  1. Lattice strain in irradiated materials unveils a prevalent defect evolution mechanism

    Science.gov (United States)

    Debelle, Aurélien; Crocombette, Jean-Paul; Boulle, Alexandre; Chartier, Alain; Jourdan, Thomas; Pellegrino, Stéphanie; Bachiller-Perea, Diana; Carpentier, Denise; Channagiri, Jayanth; Nguyen, Tien-Hien; Garrido, Frédérico; Thomé, Lionel

    2018-01-01

    Modification of materials using ion beams has become a widespread route to improve or design materials for advanced applications, from ion doping for microelectronic devices to emulation of nuclear reactor environments. Yet, despite decades of studies, major issues regarding ion/solid interactions are not solved, one of them being the lattice-strain development process in irradiated crystals. In this work, we address this question using a consistent approach that combines x-ray diffraction (XRD) measurements with both molecular dynamics (MD) and rate equation cluster dynamics (RECD) simulations. We investigate four distinct materials that differ notably in terms of crystalline structure and nature of the atomic bonding. We demonstrate that these materials exhibit a common behavior with respect to the strain development process. In fact, a strain build-up followed by a strain relaxation is observed in the four investigated cases. The strain variation is unambiguously ascribed to a change in the defect configuration, as revealed by MD simulations. Strain development is due to the clustering of interstitial defects into dislocation loops, while the strain release is associated with the disappearance of these loops through their integration into a network of dislocation lines. RECD calculations of strain depth profiles, which are in agreement with experimental data, indicate that the driving force for the change in the defect nature is the defect clustering process. This study paves the way for quantitative predictions of the microstructure changes in irradiated materials.

  2. Defect production in Ar irradiated graphene membranes under different initial applied strains

    Energy Technology Data Exchange (ETDEWEB)

    Martinez-Asencio, J., E-mail: jesusmartinez@ua.es [Dept. Física Aplicada, Facultad de Ciencias, Fase II, Universidad de Alicante, Alicante E-036090 (Spain); Ruestes, C.J.; Bringa, E. [CONICET and Facultad de Ciencias Exactas y Naturales, Universidad Nacional de Cuyo, Mendoza 5500 (Argentina); Caturla, M.J. [Dept. Física Aplicada, Facultad de Ciencias, Fase II, Universidad de Alicante, Alicante E-036090 (Spain)

    2017-02-15

    Highlights: • Defects in graphene membranes are formed due to 140 eV Ar ions irradiation using MD. • Different initial strains are applied, which influence the type and number of defects. • Mono-vacancies, di-vacancies and tri-vacancies production behaves linearly with dose. • The total number of defects under compression is slightly higher than under tension. - Abstract: Irradiation with low energy Ar ions of graphene membranes gives rise to changes in the mechanical properties of this material. These changes have been associated to the production of defects, mostly isolated vacancies. However, the initial state of the graphene membrane can also affect its mechanical response. Using molecular dynamics simulations we have studied defect production in graphene membranes irradiated with 140 eV Ar ions up to a dose of 0.075 × 10{sup 14} ions/cm{sup 2} and different initial strains, from −0.25% (compressive strain) to 0.25% (tensile strain). For all strains, the number of defects increases linearly with dose with a defect production of about 80% (80 defects every 100 ions). Defects are mostly single vacancies and di-vacancies, although some higher order clusters are also observed. Two different types of di-vacancies have been identified, the most common one being two vacancies at first nearest neighbours distance. Differences in the total number of defects with the applied strain are observed which is related to the production of a higher number of di-vacancies under compressive strain compared to tensile strain. We attribute this effect to the larger out-of-plane deformations of compressed samples that could favor the production of defects in closer proximity to others.

  3. Formation Energies of Native Point Defects in Strained-Layer Superlattices (Postprint)

    Science.gov (United States)

    2017-06-05

    potential; bulk materials; total energy calculations; entropy; strained- layer superlattice (SLS) 16. SECURITY CLASSIFICATION OF: 17. LIMITATION OF...AFRL-RX-WP-JA-2017-0217 FORMATION ENERGIES OF NATIVE POINT DEFECTS IN STRAINED- LAYER SUPERLATTICES (POSTPRINT) Zhi-Gang Yu...2016 Interim 11 September 2013 – 5 November 2016 4. TITLE AND SUBTITLE FORMATION ENERGIES OF NATIVE POINT DEFECTS IN STRAINED- LAYER SUPERLATTICES

  4. Strain effects on point defects and chain-oxygen order-disorder transition in 123 cuprate compounds

    International Nuclear Information System (INIS)

    Su Haibin; Welch, David O.; Wong-Ng, Winnie

    2004-01-01

    The energetics of Schottky defects in 123 cuprate superconductor series RBa 2 Cu 3 O 7 (where R=lanthandies) and YA 2 Cu 3 O 7 (A=alkali earths), were found to have unusual relations if one considers only the volumetric strain. Our calculations reveal the effect of nonuniform changes of interatomic distances within the R-123 structures, introduced by doping homovalent elements, on the Schottky defect formation energy. The energy of formation of Frenkel pair defects, which is an elementary disordering event, in 123 compounds can be substantially altered under both stress and chemical doping. Scaling the oxygen-oxygen short-range repulsive parameter using the calculated formation energy of Frenkel pair defects, the transition temperature between orthorhombic and tetragonal phases is computed by quasichemical approximations (QCA's). The theoretical results illustrate the same trend as the experimental measurements in that the larger the ionic radius of R, the lower the orthorhombic/tetragonal phase transition temperature. This study provides strong evidence of the strain effects on order-disorder transition due to oxygens in the CuO chain sites

  5. Stress and Strain State Analysis of Defective Pipeline Portion

    Science.gov (United States)

    Burkov, P. V.; Burkova, S. P.; Knaub, S. A.

    2015-09-01

    The paper presents computer simulation results of the pipeline having defects in a welded joint. Autodesk Inventor software is used for simulation of the stress and strain state of the pipeline. Places of the possible failure and stress concentrators are predicted on the defective portion of the pipeline.

  6. Strain modulated defect luminescence in ZnO nanostructures grown on Si substrates

    Energy Technology Data Exchange (ETDEWEB)

    Chen, Hung-Ing; Hsiao, Jui-Ju; Huang, Yi-Jen; Wang, Jen-Cheng [Graduate Institute of Electro-Optical Engineering and Department of Electronic Engineering, Chang Gung University, 259 Wen-Hwa 1st Road, Kwei-Shan, Tao-Yuan 333, Taiwan, ROC (China); Wu, Ya-Fen [Department of Electronic Engineering, Ming Chi University of Technology, Taishan, New Taipei 243, Taiwan, ROC (China); Lu, Bing-Yuh [Department of Electrical Engineering, Tun Gnan University, Shenkeng, New Taipei 222, Taiwan, ROC (China); Nee, Tzer-En, E-mail: neete@mail.cgu.edu.tw [Graduate Institute of Electro-Optical Engineering and Department of Electronic Engineering, Chang Gung University, 259 Wen-Hwa 1st Road, Kwei-Shan, Tao-Yuan 333, Taiwan, ROC (China)

    2015-12-15

    The strain modulated defect green luminescence from ZnO nanostructures grown on silicon substrates has been investigated in-depth. According to the Warren–Averbach Fourier analysis of the X-ray diffraction profiles, both the internal strain and the average crystallite size of the well-ordered nano-size ZnO nanostructures could be subtly modulated by careful adjustment of the aqueous solution of zinc nitrate (Zn(NO{sub 3}){sub 2}) and ammonium hydroxide (NH{sub 3}OH) used in the hydrothermal treatment. Visible defect-related and ultraviolet band-to-band emissions were characterized using temperature-dependent photoluminescence measurements over a broad temperature range from 20 to 300 K. It was found that the thermal-related tensile strain led to the blueshift of the green emission with increasing temperature, while the violet and ultraviolet emissions were thermally insensitive. These spectral observations were substantially corroborated by the deformation potential theory. - Highlights: • The strain modulated defect green luminescence from ZnO nanostructures. • Visible and ultraviolet emissions were characterized using photoluminescence. • The tensile strain led to the blueshift of the green emission. • The spectral observations were corroborated by the deformation potential theory.

