty Organization, Brussels, 1971), p. 449. 14. D. 0. Sprowls, T. J. Summerson, G. M. Ugianski, S. G. Epstein, and H. L. Craig , Jr., in Stress...National Association of Corrosion Engineers Houston, TX, 1972). 22. H. L. Craig , Jr. (ed.), Stress Corrosion-New Approaches, ASTM-STP- 610 (American...62. M. Hishida and H. Nakada, Corrosion 33 (11) 403 (1977). b3. D. C. Deegan and B. E. Wilde, Corrosion 34 (6), 19 (1978). 64. S. Orman, Corrosion Sci

  1. Salvianolic acid B protects the myelin sheath around injured spinal cord axons

    Directory of Open Access Journals (Sweden)

    Zhe Zhu

    2016-01-01

    Full Text Available Salvianolic acid B, an active pharmaceutical compound present in Salvia miltiorrhiza, exerts a neuroprotective effect in animal models of brain and spinal cord injury. Salvianolic acid B can promote recovery of neurological function; however, its protective effect on the myelin sheath after spinal cord injury remains poorly understood. Thus, in this study, in vitro tests showed that salvianolic acid B contributed to oligodendrocyte precursor cell differentiation, and the most effective dose was 20 μg/mL. For in vivo investigation, rats with spinal cord injury were intraperitoneally injected with 20 mg/kg salvianolic acid B for 8 weeks. The amount of myelin sheath and the number of regenerating axons increased, neurological function recovered, and caspase-3 expression was decreased in the spinal cord of salvianolic acid B-treated animals compared with untreated control rats. These results indicate that salvianolic acid B can protect axons and the myelin sheath, and can promote the recovery of neurological function. Its mechanism of action is likely to be associated with inhibiting apoptosis and promoting the differentiation and maturation of oligodendrocyte precursor cells.

  2. 3D geometry and kinematic evolution of the Wadi Mayh sheath fold, Oman, using detailed mapping from high-resolution photography

    Science.gov (United States)

    Cornish, Sam; Searle, Mike

    2017-08-01

    The Wadi Mayh sheath fold in north-eastern Oman is one of the largest and best-exposed sheath folds known, and presents a unique opportunity to better understand this somewhat enigmatic style of deformation. We undertook high-resolution photographic surveying along Wadi Mayh to document the sheath fold in 61 georeferenced panoramic photomerges. Here we present ten such images that provide a structural interpretation of the sheath fold and surrounding structure. We resolve this structure in a simplified three-dimensional model and in two orthogonal cross sections, and propose a kinematic evolution to explain the geometry. The Wadi Mayh sheath fold is the most prominent example within what we suggest is a composite sequence of sheath folds, which is itself enclosed within a SSW-closing recumbent syncline at the base of the major Saih Hatat nappe. Sheath folding is accommodated within Permian Saiq Formation limestones showing carpholite assemblages (6-8 kbar; 275-375 °C). A major discontinuity separates this sequence from enveloping older rock units. The sequence formed during progressive top-to-north, ductile shearing as the overlying nappe migrated northwards with respect to the underthrusting Hulw unit. This process occurred during SSW-directed exhumation of partially subducted continental crust in NE Oman, approximately 15 Ma after obduction of the Oman ophiolite initiated.

  3. A study of the effect of circumferential temperature variations on fuel-sheath strain in an inert atmosphere

    International Nuclear Information System (INIS)

    Ferner, J.; Rondeau, R.K.; Rosinger, H.E.

    1983-07-01

    A failure model for Zircaloy-4 fuel sheaths has been developed and used to predict the effect of circumferential temperature variations (ΔT) on fuel-sheath strain behaviour in an inert atmosphere. In addition, experimental data were generated for fuel-sheath failures in the α and (α+β)-phase regions and compared to the predictions of the model. For both the experimental data and the model predictions it was found that increasing ΔT decreases sheath strain. Most of the reduction in burst strain with increasing ΔT occurs in the first 15 K to 20 K. For high ΔT values, burst strains in the α- and (α+β)-phase regions tend to an asymptotic value in the range 5 to 20 percent, irrespective of both heating rate and circumferential temperature variation. The BURST-2 computer code was used for these calculations

  4. FUNCTION OF MALATDEHYDROGENASE COMPLEX OF MAIZE MESOPHYLL AND BUNDLE SHEATH CELLS UNDER SALT STRESS CONDITION

    Directory of Open Access Journals (Sweden)

    Еprintsev А.Т.

    2006-12-01

    Full Text Available Salt-induced changes in malatdehydrogenase system activity make the essential contribution to cell adaptation to stress condition. The enzyme systems of C4-plants are most interesting due to their ability for adaptation to environment conditions. The role of separate components of malatdehydrogenase complex of mesophyll and bundle sheath cells of corn in formation of adaptive reaction in stressful conditions is investigated in presented work.The activation of all enzymes of malatdehydrogenase system and the subsequent decrease in their activity was observed in mesophyll durring the first stage of adaptation to salt influence. In bundle sheath cells such parameters are differed from control less essentially. Fast accumulation of piruvate in cells and malate in both investigated tissues was induced. The further salinity led to falling of concentration this intermediate. The concentration of piruvate was below control level, and it was raised by the end of an exposition.The results show that sodium chloride causes induction of Krebs-cycle in mesophyll and bundle sheath cells of corn and intensification of Hatch-Slack cycle. The described differences in function malatdehydrogenase systems of mesophyll and bundle sheath cells of leaves of corn under salinity mainly consist of the activity of enzymes of a studied complex in bundle sheath cells is subject to the minimal changes in comparison with mesophyll. Role of this enzymesystem in mechanisms of adaptive reaction of various tissues of corn to salt stress is discussed.

  5. Concrete cover cracking with reinforcement corrosion of RC beam during chloride-induced corrosion process

    International Nuclear Information System (INIS)

    Zhang Ruijin; Castel, Arnaud; Francois, Raoul

    2010-01-01

    This paper deals with the evolution of the corrosion pattern based on two beams corroded by 14 years (beam B1CL1) and 23 years (beam B2CL1) of conservation in a chloride environment. The experimental results indicate that, at the cracking initiation stage and the first stage of cracking propagation, localized corrosion due to chloride ingress is the predominant corrosion pattern and pitting corrosion is the main factor that influences the cracking process. As corrosion cracking increases, general corrosion develops rapidly and gradually becomes predominant in the second stage of cracking propagation. A comparison between existing models and experimental results illustrates that, although Vidal et al.'s model can better predict the reinforcement corrosion of beam B1CL1 under localized corrosion, it cannot predict the corrosion of beam B2CL1 under general corrosion. Also, Rodriguez's model, derived from the general corrosion due to electrically accelerated corrosion experiments, cannot match natural chloride corrosion irrespective of whether corrosion is localized or general. Thus, for natural general corrosion in the second stage of cracking propagation, a new model based on the parameter of average steel cross-section loss is put forward to predict steel corrosion from corrosion cracking.

  6. Humid-air and aqueous corrosion models for corrosion-allowance barrier material

    International Nuclear Information System (INIS)

    Lee, J.H.; Atkins, J.E.; Andrews, R.W.

    1995-01-01

    Humid-air and aqueous general and pitting corrosion models (including their uncertainties) for the carbon steel outer containment barrier were developed using the corrosion data from literature for a suite of cast irons and carbon steels which have similar corrosion behaviors to the outer barrier material. The corrosion data include the potential effects of various chemical species present in the testing environments. The atmospheric corrosion data also embed any effects of cyclic wetting and drying and salts that may form on the corroding specimen surface. The humid-air and aqueous general corrosion models are consistent in that the predicted humid-air general corrosion rates at relative humidities between 85 and 100% RH are close to the predicted aqueous general corrosion rates. Using the expected values of the model parameters, the model predicts that aqueous pitting corrosion is the most likely failure mode for the carbon steel outer barrier, and an earliest failure (or initial pit penetration) of the 100-mm thick barrier may occur as early as about 500 years if it is exposed continuously to an aqueous condition at between 60 and 70 degrees C

  7. Quantitative measures of corrosion and prevention: application to corrosion in agriculture

    NARCIS (Netherlands)

    Schouten, J.C.; Gellings, P.J.

    1987-01-01

    The corrosion protection factor (c.p.f.) and the corrosion condition (c.c.) are simple instruments for the study and evaluation of the contribution and efficiency of several methods of corrosion prevention and control. The application of c.p.f. and c.c. to corrosion and prevention in agriculture in

  8. Mechanical characterisation of porcine rectus sheath under uniaxial and biaxial tension.

    LENUS (Irish Health Repository)

    Lyons, Mathew

    2014-06-03

    Incisional hernia development is a significant complication after laparoscopic abdominal surgery. Intra-abdominal pressure (IAP) is known to initiate the extrusion of intestines through the abdominal wall, but there is limited data on the mechanics of IAP generation and the structural properties of rectus sheath. This paper presents an explanation of the mechanics of IAP development, a study of the uniaxial and biaxial tensile properties of porcine rectus sheath, and a simple computational investigation of the tissue. Analysis using Laplace׳s law showed a circumferential stress in the abdominal wall of approx. 1.1MPa due to an IAP of 11kPa, commonly seen during coughing. Uniaxial and biaxial tensile tests were conducted on samples of porcine rectus sheath to characterise the stress-stretch responses of the tissue. Under uniaxial tension, fibre direction samples failed on average at a stress of 4.5MPa at a stretch of 1.07 while cross-fibre samples failed at a stress of 1.6MPa under a stretch of 1.29. Under equi-biaxial tension, failure occurred at 1.6MPa with the fibre direction stretching to only 1.02 while the cross-fibre direction stretched to 1.13. Uniaxial and biaxial stress-stretch plots are presented allowing detailed modelling of the tissue either in silico or in a surrogate material. An FeBio computational model of the tissue is presented using a combination of an Ogden and an exponential power law model to represent the matrix and fibres respectively. The structural properties of porcine rectus sheath have been characterised and add to the small set of human data in the literature with which it may be possible to develop methods to reduce the incidence of incisional hernia development.

  9. Evaluation of corrosive behavior of SAE 5155 by corrosion environment

    International Nuclear Information System (INIS)

    An, Jae Pil; Park, Keyung Dong

    2005-01-01

    In this study, the influence of shot peening and corrosive condition for corrosion property was investigated on immersed in 3.5% NaCl, 10% HNO 3 + 3% HF, 6% FeCl 3 . The immersion test was performed on two kinds of specimen. The immersion periods was performed 30days. Corrosion potential, weight loss were investigated from experimental results. From test results, the effect of shot peening on the corrosion was evaluated

  10. Malignant peripheral nerve sheath tumor of the oculomotor nerve

    DEFF Research Database (Denmark)

    Kozic, D; Nagulic, M; Ostojic, J

    2006-01-01

    We present the short-term follow-up magnetic resonance (MR) studies and 1H-MR spectroscopy in a child with malignant peripheral nerve sheath tumor of the oculomotor nerve associated with other less aggressive cranial nerve schwannomas. The tumor revealed perineural extension and diffuse nerve...

  11. Three-dimensional Doppler ultrasound findings in healthy wrist and finger tendon sheaths

    DEFF Research Database (Denmark)

    Ammitzboll-Danielsen, Mads; Janta, Iustina; Torp-Pedersen, Søren

    2016-01-01

    interpretation of Doppler signals when diagnosing tenosynovitis. Method Forty healthy participants (20 women and 20 men age 23-67 years) without prior history of arthritis, tendon diseases or present pain in their hands were included. Twenty participants had 3D Doppler US of the second and third finger...... participant. No significant difference in feeding vessels was seen between the radial and carpal level in the wrist (p = 0.06) or between the second and third flexor tendon sheath (p = 0.84). Conclusion Doppler findings in or in close proximity to the tendon sheaths were common in wrists and fingers...

  12. Synergy effect of naphthenic acid corrosion and sulfur corrosion in crude oil distillation unit

    Science.gov (United States)

    Huang, B. S.; Yin, W. F.; Sang, D. H.; Jiang, Z. Y.

    2012-10-01

    The synergy effect of naphthenic acid corrosion and sulfur corrosion at high temperature in crude oil distillation unit was studied using Q235 carbon-manganese steel and 316 stainless steel. The corrosion of Q235 and 316 in corrosion media containing sulfur and/or naphthenic acid at 280 °C was investigated by weight loss, scanning electron microscope (SEM), EDS and X-ray diffractometer (XRD) analysis. The results showed that in corrosion media containing only sulfur, the corrosion rate of Q235 and 316 first increased and then decreased with the increase of sulfur content. In corrosion media containing naphthenic acid and sulfur, with the variations of acid value or sulfur content, the synergy effect of naphthenic acid corrosion and sulfur corrosion has a great influence on the corrosion rate of Q235 and 316. It was indicated that the sulfur accelerated naphthenic acid corrosion below a certain sulfur content but prevented naphthenic acid corrosion above that. The corrosion products on two steels after exposure to corrosion media were investigated. The stable Cr5S8 phases detected in the corrosion products film of 316 were considered as the reason why 316 has greater corrosion resistance to that of Q235.

  13. Degradation of aged plants by corrosion: 'Long cell action' in unresolved corrosion issues

    International Nuclear Information System (INIS)

    Saji, Genn

    2009-01-01

    In a series of previously published papers the author has identified that 'long cell action' corrosion plays a pivotal role in practically all unresolved corrosion issues for all types of nuclear power plants (e.g. PWR/VVER, BWR/RBMK and CANDU). Some of these unresolved issues are IGSCC, PWSCC, AOA and FAC (erosion-corrosion). In conventional corrosion science it is well established that 'long cell action' can seriously accelerate or suppress the local cell corrosion activities. Although long cell action is another fundamental mechanism of corrosion, especially in a 'soil corrosion' arena, potential involvement of this corrosion process has never been studied in nuclear and fossil power plants as far as the author has been able to establish. The author believes that the omission of this basic corrosion mechanism is the root cause of practically all un-resolved corrosion issues. In this paper, the author further elaborated on his assessment to other key corrosion issues, e.g. steam generator and turbine corrosion issues, while briefly summarizing previous discussions for completeness purposes, as well as introducing additional experimental and theoretical evidence of this basic corrosion mechanism. Due to the importance of this potential mechanism the author is calling for institutional review activities and further verification experiments in the form of a joint international project.

  14. Discrete focusing effect of positive ions by a plasma-sheath lens

    International Nuclear Information System (INIS)

    Stamate, E.; Sugai, H.

    2005-01-01

    We demonstrate that the sheath created adjacent to the surface of a negatively biased electrode that interfaces an insulator acts as a lens that focuses the positive ions to distinct regions on the surface. Thus, the positive ion flux is discrete, leading to the formation of a passive surface, of no ion impact, near the edge and an active surface at the center. Trajectories of positive ions within the sheath are obtained by solving in three dimensions the Poisson equation for electrodes of different geometry. Simulations are confirmed by developing the ion flux profile on the electrode surface as the sputtering pattern produced by ion impact. Measurements are performed in a dc plasma produced in Ar gas

  15. Electromagnetic particle in cell modeling of the plasma focus: Current sheath formation and lift off

    International Nuclear Information System (INIS)

    Seng, Y. S.; Lee, P.; Rawat, R. S.

    2014-01-01

    The shaping and formation of the current sheath takes place in the breakdown phase of a plasma focus device and critically controls the device performance. Electrostatic particle in cell codes, with magnetic effects ignored, have been used to model the breakdown phase. This Letter reports the successful development and implementation of an electromagnetic particle in cell (EMPIC) code, including magnetic effects self-consistently, to simulate the breakdown phase; from the ionization, localization and gliding discharge along the insulator to the time instant of current sheath lift off. The magnetic field was found to be appreciable from the time the current sheath came into contact with the anode with increased local current, initiating the voltage breakdown of the device as a result

  16. Effects of fast monoenergetic electrons on the ion dynamics near the cathode in a pulsed direct current plasma sheath

    International Nuclear Information System (INIS)

    Sharifian, M.; Shokri, B.

    2008-01-01

    A detailed one-dimensional simulation of the ion dynamics of the plasma sheath near a substrate (cathode) in the presence of fast monoenergetic electrons has been carried out in this article. The sheath evolution is investigated by using a fluid model assuming that the ions, plasma electrons and monoenergetic, fast electrons act as three fluids (fluid approach). The effect of the density of fast electrons on the ion density, ion velocity, and ion energy near the cathode and the evolution of the sheath boundary in front of the cathode are separately explored. Also, the variation of the ion velocity and ion density at the vicinity of the cathode as a function of time is investigated in the absence and presence of the electron beam. Results indicate that the presence of fast electrons in the sheath causes significant change in the sheath thickness and therefore basically changes the ion velocity, ion density, and ion impact energy on the cathode compared to the absence of the electron beam case

  17. The influence of the breakdown electric field in the configuration of lightning corona sheath on charge distribution in the channel

    Science.gov (United States)

    Ignjatovic, Milan; Cvetic, Jovan; Heidler, Fridolin; Markovic, Slavoljub; Djuric, Radivoje

    2014-11-01

    A model of corona sheath that surrounds the thin core of the lightning channel has been investigated by using a generalized traveling current source return stroke model. The lightning channel is modeled by a charged corona sheath that stretches around a highly conductive central core through which the main current flows. The channel core with the negatively charged outer channel sheath forms a strong electric field, with an overall radial orientation. The return stroke process is modeled as the negative leader charge in the corona sheath being discharged by the positive charge coming from the channel core. Expressions that describe how the corona sheath radius evolves during the return stroke are obtained from the corona sheath model, which predicts charge motion within the sheath. The corona sheath model, set forth by Maslowski and Rakov (2006), Tausanovic et al. (2010), Marjanovic and Cvetic (2009), Cvetic et al. (2011) and Cvetic et al. (2012), divides the sheath onto three zones: zone 1 (surrounding the channel core with net positive charge), zone 2 (surrounding zone 1 with negative charge) and zone 3 (the outer zone, representing uncharged virgin air). In the present study, we have assumed a constant electric field inside zone 1, as suggested by experimental research of corona discharges in coaxial geometry conducted by Cooray (2000). The present investigation builds upon previous studies by Tausanovic et al. (2010) and Cvetic et al. (2012) in several ways. The value of the breakdown electric field has been varied for probing its effect on channel charge distribution prior and during the return stroke. With the aim of investigating initial space charge distribution along the channel, total electric field at the outer surface of the channel corona sheath, just before the return stroke, is calculated and compared for various return stroke models. A self-consistent algorithm is applied to the generalized traveling current source return stroke model, so that the

  18. Corrosion Testing Facility

    Data.gov (United States)

    Federal Laboratory Consortium — The Corrosion Testing Facility is part of the Army Corrosion Office (ACO). It is a fully functional atmospheric exposure site, called the Corrosion Instrumented Test...

