  1. Extrusion and properties of lead zirconate titanate piezoelectric ceramics

    DEFF Research Database (Denmark)

    Cai, S.; Millar, C.E.; Pedersen, L.

    1997-01-01

    The purpose of this work was to develop a procedure for fabricating electroceramic actuators with good piezoelectric properties. The preparation of lead zirconate titanate (PZT) piezoelectric ceramic rods and tubes by extrusion processing is described. The microstructure of extrudates was investi......The purpose of this work was to develop a procedure for fabricating electroceramic actuators with good piezoelectric properties. The preparation of lead zirconate titanate (PZT) piezoelectric ceramic rods and tubes by extrusion processing is described. The microstructure of extrudates...

  2. Ion Irradiation Damage in Zirconate and Titanate Ceramics for Pu Disposition

    International Nuclear Information System (INIS)

    Stewart, Martin W.; Begg, Bruce D.; Finnie, K.; Colella, Michael; Li, H.; McLeod, Terry; Smith, Katherine L.; Zhang, Zhaoming; Weber, William J.; Thevuthasan, Suntharampillai

    2004-01-01

    In this paper, we discuss the effect of ion irradiation on pyrochlore-rich titanate and defect-fluorite zirconate ceramics designed for plutonium immobilization. Samples, with Ce as an analogue for Pu, were made via oxide routes and consolidated by cold-pressing and sintering. Ion irradiation damage was carried out with 2 MeV Au2+ ions to a fluence of 5 ions nm-2 in the accelerator facilities within the Environmental Molecular Sciences Laboratory at Pacific Northwest National Laboratory. Irradiated and non-irradiated samples were examined by x-ray diffraction, scanning and transmission electron microscopy, x-ray photoelectron and infrared spectroscopy, and spectroscopic ellipsometry. Samples underwent accelerated leach testing at pH 1.75 (nitric acid) at 90 C for 28 days. The zirconate samples were more ion-irradiation damage resistant than the titanate samples, showing little change after ion-irradiation whereas the titanate samples formed an amorphous surface layer ∼ 500 nm thick. While all samples had high aqueous durability, the titanate leach rate was ∼ 5 times that of the zirconate. The ion-irradiation increased the leach rate of the titanate without impurities by ∼ 5 times. The difference in the leach rates between irradiated and unirradiated zirconate samples is small. However, the zirconates were less able to incorporate impurities than the titanate ceramics and required higher sintering temperatures, ∼ 1500 C compared to 1350 C for the titanates.

  3. Pyroelectricity versus conductivity in soft lead zirconate titanate (PZT) ceramics

    NARCIS (Netherlands)

    Kamel, T.M.; With, de G.

    2007-01-01

    The electrical behavior of modified soft lead zirconate titanate (PZT) ceramics has been studied as a function of temperature at different direct current (dc) electric fields and grain sizes. As ferroelectrics, such as PZT, are highly polarizable materials, poling, depolarization, and electric

  4. Fracture mechanisms in lead zirconate titanate ceramics

    International Nuclear Information System (INIS)

    Freiman, S.W.; Chuck, L.; Mecholsky, J.J.; Shelleman, D.L.

    1986-01-01

    Lead Zirconate Titanate (PZT) ceramics can be formed over a wide range of PbTiO 3 /PbZrO 3 ratios and exist in a number of crystal structures. This study involved the use of various fracture mechanics techniques to determine critical fracture toughness, K /SUB IC/ , as a function of composition, microstructure, temperature, and electrical and thermal history. The results of these experiments indicate that variations in K /SUB IC/ are related to phase transformations in the material as well as to other toughening mechanisms such as twinning and microcracking. In addition, the strength and fracture toughness of selected PZT ceramics were determined using specimens in which a crack was introduced by a Vicker's hardness indentor. The variation of K /SUB IC/ with composition and microstructure was related to the extent of twin-crack interaction. Comparison of the plot of strength as a function of indentation load with that predicted from indentation fracture models indicates the presence of internal stresses which contribute to failure. The magnitude of these internal stresses has been correlated with electrical properties of the ceramic. Fractographic analysis was used to determine the magnitude of internal stresses in specimens failing from ''natural flaws.''

  5. Structural and electrical properties of Nd ion modified lead zirconate titanate nanopowders and ceramics

    International Nuclear Information System (INIS)

    Da-Wei, Wang; De-Qing, Zhang; Quan-Liang, Zhao; Hong-Mei, Liu; Zhi-Ying, Wang; Mao-Sheng, Cao; Jie, Yuan

    2009-01-01

    A modified sol-gel method is used for synthesizing Nd ion doped lead zirconate titanate nanopowders Pb 1–3x/2 Nd x Zr 0.52 Ti 0.48 O 3 (PNZT) in an ethylene glycol system with zirconium nitrate as zirconium source. The results show that it is critical to add lead acetate after the reaction of zirconium nitrate with tetrabutyl titanate in the ethylene glycol system for preparing PNZT with an exact fraction of titanium content. It has been observed that the dopant of excess Nd ions can effectively improve the sintered densification and activity of the PNZT ceramics. Piezoelectric, dielectric and ferroelectric properties of the PNZT ceramics are remarkably enhanced as compared with those of monolithic lead zirconate titanate (PZT). Especially, the supreme values of piezoelectric constant (d 33 ) and dielectric constant ( element of ) for the PNZT are both about two times that of the monolithic PZT and moreover, the remnant polarization (P r ) also increases by 30%. According to the analysis of the structures and properties, we attribute the improvement in electrical properties to the lead vacancies caused by the doping of Nd ions

  6. Dielectric behaviors of lead zirconate titanate ceramics with coplanar electrodes

    International Nuclear Information System (INIS)

    Wang, Y.; Cheng, Y.L.; Zhang, Y.W.; Chan, H.L.W.; Choy, C.L.

    2003-01-01

    This paper reports on the dielectric behaviors of lead zirconate titanate (PZT) capacitors with coplanar electrodes. Usually a ferroelectric device has a metal-ferroelectric-metal configuration (parallel plate capacitor); when both the electrodes are on one side of a ceramic to form a coplanar capacitor, different dielectric behaviors will be anticipated because of the change in the distribution of the test field inside the dielectrics. This paper describes how the capacitance and dielectric loss of PZT-based coplanar capacitors change with electrode distance, area and test frequency

  7. Structural Contribution to the Ferroelectric Fatigue in Lead Zirconate Titanate (PZT) Ceramics

    OpenAIRE

    Hinterstein , Manuel; Rouquette , Jerome; Haines , J; Papet , Ph; Glaum , Julia; Knapp , Michael; Eckert , J; Hoffman , M

    2014-01-01

    International audience; Many ferroelectric devices are based on doped lead zirconate titanate (PZT) ceramics with compositions near the morphotropic phase boundary (MPB), at which the relevant material's properties approach their maximum. Based on a synchrotron x-ray diffraction study of MPB PZT, bulk fatigue is unambiguously found to arise from a less effective field induced tetragonal-to-monoclinic transformation, at which the degradation of the polarization flipping is detected by a less i...

  8. Evolution of transverse piezoelectric response of lead zirconate titanate ceramics under hydrostatic pressure

    International Nuclear Information System (INIS)

    Li Fei; Xu Zhuo; Wei Xiaoyong; Gao Junjie; Zhang, Chonghui; Yao Xi; Jin Li

    2009-01-01

    The piezoelectric properties of 31-mode resonators of lead zirconate titanate ceramics under hydrostatic pressure from 0.1 to 325 MPa were evaluated by a fitting method, in which mechanical loss was taken into account. Our results based on the fitting method showed a hydrostatic pressure independent tendency of the piezoelectric coefficient and the electromechanical coupling factor because the adopted PZT ceramic can be considered as a linear system in our experiment, while two misleading tendencies of piezoelectric coefficient were obtained based on the resonance method when ignoring the contribution of the mechanical loss. (fast track communication)

  9. Dynamic fatigue on repolarization of lead zirconate-titanate base ceramics with various ferroelectric hardness

    International Nuclear Information System (INIS)

    Gavrilyachenko, V.G.; Semenchev, A.F.; Sklyarova, E.N.; Kuznetsova, E.M.

    2006-01-01

    One studied experimentally changes of the residual polarization in lead zirconate-titanate base ceramics with various ferroelectric hardness under the effect of a strong varying field. The twinning and untwinning of crystallites accompanying repolarization is assumed to be the basic mechanism of propagation of the crystalline structure defects governing the fatigue rates of the ferroelectric-soft ceramics. In ferroelectric-hard ceramics crystallites the stable configurations of mechanical twins, the result of the secondary twinning, are formed when the hysteresis loop is formed. At repolarization in the mentioned structures one observes no motion of the twin boundaries, and the fatigue rates are low ones [ru

  10. Ferroelastic domain switching fatigue in lead zirconate titanate ceramics

    International Nuclear Information System (INIS)

    Pojprapai, Soodkhet; Jones, Jacob L.; Studer, Andrew J.; Russell, Jennifer; Valanoor, Nagarajan; Hoffman, Mark

    2008-01-01

    The influence of the frequency and amplitude of cyclic mechanical loading on soft, tetragonal lead zirconate titanate (PZT) ceramics was investigated via neutron diffraction. Intensity change in the {2 0 0} reflections provided quantitative measurements of domain switching behavior, domain texture and the strain resulting from domain switching. The results are explained using a viscoelasticity model. It was found that the magnitude of applied stress affects the level of strain accumulated, while its frequency affects the time taken for the strain to reach saturation. Furthermore, markedly different behaviors are exhibited by poled and unpoled samples. For samples loaded under identical conditions, the frequency effect is more pronounced in unpoled samples and the accumulated ferroelastic strain is greater in poled samples

  11. Contribution of the irreversible displacement of domain walls to the piezoelectric effect in barium titanate and lead zirconate titanate ceramics

    CERN Document Server

    Damjanovic, D

    1997-01-01

    The contribution from the irreversible displacement of non-180 deg domain walls to the direct longitudinal piezoelectric d sub 3 sub 3 coefficient of BaTiO sub 3 and Pb(Zr, Ti)O sub 3 ceramics was determined quantitatively by using the Rayleigh law. Effects of the crystal structure and microstructure of the ceramics as well as the external d.c. pressure on the domain wall contribution to d sub 3 sub 3 were examined. In barium titanate, this domain wall contribution is large (up to 35% of the total d sub 3 sub 3 , under the experimental conditions used) and dependent on the external d.c. pressure in coarse grained ceramics, and much smaller and independent of the external d.c. pressure in fine-grained samples. The presence of internal stresses in fine-grained ceramics could account for the observed behaviour. The analysis shows that the domain-wall contribution to the d sub 3 sub 3 in lead zirconate titanate ceramics is large in compositions close to the morphotropic phase boundary that contain a mixture of te...

  12. Barium zirconate-titanate/barium calcium-titanate ceramics via sol-gel process: novel high-energy-density capacitors

    International Nuclear Information System (INIS)

    Puli, Venkata Sreenivas; Kumar, Ashok; Scott, J F; Katiyar, Ram S; Chrisey, Douglas B; Tomozawa, M

    2011-01-01

    Lead-free barium zirconate-titanate/barium calcium-titanate, [(BaZr 0.2 Ti 0.80 )O 3 ] 1-x -[(Ba 0.70 Ca 0.30 )TiO 3 ] x (x = 0.10, 0.15, 0.20) (BZT-BCT) ceramics with high dielectric constant, low dielectric loss and moderate electric breakdown field were prepared by the sol-gel synthesis technique. X-ray diffraction patterns revealed tetragonal crystal structure and this was further confirmed by Raman spectra. Well-behaved ferroelectric hysteresis loops and moderate polarizations (spontaneous polarization, P s ∼ 3-6 μC cm -2 ) were obtained in these BZT-BCT ceramics. Frequency-dependent dielectric spectra confirmed that ferroelectric diffuse phase transition (DPT) exists near room temperature. Scanning electron microscope images revealed monolithic grain growth in samples sintered at 1280 deg. C. 1000/ε versus (T) plots revealed ferroelectric DPT behaviour with estimated γ values of ∼1.52, 1.51 and 1.88, respectively, for the studied BZT-BCT compositions. All three compositions showed packing-limited breakdown fields of ∼47-73 kV cm -1 with an energy density of 0.05-0.6 J cm -3 for thick ceramics (>1 mm). Therefore these compositions might be useful in Y5V-type capacitor applications.

  13. Improvement of conditions for ceramics sintering on the base of lead zirconate-titanate

    International Nuclear Information System (INIS)

    Glinchuk, M.D.; Kim, P.V.; Bykov, I.P.; Lyashchenko, A.B.

    1989-01-01

    Lead zirconate-titanate powders of different graininess are studied for their phase composition. The finest grains of the powder consist of lead zirconate-titanate with the rhombohedral structure. Grains of 3-5 μm size are a mixture of lead zirconate-titanate and lead titanate, the latter exceeding 50% (by weight) causes the effect of anomalous expansion in the process of sintering. Control of the technological parameters of the synthesis permits producing powder with favourable correlation of the above phases and grain sizes. Sintering of such a powder induces no effect of the anomalous expansion with an increased density of the product attained

  14. Structural contribution to the ferroelectric fatigue in lead zirconate titanate ceramics

    Science.gov (United States)

    Hinterstein, M.; Rouquette, J.; Haines, J.; Papet, Ph.; Glaum, J.; Knapp, M.; Eckert, J.; Hoffman, M.

    2014-09-01

    Many ferroelectric devices are based on doped lead zirconate titanate (PZT) ceramics with compositions near the morphotropic phase boundary (MPB), at which the relevant material's properties approach their maximum. Based on a synchrotron x-ray diffraction study of MPB PZT, bulk fatigue is unambiguously found to arise from a less effective field induced tetragonal-to-monoclinic transformation, at which the degradation of the polarization flipping is detected by a less intense and more diffuse anomaly in the atomic displacement parameter of lead. The time dependence of the ferroelectric response on a structural level down to 250 μs confirms this interpretation in the time scale of the piezolectric strain response.

  15. Barium zirconate-titanate/barium calcium-titanate ceramics via sol-gel process: novel high-energy-density capacitors

    Energy Technology Data Exchange (ETDEWEB)

    Puli, Venkata Sreenivas; Kumar, Ashok; Scott, J F; Katiyar, Ram S [SPECLAB, Department of Physics, University of Puerto Rico, San Juan, PR 00936 (Puerto Rico); Chrisey, Douglas B; Tomozawa, M, E-mail: rkatiyar@uprrp.edu [Department of Materials Science and Engineering, Rensselaer Polytechnic Institute, Troy, NY 12180-3590 (United States)

    2011-10-05

    Lead-free barium zirconate-titanate/barium calcium-titanate, [(BaZr{sub 0.2}Ti{sub 0.80})O{sub 3}]{sub 1-x}-[(Ba{sub 0.70}Ca{sub 0.30})TiO{sub 3}]{sub x} (x = 0.10, 0.15, 0.20) (BZT-BCT) ceramics with high dielectric constant, low dielectric loss and moderate electric breakdown field were prepared by the sol-gel synthesis technique. X-ray diffraction patterns revealed tetragonal crystal structure and this was further confirmed by Raman spectra. Well-behaved ferroelectric hysteresis loops and moderate polarizations (spontaneous polarization, P{sub s} {approx} 3-6 {mu}C cm{sup -2}) were obtained in these BZT-BCT ceramics. Frequency-dependent dielectric spectra confirmed that ferroelectric diffuse phase transition (DPT) exists near room temperature. Scanning electron microscope images revealed monolithic grain growth in samples sintered at 1280 deg. C. 1000/{epsilon} versus (T) plots revealed ferroelectric DPT behaviour with estimated {gamma} values of {approx}1.52, 1.51 and 1.88, respectively, for the studied BZT-BCT compositions. All three compositions showed packing-limited breakdown fields of {approx}47-73 kV cm{sup -1} with an energy density of 0.05-0.6 J cm{sup -3} for thick ceramics (>1 mm). Therefore these compositions might be useful in Y5V-type capacitor applications.

  16. Investigation of the additive induced doping effects in gelcast soft lead zirconate titanate ceramics

    International Nuclear Information System (INIS)

    Guo Dong; Cai Kai; Li Longtu; Gui Zhilun

    2009-01-01

    Due to the high sensitivity of the electrical properties of electronic ceramics to various factors, knowledge about the possible influence of the processing procedure on their electrical performance is critical for applying a new technique to the fabrication of the materials. In this study, various electrical parameters, complex impedance spectra, ferroelectric hysteresis loops, and microstructures of soft lead zirconate titanate (PZT) ceramics formed by the gelcasting technique from suspensions with various dispersants were investigated in comparison with those of the conventional dry pressed ones. We found that the sodium ion, which is the main cation in many commercial surfactants, exhibited obvious hard doping effects; thus causing deteriorated performance of the gelcast PZT ceramics. While a certain impurity ion introduced by a dispersant was also found to induce soft doping characteristics and improve the electrical performance of the materials. The results suggest that the doping effects of the metal ions or impurities introduced by the dispersants, or other additives, should be generally considered for applying a wet processing technique to forming multicomponent electronic ceramics.

  17. Determination of temperature dependence of piezoelectric coefficients matrix of lead zirconate titanate ceramics by quasi-static and resonance method

    International Nuclear Information System (INIS)

    Li Fei; Xu Zhuo; Wei Xiaoyong; Yao Xi

    2009-01-01

    The piezoelectric coefficients (d 33 , -d 31 , d 15 , g 33 , -g 31 , g 15 ) of soft and hard lead zirconate titanate ceramics were measured by the quasi-static and resonance methods, at temperatures from 20 to 300 0 C. The results showed that the piezoelectric coefficients d 33 , -d 31 and d 15 obtained by these two methods increased with increasing temperature for both hard and soft PZT ceramics, while the piezoelectric coefficients g 33 , -g 31 and g 15 decreased with increasing temperature for both hard and soft PZT ceramics. In this paper, the observed results were also discussed in terms of intrinsic and extrinsic contributions to piezoelectric response.

  18. Anisotropy of domain switching in prepoled lead titanate zirconate ceramics under multiaxial electrical loading

    Science.gov (United States)

    Liu, Yuan-Ming; Li, Fa-Xin; Fang, Dai-Ning

    2007-01-01

    The authors report an observation of anisotropic domain switching process in prepoled lead titanate zirconate (PZT) ceramics under multiaxial electrical loading. Prepoled PZT blocks were obliquely cut to apply an electric field at discrete angles θ (0°-180°) to the initial poling direction. Both the coercive field and switchable polarization are found to decrease significantly when sinθ increases from zero to unity. The measured strain curves show that most domains that accomplished 180° domain switching actually experienced two successive 90° switching. The oriented domain texture after poling plus the induced nonuniform stress are used to explain the observed domain switching anisotropy.

  19. Elution of lead from lead zirconate titanate ceramics to acid rain

    Science.gov (United States)

    Tsurumi, Takaaki; Takezawa, Shuhei; Hoshina, Takuya; Takeda, Hiroaki

    2017-10-01

    The amount of lead that eluted from lead zirconate titanate (PZT) ceramics to artificial acid rain was evaluated. Four kinds of PZT ceramics, namely, pure PZT at MPB composition, CuO-added PZT, PZT with 10 mol % substitution of Ba for Pb, and CuO-added PZT with 10 mol % substitution of Ba for Pb, were used as samples of the elution test. These PZT ceramics of 8 mm2 and 1.1-1.2 mm thickness were suspended in 300 ml of H2SO4 solution of pH 4.0. The concentration of lead eluted from PZT was in the range from 0.2 to 0.8 ppm. It was found that both liquid phase formation by the addition of CuO and the substitution of Ba for Pb were effective to reduce the amount of lead that eluted. By fitting the leaching out curve with a classical equation, a master curve assuming no sampling effect was obtained. The lead concentration evaluated from the amount of lead that eluted from a commercial PZT plate to H2SO4 solution of pH 5.3 was almost the same as the limit in city water. It is concluded that PZT is not harmful to health and the environment and the amount of lead that eluted from PZT can be controlled by modifying PZT composition.

  20. Determination of temperature dependence of piezoelectric coefficients matrix of lead zirconate titanate ceramics by quasi-static and resonance method

    Energy Technology Data Exchange (ETDEWEB)

    Li Fei; Xu Zhuo; Wei Xiaoyong; Yao Xi, E-mail: lifei1216@gmail.co [Electronic Materials Research Laboratory, Key Laboratory of the Ministry of Education, Xi' an Jiaotong University, Xi' an 710049 (China)

    2009-05-07

    The piezoelectric coefficients (d{sub 33}, -d{sub 31}, d{sub 15}, g{sub 33}, -g{sub 31}, g{sub 15}) of soft and hard lead zirconate titanate ceramics were measured by the quasi-static and resonance methods, at temperatures from 20 to 300 {sup 0}C. The results showed that the piezoelectric coefficients d{sub 33}, -d{sub 31} and d{sub 15} obtained by these two methods increased with increasing temperature for both hard and soft PZT ceramics, while the piezoelectric coefficients g{sub 33}, -g{sub 31} and g{sub 15} decreased with increasing temperature for both hard and soft PZT ceramics. In this paper, the observed results were also discussed in terms of intrinsic and extrinsic contributions to piezoelectric response.

  1. Dynamic pyroelectric response of composite based on ferroelectric copolymer of poly(vinylidene fluoride-trifluoroethylene) and ferroelectric ceramics of barium lead zirconate titanate

    Energy Technology Data Exchange (ETDEWEB)

    Solnyshkin, A.V. [Tver State University, Department of Condensed Matter Physics, Tver (Russian Federation); National Research University ' ' MIET' ' , Department of Intellectual Technical Systems, Zelenograd, Moscow (Russian Federation); Morsakov, I.M.; Bogomolov, A.A. [Tver State University, Department of Condensed Matter Physics, Tver (Russian Federation); Belov, A.N.; Vorobiev, M.I.; Shevyakov, V.I.; Silibin, M.V. [National Research University ' ' MIET' ' , Department of Intellectual Technical Systems, Zelenograd, Moscow (Russian Federation); Shvartsman, V.V. [University of Duisburg-Essen, Institute for Materials Science, Essen (Germany)

    2015-10-15

    In this work, pyroelectric properties of composite films on the basis of poly(vinylidene fluoride-trifluoroethylene) copolymer with a various level of ferroelectric ceramics inclusions of barium lead zirconate titanate solid solution were investigated by the dynamic method. The composite films were prepared by the solvent cast method. The unusual spike-like dynamic response with a quasi-stationary component was observed. It is supposed that composite films may be effectively used for pyroelectric applications. (orig.)

  2. Fractal cluster modeling of the fatigue behavior of lead zirconate titanate

    OpenAIRE

    Priya, Shashank; Kim, Hyeoung Woo; Ryu, Jungho; Uchino, Kenji; Viehland, Dwight D.

    2002-01-01

    The fatigue behavior of lead zirconate titanate ceramics (PZT) has been studied under electrical and mechanical drives. Piezoelectric fatigue was studied using a mechanical method. Under ac mechanical drive, hard and soft PZTs showed an increase in the longitudinal piezoelectric constant at short times, reaching a maximum at intermediate times. Systematic investigations were performed to characterize the electrical fatigue behavior. A decrease in the magnitude of the remanent polarization was...

  3. Dielectric properties of composite based on ferroelectric copolymer of poly(vinylidene fluoride-trifluoroethylene and ferroelectric ceramics of barium lead zirconate titanate

    Directory of Open Access Journals (Sweden)

    A. V. Solnyshkin

    2017-10-01

    Full Text Available A study of dielectric properties of composite films on the base of poly(vinylidene fluoride-trifluoroethylene copolymer P(VDF-TrFE and ferroelectric ceramics of barium lead zirconate titanate (BPZT solid solution is presented in this work. The composite films containing up to 50 vol.% of BPZT grains with size ∼1μm were prepared by the solvent cast method. Frequency dependences of real and imaginary components of the complex permittivity were determined. The concentration dependence of the dielectric constant was discussed.

  4. Effect of MnO2, Bi2O3, and ZnO additions on the electrical properties of lead zirconate titanate piezo ceramics

    International Nuclear Information System (INIS)

    Klimov, V.V.; Selikova, N.I.; Bronnikov, A.N.

    2006-01-01

    The effect of manganese dioxide additions on the electrical properties of lead zirconate titanate (PZT) piezo ceramics has been investigated. The results demonstrate that, taken alone, manganese dioxide does not ensure the formation of hard PZT. The valence state of manganese in the piezo ceramics is shown to be 4+ if no other dopants are present and 3+ if manganese is introduced in combination with Bi and Zn. Microstructural examination indicates that the grain size of the singly doped ceramics is 5-15 μm, while that of the codoped ceramics is 1-3 μm. The polarization current curves of the piezo ceramics containing manganese, bismuth, and zinc oxides have extra maxima, which points to significant internal fields. The manganese is shown to reside at grain boundaries. The conclusion is made that it is the composition of Mn-containing intergranular phases, rather than the presence of manganese ions, that plays a key role in the formation of hard piezo ceramics [ru

  5. Fracture mechanisms in ferroelectric-ferroelastic lead zirconate titanate (Zr:Ti = 0.54:0.46) ceramics

    International Nuclear Information System (INIS)

    Mehta, K.; Virkar, A.V.

    1990-01-01

    Fracture toughness, K IC , of a single-phase commercial lead zirconate titanate (PZT) ceramic of tetragonal structure was measured using the single edge notched beam method above and below the Curie temperature. Domain switching (poling) under electrical and mechanical loading was examined using x-ray diffraction. Surface grinding, electrical poling, and mechanical poling caused crystallographic texture. Similar texture, indicative of domain switching, was also observed on fracture surfaces of some samples fractured at room temperature. At room temperature, the highest K IC measured was 1.85 MPa · m 1/2 , while above the Curie temperature it was about 1.0 MPa · m 1/2 . Cracks emanating from Vickers indents in poled samples were different in the poling and the transverse directions. The difference in crack sizes is explained on the basis of domain switching during crack growth. These results indicate that ferroelastic domain switching (twinning) is a viable toughening mechanism in the PZT materials tested

  6. Improvement of fatigue resistance for multilayer lead zirconate titanate (PZT)-based ceramic actuators by external mechanical loads

    Science.gov (United States)

    Yang, Gang; Yue, Zhenxing; Ji, Ye; Chu, Xiangcheng; Li, Longtu

    2008-12-01

    The influence of external compressive loads, applied along a direction perpendicular to polarization, on fatigue behaviors of multilayer lead zirconate titanate (PZT)-based ceramic actuators was investigated. Under no external mechanical load, a normal fatigue behavior was observed, demonstrating that both switching polarization (Pswitching) and remnant polarization (Pr) progressively decreased with increasing switching cycles due to domain pinning by charge point defects. However, an anomalous enhancement in both switching and remnant polarizations was observed upon application of the external compressive loads. After 5×106 cycles of polarization switching, Pswitching and Pr increase by about 13% and 6% at 40 MPa, respectively, while Pswitching and Pr increase by about 11% and 21% at 60 MPa, respectively. The improvement of fatigue resistance can be attributed to non-180° domain switching and suppression of microcracking, triggered by external mechanical loads.

  7. Quantitative analysis method for niobium in lead zirconate titanate

    International Nuclear Information System (INIS)

    Hara, Hideo; Hashimoto, Toshio

    1986-01-01

    Lead zirconate titanate (PZT) is a strong dielectric ceramic having piezoelectric and pyroelectric properties, and is used most as a piezoelectric material. Also it is a main component of lead lanthanum zirconate titanate (PLZT), which is a typical electrical-optical conversion element. Since these have been developed, the various electronic parts utilizing the piezoelectric characteristics have been put in practical use. The characteristics can be set up by changing the composition of PZT and the kinds and amount of additives. Among the additives, niobium has the action to make metallic ion vacancy in crystals, and by the formation of this vacancy, to ease the movement of domain walls in crystal grains, and to increase resistivity. Accordingly, it is necessary to accurately determine the niobium content for the research and development, quality control and process control. The quantitative analysis methods for niobium used so far have respective demerits, therefore, the authors examined the quantitative analysis of niobium in PZT by using an inductively coupled plasma emission spectro-analysis apparatus which has remarkably developed recently. As the result, the method of dissolving a specimen with hydrochloric acid and hydrofluoric acid, and masking unstable lead with ethylene diamine tetraacetic acid 2 sodium and fluoride ions with boric acid was established. The apparatus, reagents, the experiment and the results are reported. (Kako, I.)

  8. Modification of surface texture by grinding and polishing lead zirconate titanate ceramics

    International Nuclear Information System (INIS)

    Cheng, S.; Lloyd, I.K.

    1992-01-01

    This paper reports that grinding and polishing affected the orientation of 90 degrees domains at the surface of lead zirconate titanate (PZT) ceramics. This was quantified by using changes in the intensity ratio of the (002) and (200) X-ray reflections. Grinding unpoled PZT with 600-grit SiC paper gave X-ray intensity ratios similar to those of poled material. This implies that 90 degrees domain realignments had occurred in the near surface region probed by the X-rays. Grinding poled samples with 600-grit SiC further increased the X-ray intensity ratio beyond that caused by poling, indicating that additional surface reorientation of 90 degrees domains had occurred. The effects of diamond polishing depended on the size of the diamond particles. The use of 6-μm diamond had no effect on the (002)/(200) intensity ratio of either poled or unpoled samples, while polishing with 15- or 45-μm diamond significantly enhanced the 90 degrees domain rotation. In unpoled samples, the increase in the X-ray intensity ratio then approached that induced by poling or grinding with 600-grit SiC paper. While the observed increase in X-ray intensity ratio upon grinding is attributed to the rotation of 90 degrees domains, the simultaneous formation of 180 degrees domains appears to minimize or reduce the increase in electrical polarization

  9. Grain growth kinetics and electrical properties of lanthanum modified lead zirconate titanate (9/65/35) based ferroelectric ceramics

    International Nuclear Information System (INIS)

    Roca, R. Alvarez; Guerrero, F.; Botero, E. R.; Garcia, D.; Eiras, J. A.; Guerra, J. D. S.

    2009-01-01

    The influence of the microstructural characteristics on the dielectric and electrical properties has been investigated for Nd 3+ doped lanthanum modified lead zirconate titanate ferroelectric ceramics, obtained by the conventional solid-state reaction method, by taking into account different sintering conditions. The grain growth mechanism has been investigated and a cubic-type grain growth law was observed for samples with grain size varying from 1.00 up to 2.35 μm. The porosity and grain size dependences of the phase transition parameters, such as the maximum dielectric permittivity and its corresponding temperature (ε m and T m , respectively) were also investigated. The ac conductivity analyses followed the universal Jonscher law. The behavior of the frequency exponent (s) was analyzed through the correlated barrier hopping model. Both ac and dc conductivity results have been correlated with the observed microstructural features

  10. Current—voltage characteristics of lead zirconate titanate/nickel bilayered hollow cylindrical magnetoelectric composites

    International Nuclear Information System (INIS)

    De-An, Pan; Shen-Gen, Zhang; Jian-Jun, Tian; Li-Jie, Qiao; Jun-Sai, Sun; Volinsky, Alex A.

    2010-01-01

    Current–voltage measurements obtained from lead zirconate titanate/nickel bilayered hollow cylindrical magnetoelectric composite showed that a sinusoidal current applied to the copper coil wrapped around the hollow cylinder circumference induces voltage across the lead zirconate titanate layer thickness. The current–voltage coefficient and the maximum induced voltage in lead zirconate titanate at 1 kHz and resonance (60.1 kHz) frequencies increased linearly with the number of the coil turns and the applied current. The resonance frequency corresponds to the electromechanical resonance frequency. The current–voltage coefficient can be significantly improved by optimizing the magnetoelectric structure geometry and/or increasing the number of coil turns. Hollow cylindrical lead zirconate titanate/nickel structures can be potentially used as current sensors. (condensed matter: electronic structure, electrical, magnetic, and optical properties)

  11. The determination of major and some minor constituents in lead zirconate-titanate compositions by x-ray fluorescence and atomic absorption spectrometry

    NARCIS (Netherlands)

    van Willigen, J.H.H.G.; Kruidhof, H.; Dahmen, E.A.M.F.

    1972-01-01

    An accurate X-ray fluorescence spectrometric method is described for the determination of lead, zirconium and titanium in lead zirconate-titanate ceramics. Careful matching of samples and standards by a borax fusion method resulted in a relative standard deviation of about 0.2% for the major

  12. Electric field tuning of magnetism in heterostructure of yttrium iron garnet film/lead magnesium niobate-lead zirconate titanate ceramic

    Science.gov (United States)

    Lian, Jianyun; Ponchel, Freddy; Tiercelin, Nicolas; Chen, Ying; Rémiens, Denis; Lasri, Tuami; Wang, Genshui; Pernod, Philippe; Zhang, Wenbin; Dong, Xianlin

    2018-04-01

    In this paper, the converse magnetoelectric (CME) effect by electric field tuning of magnetization in an original heterostructure composed of a polycrystalline yttrium iron garnet (YIG) film and a lead magnesium niobate-lead zirconate titanate (PMN-PZT) ceramic is presented. The magnetic performances of the YIG films with different thicknesses under a DC electric field applied to the PMN-PZT ceramics and a bias magnetic field are investigated. All the magnetization-electric field curves are found to be in good agreement with the butterfly like strain curve of the PMN-PZT ceramic. Both the sharp deformation of about 2.5‰ of PMN-PZT and the easy magnetization switching of YIG are proposed to be the reasons for the strongest CME interaction in the composite at the small electric coercive field of PMN-PZT (4.1 kV/cm) and the small magnetic coercive field of YIG (20 Oe) where the magnetic susceptibility reaches its maximum value. A remarkable CME coefficient of 3.1 × 10-7 s/m is obtained in the system with a 600 nm-thick YIG film. This heterostructure combining multiferroics and partially magnetized ferrite concepts is able to operate under a small or even in the absence of an external bias magnetic field and is more compact and power efficient than the traditional magnetoelectric devices.

  13. Molten salt synthesis of lead lanthanum zirconate titanate ceramic powders

    International Nuclear Information System (INIS)

    Cai Zongying; Xing Xianran; Li Lu; Xu Yeming

    2008-01-01

    Lead lanthanum zirconate titanate (Pb 0.95 La 0.03 )(Zr 0.52 Ti 0.48 )O 3 (PLZT) was synthesized by one step molten salt method with the starting materials of PbC 2 O 4 , La 2 O 3 , ZrO(NO 3 ) 2 .2H 2 O and TiO 2 in the NaCl-KCl eutectic mixtures in the temperature range of 700-1000 deg. C. The single phase of (Pb 0.95 La 0.03 )(Zr 0.52 Ti 0.48 )O 3 powders was prepared at a temperature as low as 850 deg. C for 5 h. The effects of process parameters, such as soaking temperature and time, salt species, and the amount of flux with respect to the starting materials were investigated. The growth process of the PLZT particles in the molten salt undergoes a transition from a diffusion controlled mechanism to an interfacial reaction controlled mechanism at 900 deg. C

  14. Electrophoretic growth of lead zirconate titanate nanorods

    Energy Technology Data Exchange (ETDEWEB)

    Limmer, S.J.; Seraji, S.; Forbess, M.J.; Wu Yun; Chou, T.P.; Nguyen, C.; Cao Guozhong [Washington Univ., Seattle, WA (United States). Dept. of Materials Science and Engineering

    2001-08-16

    Nanorods of lead zirconate titanate (PZT)-a ferro- and piezoelectric material-up to 10 {mu}m in length and 70 to 150 nm in diameter are produced by sol-gel electrophoresis of PZT in a track-etched polycarbonate membrane, which is used as a template. (orig.)

  15. Fabrication and characterization of thick-film piezoelectric lead zirconate titanate ceramic resonators by tape-casting.

    Science.gov (United States)

    Qin, Lifeng; Sun, Yingying; Wang, Qing-Ming; Zhong, Youliang; Ou, Ming; Jiang, Zhishui; Tian, Wei

    2012-12-01

    In this paper, thick-film piezoelectric lead zirconate titanate (PZT) ceramic resonators with thicknesses down to tens of micrometers have been fabricated by tape-casting processing. PZT ceramic resonators with composition near the morphotropic phase boundary and with different dopants added were prepared for piezoelectric transducer applications. Material property characterization for these thick-film PZT resonators is essential for device design and applications. For the property characterization, a recently developed normalized electrical impedance spectrum method was used to determine the electromechanical coefficient and the complex piezoelectric, elastic, and dielectric coefficients from the electrical measurement of resonators using thick films. In this work, nine PZT thick-film resonators have been fabricated and characterized, and two different types of resonators, namely thickness longitudinal and transverse modes, were used for material property characterization. The results were compared with those determined by the IEEE standard method, and they agreed well. It was found that depending on the PZT formulation and dopants, the relative permittivities ε(T)(33)/ε(0) measured at 2 kHz for these thick-films are in the range of 1527 to 4829, piezoelectric stress constants (e(33) in the range of 15 to 26 C/m(2), piezoelectric strain constants (d(31)) in the range of -169 × 10(-12) C/N to -314 × 10(-12) C/N, electromechanical coupling coefficients (k(t)) in the range of 0.48 to 0.53, and k(31) in the range of 0.35 to 0.38. The characterization results shows tape-casting processing can be used to fabricate high-quality PZT thick-film resonators, and the extracted material constants can be used to for device design and application.

  16. Displacive Transformation in Ceramics

    Science.gov (United States)

    1994-02-28

    PZT ), ceramics have attracted natural abundance. much attention for use in nonvolatile semiconductor mem- We attribute the observed spectra in Fig. I to...near a crack tip in piezoelectric ceramics of lead zirconate titanate ( PZT ) and barium titanate. They reasoned that the poling of ferroelectric... Texture in Ferroelastic Tetragonal Zirconia," J. Am. Ceram . Soc., 73 (1990) no. 6: 1777-1779. 27. J. F. Jue and A. Virkar, "Fabrication, Microstructural

  17. Mechanical and dielectric characterization of lead zirconate titanate(PZT)/polyurethane(PU) thin film composite for energy harvesting

    Science.gov (United States)

    Aboubakr, S.; Rguiti, M.; Hajjaji, A.; Eddiai, A.; Courtois, C.; d'Astorg, S.

    2014-04-01

    The Lead Zirconate titanate (PZT) ceramic is known by its piezoelectric feature, but also by its stiffness, the use of a composite based on a polyurethane (PU) matrix charged by a piezoelectric material, enable to generate a large deformation of the material, therefore harvesting more energy. This new material will provide a competitive alternative and low cost manufacturing technology of autonomous systems (smart clothes, car seat, boat sail, flag ...). A thin film of the PZT/PU composite was prepared using up to 80 vol. % of ceramic. Due to the dielectric nature of the PZT, inclusions of this one in a PU matrix raises the permittivity of the composite, on other hand this latter seems to decline at high frequencies.

  18. Real-Time Salmonella Detection Using Lead Zirconate Titanate-Titanium Microcantilevers

    National Research Council Canada - National Science Library

    McGovern, John-Paul; Shih, Wan Y; Shih, Wei-Heng; Sergi, Mauro; Chaiken, Irwin

    2005-01-01

    .... We have developed and investigated the use of a lead zirconate titanate - titanium (PZT-Ti) microcantilever for in situ detection of the common food- and water-born pathogen, Salmonella typhimurium...

  19. Evolution of bias field and offset piezoelectric coefficient in bulk lead zirconate titanate with fatigue

    International Nuclear Information System (INIS)

    Zhang Yong; Baturin, Ivan S.; Aulbach, Emil; Lupascu, Doru C.; Kholkin, Andrei L.; Shur, Vladimir Ya.; Roedel, Juergen

    2005-01-01

    Hysteresis loops of the piezoelectric coefficient, d 33 =f(E 3 ), are measured on virgin and fatigued lead zirconate titanate ceramics. Four parameters are directly extracted from the measurements: internal bias field E b , offset piezoelectric coefficient d offset , coercive field E c , and remnant piezoelectric coefficient d r . The reduction in d r displays the decreasing switchable polarization with fatigue cycling. E b and d offset are found to be linearly related. After thermal annealing, both offsets disappear, while the increase in E c and the reduction in d r withstand annealing. The microscopic entities responsible for the offsets are less stable than those for reduced switching

  20. Lead-free piezoelectric (K,Na)NbO3-based ceramic with planar-mode coupling coefficient comparable to that of conventional lead zirconate titanate

    Science.gov (United States)

    Ohbayashi, Kazushige; Matsuoka, Takayuki; Kitamura, Kazuaki; Yamada, Hideto; Hishida, Tomoko; Yamazaki, Masato

    2017-06-01

    We developed a (K,Na)NbO3-based lead-free piezoelectric ceramic with a KTiNbO5 system, (K1- x Na x )0.86Ca0.04Li0.02Nb0.85O3-δ-K0.85Ti0.85Nb1.15O5-BaZrO3-Fe2O3-MgO (K1- x N x N-NTK-FM). K1- x N x N-NTK-FM ceramic exhibits a very dense microstructure and a coupling coefficient of k p = 0.59, which is almost comparable to that of conventional lead zirconate titanate (PZT). The (K,Na)NbO3-based ceramic has the Γ15 mode for a wide x range. The nanodomains of orthorhombic (K,Na)NbO3 with the M3 mode coexist within the tetragonal Γ15 mode (K,Na)NbO3 matrix. Successive phase transition cannot occur with increasing x. The maximum k p is observed at approximately the minimum x required to generate the M3 mode phase. Unlike the behavior at the morphotropic phase boundary (MPB) in PZT, the characteristics of K1- x N x N-NTK-FM ceramic in this region changed moderately. This gentle phase transition seems to be a relaxor, although the diffuseness degree is not in line with this hypothesis. Furthermore, piezoelectric properties change from “soft” to “hard” upon the M3 mode phase aggregation.

  1. Fatigue studies in compensated bulk lead zirconate titanate

    International Nuclear Information System (INIS)

    Verdier, Cyril; Morrison, Finlay D.; Lupascu, Doru C.; Scott, James F.

    2005-01-01

    Impedance analysis studies were carried out on compensated bulk lead zirconate titanate samples. Fatigue is concomitant with the onset of dielectric loss. This is shown to be dominantly due to an irreversibly modified near-surface layer that can be polished off. The highly compensated nature of these samples minimizes the role of oxygen vacancies

  2. Dynamic processes of domain switching in lead zirconate titanate under cyclic mechanical loading by in situ neutron diffraction

    International Nuclear Information System (INIS)

    Pojprapai, Soodkhet; Luo, Zhenhua; Clausen, Bjorn; Vogel, Sven C.; Brown, Donald W.; Russel, Jennifer; Hoffman, Mark

    2010-01-01

    The performance of ferroelectric ceramics is governed by the ability of domains to switch. A decrease in the switching ability can lead to degradation of the materials and failure of ferroelectric devices. In this work the dynamic properties of domain reorientation are studied. In situ time-of-flight neutron diffraction is used to probe the evolution of ferroelastic domain texture under mechanical cyclic loading in bulk lead zirconate titanate ceramics. The high sensitivity of neutron diffraction to lattice strain is exploited to precisely analyze the change of domain texture and strain through a full-pattern Rietveld method. These results are then used to construct a viscoelastic model, which explains the correlation between macroscopic phenomena (i.e. creep and recovered deformation) and microscopic dynamic behavior (i.e. ferroelastic switching, lattice strain).

  3. Microwave emission from lead zirconate titanate induced by impulsive mechanical load

    Energy Technology Data Exchange (ETDEWEB)

    Aman, A., E-mail: alexander.aman@ovgu.de [Department of Engineering, Brandenburg University of Applied Science, 14470 Brandenburg an derHavel (Germany); Packaging Group, Institute of Micro- and Sensorsytems, Otto-von-Guericke University, Universitätsplatz 2, 39106 Magdeburg (Germany); Majcherek, S. [Packaging Group, Institute of Micro- and Sensorsytems, Otto-von-Guericke University, Universitätsplatz 2, 39106 Magdeburg (Germany); Hirsch, S. [Department of Engineering, Brandenburg University of Applied Science, 14470 Brandenburg an derHavel (Germany); Schmidt, B. [Chair of Micorsystem Technology, Institute of Micro- and Sensorsytems, Otto-von-Guericke University, Universitätsplatz 2, 39106 Magdeburg (Germany)

    2015-10-28

    This paper focuses on microwave emission from Lead zirconate titanate Pb [Zr{sub x}Ti{sub 1−x}] O{sub 3} (PZT) induced by mechanical stressing. The mechanical stress was initiated by impact of a sharp tungsten indenter on the upper surface of PZT ceramic. The sequences of microwave and current impulses, which flew from indenter to electric ground, were detected simultaneously. The voltage between the upper and lower surface of ceramic was measured to obtain the behavior of mechanical force acting on ceramic during the impact. It was found that the amplitude, form, and frequency of measured microwave impulses were different by compression and restitution phase of impact. Two different mechanisms of electron emission, responsible for microwave impulse generation, were proposed based on the dissimilar impulse behavior. The field emission from tungsten indenter is dominant during compression, whereas ferroemission dominates during restitution phase. Indeed, it was observed that the direction of the current flow, i.e., sign of current impulses is changed by transitions from compression to restitution phase of impact. The observed dissimilar behavior of microwave impulses, caused by increasing and decreasing applied force, can be used to calculate the contact time and behavior of mechanical force during mechanical impact on ceramic surface. It is shown that the generation of microwave impulses exhibits high reproducibility, impulse intensity, a low damping factor, and high mechanical failure resistance. Based on these microwave emission properties of PZT, the development of new type of stress sensor with spatial resolution of few microns becomes possible.

  4. Electrical fatigue behaviour in lead zirconate titanate: an experimental and theoretical study

    International Nuclear Information System (INIS)

    Bhattacharyya, Mainak; Arockiarajan, A

    2013-01-01

    A systematic investigation on electrical fatigue in lead zirconate titanate (PZT) is carried out for different loading frequencies. Experiments are conducted up to 10 6 cycles to measure the electrical displacement and longitudinal strain on bulk ceramics in the bipolar mode with large electrical loading conditions. A simplified macroscopic model based on physical mechanisms of domain switching is developed to predict the non-linear behaviour. In this model, the volume fraction of a domain is used as the internal variable by considering the mechanisms of domain nucleation and propagation (domain wall movement). The measured material properties at different fatigue cycles are incorporated into the switching model as damage parameters and the classical strain versus electric field and electric displacement versus electric field curves are simulated. Comparison between the experiments and simulations shows that the proposed model can reproduce the characteristics of non-linear as well as fatigue responses. (paper)

  5. Electrical fatigue behaviour in lead zirconate titanate: an experimental and theoretical study

    Science.gov (United States)

    Bhattacharyya, Mainak; Arockiarajan, A.

    2013-08-01

    A systematic investigation on electrical fatigue in lead zirconate titanate (PZT) is carried out for different loading frequencies. Experiments are conducted up to 106 cycles to measure the electrical displacement and longitudinal strain on bulk ceramics in the bipolar mode with large electrical loading conditions. A simplified macroscopic model based on physical mechanisms of domain switching is developed to predict the non-linear behaviour. In this model, the volume fraction of a domain is used as the internal variable by considering the mechanisms of domain nucleation and propagation (domain wall movement). The measured material properties at different fatigue cycles are incorporated into the switching model as damage parameters and the classical strain versus electric field and electric displacement versus electric field curves are simulated. Comparison between the experiments and simulations shows that the proposed model can reproduce the characteristics of non-linear as well as fatigue responses.

  6. Electrical and thermal properties of lead titanate glass ceramics

    International Nuclear Information System (INIS)

    Shankar, J.; Deshpande, V.K.

    2011-01-01

    Glass samples with composition of (50-X)PbO-(25+X)TiO 2 -25B 2 O 3 (where X=0, 5, 10 and 12.5 mol%) were prepared using conventional quenching technique. The glass transition temperature, T g and crystallization temperature T c were determined from the DTA. These glass samples were converted to glass ceramics by following two stage heat treatment schedule. The glass ceramic samples were characterized by XRD, SEM and dielectric constant measurements. The XRD results revealed the formation of ferroelectric lead titanate (PT) as a major crystalline phase in the glass ceramics. The density increases and the CTE decreases for all glass ceramics with increase in X (mol%). This may be attributed to increase in PT phase. The SEM results which show rounded crystallites of lead titanate, also supports other results. Hysteresis loops observed at room temperature confirms the ferroelectric nature of glass ceramics. The optimized glass ceramic sample exhibits high dielectric constant which is of technical importance. -- Research Highlights: →Lead titanate glass ceramics prepared by conventional quenching technique. →Lead titanate is a major crystalline phase in the glass ceramics. →The ferroelectric nature of glass ceramics is confirmed by the hysteresis study. →The high value of ε observed at room temperature is quite promising in the study.

  7. A polarized Raman study of the relaxor and ferroelectric states of La-modified lead zirconate titanate ceramics

    International Nuclear Information System (INIS)

    El Marssi, M.; Farhi, R.; Viehland, D.

    1997-01-01

    Lanthanum modified lead zirconate titanate ceramics with La/Zr/Ti ratios of 6/40/60, 12/40/60, 5/65/35, and 9/65/35 have been studied by polarized Raman scattering. In the two former (tetragonal-type) compositions, selection rules were rather well defined and allowed an assignment of the Raman lines at lower temperature. These selection rules disappeared for 6/40/60 but remained for 12/40/60 even at higher temperatures. The behavior of the two latter (rhombohedral-type compositions) was quite different. No assignment of lines could be done. In addition, the spectra recorded in parallel and crossed polarizations were almost identical for 5/65/35 regardless of temperature. A very smeared paraelectric to ferroelectric transition was evidenced by Raman intensity measurements for this composition. On the contrary, selection rules were always present for the relaxor composition 9/65/35 which were similar to those for 12/40/60 and 6/40/60. This suggests that both tetragonal and rhombohedral-type local polar order is present for 9/65/35. The spectra of the field induced ferroelectric phase for 9/65/35 revealed no selection rules, similar to 5/65/35. This is attributed to the onset of only medium range ferroelectric order. Finally, Raman spectra recorded on powders of every composition did not reveal any selection rules, suggesting that intergranular effects might play a significant role in the behavior of these materials. copyright 1997 American Institute of Physics

  8. Chemical characterisation of zircon-cadmium sulfoselenide ceramic pigments

    International Nuclear Information System (INIS)

    Gazulla Barreda, M. F.; Rodrigo Edo, M.; Blasco Roca, E.; Orduna Cordero, M.

    2013-01-01

    The present paper addresses the development of a methodology that allows the complete chemical characterisation of zircon cadmium sulfoselenide ceramic pigments including minor and major elements. To develop the methodology, five zircon-cadmium sulfoselenide pigments with different hues were selected, studying the different measurement process steps, from sample preparation to the optimisation of the measurement of the different components of the pigments by spectroscopic techniques (WD-XRF and elemental analysis by combustion and IR detection). The chemical characterisation method developed was validated with synthetic standards prepared from the mixture of certified reference materials and pure oxides because no certified referenced materials of this type of pigments were commercially available. The developed method can be used for a complete chemical characterization of zircon-cadmium sulfoselenide ceramic pigments with a very low uncertainty for all the elements analysed. (Author)

  9. Influence of crystal phases on electro-optic properties of epitaxially grown lanthanum-modified lead zirconate titanate films

    Science.gov (United States)

    Masuda, Shin; Seki, Atsushi; Masuda, Yoichiro

    2010-02-01

    We describe here how we have improved the crystal qualities and controlled the crystal phase of the lanthanum-modified lead zirconate titanate (PLZT) film without changing the composition ratio using an oxygen-pressure crystallization process. A PLZT film deposited on a SrTiO3 substrate with the largest electro-optic (EO) coefficient of 498 pm/V has been achieved by controlling the crystal phase of the film. Additionally, a fatigue-free lead zirconate titanate (PZT) capacitor with platinum electrodes has been realized by reducing the oxygen vacancies in the films.

  10. On the use of non-MPB lead zirconium titanate (PZT) granules for piezoelectric ceramic–polymer sensorial composites

    NARCIS (Netherlands)

    Shaji Karapuzha, A.; Kunnamkuzhakkal James, N.; van der Zwaag, S.; Groen, W.A.

    2016-01-01

    Modern flexible and sensitive sensors based on polymer–ceramic composites employ lead zirconate titanate (PZT) granulates having the morphotropic phase boundary (MPB) composition as the piezo active ingredient, as this composition gives the best properties in fully ceramic piezoelectric sensors.

  11. On the use of non-MPB lead zirconium titanate (PZT) granules for piezoelectric ceramic–polymer sensorial composites

    NARCIS (Netherlands)

    Shaji Karapuzha, A.; Zwaag, S. van der; Groen, W.A.

    2016-01-01

    Modern flexible and sensitive sensors based on polymer–ceramic composites employ lead zirconate titanate (PZT) granulates having the morphotropic phase boundary (MPB) composition as the piezo active ingredient, as this composition gives the best properties in fully ceramic piezoelectric sensors. In

  12. Understanding Microstructural Properties of Perovskite Ceramics through Their Wet-Chemical Synthesis

    NARCIS (Netherlands)

    Stawski, Tomasz

    2011-01-01

    This thesis comprises of seven full research chapters on the morphology, properties and processing of sol-gel precursor systems of barium titanate and lead zirconate titanate thin films and powders. In all the considered problems, the synthesis leading to nano-sized perovskite ceramics constitutes

  13. Potassium Sodium Niobate-Based Lead-Free Piezoelectric Multilayer Ceramics Co-Fired with Nickel Electrodes

    Directory of Open Access Journals (Sweden)

    Shinichiro Kawada

    2015-11-01

    Full Text Available Although lead-free piezoelectric ceramics have been extensively studied, many problems must still be overcome before they are suitable for practical use. One of the main problems is fabricating a multilayer structure, and one solution attracting growing interest is the use of lead-free multilayer piezoelectric ceramics. The paper reviews work that has been done by the authors on lead-free alkali niobate-based multilayer piezoelectric ceramics co-fired with nickel inner electrodes. Nickel inner electrodes have many advantages, such as high electromigration resistance, high interfacial strength with ceramics, and greater cost effectiveness than silver palladium inner electrodes. However, widely used lead zirconate titanate-based ceramics cannot be co-fired with nickel inner electrodes, and silver palladium inner electrodes are usually used for lead zirconate titanate-based piezoelectric ceramics. A possible alternative is lead-free ceramics co-fired with nickel inner electrodes. We have thus been developing lead-free alkali niobate-based multilayer ceramics co-fired with nickel inner electrodes. The normalized electric-field-induced thickness strain (Smax/Emax of a representative alkali niobate-based multilayer ceramic structure with nickel inner electrodes was 360 pm/V, where Smax denotes the maximum strain and Emax denotes the maximum electric field. This value is about half that for the lead zirconate titanate-based ceramics that are widely used. However, a comparable value can be obtained by stacking more ceramic layers with smaller thicknesses. In the paper, the compositional design and process used to co-fire lead-free ceramics with nickel inner electrodes are introduced, and their piezoelectric properties and reliabilities are shown. Recent advances are introduced, and future development is discussed.

  14. Preparation of lead titanate zirconate from metal citrates

    International Nuclear Information System (INIS)

    Bastos, C.M.R.

    1994-01-01

    Lead titanate zirconate (PZT) preparation from its metal constituent citrates have been investigated. Metal citrates were obtained by forced precipitation using a dehydration alcohol mixture. Salt solutions of lead nitrate and octahydrated zirconyl chloride, and titanium tetrachloride were treated separately with citric acid and ammonium hydroxide. Zirconium, titanium and lead oxides resulted from thermal decomposition of corresponding citrates at 500 0 C, 450 0 C and 250 0 C, respectively. Lead titanate (PT) and lead zirconate (P Z) were obtained by calcining at 450 0 C and 500 0 C, respectively, after adequate heating of citrates mechanically mixed in ethyl ether. PZT samples were obtained with different starting stoichiometry. Rhombohedral PZT-1 53/47 sample was prepared from co precipitating zirconyl ammonium and ammonium lead citrates in presence of ethanolic titanium oxide dispersion, and calcinating at 800 0 C. Rhombohedral PZT-q 52/48 sample was obtained from heating at 500 0 C for 2 hours a mixture of metal citrates coprecipitated by dehydration mixture of acetone-ethanol-formic acid (2:1:0,06). Tetragonal PZT-m stoichiometry 53/47 sample were obtained by calcining at after 600 0 C for 2 hours after heating a mechanically mixed metal citrates. PT phase arose at 400 0 C. PZT-m powders obtained in a range of 400 0 C-800 0 C were isostatically pressed, and sintered at 1100 0 C and 1200 0 C in saturated Pb O atmosphere. Rhombohedral sintered PZT was obtained with 7,78 g.cm -3 at 1200 0 C. (author). 123 refs, 53 figs, 32 tabs

  15. Phase transformations in lead zirconate-titanate doped with lanthanum

    Energy Technology Data Exchange (ETDEWEB)

    Ishchuk, V M; Morozov, E M

    1979-07-01

    Presented are the results of studies on the character of phase transitions of the lead-lanthanum zirconate-titanate (LLZT) system. The replacement of lead by lanthanum leads to the expansion of the region of antisegnetoelectric (ASE) states of solid solutions of lead zirconate-titanate (LZT) in the direction of PbTiO/sub 3/ concentration growth. An intermediate region is revealed between segnetoelectric (SE) and ASE states, material properties in which depend on their prehistory: annealed samples are in the ASE state, whereas the application of electric field exceeding some critical value induces the SE state. A family of phase diagrams obtained at consequent replacement of lead by lanthanum permits to identify phase states in any series of LLZT with a constant ratio of Zr:Ti, in the x/65/35 series in particular. Thermally depolarized state of materials of this series at x<6.5 is shown to be antisegnetoelectric at all the temperatures below the Curie point Tsub(c), and heating causes phase transition of ASE..-->..PE (paraelectric state) at Tsub(c). Polarized samples being heated, a successiveness of phase transitions of SE..-->..ASE takes place at T/sub 0/, and that of ASE reversible PE at Tsub(C) (Tsub(0)..ASE phase transition in the LZT system.

  16. Structure, dielectric and electrical properties of cerium doped barium zirconium titanate ceramics

    International Nuclear Information System (INIS)

    Feng Hongjun; Hou Jungang; Qu Yuanfang; Shan Dan; Yao Guohua

    2012-01-01

    Highlights: ► Rare-earth doped barium zirconate titanate (BZT) ceramics, Ba(Zr 0.25 Ti 0.75 )O 3 + xCeO 2 , (x = 0–1.5 at%) were obtained by a solid state reaction route. ► Morphological analysis on sintered samples by scanning electron microscopy shows that the addition of rare-earth ions affects the growth of the grain and remarkably changes the grain morphology. ► The effect of rare-earth addition to BZT on dielectric and electrical properties is analyzed, demonstrating that the samples with x = 0.4 and x = 0.6 could be semiconducting in air atmosphere. - Abstract: Rare-earth doped barium zirconium titanate (BZT) ceramics, Ba(Zr 0.25 Ti 0.75 )O 3 + xCeO 2 , (x = 0–1.5 at%) were obtained by a solid state reaction route. Perovskite-like single-phase compounds were confirmed from X-ray diffraction data and the lattice parameters were refined by the Rietveld method. It is found that, integrating with the lattice parameters and the distortion of crystal lattice, there is an alternation of substitution preference of cerium ions for the host cations in perovskite lattice. Morphological analysis on sintered samples by scanning electron microscopy shows that the addition of rare-earth ions affects the growth of the grain and remarkably changes the grain morphology. The effect of rare-earth addition to BZT on dielectric and electrical properties is analyzed. High values of dielectric tunability are obtained for cerium doped BZT. Especially, the experimental results on the effect of the contents of rare-earth addition on the resistivity of BZT ceramics were investigated, demonstrating that the samples with x = 0.4 and x = 0.6 could be semiconducting in air atmosphere.

  17. Microwave processing for ceramic materials in microsystem technology

    International Nuclear Information System (INIS)

    Rhee, S.

    2002-11-01

    In this study, the applicability of microwaves for sintering of monolithic ceramics and ceramic microcomponents was investigated. Experiments with 2.45 GHz and 30 GHz microwaves were conducted and contrasted to conventional thermal processing. The advantages and disadvantages of microwave processing were then assessed. Nanoscale zirconia and sub-micron lead-zirconate-titanate electroceramics were selected for the evaluation. (orig.)

  18. Lead zirconate titanate nanoscale patterning by ultraviolet-based lithography lift-off technique for nano-electromechanical system applications.

    Science.gov (United States)

    Guillon, Samuel; Saya, Daisuke; Mazenq, Laurent; Costecalde, Jean; Rèmiens, Denis; Soyer, Caroline; Nicu, Liviu

    2012-09-01

    The advantage of using lead zirconate titanate (PbZr(0.54)Ti(0.46)O(3)) ceramics as an active material in nanoelectromechanical systems (NEMS) comes from its relatively high piezoelectric coefficients. However, its integration within a technological process is limited by the difficulty of structuring this material with submicrometer resolution at the wafer scale. In this work, we develop a specific patterning method based on optical lithography coupled with a dual-layer resist process. The main objective is to obtain sub-micrometer features by lifting off a 100-nm-thick PZT layer while preserving the material's piezoelectric properties. A subsequent result of the developed method is the ability to stack several layers with a lateral resolution of few tens of nanometers, which is mandatory for the fabrication of NEMS with integrated actuation and read-out capabilities.

  19. Comparison of chemical solution deposition systems for the fabrication of lead zirconate titanate thin films

    International Nuclear Information System (INIS)

    Lecarpentier, F.; Daglish, M.; Kemmitt, T.

    2001-01-01

    Ferroelectric thin films of lead zirconate titanate Pb(Zr x Ti 1-x )O 3 (PZT) were prepared from five chemical solution deposition (CSD) systems, namely methoxyethanol, citrate, diol, acetic acid and triethanolamine. Physical characteristics of the solutions, processing parameters and physical and electrical properties of the films were used to assess the relative advantages and disadvantages of the different chemical systems. All the CSD systems decomposed to produce single phase perovskite PZT at temperatures above 650 deg C. Thin film deposition was influenced by the specific characteristics of each system such as wetting on the substrate and viscosity. Distinct precursor effects on the thin film crystallinity and electrical performance were revealed. The diol route yielded films with the highest crystallite size, highest permittivity and lowest loss tangent. The relative permittivity exhibited by films made by the other routes were 25% to 35% lower at equivalent thicknesses. Copyright (2001) The Australian Ceramic Society

  20. New phase transitions in lead zirconate-titanate

    International Nuclear Information System (INIS)

    Ishchuk, V.M.; Morozov, E.M.; Klimov, V.V.

    1977-01-01

    Processes of disordering are considered in the paraelectric phase of lead zirconate-titanate. Te investigations were carried out on poly- and single-crystal specimens of the composition PbZrsub(1-x)Tisub(x)O 3 (0< x(<=)0.5). The results are presented of measurements of the temperature dependence of the dielectric constant and the dependence of the polarization on the temperature and the electric field. Anomaly is observed of the investigated characteristics above the Curie point due to a first-type phase transition. The results are interpreted within the framework of the model proposed by Coms, Lambert, and Guiniot, according to which this transition is due to the disordering of chains of unit cells existing above the Curie point

  1. Cross-poling textures in a lead zirconate titanate piezoelectric material

    International Nuclear Information System (INIS)

    Wan, Shan; Bowman, Keith J.

    2000-01-01

    Tetragonal ferroelectric materials are polarized to induce the anisotropy necessary for the piezoelectric effect. This poling of the material is inherently an orientation process. Pole figure texture measurements of poling and cross-poling in a lead zirconate titanate Navy VI material show domain motion. The resulting axisymmetric and three-dimensional textures demonstrate the contribution of 90 degree sign domain motion to piezoelectricity. Cross-poling results in strong orientations with lower applied fields than in the initial poling steps. (c) 2000 Materials Research Society

  2. R-curve behaviour of ferroelectric ceramics

    International Nuclear Information System (INIS)

    Egorov, N.Ya.; Kramarov, S.O.

    2004-01-01

    The attempt's made to identify and evaluate the regularities of developing the fractures in the ferroelectric ceramics and also-study the effect of the polishing operation on the strength characteristics of the piezoceramics. The R-curve behaviour in the ferroelectric ceramics is studied on the samples of the barium titanate and lead zirconate-titanate by the four-point bending with controlled surface fractures. It is established that increasing curve of resistance to the fracture growth is observed in the piezoceramics under the conditions of the fracture stable growth. The results obtained on the polished samples prove that the mechanical processing introduces the compression surface stresses into the piezoceramic materials [ru

  3. Effect of bipolar electric fatigue on polarization switching in lead-zirconate-titanate ceramics

    Science.gov (United States)

    Zhukov, Sergey; Fedosov, Sergey; Glaum, Julia; Granzow, Torsten; Genenko, Yuri A.; von Seggern, Heinz

    2010-07-01

    From comparison of experimental results on polarization switching in fresh and electrically fatigued lead-zirconate-titanate (PZT) over a wide range of applied fields and switching times it is concluded that fatigue alters the local field distribution inside the sample due to the generation of discrete defects, such as voids and cracks. Such defects have a strong influence on the overall electric field distribution by their shape and dielectric permittivity. On this hypothesis, a new phenomenological model of polarization switching in fatigued PZT is proposed. The model assumes that the fatigued sample can be composed of different local regions which exhibit different field strengths but otherwise can be considered as unfatigued. Consequently the temporal response of a fatigued sample is assumed to be the superposition of the field-dependent temporal responses of unfatigued samples weighted by their respective volume fraction. A certain part of the volume is excluded from the overall switching process due to the domain pinning even at earlier stages of fatigue, which can be recovered by annealing. Suitability of the proposed model is demonstrated by a good correlation between experimental and calculated data for differently fatigued samples. Plausible cause of the formation of such regions is the generation of defects such as microcracks and the change in electrical properties at imperfections such as pores or voids.

  4. Bismuth Sodium Titanate Based Materials for Piezoelectric Actuators.

    Science.gov (United States)

    Reichmann, Klaus; Feteira, Antonio; Li, Ming

    2015-12-04

    The ban of lead in many electronic products and the expectation that, sooner or later, this ban will include the currently exempt piezoelectric ceramics based on Lead-Zirconate-Titanate has motivated many research groups to look for lead-free substitutes. After a short overview on different classes of lead-free piezoelectric ceramics with large strain, this review will focus on Bismuth-Sodium-Titanate and its solid solutions. These compounds exhibit extraordinarily high strain, due to a field induced phase transition, which makes them attractive for actuator applications. The structural features of these materials and the origin of the field-induced strain will be revised. Technologies for texturing, which increases the useable strain, will be introduced. Finally, the features that are relevant for the application of these materials in a multilayer design will be summarized.

  5. Piezoelectric Ceramics Characterization

    National Research Council Canada - National Science Library

    Jordan, T

    2001-01-01

    ... the behavior of a piezoelectric material. We have attempted to cover the most common measurement methods as well as introduce parameters of interest. Excellent sources for more in-depth coverage of specific topics can be found in the bibliography. In most cases, we refer to lead zirconate titanate (PZT) to illustrate some of the concepts since it is the most widely used and studied piezoelectric ceramic to date.

  6. Ferroelectric devices using lead zirconate titanate (PZT) nanoparticles.

    Science.gov (United States)

    Paik, Young Hun; Kojori, Hossein Shokri; Kim, Sung Jin

    2016-02-19

    We successfully demonstrate the synthesis of lead zirconate titanate nanoparticles (PZT NPs) and a ferroelectric device using the synthesized PZT NPs. The crystalline structure and the size of the nanocrystals are studied using x-ray diffraction and transmission electron microscopy, respectively. We observe PZT NPs and this result matches dynamic light scattering measurements. A solution-based low-temperature process is used to fabricate PZT NP-based devices on an indium tin oxide substrate. The fabricated ferroelectric devices are characterized using various optical and electrical measurements and we verify ferroelectric properties including ferroelectric hysteresis and the ferroelectric photovoltaic effect. Our approach enables low-temperature solution-based processes that could be used for various applications. To the best of our knowledge, this low-temperature solution processed ferroelectric device using PZT NPs is the first successful demonstration of its kind.

  7. In situ electrochemical etching and examination by SPM of titanate ceramics

    International Nuclear Information System (INIS)

    Thorogood, G.J.; Short, K.T; Zhang, Y.

    2002-01-01

    Full text: The aqueous durability of titanate related ceramics is of great importance for the immobilisation of high level radioactive waste-in order to observe the reaction progress at the solid-liquid interface of these durable ceramics, we have attempted to accelerate the dissolution process via electrochemical means by using a SPM cell with electrochemical capability. The experiment involves placing a titanate ceramic disk (with flat polished surfaces) in the electrochemical cell. The cell is then set up with the ceramic acting as one electrode and another electrode being placed in the solution. In a flow through cell it is possible to select the pH and observe the change, not only in surface morphology as dissolution occurs, but also the frictional characteristics of the surface. The SPM tip plays no role in the electrochemical reaction. We will be presenting results from our work and discussing possible mechanisms for dissolution and future directions of the work. Copyright (2002) Australian Society for Electron Microscopy Inc

  8. Electronic properties of lithium titanate ceramic

    International Nuclear Information System (INIS)

    Padilla-Campos, Luis; Buljan, Antonio

    2001-01-01

    Research on tritium breeder material is fundamental to the development of deuterium-tritium type fusion reactors for producing clean, non contaminating, electrical energy, since only energy and helium, a harmless gas, are produced from the fusion reaction. Lithium titanate ceramic is one of the possible candidates for the tritium breeder material. This last material is thought to form part of the first wall of the nucleus of the reactor which will provide the necessary tritium for the fusion and will also serve as a shield. Lithium titanate has advantageous characteristics compared to other materials. Some of these are low activation under the irradiation of neutrons, good thermal stability, high density of lithium atoms and relatively fast tritium release at low temperatures. However, there are still several physical and chemical properties with respect to the tritium release mechanism and mechanical properties that have not been studied at all. This work presents a theoretical study of the electronic properties of lithium titanate ceramic and the corresponding tritiated material. Band calculations using the Extended H kel Tight-Binding approach were carried out. Results show that after substituting lithium for tritium atoms, the electronic states for the latter appear in the middle of prohibited band gap which it is an indication that the tritiated material should behave as a semiconductor, contrary to Li 2 TiO 3 which is a dielectric isolator. A study was also carried out to determine the energetically most favorable sites for the substitution of lithium for tritium atoms. Additionally, we analyzed possible pathways for the diffusion of a tritium atom within the crystalline structure of the Li 2 TiO 3

  9. Patterning lead zirconate titanate nanostructures at sub-200-nm resolution by soft confocal imprint lithography and nanotransfer molding

    NARCIS (Netherlands)

    Khan, Sajid; Göbel, Ole; Blank, David H.A.; ten Elshof, Johan E.

    2009-01-01

    Patterned sol-gel-derived lead zirconate titanate (PZT) thin films with lateral resolutions down to 100 nm on silicon are reported. Both an imprint and a transfer-molding method were employed. The formed patterns after annealing were characterized with scanning electron microscopy, atomic force

  10. Fabrication of crystal-oriented barium-bismuth titanate ceramics in high magnetic field and subsequent reaction sintering

    International Nuclear Information System (INIS)

    Tanaka, Satoshi; Tomita, Yusuke; Furushima, Ryoichi; Uematsu, Keizo; Shimizu, Hiroyuki; Doshida, Yutaka

    2009-01-01

    High magnetic field was applied to fabricate novel lead-free piezoelectric ceramics with a textured structure. A compact of crystallographically oriented grains was prepared by dry forming in a high magnetic field from a mixed slurry of bismuth titanate and barium titanate powders. Bismuth titanate particles with a size of about 1 μ m were used as the host material. In the forming process, the slurry was poured into a mold and set in a magnetic field of 10 T until completely dried. Bismuth titanate particles were highly oriented in the slurry under the magnetic field. The dried powder compact consisted of highly oriented bismuth titanate particles and randomly oriented barium titanate particles. Barium bismuth titanate ceramics with a- and b-axis orientations were successfully produced from the dried compact by sintering at temperatures above 1100 deg. C.

  11. Experimental studies on 3D printing of barium titanate ceramics for medical applications

    Directory of Open Access Journals (Sweden)

    Schult Mark

    2016-09-01

    Full Text Available The present work deals with the 3D printing of porous barium titanate ceramics. Barium titanate is a biocompatible material with piezoelectric properties. Due to insufficient flowability of the starting material for 3D printing, the barium titanate raw material has been modified in three different ways. Firstly, barium titanate powder has been calcined. Secondly, flow additives have been added to the powder. And thirdly, flow additives have been added to the calcined powder. Finally, a polymer has been added to the three materials and specimens have been printed from these three material mixtures. The 3D printed parts were then sintered at 1320°C. The sintering leads to shrinkage which differs between 29.51–71.53% for the tested material mixtures. The porosity of the parts is beneficial for cell growth which is relevant for future medical applications. The results reported in this study demonstrate the possibility to fabricate porous piezoelectric barium titanate parts with a 3D printer that can be used for medical applications. 3D printed porous barium titanate ceramics can especially be used as scaffold for bone tissue engineering, where the bone formation can be promoted by electrical stimulation.

  12. Compact piezoelectric micromotor with a single bulk lead zirconate titanate stator

    Science.gov (United States)

    Yan, Liang; Lan, Hua; Jiao, Zongxia; Chen, Chin-Yin; Chen, I.-Ming

    2013-04-01

    The advance of micro/nanotechnology promotes the development of micromotors in recent years. In this article, a compact piezoelectric ultrasonic micromotor with a single bulk lead zirconate titanate stator is proposed. A traveling wave is generated by superposition of bending modes with 90° phase difference excited by d15 inverse piezoelectric effects. The operating principle simplifies the system structure significantly, and provides a miniaturization solution. A research prototype with the size of 0.75× 0.75×1.55 mm is developed. It can produce start-up torque of 0.27μNmand maximum speed of 2760 r/min at 14RMS.