  7. Channeling techniques to study strains and defects in heterostructures and multi quantum wells

    Science.gov (United States)

    Pathak, A. P.; Dhamodaran, S.; Sathish, N.

    2005-08-01

    The importance and advantages of heterostructures and Quantum Wells (QWs) in device technology has made research challenging due to lack of direct techniques for their characterization. Particularly the characterization of strain and defects at the interfaces has become important due to their dominance in the electrical and optical properties of materials and devices. RBSiC has been used to study variety of defects in single crystalline materials, for nearly four decades now. Channeling based experiments play a crucial role in giving depth information of strain and defects. Ion beams are used for both material characterizations as well as for modifications. Hence it is also possible to monitor the modifications online, which are discussed in detail. In the present work, Swift Heavy Ion (SHI) modification of III-V semiconductor heterostnictures and MQWs and the results of subsequent strain measurements by RBSiC in initially strained as well as lattice matched systems are discussed. We find that the compressive strain decreases due to SHI irradiation and a tensile strain is induced in an initially lattice matched system. The incident ion fluence dependence of strain modifications in the heterostructures will also be discussed. The use of high energy channeling for better sensitivity of strain measurements in low mismatch materials will be discussed in detail. Wherever possible, a comparison of results with those obtained by other techniques like HRXRD is given.

  8. MD simulations to evaluate effects of applied tensile strain on irradiation-induced defect production at various PKA energies

    International Nuclear Information System (INIS)

    Miyashiro, S.; Fujita, S.; Okita, T.; Okuda, H.

    2012-01-01

    Highlights: ► Strain effects on defect formation were evaluated at various PKA energies by MD. ► Radiation-induced defects were increased numerically by external strain. ► Enhanced formation of larger clusters causes the numerical increase of defects. ► Strain influence on the number of defects was greatest at about 20 keV PKA. ► Cluster size, which is mostly affected by strain, was greater with higher PKA energy. - Abstract: Molecular Dynamics (MD) simulations were conducted to investigate the influence of applied tensile strain on defect production during cascade damages at various Primary Knock-on Atom (PKA) energies of 1–30 keV. When 1% strain was applied, the number of surviving defects increased at PKA energies higher than 5 keV, although they did not increase at 1 keV. The rate of increase by strain application was higher with higher PKA energy, and attained the maximum at 20 keV PKA energy with a subsequent gradual decrease at 30 keV PKA energy The cluster size, mostly affected by strain, was larger with higher PKA energy, although clusters with fewer than seven interstitials did not increase in number at any PKA energy.

  9. Strain and defect microstructure in ion-irradiated GeSi/Si strained layers as a function of annealing temperature

    International Nuclear Information System (INIS)

    Glasko, J.M.; Elliman, R.G.; Zou, J.; Cockayne, D.J.H.; Fitz Gerald, J.D.

    1998-01-01

    High energy (1 MeV), ion irradiation of GeSi/Si strained layers at elevated temperatures can cause strain relaxation. In this study, the effect of subsequent thermal annealing was investigated. Three distinct annealing stages were identified and correlated with the evolution of the defect microstructure. In the temperature range from 350 to 600 deg C, a gradual recovery of strain is observed. This is believed to result from the annealing of small defect clusters and the growth of voids. The voids are visible at annealing temperatures in excess of 600 deg C, consistent with an excess vacancy concentration in the irradiated alloy layer. The 600 to 750 deg C range is marked by pronounced maximal recovery of strain, and is correlated with the dissolution of faulted loops in the substrate. At temperatures in the range 750-1000 deg C, strain relaxation is observed and is correlated with the growth of intrinsic dislocations within the alloy layer. These dislocations nucleate at the alloy-substrate interface and grow within the alloy layer, towards the surface. (authors)

  10. Nonlinear elastic longitudinal strain-wave propagation in a plate with nonequilibrium laser-generated point defects

    International Nuclear Information System (INIS)

    Mirzade, Fikret Kh.

    2005-01-01

    The propagation of longitudinal strain wave in a plate with quadratic nonlinearity of elastic continuum was studied in the context of a model that takes into account the joint dynamics of elastic displacements in the medium and the concentration of the nonequilibrium laser-induced point defects. The input equations of the problem are reformulated in terms of only the total displacements of the medium points. In this case, the presence of structural defects manifests itself in the emergence of a delayed response of the system to the propagation of the strain-related perturbations, which is characteristic of media with relaxation or memory. The model equations describing the nonlinear displacement wave were derived with allowance made for the values of the relaxation parameter. The influence of the generation and relaxation of lattice defects on the propagation of this wave was analyzed. It is shown that, for short relaxation times of defects, the strain can propagate in the form of shock fronts. In the case of longer relaxation times, shock waves do not form and the strain wave propagates only in the form of solitary waves or a train of solitons. The contributions of the finiteness of the defect-recombination rate to linear and nonlinear elastic modulus, and spatial dispersion are determined

  11. Accessible switching of electronic defect type in SrTi O3 via biaxial strain

    Science.gov (United States)

    Chi, Yen-Ting; Youssef, Mostafa; Sun, Lixin; Van Vliet, Krystyn J.; Yildiz, Bilge

    2018-05-01

    Elastic strain is used widely to alter the mobility of free electronic carriers in semiconductors, but a predictive relationship between elastic lattice strain and the extent of charge localization of electronic defects is still underdeveloped. Here we considered SrTi O3 , a prototypical perovskite as a model functional oxide for thin film electronic devices and nonvolatile memories. We assessed the effects of biaxial strain on the stability of electronic defects at finite temperature by combining density functional theory (DFT) and quasiharmonic approximation (QHA) calculations. We constructed a predominance diagram for free electrons and small electron polarons in this material, as a function of biaxial strain and temperature. We found that biaxial tensile strain in SrTi O3 can stabilize the small polaron, leading to a thermally activated and slower electronic transport, consistent with prior experimental observations on SrTi O3 and distinct from our prior theoretical assessment of the response of SrTi O3 to hydrostatic stress. These findings also resolved apparent conflicts between prior atomistic simulations and conductivity experiments for biaxially strained SrTi O3 thin films. Our computational approach can be extended to other functional oxides, and for the case of SrTi O3 our findings provide concrete guidance for conditions under which strain engineering can shift the electronic defect type and concentration to modulate electronic transport in thin films.

  12. Hydrogen embrittlement of austenitic stainless steels revealed by deformation microstructures and strain-induced creation of vacancies

    International Nuclear Information System (INIS)

    Hatano, M.; Fujinami, M.; Arai, K.; Fujii, H.; Nagumo, M.

    2014-01-01

    Hydrogen embrittlement of austenitic stainless steels has been examined with respect to deformation microstructures and lattice defects created during plastic deformation. Two types of austenitic stainless steels, SUS 304 and SUS 316L, uniformly hydrogen-precharged to 30 mass ppm in a high-pressure hydrogen environment, are subjected to tensile straining at room temperature. A substantial reduction of tensile ductility appears in hydrogen-charged SUS 304 and the onset of fracture is likely due to plastic instability. Fractographic features show involvement of plasticity throughout the crack path, implying the degradation of the austenitic phase. Electron backscatter diffraction analyses revealed prominent strain localization enhanced by hydrogen in SUS 304. Deformation microstructures of hydrogen-charged SUS 304 were characterized by the formation of high densities of fine stacking faults and ε-martensite, while tangled dislocations prevailed in SUS 316L. Positron lifetime measurements have revealed for the first time hydrogen-enhanced creation of strain-induced vacancies rather than dislocations in the austenitic phase and more clustering of vacancies in SUS 304 than in SUS 316L. Embrittlement and its mechanism are ascribed to the decrease in stacking fault energies resulting in strain localization and hydrogen-enhanced creation of strain-induced vacancies, leading to premature fracture in a similar way to that proposed for ferritic steels

  13. Defects/strain influenced magnetic properties and inverse of surface spin canting effect in single domain CoFe_2O_4 nanoparticles

    International Nuclear Information System (INIS)