  19. Fine structure of modal focusing effect in a three dimensional plasma-sheath-lens formed by disk electrodes

    DEFF Research Database (Denmark)

    Stamate, Eugen; Yamaguchi, Masahito

    2015-01-01

    Modal and discrete focusing effects associated with three-dimensional plasma-sheath-lenses show promising potential for applications in ion beam extraction, mass spectrometry, plasma diagnostics and for basic studies of plasma sheath. The ion focusing properties can be adjusted by controlling the...

  20. Synergy effect of naphthenic acid corrosion and sulfur corrosion in crude oil distillation unit

    Energy Technology Data Exchange (ETDEWEB)

    Huang, B.S., E-mail: yinwenfeng2010@163.com [College of Materials Science and Engineering, Southwest Petroleum University, Sichuan, Chengdu, 610500 (China); Yin, W.F. [College of Mechatronic Engineering, Southwest Petroleum University, Sichuan, Chengdu, 610500 (China); Sang, D.H. [Sheng Li Construction Group International Engineering Department, Shandong, Dongying, 257000 (China); Jiang, Z.Y. [College of Materials Science and Engineering, Southwest Petroleum University, Sichuan, Chengdu, 610500 (China)

    2012-10-15

    Highlights: Black-Right-Pointing-Pointer The corrosion of a carbon-manganese steel and a stainless steel in sulfur and/or naphthenic acid media was investigated. Black-Right-Pointing-Pointer The corrosion rate of the carbon-manganese steel increased with the increase of the acid value and sulfur content. Black-Right-Pointing-Pointer The critical values of the concentration of sulfur and acid for corrosion rate of the stainless steel were ascertained respectively. Black-Right-Pointing-Pointer The stainless steel is superior to the carbon-manganese steel in corrosion resistance because of the presence of stable Cr{sub 5}S{sub 8} phases. - Abstract: The synergy effect of naphthenic acid corrosion and sulfur corrosion at high temperature in crude oil distillation unit was studied using Q235 carbon-manganese steel and 316 stainless steel. The corrosion of Q235 and 316 in corrosion media containing sulfur and/or naphthenic acid at 280 Degree-Sign C was investigated by weight loss, scanning electron microscope (SEM), EDS and X-ray diffractometer (XRD) analysis. The results showed that in corrosion media containing only sulfur, the corrosion rate of Q235 and 316 first increased and then decreased with the increase of sulfur content. In corrosion media containing naphthenic acid and sulfur, with the variations of acid value or sulfur content, the synergy effect of naphthenic acid corrosion and sulfur corrosion has a great influence on the corrosion rate of Q235 and 316. It was indicated that the sulfur accelerated naphthenic acid corrosion below a certain sulfur content but prevented naphthenic acid corrosion above that. The corrosion products on two steels after exposure to corrosion media were investigated. The stable Cr{sub 5}S{sub 8} phases detected in the corrosion products film of 316 were considered as the reason why 316 has greater corrosion resistance to that of Q235.

  1. Erosion-corrosion

    International Nuclear Information System (INIS)

    Aghili, B.

    1999-05-01

    A literature study on erosion-corrosion of pipings in the nuclear industry was performed. Occurred incidents are reviewed, and the mechanism driving the erosion-corrosion is described. Factors that influence the effect in negative or positive direction are treated, as well as programs for control and inspection. Finally, examples of failures from databases on erosion-corrosion are given in an attachment

  2. Corrosion behaviors and effects of corrosion products of plasma electrolytic oxidation coated AZ31 magnesium alloy under the salt spray corrosion test

    International Nuclear Information System (INIS)

    Wang, Yan; Huang, Zhiquan; Yan, Qin; Liu, Chen; Liu, Peng; Zhang, Yi; Guo, Changhong; Jiang, Guirong; Shen, Dejiu

    2016-01-01

    Highlights: • Corrosion behaviors of a PEO coating was investigated after the salt spray test. • Corrosion products have significant effects on corrosion behaviors of the coating. • An electrochemical corrosion model is proposed. - Abstract: The effects of corrosion products on corrosion behaviors of AZ31 magnesium alloy with a plasma electrolytic oxidation (PEO) coating were investigated under the salt spray corrosion test (SSCT). The surface morphology, cross-sectional microstructure, chemical and phase compositions of the PEO coating were determined using scanning electron microscopy (SEM) equipped with energy dispersive X-ray spectroscopy (EDS) and X-ray diffraction analysis (XRD), respectively. Further, the corrosion process of the samples under the SSCT was examined in a non-aqueous electrolyte (methanol) using electrochemical impedance spectroscopy (EIS) coupled with equivalent circuit. The results show that the inner layer of the coating was destroyed firstly and the corrosion products have significant effects on the corrosion behaviors of the coating. The results above are discussed and an electrochemical corrosion model is proposed in the paper.

  3. Corrosion behaviors and effects of corrosion products of plasma electrolytic oxidation coated AZ31 magnesium alloy under the salt spray corrosion test

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Yan; Huang, Zhiquan; Yan, Qin; Liu, Chen; Liu, Peng; Zhang, Yi [State Key Laboratory of Metastable Materials Science and Technology, College of Materials Science and Engineering, Yanshan University, Qinhuangdao 066004 (China); Guo, Changhong; Jiang, Guirong [College of Mechanical Engineering, Yanshan University, Qinhuangdao 066004 (China); Shen, Dejiu, E-mail: DejiuShen@163.com [State Key Laboratory of Metastable Materials Science and Technology, College of Materials Science and Engineering, Yanshan University, Qinhuangdao 066004 (China)

    2016-08-15

    Highlights: • Corrosion behaviors of a PEO coating was investigated after the salt spray test. • Corrosion products have significant effects on corrosion behaviors of the coating. • An electrochemical corrosion model is proposed. - Abstract: The effects of corrosion products on corrosion behaviors of AZ31 magnesium alloy with a plasma electrolytic oxidation (PEO) coating were investigated under the salt spray corrosion test (SSCT). The surface morphology, cross-sectional microstructure, chemical and phase compositions of the PEO coating were determined using scanning electron microscopy (SEM) equipped with energy dispersive X-ray spectroscopy (EDS) and X-ray diffraction analysis (XRD), respectively. Further, the corrosion process of the samples under the SSCT was examined in a non-aqueous electrolyte (methanol) using electrochemical impedance spectroscopy (EIS) coupled with equivalent circuit. The results show that the inner layer of the coating was destroyed firstly and the corrosion products have significant effects on the corrosion behaviors of the coating. The results above are discussed and an electrochemical corrosion model is proposed in the paper.

  4. An analytic expression for the sheath criterion in magnetized plasmas with multi-charged ion species

    International Nuclear Information System (INIS)

    Hatami, M. M.

    2015-01-01

    The generalized Bohm criterion in magnetized multi-component plasmas consisting of multi-charged positive and negative ion species and electrons is analytically investigated by using the hydrodynamic model. It is assumed that the electrons and negative ion density distributions are the Boltzmann distribution with different temperatures and the positive ions enter into the sheath region obliquely. Our results show that the positive and negative ion temperatures, the orientation of the applied magnetic field and the charge number of positive and negative ions strongly affect the Bohm criterion in these multi-component plasmas. To determine the validity of our derived generalized Bohm criterion, it reduced to some familiar physical condition and it is shown that monotonically reduction of the positive ion density distribution leading to the sheath formation occurs only when entrance velocity of ion into the sheath satisfies the obtained Bohm criterion. Also, as a practical application of the obtained Bohm criterion, effects of the ionic temperature and concentration as well as magnetic field on the behavior of the charged particle density distributions and so the sheath thickness of a magnetized plasma consisting of electrons and singly charged positive and negative ion species are studied numerically

  5. Study on the Mechanical Properties of Stay Cable HDPE Sheathing Fatigue in Dynamic Bridge Environments

    Directory of Open Access Journals (Sweden)

    Danhui Dan

    2015-08-01

    Full Text Available As the main force-bearing component of a cable-stayed bridge, a durable stay cable is paramount to the safety and durability of the entire bridge. High-density polyethylene (HDPE sheathing is the main protective component of a stay cable and is the key to insuring cable durability. To address the issue of HDPE sheathing fracture on service, strain level data for in-service, HDPE bridge cable sheathing was used in this study as the basis for HDPE material aging and fatigue testing. A fatigue yield phenomenon with a yield platform on the hysteresis curve of the fatigue cycles is observed by the fatigue test. The parameters to describe this phenomenon are proposed and defined in this paper. A preliminary examination of the relationship between these parameters and the factors, such as the number of cycles, the strain amplitude, and strain rate, are presented. Based on the results obtained, it is suggested that the condition of fatigue yield of HDPE sheathing be defined as the fatigue durability limit state for the purposes of durability design, assessment, and protection of cable-stayed bridges.

  6. Out-of-pile fatigue tests on Zircaloy CANDU sheaths

    International Nuclear Information System (INIS)

    Roth, Maria; Ciocanescu, Marin; Gheorghiu, Constantin; Pitigoi, Vasile; Ducu, Catalin; Malinovschi, Viorel

    2005-01-01

    The paper outlines the achievements in the nuclear research field of cooperation on Nuclear Fuel performed as part of the collaboration under the Memorandum of Understanding, settled between Atomic Energy of Canada Limited (AECL) and Institute for Nuclear Research (ICN), The sheath behavior was simulated using out-of-pile fatigue tests, in conditions identical with those met during the operation in power cycling of CANDU reactor, except for irradiation. A special test rig, designed and carried-out at ICN ensured the experimental requirements according to the Canadian testing procedure. The description of the experimental setup and monitoring of testing parameters were also done. The fatigue life time, expressed as number of cycles to rupture (N), was measured as a function of the total strain amplitude (e) induced in the Zircaloy-4 sheath samples. Strain-Life time fatigue dependence (e-N) under low cycle fatigue conditions was also verified using the Coffin-Manson correlation. (authors)

  7. Thermionic emission from monolayer graphene, sheath formation and its feasibility towards thermionic converters

    Science.gov (United States)

    Misra, Shikha; Upadhyay Kahaly, M.; Mishra, S. K.

    2017-02-01

    A formalism describing the thermionic emission from a single layer graphene sheet operating at a finite temperature and the consequent formation of the thermionic sheath in its proximity has been established. The formulation takes account of two dimensional densities of state configuration, Fermi-Dirac (f-d) statistics of the electron energy distribution, Fowler's treatment of electron emission, and Poisson's equation. The thermionic current estimates based on the present analysis is found to be in reasonably good agreement with experimental observations (Zhu et al., Nano Res. 07, 1 (2014)). The analysis has further been simplified for the case where f-d statistics of an electron energy distribution converges to Maxwellian distribution. By using this formulation, the steady state sheath features, viz., spatial dependence of the surface potential and electron density structure in the thermionic sheath are derived and illustrated graphically for graphene parameters; the electron density in the sheath is seen to diminish within ˜10 s of Debye lengths. By utilizing the graphene based cathode in configuring a thermionic converter (TC), an appropriate operating regime in achieving the efficient energy conversion has been identified. A TC configured with the graphene based cathode (operating at ˜1200 K/work function 4.74 V) along with the metallic anode (operating at ˜400 K/ work function 2.0 V) is predicted to display ˜56% of the input thermal flux into the electrical energy, which infers approximately ˜84% of the Carnot efficiency.

  8. Stress corrosion and corrosion fatigue crack growth monitoring in metals

    International Nuclear Information System (INIS)

    Senadheera, T.; Shipilov, S.A.

    2003-01-01

    Environmentally assisted cracking (including stress corrosion cracking and corrosion fatigue) is one of the major causes for materials failure in a wide variety of industries. It is extremely important to understand the mechanism(s) of environmentally assisted crack propagation in structural materials so as to choose correctly from among the various possibilities-alloying elements, heat treatment of steels, parameters of cathodic protection, and inhibitors-to prevent in-service failures due to stress corrosion cracking and corrosion fatigue. An important step towards understanding the mechanism of environmentally assisted crack propagation is designing a testing machine for crack growth monitoring and that simultaneously provides measurement of electrochemical parameters. In the present paper, a direct current (DC) potential drop method for monitoring crack propagation in metals and a testing machine that uses this method and allows for measuring electrochemical parameters during stress corrosion and corrosion fatigue crack growth are described. (author)

  9. General Corrosion and Localized Corrosion of Waste Package Outer Barrier

    Energy Technology Data Exchange (ETDEWEB)

    K.G. Mon

    2004-10-01

    The waste package design for the License Application is a double-wall waste package underneath a protective drip shield (BSC 2004 [DIRS 168489]; BSC 2004 [DIRS 169480]). The purpose and scope of this model report is to document models for general and localized corrosion of the waste package outer barrier (WPOB) to be used in evaluating waste package performance. The WPOB is constructed of Alloy 22 (UNS N06022), a highly corrosion-resistant nickel-based alloy. The inner vessel of the waste package is constructed of Stainless Steel Type 316 (UNS S31600). Before it fails, the Alloy 22 WPOB protects the Stainless Steel Type 316 inner vessel from exposure to the external environment and any significant degradation. The Stainless Steel Type 316 inner vessel provides structural stability to the thinner Alloy 22 WPOB. Although the waste package inner vessel would also provide some performance for waste containment and potentially decrease the rate of radionuclide transport after WPOB breach before it fails, the potential performance of the inner vessel is far less than that of the more corrosion-resistant Alloy 22 WPOB. For this reason, the corrosion performance of the waste package inner vessel is conservatively ignored in this report and the total system performance assessment for the license application (TSPA-LA). Treatment of seismic and igneous events and their consequences on waste package outer barrier performance are not specifically discussed in this report, although the general and localized corrosion models developed in this report are suitable for use in these scenarios. The localized corrosion processes considered in this report are pitting corrosion and crevice corrosion. Stress corrosion cracking is discussed in ''Stress Corrosion Cracking of the Drip Shield, the Waste Package Outer Barrier, and the Stainless Steel Structural Material'' (BSC 2004 [DIRS 169985]).

  10. Corrosion and anticorrosion. Industrial practice

    International Nuclear Information System (INIS)

    Beranger, G.; Mazille, H.

    2002-01-01

    This book comprises 14 chapters written with the collaboration of about 50 French experts of corrosion. It is complementary to another volume entitled 'corrosion of metals and alloys' and published by the same editor. This volume comprises two parts: part 1 presents the basic notions of corrosion phenomena, the properties of surfaces, the electrochemical properties of corrosion etc.. Part 2 describes the most frequent forms of corrosion encountered in industrial environments and corresponding to specific problems of protection: marine environment, atmospheric corrosion, galvanic corrosion, tribo-corrosion, stress corrosion etc.. The first 8 chapters (part 1) treat of the corrosion problems encountered in different industries and processes: oil and gas production, chemical industry, phosphoric acid industry, PWR-type power plants, corrosion of automobile vehicles, civil engineering and buildings, corrosion of biomaterials, non-destructive testing for the monitoring of corrosion. The other chapters (part 2) deal with anticorrosion and protective coatings and means: choice of materials, coatings and surface treatments, thick organic coatings and enamels, paints, corrosion inhibitors and cathodic protection. (J.S.)

  11. Corrosion principles and surface modification

    International Nuclear Information System (INIS)

    Kruger, J.

    1982-01-01

    This chapter examines the important strategies provided by the newer ideas of corrosion science and engineering that surface modification techniques must utilize to help prevent corrosion, especially the most damaging kind of aqueous corrosion, localized corrosion. Provides a brief introduction to the principles underlying the phenomenon of corrosion in order to use them to discuss surface modification strategies to combat corrosion. Discusses the electrochemistry of corrosion; the thermodynamics of corrosion; the kinetics of corrosion; thermodynamic strategies; and kinetic strategies (formation of more protective passive films; resistance to breakdown; ductility; repassivation)

  12. Multimodal imaging in neurofibromatosis type 1-associated nerve sheath tumors; Multimodale Bildgebung bei Neurofibromatose-Typ-1-assoziierten Nervenscheidentumoren

    Energy Technology Data Exchange (ETDEWEB)

    Salamon, J.; Adam, G. [University Medical Center Hamburg-Eppendorf, Hamburg (Germany). Dept. of Diagnostic and Interventional Radiology; Mautner, V.F. [University Medical Center Hamburg-Eppendorf, Hamburg (Germany). Dept. of Neurology; Derlin, T. [Hannover Medical School, Hannover (Germany). Dept. of Nuclear Medicine

    2015-12-15

    Neurofibromatosis type 1 (NF1) is a neurogenetic disorder. Individuals with NF1 may develop a variety of benign and malignant tumors of which peripheral nerve sheath tumors represent the most frequent entity. Plexiform neurofibromas may demonstrate a locally destructive growth pattern, may cause severe symptoms and may undergo malignant transformation into malignant peripheral nerve sheath tumors (MPNSTs). Whole-body magnetic resonance imaging (MRI) represents the reference standard for detection of soft tissue tumors in NF1. It allows for identification of individuals with plexiform neurofibromas, for assessment of local tumor extent, and for evaluation of whole-body tumor burden on T2-weighted imaging. Multiparametric MRI may provide a comprehensive characterization of different tissue properties of peripheral nerve sheath tumors, and may identify parameters associated with malignant transformation. Due to the absence of any radiation exposure, whole-body MRI may be used for serial follow-up of individuals with plexiform neurofibromas. {sup 18}F-fluorodeoxyglucose positron-emission-tomography (FDG PET/CT) allows a highly sensitive and specific detection of MPNST, and should be used in case of potential malignant transformation of a peripheral nerve sheath tumor. PET/CT provides a sensitive whole-body tumor staging. The use of contrast-enhanced CT for diagnosis of peripheral nerve sheath tumors is limited to special indications. To obtain the most precise readings, optimized examination protocols and dedicated radiologists and nuclear medicine physicians familiar with the complex and variable morphologies of peripheral nerve sheath tumors are required.

  13. Accuracy of small diameter sheathed thermocouples for the core flow test loop

    International Nuclear Information System (INIS)

    Anderson, R.L.; Kollie, T.G.

    1979-04-01

    This report summarizes the research and development on 0.5-mm-diameter, compacted, metal sheathed thermocouples. The objectives of this research effort have been: to identify and analyze the sources of temperature measurement errors in the use of 0.5-mm-diameter sheathed thermocouples to measure the surface temperature of the cladding of fuel-rod simulators in the Core Flow Test Loop (CFTL) at ORNL; to devise methods for reducing or correcting for these temperature measurement errors; to estimate the overall temperature measurement uncertainties; and to recommend modifications in the manufacture, installation, or materials used to minimize temperature measurement uncertainties in the CFTL experiments

  14. Hedgehog signaling is required for formation of the notochord sheath and patterning of nuclei pulposi within the intervertebral discs.