  13. The Effect of Acceptor and Donor Doping on Oxygen Vacancy Concentrations in Lead Zirconate Titanate (PZT).

    Science.gov (United States)

    Slouka, Christoph; Kainz, Theresa; Navickas, Edvinas; Walch, Gregor; Hutter, Herbert; Reichmann, Klaus; Fleig, Jürgen

    2016-11-22

    The different properties of acceptor-doped (hard) and donor-doped (soft) lead zirconate titanate (PZT) ceramics are often attributed to different amounts of oxygen vacancies introduced by the dopant. Acceptor doping is believed to cause high oxygen vacancy concentrations, while donors are expected to strongly suppress their amount. In this study, La 3+ donor-doped, Fe 3+ acceptor-doped and La 3+ /Fe 3+ -co-doped PZT samples were investigated by oxygen tracer exchange and electrochemical impedance spectroscopy in order to analyse the effect of doping on oxygen vacancy concentrations. Relative changes in the tracer diffusion coefficients for different doping and quantitative relations between defect concentrations allowed estimates of oxygen vacancy concentrations. Donor doping does not completely suppress the formation of oxygen vacancies; rather, it concentrates them in the grain boundary region. Acceptor doping enhances the amount of oxygen vacancies but estimates suggest that bulk concentrations are still in the ppm range, even for 1% acceptor doping. Trapped holes might thus considerably contribute to the charge balancing of the acceptor dopants. This could also be of relevance in understanding the properties of hard and soft PZT.

  14. The Effect of Acceptor and Donor Doping on Oxygen Vacancy Concentrations in Lead Zirconate Titanate (PZT

    Directory of Open Access Journals (Sweden)

    Christoph Slouka

    2016-11-01

    Full Text Available The different properties of acceptor-doped (hard and donor-doped (soft lead zirconate titanate (PZT ceramics are often attributed to different amounts of oxygen vacancies introduced by the dopant. Acceptor doping is believed to cause high oxygen vacancy concentrations, while donors are expected to strongly suppress their amount. In this study, La3+ donor-doped, Fe3+ acceptor-doped and La3+/Fe3+-co-doped PZT samples were investigated by oxygen tracer exchange and electrochemical impedance spectroscopy in order to analyse the effect of doping on oxygen vacancy concentrations. Relative changes in the tracer diffusion coefficients for different doping and quantitative relations between defect concentrations allowed estimates of oxygen vacancy concentrations. Donor doping does not completely suppress the formation of oxygen vacancies; rather, it concentrates them in the grain boundary region. Acceptor doping enhances the amount of oxygen vacancies but estimates suggest that bulk concentrations are still in the ppm range, even for 1% acceptor doping. Trapped holes might thus considerably contribute to the charge balancing of the acceptor dopants. This could also be of relevance in understanding the properties of hard and soft PZT.

  15. Dielectric and electrical properties of gadolinium-modified lead-zirconate-titanate system

    International Nuclear Information System (INIS)

    Panigrahi, S.C.; Das, Piyush R.; Parida, B.N.; Padhee, R.; Choudhary, R.N.P.

    2014-01-01

    Highlights: • Gadolinium modified PZT have very good dielectric and ferroelectric properties. • The impedance analysis of shows grain and grain boundary phenomena. • Electrical properties of the compounds show very good transport properties. • Piezoelectric coefficient of the samples have higher values. - Abstract: The gadolinium (Gd) modified lead zirconate titanate (PbZr,TiO 3 ) ceramics with Zr/Ti = 48/52 (i.e., near morphotropic phase boundary (MPB)) in a general chemical formula Pb 1−x Gd x (Zr 0.48 Ti 0.52 ) 1−x/4 O 3 (PGZT; x = 0, 0.07, 0.10 and 0.12) have been synthesized using a high-temperature solid-state reaction method. Preliminary structural analysis using X-ray powder diffraction (XRD) shows the formation of a single-phase tetragonal structure of the compounds. Detailed studies of dielectric parameters of PGZT exhibit the diffuse phase transition but non-relaxor characteristics in the material for the higher concentration of gadolinium. The ac conductivity spectra of PGZT are found to obey Jonscher’s universal power law. The electrical impedance parameters of PGZT (near MPB) were obtained in a wide range of temperature (25–500 °C) and frequency (1–1000 kHz) using complex impedance spectroscopy (CIS) technique. Detailed analysis of these parameters shows that bulk (grain) and grain boundary resistance have significant effect on the total impedance of the materials. Temperature dependence of hysteresis characteristics of PGZT confirms that the phase transition parameter of the material is strongly affected by the substitution of Gd at the Pb-sites

  16. Materials and ceramics on the base of aluminium titanate

    International Nuclear Information System (INIS)

    Gulamova, D.

    1997-01-01

    The influence of the doping and technological parameters on the thermodynamical stability of the aluminium titanate is investigated. The condition necessary to make aluminium titanate stable and established. it is shown, how the condition of the synthesis and the content of the admixture phases affect the stability of the solid solutions. The technology of obtaining the ceramics stable with respect to decay (with thermal expansion coefficient CTE = 26x10/sup -6/ grad/sup -1/ and thermoresistancy > 80 heating cycles, sigma curve equal or greater than 80 Mpa) is worked out. (author)

  17. Fatigue-free lead zirconate titanate-based capacitors for nonvolatile memories

    International Nuclear Information System (INIS)

    Shannigrahi, S. R.; Jang, Hyun M.

    2001-01-01

    The development of lead zirconate titanate (PZT)-based capacitors has been a long time goal of ferroelectric random access memories (FRAM). However, PZT-based perovskites with common platinum (Pt) electrodes have suffered from a significant reduction of the remanent polarization (P r ) after a certain number of read/write cycles (electrical fatigue). We now report the development of fatigue-free lanthanum-modified PZT capacitors using common Pt electrodes. The capacitors fabricated at 580 o C by applying a PZT seed layer exhibited fatigue-free behavior up to 6.5 x 10 10 switching cycles, a quite stable charge retention profile with time, and comparatively high P r values, all of which assure their suitability for practical FRAM applications. Copyright 2001 American Institute of Physics

  18. Effect of compositional variations in the lead lanthanum zirconate stannate titanate system on electrical properties

    International Nuclear Information System (INIS)

    Markowski, K.; Park, S.E.; Yoshikawa, Shoko; Cross, L.E.

    1996-01-01

    The purpose of this work was to evaluate the effect of compositional modifications on the electrical properties of lead lanthanum zirconate stannate titanate (PLZST) ceramics, as well as to examine their electrically induced phase-change behavior. Variations in the Ti:Sn ratio were evaluated. Increased Ti 4+ content produced the following: decreased switching field, related to an increased antiferroelectric-ferroelectric (AFE-FE) transition temperature; constant hysteresis (ΔE) correlated with a constant temperature of the maximum dielectric constant (T max ); a sharper dielectric-constant maximum peak; and increased room-temperature dielectric constant (K). Variations in the Zr:Sn ratio also were evaluated. Increased Zr 4+ content produced the following: increased hysteresis with increased T max , decreased maximum dielectric constant, and decreased switching field with increased AFE-FE transition temperature (T AFE-FE ). From these results, with respect to compositional modifications, the AFE-FE switching field (E AFE-FE ) and ΔE were observed to be dependent strongly on T AFE-FE and T max , respectively. Negligible change existed in the strain achievable at the switching field, which remained constant for all compositions at ∼0.16%. The significance of this research was the ability demonstrated to tailor the properties of phase-change materials through compositional modifications

  19. Corrosion behavior of pyroclore-rich titanate ceramics for plutonium disposition; impurity effects

    International Nuclear Information System (INIS)

    Bakel, A. J.

    1999-01-01

    The baseline ceramic contains Ti, U, Ca, Hf, Gd, and Ce, and is made up of only four phases, pyrochlore, zirconolite, rutile, and brannerite. The impurities present in the three other ceramics represent impurities expected in the feed, and result in different phase distributions. The results from 3 day, 90 C MCC-1 tests with impurity ceramics were significantly different than the results from tests with the baseline ceramic. Overall, the addition of impurities to these titanate ceramics alters the phase distributions, which in turn, affects the corrosion behavior

  20. Assessment of full ceramic solid oxide fuel cells based on modified strontium titanates

    DEFF Research Database (Denmark)

    Holtappels, Peter; Ramos, Tania; Sudireddy, Bhaskar Reddy

    2014-01-01

    stimulated the development for full ceramic anodes based on strontium titanates. Furthermore, the Ni-cermet is primarily a hydrogen oxidation electrode and efficiency losses might occur when operating on carbon containing fuels. In the European project SCOTAS-SOFC full ceramic cells comprising CGO...

  1. Effect of zircon-based tricolor pigments on the color, microstructure, flexural strength and translucency of a novel dental lithium disilicate glass-ceramic.

    Science.gov (United States)

    Yuan, Kun; Wang, Fu; Gao, Jing; Sun, Xiang; Deng, Zai-Xi; Wang, Hui; Jin, Lei; Chen, Ji-Hua

    2014-01-01

    The purpose of this study was to investigate the effect of zircon-based tricolor pigments (praseodymium zircon yellow, ferrum zircon red, and vanadium zircon blue) on the color, thermal property, crystalline phase composition, microstructure, flexural strength, and translucency of a novel dental lithium disilicate glass-ceramic. The pigments were added to the glass frit, milled, pressed, and sintered. Ninety monochrome samples were prepared and the colors were analyzed. The effect of the pigments on thermal property, crystalline phase composition, and microstructure were determined by differential scanning calorimetry (DSC), X-ray diffraction (XRD), and scanning electron microscopy (SEM), respectively. Addition of the pigments resulted in the acquisition of subtractive primary colors as well as tooth-like colors, and did not demonstrate significant effects on the thermal property, crystalline phase composition, microstructure, and flexural strength of the experimental glass-ceramic. Although significant differences (p ceramics, the translucencies of the latter were sufficient to fabricate dental restorations. These results indicate that the zircon-based tricolor pigments can be used with dental lithium disilicate glass-ceramic to produce abundant and predictable tooth-like colors without significant adverse effects, if mixed in the right proportions. Copyright © 2013 Wiley Periodicals, Inc.

  2. Using the methods of radiospectroscopy (EPR, NMR) to study the nature of the defect structure of solid solutions based on lead zirconate titanate (PZT).

    Science.gov (United States)

    Bykov, Igor; Zagorodniy, Yuriy; Yurchenko, Lesya; Korduban, Alexander; Nejezchleb, Karel; Trachevsky, Vladimir; Dimza, Vilnis; Jastrabik, Lubomir; Dejneka, Alexander

    2014-08-01

    The nature of intrinsic and impurity point defects in lead zirconate titanate (PZT) ceramics has been explored. Using electron paramagnetic resonance (EPR), nuclear magnetic resonance (NMR), and X-ray photoelectron spectroscopy (XPS) methods, several impurity sites have been identified in the materials, including the Fe(3+)-oxygen vacancy (VO) complex and Pb ions. Both of these centers are incorporated into the PZT lattice. The Fe(3+) –VО paramagnetic complex serves as a sensitive probe of the local crystal field in the ceramic; the symmetry of this defect roughly correlates with PZT phase diagram as the composition is varied from PbTiO3 to PbZrO3. NMR spectra (207)Pb in PbTiO3, PbZrO3, and PZT with iron content from 0 to 0.4 wt% showed that increasing the iron concentration leads to a distortion of the crystal structure and to improvement of the electrophysical parameters of the piezoceramics. This is due to the formation of a phase which has a higher symmetry, but at high concentrations of iron (>0.4 wt%), it leads to sharp degradation of electrophysical parameters.

  3. Ceramic piezoelectric materials

    International Nuclear Information System (INIS)

    Kaszuwara, W.

    2004-01-01

    Ceramic piezoelectric materials conert reversibility electric energy into mechanical energy. In the presence of electric field piezoelectric materials exhibit deformations up to 0.15% (for single crystals up to 1.7%). The deformation energy is in the range of 10 2 - 10 3 J/m 3 and working frequency can reach 10 5 Hz. Ceramic piezoelectric materials find applications in many modern disciplines such as: automatics, micromanipulation, measuring techniques, medical diagnostics and many others. Among the variety of ceramic piezoelectric materials the most important appear to be ferroelectric materials such as lead zirconate titanate so called PZT ceramics. Ceramic piezoelectric materials can be processed by methods widely applied for standard ceramics, i.e. starting from simple precursors e.g. oxides. Application of sol-gel method has also been reported. Substantial drawback for many applications of piezoelectric ceramics is their brittleness, thus much effort is currently being put in the development of piezoelectric composite materials. Other important research directions in the field of ceramic piezoelectric materials composite development of lead free materials, which can exhibit properties similar to the PZT ceramics. Among other directions one has to state processing of single crystals and materials having texture or gradient structure. (author)

  4. High Discharge Energy Density at Low Electric Field Using an Aligned Titanium Dioxide/Lead Zirconate Titanate Nanowire Array.

    Science.gov (United States)

    Zhang, Dou; Liu, Weiwei; Guo, Ru; Zhou, Kechao; Luo, Hang

    2018-02-01

    Polymer-based capacitors with high energy density have attracted significant attention in recent years due to their wide range of potential applications in electronic devices. However, the obtained high energy density is predominantly dependent on high applied electric field, e.g., 400-600 kV mm -1 , which may bring more challenges relating to the failure probability. Here, a simple two-step method for synthesizing titanium dioxide/lead zirconate titanate nanowire arrays is exploited and a demonstration of their ability to achieve high discharge energy density capacitors for low operating voltage applications is provided. A high discharge energy density of 6.9 J cm -3 is achieved at low electric fields, i.e., 143 kV mm -1 , which is attributed to the high relative permittivity of 218.9 at 1 kHz and high polarization of 23.35 µC cm -2 at this electric field. The discharge energy density obtained in this work is the highest known for a ceramic/polymer nanocomposite at such a low electric field. The novel nanowire arrays used in this work are applicable to a wide range of fields, such as energy harvesting, energy storage, and photocatalysis.

  5. Thickness dependence of the poling and current-voltage characteristics of paint films made up of lead zirconate titanate ceramic powder and epoxy resin

    Science.gov (United States)

    Egusa, Shigenori; Iwasawa, Naozumi

    1995-11-01

    A specially prepared paint made up of lead zirconate titanate (PZT) ceramic powder and epoxy resin was coated on an aluminum plate and was cured at room temperature, thus forming the paint film of 25-300 μm thickness with a PZT volume fraction of 53%. The paint film was then poled at room temperature, and the poling behavior was determined by measuring the piezoelectric activity as a function of poling field. The poling behavior shows that the piezoelectric activity obtained at a given poling field increases with an increase in the film thickness from 25 to 300 μm. The current-voltage characteristic of the paint film, on the other hand, shows that the increase in the film thickness leads not only to an increase in the magnitude of the current density at a given electric field but also to an increase in the critical electric field at which the transition from the ohmic to space-charge-limited conduction takes place. This fact indicates that the amount of the space charge of electrons injected into the paint film decreases as the film thickness increases. Furthermore, comparison of the current-voltage characteristic of the paint film with that of a pure epoxy film reveals that the space charge is accumulated largely at the interface between the PZT and epoxy phases in the paint film. On the basis of this finding, a model is developed for the poling behavior of the paint film by taking into account a possible effect of the space-charge accumulation and a broad distribution of the electric field in the PZT phase. This model is shown to give an excellent fit to the experimental data of the piezoelectric activity obtained here as a function of poling field and film thickness.

  6. Electromechanical properties of textured K0.5Na0.5NbO3 ceramics

    OpenAIRE

    Pinho, Rui Manuel de Oliveira

    2014-01-01

    This work is about lead-free ceramic materials intended for electromechanical applications and candidates to replace lead-based electroceramics. One of the most widely used piezoelectric ceramics is lead zirconate titanate (PZT). However, it contains more than 60% of lead and it is toxic for humans and environment. In 2003, a directive from European Union has prohibited the use of potentially hazardous elements as lead. Due to the lack of competitive materials for PZT replacement an exception...

  7. Positively charged microporous ceramic membrane for the removal of Titan Yellow through electrostatic adsorption.

    Science.gov (United States)

    Cheng, Xiuting; Li, Na; Zhu, Mengfu; Zhang, Lili; Deng, Yu; Deng, Cheng

    2016-06-01

    To develop a depth filter based on the electrostatic adsorption principle, positively charged microporous ceramic membrane was prepared from a diatomaceous earth ceramic membrane. The internal surface of the highly porous ceramic membrane was coated with uniformly distributed electropositive nano-Y2O3 coating. The dye removal performance was evaluated through pressurized filtration tests using Titan Yellow aqueous solution. It showed that positively charged microporous ceramic membrane exhibited a flow rate of 421L/(m(2)·hr) under the trans-membrane pressure of 0.03bar. Moreover it could effectively remove Titan Yellow with feed concentration of 10mg/L between pH3 to 8. The removal rate increased with the enhancement of the surface charge properties with a maximum rejection of 99.6%. This study provides a new and feasible method of removing organic dyes in wastewater. It is convinced that there will be a broad market for the application of charged ceramic membrane in the field of dye removal or recovery from industry wastewater. Copyright © 2016. Published by Elsevier B.V.

  8. Acoustic response of piezoelectric lead-zirconate-titanate to a 400MeV/n xenon beam

    CERN Document Server

    Miyachi, T; Ito, H

    2003-01-01

    Characteristics of lead-zirconate-titanate (PZT) elements were studied by directly irradiating them with a 400 MeV/n Xe beam. The elements were sensitive to 10 sup 4 Xe ions and their output amplitudes were proportional to the beam intensity. An ensemble of those output amplitudes displayed a Bragg-curve-like response towards the range of 400 MeV/n Xe ion. We discuss the potential of PZT elements as a radiation detector and their application to high-intensity and high-energy detectors. (author)

  9. Characterization of lead zirconate titanate (PZT)--indium tin oxide (ITO) thin film interface

    International Nuclear Information System (INIS)

    Sreenivas, K.; Sayer, M.; Laursen, T.; Whitton, J.L.; Pascual, R.; Johnson, D.J.; Amm, D.T.

    1990-01-01

    In this paper the interface between ultrathin sputtered lead zirconate titanate (PZT) films and a conductive electrode (indium tin oxide-ITO) is investigated. Structural and compositional changes at the PZT-ITO interface have been examined by surface analysis and depth profiling techniques of glancing angle x-ray diffraction, Rutherford backscattering (RBS), SIMS, Auger electron spectroscopy (AES), and elastic recoil detection analysis (ERDA). Studies indicate significant interdiffusion of lead into the underlying ITP layer and glass substrate with a large amount of residual stress at the interface. Influence of such compositional deviations at the interface is correlated to an observed thickness dependence in the dielectric properties of PZT films

  10. Pressure, temperature, and electric field dependence of phase transformations in niobium modified 95/5 lead zirconate titanate

    Energy Technology Data Exchange (ETDEWEB)

    Dong, Wen D.; Carlos Valadez, J.; Gallagher, John A.; Jo, Hwan R.; Lynch, Christopher S., E-mail: cslynch@seas.ucla.edu [Department of Mechanical and Aerospace Engineering, The University of California, Los Angeles, 420 Westwood Plaza, Los Angeles, California 90095 (United States); Sahul, Raffi; Hackenberger, Wes [TRS Technologies, 2820 East College Avenue, State College, Pennsylvania 16801 (United States)

    2015-06-28

    Ceramic niobium modified 95/5 lead zirconate-lead titanate (PZT) undergoes a pressure induced ferroelectric to antiferroelectric phase transformation accompanied by an elimination of polarization and a volume reduction. Electric field and temperature drive the reverse transformation from the antiferroelectric to ferroelectric phase. The phase transformation was monitored under pressure, temperature, and electric field loading. Pressures and temperatures were varied in discrete steps from 0 MPa to 500 MPa and 25 °C to 125 °C, respectively. Cyclic bipolar electric fields were applied with peak amplitudes of up to 6 MV m{sup −1} at each pressure and temperature combination. The resulting electric displacement–electric field hysteresis loops were open “D” shaped at low pressure, characteristic of soft ferroelectric PZT. Just below the phase transformation pressure, the hysteresis loops took on an “S” shape, which split into a double hysteresis loop just above the phase transformation pressure. Far above the phase transformation pressure, when the applied electric field is insufficient to drive an antiferroelectric to ferroelectric phase transformation, the hysteresis loops collapse to linear dielectric behavior. Phase stability maps were generated from the experimental data at each of the temperature steps and used to form a three dimensional pressure–temperature–electric field phase diagram.

  11. Ferroelectric relaxor behaviour and impedance spectroscopy of Bi2O3-doped barium zirconium titanate ceramics

    Science.gov (United States)

    Mahajan, Sandeep; Thakur, O P; Bhattacharya, D K; Sreenivas, K

    2009-03-01

    Bi2O3-doped barium zirconate titanate ceramics, Ba1-xBix(Zr0.05Ti0.95)O3, have been prepared by the conventional solid-state reaction method. The ferroelectric relaxor behaviour and dielectric properties have been investigated in detail. By XRD analysis, it is suggested that up to x = 0.04, Bi3+ substitutes A-site ion, and thereafter with higher Bi3+ content, it enters the B-site sub lattice. Substitution of Bi3+ ions induces ferroelectric relaxor behaviour and the degree of relaxation behaviour increases with bismuth concentration. The remanent polarization and strain behaviour show a slight increase with the substitution level. The degree of hysteresis (strain versus electric field) also reduces from 21.4% to 4.6% with bismuth substitution. Impedance measurements were made on the prepared sample over a wide range of temperatures (300-723 K) and frequencies (40 Hz-1 MHz), which show the presence of both bulk and grain boundary effects in the material. The bulk and grain boundary conductivities determined from impedance study indicate the Arrhenius-type thermally activated process. Impedance spectroscopy is shown to be an efficient method capable of detecting the contributions of the resistances of grains and grain boundaries to the complex impedance of a ceramic system, accurately estimating its electrical conductivity as well as its corresponding activation energies and drawing conclusions on its structural properties.

  12. Ferroelectric relaxor behaviour and impedance spectroscopy of Bi2O3-doped barium zirconium titanate ceramics

    International Nuclear Information System (INIS)

    Mahajan, Sandeep; Thakur, O P; Bhattacharya, D K; Sreenivas, K

    2009-01-01

    Bi 2 O 3 -doped barium zirconate titanate ceramics, Ba 1-x Bi x (Zr 0.05 Ti 0.95 )O 3 , have been prepared by the conventional solid-state reaction method. The ferroelectric relaxor behaviour and dielectric properties have been investigated in detail. By XRD analysis, it is suggested that up to x = 0.04, Bi 3+ substitutes A-site ion, and thereafter with higher Bi 3+ content, it enters the B-site sub lattice. Substitution of Bi 3+ ions induces ferroelectric relaxor behaviour and the degree of relaxation behaviour increases with bismuth concentration. The remanent polarization and strain behaviour show a slight increase with the substitution level. The degree of hysteresis (strain versus electric field) also reduces from 21.4% to 4.6% with bismuth substitution. Impedance measurements were made on the prepared sample over a wide range of temperatures (300-723 K) and frequencies (40 Hz-1 MHz), which show the presence of both bulk and grain boundary effects in the material. The bulk and grain boundary conductivities determined from impedance study indicate the Arrhenius-type thermally activated process. Impedance spectroscopy is shown to be an efficient method capable of detecting the contributions of the resistances of grains and grain boundaries to the complex impedance of a ceramic system, accurately estimating its electrical conductivity as well as its corresponding activation energies and drawing conclusions on its structural properties.

  13. Incorporation of transuranic elements in titanate nuclear waste ceramics

    International Nuclear Information System (INIS)

    Matzke, H.J.; Ray, I.L.F.; Theile, H.; Trisoglio, C.; Walker, C.T.; White, T.J.

    1990-01-01

    The incorporation of actinide elements and their rare-earth element analogues in titanate nuclear waste forms in reviewed. New partitioning data are presented for three waste forms containing Purex waste simulant in combination with either NpO 2 , PuO 2 , or Am 2 O 3 . The greater proportion of transuranics partition between perovskite and zirconolite, while some americium may enter loveringite. Autoradiography revealed clusters of plutonium atoms which have been interpreted as unreacted dioxide or sesquioxide. It is concluded that the solid-state behavior of transuranic elements in titanate waste forms is poorly understood, certainly not well enough to tailor a ceramic for the incorporation of waste from reprocessing of fast breeder reactor fuel in which transuranic species are more abundant than in Purex waste

  14. Surface bond contraction and its effect on the nanometric sized lead zirconate titanate

    International Nuclear Information System (INIS)

    Haitao Huang; Sun, Chang Q.; Hing, Peter

    2000-01-01

    The grain size effect of lead zirconate titanate PbZr 1-x Ti x O 3 (PZT, x≥0.6) caused by surface bond contraction has been investigated by using the Landau-Ginsburg-Devonshire (LGD) phenomenological theory. It has been shown that, due to the surface bond contraction, both the Curie temperature and the spontaneous polarization of tetragonal PZT decrease with decreasing grain size. These effects become more significant when the grain size is in the nanometre range. A dielectric anomaly appears with decreasing grain size, which corresponds to a size dependent phase transformation. The ferroelectric critical size below which a loss of ferroelectricity will happen is estimated from the results obtained. (author). Letter-to-the-editor

  15. Investigation of the effect of temperature on aging behavior of Fe-doped lead zirconate titanate

    Science.gov (United States)

    Promsawat, Napatporn; Promsawat, Methee; Janphuang, Pattanaphong; Marungsri, Boonruang; Luo, Zhenhua; Pojprapai, Soodkhet

    The aging degradation behavior of Fe-doped Lead zirconate titanate (PZT) subjected to different heat-treated temperatures was investigated over 1000h. The aging degradation in the piezoelectric properties of PZT was indicated by the decrease in piezoelectric charge coefficient, electric field-induced strain and remanent polarization. It was found that the aging degradation became more pronounced at temperature above 50% of the PZT’s Curie temperature. A mathematical model based on the linear logarithmic stretched exponential function was applied to explain the aging behavior. A qualitative aging model based on polar macrodomain switchability was proposed.

  16. Chemical characterisation of zircon-cadmium sulfoselenide ceramic pigments; Caracterizacion quimica de pigmentos ceramicos a base de sulfoseleniuro de cadmio

    Energy Technology Data Exchange (ETDEWEB)

    Gazulla Barreda, M. F.; Rodrigo Edo, M.; Blasco Roca, E.; Orduna Cordero, M.

    2013-07-01

    The present paper addresses the development of a methodology that allows the complete chemical characterisation of zircon cadmium sulfoselenide ceramic pigments including minor and major elements. To develop the methodology, five zircon-cadmium sulfoselenide pigments with different hues were selected, studying the different measurement process steps, from sample preparation to the optimisation of the measurement of the different components of the pigments by spectroscopic techniques (WD-XRF and elemental analysis by combustion and IR detection). The chemical characterisation method developed was validated with synthetic standards prepared from the mixture of certified reference materials and pure oxides because no certified referenced materials of this type of pigments were commercially available. The developed method can be used for a complete chemical characterization of zircon-cadmium sulfoselenide ceramic pigments with a very low uncertainty for all the elements analysed. (Author)

  17. EXAFS and XANES analysis of plutonium and cerium edges from titanate ceramics for fissile materials disposal

    International Nuclear Information System (INIS)

    Fortner, J. A.; Kropf, A. J.; Bakel, A. J.; Hash, M. C.; Aase, S. B.; Buck, E. C.; Chamerlain, D. B.

    1999-01-01

    We report x-ray absorption near edge structure (XANES) and extended x-ray absorption fine structure (EXAFS) spectra from the plutonium L III edge and XANES from the cerium L II edge in prototype titanate ceramic hosts. The titanate ceramics studied are based upon the hafnium-pyrochlore and zirconolite mineral structures and will serve as an immobilization host for surplus fissile materials, containing as much as 10 weight % fissile plutonium and 20 weight % (natural or depleted) uranium. Three ceramic formulations were studied: one employed cerium as a ''surrogate'' element, replacing both plutonium and uranium in the ceramic matrix, another formulation contained plutonium in a ''baseline'' ceramic formulation, and a third contained plutonium in a formulation representing a high-impurity plutonium stream. The cerium XANES from the surrogate ceramic clearly indicates a mixed III-IV oxidation state for the cerium. In contrast, XANES analysis of the two plutonium-bearing ceramics shows that the plutonium is present almost entirely as Pu(IV) and occupies the calcium site in the zirconolite and pyrochlore phases. The plutonium EXAFS real-space structure shows a strong second-shell peak, clearly distinct from that of PuO 2 , with remarkably little difference in the plutonium crystal chemistry indicated between the baseline and high-impurity formulations

  18. Synthesis and characterization of nickel oxide doped barium strontium titanate ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Banerjee, M. [Dept. of Electrical Engineering, Bengal Institute of Technology Kolkata (India); Mukherjee, S. [Dept. of Metallurgical Engineering, Jadavpur University, Kolkata (India); Maitra, S. [Govt. College of Engg. and Ceramic Technology, Kolkata (India)

    2012-01-15

    Barium strontium titanate (BST) ceramics (Ba{sub 0.6}Sr{sub 0.4})TiO{sub 3} were synthesized by solid state sintering using barium carbonate, strontium carbonate and rutile as the precursor materials. The samples were doped with nickel oxide in different proportions. Different phases present in the sintered samples were determined from X-ray diffraction investigation and the distribution of different phases in the microstructure was assessed from scanning electron microscopy study. It was observed that the dielectric properties of BST were modified significantly with nickel oxide doping. These ceramics held promise for applications in tuned circuits. (author)

  19. Characterisation of glass matrix composites reinforced with lead zirconate titanate particles

    International Nuclear Information System (INIS)

    Cannillo, Valeria; Manfredini, Tiziano; Montorsi, Monia; Tavoni, Francesca; Minay, Emma J.; Boccaccini, Aldo R.

    2005-01-01

    A new type of glass matrix composite reinforced with ferroelectric particulate secondary phase was investigated. Samples containing lead zirconate titanate (PZT) particles in a silicate lead glass were fabricated. Various sintering strategies were tested in order to optimise the processing route. The densest samples were obtained by hot-pressing. The composites were characterized by means of SEM observations, X-ray diffraction, differential thermal analysis and Vickers indentations. In order to get a deeper insight into the thermo-mechanical behaviour of the material, a FEM based numerical model was prepared and applied. In particular, the crack-particle interaction was assessed and thus possible toughening mechanisms were investigated. By means of the numerical modelling supported by SEM observations, traditional toughening mechanisms (e.g. crack deflection, particle debonding) were ruled out. Since the experimentally measured indentation fracture toughness of the composite is significantly higher than that of the unreinforced glass, the findings suggest that a new toughening mechanism may be active, based on the piezoelectric effect

  20. Microstructure and dielectric properties of La2O3 doped Ti-rich barium strontium titanate ceramics for capacitor applications

    Directory of Open Access Journals (Sweden)

    Zhang Chen

    2018-03-01

    Full Text Available Microstructure and dielectric properties of La2O3 doped Ti-rich barium strontium titanate ceramics, prepared by solid state method, were investigated with non-stoichiometric level and various La2O3 content, using XRD, SEM and LCR measuring system. With an increase of non-stoichiometric level, the unit cell volumes of perovskite lattices for the single phase Ti-rich barium strontium titanate ceramics increased due to the decreasing A site vacancy concentration V″A. The unit cell volume increased and then decreased slightly with the increasing La2O3 content. Relatively high non-stoichiometric level and high La2O3 content in Ti-rich barium strontium titanate ceramics contributed to the decreased average grain size as well as fine grain size distribution, which correspondingly improved the temperature stability of the relative dielectric constant. The relative dielectric constant єrRT, dielectric loss tanδRT and the maximum relative dielectric constant єrmax decreased and then increased with the increasing non-stoichiometric level. With the increase of La2O3 doping content, the relative dielectric constant єrRT increased initially and then decreased. The maximum relative dielectric constant єrmax can be increased by applying low doping content of La2O3 in Ti-rich barium strontium titanate ceramics due to the increased spontaneous polarization.

  1. Preparation and properties of porous PMN-PZT ceramics doped with strontium

    International Nuclear Information System (INIS)

    Zeng Tao; Dong Xianlin; Mao Chaoliang; Chen Shutao; Chen Heng

    2006-01-01

    The piezoelectric and dielectric properties of lead magnesium niobate-lead zirconate titanate (PMN-PZT) ceramics were investigated as a function of density for transducer applications. A decrease in density increased elastic compliance and improved acoustic impedance matching between PMN-PZT ceramics and ambient media. The reduced dielectric constant (ε 33 ) and enhanced hydrostatic figure of merit (d h g h ) of PMN-PZT were observed with decreased density. The results showed the d h g h of PMN-PZT ceramic with density of about 5.4 g/cm 3 reached 4000 x 10 -15 m 2 /N, and the ε 33 was very close to 2000, which demonstrates that porous PMN-PZT ceramic is a promising material for transducer applications. Moreover, the low density PMN-PZT ceramics exhibited lower dielectric loss than high density PMN-PZT ceramics during the temperature from 250 deg. C to 500 deg. C

  2. Microstructure Control of Barium Titanate Grain-oriented Ceramics and Their Piezoelectric Properties

    International Nuclear Information System (INIS)

    Mori, Rintaro; Nakashima, Koichi; Fujii, Ichiro; Wada, Satoshi; Hayashi, Hiroshi; Nagamori, Yoshitaka; Yamamoto, Yuichi

    2011-01-01

    The Barium titanate (BaTiO 3 , BT) [110] grain-oriented ceramics along [110] direction were prepared by a templated grain growth (TGG) method. The [110] oriented BT platelike particles (t-BT) were used as template particles. The relationship between poling treatment program and piezoelectric constant was investigated. The change in the poling conditions did not greatly influence domain size and the piezoelectric constant. The relationship between piezoelectric properties and domain size in BT grain-oriented ceramics was investigated. The smaller domain size was required to increase the piezoelectric constant.

  3. Using the methods of radiospectroscopy (EPR, NMR) to study the nature of the defect structure of solid solutions based on lead zirconate titanate (PZT)

    Czech Academy of Sciences Publication Activity Database

    Bykov, I. P.; Zagorodniy, A.Y.; Yurchenko, L.P.; Korduban, A.M.; Nejezchleb, K.; Trachevsky, V.V.; Dimza, V.; Jastrabík, Lubomír; Dejneka, Alexandr

    2014-01-01

    Roč. 61, č. 8 (2014), 1379-1385 ISSN 0885-3010 R&D Projects: GA TA ČR TA01010517; GA ČR GAP108/12/1941 Institutional support: RVO:68378271 Keywords : lead zirconate titanate ( PZT ) * EPR * NMR * XPS spectroscopy Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 1.512, year: 2014

  4. Development of a stress sensor based on the piezoelectric lead zirconate titanate for impact stress measurement

    Science.gov (United States)

    Liu, Yiming; Xu, Bin; Li, Lifei; Li, Bing

    2012-04-01

    The measurement of stress of concrete structures under impact loading and other strong dynamic loadings is crucial for the monitoring of health and damage detection. Due to its main advantages including availability, extremely high rigidity, high natural frequency, wide measuring range, high stability, high reproducibility, high linearity and wide operating temperature range, piezoelectric (Lead Zirconate Titanate, PZT) ceramic materials has been a widely used smart material for both sensing and actuation for monitoring and control in engineering structures. In this paper, a kind of stress sensor based on piezoelectric ceramics for impact stress measuring of concrete structures is developed. Because the PZT is fragile, in order to employ it for the health monitoring of concrete structures, special handling and treatment should be taken to protect the PZT and to make it survive and work properly in concrete. The commercially available PZT patch with lead wires is first applied with an insulation coating to prevent water and moisture damage, and then is packaged by jacketing it by two small precasted cylinder concrete blocks with enough strength to form a smart aggregate (SA). The employed PZT patch has a dimension of 10mm x 10mm x 0.3mm. In order to calibrate the PZT based stress sensor for impact stress measuring, a dropping hammer was designed and calibration test on the sensitivity of the proposed transducer was carried out with an industry charge amplifier. The voltage output of the stress sensor and the impact force under different free falling heights and impact mass were recorded with a high sampling rate data acquisition system. Based on the test measurements, the sensibility of the PZT based stress sensor was determined. Results show that the output of the PZT based stress sensor is proportional to the stress level and the repeatability of the measurement is very good. The self-made piezoelectric stress sensor can be easily embedded in concrete and provide

  5. Effect of porosity on dielectric properties and microstructure of porous PZT ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Kumar, B. Praveen [PZT Centre, Armament Research and Development Establishment, Pune 411021 (India); Kumar, H.H. [PZT Centre, Armament Research and Development Establishment, Pune 411021 (India); Kharat, D.K. [PZT Centre, Armament Research and Development Establishment, Pune 411021 (India)]. E-mail: dkkharat@rediffmail.com

    2006-02-25

    Porous piezoelectric materials are of great interest because of their high hydrostatic figure of merit and low sound velocity, which results in to low acoustic impedance and efficient coupling with medium. Porous lead zirconate titanate (PZT) ceramics with varying porosity was developed using polymethyl methacrylate by burnable plastic spheres (BURPS) process. The porous PZT ceramics were characterized for dielectric constant ({epsilon}), dielectric loss factor (tan {delta}), hydrostatic charge (d {sub h}) and voltage (g {sub h}) coefficients and microstructure. The effect of the porous microstructure on the dielectric constant and loss factor at frequencies of 10-10{sup 5} Hz are discussed in this paper.

  6. Ferroelectric relaxor behaviour and impedance spectroscopy of Bi{sub 2}O{sub 3}-doped barium zirconium titanate ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Mahajan, Sandeep; Thakur, O P; Bhattacharya, D K [Electroceramics Group, Solid State Physics Laboratory, Lucknow Road, Delhi-110054 (India); Sreenivas, K, E-mail: omprakasht@hotmail.co [Department of Physics and Astrophysics, University of Delhi- 110007 (India)

    2009-03-21

    Bi{sub 2}O{sub 3}-doped barium zirconate titanate ceramics, Ba{sub 1-x}Bi{sub x}(Zr{sub 0.05}Ti{sub 0.95})O{sub 3}, have been prepared by the conventional solid-state reaction method. The ferroelectric relaxor behaviour and dielectric properties have been investigated in detail. By XRD analysis, it is suggested that up to x = 0.04, Bi{sup 3+} substitutes A-site ion, and thereafter with higher Bi{sup 3+} content, it enters the B-site sub lattice. Substitution of Bi{sup 3+} ions induces ferroelectric relaxor behaviour and the degree of relaxation behaviour increases with bismuth concentration. The remanent polarization and strain behaviour show a slight increase with the substitution level. The degree of hysteresis (strain versus electric field) also reduces from 21.4% to 4.6% with bismuth substitution. Impedance measurements were made on the prepared sample over a wide range of temperatures (300-723 K) and frequencies (40 Hz-1 MHz), which show the presence of both bulk and grain boundary effects in the material. The bulk and grain boundary conductivities determined from impedance study indicate the Arrhenius-type thermally activated process. Impedance spectroscopy is shown to be an efficient method capable of detecting the contributions of the resistances of grains and grain boundaries to the complex impedance of a ceramic system, accurately estimating its electrical conductivity as well as its corresponding activation energies and drawing conclusions on its structural properties.

  7. DIELECTRIC AND PYROELECTRIC PROPERTIES OF THE COMPOSITES OF FERROELECTRIC CERAMIC AND POLY(VINYL CHLORIDE

    Directory of Open Access Journals (Sweden)

    M.Olszowy

    2003-01-01

    Full Text Available The dielectric and pyroelectric properties of lead zirconate titanate/poly(vinyl chloride [PZT/PVC] and barium titanate/poly(vinyl chloride [BaTiO3/ PVC] composites were studied. Flexible composites were fabricated in the thin films form (200-400 μm by hot-pressed method. Powders of PZT or BaTiO3 in the shape of ≤ 75 μm ceramics particles were dispersed in a PVC matrix, providing composites with 0-3} connectivity. Distribution of the ceramic particles in the polymer phase was examined by scanning electron microscopy. The analysis of the thermally stimulated currents (TSC have also been done. The changes of dielectric and pyroelectric data on composites with different contents of ceramics up to 40% volume were investigated. The dielectric constants were measured in the frequency range from 600 Hz to 6 MHz at room temperature. The pyroelectric coefficient for BaTiO3/PVC composite at 343 K is about 35 μC/m2K which is higher than that of β-PVDF (10 μC/m2 K.

  8. Metalorganic solution deposition of lead zirconate titanate films onto an additively manufactured Ni-based superalloy

    International Nuclear Information System (INIS)

    Patel, T.; Khassaf, H.; Vijayan, S.; Bassiri-Gharb, N.; Aindow, M.; Alpay, S.P.; Hebert, R.J.

    2017-01-01

    Recent advances in additive manufacturing of high-temperature alloys for structural aerospace applications has led to interest in integrating additional functionality into such parts. Lead zirconate titanate (PZT) is a prototypical ferroelectric ceramic used as the electro-active material in many piezoelectric sensors and actuators. In this study, 300 nm thick PbZr_0_._2Ti_0_._8O_3 (PZT 20/80) films were grown using metalorganic solution deposition onto additively manufactured substrates of Inconel 718. The microstructures of the films and the nature of the film/substrate interfaces were characterized using a combination of X-ray diffraction and electron microscopy techniques. Electrical measurements were performed to determine the ferroelectric, dielectric, and conductive responses of the PZT films. Our findings show that the PZT films exhibit robust ferroelectricity characterized by well-defined polarization-applied electric field (P-E) hysteresis loops. The samples display internal bias of up to ∼40 kV/cm. The room temperature remnant polarization and the small signal dielectric permittivity are ∼70 μC/cm"2 and 205, respectively. The dielectric loss (tan δ) and the leakage current at 1 kHz are 9% and 1 nA at 1 V, respectively. We attribute the internal bias observed in the hysteresis loops and the overall large dielectric losses to the presence of an intermediate oxide layer at the PZT/Inconel interface, which forms during the high temperature crystallization of the ferroelectric film. These results show that it is possible to grow functional oxides with promising electrical properties onto additively manufactured metallic substrates.

  9. Piezoelectric and dielectric performance of poled lead zirconate titanate subjected to electric cyclic fatigue

    Science.gov (United States)

    Wang, Hong; Matsunaga, Tadashi; Lin, Hua-Tay; Mottern, Alexander M.

    2012-02-01

    Poled lead zirconate titanate (PZT) material as a single-layer plate was tested using a piezodilatometer under electric cyclic loading in both unipolar and bipolar modes. Its responses were evaluated using unipolar and bipolar measurements on the same setup. The mechanical strain and charge density loops exhibited various variations when the material was cycled for more than 108 cycles. The various quantities including loop amplitude, hysteresis, switchable polarization, and coercive field were characterized accordingly under the corresponding measurement conditions. At the same time, the offset polarization and bias electric field of the material were observed to be changed and the trend was found to be related to the measurement conditions also. Finally, the piezoelectric and dielectric coefficients were analyzed and their implications for the application of interest have been discussed.

  10. Piezoelectric and dielectric performance of poled lead zirconate titanate subjected to electric cyclic fatigue

    International Nuclear Information System (INIS)

    Wang, Hong; Matsunaga, Tadashi; Lin, Hua-Tay; Mottern, Alexander M

    2012-01-01

    Poled lead zirconate titanate (PZT) material as a single-layer plate was tested using a piezodilatometer under electric cyclic loading in both unipolar and bipolar modes. Its responses were evaluated using unipolar and bipolar measurements on the same setup. The mechanical strain and charge density loops exhibited various variations when the material was cycled for more than 10 8 cycles. The various quantities including loop amplitude, hysteresis, switchable polarization, and coercive field were characterized accordingly under the corresponding measurement conditions. At the same time, the offset polarization and bias electric field of the material were observed to be changed and the trend was found to be related to the measurement conditions also. Finally, the piezoelectric and dielectric coefficients were analyzed and their implications for the application of interest have been discussed. (paper)

  11. Maximising electro-mechanical response by minimising grain-scale strain heterogeneity in phase-change actuator ceramics

    DEFF Research Database (Denmark)

    Oddershede, Jette; Hossain, Mohammad Jahangir; Daniels, John E.

    2016-01-01

    Phase-change actuator ceramics directly couple electrical and mechanical energies through an electric-field-induced phase transformation. These materials are promising for the replacement of the most common electro-mechanical ceramic, lead zirconate titanate, which has environmental concerns. Here......, we show that by compositional modification, we reduce the grain-scale heterogeneity of the electro-mechanical response by 40%. In the materials investigated, this leads to an increase in the achievable electric-field-induced strain of the bulk ceramic of 45%. Compositions of (100-x)Bi0.5Na0.5TiO3-(x...... heterogeneity can be achieved by precise control of the lattice distortions and orientation distributions of the induced phases. The current results can be used to guide the design of next generation high-strain electro-mechanical ceramic actuator materials....

  12. The effects of sintering behavior on piezoelectric properties of porous PZT ceramics for hydrophone application

    International Nuclear Information System (INIS)

    Zeng Tao; Dong Xianlin; Chen Heng; Wang Yonglin

    2006-01-01

    Porous lead zirconate titanate (PZT) ceramics were fabricated by adding polymethyl methacrylate (PMMA) and the effects of sintering behavior on their microstructure and piezoelectric properties were investigated. The porosity of PZT ceramics decreased with an increase in the sintering temperature at a fixed PMMA addition. The dielectric constant (ε), longitudinal piezoelectric coefficient (d 33 ) and hydrostatic figures of merit (d h g h ) of 34% porous PZT ceramics increased with an increase in sintering temperature from 1050 to 1300 deg. C. When sintered at 1300 deg. C, longitudinal piezoelectric coefficient of 34% porous PZT ceramic was very close to that of 95% dense PZT ceramics, while the hydrostatic figures of merit of 34% porous PZT ceramics is about fifteen times more than that of 95% dense PZT ceramics. Compared with PZT-polymer composites, the dielectric constant of 34% porous PZT sintered at 1300 deg. C is much higher, which can be more efficient to resist the interference in receiving sensitivities caused by loading effect of the cable

  13. Thermal shock behavior of toughened gadolinium zirconate/YSZ double-ceramic-layered thermal barrier coating

    International Nuclear Information System (INIS)

    Zhong, Xinghua; Zhao, Huayu; Zhou, Xiaming; Liu, Chenguang; Wang, Liang; Shao, Fang; Yang, Kai; Tao, Shunyan; Ding, Chuanxian

    2014-01-01

    Highlights: • Gd 2 Zr 2 O 7 /YSZ DCL thermal barrier coating was designed and fabricated. • The Gd 2 Zr 2 O 7 top ceramic layer was toughened by addition of nanostructured 3YSZ. • Remarkable improvement in thermal shock resistance of the DCL coating was achieved. - Abstract: Double-ceramic-layered (DCL) thermal barrier coating system comprising of toughened Gadolinium zirconate (Gd 2 Zr 2 O 7 , GZ) as the top ceramic layer and 4.5 mol% Y 2 O 3 partially-stabilized ZrO 2 (4.5YSZ) as the bottom ceramic layer was fabricated by plasma spraying and thermal shock behavior of the DCL coating was investigated. The GZ top ceramic layer was toughened by addition of nanostructured 3 mol% Y 2 O 3 partially-stabilized ZrO 2 (3YSZ) to improve fracture toughness of the matrix. The thermal shock resistance of the DCL coating was enhanced significantly compared to that of single-ceramic-layered (SCL) GZ-3YSZ composite coating, which is believed to be primarily attributed to the two factors: (i) the increase in fracture toughness of the top ceramic layer by incorporating nanostructured YSZ particles and (ii) the improvement in strain tolerance through the utilization of 4.5YSZ as the bottom ceramic layer. In addition, the failure mechanisms are mainly attributed to the still low fracture toughness of the top ceramic layer and oxidation of the bond-coat

  14. Microstructural evaluation of alumina-niobium and alumina- niobium-zircon ceramics for ballistic application

    International Nuclear Information System (INIS)

    Mota, Juliana Machado da; Lopes, Cristina Moniz Araujo; Melo, Francisco Lourenco Cristovao de

    2009-01-01

    This study aimed to evaluate the microstructural of Alumina- Niobium and Alumina- Niobium-Zircon ceramics. Samples with 3.5 x 4.5 x 34 mm dimensions were prepared by uniaxial pressure (50 MPa) followed by isostatic pressure (300 MPa). The samples were sintered at 1500 ° C for 1 hour. The ceramics obtained were characterized by scanning electron microscopy (SEM) and X-ray diffraction, to evaluate the phases and microstructures. In order to analyze the microstructure, by SEM the samples were prepared using two techniques: heat treatment (1350 ° C for 5 minutes) and thermochemical treatment (500 ° C for 8 minutes in a solution of NaOH and KOH) on polished and fractured surfaces. The results showed that despite differences between the two etchings, both were effective to analyze the microstructure. (author)

  15. Fiscal 2000 achievement report. Venture business assisting type regional consortium - Minor business creation base type (Development of aluminum alloy casting system using aluminum titanate ceramic member); 2000 nendo chiiki consortium kenkyu kaihatsu jigyo seika hokokusho. Chitansan aluminium ceramics buzai wo shiyoshita aluminium gokin chuzo system no kaihatsu

    Energy Technology Data Exchange (ETDEWEB)

    NONE

    2001-03-01

    An automatic liquid metal charging system driven by a linear induction type electromagnetic pump is developed, with its members to be in contact with liquid aluminum alloy being constituted of aluminum titanate ceramics not to be wetted by liquid aluminum alloy and highly resistant to thermal impact. Technologies for casting aluminum titanate ceramic members in plaster molds, CIP (cold isostatic pressing) molding, and burning were established. The mechanism of wettability of liquid aluminum alloy on aluminum titanate ceramic members was elucidated, and an aluminum titanate ceramic member with a dense spinel layer formed thereon in situ was developed for improvement on non-wettability. The developed member remained non-wettable more than six times longer than conventional members. A special electronic counter mechanism was developed by installing in a conduit an aluminum titanate ceramic made impeller whose revolution was converted into electric signals for the measurement of the amount of charged liquid. A non-asbestos polycrystalline alumina-silica fiber was selected as the insulator for the melting/holding furnace, which enabled 30% energy conservation as compared with the conventional type. (NEDO)

  16. Thermodynamic properties of titanates, zirconates and hafnates of alkaline earth metals

    Energy Technology Data Exchange (ETDEWEB)

    1978-02-01

    The problems are considered arising in critical analysis and choosing recommended values of thermodynamic constants of the series of the most important perovskites-ferroelectrics-titanates, zirconates, and hafnates of alkaline-earth metals finding application in modern radioelectronics. Recommended values of standard thermodynamic values are given: heat capacity Csub(p,298) , enthalpy change H/sub 298/-H/sub 0/, entropy S/sub 298/, heat formation ..delta..Hsub(f,298 ), free energy formation ..delta..Gsub(f,298) , temperatures and heats of phase transitions with indication of errors for the adopted values. The effect of impurities on thermal constants of phase transitions is discussed. The relationships between thermodynamic characteristics of perovskites and crystal structure as well as the effect of orthorhombic distortions of ideal perovskite lattice on entropy of the compounds have been considered. Along with thermodynamic methods of investigation, a great attention is given to other physical methods which have been used for finding temperature regions of phase transitions, Curie points, and temperatures of transition from ferroelectric to paraelectric state. The importance of physical methods is emphasized in those cases when phase transitions are accompanied by small energy changes and are not fixed in measuring heat capacity.

  17. Full Ceramic Fuel Cells Based on Strontium Titanate Anodes, An Approach Towards More Robust SOFCs

    DEFF Research Database (Denmark)

    Holtappels, Peter; Irvine, J.T.S.; Iwanschitz, B.

    2013-01-01

    The persistent problems with Ni-YSZ cermet based SOFCs, with respect to redox stability and tolerance towards sulfur has stimulated the development of a full ceramic cell based on strontium titanate(ST)- based anodes and anode support materials, within the EU FCH JU project SCOTAS-SOFC. Three...

  18. Microwave assisted synthesis and characterization of barium titanate nanoparticles for multi layered ceramic capacitor applications.

    Science.gov (United States)

    Thirumalai, Sundararajan; Shanmugavel, Balasivanandha Prabu

    2011-01-01

    Barium titanate is a common ferroelectric electro-ceramic material having high dielectric constant, with photorefractive effect and piezoelectric properties. In this research work, nano-scale barium titanate powders were synthesized by microwave assisted mechano-chemical route. Suitable precursors were ball milled for 20 hours. TGA studies were performed to study the thermal stability of the powders. The powders were characterized by XRD, SEM and EDX Analysis. Microwave and Conventional heating were performed at 1000 degrees C. The overall heating schedule was reduced by 8 hours in microwave heating thereby reducing the energy and time requirement. The nano-scale, impurity-free and defect-free microstructure was clearly evident from the SEM micrograph and EDX patterns. LCR meter was used to measure the dielectric constant and dielectric loss values at various frequencies. Microwave heated powders showed superior dielectric constant value with low dielectric loss which is highly essential for the fabrication of Multi Layered Ceramic Capacitors.

  19. Dielectric characteristics of PZT 95/5 ferroelectric ceramics at high pressures

    International Nuclear Information System (INIS)

    Spears, R.K.

    1978-01-01

    The room temperature dielectric properties of a ferroelectric ceramic having a nominal composition of 95 atomic percent lead zirconate and 5 atomic percent lead titanate (designated as PZT 95/5) with a niobium dopant were examined at high hydrostatic pressures using a tetrahedral anvil apparatus. This ceramic has practical applications as a power source in which large quantities of charge are released by dynamic (shock wave) depolarization. Numerous mathematical models of this process have been proposed; however, the use of models has been limited because of the lack of high pressure electrical properties. This study attempted to provide these data on PZT 95/5 by determining the small signal and high electric field dielectric properties at pressures over 4 GPa

  20. Influence of poling on far-infrared response of lead zirconate titanate ceramics

    Czech Academy of Sciences Publication Activity Database

    Simon, E.; Hlinka, Jiří; Kamba, Stanislav; Gregora, Ivan; Erhart, J.

    2009-01-01

    Roč. 106, č. 7 (2009), 074104/1-074104/5 ISSN 0021-8979 R&D Projects: GA AV ČR KAN301370701; GA MŠk ME08109; GA ČR GA202/06/0411 Institutional research plan: CEZ:AV0Z10100520 Keywords : ceramics * dielectric polarisation * infrared spectra * lead compounds * phonons Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 2.072, year: 2009

  1. Effect of polarization fatigue on the Rayleigh coefficients of ferroelectric lead zirconate titanate thin films: Experimental evidence and implications

    Science.gov (United States)

    Lou, X. J.; Zhang, H. J.; Luo, Z. D.; Zhang, F. P.; Liu, Y.; Liu, Q. D.; Fang, A. P.; Dkhil, B.; Zhang, M.; Ren, X. B.; He, H. L.

    2014-09-01

    The effect of polarization fatigue on the Rayleigh coefficients of ferroelectric lead zirconate titanate (PZT) thin film was systematically investigated. It was found that electrical fatigue strongly affects the Rayleigh behaviour of the PZT film. Both the reversible and irreversible Rayleigh coefficients decrease with increasing the number of switching cycles. This phenomenon is attributed to the growth of an interfacial degraded layer between the electrode and the film during electrical cycling. The methodology used in this work could serve as an alternative way for evaluating the fatigue endurance and degradation in dielectric properties of ferroelectric thin-film devices during applications.

  2. Substrate clamping effects on irreversible domain wall dynamics in lead zirconate titanate thin films.

    Science.gov (United States)

    Griggio, F; Jesse, S; Kumar, A; Ovchinnikov, O; Kim, H; Jackson, T N; Damjanovic, D; Kalinin, S V; Trolier-McKinstry, S

    2012-04-13

    The role of long-range strain interactions on domain wall dynamics is explored through macroscopic and local measurements of nonlinear behavior in mechanically clamped and released polycrystalline lead zirconate-titanate (PZT) films. Released films show a dramatic change in the global dielectric nonlinearity and its frequency dependence as a function of mechanical clamping. Furthermore, we observe a transition from strong clustering of the nonlinear response for the clamped case to almost uniform nonlinearity for the released film. This behavior is ascribed to increased mobility of domain walls. These results suggest the dominant role of collective strain interactions mediated by the local and global mechanical boundary conditions on the domain wall dynamics. The work presented in this Letter demonstrates that measurements on clamped films may considerably underestimate the piezoelectric coefficients and coupling constants of released structures used in microelectromechanical systems, energy harvesting systems, and microrobots.

  3. Temperature dependence of high field electromechanical coupling in ferroelectric ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Weaver, P M; Cain, M G; Stewart, M, E-mail: paul.weaver@npl.co.u [National Physical Laboratory, Hampton Road, Teddington, Middlesex, TW11 0LW (United Kingdom)

    2010-04-28

    A study of the temperature dependence of the electromechanical response of ferroelectric lead zirconate titanate (PZT) ceramics at high electric fields (up to 1.3 kV mm{sup -1}) is reported. Simultaneous measurements were performed of strain, electric field and polarization to form a complete response map from room temperature up to 200 {sup 0}C. An electrostrictive model is shown to provide an accurate description of the electromechanical response to high levels of induced polarization and electric field. This provides a method for decoupling strain contributions from thermal expansion and polarization changes. Direct measurements of electrostriction and thermal expansion, above and below the Curie temperature, are reported. Electrostriction coefficients are shown to be temperature dependent in these ceramic materials, with different values above and below the Curie temperature.

  4. Texturing of sodium bismuth titanate-barium titanate ceramics by templated grain growth

    Science.gov (United States)

    Yilmaz, Huseyin

    2002-01-01

    Sodium bismuth titanate modified with barium titanate, (Na1/2Bi 1/2)TiO3-BaTiO3 (NBT-BT), is a candidate lead-free piezoelectric material which has been shown to have comparatively high piezoelectric response. In this work, textured (Na1/2Bi1/2)TiO 3-BaTiO3 (5.5mol% BaTiO3) ceramics with pc (where pc denotes the pseudocubic perovskite cell) orientation were fabricated by Templated Grain Growth (TGG) or Reactive Templated Grain Growth (RTGG) using anisotropically shaped template particles. In the case of TGG, molten salt synthesized SrTiO3 platelets were tape cast with a (Na1/2Bi1/2)TiO3-5.5mol%BaTiO3 powder and sintered at 1200°C for up to 12 hours. For the RTGG approach, Bi4Ti3O12 (BiT) platelets were tape cast with a Na2CO3, Bi2O3, TiO 2, and BaCO3 powder mixture and reactively sintered. The TGG approach using SrTiO3 templates gave stronger texture along [001] compared to the RTGG approach using BiT templates. The textured ceramics were characterized by X-ray and electron backscatter diffraction for the quality of texture. The texture function was quantified by the Lotgering factor, rocking curve, pole figures, inverse pole figures, and orientation imaging microscopy. Electrical and electromechanical property characterization of randomly oriented and pc textured (Na1/2Bi1/2)TiO 3-5.5 mol% BaTiO3 rhombohedral ceramics showed 0.26% strain at 70 kV/cm, d33 coefficients over 500 pC/N have been obtained for highly textured samples (f ˜ 90%). The piezoelectric coefficient from Berlincourt was d33 ˜ 200 pC/N. The materials show considerable hysteresis. The presence of hysteresis in the unipolar-electric field curve is probably linked to the ferroelastic phase transition seen in the (Na 1/2Bi1/2)TiO3 system on cooling from high temperature at ˜520°C. The macroscopic physical properties (remanent polarization, dielectric constant, and piezoelectric coefficient) of random and textured ([001] pc) rhombohedral perovskites were estimated by linear averaging of single

  5. Efficient photoemission from robust ferroelectric ceramics

    International Nuclear Information System (INIS)

    Boscolo, I.; Castellano, M.; Catani, L.; Ferrario, M.; Tazzioli, F.; Giannessi, L.

    1999-01-01

    Experimental results on photoemission by ferroelectric ceramic disks, with a possible interpretation, are present. Two types of lead zirconate titanate lanthanum doped, PLZT, ceramics have been used for tests. 25 ps light pulses of 532 and 355 nm were used for excitation. The intensity ranged within the interval 0.1-3 GW/cm 2. The upper limit of the intensity was established by the damage threshold tested by the onset of ion emission. At low value of the intensity the yield was comparable at the two wavelengths. At the highest intensity of green light the emitted charge was 1 nC per 10 mm 2, but it was limited by the space charge effect. In fact, the applied field was only 20 kV/cm, allowed both by the mechanical design of the apparatus and the poor vacuum, 10 - 4 mbar. No surface processing was required. The measurement of the electron pulse length under way

  6. Preparation of lead titanate zirconate from metal citrates; Preparacao do titanato zirconato de chumbo a partir dos citratos metalicos

    Energy Technology Data Exchange (ETDEWEB)

    Bastos, C M.R.

    1994-12-31

    Lead titanate zirconate (PZT) preparation from its metal constituent citrates have been investigated. Metal citrates were obtained by forced precipitation using a dehydration alcohol mixture. Salt solutions of lead nitrate and octahydrated zirconyl chloride, and titanium tetrachloride were treated separately with citric acid and ammonium hydroxide. Zirconium, titanium and lead oxides resulted from thermal decomposition of corresponding citrates at 500{sup 0} C, 450{sup 0} C and 250{sup 0} C, respectively. Lead titanate (PT) and lead zirconate (P Z) were obtained by calcining at 450{sup 0} C and 500{sup 0} C, respectively, after adequate heating of citrates mechanically mixed in ethyl ether. PZT samples were obtained with different starting stoichiometry. Rhombohedral PZT-1 53/47 sample was prepared from co precipitating zirconyl ammonium and ammonium lead citrates in presence of ethanolic titanium oxide dispersion, and calcinating at 800{sup 0} C. Rhombohedral PZT-q 52/48 sample was obtained from heating at 500{sup 0} C for 2 hours a mixture of metal citrates coprecipitated by dehydration mixture of acetone-ethanol-formic acid (2:1:0,06). Tetragonal PZT-m stoichiometry 53/47 sample were obtained by calcining at after 600{sup 0} C for 2 hours after heating a mechanically mixed metal citrates. PT phase arose at 400{sup 0} C. PZT-m powders obtained in a range of 400{sup 0} C-800{sup 0} C were isostatically pressed, and sintered at 1100{sup 0} C and 1200{sup 0} C in saturated Pb O atmosphere. Rhombohedral sintered PZT was obtained with 7,78 g.cm{sup -3} at 1200{sup 0} C. (author). 123 refs, 53 figs, 32 tabs.

  7. Conformable amplified lead zirconate titanate sensors with enhanced piezoelectric response for cutaneous pressure monitoring.

    Science.gov (United States)

    Dagdeviren, Canan; Su, Yewang; Joe, Pauline; Yona, Raissa; Liu, Yuhao; Kim, Yun-Soung; Huang, YongAn; Damadoran, Anoop R; Xia, Jing; Martin, Lane W; Huang, Yonggang; Rogers, John A

    2014-08-05

    The ability to measure subtle changes in arterial pressure using devices mounted on the skin can be valuable for monitoring vital signs in emergency care, detecting the early onset of cardiovascular disease and continuously assessing health status. Conventional technologies are well suited for use in traditional clinical settings, but cannot be easily adapted for sustained use during daily activities. Here we introduce a conformal device that avoids these limitations. Ultrathin inorganic piezoelectric and semiconductor materials on elastomer substrates enable amplified, low hysteresis measurements of pressure on the skin, with high levels of sensitivity (~0.005 Pa) and fast response times (~0.1 ms). Experimental and theoretical studies reveal enhanced piezoelectric responses in lead zirconate titanate that follow from integration on soft supports as well as engineering behaviours of the associated devices. Calibrated measurements of pressure variations of blood flow in near-surface arteries demonstrate capabilities for measuring radial artery augmentation index and pulse pressure velocity.

  8. Develop techniques for ion implantation of PLZT [lead-lanthanum-zirconate-titanate] for adaptive optics

    International Nuclear Information System (INIS)

    Batishko, C.R.; Brimhall, J.L.; Pawlewicz, W.T.; Stahl, K.A.; Toburen, L.H.

    1987-09-01

    Research was conducted at Pacific Northwest Laboratory to develop high photosensitivity adaptive optical elements utilizing ion implanted lanthanum-doped lead-zirconate-titanate (PLZT). One centimeter square samples were prepared by implanting ferroelectric and anti-ferroelectric PLZT with a variety of species or combinations of species. These included Ne, O, Ni, Ne/Cr, Ne/Al, Ne/Ni, Ne/O, and Ni/O, at a variety of energies and fluences. An indium-tin oxide (ITO) electrode coating was designed to give a balance of high conductivity and optical transmission at near uv to near ir wavelengths. Samples were characterized for photosensitivity; implanted layer thickness, index of refraction, and density; electrode (ITO) conductivity; and in some cases, residual stress curvature. Thin film anti-ferroelectric PLZT was deposited in a preliminary experiment. The structure was amorphous with x-ray diffraction showing the beginnings of a structure at substrate temperatures of approximately 550 0 C. This report summarizes the research and provides a sampling of the data taken during the report period

  9. Orientation of rapid thermally annealed lead zirconate titanate thin films on (111) Pt substrate

    International Nuclear Information System (INIS)

    Brooks, K.G.; Reaney, I.M.; Klissurska, R.; Huang, Y.; Bursill, L.A.; Setter, N.

    1994-01-01

    The nucleation, growth and orientation of lead zirconate titanate thin films prepared from organometallic precursor solutions by spin coating on (111) oriented platinum substrates and crystallized by rapid thermal annealing was investigated. The effects of pyrolysis temperature, post-pyrolysis thermal treatments, excess lead addition, and Nb dopant substitution are reported. The use of post pyrolysis oxygen anneals at temperatures in the regime of 350-450 deg C was found to strongly effect the kinetics of subsequent amorphous-pyrochlore perovskite crystallization by rapid thermal annealing. It has also allowed films of reproducible microstructure and textures (both (100) and (111)) to be prepared by rapid thermal annealing. It is suggested that such anneals and pyrolysis temperature affect the oxygen concentration/average Pb valence in the amorphous films prior to annealing. The changes in Pb valence state then affect the stability of the transient pyrochlore phase and thus the kinetics of perovskite crystallization. Nb dopant was also found to influence the crystallization kinetics. 28 refs., 18 figs

  10. Fatigue responses of lead zirconate titanate stacks under semibipolar electric cycling with mechanical preload

    Science.gov (United States)

    Wang, Hong; Cooper, Thomas A.; Lin, Hua-Tay; Wereszczak, Andrew A.

    2010-10-01

    Lead zirconate titanate (PZT) stacks that had an interdigital internal electrode configuration were tested to more than 108 cycles. A 100 Hz semibipolar sine wave with a field range of +4.5/-0.9 kV/mm was used in cycling with a concurrently-applied 20 MPa preload. Significant reductions in piezoelectric and dielectric responses were observed during the cycling depending on the measuring condition. Extensive partial discharges were also observed. These surface events resulted in the erosion of external electrode and the exposure of internal electrodes. Sections prepared by sequential polishing technique revealed a variety of damage mechanisms including delaminations, pores, and etch grooves. The scale of damage was correlated with the degree of fatigue-induced reduction in piezoelectric and dielectric responses. The results from this study demonstrate the feasibility of using a semibipolar mode to drive a PZT stack under a mechanical preload and illustrate the potential fatigue and damages of the stack in service.

  11. Output characteristics of piezoelectric lead zirconate titanate detector using high-energy heavy-ion beam

    International Nuclear Information System (INIS)

    Takechi, Seiji; Sekiguchi, Masahiro; Miyachi, Takashi; Kobayashi, Masanori; Hattori, Maki; Okudaira, Osamu; Shibata, Hiromi; Fujii, Masayuki; Okada, Nagaya; Murakami, Takeshi; Uchihori, Yukio

    2014-01-01

    A radiation detector fabricated using piezoelectric lead zirconate titanate (PZT) has been studied by irradiating it with a 400 MeV/n xenon (Xe) beam. The beam diameter was controlled to change the irradiation conditions. It was found that the magnitude of the output observed from the PZT detector may be related to the number of Xe ions per unit area per unit time within the limits of the experimental conditions. -- Highlights: • The performance of PZT detector was studied by irradiation of a 400 MeV/n Xe beam. • The beam diameter was controlled to change the irradiation conditions. • By the control, the number of Xe ions per one pulse was changed from ∼500 to ∼1500. • The output of the PZT detector was not always larger with more intense beam. • The energy of Xe ions per unit area per unit time may determine the output

  12. Research on output signal of piezoelectric lead zirconate titanate detector using Monte Carlo method

    Energy Technology Data Exchange (ETDEWEB)

    Takechi, Seiji, E-mail: takechi@elec.eng.osaka-cu.ac.jp [Graduate School of Engineering, Osaka City University, Osaka 558-8585 (Japan); Mitsuhashi, Tomoaki; Miura, Yoshinori [Graduate School of Engineering, Osaka City University, Osaka 558-8585 (Japan); Miyachi, Takashi; Kobayashi, Masanori; Okudaira, Osamu [Planetary Exploration Research Center, Chiba Institute of Technology, Narashino, Chiba 275-0016 (Japan); Shibata, Hiromi [The Institute of Scientific and Industrial Research, Osaka University, Ibaraki, Osaka 567-0047 (Japan); Fujii, Masayuki [Famscience Co., Ltd., Tsukubamirai, Ibaraki 300-2435 (Japan); Okada, Nagaya [Honda Electronics Co., Ltd., Toyohashi, Aichi 441-3193 (Japan); Murakami, Takeshi; Uchihori, Yukio [National Institute of Radiological Sciences, Chiba 263-8555 (Japan)

    2017-06-21

    The response of a radiation detector fabricated from piezoelectric lead zirconate titanate (PZT) was studied. The response signal due to a single 400 MeV/n xenon (Xe) ion was assumed to have a simple form that was composed of two variables, the amplitude and time constant. These variables were estimated by comparing two output waveforms obtained from a computer simulation and an experiment on Xe beam irradiation. Their values appeared to be dependent on the beam intensity. - Highlights: • The performance of PZT detector was studied by irradiation of a 400 MeV/n Xe beam. • Monte Carlo simulation was used to examine the formation process of the output. • The response signal due to a single Xe ion was assumed to have a simple form. • The form was composed of two variables, the amplitude and time constant. • These variables appeared to be dependent on the beam intensity.

  13. Study of influence of fuel on dielectric and ferroelectric properties of bismuth titanate ceramics synthesized using solution based combustion technique

    International Nuclear Information System (INIS)

    Subohi, Oroosa; Malik, M M; Kurchania, Rajnish; Kumar, G S

    2015-01-01

    The effect of fuel characteristics on the processing and properties of bismuth titanate (BIT) ceramics obtained by solution combustion route using different fuels are reported in this paper. Dextrose, urea and glycine were used as fuel in this study. The obtained bismuth titanate ceramics were characterized by using XRD, SEM at different stages of sample preparation. It was observed that BIT obtained by using dextrose as fuel shows higher dielectric constant and higher remnant polarization due to smaller grain size and lesser c-axis growth as compared to the samples with urea and glycine as fuel. The electrical behavior of the samples with respect to temperature and frequency was also investigated to understand relaxation phenomenon. (paper)

  14. Piezoelectric Lead Zirconate Titanate (PZT) Ring Shaped Contour-Mode MEMS Resonators

    Science.gov (United States)

    Kasambe, P. V.; Asgaonkar, V. V.; Bangera, A. D.; Lokre, A. S.; Rathod, S. S.; Bhoir, D. V.

    2018-02-01

    Flexibility in setting fundamental frequency of resonator independent of its motional resistance is one of the desired criteria in micro-electromechanical (MEMS) resonator design. It is observed that ring-shaped piezoelectric contour-mode MEMS resonators satisfy this design criterion than in case of rectangular plate MEMS resonators. Also ring-shaped contour-mode piezoelectric MEMS resonator has an advantage that its fundamental frequency is defined by in-plane dimensions, but they show variation of fundamental frequency with different Platinum (Pt) thickness referred as change in ratio of fNEW /fO . This paper presents the effects of variation in geometrical parameters and change in piezoelectric material on the resonant frequencies of Platinum piezoelectric-Aluminium ring-shaped contour-mode MEMS resonators and its electrical parameters. The proposed structure with Lead Zirconate Titanate (PZT) as the piezoelectric material was observed to be a piezoelectric material with minimal change in fundamental resonant frequency due to Platinum thickness variation. This structure was also found to exhibit extremely low motional resistance of 0.03 Ω as compared to the 31-35 Ω range obtained when using AlN as the piezoelectric material. CoventorWare 10 is used for the design, simulation and corresponding analysis of resonators which is Finite Element Method (FEM) analysis and design tool for MEMS devices.

  15. Titanate ceramics for immobilisation of uranium-rich radioactive wastes arising from {sup 99}Mo production

    Energy Technology Data Exchange (ETDEWEB)

    Carter, M.L.; Li, H. [Institute of Materials Engineering, Australian Nuclear Science and Technology Organisation, PMB 1, Menai, Sydney, NSW 2232 (Australia); Zhang, Y. [Institute of Materials Engineering, Australian Nuclear Science and Technology Organisation, PMB 1, Menai, Sydney, NSW 2232 (Australia)], E-mail: yzx@ansto.gov.au; Vance, E.R.; Mitchell, D.R.G. [Institute of Materials Engineering, Australian Nuclear Science and Technology Organisation, PMB 1, Menai, Sydney, NSW 2232 (Australia)

    2009-02-28

    Uranium-rich liquid wastes arising from UO{sub 2} targets which have been neutron-irradiated to generate medical radioisotopes such as {sup 99m}Tc require immobilisation. A pyrochlore-rich hot isostatically pressed titanate ceramic can accommodate at least 40 wt% of such waste expressed on an oxide basis. In this paper, the baseline waste form composition (containing 40 wt% UO{sub 2}) was adjusted in two ways: (a) varying the UO{sub 2} loading with constant precursor oxide materials, (b) varying the precursor composition with constant waste loading of UO{sub 2}. This resulted in the samples having a similar phase assemblage but the amounts of each phase varied. The oxidation states of U in selected samples were determined using diffuse reflection spectroscopy (DRS) and electron energy loss spectroscopy (EELS). Leaching studies showed that there was no significant difference in the normalised elemental release rates and the normalised release rates are comparable with those from synroc-C. This demonstrates that waste forms based on titanate ceramics are robust and flexible for the immobilisation of U-rich waste streams from radioisotope processing.