    Singh, Simrjit; Khare, Neeraj

    2016-01-01

    Graphical abstract: - Highlights: • Synthesized single domain CoFe_2O_4 nanoparticles with different amount of strain. • Demonstrated a correlation between size, strain and magnetic properties of CoFe_2O_4. • Strain induces cationic redistribution at tetrahedral and octahedral sites of CoFe_2O_4. • Inverse of spin canting effect due to the redistribution of Fe"3"+ ions is demonstrated. - Abstract: Single domain CoFe_2O_4 nanoparticles with different amount of defects/strain have been synthesized by varying the growth temperature in the hydrothermal method. Nanoparticles grown at lower temperature are of larger size and exhibit more planar defects and oxygen vacancies as compared to nanoparticles grown at higher temperatures which are of smaller sizes and exhibit less planar defects and oxygen vacancies. The nanoparticles with larger amount of defects also possess a higher value of intrinsic strain as compared to nanoparticles with fewer defects. The presence of intrinsic strain in the nanoparticles is found to shift the cationic distribution at the tetrahedral and octahedral sites. The saturation magnetization (M_s) of the nanoparticles is found to depend upon both the intrinsic strain and size of the nanoparticles. The M_s increases with the decrease in the nanoparticles size from 32 nm to 20 nm, and this is correlated to the inverse of spin canting effect due to decrease in the intrinsic strain which leads to shifting of Co"2"+ ions from tetrahedral to octahedral sites. However, with further decrease in the size of the nanoparticles (16 nm), the size effect dominates over the strain effect leading to decrease in M_s. The coercivity is found to be higher in the nanoparticles with larger amount of defects/strain and has been attributed to strain induced strong spin canting and pinning due to defect sites. The variation of coercivity with particle size (D) exhibits deviation from D"3"/"2 dependence for the nanoparticles with larger amount of strain/defects.

  14. Structure and strain relaxation effects of defects in InxGa1−xN epilayers

    International Nuclear Information System (INIS)

    Rhode, S. L.; Fu, W. Y.; Massabuau, F. C.-P.; Kappers, M. J.; McAleese, C.; Oehler, F.; Humphreys, C. J.; Sahonta, S.-L.; Moram, M. A.; Dusane, R. O.

    2014-01-01

    The formation of trench defects is observed in 160 nm-thick In x Ga 1−x N epilayers with x ≤ 0.20, grown on GaN on (0001) sapphire substrates using metalorganic vapour phase epitaxy. The trench defect density increases with increasing indium content, and high resolution transmission electron microscopy shows an identical structure to those observed previously in InGaN quantum wells, comprising meandering stacking mismatch boundaries connected to an I 1 -type basal plane stacking fault. These defects do not appear to relieve in-plane compressive strain. Other horizontal sub-interface defects are also observed within the GaN pseudosubstrate layer of these samples and are found to be pre-existing threading dislocations which form half-loops by bending into the basal plane, and not basal plane stacking faults, as previously reported by other groups. The origins of these defects are discussed and are likely to originate from a combination of the small in-plane misorientation of the sapphire substrate and the thermal mismatch strain between the GaN and InGaN layers grown at different temperatures.

  15. Ab initio study of native defects in SnO under strain

    KAUST Repository

    Bianchi Granato, Danilo

    2014-04-01

    Tin monoxide (SnO) has promising properties to be applied as a p-type semiconductor in transparent electronics. To this end, it is necessary to understand the behaviour of defects in order to control them. We use density functional theory to study native defects of SnO under tensile and compressive strain. We show that Sn vacancies are less stable under tension and more stable under compression, irrespectively of the charge state. In contrast, O vacancies behave differently for different charge states. It turns out that the most stable defect under compression is the +1 charged O vacancy in an Sn-rich environment and the charge neutral O interstitial in an O-rich environment. Therefore, compression can be used to transform SnO from a p-type into either an n-type or an undoped semiconductor. Copyright © EPLA, 2014.

  16. Evolution of microstructural defects with strain effects in germanium nanocrystals synthesized at different annealing temperatures

    Energy Technology Data Exchange (ETDEWEB)

    Zhang, Minghuan; Cai, Rongsheng; Zhang, Yujuan; Wang, Chao [The Cultivation Base for State Key Laboratory, Qingdao University, No. 308, Ningxia Road, Qingdao 266071 (China); College of Chemistry and Chemical Engineering, Qingdao University, No. 308, Ningxia Road, Qingdao 266071 (China); Wang, Yiqian, E-mail: yqwang@qdu.edu.cn [The Cultivation Base for State Key Laboratory, Qingdao University, No. 308, Ningxia Road, Qingdao 266071 (China); College of Physics Science, Qingdao University, No. 308, Ningxia Road, Qingdao 266071 (China); Ross, Guy G.; Barba, David [INRS-EMT, 1650 Boulevard Lionel-Boulet, Varennes, Quebec J3X 1S2 (Canada)

    2014-07-01

    Ge nanocrystals (Ge-ncs) were produced by implantation of {sup 74}Ge{sup +} into a SiO{sub 2} film on (100) Si, followed by high-temperature annealing from 700 °C to 1100 °C. Transmission electron microscopy (TEM) studies show that the average size of Ge-ncs increases with the annealing temperature. High-resolution TEM (HRTEM) investigations reveal the presence of planar and linear defects in the formed Ge-ncs, whose relative concentrations are determined at each annealing temperature. The relative concentration of planar defects is almost independent of the annealing temperature up to 1000 °C. However, from 1000 °C to 1100 °C, its concentration decreases dramatically. For the linear defects, their concentration varies considerably with the annealing temperatures. In addition, by measuring the interplanar spacing of Ge-ncs from the HRTEM images, a strong correlation is found between the dislocation percentage and the stress field intensity. Our results provide fundamental insights regarding both the presence of microstructural defects and the origin of the residual stress field within Ge-ncs, which can shed light on the fabrication of Ge-ncs with quantified crystallinity and appropriate size for the advanced Ge-nc devices. - Highlights: • Growth of Ge nanocrystals at different annealing temperatures was investigated. • Strain field has great effects on the formation of dislocations. • Different mechanisms are proposed to explain growth regimes of Ge nanocrystals.

  17. Influence of defects and nanoscale strain on the photovoltaic properties of CdS/CdSe nanocomposite co-sensitized ZnO nanowire solar cells

    International Nuclear Information System (INIS)

    Jung, Kyungeun; Lee, Jeongwon; Kim, Young-Min; Kim, Joosun; Kim, Choong-Un; Lee, Man-Jong

    2016-01-01

    Highlights: • CdSe/CdS nanocomposites were coated on ZnO nanowires using solution processes. • In situ CdSe/CdS co-sensitizers resulted in a 3-fold increase in efficiency. • Nano-strain analyses at interfaces and CdS layers were performed. • Drastic decrease of nano-strain in CdSe/CdS was observed. • Relaxed nano-strain was attributed to the increase of efficiency. - Abstract: This paper reports the mechanism of the power conversion efficiency (PCE) improvement in the ZnO nanowires (NW) based solar cells by using CdS/CdSe nanocomposite sensitizers instead of a single CdS quantum-dot (QD) sensitization layer. Two cells with the different type of the sensitization layers were essentially consists of the high-density ZnO nanowire (NW) and a sensitization layer of either CdS-QD or CdS/CdSe nanocomposite, which were produced by an in-situ sequential assembly process of both ionic layer absorption and reaction (SILAR) and chemical bath deposition (CBD). Measurement on the PCE revealed that the cell with CdS/CdSe nanocomposite showed a three-fold increase in PCE compared to the one with a CdS-QD layer. While such improvement in PCE appeared to be consistent with the step-wise band alignment mechanism suggested for the type-II heterojunction of CdSe/CdS/ZnO structures, our microstructural analysis of the cell structure yielded results strongly indicating that the reduction of both interface defects and misfit strain in the CdS lattices plays an additional role on the PCE improvement. Analyses on the interface and the CdS crystallinity using high-resolution electron microscopy (HRTEM) combined with the geometric phase analysis (GPA) revealed that the addition of CdSe effectively reduced the lattice strain in the CdS without introducing misfit dislocations at CdS/CdSe interface, probably owing to Se anion diffusion (or exchange) to the defective SILAR CdS layer during the CBD process. Although an entire enhancement in PCE by the addition of CdSe layer seen in our

  18. Evaluation of crystallographic strain, rotation and defects in functional oxides by the moiré effect in scanning transmission electron microscopy

    Science.gov (United States)

    Naden, A. B.; O'Shea, K. J.; MacLaren, D. A.