    Science.gov (United States)

    Choi, Kyung-Suk; Harfe, Brian D

    2011-06-07

    The vertebrae notochord is a transient rod-like structure that produces secreted factors that are responsible for patterning surrounding tissues. During later mouse embryogenesis, the notochord gives rise to the middle part of the intervertebral disc, called the nucleus pulposus. Currently, very little is known about the molecular mechanisms responsible for forming the intervertebral discs. Here we demonstrate that hedgehog signaling is required for formation of the intervertebral discs. Removal of hedgehog signaling in the notochord and nearby floorplate resulted in the formation of an aberrant notochord sheath that normally surrounds this structure. In the absence of the notochord sheath, small nuclei pulposi were formed, with most notochord cells dispersed throughout the vertebral bodies during embryogenesis. Our data suggest that the formation of the notochord sheath requires hedgehog signaling and that the sheath is essential for maintaining the rod-like structure of the notochord during early embryonic development. As notochord cells form nuclei pulposi, we propose that the notochord sheath functions as a "wrapper" around the notochord to constrain these cells along the vertebral column.

  15. Development of Copper Corrosion Products and Relation between Surface Appearance and Corrosion Rate

    International Nuclear Information System (INIS)

    Lan, Tran Thi Ngoc; Binh, Nguyen Thi Thanh; Tru, Nguyen Nhi; Yoshino, Tsujino; Yasuki, Maeda

    2008-01-01

    Copper was exposed unsheltered and sheltered in four humid tropical sites, representing urban, urban-industrial, urban-marine and rural environments. The corrosion rates and the sequence of corrosion product formation are presented and discussed in relation with climatic and atmospheric pollution parameters. Chemical compositions of corrosion products were found to depend on environments and duration of exposure. In all environments, cuprite was the predominating corrosion product that formed first and continuously increased during the exposure. Among the sulphur-containing corrosion products, posnjakite and brochantite were more frequently found and the first formed earlier. Nantokite was the most common chlorine-containing products for most cases, except the high-chloride environment, where atacamite was detected instead. The corrosion rate of copper was well indicated by the colour of patina. The red-purple colour corresponded to the high corrosion rate and the greenish grey colour corresponded to the low corrosion rate. Corrosion rate of sheltered copper in urban-marine environment increased with the exposure time

  16. Effect of radiofrequency on capacitance of low density plasma sheath

    International Nuclear Information System (INIS)

    Carneiro, L.T.; Cunha Rapozo, C. da

    1988-01-01

    It is shown that the influence of induced radiofrequency potential (V RF ) modifies the Bohm theory on ion saturation current, measured with Langmuir probes. The effect of radiofrequency potential on diode type plasma sheath resonance is also investigated. (M.C.K.)

  17. Study on models for gap conductance between fuel and sheath for CANDU reactors

    International Nuclear Information System (INIS)

    Lee, K.M.; Ohn, M.Y.; Lim, H.S.; Choi, J.H.; Hwang, S.T.

    1995-01-01

    The gap conductance between the fuel and the sheath depends strongly on the gap width and has a significant influence on the amount of initial stored energy. The modified Ross and Stoute gap conductance model in ELESTRES is based on a simplified thermal deformation model for steady-state fuel temperature calculations. A review on a series of experiments reveals that fuel pellets crack, relocate, and are eccentrically positioned within the sheath rather than solid concentric cylinders. In this paper, the two recently-proposed gap conductance models (offset gap model and relocated gap model) are described and are applied to calculate the fuel-sheath gap conductances under experimental conditions and normal operating conditions in CANDU reactors. The good agreement between the experimentally-inferred and calculated gap conductance values demonstrates that the modified Ross and Stoute model was implemented correctly in ELESTRES. The predictions of the modified Ross and Stoute model provide conservative values for gap heat transfer and fuel surface temperature compared to the offset gap and relocated gap models for a limiting power envelope. (author)

  18. Targeting the ECM to Enhance Drug Delivery in Nf1-Associated Nerve Sheath Tumors

    Science.gov (United States)

    2016-10-01

    development of the principal discipline(s) of the project? • We have learned that the drug PEGPH20, which degrades a component of connective tissue called...AWARD NUMBER: W81XWH-15-1-0114 TITLE: Targeting the ECM to Enhance Drug Delivery in Nf1-Associated Nerve Sheath Tumors PRINCIPAL INVESTIGATOR...14 Sep 2016 4. TITLE AND SUBTITLE 5a. CONTRACT NUMBER NF140089 Targeting the ECM to Enhance Drug Delivery in Nf1-Associated Nerve Sheath Tumors 5b

  19. Effect of Flow Velocity on Corrosion Rate and Corrosion Protection Current of Marine Material

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Seong Jong [Kunsan National University, Kunsan (Korea, Republic of); Han, Min Su; Jang, Seok Ki; Kim, Seong Jong [Mokpo National Maritime University, Mokpo (Korea, Republic of)

    2015-10-15

    In spite of highly advanced paint coating techniques, corrosion damage of marine metal and alloys increase more and more due to inherent micro-cracks and porosities in coatings formed during the coating process. Furthermore, flowing seawater conditions promote the breakdown of the protective oxide of the materials introducing more oxygen into marine environments, leading to the acceleration of corrosion. Various corrosion protection methods are available to prevent steel from marine corrosion. Cathodic protection is one of the useful corrosion protection methods by which the potential of the corroded metal is intentionally lowered to an immune state having the advantage of providing additional protection barriers to steel exposed to aqueous corrosion or soil corrosion, in addition to the coating. In the present investigation, the effect of flow velocity was examined for the determination of the optimum corrosion protection current density in cathodic protection as well as the corrosion rate of the steel. It is demonstrated from the result that the material corrosion under dynamic flowing conditions seems more prone to corrosion than under static conditions.

  20. NASA's Beachside Corrosion Test Site and Current Environmentally Friendly Corrosion Control Initiatives

    Science.gov (United States)

    Russell, Richard W.; Calle, Luz Marina; Johnston, Frederick; Montgomery, Eliza L.; Curran, Jerome P.; Kolody, Mark R.

    2013-01-01

    NASA began corrosion studies at the Kennedy Space Center (KSC) in 1966 during the Gemini/Apollo Programs with the evaluation of long-term corrosion protective coatings for carbon steel. KSC's Beachside Corrosion Test Site (BCTS), which has been documented by the American Society of Materials (ASM) as one of the most corrosive, naturally occurring, environments in the world, was established at that time. With the introduction of the Space Shuttle in 1981, the already highly corrosive conditions at the launch pad were rendered even more severe by the acid ic exhaust from the solid rocket boosters. In the years that followed, numerous studies have identified materials, coatings, and maintenance procedures for launch hardware and equipment exposed to the highly corrosive environment at the launch pad. This paper presents a historical overview of over 45 years of corrosion and coating evaluation studies and a description of the BCTS's current capabilities. Additionally, current research and testing programs involving chromium free coatings, environmentally friendly corrosion preventative compounds, and alternates to nitric acid passivation will be discussed.

  1. NASA's Corrosion Technology Laboratory at the Kennedy Space Center: Anticipating, Managing, and Preventing Corrosion

    Science.gov (United States)

    Calle, Luz Marina

    2015-01-01

    The marine environment at NASAs Kennedy Space Center (KSC) has been documented by ASM International (formerly American Society for Metals) as the most corrosive in North America. With the introduction of the Space Shuttle in 1981, the already highly corrosive conditions at the launch pads were rendered even more severe by the highly corrosive hydrochloric acid (HCl) generated by the solid rocket boosters (SRBs). Numerous failures at the launch pads are caused by corrosion. The structural integrity of ground infrastructure and flight hardware is critical to the success, safety, cost, and sustainability of space missions. NASA has over fifty years of experience dealing with unexpected failures caused by corrosion and has developed expertise in corrosion control in the launch and other environments. The Corrosion Technology Laboratory at KSC evolved, from what started as an atmospheric exposure test site near NASAs launch pads, into a capability that provides technical innovations and engineering services in all areas of corrosion for NASA, external partners, and customers.This paper provides a chronological overview of NASAs role in anticipating, managing, and preventing corrosion in highly corrosive environments. One important challenge in managing and preventing corrosion involves the detrimental impact on humans and the environment of what have been very effective corrosion control strategies. This challenge has motivated the development of new corrosion control technologies that are more effective and environmentally friendly. Strategies for improved corrosion protection and durability can have a huge impact on the economic sustainability of human spaceflight operations.

  2. Parallel Transport with Sheath and Collisional Effects in Global Electrostatic Turbulent Transport in FRCs

    Science.gov (United States)

    Bao, Jian; Lau, Calvin; Kuley, Animesh; Lin, Zhihong; Fulton, Daniel; Tajima, Toshiki; Tri Alpha Energy, Inc. Team

    2017-10-01

    Collisional and turbulent transport in a field reversed configuration (FRC) is studied in global particle simulation by using GTC (gyrokinetic toroidal code). The global FRC geometry is incorporated in GTC by using a field-aligned mesh in cylindrical coordinates, which enables global simulation coupling core and scrape-off layer (SOL) across the separatrix. Furthermore, fully kinetic ions are implemented in GTC to treat magnetic-null point in FRC core. Both global simulation coupling core and SOL regions and independent SOL region simulation have been carried out to study turbulence. In this work, the ``logical sheath boundary condition'' is implemented to study parallel transport in the SOL. This method helps to relax time and spatial steps without resolving electron plasma frequency and Debye length, which enables turbulent transports simulation with sheath effects. We will study collisional and turbulent SOL parallel transport with mirror geometry and sheath boundary condition in C2-W divertor.

  3. Density and velocity measurements of a sheath plasma from MPD thruster

    Energy Technology Data Exchange (ETDEWEB)

    Ko, J.J.; Cho, T.S.; Choi, M.C.; Choi, E.H.; Cho, G.S.; Uhm, H.S.

    1999-07-01

    Magnetoplasma is the plasma that the electron and ion orbits are strongly confined by intense magnetic field. Recently, magnetoplasma dynamics (MPD) has been investigated in connection with applications to the rocket thruster in USA, Germany, etc. It can be widely applicable, including modification of satellite position and propulsion of the interplanetary space shuttle. A travel for a long distance journey is possible because a little amount of neutral gases is needed for the plasma source. Besides, this will provide a pollution free engine for future generations. MPD thruster is not a chemical engine. The authors have built a Mather type MPD thruster, which has 1 kV max charging, 10 kA max current flows, and has about 1 ms characteristic operation time. The Paschen curve of this thruster is measured and its minimum breakdown voltage occurs in the pressure range of 0.1 to 1 Torr. Langmuir and double probes are fabricated to diagnose the sheath plasma from the thruster. The temperature and density are calculated to be 2.5 eV and 10{sup 15} cm {sup {minus}3}, respectively, from the probe data. Making use of photo diode, an optical probe is fabricated to measure propagation velocity of the sheath plasma. The sheath plasma from the MPD thruster in the experiment propagates with velocity of 1 cm/{micro}s.

  4. Hemostatic completion of percutaneous nephrolithotomy using electrocauterization and a clear amplatz renal sheath

    Directory of Open Access Journals (Sweden)

    Ho Song Yu

    2016-02-01

    Full Text Available ABSTRACT Background and Purpose A tubeless PCNL can reduce postoperative pain, the need for analgesics, hospital stay, and postoperative urinary leakage. However, perioperative or delayed bleeding remains the primary postoperative concern. We demonstrate a simple and cost-effective method to develop a clear nephrostomy tract after completion of a tubeless PCNL. Materials and Methods Four consecutive patients with renal calculi >3cm underwent a tubeless PCNL. We used a 24 Fr nephroscope and a 24 Fr transurethral resectoscope. Intraoperative urologist-directed percutaneous renal access was performed under fluoroscopy. After calculi removal, active bleeders were identified via a clear Amplatz renal sheath. The sheath provided excellent visualization of the nephrostomy tract for the detection of bleeders and surrounding structures. Bleeders were electrocauterized using a roller barrel electrode. During extraction of the renal sheath, the surgeon can confirm hemostasis in the tract and apply intermittent suction. Results Bleeding primarily originated from the torn calyeceal mucosa and the parenchyma. Tract electrocauterization was successful. All patients had mild hematuria, which resolved within two days. The average hemoglobin decrease was 1.65g/dL (0.8-2.1 and no patients required a transfusion. No perioperative complications occurred. On postoperative day 2, the patients could ambulate without a Foley catheter. During three months of follow-up, delayed bleeding or percutaneous urine leakage did not occur. Conclusions Electrocauterization with a roller barrel electrode and a clear Amplatz renal sheath is an effective method to obtain hemostasis after completion of a PCNL. Our technique is cost-effective and readily adapted without the need for additional instruments.

  5. Fighting corrosion in India

    Energy Technology Data Exchange (ETDEWEB)

    Rajagopalan, K S; Rangaswamy, N S

    1979-03-01

    A survey covers the cost of corrosion in India; methods of preventing corrosion in industrial plants; some case histories, including the prevention of corrosion in pipes through which fuels are pumped to storage and the stress-corrosion cracking of evaporators in fertilizer plants; estimates of the increase in demand in 1979-89 for anticorrosion products and processes developed by the Central Electrochemical Research Institute (CECRI) at Karaikudi, India; industries that may face corrosion problems requiring assistance from CECRI, including the light and heavy engineering structural, and transport industries and the chemical industry; and some areas identified for major efforts, including the establishment of a Corrosion Advisory Board with regional centers and the expansion of the Tropical Corrosion Testing Station at Mandapam Camp, Tamil Nadu.

  6. Electron sheath collapse in an applied-B ion diode

    International Nuclear Information System (INIS)

    Grechikha, A.V.

    1996-01-01

    The effect of the electron sheath collapse in an applied-B ion diode due to the presence of the resistive anode plasma layer was found. This effect is more damaging at higher diode voltages and may be responsible for the parasitic load effect observed in the experiments. (author). 4 figs., 2 refs

  7. Electron sheath collapse in an applied-B ion diode

    Energy Technology Data Exchange (ETDEWEB)

    Grechikha, A V [Forschungszentrum Karlsruhe (Germany). Institut fuer Neutronenphysik und Reaktortechnik

    1997-12-31

    The effect of the electron sheath collapse in an applied-B ion diode due to the presence of the resistive anode plasma layer was found. This effect is more damaging at higher diode voltages and may be responsible for the parasitic load effect observed in the experiments. (author). 4 figs., 2 refs.

  8. Bounds imposed on the sheath velocity of a dense plasma focus by conservation laws and ionization stability condition

    Energy Technology Data Exchange (ETDEWEB)

    Auluck, S. K. H., E-mail: skhauluck@gmail.com, E-mail: skauluck@barc.gov.in [Physics Group, Bhabha Atomic Research Center, Mumbai (India)

    2014-09-15

    Experimental data compiled over five decades of dense plasma focus research are consistent with the snowplow model of sheath propagation, based on the hypothetical balance between magnetic pressure driving the plasma into neutral gas ahead and “wind pressure” resisting its motion. The resulting sheath velocity, or the numerically proportional “drive parameter,” is known to be approximately constant for devices optimized for neutron production over 8 decades of capacitor bank energy. This paper shows that the validity of the snowplow hypothesis, with some correction, as well as the non-dependence of sheath velocity on device parameters, have their roots in local conservation laws for mass, momentum, and energy coupled with the ionization stability condition. Both upper and lower bounds on sheath velocity are shown to be related to material constants of the working gas and independent of the device geometry and capacitor bank impedance.

  9. Bounds imposed on the sheath velocity of a dense plasma focus by conservation laws and ionization stability condition

    International Nuclear Information System (INIS)

    Auluck, S. K. H.

    2014-01-01

    Experimental data compiled over five decades of dense plasma focus research are consistent with the snowplow model of sheath propagation, based on the hypothetical balance between magnetic pressure driving the plasma into neutral gas ahead and “wind pressure” resisting its motion. The resulting sheath velocity, or the numerically proportional “drive parameter,” is known to be approximately constant for devices optimized for neutron production over 8 decades of capacitor bank energy. This paper shows that the validity of the snowplow hypothesis, with some correction, as well as the non-dependence of sheath velocity on device parameters, have their roots in local conservation laws for mass, momentum, and energy coupled with the ionization stability condition. Both upper and lower bounds on sheath velocity are shown to be related to material constants of the working gas and independent of the device geometry and capacitor bank impedance

  10. Corrosion evaluation technology

    International Nuclear Information System (INIS)

    Kim, Uh Chul; Han, Jeong Ho; Nho, Kye Ho; Lee, Eun Hee; Kim, Hong Pyo; Hwang, Seong Sik; Lee, Deok Hyun; Hur, Do Haeng; Kim, Kyung Mo.

    1997-09-01

    A multifrequency ACPD system was assembled which can measure very small crack. Stress corrosion cracking test system with SSRT operating high temperature was installed. Stress corrosion cracking test of newly developed alloy 600 and existing alloy 600 was carried out in steam atmosphere of 400 deg C. No crack was observed in both materials within a test period of 2,000 hrs. Corrosion fatigue test system operating at high temperature was installed in which fatigue crack was measured by CDPD. Lead enhanced the SCC of the Alloy 600 in high temperature water, had a tendency to modify a cracking morphology from intergranular to transgranular. Pit initiation preferentially occurred at Ti-rich carbide. Resistance to pit initiation decreased with increasing temperature up to 300 deg C. Test loop for erosion corrosion was designed and fabricated. Thin layer activation technique was very effective in measuring erosion corrosion. Erosion corrosion of a part of secondary side pipe was evaluated by the Check Family Codes of EPRI. Calculated values of pipe thickness by Check Family Codes coincided with the pipe thickness measured by UT with an error of ± 20%. Literature review on turbine failure showed that failure usually occurred in low pressure turbine rotor disc and causes of failure are stress corrosion cracking and corrosion fatigue. (author). 12 refs., 20 tabs., 77 figs

  11. Spine Patterning Is Guided by Segmentation of the Notochord Sheath

    NARCIS (Netherlands)

    Wopat, Susan; Bagwell, Jennifer; Sumigray, Kaelyn D.; Dickson, Amy L.; Huitema, Leonie F.A.; Poss, Kenneth D.; Schulte-Merker, Stefan; Bagnat, Michel

    2018-01-01

    The spine is a segmented axial structure made of alternating vertebral bodies (centra) and intervertebral discs (IVDs) assembled around the notochord. Here, we show that, prior to centra formation, the outer epithelial cell layer of the zebrafish notochord, the sheath, segments into alternating

  12. Comprehensive Study of Plasma-Wall Sheath Transport Phenomena

    Science.gov (United States)

    2016-10-26

    the floating potential of wall material samples immersed in a low-temperature plasma were studied. Hysteresis is found to be due to secondary electron...continued research into plasma sheath physics. Hysteresis effects observed in the floating potential of wall material samples immersed in a low... Journal of Applied Physics, Volume 119, March 2016, pp. 113305 1-5. DISTRIBUTION A: Distribution approved for public release. 8 Figure 2

  13. Corrosion Cost and Corrosion Map of Korea - Based on the Data from 2005 to 2010

    International Nuclear Information System (INIS)

    Kim, Y. S.; Lim, H. K.; Kim, J. J.; Hwang, W. S.; Park, Y. S.