  16. Barium titanate coated with magnesium titanate via fused salt method and its dielectric property

    International Nuclear Information System (INIS)

    Chen Renzheng; Cui Aili; Wang Xiaohui; Li Longtu

    2003-01-01

    Barium titanate fine particles were coated homogeneously with magnesium titanate via the fused salt method. The thickness of the magnesium titanate film is 20 nm, as verified by TEM and XRD. The mechanism of the coating is that: when magnesium chloride is liquated in 800 deg. C, magnesium will replace barium in barium titanate, and form magnesium titanate film on the surface of barium titanate particles. Ceramics sintered from the coated particles show improved high frequency ability. The dielectric constant is about 130 at the frequency from 1 to 800 MHz

  17. Effects of Polarization on Mechanical Properties of Lead Zirconate Titanate Ceramics Evaluated by Modified Small Punch Tests

    Science.gov (United States)

    Deng, Qihuang; Fan, Yuchi; Wang, Lianjun; Xiong, Zhi; Wang, Hongzhi; Li, Yaogang; Zhang, Qinghong; Kawasaki, Akira; Jiang, Wan

    2012-01-01

    Pb(Zr,Ti)O3 (PZT) ceramics were prepared by the conventional mixed oxide method, and the strength of the resultant PZT ceramics was evaluated using modified small punch (MSP) tests. Load-displacement curve test results showed that the crack-initiation and fracture strengths of PZT ceramics decreased after polarization. The effect of the polarization accelerated the fatigue properties of PZT ceramics. Scanning electron microscopy (SEM) results showed that microcracks were formed before the maximum load in the MSP test, and the first load drop corresponded to crack initiation.

  18. Non-aqueous electrochemical deposition of lead zirconate titanate films for flexible sensor applications

    Science.gov (United States)

    Joseph, Sherin; Kumar, A. V. Ramesh; John, Reji

    2017-11-01

    Lead zirconate titanate (PZT) is one of the most important piezoelectric materials widely used for underwater sensors. However, PZTs are hard and non-compliant and hence there is an overwhelming attention devoted toward making it flexible by preparing films on flexible substrates by different routes. In this work, the electrochemical deposition of composition controlled PZT films over flexible stainless steel (SS) foil substrates using non-aqueous electrolyte dimethyl sulphoxide (DMSO) was carried out. Effects of various key parameters involved in electrochemical deposition process such as current density and time of deposition were studied. It was found that a current density of 25 mA/cm2 for 5 min gave a good film. The morphology and topography evaluation of the films was carried out by scanning electron microscopy (SEM) and atomic force microscopy (AFM), respectively, which showed a uniform morphology with a surface roughness of 2 nm. The PZT phase formation was studied using X-ray diffraction (XRD) and corroborated with Raman spectroscopic studies. The dielectric constant, dielectric loss, hysteresis and I-V characteristics of the film was evaluated.

  19. Sol–gel followed by urea–acetone spherodization for preparation of lithium titanate ceramics pebbles and preliminary characterization

    Energy Technology Data Exchange (ETDEWEB)

    Sinha, S.K., E-mail: sk.sinha@bitmesra.ac.in [Department of Physics, Birla Institute of Technology, Patna 800014 (India); Yadav, S. [Department of Physics, Birla Institute of Technology, Patna 800014 (India); Raole, P.M. [Institute for Plasma Research, Bhat, Gandhinagar 382428 (India)

    2016-12-15

    Lithium titanate ceramics pebbles were prepared by chemical method of sol. gel followed by urea-aceton spherodization technique. Lithium titanate having monoclinic phase was obtained. Laser flash method was used to study thermal conductivity and diffusivity of the ceramics. At near 472 K the average value of diffusivity was around 0.0052 cm{sup 2} s{sup −1} while the specific heat capacity was 3101.3 J kg{sup −1} K{sup −1} while the same two parameters had values of 0.0041 cm{sup 2} s{sup −1} and 3894.4 J kg{sup −1} K{sup −1} at a temperature 1050 K. The crush strength of pebble was measured on Universal Testing Machine (UTM) and was found as 37.08 N. The density was measured and found to be 2.8 g/cc (81.63% of TD of value 3.43 g/cc).

  20. Electrical characterization of strontium titanate borosilicate glass ceramics system with bismuth oxide addition using impedance spectroscopy

    International Nuclear Information System (INIS)

    Thakur, O.P.; Kumar, Devendra; Parkash, Om; Pandey, Lakshman

    2003-01-01

    The ac electrical data, measured in the frequency range 0.1 kHz-1 MHz, were used to study the electrical response of strontium titanate borosilicate glass ceramic system with bismuth oxide addition. Complex plane plots from these electrical data for various glass ceramic samples reveal contributions from simultaneously operating polarization mechanisms to overall dielectric behavior. The complex modulus (M * ) representation of electrical data for various glass ceramic samples were found to be more informative. Equivalent circuit models, which represent the electrical behavior of glass ceramic samples, were determined using complex non-linear least square (CNLS) fitting. An attempt has been made to understand the dielectric behavior of various glass ceramics in terms of contributions arising from different polarization processes occurring at glassy matrix, crystalline phases, glass to crystal interface region and blocking electrodes. Glass ceramics containing SrTiO 3 and TiO 2 (rutile) phases show thermally stable dielectric behavior

  1. Energy Harvesting with Coupled Magnetorestrictive Resonators

    Science.gov (United States)

    2013-09-01

    matching, small hysteresis, and low coercivity2. Ceramic material like PZT tends to develop fatigue during its cycles whereas Galfenol does not have...Magnetostrictive Material PZT Pb [ZrxTi1-x] O3, 0<xə, Lead Zirconate Titanate RX Receiver SHM Structural Health Monitoring...zirconate titanate [ PZT ]) have lead in their fabrication process, which is an environmental risk. Another major issue with standard energy

  2. Anion and cation diffusion in barium titanate and strontium titanate

    International Nuclear Information System (INIS)

    Kessel, Markus Franz

    2012-01-01

    Perovskite oxides show various interesting properties providing several technical applications. In many cases the defect chemistry is the key to understand and influence the material's properties. In this work the defect chemistry of barium titanate and strontium titanate is analysed by anion and cation diffusion experiments and subsequent time-of-flight secondary ion mass spectrometry (ToF-SIMS). The reoxidation equation for barium titanate used in multi-layer ceramic capacitors (MLCCs) is found out by a combination of different isotope exchange experiments and the analysis of the resulting tracer diffusion profiles. It is shown that the incorporation of oxygen from water vapour is faster by orders of magnitude than from molecular oxygen. Chemical analysis shows the samples contain various dopants leading to a complex defect chemistry. Dysprosium is the most important dopant, acting partially as a donor and partially as an acceptor in this effectively acceptor-doped material. TEM and EELS analysis show the inhomogeneous distribution of Dy in a core-shell microstructure. The oxygen partial pressure and temperature dependence of the oxygen tracer diffusion coefficients is analysed and explained by the complex defect chemistry of Dy-doped barium titanate. Additional fast diffusion profiles are attributed to fast diffusion along grain boundaries. In addition to the barium titanate ceramics from an important technical application, oxygen diffusion in cubic, nominally undoped BaTiO 3 single crystals has been studied by means of 18 O 2 / 16 O 2 isotope exchange annealing and subsequent determination of the isotope profiles in the solid by ToF-SIMS. It is shown that a correct description of the diffusion profiles requires the analysis of the diffusion through the surface space-charge into the material's bulk. Surface exchange coefficients, space-charge potentials and bulk diffusion coefficients are analysed as a function of oxygen partial pressure and temperature. The

  3. In situ synchrotron diffraction of lead-zirconate-titanate at its morphotropic phase boundary

    International Nuclear Information System (INIS)

    Schoenau, K.A.

    2008-01-01

    Ferroelectric lead zirconate titanate ceramics (PZT,Pb(Zr x Ti 1-x )O 3 ) find in industry intensifiedly applications as piezoactors. Their largest macroscopic strain under electric field they show in the region of the morphotropic phase boundary (MPB), the transition region between the Ti rich tetragonal and the Zr rich structure. The structure of PZT at the MPB was controversially discussed since the detection of a monoclinic intermediate phase by Noheda et al. [Appl. Phys. Lett.,74(14), 2059(1999)], whereby into the considerations the domain structure of the material not entered, which however is essentially responsible for the reaction under electric field. In order to understand the domain structure of PZT under electric field and to study possible causes for the fatigue behaviour of the material under bipolar cycling a bridge must be built between macroscopic and local structure. For this at the measuring place B2 of the Hasylab, Hamburg, synchrotron X-ray powder diffractometry was in situ performed under different sample environments in transmission geometry, which was correlated with transmission-electron-microscopical studies and electron spin resonance. Samples with compositions over the whole MPB were beside temperature-dependent measurements measured at room temperature in high resolution and under applied electric field. Furthermore for studies under electric field at elevated temperatures a special E-field furnace was constructed. It could be shown the large piezoelectric reaction of PZT at its MPB is strongly correlated with a diminishment of the domain structure, which simulates in X-ray diffraction a lower symmetric phase. The stability range of the nanodomains with temperature and electric field reflects in the switching behaviour of the matter and by the detection of a relaxor behavior of the nanodomain structure for the first time a direct comparison with relaxoceramics is possible. The varying stress conditions within the sample influence

  4. Adhesion strength of lead zirconate titanate sol-gel thin films

    Energy Technology Data Exchange (ETDEWEB)

    Berfield, Thomas A., E-mail: tom.berfield@louisville.edu [Department of Mechanical Engineering, University of Louisville, Louisville, KY 40292 (United States); Kitey, Rajesh [Department of Aerospace Engineering, Indian Institute of Technology Kanpur, Kanpur (India); Kandula, Soma S. [Intel Corporation, Portland, OR (United States)

    2016-01-01

    The adhesion strength between a thin film and substrate is often the critical parameter that controls the initiation as well as the mode of film failure. In this work, a laser-based spallation method is used to determine the adhesion strength of “as deposited” lead zirconate titanate (PZT) sol-gel thin films on the two functionally different substrates. For the first case, PZT sol-gel film is deposited onto bare Si/SiO{sub 2} substrates via spin casting. The extremely high adhesion strength between the film and the substrate necessitated an additional platinum mass superlayer to be deposited on top of the PZT film in order to induce interfacial failure. For the superlayer film system, a hybrid experimental/numerical method is employed for determining the substrate/film interfacial strength, quantified to be in the range of 460–480 MPa. A second substrate variation with lower adhesion strength is also prepared by applying a self-assembled octadecyltrichlorosilane (ODS) monolayer to the Si/SiO{sub 2} substrate prior to the film deposition. For the monolayer-coated substrate case, the adhesion strength is observed to be significantly lower (54.7 MPa) when compared to the earlier case. - Highlights: • A non-contact laser spallation method is used to determine PZT film adhesion. • A mediated self-assembled monolayer is shown to greatly reduce interface strength. • Adhesion strength for even well-bonded thin films was found using a superlayer.

  5. Experimental Determination of Effect of Variable Resistance on Lead ZirconateTitanate (PZT-5A4Eunder various Thermal and Frequency Conditions

    Directory of Open Access Journals (Sweden)

    Hassan Elahi

    2014-12-01

    Full Text Available A specially designed apparatus and circuit working on the principle of inverse piezoelectricity due to the effect of polarization was used to find the relationship between resistance and peak to peak voltage of Lead Zirconate Titanate (PZT-5A4E by shocking it at variable frequencies and at variable resistances under various thermal conditions within Curie temperature limit using equivalent circuit method. It was found that by increasing temperature, peak to peak voltage increases and similarly by increasing frequency, peak to peak voltage decreases and with the increase in resistance peak to peak voltage decreases.

  6. Generation of electrical energy using lead zirconate titanate (PZT-5A) piezoelectric material: Analytical, numerical and experimental verifications

    Energy Technology Data Exchange (ETDEWEB)

    Butt, Zubair; Ahmad, Nasir [Dept. of Mechanical, Mechatronics and Manufacturing Engineering, UET Lahore, Faisalabad Campus, Lahore (Pakistan); Pasha, Riffat Asim; Qayyum, Faisal; Anjum, Zeeshan [Dept. of Mechanical Engineering, University of Engineering and Technology, Taxila (Pakistan); Elahi, Hassan [Northwestern Polytechnical University, Xian (China)

    2016-08-15

    Energy harvesting is the process of attaining energy from the external sources and transforming it into usable electrical energy. An analytical model of piezoelectric energy harvester has been developed to determine the output voltage across an electrical circuit when it is forced to undergo a base excitation. This model gives an easy approach to design and investigate the behavior of piezoelectric material. Numerical simulations have been carried out to determine the effect of frequency and loading on a Lead zirconate titanate (PZT-5A) piezoelectric material. It has been observed that the output voltage from the harvester increases when loading increases whereas its resonance frequency decreases. The analytical results were found to be in good agreement with the experimental and numerical simulation results.

  7. Structural and electrical properties of Sm{sup 3+} substituted PZT ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Pandey, S.K. [Solid State Physics Laboratory, Timarpur, Delhi 110 054 (India)], E-mail: 628@ssplnet.org; Thakur, O.P.; Bhattacharya, D.K. [Solid State Physics Laboratory, Timarpur, Delhi 110 054 (India); Prakash, Chandra [DRDO Bhawan, DHQ, New Delhi 110 011 (India); Chatterjee, Ratnamala [Department of Physics, Indian Institute of Technology, New Delhi 110 016 (India)

    2009-01-22

    Samarium modified lead zirconate titanate (PSZT: Pb{sub 1-x}Sm{sub x}(Zr{sub 0.65}Ti{sub 0.35})O{sub 3}: x = 0, 0.02, 0.04, 0.06) ceramics were synthesized by solid state ceramic route. XRD shows single-phase formation with rhombohedral structure up to x = 0.04. With Sm-substitution, the grain size first increases up to x = 0.02 and then decreases. A metal/ferroelectric/metal (MFM) structure was made by depositing gold electrode on the flat surfaces for electrical measurements. All samples show normal ferroelectric behaviour, however, a squareness of P-E loop (polarization vs. electric field) was observed to increase with Sm content. Higher electromechanical coupling coefficients (K{sub p} and K{sub t}) have been achieved for the PZT with 6 mol% Sm substitution and having fine grain size.

  8. Study of grain boundary tunneling in barium-titanate ceramic films

    CERN Document Server

    Wong, H; Poon, M C

    1999-01-01

    The temperature and the electric-field dependences of the current-voltage characteristics and the low-frequency noise of barium-titanate ceramic films are studied. An abnormal field dependence is observed in the resistivity of BaTiO sub 3 materials with a small average grain size. In addition, experiments show that the low-frequency noise behaviors are governed by grain-boundary tunneling at room temperature and by trapping-detrapping of grain-boundary states at temperatures above the Curie point. Physical models for the new observations are developed. Results suggest that grain-boundary tunneling of carriers is as important as the double Schottky barrier in the current conduction in BaTiO sub 3 materials with small grain sizes.

  9. Fabrication and properties of yttrium doped barium titanate film by RF sputtering

    International Nuclear Information System (INIS)

    Igarashi, H.; Yuasa, M.; Okazaki, K.

    1985-01-01

    Semiconductive barium titanate films were fabricated by RF sputtering on fused quartz, alumina and barium titanate ceramic substrates using barium titanate ceramic with a small amount of yttria as a target. The films on the barium titanate substrates turned blue color and showed a small PTC effect by heat-treating at 1000 0 C in the air after deposition at the substrate temperature of 600 0 C

  10. Fracture mechanics of ceramics. Vol. 8. Microstructure, methods, design, and fatigue

    International Nuclear Information System (INIS)

    Bradt, R.C.; Evans, A.G.; Hasselman, D.P.H.; Lange, F.F.

    1986-01-01

    This paper presents information on the following topics: fracture mechanics and microstructures; non-lubricated sliding wear of Al 2 O 3 , PSZ and SiC; mixed-mode fracture of ceramics; some fracture properties of alumina-containing electrical porcelains; transformation toughening in the Al 2 O 3 -Cr 2 O 3 /ZrO 2 -HfO 2 system; strength toughness relationships for transformation toughened ceramics; tensile strength and notch sensitivity of Mg-PSZ; fracture mechanisms in lead zirconate titanate ceramics; loading-unloading techniques for determining fracture parameters of brittle materials utilizing four-point bend, chevron-notched specimens; application of the potential drop technique to the fracture mechanics of ceramics; ceramics-to-metal bonding from a fracture mechanics perspective; observed changes in fracture strength following laser irradiation and ion beam mixing of Ni overlayers on sintered alpha-SiC; crack growth in single-crystal silicon; a fracture mechanics and non-destructive evaluation investigation of the subcritical-fracture process in rock; slow crack growth in sintered silicon nitride; uniaxial tensile fatigue testing of sintered silicon carbide under cyclic temperature change; and effect of surface corrosion on glass fracture

  11. Synthesis and characterization of lead zirconate titanate powders obtained by the oxidant peroxo method

    International Nuclear Information System (INIS)

    Camargo, Emerson R.; Leite, Edson R.; Longo, Elson

    2009-01-01

    Lead zirconate titanate (PbZr 1-x Ti x O 3 ) was synthesized by the 'oxidant peroxo method (OPM)' with 'x' between 0.25 and 0.50. Titanium metal was dissolved into a hydrogen peroxide/ammonia aqueous solution, followed by the addition of lead and zirconium nitrate solution. The amorphous precipitated precursor obtained was crystallized by heat treatment between 400 and 1000 deg. C. Images of transmission microscopy showed spherical particles with average diameter between 20 and 60 nm, and the presence of necks between particles treated at 700 deg. C. All of the unpressed powders were characterized by X-ray diffractometry and FT-Raman spectroscopy. Powder samples with 'x' up to 0.35 showed rhombohedral structure when treated at temperatures higher than 500 deg. C, and tetragonal structure when 'x' was higher than 0.40. Analysis of XRD and Raman spectroscopy of the precursor powders showed amorphous-like structures, however powders treated at 400 deg. C showed a structure identified as an intermediate pyrochlore phase, independently of the Zr and Ti mole ratio

  12. Fatigue of extracted lead zirconate titanate multilayer actuators under unipolar high field electric cycling

    International Nuclear Information System (INIS)

    Wang, Hong; Lee, Sung-Min; Wang, James L.; Lin, Hua-Tay

    2014-01-01

    Testing of large prototype lead zirconate titanate (PZT) stacks presents substantial technical challenges to electronic testing systems, so an alternative approach that uses subunits extracted from prototypes has been pursued. Extracted 10-layer and 20-layer plate specimens were subjected to an electric cycle test under an electric field of 3.0/0.0 kV/mm, 100 Hz to 10 8 cycles. The effects of measurement field level and stack size (number of PZT layers) on the fatigue responses of piezoelectric and dielectric coefficients were observed. On-line monitoring permitted examination of the fatigue response of the PZT stacks. The fatigue rate (based on on-line monitoring) and the fatigue index (based on the conductance spectrum from impedance measurement or small signal measurement) were developed to quantify the fatigue status of the PZT stacks. The controlling fatigue mechanism was analyzed against the fatigue observations. The data presented can serve as input to design optimization of PZT stacks and to operation optimization in critical applications, such as piezoelectric fuel injectors in heavy-duty diesel engines

  13. Fatigue of extracted lead zirconate titanate multilayer actuators under unipolar high field electric cycling

    Science.gov (United States)

    Wang, Hong; Lee, Sung-Min; Wang, James L.; Lin, Hua-Tay

    2014-12-01

    Testing of large prototype lead zirconate titanate (PZT) stacks presents substantial technical challenges to electronic testing systems, so an alternative approach that uses subunits extracted from prototypes has been pursued. Extracted 10-layer and 20-layer plate specimens were subjected to an electric cycle test under an electric field of 3.0/0.0 kV/mm, 100 Hz to 108 cycles. The effects of measurement field level and stack size (number of PZT layers) on the fatigue responses of piezoelectric and dielectric coefficients were observed. On-line monitoring permitted examination of the fatigue response of the PZT stacks. The fatigue rate (based on on-line monitoring) and the fatigue index (based on the conductance spectrum from impedance measurement or small signal measurement) were developed to quantify the fatigue status of the PZT stacks. The controlling fatigue mechanism was analyzed against the fatigue observations. The data presented can serve as input to design optimization of PZT stacks and to operation optimization in critical applications, such as piezoelectric fuel injectors in heavy-duty diesel engines.

  14. Fatigue of extracted lead zirconate titanate multilayer actuators under unipolar high field electric cycling

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Hong, E-mail: wangh@ornl.gov; Lee, Sung-Min; Wang, James L. [Materials Science and Technology Division, Oak Ridge National Laboratory, Oak Ridge, Tennessee 37831 (United States); Lin, Hua-Tay [School of Mechanical and Electronic Engineering, Guangdong University of Technology, Guangzhou, 510006 (China)

    2014-12-21

    Testing of large prototype lead zirconate titanate (PZT) stacks presents substantial technical challenges to electronic testing systems, so an alternative approach that uses subunits extracted from prototypes has been pursued. Extracted 10-layer and 20-layer plate specimens were subjected to an electric cycle test under an electric field of 3.0/0.0 kV/mm, 100 Hz to 10{sup 8} cycles. The effects of measurement field level and stack size (number of PZT layers) on the fatigue responses of piezoelectric and dielectric coefficients were observed. On-line monitoring permitted examination of the fatigue response of the PZT stacks. The fatigue rate (based on on-line monitoring) and the fatigue index (based on the conductance spectrum from impedance measurement or small signal measurement) were developed to quantify the fatigue status of the PZT stacks. The controlling fatigue mechanism was analyzed against the fatigue observations. The data presented can serve as input to design optimization of PZT stacks and to operation optimization in critical applications, such as piezoelectric fuel injectors in heavy-duty diesel engines.

  15. Reaction of strontium zirconate with refractory borides and carbides

    International Nuclear Information System (INIS)

    Bowker, J.C.; Lane, J.E.

    1990-01-01

    The chemical compatibility of the potential oxide ceramic matrix material, strontium zirconate, and several different potential nonoxide ceramic reinforcement materials was studied by elevated temperature reaction. Results are presented in this paper

  16. Preparation and characterization of Grain-Oriented Barium Titanate Ceramics Using Electrophoresis Deposition Method under A High Magnetic Field

    Energy Technology Data Exchange (ETDEWEB)

    Kita, T; Kondo, S; Takei, T; Kumada, N; Nakashima, K; Fujii, I; Wada, S [Material Science and Technology, Interdisciplinary Graduate School of Medical and Engineering, University of Yamanashi, 4-4-37 Takeda, Kofu, Yamanashi 400-8510 (Japan); Suzuki, T S; Uchikoshi, T; Sakka, Y [National Institute for materials Science, 1-2-1 Sengen, Tsukuba, Ibaraki 305-0047 (Japan); Miwa, Y; Kawada, S; Kimura, M, E-mail: swada@yamanashi.ac.jp [Murata Manufacturing Co., Ltd. 2288 Ooshinohara, Yasu, Shiga 520-2393 (Japan)

    2011-10-29

    Barium titanate (BaTiO{sub 3}) grain-oriented ceramics were prepared using electrophoresis deposition (EPD) method under high magnetic field of 12 T. First, BaTiO{sub 3} nanoparticles with high c/a ratio of 1.008 and size of 84 nm were prepared by two-step thermal decomposition method with barium titanyl oxalate nanoparticles. Using the BaTiO{sub 3} slurry, BaTiO{sub 3} nanoparticle accumulations were prepared by EPD method under high magnetic field. After binder burnout, the accumulations were sintered and BaTiO{sub 3} grain-oriented ceramics were prepared. Moreover, dielectric properties of their ceramics were investigated

  17. Effect of Semiconductor Element Substitution on the Electric Properties of Barium Titanate Ceramics

    Directory of Open Access Journals (Sweden)

    Garbarz-Glos B.

    2016-06-01

    Full Text Available The investigated ceramics were prepared by a solid-state reaction from simple oxides and carbonates with the use of a mixed oxide method (MOM. The morphology of BaTi0.96Si0.04O3 (BTSi04 ceramics was characterised by means of a scanning electron microscopy (SEM. It was found that Si+4 ion substitution supported the grain growth process in BT-based ceramics. The EDS results confirmed the high purity and expected quantitative composition of the synthesized material. The dielectric properties of the ceramics were also determined within the temperature range (ΔT=130-500K. It was found that the substitution of Si+4 ions had a significant influence on temperature behavior of the real (ε’ and imaginary (ε” parts of electric permittivity as well as the temperature dependence of a.c. conductivity. Temperature regions of PTCR effect (positive temperature coefficient of resistivity were determined for BTSi04 ceramics in the vicinity of structural phase transitions typical for barium titanate. No distinct maximum indicating a low-temperature structural transition to a rhombohedral phase in BTSi04 was found. The activation energy of conductivity was determined from the Arrhenius plots. It was found that substitution of Si ions in amount of 4wt.% caused almost 50% decrease in an activation energy value.

  18. Enhanced electrocaloric analysis and energy-storage performance of lanthanum modified lead titanate ceramics for potential solid-state refrigeration applications.

    Science.gov (United States)

    Zhang, Tian-Fu; Huang, Xian-Xiong; Tang, Xin-Gui; Jiang, Yan-Ping; Liu, Qiu-Xiang; Lu, Biao; Lu, Sheng-Guo

    2018-01-10

    The unique properties and great variety of relaxer ferroelectrics make them highly attractive in energy-storage and solid-state refrigeration technologies. In this work, lanthanum modified lead titanate ceramics are prepared and studied. The giant electrocaloric effect in lanthanum modified lead titanate ceramics is revealed for the first time. Large refrigeration efficiency (27.4) and high adiabatic temperature change (1.67 K) are achieved by indirect analysis. Direct measurements of electrocaloric effect show that reversible adiabatic temperature change is also about 1.67 K, which exceeds many electrocaloric effect values in current direct measured electrocaloric studies. Both theoretical calculated and direct measured electrocaloric effects are in good agreements in high temperatures. Temperature and electric field related energy storage properties are also analyzed, maximum energy-storage density and energy-storage efficiency are about 0.31 J/cm 3 and 91.2%, respectively.

  19. Effect of oxygen partial pressure on texture development in lead zirconate titanate thin films processed from metalorganic precursors

    International Nuclear Information System (INIS)

    Norton, Jarrod L.; Liedl, Gerald L.; Slamovich, Elliott B.

    1999-01-01

    Metalorganic liquid precursors were used to examine the effects of processing atmosphere on texture development in oriented Pb(Zr 0.60 Ti 0.40 )O 3 thin films. After removal of organic ligands via pyrolysis, the films were heated at 25 degree sign C/min in a 5% H 2 /Ar atmosphere until a switching temperature, after which the atmosphere was switched to pure oxygen. The films were heated to a maximum temperature of 650 degree sign C with switching temperatures ranging from 450 to 600 degree sign C. The degree of (111) orientation in the lead zirconate titanate (PZT) films increased with increasing switching temperature, resulting in highly textured (111) PZT films. These results suggest that atmosphere control plays a significant role in texture development during rapid thermal processing. (c) 1999 Materials Research Society

  20. Residual stress relief due to fatigue in tetragonal lead zirconate titanate ceramics

    International Nuclear Information System (INIS)

    Hall, D. A.; Mori, T.; Comyn, T. P.; Ringgaard, E.; Wright, J. P.

    2013-01-01

    High energy synchrotron XRD was employed to determine the lattice strain ε{111}and diffraction peak intensity ratio R{200}in tetragonal PZT ceramics, both in the virgin poled state and after a bipolar fatigue experiment. It was shown that the occurrence of microstructural damage during fatigue was accompanied by a reduction in the gradient of the ε{111}–cos 2 ψ plot, indicating a reduction in the level of residual stress due to poling. In contrast, the fraction of oriented 90° ferroelectric domains, quantified in terms of R{200}, was not affected significantly by fatigue. The change in residual stress due to fatigue is interpreted in terms of a change in the average elastic stiffness of the polycrystalline matrix due to the presence of inter-granular microcracks

  1. Residual stress relief due to fatigue in tetragonal lead zirconate titanate ceramics

    Science.gov (United States)

    Hall, D. A.; Mori, T.; Comyn, T. P.; Ringgaard, E.; Wright, J. P.

    2013-07-01

    High energy synchrotron XRD was employed to determine the lattice strain ɛ{111} and diffraction peak intensity ratio R{200} in tetragonal PZT ceramics, both in the virgin poled state and after a bipolar fatigue experiment. It was shown that the occurrence of microstructural damage during fatigue was accompanied by a reduction in the gradient of the ɛ{111}-cos2 ψ plot, indicating a reduction in the level of residual stress due to poling. In contrast, the fraction of oriented 90° ferroelectric domains, quantified in terms of R{200}, was not affected significantly by fatigue. The change in residual stress due to fatigue is interpreted in terms of a change in the average elastic stiffness of the polycrystalline matrix due to the presence of inter-granular microcracks.

  2. Mechanical Pre-Stressing a Transducer through a Negative DC Biasing Field

    Science.gov (United States)

    2017-04-21

    Undersea Warfare Center ONR Office of Naval Research PMN-PT Lead Magnesium Niobate-Lead Titanate PZT Lead Zirconate Titanate 1 MECHANICAL...stiff material (such as aluminum or magnesium ). With the ceramic stack sandwiched between the two masses, a two degree-of-freedom system is...Aerotech, Inc., Pittsburgh, PA. Sayer, M., Judd, B.A., EI -Assal, K., Prasad, E., “Poling of Piezoelectric Ceramics,” Journal of the Canadian

  3. Description of tritium release from lithium titanate at constant temperature

    Energy Technology Data Exchange (ETDEWEB)

    Pena, L; Lagos, S; Jimenez, J; Saravia, E [Comision Chilena de Energia Nuclear, Santiago (Chile)

    1998-03-01

    Lithium Titanate Ceramics have been prepared by the solid-state route, pebbles and pellets were fabricated by extrusion and their microstructure was characterized in our laboratories. The ceramic material was irradiated in the La Reina Reactor, RECH-1. A study of post-irradiation annealing test, was performed measuring Tritium release from the Lithium Titanate at constant temperature. The Bertone`s method modified by R. Verrall is used to determine the parameters of Tritium release from Lithium Titanate. (author)

  4. Chemical solution deposited BaPbO3 buffer layers for lead zirconate titanate ferroelectric films

    International Nuclear Information System (INIS)

    Tseng, T.-K.; Wu, J.-M.

    2005-01-01

    Conductive perovskite BaPbO 3 (BPO) films have been prepared successfully by chemical solution deposition method through spin-coating on Pt/Ti/SiO 2 /Si substrates. The choice of baking temperature is a key factor on the development of conducting BPO perovskite phase. When the baking temperature is higher than 350 deg. C, the BPO films contain a high content of BaCO 3 phase after annealing at temperatures higher than 500 deg. C. If the baking temperature is chosen lower than 300 deg. C, such as 200 deg. C, the annealed BPO films consist mostly of perovskite with only traces of BaCO 3 . Choosing 200 deg. C as the baking temperature, the BPO films developed single perovskite phase at temperatures as low as 550 deg. C. The perovskite BPO phase is stable in the range of 550-650 deg. C and the measured sheet resistance of the BPO films is about 2-3 Ω/square. The perovskite BPO film as a buffer layer provides improvement in electric properties of lead zirconate titanate films

  5. Dielectric Strontium Zirconate Sprayed by a Plasma Torch.

    Czech Academy of Sciences Publication Activity Database

    Ctibor, Pavel; Sedláček, J.; Janata, Marek

    2017-01-01

    Roč. 10, č. 4 (2017), s. 225-230 ISSN 2008-2134 Institutional support: RVO:61389021 Keywords : Plasma spraying * Electrical properties * Strontium Zirconate * Insulators Subject RIV: JH - Ceramics, Fire-Resistant Materials and Glass OBOR OECD: Ceramics www.pccc.icrc.ac.ir/Articles/18/1/18/1010/

  6. Auto-regenerative thermoluminescence dating using zircon inclusions

    International Nuclear Information System (INIS)

    Templer, R.H.

    1993-01-01

    Fired ceramics containing zircon inclusions have been dated by allowing the zircons to regenerate their own thermoluminescence (TL) signal, hence auto-regenerative TL dating. The technique is conceptually straightforward. One first measures the TL accrued since the last heating of the material. The zircon grains are then stored for six months and the TL signal regenerated through self-irradiation is measured. Since the internal dose-rate for zircon is dominated by the internal component the age of the sample is simply given by the ratio of the natural to auto-regenerated signal times the laboratory storage period. The technique, however, requires the measurement of a very small auto-regenerated signal, which introduces a number of experimental and physical complications. The methods for overcoming these problems and successfully dating zircons by auto-regeneration are described. (Author)

  7. Synthesis and characterization of lead zirconate titanate powders obtained by the oxidant peroxo method

    Energy Technology Data Exchange (ETDEWEB)

    Camargo, Emerson R. [LIEC-Laboratorio Interdisciplinar de Eletroquimica e Ceramica, Department of Chemistry, UFSCar-Federal University of Sao Carlos, Rod. Washington Luis km 235, CP 676, Sao Carlos SP, 13565-905 (Brazil)], E-mail: camargo@ufscar.br; Leite, Edson R. [LIEC-Laboratorio Interdisciplinar de Eletroquimica e Ceramica, Department of Chemistry, UFSCar-Federal University of Sao Carlos, Rod. Washington Luis km 235, CP 676, Sao Carlos SP, 13565-905 (Brazil)], E-mail: derl@power.ufscar.br; Longo, Elson [Department of Biochemistry, Chemistry Institute of Araraquara, UNESP, Sao Paulo State University Rua Francisco Degni, CP 355 Araraquara SP, 14801-907 Brazil (Brazil)], E-mail: elson@iq.unesp.br

    2009-02-05

    Lead zirconate titanate (PbZr{sub 1-x}Ti{sub x}O{sub 3}) was synthesized by the 'oxidant peroxo method (OPM)' with 'x' between 0.25 and 0.50. Titanium metal was dissolved into a hydrogen peroxide/ammonia aqueous solution, followed by the addition of lead and zirconium nitrate solution. The amorphous precipitated precursor obtained was crystallized by heat treatment between 400 and 1000 deg. C. Images of transmission microscopy showed spherical particles with average diameter between 20 and 60 nm, and the presence of necks between particles treated at 700 deg. C. All of the unpressed powders were characterized by X-ray diffractometry and FT-Raman spectroscopy. Powder samples with 'x' up to 0.35 showed rhombohedral structure when treated at temperatures higher than 500 deg. C, and tetragonal structure when 'x' was higher than 0.40. Analysis of XRD and Raman spectroscopy of the precursor powders showed amorphous-like structures, however powders treated at 400 deg. C showed a structure identified as an intermediate pyrochlore phase, independently of the Zr and Ti mole ratio.

  8. Raman analysis of ferroelectric switching in niobium-doped lead zirconate titanate thin films

    International Nuclear Information System (INIS)

    Ferrari, P.; Ramos-Moore, E.; Guitar, M.A.; Cabrera, A.L.

    2014-01-01

    Characteristic Raman vibration modes of niobium-doped lead zirconate titanate (PNZT) are studied as a function of ferroelectric domain switching. The microstructure of PNZT is characterized by scanning electron microscopy and X-ray diffraction. Ferroelectric switching is achieved by applying voltages between the top (Au) and bottom (Pt) electrodes, while acquiring the Raman spectra in situ. Vibrational active modes associated with paraelectric and ferroelectric phases are identified after measuring above and below the ferroelectric Curie temperature, respectively. Changes in the relative intensities of the Raman peaks are observed as a function of the switching voltage. The peak area associated with the ferroelectric modes is analyzed as a function of the applied voltage within one ferroelectric polarization loop, showing local maxima around the coercive voltage. This behavior can be understood in terms of the correlation between vibrational and structural properties, since ferroelectric switching modifies the interaction between the body-centered atom (Zr, Ti or Nb) and the Pb–O lattice. - Highlights: • Electric fields induce structural distortions on ferroelectric perovskites. • Ferroelectric capacitor was fabricated to perform hysteresis loops. • Raman analysis was performed in situ during ferroelectric switching. • Raman modes show hysteresis and inflections around the coercive voltages. • Data can be understood in terms of vibrational–structural correlations

  9. NOVEL CERAMIC MEMBRANE FOR HIGH TEMPERATURE CARBON DIOXIDE SEPARATION; SEMIANNUAL

    International Nuclear Information System (INIS)

    Jerry Y.S. Lin; Jun-ichi Ida

    2001-01-01

    This project is aimed at demonstrating technical feasibility for a lithium zirconate based dense ceramic membrane for separation of carbon dioxide from flue gas at high temperature. The research work conducted in this reporting period was focused on several fundamental issues of lithium zirconate important to the development of the dense inorganic membrane. These fundamental issues include material synthesis of lithium zirconate, phases and microstructure of lithium zirconate and structure change of lithium zirconate during sorption/desorption process. The results show difficulty to prepare the dense ceramic membrane from pure lithium zirconate, but indicate a possibility to prepare the dense inorganic membrane for carbon dioxide separation from a composite lithium zirconate

  10. A multi-feature integration method for fatigue crack detection and crack length estimation in riveted lap joints using Lamb waves

    Data.gov (United States)

    National Aeronautics and Space Administration — This paper presents an experimental study of damage detection and quantification in riveted lap joints. Embedded lead zirconate titanate piezoelectric (PZT) ceramic...

  11. Observation of potential barriers on barium strontium titanate PTCR ceramics by electrostatic force microscopy

    International Nuclear Information System (INIS)

    Manfredini, J.P.; Paulin Filho, P.I.; Gheno, S.M.

    2011-01-01

    A composition of PTCR ceramic based in barium titanate with isovalent replacement of part of barium by strontium using lanthanum and manganese as additives was investigated. The transition temperature, typical of these materials, was shifted below the room temperature by the presence of strontium, whose behavior was detected by tests of DC resistivity and impedance spectroscopy. The observation of potential barriers at grain boundaries was possible through the technique of electrostatic force microscopy (EFM). The results also showed the presence of space charges in regions inside grains, possibly at subgrain boundaries. (author)

  12. Ferroelectrics principles, structure and applications

    CERN Document Server

    Merchant, Serena

    2014-01-01

    Ferroelectric physics is a theory on ferroelectric phase transition for explaining various related phenomena, which is different from dielectric physics. Ferroelectric materials are important functional materials for various applications such as NVRAMs, high energy density capacitors, actuators, MEMs, sonar sensors, microphones and scanning electron microscopes (SEM). This book investigates the dielectric, ferroelectric and energy storage properties of barium zirconate-titanate/barium calcium-titanate (BZT-BCT) based ceramic for high energy density capacitors. It also compares the energy storage capabilities of ceramic powders with polymer-ceramic nanocomposites; and discusses dielectric properties of ferroelectricity in composition distributions.

  13. Dynamic magnetoelectric effects in bulk and layered composites of cobalt zinc ferrite and lead zirconate titanate

    Energy Technology Data Exchange (ETDEWEB)

    Srinivasan, G.; Hayes, R.; DeVreugd, C.P. [Oakland University, Physics Department, Rochester, MI (United States); Laletsin, V.M.; Paddubnaya, N. [National Academy of Sciences, Institute of Technical Acoustics, Vitebsk (Belarus)

    2005-02-01

    Low-frequency magnetoelectric (ME) coupling is investigated in bulk samples and multilayers of cobalt zinc ferrite, Co{sub 1-x}Zn{sub x}Fe{sub 2}O{sub 4} (x=0-0.6), and lead zirconate titanate. In bulk samples, the transverse and longitudinal couplings are weak and of equal magnitude. A substantial strengthening of ME interactions is evident in layered structures, with the ME voltage coefficient a factor of 10-30 higher than in bulk samples. Important findings of our studies of layered composites are as follows. (i) The transverse coupling is stronger than the longitudinal coupling. (ii) The strength of ME interactions is dependent on Zn substitution, with a maximum for x=0.4. (iii) A weak coupling exists at the ferromagnetic-piezoelectric interface, as revealed by an analysis of the volume and static magnetic field dependence of ME voltage coefficients. (iv) The interface coupling k increases with Zn substitution and the k versus x profile shows a maximum centered at x=0.4. (v) The Zn-assisted enhancement can be attributed to efficient magneto-mechanical coupling in the ferrite. (orig.)

  14. Effect of electrical and mechanical poling history on domain orientation and piezoelectric properties of soft and hard PZT ceramics

    International Nuclear Information System (INIS)

    Marsilius, Mie; Granzow, Torsten; Jones, Jacob L

    2011-01-01

    The superior piezoelectric properties of all polycrystalline ferroelectrics are based on the extent of non-180 0 domain wall motion under electrical and mechanical poling loads. To distinguish between 180 0 and non-180 0 domain wall motion in a soft-doped and a hard-doped lead zirconate titanate (PZT) ceramic, domain texture measurements were performed using x-ray and neutron diffraction after different loading procedures. Comparing the results to measurements of the remanent strain and piezoelectric coefficient allowed the differentiation between different microstructural contributions to the macroscopic parameters. Both types of ceramic showed similar behavior under electric field, but the hard-doped material was more susceptible to mechanical load. A considerable fraction of the piezoelectric coefficient originated from poling by the preferred orientation of 180 0 domains.

  15. Effect of electrical and mechanical poling history on domain orientation and piezoelectric properties of soft and hard PZT ceramics

    Science.gov (United States)

    Marsilius, Mie; Granzow, Torsten; Jones, Jacob L.

    2011-02-01

    The superior piezoelectric properties of all polycrystalline ferroelectrics are based on the extent of non-180° domain wall motion under electrical and mechanical poling loads. To distinguish between 180° and non-180° domain wall motion in a soft-doped and a hard-doped lead zirconate titanate (PZT) ceramic, domain texture measurements were performed using x-ray and neutron diffraction after different loading procedures. Comparing the results to measurements of the remanent strain and piezoelectric coefficient allowed the differentiation between different microstructural contributions to the macroscopic parameters. Both types of ceramic showed similar behavior under electric field, but the hard-doped material was more susceptible to mechanical load. A considerable fraction of the piezoelectric coefficient originated from poling by the preferred orientation of 180° domains.

  16. Electric properties and phase transition behavior in lead lanthanum zirconate stannate titanate ceramics with low zirconate content

    Science.gov (United States)

    Zeng, Tao; Lou, Qi-Wei; Chen, Xue-Feng; Zhang, Hong-Ling; Dong, Xian-Lin; Wang, Gen-Shui

    2015-11-01

    The phase transitions, dielectric properties, and polarization versus electric field (P-E) hysteresis loops of Pb0.97La0.02(Zr0.42Sn0.58-xTix)O3 (0.13≤ x ≤0.18) (PLZST) bulk ceramics were systematically investigated. This study exhibited a sequence of phase transitions by analyzing the change of the P-E hysteresis loops with increasing temperature. The antiferroelectric (AFE) to ferroelectric (FE) phase boundary of PLZST with the Zr content of 0.42 was found to locate at the Ti content between 0.14 and 0.15. This work is aimed to improve the ternary phase diagram of lanthanum-doped PZST with the Zr content of 0.42 and will be a good reference for seeking high energy storage density in the PLZST system with low-Zr content. Project supported by the National Natural Science Foundation of China (Grant Nos. 51202273, 11204304, and 11304334) and the Science and Technology Commission of Shanghai Municipality, China (Grant No. 14DZ2261000).

  17. The production of grain oriented lanthanum titanate (La2Ti2O7) ceramics by uniaxial hot-forging process for improved fracture toughness

    International Nuclear Information System (INIS)

    Ceylan, Ali

    2008-01-01

    The layered-structural ceramics, such as lanthanum titanate (La 2 Ti 2 O 7 ), have been known for their good electrical and optical properties at high frequencies and temperatures. However, few studies have been conducted on the mechanical properties of these ceramics. The interest in ceramic hot-forging (HF) has been greatly increased recently due to the enhancement in fracture toughness via bridging effect of oriented grains. In this study, grain oriented lanthanum titanate was produced by the hot-forging process. The characterizations of the samples were achieved by density measurement, scanning electron microscopy (SEM), optical microscopy, X-ray diffraction (XRD), Vickers indentation and three-point bending test. According to X-ray diffraction patterns, the orientation factor (f) was found to be 0.73 for certain hot-forging conditions resulting an improved fracture toughness. The improved fracture toughness of La 2 Ti 2 O 7 (3.2 MPa m 1/2 ) reached to the value of monolithic alumina (Al 2 O 3 ) between 3 and 4 MPa m 1/2

  18. Development, Characterization and Piezoelectric Fatigue Behavior of Lead-Free Perovskite Piezoelectric Ceramics

    Science.gov (United States)

    Patterson, Eric Andrew

    Much recent research has focused on the development lead-free perovskite piezoelectrics as environmentally compatible alternatives to lead zirconate titanate (PZT). Two main categories of lead free perovskite piezoelectric ceramic systems were investigated as potential replacements to lead zirconate titanate (PZT) for actuator devices. First, solid solutions based on Li, Ta, and Sb modified (K0.5Na0.5)NbO3 (KNN) lead-free perovskite systems were created using standard solid state methods. Secondly, Bi-based materials a variety of compositions were explored for (1-x)(Bi 0.5Na0.5)TiO3-xBi(Zn0.5Ti0.5)O 3 (BNT-BZT) and Bi(Zn0.5Ti0.5)O3-(Bi 0.5K0.5)TiO3-(Bi0.5Na0.5)TiO 3 (BZT-BKT-BNT). It was shown that when BNT-BKT is combined with increasing concentrations of Bi(Zn1/2i1/2)O3 (BZT), a transition from normal ferroelectric behavior to a material with large electric field induced strains was observed. The higher BZT containing compositions are characterized by large hysteretic strains(> 0.3%) with no negative strains that might indicate domain switching. This work summarizes and analyzes the fatigue behavior of the new generation of Pb-free piezoelectric materials. In piezoelectric materials, fatigue is observed as a degradation in the electromechanical properties under the application of a bipolar or unipolar cyclic electrical load. In Pb-based materials such as lead zirconate titanate (PZT), fatigue has been studied in great depth for both bulk and thin film applications. In PZT, fatigue can result from microcracking or electrode effects (especially in thin films). Ultimately, however, it is electronic and ionic point defects that are the most influential mechanism. Therefore, this work also analyzes the fatigue characteristics of bulk polycrystalline ceramics of the modified-KNN and BNT-BKT-BZT compositions developed. The defect chemistry that underpins the fatigue behavior will be examined and the results will be compared to the existing body of work on PZT. It will

  19. Crystallization of sol-gel derived lead zirconate titanate thin films in argon and oxygen atmospheres

    International Nuclear Information System (INIS)

    Bursill, L.A.

    1994-01-01

    Electron diffraction and high-resolution electron microscopic techniques are applied to reveal the mechanisms of crystallization of 75 nm thin films of ferroelectric lead-zirconate-titanate (PZT). Sol-gel methods, followed by pyrolysis at 350 deg C, were used to provide a common starting point after which a variety of rapid-thermal annealing (RTA) experiments in the temperature range 400-700 deg C were made in argon, oxygen and nitrogen/hydrogen atmospheres. The results are interpreted in terms of the crystal chemical analysis, which points out that partial pressure of oxygen and heating rate are important experimental parameters which must be controlled if ferroelectric perovskite-type Pb 2 ZrTiO 6 , rather than pyrochlore-type Pb 2 ZrTiO 6+x , where O < X < 1 or -1 < X < O, is to be obtained after the RTA step. Thus significant improvements in the crystallization of perovskite-type PZT were clearly demonstrated by using argon atmospheres for the RTA step. The results have significance for the production of high-quality ferroelectric thin films, with improved switching and fatigue characteristics, since even small amounts of the pyrochlore phase prove detrimental for these properties. 18 refs., 1 tab., 10 figs

  20. Unexpectedly high piezoelectricity of Sm-doped lead zirconate titanate in the Curie point region.

    Science.gov (United States)

    Seshadri, Shruti B; Nolan, Michelle M; Tutuncu, Goknur; Forrester, Jennifer S; Sapper, Eva; Esteves, Giovanni; Granzow, Torsten; Thomas, Pam A; Nino, Juan C; Rojac, Tadej; Jones, Jacob L

    2018-03-07

    Large piezoelectric coefficients in polycrystalline lead zirconate titanate (PZT) are traditionally achieved through compositional design using a combination of chemical substitution with a donor dopant and adjustment of the zirconium to titanium compositional ratio to meet the morphotropic phase boundary (MPB). In this work, a different route to large piezoelectricity is demonstrated. Results reveal unexpectedly high piezoelectric coefficients at elevated temperatures and compositions far from the MPB. At temperatures near the Curie point, doping with 2 at% Sm results in exceptionally large piezoelectric coefficients of up to 915 pm/V. This value is approximately twice those of other donor dopants (e.g., 477 pm/V for Nb and 435 pm/V for La). Structural changes during the phase transitions of Sm-doped PZT show a pseudo-cubic phase forming ≈50 °C below the Curie temperature. Possible origins of these effects are discussed and the high piezoelectricity is posited to be due to extrinsic effects. The enhancement of the mechanism at elevated temperatures is attributed to the coexistence of tetragonal and pseudo-cubic phases, which enables strain accommodation during electromechanical deformation and interphase boundary motion. This work provides insight into possible routes for designing high performance piezoelectrics which are alternatives to traditional methods relying on MPB compositions.

  1. Power harvesting using PZT ceramics embedded in orthopedic implants.

    Science.gov (United States)

    Chen, Hong; Liu, Ming; Jia, Chen; Wang, Zihua

    2009-09-01

    Battery lifetime has been the stumbling block for many power-critical or maintenance-free real-time embedded applications, such as wireless sensors and orthopedic implants. Thus a piezoelectric material that could convert human motion into electrical energy provides a very attractive solution for clinical implants. In this work, we analyze the power generation characteristics of stiff lead zirconate titanate (PZT) ceramics and the equivalent circuit through extensive experiments. Our experimental framework allows us to explore many important design considerations of such a PZT-based power generator. Overall we can achieve a PZT element volume of 0.5 x 0.5 x 1.8 cm, which is considerably smaller than the results reported so far. Finally, we outline the application of our PZT elements in a total knee replacement (TKR) implant.

  2. High-temperature mechanical properties of a uniaxially reinforced zircon-silicon carbide composite

    International Nuclear Information System (INIS)

    Singh, R.N.

    1990-01-01

    This paper reports that mechanical properties of a monolithic zircon ceramic and zircon-matrix composites uniaxially reinforced with either uncoated or BN-coated silicon carbide monofilaments were measured in flexure between 25 degrees and 1477 degrees C. Monolithic zircon ceramics were weak and exhibited a brittle failure up to abut 1300 degrees C. An increasing amount of the plastic deformation was observed before failure above about 1300 degrees C. In contrast, composites reinforced with either uncoated or BN-coated Sic filaments were stronger and tougher than the monolithic zircon at all test temperatures between 25 degrees and 1477 degrees. The ultimate strength and work-of-fracture of composite samples decreased with increasing temperature. A transgranular matrix fracture was shown by the monolithic and composite samples tested up to about 1200 degrees C, whereas an increasing amount of the intergranular matrix fracture was displayed above 1200 degrees C

  3. Analyze of viability of ZrSiO_4-Fe_2O_3 pigments synthesis, from decomposition of the zircon

    International Nuclear Information System (INIS)

    Prim, S.R.; Folgueiras, M.V.; Winter, D.M.

    2011-01-01

    Zircon pigments are commonly used in ceramic industry due to their high chemical and thermal stability. In the present work, the viability of synthesis of a zircon ceramic pigment from intermediate products obtained from decomposition zircon sand with NaOH and/or KOH at 750 and 850 °C was studied. The intermediate products were used as raw materials to produce pigments. Iron oxide from rolling process of sheet metal was used as chromophore. The crystalline phases formed were characterized by X-ray diffraction. The results have shown that it was possible to obtain the partial decomposition of zircon which enables the development of the synthesis of zircon pigment. (author)

  4. Transverse piezoelectric coefficient measurement of flexible lead zirconate titanate thin films

    Energy Technology Data Exchange (ETDEWEB)

    Dufay, T.; Guiffard, B.; Seveno, R. [LUNAM Université, Université de Nantes, IETR (Institut d' Électronique et de Télécommunications de Rennes), UMR CNRS 6164, 2 rue de la Houssinière, BP 92208, 44322 Nantes Cedex 3 (France); Thomas, J.-C. [LUNAM Université, Université de Nantes-École Centrale Nantes, GeM (Institut de Recherche en Génie Civil et Ingénierie Mécanique), UMR CNRS 6183, 2 rue de la Houssinière, BP 92208, 44322 Nantes Cedex 3 (France)

    2015-05-28

    Highly flexible lead zirconate titanate, Pb(Zr,Ti)O{sub 3} (PZT), thin films have been realized by modified sol-gel process. The transverse piezoelectric coefficient d{sub 31} was determined from the tip displacement of bending-mode actuators made of PZT cantilever deposited onto bare or RuO{sub 2} coated aluminium substrate (16 μm thick). The influence of the thickness of ruthenium dioxide RuO{sub 2} and PZT layers was investigated for Pb(Zr{sub 0.57}Ti{sub 0.43})O{sub 3}. The modification of Zr/Ti ratio from 40/60 to 60/40 was done for 3 μm thick PZT thin films onto aluminium (Al) and Al/RuO{sub 2} substrates. A laser vibrometer was used to measure the beam displacement under controlled electric field. The experimental results were fitted in order to find the piezoelectric coefficient. Very large tip deflections of about 1 mm under low voltage (∼8 V) were measured for every cantilevers at the resonance frequency (∼180 Hz). For a given Zr/Ti ratio of 58/42, it was found that the addition of a 40 nm thick RuO{sub 2} interfacial layer between the aluminium substrate and the PZT layer induces a remarkable increase of the d{sub 31} coefficient by a factor of 2.7, thus corresponding to a maximal d{sub 31} value of 33 pC/N. These results make the recently developed PZT/Al thin films very attractive for both low frequency bending mode actuating applications and vibrating energy harvesting.

  5. Bath temperature effect on magnetoelectric performance of Ni-lead zirconate titanate-Ni laminated composites synthesized by electroless deposition

    Energy Technology Data Exchange (ETDEWEB)

    Wu, W. [College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016 (China); Wang, Y.G., E-mail: yingang.wang@nuaa.edu.c [College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016 (China); Bi, K. [College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016 (China)

    2011-03-15

    Magnetoelectric (ME) Ni-lead zirconate titanate-Ni laminated composites have been prepared by electroless deposition at various bath temperatures. The structure of the Ni layers deposited at various bath temperatures was characterized by X-ray diffraction, and microstructures were investigated by transmission electron microscopy. The magnetostrictive coefficients were measured by means of a resistance strain gauge. The transverse ME voltage coefficient {alpha}{sub E,31} was measured with the magnetic field applied parallel to the sample plane. The deposition rate of Ni increases with bath temperature. Ni layer with smaller grain size is obtained at higher bath temperature and shows higher piezomagnetic coefficient, promoting the ME effect of corresponding laminated composites. It is advantageous to increase the bath temperature, while trying to avoid the breaking of bath constituents. - Research Highlights: Laminated composites without interlayer are prepared by electroless deposition. Bath temperature affects the grain size of the deposited Ni layers. Higher bath temperature is beneficial to obtain stronger ME response.

  6. Coaxial Transducer

    National Research Council Canada - National Science Library

    Ruffa, Anthony A

    2008-01-01

    The invention as disclosed is of a coaxial transducer that uses lead zirconate titanate ceramic or other suitable material as an isolator between the conductors in a coaxial cable to transmit acoustic...

  7. Bulletin of Materials Science | Indian Academy of Sciences

    Indian Academy of Sciences (India)

    Home; Journals; Bulletin of Materials Science. D K Kharat. Articles written in Bulletin of Materials Science. Volume 28 Issue 5 August 2005 pp 453-455 Ceramics and Glasses. Characterization and microstructure of porous lead zirconate titanate ceramics · B Praveenkumar H H Kumar D K Kharat · More Details Abstract ...

  8. Anion and cation diffusion in barium titanate and strontium titanate; Anionen- und Kationendiffusion in Barium- und Strontiumtitanat

    Energy Technology Data Exchange (ETDEWEB)

    Kessel, Markus Franz

    2012-12-19

    Perovskite oxides show various interesting properties providing several technical applications. In many cases the defect chemistry is the key to understand and influence the material's properties. In this work the defect chemistry of barium titanate and strontium titanate is analysed by anion and cation diffusion experiments and subsequent time-of-flight secondary ion mass spectrometry (ToF-SIMS). The reoxidation equation for barium titanate used in multi-layer ceramic capacitors (MLCCs) is found out by a combination of different isotope exchange experiments and the analysis of the resulting tracer diffusion profiles. It is shown that the incorporation of oxygen from water vapour is faster by orders of magnitude than from molecular oxygen. Chemical analysis shows the samples contain various dopants leading to a complex defect chemistry. Dysprosium is the most important dopant, acting partially as a donor and partially as an acceptor in this effectively acceptor-doped material. TEM and EELS analysis show the inhomogeneous distribution of Dy in a core-shell microstructure. The oxygen partial pressure and temperature dependence of the oxygen tracer diffusion coefficients is analysed and explained by the complex defect chemistry of Dy-doped barium titanate. Additional fast diffusion profiles are attributed to fast diffusion along grain boundaries. In addition to the barium titanate ceramics from an important technical application, oxygen diffusion in cubic, nominally undoped BaTiO{sub 3} single crystals has been studied by means of {sup 18}O{sub 2}/{sup 16}O{sub 2} isotope exchange annealing and subsequent determination of the isotope profiles in the solid by ToF-SIMS. It is shown that a correct description of the diffusion profiles requires the analysis of the diffusion through the surface space-charge into the material's bulk. Surface exchange coefficients, space-charge potentials and bulk diffusion coefficients are analysed as a function of oxygen partial

  9. The temperature dependences of electromechanical properties of PLZT ceramics

    Science.gov (United States)

    Czerwiec, M.; Zachariasz, R.; Ilczuk, J.

    2008-02-01

    The mechanical and electrical properties in lanthanum modified lead zirconate-titanate ceramics of 5/50/50 and 10/50/50 were studied by mechanical loss Q - 1, Young's modulus E, electric permittivity ɛ and tangent of dielectric loss of angle tgδ measurements. The internal friction Q - 1 and Young modulus E measured from 290 K to 600 K shows that Curie temperature TC is located at 574 K and 435 K (1st cycle of heating) respectively for ceramic samples 5/50/50 and 10/50/50. The movement of TC in second cycle of heating to lower temperature (561 K for 5/50/50 and 420 K for 10/50/50) has been observed. Together with Q - 1 and E measurements, temperature dependences of ɛ=f(T) and tgδ=f(T) were determinated in temperature range from 300 K to 730 K. The values of TC obtained during ɛ and tgδ measurements were respectively: 560 K for 5/50/50 and 419 K for 10/50/50. These temperatures are almost as high as the temperatures obtained by internal friction Q - 1 measurements in second cycle of heating. In ceramic sample 10/50/50 the additional maximum on internal friction Q - 1 curve at the temperature 316 K was observed.

  10. Fabrication and energy harvesting characteristics of unimorph piezoelectric cantilever generators with interdigitated electrode lead zirconate titanate laminates

    Science.gov (United States)

    Lee, Min-seon; Yun, Ji-sun; Park, Woon-ik; Hong, Youn-woo; Cho, Jeong-ho; Paik, Jong-hoo; Park, Yong Ho; Son, Chun-myung; Jeong, Young Hun

    2017-12-01

    Interdigitated electrode (IDE) unimorph piezoelectric cantilever generators (UPCGs) were fabricated and their energy harvesting characteristics were investigated. A hard lead zirconate titanate (PZT) material with a high mechanical quality factor (Q m) of 1280 was used for the active piezoelectric film of the IDE UPCGs. Two different laminated IDE UPCGs were prepared; one has Ag/Pd interdigitated electrode (IDE) formed only on the top and bottom PZT sheets (D-IDE), while the other has Ag/Pd IDE on all of the PZT sheets (M-IDE). Cofiring was conducted at 1050 °C for 2 h for PZT laminates with IDEs. The fabricated IDE UPCGs exhibited power densities of 50.4 µW/cm3 for the D-IDE and 820 µW/cm3 for the M-IDE. The UPCG with the M-IDE exhibited a higher performance than that with the D-IDE. Specifically, a significantly enhanced normalized power factor of 670 µW/(g2·cm3) was found at 118 Hz across 100 kΩ.

  11. Ceria and strontium titanate based electrodes

    DEFF Research Database (Denmark)

    2010-01-01

    A ceramic anode structure obtainable by a process comprising the steps of: (a) providing a slurry by dispersing a powder of an electronically conductive phase and by adding a binder to the dispersion, in which said powder is selected from the group consisting of niobium-doped strontium titanate......, vanadium-doped strontium titanate, tantalum-doped strontium titanate, and mixtures thereof, (b) sintering the slurry of step (a), (c) providing a precursor solution of ceria, said solution containing a solvent and a surfactant, (d) impregnating the resulting sintered structure of step (b...

  12. Study of samarium modified lead zirconate titanate and nickel zinc ferrite composite system

    Energy Technology Data Exchange (ETDEWEB)

    Rani, Rekha [Department of Physics, SD PG College, Panipat 132103 (India); School of Physics and Materials Science, Thapar University, Patiala 147004 (India); Juneja, J.K., E-mail: jk_juneja@yahoo.com [Department of Physics, Hindu College, Sonepat 131001 (India); Singh, Sangeeta [Department of Physics, GVM Girls College, Sonepat 131001 (India); Raina, K.K. [School of Physics and Materials Science, Thapar University, Patiala 147004 (India); Prakash, Chandra [Solid State Physics Laboratory, Timarpur, Delhi 110054 (India)

    2015-03-15

    In the present work, composites of samarium substituted lead zirconate titanate and nickel zinc ferrite with compositional formula 0.95Pb{sub 1−3x/2} Sm{sub x}Zr{sub 0.65}Ti{sub 0.35}O{sub 3}–0.05Ni{sub 0.8}Zn{sub 0.2}Fe{sub 2}O{sub 4} (x=0, 0.01, 0.02 and 0.03) were prepared by the conventional solid state route. X-ray diffraction analysis was carried out to confirm the coexistence of individual phases. Microstructural study was done by using scanning electron microscope. Dielectric constant and loss were studied as a function of temperature and frequency. To study ferroelectric and magnetic properties of the composite samples, corresponding P–E and M–H hysteresis loops were recorded. Change in magnetic properties of electrically poled composite sample (x=0.02) was studied to confirm the magnetoelectric (ME) coupling. ME coefficient (dE/dH) of the samples (x=0 and 0.02) was measured as a function of DC magnetic field. - Highlights: • We are reporting the effect of Sm substitution on PZT–NiZn ferrite composites. • Observation of both P–E and M–H loops confirms ferroelectric and magnetic ordering. • With Sm substitution, significant improvement in properties was observed. • Increase in magnetization for electrically poled sample is evidence of ME coupling. • Electric polarization is generated by applying magnetic field.

  13. Characterization and microstructure of porous lead zirconate titanate ...

    Indian Academy of Sciences (India)

    Unknown

    need to have porous piezoelectric materials. These can be made by combining a PZT ceramic with a passive polymer or air phase. These materials greatly extend the range of properties offered by conventional PZT ceramics. More- over, porosity in the materials could reduce the effective acoustical impedance leading to an ...

  14. Design, Modeling and Optimization of a Piezoelectric Pressure Sensor based on a Thin-Film PZT Membrane Containing Nanocrystalline Powders

    Directory of Open Access Journals (Sweden)

    Vahid MOHAMMADI

    2009-11-01

    Full Text Available In this paper fabrication of a 0-3 ceramic/ceramic composite lead zirconate titanate, Pb(Zr0.52Ti0.48O3 thin film has been presented and then a pressure sensor based on multilayer thin-film PZT diaphragm contain of Lead Zirconate Titanate nanocrystalline powders was designed, modeled and optimized. Dynamics characteristics of this multilayer diaphragm have been investigated by ANSYS® FE software. By this simulation the effective parameters of the multilayer PZT diaphragm for improving the performance of a pressure sensor in different ranges of pressure are optimized. The optimized thickness ratio of PZT layer to SiO2 was given in the paper to obtain the maximum deflection of the multilayer thin-film PZT diaphragm. A 0-3 ceramic/ceramic composite lead zirconate titanate, Pb(Zr0.52Ti0.48O3 film has been developed to fabricate the pressure sensor by a hybrid sol gel process. PZT nanopowders fabricated via conventional sol gel method and uniformly dispersed in PZT precursor solution by an attrition mill. XRD analysis shows that perovskite structure would be formed due to the presence of a significant amount of ceramic nanopowders. This texture has a good effect on piezoelectric properties of perovskite structure. The film forms a strongly bonded network and less shrinkage occurs, so the films do not crack during process. Also the aspect ratio through this process would be increased. SEM micrographs indicated that PZT films were uniform, crack free and have a composite microstructure and a piezoelectric coefficient d31 of -40 pC.N-1 and d33 ranged from 50pm.N-1 to 60pm.N-1.

  15. Crystallization of sol-gel derived lead zirconate titanate thin films in argon and oxygen atmospheres

    Energy Technology Data Exchange (ETDEWEB)

    Bursill, L A [Melbourne Univ., Parkville, VIC (Australia). School of Physics; Brooks, K G [Ecole Polytechnique Federale, Lausanne (Switzerland)

    1994-12-31

    Electron diffraction and high-resolution electron microscopic techniques are applied to reveal the mechanisms of crystallization of 75 nm thin films of ferroelectric lead-zirconate-titanate (PZT). Sol-gel methods, followed by pyrolysis at 350 deg C, were used to provide a common starting point after which a variety of rapid-thermal annealing (RTA) experiments in the temperature range 400-700 deg C were made in argon, oxygen and nitrogen/hydrogen atmospheres. The results are interpreted in terms of the crystal chemical analysis, which points out that partial pressure of oxygen and heating rate are important experimental parameters which must be controlled if ferroelectric perovskite-type Pb{sub 2}ZrTiO{sub 6}, rather than pyrochlore-type Pb{sub 2}ZrTiO{sub 6+x}, where O < X < 1 or -1 < X < O, is to be obtained after the RTA step. Thus significant improvements in the crystallization of perovskite-type PZT were clearly demonstrated by using argon atmospheres for the RTA step. The results have significance for the production of high-quality ferroelectric thin films, with improved switching and fatigue characteristics, since even small amounts of the pyrochlore phase prove detrimental for these properties. 18 refs., 1 tab., 10 figs.

  16. Wafer scale lead zirconate titanate film preparation by sol-gel method using stress balance layer

    International Nuclear Information System (INIS)

    Lu Jian; Kobayashi, Takeshi; Yi Zhang; Maeda, Ryutaro; Mihara, Takashi

    2006-01-01

    In this paper, platinum/titanium (Pt/Ti) film was introduced as a residual stress balance layer into wafer scale thick lead zirconate titanate (PZT) film fabrication by sol-gel method. The stress developing in PZT film's bottom electrode as well as in PZT film itself during deposition were analyzed; the wafer curvatures, PZT crystallizations and PZT electric properties before and after using Pt/Ti stress balance layer were studied and compared. It was found that this layer is effective to balance the residual stress in PZT film's bottom electrode induced by thermal expansion coefficient mismatch and Ti diffusion, thus can notably reduce the curvature of 4-in. wafer from - 40.5 μm to - 12.9 μm after PZT film deposition. This stress balance layer was also found effective to avoid the PZT film cracking even when annealed by rapid thermal annealing with heating-rate up to 10.5 deg. C/s. According to X-ray diffraction analysis and electric properties characterization, crack-free uniform 1-μm-thick PZT film with preferred pervoskite (001) orientation, excellent dielectric constant, as high as 1310, and excellent remanent polarization, as high as 39.8 μC/cm 2 , can be obtained on 4-in. wafer

  17. Thickness effect on the structure, grain size, and local piezoresponse of self-polarized lead lanthanum zirconate titanate thin films

    Energy Technology Data Exchange (ETDEWEB)

    Melo, M.; Araújo, E. B., E-mail: eudes@dfq.feis.unesp.br [Departamento de Física e Química, Faculdade de Engenharia de Ilha Solteira, UNESP—Univ. Estadual Paulista, 15385-000 Ilha Solteira, SP (Brazil); Shvartsman, V. V. [Institute for Materials Science, University Duisburg-Essen, 45141 Essen (Germany); Shur, V. Ya. [Institute of Natural Sciences, Ural Federal University, 620000 Ekaterinburg (Russian Federation); Kholkin, A. L. [Institute of Natural Sciences, Ural Federal University, 620000 Ekaterinburg (Russian Federation); Department of Physics and CICECO—Aveiro Institute of Materials, University of Aveiro, 3810-193 Aveiro (Portugal)

    2016-08-07

    Polycrystalline lanthanum lead zirconate titanate (PLZT) thin films were deposited on Pt/TiO{sub 2}/SiO{sub 2}/Si substrates to study the effects of the thickness and grain size on their structural and piezoresponse properties at nanoscale. Thinner PLZT films show a slight (100)-orientation tendency that tends to random orientation for the thicker film, while microstrain and crystallite size increases almost linearly with increasing thickness. Piezoresponse force microscopy and autocorrelation function technique were used to demonstrate the existence of local self-polarization effect and to study the thickness dependence of correlation length. The obtained results ruled out the bulk mechanisms and suggest that Schottky barriers near the film-substrate are likely responsible for a build-in electric field in the films. Larger correlation length evidence that this build-in field increases the number of coexisting polarization directions in larger grains leading to an alignment of macrodomains in thinner films.

  18. Three-degree-of-freedom ultrasonic motor using a 5-mm-diameter piezoelectric ceramic tube.

    Science.gov (United States)

    Mingsen Guo; Junhui Hu; Hua Zhu; Chunsheng Zhao; Shuxiang Dong

    2013-07-01

    A small three-degree-of-freedom ultrasonic motor has been developed using a simple piezoelectric lead zirconate titanate (PZT)-tube stator (OD 5 mm, ID 3 mm, length 15 mm). The stator drives a ball-rotor into rotational motion around one of three orthogonal (x-, y-, and z-) axes by combing the first longitudinal and second bending vibration modes. A motor prototype was fabricated and characterized; its performance was superior to those of previous motors made with a PZT ceramic/metal composite stator of comparable size. The method for further improving the performance was discussed. The motor can be further miniaturized and it has potential to be applied to medical microrobots, endoscopes or micro laparoscopic devices, and cell manipulation devices.

  19. Process for fabricating mixed-oxide powders

    International Nuclear Information System (INIS)

    Elmaleh, D.; Giraudel, A.

    1975-01-01

    A physical-chemical process for fabricating homogeneous powders suitable for sintering is described. It can be applied to the synthesis of all mixed oxides having mutually compatible and water soluble salts. As a specific example, the fabrication of lead titanate-zirconate powders used to make hot pressed ceramics is described. These ceramics show improved piezoelectric properties [fr

  20. Recent developments in piezoelectric ceramic materials and deterioration of their properties

    International Nuclear Information System (INIS)

    Pasha, R.A.; Khan, M.Z.

    2006-01-01

    There has been growing interest in recent years in piezoelectric ceramic materials because of their excellent dielectric, sensing, actuating and efficient process control applications. Lead Zirconate Titanate (PZT), Barium Titanate (BaTi O/sub 3/) and Lead Metaniobate (PbNb/sub 2/ O/sub 6/) and PVDF Polymers and generally favored as smart sensing materials. These materials are being used in critical engineering systems and smart structure. Fatigue failure due to electrical and thermal shocking is a major issue in degradation of these materials. Lot of work has been done in this area but still various issues need to investigate. Recent developments and current issues in piezoelectric materials and deterioration of their properties in different working conditions are discussed. The development of Finite Element codes incorporating smart material element has provided an opportunity to solve some practical problems. The new piezoelectric finite element capability available in some commercial package like ANSYS makes it convenient to perform static dynamic and thermal analysis for the fully coupled piezoelectric and structural response. Researchers have a great scope to uncover the various properties of these smart materials in different environmental conditions. In present work an overall review of the title is presented. (author)

  1. Improved dielectric and ferroelectric properties of Mn doped barium zirconium titanate (BZT) ceramics for energy storage applications

    Science.gov (United States)

    Sangwan, Kanta Maan; Ahlawat, Neetu; Kundu, R. S.; Rani, Suman; Rani, Sunita; Ahlawat, Navneet; Murugavel, Sevi

    2018-06-01

    Lead free Mn doped barium zirconium titanate ceramic of composition BaZr0.045 (MnxTi1-x)0.955O3 (x = 0.00, 0.01, 0.02) were prepared by solid state reaction method. Tetragonal perovskite structure was confirmed by Rietveld refinement of X-ray diffraction pattern. Analysis of Scanning electron microscope (SEM) micrographs revealed that addition of Mn up to a certain limit accelerates grain growth of BZT ceramic. Static dielectric constant was successfully extended up to high frequencies with an appreciable decrease in dielectric loss about 70% for Mn doped BZT ceramics. The experimental data fitted with Curie Weiss Law and Power Law confirmed first order transition and diffusive behavior of the investigated system. The shifting of Curie temperature (Tc) from 387 K to 402 K indicated tendency for sustained ferroelectricity in doped BZMT ceramics. High value of percentage temperature coefficient of capacitance TCC >10% near Tc was observed for all the compositions and increases with Mn content in pure BZT. At room temperature, BZT modified ceramic corresponding to x = 0.01 composition shows better values of remnant polarization (Pr = 5.718 μC/cm2), saturation polarization (Ps = 14.410 μC/cm2), low coercive field (Ec = 0.612 kV/cm), and highest value of Pr/Ps = 0.396.