    2018-04-01

    Moiré patterns in scanning transmission electron microscopy (STEM) images of epitaxial perovskite oxides are used to assess strain and defect densities over fields of view extending over several hundred nanometers. The patterns arise from the geometric overlap of the rastered STEM electron beam and the samples’ crystal periodicities and we explore the emergence and application of these moiré fringes for rapid strain analysis. Using the epitaxial functional oxide perovskites BiFeO3 and Pr1-x Ca x MnO3, we discuss the impact of large degrees of strain on the quantification of STEM moiré patterns, identify defects in the fringe patterns and quantify strain and lattice rotation. Such a wide-area analysis of crystallographic strain and defects is crucial for developing structure-function relations of functional oxides and we find the STEM moiré technique to be an attractive means of structural assessment that can be readily applied to low dose studies of damage sensitive crystalline materials.

  19. Structure defects in malachite revealed by positron annihilation

    International Nuclear Information System (INIS)

    Geffroy, B.; Diallo, I.; Paulin, R.

    1984-01-01

    Positron lifetime is measured between 77 and 400 K in two malachite samples with different mineralogical structures. The complex spectrum found in zoned malachite reveals a microporosity which remains stable in this range of temperature. Besides, above 200 K, equilibrium defects appear. Their formation energy is estimated to be Esub(f) = 0.27 +- 0.02 eV [fr

  20. Structure defects in malachite revealed by positron annihilation

    Energy Technology Data Exchange (ETDEWEB)

    Geffroy, B; Diallo, I; Paulin, R [Institut National des Sciences et Techniques Nucleaires, CEN/Saclay, 91 - Gif-sur-Yvette (France)

    1984-01-01

    Positron lifetime is measured between 77 and 400 K in two malachite samples with different mineralogical structures. The complex spectrum found in zoned malachite reveals a microporosity which remains stable in this range of temperature. Besides, above 200 K, equilibrium defects appear. Their formation energy is estimated to be Esub(f) = 0.27 +- 0.02 eV.

  1. Tailoring the strain in Si nano-structures for defect-free epitaxial Ge over growth.

    Science.gov (United States)

    Zaumseil, P; Yamamoto, Y; Schubert, M A; Capellini, G; Skibitzki, O; Zoellner, M H; Schroeder, T

    2015-09-04

    We investigate the structural properties and strain state of Ge nano-structures selectively grown on Si pillars of about 60 nm diameter with different SiGe buffer layers. A matrix of TEOS SiO2 surrounding the Si nano-pillars causes a tensile strain in the top part at the growth temperature of the buffer that reduces the misfit and supports defect-free initial growth. Elastic relaxation plays the dominant role in the further increase of the buffer thickness and subsequent Ge deposition. This method leads to Ge nanostructures on Si that are free from misfit dislocations and other structural defects, which is not the case for direct Ge deposition on these pillar structures. The Ge content of the SiGe buffer is thereby not a critical parameter; it may vary over a relatively wide range.

  2. Structure and strain relaxation effects of defects in In{sub x}Ga{sub 1–x}N epilayers

    Energy Technology Data Exchange (ETDEWEB)

    Rhode, S. L., E-mail: sr583@cam.ac.uk; Fu, W. Y.; Massabuau, F. C.-P.; Kappers, M. J.; McAleese, C.; Oehler, F.; Humphreys, C. J.; Sahonta, S.-L. [Department of Materials Science and Metallurgy, University of Cambridge, Charles Babbage Road, Cambridge CB3 0FS (United Kingdom); Moram, M. A. [Department of Materials Science and Metallurgy, University of Cambridge, Charles Babbage Road, Cambridge CB3 0FS (United Kingdom); Department of Materials, Imperial College London, Exhibition Road, London SW7 2AZ (United Kingdom); Dusane, R. O. [Department of Metallurgical Engineering and Materials Science, Indian Institute of Technology Bombay, Mumbai 400076 (India)

    2014-09-14

    The formation of trench defects is observed in 160 nm-thick In{sub x}Ga{sub 1–x}N epilayers with x≤0.20, grown on GaN on (0001) sapphire substrates using metalorganic vapour phase epitaxy. The trench defect density increases with increasing indium content, and high resolution transmission electron microscopy shows an identical structure to those observed previously in InGaN quantum wells, comprising meandering stacking mismatch boundaries connected to an I₁-type basal plane stacking fault. These defects do not appear to relieve in-plane compressive strain. Other horizontal sub-interface defects are also observed within the GaN pseudosubstrate layer of these samples and are found to be pre-existing threading dislocations which form half-loops by bending into the basal plane, and not basal plane stacking faults, as previously reported by other groups. The origins of these defects are discussed and are likely to originate from a combination of the small in-plane misorientation of the sapphire substrate and the thermal mismatch strain between the GaN and InGaN layers grown at different temperatures.

  3. Strained interface defects in silicon nanocrystals

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Benjamin G.; Stradins, Paul [National Center for Photovoltaics, National Renewable Energy Laboratory, Golden, CO (United States); Hiller, Daniel; Zacharias, Margit [IMTEK - Faculty of Engineering, Albert-Ludwigs-University Freiburg (Germany); Luo, Jun-Wei; Beard, Matthew C. [Chemical and Materials Science, National Renewable Energy Laboratory, Golden, CO (United States); Semonin, Octavi E. [Chemical and Materials Science, National Renewable Energy Laboratory, Golden, CO (United States); Department of Physics, University of Colorado, Boulder, CO (United States)

    2012-08-07

    The surface of silicon nanocrystals embedded in an oxide matrix can contain numerous interface defects. These defects strongly affect the nanocrystals' photoluminescence efficiency and optical absorption. Dangling-bond defects are nearly eliminated by H{sub 2} passivation, thus decreasing absorption below the quantum-confined bandgap and enhancing PL efficiency by an order of magnitude. However, there remain numerous other defects seen in absorption by photothermal deflection spectroscopy; these defects cause non-radiative recombination that limits the PL efficiency to <15%. Using atomistic pseudopotential simulations, we attribute these defects to two specific types of distorted bonds: Si-Si and bridging Si-O-Si bonds between two Si atoms at the nanocrystal surface. (Copyright copyright 2012 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  4. Genetic variation in the Staphylococcus aureus 8325 strain lineage revealed by whole-genome sequencing.

    Directory of Open Access Journals (Sweden)

    Kristoffer T Bæk

    Full Text Available Staphylococcus aureus strains of the 8325 lineage, especially 8325-4 and derivatives lacking prophage, have been used extensively for decades of research. We report herein the results of our deep sequence analysis of strain 8325-4. Assignment of sequence variants compared with the reference strain 8325 (NRS77/PS47 required correction of errors in the 8325 reference genome, and reassessment of variation previously attributed to chemical mutagenesis of the restriction-defective RN4220. Using an extensive strain pedigree analysis, we discovered that 8325-4 contains 16 single nucleotide polymorphisms (SNP arising prior to the construction of RN4220. We identified 5 indels in 8325-4 compared with 8325. Three indels correspond to expected Φ11, 12, 13 excisions, one indel is explained by a sequence assembly artifact, and the final indel (Δ63bp in the spa-sarS intergenic region is common to only a sub-lineage of 8325-4 strains including SH1000. This deletion was found to significantly decrease (75% steady state sarS but not spa transcript levels in post-exponential phase. The sub-lineage 8325-4 was also found to harbor 4 additional SNPs. We also found large sequence variation between 8325, 8325-4 and RN4220 in a cluster of repetitive hypothetical proteins (SA0282 homologs near the Ess secretion cluster. The overall 8325-4 SNP set results in 17 alterations within coding sequences. Remarkably, we discovered that all tested strains of the 8325-4 lineage lack phenol soluble modulin α3 (PSMα3, a virulence determinant implicated in neutrophil chemotaxis, biofilm architecture and surface spreading. Collectively, our results clarify and define the 8325-4 pedigree and reveal clear evidence that mutations existing throughout all branches of this lineage, including the widely used RN6390 and SH1000 strains, could conceivably impact virulence regulation.

  5. Characterization of plastic strains and crystallographic properties surrounding defects in steam generator tubes by orientation imaging microscopy

    International Nuclear Information System (INIS)

    Lehockey, E.M.; Brennenstuhl, A.M.