    2011-01-01

    Corrosion of metallic materials occurs by the reaction with corrosive environment such as atmosphere, marine, soil, urban, high temperature etc. In general, reduction of thickness and cracking and degradation are resulted from corrosion. Corrosion in all industrial facilities and infrastructure causes large economic losses as well as a large number of accidents. Economic loss by corrosion has been reported to be nearly 1-6% of GNP or GDP. In order to reduce corrosion damage of industrial facilities, corrosion map as well as a systematic investigation of the loss of corrosion in each industrial sector is needed. The Corrosion Science Society of Korea in collaboration with 15 universities and institutes has started to survey on the cost of corrosion and corrosion map of Korea since 2005. This work presents the results of the survey on cost of corrosion by Uhlig, Hoar, and input-output methods, and the evaluation of atmospheric corrosion rate of carbon steel, weathering steel, galvanized steel, copper, and aluminum in Korea. The total corrosion cost was estimated in terms of the percentage of the GDP of industry sectors and the total GDP of Korea. According to the result of Input/output method, corrosion cost of Korea was calculated as 2.9% to GDP (2005). Time of wetness was shown to be categories 3 to 4 in all exposure areas. A definite seasonal difference was observed in Korea. In summer and fall, time of wetness was higher than in other seasons. Because of short exposure period (12 months), significant corrosion trends depending upon materials and exposure corrosion environments were not revealed even though increased mass loss and decreased corrosion rate by exposure time

  14. Theory of a wall sheath in a gas-discharge plasma

    International Nuclear Information System (INIS)

    Dvinin, S.A.; Dovzhenko, V.A.; Kuzovnikov, A.A.

    1999-01-01

    An integro-differential equation is proposed that generalizes the plasma-sheath (Langmuir-Tonks) equation to include charge exchange between ions and neutrals in a discharge plasma and makes it possible to correctly analyze how the discharge evolves from the regime of collisionless ion motion to the diffusive regime in pure gases with allowance for the space charge in the sheath at the plasma boundary. The integro-differential equation is solved numerically, and the ionization rate is calculated as a function of the ratio between the ion mean free path and the characteristic discharge dimension. The ion energy distribution function in the positive column of a discharge plasma is computed. The parameter range in which the positive column can exist is examined, and the limits of applicability of different discharge models are analyzed depending on the relations between the ion mean free path, Debye length, and discharge dimension

  15. Exploratory shaft liner corrosion estimate

    International Nuclear Information System (INIS)

    Duncan, D.R.

    1985-10-01

    An estimate of expected corrosion degradation during the 100-year design life of the Exploratory Shaft (ES) is presented. The basis for the estimate is a brief literature survey of corrosion data, in addition to data taken by the Basalt Waste Isolation Project. The scope of the study is expected corrosion environment of the ES, the corrosion modes of general corrosion, pitting and crevice corrosion, dissimilar metal corrosion, and environmentally assisted cracking. The expected internal and external environment of the shaft liner is described in detail and estimated effects of each corrosion mode are given. The maximum amount of general corrosion degradation was estimated to be 70 mils at the exterior and 48 mils at the interior, at the shaft bottom. Corrosion at welds or mechanical joints could be significant, dependent on design. After a final determination of corrosion allowance has been established by the project it will be added to the design criteria. 10 refs., 6 figs., 5 tabs

  16. Child–Langmuir law applicability for a cathode sheath description of glow discharge in hydrogen

    International Nuclear Information System (INIS)

    Lisovskiy, V A; Artushenko, K P; Yegorenkov, V D

    2016-01-01

    The present paper reveals that the Child-Langmuir law version with the constant ion mobility has to be applied for the cathode sheath description of the glow discharge in hydrogen. Using the analytical model we demonstrate that even in a high electric field the constant mobility law version rather than that for the constant ion mean free path has to hold in the case of impeded charge exchange and the dominant effect of polarization forces on the ion motion through the cathode sheath. (paper)

  17. Dictionary corrosion and corrosion control. English-German/German-English. Fachwoerterbuch Korrosion und Korrosionsschutz. Englisch-Deutsch/Deutsch-Englisch

    Energy Technology Data Exchange (ETDEWEB)

    1985-01-01

    This dictionary has 13000 entries in both languages. Keywords and extensive accompanying information simplify the choice of word for the user. The following topics are covered: Theoretical principles of corrosion; Corrosion of the metals and alloys most frequently used in engineering. Types of corrosion - (chemical-, electro-chemical, biological corrosion); forms of corrosion (superficial, pitting, selective, intercrystalline and stress corrosion; vibrational corrosion cracking); erosion and cavitation. Methods of corrosion control (material selection, temporary corrosion protection media, paint and plastics coatings, electro-chemical coatings, corrosion prevention by treatment of the corrosive media); Corrosion testing methods.

  18. Malignant Peripheral Nerve Sheath Tumor: MRI and CT Findings

    Directory of Open Access Journals (Sweden)

    K. O. Kragha

    2015-01-01

    important in its diagnosis. A rare case of MPNST that produced urinary retention and bowel incontinence is presented that may aid clinicians in the diagnosis of this rare clinical entity. Motor weakness, central enhancement, and immunohistochemistry may assist in the diagnosis of MPNST and differentiation between benign peripheral nerve sheath tumor (BPNST and MPNST.

  19. Penetration of corrosion products and corrosion-induced cracking in reinforced cementitious materials

    DEFF Research Database (Denmark)

    Michel, Alexander; Pease, Brad J.; Peterova, Adela

    2014-01-01

    This paper describes experimental investigations on corrosion-induced deterioration in reinforced cementitious materials and the subsequent development and implementation of a novel conceptual model. Rejnforced mortar specimens of varying water-to-cement ratios were subjected to current-induced c......This paper describes experimental investigations on corrosion-induced deterioration in reinforced cementitious materials and the subsequent development and implementation of a novel conceptual model. Rejnforced mortar specimens of varying water-to-cement ratios were subjected to current......-dependent concentrations of corrosion products averaged through the specimen thickness. Digital image correlation (DIC) was used to measure corrosion-induced deformations including deformations between steel and cementitious matrix as well as formation and propagation of corrosion-induced cracks. Based on experimental...... observations, a conceptual model was developed to describe the penetration of solid corrosion products into capillary pores of the cementitious matrix. Only capillary pores within a corrosion accommodating region (CAR), i.e. in close proximity of the steel reinforcement, were considered accessible...

  20. Annihilation model of the Tormac sheath

    International Nuclear Information System (INIS)

    Hammer, J.H.

    1979-02-01

    A one-dimensional, steady state fluid model is developed to describe the boundary layer between plasma and magnetic field that occurs in the Tormac sheath. Similar systems which may be treatable by the same model are tokamaks with divertors and reversed field mirrors. The model includes transport across the magnetic field as well as mirror losses along the field, the latter being represented as annihilation terms in the one-dimensional equations. The model equations are derived from the two-dimensional, time dependent hierarchy of equations generated by taking velocity moments of the kinetic equation including collisions

  1. Collision-dominated dust sheaths and voids - observations in micro-gravity experiments and numerical investigation of the force balance relations

    International Nuclear Information System (INIS)

    Tsytovich, V N; Morfill, G; Konopka, U; Thomas, H

    2003-01-01

    Numerical solutions of stationary force balance equations are used to investigate the possible dust configurations (dust structures) in complex plasmas between two floating potential plane electrodes. The distance between electrodes is assumed to be larger than the ion-neutral mean free path and the hydrodynamic description is used. It includes the known forces operating in this limit, the ionization source and the dust charge variations. The stationary balance equations are solved both in the case of the presence of one-size dust grains and for the case of a mixture of grains with two different sizes. Recent micro-gravity experiments with single-size dust grains and two-different-size dust grains show the formation of a system of dust sheaths and dust voids between the two plane electrodes. The observed configurations of dust structures depend strongly on the gas pressure and the degree of ionization used. The numerical investigations are able to show the necessary conditions for the types of structure to be created and give their size. The size of the structures observed is larger than the ion-neutral mean free path and is of the order of magnitude of that obtained numerically. The numerical investigations give details of the spatial distributions, the dust particles, the electron/ion densities, the ion drift velocity and dust charges inside and outside different dust structures. These details have not yet been investigated experimentally and can indicate directions for further experimental work to be performed. The single-dust-sheath structure with single-size dust particles surrounded by dust free regions (dust wall-voids) and floating potential electrodes is computed. Such a structure was observed recently and the computational results are in agreement with observations. It is shown that more often a dust void in the centre is observed. It is found that a dust void in the centre region between two electrodes is formed if the ionization rate is larger than the

  2. Genetic instability in nerve sheath cell tumors

    DEFF Research Database (Denmark)

    Rogatto, Silvia Regina; Casartelli, Cacilda; Rainho, Claudia Aparecida

    1995-01-01

    After in vitro culture, we analyzed cytogenetically four acoustic nerve neurinomas, one intraspinal neurinoma and one neurofibroma obtainedfrom unrelated patients. Monosomy of chromosomes 22 and 16 was an abnormality common to all cases, followed in frequency by loss of chromosomes 18 (three cases...... by the presence of polyploid cells with inconsistent abnormalities, endoreduplications and telomeric associations resulting in dicentric chromosomes. It is probable that these cytogenetic abnormalities represent some kind of evolutionary advantage for the in vitro progression of nerve sheath tumors....

  3. NASA's Corrosion Technology Laboratory at the Kennedy Space Center: Anticipating, Managing, and Preventing Corrosion

    Science.gov (United States)

    Calle, Luz Marina

    2014-01-01

    Corrosion is the degradation of a material that results from its interaction with the environment. The marine environment at NASAs Kennedy Space Center (KSC) has been documented by ASM International (formerly American Society for Metals) as the most corrosive in the United States. With the introduction of the Space Shuttle in 1981, the already highly corrosive conditions at the launch pads were rendered even more severe by the 70 tons of highly corrosive hydrochloric acid that were generated by the solid rocket boosters. Numerous failures at the launch pads are caused by corrosion.The structural integrity of ground infrastructure and flight hardware is critical to the success, safety, cost, and sustainability of space missions. As a result of fifty years of experience with launch and ground operations in a natural marine environment that is highly corrosive, NASAs Corrosion Technology Laboratory at KSC is a major source of corrosion control expertise in the launch and other environments. Throughout its history, the Laboratory has evolved from what started as an atmospheric exposure facility near NASAs launch pads into a world-wide recognized capability that provides technical innovations and engineering services in all areas of corrosion for NASA and external customers.This presentation will provide a historical overview of the role of NASAs Corrosion Technology in anticipating, managing, and preventing corrosion. One important challenge in managing and preventing corrosion involves the detrimental impact on humans and the environment of what have been very effective corrosion control strategies. This challenge has motivated the development of new corrosion control technologies that are more effective and environmentally friendly. Strategies for improved corrosion protection and durability can have a huge impact on the economic sustainability of human spaceflight operations.

  4. Corrosion behavior of corrosion resistant alloys in stimulation acids

    Energy Technology Data Exchange (ETDEWEB)

    Cheldi, Tiziana [ENI E and P Division, 20097 San Donato Milanese Milano (Italy); Piccolo, Eugenio Lo; Scoppio, Lucrezia [Centro Sviluppo Materiali, via Castel Romano 100, 00128 Rome (Italy)

    2004-07-01

    In the oil and gas industry, selection of CRAs for downhole tubulars is generally based on resistance to corrosive species in the production environment containing CO{sub 2}, H{sub 2}S, chloride and in some case elemental sulphur. However, there are non-production environments to which these materials must also be resistant for either short term or prolonged duration; these environments include stimulation acids, brine and completion fluids. This paper reports the main results of a laboratory study performed to evaluate the corrosion and stress corrosion behaviour to the acidizing treatments of the most used CRAs for production tubing and casing. Laboratory tests were performed to simulate both 'active' and 'spent' acids operative phases, selecting various environmental conditions. The selected steel pipes were a low alloyed steel, martensitic, super-martensitic, duplex 22 Cr, superduplex 25 Cr and super-austenitic stainless steels (25 Cr 35 Ni). Results obtained in the 'active' acid environments over the temperature range of 100-140 deg. C, showed that the blend acids with HCl at high concentration and HCl + HF represented too much severe conditions, where preventing high general corrosion and heavy localised corrosion by inhibition package becomes very difficult, especially for duplex steel pipe, where, in some case, the specimens were completely dissolved into the solution. On the contrary, all steels pipes were successfully protected by inhibitor when organic acid solution (HCOOH + CH{sub 3}COOH) were used. Furthermore, different effectiveness on corrosion protection was showed by the tested inhibitors packages: e.g. in the 90% HCl at 12% + 10 CH{sub 3}COOH acid blend. In 'spent' acid environments, all steel pipes showed to be less susceptible to the localised and general corrosion attack. Moreover, no Sulphide Stress Corrosion Cracking (SSC) was observed. Only one super-austenitic stainless steel U-bend specimen showed

  5. Corrosion failure analysis as related to prevention of corrosion failures

    International Nuclear Information System (INIS)

    Suss, H.

    1977-10-01

    The factors and conditions which have contributed to many of the corrosion related service failures are discussed based on a review of actual case histories. The anti-corrosion devices which developed as a result of these failure analyses are reviewed, and the method which must be adopted and used to take advantage of the available corrosion prevention techniques is discussed

  6. Particle flows to shape and voltage surface discontinuities in the electron sheath surrounding a high voltage solar array in LEO

    Science.gov (United States)

    Metz, Roger N.

    1991-01-01

    This paper discusses the numerical modeling of electron flows from the sheath surrounding high positively biased objects in LEO (Low Earth Orbit) to regions of voltage or shape discontinuity on the biased surfaces. The sheath equations are derived from the Two-fluid, Warm Plasma Model. An equipotential corner and a plane containing strips of alternating voltage bias are treated in two dimensions. A self-consistent field solution of the sheath equations is outlined and is pursued through one cycle. The electron density field is determined by numerical solution of Poisson's equation for the electrostatic potential in the sheath using the NASCAP-LEO relation between electrostatic potential and charge density. Electron flows are calculated numerically from the electron continuity equation. Magnetic field effects are not treated.

  7. Accuracy and complications of CT-guided core needle biopsy of peripheral nerve sheath tumours

    Energy Technology Data Exchange (ETDEWEB)

    Pianta, Marcus; Chock, Eric; Schlicht, Stephen [St Vincent' s Hospital, Fitzroy, VIC (Australia); McCombe, David [St Vincent' s Hospital and Victorian Hand Surgery Associates, Victoria (Australia)

    2015-09-15

    This single-centre study retrospectively reviews the complications in patients that have occurred following peripheral nerve sheath tumour biopsy, and assesses whether there is an association with biopsy technique or underlying lesion characteristics. 41 consecutive core needle biopsies of proven peripheral nerve sheath tumours over a 2-year period in a tertiary teaching hospital were reviewed. Patient demographics and symptoms, tumour characteristics and radiological appearances were recorded. Biopsy and surgical histology were correlated, and post-biopsy and surgical complications analyzed. 41 biopsies were performed in 38 patients. 68 % schwannomas, 24 % neurofibromas and 7 % malignant peripheral nerve sheath tumours. Biopsy histology correlated with surgery in all cases. 71 % of lesions were surgically excised. 60 % of patients reported pain related to their lesion. Following the biopsy, 12 % reported increased pain, which resolved in all cases. Pain exacerbation was noted in tumours smaller in size, more superficial and in closer proximity of the biopsy needle tip to the traversing nerve. Number of biopsy needle passes was not associated with an increased incidence of procedure-related pain. Core biopsy of a suspected peripheral nerve sheath tumour may be performed safely before excisional surgery to confirm lesion histology and assist prognosis. There is excellent correlation between core biopsy and excised surgical specimen histology. The most common complication of pain exacerbation is seen in a minority and is temporary, and more likely with smaller, more superficial lesions and a closer needle-tip to traversing nerve distance during biopsy. (orig.)

  8. Accuracy and complications of CT-guided core needle biopsy of peripheral nerve sheath tumours

    International Nuclear Information System (INIS)

    Pianta, Marcus; Chock, Eric; Schlicht, Stephen; McCombe, David

    2015-01-01

    This single-centre study retrospectively reviews the complications in patients that have occurred following peripheral nerve sheath tumour biopsy, and assesses whether there is an association with biopsy technique or underlying lesion characteristics. 41 consecutive core needle biopsies of proven peripheral nerve sheath tumours over a 2-year period in a tertiary teaching hospital were reviewed. Patient demographics and symptoms, tumour characteristics and radiological appearances were recorded. Biopsy and surgical histology were correlated, and post-biopsy and surgical complications analyzed. 41 biopsies were performed in 38 patients. 68 % schwannomas, 24 % neurofibromas and 7 % malignant peripheral nerve sheath tumours. Biopsy histology correlated with surgery in all cases. 71 % of lesions were surgically excised. 60 % of patients reported pain related to their lesion. Following the biopsy, 12 % reported increased pain, which resolved in all cases. Pain exacerbation was noted in tumours smaller in size, more superficial and in closer proximity of the biopsy needle tip to the traversing nerve. Number of biopsy needle passes was not associated with an increased incidence of procedure-related pain. Core biopsy of a suspected peripheral nerve sheath tumour may be performed safely before excisional surgery to confirm lesion histology and assist prognosis. There is excellent correlation between core biopsy and excised surgical specimen histology. The most common complication of pain exacerbation is seen in a minority and is temporary, and more likely with smaller, more superficial lesions and a closer needle-tip to traversing nerve distance during biopsy. (orig.)

  9. Corrosion and corrosion fatigue of airframe aluminum alloys

    Science.gov (United States)

    Chen, G. S.; Gao, M.; Harlow, D. G.; Wei, R. P.

    1994-01-01

    Localized corrosion and corrosion fatigue crack nucleation and growth are recognized as degradation mechanisms that effect the durability and integrity of commercial transport aircraft. Mechanically based understanding is needed to aid the development of effective methodologies for assessing durability and integrity of airframe components. As a part of the methodology development, experiments on pitting corrosion, and on corrosion fatigue crack nucleation and early growth from these pits were conducted. Pitting was found to be associated with constituent particles in the alloys and pit growth often involved coalescence of individual particle-nucleated pits, both laterally and in depth. Fatigue cracks typically nucleated from one of the larger pits that formed by a cluster of particles. The size of pit at which fatigue crack nucleates is a function of stress level and fatigue loading frequency. The experimental results are summarized, and their implications on service performance and life prediction are discussed.

  10. Plasma-Sheath Instability in Hall Thrusters Due to Periodic Modulation of the Energy of Secondary Electrons in Cyclotron Motion

    International Nuclear Information System (INIS)

    Sydorenko, D.; Smolyakov, A.; Kaganovich, I.; Raitses, Y.