  2. Study of the microstructure and the hardness of PZT piezoelectric ceramics types I and III used in electro acoustic transducers; Estudo da microestrutura e da microdureza das ceramicas piezoeletricas tipos PZT I e III utilizadas em transdutores eletroacusticos

    Energy Technology Data Exchange (ETDEWEB)

    Cabral, Ricardo de Freitas; Itaboray, Lucas Mendes; Santos, Anna Paula de Oliveira [Centro Universitario de Volta Redonda (UNIFOA), Volta Redonda, RJ (Brazil)

    2015-12-15

    The field of electronic processing of the ceramic piezoelectric type imported powdered led to the production of ceramics with 97% of theoretical density, homogeneous microstructure with great potential for applications in piezoelectric devices such as electro acoustic transducers. However, the production of electronic ceramics National piezoelectric type is not yet able to have as raw material zirconate titanate Lead (PZT) 100% made in Brazil. Thus, this is used for supply of domestic production, the zirconium oxide. In this work, both post PZT types I and III, imported, were uniaxially pressed at 70 MPa and sintered at 1200 and 1250 deg C for 3 hours. Hardness measurements were performed by micro indentation, X-ray diffraction analysis and Scanning Electron Microscopy. The hardness of PZT I was 393 HV. (author)

  3. Mechanical properties of porous PNZT polycrystalline ceramics

    International Nuclear Information System (INIS)

    Biswas, D.R.; Fulrath, R.M.

    1977-08-01

    Niobium-doped lead zirconate-titanate (PNZT) was used to investigate the effect of porosity on the mechanical properties of a polycrystalline ceramic. Spherical pores (110 to 150 μm diameter) were introduced by using organic materials in the initial specimen fabrication. The matrix grain size (2 to 5 μm) was kept constant. Small pores (2 to 3 μm diameter) of the order of the grain size were formed by varying the sintering conditions. The effect of porosity on strength was predicted quite well by Weibull's probabilistic approach. The Young's modulus showed a linear relationship with increase in porosity. A decrease in fracture toughness with increase in porosity was also observed. It was found that at equivalent porosities, small pore specimens gave higher strength, Young's modulus and fracture toughness compared to specimens containing large pores. Fracture surface analysis, by scanning electron microscopy, showed fracture originated either at the tensile surface or at the edge of the specimen

  4. Effect of donor and acceptor dopants on crystallization, microstructural and dielectric behaviors of barium strontium titanate glass ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Yadav, Avadhesh Kumar, E-mail: yadav.av11@gmail.com [Department of Physics, Dr. Bheem Rao Ambedkar Government Degree College, Anaugi, Kannauj (India); Gautam, C.R. [Department of Physics, University of Lucknow, Lucknow 226007 (India); Singh, Prabhakar [Department of Physics, Indian Institute of Technology (Banaras Hindu University), Varanasi 221005 (India)

    2016-07-05

    Bulk transparent barium strontium titanate borosilicate glasses in glass system (65-x)[(Ba{sub 0.6}Sr{sub 0.4}).TiO{sub 3}]-30[2SiO{sub 2}.B{sub 2}O{sub 3}]-5[K{sub 2}O]-x[A{sub 2}O{sub 3}], A = La, Fe (x = 2, 5 and 10) were prepared by rapid melt-quench technique and subsequently, converted into glass ceramics by regulated heat treatment process. The phase identification was carried out by X-ray powder diffraction and their surface morphology was studied by scanning electron microscopy. The dielectric properties were studied by impedance spectroscopic technique. Investigated glass samples were crystallized into major and secondary phases of Ba{sub 1.91}Sr{sub 0.09}TiO{sub 4} and Ba{sub 2}TiSi{sub 2}O{sub 8}, respectively. A very high dielectric constant having value upto 68000 was found in glass ceramic sample BST5K10F. This high value of dielectric constant was attributed to interfacial polarization, which arose due to conductivity difference among semiconducting crystalline phases, conducting grains and insulating grain boundaries. Donor dopant La{sub 2}O{sub 3} and acceptor dopant Fe{sub 2}O{sub 3} play an important role for enhancing crystallization, dielectric constant and retardation of dielectric loss in the samples. Moreover, higher value of dielectric constant and lower value of dielectric loss was found in Fe{sub 2}O{sub 3} doped samples in comparison to La{sub 2}O{sub 3} doped samples. - Highlights: • Bulk transparent barium strontium titanate glasses are successfully prepared. • A very high dielectric constant upto 68000 was found in glass ceramics. • La{sub 2}O{sub 3} and Fe{sub 2}O{sub 3} play role for enhancing value of dielectric constant. • Higher dielectric constant with low dielectric loss was found in Fe{sub 2}O{sub 3} doped sample. • Such glass ceramics may be used in making capacitors for high energy storage.

  5. Structural and dielectric characterization of praseodymium-modified lead titanate ceramics synthesized by the OPM route

    Energy Technology Data Exchange (ETDEWEB)

    Pinto, Alexandre H., E-mail: alehp1@yahoo.com.br [LIEC-Laboratorio Interdisciplinar de Eletroquimica e Ceramica, Department of Chemistry, UFSCar-Federal University of Sao Carlos, Rod. Washington Luis km 235, CP 676, Sao Carlos 13565-905, SP (Brazil); Souza, Flavio L., E-mail: fleandro.ufabc@gmail.com [Centro de Ciencias Naturais e Humanas, UFABC - Universidade Federal do ABC, Santo Andre 09210-170, SP (Brazil); Longo, Elson, E-mail: elson@iq.unesp.br [Department of Biochemistry, Chemistry Institute of Araraquara, UNESP - Sao Paulo State University, Rua Francisco Degni, CP 355, Araraquara 14801-907, SP (Brazil); Leite, Edson R., E-mail: derl@power.ufscar.br [LIEC-Laboratorio Interdisciplinar de Eletroquimica e Ceramica, Department of Chemistry, UFSCar-Federal University of Sao Carlos, Rod. Washington Luis km 235, CP 676, Sao Carlos 13565-905, SP (Brazil); Camargo, Emerson R., E-mail: camargo@ufscar.br [LIEC-Laboratorio Interdisciplinar de Eletroquimica e Ceramica, Department of Chemistry, UFSCar-Federal University of Sao Carlos, Rod. Washington Luis km 235, CP 676, Sao Carlos 13565-905, SP (Brazil)

    2011-10-17

    Highlights: {yields} Highly reactive nanosized powders of Pb(0.8)Pr(0.2)TiO(3) were obtained by the OPM route. {yields} Tetragonal phase was observed by X-ray diffraction and confirmed by Raman spectroscopy. {yields} SEM images showed powders partially sintered with particles of approximately 54 nm. {yields} Dielectric measurements show a normal behavior for the ferroelectric to paraelectric transition. - Abstract: Quasi-spherical nanoparticles of praseodymium-modified lead titanate powder (Pb{sub 0.80}Pr{sub 0.20}TiO{sub 3}) with an average size of 54.8 nm were synthesized successfully by the oxidant-peroxo method (OPM) and were used to prepare highly dense ceramic bodies which were sintered at 1100 and 1150 deg. C for 2 h. A tetragonal phase was identified in the powder and ceramic samples by X-ray powder diffraction and FT-Raman spectroscopy at room temperature. The fractured surface of the ceramic sample showed a high degree of densification with fairly uniform grain sizes. Dielectric constants measured in the range of 30-300 deg. C at different frequencies (120 Hz and at 1, 10 and 100 kHz) indicated that samples with 20 mol% praseodymium showed normal ferroelectric behavior regardless of the sintering temperature.

  6. Structural and dielectric characterization of praseodymium-modified lead titanate ceramics synthesized by the OPM route

    International Nuclear Information System (INIS)

    Pinto, Alexandre H.; Souza, Flavio L.; Longo, Elson; Leite, Edson R.; Camargo, Emerson R.

    2011-01-01

    Highlights: → Highly reactive nanosized powders of Pb(0.8)Pr(0.2)TiO(3) were obtained by the OPM route. → Tetragonal phase was observed by X-ray diffraction and confirmed by Raman spectroscopy. → SEM images showed powders partially sintered with particles of approximately 54 nm. → Dielectric measurements show a normal behavior for the ferroelectric to paraelectric transition. - Abstract: Quasi-spherical nanoparticles of praseodymium-modified lead titanate powder (Pb 0.80 Pr 0.20 TiO 3 ) with an average size of 54.8 nm were synthesized successfully by the oxidant-peroxo method (OPM) and were used to prepare highly dense ceramic bodies which were sintered at 1100 and 1150 deg. C for 2 h. A tetragonal phase was identified in the powder and ceramic samples by X-ray powder diffraction and FT-Raman spectroscopy at room temperature. The fractured surface of the ceramic sample showed a high degree of densification with fairly uniform grain sizes. Dielectric constants measured in the range of 30-300 deg. C at different frequencies (120 Hz and at 1, 10 and 100 kHz) indicated that samples with 20 mol% praseodymium showed normal ferroelectric behavior regardless of the sintering temperature.

  7. Effect of multi-layered bottom electrodes on the orientation of strontium-doped lead zirconate titanate thin films

    Energy Technology Data Exchange (ETDEWEB)

    Bhaskaran, M. [Microelectronics and Materials Technology Centre, School of Electrical and Computer Engineering, RMIT University, GPO Box 2476V, Melbourne, Victoria 3001 (Australia)], E-mail: madhu.bhaskaran@gmail.com; Sriram, S. [Microelectronics and Materials Technology Centre, School of Electrical and Computer Engineering, RMIT University, GPO Box 2476V, Melbourne, Victoria 3001 (Australia); Mitchell, D.R.G.; Short, K.T. [Institute of Materials Engineering, Australian Nuclear Science and Technology Organisation (ANSTO), PMB 1, Menai, New South Wales 2234 (Australia); Holland, A.S. [Microelectronics and Materials Technology Centre, School of Electrical and Computer Engineering, RMIT University, GPO Box 2476V, Melbourne, Victoria 3001 (Australia)

    2008-09-30

    This article discusses the results from X-ray diffraction (XRD) analysis of piezoelectric strontium-doped lead zirconate titanate (PSZT) thin films deposited on multi-layer coatings on silicon. The films were deposited by RF magnetron sputtering on a metal coated substrate. The aim was to exploit the pronounced piezoelectric effect that is theoretically expected normal to the substrate. This work highlighted the influence that the bottom electrode architecture exerts on the final crystalline orientation of the deposited thin films. A number of bottom electrode architectures were used, with the uppermost metal layer on which PSZT was deposited being gold or platinum. The XRD analysis revealed that the unit cell of the PSZT thin films deposited on gold and on platinum were deformed, relative to expected unit cell dimensions. Experimental results have been used to estimate the unit cell parameters. The XRD results were then indexed based on these unit cell parameters. The choice and the thickness of the intermediate adhesion layers influenced the relative intensity, and in some cases, the presence of perovskite peaks. In some cases, undesirable reactions between the bottom electrode layers were observed, and layer architectures to overcome these reactions are also discussed.

  8. Thermo-mechanical properties of mullite/zirconia reinforced alumina ceramic composites

    International Nuclear Information System (INIS)

    Wahsh, M.M.S.; Khattab, R.M.; Awaad, M.

    2012-01-01

    Highlights: ► Alumina–mullite–zirconia ceramic composites were prepared from alumina and zircon. ► Constant amount of magnesia was added as a sintering aid. ► Mechanical properties were enhanced with increasing of zircon up to 30.52 mass%. ► All of ceramic composites were achieved excellent thermal shock resistance. -- Abstract: Alumina–mullite–zirconia ceramic composites were prepared by reaction bonding of alumina and zircon mixtures after firing at different temperatures 1300°, 1400° and 1500 °C. Constant amount of magnesia was added as a sintering aid. The technological parameters of the sintered ceramic composites, i.e. the mechanical properties and densification parameter as well as thermal shock resistance, have been investigated. The phase compositions and microstructure of the sintered ceramic composites were detected by using X-ray diffraction (XRD) and scanning electron microscopy (SEM). Results indicated that alumina–mullite–zirconia ceramic composites fired at 1500 °C for 2 h were achieved a good densification parameters and mechanical properties as well as excellent thermal shock resistance. In addition, these ceramic composites were showed enhancement in Vickers’ microhardness and fracture toughness values.

  9. Towards a digital sound reconstruction MEMS device: Characterization of a single PZT based piezoelectric actuator

    KAUST Repository

    Carreno, Armando Arpys Arevalo; Conchouso Gonzalez, David; Castro, David; Jaber, Nizar; Younis, Mohammad I.; Foulds, Ian G.

    2015-01-01

    of acoustic actuators. These actuators consist of a flexible membrane fabricated using polyimide, which is actuated using a Lead-Zirconate-Titanate (PZT) piezoelectric ceramic layer working in the d31 actuation mode. The dimensions of the membrane are of 1mm

  10. Bulletin of Materials Science | Indian Academy of Sciences

    Indian Academy of Sciences (India)

    The effect of temperature on polarization reversal of strontium-doped lead zirconate titanate ceramics was studied. The piezoelectric properties viz. dielectric constant and piezoelectric coupling coefficient, were used for polarization reversal characteristic. These properties and apparent coercive field weremeasured during ...

  11. Ionic and electronic conductivity in lead-zirconate-titanate (PZT)

    NARCIS (Netherlands)

    Boukamp, Bernard A.; Pham thi ngoc mai, P.T.N.M.; Blank, David H.A.; Bouwmeester, Henricus J.M.

    2004-01-01

    Accurate impedance measurements on differently sized samples of lead–zirconate–titanate (PbZr0.53Ti0.47O3, PZT) have been analyzed with a CNLS procedure, resulting in the separation of the ionic and electronic conductivities over a temperature range from f150 to 630 jC. At 603 jC the electronic

  12. History and challenges of barium titanate: Part I

    Directory of Open Access Journals (Sweden)

    Vijatović M.M.

    2008-01-01

    Full Text Available Barium titanate is the first ferroelectric ceramics and a good candidate for a variety of applications due to its excellent dielectric, ferroelectric and piezoelectric properties. Barium titanate is a member of a large family of compounds with the general formula ABO3 called perovskites. Barium titanate can be prepared using different methods. The synthesis method depends on the desired characteristics for the end application. The used method has a significant influence on the structure and properties of barium titanate materials. In this review paper, Part I contains a study of the BaTiO3 structure and frequently used synthesis methods.

  13. Lithium ceramics: sol-gel preparation and tritium release

    International Nuclear Information System (INIS)

    Renoult, O.

    1994-04-01

    Ceramics based on lithium aluminate (LiA1O 2 ), lithium zirconate (Li 2 ZrO 3 ) and lithium titanate (Li 2 TiO 3 ) are candidates as tritium breeder blanket materials for forthcoming nuclear fusion reactors. Lithium silico-aluminate Li 4+x A1 4-3x Si 2x O 8 (0 ≤ x ≤ 0,25) powders were synthetized from alkoxyde-hydroxyde sol-gel route. By direct sintering at 850-1100 deg C (without prior calcination), ceramics with controlled stoichiometry and homogenous microstructure were obtained. We have also prepared, using a comparable method, Li 2 Zr 1-x Ti x O 3 (x = 0, x = 0,1 et x = 1) materials. All these ceramics, with different microstructures and compositions, have been tested in out-of-reactor experiments. Concerning lithium aluminate microporous ceramics, the silicon substitution leads to a significant improvement of the tritrium release. Classical models taking into account independent surface mechanisms are not able to describe correctly the observed tritium release kinetics. We show, using a simple model, that the release kinetics is in fact limited by an intergranular diffusion followed by a desorption. The delay in tritium release, which occurs when the ceramic compacity increases, is explained in terms of an enhancement of the ionic T + diffusion path length. The energy required for desorption includes a leading term independent of hydrogen contained in the sweep gas. This term is attributed to the limiting recombination step of T + in molecular species HTO. For similar microstructures, the facility of tritium release for the different studied materials is explained by three properties: the crystal structure of the ceramic, the acidity of oxides and finally the presence of electronic non-stoichiometric defects. (author). 89 refs., 50 figs., 2 tabs., 1 annexe

  14. Impurities in barium titanate posistor ceramics

    Czech Academy of Sciences Publication Activity Database

    Korniyenko, S. M.; Bykov, I. P.; Glinchuk, M. J.; Laguta, V. V.; Belous, A. G.; Jastrabík, Lubomír

    2000-01-01

    Roč. 239, - (2000), s. 1209-1218 ISSN 0015-0193 Institutional research plan: CEZ:AV0Z1010914 Keywords : barium titanate phase transition * ESR * positive temperature coefficient of resistivity Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 0.547, year: 2000

  15. Enhanced ferroelectric and piezoelectric properties in La-modified PZT ceramics

    Science.gov (United States)

    Kour, P.; Pradhan, S. K.; Kumar, Pawan; Sinha, S. K.; Kar, Manoranjan

    2016-06-01

    The effect of lanthanum (La) doping on ferroelectric and piezoelectric properties of lead zirconate titanate (PZT) sample has been investigated. Pb1- x La x Zr0.52Ti0.48O3 ceramics with x = 0.00, 0.02, 0.04, 0.06 and 0.10 were prepared by the sol-gel technique. Raman and Fourier transforms infrared spectroscopy have been employed to understand the structural modification due to ionic size mismatch. Raman spectra show the existence of both rhombohedral and tetragonal crystal symmetries. It also shows the dielectric relaxation with increase in La concentration in the sample. The increase in lattice strain due to La doping increases the remnant polarization and coercive field. The linear piezoelectric coefficient increases with the increase in La concentration. It reveals that La-substituted PZT is a better candidate for piezoelectric sensor applications as compared to that of PZT.

  16. Polyphase ceramic and glass-ceramic forms for immobilizing ICPP high-level nuclear waste

    International Nuclear Information System (INIS)

    Harker, A.B.; Flintoff, J.F.

    1984-01-01

    Polyphase ceramic and glass-ceramic forms have been consolidated from simulated Idaho Chemical Processing Plant wastes by hot isostatic pressing calcined waste and chemical additives by 1000 0 C or less. The ceramic forms can contain over 70 wt% waste with densities ranging from 3.5 to 3.85 g/cm 3 , depending upon the formulation. Major phases are CaF 2 , CaZrTi 207 , CaTiO 3 , monoclinic ZrO 2 , and amorphous intergranular material. The relative fraction of the phases is a function of the chemical additives (TiO 2 , CaO, and SiO 2 ) and consolidation temperature. Zirconolite, the major actinide host, makes the ceramic forms extremely leach resistant for the actinide simulant U 238 . The amorphous phase controls the leach performance for Sr and Cs which is improved by the addition of SiO 2 . Glass-ceramic forms were also consolidated by HIP at waste loadings of 30 to 70 wt% with densities of 2.73 to 3.1 g/cm 3 using Exxon 127 borosilicate glass frit. The glass-ceramic forms contain crystalline CaF 2 , Al 203 , and ZrSi 04 (zircon) in a glass matrix. Natural mineral zircon is a stable host for 4+ valent actinides. 17 references, 3 figures, 5 tables

  17. An investigation of vacancy-like defects in differently doped and treated Pb(ZrxTi1-x)O3 ceramics

    International Nuclear Information System (INIS)

    Puff, W.; Balogh, A.G.; Balke, N.; Gottschalk, S.

    2006-01-01

    Full text: Important macroscopic properties of lead zirconate-titanate (PZT) ceramics are strongly affected by defect structure and diffusivity. In this study we discuss vacancy like defects in ferroelectric Pb(Zr x Ti 1-x )O 3 ceramics doped either with Fe or Ni and Sb. The investigations were performed with positron lifetime and Doppler broadening spectroscopy. The undoped samples show one defect lifetime component with a value of about 250 and 270 ps in dependence of the sintering atmosphere and sintering temperature. After doping this defect lifetime increases to about 290 to 300 ps. The Fe doped samples, Fe concentration from 0.1 to 1.0 mol-%, were measured also at low temperature to study the charge state of the observed defects. To study the aging behaviour of the Ni and Sb doped samples measurements were performed either after dc loading for 24 hours or ac loading up to 3 x 10 7 cycles. (author)

  18. Ferroelectric and Piezoelectric properties of (111) oriented lanthanum modified lead zirconate titanate film

    International Nuclear Information System (INIS)

    Dutta, Soma; Antony Jeyaseelan, A.; Sruthi, S.

    2014-01-01

    Lanthanum modified lead zirconate titanate (PLZT) thick film with molecular formula of Pb 0.92 La 0.08 (Zr 0.52 Ti 0.48 ) 0.98 O 3 was grown preferentially along (111) direction on Pt/SiO 2 /Si (platinum/silicon oxide/silicon) substrate by spin coating of chemical solution. The directional growth of the film was facilitated by platinum (Pt) (111) template and rapid thermal annealing. X-ray diffraction pattern and atomic force microscopy revealed the preferential growth of the PLZT film. The film was characterized for ferroelectric and detailed piezoelectric properties in a parallel plate capacitor (metal–PLZT–metal) configuration. Ferroelectric characterization of the film showed saturated hysteresis loop with remanent polarization and coercive electric field values of 10.14 μC/cm 2 and 42 kV/cm, respectively, at an applied field of 300 kV/cm. Longitudinal piezoelectric coefficient (d 33,f ) was measured by employing converse piezoelectric effect where electrical charge response and displacement were measured with electrical voltage excitation on the sample electrodes. The effective transverse piezoelectric coefficient (e 31,f ) was derived from charge measurement with an applied mechanical excitation strain by using the four point bending method. d 33,f and e 31,f coefficients of PLZT films were found to be 380 pm/V and − 0.831 C/m 2 respectively. - Highlights: • PLZT (111) film is prepared by spin coating of chemical sol on Pt (111) template. • Piezoelectric d 33 value (380 pm/V) of PLZT film is found 20% higher than PZT. • Transverse piezocoefficient e 31,f of PLZT film is reported for the first time

  19. Piezoelectric effect in polarized and electrically depolarized ferrotextures

    International Nuclear Information System (INIS)

    Luchaninov, A.G.; Shil'nikov, A.V.; Shuvalov, L.A.

    1999-01-01

    Piezoelectric moduli were calculated for ferroelectric textures in the states with the greatest possible (in terms of symmetry) polarization and the zero polarization (obtained from the former by electrical depolarization). The calculations were performed for the textures of crystals of the classes 2, 3, 4, 6, mm2, 3m, 4mm,and 6mm. The experimental results for lead zirconate-titanate- and barium-titanate-based piezoelectric ceramic are reported

  20. Microcracking in ceramics and acoustic emission

    International Nuclear Information System (INIS)

    Subbarao, E.C.

    1991-01-01

    One of the limitations in the use of ceramics in critical applications is due to the presence of microcracks, which may arise from differential thermal expansion and phase changes, among others. Acoustic emission signals occur when there are abrupt microdeformations in a material and thus offer a convenient means of non-destructive detection of microcracking. Examples of a study of acoustic emission from microcracking due to anisotropic thermal expansion in low thermal expansion single phase ceramics such as niobia and sodium zirconium phosphate ceramics and due to phase changes in zirconia and superconducting YBa 2 Cu 3 Osub(7-x) ceramics are presented, together with the case of lead titanate ceramics, which exhibits both a phase change (paraelectric to ferroelectric) and an anisotropic thermal expansion. The role of grain size on the extent of microcracking is illustrated in the case of niobia ceramics. Some indirect evidence of healing of microcracks on heating niobia and lead titanate ceramics is presented from the acoustic emission results. (author). 69 refs., 9 figs

  1. Towards a single host phase ceramic formulation for UK plutonium disposition

    International Nuclear Information System (INIS)

    Stennett, M. C.; Hyatt, N. C.; Gilbert, M.; Livens, F. R.; Maddrell, E. R.

    2008-01-01

    The UK has a considerable stockpile of separated plutonium; a legacy of over 50 years of civilian nuclear programmes. This material has been considered both as an asset for future energy generation and a liability due to the proliferation threat. A proportion of the PuO 2 stocks may be consumed by nuclear fission, in mixed oxide (MOx) or inert matrix (IMF) fuels but a quantity of waste PuO 2 will remain which is unsuitable for fuel manufacture and will require immobilisation. A research program is currently underway to investigate the potential of various single phase ceramic formulations for the immobilisation of this waste PuO 2 fraction. In this work a number of synthetic mineral systems have been considered including titanate, zirconate, phosphate and silicate based matrices. Although a wealth of information on plutonium disposition in some of the systems exists in the literature, the data is not always directly comparable which hinders comparison between different ceramic hosts. The crux of this research has been to compile a database of information on the proposed hosts to allow impartial comparison of the relative merits and shortcomings in each system. (authors)

  2. Reduction of etching damage in lead-zirconate-titanate thin films with inductively coupled plasma

    International Nuclear Information System (INIS)

    Lim, Kyu-Tae; Kim, Kyoung-Tae; Kim, Dong-Pyo; Kim, Chang-Il

    2003-01-01

    In this work, we etched lead-zirconate-titanate (PZT) films with various additive gases (O 2 and Ar) in Cl 2 /CF 4 plasmas, while mixing ratio was fixed at 8/2. After the etching, the plasma induced damages are characterized in terms of hysteresis curves, leakage current, retention properties, and switching polarization. When the electrical properties of PZT etched in O 2 or Ar added to Cl 2 /CF 4 were compared, the value of remanent polarization in O 2 added to Cl 2 /CF 4 plasma is higher than that in Ar added plasma. The maximum etch rate of the PZT thin films was 145 nm/min for 30% Ar added Cl 2 /CF 4 gas having mixing ratio of 8/2 and 110 nm/min for 10% O 2 added to that same gas mixture. In order to recover the ferroelectric properties of the PZT thin films after etching, we annealed the etched PZT thin films at 550 deg. C in an O 2 atmosphere for 10 min. From the hysteresis curves, leakage current, retention property, and switching polarization, the reduction of the etching damage and the recovery via the annealing turned out to be more effective when O 2 was added to Cl 2 /CF 4 than Ar. X-ray diffraction showed that the structural damage was lower when O 2 was added to Cl 2 /CF 4 and the improvement in the ferroelectric properties of the annealed samples was consistent with the increased intensities of the (100) and the (200) PZT peaks

  3. Sound velocity variation as function of polarization state in Lead Zirconate Titanate (PZT) Ceramics

    International Nuclear Information System (INIS)

    Essolaani, W; Farhat, N

    2012-01-01

    There are several ultrasonic techniques to measure the sound velocity, for example, the pulse-echo method. In such method, the size of transducer used to measure the sound velocity must be in the same order of the sample size. If not, the incompatibility of sizes becomes an error source of the sound velocity measurement. In this work, the Laser Induced Pressure Pulse (LIPP) method is used as ultrasonic method. This method has been very useful for studying the spatial distribution of charges and polarization in dielectrics. We take advantage of the fact that the method allows the sound velocity measurement, to study its variation as function of polarization state in (PZT) ceramics. In a sample with a known thickness e, the sound velocity ν is deduced from the measurement of the transit time T. The sound velocity depends on the elastic constants which in turn they depend on poling conditions. Thus, the variation of the sound velocity is related to the direction and the amplitude of the polarization.

  4. Pulsed laser deposition of piezoelectric lead zirconate titanate thin films maintaining a post-CMOS compatible thermal budget

    Science.gov (United States)

    Schatz, A.; Pantel, D.; Hanemann, T.

    2017-09-01

    Integration of lead zirconate titanate (Pb[Zrx,Ti1-x]O3 - PZT) thin films on complementary metal-oxide semiconductor substrates (CMOS) is difficult due to the usually high crystallization temperature of the piezoelectric perovskite PZT phase, which harms the CMOS circuits. In this work, a wafer-scale pulsed laser deposition tool was used to grow 1 μm thick PZT thin films on 150 mm diameter silicon wafers. Three different routes towards a post-CMOS compatible deposition process were investigated, maintaining a post-CMOS compatible thermal budget limit of 445 °C for 1 h (or 420 °C for 6 h). By crystallizing the perovskite LaNiO3 seed layer at 445 °C, the PZT deposition temperature can be lowered to below 400 °C, yielding a transverse piezoelectric coefficient e31,f of -9.3 C/m2. With the same procedure, applying a slightly higher PZT deposition temperature of 420 °C, an e31,f of -10.3 C/m2 can be reached. The low leakage current density of below 3 × 10-6 A/cm2 at 200 kV/cm allows for application of the post-CMOS compatible PZT thin films in low power micro-electro-mechanical-systems actuators.

  5. A poling study on lead zirconate titanate composition

    International Nuclear Information System (INIS)

    Bryant, P.J.

    1992-01-01

    Ceramics produced by the conventional mixed oxide route are dual phased. Because the titania and zirconia are not perfectly homogenized, some parts of the ceramic are more tetragonal (titanium rich) and other parts more rhombohedral (zirconium rich). This inhomogeneity means that some domains can be more easily poled than others. Lastly, the density and porosity can affect the poling process if the flaw density becomes such that the breakdown voltage is exceeded by the required poling voltage. The phase boundary determined by most dielectric and piezoelectric measurements is significantly removed from the 44% titanium content determined by neutron diffraction. The indicators that are most consistent with this value are the minimum in the poling efficiency curve and the shape of the dissipative factor curve. The reason for the discrepancy appears to be related to the broad coexistence region of the two phases and the differing poling efficiencies of each phase. It has been established that different poling temperature profiles can substantially modify the observed properties. Such behaviour is again related to the inhomogeneity of the ceramic and the presence of the two phases. 4 refs., 5 figs

  6. Dielectric and piezoelectric properties of neodymium oxide doped ...

    Indian Academy of Sciences (India)

    Unknown

    Abstract. The dielectric and electromechanical properties of lead zirconate titanate [Pb(Zr, Ti)O3] ceramic added with neodymium oxide have been systematically studied employing the vector impedance spectroscopic. (VIS) technique. The specimens were prepared using the mixed oxide route by adding different mol% of.

  7. Structure and phase formation behavior and dielectric and magnetic properties of lead iron tantalate-lead zirconate titanate multiferroic ceramics

    International Nuclear Information System (INIS)

    Wongmaneerung, R.; Tipakontitikul, R.; Jantaratana, P.; Bootchanont, A.; Jutimoosik, J.; Yimnirun, R.; Ananta, S.

    2016-01-01

    Highlights: • The multiferroic ceramics consisted of PFT and PZT. • Crystal structure changed from cubic to mixedcubic and tetragonal with increasing PZT content. • Dielectric showed the samples underwent a typical relaxor ferroelectric behavior. • Magnetic properties showed very interesting behavior with square saturated magnetic hysteresis loops. - Abstract: Multiferroic (1 − x)Pb(Fe_0_._5Ta_0_._5)O_3–xPb(Zr_0_._5_3Ti_0_._4_7)O_3 (or PFT–PZT) ceramics were synthesized by solid-state reaction method. The crystal structure and phase formation of the ceramics were examined by X-ray diffraction (XRD). The local structure surrounding Fe and Ti absorbing atoms was investigated by synchrotron X-ray Absorption Near-Edge Structure (XANES) measurement. Dielectric properties were studied as a function of frequency and temperature using a LCR meter. A vibrating sample magnetometer (VSM) was used to determine the magnetic hysteresis loops. XRD study indicated that the crystal structure of the sample changed from pure cubic to mixed cubic and tetragonal with increasing PZT content. XANES measurements showed that the local structure surrounding Fe and Ti ions was similar. Dielectric study showed that the samples underwent a typical relaxor ferroelectric behavior while the magnetic properties showed very interesting behavior with square saturated magnetic hysteresis loops.

  8. Fatigue and failure responses of lead zirconate titanate multilayer actuator under unipolar high-field electric cycling

    Science.gov (United States)

    Zeng, Fan Wen; Wang, Hong; Lin, Hua-Tay

    2013-07-01

    Lead zirconate titanate (PZT) multilayer actuators with an interdigital electrode design were studied under high electric fields (3 and 6 kV/mm) in a unipolar cycling mode. A 100 Hz sine wave was used in cycling. Five specimens tested under 6 kV/mm failed from 3.8 × 105 to 7 × 105 cycles, whereas three other specimens tested under 3 kV/mm were found to be still functional after 108 cycles. Variations in piezoelectric and dielectric responses of the tested specimens were observed during the fatigue test, depending on the measuring and cycling conditions. Selected fatigued and damaged actuators were characterized using an impedance analyzer or small signal measurement. Furthermore, involved fatigue and failure mechanisms were investigated using scanning acoustic microscope and scanning electron microscope. The extensive cracks and porous regions were revealed across the PZT layers on the cross sections of a failed actuator. The results from this study have demonstrated that the high-field cycling can accelerate the fatigue of PZT stacks as long as the partial discharge is controlled. The small signal measurement can also be integrated into the large signal measurement to characterize the fatigue response of PZT stacks in a more comprehensive basis. The former can further serve as an experimental method to test and monitor the behavior of PZT stacks.

  9. Dielectric properties and vacancy-like defects in plasma-sprayed barium titanate.

    Czech Academy of Sciences Publication Activity Database

    Ctibor, Pavel; Čížek, J.; Sedláček, J.; Lukáč, František

    2017-01-01

    Roč. 100, č. 7 (2017), s. 2972-2983 ISSN 0002-7820 Institutional support: RVO:61389021 Keywords : barium titanate * plasma spraying * vacancies Subject RIV: JH - Ceramic s, Fire-Resistant Materials and Glass OBOR OECD: Ceramic s Impact factor: 2.841, year: 2016

  10. Effect of Nb doping on sintering and dielectric properties of PZT ceramics

    Directory of Open Access Journals (Sweden)

    Ali Mirzaei

    2016-09-01

    Full Text Available The extensive use of piezoelectric ceramics such as lead zirconate titanate (PZT in different applications became possible with the development of donor or acceptor dopants. Therefore, studies on the effect of dopants on the properties of PZT ceramics are highly demanded. In this study undoped and 2.4 mol% Nb-doped PZT (PZTN powders were successfully obtained by a solid-state reaction and calcination at 850 °C for 2 h. Crystallinity and phase formation of the prepared powders were studied using X-ray diffraction (XRD. In order to study morphology of powders, scanning electron microscopy (SEM was performed. The crystalline PZT and Nb-doped PZT powders were pelleted into discs and sintered at 1100, 1150 and 1200 °C, with a heating rate of 10 °C/min, and holding time of 1–6 h to find the optimum combination of temperature and time to produce high density ceramics. Microstructural characterization was conducted on the fractured ceramic surfaces using SEM. Density measurements showed that maximal density of 95% of the theoretical density was achieved after sintering of PZT and PZTN ceramics at 1200 °C for 2 h and 4 h, respectively. However, the results of dielectric measurements showed that PZTN ceramics have higher relative permittivity (εr ∼17960 with lower Curie temperature (∼358 °C relative to PZT (εr = 16000 at ∼363 °C as a result of fine PZTN structure as well as presence of vacancies. In addition, dielectric loss (at 1 kHz of PZT and PZTN ceramics with 95% theoretical density was 0.0087 and 0.02, respectively. The higher dielectric loss in PZTN was due to easier domain wall motions in PZTN ceramics.

  11. Study of barium bismuth titanate prepared by mechanochemical synthesis

    Directory of Open Access Journals (Sweden)

    Lazarević Z.Ž.

    2009-01-01

    Full Text Available Barium-bismuth titanate, BaBi4Ti4O15 (BBT, a member of Aurivillius bismuth-based layer-structure perovskites, was prepared from stoichiometric amounts of barium titanate and bismuth titanate obtained via mechanochemical synthesis. Mechanochemical synthesis was performed in air atmosphere in a planetary ball mill. The reaction mechanism of BaBi4Ti4O15 and the preparation and characteristics of BBT ceramic powders were studied using XRD, Raman spectroscopy, particle analysis and SEM. The Bi-layered perovskite structure of BaBi4Ti4O15 ceramic forms at 1100 °C for 4 h without a pre-calcination step. The microstructure of BaBi4Ti4O15 exhibits plate-like grains typical for the Bi-layered structured material and spherical and polygonal grains. The Ba2+ addition leads to changes in the microstructure development, particularly in the change of the average grain size.

  12. Structure and phase formation behavior and dielectric and magnetic properties of lead iron tantalate-lead zirconate titanate multiferroic ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Wongmaneerung, R., E-mail: re_nok@yahoo.com [Faculty of Science, Maejo University, Chiang Mai 50290 (Thailand); Tipakontitikul, R. [Department of Physics, Ubonratchathani University, Ubonratchathani 31490 (Thailand); Jantaratana, P. [Department of Physics, Kasetsart University, Bangkok 10900 (Thailand); Bootchanont, A.; Jutimoosik, J.; Yimnirun, R. [School of Physics, Institute of Science, and NANOTEC-SUT Center of Excellence on Advanced Functional Nanomaterials, Suranaree University of Technology, Nakhon Ratchasima 30000 (Thailand); Ananta, S. [Department of Physics and Materials Science, Faculty of Science, Chiang Mai University, Chiang Mai 50200 (Thailand)

    2016-03-15

    Highlights: • The multiferroic ceramics consisted of PFT and PZT. • Crystal structure changed from cubic to mixedcubic and tetragonal with increasing PZT content. • Dielectric showed the samples underwent a typical relaxor ferroelectric behavior. • Magnetic properties showed very interesting behavior with square saturated magnetic hysteresis loops. - Abstract: Multiferroic (1 − x)Pb(Fe{sub 0.5}Ta{sub 0.5})O{sub 3}–xPb(Zr{sub 0.53}Ti{sub 0.47})O{sub 3} (or PFT–PZT) ceramics were synthesized by solid-state reaction method. The crystal structure and phase formation of the ceramics were examined by X-ray diffraction (XRD). The local structure surrounding Fe and Ti absorbing atoms was investigated by synchrotron X-ray Absorption Near-Edge Structure (XANES) measurement. Dielectric properties were studied as a function of frequency and temperature using a LCR meter. A vibrating sample magnetometer (VSM) was used to determine the magnetic hysteresis loops. XRD study indicated that the crystal structure of the sample changed from pure cubic to mixed cubic and tetragonal with increasing PZT content. XANES measurements showed that the local structure surrounding Fe and Ti ions was similar. Dielectric study showed that the samples underwent a typical relaxor ferroelectric behavior while the magnetic properties showed very interesting behavior with square saturated magnetic hysteresis loops.

  13. Ferroelectric and Piezoelectric properties of (111) oriented lanthanum modified lead zirconate titanate film

    Energy Technology Data Exchange (ETDEWEB)

    Dutta, Soma, E-mail: som@nal.res.in; Antony Jeyaseelan, A.; Sruthi, S.

    2014-07-01

    Lanthanum modified lead zirconate titanate (PLZT) thick film with molecular formula of Pb{sub 0.92}La{sub 0.08}(Zr{sub 0.52}Ti{sub 0.48}){sub 0.98}O{sub 3} was grown preferentially along (111) direction on Pt/SiO{sub 2}/Si (platinum/silicon oxide/silicon) substrate by spin coating of chemical solution. The directional growth of the film was facilitated by platinum (Pt) (111) template and rapid thermal annealing. X-ray diffraction pattern and atomic force microscopy revealed the preferential growth of the PLZT film. The film was characterized for ferroelectric and detailed piezoelectric properties in a parallel plate capacitor (metal–PLZT–metal) configuration. Ferroelectric characterization of the film showed saturated hysteresis loop with remanent polarization and coercive electric field values of 10.14 μC/cm{sup 2} and 42 kV/cm, respectively, at an applied field of 300 kV/cm. Longitudinal piezoelectric coefficient (d{sub 33,f}) was measured by employing converse piezoelectric effect where electrical charge response and displacement were measured with electrical voltage excitation on the sample electrodes. The effective transverse piezoelectric coefficient (e{sub 31,f}) was derived from charge measurement with an applied mechanical excitation strain by using the four point bending method. d{sub 33,f} and e{sub 31,f} coefficients of PLZT films were found to be 380 pm/V and − 0.831 C/m{sup 2} respectively. - Highlights: • PLZT (111) film is prepared by spin coating of chemical sol on Pt (111) template. • Piezoelectric d{sub 33} value (380 pm/V) of PLZT film is found 20% higher than PZT. • Transverse piezocoefficient e{sub 31,f} of PLZT film is reported for the first time.

  14. Guided-Wave Testing of Trunnion Rods at Greenup Lock and Dam, Kentucky

    Science.gov (United States)

    2014-04-01

    fatigue cracks which go through opening and closing periods during their progression, microcracks in post-tension trunnion anchor rods are believed to be...produce undesired interference effects. A new 1.5 in. diameter, medium-damped lead zirconate titanate ( PZT ), ceramic-based crystal (i.e., an Accuscan

  15. Mapping of strain mechanisms in barium titanate by three-dimensional X-ray diffraction

    DEFF Research Database (Denmark)

    Majkut, Marta

    This thesis presents an in-situ three-dimensional study of the grain-scale response of a prototypical piezoelectric ceramic, barium titanate (BT), to an exernally applied electric field. Piezoceramics take advantage of the coupling of electrical and mechanical energies for use in sensors and actu......This thesis presents an in-situ three-dimensional study of the grain-scale response of a prototypical piezoelectric ceramic, barium titanate (BT), to an exernally applied electric field. Piezoceramics take advantage of the coupling of electrical and mechanical energies for use in sensors...

  16. A high-temperature-capacitor dielectric based on K.sub.0.5./sub.Na.sub.0.5./sub.NbO.sub.3./sub.–modified Bi.sub.1/2./sub.Na.sub.1/2./sub.TiO.sub.3./sub.–Bi.sub.1/2./sub.K.sub.1/2./sub.TiO.sub.3./sub

    Czech Academy of Sciences Publication Activity Database

    Dittmer, R.; Anton, E.-M.; Jo, W.; Simons, H.; Daniels, J.E.; Hoffman, M.; Pokorný, Jan; Reaney, I. M.; Rödel, J.

    2012-01-01

    Roč. 95, č. 11 (2012), s. 3519-3524 ISSN 0002-7820 Institutional research plan: CEZ:AV0Z10100520 Keywords : lead-zirconate-titanate * relaxor ferroelectric ceramics * raman-spectroscopy * thin-films * electronics * lanthanum * resistance * bias Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 2.107, year: 2012

  17. Formulation and synthesis by melting process of titanate enriched glass-ceramics and ceramics

    International Nuclear Information System (INIS)

    Advocat, T.; Fillet, C.; Lacombe, J.; Bonnetier, A.; McGlinn, P.

    1999-01-01

    The main objective of this work is to provide containment for the separated radionuclides in stable oxide phases with proven resistance to leaching and irradiation damage and in consequence to obtain a glass ceramic or a ceramic material using a vitrification process. Sphene glass ceramic, zirconolite glass ceramic and zirconolite enriched ceramic have been fabricated and characterized by XRD, SEM/EDX and DTA

  18. Radiophase development in hot-pressed alkoxide-derived titanate ceramics for nuclear waste stabilization

    International Nuclear Information System (INIS)

    Dickson, F.J.; Mitamura, H.; White, T.J.

    1989-01-01

    This paper reports phase development as a function of hot-pressing temperature studied in alkoxide-derived titanate-based ceramics doped with a 10 wt% loading of a sodium-rich (NAR) and a sodium-poor (NAP) simulated high-level waste. Pyrochlore was found to be the most abundant phase in both calcine powders. A pseudobrookite phase existed metastably at hot-pressing temperatures between 890 degrees and 920 degrees C. After hot-pressing at 1100 degrees C, the final phase assemblage for the NAP material consisted of zirconolite, hollandite-type, perovskite, alloy, and reduced rutile (Magneli phases). In addition, NAR samples contained hibonite, freudenbergite, and loveringite. Phase development was driven to completion over a very narrow temperature range (≤50 degrees C), beginning at 870 degrees and 850 degrees C for NAP and NAR, respectively, although full densification was not achieved below 1100 degrees C. Both waste forms exhibited comparable microstructure and aqueous durability

  19. Raman study of lead zirconate titanate under uniaxial stress

    International Nuclear Information System (INIS)

    Tallant, David R.; Simpson, Regina L.; Grazier, J. Mark; Zeuch, David H.; Olson, Walter R.; Tuttle, Bruce A.

    2000-01-01

    The authors used micro-Raman spectroscopy to monitor the ferroelectric (FE) to antiferroelectric (AFE) phase transition in PZT ceramic bars during the application of uniaxial stress. They designed and constructed a simple loading device, which can apply sufficient uniaxial force to transform reasonably large ceramic bars while being small enough to fit on the mechanical stage of the microscope used for Raman analysis. Raman spectra of individual grains in ceramic PZT bars were obtained as the stress on the bar was increased in increments. At the same time gauges attached to the PZT bar recorded axial and lateral strains induced by the applied stress. The Raman spectra were used to calculate an FE coordinate, which is related to the fraction of FE phase present. The authors present data showing changes in the FE coordinates of individual PZT grains and correlate these changes to stress-strain data, which plot the macroscopic evolution of the FE-to-AFE transformation. Their data indicates that the FE-to-AFE transformation does not occur simultaneously for all PZT grains but that grains react individually to local conditions

  20. Natural radioactivity and radon specific exhalation rate of zircon sands

    International Nuclear Information System (INIS)

    Righi, S.; Verita, S.; Bruzzi, L.; Albertazzi, A.

    2006-01-01

    The study focuses on the radon emanation from zircon sands and their derivatives, which are widely used in many sectors of industry. In particular, the results obtained by experimental measurements on samples of zircon sands and zircon flours commonly used in Italian ceramic industries are reported. Zircon sands contain a significant concentration of natural radioactivity because Th and U may substitute zirconium in the zircon crystal lattice. The relevant routes of exposure of workers to T.E.N.O.R.M. from zircon materials are external radiation and internal exposure, either by inhalation of aerosols in dusty working conditions or by inhalation of radon in workplaces. The main objective of this investigation is to provide experimental data able to better calculate the internal exposure of workers due to radon inhalation. Zircon samples were surveyed for natural radioactivity, radon specific exhalation rate and emanation fraction. Measurements of radioactivity concentration were carried out using γ-spectrometry. Methods used for determining radon consisted in determining the 222 Rn activity accumulated in a vessel after a given accumulation build-up time. The average activity concentrations of 238 U and 232 Th in samples result about 2600 and 550 Bq kg-1, respectively; these concentrations are significantly higher than the world average noticed in soils, rocks and Earth crust. The 222 Rn specific exhalation rates result very low probably due to the low porosity of the material and the consequent difficulty for radon to be released from the zircon crystal lattice. (author)

  1. Development of crystalline ceramic for immobilization of TRU wastes in V.G. Khlopin Radium Institute

    International Nuclear Information System (INIS)

    Burakov, B.E.; Anderson, E.B.

    1999-01-01

    This paper discusses the Radium Institute's experience in the synthesis of crystalline ceramics based on two groups of actinide host-phases: 1) Zircon/zirconia-(Zn, Ac)SiO 4 /(Zr, Ac)O 2 , where Ac=Pu, Np, Am, Cm; 2) Garnet/perovskite-(Y, Gd, Ac) 3 (Al, Ga, Ac,..) 5 O 12 /(Y, Gd, Ac)(Al, Ga)O 3 . The zircon/zirconia ceramic was suggested as an universal waste form for the immobilization of TRU as well as weapon-grade Pu. Because the position of the Russian Ministry of Atomic Energy (Minatom) does not consider weapons Pu as a waste', the Radium Institute proposed the use of the same ceramic (mainly monophase zirconia ) as a Pu-fuel. The garnet/perovskite ceramic was suggested for the immobilization of military TRU wastes of complex chemical composition. The advantage of this ceramic is that Garnet and Perovskite host-phases can incorporate in their lattices not only actinides, but also other elements including neutron absorbers in a broad range of concentration and in different valence state. Sample of zircon/zirconia ceramic were prepared by hot uniaxial pressing (at temperature T=1300, 1400, 1500degC and pressure P=25 MPa) and sintering (at T=1450, 1490, 1500, 1600degC) methods using different types of initial precursor. Samples of garnet/perovskite ceramic were synthesized by melting method at T=2000degC. Ce, U, Gd were used as TRU stimulants for both types of ceramic. One sample of zircon/zirconia ceramic was doped with 10 wt.% of Pu 239 . Physico-chemical features of these ceramics are described. In conclusion we propose that the pressureless technology based on sintering or melting methods be used for the synthesis of ceramics for the immobilization of all types of TRU wastes. (author)

  2. Phase quantification of mullite-zirconia and zircon commercial powders using PAC and XRD techniques

    Energy Technology Data Exchange (ETDEWEB)

    Rendtorff, Nicolas M.; Conconi, Maria S.; Aglietti, Esteban F. [Centro de Tecnologia de Recursos Minerales y Ceramica (CETMIC: CONICET-CIC) (Argentina); Chain, Cecilia Y.; Pasquevich, Alberto F. [Universidad Nacional de La Plata, Departamento de Fisica, IFLP, Facultad de Ciencias Exactas (Argentina); Rivas, Patricia C. [CONICET (Argentina); Martinez, Jorge A., E-mail: toto@fisica.unlp.edu.ar; Caracoche, Maria C. [Universidad Nacional de La Plata, Departamento de Fisica, IFLP, Facultad de Ciencias Exactas (Argentina)

    2010-06-15

    The short range technique of the Perturbed Angular Correlation (PAC) and x-ray diffraction (Rietveld) methods have been employed to determine the phase content in commercial mullite-zirconia and zircon raw materials that are ordinarily used to produce ceramic materials. The PAC technique, which probes zirconium-containing compounds at nanoscopic level, showed that zircon contains crystalline ZrSiO{sub 4} and an important amount of a structurally distorted zircon, which is also observed accompanying monoclinic zirconia in mullite-zirconia. This particular zircon phase was not detected by the long range x-ray diffraction-Rietveld technique. After an annealing treatment, important changes in crystalline contents of the powders allow confirming, by the x-ray diffraction-Rietveld method, the preexistence of this particular zircon phase. This fact must be taken into account when preparing multicomposites based on the present raw materials.

  3. A Study of Ultrasonic Wavefront Distortion Compensation.

    Science.gov (United States)

    1998-08-01

    arrays. The array is made of piezoelectric composite consisting of PZT (lead zirconate titanate) ceramic rods in a polymer matrix. The transducer...We have developed the procedures for making the final transducer array package by a series of steps. The arrays utilize PZT piezoelectric ceramic ...the low contrast cyst at coordinates (250,425) in Figure 6a. Seen below the cyst is a region with an altered texture and poorer angular resolution, a

  4. High Gain and High Directive of Antenna Arrays Utilizing Dielectric Layer on Bismuth Titanate Ceramics

    Directory of Open Access Journals (Sweden)

    F. H. Wee

    2012-01-01

    Full Text Available A high gain and high directive microstrip patch array antenna formed from dielectric layer stacked on bismuth titanate (BiT ceramics have been investigated, fabricated, and measured. The antennas are designed and constructed with a combination of two-, four-, and six-BiT elements in an array form application on microwave substrate. For gain and directivity enhancement, a layer of dielectric was stacked on the BiT antenna array. We measured the gain and directivity of BiT array antennas with and without the dielectric layer and found that the gain of BiT array antenna with the dielectric layer was enhanced by about 1.4 dBi of directivity and 1.3 dB of gain over the one without the dielectric layer at 2.3 GHz. The impedance bandwidth of the BiT array antenna both with and without the dielectric layer is about 500 MHz and 350 MHz, respectively, which is suitable for the application of the WiMAX 2.3 GHz system. The utilization of BiT ceramics that covers about 90% of antenna led to high radiation efficiency, and small-size antennas were produced. In order to validate the proposed design, theoretical and measured results are provided and discussed.

  5. Analysis of elastic strain and crystallographic texture in poled rhombohedral PZT ceramics

    International Nuclear Information System (INIS)

    Hall, D.A.; Steuwer, A.; Cherdhirunkorn, B.; Mori, T.; Withers, P.J.

    2006-01-01

    The elastic strain and crystallographic texture of a rhombohedral lead zirconate titanate ceramic have been characterised in the remanent state, after poling, using high-energy synchrotron X-ray diffraction as a function of the grain orientation ψ relative to the poling direction. It is observed that the (2 0 0) diffraction peak exhibits pronounced shifts as a function of ψ, indicating an elastic lattice strain, while others ({1 1 1}, {1 1 2} and {2 2 0}) show marked changes in intensity as a result of preferred ferroelectric domain orientation. It is shown that the (2 0 0) peak is not affected by the domain switching itself but rather acts like an elastic macrostrain sensor. A simple Eshelby analysis is used to demonstrate that both the elastic strain and texture vary systematically with ψ according to the factor (3cos 2 ψ - 1). This angular dependence is evaluated through micromechanics modelling. The physical meaning of the texture variations with ψ is also discussed

  6. Ceramics: Durability and radiation effects

    Energy Technology Data Exchange (ETDEWEB)

    Ewing, R.C.; Lutze, W. [Univ. of New Mexico, Albuquerque, NM (United States); Weber, W.J. [Pacific Northwest National Lab., Richland, WA (United States)

    1996-05-01

    At present, there are three seriously considered options for the disposition of excess weapons plutonium: (1) incorporation, partial burn-up and direct disposal of MOX-fuel; (2) vitrification with defense waste and disposal as glass {open_quotes}logs{close_quotes}; (3) deep borehole disposal. The first two options provide a safeguard due to the high activity of fission products in the irradiated fuel and the defense waste. The latter option has only been examined in a preliminary manner, and the exact form of the plutonium has not been identified. In this paper, we review the potential for the immobilization of plutonium in highly durable crystalline ceramics apatite, pyrochlore, zirconolite, monazite and zircon. Based on available data, we propose zircon as the preferred crystalline ceramic for the permanent disposition of excess weapons plutonium.

  7. Effects of Thickness, Pulse Duration, and Size of Strip Electrode on Ferroelectric Electron Emission of Lead Zirconate Titanate Films

    Science.gov (United States)

    Yaseen, Muhammad; Ren, Wei; Chen, Xiaofeng; Feng, Yujun; Shi, Peng; Wu, Xiaoqing

    2018-02-01

    Sol-gel-derived lead zirconate titanate (PZT) thin-film emitters with thickness up to 9.8 μm have been prepared on Pt/TiO2/SiO2/Si wafer via chemical solution deposition with/without polyvinylpyrrolidone (PVP) modification, and the relationship between the film thickness and electron emission investigated. Notable electron emission was observed on application of a trigger voltage of 120 V for PZT film with thickness of 1.1 μm. Increasing the film thickness decreased the threshold field to initiate electron emission for non-PVP-modified films. In contrast, the electron emission behavior of PVP-modified films did not show significant dependence on film thickness, probably due to their porous structure. The emission current increased with decreasing strip width and space between strips. Furthermore, it was observed that increasing the duration of the applied pulse increased the magnitude of the emission current. The stray field on the PZT film thickness was also calculated and found to increase with increasing ferroelectric sample thickness. The PZT emitters were found to be fatigue free up to 105 emission cycles. Saturated emission current of around 25 mA to 30 mA was achieved for the electrode pattern used in this work.

  8. N Nwathore

    Indian Academy of Sciences (India)

    Home; Journals; Bulletin of Materials Science. N Nwathore. Articles written in Bulletin of Materials Science. Volume 34 Issue 1 February 2011 pp 129-132. Effect of temperature on polarization reversal of strontium-doped lead zirconate titanate (PSZT) ceramics · N Nwathore C M Lonkar D K Kharat · More Details Abstract ...

  9. Ceramic injection molding

    International Nuclear Information System (INIS)

    Agueda, Horacio; Russo, Diego

    1988-01-01

    Interest in making complex net-shape ceramic parts with good surface finishing and sharp tolerances without machining is a driving force for studying the injection molding technique. This method consists of softhening the ceramic material by means of adding some plastic and heating in order to inject the mixture under pressure into a relatively cold mold where solidification takes place. Essentially, it is the same process used in thermoplastic industry but, in the present case, the ceramic powder load ranges between 80 to 90 wt.%. This work shows results obtained from the fabrication of pieces of different ceramic materials (alumina, barium titanate ferrites, etc.) in a small scale, using equipments developed and constructed in the laboratory. (Author) [es

  10. Pressure-assisted sintering of high purity barium titanate

    NARCIS (Netherlands)

    van den Cruijsem, S.; Varst, van der P.G.T.; With, de G.; Bortzmeyer, D.; Boussuge, M.; Chartier, Th.; Hausonne, J.M.; Mocellin, A.; Rousset, A.; Thevenot, F.

    1997-01-01

    The dielectric behaviour of High Purity Barium titanate (HPB) ceramics is strongly dependent on the grain size and porosity. For applications, control of grain size and porosity is required. Pressure-assisted sintering techniques at relatively low temperatures meet these requirements. In this study,

  11. Ceramic component with reinforced protection against radiations

    International Nuclear Information System (INIS)

    Dubuisson, J.; Laville, H.; Le Gal, P.

    1986-01-01

    Ceramic components hardened against radiations are claimed (for example capacitors or ceramic substrates for semiconductors). They are prepared with a sintered ceramic containing a high proportion of heavy atoms (for instance barium titanate and a bismuth salt) provided with a glass layer containing a high proportion of light atoms. The two materials are joined by vitrification producing a diffusion zone at the interface [fr

  12. Predicting the effective response of bulk polycrystalline ferroelectric ceramics via improved spectral phase field methods

    Science.gov (United States)

    Vidyasagar, A.; Tan, W. L.; Kochmann, D. M.

    2017-09-01

    Understanding the electromechanical response of bulk polycrystalline ferroelectric ceramics requires scale-bridging approaches. Recent advances in fast numerical methods to compute the homogenized mechanical response of materials with heterogeneous microstructure have enabled the solution of hitherto intractable systems. In particular, the use of a Fourier-based spectral method as opposed to the traditional finite element method has gained significant interest in the homogenization of periodic microstructures. Here, we solve the periodic, electro-mechanically-coupled boundary value problem at the mesoscale of polycrystalline ferroelectrics in order to extract the effective response of barium titanate (BaTiO3) and lead zirconate titanate (PZT) under applied electric fields. Results include the effective electric hysteresis and the associated butterfly curve of strain vs. electric field for mean stress-free electric loading. Computational predictions of the 3D polycrystalline response show convincing agreement with our experimental electric cycling and strain hysteresis data for PZT-5A. In addition to microstructure-dependent effective physics, we also show how finite-difference-based approximations in the spectral solution scheme significantly reduce instability and ringing phenomena associated with spectral techniques and lead to spatial convergence with h-refinement, which have been major challenges when modeling high-contrast systems such as polycrystals.

  13. Microstructure evolution and electrical characterization of Lanthanum doped Barium Titanate (BaTiO_3) ceramics

    International Nuclear Information System (INIS)

    Billah, Masum; Ahmed, A.; Rahman, Md. Miftaur; Mahbub, Rubbayat; Gafur, M. A.; Bashar, M. Shahriar

    2016-01-01

    In the current work, we investigated the structural and dielectric properties of Lanthanum oxide (La_2O_3) doped Barium Titanate (BaTiO_3) ceramics and established a correlation between them. Solid state sintering method was used to dope BaTiO_3 with 0.3, 0.5 and 0.7 mole% La_2O_3 under different sintering parameters. The raw materials used were La_2O_3 nano powder of ~80 nm grain size and 99.995% purity and BaTiO_3 nano powder of 100 nm grain size and 99.99% purity. Grain size distribution and morphology of fracture surface of sintered pellets were examined by Field Emission Scanning Electron Microscope and X-Ray Diffraction analysis was conducted to confirm the formation of desired crystal structure. The research result reveal that grain size and electrical properties of BaTiO_3 ceramic significantly enhanced for small amount of doping (up to 0.5 mole% La_2O_3) and then decreased with increasing doping concentration. Desired grain growth (0.80-1.3 µm) and high densification (<90% theoretical density) were found by proper combination of temperature, sintering parameters and doping concentration. We found the resultant stable value of dielectric constant was 10000-12000 at 100-300 Hz in the temperature range of 30°-50° C for 0.5 mole% La_2O_3 with corresponding shift of curie temperature around 30° C. So overall this research showed that proper La"3"+ concentration can control the grain size, increase density, lower curie temperature and hence significantly improve the electrical properties of BaTiO_3 ceramics.

  14. Crystallization and dielectric properties of PbTiO3 based glass ceramics

    Science.gov (United States)

    Shankar, J.; Rani, G. Neeraja; Deshpande, V. K.

    2018-04-01

    Glass samples with composition (50 - X) PbO - (25 + X) TiO2 - 25 B2O3 (where X = 0, 5, 10 and 12.5 mol %) were prepared using conventional quenching technique. These glass samples were converted to glass ceramics by following two stage heat treatment schedule. The XRD results in the glass ceramics revealed the formation of tetragonal lead titanate as a major crystalline phase. The SEM results show rounded crystallite of lead titanate. The ferroelectric nature of all the glass ceramic samples is confirmed by P - E hysteresis measurements. The extended heat treatment of glass ceramic samples at 593K for 10 h exhibited saturated hysteresis loops with higher values of remnant polarization.

  15. Development of low-expansion ceramics with strength retention to elevated temperatures. Final report

    Energy Technology Data Exchange (ETDEWEB)

    Hirschfeld, D.A.; Brown, J.J. Jr. [Virginia Polytechnic Inst. and State Univ., Blacksburg, VA (United States)

    1994-09-01

    The development of advanced engines has resulted in the need for new ceramic compositions which exhibit thermo-mechanical properties suitable for the engine environment, e.g., low thermal expansion, stability to 1,200 C, and thermal shock resistance. To meet these goals, a two phase research program was instituted. In the first phase, new oxide ceramics were identified in the AlPO{sub 4}-{beta}-eucryptite, {beta}-cristobalite, mullite and zircon systems. This research focused on screening and property characterization of ceramics in the four systems. The most promising compositions in the AlPO{sub 4}-{beta}-eucryptite and zircon systems were then further evaluated and developed in the second phase with the goal of being ready for prototype testing in actual engines. Of the compositions, calcium magnesium zirconium phosphate (zircon system) exhibits the most desirable properties and is presently being developed for commercialization.

  16. A short and long range study of mullite-zirconia-zircon composites

    Energy Technology Data Exchange (ETDEWEB)

    Rendtorff, Nicolas M.; Conconi, Maria S.; Aglietti, Esteban F. [Centro de Tecnologia de Recursos Minerales y Ceramica (CETMIC: CONICET-CIC) (Argentina); Chain, Cecilia Y.; Pasquevich, Alberto F. [Universidad Nacional de La Plata, Departamento de Fisica, IFLP, Facultad de Ciencias Exactas (Argentina); Rivas, Patricia C. [CONICET (Argentina); Martinez, Jorge A., E-mail: toto@fisica.unlp.edu.ar; Caracoche, Maria C. [Universidad Nacional de La Plata, Departamento de Fisica, IFLP, Facultad de Ciencias Exactas (Argentina)

    2010-06-15

    In the field of refractory materials, ceramics containing mullite-zirconia are the basis of those most used in the industry of glass and steel. It is known that the addition of zircon improves the behavior of the refractory used in service. Knowing that some mullite-zirconia composites properties as fracture strength and the elastic modulus E are associated with the material microstructure integrity, the eventual thermal decomposition of zircon into zirconia and silica could seriously alter the material elastic properties. In this paper the phase content of a series of mullite-zirconia-zircon (3Al{sub 2}O{sub 3}.2SiO{sub 2}-ZrO{sub 2}-ZrSiO{sub 4}) composites is determined at atomic level via perturbed angular correlations (PAC) and compared with that derived from the long range X-ray diffraction technique. PAC results on the as-prepared materials indicate that all nominal zircon is present and that it involves two types of nanoconfigurations, one of them describing aperiodic regions. The thermomechanical properties already reported for these materials could be related to the crystalline to aperiodic zircon concentrations ratio they exhibit.

  17. Effects of surrounding powder in sintering process on the properties of Sb and Mn- doped barium-strontium titanate PTCR ceramics

    Directory of Open Access Journals (Sweden)

    Pornsuda Bomlai

    2006-05-01

    Full Text Available In this research, the effects of surrounding powder used during sintering of Sb and Mn doped bariumstrontium titanate (BST ceramics were studied. The ceramic samples were prepared by a conventional mixed-oxide method and placed on different powders during sintering. Phase formation, microstructure and PTCR behavior of the samples were then observed. Microstructures and PTCR behavior varied with the type of surrounding powder, whereas the crystal structure did not change. The surrounding powder has more effects on the shape of the grain than on the size. The grain size of samples was in the range of 5-20 μm. The most uniform grain size and the highest increase of the ratio of ρmax/ρRT were found to be about 106 for samples which had been sintered on Sb-doped BST powder. This value was an order of magnitude greater than for samples sintered on a powder of the equivalent composition to that of the sample pellet.

  18. Broadband Electromagnetic Emission from PZT Ferroelectric Ceramics after Shock Loading

    Directory of Open Access Journals (Sweden)

    Fiodoras ANISIMOVAS

    2013-12-01

    Full Text Available It was experimentally registered pulsed electromagnetic (EM radiation in frequency range higher than television one using wideband horns with coaxial and waveguide outputs. The EM radiation was received during shock loading of lead zirconate titanate (PZT ceramics cylinders in conventional piezoelectric ignition mechanisms. Digital oscilloscope allows registering whole series of EM pulses and each pulse from the series transmitted from horn antenna of (1 – 18 GHz operating band frequencies. There is (1 – 4 ms delay between the shock and the first pulse of the series. Duration of the series is about (3 – 4 ms. The PZT cylinders were cleaved along their axes and the surfaces formed in the process were investigated by scanning electron microscope. It was concluded that from electrical point of view PZT ceramics contain interacting subsystems. It was found that EM radiation spectrum of pulse detected by waveguide detector heads has harmonics reaching 80 GHz. Presence of harmonics higher than 20 GHz indicates on radiation due to deceleration of electrons emitted during the switching. The EM pulses in the series appear randomly and have different amplitudes which partly confirmed thesis on independent switching dynamics of small volumes governed by a local electric field.DOI: http://dx.doi.org/10.5755/j01.ms.19.4.3137

  19. PZT/PLZT - elastomer composites with improved piezoelectric voltage coefficient

    Science.gov (United States)

    Harikrishnan, K.; Bavbande, D. V.; Mohan, Dhirendra; Manoharan, B.; Prasad, M. R. S.; Kalyanakrishnan, G.

    2018-02-01

    Lead Zirconate Titanate (PZT) and Lanthanum-modified Lead Zirconate Titanate (PLZT) ceramic sensor materials are widely used because of their excellent piezoelectric coefficients. These materials are brittle, high density and have low achievable piezoelectric voltage coefficients. The density of the sintered ceramics shall be reduced by burnable polymeric sponge method. The achievable porosity level in this case is nearly 60 - 90%. However, the porous ceramic structure with 3-3 connectivity produced by this method is very fragile in nature. The strength of the porous structure is improved with Sylgard®-184 (silicone elastomer) by vacuum impregnation method maintaining the dynamic vacuum level in the range of -650 mm Hg. The elastomer Sylgard®-184 is having low density, low dielectric constant and high compliance (as a resultant stiffness of the composites is increased). To obtain a net dipole moment, the impregnated ceramic composites were subjected to poling treatment with varying conditions of D.C. field and temperature. The properties of the poled PZT/PLZT - elastomer composites were characterized with LCR meter for measuring the dielectric constant values (k), d33 meter used for measuring piezo-electric charge coefficient values (d33) and piezo-electric voltage coefficient (g33) values which were derived from d33 values. The voltage coefficient (g33) values of these composites are increased by 10 fold as compared to the conventional solid ceramics demonstrates that it is possible to fabricate a conformable detector.

  20. Synthesis, by alkaline fusion of zirconia from zirconite: characterization and preparation of lead zirconate-titanate

    International Nuclear Information System (INIS)

    Zaghete, M.A.

    1985-01-01

    Zirconium oxide was prepared from zirconite by alkaline fusion. The purity of zirconia was determined by atomic absorption spectroscopy and was found to be 99,94 wt%. In order to prepare en unglomerated and dry hidrous zirconia powder it was used alcohol and acetone for washing and gel suspension; control of the drying rate; and control of the atmosphere and temperature of the oven. The physical characteristics of the hidrous zirconia powder were determined after calcining in several conditions. The zirconia obtained by calcining at 800 0 C during 5 hours (13,9m 2 /g) was used with titanium oxide (7,6m 2 /g and lead oxide (0,6m 2 /g) to prepare a lead zirconate-titanate (PZT) with composition Pb(Zr 0,5 Ti 0,5 O 3 . Two different procedures were used to obtain high densits PZT pellets: in the first procedure the misture of the oxide powder with above composition were reacted at 850 0 C for 4 hours. Then the powder was pressed and sintered at 1200 0 C during 4 and 6 hours; in the second procedure the mixture of unreacted oxide were pressed in pellets and then reacted at 850 0 C during 4 hours and sintered at 1200 0 C during 4 and 6 hours. The apparent density of the sintered pellets were determined By mercury displacement and ranged from 7,25 to 7,39 g/cm 3 for the compacts obtained by the second procedure and from 8,08 to 8,10g/cm 3 for the compacts obtained by the first procedure. The microstructure observed by scanning electron microscopy showed that sintered compact obtained by the first procedure has a more homogeneous size distribution when compared with samples obtained be the second procedure. (author) [pt

  1. Electron Emission And Beam Generation Using Ferroelectric Cathodes (electron Beam Generation, Lead Lanthanum Zicronate Titanate, High Power Traveling Wave Tube Amplfier)

    CERN Document Server

    Flechtner, D D

    1999-01-01

    In 1989, researchers at CERN published the discovery of significant electron emission (1– 100 A/cm2) from Lead- Lanthanum-Zirconate-Titanate (PLZT). The publication of these results led to international interest in ferroelectric cathodes studies for use in pulsed power devices. At Cornell University in 1991, experiments with Lead-Zirconate-Titanate (PZT) compositions were begun to study the feasibility of using this ferroelectric material as a cathode in the electron gun section of High Power Traveling Wave Tube Amplifier Experiments. Current-voltage characteristics were documented for diode voltages ranging from 50– 500,000 V with anode cathode gaps of.5– 6 cm. A linear current-voltage relation was found for voltages less than 50 kV. For diode voltages ≥ 200 kV, a typical Child-Langmuir V3/2 dependence was observed...

  2. IR study of Pb–Sr titanate borosilicate glasses

    Indian Academy of Sciences (India)

    Administrator

    IR study of Pb–Sr titanate borosilicate glasses. C R GAUTAM*, DEVENDRA KUMAR. † and OM PARKASH. †. Department of Physics, University of Lucknow, Lucknow 226 007, India. †. Department of Ceramic Engineering, Institute of Technology, Banaras Hindu University, Varanasi 221 005, India. MS received 3 January ...

  3. Synthesis and structural characterization of Ce-doped bismuth titanate

    International Nuclear Information System (INIS)

    Pavlovic, Nikolina; Srdic, Vladimir V.

    2009-01-01

    Ce-modified bismuth titanate nanopowders Bi 4-x Ce x Ti 3 O 12 (x ≤ 1) have been synthesized using a coprecipitation method. DTA/TG, FTIR, XRD, SEM/EDS and BET methods were used in order to investigate the effect of Ce-substitution on the structure, morphology and sinterability of the obtained powders. The phase structure investigation revealed that after calcinations at 600 deg. C powder without Ce addition exhibited pure bismuth titanate phase; however, powders with Ce (x = 0.25, 0.5 and 0.75) had bismuth titanate pyrochlore phase as the second phase. The strongest effect of Ce addition on the structure was noted for the powder with the highest amount of Ce (x = 1) having a cubic pyrochlore structure. The presence of pure pyrochlore phase was explained by its stabilization due to the incorporation of cerium ions in titanate structure. Ce-modified bismuth titanate ceramic had a density over 95% of theoretical density and the fracture in transgranular manner most probably due to preferable distribution of Ce in boundary region

  4. The phase stability and toughening effect of 3Y-TZP dispersed in the lanthanum zirconate ceramics

    International Nuclear Information System (INIS)

    Wang, Yanfei; Xiao, Ping

    2014-01-01

    The low fracture toughness of lanthanum zirconate (La 2 Zr 2 O 7 , LZ) greatly impedes its wide application as thermal barrier coatings (TBC). The 3 mol% Y 2 O 3 -stabilized tetragonal zirconia polycrystals (3Y-TZP) have been introduced to toughen the brittle LZ ceramics. The dispersive 3Y-TZP undergoes a simultaneous t–m transformation upon cooling below a critical volume fraction x of 3Y-TZP, above which its tetragonal phases can however be preserved. The different stabilities of 3Y-TZP second phases arise from a variation of residual tensile stress within them. The fracture toughness has been greatly improved by dispersing the tetragonal particulates (t-3YSZ) in the LZ matrix and the primary toughening mechanisms are phase transformations of the dispersive second phases and the residual compressive stress within the matrix. An anticipated increase of fracture toughness from the ferroelastic toughening and the residual compressive stress toughening highlights the great potentials to improve coating durability by depositing t′-3YSZ/LZ composite TBCs by the industrial non-equilibrium route

  5. Study of nanoconfigurations in Zircon-Mullite composites using perturbed angular correlations

    Energy Technology Data Exchange (ETDEWEB)

    Chain, Cecilia Y., E-mail: yamil@fisica.unlp.edu.ar; Pasquevich, Alberto F. [Universidad Nacional de La Plata, Departamento de Fisica, IFLP, Facultad de Ciencias Exactas (Argentina); Rivas, Patricia C. [CONICET (Argentina); Martinez, Jorge A.; Caracoche, Maria C. [Universidad Nacional de La Plata, Departamento de Fisica, IFLP, Facultad de Ciencias Exactas (Argentina); Rendtorff, Nicolas M. [CONICET (Argentina); Conconi, Maria S. [Centro de Tecnologia de Recursos Minerales y Ceramica (CETMIC: CONICET-CIC) (Argentina); Aglietti, Esteban F. [CONICET (Argentina)

    2010-06-15

    It has been already published that, at nanoscopic level, zircon exhibits wide regions of aperiodic material not detected by the ordinary techniques used to analyse the obtained product in the production of ceramic materials. In this paper it is reported how the Perturbed Angular Correlations (PAC) technique has assisted the interpretation of a mismatch between experiment and theoretical estimation of a mechanical property in some zircon-mullite composites. In fact, it has been proved that the difference observed between the calculated and the experimental value of the elastic modulus in composites of the form (1-x) ZrSiO{sub 4} - x 3Al{sub 2}O{sub 3}.2SiO{sub 2} (with x = 15, 25, 35 and 45 wt.%) behaves very similarly as the relative amount of aperiodic zircon determined by PAC. This result allows to re-interpret the mullite role during the materials preparation.