    2002-01-01

    Orientation Imaging Microscopy (OIM) has become a valuable technique for characterizing grain boundary structure, texture, and grain size distribution, which govern material susceptibility to degenerative effects (e.g. IGSCC). Methods recently developed, by Kinectrics, have extended OIM capabilities toward mapping and quantifying residual plastic strains in materials. OIM is applied in the present work to characterize the distribution of plastic strains, that accumulate in CANDU steam generator tubing during installation and service potentially undermining the performance, reliability, and fitness-for-service of these components. Plastic strain that evolves in response to roller-expansion was characterized in simulated roll joints constructed from Alloy 600 tubing. Results underscore the effect of over-rolling in generating intense gradients with broad variations in strain that extend significant distances through the wall thickness. Of greater relevance is the orientation of these gradients in the transverse direction, relative to the tube axis and potential for the development of abnormal grain growth during post-expansion heat treatments. The magnitude and distribution of strain measured by OIM are remarkably consistent with Finite Element Analysis (FEA) predictions offering compelling evidence as to the reliability of the OIM technique. OIM offers superior resolution than can be practically achieved with FEA having particular relevance in identifying highly localized concentrations of strain surrounding metallurgical defects that can serve as precursors to stress-related degenerative effects (e.g. IGSCC). The spatial distribution of residual plastic strain was also characterized within the context of localized texture, and grain size morphology surrounding (OD) 'pits' and indentations found in ex-service Monel 400 and Alloy 800 SG tubes, respectively. An absence of strain surrounding these surface defects suggests their propensity for promoting more deleterious

  6. Relaxation of a strained 3C-SiC(1 1 1) thin film on silicon by He+ and O+ ion beam defect engineering

    International Nuclear Information System (INIS)

    Häberlen, M.; Murphy, B.; Stritzker, B.; Lindner, J.K.N.

    2012-01-01

    In this paper we report on the successful reduction of tensile strain in a thin strained ion-beam synthesized 3C-SiC(1 1 1) layer on silicon. The creation of a near-interface defect structure consisting of nanometric voids and stacking fault type defects by He ion implantation and subsequent annealing yields significant relaxation in the top SiC film. The microstructure of the defect layer is studied by transmission electron microscopy, and the strain state of the 3C-SiC layer was studied by high-resolution X-ray diffraction in a parallel beam configuration. Typical process conditions for the growth of GaN films on the SiC layer were emulated by high temperature treatments in a rapid thermal annealer or a quartz tube furnace. It is found that prolonged annealing at high temperatures leads to ripening of the voids and to a weaker reduction of the tensile strain. It is shown that this problem can be overcome by the co-implantation of oxygen ions to form highly thermally stable void/extended defect structures.

  7. Study of low-defect and strain-relaxed GeSn growth via reduced pressure CVD in H2 and N2 carrier gas

    Science.gov (United States)

    Margetis, J.; Mosleh, A.; Al-Kabi, S.; Ghetmiri, S. A.; Du, W.; Dou, W.; Benamara, M.; Li, B.; Mortazavi, M.; Naseem, H. A.; Yu, S.-Q.; Tolle, J.

    2017-04-01

    High quality, thick (up to 1.1 μm), strain relaxed GeSn alloys were grown on Ge-buffered Si (1 0 0) in an ASM Epsilon® chemical vapor deposition system using SnCl4 and low-cost commercial GeH4 precursors. The significance of surface chemistry in regards to growth rate and Sn-incorporation is discussed by comparing growth kinetics data in H2 and N2 carrier gas. The role of carrier gas is also explored in the suppression of Sn surface segregation and evolution of layer composition and strain profiles via secondary ion mass spectrometry and X-ray diffraction. Transmission electron microscopy revealed the spontaneous compositional splitting and formation of a thin intermediate layer in which dislocations are pinned. This intermediate layer enables the growth of a thick, strain relaxed, and defect-free epitaxial layer on its top. Last, we present photoluminescence results which indicate that both N2 and H2 growth methods produce optoelectronic device quality material.

  8. Atomic defects and doping of monolayer NbSe2

    OpenAIRE

    Nguyen, Lan; Komsa, Hannu-Pekka; Khestanova, Ekaterina; Kashtiban, Reza J; Peters, Jonathan J.P.; Lawlor, Sean; Sanchez, Ana M.; Sloan, Jeremy; Gorbachev, Roman; Grigorieva, Irina; Krasheninnikov, Arkady V.; Haigh, Sarah

    2017-01-01

    We have investigated the structure of atomic defects within monolayer NbSe2 encapsulated in graphene by combining atomic resolution transmission electron microscope imaging, density functional theory (DFT) calculations, and strain mapping using geometric phase analysis. We demonstrate the presence of stable Nb and Se monovacancies in monolayer material and reveal that Se monovacancies are the most frequently observed defects, consistent with DFT calculations of their formation energy. We reve...

  9. Effects of ambroxol on biofilm adhesion and viability of Pseudomonas aeruginosa quorum sensing defective strain

    Directory of Open Access Journals (Sweden)

    Qi LU

    2013-07-01

    Full Text Available Objective To investigate the effects of ambroxol on the biofilm viability and pristine adhesion of Pseudomonas aeruginosa wild (PAO1 and quorum sensing defective strain (QS, gene deletion of ∆lasI and ∆rhlI. Methods The biofilm was treated by different concentrations (0, 1.875, 3.75mg/ml of ambroxol. The number of colony was measured with agar plate, multifunction fluorometer was used to measure the fluorescence intensity of PAO1 and QS strains at the bottom of 96-well plate. The adhesion ratio (% was calculated to determine the effects of ambroxol on bacterial biofilm adhesion. Results Ambroxol treatment reduced the survival rate of the mutant strains compared to that of wild strain, even though the QS strain had increased the adhesion in the presence of ambroxol compared to that of wild strain (P<0.05. Conclusion Ambroxol has a property of significantly antagonizing quorum-sensing system, suggesting that it might be of importance in treatment against chronic Pseudomonasaeruginosainfections.

  10. A loss-of-function mutation in the PAS kinase Rim15p is related to defective quiescence entry and high fermentation rates of Saccharomyces cerevisiae sake yeast strains.

    Science.gov (United States)

    Watanabe, Daisuke; Araki, Yuya; Zhou, Yan; Maeya, Naoki; Akao, Takeshi; Shimoi, Hitoshi

    2012-06-01

    Sake yeast cells have defective entry into the quiescent state, allowing them to sustain high fermentation rates. To reveal the underlying mechanism, we investigated the PAS kinase Rim15p, which orchestrates initiation of the quiescence program in Saccharomyces cerevisiae. We found that Rim15p is truncated at the carboxyl terminus in modern sake yeast strains as a result of a frameshift mutation. Introduction of this mutation or deletion of the full-length RIM15 gene in a laboratory strain led to a defective stress response, decreased synthesis of the storage carbohydrates trehalose and glycogen, and impaired G(1) arrest, which together closely resemble the characteristic phenotypes of sake yeast. Notably, expression of a functional RIM15 gene in a modern sake strain suppressed all of these phenotypes, demonstrating that dysfunction of Rim15p prevents sake yeast cells from entering quiescence. Moreover, loss of Rim15p or its downstream targets Igo1p and Igo2p remarkably improved the fermentation rate in a laboratory strain. This finding verified that Rim15p-mediated entry into quiescence plays pivotal roles in the inhibition of ethanol fermentation. Taken together, our results suggest that the loss-of-function mutation in the RIM15 gene may be the key genetic determinant of the increased ethanol production rates in modern sake yeast strains.

  11. The Role of Hydrogen-Enhanced Strain-Induced Lattice Defects on Hydrogen Embrittlement Susceptibility of X80 Pipeline Steel

    Science.gov (United States)

    Hattori, M.; Suzuki, H.; Seko, Y.; Takai, K.