    2008-01-01

    Particle-in-cell simulation of Hall thruster plasmas reveals a plasma-sheath instability manifesting itself as a rearrangement of the plasma sheath near the thruster channel walls accompanied by a sudden change of many discharge parameters. The instability develops when the sheath current as a function of the sheath voltage is in the negative conductivity regime. The major part of the sheath current is produced by beams of secondary electrons counter-streaming between the walls. The negative conductivity is the result of nonlinear dependence of beam-induced secondary electron emission on the plasma potential. The intensity of such emission is defined by the beam energy. The energy of the beam in crossed axial electric and radial magnetic fields is a quasi-periodical function of the phase of cyclotron rotation, which depends on the radial profile of the potential and the thruster channel width. There is a discrete set of stability intervals determined by the final phase of the cyclotron rotation of secondary electrons. As a result, a small variation of the thruster channel width may result in abrupt changes of plasma parameters if the plasma state jumps from one stability interval to another

  11. Atmospheric corrosion of uranium-carbon alloys; Corrosion atmospherique des alliages uranium-carbone

    Energy Technology Data Exchange (ETDEWEB)

    Rousset, P; Accary, A [Commissariat a l' Energie Atomique, Saclay (France). Centre d' Etudes Nucleaires

    1965-07-01

    The authors study the corrosion of uranium-carbon alloys having compositions close to that of the mono-carbide; they show that the extent of the observed corrosion effects increases with the water vapour content of the surrounding gas and they conclude that the atmospheric corrosion of these alloys is due essentially to the humidity of the air, the effect of the oxygen being very slight at room temperature. They show that the optimum conditions for preserving U-C alloys are either a vacuum or a perfectly dry argon atmosphere. The authors have also established that the type of corrosion involved is a corrosion which 'cracks under stress' and is transgranular (it can also be intergranular in the case of sub-stoichiometric alloys). They propose, finally, two hypotheses for explaining this mechanism, one of which is illustrated by the existence, at the fissure interface, of corrosion products which can play the role of 'corners' in the mono-carbide grains. (authors) [French] Les auteurs etudient la corrosion des alliages uranium-carbone de composition voisine du monocarbure; ils montrent que l'importance des effets de la corrosion observee augmente avec la teneur en vapeur d'eau du milieu gazeux ambiant et concluent que la corrosion atmospherique de ces alliages est due essentiellement a l'humidite de l'air, l'action de l'oxygene de l'air etant tres faible a la temperature ambiante. Ils indiquent que les conditions optimales de conservation des alliages U-C sont le vide ou une atmosphere d'argon parfaitement desseches. D'autre part, les auteurs etablissent que le type de corrosion mis en jeu est une corrosion 'fissurante sous contrainte', transgranulaire (pouvant egalement etre intergranulaire dans le cas d'alliages sous-stoechiometriques). Ils proposent enfin deux hypotheses pour rendre compte de ce mecanisme, dont l'une est illustree par la mise en evidence, a l'interface des fissures, de produits de corrosion pouvant jouer le role de 'coins' dans les grains de

  12. Corrosion and corrosion protection of support structures for offshore wind energy devices (OWEA)

    Energy Technology Data Exchange (ETDEWEB)

    Momber, A. [Muehlhan AG, Schlinckstrasse 3, D-21107 Hamburg (Germany)

    2011-05-15

    The paper provides a review about the corrosion and corrosion protection of offshore wind energy devices (OWEA). Firstly, special features resulting from location and operation of OWEA are being discussed. Secondly, types of corrosion and corrosion phenomena are summarized in a systematic way. Finally, practical solutions to the corrosion protection of OWEA, including steel allowances, cathodic protection and coatings and linings, are discussed. (Copyright copyright 2011 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  13. Corrosion behaviors and effects of corrosion products of plasma electrolytic oxidation coated AZ31 magnesium alloy under the salt spray corrosion test

    Science.gov (United States)

    Wang, Yan; Huang, Zhiquan; Yan, Qin; Liu, Chen; Liu, Peng; Zhang, Yi; Guo, Changhong; Jiang, Guirong; Shen, Dejiu

    2016-08-01

    The effects of corrosion products on corrosion behaviors of AZ31 magnesium alloy with a plasma electrolytic oxidation (PEO) coating were investigated under the salt spray corrosion test (SSCT). The surface morphology, cross-sectional microstructure, chemical and phase compositions of the PEO coating were determined using scanning electron microscopy (SEM) equipped with energy dispersive X-ray spectroscopy (EDS) and X-ray diffraction analysis (XRD), respectively. Further, the corrosion process of the samples under the SSCT was examined in a non-aqueous electrolyte (methanol) using electrochemical impedance spectroscopy (EIS) coupled with equivalent circuit. The results show that the inner layer of the coating was destroyed firstly and the corrosion products have significant effects on the corrosion behaviors of the coating. The results above are discussed and an electrochemical corrosion model is proposed in the paper.

  14. Measurements of the asymmetric dynamic sheath around a pulse biased sphere immersed in flowing metal plasma

    Science.gov (United States)

    Wu, Hongchen; Anders, André

    2008-08-01

    A long-probe technique was utilized to record the expansion and retreat of the dynamic sheath around a spherical substrate immersed in pulsed cathode arc metal plasma. Positively biased, long cylindrical probes were placed on the side and downstream of a negatively pulsed biased stainless steel sphere of 1 in. (25.4 mm) diameter. The amplitude and width of the negative high voltage pulses (HVPs) were 2 kV, 5 kV, 10 kV, and 2 µs, 4 µs, 10 µs, respectively. The variation of the probe (electron) current during the HVP is a direct measure for the sheath expansion and retreat. Maximum sheath sizes were determined for the different parameters of the HVP. The expected rarefaction zone behind the biased sphere (wake) due to the fast plasma flow was clearly established and quantified.

  15. Long-term corrosion studies

    International Nuclear Information System (INIS)

    Gdowski, G.

    1998-01-01

    The scope of this activity is to assess the long-term corrosion properties of metallic materials under consideration for fabricating waste package containers. Three classes of metals are to be assessed: corrosion resistant, intermediate corrosion resistant, and corrosion allowance. Corrosion properties to be evaluated are general, pitting and crevice corrosion, stress-corrosion cracking, and galvanic corrosion. The performance of these materials will be investigated under conditions that are considered relevant to the potential emplacement site. Testing in four aqueous solutions, and vapor phases above them, and at two temperatures are planned for this activity. (The environmental conditions, test metals, and matrix are described in detail in Section 3.0.) The purpose and objective of this activity is to obtain the kinetic and mechanistic information on degradation of metallic alloys currently being considered for waste package containers. This information will be used to provide assistance to (1) waste package design (metal barrier selection) (E-20-90 to E-20-92), (2) waste package performance assessment activities (SIP-PA-2), (3) model development (E-20-75 to E-20-89). and (4) repository license application

  16. Photovoltaic sheathing element with one or more tabs

    Energy Technology Data Exchange (ETDEWEB)

    Keenihan, James R; Langmaid, Joseph A; Lopez, Leonardo C.

    2017-02-07

    The present invention is premised upon an assembly that includes at least a photovoltaic sheathing element capable of being affixed on a building structure. The shingle including at least a photovoltaic cell assembly, a body portion attached to one or more portions of the photovoltaic cell assembly. Wherein the body portion includes one or more top peripheral tabs each capable of fitting under one or more vertically adjoining devices.

  17. Formation of intermediate cementum. III: 3H-tryptophan and 3H-proline uptake into the epithelial root sheath of Hertwig in vitro

    International Nuclear Information System (INIS)

    Lindskog, S.; Hammarstroem, L.

    1982-01-01

    The intermediate cementum is a narrow, mineralized tissue between the cementum and dentin. Recent studies have shown that this tissue is mineralized by the epithelial root sheath in a way similar to the mineralization of the innermost layer of aprismatic enamel. In the present investigation uptake of proline and tryptophan into the epithelial root sheath was studied with autoradiography. Tryptophan is an amino acid that is incorporated into enamel matrix but not into collagen. Tryptophan uptake was significant in the whole epithelial root sheath, but not into the odontoblasts or predentin. Proline was incorporated into the predentin while the root sheath was unlabeled. This indicated that the matrix of the intermediate cementum was formed by the epithelial root sheath of Hertwig, and that this matrix was a noncollagenous matrix possibly of the same nature as enamel matrix

  18. Retroperitoneal Malignant Peripheral Nerve Sheath Tumour: A Rare Case Report.

    Science.gov (United States)

    Deger, Ayse Nur; Bayar, Mehmet Akif; Caydere, Muzaffer; Deger, Hakki; Tayfur, Mahir

    2015-09-01

    Malignant nerve sheath tumours (MPNST) are rare neoplasias and retroperitoneal cases are fairly rare and clinically difficult to be detected, but they are very agressive neoplasias. MPNST are frequently seen in head, neck and upper extremities. In patients with NF1; MPNST, a poor-prognostic lesion, may result from a malignant degeneration of a former plexiform neurofibroma. It is necessary to be aware of a potential malignancy in patients diagnosed with plexiform neurofibroma. We present a 21-year-old female with a diagnosis of MPNST. The patient was admited to the hospital because of a tumour in the subcutaneous region on her left buttock. The surgeon's clinical diagnosis was lipoma. After the pathological examination of biopsy specimen, the lesion was identified as "plexiform neurofibroma" and then the patient was diagnosed with Neurofibromatosis Type 1 (NF1). Simultaneously, another mass on the retroperitoneal region was identified as malignant peripheral nerve sheath tumour (MPNST).

  19. Cilia-like structures anchor the amphioxus notochord to its sheath.

    Science.gov (United States)

    Bočina, Ivana; Ljubešić, Nikola; Saraga-Babić, Mirna

    2011-01-01

    Body stiffness is important during undulatory locomotion in fish. In amphioxus, the myosepta play an important role in transmission of muscular forces to the notochord. In order to define the specific supporting role of the notochord in amphioxus during locomotion, the ultrastructure of 10 adult amphioxus specimens was analyzed using transmission electron microscopy. Numerous cilia-like structures were found on the surface of each notochordal cell at the sites of their attachment to the notochordal sheath. Ultrastructurally, these structures consisted of the characteristic arrangement of peripheral and central microtubular doublets and were anchored to the inner layer of the notochordal sheath. Immunohistochemically, a positive reaction to applied dynein and β-tubulin antibodies characterized the area of the cilia-like structures. We propose that reduced back-and-forth movements of the cilia-like structures might contribute to the flow of the fluid content inside the notochord, thus modulating the stiffness of the amphioxus body during its undulatory locomotion. Copyright © 2009 Elsevier GmbH. All rights reserved.

  20. Corrosion of beryllium

    International Nuclear Information System (INIS)

    Mueller, J.J.; Adolphson, D.R.

    1987-01-01

    The corrosion behavior of beryllium in aqueous and elevated-temperature oxidizing environments has been extensively studied for early-intended use of beryllium in nuclear reactors and in jet and rocket propulsion systems. Since that time, beryllium has been used as a structural material in les corrosive environments. Its primary applications include gyro systems, mirror and reentry vehicle structures, and aircraft brakes. Only a small amount of information has been published that is directly related to the evaluation of beryllium for service in the less severe or normal atmospheric environments associated with these applications. Despite the lack of published data on the corrosion of beryllium in atmospheric environments, much can be deduced about its corrosion behavior from studies of aqueous corrosion and the experiences of fabricators and users in applying, handling, processing, storing, and shipping beryllium components. The methods of corrosion protection implemented to resist water and high-temperature gaseous environments provide useful information on methods that can be applied to protect beryllium for service in future long-term structural applications

  1. Sheath formation and extraction of ions from a constricted R.F ion source

    Energy Technology Data Exchange (ETDEWEB)

    Abdel-Salam, F W; Helal, A G; El-Khabeary, H; El-Merai, N T [Accelerators Dept., Nuclear Research Center, Atomic Energy Authority, Cairo, (Egypt)

    1997-12-31

    The present work investigates the plasma characteristics in a constricted R. F. ion source. The extraction of ions from the plasma boundary and sheath formation were studied. The ion source physical parameters are discussed in order to understand the physical processes occurring within the discharge region up to the extraction system. Electron temperature and density were determined using Langmuir probe. The probe current-voltage characteristics were measured for different extraction voltages (ext.) = 0,500,1000, and 1250 volt at various constant R.F. powers. The effect of R.F. power on electron temperature was deduced for a beam = plasma discharge. This revealed that for a quasi-neutral (plasma) region the electron temperature increased linearly with the R.F. Power which leads to substantial electron heating and efficient electron energy transport in this region. Applying extraction voltage, the electron temperature drops as the ionization rate increases. The sheath thickness was obtained at constant extraction voltages. The curves show that if the ion current density increased, the sheath thickness decreased while it increases by increasing extraction voltage, and it is negligible in the plasma region. 13 figs.

  2. Sheath-flow electrochemical detection of amino acids with a copper wire electrode in capillary electrophoresis.

    Science.gov (United States)

    Inoue, Junji; Kaneta, Takashi; Imasaka, Totaro

    2012-09-01

    Here, we report the detection of native amino acids using a sheath-flow electrochemical detector with a working electrode made of copper wire. A separation capillary that was inserted into a platinum tube in the detector acted as a grounded electrode for electrophoresis and as a flow channel for sheath liquid. Sheath liquid flowed outside the capillary to support the transport of the separated analytes to the working electrode for electrochemical detection. The copper wire electrode was aligned at the outlet of the capillary in a wall-jet configuration. Amino acids injected into the capillary were separated following elution from the end of the capillary and detection by the copper electrode. Three kinds of copper electrodes with different diameters-50, 125, and 300 μm-were examined to investigate the effect of the electrode diameter on sensitivity. The peak widths of the analytes were independent of the diameter of the working electrode, while the 300-μm electrode led to a decrease in the signal-to-noise ratio compared with the 50- and 125-μm electrodes, which showed no significant difference. The flow rate of the sheath liquid was also varied to optimize the detection conditions. The limits of detection for amino acids ranged from 4.4 to 27 μM under optimal conditions. © 2012 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

  3. Initiation and inhibition of pitting corrosion on reinforcing steel under natural corrosion conditions

    Energy Technology Data Exchange (ETDEWEB)

    Abd El Wanees, S., E-mail: s_wanees@yahoo.com [Chemistry Department, Faculty of Science, University of Tabuk, Tabuk (Saudi Arabia); Chemistry Department, Faculty of Science, Zagazig University, Zagazig 44519 (Egypt); Bahgat Radwan, A. [Center for Advanced Materials, Qatar University, Doha 2713 (Qatar); Alsharif, M.A. [Chemistry Department, Faculty of Science, University of Tabuk, Tabuk (Saudi Arabia); Abd El Haleem, S.M. [Chemistry Department, Faculty of Science, Zagazig University, Zagazig 44519 (Egypt)

    2017-04-01

    Initiation and inhibition of pitting corrosion on reinforcing steel in saturated, naturally aerated Ca(OH){sub 2} solutions, under natural corrosion conditions, are followed through measurements of corrosion current, electrochemical impedance spectroscopy and SEM investigation. Induction period for pit initiation and limiting corrosion current for pit propagation are found to depend on aggressive salt anion and cation-types, as well as, concentration. Ammonium chlorides and sulfates are more corrosive than the corresponding sodium salts. Benzotriazole and two of its derivatives are found to be good inhibitors for pitting corrosion of reinforcing steel. Adsorption of these compounds follows a Langmuir adsorption isotherm. The thermodynamic functions ΔE{sup ∗}, ΔH{sup ∗} and ΔS{sup ∗} for pitting corrosion processes in the absence and presence of inhibitor are calculated and discussed. - Highlights: • Cl{sup −} and SO{sub 4} {sup 2-} induce pitting corrosion on passive reinforcing steel. • Initiation and propagation of pitting depend on cation and anion types. • Inhibition is based on adsorption according to Langmuir isotherm.

  4. Real time corrosion monitoring in atmosphere using automated battery driven corrosion loggers

    DEFF Research Database (Denmark)

    Prosek, T.; Kouril, M.; Hilbert, Lisbeth Rischel

    2008-01-01

    diminishes due to corrosion. Zinc, iron, copper and nickel sensors at several thicknesses are available. Sensitivity of the corrosion measurement varies from 1 to 10 nm depending on the type and thickness of the sensor. Changes in the air corrosivity can be thus detected within hours or even tens of minutes......A logger enabling continuous measurement of corrosion rate of selected metals in indoor and outdoor atmospheres has been developed. Principle of the measurement method is based on the increasing electrical resistance of a measuring element made of the material concerned as its cross-sectional area....... The logger lifetime in medium corrosive environments is designed to be 2 years with full autonomy. Data on the sensor corrosion rate are available any time through GPRS connection or by a non-contact inductive reading without the need of retracting the logger from the exposure site....

  5. ICRF antenna Faraday shield plasma sheath model

    International Nuclear Information System (INIS)

    Whealton, J.H.; Ryan, P.M.; Raridon, R.J.

    1990-01-01

    A two-dimensional nonlinear formulation that explicitly considers the plasma edge near a Faraday shield in a self-consistent manner is used in the modeling of the ion motion for a Faraday shield concept and model suggested by Perkins. Two models are considered that may provide significant insight into the generation of impurities for ion cyclotron resonance heating (ICRH) antennas. In one of these models a significant sheath periodically forms next to the Faraday screen, with ion acoustic waves heating the ions in the plasma. (orig.)

  6. Corrosion-resistant metal surfaces

    Science.gov (United States)

    Sugama, Toshifumi [Wading River, NY

    2009-03-24

    The present invention relates to metal surfaces having thereon an ultrathin (e.g., less than ten nanometer thickness) corrosion-resistant film, thereby rendering the metal surfaces corrosion-resistant. The corrosion-resistant film includes an at least partially crosslinked amido-functionalized silanol component in combination with rare-earth metal oxide nanoparticles. The invention also relates to methods for producing such corrosion-resistant films.

  7. Corrosion testing facilities in India

    International Nuclear Information System (INIS)

    Viswanathan, R.; Subramanian, Venu

    1981-01-01

    Major types of corrosion tests, establishment of specifications on corrosion testing and scope of their application in practice are briefly described. Important organizations in the world which publish specifications/standards are listed. Indian organizations which undertake corrosion testing and test facilities available at them are also listed. Finally in an appendix, a comprehensive list of specifications relevant to corrosion testing is given. It is arranged under the headings: environmental testing, humidity tests, salt spray/fog tests, immersion tests, specification corrosion phenomena, (tests) with respect to special corrosion media, (tests) with respect to specific corrosion prevention methods, and specific corrosion tests using electrical and electrochemical methods (principles). Each entry in the list furnishes information about: nature of the test, standard number, and its specific application. (M.G.B.)