  6. Microstructure of lead zirconium titanate (PZT) by electron microscopy

    International Nuclear Information System (INIS)

    Bursill, L.A.; Peng JuLin

    1989-01-01

    Transmission and high-resolution electron microscopy reveal the microtexture of lead zirconium titanate ceramics. Fine scale (≤ 500 Aangstroem) ferroelastic and ferroelectric twin domains, as well as dislocations were found in a complex texture. Correlations between stoichiometry, microstructure and piezoelectric properties are discussed. 6 refs., 3 figs

  7. Tritium release from lithium titanate, a low-activation tritium breeding material

    International Nuclear Information System (INIS)

    Kopasz, J.P.; Miller, J.M.; Johnson, C.E.

    1994-01-01

    The goals for fusion power are to produce energy in as safe, economical, and environmentally benign a manner as possible. To ensure environmentally sound operation low-activation materials should be used where feasible. The ARIES Tokamak Reactor Study has based reactor designs on the concept of using low-activation materials throughout the fusion reactor. For the tritium breeding blanket, the choices for low activation tritium breeding materials are limited. Lithium titanate is an alternative low-activation ceramic material for use in the tritium breeding blanket. To date, very little work has been done on characterizing the tritium release for lithium titanate. We have thus performed laboratory studies of tritium release from irradiated lithium titanate. The results indicate that tritium is easily removed from lithium titanate at temperatures as low as 600 K. The method of titanate preparation was found to affect the tritium release, and the addition of 0.1% H 2 to the helium purge gas did not improve tritium recovery. ((orig.))

  8. In Vitro Comparison of the Bond Strength between Ceramic Repair Systems and Ceramic Materials and Evaluation of the Wettability.

    Science.gov (United States)

    Kocaağaoğlu, Hasan; Manav, Taha; Albayrak, Haydar

    2017-04-01

    When fracture of an all-ceramic restoration occurs, it can be necessary to repair without removing the restoration. Although there are many studies about the repair of metal-ceramic restorations, there are few about all-ceramic restorations. The aim of this study was to evaluate the shear bond strength between ceramic repair systems and esthetic core materials and to evaluate the wettability of all-ceramic core materials. Disk-like specimens (N = 90) made of three dental ceramic infrastructure materials (zirconia ceramic, alumina ceramic, glass ceramic) were polished with silicon carbide paper, prepared for bonding (abrasion with 30 μm diamond rotary cutting instrument). Thirty specimens of each infrastructure were obtained. Each infrastructure group was divided into three subgroups; they were bonded using 3 repair systems: Bisco Intraoral Repair Kit, Cimara & Cimara Zircon Repair System, and Clearfil Repair System. After 1200 thermocycles, shear bond strength was measured in a universal testing machine at a 0.5 mm/min crosshead speed. In addition, the contact angle values of the infrastructures after surface treatments were examined for wettability. Data were analyzed by using ANOVA and Tukey post hoc tests. Although there were no significant differences among the repair systems (p > 0.05) in the glass ceramic and zirconia groups, a significant difference was found among the repair systems in alumina infrastructure (p 0.05); however, a statistically significant difference was found among the repair systems (p < 0.05). No difference was found among the infrastructures and repair systems in terms of contact angle values. Cimara & Cimara Zircon Repair System had higher bond strength values than the other repair systems. Although no difference was found among the infrastructures and repair systems, contact wettability angle was decreased by surface treatments compared with polished surfaces. © 2015 by the American College of Prosthodontists.

  9. Formation and corrosion of a 410 SS/ceramic composite

    Energy Technology Data Exchange (ETDEWEB)

    Chen, X., E-mail: xin.chen@anl.gov [Civil and Materials Engineering Department, University of Illinois at Chicago, 842 W. Taylor St., Chicago, IL 60607 (United States); Nuclear Engineering Division, Argonne National Laboratory, 9700 S Cass Ave, Lemont, IL 60439 (United States); Ebert, W.L. [Nuclear Engineering Division, Argonne National Laboratory, 9700 S Cass Ave, Lemont, IL 60439 (United States); Indacochea, J.E. [Civil and Materials Engineering Department, University of Illinois at Chicago, 842 W. Taylor St., Chicago, IL 60607 (United States)

    2016-11-15

    This study addressed the possible use of alloy/ceramic composite waste forms to immobilize metallic and oxide waste streams generated during the electrochemical reprocessing of spent reactor fuel using a single waste form. A representative composite material was made to evaluate the microstructure and corrosion behavior at alloy/ceramic interfaces by reacting 410 stainless steel with Zr, Mo, and a mixture of lanthanide oxides. Essentially all of the available Zr reacted with lanthanide oxides to generate lanthanide zirconates, which combined with the unreacted lanthanide oxides to form a porous ceramic network that filled with alloy to produce a composite puck. Alloy present in excess of the pore volume of the ceramic generated a metal bead on top of the puck. The alloys in the composite and forming the bead were both mixtures of martensite grains and ferrite grains bearing carbide precipitates; FeCrMo intermetallic phases also precipitated at ferrite grain boundaries within the composite puck. Micrometer-thick regions of ferrite surrounding the carbides were sensitized and corroded preferentially in electrochemical tests. The lanthanide oxides dissolved chemically, but the lanthanide zirconates did not dissolve and are suitable host phases. The presence of oxide phases did not affect corrosion of the neighboring alloy phases. - Highlights: • An alloy/ceramic composite was made to evaluate corrosion at phase boundaries. • Lanthanide oxides and Zr added to 410 steel reacted to form durable zirconates. • Corrosion behavior was evaluated using electrochemical tests and SEM analyses. • Regions of active, passive, galvanic, sensitized, and chemical corrosion observed. • The corrosion current was proportional to relative areas of active alloy phases.

  10. Electrospinning of Ceramic Solid Electrolyte Nanowires for Lithium-Ion Batteries with Enhanced Ionic Conductivity

    Science.gov (United States)

    Yang, Ting

    Solid electrolytes have great potential to address the safety issues of Li-ion batteries, but better synthesis methods are still required for ceramics electrolytes such as lithium lanthanum titanate (LLTO) and lithium lanthanum zirconate (LLZO). Pellets made from ceramic nanopowders using conventional sintering can be porous due to the agglomeration of nanoparticles (NPs). Electrospinning is a simple and versatile technique for preparing oxide ceramic nanowires (NWs) and was used to prepare electrospun LLTO and LLZO NWs. Pellets prepared from the electrospun LLTO NWs had higher density, less void space, and higher Li+ conductivity compared to those comprised of LLTO prepared with conventional sol-gel methods, which demonstrated the potential that electrospinning can provide towards improving the properties of sol-gel derived ceramics. Cubic phase LLZO was stabilized at room temperature in the form of electrospun NWs without extrinsic dopants. Bulk LLZO with tetragonal structure was transformed to the cubic phase using particle size reduction via ball milling. Heating conditions that promoted particle coalescence and grain growth induced a transformation from the cubic to tetragonal phase in both types of nanostructured LLZO. Composite polymer solid electrolyte was fabricated using LLZO NWs as the filler and showed an improved ionic conductivity at room temperature. Nuclear magnetic resonance studies show that LLZO NWs partially modify the polymer matrix and create preferential pathways for Li+ conduction through the modified polymer regions. Doping did not have significant effect on improving the overall conductivity as the interfaces played a predominant role. By comparing fillers with different morphologies and intrinsic conductivities, it was found that both NW morphology and high intrinsic conductivity are desired.

  11. Reconstruction of the domain orientation distribution function of polycrystalline PZT ceramics using vector piezoresponse force microscopy.

    Science.gov (United States)

    Kratzer, Markus; Lasnik, Michael; Röhrig, Sören; Teichert, Christian; Deluca, Marco

    2018-01-11

    Lead zirconate titanate (PZT) is one of the prominent materials used in polycrystalline piezoelectric devices. Since the ferroelectric domain orientation is the most important parameter affecting the electromechanical performance, analyzing the domain orientation distribution is of great importance for the development and understanding of improved piezoceramic devices. Here, vector piezoresponse force microscopy (vector-PFM) has been applied in order to reconstruct the ferroelectric domain orientation distribution function of polished sections of device-ready polycrystalline lead zirconate titanate (PZT) material. A measurement procedure and a computer program based on the software Mathematica have been developed to automatically evaluate the vector-PFM data for reconstructing the domain orientation function. The method is tested on differently in-plane and out-of-plane poled PZT samples, and the results reveal the expected domain patterns and allow determination of the polarization orientation distribution function at high accuracy.

  12. Lithium ceramics: sol-gel preparation and tritium release; Ceramiques lithiees: elaboration sol-gel et relachement du tritium

    Energy Technology Data Exchange (ETDEWEB)

    Renoult, O

    1994-04-01

    Ceramics based on lithium aluminate (LiA1O{sub 2}), lithium zirconate (Li{sub 2}ZrO{sub 3}) and lithium titanate (Li{sub 2}TiO{sub 3}) are candidates as tritium breeder blanket materials for forthcoming nuclear fusion reactors. Lithium silico-aluminate Li{sub 4+x}A1{sub 4-3x}Si{sub 2x}O{sub 8} (0 {<=} x {<=} 0,25) powders were synthetized from alkoxyde-hydroxyde sol-gel route. By direct sintering at 850-1100 deg C (without prior calcination), ceramics with controlled stoichiometry and homogenous microstructure were obtained. We have also prepared, using a comparable method, Li{sub 2}Zr{sub 1-x}Ti{sub x}O{sub 3} (x = 0, x = 0,1 et x = 1) materials. All these ceramics, with different microstructures and compositions, have been tested in out-of-reactor experiments. Concerning lithium aluminate microporous ceramics, the silicon substitution leads to a significant improvement of the tritrium release. Classical models taking into account independent surface mechanisms are not able to describe correctly the observed tritium release kinetics. We show, using a simple model, that the release kinetics is in fact limited by an intergranular diffusion followed by a desorption. The delay in tritium release, which occurs when the ceramic compacity increases, is explained in terms of an enhancement of the ionic T{sup +} diffusion path length. The energy required for desorption includes a leading term independent of hydrogen contained in the sweep gas. This term is attributed to the limiting recombination step of T{sup +} in molecular species HTO. For similar microstructures, the facility of tritium release for the different studied materials is explained by three properties: the crystal structure of the ceramic, the acidity of oxides and finally the presence of electronic non-stoichiometric defects. (author). 89 refs., 50 figs., 2 tabs., 1 annexe.

  13. Microstructure evolution and electrical characterization of Lanthanum doped Barium Titanate (BaTiO{sub 3}) ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Billah, Masum, E-mail: masum.buet09@gmail.com; Ahmed, A., E-mail: jhinukbuetmme@gmail.com; Rahman, Md. Miftaur, E-mail: miftaurrahman@mme.buet.ac.bd [Department of Materials & Metallurgical Engineering, Bangladesh University of Engineering and Technology, Dhaka-1000 (Bangladesh); Mahbub, Rubbayat, E-mail: rubayyatm@gce.buet.ac.bd [Department of Glass and Ceramic Engineering, Bangladesh University of Engineering and Technology, Dhaka-1000 (Bangladesh); Gafur, M. A., E-mail: d-r-magafur@bcsir.gov.bd [Bangladesh Council of Scientific & Industrial Research (BCSIR), Dhaka-1205 (Bangladesh); Bashar, M. Shahriar, E-mail: bashar@agni.com [Institute of Fuel Research & Development, Bangladesh Council of Scientific & Industrial Research (BCSIR), Dhaka-1205 (Bangladesh)

    2016-07-12

    In the current work, we investigated the structural and dielectric properties of Lanthanum oxide (La{sub 2}O{sub 3}) doped Barium Titanate (BaTiO{sub 3}) ceramics and established a correlation between them. Solid state sintering method was used to dope BaTiO{sub 3} with 0.3, 0.5 and 0.7 mole% La{sub 2}O{sub 3} under different sintering parameters. The raw materials used were La{sub 2}O{sub 3} nano powder of ~80 nm grain size and 99.995% purity and BaTiO{sub 3} nano powder of 100 nm grain size and 99.99% purity. Grain size distribution and morphology of fracture surface of sintered pellets were examined by Field Emission Scanning Electron Microscope and X-Ray Diffraction analysis was conducted to confirm the formation of desired crystal structure. The research result reveal that grain size and electrical properties of BaTiO{sub 3} ceramic significantly enhanced for small amount of doping (up to 0.5 mole% La{sub 2}O{sub 3}) and then decreased with increasing doping concentration. Desired grain growth (0.80-1.3 µm) and high densification (<90% theoretical density) were found by proper combination of temperature, sintering parameters and doping concentration. We found the resultant stable value of dielectric constant was 10000-12000 at 100-300 Hz in the temperature range of 30°-50° C for 0.5 mole% La{sub 2}O{sub 3} with corresponding shift of curie temperature around 30° C. So overall this research showed that proper La{sup 3+} concentration can control the grain size, increase density, lower curie temperature and hence significantly improve the electrical properties of BaTiO{sub 3} ceramics.

  14. Dielectric silicone elastomers with mixed ceramic nanoparticles

    International Nuclear Information System (INIS)

    Stiubianu, George; Bele, Adrian; Cazacu, Maria; Racles, Carmen; Vlad, Stelian; Ignat, Mircea

    2015-01-01

    Highlights: • Composite ceramics nanoparticles (MCN) with zirconium dioxide and lead zirconate. • Dielectric elastomer films wDith PDMS matrix and MCN as dielectric filler. • Hydrophobic character—water resistant and good flexibility specific to siloxanes. • Increased value of dielectric constant with the content of MCN in dielectric films. • Increased energy output from uniaxial deformation of the dielectric elastomer films. - Abstract: A ceramic material consisting in a zirconium dioxide-lead zirconate mixture has been obtained by precipitation method, its composition being proved by wide angle X-ray powder diffraction and energy-dispersive X-ray spectroscopy. The average diameter of the ceramic particles ranged between 50 and 100 nm, as revealed by transmission electron microscopy images. These were surface treated and used as filler for a high molecular mass polydimethylsiloxane-α,ω-diol (Mn = 450,000) prepared in laboratory, the resulted composites being further processed as films and crosslinked. A condensation procedure, unusual for polydimethylsiloxane having such high molecular mass, with a trifunctional silane was approached for the crosslinking. The effect of filler content on electrical and mechanical properties of the resulted materials was studied and it was found that the dielectric permittivity of nanocomposites increased in line with the concentration of ceramic nanoparticles

  15. Dielectric silicone elastomers with mixed ceramic nanoparticles

    Energy Technology Data Exchange (ETDEWEB)

    Stiubianu, George, E-mail: george.stiubianu@icmpp.ro [“Petru Poni” Institute of Macromolecular Chemistry, Aleea Gr. Ghica Voda 41A, Iasi 700487 (Romania); Bele, Adrian; Cazacu, Maria; Racles, Carmen; Vlad, Stelian [“Petru Poni” Institute of Macromolecular Chemistry, Aleea Gr. Ghica Voda 41A, Iasi 700487 (Romania); Ignat, Mircea [National R& D Institute for Electrical Engineering ICPE-CA Bucharest, Splaiul Unirii 313, District 3, Bucharest 030138 (Romania)

    2015-11-15

    Highlights: • Composite ceramics nanoparticles (MCN) with zirconium dioxide and lead zirconate. • Dielectric elastomer films wDith PDMS matrix and MCN as dielectric filler. • Hydrophobic character—water resistant and good flexibility specific to siloxanes. • Increased value of dielectric constant with the content of MCN in dielectric films. • Increased energy output from uniaxial deformation of the dielectric elastomer films. - Abstract: A ceramic material consisting in a zirconium dioxide-lead zirconate mixture has been obtained by precipitation method, its composition being proved by wide angle X-ray powder diffraction and energy-dispersive X-ray spectroscopy. The average diameter of the ceramic particles ranged between 50 and 100 nm, as revealed by transmission electron microscopy images. These were surface treated and used as filler for a high molecular mass polydimethylsiloxane-α,ω-diol (Mn = 450,000) prepared in laboratory, the resulted composites being further processed as films and crosslinked. A condensation procedure, unusual for polydimethylsiloxane having such high molecular mass, with a trifunctional silane was approached for the crosslinking. The effect of filler content on electrical and mechanical properties of the resulted materials was studied and it was found that the dielectric permittivity of nanocomposites increased in line with the concentration of ceramic nanoparticles.

  16. Piezoelectric ceramic implants: in vivo results.

    Science.gov (United States)

    Park, J B; Kelly, B J; Kenner, G H; von Recum, A F; Grether, M F; Coffeen, W W

    1981-01-01

    The suitability of barium titanate (BaTiO3) ceramic for direct substitution of hard tissues was evaluated using both electrically stimulated (piezoelectric) and inactive (nonpolarized) test implants. Textured cylindrical specimens, half of them made piezoelectric by polarization in a high electric field, were implanted into the cortex of the midshaft region of the femora of dogs for various periods of time. Interfacial healing and bio-compatibility of the implant material were studied using mechanical, microradiographical, and histological techniques. Our results indicate that barium titanate ceramic shows a very high degree of biocompatibility as evidenced by the absence of inflammatory or foreign body reactions at the implant-tissue interface. Furthermore, the material and its surface porosity allowed a high degree of bone ingrowth as evidenced by microradiography and a high degree of interfacial tensile strength. No difference was found between the piezoelectric and the electrically neutral implant-tissue interfaces. Possible reasons for this are discussed. The excellent mechanical properties of barium titanate, its superior biocompatibility, and the ability of bone to form a strong mechanical interfacial bond with it, makes this material a new candidate for further tests for hard tissue replacement.

  17. High temperature dielectric relaxation anomaly of Y3+ and Mn2+ doped barium strontium titanate ceramics

    International Nuclear Information System (INIS)

    Yan, Shiguang; Mao, Chaoliang; Wang, Genshui; Yao, Chunhua; Cao, Fei; Dong, Xianlin

    2014-01-01

    Relaxation like dielectric anomaly is observed in Y 3+ and Mn 2+ doped barium strontium titanate ceramics when the temperature is over 450 K. Apart from the conventional dielectric relaxation analysis method with Debye or modified Debye equations, which is hard to give exact temperature dependence of the relaxation process, dielectric response in the form of complex impedance, assisted with Cole-Cole impedance model corrected equivalent circuits, is adopted to solve this problem and chase the polarization mechanism in this paper. Through this method, an excellent description to temperature dependence of the dielectric relaxation anomaly and its dominated factors are achieved. Further analysis reveals that the exponential decay of the Cole distribution parameter n with temperature is confirmed to be induced by the microscopic lattice distortion due to ions doping and the interaction between the defects. At last, a clear sight to polarization mechanism containing both the intrinsic dipolar polarization and extrinsic distributed oxygen vacancies hopping response under different temperature is obtained.

  18. Giant Electric Field Control of Magnetism and Narrow Ferromagnetic Resonance Linewidth in FeCoSiB/Si/SiO2/PMN PT Multiferroic Heterostructures (Open Access Author’s Manuscript)

    Science.gov (United States)

    2016-06-06

    the widely used lead zirconate titanate ceramics which have a typical piezoelectric coefficient d31 of ~- 200pC/N, PMN-PT single crystals used in...substrate clamping effect, therefore, a relatively giant tunability can be obtained. However, the normally large roughness of piezoelectric layer...is the saturation magnetostriction constant, Y the Young’s modulus of the magnetic film, deff the effective piezoelectric coefficient, E

  19. Toward a unified description of nonlinearity and frequency dispersion of piezoelectric and dielectric responses in Pb(Zr,Ti)O3

    International Nuclear Information System (INIS)

    Damjanovic, D.; Bharadwaja, S.S.N.; Setter, N.

    2005-01-01

    A phenomenological approach is proposed describing both nonlinearity and frequency dispersion in dielectric and piezoelectric properties of lead zirconate titanate, Pb(Zr,Ti)O 3 (PZT), thin films and ceramics. The approach couples the frequency dependent response in form of the power law, 1/ω β , with the rate-independent nonlinear response described by the Rayleigh law. The main experimental trends are well described by the model

  20. Ion-implanted PLZT ceramics: a new high-sensitivity image storage medium

    International Nuclear Information System (INIS)

    Peercy, P.S.; Land, C.E.

    1980-01-01

    Results were presented of our studies of photoferroelectric (PFE) image storage in H- and He-ion implanted PLZT (lead lanthanum zirconate titanate) ceramics which demonstrate that the photosensitivity of PLZT can be significantly increased by ion implantation in the ceramic surface to be exposed to image light. More recently, implantations of Ar and Ar + Ne into the PLZT surface have produced much greater photosensitivity enhancement. For example, the photosensitivity after implantation with 1.5 x 10 14 350 keV Ar/cm 2 + 1 x 10 15 500 keV Ne/cm 2 is increased by about four orders of magnitude over that of unimplanted PLZT. Measurements indicate that the photosensitivity enhancement in ion-implanted PLZT is controlled by implantation-produced disorder which results in marked decreases in dielectric constant and dark conductivity and changes in photoconductivity of the implanted layer. The effects of Ar- and Ar + Ne-implantation are presented along with a phenomenological model which describes the enhancement in photosensitivity obtained by ion implantation. This model takes into account both light- and implantation-induced changes in conductivity and gives quantitative agreement with the measured changes in the coercive voltage V/sub c/ as a function of near-uv light intensity for both unimplanted and implanted PLZT. The model, used in conjunction with calculations of the profiles of implantation-produced disorder, has provided the information needed for co-implanting ions of different masses, e.g., Ar and Ne, to improve photosensitivity

  1. Stress- and temperature-dependent scaling behavior of dynamic hysteresis in soft PZT bulk ceramics

    International Nuclear Information System (INIS)

    Yimnirun, R; Wongsaenmai, S; Wongmaneerung, R; Wongdamnern, N; Ngamjarurojana, A; Ananta, S; Laosiritaworn, Y

    2007-01-01

    Effects of electric field-frequency, electric field-amplitude, mechanical stress, and temperature on the hysteresis area, especially the scaling form, were investigated in soft lead zirconate titanate (PZT) bulk ceramics. The hysteresis area was found to depend on the frequency and field-amplitude with the same set of exponents as the power-law scaling for both with and without stresses. The inclusion of stresses into the power-law was obtained in the form of σ=0 > ∝ f -0.25 E 0 σ 0.45 which indicates the difference in energy dissipation between the under-stress and stress-free conditions. The power-law temperature scaling relations were obtained for hysteresis area (A) and remanent polarization P r , while the coercivity E C was found to scale linearly with temperature T. The three temperature scaling relations were also field-dependent. At fixed field amplitude E 0 , the scaling relations take the forms of ∝ T -1.1024 , P r ∼T -1.2322 and (E C0 - E C ) ∼T

  2. Piezoelectric displacement in ceramics

    International Nuclear Information System (INIS)

    Stewart, M.; Cain, M.; Gee, M.

    1999-01-01

    This Good Practice Guide is intended to aid a user to perform displacement measurements on piezoelectric ceramic materials such as PZT (lead zirconium titanate) in either monolithic or multilayer form. The various measurement issues that the user must consider are addressed, and good measurement practise is described for the four most suitable methods. (author)

  3. Cerium-modified Aurivillius-type sodium lanthanum bismuth titanate with enhanced piezoactivities

    International Nuclear Information System (INIS)

    Wang Chunming; Zhao Liang; Wang Jinfeng; Zheng Limei; Du Juan; Zhao Minglei; Wang Chunlei

    2009-01-01

    The electrical, piezoelectric and dielectric properties of cerium-modified Aurivillius-type sodium lanthanum bismuth titanate (Na 0.5 La 0.5 Bi 4 Ti 4 O 15 , NLBT) ceramics were investigated. It was found the piezoelectric activities of NLBT ceramics were significantly improved by cerium modification. The piezoelectric coefficient d 33 and Curie temperature T c for the 0.50 wt.% cerium-modified NLBT were found to be 29 pC/N and 573 deg. C, respectively. The reasons for piezoelectric activities improvement by cerium modification were given. A small dielectric abnormity was observed in NLBT ceramics, which can be suppressed by cerium modification.

  4. UV laser micromachining of piezoelectric ceramic using a pulsed Nd:YAG laser

    International Nuclear Information System (INIS)

    Zeng, D.W.; Xie, C.S.; Li, K.; Chan, H.L.W.; Choy, C.L.; Yung, K.C.

    2004-01-01

    UV laser (λ=355 nm) ablation of piezoelectric lead zirconate titanate (PZT) ceramics in air has been investigated under different laser parameters. It has been found that there is a critical pulse number (N=750). When the pulse number is smaller than the critical value, the ablation rate decreases with increasing pulse number. Beyond the critical value, the ablation rate becomes constant. The ablation rate and concentrations of O, Zr and Ti on the ablated surface increase with the laser fluence, while the Pb concentration decreases due to the selective evaporation of PbO. The loss of the Pb results in the formation of a metastable pyrochlore phase. ZrO 2 was detected by XPS in the ablated zone. Also, the concentrations of the pyrochlore phase and ZrO 2 increase with increasing laser fluence. These results clearly indicate that the chemical composition and phase structure in the ablated zone strongly depend on the laser fluence. The piezoelectric properties of the cut PZT ceramic samples completely disappear due to the loss of the Pb and the existence of the pyrochlore phase. After these samples were annealed at 1150 C for 1 h in a PbO-controlled atmosphere, their phase structure and piezoelectric properties were recovered again. Finally, 1-3 and concentric-ring 2-2 PZT/epoxy composites were fabricated by UV laser micromachining and their thickness modes were measured by impedance spectrum analysis and a d 33 meter. Both composites show high piezoelectric properties. (orig.)

  5. Ultrasonic testing device

    International Nuclear Information System (INIS)

    Lawrie, W.E.

    1978-01-01

    The ultrasonic transmitter made of polarized ferroelectric ceramic material (lead zirconate titanate) is arranged in a strip carrier which allows it to be introduced between the fuel elements of a fuel subassembly in a water cooled nuclear reactor. The ultrasonic transmitter is insulated relative to the carrier. The echo of the ra dal ultrasonic pulse is recorded which changes as faulty water filled fuel elements are detected. (RW) [de

  6. Microelectromechanical Systems (MEMS) Photoacoustic (PA) Detector of Terahertz (THz) Radiation for Chemical Sensing

    Science.gov (United States)

    2014-03-01

    films. The seed layer established the desired orientation and texture for the preferential crystal formation of the PZT . Deposited by chemical...34Stoichiometry and crystal orientation of YAG-PLD derived ferroelectric PZT thin film," Journal of the European Ceramic Society, vol. 24, no. 6, pp...results performed on the lead zirconate titanate ( PZT ) target used in previous attempts at fabricating piezoelectric cantilever. It is shown that the

  7. International Infantry and Joint Services Small Arms Systems Section Symposium, Exhibition and Firing Demonstration. Held in Atlantic City, NJ on 13-16 May 2002. Volume 2

    Science.gov (United States)

    2002-05-13

    going efforts to gather data Types of Sound Generation Sources • Piezo - Electric – High Performance Speakers & Ceramics – Smallest Volume Package...40-µm DRIE spring Stage 2 Devices-Fab 2 Texture of DRIE- machined surface Details of undercutting and release etch for 40-µm spring 1 Tank-automotive... PZT -5A Piezoceramic Sheets Nomenclature - Lead-Zirconate Titanate Micro-Flex Actuator* * Fundamentals of Adaptive/Smart Aerostructures Short Course

  8. Crystalline ceramics: Waste forms for the disposal of weapons plutonium

    International Nuclear Information System (INIS)

    Ewing, R.C.; Lutze, W.; Weber, W.J.

    1995-05-01

    At present, there are three seriously considered options for the disposition of excess weapons plutonium: (i) incorporation, partial burn-up and direct disposal of MOX-fuel; (ii) vitrification with defense waste and disposal as glass ''logs''; (iii) deep borehole disposal (National Academy of Sciences Report, 1994). The first two options provide a safeguard due to the high activity of fission products in the irradiated fuel and the defense waste. The latter option has only been examined in a preliminary manner, and the exact form of the plutonium has not been identified. In this paper, we review the potential for the immobilization of plutonium in highly durable crystalline ceramics apatite, pyrochlore, monazite and zircon. Based on available data, we propose zircon as the preferred crystalline ceramic for the permanent disposition of excess weapons plutonium

  9. Formation and corrosion of a 410 SS/ceramic composite

    Science.gov (United States)

    Chen, X.; Ebert, W. L.; Indacochea, J. E.

    2016-11-01

    This study addressed the possible use of alloy/ceramic composite waste forms to immobilize metallic and oxide waste streams generated during the electrochemical reprocessing of spent reactor fuel using a single waste form. A representative composite material was made to evaluate the microstructure and corrosion behavior at alloy/ceramic interfaces by reacting 410 stainless steel with Zr, Mo, and a mixture of lanthanide oxides. Essentially all of the available Zr reacted with lanthanide oxides to generate lanthanide zirconates, which combined with the unreacted lanthanide oxides to form a porous ceramic network that filled with alloy to produce a composite puck. Alloy present in excess of the pore volume of the ceramic generated a metal bead on top of the puck. The alloys in the composite and forming the bead were both mixtures of martensite grains and ferrite grains bearing carbide precipitates; FeCrMo intermetallic phases also precipitated at ferrite grain boundaries within the composite puck. Micrometer-thick regions of ferrite surrounding the carbides were sensitized and corroded preferentially in electrochemical tests. The lanthanide oxides dissolved chemically, but the lanthanide zirconates did not dissolve and are suitable host phases. The presence of oxide phases did not affect corrosion of the neighboring alloy phases.

  10. Phase transitions of Pb(ZrxTi1-x)O3 ceramics

    International Nuclear Information System (INIS)

    Frantti, J.; Kakihana, M.; Ivanov, S.; Eriksson, S.; Rundloef, H.; Lantto, V.; Lappalainen, J.

    2002-01-01

    Recent experimental and theoretical reports on the structure of lead zirconate titanate [Pb(Zr x Ti 1-x )O 3 (PZT)] ceramics with compositions in the vicinity of the morphotropic phase boundary are discussed. There has been ambiguity concerning the low-temperature structure of x=0.52 samples, due to the superlattice reflections which were not explained by the reported monoclinic phase Cm [B. Noheda, D. E. Cox, G. Shirane, R. Guo, B. Jones, and L. E. Cross, Phys. Rev. B 63, 014103 (2001)]. Neutron powder diffraction (NPD) and Rietveld refinement were used to identify the space group symmetries of x=0.52 and x=0.53 samples at 10 K. Both samples had two coexisting phases R3c and Cm at 10 K. At 10 K, monoclinic angles of both samples were larger than at 295 K, as was the octahedral tilt angle of the R3c phase of the x=0.53 sample. We analyzed our previous and current NPD data to study the structural changes in PZT ceramics, 0.20≤x≤0.53, as a function of x and temperature. Bond-valence calculations were carried out to test the models used in Rietveld refinements. Valences of Zr and Ti ions were larger and smaller than their nominal valences, respectively, although the anomaly decreased with increasing x. The composition-weighted-average valence of Zr and Ti ions was close to +4, and the relationship between the positions and valences of Zr and Ti ions explains the main structural features of PZT ceramics as a function of x. The valence of Pb ions was slightly below +2 and decreased with increasing x until it started to slightly increase for x≥0.50. Average oxygen valency was found to be close to -2. Also spontaneous polarization values were computed and found to be reasonable

  11. Ceramic-polymer nanocomposites with increased dielectric permittivity and low dielectric loss

    International Nuclear Information System (INIS)

    Bhardwaj, Sumit; Paul, Joginder; Raina, K. K.; Thakur, N. S.; Kumar, Ravi

    2014-01-01

    The use of lead free materials in device fabrication is very essential from environmental point of view. We have synthesized the lead free ferroelectric polymer nanocomposite films with increased dielectric properties. Lead free bismuth titanate has been used as active ceramic nanofillers having crystallite size 24nm and PVDF as the polymer matrix. Ferroelectric β-phase of the polymer composite films was confirmed by X-ray diffraction pattern. Mapping data confirms the homogeneous dispersion of ceramic particles into the polymer matrix. Frequency dependent dielectric constant increases up to 43.4 at 100Hz, whereas dielectric loss decreases with 7 wt% bismuth titanate loading. This high dielectric constant lead free ferroelectric polymer films can be used for energy density applications

  12. Zirconia-based colors for ceramic glazes

    International Nuclear Information System (INIS)

    Eppler, R.A.

    1977-01-01

    The history of color development for use in ceramic glazes is outlined. The most significant modern development is based on zirconia and zircon. These materials have gained increasing acceptance in the industry since their introduction in the late 1950's and early 1960's, due to their superior stability during firing of the glaze

  13. Effect of dielectrophoretic structuring on piezoelectric and pyroelectric properties of lead titanate-epoxy composites

    NARCIS (Netherlands)

    Khanbareh, H.; Zwaag, S. van der; Groen, W.A.

    2014-01-01

    Functional granular composites of lead titanate particles in an epoxy matrix prepared by dielectrophoresis show enhanced dielectric, piezoelectric and pyroelectric properties compared to 0-3 composites for different ceramic volume content from 10% to 50%. Two structuring parameters, the

  14. Wear and microstructural characteristics of spray atomized zircon sand reinforced LM13 alloy

    Energy Technology Data Exchange (ETDEWEB)

    Kaur, K.; Pandey, O.P. [School of Physics and Materials Science, Thapar University Patiala, Punjab (India)

    2010-07-15

    The requirement of the high performance light weight materials demands the development of varieties of materials within the economical range to get it commercialized. Light weight aluminium alloys are used in several structural applications like automotive, aerospace, defense industry and other fields of engineering. The ceramic particle reinforced aluminium metal matrix composites (AMCs) have emerged as a suitable candidate for commercial applications. A variety of processing routes have been adopted to manufacture AMCs. In the present work LM13 alloy reinforced with zircon sand is formed via spray forming. During experimentation a self prepared convergent-divergent nozzle is used for inert gas atomization of the melt which is subsequently deposited on copper substrate placed vertically below the atomizer. The zircon sand particles are injected in the atomization zone by external injectors aligned perpendicular to the gas atomization axis. Zircon sand has been found to have new promising economical commercial candidate due to its easy availability and good mechanical properties like high hardness, high modulus of elasticity and good thermal stability. The microhardness of cast alloy and spray formed composite shows that the spray formed zircon sand reinforced composite has higher hardness. Also the lower wear rate has been observed in case of the zircon sand reinforced AMC as compared to LM13 alloy. This behaviour is further analyzed in light of microstructural features of the spray deposited composite using optical and scanning electron microscope (SEM). A comparative study of this material (LM13/Zircon sand) with the parent alloy (LM13) is presented in this work. (Abstract Copyright [2010], Wiley Periodicals, Inc.)

  15. Electrical Degradation in Ceramic Dielectrics

    Science.gov (United States)

    1988-09-09

    and D. M. Smyth, " Positron Annihilation in Calcium-Doped Barium Titanate", in Electro- Ceramics and Solid State Ionsi, H. L. Tuller and D. M. Smyth...2 with the formation of ompensating oxygen vacancies, and this causes an increase in the ioni conductivity: 2CaO CaC + Call + 20 + (5) TiO2 --- V

  16. Improvement of transmission loss of a double panel by using active control with a virtual modal mass

    OpenAIRE

    Lhuillier , Vincent; Chesné , Simon; Gaudiller , Luc; Pezerat , Charles

    2013-01-01

    International audience; In this article, modal feedback control is proposed to reduce the sound transmission through finite double panels using lead zirconate titanate ceramic sensors and actuators bonded to the structure. Active control allows adding virtual modal damping and mass to the structure by the use of modal velocities and accelerations. In a first step, the equations describing the structure, the actuators, the acoustic excitation, and the acoustic radiation are detailed. Next, the...

  17. Thermoluminescence study of materials (natural minerals) used in ceramic tiles industry

    Energy Technology Data Exchange (ETDEWEB)

    Murthy, K V R, E-mail: drmurthykvr@yahoo.com [Display Materials Laboratory Applied Physics Department Faculty of Technology and Engineering M.S. University of Baroda, Baroda-390 001 (India)

    2009-07-15

    Mother earth is giving many materials in the natural form as well as in mineral form. Among them the marbles, granites and other variety of slabs for house hold flooring purposes. The people demand for variety of flooring materials leads to develop various types of ceramic tile. In India ceramic tiles industry is one of the fast growing one. More than two hundred units are manufacturing the ceramic tiles situated around Morbi, Rajkot, Gujarat, India. The basic raw materials required for manufacturing the various types of ceramic tiles are natural minerals. The following are the minerals used to manufacture the ceramic tiles i.e. quartz, feldspar, zircon, china clay, talc, grok, Aluminum oxide etc.,

  18. Thermoluminescence study of materials (natural minerals) used in ceramic tiles industry

    International Nuclear Information System (INIS)

    Murthy, K V R

    2009-01-01

    Mother earth is giving many materials in the natural form as well as in mineral form. Among them the marbles, granites and other variety of slabs for house hold flooring purposes. The people demand for variety of flooring materials leads to develop various types of ceramic tile. In India ceramic tiles industry is one of the fast growing one. More than two hundred units are manufacturing the ceramic tiles situated around Morbi, Rajkot, Gujarat, India. The basic raw materials required for manufacturing the various types of ceramic tiles are natural minerals. The following are the minerals used to manufacture the ceramic tiles i.e. quartz, feldspar, zircon, china clay, talc, grok, Aluminum oxide etc.,

  19. Structural and functional characterization of barium zirconium titanate / epoxy composites

    Directory of Open Access Journals (Sweden)

    Filiberto González Garcia

    2011-12-01

    Full Text Available The dielectric behavior of composite materials (barium zirconium titanate / epoxy system was analyzed as a function of ceramic concentration. Structure and morphologic behavior of the composites was investigated by X-ray Diffraction (XRD, Fourier transformed infrared spectroscopy (FT-IR, Raman spectroscopy, field emission scanning electron microscopy (FE-SEM and transmission electron microscopy (TEM analyses. Composites were prepared by mixing the components and pouring them into suitable moulds. It was demonstrated that the amount of inorganic phase affects the morphology of the presented composites. XRD revealed the presence of a single phase while Raman scattering confirmed structural transitions as a function of ceramic concentration. Changes in the ceramic concentration affected Raman modes and the distribution of particles along into in epoxy matrix. Dielectric permittivity and dielectric losses were influenced by filler concentration.

  20. Development of Advanced Materials for Electro-Ceramic Application Final Report CRADA No. TC-1331-96

    Energy Technology Data Exchange (ETDEWEB)

    Caplan, M. [Lawrence Livermore National Lab. (LLNL), Livermore, CA (United States); Olstad, R. [General Atomics, San Diego, CA (United States); McMillan, L. [Symetrix International, Inc., Colorado Springs, CO (United States); Tulupov, A. [Soliton-NTT, Moscow (Russia)

    2017-10-19

    The goal of this project was to further develop and characterize the electrochemical methods originating in Russia for producing ultra high purity organometallic compounds utilized as precursors in the production of high quality electro-ceramic materials. Symetrix planned to use electro-ceramic materials with high dielectric constant for microelectronic memory circuit applications. General Atomics planned to use the barium titanate type ceramics with low loss tangent for producing a high power ferroelectric tuner used to match radio frequency power into their Dill-D fusion machine. Phase I of the project was scheduled to have a large number of organometallic (alkoxides) chemical samples produced using various methods. These would be analyzed by LLNL, Soliton and Symetrix independently to determine the level of chemical impurities thus verifying each other's analysis. The goal was to demonstrate a cost-effective production method, which could be implemented in a large commercial facility to produce high purity organometallic compounds. In addition, various compositions of barium-strontium-titanate ceramics were to be produced and analyzed in order to develop an electroceramic capacitor material having the desired characteristics with respect to dielectric constant, loss tangent, temperature characteristics and non-linear behavior under applied voltage. Upon optimizing the barium titanate material, 50 capacitor preforms would be produced from this material demonstrating the ability to produce, in quantity, the pills ultimately required for the ferroelectric tuner (approx 2000-3000 ceramic pills).

  1. Characterization of domain reorientation in Pzt ceramics

    International Nuclear Information System (INIS)

    Lente, Manuel Henrique; Povoa, Jose Marques; Eiras, Jose Antonio

    1997-01-01

    The dynamic of domains in ferroelectric materials has been intensively studied due to its importance in applications like non volatile memories. Domain reorientation was characterized in lead zirconate titanate samples, pure and doped, through measurements of the transient current, after reversal a electric field. The reorientation behavior of the domains showed to be influenced by type of impurity (Nb or Fe) and by the electrical field intensity. Analysis of the experimental results reveals mainly the existence of two contributions: a dependent (t 0.1 s) of the field intensity. (author)

  2. Titan

    Science.gov (United States)

    Müller-Wodarg, Ingo; Griffith, Caitlin A.; Lellouch, Emmanuel; Cravens, Thomas E.

    2014-03-01

    Introduction I. C. F. Müller-Wodarg, C. A. Griffith, E. Lellouch and T. E. Cravens; Prologue 1: the genesis of Cassini-Huygens W.-H. Ip, T. Owen and D. Gautier; Prologue 2: building a space flight instrument: a P.I.'s perspective M. Tomasko; 1. The origin and evolution of Titan G. Tobie, J. I. Lunine, J. Monteux, O. Mousis and F. Nimmo; 2. Titan's surface geology O. Aharonson, A. G. Hayes, P. O. Hayne, R. M. Lopes, A. Lucas and J. T. Perron; 3. Thermal structure of Titan's troposphere and middle atmosphere F. M. Flasar, R. K. Achterberg and P. J. Schinder; 4. The general circulation of Titan's lower and middle atmosphere S. Lebonnois, F. M. Flasar, T. Tokano and C. E. Newman; 5. The composition of Titan's atmosphere B. Bézard, R. V. Yelle and C. A. Nixon; 6. Storms, clouds, and weather C. A. Griffith, S. Rafkin, P. Rannou and C. P. McKay; 7. Chemistry of Titan's atmosphere V. Vuitton, O. Dutuit, M. A. Smith and N. Balucani; 8. Titan's haze R. West, P. Lavvas, C. Anderson and H. Imanaka; 9. Titan's upper atmosphere: thermal structure, dynamics, and energetics R. V. Yelle and I. C. F. Müller-Wodarg; 10. Titan's upper atmosphere/exosphere, escape processes, and rates D. F. Strobel and J. Cui; 11. Titan's ionosphere M. Galand, A. J. Coates, T. E. Cravens and J.-E. Wahlund; 12. Titan's magnetospheric and plasma environment J.-E. Wahlund, R. Modolo, C. Bertucci and A. J. Coates.

  3. Photovoltaic effect in ferroelectric ceramics

    Science.gov (United States)

    Epstein, D. J.; Linz, A.; Jenssen, H. P.

    1982-01-01

    The ceramic structure was simulated in a form that is more tractable to correlation between experiment and theory. Single crystals (of barium titanate) were fabricated in a simple corrugated structure in which the pedestals of the corrugation simulated the grain while the intervening cuts could be filled with materials simulating the grain boundaries. The observed photovoltages were extremely small (100 mv).

  4. Zirconium titanate: stability and thermal expansion; Titanato de circonio: estabilidad termodinamica y expansion termica

    Energy Technology Data Exchange (ETDEWEB)

    Lopez-Lopez, E.; Moreno, R.; Baudin, C.

    2011-07-01

    Zirconium titanate is a well known compound in the field of electro ceramics, although it has also been used in catalyst and sensors applications. The crystallographic thermal expansion anisotropy of this compound makes it a potential candidate as constituent of structural components. In general, to assure the structural integrity and microstructural homogeneity of a ceramic piece, relatively low cooling rates from the fabrication temperature are required. This requirement is essential for zirconium titanate because thermal expansion as well as phase distribution is affected by small variations in the composition and cooling rate. This work reviews the available data on the phase equilibrium relationships in the systems ZrO{sub 2}-TiO{sub 2} and ZrO{sub 2}-TiO{sub 2}-Y{sub 2}O{sub 3}. The main discrepancies as well as the possible origins of them are discussed. Additionally, the crystallographic thermal expansion data in the current literature are reviewed. (Author) 56 refs.

  5. Summary of ceramic pigments by polymer precursors Pechini method

    International Nuclear Information System (INIS)

    Silva, E.M. da; Galvao, S.B.; Paskocimas, C.A.

    2010-01-01

    In this work were synthesized nitrate chromium nitrate and iron-doped titanium oxide by the polymeric precursor method, for application as ceramic pigments. The stains were developed between the temperatures 700 deg C to 1000 deg C, in green for chromium oxide and orange for iron. Noticing an increase of its opacity by increasing temperature. Characterization by thermogravimetry (TG) showed strong thermo decomposition from 355 deg C for the chromium oxide and thermo decomposition gradual for the iron. By analysis of X-ray diffraction revealed the formation of crystalline phases as Iron Titanate (FeTiO3) and Chrome Titanate (CrTiO3), respectively. The scanning electron microscopy showed the formation of rounded particles for both oxides. Thus, the synthesized oxides were within the requirements to be applied as pigments and shown to be possible to propose its use in ceramic materials. (author)

  6. Spark Plasma Sintering of Dielectric Ceramics Zr0.8Sn0.2TiO4

    Czech Academy of Sciences Publication Activity Database

    Ctibor, P.; Kubatík, Tomáš František; Sedláček, J.; Kotlan, Jiří

    2016-01-01

    Roč. 22, č. 3 (2016), s. 435-439 ISSN 1392-1320 Institutional support: RVO:61389021 Keywords : titanates * dielectric ceramics * spark plasma sintering Subject RIV: JH - Ceramics, Fire-Resistant Materials and Glass Impact factor: 0.393, year: 2016 http://www.matsc.ktu.lt/index.php/MatSc/article/view/8767

  7. Scandium doped Strontium Titanate Ceramics: Structure, Microstructure, and Dielectric Properties

    Directory of Open Access Journals (Sweden)

    Tkach, Alexander

    2008-08-01

    Full Text Available Sc-doped strontium titanate (ST ceramics were synthesised by solid state reaction, according to the composition Sr1-1.5xScxTiO3 with x = 0-0.01. Structural properties and microstructure development was examined by XRD and SEM. The dielectric properties were evaluated as a function of the temperature and frequency in the radio frequency range. Lattice parameter, density and grain size, were found to decrease slightly with increasing Sc content. The dielectric permittivity and losses decrease also. Sc-doping has only a weak effect on the quantum paraelectric behaviour of ST and no dielectric anomaly was observed, what is probably related to the limited solubility of Sc on the Sr site of the perovskite lattice of ST.

    Se sintetizaron materiales cerámicos de titanato de estroncio dopado con escandio mediante reacción en estado sólido De acuerdo a la composición Sr1-1.5xScxTiO3 con x= 0-0.1. Las propiedades estructurales y el desarrollo microestructural se estudiaron mediante XRD y SEM. La propiedades dieléctricas se estudiaron como función de la temperatura y de la frecuencia en el rango de la frecuencias de radio. Se observó que los parámetros de red, la densidad y el tamaño del grano disminuyen ligeramente con el contenido en Sc. La permitividad dieléctrica y las perdidas también disminuyen. El dopado con Sc tiene un efecto muy ligero sobre el comportamiento paraeléctrico cuántico del titanato de estroncio y no se observó anomalías dioeléctricas , lo que está probablemente relacionado con la baja solubilidad del Sc en posiciones del Sr en la estructura tipo perovskita del titanato de estroncio.

  8. Method of bistable optical information storage using antiferroelectric phase PLZT ceramics

    Science.gov (United States)

    Land, Cecil E.

    1990-01-01

    A method for bistable storage of binary optical information includes an antiferroelectric (AFE) lead lanthanum zirconate titanate (PLZT) layer having a stable antiferroelectric first phase and a ferroelectric (FE) second phase obtained by applying a switching electric field across the surface of the device. Optical information is stored by illuminating selected portions of the layer to photoactivate an FE to AFE transition in those portions. Erasure of the stored information is obtained by reapplying the switching field.

  9. X-ray and neutron scattering on disordered nanosize clusters: a case study of lead-zirconate-titanate solid solutions

    Energy Technology Data Exchange (ETDEWEB)

    Frantti, Johannes; Fujioka, Yukari [Finnish Research and Engineering, Helsinki (Finland)

    2015-04-01

    Defects and frequently used defect models of solids are reviewed. Signatures for identifying the disorder from x-ray and neutron scattering data are given. To give illustrative examples how technologically important defects contribute to x-ray and neutron scattering numerical method able to treat non-periodical solids possessing several simultaneous defect types is given for simulating scattering in nanosize disordered clusters. The approach takes particle size, shape, and defects into account and isolates element specific signals. As a case study a statistical approximation model for lead-zirconate titanate [Pb(Zr{sub x}Ti{sub 1-x})O{sub 3}, PZT] is introduced. PZT is a material possessing several defect types, including substitutional, displacement and surface defects. Spatial composition variation is taken into account by introducing a model in which the edge lengths of each cell depend on the distribution of Zr and Ti ions in the cluster. Spatially varying edge lengths and angles is referred to as microstrain. The model is applied to compute the scattering from ellipsoid shaped PZT clusters and to simulate the structural changes as a function of average composition. Two-phase co-existence range, the so called morphotropic phase boundary composition is given correctly. The composition at which the rhombohedral and tetragonal cells are equally abundant was x ∼ 0.51. Selected x-ray and neutron Bragg reflection intensities and line shapes were simulated. Examples of the effect of size and shape of the scattering clusters on diffraction patterns are given and the particle dimensions, computed through Scherrer equation, are compared with the exact cluster dimensions. Scattering from two types of 180 domains in spherical particles, one type assigned to Ti-rich PZT and the second to the MPB and Zr-rich PZT, is computed. We show how the method can be used for modelling polarization reversal. (copyright 2015 by WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  10. Dielectric behaviour of (Ba0.77Ca0.23(Ti0.98Dy0.02O3 ceramics

    Directory of Open Access Journals (Sweden)

    Abdul Moquim

    2015-06-01

    Full Text Available In this study, BaTiO3 is modified with Ca2+ and in addition doped with Dy3+ at the B site lattice. The main idea is to search for new lead-free ferroelectric material and improve their properties. For this purpose, the barium calcium titanate (BCT as a host and the rare earth element Dy3+ as an activator were used to fabricate a multifunctional material. The obtained ceramics was found to be homogeneous, dense and a single phase material with no evidence of secondary phases. The dielectric study showed that TC increases with the addition of dopants and the obtained ceramics behaves like a relaxor ferroelectric. Some important structural parameters and dielectric properties of dysprosium modified barium (calcium titanate ceramics are presented.

  11. Damage-free patterning of ferroelectric lead zirconate titanate thin films for microelectromechanical systems via contact printing

    Science.gov (United States)

    Welsh, Aaron

    This thesis describes the utilization and optimization of the soft lithographic technique, microcontact printing, to additively pattern ferroelectric lead zirconate titanate (PZT) thin films for application in microelectromechanical systems (MEMS). For this purpose, the solution wetting, pattern transfer, printing dynamics, stamp/substrate configurations, and processing damages were optimized for incorporation of PZT thin films into a bio-mass sensor application. This patterning technique transfers liquid ceramic precursors onto a device stack in a desired configuration either through pattern definition in the stamp, substrate or both surfaces. It was determined that for ideal transfer of the pattern from the stamp to the substrate surface, wetting between the solution and the printing surface is paramount. To this end, polyurethane-based stamp surfaces were shown to be wet uniformly by polar solutions. Patterned stamp surfaces revealed that printing from raised features onto flat substrates could be accomplished with a minimum feature size of 5 mum. Films patterned by printing as a function of thickness (0.1 to 1 mum) showed analogous functional properties to continuous films that were not patterned. Specifically, 1 mum thick PZT printed features had a relative permittivity of 1050 +/- 10 and a loss tangent of 2.0 +/- 0.4 % at 10 kHz; remanent polarization was 30 +/- 0.4 muC/cm 2 and the coercive field was 45 +/- 1 kV/cm; and a piezoelectric coefficient e31,f of -7 +/- 0.4 C/m2. No pinching in the minor hysteresis loops or splitting of the first order reversal curve (FORC) distributions was observed. Non-uniform distribution of the solution over the printed area becomes more problematic as feature size is decreased. This resulted in solutions printed from 5 mum wide raised features exhibiting a parabolic shape with sidewall angles of ˜ 1 degree. As an alternative, printing solutions from recesses in the stamp surface resulted in more uniform solution thickness

  12. Characterization of dense lead lanthanum titanate ceramics prepared from powders synthesized by the oxidant peroxo method

    Energy Technology Data Exchange (ETDEWEB)

    Pinto, Alexandre H. [LIEC-Laboratorio Interdisciplinar de Eletroquimica e Ceramica, Departamento de Quimica, UFSCar-Universidade Federal de Sao Carlos, Rod.Washington Luis km 235, CP 676 Sao Carlos, SP 13565-905 (Brazil); Souza, Flavio L., E-mail: flavio.souza@ufabc.edu.br [Centro de Ciencias Naturais e Humanas, Universidade Federal do ABC, Rua Santa Adelia 166, Bangu, Santo Andre, SP 09210-170 (Brazil); Chiquito, Adenilson J., E-mail: chiquito@df.ufscar.br [Departamento de Fisica, UFSCar-Federal University of Sao Carlos, Rod.Washington Luis km 235, CP 676 Sao Carlos, SP 13565-905 (Brazil); Longo, Elson, E-mail: elson@iq.unesp.br [Instituto de Quimica de Araraquara, UNESP-Universidade Estadual Paulista, Rua Francisco Degni, CP 355 Araraquara, SP 14801-907 (Brazil); Leite, Edson R., E-mail: derl@power.ufscar.br [LIEC-Laboratorio Interdisciplinar de Eletroquimica e Ceramica, Departamento de Quimica, UFSCar-Universidade Federal de Sao Carlos, Rod.Washington Luis km 235, CP 676 Sao Carlos, SP 13565-905 (Brazil); Camargo, Emerson R., E-mail: camargo@ufscar.br [LIEC-Laboratorio Interdisciplinar de Eletroquimica e Ceramica, Departamento de Quimica, UFSCar-Universidade Federal de Sao Carlos, Rod.Washington Luis km 235, CP 676 Sao Carlos, SP 13565-905 (Brazil)

    2010-12-01

    Nanosized powders of lead lanthanum titanate (Pb{sub 1-x}La{sub x}TiO{sub 3}) were synthesized by means of the oxidant-peroxo method (OPM). Lanthanum was added from 5 to 30% in mol through the dissolution of lanthanum oxide in nitric acid, followed by the addition of lead nitrate to prepare a solution of lead and lanthanum nitrates, which was dripped into an aqueous solution of titanium peroxo complexes, forming a reactive amorphous precipitate that could be crystallized by heat treatment. Crystallized powders were characterized by FT-Raman spectroscopy and X-ray powder diffraction, showing that tetragonal perovskite structure is obtained for samples up to 25% of lanthanum and cubic perovskite for samples with 30% of lanthanum. Powders containing 25 and 30% in mol of lanthanum were calcined at 700 deg. C for 2 h, and in order to determine the relative dielectric permittivity and the phase transition behaviour from ferroelectric-to-paraelectric, ceramic pellets were prepared and sintered at 1100 or 1150 deg. C for 2 h and subjected to electrical characterization. It was possible to observe that sample containing 25% in mol of La presented a normal behaviour for the phase transition, whereas the sample containing 30% in mol of La presented a diffuse phase transition and relaxor behaviour.

  13. Characterization of dense lead lanthanum titanate ceramics prepared from powders synthesized by the oxidant peroxo method

    International Nuclear Information System (INIS)

    Pinto, Alexandre H.; Souza, Flavio L.; Chiquito, Adenilson J.; Longo, Elson; Leite, Edson R.; Camargo, Emerson R.

    2010-01-01

    Nanosized powders of lead lanthanum titanate (Pb 1-x La x TiO 3 ) were synthesized by means of the oxidant-peroxo method (OPM). Lanthanum was added from 5 to 30% in mol through the dissolution of lanthanum oxide in nitric acid, followed by the addition of lead nitrate to prepare a solution of lead and lanthanum nitrates, which was dripped into an aqueous solution of titanium peroxo complexes, forming a reactive amorphous precipitate that could be crystallized by heat treatment. Crystallized powders were characterized by FT-Raman spectroscopy and X-ray powder diffraction, showing that tetragonal perovskite structure is obtained for samples up to 25% of lanthanum and cubic perovskite for samples with 30% of lanthanum. Powders containing 25 and 30% in mol of lanthanum were calcined at 700 deg. C for 2 h, and in order to determine the relative dielectric permittivity and the phase transition behaviour from ferroelectric-to-paraelectric, ceramic pellets were prepared and sintered at 1100 or 1150 deg. C for 2 h and subjected to electrical characterization. It was possible to observe that sample containing 25% in mol of La presented a normal behaviour for the phase transition, whereas the sample containing 30% in mol of La presented a diffuse phase transition and relaxor behaviour.

  14. Radiation Damage Effects in Candidate Ceramics for Plutonium Immobilization: Final Report

    International Nuclear Information System (INIS)

    Strachan, Denis M.; Scheele, Randall D.; Icenhower, Jonathan P.; Buck, Edgar C.; Kozelisky, Anne E.; Sell, Rachel L.; Elovich, Robert J.; Buchmiller, William C.

    2004-01-01

    In this document, we summarize our study of the effects of radiation induced damage to the titanate ceramics that were to be the immobilization form for surplus weapons-grade Pu. In this study, we made five ceramic materials: pure-phase pyrochlore, pure-phase zirconolite, pyrochlore-rich baseline, zirconolite-rich baseline, and impurity baseline. Two-hundred specimens were made of which 130 contained approximately 10 mass% 238Pu and 70 contained 10 mass% 239Pu. The specimens containing 239Pu served as materials against which the behavior of the 238Pu-bearing specimens could be compared. In our studies, we measured the true density (density exclusive of surface connected porosity), bulk density, crystalline-phase composition with X-ray diffraction (XRD), and dissolution rates as radiation induced damage accumulated in the 238Pu-bearing specimens. We routinely took photographs of the specimens during each characterization period. From our studies, we determined that these materials swell less than 10% and generally less than 5%. As the material swells, some open porosity can be converted to closed porosity, often causing the true density to decrease more rapidly than the bulk density. In general, 3?1018 a/g of damage accumulation were required for the materials to become amorphous as determined with the XRD method. The order in which the phases became amorphous was brannerite, pyrochlore, and zirconolite with brannerite being the most susceptible to radiation induced damage. However, we also show that Pu is not evenly distributed amongst the phases when multiple phases are present. We were unsuccessful in making a pure brannerite to study. Therefore, the brannerite was always present with other phases. For a material containing about 10 mass% 239Pu, 3?1018 a/g represent about 500 years in the geologic repository. At no time in our studies was there evidence for microcracking in these materials, even upon close examination in a scanning-electron microscope . Upon

  15. Incipient ferroelectric to a possible ferroelectric transition in Te4+ doped calcium copper titanate (CaCu3Ti4O12 ceramics at low temperature as evidenced by Raman and dielectric spectroscopy

    Directory of Open Access Journals (Sweden)

    Nabadyuti Barman

    2017-03-01

    Full Text Available Partial replacement of Ti4+ by Te4+ ions in calcium copper titanate lattice improved its dielectric behaviour mostly due to cubic-to-tetragonal structural transformation and associated distortion in TiO6 octahedra. The relative permittivity values (23–30 x 103 of Te4+ doped ceramics is more than thrice that of un-doped ceramics (8 x 103 at 1 kHz. A decreasing trend in relative permittivity with increasing temperature (50–300 K is observed for all the samples. Barrett’s formula, as a signature of incipient ferroelectricity, is invoked to rationalize the relative permittivity variation as a function of temperature. A systematic investigation supported by temperature dependent Raman studies reveal a possible ferroelectric transition in Te4+ doped ceramic samples below 120 K. The possible ferroelectric transition is attributed to the interactions between quasi-local vibrations associated with the micro-clusters comprising TiO6 and TeO6 structural units and indirect dipole-dipole interactions of off-center B–cations (Ti4+ and Te4+ in double perovskite lattice.

  16. Sinterização de cerâmicas à base de PZT em forno de microondas Microwave synthesis of PZT based ceramics

    Directory of Open Access Journals (Sweden)

    M. V. Gelfuso

    2007-09-01

    Full Text Available Cerâmicas de titanato e zirconato de chumbo dopadas com neodímio foram sinterizadas em um forno de microondas de uso doméstico modificado. Neste tipo de aquecimento, a energia eletromagnética é transferida diretamente para o material, sendo convertida em calor pelo material cerâmico, reduzindo o tempo e energia durante o processamento. Desta forma, foram produzidos corpos cerâmicos com tempo de sinterização que variou até 30 min, a 1100 e 1200 ºC. As fases foram investigadas por meio de difratometria de raios X. Corpos cerâmicos com densidade de 95% da teórica foram obtidos com tempo de sinterização de 10 min em 1100 ºC, com uma taxa de aquecimento de 400 ºC/min. Para as cerâmicas com densidade superior a 90% da teórica foram medidos os valores de constante dielétrica e fator de perda.Ferroelectric ceramics based on lead zirconate titanate doped with neodymium were sintered using a modified microwave oven. In this process the energy is transferred directly to the material through the interaction between molecules of the material with the electromagnetic field. The microwave sintering process has an advantage to reduce the time and save energy. This type of process involves energy conversion, opposing to heat transfer. Ceramic parts were produced by thermal treatments at 1100 ºC and 1200 ºC up to 30 min. The formed crystalline phases were investigated by X-ray diffraction. Ceramic parts with densities above 95% of the theoretical density were produced in 10 min by heating at 1100 ºC, with heating rate of 400 ºC/min. Values of dielectric constant and loss factor of ceramics with density above 90%T.D. were determined.

  17. High temperature crystallographic and thermodynamic investigations on synthetic calzirtite (Ca2Zr5Ti2O16)

    International Nuclear Information System (INIS)

    Jafar, M.; Phapale, S.; Achary, S.N.; Mishra, R.; Tyagi, A.K.

    2016-01-01

    Immobilization of actinides in the high level waste (HLW) produced from nuclear reactors in durable host matrix is one of the important concerns in nuclear power technology. Rock analogue (SYNROC) ceramic composites of titanates and zirconates namely zirconolite, calzirtite etc. have been proposed as alternate host matrix for disposal of long lived fission products. These minerals have ability to incorporate or immobilize a wider variety of ions simultaneously without further segregation to any other phases and are stable in geothermal conditions. Knowledge of thermodynamic stability of these minerals is important for their deployment as host matrix for actinide waste disposal. In this work crystal structure and thermodynamic parameters of a mineral analogous titanate termed as calzirtite (Ca 2 Zr 5 Ti 2 O 16 ) has been determined

  18. Titan!

    Science.gov (United States)

    Matson, Dennis L.

    2010-05-01

    Cassini-Huygens achieved Saturnian orbit on July 1, 2004. The first order of business was the safe delivery of the Huygens atmospheric probe to Titan that took place on January 14, 2005. Huygens descended under parachute obtaining observations all the way down to a safe landing. It revealed Titan for the first time. Stunning are the similarities between Titan and the Earth. Viewing the lakes and seas, the fluvial terrain, the sand dunes and other features through the hazy, nitrogen atmosphere, brings to mind the geological processes that created analogous features on the Earth. On Titan frozen water plays the geological role of rock; liquid methane takes the role of terrestrial water. The atmospheres of both Earth and Titan are predominately nitrogen gas. Titan's atmosphere contains 1.5% methane and no oxygen. The surface pressure on Titan is 1.5 times the Earth's. There are aerosol layers and clouds that come and go. Now, as Saturn proceeds along its solar orbit, the seasons are changing. The effects upon the transport of methane are starting to be seen. A large lake in the South Polar Region seems to be filling more as winter onsets. Will the size and number of the lakes in the South grow during winter? Will the northern lakes and seas diminish or dry up as northern summer progresses? How will the atmospheric circulation change? Much work remains not only for Cassini but also for future missions. Titan has many different environments to explore. These require more capable instruments and in situ probes. This work was conducted at the Jet Propulsion Laboratory, California Institute of Technology under contract with the National Aeronautics and Space Administration.

  19. Analysis of isothermal sintering of zinc-titanate doped with MgO

    Directory of Open Access Journals (Sweden)

    Obradović N.

    2007-01-01

    Full Text Available The aim of this work was analysis of isothermal sintering of zinc titanate ceramics doped with MgO obtained by mechanical activation. Mixtures of ZnO, TiO2 and MgO (0, 1.25 and 2.5% were mechanically activated 15 minutes in a planetary ball mill. The powders obtained were pressed under different pressures and the results were fitted with a phenomenological compacting equation. Isothermal sintering was performed in air for 120 minutes at four different temperatures. Structural characterization of ZnO-TiO2-MgO system after milling was performed at room temperature using XRPD measurements. DTA measurements showed different activation energies for pure and doped ZnO-TiO2 systems. Thus addition of MgO stabilizes the crystal structure of zinc titanate.

  20. Electrical characteristics of high density, high purity titanate ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Lupfer, D A [Electronics Laboratory, General Electric Company, Syracuse, NY (United States)

    1958-07-01

    This report is concerned with the electrical behaviour of cubic (Ba,Sr)TiO{sub 3} ceramics at very high values of the electric field. The work was undertaken to develop a dielectric system to be used in capacitors for the storage and discharge of electrical energy. Objectives for the finished system were to store large amounts of energy per unit volume, to release at least 75% of the energy in 0.2 x 10{sup -6} seconds, and to operate over a limited temperature range above 20 deg. C. The work is incomplete, but the results to date show that (Ba,Sr) TiO{sub 3} ceramics can store more electrical energy per unit volume than any other known dielectric system.

  1. Atomic profile imaging of ceramic oxide surfaces

    International Nuclear Information System (INIS)

    Bursill, L.A.; Peng JuLin; Sellar, J.R.

    1989-01-01

    Atomic surface profile imaging is an electron optical technique capable of revealing directly the surface crystallography of ceramic oxides. Use of an image-intensifier with a TV camera allows fluctuations in surface morphology and surface reactivity to be recorded and analyzed using digitized image data. This paper reviews aspects of the electron optical techniques, including interpretations based upon computer-simulation image-matching techniques. An extensive range of applications is then presented for ceramic oxides of commercial interest for advanced materials applications: including uranium oxide (UO 2 ); magnesium and nickel oxide (MgO,NiO); ceramic superconductor YBa 2 Cu 3 O 6.7 ); barium titanate (BaTiO 3 ); sapphire (α-A1 2 O 3 ); haematite (α-Fe-2O 3 ); monoclinic, tetragonal and cubic monocrystalline forms of zirconia (ZrO 2 ), lead zirconium titanate (PZT + 6 mol.% NiNbO 3 ) and ZBLAN fluoride glass. Atomic scale detail has been obtained of local structures such as steps associated with vicinal surfaces, facetting parallel to stable low energy crystallographic planes, monolayer formation on certain facets, relaxation and reconstructions, oriented overgrowth of lower oxides, chemical decomposition of complex oxides into component oxides, as well as amorphous coatings. This remarkable variety of observed surface stabilization mechanisms is discussed in terms of novel double-layer electrostatic depolarization mechanisms, as well as classical concepts of the physics and chemistry of surfaces (ionization and affinity energies and work function). 46 refs., 16 figs

  2. Separation of zircon from the beach sand deposit of Srikurmam area, Srikakulam district, Andhra Pradesh - a case study

    International Nuclear Information System (INIS)

    Rao, G.V.S.U.; Sharma, A.K.; Seshadrinath, S.T.; Fahmi, Sohail; William Prasad, Ch.; Nagabhushanam, B.

    2011-01-01

    Beach sand placer deposits occur along the eastern and western coasts of India, which contain heavy minerals, such as ilmenite, rutile, garnet, monazite, zircon and sillimanite. Among these, zircon is used in zircaloys (nuclear industry), ceramics, refractories, abrasives, etc. Separation and chemical characterization of pure zircon is a prelude for understanding the different elements and impurities present and its industrial application. In recent times, several methods are developed for beneficiation and separation of individual heavy minerals from beach sands. In this paper, separation of zircon from beach sand of Srikurmam area, Andhra Pradesh was taken up as a case study. The process flow sheet adopted for separation and isolation of pure zircon from beach sand sample consists of desliming of beach sand, wet tabling of sand fraction, removal of magnetite by low intensity magnetic separation from table concentrate, perm roll magnetic separation and induced roll magnetic separation of table concentrate. The concentrates were further subjected to iso-dynamic magnetic separator after observing impurity present in the sample under binocular stereomicroscope. In the present process, about 95% pure zircon was obtained. Further concentration of zircon was carried out under the binocular stereomicroscope by hand picking of impurity to obtain 99.5% pure zircon concentrate. The pure zircon concentrate was analyzed for major, minor and trace elements by chemical method for characterization of zircon and cross validation of physical processes through which the zircon concentrate was obtained. Chemical analysis of the pure zircon concentrate indicated 63.15 to 64.79% ZrO 2 and 32.2 to 32.8% SiO 2 . These values are nearer to that of pure zircon, which stoichiometrically contains 67.2% ZrO 2 and 32.8 % SiO 2 with little iron. In the present study, ZrO 2 +HfO 2 content varies from 65.27 to 66.17% and hafnium from 1.25 to 1.46% HfO 2 in the zircon concentrate. The variation

  3. Influence of sintering temperature on microstructures and energy-storage properties of barium strontium titanate glass-ceramics prepared by sol-gel process

    Energy Technology Data Exchange (ETDEWEB)

    Zhu, Jia; Zhang, Yong; Song, Xiaozhen; Zhang, Qian; Yang, Dongliang; Chen, Yongzhou [Beijing Key Laboratory of Fine Ceramics, State Key Laboratory of New Ceramics and Fine Processing, Institute of Nuclear and New Energy Technology, Tsinghua University, Beijing, 100084 (China)

    2015-12-15

    The sol-gel processing, microstructures, dielectric properties and energy-storage properties of barium strontium titanate glass-ceramics over the sintering temperature range of 1000-1150 C were studied. Through the X-ray diffraction result, it is revealed that the crystallinity increases as the sintering temperature increased from 1000 to 1080 C and has reached a steady-state regime above 1100 C. Scanning electron microscopy images showed that with the increase of sintering temperature, the crystal size increased. Dielectric measurements revealed that the increase in the sintering temperature resulted in a significant increase in the dielectric constant, a strong sharpness of the temperature-dependent dielectric response and a pronounced decrease of the temperature of the dielectric maximum. The correlation between charge spreading behavior and activation energies of crystal and glass was discussed by the employment of the impedance spectroscopy studies. As a result of polarization-electric field hysteresis loops, both the charged and discharged densities increased with increasing sintering temperature. And the maximum value of energy storage efficiency was found to occur at 1130 C. Finally, the dependence of released energy and power densities calculated from the discharged current-time (I-t) curves on the sintering temperature was studied. The relationship between the energy storage properties and microstructure was correlated. Polarization-electric field hysteresis loops for the BST glass-ceramics sintered at different temperatures. (copyright 2015 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  4. Ti-in-zircon thermometry: applications and limitations

    Science.gov (United States)

    Fu, Bin; Page, F. Zeb; Cavosie, Aaron J.; Fournelle, John; Kita, Noriko T.; Lackey, Jade Star; Wilde, Simon A.; Valley, John W.