    2017-08-01

    Studies to date have not completely determined the factors influencing hydrogen embrittlement of ferrite/bainite X80 pipeline steel. Hydrogen embrittlement susceptibility was evaluated based on fracture strain in tensile testing. We conducted a thermal desorption analysis to measure the amount of tracer hydrogen corresponding to that of lattice defects. Hydrogen embrittlement susceptibility and the amount of tracer hydrogen significantly increased with decreasing crosshead speed. Additionally, a significant increase in the formation of hydrogen-enhanced strain-induced lattice defects was observed immediately before the final fracture. In contrast to hydrogen-free specimens, the fracture surface of the hydrogen-charged specimens exhibited shallower dimples without nuclei, such as secondary phase particles. These findings indicate that the presence of hydrogen enhanced the formation of lattice defects, particularly just prior to the occurrence of final fracture. This in turn enhanced the formation of shallower dimples, thereby potentially causing premature fracture of X80 pipeline steel at lower crosshead speeds.

  12. Ductile failure analysis of defective API X65 pipes based on stress-modified fracture strain criterion

    International Nuclear Information System (INIS)

    Oh, Chang Kyun; Kim, Yun Jae; Baek, Jong Hyun; Kim, Young Pyo; Kim, Woo Sik

    2006-01-01

    A local failure criterion for the API X65 steel is applied to predict ductile failure of full-scale API X65 pipes with simulated corrosion and gouge defects under internal pressure. The local failure criterion is the stress-modified fracture strain for the API X65 steel as a function of the stress triaxiality (defined by the ratio of the hydrostatic stress to the effective stress). Based on detailed FE analyses with the proposed local failure criteria, burst pressures of defective pipes are estimated and compared with experimental data. The predicted burst pressures are in good agreement with experimental data. Noting that an assessment equation against the gouge defect is not yet available, parametric study is performed, from which a simple equation is proposed to predict burst pressure for API X65 pipes with gouge defects

  13. Vibrio cholerae classical biotype strains reveal distinct signatures in Mexico.

    Science.gov (United States)

    Alam, Munirul; Islam, M Tarequl; Rashed, Shah Manzur; Johura, Fatema-tuz; Bhuiyan, Nurul A; Delgado, Gabriela; Morales, Rosario; Mendez, Jose Luis; Navarro, Armando; Watanabe, Haruo; Hasan, Nur-A; Colwell, Rita R; Cravioto, Alejandro

    2012-07-01

    Vibrio cholerae O1 classical (CL) biotype caused the fifth and sixth pandemics, and probably the earlier cholera pandemics, before the El Tor (ET) biotype initiated the seventh pandemic in Asia in the 1970s by completely displacing the CL biotype. Although the CL biotype was thought to be extinct in Asia and although it had never been reported from Latin America, V. cholerae CL and ET biotypes, including a hybrid ET, were found associated with areas of cholera endemicity in Mexico between 1991 and 1997. In this study, CL biotype strains isolated from areas of cholera endemicity in Mexico between 1983 and 1997 were characterized in terms of major phenotypic and genetic traits and compared with CL biotype strains isolated in Bangladesh between 1962 and 1989. According to sero- and biotyping data, all V. cholerae strains tested had the major phenotypic and genotypic characteristics specific for the CL biotype. Antibiograms revealed the majority of the Bangladeshi strains to be resistant to trimethoprim-sulfamethoxazole, furazolidone, ampicillin, and gentamicin, while the Mexican strains were sensitive to all of these drugs, as well as to ciprofloxacin, erythromycin, and tetracycline. Pulsed-field gel electrophoresis (PFGE) of NotI-digested genomic DNA revealed characteristic banding patterns for all of the CL biotype strains although the Mexican strains differed from the Bangladeshi strains in 1 to 2 DNA bands. The difference was subtle but consistent, as confirmed by the subclustering patterns in the PFGE-based dendrogram, and can serve as a regional signature, suggesting the pre-1991 existence and evolution of the CL biotype strains in the Americas, independent from Asia.

  14. Mechanical properties of highly defective graphene: from brittle rupture to ductile fracture.

    Science.gov (United States)

    Xu, Lanqing; Wei, Ning; Zheng, Yongping

    2013-12-20

    Defects are generally believed to deteriorate the superlative performance of graphene-based devices but may also be useful when carefully engineered to tailor the local properties and achieve new functionalities. Central to most defect-associated applications is the defect coverage and arrangement. In this work, we investigate, by molecular dynamics simulations, the mechanical properties and fracture dynamics of graphene sheets with randomly distributed vacancies or Stone-Wales defects under tensile deformations over a wide defect coverage range. With defects presented, an sp-sp(2) bonding network and an sp-sp(2)-sp(3) bonding network are observed in vacancy-defected and Stone-Wales-defected graphene, respectively. The ultimate strength degrades gradually with increasing defect coverage and saturates in the high-ratio regime, whereas the fracture strain presents an unusual descending-saturating-improving trend. In the dense vacancy defect situation, the fracture becomes more plastic and super-ductility is observed. Further fracture dynamics analysis reveals that the crack trapping by sp-sp(2) and sp-sp(2)-sp(3) rings and the crack-tip blunting account for the ductile fracture, whereas geometric rearrangement on the entire sheet for vacancy defects and geometric rearrangement on the specific defect sites for Stone-Wales defects account for their distinctive rules of the evolution of the fracture strain.

  15. Atomic Defects and Doping of Monolayer NbSe2.

    Science.gov (United States)

    Nguyen, Lan; Komsa, Hannu-Pekka; Khestanova, Ekaterina; Kashtiban, Reza J; Peters, Jonathan J P; Lawlor, Sean; Sanchez, Ana M; Sloan, Jeremy; Gorbachev, Roman V; Grigorieva, Irina V; Krasheninnikov, Arkady V; Haigh, Sarah J

    2017-03-28

    We have investigated the structure of atomic defects within monolayer NbSe 2 encapsulated in graphene by combining atomic resolution transmission electron microscope imaging, density functional theory (DFT) calculations, and strain mapping using geometric phase analysis. We demonstrate the presence of stable Nb and Se monovacancies in monolayer material and reveal that Se monovacancies are the most frequently observed defects, consistent with DFT calculations of their formation energy. We reveal that adventitious impurities of C, N, and O can substitute into the NbSe 2 lattice stabilizing Se divacancies. We further observe evidence of Pt substitution into both Se and Nb vacancy sites. This knowledge of the character and relative frequency of different atomic defects provides the potential to better understand and control the unusual electronic and magnetic properties of this exciting two-dimensional material.

  16. Length-scale and strain rate-dependent mechanism of defect formation and fracture in carbon nanotubes under tensile loading

    Energy Technology Data Exchange (ETDEWEB)

    Javvaji, Brahmanandam [Indian Institute of Science, Department of Aerospace Engineering (India); Raha, S. [Indian Institute of Science, Department of Computational and Data Sciences (India); Mahapatra, D. Roy, E-mail: droymahapatra@aero.iisc.ernet.in [Indian Institute of Science, Department of Aerospace Engineering (India)

    2017-02-15

    Electromagnetic and thermo-mechanical forces play a major role in nanotube-based materials and devices. Under high-energy electron transport or high current densities, carbon nanotubes fail via sequential fracture. The failure sequence is governed by certain length scale and flow of current. We report a unified phenomenological model derived from molecular dynamic simulation data, which successfully captures the important physics of the complex failure process. Length-scale and strain rate-dependent defect nucleation, growth, and fracture in single-walled carbon nanotubes with diameters in the range of 0.47 to 2.03 nm and length which is about 6.17 to 26.45 nm are simulated. Nanotubes with long length and small diameter show brittle fracture, while those with short length and large diameter show transition from ductile to brittle fracture. In short nanotubes with small diameters, we observe several structural transitions like Stone-Wales defect initiation, its propagation to larger void nucleation, formation of multiple chains of atoms, conversion to monatomic chain of atoms, and finally complete fracture of the carbon nanotube. Hybridization state of carbon-carbon bonds near the end cap evolves, leading to the formation of monatomic chain in short nanotubes with small diameter. Transition from ductile to brittle fracture is also observed when strain rate exceeds a critical value. A generalized analytical model of failure is established, which correlates the defect energy during the formation of atomic chain with aspect ratio of the nanotube and strain rate. Variation in the mechanical properties such as elastic modulus, tensile strength, and fracture strain with the size and strain rate shows important implications in mitigating force fields and ways to enhance the life of electronic devices and nanomaterial conversion via fracture in manufacturing.