  8. Incidence of enhancement of the optic nerve/sheath complex in fat-suppression orbit MRI

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Ho Kyu; Yoon, Kwon Ha; Choi, Choong Gon; Suh, Dae Chul [Asan Medical Center, University of Ulsan College of Medicine, Seoul (Korea, Republic of)

    1995-04-15

    To elucidate the incidence of Gd-DTPA enhancement of the optic nerve/sheath complex (ONC) in patients with various ophthalmopathies using fat-suppression MRI. Orbit MRI with fat-suppression technique (ChemSat) was performed in 58 patients with normal and various orbital lesions. The fat-suppression MR was done with and without Gd-DTPA injection in all cases. MR findings were reviewed retrospectively in a blind fashion with respect to presence or absence of contrast enhancement of the ONC. Contrast enhancement of the ONC was seen in 86% (6/7) of cavernous sinus lesions, 80% (8/10) of intraconal lesions excluding the ONC, 57% (16/28) of ONC lesions, 38% (3/8) of ocular lesions, and 2% (1/55) of normal orbits. The ONC enhancement was the most common in optic nerve/sheath tumors (10/10), and pseudotumors (6/6), cavernous sinus dural arteriovenous malformations (3/3) and cavernous sinus thrombosis (2/2), and less frequently seen in optic neuritis (3/14). Enhancement of the ONC may be seen in lesions of the cavernous sinus and orbit other than optic nerve/sheath lesion.

  9. The study of sheath flow dark zone phenomenon in dynamic individual cells scattering measurement

    Science.gov (United States)

    Zhang, Lu; Zhao, Hong; Wang, Xiaopin; Zhang, Weiguang

    2008-09-01

    Dynamic cells scattering is one of the most efficient approaches exploring in measurements of cells size, morphology and growth states. This technique can be widely applied in real-time detection for pharmaceutical industry, food industry, liquor industry and other biological fields. A novel method named dynamic individual cells scattering measurement is designed in this paper, which can make cells pass through quartz glass measurement zone one by one with sheath flow driving force. During the experiments, an obvious phenomenon has been found which is called sheath flow dark zone phenomenon (SFDZ). Under the influence of SFDZ, sheath flow forming detection becomes very difficult. In this paper, the causes giving rise to SFDZ have been analyzed. And an improved method is put forward, in which the orifice inside the measurement zone is set as an optical system. Then the illuminating system is redesigned. In this way, almost all the illuminating light can enter orifice so that the total reflection energy decreases substantially. A comparison experiments have been done, which proves the efficiency of this redesigned optical system and its sound effects on SFDZ avoiding.

  10. Modeling of polarization phenomena due to RF sheaths and electron beams in magnetized plasma

    International Nuclear Information System (INIS)

    Faudot, E.

    2005-01-01

    This work investigates the problematic of hot spots induced by accelerated particle fluxes in tokamaks. It is shown that the polarization due to sheaths in the edge plasma in which an electron beam at a high level of energy is injected, can reach several hundreds volts and thus extend the deposition area. The notion of obstructed sheath is introduced and explains the acceleration of energy deposition by the decreasing of the sheath potential. Then, a 2-dimensional fluid modeling of flux tubes in front of ICRF antennae allows us to calculate the rectified potentials taking into account RF polarization currents transverse to magnetic field lines. The 2-dimensional fluid code designed validates the analytical results which show that the DC rectified potential is 50% greater with polarization currents than without. Finally, the simultaneous application of an electron beam and a RF potential reveals that the potentials due to each phenomenon are additives when RF potential is much greater than beam polarization. The density depletion of polarized flux tubes in 2-dimensional PIC (particles in cells) simulations is characterized but not yet explained. (author)

  11. Analysis of zircaloy oxide thickness data from PWRs

    International Nuclear Information System (INIS)

    Sheppard, K.D.; Speyer, D.M.; Chan, Y.Y.; Frankl, I.; Strasser, A.A.

    1990-02-01

    Prior EPRI funded research (Project 1250-1) resulted in a set of Zircaloy waterside corrosion models. These models were based principally on KWU reactor data. The objective of this study was to evaluate the ability of the KWU corrosion models to predict available domestic USA data for all domestic PWR vendors in order to further validate the models and to provide a consistent basis to judge the corrosion data of the domestic plants. A methodology for analyzing the large amount of data was developed and implemented in a single channel model. This model includes the capability, by a method described herein, of accounting for open core related effects (crossflow) and the effect of the immediately adjacent fuel rods, guide tubes, etc., on the coolant conditions around the fuel rods that were measured for oxide thickness. Data from the Arkansas Unit number-sign 2 (ANO-2) Combustion Engineering (C-E), Oconee Units 1 and 2 built by Babcock ampersand Wilcox (B ampersand W), and the Trojan reactor built by Westinghouse (W) were used in this study. The corrosion models previously developed, and the present single channel model methodology, were able to predict the corrosion data quite well. The maximum corrosion thickness was on the order of 20 to 40 microns in all plants studied. 13 refs., 11 figs., 5 tabs

  12. Corrosion characteristics of K-claddings

    International Nuclear Information System (INIS)

    Park, J. Y.; Choi, B. K.; Jung, Y. H.; Jung, Y. H.

    2004-01-01

    The Improvement of the corrosion resistance of nuclear fuel claddings is the critical issue for the successful development of the high burn-up fuel. KAERI have developed the K-claddings having a superior corrosion resistance by controlling the alloying element addition and optimizing the manufacturing process. The comparative evaluation of the corrosion resistance for K-claddings and the foreign claddings was performed and the effect of the heat treatment on the corrosion behavior of K-claddings was also examined. Corrosion tests were carried out in the conditions of 360 .deg. C pure water, PWR-simulating loop and 400 .deg. C steam, From the results of the corrosion tests, it was found that the corrosion resistance of K-claddings is superior to those of Zry4 and A claddings and K6 showed a better corrosion resistance than K3. The corrosion behavior of K-cladding was strongly influenced by the final annealing rather than the intermediate annealing, and the corrosion resistance increased with decreasing the final annealing temperature

  13. Corrosion control. 2. ed.

    International Nuclear Information System (INIS)

    Bradford, S.A.

    2001-01-01

    The purpose of this text is to train engineers and technologists not just to understand corrosion but to control it. Materials selection, coatings, chemical inhibitors, cathodic and anodic protection, and equipment design are covered in separate chapters. High-temperature oxidation is discussed in the final two chapters ne on oxidation theory and one on controlling oxidation by alloying and with coatings. This book treats corrosion and high-temperature oxidation separately. Corrosion is divided into three groups: (1) chemical dissolution including uniform attack, (2) electrochemical corrosion from either metallurgical or environmental cells, and (3) stress-assisted corrosion. Corrosion is logically grouped according to mechanisms rather than arbitrarily separated into different types of corrosion as if they were unrelated. For those university students and industry personnel who approach corrosion theory very hesitantly, this text will present the electrochemical reactions responsible for corrosion summed up in only five simple half-cell reactions. When these are combined on a polarization diagram, which is also explained in detail, the electrochemical processes become obvious. For those who want a text stripped bare of electrochemical theory, several noted sections can be omitted without loss of continuity. However, the author has presented the material in such a manner that these sections are not beyond the abilities of any high school graduate who is interested in technology

  14. Measurements of the asymmetric dynamic sheath around a pulse biased sphere immersed in flowing metal plasma

    International Nuclear Information System (INIS)

    Wu Hongchen; Anders, Andre

    2008-01-01

    A long-probe technique was utilized to record the expansion and retreat of the dynamic sheath around a spherical substrate immersed in pulsed cathode arc metal plasma. Positively biased, long cylindrical probes were placed on the side and downstream of a negatively pulsed biased stainless steel sphere of 1 in. (25.4 mm) diameter. The amplitude and width of the negative high voltage pulses (HVPs) were 2 kV, 5 kV, 10 kV, and 2 μs, 4 μs, 10 μs, respectively. The variation of the probe (electron) current during the HVP is a direct measure for the sheath expansion and retreat. Maximum sheath sizes were determined for the different parameters of the HVP. The expected rarefaction zone behind the biased sphere (wake) due to the fast plasma flow was clearly established and quantified.

  15. Corrosion in the oil industry

    Energy Technology Data Exchange (ETDEWEB)

    Brondel, D [Sedco Forex, Montrouge (France); Edwards, R [Schlumberger Well Services, Columbus, OH (United States); Hayman, A [Etudes et Productions Schlumberger, Clamart (France); Hill, D [Schlumberger Dowell, Tulsa, OK (United States); Mehta, S [Schlumberger Dowell, St. Austell (United Kingdom); Semerad, T [Mobil Oil Indonesia, Inc., Sumatra (Indonesia)

    1994-04-01

    Corrosion costs the oil industry billions of dollars a year, a fact that makes the role of the corrosion engineer an increasingly important one. Attention is paid to how corrosion affects every aspect of exploration and production, from offshore rigs to casing. Also the role of corrosion agents such as drilling and production fluids is reviewed. Methods of control and techniques to monitor corrosion are discussed, along with an explanation of the chemical causes of corrosion. 21 figs., 32 refs.

  16. Phytochemicals as Green Corrosion Inhibitors in Various Corrosive ...

    African Journals Online (AJOL)

    There is an intensive effort underway to develop new plant origin corrosion inhibitors for metal subjected to various environmental conditions. These efforts have been motivated by the desire to replace toxic inhibitors used for mitigation of corrosion of various metals and alloys in aqueous solutions. Plants represent a class ...

  17. Excitation of surface waves and electrostatic fields by a RF (radiofrequency systems) wave in a plasma sheath with current

    International Nuclear Information System (INIS)

    Gutierrez Tapia, C.

    1990-01-01

    It is shown in a one-dimensional model that when a current in a plasma sheath is present, the excitation of surface waves and electrostatic fields by a RF wave is possible in the sheath. This phenomena depends strongly on the joint action of Miller's and driven forces. It is also shown that the action of these forces are carried out at different characteristic times when the wave front travels through the plasma sheath. The influence of the current, in the steady limit, is taken into account by a small functional variation of the density perturbations and generated electrostatic field. (Author)

  18. Charge of a macroscopic particle in a plasma sheath

    International Nuclear Information System (INIS)

    Samarian, A.A.; Vladimirov, S.V.

    2003-01-01

    Charging of a macroscopic body levitating in a rf plasma sheath is studied experimentally and theoretically. The nonlinear charge vs size dependence is obtained. The observed nonlinearity is explained on the basis of an approach taking into account different plasma conditions for the levitation positions of different particles. The importance of suprathermal electrons' contribution to the charging process is demonstrated

  19. Interaction of magnetized electrons with a boundary sheath: investigation of a specular reflection model

    Science.gov (United States)

    Krüger, Dennis; Brinkmann, Ralf Peter

    2017-11-01

    This publication reports analytical and numerical results concerning the interaction of gyrating electrons with a plasma boundary sheath, with focus on partially magnetized technological plasmas. It is assumed that the electron Debye length {λ }{{D}} is much smaller than the electron gyroradius {r}{{L}}, and {r}{{L}} in turn much smaller than the mean free path λ and the gradient length L of the fields. Focusing on the scale of the gyroradius, the sheath is assumed as infinitesimally thin ({λ }{{D}}\\to 0), collisions are neglected (λ \\to ∞ ), the magnetic field is taken as homogeneous, and electric fields (=potential gradients) in the bulk are neglected (L\\to ∞ ). The interaction of an electron with the electric field of the plasma boundary sheath is represented by a specular reflection {v}\\to {v}-2{v}\\cdot {{e}}z {{e}}z of the velocity {v} at the plane z = 0 of a naturally oriented Cartesian coordinate system (x,y,z). The electron trajectory is then given as sequences of helical sections, with the kinetic energy ɛ and the canonical momenta p x and p y conserved, but not the position of the axis (base point {{R}}0), the slope (pitch angle χ), and the phase (gyrophase φ). A ‘virtual interaction’ which directly maps the incoming electrons to the outgoing ones is introduced and studied in dependence of the angle γ between the field and the sheath normal {{e}}z. The corresponding scattering operator is constructed, mathematically characterized, and given as an infinite matrix. An equivalent boundary condition for a transformed kinetic model is derived.

  20. Structural characterization of the human cerebral myelin sheath by small angle x-ray scattering

    International Nuclear Information System (INIS)

    De Felici, M; Felici, R; Ferrero, C; Tartari, A; Gambaccini, M; Finet, S

    2008-01-01

    Myelin is a multi-lamellar membrane surrounding neuronal axons and increasing their conduction velocity. When investigated by small-angle x-ray scattering (SAXS), the lamellar quasi-periodical arrangement of the myelin sheath gives rise to distinct peaks, which allow the determination of its molecular organization and the dimensions of its substructures. In this study we report on the myelin sheath structural determination carried out on a set of human brain tissue samples coming from surgical biopsies of two patients: a man around 60 and a woman nearly 90 years old. The samples were extracted either from white or grey cerebral matter and did not undergo any manipulation or chemical-physical treatment, which could possibly have altered their structure, except dipping them into a formalin solution for their conservation. Analysis of the scattered intensity from white matter of intact human cerebral tissue allowed the evaluation not only of the myelin sheath periodicity but also of its electronic charge density profile. In particular, the thicknesses of the cytoplasm and extracellular regions were established, as well as those of the hydrophilic polar heads and hydrophobic tails of the lipid bilayer. SAXS patterns were measured at several locations on each sample in order to establish the statistical variations of the structural parameters within a single sample and among different samples. This work demonstrates that a detailed structural analysis of the myelin sheath can also be carried out in randomly oriented samples of intact human white matter, which is of importance for studying the aetiology and evolution of the central nervous system pathologies inducing myelin degeneration.

  1. Monitoring Microbially Influenced Corrosion

    DEFF Research Database (Denmark)

    Hilbert, Lisbeth Rischel

    and diffusional effects and unreliable corrosion rates, when biofilm and ferrous sulphide corrosion products cover the steel surface. Corrosion rates can be overestimated by a factor of 10 to 100 by electrochemical techniques. Weight loss coupons and ER are recommended as necessary basic monitoring techniques......Abstract Microbially influenced corrosion (MIC) of carbon steel may occur in media with microbiological activity of especially sulphate-reducing bacteria (SRB). The applicability and reliability of a number of corrosion monitoring techniques for monitoring MIC has been evaluated in experiments....... EIS might be used for detection of MIC as the appearance of very large capacitances can be attributed to the combined ferrous sulphide and biofilm formation. Capacitance correlates directly with sulphide concentration in sterile sulphide media. Keywords: Corrosion monitoring, carbon steel, MIC, SRB...

  2. SRB seawater corrosion project

    Science.gov (United States)

    Bozack, M. J.

    1991-01-01

    The corrosion behavior of 2219 aluminum when exposed to seawater was characterized. Controlled corrosion experiments at three different temperatures (30, 60 and 100 C) and two different environments (seawater and 3.5 percent salt solution) were designed to elucidate the initial stages in the corrosion process. It was found that 2219 aluminum is an active catalytic surface for growth of Al2O3, NaCl, and MgO. Formation of Al2O3 is favored at lower temperatures, while MgO is favored at higher temperatures. Visible corrosion products are formed within 30 minutes after seawater exposure. Corrosion characteristics in 3.5 percent salt solution are different than corrosion in seawater. Techniques utilized were: (1) scanning electron microscopy, (2) energy dispersive x-ray spectroscopy, and (3) Auger electron spectroscopy.

  3. Corrosion of circulating water pipings in thermal and nuclear power stations and corrosion prevention measures

    International Nuclear Information System (INIS)

    Hachiya, Minoru

    1982-01-01

    In the age of energy conservation at present, the power generation facilities have been examined from the viewpoint of performance, endurance and economy, and in particular, the prevention of the loss due to the corrosion of various facilities is one of most important problems. Since circulating water pipings are in contact with sea water and soil, the peculiar corrosion phenomena are brought about on their external and internal surfaces. Namely, the pitting corrosion due to the environment of soil quality difference, the defects of coating and the contact with reinforcing bars in concrete occurs on the external surface, and the overall corrosion due to the increase of flow velocity and the pitting corrosion due to the defects of coating, the contact with different kinds of metals and the gap in corrosion-resistant steel occur on the internal surface. As the measures for corrosion prevention, corrosion-preventive coating and electric corrosion prevention are applied. The principle, the potential and current density, the system, the design procedure and the examples of application of electric corrosion prevention are described. (Kako, I.)

  4. Cyst(e)ine Is the Transport Metabolite of Assimilated Sulfur from Bundle-Sheath to Mesophyll Cells in Maize Leaves1

    Science.gov (United States)

    Burgener, Marta; Suter, Marianne; Jones, Stephanie; Brunold, Christian

    1998-01-01

    The intercellular distribution of the enzymes and metabolites of assimilatory sulfate reduction and glutathione synthesis was analyzed in maize (Zea mays L. cv LG 9) leaves. Mesophyll cells and strands of bundle-sheath cells from second leaves of 11-d-old maize seedlings were obtained by two different mechanical-isolation methods. Cross-contamination of cell preparations was determined using ribulose bisphosphate carboxylase (EC 4.1.1.39) and nitrate reductase (EC 1.6.6.1) as marker enzymes for bundle-sheath and mesophyll cells, respectively. ATP sulfurylase (EC 2.7.7.4) and adenosine 5′-phosphosulfate sulfotransferase activities were detected almost exclusively in the bundle-sheath cells, whereas GSH synthetase (EC 6.3.2.3) and cyst(e)ine, γ-glutamylcysteine, and glutathione were located predominantly in the mesophyll cells. Feeding experiments using [35S]sulfate with intact leaves indicated that cyst(e)ine was the transport metabolite of reduced sulfur from bundle-sheath to mesophyll cells. This result was corroborated by tracer experiments, which showed that isolated bundle-sheath strands fed with [35S]sulfate secreted radioactive cyst(e)ine as the sole thiol into the resuspending medium. The results presented in this paper show that assimilatory sulfate reduction is restricted to the bundle-sheath cells, whereas the formation of glutathione takes place predominantly in the mesophyll cells, with cyst(e)ine functioning as a transport metabolite between the two cell types. PMID:9536048

  5. Mobile evaporator corrosion test results

    International Nuclear Information System (INIS)

    Rozeveld, A.; Chamberlain, D.B.