    2008-08-01

    The titanium concentrations of 484 zircons with U-Pb ages of ˜1 Ma to 4.4 Ga were measured by ion microprobe. Samples come from 45 different igneous rocks (365 zircons), as well as zircon megacrysts (84) from kimberlite, Early Archean detrital zircons (32), and zircon reference materials (3). Samples were chosen to represent a large range of igneous rock compositions. Most of the zircons contain less than 20 ppm Ti. Apparent temperatures for zircon crystallization were calculated using the Ti-in-zircon thermometer (Watson et al. 2006, Contrib Mineral Petrol 151:413-433) without making corrections for reduced oxide activities (e.g., TiO2 or SiO2), or variable pressure. Average apparent Ti-in-zircon temperatures range from 500° to 850°C, and are lower than either zircon saturation temperatures (for granitic rocks) or predicted crystallization temperatures of evolved melts (˜15% melt residue for mafic rocks). Temperatures average: 653 ± 124°C (2 standard deviations, 60 zircons) for felsic to intermediate igneous rocks, 758 ± 111°C (261 zircons) for mafic rocks, and 758 ± 98°C (84 zircons) for mantle megacrysts from kimberlite. Individually, the effects of reduced a_{TiO2} or a_{SiO2}, variable pressure, deviations from Henry’s Law, and subsolidus Ti exchange are insufficient to explain the seemingly low temperatures for zircon crystallization in igneous rocks. MELTs calculations show that mafic magmas can evolve to hydrous melts with significantly lower crystallization temperature for the last 10-15% melt residue than that of the main rock. While some magmatic zircons surely form in such late hydrous melts, low apparent temperatures are found in zircons that are included within phenocrysts or glass showing that those zircons are not from evolved residue melts. Intracrystalline variability in Ti concentration, in excess of analytical precision, is observed for nearly all zircons that were analyzed more than once. However, there is no systematic change in Ti

  5. Microstructure and Properties of Plasma Sprayed Lead Zirconate Titanate (PZT) Ceramics

    Czech Academy of Sciences Publication Activity Database

    Ctibor, Pavel; Pala, Zdeněk; Boldyryeva, Hanna; Sedláček, J.; Kmetík, Viliam

    2012-01-01

    Roč. 2, č. 2 (2012), s. 64-75 ISSN 2079-6412 R&D Projects: GA TA ČR TA01010878 Institutional research plan: CEZ:AV0Z20430508 Keywords : plasma spraying * electroceramics * PZT * phase composition * permittivity Subject RIV: JK - Corrosion ; Surface Treatment of Materials http://www.mdpi.com/2079-6412/2/2/64

  6. Processing and electrical properties of gallium-substituted lead zirconate titanate ceramics

    Science.gov (United States)

    Hajra, Sugato; Sharma, Pulkit; Sahoo, Sushrisangita; Rout, P. K.; Choudhary, R. N. P.

    2017-12-01

    In the present paper, the effect of gallium (Ga) substitution on structural, microstructural, electrical conductivity of Pb(ZrTi)O3 (PZT) in the morphotropic phase boundary (MPB) region (i.e., Pb0.96Ga0.04(Zr0.48Ti0.52)0.99O3 (PGaZT-4)) was investigated. Increased grain density increases the resistivity of the Ga-modified PZT system. Preliminary structural analysis using X-ray diffraction pattern and data showed the existence of two phases [major tetragonal (T) and minor monoclinic (M)]. Field emission scanning electron micrograph (FESEM) showed the distribution of spherical as well as platelet type grains with small pores. The behavior of dielectric constant with temperature of PGaZT-4 exhibited the suppression of the ferroelectric phase transition [i.e., disappearance of Curie temperature ( T c)]. The complex impedance spectroscopy (CIS) technique helped to investigate the impedance parameters of PGaZT-4 in MPB region in a wide range of temperature (250-500 °C) and frequency (1-1000 kHz) region. The impedance parameters of the material are found to be strongly dependent on frequency of AC electric field and temperature. The substitution of gallium at the Pb site of PZT generally enhances the dielectric constant and decreases loss tangent. The AC conductivity vs frequency ( f = ω2 π) in the region of dispersion follows the universal response of Jonscher's equation. Enhanced resistive characteristics were observed for Ga-substituted PZT in comparison to the pure PZT, which was well ensured from the studies of electrical parameters, such as impedance and AC conductivity.

  7. Processing and electrical properties of gallium-substituted lead zirconate titanate ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Hajra, Sugato; Sharma, Pulkit; Rout, P.K. [Siksha O Anusandhan University, Department of Electrical and Electronics Engineering, Bhubaneswar (India); Sahoo, Sushrisangita; Choudhary, R.N.P. [Siksha O Anusandhan University, Department of Physics, Bhubaneswar (India)

    2017-12-15

    In the present paper, the effect of gallium (Ga) substitution on structural, microstructural, electrical conductivity of Pb(ZrTi)O{sub 3} (PZT) in the morphotropic phase boundary (MPB) region (i.e., Pb{sub 0.96}Ga{sub 0.04}(Zr{sub 0.48}Ti{sub 0.52}){sub 0.99}O{sub 3} (PGaZT-4)) was investigated. Increased grain density increases the resistivity of the Ga-modified PZT system. Preliminary structural analysis using X-ray diffraction pattern and data showed the existence of two phases [major tetragonal (T) and minor monoclinic (M)]. Field emission scanning electron micrograph (FESEM) showed the distribution of spherical as well as platelet type grains with small pores. The behavior of dielectric constant with temperature of PGaZT-4 exhibited the suppression of the ferroelectric phase transition [i.e., disappearance of Curie temperature (T{sub c})]. The complex impedance spectroscopy (CIS) technique helped to investigate the impedance parameters of PGaZT-4 in MPB region in a wide range of temperature (250-500 C) and frequency (1-1000 kHz) region. The impedance parameters of the material are found to be strongly dependent on frequency of AC electric field and temperature. The substitution of gallium at the Pb site of PZT generally enhances the dielectric constant and decreases loss tangent. The AC conductivity vs frequency (f = ω2π) in the region of dispersion follows the universal response of Jonscher's equation. Enhanced resistive characteristics were observed for Ga-substituted PZT in comparison to the pure PZT, which was well ensured from the studies of electrical parameters, such as impedance and AC conductivity. (orig.)

  8. Studies on zirconia-mullite ceramic

    International Nuclear Information System (INIS)

    Virkar, Alka N.

    2014-01-01

    Zirconia Toughened Alumina (ZTA) ceramics with much improved Fracture Toughness and Strength have been used as a front material to fabricate composite Armour-Applications, Al 2 O 3 has very different fluxing ability with silica by sufficiently lowering the melting point. Addition of small amount of Fe 2 O 3 , TiO 2 , in an Al 2 O 3 -SiO 2 mixture enhances needle shaped Mullite crystal growth and also assist Liquid phase Sintering. In the present investigation, Zircon was used as a source of ZrO 2 and SiO 2 . Zircon (ZrSiO 4 ) has a low coefficient of Thermal Expansion and good Thermal Shock Resistance. Densification in terms of Relative Density and App. Porosity, Tetragonal ZrO 2 , phases, Thermal Expansion Coefficient, Hardness etc. were studied on Zirconia-Mullite system with and without additives. Z-M system with Y 2 O 3 additives show improved properties owing to the partial stabilization of Zirconia phase (PSZ). (author)

  9. Prospects of ceramic tritium breeder materials

    International Nuclear Information System (INIS)

    Roth, E.; Roux, N.; Conservatoire National des Arts et Metiers; CEA Centre d'Etudes Nucleaires de Saclay, 91 - Gif-sur-Yvette

    1989-01-01

    In this paper the authors examine the prospects of the main ceramics proposed as breeder materials for fusion reactors, i.e. Li-2O, Li-2ZrO-3, LiAlO-2, Li-4SiO-4. To do so they review terms of reference of contemplated blankets for NET, ITER and DEMO, and the proposed blanket concepts and materials. Issues respective to the use of each breeder material are examined, and from this review it is concluded that ceramics are the most favorable breeder materials whose use can be contemplated as well for a driver blanket for NET or ITER and for a DEMO blanket. Ceramics are then compared between themselves and it is seen that, subject to the confirmation of recent experimental results, lithium zirconate could be used with advantage in any of the present blanket concepts, except in those employing lithium at its natural isotopic abundance, in which case only Li-2O can be used. However in specific cases, or in parts of a blanket, other ceramics may be profitably employed. As a general conclusion suggestions are made to further improve ceramic breeder performances, and it is recommended to intensify also work on problems that have to be solved in order to operate ceramic breeder blankets e.g. tritium extraction and recovery systems and conditions of beryllium use. (author). 37 refs.; 12 tabs

  10. Synthesis and characterization of some inorganic ion exchange materials and its application in the treatment of hazardous waste

    International Nuclear Information System (INIS)

    El-Deeb, A.B.I.M.

    2008-01-01

    inorganic ion exchange materials play an important role in the last decays in the fields of industry, medicine, agriculture and nuclear technology due to their stabilities towards thermal and radiation and their resistance to chemical attack. the most important property of inorganic ion exchangers enabling their use in the various chemical separation is the selectivity. the selectivity behaviour of synthetic inorganic ion exchanges are still far from being clearly understood. this work had been done in an attempt to synthesize of inorganic ion exchangers such as zircon-titanate and doping alkali metals with zircon-titanate to produce a new developed ion exchanger with properties allow to used in the treatment of hazardous wastes. this work is concerned with the preparation of zircon-titanate and the doping of some alkali metals (K,Na,Li and Cs)with zircon-titanate. characterization of the synthesized ion exchangers using x-ray diffraction, x-ray fluorescence, infrared spectroscopy, surface area and thermal analysis were conducted. equilibrium measurements and effect of batch factor, ph of the medium on percent uptake were determined. capacity measurements and sorption isotherm studies were also investigated on zircon-titanate and its dopant products.

  11. Determination of the Steady State Leakage Current in Structures with Ferroelectric Ceramic Films

    Science.gov (United States)

    Podgornyi, Yu. V.; Vorotilov, K. A.; Sigov, A. S.

    2018-03-01

    Steady state leakage currents have been investigated in capacitor structures with ferroelectric solgel films of lead zirconate titanate (PZT) formed on silicon substrates with a lower Pt electrode. It is established that Pt/PZT/Hg structures, regardless of the PZT film thickness, are characterized by the presence of a rectifying contact similar to p-n junction. The steady state leakage current in the forward direction increases with a decrease in the film thickness and is determined by the ferroelectric bulk conductivity.

  12. Piezoelectric properties and thermal stabilities of cobalt-modified potassium bismuth titanate

    International Nuclear Information System (INIS)

    Guo, Zhen-Lei; Wang, Chun-Ming; Zhao, Tian-Long; Yu, Si-Long; Cao, Zhao-Peng

    2013-01-01

    The cobalt-modified potassium bismuth titanate (K 0.5 Bi 4.5 Ti 4 O 15 , KBT) piezoelectric ceramics have been prepared using conventional solid–state reaction. X-ray diffraction analysis revealed that the cobalt-modified KBT ceramics have a pure four-layer (m = 4) Aurivillius-type structure. The dielectric, ferroelectric, and piezoelectric properties of cobalt-modified KBT ceramics were investigated in detail. The piezoelectric activities of KBT ceramics were significantly improved by the cobalt modification. The reasons for piezoelectric activities enhancement with cobalt modification were given. The piezoelectric coefficient d 33 and Curie temperature T c for the 5 mol% cobalt-modified KBT ceramics (KBT-Co5) were found to be 28 pC/N and 575 °C, respectively. The DC resistivity, frequency constants (N p and N t ), and electromechanical properties at elevated temperature were investigated, indicating the cobalt-modified KBT piezoelectric ceramics possess stable piezoelectric properties up to 500 °C. The results show the cobalt-modified KBT ceramics are potential materials for high temperature piezoelectric applications. - Highlights: • We examine the piezoelectric properties of the cobalt-modified K 0.5 Bi 4.5 Ti 4 O 15 . • A high level of piezoelectric activities (d 33 = 28 pC/N) are obtained. • High Curie temperature (T c = 575 °C) is acquired for the optimal composition. • The Co-modified K 0.5 Bi 4.5 Ti 4 O 15 is promising as high temperature materials

  13. Piezoelectric ultrasonic micromotor with 1.5 mm diameter.

    Science.gov (United States)

    Dong, Shuxiang; Lim, Siak P; Lee, Kwork H; Zhang, Jingdong; Lim, Leong C; Uchino, Kenji

    2003-04-01

    A piezoelectric ultrasonic micromotor has been developed using a lead zirconate titanate (PZT) ceramic/metal composite tube stator that was 1.5 mm in diameter and 7 mm in length. The micromotor was operated in its first bending vibration mode (approximately 70 kHz), producing speeds from hundreds to over 2000 rpm in both rotational directions. The maximum torque-output was 45 microN-m, which is far superior to previous PZT thin film-based micromotors. This micromotor showed good reliability and stability for more than 300 hours of continued operation.

  14. Preparation and Characterization of Nano-structured Ceramic Powders Synthesized by Emulsion Combustion Method

    International Nuclear Information System (INIS)

    Takatori, Kazumasa; Tani, Takao; Watanabe, Naoyoshi; Kamiya, Nobuo

    1999-01-01

    The emulsion combustion method (ECM), a novel powder production process, was originally developed to synthesize nano-structured metal-oxide powders. Metal ions in the aqueous droplets were rapidly oxidized by the combustion of the surrounding flammable liquid. The ECM achieved a small reaction field and a short reaction period to fabricate the submicron-sized hollow ceramic particles with extremely thin wall and chemically homogeneous ceramic powder. Alumina, zirconia, zirconia-ceria solid solutions and barium titanate were synthesized by the ECM process. Alumina and zirconia powders were characterized to be metastable in crystalline phase and hollow structure. The wall thickness of alumina was about 10 nm. The zirconia-ceria powders were found to be single-phase solid solutions for a wide composition range. These powders were characterized as equiaxed-shape, submicron-sized chemically homogeneous materials. The powder formation mechanism was investigated through the synthesis of barium titanate powder with different metal sources

  15. Synthesis and characterization of bismuth alkaline titanate powders

    Energy Technology Data Exchange (ETDEWEB)

    Torres-Huerta, A.M., E-mail: atorresh@ipn.mx [CICATA-Altamira, Instituto Politecnico Nacional, Km. 14.5 Carretera Tampico Puerto Industrial Altamira, Altamira, Tamps. 89600 (Mexico); Dominguez-Crespo, M.A. [CICATA-Altamira, Instituto Politecnico Nacional, Km. 14.5 Carretera Tampico Puerto Industrial Altamira, Altamira, Tamps. 89600 (Mexico); Hernandez-Perez, M.A. [ESIQIE, Metalurgia, Instituto Politecnico Nacional, Mexico, D. F (Mexico); Garcia-Zaleta, D.S. [CICATA-Altamira, Instituto Politecnico Nacional, Km. 14.5 Carretera Tampico Puerto Industrial Altamira, Altamira, Tamps. 89600 (Mexico); Brachetti-Sibaja, S.B. [CICATA-Altamira, Instituto Politecnico Nacional, Km. 14.5 Carretera Tampico Puerto Industrial Altamira, Altamira, Tamps. 89600 (Mexico); Instituto Tecnologico de Ciudad Madero, Av. 1o. de Mayo esq. Sor Juana Ines de la Cruz s/n Col. Los Mangos C.P.89440 Cd. Madero Tamaulipas (Mexico)

    2011-06-15

    In this work, samples of bismuth alkaline titanate, (K{sub 0.5}Na{sub 0.5}){sub (2-x/2)}Bi{sub (x/6)}TiO{sub 3}, (x = 0.05-0.75) have been prepared by conventional ceramic technique and molten salts. Metal oxides or carbonates powders were used as starting raw materials. The crystalline phase of the synthesized powders was identified by the X-ray diffraction (XRD) and particle morphology was characterized by scanning electron microscopy (SEM). Solid state reaction method was unsuccessful to obtain pellets. From XRD results, a rhombohedral structure was detected and the parameter lattice were estimated to be a = 5.5478 A and {alpha} = 59.48{sup o}. These parameters were used to refine the structure by Rietveld analysis. SEM results showed several morphologies. Apparently, bismuth is promoting the grain growth whose sizes vary from 30 nm to 180 nm It is expected that these materials can be utilized in practical applications as substitutes for lead zirconatetitanate (PZT)-based ceramics.

  16. Piezoelectric Materials Synthesized by the Hydrothermal Method and Their Applications

    Directory of Open Access Journals (Sweden)

    Takeshi Morita

    2010-12-01

    Full Text Available Synthesis by the hydrothermal method has various advantages, including low reaction temperature, three-dimensional substrate availability, and automatic polarization alignment during the process. In this review, powder synthesis, the fabrication of piezoelectric thin films, and their applications are introduced. A polycrystalline lead zirconate titanate (PZT thin film was applied to a micro ultrasonic motor, and an epitaxial lead titanate (PbTiO3 thin film was estimated as a ferroelectric data storage medium. Ferroelectric and piezoelectric properties were successfully obtained for epitaxial PbTiO3 films. As lead-free piezoelectric powders, KNbO3 and NaNbO3 powders were synthesized by the hydrothermal method and sintered together to form (K,NaNbO3 ceramics, from which reasonable piezoelectric performance was achieved.

  17. Flexoelectricity: strain gradient effects in ferroelectrics

    Energy Technology Data Exchange (ETDEWEB)

    Ma Wenhui [Department of Physics, Shantou Unversity, Shantou, Guangdong 515063 (China)

    2007-12-15

    Mechanical strain gradient induced polarization effect or flexoelectricity in perovskite-type ferroelectric and relaxor ferroelectric ceramics was investigated. The flexoelectric coefficients measured at room temperature ranged from about 1 {mu} C m{sup -1} for lead zirconate titanate to 100 {mu} C m{sup -1} for barium strontium titanate. Flexoelectric effects were discovered to be sensitive to chemical makeup, phase symmetry, and domain structures. Based on phenomenological discussion and experimental data on flexoelectricity, the present study proposed that mechanical strain gradient field could influence polarization responses in a way analogous to electric field. Flexoelectric coefficients were found to be nonlinearly enhanced by dielectric permittivity and strain gradient. Interfacial mismatch in epitaxial thin films can give rise to high strain gradients, enabling flexoelectric effects to make a significant impact in properly engineered ferroelectric heterostructure systems.

  18. Barium titanate nanometric polycrystalline ceramics fired by spark plasma sintering.

    Czech Academy of Sciences Publication Activity Database

    Ctibor, Pavel; Sedláček, J.; Ryukhtin, Vasyl; Cinert, Jakub; Lukáč, František

    2016-01-01

    Roč. 42, č. 14 (2016), s. 15989-15993 ISSN 0272-8842 R&D Projects: GA ČR GB14-36566G; GA MŠk LM2015056 Institutional support: RVO:61389021 ; RVO:61389005 Keywords : BaTiO3 * Spark plasma sintering * Electrical properties Subject RIV: JH - Ceramics, Fire-Resistant Materials and Glass; JH - Ceramics, Fire-Resistant Materials and Glass (UJF-V) Impact factor: 2.986, year: 2016 http://www.sciencedirect.com/science/article/pii/S0272884216311695

  19. Obtaining and electrical characterization of silicone/barium titanate composite for variable capacitor applications; Obtencao e caracterizacao eletrica de composito silicone/titanato de bario para aplicacoes em capacitor variavel

    Energy Technology Data Exchange (ETDEWEB)

    Vieira, D.A.; Souza, P.S.S.; Souza, C.P., E-mail: debora.vieira@cear.ufpb.br [Universidade Federal da Paraiba (UFPB), Joao Pessoa, PB (Brazil). Centro de Energias Alternativas e Renovaveis. Departamento de Engenharia Eletrica; Menezes, P.C.F. [Universidade Federal de Campina Grande (UFCG), Campina Grande, PB (Brazil). Departamento de Engenharia de Materiais

    2014-07-01

    Silicone/barium titanate composites are excellent candidates for applications in the production of electronics components. In this work, silicone/barium titanate composite was obtained for the production of capacitors with variable dielectric distance. The mixture of composite (20% of barium titanate) was performed in a mixer with stem type propellers, at room temperature for 20 minutes. The cure was held in vacuum kiln. After obtaining the composite, was mounted a parallel plate capacitor, using composite as dielectric. The composite obtained was subjected to x-ray diffraction, scanning electron microscopy and capacitive electrical test. The DRX confirms the presence of ceramic charge in composite with the presence of broad peaks of barium titanate and micrographs show the barium titanate particles dispersed in polymer matrix. The capacitance of the sample was approximately 28,7pF. (author)

  20. Small-scale dislocation plasticity in strontium titanate

    Energy Technology Data Exchange (ETDEWEB)

    Stukowski, Alexander; Javaid, Farhan; Durst, Karsten; Albe, Karsten [Technische Universitaet Darmstadt (Germany)

    2016-07-01

    Strontium titanate (STO) is an optically transparent perovskite oxide ceramic material. In contrast to other ceramics, single crystal STO plastically deforms under ambient condition, without showing a phase transition or early fracture. This remarkable ductility makes it a prime candidate for different technological applications. However, while the mechanical behavior of bulk STO has been studied extensively using uniaxial compression testing techniques, little is known about the local, small-scale behavior and the details of dislocation-based nanoplasticity in this perovskite material. In this contribution we compare results obtained from new nanoindentation experiments and corresponding large-scale molecular dynamics simulations. The evolution of the plastic zone and dislocation structures that form underneath the indenter is investigated using etch-pit methods in experiments and a novel three-dimensional defect identification technique in atomistic computer models. The latter allows tracing the evolution of the complete dislocation line network as function of indentation depth, quantifying the activity of different slip systems, and correlating this information with the recorded load-displacement curves and hardness data.

  1. Formation of chemical compounds under vacuum plasma-arc deposition of nickel and its alloy onto piezoceramics

    International Nuclear Information System (INIS)

    Grinchenko, V.T.; Lyakhovich, T.K.; Prosina, N.I.; Khromov, S.M.

    1988-01-01

    The phase composition of the transition layer appearing during vacuum-arc coating of nickel and nickel alloy with copper on barium titanate and lead zirconate-titanate is identified. During vacuum plasma-arc coating of nickel and its alloy at the boundary with barium titanate and lead zirconate-titanate the Ni 2 Ti 4 O compound appears which has the crystal lattice type identical with substrate with the parity of lattice parameters. The transition layer contains nickel oxides and NiTiO 3 in the case of barium titanate. When titanate content in substrate increases the zone of reaction diffusion increases in value and becomes more complicate in composition

  2. Zircon-rutile-ilmenite froth flotation process

    International Nuclear Information System (INIS)

    Schmidt, R.; Denham, D.L. Jr.

    1992-01-01

    This patent describes a method for separating a mixture of minerals comprising at least zircon, ilmenite and rutile. It comprises adding an acid solution to the mixture to acidify to a pH of between about 2.0 and 6.0; adding starch to the mixture to depress the ilmenite and the rutile; adding a source of fluoride ions to the mixture to provide a negative surface charge on the zircon surface to activate the zircon; adding an amine cationic collector to the mixture to float the activated zircon; subjecting the mixture containing the added acid solution, the fluoride ions, the starch and the cationic collector, to froth flotation; and withdrawing a float product comprising the zircon and a sink product comprising the ilmenite and rutile

  3. Effects of Pb concentration on phase, microstructure and electrical properties of Bi3.25La0.75Ti3O12 ceramics

    International Nuclear Information System (INIS)

    Lawita, P.; Siriprapa, P.; Watcharapasorn, A.; Jiansirisomboon, S.

    2012-01-01

    In this work, effects of Pb-doping concentration on phase, microstructure and electrical properties of bismuth lead lanthanum titanate (Bi 1−x Pb x ) 3.25 La 0.75 Ti 3 O 12 or BPLT ceramics when x = 0, 0.01, 0.03, 0.05, 0.07, 0.09 and 0.1 were investigated. Phase analysis by X-ray diffraction indicated the existence of orthorhombic phase for all BPLT powders and ceramics. Microstructural investigation using scanning electron microscope showed that all ceramics composed mainly of plate-like grains. An increase in PbO doping content reduced not only diameter and thickness of the grains but also density of the ceramics. Electrical conductivity was found to decrease while dielectric constant increased with Pb-doping concentration. Small reduction of remanent polarization and coercive field was observed in Pb-doped samples. - Highlights: ► We prepared bismuth lead lanthanum titanate ceramics by a solid state mixed-oxide method. ► The optimum sintering temperature was found to be 1150 °C. ► BPLT ceramic was identified by X-ray diffraction method to possess an orthorhombic structure. ► All samples shows plate-like morphology with varying grain size and orientation. ► Increasing Pb-doping content tended to decrease electrical conductivity values.

  4. Barium titanate nanocomposite capacitor FY09 year end report.

    Energy Technology Data Exchange (ETDEWEB)

    Stevens, Tyler E.; DiAntonio, Christopher Brian; Yang, Pin; Chavez, Tom P.; Winter, Michael R.; Monson, Todd C.; Roesler, Alexander William; Fellows, Benjamin D.

    2009-11-01

    This late start RTBF project started the development of barium titanate (BTO)/glass nanocomposite capacitors for future and emerging energy storage applications. The long term goal of this work is to decrease the size, weight, and cost of ceramic capacitors while increasing their reliability. Ceramic-based nanocomposites have the potential to yield materials with enhanced permittivity, breakdown strength (BDS), and reduced strain, which can increase the energy density of capacitors and increase their shot life. Composites of BTO in glass will limit grain growth during device fabrication (preserving nanoparticle grain size and enhanced properties), resulting in devices with improved density, permittivity, BDS, and shot life. BTO will eliminate the issues associated with Pb toxicity and volatility as well as the variation in energy storage vs. temperature of PZT based devices. During the last six months of FY09 this work focused on developing syntheses for BTO nanoparticles and firing profiles for sintering BTO/glass composite capacitors.

  5. ALKALI FUSION OF ROSETTA ZIRCON

    International Nuclear Information System (INIS)

    DAHER, A.

    2008-01-01

    The decomposition of Rosetta zircon by fusion with different types of alkalis has been investigated. These alkalis include sodium hydroxide, potassium hydroxide and eutectic mixture of both. The influences of the reaction temperature, zircon to alkalis ratio, fusion time and the stirring of the reactant on the fusion reaction have been evaluated. The obtained results favour the decomposition of zircon with the eutectic alkalis mixture by a decomposition efficiency of 96% obtained at 500 0 C after one hour

  6. Characteristics of solder joints under fatigue loads using piezomechanical actuation

    Science.gov (United States)

    Shim, Dong-Jin; Spearing, S. Mark

    2003-07-01

    Crack initiation and growth characteristics of solder joints under fatigue loads are investigated using piezomechanical actuation. Cracks in solder joints, which can cause failure in microelectronics components, are induced via piezoelectricity in piezo-ceramic bonded joints. Lead-zirconate-titanate ceramic plates and eutectic Sn-Pb solder bonded in a double-lap shear configuration are used in the investigation. Electric field across each piezo-ceramic plate is applied such that shear stresses/strains are induced in the solder joints. The experiments show that cracks initiate in the solder joints around defects such as voids and grow in length until they coalesce with other cracks from adjacent voids. These observations are compared with the similar thermal cycling tests from the literature to show feasibility and validity of the current method in investigating the fatigue characteristics of solder joints. In some specimens, cracks in the piezo-ceramic plates are observed, and failure in the specimens generally occurred due to piezo-ceramic plate fracture. The issues encountered in implementing this methodology such as low actuation and high processing temperatures are further discussed.

  7. Processing, microstructure, leaching, and long-term stability studies related to titanate high-level waste forms

    International Nuclear Information System (INIS)

    Dosch, R.G.; Headley, T.J.; Northrup, C.J.; Hlava, P.F.

    1983-05-01

    A process leading to titanate-based waste forms for commercial high-level nuclear waste is described. Radionuclides are fixed on hydrous calcium titanate by ion exchange/sorption reactions and the material is converted to a dense, ceramic form by hot pressing. Transmission electron microscopy-electron microprobe characterization was done to determine the effects of compositional changes and process variations on microstructure. Leaching studies in the range of 22 to 150 0 C and pH 2 to 12 were done to assess the effects of the same variables on leaching behavior. Samples of a reference borosilicate glass waste form were leached under the same conditions to provide a direct comparison between the two waste forms. Lead-ion implantation was used to simulate long-term α-recoil damage in the crystalline titanate phases. Comparison of α-recoil damage in natural minerals with damage induced in synthesized samples of the same mineral suggest that Pb-ion implantation is a valid technique for simulating α-recoil effects. All the titanate phases sustained significant lattice damage at equivalent α-doses of 1 x 10 19 /cm 3 ; however, Rutherford backscattering and transmission electron microscopy studies showed that the damage did not result in significant matrix dissolution in these leaching tests

  8. Synthesis and characterization of ceramic pigments based on oxides of chromium and iron, on TiO2

    International Nuclear Information System (INIS)

    Silva, E.M. da; Galvao, S.B.; Paskocimas, C.A.

    2011-01-01

    This work used oxides of chromium and iron, as precursors of the synthesis of ceramic pigments. The synthesis is based on the dissolution of citric acid as a complexing agent, addition of metal oxides, such as ion chromophores; polymerization with ethylene glycol and doping with titanium oxide. Passing through pre-calcination, breakdown, calcination at different temperatures (900 and 1100 ° C), resulting in pigments: green for pigment chrome deposited on TiO 2 and orange for iron on TiO 2 . Noticing an increase in the opacity with increasing temperature. The thermal analysis (TG and DTA), evaluated their thermal behavior, the XRD revealed the formation of crystalline phases as Iron Titanate and Chrome Titanate; SEM showed the formation of hexagonal particles for both oxides. Thus, the synthesized oxides were within the requirements for application as ceramic pigments. (author)

  9. Effect Of Electric Field Induced Texture On The Properties Of Piezoelectric Lead Zirconate Titanate

    International Nuclear Information System (INIS)

    Alkoy, S.

    2010-01-01

    Texturing a polycrystalline piezoelectric ceramic provide single-crystal like properties without experiencing any difficulties of single crystal growth process. This study reports a method to obtain texture in PbZr 0 .5Ti 0 .5O 3 ceramics by application of an electric field during gelation of a gelcast slurry. Gelcasting provides a means to lock the particles aligned under the application of a high electric field via gelation and this alignment in green body was retained after sintering. Monomer, cross linker and dispersant were dissolved in DI water and PZT powder was dispersed in this premix. Iniator and catalyzer were added to the slurry. An electric field was applied to the slurry for 30 min during gelation. XRD pattern of sintered samples indicates that PZT develops a tetragonal symmetry as a result of E-field applied during gelation. Dielectric constants and piezoelectric d 3 3 coefficients along and perpendicular to E-field are 1070 and 450 and 390 and 280 pC/N, respectively.

  10. Plutonium immobilization plant using ceramic in existing facilities at the Savannah River site

    International Nuclear Information System (INIS)

    DiSabatino, A.

    1998-01-01

    The Plutonium Immobilization Plant (PIP) accepts plutonium (Pu) from pit conversion and from non-pit sources, and through a ceramic immobilization process converts the plutonium into an immobilized form that can be disposed of in a high level waste (HLW) repository. This immobilization process is shown conceptually in Figure 1-1. The objective is to make an immobilized form, suitable for geologic disposal, in which the plutonium is as inherently unattractive and inaccessible as the plutonium in spent fuel from commercial reactors. The ceramic immobilization alternative presented in this report consists of first converting the surplus material to an oxide, followed by incorporating the plutonium oxide into a titanate-based ceramic material that is placed in metal cans

  11. Phase transition stability within ceramics

    International Nuclear Information System (INIS)

    Wang, E.; Wang, D.

    1992-01-01

    Irreversible thermodynamics is applied to analyse nucleation, both in metals and ceramics, in order to distinguish the stability of metastable under cooled melts. The hypothesis of local equilibrium has been used to apply research results from equilibrium thermodynamics, for the study of irreversible processes. The under cooling equation for homogenous nucleation only depends on a coefficient which is not related to the melting point of the material. The calculated critical under cooling values for metals are compared with experimental data. The metastable phase formation of plasma-sprayed alumina and zircon coatings has been discussed based on irreversible thermodynamics. A critical under cooling parameter (β) is defined. The metastable phase formation of plasma-sprayed alumina and zircon has been discussed. The analysis shows that γ-Al 2 O 3 is first formed in the coating since it has a lower β value than α-Al 2 O 3 . Zircon dissociates into ZrO 2 and SiO 2 , and rapid quenching of plasma spraying prevents their re association. The cooling rate determines whether t-ZrO 2 or c-ZrO 2 will form in the sprayed coating. It can be confirmed by the experiments that the content of t-ZrO 2 will increase correspondingly as the sprayed particle size decreases. At high transition temperatures, c-ZrO 2 will be formed because of the anisotropic thermal expansion behaviour in the crystal structure. 22 refs., 2 tabs

  12. Design and fabrication of aspherical bimorph PZT optics

    CERN Document Server

    Tseng, T C; Yeh, Z C; Perng, S Y; Wang, D J; Kuan, C K; Chen, J R; Chen, C T

    2001-01-01

    Bimorph piezoelectric optics with a third-order-polynomial surface is designed and a prototype is fabricated as active optics. Two pairs of silicon (Si) and lead zirconate titanate (PZT) piezoelectric ceramic are bonded as Si-PZT-PZT-Si together with a multi-electrode or thin film resistor coating used as the control electrode between Si and PZT and metallic films as grounding between the interface of PZT ceramics. A linear voltage is applied to the bimorph PZT optics by probing the control electrodes from a two-channel controllable power supplier. In doing so, the optics surface can achieve a desired third-order-polynomial surface. Reducing hysteresis and creep in bimorph PZT X-ray optics is the only feasible way by inserting an appropriate capacitor in series with bimorph PZT optics to significantly reduce both effects.

  13. A finite element model of ferroelectric/ferroelastic polycrystals

    Energy Technology Data Exchange (ETDEWEB)

    HWANG,STEPHEN C.; MCMEEKING,ROBERT M.

    2000-02-17

    A finite element model of polarization switching in a polycrystalline ferroelectric/ferroelastic ceramic is developed. It is assumed that a crystallite switches if the reduction in potential energy of the polycrystal exceeds a critical energy barrier per unit volume of switching material. Each crystallite is represented by a finite element with the possible dipole directions assigned randomly subject to crystallographic constraints. The model accounts for both electric field induced (i.e. ferroelectric) switching and stress induced (i.e. ferroelastic) switching with piezoelectric interactions. Experimentally measured elastic, dielectric, and piezoelectric constants are used consistently, but different effective critical energy barriers are selected phenomenologically. Electric displacement versus electric field, strain versus electric field, stress versus strain, and stress versus electric displacement loops of a ceramic lead lanthanum zirconate titanate (PLZT) are modeled well below the Curie temperature.

  14. Interfacial morphology and domain configurations in 0-3 PZT-Portland cement composites

    International Nuclear Information System (INIS)

    Jaitanong, N.; Zeng, H.R.; Li, G.R.; Yin, Q.R.; Vittayakorn, W.C.; Yimnirun, R.; Chaipanich, A.

    2010-01-01

    Cement-based piezoelectric composites have attracted great attention recently due to their promising applications as sensors in smart structures. Lead zirconate titanate (PZT) and Portland cement (PC) composite were fabricated using 60% of PZT by volume. Scanning Electron Microscope and piezoresponse force microscope were used to investigate the morphology and domain configurations at the interfacial zone of PZT-Portland cement composites. Angular PZT ceramic grains were found to bind well with the cement matrix. The submicro-scale domains were clearly observed by piezoresponse force microscope at the interfacial regions between the piezoelectric PZT phase and Portland cement phase, and are clearer than the images obtained for pure PZT. This is thought to be due to the applied internal stress of cement to the PZT ceramic particle which resulted to clearer images.

  15. Determination of the reduced matrix of the piezoelectric, dielectric, and elastic material constants for a piezoelectric material with C∞ symmetry.

    Science.gov (United States)

    Sherrit, Stewart; Masys, Tony J; Wiederick, Harvey D; Mukherjee, Binu K

    2011-09-01

    We present a procedure for determining the reduced piezoelectric, dielectric, and elastic coefficients for a C(∞) material, including losses, from a single disk sample. Measurements have been made on a Navy III lead zirconate titanate (PZT) ceramic sample and the reduced matrix of coefficients for this material is presented. In addition, we present the transform equations, in reduced matrix form, to other consistent material constant sets. We discuss the propagation of errors in going from one material data set to another and look at the limitations inherent in direct calculations of other useful coefficients from the data.

  16. An Experimental Investigation of the Structural Dynamics of a Torsionally Soft Rotor in Vacuum.

    Science.gov (United States)

    1986-07-01

    attached to the blades for the present test program were of G1356 material supplied by Piezo Electric Products. They were made of lead zirconate...titanate ceramic material with nickel surface electrodes. The elements, nominally measuring 1.0 x 0.5 x 0.010 inch, were epoxied directly to the upper...DAMPING- 0.53 Z RECURO Me. 221 :&CORD ND. 2Z2 RECORD NO. 23) O23 MUg 1 (MLI 6) Ku 2 I.D Si MuM 3 (1A 80 R"T 26 1U SG AP $S SCM AP VMS SGS AMP P94 SGC

  17. Titan's Radioactive Haze : Production and Fate of Radiocarbon On Titan

    Science.gov (United States)

    Lorenz, R. D.; Jull, A. J. T.; Swindle, T. D.; Lunine, J. I.

    Just as cosmic rays interact with nitrogen atoms in the atmosphere of Earth to gener- ate radiocarbon (14C), the same process should occur in Titan`s nitrogen-rich atmo- sphere. Titan`s atmosphere is thick enough that cosmic ray flux, rather than nitrogen column depth, limits the production of 14 C. Absence of a strong magnetic field and the increased distance from the sun suggest production rates of 9 atom/cm2/s, approx- imately 4 times higher than Earth. On Earth the carbon is rapidly oxidised into CO2. The fate and detectability of 14C on Titan depends on the chemical species into which it is incorporated in Titan's reducing atmosphere : as methane it would be hopelessly diluted even in only the atmosphere (ignoring the other, much more massive carbon reservoirs likely to be present on Titan, like hydrocarbon lakes.) However, in the more likely case that the 14C attaches to the haze that rains out onto the surface (as tholin, HCN or acetylene and their polymers - a much smaller carbon reservoir) , haze in the atmosphere or recently deposited on the surface would therefore be quite intrinsically radioactive. Such activity may modify the haze electrical charging and hence its coag- ulation. Measurements with compact instrumentation on future in-situ missions could place useful constraints on the mass deposition rates of photochemical material on the surface and identify locations where surface deposits of such material are `freshest`.

  18. Piezoelectric ceramic (PZT) modulates axonal guidance growth of rat cortical neurons via RhoA, Rac1, and Cdc42 pathways.

    Science.gov (United States)

    Wen, Jianqiang; Liu, Meili

    2014-03-01

    Electrical stimulation is critical for axonal connection, which can stimulate axonal migration and deformation to promote axonal growth in the nervous system. Netrin-1, an axonal guidance cue, can also promote axonal guidance growth, but the molecular mechanism of axonal guidance growth under indirect electric stimulation is still unknown. We investigated the molecular mechanism of axonal guidance growth under piezoelectric ceramic lead zirconate titanate (PZT) stimulation in the primary cultured cortical neurons. PZT induced marked axonal elongation. Moreover, PZT activated the excitatory postsynaptic currents (EPSCs) by increasing the frequency and amplitude of EPSCs of the cortical neurons in patch clamp assay. PZT downregulated the expression of Netrin-1 and its receptor Deleted in Colorectal Cancer (DCC). Rho GTPase signaling is involved in interactions of Netrin-1 and DCC. PZT activated RhoA. Dramatic decrease of Cdc42 and Rac1 was also observed after PZT treatment. RhoA inhibitor Clostridium botulinum C3 exoenzyme (C3-Exo) prevented the PZT-induced downregulation of Netrin-1 and DCC. We suggest that PZT can promote axonal guidance growth by downregulation of Netrin-1 and DCC to mediate axonal repulsive responses via the Rho GTPase signaling pathway. Obviously, piezoelectric materials may provide a new approach for axonal recovery and be beneficial for clinical therapy in the future.

  19. Sulfur in zircons: A new window into melt chemistry

    Science.gov (United States)

    Tang, H.; Bell, E. A.; Boehnke, P.; Barboni, M.; Harrison, T. M.

    2017-12-01

    The abundance and isotopic composition of sulfur are important tools for exploring the photochemistry of the atmosphere, the thermal history of mantle and igneous rocks, and ancient metabolic processes on the early Earth. Because the oldest terrestrial samples are zircons, we developed a new in-situ procedure to analyze the sulfur content of zircons using the CAMECA ims 1290 at UCLA. We analyzed zircons from three metaluminous/I-type granites (reduced and oxidized Peninsular range and Elba), which exhibit low sulfur abundance with the average of 0.5ppm, and one peraluminous/S-type zircon (Strathbogie Range), which shows an elevated sulfur level with the average of 1.5ppm. Additionally, we found that sulfur content ranges between 0.4 and 2.3 ppm in young volcanic zircons (St. Lucia). Our analyses of zircons from the Jack Hills, Western Australia, whose ages range between 3.4 and 4.1 Ga, show a variety of sulfur contents. Three out of the ten zircons are consistent with the sulfur contents of S-type zircons; the rest have low sulfur contents, which are similar to those of I-type zircons. The high sulfur content in some of these Jack Hills zircons can be interpreted as indicating their origin in either a S-type granite or a volcanic reservoir. We favor the former interpretation since the Ti-in-zircon temperatures of our Jack Hills zircons is lower than those of volcanic zircons. Future work will be undertaken to develop a systematic understanding of the relationship between melt volatile content, melt chemistry, and zircon sulfur content.

  20. Structural and impedance spectroscopic studies of samarium modified lead zirconate titanate ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Ranjan, Rajiv [Department of Physics, Jamshedpur Co-operative College, Jamshedpur 831036 (India); Kumar, Rajiv [Department of Physics, Jamshedpur Worker' s College, Jamshedpur 831012 (India); Behera, Banarji [Department of Physics and Meteorology, I.I.T. Kharagpur 721302 (India); Choudhary, R.N.P., E-mail: crnpfl@phy.iitkgp.ernet.i [Department of Physics and Meteorology, I.I.T. Kharagpur 721302 (India)

    2009-11-01

    The polycrystalline samples of Pb{sub 1-x}Sm{sub x}(Zr{sub 0.60}Ti{sub 0.40}){sub 1-x/4}O{sub 3} (PSZT) where x=0.00, 0.03, 0.06 and 0.09 were prepared by a high-temperature solid-state reaction technique. The preliminary structural analysis using X-ray diffraction (XRD) data collected at room temperature has confirmed the formation of single-phase compounds in tetragonal crystal system. The morphological study of each sample using scanning electron microscope (SEM) has revealed that the grains are uniformly distributed through out the surfaces of the samples. Using complex impedance spectroscopy (CIS) technique, the electrical impedance and modulus properties of the materials were studied in a wide range of temperatures at different frequencies. The impedance analysis indicates the presence of bulk resistive contributions in the materials which is found to decrease on increasing temperature. The nature of variation of resistances with temperature suggests a typical negative temperature coefficient of resistance (NTCR) type behavior of the materials. The complex modulus plots clearly exhibits the presence of grain boundaries along with the bulk contributions in the PSZT materials. The presence of non-Debye type of relaxation has been confirmed by the complex impedance analysis. The variation of dc conductivity (bulk) with temperature demonstrates that the compounds exhibit Arrhenius type of electrical conductivity.

  1. Fatigue properties and impedance analysis of potassium sodium niobate-strontium titanate transparent ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Liu, Zhiyong; Fan, Huiqing; Lei, Shenhui; Wang, Ju; Tian, Hailin [Northwestern Polytechnical University, State Key Laboratory of Solidification Processing, School of Materials Science and Engineering, Xi' an (China)

    2016-10-15

    Highly transparent ferroelectric ceramics based on 0.9K{sub 0.5}Na{sub 0.5}NbO{sub 3}-0.1SrTiO{sub 3} were prepared using a pressure-less solid-state sintering method without using hot isostatic pressing and spark plasma sintering. An independence electromechanical response of bipolar switching cycles (S{sub 33} only degraded 3.2 % up to 10{sup 7} cycles) was presented in this transparent ceramics, which indicated an extremely stable property under electric field. From impedance spectroscopy and X-ray photoelectron spectroscopy analyses, it was concluded that such optical transparency and fatigue-resistant behaviors were mainly attributed to the lower density of oxygen vacancies in the ceramics. (orig.)

  2. Comparison of Piezo-material based Energy Transduction Systems for Artificial Nanoswimmer

    Science.gov (United States)

    Nain, S.; Rathore, J. S.; Sharma, N. N.

    2018-04-01

    The energy harnessing is a process of obtaining energy from the surrounding environment and converting into electrical energy. In the last two decades, there has been a plenteous study in energy harnessing. Now a day, energy harnessing using piezoelectric materials has drawn attention of researchers due to low cost, flexibility and light weight. The benefits of piezoelectric material can be utilized by designing a self-powered device for artificial nanoswimmer. Some of the ceramics which displays the piezoelectric effect are lead-zirconate-titanate (PZT), lead-titanate (PbTiO2), lead-zirconate (PbZrO3) and Barium Titanate (BaTiO3). PZT is most extensively used piezoelectric material in the field of energy harnessing but it is brittle in nature. Lead based piezoelectric materials are toxic in nature and may not suitable for in-vivo biomedical applications. To eradicate this problem, researchers are interested in synthesizing lead free piezoelectric material such as Aluminium Nitride (AIN), Barium Titanate (BaTiO3) and Polyvinylidenefluoride (PVDF). The biocompatibility of PVDF makes it appropriate to be used for energy harnessing in human body for applications like on board powering of nanoswimmer for various disease detection and drug delivery. In this paper, a cantilever beam is being simulated in COMSOL to study electric potential generated on the surface of beam made of different piezoelectric materials such as AIN, PVDF and PZT due to fluidic pressure, which will be utilized as energy for actuation of artificial nanoswimmer. Piezo-based cantilever beams have been compared and maximum electric potential is being observed in PVDF based beam. PVDF seems most promising piezoelectric material for in-vivo biomedical application and it is readily available.

  3. Emerging technologies for processing and utilization of zircon

    International Nuclear Information System (INIS)

    Rao, S.M.; Balkishan, B.

    2013-01-01

    Zirconium occupies a prominent place in today's industry due to diverse applications of its chemical compounds. About 95% of zirconium is consumed in the form of zircon, zirconia and zirconium chemicals. The balance 5% of zirconium is consumed as the metal and its alloys. Because of its attractive nuclear properties zirconium alloys with very low hafnium content are used in the nuclear industry. Bio-compatibility, corrosion resistance and mechanical strength of zirconium alloys make them suitable for the manufacture of human organs and medicinal and pharmaceutical equipment. Other commercial areas of application of zirconium compounds include foundry, refractory, abrasives, opacifiers, oxygen sensors, catalysis, advanced ceramics, gems, paint dryers, pigments etc. The talk outlines the technologies involved in the production of nuclear grade zirconium alloys, manufacture of zirconium metal powder, gem grade zirconia and zirconium compounds like oxy-chloride, basic sulphate and basic carbonate etc. (author)

  4. Inflight dissociation of zircon in air plasma

    Energy Technology Data Exchange (ETDEWEB)

    Yugeswaran, S; Selvarajan, V [Bharathiar University, Coimbatore 641046 (India); Ananthapadmanabhan, P V; Thiyagarajan, T K [Laser and Plasma Technology Division, Bhabha Atomic Research Centre, Mumbai - 400 085 (India); Nair, Janardhanan [Ion Arc Technologies Pvt Ltd, Coimbatore (India)

    2010-02-01

    Thermal dissociation of zircon can be conveniently carried out in a plasma reactor, which is characterized by high temperature, high energy density and high quench rate. Zirconia is recovered from this partially dissociated zircon by alkali leaching. Dissociation of zircon has been conventionally carried out in argon gas, which is expensive. The present paper reports experimental results on thermal dissociation of zircon in air plasma medium. Process simulation for 'inflight' dissociation of zircon in air plasma medium is also presented. The experimental system consists of a central hollow graphite electrode, which acts as the cathode and a graphite anode. The material to be processed is fed centrally through the cathode. The unique feature of the system is that it uses air as the working gas to generate the thermal plasma. The system has been used to study in-flight dissociation of zircon in the thermal plasma jet. Dissociation was carried out over 10-25 kW power range. Results of the study indicate that complete dissociation of zircon to ZrO{sub 2} and silica could be accomplished at 25 kW in air plasma.

  5. Inflight dissociation of zircon in air plasma

    International Nuclear Information System (INIS)

    Yugeswaran, S; Selvarajan, V; Ananthapadmanabhan, P V; Thiyagarajan, T K; Nair, Janardhanan

    2010-01-01

    Thermal dissociation of zircon can be conveniently carried out in a plasma reactor, which is characterized by high temperature, high energy density and high quench rate. Zirconia is recovered from this partially dissociated zircon by alkali leaching. Dissociation of zircon has been conventionally carried out in argon gas, which is expensive. The present paper reports experimental results on thermal dissociation of zircon in air plasma medium. Process simulation for 'inflight' dissociation of zircon in air plasma medium is also presented. The experimental system consists of a central hollow graphite electrode, which acts as the cathode and a graphite anode. The material to be processed is fed centrally through the cathode. The unique feature of the system is that it uses air as the working gas to generate the thermal plasma. The system has been used to study in-flight dissociation of zircon in the thermal plasma jet. Dissociation was carried out over 10-25 kW power range. Results of the study indicate that complete dissociation of zircon to ZrO 2 and silica could be accomplished at 25 kW in air plasma.

  6. Titan Casts Revealing Shadow

    Science.gov (United States)

    2004-05-01

    A rare celestial event was captured by NASA's Chandra X-ray Observatory as Titan -- Saturn's largest moon and the only moon in the Solar System with a thick atmosphere -- crossed in front of the X-ray bright Crab Nebula. The X-ray shadow cast by Titan allowed astronomers to make the first X-ray measurement of the extent of its atmosphere. On January 5, 2003, Titan transited the Crab Nebula, the remnant of a supernova explosion that was observed to occur in the year 1054. Although Saturn and Titan pass within a few degrees of the Crab Nebula every 30 years, they rarely pass directly in front of it. "This may have been the first transit of the Crab Nebula by Titan since the birth of the Crab Nebula," said Koji Mori of Pennsylvania State University in University Park, and lead author on an Astrophysical Journal paper describing these results. "The next similar conjunction will take place in the year 2267, so this was truly a once in a lifetime event." Animation of Titan's Shadow on Crab Nebula Animation of Titan's Shadow on Crab Nebula Chandra's observation revealed that the diameter of the X-ray shadow cast by Titan was larger than the diameter of its solid surface. The difference in diameters gives a measurement of about 550 miles (880 kilometers) for the height of the X-ray absorbing region of Titan's atmosphere. The extent of the upper atmosphere is consistent with, or slightly (10-15%) larger, than that implied by Voyager I observations made at radio, infrared, and ultraviolet wavelengths in 1980. "Saturn was about 5% closer to the Sun in 2003, so increased solar heating of Titan may account for some of this atmospheric expansion," said Hiroshi Tsunemi of Osaka University in Japan, one of the coauthors on the paper. The X-ray brightness and extent of the Crab Nebula made it possible to study the tiny X-ray shadow cast by Titan during its transit. By using Chandra to precisely track Titan's position, astronomers were able to measure a shadow one arcsecond in

  7. Production of continuous piezoelectric ceramic fibers for smart materials and active control devices

    Science.gov (United States)

    French, Jonathan D.; Weitz, Gregory E.; Luke, John E.; Cass, Richard B.; Jadidian, Bahram; Bhargava, Parag; Safari, Ahmad

    1997-05-01

    Advanced Cerametrics Inc. has conceived of and developed the Viscous-Suspension-Spinning Process (VSSP) to produce continuous fine filaments of nearly any powdered ceramic materials. VSSP lead zirconate titanate (PZT) fiber tows with 100 and 790 filaments have been spun in continuous lengths exceeding 1700 meters. Sintered PZT filaments typically are 10 - 25 microns in diameter and have moderate flexibility. Prior to carrier burnout and sintering, VSSP PZT fibers can be formed into 2D and 3D shapes using conventional textile and composite forming processes. While the extension of PZT is on the order of 20 microns per linear inch, a woven, wound or braided structure can contain very long lengths of PZT fiber and generate comparatively large output strokes from relatively small volumes. These structures are intended for applications such as bipolar actuators for fiber optic assembly and repair, vibration and noise damping for aircraft, rotorcraft, automobiles and home applications, vibration generators and ultrasonic transducers for medical and industrial imaging. Fiber and component cost savings over current technologies, such as the `dice-and-fill' method for transducer production, and the range of unique structures possible with continuous VSSP PZT fiber are discussed. Recent results have yielded 1-3 type composites (25 vol% PZT) with d33 equals 340 pC/N, K equals 470, and g33 equals 80 mV/N, kt equals 0.54, kp equals 0.19, dh equals 50.1pC/N and gh equals 13 mV/N.

  8. At what conditions does zircon grow/dissolve during high-T metamorphism? Relating zircon textures to PT-conditions

    Science.gov (United States)

    Kunz, Barbara E.; Regis, Daniele; Manzotti, Paola; Engi, Martin

    2015-04-01

    A key question in ziconology is when and how zircon grows during metamorphism. To shed light on zircon forming processes and the corresponding PT-conditions during high-T metamorphism a case study was undertaken. The Ivrea Zone (N-Italy) exposes a lower continental crustal section in which a continuous metamorphic field gradient from amphibolite to granulite facies is documented. This field gradient is thought to reflect protracted heating during late Paleozoic times, with a probable high-T peak in the Permian. We present first results from a primarily textural study supported by U-Pb ages, Th/U ratios and Ti-in-Zrn thermometry. Four types of zircon were identified based on their overgrowth proportions and the preservation of detrital cores. Zircon grains were thus classified as Type1 - detrital grains with no overgrowth or very narrow rims (300 Ma) and appears to reflect an early dehydration phase. Rim2b has Permian ages (median 275 Ma), is by far the most common overgrowth type, found in a wide PT-range. Its development appears related to biotite breakdown. Rim3 is texturally indicative of magmatic zircon, occurs only in diatexites. Rim4 is the latest overgrowth and is locally found at all metamorphic grades. Textural features suggest late fluid-related recrystallization of existing zircon. At lowest grade (675±35°C, 6±2 kbar) zircons show type1 only, overgrowths are too thin to clearly identify the rim type. Further upgrade (~700°C, 7 kbar) type1 and type2 dominate. Type2 zircons show rim1, rim2a and occasionally rim4. At the Mu-out isograd (750±50°C, 8.2±1.4 kbar) most zircons are of type2, now with rim2b instead of 2a, in addition to rim1 and rim4. Near and in granulite facies (to 800°C, 8±2 kbar) mostly zircon type2 and type4 are present. While rim1 gets more narrow with increasing metamorphic grade, rim2b grows significantly thicker. Occasionally rim2a and rim4 occur. Close to the Bt-out isograd (~860°C, 9.2±1.7 kbar), mostly type3 and type4 are

  9. Occupational exposure to natural radioactivity in a zircon sand milling plant

    International Nuclear Information System (INIS)

    Ballesteros, Luisa; Zarza, Isidoro; Ortiz, Josefina; Serradell, Vicente

    2008-01-01

    Raw zirconium sand is one of the substances (naturally occurring radioactive material, NORM) which is widely used in the ceramic industry. This sand contains varying concentrations of natural radionuclides: mostly U-238 but also Th-232 and U-235, together with their daughters, and therefore may need to be regulated by Directive 96/29/EURATOM. This paper describes the method used to perform the radiological study on a zircon sand milling plant and presents the results obtained. Internal and external doses were evaluated using radioactivity readings from sand, airborne dust, intermediate materials and end products. The results on total effective dose show the need for this type of industry to be carefully controlled, since values near to 1 mSv were obtained

  10. Occupational exposure to natural radioactivity in a zircon sand milling plant

    Energy Technology Data Exchange (ETDEWEB)

    Ballesteros, Luisa [Laboratorio de Radioactividad Ambiental, Universidad Politecnica de Valencia, Apartado 22012, E-46071 Valencia (Spain)], E-mail: lballest@upvnet.upv.es; Zarza, Isidoro [Laboratorio de Radioactividad Ambiental, Universidad Politecnica de Valencia, Apartado 22012, E-46071 Valencia (Spain)], E-mail: iszarpe@upvnet.upv.es; Ortiz, Josefina [Laboratorio de Radioactividad Ambiental, Universidad Politecnica de Valencia, Apartado 22012, E-46071 Valencia (Spain)], E-mail: jortiz@iqn.upv.es; Serradell, Vicente [Laboratorio de Radioactividad Ambiental, Universidad Politecnica de Valencia, Apartado 22012, E-46071 Valencia (Spain)], E-mail: vserradell@iqn.upv.es

    2008-10-15

    Raw zirconium sand is one of the substances (naturally occurring radioactive material, NORM) which is widely used in the ceramic industry. This sand contains varying concentrations of natural radionuclides: mostly U-238 but also Th-232 and U-235, together with their daughters, and therefore may need to be regulated by Directive 96/29/EURATOM. This paper describes the method used to perform the radiological study on a zircon sand milling plant and presents the results obtained. Internal and external doses were evaluated using radioactivity readings from sand, airborne dust, intermediate materials and end products. The results on total effective dose show the need for this type of industry to be carefully controlled, since values near to 1 mSv were obtained.

  11. Zircon-scale insights into the history of a Supervolcano, Bishop Tuff, Long Valley, California, with implications for the Ti-in-zircon geothermometer

    Science.gov (United States)

    Reid, M.R.; Vazquez, J.A.; Schmitt, A.K.

    2011-01-01

    Zircon has the outstanding capacity to record chronological, thermal, and chemical information, including the storage history of zoned silicic magma reservoirs like the one responsible for the Bishop Tuff of eastern California, USA. Our novel ion microprobe approach reveals that Bishop zircon rims with diverse chemical characteristics surround intermediate domains with broadly similar compositions. The highest Y, REE, U, and Th concentrations tend to accompany the largest excesses in Y + REE3+:P beyond what can be explained by xenotime substitution in zircon. Apparent Ti-in-zircon temperatures of Ti-in-zircon temperatures are probably better explained by sources of inaccuracy in the temperature estimates. After apparently nucleating from different melts, zircons from across the Bishop Tuff compositional spectrum may have evolved to broadly similar chemical and thermal conditions and therefore it is possible that there was no significant thermal gradient in the magma reservoir at some stage in its evolution. There is also no compelling evidence for punctuated heat ?? chemical influxes during the intermediate stages of zircon growth. Judging by the zircon record, the main volume of the erupted magma evolved normally by secular cooling but the latest erupted portion is characterized by a reversal in chemistry that appears to indicate perfusion of the magma reservoir by-or zircon entrainment in-a less evolved melt from the one in which the zircons had previously resided. ?? 2010 Springer-Verlag.

  12. Development of new functional properties in traditional ceramics field

    International Nuclear Information System (INIS)

    Carda, J.B.; Pedra, J.M.; Nunez, I.; Peiro, N.C.; Gil, C.; Navarro, E.; Gomez, J.J.; Chiva, L.

    2004-01-01

    In the present communication, several ways to obtain functional properties in ceramic tiles will be exposed, developed by the research group in Solid State Chemistry of Jaume I University from Castellon, in close collaboration with the ceramic industry set in Castellon (Spain). Then, searching for a new properties, those that involve advanced fields in ceramics, such as mechanical, electrical or optical properties have been chosen, transferring their application to traditional products, selecting for it the development of this properties in surface (as the obtaining if glass-ceramic glazes) or in the ceramic body (increasing its mechanical resistance, more dense and with less thickness of layer). Related to the surface properties interesting in traditional ceramics field, glass-ceramic glazes have been designed, presenting high resistance to abrasion and chemical agents attack, formulating systems of devitrification of α-SiO 2 crystallization (cristobalite), anoritite and zircon. Systems that reduce resistivity of glazes have been developed too, causing the discharge to the ground of the static charge, designing a semiconductor system SnO 2 -Sb 2 O 3 . o finish with surface properties, bactericidal properties glazes have been originated, working with CeO 2 -ZrO 2 and TiO 2 (anatase) systems. According to ceramic bodies, highly gressificated systems have been developed, with an open porosity lower than 0.5% of water absorption and with high mechanical resistance, aspects that open ways to develop multilayer systems allowing the reduction of body thickness without a decrease of its technical features. (author)

  13. Production of mullite-zirconia ceramics composites by 'In situ' reaction

    International Nuclear Information System (INIS)

    Melo, F.C.L. de; Cairo, C.A.A.; Piorino Neto, F.; Devezas, T.C.

    1987-01-01

    Mullita-zirconia ceramic composites were produced by 'In situ' reaction of alumina and brazilian zircon. The ideal curve of thermal treatment (reaction + sinterization) was determined for the obtention of composites of maximum mechanical resistence. The retained fraction of tetragonal fase was evaluated by X-ray difraction and correlated with the values of mechanical resistence obtained by different treatment curves. The performance of the developed composites under corrosion and thermal shock was evaluated by glass casting. (Author) [pt

  14. The Effect of Element Substitution on Ti-in-Zircon Geothermometry in Volcanic Zircons from Mount Pinatubo, Philippines

    Science.gov (United States)

    Lee, S. L.; Hattori, K.

    2017-12-01

    Despite the extensive application of the Ti-in-zircon geothermometer, its accuracy in natural systems remains uncertain. In order to investigate the parameters contributing to Ti in zircon, we examined zircons from dacitic eruption products of Mount Pinatubo, Philippines, from the Pliocene (>2.5-2.7 Ma), 35000BP and 1991AD. All samples are unaltered and quenched from magmas at 790-825°C (Fe-Ti-oxide thermometry). Furthermore, the magma conditions of 1991 samples are well characterized: 780°C (cummingtonite rims on hornblende, Fe-Ti-oxide thermometry), 2 kbar pressure, 5.5-6.5 wt.% H2O and fO2 of NNO+1.6. Calculated zircon saturation temperatures are 760, 744 and 738°C (oldest to youngest). Zircon Ti concentrations are low (2.0-8.8 ppm), show positive covariation with U (35.6-639 ppm), Th (18.7-696 ppm), ∑REE (237-1310 ppm) and Y (247-1770 ppm), and negative covariation with Hf (7610-12000 ppm). The Ti-in-zircon geothermometer by Ferry and Watson (2007) yields mean temperatures of 690, 666 and 663°C (oldest to youngest), using TiO2 activity=0.6, SiO2 activity=1 and -40°C pressure correction. Therefore, temperatures calculated using this method are underestimated by >100°C. We suggest that elements in the Zr site impact the substitution of Ti in the Si site of zircon. Ti shows a positive covariation with Zr/Hf (37.0-57.3, r2=0.551). The ionic radius of Hf4+ is smaller than Zr4+, whereas cations like U4+, Th4+, REE3+ and Y3+ are larger. The departure from the ideal crystal configuration is evaluated using the parameter Zr/(Hf-x), whereby x=U4+, Th4+, ∑REE and Y3+. Ti contents are more strongly correlated with the parameter than Zr/Hf (r2=0.559, 0.565, 0.608, 0.616; respectively). This suggests that large cations replacing Zr strain the lattice, reducing the amount of Ti incorporated into zircon. This further suggests that ZrSiO4 activity is less than 1 in natural rocks, resulting in the systematic underestimation of Ti-in-zircon temperatures.

  15. Transformations to granular zircon revealed: Twinning, reidite, and ZrO2 in shocked zircon from Meteor Crater (Arizona, USA)

    Science.gov (United States)

    Cavosie, Aaron; Timms, Nicholas E.; Erickson, Timmons M.; Hagerty, Justin J.; Hörz, Friedrich

    2016-01-01

    Granular zircon in impact environments has long been recognized but remains poorly understood due to lack of experimental data to identify mechanisms involved in its genesis. Meteor Crater in Arizona (United States) contains abundant evidence of shock metamorphism, including shocked quartz, the high pressure polymorphs coesite and stishovite, diaplectic SiO2 glass, and lechatelierite (fused SiO2). Here we report the presence of granular zircon, a new shocked mineral discovery at Meteor Crater, that preserve critical orientation evidence of specific transformations that occurred during its formation at extreme impact conditions. The zircon grains occur as aggregates of sub-µm neoblasts in highly shocked Coconino Formation Sandstone (CFS) comprised of lechatelierite. Electron backscatter diffraction shows that each grain consists of multiple domains, some with boundaries disoriented by 65°, a known {112} shock-twin orientation. Other domains have crystallographic c-axes in alignment with {110} of neighboring domains, consistent with the former presence of the high pressure ZrSiO4 polymorph reidite. Additionally, nearly all zircon preserve ZrO2 + SiO2, providing evidence of partial dissociation. The genesis of CFS granular zircon started with detrital zircon that experienced shock-twinning and reidite formation from 20 to 30 GPa, ultimately yielding a phase that retained crystallographic memory; this phase subsequently recrystallized to systematically oriented zircon neoblasts, and in some areas partially dissociated to ZrO2. The lechatelierite matrix, experimentally constrained to form at >2000 °C, provided an ultra high-temperature environment for zircon dissociation (~1670 °C) and neoblast formation. The capacity of granular zircon to preserve a cumulative P-T record has not been recognized previously, and provides a new method for retrieving histories of impact-related mineral transformations in the crust at conditions far beyond which most rocks melt.

  16. Summary of ceramic pigments by polymer precursors Pechini method; Sintese de pigmentos ceramicos pelo metodo dos precursores polimericos

    Energy Technology Data Exchange (ETDEWEB)

    Silva, E.M. da; Galvao, S.B.; Paskocimas, C.A., E-mail: everlania_siva@yahoo.com.b [Universidade Federal do Rio Grande do Norte (UFRN), Natal, RN (Brazil)

    2010-07-01

    In this work were synthesized nitrate chromium nitrate and iron-doped titanium oxide by the polymeric precursor method, for application as ceramic pigments. The stains were developed between the temperatures 700 deg C to 1000 deg C, in green for chromium oxide and orange for iron. Noticing an increase of its opacity by increasing temperature. Characterization by thermogravimetry (TG) showed strong thermo decomposition from 355 deg C for the chromium oxide and thermo decomposition gradual for the iron. By analysis of X-ray diffraction revealed the formation of crystalline phases as Iron Titanate (FeTiO3) and Chrome Titanate (CrTiO3), respectively. The scanning electron microscopy showed the formation of rounded particles for both oxides. Thus, the synthesized oxides were within the requirements to be applied as pigments and shown to be possible to propose its use in ceramic materials. (author)

  17. (De)coupled zircon metamictization, radiation damage, and He diffusivity

    Science.gov (United States)

    Ault, A. K.; Guenthner, W.; Reiners, P. W.; Moser, A. C.; Miller, G. H.; Refsnider, K. A.

    2017-12-01

    We develop and apply a new protocol for targeting crystals for the zircon (U-Th)/He (He) thermochronometry to maximize effective U (eU) and corresponding closure temperature variability to develop zircon He date-eU correlations observed in some datasets. Our approach exploits visual proxies for radiation damage accumulation (metamictization) during zircon selection. We show that by purposefully targeting a spectrum of zircon textures from pristine to metamict grains, it is possible to generate broad eU variation in suites of zircon from a single sample and zircon He date-eU-metamictization trends that can be exploited to resolve increasingly complex thermal histories. We present plane light photographs, eU concentration, and zircon He results from 59 individual zircons from nine crystalline rock samples. Six of the nine samples come from exposed Proterozoic granitoids on SE Baffin Island, Canada; Boulder Creek, CO; Sandia Mountains, NM; and Mecca Hills, CA. We report data from three Archean Baffin samples to compare with the Proterozoic Baffin sample date-eU-metamictization trend. In each Proterozoic sample, target zircons display a spectrum of metamictization from pristine, transparent crystals to purple-brown, translucent grains. Progressive loss of transparency and increase in discoloration consistently corresponds to an increase in eU in all samples. Individual zircon eU varies from 89-1885 ppm and, within each sample, the total eU spread is 538 ppm to 1374 ppm. For any given eU value, the Archean zircon appear comparatively more metamict than the Proterozoic Baffin grains and samples collectively define a 1681 ppm range in eU, with more restrictive intrasample eU spreads (199-1120 ppm). Proterozoic samples from Baffin, Sandia, and Front Range yield negative zircon He date-eU correlations with intrasample date ranges of 90-783 Ma. Increasing eU and younger dates correspond with increasing metamictization. In contrast, all three Proterozoic Mecca Hills samples

  18. Synroc - a multiphase ceramic for high level nuclear waste immobilisation

    International Nuclear Information System (INIS)

    Reeve, K.D.; Vance, E.R.; Hart, K.P.; Smith, K.L.; Lumpkin, G.R.; Mercer, D.J.

    1992-01-01

    Many natural minerals - particularly titanates - are very durable geochemically, having survived for millions of years with very little alteration. Moreover, some of these minerals have quantitatively retained radioactive elements and their daughter products over this time. The Synroc concept mimics nature by providing an all-titanate synthetic mineral phase assemblage to immobilise high level waste (HLW) from nuclear fuel reprocessing operations for safe geological disposal. In principle, many chemically hazardous inorganic wastes arising from industry could also be immobilised in highly durable ceramics and disposed of geologically, but in practice the cost structure of most industries is such that lower cost waste management solutions - for example, the development of reusable by-products or the use of cements rather than ceramics - have to be devised. In many thousands of aqueous leach tests at ANSTO, mostly at 70-90 deg C, Synroc has been shown to be exceptionally durable. The emphases of the recent ANSTO program have been on tailoring of the Synroc composition to varying HLW compositions, leach testing of Synroc containing radioactive transuranic actinides, study of leaching mechanisms by SEM and TEM, and the development and costing of a conceptual fully active Synroc fabrication plant design. A summary of recent results on these topics will be presented. 29 refs., 4 figs

  19. Role of zircon in tracing crustal growth and recycling

    Science.gov (United States)

    Compston, W.; Williams, I. S.; Armstrong, R. A.; Claoue-Long, J. C.; Kinny, P. D.; Foster, J. J.; Kroener, A.; Pidgeon, R. T.; Myers, J. S.

    Single crystal ion probe ages of zircons is discussed, which allow much better time resolution compared to other geochronological methods, although the technique is not without problems. Rocks from two areas that contain composite zircon populations, including true magmatic zircons as well as a variety of xenocrystic types are described. It is often difficult to distinguish these; xenocrystic zircons, for example, cannot always be identified on the basis of morphology alone. Additional evidence is needed before making age interpretations. Evidence is also presented of zircon growth long after the original time of crystallization, in some cases apparently at temperatures less than 300 C. The spectacular discovery of 4.1 to 4.2 Ga detrital zircons in metaquartzites from the Mount Narryer area of Western Australia is described. Similar zircons with ages as old as 4276 Ma have been found in the nearby Jack Hills area. The source areas or parent lithologies of these zircons have not yet been determined, but the author expects that they may be unrecognized or buried antecedents of the K rich Narryer gneisses. U or Th concentrations of zircon cannot be used to discriminate between felsic and mafic source rocks.

  20. Response of zircon to electron and Ne+ irradiation

    International Nuclear Information System (INIS)

    Devanathan, R.; Weber, W.J.; Boatner, L.A.

    1997-01-01

    Zircon (ZrSiO 4 ) is an actinide host phase in vitreous ceramic nuclear waste forms and a potential host phase for the disposition of excess weapons plutonium. In the present work, the effects of 800 and 900 keV electron and 1 MeV Ne + irradiations on the structure of single crystals of ZrSiO 4 have been investigated. The microstructural evolution during the irradiations was studied in situ using a high-voltage electron microscope interfaced to an ion accelerator at Argonne National Laboratory. The results indicate that electron irradiation at 15 K cannot amorphize ZrSiO 4 even at fluences an order of magnitude higher than that required for amorphization by 1.5 MeV Kr + ions. However, the material is readily amorphized by 1 MeV Ne + irradiation at 15 K. The temperature dependence of this amorphization is discussed in light of previous studies of radiation damage in ZrSiO 4

  1. A review and discussion of candidate ceramics for immobilization of high-level fuel reprocessing wastes

    International Nuclear Information System (INIS)

    Hayward, P.J.

    1982-08-01

    This review discusses and attempts to evaluate 11 of the leading ceramic processes for hosting the high-level and high-level plus medium-level wastes which would arise from the reprocessing of used UO 2 , (Th,Pu)O 2 and (Th,U)O 2 fuels. The wasteform materials considered include glass ceramics, supercalcine ceramics, SYNROC ceramics, 'stuffed glass', titanate ceramics, cermets, clay ceramics, cement-based materials and multibarrier wasteforms. Although no attempt has been made to rank these candidates in order of superiority, the conclusion is drawn that, of the materials proposed so far, a glass ceramic appears to be best suited to the Canadian program, taking into account durability in the potential environment of a flooded vault, ability to withstand radiation and transmutation damage without serious loss of durability, ability to accommodate variable waste compositions, and ease of processing and quality control. This conclusion does not necessarily apply to other national waste management programs. However, many of the points raised might be included in any critical assessment of alternative wasteform materials

  2. Beneficiation of low grade zircon concentrate

    International Nuclear Information System (INIS)

    Rehim, A.A.

    1976-01-01

    The zircon concentrate obtained from black sands, contains considerable amount of rutile and some ilmenite. It is necessary to separate these minerals before the metallurgical processing of zircon, as otherwise the zirconium products obtained will be contaminated with large amount of titanium. The present work explores the possibility of purification of zircon from rutile and other minerals by flotation. Effective separation can be obtained by selective flotation using oleic acid and liquid glass in alkaline medium or sodium silicon fluoride in weak acidic medium. (author)

  3. Titan Aerial Daughtercraft

    Data.gov (United States)

    National Aeronautics and Space Administration — Saturn's giant moon Titan has become one of the most fascinating bodies in the Solar System. Titan is the richest laboratory in the solar system for studying...

  4. Effect of material constants on power output in piezoelectric vibration-based generators.

    Science.gov (United States)

    Takeda, Hiroaki; Mihara, Kensuke; Yoshimura, Tomohiro; Hoshina, Takuya; Tsurumi, Takaaki

    2011-09-01

    A possible power output estimation based on material constants in piezoelectric vibration-based generators is proposed. A modified equivalent circuit model of the generator was built and was validated by the measurement results in the generator fabricated using potassium sodium niobate-based and lead zirconate titanate (PZT) ceramics. Subsequently, generators with the same structure using other PZT-based and bismuth-layered structure ferroelectrics ceramics were fabricated and tested. The power outputs of these generators were expressed as a linear functions of the term composed of electromechanical coupling coefficients k(sys)(2) and mechanical quality factors Q*(m) of the generator. The relationship between device constants (k(sys)(2) and Q*(m)) and material constants (k(31)(2) and Q(m)) was clarified. Estimation of the power output using material constants is demonstrated and the appropriate piezoelectric material for the generator is suggested.