  17. Mechanical properties of highly defective graphene: from brittle rupture to ductile fracture

    International Nuclear Information System (INIS)

    Xu, Lanqing; Wei, Ning; Zheng, Yongping

    2013-01-01

    Defects are generally believed to deteriorate the superlative performance of graphene-based devices but may also be useful when carefully engineered to tailor the local properties and achieve new functionalities. Central to most defect-associated applications is the defect coverage and arrangement. In this work, we investigate, by molecular dynamics simulations, the mechanical properties and fracture dynamics of graphene sheets with randomly distributed vacancies or Stone–Wales defects under tensile deformations over a wide defect coverage range. With defects presented, an sp–sp 2 bonding network and an sp–sp 2 –sp 3 bonding network are observed in vacancy-defected and Stone–Wales-defected graphene, respectively. The ultimate strength degrades gradually with increasing defect coverage and saturates in the high-ratio regime, whereas the fracture strain presents an unusual descending–saturating–improving trend. In the dense vacancy defect situation, the fracture becomes more plastic and super-ductility is observed. Further fracture dynamics analysis reveals that the crack trapping by sp–sp 2 and sp–sp 2 –sp 3 rings and the crack-tip blunting account for the ductile fracture, whereas geometric rearrangement on the entire sheet for vacancy defects and geometric rearrangement on the specific defect sites for Stone–Wales defects account for their distinctive rules of the evolution of the fracture strain. (paper)

  18. Revealing origin of quasi-one dimensional current transport in defect rich two dimensional materials

    DEFF Research Database (Denmark)

    Lotz, Mikkel Rønne; Boll, Mads; Hansen, Ole

    2014-01-01

    to a non-uniform current flow characteristic of lower dimensionality. In this work, simulations based on a finite element method together with a Monte Carlo approach are used to establish the transition from 2D to quasi-1D current transport, when applying a micro four-point probe to measure on 2D...... conductors with an increasing amount of line-shaped defects. Clear 2D and 1D signatures are observed at low and high defect densities, respectively, and current density plots reveal the presence of current channels or branches in defect configurations yielding 1D current transport. A strong correlation...

  19. Observation of silicon self-diffusion enhanced by the strain originated from end-of-range defects using isotope multilayers

    Energy Technology Data Exchange (ETDEWEB)

    Isoda, Taiga; Uematsu, Masashi; Itoh, Kohei M., E-mail: kitoh@appi.keio.ac.jp [School of Fundamental Science and Technology, Keio University, 3-14-1 Hiyoshi, Kohoku-ku, Yokohama 223-8522 (Japan)

    2015-09-21

    Si self-diffusion in the presence of end-of-range (EOR) defects is investigated using {sup nat}Si/{sup 28}Si isotope multilayers. The isotope multilayers were amorphized by Ge ion implantation, and then annealed at 800–950 °C. The behavior of Si self-interstitials is investigated through the {sup 30}Si self-diffusion. The experimental {sup 30}Si profiles show further enhancement of Si self-diffusion at the EOR defect region, in addition to the transient enhanced diffusion via excess Si self-interstitials by EOR defects. To explain this additional enhanced diffusion, we propose a model which takes into account enhanced diffusion by tensile strain originated from EOR defects. The calculation results based on this model have well reproduced the experimental {sup 30}Si profiles.

  20. Great Disparity in Photoluminesence Quantum Yields of Colloidal CsPbBr3 Nanocrystals with Varied Shape: The Effect of Crystal Lattice Strain.

    Science.gov (United States)

    Zhao, Jiangtao; Liu, Mei; Fang, Li; Jiang, Shenlong; Zhou, Jingtian; Ding, Huaiyi; Huang, Hongwen; Wen, Wen; Luo, Zhenlin; Zhang, Qun; Wang, Xiaoping; Gao, Chen

    2017-07-06

    Understanding the big discrepancy in the photoluminesence quantum yields (PLQYs) of nanoscale colloidal materials with varied morphologies is of great significance to its property optimization and functional application. Using different shaped CsPbBr 3 nanocrystals with the same fabrication processes as model, quantitative synchrotron radiation X-ray diffraction analysis reveals the increasing trend in lattice strain values of the nanocrystals: nanocube, nanoplate, nanowire. Furthermore, transient spectroscopic measurements reveal the same trend in the defect quantities of these nanocrystals. These experimental results unambiguously point out that large lattice strain existing in CsPbBr 3 nanoparticles induces more crystal defects and thus decreases the PLQY, implying that lattice strain is a key factor other than the surface defect to dominate the PLQY of colloidal photoluminesence materials.

  1. Dependence of hydrogen-induced lattice defects and hydrogen embrittlement of cold-drawn pearlitic steels on hydrogen trap state, temperature, strain rate and hydrogen content

    International Nuclear Information System (INIS)

    Doshida, Tomoki; Takai, Kenichi

    2014-01-01

    The effects of the hydrogen state, temperature, strain rate and hydrogen content on hydrogen embrittlement susceptibility and hydrogen-induced lattice defects were evaluated for cold-drawn pearlitic steel that absorbed hydrogen in two trapping states. Firstly, tensile tests were carried out under various conditions to evaluate hydrogen embrittlement susceptibility. The results showed that peak 2 hydrogen, desorbed at temperatures above 200 °C as determined by thermal desorption analysis (TDA), had no significant effect on hydrogen embrittlement susceptibility. In contrast, hydrogen embrittlement susceptibility increased in the presence of peak 1 hydrogen, desorbed from room temperature to 200 °C as determined by TDA, at temperatures higher than −30 °C, at lower strain rates and with higher hydrogen content. Next, the same effects on hydrogen-induced lattice defects were also evaluated by TDA using hydrogen as a probe. Peak 2 hydrogen showed no significant effect on either hydrogen-induced lattice defects or hydrogen embrittlement susceptibility. It was found that hydrogen-induced lattice defects formed under the conditions where hydrogen embrittlement susceptibility increased. This relationship indicates that hydrogen embrittlement susceptibility was higher under the conditions where the formation of hydrogen-induced lattice defects tended to be enhanced. Since hydrogen-induced lattice defects formed by the interaction between hydrogen and strain were annihilated by annealing at a temperature of 200 °C, they were presumably vacancies or vacancy clusters. One of the common atomic-level changes that occur in cold-drawn pearlitic steel showing higher hydrogen embrittlement susceptibility is the formation of vacancies and vacancy clusters

  2. Thermal buckling behavior of defective CNTs under pre-load: A molecular dynamics study.

    Science.gov (United States)

    Mehralian, Fahimeh; Tadi Beni, Yaghoub; Kiani, Yaser

    2017-05-01

    Current study is concentrated on the extraordinary properties of defective carbon nanotubes (CNTs). The role of vacancy defects in thermal buckling response of precompressed CNTs is explored via molecular dynamics (MD) simulations. Defective CNTs are initially compressed at a certain ratio of their critical buckling strain and then undergo a uniform temperature rise. Comprehensive study is implemented on both armchair and zigzag CNTs with different vacancy defects including monovacancy, symmetric bivacancy and asymmetric bivacancy. The results reveal that defects have a pronounced impact on the buckling behavior of CNTs; interestingly, defective CNTs under compressive pre-load show higher resistance to thermal buckling than pristine ones. In the following, the buckling response of defective CNTs is shown to be dependent on the vacancy defects, location of defects and chirality. Copyright © 2017 Elsevier Inc. All rights reserved.

  3. High-resolution spatiotemporal strain mapping reveals non-uniform deformation in micropatterned elastomers

    Science.gov (United States)

    Aksoy, B.; Rehman, A.; Bayraktar, H.; Alaca, B. E.