    1997-05-01

    Laboratory corrosion tests were conducted on eight candidates to select a durable and cost-effective alloy for use in mobile evaporators to process radioactive waste solutions. Based on an extensive literature survey of corrosion data, three stainless steel alloys (304L, 316L, AL-6XN), four nickel-based alloys (825, 625, 690, G-30), and titanium were selected for testing. The corrosion tests included vapor phase, liquid junction (interface), liquid immersion, and crevice corrosion tests on plain and welded samples of candidate materials. Tests were conducted at 80 degrees C for 45 days in two different test solutions: a nitric acid solution. to simulate evaporator conditions during the processing of the cesium ion-exchange eluant and a highly alkaline sodium hydroxide solution to simulate the composition of Tank 241-AW-101 during evaporation. All of the alloys exhibited excellent corrosion resistance in the alkaline test solution. Corrosion rates were very low and localized corrosion was not observed. Results from the nitric acid tests showed that only 316L stainless steel did not meet our performance criteria. The 316L welded interface and crevice specimens had rates of 22.2 mpy and 21.8 mpy, respectively, which exceeds the maximum corrosion rate of 20 mpy. The other welded samples had about the same corrosion resistance as the plain samples. None of the welded samples showed preferential weld or heat-affected zone (HAZ) attack. Vapor corrosion was negligible for all alloys. All of the alloys except 316L exhibited either open-quotes satisfactoryclose quotes (2-20 mpy) or open-quotes excellentclose quotes (<2 mpy) corrosion resistance as defined by National Association of Corrosion Engineers. However, many of the alloys experienced intergranular corrosion in the nitric acid test solution, which could indicate a susceptibility to stress corrosion cracking (SCC) in this environment

  6. Electric field measurements in the sheath of an argon RF discharge by probing with microparticles under varying gravity conditions

    NARCIS (Netherlands)

    Beckers, J.; Stoffels, W.W.; Kroesen, G.M.W.; Ockenga, T.; Wolter, M.; Kersten, H.

    2010-01-01

    The electric field profile in the plasma sheath of an argon rf plasma has been determined by measuring the equilibrium height and the resonance frequency of plasma-confined microparticles. In order to determine the electric field structure at any position in the plasma sheath without the discharge

  7. The corrosion and corrosion mechanical properties evaluation for the LBB concept in VVERs

    Energy Technology Data Exchange (ETDEWEB)

    Ruscak, M.; Chvatal, P.; Karnik, D.

    1997-04-01

    One of the conditions required for Leak Before Break application is the verification that the influence of corrosion environment on the material of the component can be neglected. Both the general corrosion and/or the initiation and, growth of corrosion-mechanical cracks must not cause the degradation. The primary piping in the VVER nuclear power plant is made from austenitic steels (VVER 440) and low alloy steels protected with the austenitic cladding (VVER 1000). Inspection of the base metal and heterogeneous weldments from the VVER 440 showed that the crack growth rates are below 10 m/s if a low oxygen level is kept in the primary environment. No intergranular cracking was observed in low and high oxygen water after any type of testing, with constant or periodic loading. In the framework of the LBB assessment of the VVER 1000, the corrosion and corrosion mechanical properties were also evaluated. The corrosion and corrosion mechanical testing was oriented predominantly to three types of tests: stress corrosion cracking tests corrosion fatigue tests evaluation of the resistance against corrosion damage. In this paper, the methods used for these tests are described and the materials are compared from the point of view of response on static and periodic mechanical stress on the low alloyed steel 10GN2WA and weld metal exposed in the primary circuit environment. The slow strain rate tests and static loading of both C-rings and CT specimens were performed in order to assess the stress corrosion cracking characteristics. Cyclic loading of CT specimens was done to evaluate the kinetics of the crack growth under periodical loading. Results are shown to illustrate the approaches used. The data obtained were evaluated also from the point of view of comparison of the influence of different structure on the stress corrosion cracking appearance. The results obtained for the base metal and weld metal of the piping are presented here.

  8. An evaluation of corrosion resistant alloys by field corrosion test in Japanese refuse incineration plants

    International Nuclear Information System (INIS)

    Kawahara, Yuuzou; Nakamura, Masanori; Shibuya, Eiichi; Yukawa, Kenichi

    1995-01-01

    As the first step for development of the corrosion resistant superheater tube materials of 500 C, 100 ata used in high efficient waste-to-energy plants, field corrosion tests of six conventional alloys were carried out at metal temperatures of 450 C and 550 C for 700 and 3,000 hours in four typical Japanese waste incineration plants. The test results indicate that austenitic alloys containing approximately 80 wt% [Cr+Ni] show excellent corrosion resistance. When the corrosive environment is severe, intergranular corrosion of 40∼200 microm depth occurs in stainless steel and high alloyed materials. It is confirmed quantitatively that corrosion behavior is influenced by environmental corrosion factors such as Cl concentration and thickness of deposits on tube surface, metal temperature, and flue gas temperature. The excellent corrosion resistance of high [Cr+Ni+Mo] alloys such as Alloy 625 is explained by the stability of its protective oxide, such that the time dependence of corrosion nearly obeys the parabolic rate law

  9. Moisture performance properties of exterior sheathing products made of spruce plywood or OSB

    Energy Technology Data Exchange (ETDEWEB)

    Ojanen, T.; Ahonen, J. [VTT Building and Transport, Espoo (Finland)

    2005-02-01

    Plywood and OSB (Oriented Strand Board) are building boards that are made of timber and glue and that have good structural strength. OSB is a relatively new product that is produced from various timber materials and even some wastewood can be used as raw material for this product. Due to the easy access of raw material and economical reasons, the use of OSB has been highly increasing. The moisture safety of the building envelope depends on the properties of the building products. The moisture performance properties of the sheathing boards have not got enough attention, too often these wood based materials are equated without considering the real properties and their effect on the overall moisture performance. This research was carried out to experimentally determine the material properties and performance characteristics that have an effect on the moisture performance of building structures where OSB or spruce plywood are applied as exterior sheathing boards. A relatively representative amount of samples were used to study the moisture properties of European OSB and plywood products and a comparison to one Canadian OSB and one plywood product was done. All the products used in this research were meant to be used also as exterior sheathing boards. The results shows clearly the differences between OSB and plywood products. The products are not interchangeable. The main differences can be found from the vapour permeability levels that have an effect on the drying efficiency of building structures. The products have different performance criteria, and the climate conditions and moisture loads have to be studied to evaluate their suitability and moisture safety aspects in different applications. Water repellent features and drying efficiency are somewhat opposite properties of the products and the dimensional changes under varying moisture contents can set some boundary conditions when the optimum solution for the exterior sheathing is considered. (orig.)

  10. Modelling reinforcement corrosion in concrete

    DEFF Research Database (Denmark)

    Michel, Alexander; Geiker, Mette Rica; Stang, Henrik

    2012-01-01

    A physio-chemical model for the simulation of reinforcement corrosion in concrete struc-tures was developed. The model allows for simulation of initiation and subsequent propaga-tion of reinforcement corrosion. Corrosion is assumed to be initiated once a defined critical chloride threshold......, a numerical example is pre-sented, that illustrates the formation of corrosion cells as well as propagation of corrosion in a reinforced concrete structure....

  11. Simulation of a two-dimensional sheath over a flat insulator-conductor interface on a radio-frequency biased electrode in a high-density plasma

    International Nuclear Information System (INIS)

    Kim, Doosik; Economou, Demetre J.

    2004-01-01

    A combined fluid/Monte Carlo (MC) simulation was developed to study the two-dimensional (2D) sheath over a flat insulator/conductor interface on a radio-frequency (rf) biased electrode in a high-density plasma. The insulator capacitance increased the local impedance between the plasma and the bias voltage source. Thus, for uniform ion density and electron temperature far away from the wall, the sheath potential over the insulator was only a fraction of that over the conductor, resulting in a thinner sheath over the insulator. The fluid model provided the spatiotemporal profiles of the 2D sheath electric field. These were used as input to the MC simulation to compute the ion energy distribution (IED) and ion angular distribution (IAD) at different locations on the surface. The ion flux, IED, and IAD changed drastically across the insulator/conductor interface due to the diverging rf electric field in the distorted sheath. The ion flux was larger on the conductor at the expense of that on the insulator. Both the ion impact angle and angular spread increased progressively as the material interface was approached. The ion impact energy and energy spread were smaller on the insulator as compared to the conductor. For given plasma parameters, as the insulator thickness was increased, the sheath potential and thickness over the insulator decreased, and sheath distortion became more pronounced

  12. Understanding corrosion via corrosion product characterization: II. Role of alloying elements in improving the corrosion resistance of Zn-Al-Mg coatings on steel

    International Nuclear Information System (INIS)

    Volovitch, P.; Vu, T.N.; Allely, C.; Abdel Aal, A.; Ogle, K.

    2011-01-01

    Highlights: → Origins of better corrosion resistance of ZnAlMg coatings than galvanized steel. → Comparative study of corrosion products formed on ZnAlMg, ZnMg and Zn coatings. → Modeling of dissolution and precipitation stages of corrosion. → At early stages Mg stabilizes protective zinc basic salts during dry-wet cycling. → At later stages Al dissolves at high pH forming protective layered double hydroxides. - Abstract: Corrosion products are identified on Zn, ZnMg and ZnAlMg coatings in cyclic corrosion tests with NaCl or Na 2 SO 4 containing atmospheres. For Mg-containing alloys the improved corrosion resistance is achieved by stabilization of protective simonkolleite and zinc hydroxysulfate. At later stages, the formation of layered double hydroxides (LDH) is observed for ZnAlMg. According to thermodynamic modeling, Mg 2+ ions bind the excess of carbonate or sulfate anions preventing the formation of soluble or less-protective products. A preferential dissolution of Zn and Mg at initial stages of corrosion is confirmed by in situ dissolution measurement. The physicochemical properties of different corrosion products are compared.

  13. Modelling of Corrosion Cracks

    DEFF Research Database (Denmark)

    Thoft-Christensen, Palle

    Modelling of corrosion cracking of reinforced concrete structures is complicated as a great number of uncertain factors are involved. To get a reliable modelling a physical and mechanical understanding of the process behind corrosion in needed.......Modelling of corrosion cracking of reinforced concrete structures is complicated as a great number of uncertain factors are involved. To get a reliable modelling a physical and mechanical understanding of the process behind corrosion in needed....

  14. Retroperitoneal Malignant Peripheral Nerve Sheath Tumor Replacing an Absent Kidney in a Child

    Directory of Open Access Journals (Sweden)

    Samin Alavi

    2013-01-01

    Full Text Available Malignant peripheral nerve sheath tumors (MPNSTs are nonrhabdomyosarcoma soft tissue sarcomas with rare occurrence in children specially in the retroperitoneum. We describe a young child who presented with an abdominal mass. Both ultrasound and computed tomography revealed a large right-sided abdominal mass in the anatomic place of right kidney, while no kidney or ureter was observed at that side. He underwent surgical resection of the tumor with a primary impression of Wilms tumor. To the authors’ knowledge, this is the first case of retroperitoneal malignant peripheral nerve sheath tumor and absent kidney. This case suggests the very rare probability of association of MPNSTs in children with genitourinary tract anomalies such as renal agenesis.

  15. Dural ectasia of the optic nerve sheath: is it always benign?

    Directory of Open Access Journals (Sweden)

    Berker Bakbak

    2009-11-01

    Full Text Available Berker Bakbak1, Hava Dönmez2, Tülay Kansu3, Hayyam Kiratli41Hacettepe University Institute of Neurological Sciences and Psychiatry, Neuro-ophthalmology Unit, Ankara, Turkey; 2Diskapi Yildirim Beyazid Education and Research Hospital Neurology Clinic, Ankara, Turkey; 3Hacettepe University Medical Faculty, Department of Neurology, Neuro-Ophthalmology Unit, Ankara, Turkey; 4Hacettepe University Medical Faculty, Department of Ophthalmology, Ocular Oncology Unit, Ankara, TurkeyAbstract: A 36-year-old woman with a 3-month history of progressive visual loss had papilledema, dilatation of the optic nerve sheaths and normal cerebrospinal fluid pressures. She was diagnosed as dural ectasia of the optic nerve sheaths and surgical decompression was performed. In this case report, severe visual loss is described as a serious complication of this rare disease and the importance of early surgical intervention is emphasized.Keywords: optic nerve, dural ectasia, meningocele

  16. Exposure testing of fasteners in preservative treated wood: Gravimetric corrosion rates and corrosion product analyses

    Energy Technology Data Exchange (ETDEWEB)

    Zelinka, Samuel L., E-mail: szelinka@fs.fed.u [USDA Forest Products Laboratory, One Gifford Pinchot Drive, Madison, WI 53726 (United States); Sichel, Rebecca J. [College of Engineering, University of Wisconsin, Madison, WI 53706 (United States); Stone, Donald S. [Department of Materials Science and Engineering, College of Engineering, University of Wisconsin, Madison, WI 53706 (United States)

    2010-12-15

    Research highlights: {yields} The composition of the corrosion products was similar for the nail head and shank. {yields} Reduced copper was not detected on any of the fasteners. {yields} Measured corrosion rates were between 1 and 35 {mu}m year{sup -1}. - Abstract: Research was conducted to determine the corrosion rates of metals in preservative treated wood and also understand the mechanism of metal corrosion in treated wood. Steel and hot-dip galvanized steel fasteners were embedded in wood treated with one of six preservative treatments and exposed to 27 {sup o}C at 100% relative humidity for 1 year. The corrosion rate was determined gravimetrically and the corrosion products were analyzed with scanning electron microscopy, energy dispersive X-ray spectroscopy, and X-ray diffraction. Although the accepted mechanism of corrosion in treated wood involves the reduction of cupric ions from the wood preservative, no reduced copper was found on the corrosion surfaces. The galvanized corrosion products contained sulfates, whereas the steel corrosion products consisted of iron oxides and hydroxides. The possible implications and limitations of this research on fasteners used in building applications are discussed.

  17. Management of Reinforcement Corrosion

    DEFF Research Database (Denmark)

    Küter, André; Geiker, Mette Rica; Møller, Per

    Reinforcement corrosion is the most important cause for deterioration of reinforced concrete structures, both with regard to costs and consequences. Thermodynamically consistent descriptions of corrosion mechanisms are expected to allow the development of innovative concepts for the management...... of reinforcement corrosion....

  18. Microbiologically induced corrosion

    International Nuclear Information System (INIS)

    Stein, A.A.

    1988-01-01

    Biological attack is a problem that can affect all metallic materials in a variety of environments and systems. In the power industry, corrosion studies have focused on condensers and service water systems where slime, barnacles, clams, and other macro-organisms are easily detected. Efforts have been made to eliminate the effect of these organisms through the use of chlorination, backflushing, organic coating, or thermal shock. The objective is to maintain component performance by eliminating biofouling and reducing metallic corrosion. Recently, corrosion of power plant components by micro-organisms (bacteria) has been identified even in very clean systems. A system's first exposure to microbiologically induced corrosion (MIC) occurs during its first exposure to an aqueous environment, such as during hydrotest or wet layup. Corrosion of buried pipelines by sulfate-reducing bacteria has been studied by the petrochemical industry for years. This paper discusses various methods of diagnosing, monitoring, and controlling MIC in a variety of systems, as well as indicates areas where further study is needed

  19. CORROSION RATE OF STEELS DX51D AND S220GD IN DIFFERENT CORROSION ENVIRONMENT

    Directory of Open Access Journals (Sweden)

    Alina Crina CIUBOTARIU

    2016-06-01

    Full Text Available Corrosion in the marine environment is an important issue because the costs causes by marine corrosion increased year upon year. It is necessary a correctly approach to materials selection, protection and corrosion control to reduce this burden of wasted materials, wasted energy and wasted money. Many different types of corrosion attack can be observed to structures, ships and other equipment used in sea water service. Shipping containers are exposed to various corrosive mediums like as airborne salt, industrial pollutants, rain and saltwater. Transport damage during loading onto and unloading off trucks, train beds and ships breaches the paint coating which further contributes to corrosion. The result is shortened container life and high costs for container repair or replacement. The paper intends to evaluate, by gravimetric method, the corrosion rate and corrosion penetration rate of two types of carbon steel DX51D and S220GD. Carbon steel DX51D and hot-dip galvanized steel S220GD are used in marine and industrial applications for buildings cargo vessels, container ships and oil tankers. For testing it was used different corrosive environments: 5% NaOH solution; 5% HCL solution and 0.5M NaCl solution. The samples were immersed in 400mL of testing solution for exposure period of 28 days. Periodically at 3 days, 7 days, 14 days, 21 days and 28 days was measured de mass loss and evaluate the corrosion rate and corrosion stability coefficient. The steel DX51D was stable in 5% NaOH solution for 28 days, the values of corrosion stability coefficient was 7 after 3 days and 6 after 28 days of immersion in corrosive medium. In 5% HCL solution steels DX51D and S220GD was completely corroded in 21 days with a corrosion stability coefficient equal with 9 for 7 days and 8 for 21 days of immersion in corrosive solution. It was observed a good resistance for 3 days in 0.5M NaCl solution with a corrosion stability coefficient equal with 5, but after that

  20. An unusual case of cycticercosis of the tendon sheath of the tendoachilles.

    Directory of Open Access Journals (Sweden)

    Sharat Agarwal

    2010-04-01

    Full Text Available Cysticercosis is an infection by the larval stage (cystcercus cellulosae of the cestode, Taenia Solium (pork tape worm, especially in those individuals who live in the endemic areas. After gaining entry into the body, the larvae become encysted and may lie in subcutaneous tissue, striated muscle, the vitreous humor, or other tissues. We report an unusual case of cysticercosis of the the tendon sheath of the tendoachilles that presented as a swelling of the tendoachilles. Upon Fine Needle Aspiration and Cytology (FNAC that were conducted preoperatively, the possibility of villonodular synovitis was identified. However, the cysticercosis diagnosis was confirmed later after an excisional biopsy was performed. We could find no reports in the literature concerning an occurrence of cysticercosis in the tendon sheath of tendoachilles.

  1. General Corrosion and Localized Corrosion of the Drip Shield

    Energy Technology Data Exchange (ETDEWEB)

    F. Hua

    2004-09-16

    The repository design includes a drip shield (BSC 2004 [DIRS 168489]) that provides protection for the waste package both as a barrier to seepage water contact and a physical barrier to potential rockfall. The purpose of the process-level models developed in this report is to model dry oxidation, general corrosion, and localized corrosion of the drip shield plate material, which is made of Ti Grade 7. This document is prepared according to ''Technical Work Plan For: Regulatory Integration Modeling and Analysis of the Waste Form and Waste Package'' (BSC 2004 [DIRS 171583]). The models developed in this report are used by the waste package degradation analyses for TSPA-LA and serve as a basis to determine the performance of the drip shield. The drip shield may suffer from other forms of failure such as the hydrogen induced cracking (HIC) or stress corrosion cracking (SCC), or both. Stress corrosion cracking of the drip shield material is discussed in ''Stress Corrosion Cracking of the Drip Shield, the Waste Package Outer Barrier, and the Stainless Steel Structural Material'' (BSC 2004 [DIRS 169985]). Hydrogen induced cracking of the drip shield material is discussed in ''Hydrogen Induced Cracking of Drip Shield'' (BSC 2004 [DIRS 169847]).