  5. Enhancement of the piezoelectric properties of sodium lanthanum bismuth titanate (Na0.5La0.5Bi4Ti4O15) through modification with cobalt

    International Nuclear Information System (INIS)

    Wang Chunming; Wang Jinfeng; Zheng Limei; Zhao Minglei; Wang Chunlei

    2010-01-01

    The dielectric, piezoelectric, and electromechanical properties of B-site cobalt-modified sodium lanthanum bismuth titanate (Na 0.5 La 0.5 Bi 4 Ti 4 O 15 , NLBT) piezoelectric ceramics were investigated. The piezoelectric properties of NLBT ceramics can be enhanced by cobalt modifications. The NLBT ceramics modified with 0.2 wt.% cobalt trioxide (NLBT-C4) possess good piezoelectric properties, with piezoelectric coefficient d 33 of 27 pC/N, electromechanical coupling factors (k p and k t ) of 6.5% and 28.5%, and mechanical quality factor Q m (k p mode) of 3400. The Curie temperature T c of cobalt-modified NLBT ceramics was found to slightly higher than that of pure NLBT ceramics. A large dielectric abnormity in dielectric loss tan δ was observed in NLBT ceramics, which can be significantly suppressed by cobalt modification. Thermal annealing studies presented the cobalt-modified NLBT ceramics possess stable piezoelectric properties.

  6. Zircon/fluid trace element partition coefficients measured by recrystallization of Mud Tank zircon at 1.5 GPa and 800-1000 °C

    Science.gov (United States)

    Ayers, John C.; Peters, Timothy J.

    2018-02-01

    Hydrothermal zircon grains have trace element characteristics such as low Th/U, high U, and high rare earth element (REE) concentrations that distinguish them from magmatic, metamorphic, and altered zircon grains, but it is unclear whether these characteristics result from distinctive fluid compositions or zircon/fluid fractionation effects. New experiments aimed at measuring zircon/fluid trace element partition coefficients Dz/f involved recrystallizing natural Mud Tank zircon with low trace element concentrations in the presence of H2O, 1 m NaOH, or 1 m HCl doped with ∼1000 ppm of rare earth elements (REE), Y, U and Th and ∼500 ppm of Li, B, P, Nb, Ba, Hf, and Ta. Experiments were run for 168 h at 1.5 GPa, 800-1000 °C, and fO2 = NNO in a piston cylinder apparatus using the double capsule method. LA-ICP-MS analysis shows that run product zircon crystals have much higher trace element concentrations than in Mud Tank zircon starting material. Dz/f values were estimated from run product zircon analyses and bulk composition using mass balance. Most elements behave incompatibly, with median Dz/f being highest for Hf = 8 and lowest for B = 0.02. Addition of NaOH or HCl had little influence on Dz/f values. Dz/f for LREE are anomalously high, likely due to contamination of run product zircon with quenched solutes enriched in incompatible elements, so DLREE were estimated using lattice strain theory. Brice curves for +3 ions yield zircon/fluid DLu/DLa of ∼800-5000. A Brice curve fit to +4 ions yielded DCe4+ values. Estimated concentrations of Ce3+ and Ce4+ show that the average Ce4+/Ce3+ in zircon of 27 is much higher than in fluid of 0.02. Th and U show little fractionation, with median DTh/DU = 0.7, indicating that the low Th/U in natural hydrothermal zircon is inherited from the fluid. Natural fluid compositions estimated from measured Dz/f and published compositions of hydrothermal zircon grains from aplite and eclogite reflect the mineralogy of the host rock, e

  7. Scaling up aqueous processing of A-site deficient strontium titanate for SOFC anode supports

    DEFF Research Database (Denmark)

    Verbraeken, Maarten C.; Sudireddy, Bhaskar Reddy; Vasechko, Viacheslav

    2018-01-01

    All ceramic anode supported half cells of technically relevant scale were fabricated in this study, using a novel strontium titanate anode material. The use of this material would be highly advantageous in solid oxide fuel cells due to its redox tolerance and resistance to coking and sulphur...... poisoning. Successful fabrication was possible through aqueous tape casting of both anode support and electrolyte layers and subsequent lamination. Screen printing of electrolyte layers onto green anode tapes was also attempted but resulted in cracked electrolyte layers upon firing. Microstructural...

  8. Fission track dating of zircon: a multichronometer

    International Nuclear Information System (INIS)

    Carpena, J.

    1992-01-01

    Scattering in Fission Track ages of zircons of a single rock is possible when they present morphological and geochemical variations, if the greatest care is not taken in the choice of the etching conditions and the counting of tracks. The Fission Track study of two heterogeneous populations of zircons from the Mont Blanc granite and from the Gran Paradiso gneisses allows to show that zircon may work as a multichronometer

  9. Status of plutonium ceramic immobilization processes and immobilization forms

    International Nuclear Information System (INIS)

    Ebbinghaus, B.B.; Van Konynenburg, R.A.; Vance, E.R.; Jostsons, A.

    1996-01-01

    Immobilization in a ceramic followed by permanent emplacement in a repository or borehole is one of the alternatives currently being considered by the Fissile Materials Disposition Program for the ultimate disposal of excess weapons-grade plutonium. To make Pu recovery more difficult, radioactive cesium may also be incorporated into the immobilization form. Valuable data are already available for ceramics form R ampersand D efforts to immobilize high-level and mixed wastes. Ceramics have a high capacity for actinides, cesium, and some neutron absorbers. A unique characteristic of ceramics is the existence of mineral analogues found in nature that have demonstrated actinide immobilization over geologic time periods. The ceramic form currently being considered for plutonium disposition is a synthetic rock (SYNROC) material composed primarily of zirconolite (CaZrTi 2 O 7 ), the desired actinide host phase, with lesser amounts of hollandite (BaAl 2 Ti 6 O 16 ) and rutile (TiO 2 ). Alternative actinide host phases are also being considered. These include pyrochlore (Gd 2 Ti 2 O 7 ), zircon (ZrSiO 4 ), and monazite (CePO 4 ), to name a few of the most promising. R ampersand D activities to address important technical issues are discussed. Primarily these include moderate scale hot press fabrications with plutonium, direct loading of PuO 2 powder, cold press and sinter fabrication methods, and immobilization form formulation issues

  10. Measurement of blowdown flow rates using load cells

    International Nuclear Information System (INIS)

    Dolas, P.K.; Venkat Raj, V.; Ghosh, A.K.; Murty, L.G.K.; Muralidhar Rao, S.

    1980-01-01

    To establish a reliable method for measuring two-phase flow, experiments were planned for measurement of transient single phase flow rates from vessels using load cells. Suitability of lead-zirconate-titanate piezoelectric ceramic discs was examined. Discharge time constant of the disc used was low, leading to large measurement errors. Subsequently, experiments were carried out using strain gauge load cells and these were found satisfactory. The unsteady flow equation has been derived for the system under investigation. The equation has been solved numerically using the fourth order Runge-Kutta method and also by integrating it analytically. The experimental results are compared with the theoretical results and presented in this report. (auth.)

  11. Texture of poled tetragonal PZT detected by synchrotron X-ray diffraction and micromechanics analysis

    International Nuclear Information System (INIS)

    Hall, D.A.; Steuwer, A.; Cherdhirunkorn, B.; Withers, P.J.; Mori, T.

    2005-01-01

    The texture and lattice elastic strain due to electrical poling of tetragonal PZT (lead zirconate titanate) ceramics have been measured using high energy synchrotron X-ray diffraction. It is shown that XRD peak intensity ratios associated with crystal planes of the form {002}, {112} and {202} exhibit a linear dependence on cos-bar 2 Ψ, where Ψ represents the orientation angle between the plane normal and the macroscopic poling axis. The observed dependence of texture and lattice strain on the grain orientation can be understood on the basis that the macroscopic strain due to poling is the average of the poling strains of all the individual grains

  12. Hyperfine interaction measurements on ceramics: PZT revisited

    International Nuclear Information System (INIS)

    Guarany, Cristiano A.; Araujo, Eudes B.; Silva, Paulo R.J.; Saitovitch, Henrique

    2007-01-01

    The solid solution of PbZr 1- x Ti x O 3 , known as lead-zirconate titanate (PZT), was probably one of the most studied ferroelectric materials, especially due to its excellent dielectric, ferroelectric and piezoelectric properties. The highest piezoelectric coefficients of the PZT are found near the morphotropic phase boundary (MPB) (0.46≤x≤0.49), between the tetragonal and rhombohedral regions of the composition-temperature phase diagram. Recently, a new monoclinic phase near the MPB was observed, which can be considered as a 'bridge' between PZT's tetragonal and rhombohedral phases. This work is concerned with the study of the structural properties of the ferroelectric PZT (Zr/Ti=52/48, 53/47) by hyperfine interaction (HI) measurements obtained from experiments performed by using the nuclear spectroscopy time differential perturbed angular correlation (TDPAC) in a wide temperature range

  13. Single-zircon dating by stepwise Pb-evaporation constrains the Archean history of detrital zircons from the Jack Hills, Western Australia

    International Nuclear Information System (INIS)

    Kober, B.; Lippolt, H.J.; Pidgeon, R.T.

    1989-01-01

    Pb isotope analyses have been carried out on 42 zircon grains from a Western Australian metaconglomerate using stepwise Pb-evaporation directly in the ion source of a thermal ionization mass spectrometer. The metaconglomerate is from the Archean Jack Hills Metasedimentary Belt, and is known from ion microprobe (''SHRIMP'') analyses to contain a complex zircon population with ages between 4.2 Ga and 3.1 Ga. The same complex pattern of ages is found by the Pb evaporation studies. Five grains yielded minimum crystallization ages from 4.17 Ga to 4.07 Ga. The main population appears significantly younger, having been generated at about 3.55-3.3 Ga. The agreement between the two analytical approaches confirms the SHRIMP results and demonstrates the value of the stepwise-evaporation technique in determining the age patterns of mixing zircon populations. In many of the evaporative Pb isotope records the 207/206 ratios remained constant for all evaporation steps, which we interpret as evaporation from concordant zircon phases. However, for the majority of zircons 207/206 ratios increased with increasing evaporation temperature, and usually approached constant values during evaporation at the highest temperatures. This can be attributed to mixing of different radiogenic Pb components from either crystalline zircon phases of different ages or from domains of isotopically disturbed metamict zircon. Present results confirm > 4 Ga zircon ages in the metaconglomerate from the Hack Hills and substantiate formation of crust at a very early stage in the evolution of the earth. Results also confirm a major crust-forming event 3.55-3.3 Ga ago. (orig.)

  14. PZ, PT and PZT formation from metal citrates

    International Nuclear Information System (INIS)

    Bastos, C.M.R.; Zaghette, M.A.; Jafelicci Junior, M.; Varela, J.A.

    1990-01-01

    Lead zirconate, lead titanate and lead titanate-zirconate were obtained by mechanical mixing of lead, titanium and zirconium citrates in ether and by calcination. The process was analyzed by DTA, TGA, IR, pore size distribution and surface area measurements. The results indicate that the decomposition reaction and formation of PZ, PT occur simultaneaously without formation of intermediate compounds. PZT was formed from 500 0 C. (author) [pt

  15. Fission track dating of kimberlitic zircons

    International Nuclear Information System (INIS)

    Haggerty, S.E.

    1983-01-01

    The only reliable method for dating kimberlites at present is the lengthy and specialized hydrothermal procedure that extracts 206 Pb and 238 U from low-uranium zircons. This paper describes a second successful method by fission track dating of large single-crystal zircons, 1.0-1.5 cm in dimension. The use of large crystals overcomes the limitations imposed in conventional fission track analysis which utilizes crushed fragments. Low track densities, optical track dispersion, and the random orientation of polished surfaces in the etch and irradiation cycle are effectively overcome. Fission track ages of zircons from five African kimberlites are reported, from the Kimberley Pool (90.0 +- 6.5 m.y.), Orapa (87.4 +- 5.7 and 92.4 +- 6.1 m.y.), Nzega (51.1 +- 3.8 m.y.), Koffiefontein (90.9 +- 8.2 m.y.), and Val do Queve (133.4 +- 11.5 m.y.). In addition we report the first radiometric ages (707.9 +- 59.6 and 705.5 +- 61.0 m.y.) of crustal zircons from kimberlites in northwest Liberia. The fission track ages agree well with earlier age estimates. Most of the zircons examined in this study are zoned with respect to uranium but linear correlations are established (by regression analysis) between zones of variable uranium content, and within zones of constant uranium content (by analysis of variance). Concordance between the fission track method and the U/Pb technique is established and we concluded that track fading from thermal annealing has not taken place. Kimberlitic zircons dated in this study, therefore, record the time of eruption. (orig.)

  16. Thermal diffusivity of samarium-gadolinium zirconate solid solutions

    International Nuclear Information System (INIS)

    Pan, W.; Wan, C.L.; Xu, Q.; Wang, J.D.; Qu, Z.X.

    2007-01-01

    We synthesized samarium-gadolinium zirconate solid solutions and determined their thermal diffusivities, Young's moduli and thermal expansion coefficients, which are very important for their application in thermal barrier coatings. Samarium-gadolinium zirconate solid solutions have extremely low thermal diffusivity between 20 and 600 deg. C. The solid solutions have lower Young's moduli and higher thermal expansion coefficients than those of pure samarium and gadolinium zirconates. This combination of characteristics is promising for the application of samarium and gadolinium zirconates in gas turbines. The mechanism of phonon scattering by point defects is discussed

  17. Testing the reliability of information extracted from ancient zircon

    Science.gov (United States)

    Kielman, Ross; Whitehouse, Martin; Nemchin, Alexander

    2015-04-01

    Studies combining zircon U-Pb chronology, trace element distribution as well as O and Hf isotope systematics are a powerful way to gain understanding of the processes shaping Earth's evolution, especially in detrital populations where constraints from the original host are missing. Such studies of the Hadean detrital zircon population abundant in sedimentary rocks in Western Australia have involved analysis of an unusually large number of individual grains, but also highlighted potential problems with the approach, only apparent when multiple analyses are obtained from individual grains. A common feature of the Hadean as well as many early Archaean zircon populations is their apparent inhomogeneity, which reduces confidence in conclusions based on studies combining chemistry and isotopic characteristics of zircon. In order to test the reliability of information extracted from early Earth zircon, we report results from one of the first in-depth multi-method study of zircon from a relatively simple early Archean magmatic rock, used as an analogue to ancient detrital zircon. The approach involves making multiple SIMS analyses in individual grains in order to be comparable to the most advanced studies of detrital zircon populations. The investigated sample is a relatively undeformed, non-migmatitic ca. 3.8 Ga tonalite collected a few kms south of the Isua Greenstone Belt, southwest Greenland. Extracted zircon grains can be combined into three different groups based on the behavior of their U-Pb systems: (i) grains that show internally consistent and concordant ages and define an average age of 3805±15 Ma, taken to be the age of the rock, (ii) grains that are distributed close to the concordia line, but with significant variability between multiple analyses, suggesting an ancient Pb loss and (iii) grains that have multiple analyses distributed along a discordia pointing towards a zero intercept, indicating geologically recent Pb-loss. This overall behavior has

  18. EIS Data Call Report: Plutonium immobilization plant using ceramic in new facilities at the Savannah River Site

    International Nuclear Information System (INIS)

    DiSabatino, A.

    1998-01-01

    The Plutonium Immobilization Plant (PIP) accepts plutonium (Pu) from pit conversion and from non-pit sources and, through a ceramic immobilization process, converts the plutonium into an immobilized form that can be disposed of in a high level waste (HLW) repository. This immobilization process is shown conceptually in Figure 1-1. The objective is to make an immobilized form, suitable for geologic disposal, in which the plutonium is as inherently unattractive and inaccessible as the plutonium in spent fuel from commercial reactors. The ceramic immobilization alternative presented in this report consists of first converting the surplus material to an oxide, followed by incorporating the plutonium oxide into a titanate-based ceramic material that is placed in metal cans

  19. The TITAN reversed-field-pinch fusion reactor study

    International Nuclear Information System (INIS)

    1990-01-01

    This report discusses the following topics: overview of titan-2 design; titan-2 fusion-power-core engineering; titan-2 divertor engineering; titan-2 tritium systems; titan-2 safety design and radioactive-waste disposal; and titan-2 maintenance procedures

  20. The TITAN reversed-field-pinch fusion reactor study

    Energy Technology Data Exchange (ETDEWEB)

    1990-01-01

    This report discusses the following topics: overview of titan-2 design; titan-2 fusion-power-core engineering; titan-2 divertor engineering; titan-2 tritium systems; titan-2 safety design and radioactive-waste disposal; and titan-2 maintenance procedures.

  1. Titan's organic chemistry

    Science.gov (United States)

    Sagan, C.; Thompson, W. R.; Khare, B. N.

    1985-01-01

    Voyager discovered nine simple organic molecules in the atmosphere of Titan. Complex organic solids, called tholins, produced by irradiation of the simulated Titanian atmosphere, are consistent with measured properties of Titan from ultraviolet to microwave frequencies and are the likely main constituents of the observed red aerosols. The tholins contain many of the organic building blocks central to life on earth. At least 100-m, and possibly kms thicknesses of complex organics have been produced on Titan during the age of the solar system, and may exist today as submarine deposits beneath an extensive ocean of simple hydrocarbons.

  2. A green synthesis of a layered titanate, potassium lithium titanate; lower temperature solid-state reaction and improved materials performance

    International Nuclear Information System (INIS)

    Ogawa, Makoto; Morita, Masashi; Igarashi, Shota; Sato, Soh

    2013-01-01

    A layered titanate, potassium lithium titanate, with the size range from 0.1 to 30 µm was prepared to show the effects of the particle size on the materials performance. The potassium lithium titanate was prepared by solid-state reaction as reported previously, where the reaction temperature was varied. The reported temperature for the titanate preparation was higher than 800 °C, though 600 °C is good enough to obtain single-phase potassium lithium titanate. The lower temperature synthesis is cost effective and the product exhibit better performance as photocatalysts due to surface reactivity. - Graphical abstract: Finite particle of a layered titanate, potassium lithium titanate, was prepared by solid-state reaction at lower temperature to show modified materials performance. Display Omitted - Highlights: • Potassium lithium titanate was prepared by solid-state reaction. • Lower temperature reaction resulted in smaller sized particles of titanate. • 600 °C was good enough to obtain single phased potassium lithium titanate. • The product exhibited better performance as photocatalyst

  3. Oxygen diffusion in zircon

    Science.gov (United States)

    Watson, E. B.; Cherniak, D. J.

    1997-05-01

    Oxygen diffusion in natural, non-metamict zircon was characterized under both dry and water-present conditions at temperatures ranging from 765°C to 1500°C. Dry experiments were performed at atmospheric pressure by encapsulating polished zircon samples with a fine powder of 18O-enriched quartz and annealing the sealed capsules in air. Hydrothermal runs were conducted in cold-seal pressure vessels (7-70 MPa) or a piston cylinder apparatus (400-1000 MPa) on zircon samples encapsulated with both 18O-enriched quartz and 18O water. Diffusive-uptake profiles of 18O were measured in all samples with a particle accelerator, using the 18O(p, α) 15N reaction. For dry experimental conditions at 1100-1500°C, the resulting oxygen diffusivities (24 in all) are well described by: D dry (m 2/s) = 1.33 × 10 -4exp(-53920/T) There is no suggestion of diffusive anisotropy. Under wet conditions at 925°C, oxygen diffusion shows little or no dependence upon P H 2O in the range 7-1000 MPa, and is insensitive to total pressure as well. The results of 27 wet experiments at 767-1160°C and 7-1000 MPa can be described a single Arrhenius relationship: D wet (m 2/s) = 5.5 × 10 -12exp(-25280/T) The insensitivity of oxygen diffusion to P H 2O means that applications to geologic problems can be pursued knowing only whether the system of interest was 'wet' (i.e., P H 2O > 7MPa ) or 'dry'. Under dry conditions (presumably rare in the crust), zircons are extremely retentive of their oxygen isotopic signatures, to the extent that δ 18O would be perturbed at the center of a 200 μm zircon only during an extraordinarily hot and protracted event (e.g., 65 Ma at 900°C). Under wet conditions, δ 18O may or may not be retained in the central regions of individual crystals, cores or overgrowth rims, depending upon the specific thermal history of the system.

  4. The TITAN reversed-field-pinch fusion reactor study

    International Nuclear Information System (INIS)

    1990-01-01

    This report discusses research on the titan-1 fusion power core. The major topics covered are: titan-1 fusion-power-core engineering; titan-1 divertor engineering; titan-1 tritium systems; titan-1 safety design and radioactive-waste disposal; and titan-1 maintenance procedures

  5. The TITAN reversed-field-pinch fusion reactor study

    Energy Technology Data Exchange (ETDEWEB)

    1990-01-01

    This report discusses research on the titan-1 fusion power core. The major topics covered are: titan-1 fusion-power-core engineering; titan-1 divertor engineering; titan-1 tritium systems; titan-1 safety design and radioactive-waste disposal; and titan-1 maintenance procedures.

  6. Control of piezoelectricity in amino acids by supramolecular packing

    Science.gov (United States)

    Guerin, Sarah; Stapleton, Aimee; Chovan, Drahomir; Mouras, Rabah; Gleeson, Matthew; McKeown, Cian; Noor, Mohamed Radzi; Silien, Christophe; Rhen, Fernando M. F.; Kholkin, Andrei L.; Liu, Ning; Soulimane, Tewfik; Tofail, Syed A. M.; Thompson, Damien

    2018-02-01

    Piezoelectricity, the linear relationship between stress and induced electrical charge, has attracted recent interest due to its manifestation in biological molecules such as synthetic polypeptides or amino acid crystals, including gamma (γ) glycine. It has also been demonstrated in bone, collagen, elastin and the synthetic bone mineral hydroxyapatite. Piezoelectric coefficients exhibited by these biological materials are generally low, typically in the range of 0.1-10 pm V-1, limiting technological applications. Guided by quantum mechanical calculations we have measured a high shear piezoelectricity (178 pm V-1) in the amino acid crystal beta (β) glycine, which is of similar magnitude to barium titanate or lead zirconate titanate. Our calculations show that the high piezoelectric coefficients originate from an efficient packing of the molecules along certain crystallographic planes and directions. The highest predicted piezoelectric voltage constant for β-glycine crystals is 8 V mN-1, which is an order of magnitude larger than the voltage generated by any currently used ceramic or polymer.

  7. Control of piezoelectricity in amino acids by supramolecular packing.

    Science.gov (United States)

    Guerin, Sarah; Stapleton, Aimee; Chovan, Drahomir; Mouras, Rabah; Gleeson, Matthew; McKeown, Cian; Noor, Mohamed Radzi; Silien, Christophe; Rhen, Fernando M F; Kholkin, Andrei L; Liu, Ning; Soulimane, Tewfik; Tofail, Syed A M; Thompson, Damien

    2018-02-01

    Piezoelectricity, the linear relationship between stress and induced electrical charge, has attracted recent interest due to its manifestation in biological molecules such as synthetic polypeptides or amino acid crystals, including gamma (γ) glycine. It has also been demonstrated in bone, collagen, elastin and the synthetic bone mineral hydroxyapatite. Piezoelectric coefficients exhibited by these biological materials are generally low, typically in the range of 0.1-10 pm V -1 , limiting technological applications. Guided by quantum mechanical calculations we have measured a high shear piezoelectricity (178 pm V -1 ) in the amino acid crystal beta (β) glycine, which is of similar magnitude to barium titanate or lead zirconate titanate. Our calculations show that the high piezoelectric coefficients originate from an efficient packing of the molecules along certain crystallographic planes and directions. The highest predicted piezoelectric voltage constant for β-glycine crystals is 8 V mN -1 , which is an order of magnitude larger than the voltage generated by any currently used ceramic or polymer.

  8. THE APPLICATION OF STEREOLOGY METHOD FOR ESTIMATING THE NUMBER OF 3D BaTiO3 – CERAMIC GRAINS CONTACT SURFACES

    Directory of Open Access Journals (Sweden)

    Vojislav V Mitić

    2011-05-01

    Full Text Available Methods of stereological study are of great importance for structural research of electronic ceramic materials including BaTiO3-ceramic materials. The broad application of ceramics, based on barium-titanate, in advanced electronics nowadays demands a constant research of its structure, that through the correlation structureproperties, a fundamental in the basic materials properties prognosis triad (technology-structure-properties, leads to further prognosis and properties design of these ceramics. Microstructure properties of BaTiO3- ceramic material, expressed in grains' boundary contact, are of basic importance for electric properties of this material, particularly the capacity. In this paper, a significant step towards establishing control under capacitive properties of BaTiO3-ceramics is being done by estimating the number of grains contact surfaces. Defining an efficient stereology method for estimating the number of BaTiO3-ceramic grains contact surfaces, we have started from a mathematical model of mutual grains distribution in the prescribed volume of BaTiO3-ceramic sample. Since the real microstructure morphology of BaTiO3-ceramics is in some way disordered, spherical shaped grains, using computer-modelling methods, are approximated by polyhedra with a great number of small convex polygons. By dividing the volume of BaTiO3-ceramic sample with the definite number of parallel planes, according to a given pace, into the intersection plane a certain number of grains contact surfaces are identified. According to quantitative estimation of 2D stereological parameters the modelled 3D internal microstructure is obtained. Experiments were made by using the scanning electronic microscopy (SEM method with the ceramic samples prepared under pressing pressures up to 150 MPa and sintering temperature up to 1370°C while the obtained microphotographs were used as a base of confirming the validity of presented stereology method. This paper, by applying

  9. Are there impact-formed zircons in the Hadean record?

    Science.gov (United States)

    Wielicki, M. M.; Lu, X.; Bell, E. A.; Schmitt, A. K.; Harrison, T. M.

    2008-12-01

    Detrital Hadean zircons from the Jack Hills, Western Australia, show a remarkable cluster of crystallization temperatures at 680±25°C. This is particularly surprising as a simple model relating rock composition and Zr concentration predicts that a very broad spectrum of crystallization temperatures (ca. 650°C to 1000°C) with a median value of 780°C, would result from impact melting of the Earth's surface. Magmatic fractionation would tend to increase the aforementioned values. Given the predicted high rate of impacts during the Hadean, the absence of such a population in the Jack Hills zircons could signal a profound sampling problem, a hint of a history much different than previously supposed, or our lack of understanding of zircon formation due to impact related processes. We have begun to examine the latter issue by investigating the crystallization temperatures of zircons formed in melt sheets preserved in the geologic record. The Sudbury Igneous Complex, formed at 1850±3 Ma within the second largest impact crater on Earth, includes two igneous units termed the Black and Felsic Norites. Examination of zircons from each by SIMS confirms their crystallization age at 1847.3±2.2 Ma and yields Ti-in-zircon temperatures of 720°C and 750°C, respectively. This is consistent with that predicted from zircon saturation systematics. A statistical test indicates that the combined norite population is distinct from the Hadean temperature distribution. Thus the question arises: where are the Hadean zircons expected to have formed at >780°C via impact processes? Similar analysis is being pursued for zircons from the Vredefort Impact Structure, South Africa, which should provide further information on impact-formed zircon temperature spectra.

  10. Room temperature surface piezoelectricity in SrTiO.sub.3./sub. ceramics via piezoresponse force microscopy

    Czech Academy of Sciences Publication Activity Database

    Kholkin, A.; Bdikin, I.; Ostapchuk, Tetyana; Petzelt, Jan

    2008-01-01

    Roč. 93, č. 22 (2008), 222905/1-222905/3 ISSN 0003-6951 R&D Projects: GA ČR GP202/06/P219 Institutional research plan: CEZ:AV0Z10100520 Keywords : strontium titanate ceramics * piezoresponse force microscopy * flexoelectric effect * polar grain boundaries Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 3.726, year: 2008

  11. Titan's Methane Cycle is Closed

    Science.gov (United States)

    Hofgartner, J. D.; Lunine, J. I.

    2013-12-01

    Doppler tracking of the Cassini spacecraft determined a polar moment of inertia for Titan of 0.34 (Iess et al., 2010, Science, 327, 1367). Assuming hydrostatic equilibrium, one interpretation is that Titan's silicate core is partially hydrated (Castillo-Rogez and Lunine, 2010, Geophys. Res. Lett., 37, L20205). These authors point out that for the core to have avoided complete thermal dehydration to the present day, at least 30% of the potassium content of Titan must have leached into an overlying water ocean by the end of the core overturn. We calculate that for probable ammonia compositions of Titan's ocean (compositions with greater than 1% ammonia by weight), that this amount of potassium leaching is achievable via the substitution of ammonium for potassium during the hydration epoch. Formation of a hydrous core early in Titan's history by serpentinization results in the loss of one hydrogen molecule for every hydrating water molecule. We calculate that complete serpentinization of Titan's core corresponds to the release of more than enough hydrogen to reconstitute all of the methane atoms photolyzed throughout Titan's history. Insertion of molecular hydrogen by double occupancy into crustal clathrates provides a storage medium and an opportunity for ethane to be converted back to methane slowly over time--potentially completing a cycle that extends the lifetime of methane in Titan's surface atmosphere system by factors of several to an order of magnitude over the photochemically-calculated lifetime.

  12. Direct large-scale synthesis of perovskite barium strontium titanate nano-particles from solutions

    International Nuclear Information System (INIS)

    Qi Jianquan; Wang Yu; Wan Pingchen; Long Tuli; Chan, Helen Lai Wah

    2005-01-01

    This paper reports a wet chemical synthesis technique for large-scale fabrication of perovskite barium strontium titanate nano-particles near room temperature and under ambient pressure. The process employs titanium alkoxide and alkali earth hydroxides as starting materials and involves very simple operation steps. Particle size and crystallinity of the particles are controllable by changing the processing parameters. Observations by X-ray diffraction, scanning electron microscopy and transmission electron microscopy TEM indicate that the particles are well-crystallized, chemically stoichiometric and ∼50nm in diameter. The nanoparticles can be sintered into ceramics at 1150 deg. C and show typical ferroelectric hysteresis loops

  13. (Nd0⋅065Ti0⋅87Nb0⋅065)O3 ceramic

    Indian Academy of Sciences (India)

    Unknown

    Polycrystalline ceramic samples of sodium bismuth titanate with simultaneous doping at A and B sites have been studied for the influence of ... of Nd and Nb at B site in BaTiO3 (BaNdxTi1–2xNbxO3). (Mahboob et al 2005a). Dielectric ..... hence the conduction arises due to short range translation hopping via large polarons.

  14. Microstructure evolution during pressureless sintering of bulk oxide ceramics

    Directory of Open Access Journals (Sweden)

    Karel Maca

    2009-06-01

    Full Text Available The author’s experience concerning the infl uence of the choice of different pressureless heating schedules on the fi nal microstructure of oxide ceramic materials is summarized in the paper. Alumina, ceria, strontium titanate, as well as tetragonal (3 mol% Y2O3 and cubic (8 mol% Y2O3 zirconia were cold isostatically pressed or injection moulded and pressureless sintered with different heating schedules – namely with Constant-Rate of Heating with different dwell temperatures (CRH, with Rate-Controlled Sintering (RCS and with Two-Step Sintering (TSS. It was examined whether some of these three sintering schedules, with the same fi nal density achieved, can lead to a decrease of the grain size of sintered ceramics. The results showed that only TSS (and only for selected materials brought significant decrease of the grain size.

  15. Hyperfine interaction measurements on ceramics: PZT revisited

    Energy Technology Data Exchange (ETDEWEB)

    Guarany, Cristiano A. [Universidade Estadual Paulista (Unesp), Departmento de Fisica Quimica, Caixa Postal 31, 15.385-000 Ilha Solteira, SP (Brazil); Araujo, Eudes B. [Universidade Estadual Paulista (Unesp), Departmento de Fisica Quimica, Caixa Postal 31, 15.385-000 Ilha Solteira, SP (Brazil); Silva, Paulo R.J. [Centro Brasileiro de Pesquisas Fisicas-Rua Dr. Xavier Sigaud, 150, 22290-180 Rio de Janeiro, RJ (Brazil); Saitovitch, Henrique [Centro Brasileiro de Pesquisas Fisicas-Rua Dr. Xavier Sigaud, 150, 22290-180 Rio de Janeiro, RJ (Brazil)]. E-mail: henrique@cbpf.br

    2007-02-01

    The solid solution of PbZr{sub 1-} {sub x} Ti {sub x} O{sub 3}, known as lead-zirconate titanate (PZT), was probably one of the most studied ferroelectric materials, especially due to its excellent dielectric, ferroelectric and piezoelectric properties. The highest piezoelectric coefficients of the PZT are found near the morphotropic phase boundary (MPB) (0.46{<=}x{<=}0.49), between the tetragonal and rhombohedral regions of the composition-temperature phase diagram. Recently, a new monoclinic phase near the MPB was observed, which can be considered as a 'bridge' between PZT's tetragonal and rhombohedral phases. This work is concerned with the study of the structural properties of the ferroelectric PZT (Zr/Ti=52/48, 53/47) by hyperfine interaction (HI) measurements obtained from experiments performed by using the nuclear spectroscopy time differential perturbed angular correlation (TDPAC) in a wide temperature range.

  16. Chemistry and evolution of Titan's atmosphere

    International Nuclear Information System (INIS)

    Strobel, D.F.

    1982-01-01

    The chemistry and evolution of Titan's atmosphere is reviewed in the light of the scientific findings from the Voyager mission. It is argued that the present N 2 atmosphere may be Titan's initial atmosphere rather than photochemically derived from an original NH 3 atmosphere. The escape rate of hydrogen from Titan is controlled by photochemical production from hydrocarbons. CH 4 is irreversibly converted to less hydrogen rich hydrocarbons, which over geologic time accumulate on the surface to a layer thickness of approximately 0.5 km. Magnetospheric electrons interacting with Titan's exosphere may dissociate enough N 2 into hot, escaping N atoms to remove approximately 0.2 of Titan's present atmosphere over geologic time. The energy dissipation of magnetospheric electrons exceeds solar e.u.v. energy deposition in Titan's atmosphere by an order of magnitude and is the principal driver of nitrogen photochemistry. The environmental conditions in Titan's upper atmosphere are favorable to building up complex molecules, particularly in the north polar cap region. (author)

  17. Revisiting the blocking force test on ferroelectric ceramics using high energy x-ray diffraction

    Energy Technology Data Exchange (ETDEWEB)

    Daniel, L., E-mail: laurent.daniel@u-psud.fr [School of Materials, University of Manchester, Manchester M13 9PL (United Kingdom); GeePs (CNRS UMR8507, CentraleSupelec, UPMC, Univ Paris-Sud), 91192 Gif sur Yvette cedex (France); Hall, D. A.; Withers, P. J. [School of Materials, University of Manchester, Manchester M13 9PL (United Kingdom); Koruza, J.; Webber, K. G. [Institute of Materials Science, Technische Universität Darmstadt, Alarich-Weiss-Straße 2, 64287 Darmstadt (Germany); King, A. [European Synchrotron Radiation Facility (ESRF), 6 rue J. Horowitz, 38043 Grenoble (France); Synchrotron SOLEIL, BP 48, 91192 Gif sur Yvette cedex (France)

    2015-05-07

    The blocking force test is a standard test to characterise the properties of piezoelectric actuators. The aim of this study is to understand the various contributions to the macroscopic behaviour observed during this experiment that involves the intrinsic piezoelectric effect, ferroelectric domain switching, and internal stress development. For this purpose, a high energy diffraction experiment is performed in-situ during a blocking force test on a tetragonal lead zirconate titanate (PZT) ceramic (Pb{sub 0.98}Ba{sub 0.01}(Zr{sub 0.51}Ti{sub 0.49}){sub 0.98}Nb{sub 0.02}O{sub 3}). It is shown that the usual macroscopic linear interpretation of the test can also be performed at the single crystal scale, allowing the identification of local apparent piezoelectric and elastic properties. It is also shown that despite this apparent linearity, the blocking force test involves significant non-linear behaviour mostly due to domain switching under electric field and stress. Although affecting a limited volume fraction of the material, domain switching is responsible for a large part of the macroscopic strain and explains the high level of inter- and intra-granular stresses observed during the course of the experiment. The study shows that if apparent piezoelectric and elastic properties can be identified for PZT single crystals from blocking stress curves, they may be very different from the actual properties of polycrystalline materials due to the multiplicity of the physical mechanisms involved. These apparent properties can be used for macroscopic modelling purposes but should be considered with caution if a local analysis is aimed at.

  18. Titan Polar Landscape Evolution

    Science.gov (United States)

    Moore, Jeffrey M.

    2016-01-01

    With the ongoing Cassini-era observations and studies of Titan it is clear that the intensity and distribution of surface processes (particularly fluvial erosion by methane and Aeolian transport) has changed through time. Currently however, alternate hypotheses substantially differ among specific scenarios with respect to the effects of atmospheric evolution, seasonal changes, and endogenic processes. We have studied the evolution of Titan's polar region through a combination of analysis of imaging, elevation data, and geomorphic mapping, spatially explicit simulations of landform evolution, and quantitative comparison of the simulated landscapes with corresponding Titan morphology. We have quantitatively evaluated alternate scenarios for the landform evolution of Titan's polar terrain. The investigations have been guided by recent geomorphic mapping and topographic characterization of the polar regions that are used to frame hypotheses of process interactions, which have been evaluated using simulation modeling. Topographic information about Titan's polar region is be based on SAR-Topography and altimetry archived on PDS, SAR-based stereo radar-grammetry, radar-sounding lake depth measurements, and superposition relationships between geomorphologic map units, which we will use to create a generalized topographic map.

  19. Status of plutonium ceramic immobilization processes and immobilization forms

    Energy Technology Data Exchange (ETDEWEB)

    Ebbinghaus, B.B.; Van Konynenburg, R.A. [Lawrence Livermore National Lab., CA (United States); Vance, E.R.; Jostsons, A. [Australian Nuclear Science and Technology Organization, Menai (Australia)] [and others

    1996-05-01

    Immobilization in a ceramic followed by permanent emplacement in a repository or borehole is one of the alternatives currently being considered by the Fissile Materials Disposition Program for the ultimate disposal of excess weapons-grade plutonium. To make Pu recovery more difficult, radioactive cesium may also be incorporated into the immobilization form. Valuable data are already available for ceramics form R&D efforts to immobilize high-level and mixed wastes. Ceramics have a high capacity for actinides, cesium, and some neutron absorbers. A unique characteristic of ceramics is the existence of mineral analogues found in nature that have demonstrated actinide immobilization over geologic time periods. The ceramic form currently being considered for plutonium disposition is a synthetic rock (SYNROC) material composed primarily of zirconolite (CaZrTi{sub 2}O{sub 7}), the desired actinide host phase, with lesser amounts of hollandite (BaAl{sub 2}Ti{sub 6}O{sub 16}) and rutile (TiO{sub 2}). Alternative actinide host phases are also being considered. These include pyrochlore (Gd{sub 2}Ti{sub 2}O{sub 7}), zircon (ZrSiO{sub 4}), and monazite (CePO{sub 4}), to name a few of the most promising. R&D activities to address important technical issues are discussed. Primarily these include moderate scale hot press fabrications with plutonium, direct loading of PuO{sub 2} powder, cold press and sinter fabrication methods, and immobilization form formulation issues.

  20. Morphology versus U-Pb systematics in zircon: A high-resolution isotopic study of a zircon population from a Variscan dike in the Central Alps

    International Nuclear Information System (INIS)

    Bossart, P.J.; Meier, M.; Oberli, F.; Steiger, R.H.

    1986-01-01

    U/Pb isotopic measurements on individual zircon crystals combined with morphological analyses permit the identification of three distinct components within the zircon population of the Saedelhorn diorite, a Variscan dike from the western Gotthard (Central Alps, Switzerland): (i) 94% of the grains in the zircon population are elongate crystals with pronounced skeletal morphology indicative of rapid growth from a supercooled melt. (ii) 5% of the population consist of turbid, mostly subhedral zircons frequently showing D-type morphology and elevated uranium contents compared to the skeletal variety. Single-crystal and multi-grain U-Pb isotopic data of group (i) and (ii) zircons define an intrusion age of 293 + 5/ -4 m.y. for the dike. (iii) Rare, transparent zircon crystals (< 1% of the zircons population) yield apparent U-Pb ages in the range of 370-490 m.y. and display morphological and isotopic characteristics closely resembling those of a Caledonian orthogneiss intruded by the dike. This implies presence of assimilated wall-rock components in the macroscopically homogeneous dike sample. (orig./WB)

  1. Preparation and properties of calcium zirconate

    International Nuclear Information System (INIS)

    Dudek, M.; Bucko, M.; Rog, G.

    2001-01-01

    Dense samples of calcium zirconate were prepared. Electrical conductivity of the samples were measured in the temperature range 873 - 1273 K by both the d.c. four probe and the impedance spectroscopy methods. Calcium zirconate with small excess of calcium oxide appeared to be oxygen ion conductor. It was applied as an electrolyte in solid-state galvanic cells. (author)

  2. Dielectric behaviour of (Ba,Sr)TiO3 perovskite borosilicate glass ceramics

    International Nuclear Information System (INIS)

    Yadav, Avadhesh Kumar; Gautam, C.R.

    2013-01-01

    Various perovskite (Ba,Sr)TiO 3 borosilicate glasses were prepared by rapid melt-quench technique in the glass system ((Ba 1-x Sr x ).TiO 3 )-(2SiO 2 .B 2 O 3 )-(K 2 O)-(La 2 O 3 ). On the basis of differential thermal analysis results, glasses were converted into glass ceramic samples by regulated heat treatment schedules. The dielectric behaviour of crystallized barium strontium titanate borosilicate glass ceramic samples shows diffuse phase transition. The study depicts the dielectric behaviour of glass ceramic sample BST5K1L0.2S814. The double relaxation was observed in glass ceramic samples corresponding 80/20% Ba/Sr due to change in crystal structure from orthorhombic to tetragonal and tetragonal to cubic with variation of temperature. The highest value of dielectric constant was found to be 48289 for the glass ceramic sample BST5K1L0.2S814. The high value of dielectric constant attributed to space charge polarization between the glassy phase and perovskite phase. Due to very high value of dielectric constant, such glass ceramics are used for high energy storage devices. La 2 O 3 acts as nucleating agent for crystallization of glass to glass ceramics and enhances the dielectric constant and retarded dielectric loss. Such glass ceramics can be used in high energy storage devices such as barrier layer capacitors, multilayer capacitors etc. (author)

  3. Dielectric characterization of low-loss calcium strontium titanate fibers produced by laser floating zone technique for wireless communication

    International Nuclear Information System (INIS)

    Amaral, F.; Valente, M.A.; Costa, L.C.; Costa, F.M.

    2014-01-01

    Wireless communication technology assisted to a huge development during the last two decades, responding to the growing demand for small size and low weight devices such as cell phones and global positioning systems. The need for miniaturization and higher autonomy resulted in the development of new dielectric oxide ceramics with very specific properties, to be applied as dielectric resonators in filters, oscillators, and antennas. Some crucial properties as a high quality factor, high dielectric constant, and near zero temperature coefficient of resonant frequency must be considered during the selection of the appropriate materials. The present work deals with the preparation of calcium titanate (CaTiO 3 ), strontium titanate (SrTiO 3 ), and calcium strontium titanate (Ca x Sr 1-x TiO 3 ) fibers produced by laser floating zone (LFZ) technique. Our results show that fibers grown at lower pulling rates exhibit higher ε', for all the studied frequency range, including the microwave region. Moreover, the quality factor is always high envisaging the possibility to include these materials in future wireless device applications. (copyright 2014 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  4. Dielectric characterization of low-loss calcium strontium titanate fibers produced by laser floating zone technique for wireless communication

    Energy Technology Data Exchange (ETDEWEB)

    Amaral, F. [Department of Physics and I3N, University of Aveiro, 3810-193, Aveiro (Portugal); Polytechnic Institute of Coimbra, 3000-271, Coimbra (Portugal); Valente, M.A.; Costa, L.C.; Costa, F.M. [Department of Physics and I3N, University of Aveiro, 3810-193, Aveiro (Portugal)

    2014-09-15

    Wireless communication technology assisted to a huge development during the last two decades, responding to the growing demand for small size and low weight devices such as cell phones and global positioning systems. The need for miniaturization and higher autonomy resulted in the development of new dielectric oxide ceramics with very specific properties, to be applied as dielectric resonators in filters, oscillators, and antennas. Some crucial properties as a high quality factor, high dielectric constant, and near zero temperature coefficient of resonant frequency must be considered during the selection of the appropriate materials. The present work deals with the preparation of calcium titanate (CaTiO{sub 3}), strontium titanate (SrTiO{sub 3}), and calcium strontium titanate (Ca{sub x}Sr{sub 1-x}TiO{sub 3}) fibers produced by laser floating zone (LFZ) technique. Our results show that fibers grown at lower pulling rates exhibit higher ε', for all the studied frequency range, including the microwave region. Moreover, the quality factor is always high envisaging the possibility to include these materials in future wireless device applications. (copyright 2014 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  5. Interaction of Titan's atmosphere with Saturn's magnetosphere

    International Nuclear Information System (INIS)

    Hartle, R.E.

    1985-01-01

    The Voyager 1 measurements made during the Titan flyby reveal that Saturn's rotating magnetospheric plasma interacts directly with Titan's neutral atmosphere and ionosphere. This results from the lack of an intrinsic magnetic field at Titan. The interaction induces a magnetosphere which deflects the flowing plasma around Titan and forms a plasma wake downstream. Within the tail of the induced magnetosphere, ions of ionospheric origin flow away from Titan. Just outside Titan's magnetosphere, a substantial ion-exosphere forms from an extensive hydrogen-nitrogen exosphere. The exospheric ions are picked up and carried downstream into the wake by the plasma flowing around Titan. Mass loading produced by the addition of exospheric ions slows the wake plasma down considerably in the vicinity of the magnetopause. 36 references

  6. PLZT-based photovoltaic Piezoelectric Transformer with light feedback

    Energy Technology Data Exchange (ETDEWEB)

    Kozielski, L [University of Silesia, Dep. Materials Sc, 2, Sniezna St. Sosnowiec, 41-200 Poland (Poland); Adamczyk, M [University of Silesia, Institute Phys., 4, Uniwersytecka St. Katowice, 40-007 Poland (Poland); Erhart, J, E-mail: lucjan.kozielski@us.edu.pl [Technical University of Liberec, Studencka St. 2, CZ-461 17 Liberec (Czech Republic)

    2011-10-29

    Piezoelectric Transformer (PT) converts an electrical AC input voltage into ultrasonic vibrations and reconverts back to an output as AC voltage. Hard lead zirconate titanate (PZT) ceramics is typically used for fabrications of such devices. In case of lanthaniun ion La{sup 3+} addition in PZT solid solution we can achieve piezoelectric ceramics with good transparency exhibiting both optical Pockels and Kerr effects. Values of these coefficients in the PLZT system are much bigger than in LiNbO{sub 3} or SBN single crystals. Among the various PLZT compositions 8/65/35, near the morphotropic boundary, exhibit large electrooptic effect and thus have found applications in light shutters and displays. In the present study we have investigated radial mode piezoelectric transformer based on optically transparent PLZT8/65/35 ceramics. The effect of the UV light generated photovoltage and photostriction on the efficiency and voltage step-up ratio of piezoelectric transformer have been demonstrated. Novel functions of this device is proposed by superimposing two sophistically coupled effects of piezoelectricity and photostriction.

  7. Application Of Light Valves For Continuous-Tone Printing

    Science.gov (United States)

    Vergona, Albert B.

    1989-07-01

    New opportunities are emerging in the graphic-arts pre-press market stimulated by the need for digitally created images. To meet this need, we have designed a cost-effective three-color digital printer using PLZT light valves. Transparent lead lanthanum zirconate titanate (PLZT) ceramic crystals when used as a linear modulator offer a number of significant benefits. The primary advantage is that the light valve is an efficient modulator of incoherent light providing a broad spectral output ranging from 400nm to well into the infrared region. In addition, light valves offer the advantages of being small, low cost, have a wide dynamic range (>1000 to 1), and can be used with simple optical designs. The characteristics of the PLZT material plays an important role in the performance of the light valve. A number of variables such as ceramic composition, electrode spacing, and ceramic thickness can be altered to affect its quadratic electrooptic behavior. Additionally, the modulator design requires a closed-loop servo to eliminate the errors caused by the device's remanent polarization and nonlinear behavior.

  8. Carbon Dioxide Adsorption by Calcium Zirconate at Higher Temperature

    Directory of Open Access Journals (Sweden)

    K. B. Kale

    2012-12-01

    Full Text Available The CO2 adsorption by calcium zirconate was explored at pre- and post- combustion temperature condition. The several samples of the calcium zirconate were prepared by different methods such as sol-gel, solid-solid fusion, template and micro-emulsion. The samples of the calcium zirconate were characterized by measurement of surface area, alkalinity/acidity, and recording the XRD patterns and SEM images. The CO2 adsorptions by samples of the calcium zirconate were studied in the temperature range 100 to 850 oC and the CO2 adsorptions were observed in the ranges of 6.88 to 40.6 wt % at 600 0C and 8 to 16.82 wt% at in between the temperatures 200 to 300 oC. The effect of Ca/Zr mol ratio in the samples of the calcium zirconate on the CO2 adsorption and alkalinity were discussed. The adsorbed moisture by the samples of the calcium zirconate was found to be useful for the CO2 adsorption. The promoted the samples of the calcium zirconate by K+, Na+, Rb+, Cs+, Ag+ and La3+ showed the increased CO2 adsorption. The exposure time of CO2 on the samples of the calcium zirconate showed the increased CO2 adsorption. The samples of the calcium zirconate were found to be regenerable and reusable several times for the adsorption of CO2 for at the post- and pre-combustion temperature condition. Copyright © 2012 by BCREC Undip. All rights reservedReceived: 23rd June 2012, Revised: 28th August 2012, Accepted: 30th August 2012[How to Cite: K. B. Kale, R. Y. Raskar, V. H. Rane and A. G.  Gaikwad (2012. Carbon Dioxide Adsorption by Calcium Zirconate at Higher Temperature. Bulletin of Chemical Reaction Engineering & Catalysis, 7 (2: 124-136. doi:10.9767/bcrec.7.2.3686.124-136] [How to Link / DOI: http://dx.doi.org/10.9767/bcrec.7.2.3686.124-136 ] | View in 

  9. Evaluation of Data Retention Characteristics for Ferroelectric Random Access Memories (FRAMs)

    Science.gov (United States)

    Sharma, Ashok K.; Teverovsky, Alexander

    2001-01-01

    Data retention and fatigue characteristics of 64 Kb lead zirconate titanate (PZT)-based Ferroelectric Random Access Memories (FRAMs) microcircuits manufactured by Ramtron were examined over temperature range from -85 C to +310 C for ceramic packaged parts and from -85 C to +175 C for plastic parts, during retention periods up to several thousand hours. Intrinsic failures, which were caused by a thermal degradation of the ferroelectric cells, occurred in ceramic parts after tens or hundreds hours of aging at temperatures above 200 C. The activation energy of the retention test failures was 1.05 eV and the extrapolated mean-time-to-failure (MTTF) at room temperature was estimated to be more than 280 years. Multiple write-read cycling (up to 3x10(exp 7)) during the fatigue testing of plastic and ceramic parts did not result in any parametric or functional failures. However, operational currents linearly decreased with the logarithm of number of cycles thus indicating fatigue process in PZT films. Plastic parts, that had more recent date code as compared to ceramic parts, appeared to be using die with improved process technology and showed significantly smaller changes in operational currents and data access times.

  10. Effects of electric field on the fracture toughness (KIc) of ceramic PZT

    International Nuclear Information System (INIS)

    Goljahi, Sam; Lynch, Christopher S

    2013-01-01

    This work was motivated by the observation that a small percentage of the ceramic lead zirconate titanate (PZT) parts in a device application, one that requires an electrode pattern on the PZT surface, developed fatigue cracks at the edges of the electrodes; yet all of the parts were subjected to similar loading. To obtain additional information on the fracture behavior of this material, similar specimens were run at higher voltage in the laboratory under a microscope to observe the initiation and growth of the fatigue cracks. A sequence of experiments was next performed to determine whether there were fracture toughness variations that depended on material processing. Plates were cut from a single bar in different locations and the Vickers indentation technique was used to measure the relative fracture toughness as a function of position along the bar. Small variations in toughness were found, that may account for some of the devices developing fatigue cracks and not others. Fracture toughness was measured next as a function of electric field. The surface crack in flexure technique was modified to apply an electric field perpendicular to a crack. The results indicate that the fracture toughness drops under a positive electric field and increases under a negative electric field that is less than the coercive field, but as the negative coercive field is approached the fracture toughness drops. Examination of the fracture surfaces using an optical microscope and a surface profilometer reveal the initial indentation crack shape and (although less accurately) the crack shape and size at the transition from stable to unstable growth. These results are discussed in terms of a ferroelastic toughening mechanism that is dependent on electric field. (paper)

  11. Effects of electric field on the fracture toughness (KIc) of ceramic PZT

    Science.gov (United States)

    Goljahi, Sam; Lynch, Christopher S.

    2013-09-01

    This work was motivated by the observation that a small percentage of the ceramic lead zirconate titanate (PZT) parts in a device application, one that requires an electrode pattern on the PZT surface, developed fatigue cracks at the edges of the electrodes; yet all of the parts were subjected to similar loading. To obtain additional information on the fracture behavior of this material, similar specimens were run at higher voltage in the laboratory under a microscope to observe the initiation and growth of the fatigue cracks. A sequence of experiments was next performed to determine whether there were fracture toughness variations that depended on material processing. Plates were cut from a single bar in different locations and the Vickers indentation technique was used to measure the relative fracture toughness as a function of position along the bar. Small variations in toughness were found, that may account for some of the devices developing fatigue cracks and not others. Fracture toughness was measured next as a function of electric field. The surface crack in flexure technique was modified to apply an electric field perpendicular to a crack. The results indicate that the fracture toughness drops under a positive electric field and increases under a negative electric field that is less than the coercive field, but as the negative coercive field is approached the fracture toughness drops. Examination of the fracture surfaces using an optical microscope and a surface profilometer reveal the initial indentation crack shape and (although less accurately) the crack shape and size at the transition from stable to unstable growth. These results are discussed in terms of a ferroelastic toughening mechanism that is dependent on electric field.

  12. Enhanced piezoelectric properties and excellent thermal stabilities of cobalt-modified Aurivillius-type calcium bismuth titanate (CaBi_4Ti_4O_1_5)

    International Nuclear Information System (INIS)

    Zhao, Tian-Long; Wang, Chun-Ming; Wang, Chun-Lei; Wang, Yi-Ming; Dong, Shuxiang

    2015-01-01

    Highlights: • Cobalt oxide modified CBT-based ceramics were prepared and investigated in detail. • XRPD analysis revealed Co ions enter into B-site of CBT-based ceramics. • CBT-Co4 ceramics show the enhanced d_3_3 of 14 pC/N and T_c of 782 °C. • CBT-Co4 ceramics present the improved high-temperature resistivity. • Thermal depoling behavior indicates CBT-Co4 ceramics exhibit good thermal stability. - Abstract: Bismuth layer-structured ferroelectric (BLSF) calcium bismuth titanate (CaBi_4Ti_4O_1_5, CBT) piezoelectric ceramics with 0.0–1.0 wt.% cobalt oxide (Co_2O_3) have been prepared via a conventional solid-state reaction method. Microstructural morphology and electrical properties of cobalt oxide-modified CBT ceramics were investigated in detail. X-ray powder diffraction (XRPD) analysis revealed that the cobalt oxide-modified CBT ceramics have a pure four-layer Aurivillius-type structure. The piezoelectric properties of CBT ceramics were significantly enhanced by cobalt oxide modifications. The piezoelectric coefficient d_3_3 and Curie temperature T_c of 0.2 wt.% cobalt oxide-modified CBT ceramics (CBT-Co4) are 14 pC/N and 782 °C, respectively. The DC resistivity and thermal depoling behavior at elevated temperature indicated that the CBT-Co4 ceramics exhibit good thermal stability, demonstrating that the CBT-Co4 ceramics are potential materials for high temperature piezoelectric applications.

  13. Gold in Accessory Zircon (the Kozhim Massif, Subpolar Urals)

    Science.gov (United States)

    Denisova, Yuliya; Pystin, Aleksandr

    2017-12-01

    The crystals of zircon due to their resistance to external impact of various processes can reveal information about the environment of their formation and the inclusions observed of them. Zircon contains different mineral inclusions: biotite, plagioclase, quartz, apatite, etc. However, there is no information about gold inclusions in the zircons from granites of the Sudpolar Urals. The study results of the inclusions of gold in accessory zircon of the Kozhim granitic massif are presented in this paper. The studied mineral is a dark-brown translucent short-prismatic crystal containing the inclusion of gold and the allocations of quartz. According to studies, the inclusion of gold formed during the growth of zircon and it is the gold covered with a thin film of oxide gold. It was confirmed that the crystallization of the studied zircon occurred at a temperature of 800°C and above on the stage of formation of granites of Kozhim massif. The assumption is made about the additional temperature in the course of which was caused by decreasing of temperature up to 700° C and below during postmagmatic stage.

  14. Titanic: A Statistical Exploration.

    Science.gov (United States)

    Takis, Sandra L.

    1999-01-01

    Uses the available data about the Titanic's passengers to interest students in exploring categorical data and the chi-square distribution. Describes activities incorporated into a statistics class and gives additional resources for collecting information about the Titanic. (ASK)

  15. The age of Titan's surface

    Science.gov (United States)

    Neish, C. D.; Lorenz, R. D.

    2010-04-01

    High-resolution images of the surface of Titan taken by the Cassini spacecraft reveal a world with an extreme paucity of impact craters. Planetary surfaces are commonly dated by dividing the number of impact craters by the estimated impactor flux, but this approach has been confounded at Titan by several difficulties. First, high-resolution imaging of the surface of Titan is far from complete (in the near-infrared as well as radar). As of December 2007, Cassini RADAR images covered only 22% of its surface. However, we can use Monte-Carlo models to explore how many craters of a given size (with large or very large craters being of particular interest) may be present in the unobserved areas. Second, literature descriptions of the crater formation rate (e.g. Korycansky and Zahnle 2005 and Artemieva and Lunine 2005) are apparently not in agreement. We discuss possible resolutions. Third, since surface modification processes are ongoing, the actual number of craters on Titan's surface remains uncertain, as craters may be eroded beyond recognition, or obscured by lakes or sand seas. In this connection, we use the Earth as an analogue. The Earth is in many ways the most "Titan-like" world in the solar system, with extensive modification by erosion, burial, tectonism, and volcanism. We compare the observed number of terrestrial craters to the expected terrestrial impactor flux to determine the crater reduction factor for a world similar to Titan. From this information, we can back out the actual number of craters on Titan's surface and estimate its crater retention age. An accurate age estimate will be critical for constraining models of Titan's formation and evolution.

  16. Twinning in Zircon: Not a High-Pressure Phenomenon

    Science.gov (United States)

    Jones, G. A.; Moser, D.; Shieh, S. R.; Barker, I.

    2017-12-01

    Microtwins in zircon are commonly found in shocked terrestrial and extraterrestrial samples and are potentially important for shock history and crater reconstruction. Twinning is easily observed with both the optical microscope and variety of electron beam techniques. Twinning as a deformation mechanism is consistent with the high strain rates generated during impact. No constitutive relationships, or even general limits on the physical conditions required for twinning in zircon are known, however. Present speculation on the critical quantity for twin formation, i.e. 10s of GPa of shock pressure (Moser et al. 2011, Timms et al., 2012), has no basis in the underlying mechanisms of twin nucleation, which are related to the motion of dislocations. This erroneous value is due to conflation of twinning sensu stricto with a phase transformation to reidite. Reidite occurs as twin-like lamellae occupying the {112} planes which are thought to be a mirror plane for twinning. We review the crystallographic theory of twinning in zircon. We then evaulate several theories on the nucleation of twins along with their necessary stresses involved. Our aim is to show that shock microtwins in zircon can be a `low pressure' shock phenomenon. This 'low pressure' hypothesis is supported by natural samples. These zircons are from the lower crust nearly 80 km from the centre of the Vredefort impact structure—the most distal zircon shock microstructures yet found in the lithosphere. Twins are present in 10% of the zircon grains greater than 50 µm in diameter. As an extensive, 'low pressure' phenomenon, twins are an easily recognized and potentially widespread record of Earth's impact history.Moser, D.E., Cupelli, C. L., Barker, I., Flowers, R. M., Mowman, J. R., Wooden, J. and Hart, R. (2011) New zircon shock phenomena and their use for dating and […] analysis of the Vredefort dome, Canadian Journal of Earth Sciences 48(2), 117-139.Timms, N.E., Reddy, S. M., Healy, D., Nemchin, A. A

  17. The Titan Sky Simulator ™ - Testing Prototype Balloons in Conditions Approximating those in Titan's Atmosphere

    Science.gov (United States)

    Nott, Julian

    This paper will describe practical work flying prototype balloons in the "The Titan Sky Simulator TM " in conditions approximating those found in Titan's atmosphere. Saturn's moon, Titan, is attracting intense scientific interest. This has led to wide interest in exploring it with Aerobots, balloons or airships. Their function would be similar to the Rovers exploring Mars, but instead of moving laboriously across the rough terrain on wheels, they would float freely from location to location. To design any balloon or airship it is essential to know the temperature of the lifting gas as this influences the volume of the gas, which in turn influences the lift. To determine this temperature it is necessary to know how heat is transferred between the craft and its surroundings. Heat transfer for existing balloons is well understood. However, Titan conditions are utterly different from those in which balloons have ever been flown, so heat transfer rates cannot currently be calculated. In particular, thermal radiation accounts for most heat transfer for existing balloons but over Titan heat transfer will be dominated by convection. To be able to make these fundamental calculations, it is necessary to get fundamental experimental data. This is being obtained by flying balloons in a Simulator filled with nitrogen gas at very low temperature, about 95° K / minus 180° C, typical of Titan's temperatures. Because the gas in the Simulator is so cold, operating at atmospheric pressure the density is close to that of Titan's atmosphere. "The Titan Sky Simulator TM " has an open interior approximately 4.5 meter tall and 2.5 meters square. It has already been operated at 95° K/-180° C. By the time of the Conference it is fully expected to have data to present from actual balloons flying at this temperature. Perhaps the most important purpose of this testing is to validate numerical [computational fluid dynamics] models being developed by Tim Colonius of Caltech. These numerical

  18. Evaluation of electromechanical coupling parameters of piezoelectric materials by using piezoelectric cantilever with coplanar electrode structure in quasi-stasis.

    Science.gov (United States)

    Zheng, Xuejun; Zhu, Yuankun; Liu, Xun; Liu, Jing; Zhang, Yong; Chen, Jianguo

    2014-02-01

    Based on Timoshenko beam theory, a principle model is proposed to establish the relationship between electric charge and excitation acceleration, and in quasi-stasis we apply the direct piezoelectric effect of multilayer cantilever with coplanar electrode structure to evaluate the piezoelectric strain coefficient d15 and electromechanical coupling coefficient k15. They are measured as 678 pC/N and 0.74 for the commercial piezoelectric ceramic lead zirconate titanate (PZT-51) bulk specimen and 656 pC/N and 0.63 for the lead magnesium niobate (PMN) bulk specimen, and they are in agreement with the calibration and simulation values. The maximum of relative errors is less than 4.2%, so the proposed method is reliable and convenient.

  19. Longitudinal-bending mode micromotor using multilayer piezoelectric actuator.

    Science.gov (United States)

    Yao, K; Koc, B; Uchino, K

    2001-07-01

    Longitudinal-bending mode ultrasonic motors with a diameter of 3 mm were fabricated using stacked multilayer piezoelectric actuators, which were self-developed from hard lead zirconate titanate (PZT) ceramic. A bending vibration was converted from a longitudinal vibration with a longitudinal-bending coupler. The motors could be bidirectionally operated by changing driving frequency. Their starting and braking torque were analyzed based on the transient velocity response. With a load of moment of inertia 2.5 x 10(-7) kgm2, the motor showed a maximum starting torque of 127.5 microNm. The braking torque proved to be a constant independent on the motor's driving conditions and was roughly equivalent to the maximum starting torque achievable with our micromotors.

  20. The atmospheric temperature structure of Titan

    Science.gov (United States)

    Mckay, Christopher P.; Pollack, J. B.; Courtin, Regis; Lunine, Jonathan I.

    1992-01-01

    The contribution of various factors to the thermal structure of Titan's past and present atmosphere are discussed. A one dimensional model of Titan's thermal structure is summarized. The greenhouse effect of Titan's atmosphere, caused primarily by pressure induced opacity of N2, CH4, and H2, is discussed together with the antigreenhouse effect dominated by the haze which absorbs incident sunlight. The implications for the atmosphere of the presence of an ocean on Titan are also discussed.

  1. Lanthanide stannate pyrochlores (Ln2Sn2O7; Ln = Nd, Gd, Er) at high pressure.

    Science.gov (United States)

    Turner, Katlyn M; Tracy, Cameron L; Mao, Wendy L; Ewing, Rodney C

    2017-11-09

    Lanthanide stannate pyrochlores (Ln2Sn2O7; Ln=Nd, Gd, and Er) were investigated in situ to 50 GPa in order to determine their structural response to compression and compare it to that of lanthanide titanate, zirconate, and hafnate pyrochlores. The cation radius ratio of A3+/B4+ in pyrochlore oxides (A2B2O7) is thought to be the dominant property that influences their compression response. The ionic radius of Sn4+ is intermediate to that of Ti4+, Zr4+, and Hf4+, but the bond in stannate pyrochlore is more covalent than the bonds in titanates, zirconate, and hafnates. In stannates, the pyrochlore cation and anion sublattices begin to disorder at 0.3 GPa. The extent of sublattice disorder vs. pressure is greater in stannates with a smaller Ln3+ cation. Stannate pyrochlores (Fd-3m) begin a sluggish transformation to a cotunnite-like structure (Pnma) at ~28 GPa; similar transitions have been observed in titanate, zirconate, and hafnate pyrochlore at varying pressures with cation radius ratio. The extent of the phase transition vs. pressure varies directly with the size of the Ln3+ cation. Post-decompression from ~50 GPa, Er2Sn2O7 and Gd2Sn2O7 adopt a pyrochlore structure, rather than the multiscale defect-fluorite + weberite structure adopted by Nd2Sn2O7 that is characteristic of titanate, zirconate, and hafnate pyrochlore treated to similar conditions. Like pyrochlore titanates, zirconates, and hafnates, the bulk modulus, B0, of stannates varies linearly and inversely with cation radius ratio. The trends of bulk moduli in stannates in this study are in excellent agreement with previous experimental studies on stannates, and suggest that the size of the Ln3+ cation is a primary determining factor of B0. Additionally, when normalized to rA/rB, the bulk moduli of stannates are comparable to those of zirconates and hafnates, which vary from titanates. Our results suggest that the cation radius ratio strongly influences the bulk moduli of stannates as well as

  2. Fabrication of zircon for disposition of weapons plutonium

    International Nuclear Information System (INIS)

    Kim, K.C.; Huang, J.Y.; Serrano, P.L.

    1997-01-01

    This is the final report of a one-year, Laboratory-Directed Research and Development (LDRD) project at the Los Alamos National Laboratory (LANL). In an effort to address the problems of long term storage and nuclear waste minimization, zircon has been proposed as a host medium for plutonium and other actinides recovered from dismantled nuclear weapons. The objective of this work is to investigate the feasibility of large scale fabrication of Pu-bearing zircon. Since PuO 2 is thermodynamically less stable than ZrO 2 , it is expected that the process parameters determined for synthesizing ZrSiO 4 (zircon) would be applicable to those for PuSiO 4 (Pu-zircon). Furthermore, since the foremost concern in plutonium processing is the potential for contamination release, this work emphasizes the development of process parameters, using zircon first, to anticipate potential material problems in the containment system for reaction mixtures during processing. Stoichiometric mixtures of ZrO 2 and SiO 2 , in hundred-gram batches, have been subjected to hot isostatic pressing (HIP) at temperatures near 1,500 C and pressures approximately 10,000 psi. The product materials have been analyzed by x-ray powder diffraction, and are found to consist of zircon after approximately two hours of reaction time. From this work, it is clear that the fabrication of large quantities of Pu-zircon is feasible. The most notable result of this work is evidence for the existence of container problems. This result, in turn, suggests potential solutions to these problems. Experiments with the quartz inner container, the glass sealant, a sacrificial metal barrier, and a metal outer container are being investigated to mitigate these potential hazards

  3. Stress engineering for the design of morphotropic phase boundary in piezoelectric material

    Energy Technology Data Exchange (ETDEWEB)

    Ohno, Tomoya, E-mail: ohno@mail.kitami-it.ac.jp [Department of Materials Science, Kitami Institute of Technology, 165 Kouen-cho, Kitami 090-8507 (Japan); Yanagida, Hiroshi; Maekawa, Kentaroh [Department of Materials Science, Kitami Institute of Technology, 165 Kouen-cho, Kitami 090-8507 (Japan); Arai, Takashi; Sakamoto, Naonori; Wakiya, Naoki; Suzuki, Hisao [Graduate School of Science and Technology, Shizuoka University, 3-5-1 Johoku, Hamamatsu, Shizuoka 432-8561 (Japan); Satoh, Shigeo [Graduate School of Science and Engineering, Ibaragi University, 4-12-1 Nakanarusawa-cho, Hitachi, Ibaragi 316-0033 (Japan); Matsuda, Takeshi [Department of Materials Science, Kitami Institute of Technology, 165 Kouen-cho, Kitami 090-8507 (Japan)

    2015-06-30

    Alkoxide-derived lead zirconate titanate thin films having Zr/Ti = 50/50 to 60/40 compositions with different residual stress conditions were deposited on a Si wafer to clarify the effects of the residual stress on the morphotropic phase boundary shift. The residual stress condition was controlled to − 0.1 to − 0.9 GPa by the design of the buffer layer structure on the Si wafer. Results show that the maximum effective piezoelectric constant d{sub 33} was obtained at 58/42 composition under − 0.9 GPa compressive residual stress condition. Moreover, the MPB composition shifted linearly to Zr-rich phase with increasing compressive residual stress. - Highlights: • The residual stress in lead zirconate titanate film on silicon was controlled. • The maximum residual stress in lead zirconate titanate film was − 0.9 GPa. • The morphotropic phase boundary shifted to zirconium rich phase by the strain.

  4. Silica-calcium zirconate nanocomposite, studying its thermal

    Indian Academy of Sciences (India)

    Silica–calcium zirconate nanocomposite was prepared in a two-step procedure. First, nanocalcium zirconate was synthesized by the modified sol–gel method; then, silica was added to the prepared sol and the resulting product was calcined at 700–1000° C. Dilatometric measurements were performed to determine the ...

  5. Enhancement of isotope exchange reactions over ceramic breeder material by deposition of catalyst metal

    International Nuclear Information System (INIS)

    Narisato, Y.; Munakata, K.; Koga, A.; Yokoyama, Y.; Takata, T.; Okabe, H.

    2004-01-01

    The deposition of catalyst metals in ceramic breeders could enhance the release rate of tritium due to the promotion of isotope exchange reactions taking place at the interface of the breeder surface and the sweep gas. In this work, the authors examined the effects of catalytic active metal deposited on lithium titanate on the isotope exchange reactions. With respect to the virgin lithium titanate, it was found that the rate of the isotope exchange reactions taking place on the surface is quite low. However, the deposition of palladium greatly increased the exchange reaction rate. The effect of the amounts of deposited palladium on the isotope exchange reaction rate was also investigated. The results indicate that the exchange reactions are still enhanced even if the amounts of deposited palladium are as low as 0.04%

  6. Mid-1970's imbalance in zircon supply and demand

    International Nuclear Information System (INIS)

    Van Gordon, D.V.; Collins, R.E.

    1975-01-01

    Mining and the historical development of the zircon market are briefly reviewed. Causes of the fluctuations in the zircon demand and supply and in the price are discussed. Possible adjustments (such as substitution of other materials in the steel foundry) are listed. Future uses of zircon will probably be limited to those which can justify high prices and those for which there are no substitutes. (DLC)

  7. Correlation between nanostructural and electrical properties of barium titanate-based glass-ceramic nano-composites

    Energy Technology Data Exchange (ETDEWEB)

    Al-Assiri, M.S., E-mail: msassiri@kku.edu.sa [Department of Physics, King Khaled University, P.O. Box 9003, Abha (Saudi Arabia); El-Desoky, M.M., E-mail: mmdesoky@gmail.com [Department of Physics, King Khaled University, P.O. Box 9003, Abha (Saudi Arabia); Department of Physics, Faculty of Science, Suez Canal University, Suez (Egypt)

    2011-09-08

    Highlights: > Glasses have been transformed into nanomaterials by annealing at crystallization temperature. > Glass-ceramic nano-composites are important because of their new physical. > Grain sizes are the most significant structural parameter in electronic nanocrystalline phases. > These phases are very high electrical conductivity. > Hence, glass-ceramic nanocrystals are expected to be used, as gas sensors. - Abstract: Glasses in the system BaTiO{sub 3}-V{sub 2}O{sub 5}-Bi{sub 2}O{sub 3} have been transformed into glass-ceramic nano-composites by annealing at crystallization temperature T{sub cr} determined from DSC thermograms. After annealing they consist of small crystallites embedded in glassy matrix. The crystallization temperature T{sub cr} increases with increasing BaTiO{sub 3} content. XRD and TEM of the glass-ceramic nano-composites show that nanocrystals were embedded in the glassy matrix with an average grain size of 25 nm. The resulting materials exhibit much higher electrical conductivity than the initial glasses. It was postulated that the major role in the conductivity enhancement of these nanomaterials is played by the developed interfacial regions between crystalline and amorphous phases, in which the concentration of V{sup 4+}-V{sup 5+} pairs responsible for electron hopping, has higher than values that inside the glassy matrix. The experimental results were discussed in terms of a model proposed in this work and based on a 'core-shell' concept. From the best fits, reasonable values of various small polaron hopping (SPH) parameters were obtained. The conduction was attributed to non-adiabatic hopping of small polaron.

  8. Titan Orbiter Aerorover Mission

    Science.gov (United States)

    Sittler Jr., E. C.; Acuna, M.; Burchell, M. J.; Coates, A.; Farrell, W.; Flasar, M.; Goldstein, B. E.; Gorevan, S.; Hartle, R. E.; Johnson, W. T. K.

    2001-01-01

    We propose a combined Titan orbiter and Titan Aerorover mission with an emphasis on both in situ and remote sensing measurements of Titan's surface, atmosphere, ionosphere, and magnetospheric interaction. The biological aspect of the Titan environment will be emphasized by the mission (i.e., search for organic materials which may include simple organics to 'amono' analogues of amino acids and possibly more complex, lightening detection and infrared, ultraviolet, and charged particle interactions with Titan's surface and atmosphere). An international mission is assumed to control costs. NASA will provide the orbiter, launch vehicle, DSN coverage and operations, while international partners will provide the Aerorover and up to 30% of the cost for the scientific instruments through collaborative efforts. To further reduce costs we propose a single PI for orbiter science instruments and a single PI for Aerorover science instruments. This approach will provide single command/data and power interface between spacecraft and orbiter instruments that will have redundant central DPU and power converter for their instruments. A similar approach could be used for the Aerorover. The mission profile will be constructed to minimize conflicts between Aerorover science, orbiter radar science, orbiter radio science, orbiter imaging science, and orbiter fields and particles (FP) science. Additional information is contained in the original extended abstract.

  9. Response of zircon to melting and metamorphism in deep arc crust, Fiordland (New Zealand): implications for zircon inheritance in cordilleran granites

    Science.gov (United States)

    Bhattacharya, Shrema; Kemp, A. I. S.; Collins, W. J.

    2018-04-01

    The Cretaceous Mount Daniel Complex (MDC) in northern Fiordland, New Zealand was emplaced as a 50 m-thick dyke and sheet complex into an active shear zone at the base of a Cordilleran magmatic arc. It was emplaced below the 20-25 km-thick, 125.3 ± 1.3 Ma old Western Fiordland Orthogneiss (WFO) and is characterized by metre-scale sheets of sodic, low and high Sr/Y diorites and granites. 119.3 ± 1.2 Ma old, pre-MDC lattice dykes and 117.4 ± 3.1 Ma late-MDC lattice dykes constrain the age of the MDC itself. Most dykes were isoclinally folded as they intruded, but crystallised within this deep-crustal, magma-transfer zone as the terrain cooled and was buried from 25 to 50 km (9-14 kbar), based on published P-T estimated from the surrounding country rocks. Zircon grains formed under these magmatic/granulite facies metamorphic conditions were initially characterized by conservatively assigning zircons with oscillatory zoning as igneous and featureless rims as metamorphic, representing 54% of the analysed grains. Further petrological assignment involved additional parameters such as age, morphology, Th/U ratios, REE patterns and Ti-in-zircon temperature estimates. Using this integrative approach, assignment of analysed grains to metamorphic or igneous groupings improved to 98%. A striking feature of the MDC is that only 2% of all igneous zircon grains reflect emplacement, so that the zircon cargo was almost entirely inherited, even in dioritic magmas. Metamorphic zircons of MDC show a cooler temperature range of 740-640 °C, reflects the moderate ambient temperature of the lower crust during MDC emplacement. The MDC also provides a cautionary tale: in the absence of robust field and microstructural relations, the igneous-zoned zircon population at 122.1 ± 1.3 Ma, derived mostly from inherited zircons of the WFO, would be meaningless in terms of actual magmatic emplacement age of MDC, where the latter is further obscured by younger (ca. 114 Ma) metamorphic overgrowths

  10. Titan AVIATR - Aerial Vehicle for In Situ and Airborne Titan Reconnaissance

    Science.gov (United States)

    Kattenhorn, Simon A.; Barnes, J. W.; McKay, C. P.; Lemke, L.; Beyer, R. A.; Radebaugh, J.; Adamkovics, M.; Atkinson, D. H.; Burr, D. M.; Colaprete, T.; Foch, R.; Le Mouélic, S.; Merrison, J.; Mitchell, J.; Rodriguez, S.; Schaller, E.

    2010-10-01

    Titan AVIATR - Aerial Vehicle for In Situ and Airborne Titan Reconnaissance - is a small (120 kg), nuclear-powered Titan airplane in the Discovery/New Frontiers class based on the concept of Lemke (2008 IPPW). The scientific goals of the mission are designed around the unique flexibility offered by an airborne platform: to explore Titan's diversity of surface landforms, processes, and compositions, as well as to study and measure the atmospheric circulation, aerosols, and humidity. AVIATR would address and surpass many of the science goals of hot-air balloons in Titan flagship studies. The strawman instrument payload is narrowly focused on the stated scientific objectives. The optical remote sensing suite comprises three instruments - an off-nadir high-resolution 2-micron camera, a horizon-looking 5-micron imager, and a 1-6 micron pushbroom near-infrared spectrometer. The in situ instruments include atmospheric structure, a methane humidity sensor, and a raindrop detector. An airplane has operational advantages over a balloon. Its piloted nature allows a go-to capability to image locations of interest in real time, thereby allowing for directed exploration of many features of primary geologic interest: Titan's sand dunes, mountains, craters, channels, and lakes. Subsequent imaging can capture changes in these features during the primary mission. AVIATR can fly predesigned routes, building up large context mosaics of areas of interest before swooping down to low altitude to acquire high-resolution images at 30-cm spatial sampling, similar to that of HiRISE at Mars. The elevation flexibility of the airplane allows us to acquire atmospheric profiles as a function of altitude at any desired location. Although limited by the direct-to-Earth downlink bandwidth, the total scientific data return from AVIATR will be >40 times that returned from Huygens. To maximize the science per bit, novel data storage and downlink techniques will be employed, including lossy compression

  11. Titan's greenhouse and antigreenhouse effects

    Science.gov (United States)

    Mckay, Christopher P.; Pollack, James B.; Courtin, Regis

    1992-01-01

    Thermal mechanisms active in Titan's atmosphere are discussed in a brief review of data obtained during the Voyager I flyby in 1980. Particular attention is given to the greenhouse effect (GHE) produced by atmospheric H2, N2, and CH4; this GHE is stronger than that on earth, with CH4 and H2 playing roles similar to those of H2O and CO2 on earth. Also active on Titan is an antigreenhouse effect, in which dark-brown and orange organic aerosols block incoming solar light while allowing IR radiation from the Titan surface to escape. The combination of GHE and anti-GHE leads to a surface temperature about 12 C higher than it would be if Titan had no atmosphere.

  12. Enhanced piezoelectric properties and excellent thermal stabilities of cobalt-modified Aurivillius-type calcium bismuth titanate (CaBi{sub 4}Ti{sub 4}O{sub 15})

    Energy Technology Data Exchange (ETDEWEB)

    Zhao, Tian-Long [School of Physics, State Key Laboratory of Crystal Materials, Shandong University, Jinan 250100 (China); Wang, Chun-Ming, E-mail: wangcm@sdu.edu.cn [School of Physics, State Key Laboratory of Crystal Materials, Shandong University, Jinan 250100 (China); Wang, Chun-Lei; Wang, Yi-Ming [School of Physics, State Key Laboratory of Crystal Materials, Shandong University, Jinan 250100 (China); Dong, Shuxiang [Department of Materials Science and Engineering, College of Engineering, Peking University, Beijing 100871 (China)

    2015-11-15

    Highlights: • Cobalt oxide modified CBT-based ceramics were prepared and investigated in detail. • XRPD analysis revealed Co ions enter into B-site of CBT-based ceramics. • CBT-Co4 ceramics show the enhanced d{sub 33} of 14 pC/N and T{sub c} of 782 °C. • CBT-Co4 ceramics present the improved high-temperature resistivity. • Thermal depoling behavior indicates CBT-Co4 ceramics exhibit good thermal stability. - Abstract: Bismuth layer-structured ferroelectric (BLSF) calcium bismuth titanate (CaBi{sub 4}Ti{sub 4}O{sub 15}, CBT) piezoelectric ceramics with 0.0–1.0 wt.% cobalt oxide (Co{sub 2}O{sub 3}) have been prepared via a conventional solid-state reaction method. Microstructural morphology and electrical properties of cobalt oxide-modified CBT ceramics were investigated in detail. X-ray powder diffraction (XRPD) analysis revealed that the cobalt oxide-modified CBT ceramics have a pure four-layer Aurivillius-type structure. The piezoelectric properties of CBT ceramics were significantly enhanced by cobalt oxide modifications. The piezoelectric coefficient d{sub 33} and Curie temperature T{sub c} of 0.2 wt.% cobalt oxide-modified CBT ceramics (CBT-Co4) are 14 pC/N and 782 °C, respectively. The DC resistivity and thermal depoling behavior at elevated temperature indicated that the CBT-Co4 ceramics exhibit good thermal stability, demonstrating that the CBT-Co4 ceramics are potential materials for high temperature piezoelectric applications.

  13. Field-induced strain memory with non-180 .deg. domain-reorientation control

    International Nuclear Information System (INIS)

    Kadota, Yoichi; Hosaka, Hiroshi; Morita, Takeshi

    2010-01-01

    Using non-180 .deg. domain-reorientation control, we propose the strain memory effect in ferroelectric ceramics. Electric fields with asymmetric amplitudes were applied to soft-type lead zirconate titanate (PZT) ceramics, and the strain hysteresis and the polarization loop were measured. The butterfly curve became asymmetric under an electric field with a particular asymmetric amplitude. The asymmetric butterfly curve had two stable strain states at zero electric field. Thus, the strain memory effect was realized as the difference between the two stable strain states. An XRD analysis was carried out to verify the contribution of the non-180 .deg. domain reorientation to the strain memory effect. The non-180 .deg. domain reorientation was determined as the intensity ratio of the (002) to the (200) peak. The strain memory determined from macroscopic strain measurements had a linear relationship to the non-180 .deg. domain volume fraction. This result indicated the origin of the strain memory to be the non-180 .deg. domain reorientation.

  14. The effects of dopants on the electrical resistivity in lead magnesium niobate multilayer ceramic capacitors

    International Nuclear Information System (INIS)

    Chang, D.D.; Ling, H.C.

    1989-01-01

    Electrical resistivity studies were performed on multilayer ceramic capacitors (MLC) based on lead magnesium niobate and containing dopants of lead titanate, lead zinc niobate, and lead cobalt niobate. The results showed that lead titanate and/or lead zinc niobate had no effect on the electrical resistivity while lead cobalt niobate decreased the resistivity. In samples without lead cobalt niobate, we observed a conduction mechanism with an activation energy of --1 eV, which is commonly observed in barium titanate based dielectrics. This is attributed to ionic conduction via the motion of oxygen vacancies. The increase in conductivity (or decrease in resistivity) resulting from the addition of lead cobalt niobate was rationalized as due to electronic conduction through charge hopping among the cations. This conduction mechanism was characterized by an activation energy of --0.5 eV. Since the activation energy associated with the long-term failure was previously determined by a matrix of temperature and voltage accelerated life tests to be -- 1 eV, they conclude that conduction through charge hopping is not affecting the long-term reliability of these devices

  15. Influence of some additions on zircon synthesis and its properties

    International Nuclear Information System (INIS)

    Goryacheva, Z.E.; Poplevina, O.G.; Suvorov, S.A.; Toropov, A.N.

    1978-01-01

    Kinetics of zircon synthesis from pure ZrO 2 and SiO 2 is studied in the presence of additions of magnesium, calcium and rare earth oxides. The addition introduction accelerates zircon formation, its yield reaching 97% at 1600 deg C. Constants of zircon formation reaction rate are determined in the presence of additions of various oxides. It is shown that synthetic zircon surpasses the natural one in tensile and density properties at similar thermostability. It is stable to the effect of molten alkaline borosilicate glass and does not polute it

  16. Titan Orbiter with Aerorover Mission (TOAM)

    Science.gov (United States)

    Sittler, Edward C.; Cooper, J. F.; Mahaffey, P.; Esper, J.; Fairbrother, D.; Farley, R.; Pitman, J.; Kojiro, D. R.; TOAM Team

    2006-12-01

    We propose to develop a new mission to Titan called Titan Orbiter with Aerorover Mission (TOAM). This mission is motivated by the recent discoveries of Titan, its atmosphere and its surface by the Huygens Probe, and a combination of in situ, remote sensing and radar mapping measurements of Titan by the Cassini orbiter. Titan is a body for which Astrobiology (i.e., prebiotic chemistry) will be the primary science goal of any future missions to it. TOAM is planned to use an orbiter and balloon technology (i.e., aerorover). Aerobraking will be used to put payload into orbit around Titan. The Aerorover will probably use a hot air balloon concept using the waste heat from the MMRTG 500 watts. Orbiter support for the Aerorover is unique to our approach for Titan. Our strategy to use an orbiter is contrary to some studies using just a single probe with balloon. Autonomous operation and navigation of the Aerorover around Titan will be required, which will include descent near to the surface to collect surface samples for analysis (i.e., touch and go technique). The orbiter can provide both relay station and GPS roles for the Aerorover. The Aerorover will have all the instruments needed to sample Titan’s atmosphere, surface, possible methane lakes-rivers, use multi-spectral imagers for surface reconnaissance; to take close up surface images; take core samples and deploy seismometers during landing phase. Both active and passive broadband remote sensing techniques will be used for surface topography, winds and composition measurements.

  17. Dating of zircons by the fission track method

    International Nuclear Information System (INIS)

    Tenorio Hernandez, L.M.

    1992-01-01

    This work describes the methodology to date zircons by the Fission Track Method. A brief discussion is made of the physical principles of the method, physical properties of zircons and the geochemical properties of uranium. When starting with a hand sample, a mineral separation is required; to do this the following steps are needed: crushing and sieving of the sample, washing and drying, magnetic separation, heavy liquid separation (Bromoform 2.89 g/cm 3 , Diyodomethane = 3.31 g/cm 3 ), and manual separation on a stereoscopic microscope. Once the zircon concentrate is obtained, these are mounted on a FEP teflon mount, then polished and etched on an eutectic mix of 10 g. of KOH + 7.2 g. of NaOH, heated to 210 Centigrade degrees. Afterwards the mounts are prepared for irradiation, sterilizing and putting on top of them an external detector (a thin sheet of muscovite poor in uranium content). The package is then wrapped in plastic and sent to the reactor together with standard zircons of known age (Fish Canyon Tuff: Naeser et.al., 1981), mounted in the same way, plus standard glasses of known uranium content. The package was irradiated in a site known as SIRCA (Rotatory Capsules Irradiation System). Then the package is left to decay for several days, and then the external detectors are etched in a 48% concentrated hydrofluoric acid for 5 minutes. Once the samples are processed through the mentioned steps, spontaneous tracks appear in the zircons and induced tracks appear in the external detectors. On counting the tracks one obtains ρ s (spontaneous track density) and ρ 1 (induced track density). These two parameters together with another one called '#zeta #' (obtained from the standard zircons and glasses), are used to obtain the age of the sample. Zircons from Cerro de Mercado, Durango were dated and the age obtained was 30 ±5 Ma. This date is in agreement with similar results obtained by Fleisher and Naeser (1975) for zircons of the same locality and dated by the

  18. Detrital Zircons Split Sibumasu in East Gondwana

    Science.gov (United States)

    Zhang, X.; Chung, S. L.

    2017-12-01

    It is widely accepted that Sibumasu developed as a united terrane and originated from NW Australian margin in East Gondwana. Here we report new detrital zircon U-Pb-Hf isotopic data from Sumatra that, in combination with literature data, challenge and refute the above long-held view. In particular, the East and West Sumatra terranes share nearly identical Precambrian to Paleozoic detrital zircon age distributions and Hf isotopes, indicating a common provenance/origin for them. The Sumatra detrital zircons exhibit a prominent population of ca. 1170-1070 Ma, indistinguishable from those of the Lhasa and West Burma terranes, with detritus most probably sourcing from western Australia. By contrast, Sibuma (Sibumasu excluding Sumatra) detrital zircons display a prevailing population of ca. 980-935 Ma, strongly resembling those of the western Qiangtang terrane, with detrital materials most likely derived from Greater India and Himalayas. Such markedly distinct detrital zircon age profiles between Sumatra and Sibuma require disparate sources/origin for them, provoking disintegration of the widely-adopted, but outdated, term Sibumasu and thus inviting a new configuration of East Gondwana in the early Paleozoic, with Sumatra and West Burma lying outboard the Lhasa terrane in the NW Australian margin and Sibuma situated in the northern Greater Indian margin. More future investigations are needed to establish the precise rifting and drifting histories of Sumatra and Sibuma, as two separated terranes, during the breakup of Gondwana.

  19. Titan's Ammonia Feature

    Science.gov (United States)

    Smythe, W.; Nelson, R.; Boryta, M.; Choukroun, M.

    2011-01-01

    NH3 has long been considered an important component in the formation and evolution of the outer planet satellites. NH3 is particularly important for Titan, since it may serve as the reservoir for atmospheric nitrogen. A brightening seen on Titan starting in 2004 may arise from a transient low-lying fog or surface coating of ammonia. The spectral shape suggests the ammonia is anhydrous, a molecule that hydrates quickly in the presence of water.

  20. The Investigation of E-beam Deposited Titanium Dioxide and Calcium Titanate Thin Films

    Directory of Open Access Journals (Sweden)

    Kristina BOČKUTĖ

    2013-09-01

    Full Text Available Thin titanium dioxide and calcium titanate films were deposited using electron beam evaporation technique. The substrate temperature during the deposition was changed from room temperature to 600 °C to test its influence on TiO2 film formation and optical properties. The properties of CaTiO3 were investigated also. For the evaluation of the structural properties the formed thin ceramic films were studied by X-ray diffraction (XRD, energy dispersive spectrometry (EDS, scanning electron microscopy (SEM and atomic force microscopy (AFM. Optical properties of thin TiO2 ceramics were investigated using optical spectroscope and the experimental data were collected in the ultraviolet-visible and near-infrared ranges with a step width of 1 nm. Electrical properties were investigated by impedance spectroscopy.It was found that substrate temperature has influence on the formed thin films density. The density increased when the substrate temperature increased. Substrate temperature had influence on the crystallographic, structural and optical properties also. DOI: http://dx.doi.org/10.5755/j01.ms.19.3.1805

  1. Direct Chlorination of Zircon Sand

    International Nuclear Information System (INIS)

    Dwiretnani Sudjoko; Budi Sulistyo; Pristi Hartati; Sunardjo

    2002-01-01

    It was investigated the direct chlorination of zircon sand in a unit chlorination equipment. The process was in semi batch. The product gas was scrubbed in aqueous NaOH. It was search the influence of time, ratio of reactant and size of particle sand to the concentration of Zr and Si in the product. From these research it was found that as the times, ratio of reactant increased, the concentration of Zr increased, but the concentration of Si decreased, while as grain size of zircon sand decreased the concentration of Zr decreased, but the concentration of Si increased. (author)

  2. INFLUENCE OF REOXIDATION ON SILICA-CONTAINING BARIUM TITANATE CERAMICS FOR PTCR THERMISTORS PREPARED BY TAPE CASTING

    Directory of Open Access Journals (Sweden)

    Jianqiao Liu

    2016-03-01

    Full Text Available Silica-containing barium-rich BaTiO₃ ceramics for thermistors with a positive temperature coefficient of resistance are prepared by a tape-casting technique. The ceramics are sintered in a reducing atmosphere at low temperatures of 1175-1225°C. The influences of reoxidation are investigated after the reduced ceramics are reoxidized in air at 700-900°C. An anomalous correlation is illustrated between room temperature resistivity and reoxidation temperature. The anomaly results from the ferroelectricity rebuilding mechanism, which includes the spontaneous polarization theory and the ferroelectricity degradation caused by oxygen vacancies. The acceptor-state densities are estimated from the temperature-dependent resistivity. A critical temperature of 750-800°C is concluded for the grain boundary reoxidation.

  3. Dielectric Properties of Sol-Gel Derived Barium Strontium Titanate and Microwave Sintering of Ceramics

    Science.gov (United States)

    Selmi, Fathi A.

    This thesis consists of two areas of research: (1) sol-gel processing of Ba_{rm 1-x}Sr_{rm x} TiO_3 ceramics and their dielectric properties measurement; and (2) microwave versus conventional sintering of ceramics such as Al_2 O_3, Ba_{ rm 1-x}Sr_{rm x}TiO_3, Sb-doped SnO _2 and YBa_2Cu _3O_7. Sol-gel powders of BaTiO_3, SrTiO_3, and their solid solutions were synthesized by the hydrolysis of titanium isopropoxide and Ba and Sr methoxyethoxides. The loss tangent and dielectric constant of both sol-gel and conventionally prepared and sintered Ba_{rm 1-x}Sr _{rm x}TiO _3 ceramics were investigated at high frequencies. The sol-gel prepared ceramics showed higher dielectric constant and lower loss compared to those prepared conventionally. Ba _{rm 1-x}Sr _{rm x}TiO_3 ceramics were tunable with applied bias, indicating the potential use of this material for phase shifter applications. Porous Ba_{0.65}Sr _{0.35}TiO_3 was also investigated to lower the dielectric constant. Microwave sintering of alpha -Al_2O_3 and SrTiO_3 was investigated using an ordinary kitchen microwave oven (2.45 GHz; 600 Watts). The use of microwaves with good insulation of alpha -Al_2O_3 and SrTiO_3 samples resulted in their rapid sintering with good final densities of 96 and 98% of the theoretical density, respectively. A comparison of grain size for conventionally and microwave sintered SrTiO_3 samples did not show a noticeable difference. However, the grain size of microwave sintered alpha-Al_2O _3 was found to be larger than that of conventionally sintered sample. These results show that rapid sintering of ceramics can be achieved by using microwave radiation. The sintering behavior of coprecipitated Sb-doped SnO_2 was investigated using microwave power absorption. With microwave power, samples were sintered at 1450^circC for 20 minutes and showed a density as high as 99.9% of theoretical. However, samples fired in a conventional electric furnace at the same temperature for 4 hours showed only

  4. Organic chemistry on Titan: Surface interactions

    Science.gov (United States)

    Thompson, W. Reid; Sagan, Carl

    1992-01-01

    The interaction of Titan's organic sediments with the surface (solubility in nonpolar fluids) is discussed. How Titan's sediments can be exposed to an aqueous medium for short, but perhaps significant, periods of time is also discussed. Interactions with hydrocarbons and with volcanic magmas are considered. The alteration of Titan's organic sediments over geologic time by the impacts of meteorites and comets is discussed.

  5. AVIATR - Aerial Vehicle for In-situ and Airborne Titan Reconnaissance A Titan Airplane Mission Concept

    Science.gov (United States)

    Barnes, Jason W.; Lemke, Lawrence; Foch, Rick; McKay, Christopher P.; Beyer, Ross A.; Radebaugh, Jani; Atkinson, David H.; Lorenz, Ralph D.; LeMouelic, Stephane; Rodriguez, Sebastien; hide

    2011-01-01

    We describe a mission concept for a stand-alone Titan airplane mission: Aerial Vehicle for In-situ and Airborne Titan Reconnaissance (AVIATR). With independent delivery and direct-to-Earth communications, AVIATR could contribute to Titan science either alone or as part of a sustained Titan Exploration Program. As a focused mission, AVIATR as we have envisioned it would concentrate on the science that an airplane can do best: exploration of Titan's global diversity. We focus on surface geology/hydrology and lower-atmospheric structure and dynamics. With a carefully chosen set of seven instruments-2 near-IR cameras, 1 near-IR spectrometer, a RADAR altimeter, an atmospheric structure suite, a haze sensor, and a raindrop detector-AVIATR could accomplish a significant subset of the scientific objectives of the aerial element of flagship studies. The AVIATR spacecraft stack is composed of a Space Vehicle (SV) for cruise, an Entry Vehicle (EV) for entry and descent, and the Air Vehicle (AV) to fly in Titan's atmosphere. Using an Earth-Jupiter gravity assist trajectory delivers the spacecraft to Titan in 7.5 years, after which the AVIATR AV would operate for a 1-Earth-year nominal mission. We propose a novel 'gravity battery' climb-then-glide strategy to store energy for optimal use during telecommunications sessions. We would optimize our science by using the flexibility of the airplane platform, generating context data and stereo pairs by flying and banking the AV instead of using gimbaled cameras. AVIATR would climb up to 14 km altitude and descend down to 3.5 km altitude once per Earth day, allowing for repeated atmospheric structure and wind measurements all over the globe. An initial Team-X run at JPL priced the AVIATR mission at FY10 $715M based on the rules stipulated in the recent Discovery announcement of opportunity. Hence we find that a standalone Titan airplane mission can achieve important science building on Cassini's discoveries and can likely do so within

  6. TSSM: The in situ exploration of Titan

    Science.gov (United States)

    Coustenis, A.; Lunine, J. I.; Lebreton, J. P.; Matson, D.; Reh, K.; Beauchamp, P.; Erd, C.

    2008-09-01

    The Titan Saturn System Mission (TSSM) mission was born when NASA and ESA decided to collaborate on two missions independently selected by each agency: the Titan and Enceladus mission (TandEM), and Titan Explorer, a 2007 Flagship study. TandEM, the Titan and Enceladus mission, was proposed as an L-class (large) mission in response to ESA's Cosmic Vision 2015-2025 Call. The mission concept is to perform remote and in situ investigations of Titan primarily, but also of Enceladus and Saturn's magentosphere. The two satellites are tied together by location and properties, whose remarkable natures have been partly revealed by the ongoing Cassini-Huygens mission. These bodies still hold mysteries requiring a complete exploration using a variety of vehicles and instruments. TSSM will study Titan as a system, including its upper atmosphere, the interactions with the magnetosphere, the neutral atmosphere, surface, interior, origin and evolution, as well as the astrobiological potential of Titan. It is an ambitious mission because its targets are two of the most exciting and challenging bodies in the Solar System. It is designed to build on but exceed the scientific and technological accomplishments of the Cassini- Huygens mission, exploring Titan and Enceladus in ways that are not currently possible (full close-up and in situ coverage over long periods of time for Titan, several close flybys of Enceladus). One overarching goal of the TSSM mission is to explore in situ the atmosphere and surface of Titan. In the current mission architecture, TSSM consists of an orbiter (under NASA's responsibility) with a large host of instruments which would perform several Enceladus and Titan flybys before stabilizing in an orbit around Titan alone, therein delivering in situ elements (a Montgolfière, or hot air balloon, and a probe/lander). The latter are being studied by ESA. The balloon will circumnavigate Titan above the equator at an altitude of about 10 km for several months. The

  7. Diurnal variations of Titan

    Science.gov (United States)

    Cui, J.; Galand, M.; Yelle, R. V.; Vuitton, V.; Wahlund, J.-E.; Lavvas, P. P.; Mueller-Wodarg, I. C. F.; Kasprzak, W. T.; Waite, J. H.

    2009-04-01

    We present our analysis of the diurnal variations of Titan's ionosphere (between 1,000 and 1,400 km) based on a sample of Ion Neutral Mass Spectrometer (INMS) measurements in the Open Source Ion (OSI) mode obtained from 8 close encounters of the Cassini spacecraft with Titan. Though there is an overall ion depletion well beyond the terminator, the ion content on Titan's nightside is still appreciable, with a density plateau of ~700 cm-3 below ~1,300 km. Such a plateau is associated with the combination of distinct diurnal variations of light and heavy ions. Light ions (e.g. CH5+, HCNH+, C2H5+) show strong diurnal variation, with clear bite-outs in their nightside distributions. In contrast, heavy ions (e.g. c-C3H3+, C2H3CNH+, C6H7+) present modest diurnal variation, with significant densities observed on the nightside. We propose that the distinctions between light and heavy ions are associated with their different chemical loss pathways, with the former primarily through "fast" ion-neutral chemistry and the latter through "slow" electron dissociative recombination. The INMS data suggest day-to-night transport as an important source of ions on Titan's nightside, to be distinguished from the conventional scenario of auroral ionization by magnetospheric particles as the only ionizing source on the nightside. This is supported by the strong correlation between the observed night-to-day ion density ratios and the associated ion lifetimes. We construct a time-dependent ion chemistry model to investigate the effects of day-to-night transport on the ionospheric structures of Titan. The predicted diurnal variation has similar general characteristics to those observed, with some apparent discrepancies which could be reconciled by imposing fast horizontal thermal winds in Titan's upper atmosphere.

  8. Effect of processing routes on microstructure, electrical and dielectric behavior of Mg-doped CaCu3Ti4O12 electro-ceramic

    Science.gov (United States)

    Singh, Laxman; Rai, U. S.; Mandal, K. D.; Rai, Alok Kumar

    2013-09-01

    In the present communication, data on magnesium-doped calcium copper titanate CaCu2.90Mg0.10Ti4O12 (CCMTO) electro-ceramic, synthesized by the semi-wet route (SWR), ball-milled route (BMR) and solid-state route (SSR), is characterized by TG-DTA, XRD, SEM, EDX and TEM techniques. XRD confirmed the formation of single phase in CCMTO ceramic. The CuO phase present at grain boundaries in SWR ceramic was shown by the SEM micrograph, which was verified by EDX. The TEM image of SWR ceramic shows nanocrystalline particles in the range 80±20 nm. The value of the dielectric constant of SWR ( ɛ r ˜20091) ceramic is higher than those of BMR and SSR ( ɛ r ˜1247) ceramics at 1 kHz at 450 K. A dielectric relaxation has been observed in the frequency range 100 Hz-100 kHz. The high-temperature dielectric dispersion shows one large low-frequency response and two Debye-type relaxations. The impedance and modulus studies show the highest grain-boundary resistance for BMR ceramic.

  9. Empirical constraints on the effects of radiation damage on helium diffusion in zircon

    Science.gov (United States)

    Anderson, Alyssa J.; Hodges, Kip V.; van Soest, Matthijs C.

    2017-12-01

    In this study, we empirically evaluate the impact of radiation damage on zircon (U-Th)/He closure temperatures for a suite of zircon crystals from the slowly cooled McClure Mountain syenite of south-central Colorado, USA. We present new zircon, titanite, and apatite conventional (U-Th)/He dates, zircon laser ablation (U-Th)/He and U-Pb dates, and zircon Raman spectra for crystals from the syenite. Titanite and apatite (U-Th)/He dates range from 447 to 523 Ma and 88.0 to 138.9 Ma, respectively, and display no clear correlation between (U-Th)/He date and effective uranium concentration. Conventional zircon (U-Th)/He dates range from 230.3 to 474 Ma, while laser ablation zircon (U-Th)/He dates show even greater dispersion, ranging from 5.31 to 520 Ma. Dates from both zircon (U-Th)/He datasets decrease with increasing alpha dose, indicating that most of the dispersion can be attributed to radiation damage. Alpha dose values for the dated zircon crystals range from effectively zero to 2.15 × 1019 α /g, spanning the complete damage spectrum. We use an independently constrained thermal model to empirically assign a closure temperature to each dated zircon grain. If we assume that this thermal model is robust, the zircon radiation damage accumulation and annealing model of Guenthner et al. (2013) does not accurately predict closure temperatures for many of the analyzed zircon crystals. Raman maps of the zircons dated by laser ablation document complex radiation damage zoning, sometimes revealing crystalline zones in grains with alpha dose values suggestive of amorphous material. Such zoning likely resulted in heterogeneous intra-crystalline helium diffusion and may help explain some of the discrepancies between our empirical findings and the Guenthner et al. (2013) model predictions. Because U-Th zoning is a common feature in zircon, radiation damage zoning is likely to be a concern for most ancient, slowly cooled zircon (U-Th)/He datasets. Whenever possible, multiple

  10. Silicic melt evolution in the early Izu-Bonin arc recorded in detrital zircons: Zircon U-Pb geochronology and trace element geochemistry for Site U1438, Amami Sankaku Basin

    Science.gov (United States)

    Barth, A. P.; Tani, K.; Meffre, S.; Wooden, J. L.; Coble, M. A.

    2016-12-01

    Understanding the petrologic evolution of oceanic arc magmas through time is important because these arcs reveal the processes of formation and the early evolution of juvenile continental crust. The Izu-Bonin (IB) arc system has been targeted because it is one of several western Pacific intraoceanic arcs initiated at 50 Ma and because of its prominent spatial asymmetry, with widespread development of relatively enriched rear arc lavas. We examined Pb/U and trace element compositions in zircons recovered at IODP Site 351-U1438 and compared them to regional and global zircon suites. These new arc zircon data indicate that detrital zircons will yield new insights into the generation of IB silicic melts and form a set of useful geochemical proxies for interpreting ancient arc detrital zircon provenance. Project IBM drilling target IBM1 was explored by Expedition 351 at Site U1438, located in the proximal back-arc of the northern Kyushu-Palau Ridge (KPR) at 27.3°N. A 1.2 km thick section of Paleogene volcaniclastic rocks, increasingly lithified and hydrothermally altered with depth, constitutes a proximal rear arc sedimentary record of IB arc initiation and early arc evolution. The ages and compositions of U1438 zircons are compatible with provenance in one or more edifices of the northern KPR and are incompatible with drilling contamination. Melt zircon saturation temperatures and Ti-in-zircon thermometry suggest a provenance in relatively cool and silicic KPR melts. The abundances of selected trace elements with high native concentrations provide insight into the petrogenesis of U1438 detrital zircon host melts, and may be useful indicators of both short and long-term variations in melt compositions in arc settings. The U1438 zircons are slightly enriched in U and LREE and are depleted in Nb compared to zircons from mid-ocean ridges and the Parece-Vela Basin, as predicted for melts in a primitive oceanic arc setting with magmas derived from a highly depleted mantle

  11. XRF analysis of ceramics, minerals and allied materials

    International Nuclear Information System (INIS)

    Bennett, H.; Oliver, G.J.

    1992-01-01

    This book is a compilation of practical information on the X-ray fluorescence analysis by the fused, cast bead method of mineral type materials and products. A range of general information about equipment and apparatus and its use and care is given and particular attention is devoted to the spectrometer and the topic of line selection. Experimental details of the method, including calibration, are presented. In the final section of the book, analytical procedures for a wide range of materials are described. This includes sampling, drying, weighing, loss on ignition, fusion, casting, constituents to be determined, calibration ranges and reporting of results. The materials covered are silica/alumina range materials, calcium-rich materials, magnesium rich materials, zircon-bearing materials, various oxides and titanates, reduced materials and samples of unknown composition. The appendices contain data on loss on ignition techniques, specific fusion techniques, problem elements or oxides, certified references materials and details on laboratory accreditation. (UK)

  12. A method of making an ultrasonic transducer

    International Nuclear Information System (INIS)

    Bishop, J.

    1980-01-01

    A wafer of lead zirconate titanate (piezo-electric material) having silver face coatings is heat and pressure bonded, under vacuum, to a nickel diaphragm with the interposition of lead, and the wafer of lead zirconate titanate is slidably rotated relative to the surface of the diaphragm during the bonding process to effect an improved bond. The wafer is pressed and rotated by a shaft 'S' about the lower end of which R.F. induction heating coils are disposed. The bonding produces a lead/silver eutectic alloy. (author)

  13. Amino acidis derived from Titan tholins

    Science.gov (United States)

    Khare, Bishun N.; Sagan, Carl; Ogino, Hiroshi; Nagy, Bartholomew; Er, Cevat

    1986-01-01

    The production of amino acids by acid treatment of Titan tholin is experimentally investigated. The synthesis of Titan tholin and the derivatization of amino acids to N-trifluoroacetyl isopropyl esters are described. The gas chromatography/mass spectroscopy analysis of the Titan tholins reveals the presence of glycine, alpha and beta alainine, and aspartic acid, and the total yield of amino acids is about 0.01.

  14. Thermoluminescence of zircon: a kinetic model

    CERN Document Server

    Turkin, A A; Vainshtein, D I; Hartog, H W D

    2003-01-01

    The mineral zircon, ZrSiO sub 4 , belongs to a class of promising materials for geochronometry by means of thermoluminescence (TL) dating. The development of a reliable and reproducible method for TL dating with zircon requires detailed knowledge of the processes taking place during exposure to ionizing radiation, long-term storage, annealing at moderate temperatures and heating at a constant rate (TL measurements). To understand these processes one needs a kinetic model of TL. This paper is devoted to the construction of such a model. The goal is to study the qualitative behaviour of the system and to determine the parameters and processes controlling TL phenomena of zircon. The model considers the following processes: (i) Filling of electron and hole traps at the excitation stage as a function of the dose rate and the dose for both (low dose rate) natural and (high dose rate) laboratory irradiation. (ii) Time dependence of TL fading in samples irradiated under laboratory conditions. (iii) Short time anneali...

  15. Radioactivity and associated radiation hazards in ceramic raw materials and end products.

    Science.gov (United States)

    Viruthagiri, G; Rajamannan, B; Suresh Jawahar, K

    2013-12-01

    Studies have been planned to obtain activity and associated radiation hazards in ceramic raw materials (quartz, feldspar, clay, zircon, kaolin, grog, alumina bauxite, baddeleyite, masse, dolomite and red mud) and end products (ceramic brick, glazed ceramic wall and floor tiles) as the activity concentrations of uranium, thorium and potassium vary from material to material. The primordial radionuclides in ceramic raw materials and end products are one of the sources of radiation hazard in dwellings made of these materials. By the determination of the activity level in these materials, the indoor radiological hazard to human health can be assessed. This is an important precautionary measure whenever the dose rate is found to be above the recommended limits. The aim of this work was to measure the activity concentration of (226)Ra, (232)Th and (40)K in ceramic raw materials and end products. The activity of these materials has been measured using a gamma-ray spectrometry, which contains an NaI(Tl) detector connected to multichannel analyser (MCA). Radium equivalent activity, alpha-gamma indices and radiation hazard indices associated with the natural radionuclides are calculated to assess the radiological aspects of the use of the ceramic end products as decorative or covering materials in construction sector. Results obtained were examined in the light of the relevant international legislation and guidance and compared with the results of similar studies reported in different countries. The results suggest that the use of ceramic end product samples examined in the construction of dwellings, workplace and industrial buildings is unlikely to give rise to any significant radiation exposure to the occupants.

  16. Radioactivity and associated radiation hazards in ceramic raw materials and end products

    International Nuclear Information System (INIS)

    Viruthagiri, G.; Rajamannan, B.; Suresh Jawahar, K.

    2013-01-01

    Studies have been planned to obtain activity and associated radiation hazards in ceramic raw materials (quartz, feldspar, clay, zircon, kaolin, grog, alumina bauxite, baddeleyite, masse, dolomite and red mud) and end products (ceramic brick, glazed ceramic wall and floor tiles) as the activity concentrations of uranium, thorium and potassium vary from material to material. The primordial radionuclides in ceramic raw materials and end products are one of the sources of radiation hazard in dwellings made of these materials. By the determination of the activity level in these materials, the indoor radiological hazard to human health can be assessed. This is an important precautionary measure whenever the dose rate is found to be above the recommended limits. The aim of this work was to measure the activity concentration of 226 Ra, 232 Th and 40 K in ceramic raw materials and end products. The activity of these materials has been measured using a gamma-ray spectrometry, which contains an NaI(Tl) detector connected to multichannel analyser (MCA). Radium equivalent activity, alpha-gamma indices and radiation hazard indices associated with the natural radionuclides are calculated to assess the radiological aspects of the use of the ceramic end products as decorative or covering materials in construction sector. Results obtained were examined in the light of the relevant international legislation and guidance and compared with the results of similar studies reported in different countries. The results suggest that the use of ceramic end product samples examined in the construction of dwellings, workplace and industrial buildings is unlikely to give rise to any significant radiation exposure to the occupants. (authors)

  17. Bismuth titanate nanorods and their visible light photocatalytic properties

    International Nuclear Information System (INIS)

    Pei, L.Z.; Liu, H.D.; Lin, N.; Yu, H.Y.

    2015-01-01

    Highlights: • Bismuth titanate nanorods have been synthesized by a simple hydrothermal process. • The size of bismuth titanate nanorods can be controlled by growth conditions. • Bismuth titanate nanorods show good photocatalytic activities of methylene blue and Rhodamine B. - Abstract: Bismuth titanate nanorods have been prepared using a facile hydrothermal process without additives. The bismuth titanate products were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), high-resolution TEM (HRTEM) and UV-vis diffusion reflectance spectrum. XRD pattern shows that the bismuth titanate nanorods are composed of cubic Bi 2 Ti 2 O 7 phase. Electron microscopy images show that the length and diameter of the bismuth titanate nanorods are 50-200 nm and 2 μm, respectively. Hydrothermal temperature and reaction time play important roles on the formation and size of the bismuth titanate nanorods. UV-vis diffusion reflectance spectrum indicates that bismuth titanate nanorods have a band gap of 2.58 eV. The bismuth titanate nanorods exhibit good photocatalytic activities in the photocatalytic degradation of methylene blue (MB) and Rhodamine B (RB) under visible light irradiation. The bismuth titanate nanorods with cubic Bi 2 Ti 2 O 7 phase are a promising candidate as a visible light photocatalyst

  18. Hubble Observes Surface of Titan

    Science.gov (United States)

    1994-01-01

    Scientists for the first time have made images of the surface of Saturn's giant, haze-shrouded moon, Titan. They mapped light and dark features over the surface of the satellite during nearly a complete 16-day rotation. One prominent bright area they discovered is a surface feature 2,500 miles across, about the size of the continent of Australia.Titan, larger than Mercury and slightly smaller than Mars, is the only body in the solar system, other than Earth, that may have oceans and rainfall on its surface, albeit oceans and rain of ethane-methane rather than water. Scientists suspect that Titan's present environment -- although colder than minus 289 degrees Fahrenheit, so cold that water ice would be as hard as granite -- might be similar to that on Earth billions of years ago, before life began pumping oxygen into the atmosphere.Peter H. Smith of the University of Arizona Lunar and Planetary Laboratory and his team took the images with the Hubble Space Telescope during 14 observing runs between Oct. 4 - 18. Smith announced the team's first results last week at the 26th annual meeting of the American Astronomical Society Division for Planetary Sciences in Bethesda, Md. Co-investigators on the team are Mark Lemmon, a doctoral candidate with the UA Lunar and Planetary Laboratory; John Caldwell of York University, Canada; Larry Sromovsky of the University of Wisconsin; and Michael Allison of the Goddard Institute for Space Studies, New York City.Titan's atmosphere, about four times as dense as Earth's atmosphere, is primarily nitrogen laced with such poisonous substances as methane and ethane. This thick, orange, hydrocarbon haze was impenetrable to cameras aboard the Pioneer and Voyager spacecraft that flew by the Saturn system in the late 1970s and early 1980s. The haze is formed as methane in the atmosphere is destroyed by sunlight. The hydrocarbons produced by this methane destruction form a smog similar to that found over large cities, but is much thicker

  19. The rotation of Titan and Ganymede

    Science.gov (United States)

    Van Hoolst, Tim; Coyette, Alexis; Baland, Rose-Marie; Trinh, Antony

    2016-10-01

    The rotation rates of Titan and Ganymede, the largest satellites of Saturn and Jupiter, are on average equal to their orbital mean motion. Here we discuss small deviations from the average rotation for both satellites and evaluate the polar motion of Titan induced by its surface fluid layers. We examine different causes at various time scales and assess possible consequences and the potential of using librations and polar motion as probes of the interior structure of the satellites.The rotation rate of Titan and Ganymede cannot be constant on the orbital time scale as a result of the gravitational torque of the central planet acting on the satellites. Titan is moreover expected to show significant polar motion and additional variations in the rotation rate due to angular momentum exchange with the atmosphere, mainly at seasonal periods. Observational evidence for deviations from the synchronous state has been reported several times for Titan but is unfortunately inconclusive. The measurements of the rotation variations are based on determinations of the shift in position of Cassini radar images taken during different flybys. The ESA JUICE (JUpiter ICy moons Explorer) mission will measure the rotation variations of Ganymede during its orbital phase around the satellite starting in 2032.We report on different theoretical aspects of the librations and polar motion. We consider the influence of the rheology of the ice shell and take into account Cassini measurements of the external gravitational field and of the topography of Titan and similar Galileo data about Ganymede. We also evaluate the librations and polar motion induced by Titan's hydrocarbon seas and use the most recent results of Titan's atmosphere dynamics. We finally evaluate the potential of rotation variations to constrain the satellite's interior structure, in particular its ice shell and ocean.

  20. Pengaruh Temperatur, Waktu, dan Aditif Dalam Pembuatan Zircon Micronized

    Directory of Open Access Journals (Sweden)

    Sajima

    2017-05-01

    Full Text Available Research on temperature, time and additives effects on milling process in micronized-zircon production has been conducted. The production of zircon micronized started from sorting process on mining products then followed by beneficiation, roasting, leaching, dryng and milling processes. The results showed that the optimum conditions of the roasting process was at the temperature of 425 °C, in 25 minutes and using 4% additives. In these conditions, micronized zircon (2 µm obtained as much as 92.10% in10 minutes milling time.

  1. Future Exploration of Titan and Enceladus

    Science.gov (United States)

    Matson, D. L.; Coustenis, A.; Lunine, J.; Lebreton, J.; Reh, K.; Beauchamp, P.

    2009-05-01

    The future exploration of Titan and Enceladus has become very important for the planetary community. The study conducted last year of the Titan Saturn System Mission (TSSM) led to an announcement in which ESA and NASA prioritized future OPF missions, stating that TSSM is planned after EJSM (for details see http://www.lpi.usra.edu/opag/). TSSM consists of a TSSM Orbiter that would carry two in situ elements: the Titan Montgolfiere hot air balloon and the Titan Lake Lander. The mission could launch in the 2023-2025 timeframe on a trajectory to arrive ~9 years later for a 4-year mission in the Saturn system. Soon after arrival at Saturn, the montgolfiere would be delivered to Titan to begin its mission of airborne, scientific observations of Titan from an altitude of about 10 km. The montgolfiere would have a Multi-Mission Radioisotope Thermoelectric Generator (MMRTG) power system and would be designed to last at least 6-12 months in Titan's atmosphere. With the predicted winds and weather, that would be sufficient to circumnavigate the globe! On a subsequent fly-by, the TSSM orbiter would release the Lake Lander on a trajectory toward Titan for a targeted entry. It would descend through the atmosphere making scientific measurements, much like Huygens did, and then land and float on one of Titan's seas. This would be its oceanographic phase, making a physical and chemical assessment of the sea. The Lake Lander would operate 8-10 hours until its batteries become depleted. Following the delivery of the in situ elements, the TSSM orbiter would explore the Saturn system via a 2-year tour that includes in situ sampling of Enceladus' plumes as well as Titan flybys. After the Saturn system tour, the TSSM orbiter would enter orbit around Titan for a global survey phase. Synergistic and coordinated observations would be carried out between the TSSM orbiter and the in situ elements. The scientific requirements were developed by the international TSSM Joint Science Definition

  2. Characterization of inclusions in terrestrial impact formed zircon: Constraining the formation conditions of Hadean zircon from Jack Hills, Western Australia

    Science.gov (United States)

    Faltys, J. P.; Wielicki, M. M.; Sizemore, T. M.

    2017-12-01

    Due to the discovery and subsequent geochemical analysis of Hadean terrestrial material (e.g. detrital zircon from Jack Hills, Western Australia), a dramatic paradigm shift has occurred in the hypothesized near surface conditions of the first 500 million years of Earth's evolution. From a hellish setting riddled with impactors and not fit for life to a much milder environment that may have been uniquely suitable for the origin of life. Geochemical analyses of these ancient materials have been used to suggest the presence of water at or near the surface as well as the existence of continental crust during the Hadean, both of which have been suggested as necessary for the origin of life. However, the intensity of extraterrestrial bombardment during the Hadean and the effects of such events on the origin of life remains poorly understood. Clearly, as evidenced by Phanerozoic impact events, extraterrestrial impactors have the potential to dramatically effect the environment, particularly the biosphere. Early Earth likely experienced multiple large impact events, as evidenced by the lunar record, however whether those impacts were sufficient to frustrate the origin of life remains an open question. Although multiple lines of evidence, including the inclusion population, suggest the formation of Hadean zircon from Jack Hills as crystallizing in an under-thrust environment from S-type magmas, a recent study has suggested their formation in an impact melt environment analogous to a portion of the Sudbury Igneous Complex at the Sudbury impact structure. To determine between these two formation scenarios we have under-taken an inclusion study of terrestrial impact formed zircon from four of the largest terrestrial impact structures (Sudbury, Canada; Manicouagan, Canada; Vredefort, South Africa; Morokweng, South Africa), to compare to the vast inclusion dataset that exists for Jack Hills zircon. Preliminary data suggests a different inclusion population, from Hadean zircon

  3. Clash of the Titans

    Science.gov (United States)

    Subramaniam, Karthigeyan

    2010-01-01

    WebQuests and the 5E learning cycle are titans of the science classroom. These popular inquiry-based strategies are most often used as separate entities, but the author has discovered that using a combined WebQuest and 5E learning cycle format taps into the inherent power and potential of both strategies. In the lesson, "Clash of the Titans,"…

  4. Large Displacement in Relaxor Ferroelectric Terpolymer Blend Derived Actuators Using Al Electrode for Braille Displays

    Science.gov (United States)

    Lu, S. G.; Chen, X.; Levard, T.; Diglio, P. J.; Gorny, L. J.; Rahn, C. D.; Zhang, Q. M.

    2015-06-01

    Poly(vinylidene fluoride) (PVDF) based polymers are attractive for applications for artificial muscles, high energy density storage devices etc. Recently these polymers have been found great potential for being used as actuators for refreshable full-page Braille displays for visually impaired people in terms of light weight, miniaturized size, and larger displacement, compared with currently used lead zirconate titanate ceramic actuators. The applied voltages of published polymer actuators, however, cannot be reduced to meet the requirements of using city power. Here, we report the polymer actuator generating quite large displacement and blocking force at a voltage close to the city power. Our embodiments also show good self-healing performance and disuse of lead-containing material, which makes the Braille device safer, more reliable and more environment-friendly.

  5. Electroactive properties of flexible piezoelectric composites

    Directory of Open Access Journals (Sweden)

    Sakamoto Walter Katsumi

    2001-01-01

    Full Text Available A flexible piezoelectric composite with 0-3 connectivity, made from Lead Zirconate Titanate (PZT powder and vegetable-based polyurethane (PU, was doped with small amount of semiconductor powder. As a result a composite with 0-0-3 connectivity was obtained. The nature of absorption and steady state electrical conduction and the dielectric behaviour have been studied for this ceramic/polymer composite. The dielectric loss processes of the composite were observed to be dominated by those the polymer. Adding a semiconductor phase in the composite the electrical conductivity can be controlled and a continuous electric flux path could be created between the PZT grains. This composite may be poled at low voltage and in shorter time compared with composites without a conductive phase.

  6. U-Th-Pb systematics in zircon and titanite

    International Nuclear Information System (INIS)

    Zartman, R.E.; Kwak, L.M.

    1990-01-01

    U-Th-Pb isotopic analyses of zircon and titanite were made for two core samples of granite from borehole ATK-1 drilled into the Eye-Dashwa Lakes pluton. One of the samples from near the bottom of the hole (990.97 to 996.78 m) yielded zircon and titanite that were slightly to severely disturbed isotopically. Eight fractions of zircon give an upper concordia intercept age of 2625 ± 16 Ma (MSWD = 34), which, based on an evaluation of the more concordant data points and on other geochronological results, is interpreted as being slightly too young. The time of crystallization is probably better approximated by the 207 Pb/ 206 Pb age of 2665 Ma determined on a slightly (∼8 percent) discordant titanite. The other sample from near the surface (3.85 to 9.61 m) generally revealed even more severely disturbed isotopic systematics for both zircon and titanite. The complex nature of the disturbances probably resulted from the penetration of meteoritic water into rock already modified by post-crystallization hydrothermal alteration. Nuclide migration occurred in both minerals -- during the Middle or Late Proterozoic for the zircon and during the modern weathering cycle for the titanite. Material balance calculations are used to demonstrate a recent relative gain of radiogenic Pb and/or loss of Th and U from the freshest-looking, least-altered titanite by exchange with altered, leucoxenite-bearing titanite

  7. Recovery and recycling of lithium value from spent lithium titanate (Li{sub 2}TiO{sub 3}) pebbles

    Energy Technology Data Exchange (ETDEWEB)

    Mandal, D., E-mail: dmandal10@gmail.com

    2013-09-15

    Graphical abstract: Effects of various process parameters on the recovery of Li-from spent Li{sub 2}TiO{sub 3} pebbles were investigated. From the experimental results it was observed that the leaching rate increases with speed of stirring till 450 rpm and then above 450 rpm; the increase in speed of stirring does not have any significant effect on the leaching rate as shown in the following figure. Effects of other parameters on the Li-recovery from spent Li{sub 2}TiO{sub 3} pebbles are discussed in this paper. Abstract: In the first generation fusion reactors the fusion of deuterium (D) and tritium (T) is considered to produce energy to meet the future energy demand. Deuterium is available in nature whereas, tritium is not. Lithium-6 (Li{sup 6}) isotope has the ability to produce tritium in the n, α nuclear reaction with neutrons. Thus lithium-based ceramics enriched by Li{sup 6} isotope are considered for the tritium generation for its use in future fusion reactors. Lithium titanate is one such Li-based ceramic material being considered for its some attractive properties viz., high thermal and chemical stability, high thermal conductivity, and low tritium solubility. It is reported in the literature, that the burn up of these pebbles in the fusion reactor will be limited to only 15–17 atomic percentage. At the end of life, the pebbles will contain more than 45% unused Li{sup 6} isotope. Due to the high cost of enriched Li{sup 6} and the waste disposal considerations, it is necessary to recover the unused Li from the spent lithium titanate pebbles. Till date, only the feasibilities of different processes are reported, but no process details are available. Experiments were carried out for the recovery of Li from simulated Li{sub 2}TiO{sub 3} pebbles and to reuse of lithium in lithium titanate pebble fabrication. The details of the experiments and results are discussed in this paper.

  8. Characterization And Operation Of PZT Ceramic Filters On Gamma-Radiation Environment

    International Nuclear Information System (INIS)

    Fawzy, Y.H.A.; Soliman, F.A.S.; Swidan, A.; Abdelmagid, A.

    2008-01-01

    The present paper deals with the gamma-ray effects on the electrical characteristics of ferroelectric materials used as an electronic frequency filters. After the recall of main observations, mechanisms are analyzed and proposed to take into account the effects in Lead- Zirconate-Titanate (PZT) based materials. In this concern, a wide frequency range samples, extends from 400 k Hz up to 6.5 MHz, were chosen for studying their frequency response and related terminologies, dynamic characteristics, and equivalent circuits. In general, for all samples, a shift on the frequency values was recorded, where the values of the center frequency, resonance frequency and anti-resonance frequency were shown to be shifted. The observed shift is mainly due to the noticed changes on the equivalent circuit elements of the devices, where a pronounced shift on the values of L,,,CP and R,, were recorded

  9. Spectroscopic determination of optimal hydration time of zircon surface

    Energy Technology Data Exchange (ETDEWEB)

    Ordonez R, E. [ININ, Departamento de Quimica, Carretera Mexico-Toluca s/n, 52750 Ocoyoacac, Estado de Mexico (Mexico); Garcia R, G. [Instituto Tecnologico de Toluca, Division de Estudios del Posgrado, Av. Tecnologico s/n, Ex-Rancho La Virgen, 52140 Metepec, Estado de Mexico (Mexico); Garcia G, N., E-mail: eduardo.ordonez@inin.gob.m [Universidad Autonoma del Estado de Mexico, Facultad de Quimica, Av. Colon y Av. Tollocan, 50180 Toluca, Estado de Mexico (Mexico)

    2010-07-01

    When a mineral surface is immersed in an aqueous solution, it develops and electric charge produced by the amphoteric dissociation of hydroxyl groups created by the hydration of the solid surface. This is one influential surface property. The complete hydration process takes a time which is specific for each mineral species. The knowledge of the aqueous solution contact time for complete surface hydration is mandatory for further surface phenomena studies. This study deals with the optimal hydration time of the raw zircon (ZrSiO{sub 4}) surface comparing the classical potentiometric titrations with a fluorescence spectroscopy technique. The latter is easy and rea liable as it demands only one sample batch to determine the optimal time to ensure a total hydration of the zircon surface. The analytical results of neutron activation analysis showed the presence of trace quantities of Dy{sup 3+}, Eu{sup 3+} and Er{sup 3} in the bulk of zircon. The Dy{sup 3+} is structured in the zircon crystalline lattice and undergoes the same chemical reactions as zircon. Furthermore, the Dy{sup 3+} has a good fluorescent response whose intensity is enhanced by hydration molecules. The results show that, according to the potentiometric analysis, the hydration process for each batch (at least 8 sample batches) takes around 2 h, while the spectrometric method indicates only 5 minutes from only one batch. Both methods showed that the zircon surface have a 16 h optimal hydration time. (Author)

  10. Spectroscopic determination of optimal hydration time of zircon surface

    International Nuclear Information System (INIS)

    Ordonez R, E.; Garcia R, G.; Garcia G, N.

    2010-01-01

    When a mineral surface is immersed in an aqueous solution, it develops and electric charge produced by the amphoteric dissociation of hydroxyl groups created by the hydration of the solid surface. This is one influential surface property. The complete hydration process takes a time which is specific for each mineral species. The knowledge of the aqueous solution contact time for complete surface hydration is mandatory for further surface phenomena studies. This study deals with the optimal hydration time of the raw zircon (ZrSiO 4 ) surface comparing the classical potentiometric titrations with a fluorescence spectroscopy technique. The latter is easy and rea liable as it demands only one sample batch to determine the optimal time to ensure a total hydration of the zircon surface. The analytical results of neutron activation analysis showed the presence of trace quantities of Dy 3+ , Eu 3+ and Er 3 in the bulk of zircon. The Dy 3+ is structured in the zircon crystalline lattice and undergoes the same chemical reactions as zircon. Furthermore, the Dy 3+ has a good fluorescent response whose intensity is enhanced by hydration molecules. The results show that, according to the potentiometric analysis, the hydration process for each batch (at least 8 sample batches) takes around 2 h, while the spectrometric method indicates only 5 minutes from only one batch. Both methods showed that the zircon surface have a 16 h optimal hydration time. (Author)

  11. TITAN'S TRANSPORT-DRIVEN METHANE CYCLE

    International Nuclear Information System (INIS)

    Mitchell, Jonathan L.

    2012-01-01

    The mechanisms behind the occurrence of large cloud outbursts and precipitation on Titan have been disputed. A global- and annual-mean estimate of surface fluxes indicated only 1% of the insolation, or ∼0.04 W m –2 , is exchanged as sensible and/or latent fluxes. Since these fluxes are responsible for driving atmospheric convection, it has been argued that moist convection should be quite rare and precipitation even rarer, even if evaporation globally dominates the surface-atmosphere energy exchange. In contrast, climate simulations indicate substantial cloud formation and/or precipitation. We argue that the top-of-atmosphere (TOA) radiative imbalance is diagnostic of horizontal heat transport by Titan's atmosphere, and thus constrains the strength of the methane cycle. Simple calculations show the TOA radiative imbalance is ∼0.5-1 W m –2 in Titan's equatorial region, which implies 2-3 MW of latitudinal heat transport by the atmosphere. Our simulation of Titan's climate suggests this transport may occur primarily as latent heat, with net evaporation at the equator and net accumulation at higher latitudes. Thus, the methane cycle could be 10-20 times previous estimates. Opposing seasonal transport at solstices, compensation by sensible heat transport, and focusing of precipitation by large-scale dynamics could further enhance the local, instantaneous strength of Titan's methane cycle by a factor of several. A limited supply of surface liquids in regions of large surface radiative imbalance may throttle the methane cycle, and if so, we predict more frequent large storms over the lakes district during Titan's northern summer.

  12. Radiation stability of sodium titanate ion exchange materials

    International Nuclear Information System (INIS)

    Kenna, B.T.

    1980-02-01

    Sodium titanate and sodium titanate loaded macroreticular resin are being considered as ion exchangers to remove 90 Sr and actinides from the large volume of defense waste stored at Hanford Site in Washington. Preliminary studies to determine the radiation effect on Sr +2 and I - capacity of these ion-exchange materials were conducted. Samples of sodium titanate powder, sodium titanate loaded macroreticular resin, as well as the nitrate form of macroreticular anion resin were irradiated with up to 2 x 10 9 Rads of 60 Co gamma rays. Sodium titanate cation capacity decreased about 50% while the sodium titanate loaded macroeticular resin displayed a dramatic decrease in cation capacity when irradiated with 10 8 -10 9 Rad. The latter decrease is tentatively ascribed to radiation damage to the organic portion which subsequently inhibits interaction with the contained sodium titanate. The anion capacity of both macroreticular resin and sodium titanate loaded macroreticular resin exhibited significant decreases with increasing radiation exposure. These results suggest that consideration should be given to the potential effects of radiation degradation if column regeneration is to be used. 5 figures, 2 tables

  13. Processing, properties, and application of textured 0.72lead(magnesium niobate)-0.28lead titanate ceramics

    Science.gov (United States)

    Brosnan, Kristen H.

    In this study, XRD and electron backscatter diffraction (EBSD) techniques were used to characterize the fiber texture in oriented PMN-28PT and the intensity data were fit with a texture model (the March-Dollase equation) that describes the texture in terms of texture fraction (f), and the width of the orientation distribution (r). EBSD analysis confirmed the orientation of the microstructure, with no distinguishable randomly oriented, fine grain matrix. Although XRD rocking curve and EBSD data analysis gave similar f and r values, XRD rocking curve analysis was the most efficient and gave a complete description of texture fraction and texture orientation (f = 0.81 and r = 0.21, respectively). XRD rocking curve analysis was the preferred approach for characterization of the texture volume and the orientation distribution of texture in fiber-oriented PMN-PT. The dielectric, piezoelectric and electromechanical properties for random ceramic, 69 vol% textured, 81 vol% textured, and single crystal PMN-28PT were fully characterized and compared. The room temperature dielectric constant at 1 kHz for highly textured PMN-28PT was epsilonr ≥ 3600 with low dielectric loss (tan delta = 0.004). The temperature dependence of the dielectric constant for 81 vol% textured ceramic followed a similar trend as the single crystal PMN-28PT up to the rhombohedral to tetragonal transition temperature (TRT) at 104°C. 81 vol% textured PMN-28PT consistently displayed 60 to 65% of the single crystal PMN-28PT piezoelectric coefficient (d33) and 1.5 to 3.0 times greater than the random ceramic d33 (measured by Berlincourt meter, unipolar strain-field curves, IEEE standard resonance method, and laser vibrometry). The 81 vol% textured PMN-28PT displayed similarly low piezoelectric hysteresis as single crystal PMN-28PT measured by strain-field curves at 5 kV/cm. 81 vol% textured PMN-28PT and single crystal PMN-28PT displayed similar mechanical quality factors of QM = 74 and 76, respectively. The

  14. Synthesis of SiCN@TiO2 core-shell ceramic microspheres via PDCs method

    Science.gov (United States)

    Liu, Hongli; Wei, Ning; Li, Jing; Zhang, Haiyuan; Chu, Peng

    2018-02-01

    A facile and effective polymer-derived ceramics (PDCs) emulsification-crosslinking-pyrolysis method was developed to fabricate SiCN@TiO2 core-shell ceramic microspheres with polyvinylsilazane (PVSZ) and tetrabutyl titanate (TBT) as precursors. The TBT: PVSZ mass ratios, emulsifier concentrations and the pyrolysis temperature were examined as control parameters to tune the size and morphology of microspheres. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) confirmed the synthesized SiCN@TiO2 microspheres to be comprised of SiCN core coated with TiO2 crystals, with an average size of 0.88 μm when pyrolyzed at 1400 °C. The analysis of Fourier transform infrared spectroscopy (FT-IR), energy dispersive spectroscopy (EDS) and X-ray diffraction (XRD) ensured that SiCN@TiO2 core-shell ceramic microspheres composed of rutile TiO2, β-SiC and Si3N4 crystalline phases, The thermal properties were characterized by thermogravimetric analysis (TGA). The obtained SiCN@TiO2 core-shell ceramic microspheres were the promising candidate of the infrared opacifier in silica aerogels and this technique can be extended to other preceramic polymers.

  15. Chemical investigation of Titan and Triton tholins

    Science.gov (United States)

    Mcdonald, Gene D.; Thompson, W. R.; Heinrich, Michael; Khare, Bishun N.; Sagan, Carl

    1994-01-01

    We report chromatographic and spectroscopic analyses of both Titan and Triton tholins, organic solids made from the plasma irradiation of 0.9:0.1 and 0.999:0.001 N2/CH4 gas mixtures, respectively. The lower CH4 mixing ratio leads to a nitrogen-richer tholin (N/C greater than 1), probably including nitrogen heterocyclic compounds. Unlike Titan tholin, bulk Triton tholin is poor in nitriles. From high-pressure liquid chromatography, ultraviolet and infrared spectroscopy, and molecular weight estimation by gel filtration chromatography, we conclude that (1) several H2O-soluble fractions, each with distinct UV and IR spectral signatures, are present, (2) these fractions are not identical in the two tholins, (3) the H2O-soluble fractions of Titan tholins do not contain significant amounts of nitriles, despite the major role of nitriles in bulk Titan tholin, and (4) the H2O-soluble fractions of both tholins are mainly molcules containing about 10 to 50 (C + N) atoms. We report yields of amino acids upon hydrolysis of Titan and Triton tholins. Titan tholin is largely insoluble in the putative hydrocarbon lakes or oceans on Titan, but can yield the H2O-soluble species investigated here upon contact with transient (e.g., impact-generated) liquid water.

  16. Two-stage model of development of heterogeneous uranium-lead systems in zircon

    International Nuclear Information System (INIS)

    Mel'nikov, N.N.; Zevchenkov, O.A.

    1985-01-01

    Behaviour of isotope systems of multiphase zircons at their two-stage distortion is considered. The results of calculations testify to the fact that linear correlations on the diagram with concordance can be explained including two-stage discovery of U-Pb systems of cogenetic zircons if zircon is considered physically heterogeneous and losing in its different part different ratios of accumulated radiogenic lead. ''Metamorphism ages'' obtained by these two-stage opening zircons are intermediate, and they not have geochronological significance while ''crystallization ages'' remain rather close to real ones. Two-stage opening zircons in some cases can be diagnosed by discordance of their crystal component

  17. The Exploration of Titan and the Saturnian System

    Science.gov (United States)

    Coustenis, Athena

    The exploration of the outer solar system and in particular of the giant planets and their environments is an on-going process with the Cassini spacecraft currently around Saturn, the Juno mission to Jupiter preparing to depart and two large future space missions planned to launch in the 2020-2025 time frame for the Jupiter system and its satellites (Europa and Ganymede) on the one hand, and the Saturnian system and Titan on the other hand [1,2]. Titan, Saturn's largest satellite, is the only other object in our Solar system to possess an extensive nitrogen atmosphere, host to an active organic chemistry, based on the interaction of N2 with methane (CH4). Following the Voyager flyby in 1980, Titan has been intensely studied from the ground-based large telescopes (such as the Keck or the VLT) and by artificial satellites (such as the Infrared Space Observatory and the Hubble Space Telescope) for the past three decades. Prior to Cassini-Huygens, Titan's atmospheric composition was thus known to us from the Voyager missions and also through the explorations by the ISO. Our perception of Titan had thus greatly been enhanced accordingly, but many questions remained as to the nature of the haze surrounding the satellite and the composition of the surface. The recent revelations by the Cassini-Huygens mission have managed to surprise us with many discoveries [3-8] and have yet to reveal more of the interesting aspects of the satellite. The Cassini-Huygens mission to the Saturnian system has been an extraordinary success for the planetary community since the Saturn-Orbit-Insertion (SOI) in July 2004 and again the very successful probe descent and landing of Huygens on January 14, 2005. One of its main targets was Titan. Titan was revealed to be a complex world more like the Earth than any other: it has a dense mostly nitrogen atmosphere and active climate and meteorological cycles where the working fluid, methane, behaves under Titan conditions the way that water does on

  18. Crystallization process of zircon and fergusonite during hydrothermal alteration in Nechalacho REE deposit, Thor Lake, Canada

    Science.gov (United States)

    Hoshino, M.; Watanabe, Y.; Murakami, H.; Kon, Y.; Tsunematsu, M.

    2012-04-01

    The core samples of two drill holes, which penetrate sub-horizontal mineralized horizons at Nechalacho REE deposit in the Proterozoic Thor Lake syenite, Canada, were studied in order to clarify magmatic and hydrothermal processes that enriched HFSE (e.g. Zr, Nb, Y and REE). Zircon is the most common REE minerals in Nechalacho REE deposit. The zircon is divided into five types as follows: Type-1 zircon occurs as single grain in phlogopite and the chondrite-normalized REE pattern is characterized by a steeply-rising slope from the LREE to the HREE with a positive Ce-anomaly and negative Eu-anomaly. This chemical characteristic is similar to that of igneous zircon. Type-2 zircon consists of HREE-rich magmatic porous core and LREE-Nb-F-rich hydrothermal rim. This type zircon is mostly included in phlogopite and fluorite, and occasionally in microcline. Type-3 zircon is characterized by euhedral to anhedral crystal, occurring in a complex intergrowth with REE fluorocarbonates. Type-3 zircons have high contents of REE, Nb and fluorine. Type-4 zircon consists of porous-core and -rim zones, but their chemical compositions are similar to each other. This type zircon is a subhedral crystal rimmed by fergusonite. Type-5 zircon is characterized by smaller, porous and subhedral to anhedral crystals. The interstices between small zircons are filled by fergusonite. Type-4 and -5 zircons show low REE and Nb contents. Occurrences of these five types of zircon are different according to the depth and degree of the alteration by hydrothermal solutions rich in F- and CO3 of the two drill holes, which permit a model for evolution of the zircon crystallization in Nechalacho REE deposit as follows: (1) type-1 (single magmatic zircon) is formed in miaskitic syenite. (2) LREE-Nb-F-rich hydrothermal zircon formed around HREE-rich magmatic zircon (type-2 zircon); (3) type-3 zircon crystallized thorough F and CO3-rich hydrothermal alteration of type-2 zircon which formed the complex

  19. Developing Zircon as a Probe of Planetary Impact History

    Science.gov (United States)

    Wielicki, Matthew

    2014-12-01

    The identification of Meteor Crater in Arizona as an extraterrestrial impact by Eugene Shoemaker provided the first evidence of this geologic phenomenon and opened the door to a new field of research that has eventually lead to the identification of over ~150 terrestrial impact structures. Subsequently impacts have been evoked in the formation of the moon, delivery of volatiles and bio-precursors to early Earth, creation of habitats for the earliest life and, in more recent times, major mass extinction events. However, understanding the impact flux to the Earth-Moon system has been complicated by the constant weathering and erosion at Earth's surface and the complex nature of impactite samples such that only a hand full of terrestrial craters have been accurately and precisely dated. Currently 40Ar/39Ar step-heating analysis of impactite samples is commonly used to infer impact ages but can be problematic due to the presence of relic clasts, incomplete 40Ar outgassing or excess 40Ar, and recoil and shock effects. The work presented here attempts to develop zircon geochronology to probe planetary impact histories as an alternative to current methods and provides another tool by which to constrain the bolide flux to the Earth-Moon system. Zircon has become the premier geo-chronometer in earth science and geochemical investigation of Hadean zircon from Western Australia has challenged the long-standing, popular conception that the near-surface Hadean Earth was an uninhabitable and hellish world; Zircons may preserve environmental information regarding their formation and thus provide a rare window into conditions on early Earth. Isotopic and petrologic analyses of these ancient grains have been interpreted to suggest that early Earth was more habitable than previously envisioned, with water oceans, continental crust, and possibly even plate tectonics. The Hadean is also suspected to be a time of major planetary bombardment however identifying impact signatures within

  20. Seasonal Changes in Titan's Meteorology

    Science.gov (United States)

    Turtle, E. P.; DelGenio, A. D.; Barbara, J. M.; Perry, J. E.; Schaller, E. L.; McEwen, A. S.; West, R. A.; Ray, T. L.

    2011-01-01

    The Cassini Imaging Science Subsystem has observed Titan for 1/4 Titan year, and we report here the first evidence of seasonal shifts in preferred locations of tropospheric methane clouds. South \\polar convective cloud activity, common in late southern summer, has become rare. North \\polar and northern mid \\latitude clouds appeared during the approach to the northern spring equinox in August 2009. Recent observations have shown extensive cloud systems at low latitudes. In contrast, southern mid \\latitude and subtropical clouds have appeared sporadically throughout the mission, exhibiting little seasonality to date. These differences in behavior suggest that Titan s clouds, and thus its general circulation, are influenced by both the rapid temperature response of a low \\thermal \\inertia surface and the much longer radiative timescale of Titan s cold thick troposphere. North \\polar clouds are often seen near lakes and seas, suggesting that local increases in methane concentration and/or lifting generated by surface roughness gradients may promote cloud formation. Citation