  2. General Corrosion and Localized Corrosion of the Drip Shield

    International Nuclear Information System (INIS)

    F. Hua

    2004-01-01

    The repository design includes a drip shield (BSC 2004 [DIRS 168489]) that provides protection for the waste package both as a barrier to seepage water contact and a physical barrier to potential rockfall. The purpose of the process-level models developed in this report is to model dry oxidation, general corrosion, and localized corrosion of the drip shield plate material, which is made of Ti Grade 7. This document is prepared according to ''Technical Work Plan For: Regulatory Integration Modeling and Analysis of the Waste Form and Waste Package'' (BSC 2004 [DIRS 171583]). The models developed in this report are used by the waste package degradation analyses for TSPA-LA and serve as a basis to determine the performance of the drip shield. The drip shield may suffer from other forms of failure such as the hydrogen induced cracking (HIC) or stress corrosion cracking (SCC), or both. Stress corrosion cracking of the drip shield material is discussed in ''Stress Corrosion Cracking of the Drip Shield, the Waste Package Outer Barrier, and the Stainless Steel Structural Material'' (BSC 2004 [DIRS 169985]). Hydrogen induced cracking of the drip shield material is discussed in ''Hydrogen Induced Cracking of Drip Shield'' (BSC 2004 [DIRS 169847])

  3. Collaborative Research: Understanding Ion Losses to Plasma Boundaries Sheaths and Presheaths

    Energy Technology Data Exchange (ETDEWEB)

    Hershkowitz, Noah [Univ. of Wisconsin, Madison, WI (United States)

    2015-10-01

    Sheaths are common to all bounded steady-state plasmas. This includes laboratory, industrial, fusion, and in some cases even space plasmas. They form in general to balance particle loss and maintain quasi-neutrality in plasmas. Electrons are lighter than the ions by 2000 times or more (depending on the gas), and in most plasmas ion temperatures are rarely higher than the electron temperature and generally much lower. Thus in most cases, negative potential sheaths occur to confine electrons and allow ions to be freely lost. We have investigated how a plasma locally response to a positive bias on a small electrode, and have established area criteria which plasma reacts differently to the positive bias – first a pure electron sheath, and a global non-ambipolar regime where all electrons are lost to the electrode, and a double layer structure identified as a virtual cathode forms to limiting electron loss and maintain quasi-neutrality, and finally a anode spot regime where a secondary discharge occurs in front of the electrode, turning it into the major loss area of the entire plasma. Electrode area and plasma parameters criteria for these regimes were established, and the effect of the virtual cathode on the electrode’s I-V characteristics was investigated. We have also developed a global non-ambipolar electron source to replace hollow cathodes in a number of plasma applications. This eliminates the lifetime limitation and maintenance cost of hollow cathodes as they easily wear out easily and cannot be replaced in space applications.

  4. The dust characteristics in the collisional plasma sheath at the presence of external magnetic field

    Energy Technology Data Exchange (ETDEWEB)

    Shourkaei, Hossein Akbarian [AEOI, Tehran (Iran, Islamic Republic of). Plasma Physics Research Group

    2015-05-15

    The characteristics of dust in a plasma sheath are investigated in the presence of an external magnetic field and taking into account neutral collision forces. By using the fluid model, the continuity and momentum equations of ions and dusts are solved numerically with various magnitudes of collision force. In various magnitude and directions of the magnetic field, the electron and ion density distribution, ion flow velocity, electron potential have been calculated. It is shown that magnetic field has obvious effect on the plasma sheath and the collision force reduces the dust kinetic energy.

  5. Catastrophes caused by corrosion

    OpenAIRE

    PETROVIC ZORAN C.

    2016-01-01

    For many years, huge attention has been paid to the problem of corrosion damage and destruction of metallic materials. Experience shows that failures due to corrosion problems are very important, and statistics at the world level shows that the damage resulting from the effects of various forms of corrosion is substantial and that, for example, in industrialized countries it reaches 4-5% of national incomes. Significant funds are determined annually for the prevention and control of corrosion...

  6. An overview of erosion corrosion models and reliability assessment for corrosion defects in piping system

    International Nuclear Information System (INIS)

    Srividya, A.; Suresh, H.N.; Verma, A.K.; Gopika, V.; Santosh

    2006-01-01

    Piping systems are part of passive structural elements in power plants. The analysis of the piping systems and their quantification in terms of failure probability is of utmost importance. The piping systems may fail due to various degradation mechanisms like thermal fatigue, erosion-corrosion, stress corrosion cracking and vibration fatigue. On examination of previous results, erosion corrosion was more prevalent and wall thinning is a time dependent phenomenon. The paper is intended to consolidate the work done by various investigators on erosion corrosion in estimating the erosion corrosion rate and reliability predictions. A comparison of various erosion corrosion models is made. The reliability predictions based on remaining strength of corroded pipelines by wall thinning is also attempted. Variables in the limit state functions are modelled using normal distributions and Reliability assessment is carried out using some of the existing failure pressure models. A steady state corrosion rate is assumed to estimate the corrosion defect and First Order Reliability Method (FORM) is used to find the probability of failure associated with corrosion defects over time using the software for Component Reliability evaluation (COMREL). (author)

  7. Corrosion protection and control using nanomaterials

    CERN Document Server

    Cook, R

    2012-01-01

    This book covers the use of nanomaterials to prevent corrosion. The first section deals with the fundamentals of corrosion prevention using nanomaterials. Part two includes a series of case studies and applications of nanomaterials for corrosion control.$bCorrosion is an expensive and potentially dangerous problem in many industries. The potential application of different nanostructured materials in corrosion protection, prevention and control is a subject of increasing interest. Corrosion protection and control using nanomaterials explores the potential use of nanotechnology in corrosion control. The book is divided into two parts. Part one looks at the fundamentals of corrosion behaviour and the manufacture of nanocrystalline materials. Chapters discuss the impact of nanotechnology in reducing corrosion cost, and investigate the influence of various factors including thermodynamics, kinetics and grain size on the corrosion behaviour of nanocrystalline materials. There are also chapters on electrodeposition ...

  8. Role of CD44 in Malignant Peripheral Nerve Sheath Tumor Growth and Metastasis

    National Research Council Canada - National Science Library

    Sherman, Larry

    2003-01-01

    Malignant peripheral nerve sheath tumors (MPNST) are aggressive, difficult to treat tumors that occur in type I neurofibromatosis patients with an increased incidence compared to the general population...

  9. Role of CD44 in Malignant Peripheral Nerve Sheath Tumor Growth and Metastasis

    National Research Council Canada - National Science Library

    Sherman, Larry

    2001-01-01

    Malignant peripheral nerve sheath tumors (MPNST) are aggressive, difficult to treat tumors that occur in type I neurofibromatosis patients with an increased incidence compared to the general population...

  10. Reduction of shunt obstructions by using a peel-away sheath technique? A multicenter prospective randomized trial.

    Science.gov (United States)

    Kehler, Uwe; Langer, Niels; Gliemroth, Jan; Meier, Ullrich; Lemcke, Johannes; Sprung, Christian; Schlosser, Hans-Georg; Kiefer, Michael; Eymann, Regina; Heese, Oliver

    2012-05-01

    Shunt obstructions may partly be caused by brain debris, which intrude into the ventricular catheter during ventricle puncture. Avoiding contact between the catheter and brain tissue, by using a peel-away sheath, should reduce the number of shunt failures caused by obstruction. To test this hypothesis, we conducted a randomized, prospective multicenter study. 201 patients from 6 different neurosurgical centers in Germany receiving a ventriculo-peritoneal shunt were included in this study. Of these, 177 patients completed a 1-year follow-up period. Surgery was randomized in a 1 to 1 fashion, such that out of 177 procedures, 91 were performed using a peel-away sheath and 86 were performed without. The rate of surgical re-interventions and shunt obstructions within a 12-month period was recorded. Within 1 year post-surgery, 17 shunt obstructions (9.6%) leading to shunt revisions were recorded. However, no difference was found between surgeries performed using a peel-away sheath (9.9%) or not (9.3%). The overall shunt infection rate was 2.8% and the shunt revision rate for overdrainage was 3.9%. The theoretical advantages attributed to the use of a peel-away sheath to introduce a ventricular catheter could not be confirmed in this randomized study, suggesting that the proposed role of brain debris in shunt obstructions may be overestimated. Copyright © 2011 Elsevier B.V. All rights reserved.

  11. The Sheath-less Planar Langmuir Probe

    Science.gov (United States)

    Cooke, D. L.

    2017-12-01

    The Langmuir probe is one of the oldest plasma diagnostics, provided the plasma density and species temperature from analysis of a current-voltage curve as the voltage is swept over a practically chosen range. The analysis depends on a knowledge or theory of the many factors that influence the current-voltage curve including, probe shape, size, nearby perturbations, and the voltage reference. For applications in Low Earth Orbit, the Planar Langmuir Probe, PLP, is an attractive geometry because the ram ion current is very constant over many Volts of a sweep, allowing the ion density and electron temperature to be determined independently with the same instrument, at different points on the sweep. However, when the physical voltage reference is itself small and electrically floating as with a small spacecraft, the spacecraft and probe system become a double probe where the current collection theory depends on the interaction of the spacecraft with the plasma which is generally not as simple as the probe itself. The Sheath-less PLP, SPLP, interlaces on a single ram facing surface, two variably biased probe elements, broken into many small and intertwined segments on a scale smaller than the plasma Debye length. The SPLP is electrically isolated from the rest of the spacecraft. For relative bias potentials of a few volts, the ion current to all segments of each element will be constant, while the electron currents will vary as a function of the element potential and the electron temperature. Because the segments are small, intertwined, and floating, the assembly will always present the same floating potential to the plasma, with minimal growth as a function of voltage, thus sheath-less and still planar. This concept has been modelled with Nascap, and tested with a physical model inserted into a Low Earth Orbit-like chamber plasma. Results will be presented.

  12. Monitoring and modeling stress corrosion and corrosion fatigue damage in nuclear reactors

    International Nuclear Information System (INIS)

    Andresen, P.L.; Ford, F.P.; Solomon, H.D.; Taylor, D.F.

    1990-01-01

    Stress corrosion and corrosion fatigue are significant problems in many industries, causing economic penalties from decreased plant availability and component repair or replacement. In nuclear power reactors, environmental cracking occurs in a wide variety of components, including reactor piping and steam generator tubing, bolting materials and pressure vessels. Life assessment for these components is complicated by the belief that cracking is quite irreproducible. Indeed, for conditions which were once viewed as nominally similar, orders of magnitude variability in crack growth rates are observed for stress corrosion and corrosion fatigue of stainless steels and low-alloy steels in 288 degrees C water. This paper shows that design and life prediction approaches are destined to be overly conservative or to risk environmental failure if life is predicted by quantifying only the effects of mechanical parameters and/or simply ignoring or aggregating environmental and material variabilities. Examples include the Nuclear Regulatory Commission (NRC) disposition line for stress-corrosion cracking of stainless steel in boiling water reactor (BWR) water and the American Society of Mechanical Engineers' Section XI lines for corrosion fatigue

  13. Recognition and Analysis of Corrosion Failure Mechanisms

    Directory of Open Access Journals (Sweden)

    Steven Suess

    2006-02-01

    Full Text Available Corrosion has a vast impact on the global and domestic economy, and currently incurs losses of nearly $300 billion annually to the U.S. economy alone. Because of the huge impact of corrosion, it is imperative to have a systematic approach to recognizing and mitigating corrosion problems as soon as possible after they become apparent. A proper failure analysis includes collection of pertinent background data and service history, followed by visual inspection, photographic documentation, material evaluation, data review and conclusion procurement. In analyzing corrosion failures, one must recognize the wide range of common corrosion mechanisms. The features of any corrosion failure give strong clues as to the most likely cause of the corrosion. This article details a proven approach to properly determining the root cause of a failure, and includes pictographic illustrations of the most common corrosion mechanisms, including general corrosion, pitting, galvanic corrosion, dealloying, crevice corrosion, microbiologically-influenced corrosion (MIC, corrosion fatigue, stress corrosion cracking (SCC, intergranular corrosion, fretting, erosion corrosion and hydrogen damage.

  14. Linear electromagnetic excitation of an asymmetric low pressure capacitive discharge with unequal sheath widths

    Energy Technology Data Exchange (ETDEWEB)

    Lieberman, M. A., E-mail: lieber@eecs.berkeley.edu; Lichtenberg, A. J.; Kawamura, E. [Department of Electrical Engineering and Computer Science, University of California, Berkeley, California 94720-1770 (United States); Chabert, P. [Laboratoire de Physique des Plasmas, CNRS, Ecole Polytechnique, UPMC, Paris XI, Observatoire de Paris, 91128 Palaiseau (France)

    2016-01-15

    It is well-known that standing waves having radially center-high radio frequency (rf) voltage profiles exist in high frequency capacitive discharges. In this work, we determine the symmetric and antisymmetric radially propagating waves in a cylindrical capacitive discharge that is asymmetrically driven at the lower electrode by an rf voltage source. The discharge is modeled as a uniform bulk plasma which at lower frequencies has a thicker sheath at the smaller area powered electrode and a thinner sheath at the larger area grounded electrode. These are self-consistently determined at a specified density using the Child law to calculate sheath widths and the electron power balance to calculate the rf voltage. The fields and the system resonant frequencies are determined. The center-to-edge voltage ratio on the powered electrode is calculated versus frequency, and central highs are found near the resonances. The results are compared with simulations in a similar geometry using a two-dimensional hybrid fluid-analytical code, giving mainly a reasonable agreement. The analytic model may be useful for finding good operating frequencies for a given discharge geometry and power.

  15. Corrosion of PWR steam generators

    International Nuclear Information System (INIS)

    Garnsey, R.

    1979-01-01

    Some designs of pressurized water reactor (PWR) steam generators have experienced a variety of corrosion problems which include stress corrosion cracking, tube thinning, pitting, fatigue, erosion-corrosion and support plate corrosion resulting in 'denting'. Large international research programmes have been mounted to investigate the phenomena. The operational experience is reviewed and mechanisms which have been proposed to explain the corrosion damage are presented. The implications for design development and for boiler and feedwater control are discussed. (author)

  16. Archaeological analogs and corrosion; Analogues archeologiques et corrosion

    Energy Technology Data Exchange (ETDEWEB)

    David, D

    2008-07-01

    In the framework of the high level and long life radioactive wastes disposal deep underground, the ANDRA built a research program on the material corrosion. In particular they aim to design containers for a very long time storage. Laboratory experiments are in progress and can be completed by the analysis of metallic archaeological objects and their corrosion after hundred years. (A.L.B.)

  17. The Corrosion Inhibition Characteristics of Sodium Nitrite Using an On-line Corrosion Rate Measurement System

    International Nuclear Information System (INIS)

    Park, Mal-Yong; Kang, Dae-Jin; Moon, Jeon-Soo

    2015-01-01

    An on-line corrosion rate measurement system was developed using a personal computer, a data acquisition board and program, and a 2-electrode corrosion probe. Reliability of the developed system was confirmed with through comparison test. With this system, the effect of sodium nitrite (NaNO 2 ) as a corrosion inhibitor were studied on iron and aluminum brass that were immersed in sodium chloride (NaCl) solution. Corrosion rate was measured based on the linear polarization resistance method. The corrosion rates of aluminum brass and iron in 1% NaCl solutions were measured to be 0.290 mm per year (mmpy) and 0.2134 mmpy, respectively. With the addition of 200 ppm of NO 2 - , the corrosion rates decreased to 0.0470 mmpy and 0.0254 mmpy. The addition of NO 2 - caused a decrease in corrosion rates of both aluminum brass and iron, yet the NO 2 - acted as a more effective corrosion inhibitor for iron. than aluminum brass

  18. Use of a pressure sensing sheath: comparison with standard means of blood pressure monitoring in catheterization procedures.

    Science.gov (United States)

    Purdy, Phillip D; South, Charles; Klucznik, Richard P; Liu, Kenneth C; Novakovic, Robin L; Puri, Ajit S; Pride, G Lee; Aagaard-Kienitz, Beverly; Ray, Abishek; Elliott, Alan C

    2017-08-01

    Monitoring of blood pressure (BP) during procedures is variable, depending on multiple factors. Common methods include sphygmomanometer (BP cuff), separate radial artery catheterization, and side port monitoring of an indwelling sheath. Each means of monitoring has disadvantages, including time consumption, added risk, and signal dampening due to multiple factors. We sought an alternative approach to monitoring during procedures in the catheterization laboratory. A new technology involving a 330 µm fiberoptic sensor embedded in the wall of a sheath structure was tested against both radial artery catheter and sphygmomanometer readings obtained simultaneous with readings recorded from the pressure sensing system (PSS). Correlations and Bland-Altman analysis were used to determine whether use of the PSS could substitute for these standard techniques. The results indicated highly significant correlations in systolic, diastolic, and mean arterial pressures (MAP) when compared against radial artery catheterization (p<0.0001), and MAP means differed by <4%. Bland-Altman analysis of the data suggested that the sheath measurements can replace a separate radial artery catheter. While less striking, significant correlations were seen when PSS readings were compared against BP cuff readings. The PSS has competitive functionality to that seen with a dedicated radial artery catheter for BP monitoring and is available immediately on sheath insertion without the added risk of radial catheterization. The sensor is structurally separated from the primary sheath lumen and readings are unaffected by device introduction through the primary lumen. Time delays and potential complications from radial artery catheterization are avoided. Published by the BMJ Publishing Group Limited. For permission to use (where not already granted under a licence) please go to http://www.bmj.com/company/products-services/rights-and-licensing/.

  19. Effects of MgO impurities and micro-cracks on the critical current density of Ti-sheathed MgB2 wires

    International Nuclear Information System (INIS)

    Liang, G.; Alessandrini, M.; Yen, F.; Hanna, M.; Fang, H.; Hoyt, C.; Lv, B.; Zeng, J.; Salama, K.

    2007-01-01

    Ti-sheathed monocore MgB 2 wires with improved magnetic critical current density (J c ) have been fabricated by in situ powder-in-tube (PIT) method and characterized by magnetization, X-ray diffraction, scanning electron microscopy and electrical resistivity measurements. For the best wire, the magnetic J c values at 5 K and fields of 2 T, 5 T, and 8 T are 4.1 x 10 5 A/cm 2 , 7.8 x 10 4 A/cm 2 , and 1.4 x 10 4 A/cm 2 , respectively. At 20 K and fields of 0.5 T and 3 T, the J c values are about 3.6 x 10 5 A/cm 2 and 3.1 x 10 4 A/cm 2 , respectively, which are much higher than those of the Fe-sheathed mono-core MgB 2 wires fabricated with the same in situ PIT process and under the same fabricating conditions. It appears that the overall J c for the average Ti-sheathed wires is comparable to that of the Fe-sheathed wires. Our X-ray diffraction and scanning electron microscopy analysis indicates that J c in the Ti-sheathed MgB 2 wires can be strongly suppressed by MgO impurities and micro-cracks

  20. Corrosion Engineering.

    Science.gov (United States)

    White, Charles V.

    A description is provided for a Corrosion and Corrosion Control course offered in the Continuing Engineering Education Program at the General Motors Institute (GMI). GMI is a small cooperative engineering school of approximately 2,000 students who alternate between six-week periods of academic study and six weeks of related work experience in…