    2017-04-01

    Micropatterns are generated on a vast selection of polymeric substrates for various applications ranging from stretchable electronics to cellular mechanobiological systems. When these patterned substrates are exposed to external loading, strain field is primarily affected by the presence of microfabricated structures and similarly by fabrication-related defects. The capturing of such nonhomogeneous strain fields is of utmost importance in cases where study of the mechanical behavior with a high spatial resolution is necessary. Image-based non-contact strain measurement techniques are favorable and have recently been extended to scanning tunneling microscope and scanning electron microscope images for the characterization of mechanical properties of metallic materials, e.g. steel and aluminum, at the microscale. A similar real-time analysis of strain heterogeneity in elastomers is yet to be achieved during the entire loading sequence. The available measurement methods for polymeric materials mostly depend on cross-head displacement or precalibrated strain values. Thus, they suffer either from the lack of any real-time analysis, spatiotemporal distribution or high resolution in addition to a combination of these factors. In this work, these challenges are addressed by integrating a tensile stretcher with an inverted optical microscope and developing a subpixel particle tracking algorithm. As a proof of concept, the patterns with a critical dimension of 200 µm are generated on polydimethylsiloxane substrates and strain distribution in the vicinity of the patterns is captured with a high spatiotemporal resolution. In the field of strain measurement, there is always a tradeoff between minimum measurable strain value and spatial resolution. Current noncontact techniques on elastomers can deliver a strain resolution of 0.001% over a minimum length of 5 cm. More importantly, inhomogeneities within this quite large region cannot be captured. The proposed technique can

  4. High-resolution spatiotemporal strain mapping reveals non-uniform deformation in micropatterned elastomers

    International Nuclear Information System (INIS)

    Aksoy, B; Alaca, B E; Rehman, A; Bayraktar, H

    2017-01-01

    Micropatterns are generated on a vast selection of polymeric substrates for various applications ranging from stretchable electronics to cellular mechanobiological systems. When these patterned substrates are exposed to external loading, strain field is primarily affected by the presence of microfabricated structures and similarly by fabrication-related defects. The capturing of such nonhomogeneous strain fields is of utmost importance in cases where study of the mechanical behavior with a high spatial resolution is necessary. Image-based non-contact strain measurement techniques are favorable and have recently been extended to scanning tunneling microscope and scanning electron microscope images for the characterization of mechanical properties of metallic materials, e.g. steel and aluminum, at the microscale. A similar real-time analysis of strain heterogeneity in elastomers is yet to be achieved during the entire loading sequence. The available measurement methods for polymeric materials mostly depend on cross-head displacement or precalibrated strain values. Thus, they suffer either from the lack of any real-time analysis, spatiotemporal distribution or high resolution in addition to a combination of these factors. In this work, these challenges are addressed by integrating a tensile stretcher with an inverted optical microscope and developing a subpixel particle tracking algorithm. As a proof of concept, the patterns with a critical dimension of 200 µ m are generated on polydimethylsiloxane substrates and strain distribution in the vicinity of the patterns is captured with a high spatiotemporal resolution. In the field of strain measurement, there is always a tradeoff between minimum measurable strain value and spatial resolution. Current noncontact techniques on elastomers can deliver a strain resolution of 0.001% over a minimum length of 5 cm. More importantly, inhomogeneities within this quite large region cannot be captured. The proposed technique can

  5. Revealing origin of quasi-one dimensional current transport in defect rich two dimensional materials

    International Nuclear Information System (INIS)

    Lotz, Mikkel R.; Boll, Mads; Bøggild, Peter; Petersen, Dirch H.; Hansen, Ole; Kjær, Daniel

    2014-01-01

    The presence of defects in graphene have for a long time been recognized as a bottleneck for its utilization in electronic and mechanical devices. We recently showed that micro four-point probes may be used to evaluate if a graphene film is truly 2D or if defects in proximity of the probe will lead to a non-uniform current flow characteristic of lower dimensionality. In this work, simulations based on a finite element method together with a Monte Carlo approach are used to establish the transition from 2D to quasi-1D current transport, when applying a micro four-point probe to measure on 2D conductors with an increasing amount of line-shaped defects. Clear 2D and 1D signatures are observed at low and high defect densities, respectively, and current density plots reveal the presence of current channels or branches in defect configurations yielding 1D current transport. A strong correlation is found between the density filling factor and the simulation yield, the fraction of cases with 1D transport and the mean sheet conductance. The upper transition limit is shown to agree with the percolation threshold for sticks. Finally, the conductance of a square sample evaluated with macroscopic edge contacts is compared to the micro four-point probe conductance measurements and we find that the micro four-point probe tends to measure a slightly higher conductance in samples containing defects

  6. Methyltransferase-defective avian metapneumovirus vaccines provide complete protection against challenge with the homologous Colorado strain and the heterologous Minnesota strain.

    Science.gov (United States)

    Sun, Jing; Wei, Yongwei; Rauf, Abdul; Zhang, Yu; Ma, Yuanmei; Zhang, Xiaodong; Shilo, Konstantin; Yu, Qingzhong; Saif, Y M; Lu, Xingmeng; Yu, Lian; Li, Jianrong

    2014-11-01

    Avian metapneumovirus (aMPV), also known as avian pneumovirus or turkey rhinotracheitis virus, is the causative agent of turkey rhinotracheitis and is associated with swollen head syndrome in chickens. Since its discovery in the 1970s, aMPV has been recognized as an economically important pathogen in the poultry industry worldwide. The conserved region VI (CR VI) of the large (L) polymerase proteins of paramyxoviruses catalyzes methyltransferase (MTase) activities that typically methylate viral mRNAs at guanine N-7 (G-N-7) and ribose 2'-O positions. In this study, we generated a panel of recombinant aMPV (raMPV) Colorado strains carrying mutations in the S-adenosyl methionine (SAM) binding site in the CR VI of L protein. These recombinant viruses were specifically defective in ribose 2'-O, but not G-N-7 methylation and were genetically stable and highly attenuated in cell culture and viral replication in the upper and lower respiratory tracts of specific-pathogen-free (SPF) young turkeys. Importantly, turkeys vaccinated with these MTase-defective raMPVs triggered a high level of neutralizing antibody and were completely protected from challenge with homologous aMPV Colorado strain and heterologous aMPV Minnesota strain. Collectively, our results indicate (i) that aMPV lacking 2'-O methylation is highly attenuated in vitro and in vivo and (ii) that inhibition of mRNA cap MTase can serve as a novel target to rationally design live attenuated vaccines for aMPV and perhaps other paramyxoviruses. Paramyxoviruses include many economically and agriculturally important viruses such as avian metapneumovirus (aMPV), and Newcastle disease virus (NDV), human pathogens such as human respiratory syncytial virus, human metapneumovirus, human parainfluenza virus type 3, and measles virus, and highly lethal emerging pathogens such as Nipah virus and Hendra virus. For many of them, there is no effective vaccine or antiviral drug. These viruses share common strategies for viral gene

  7. Qualification of a new defect revealing etch for CdTe using cathodoluminescence microscopy

    Energy Technology Data Exchange (ETDEWEB)

    Watson, C.C.R.; Durose, K. (Dept. of Physics, Univ. of Durham (United Kingdom)); Banister, A.J. (Dept. of Chemistry, Univ. of Durham (United Kingdom)); O' Keefe, E.; Bains, S.K. (Philips Infrared Defence Components, Southampton (United Kingdom))

    1993-01-30

    The action of a new defect revealing etch comprising a saturated FeCl[sub 3] solution has been investigated. The etch was found suitable for use on (111)A, (anti 1anti 1anti 1)B and other surface orientations of CdTe, and (111)A and (anti 1anti 1anti 1)B surfaces of Cd[sub 0.96]Zn[sub 0.04] Te. Direct correlations with cathodoluminescence and infra-red microscopy have shown the etch to successfully reveal twin boundaries, precipitates and dislocations. A background etch rate of approximately 2 [mu]m min[sup -1] has been measured. (orig.).

  8. Critical strain region evaluation of self-assembled semiconductor quantum dots

    Energy Technology Data Exchange (ETDEWEB)

    Sales, D L [Departamento de Ciencia de los Materiales e I. M. y Q. I., Universidad de Cadiz, Puerto Real, Cadiz (Spain); Pizarro, J [Departamento de Lenguajes y Sistemas Informaticos, Universidad de Cadiz, Puerto Real, Cadiz (Spain); Galindo, P L [Departamento de Lenguajes y Sistemas Informaticos, Universidad de Cadiz, Puerto Real, Cadiz (Spain); Garcia, R [Departamento de Ciencia de los Materiales e I. M. y Q. I., Universidad de Cadiz, Puerto Real, Cadiz (Spain); Trevisi, G [CNR-IMEM Institute, Parco delle Scienze 37a, 43100, Parma (Italy); Frigeri, P [CNR-IMEM Institute, Parco delle Scienze 37a, 43100, Parma (Italy); Nasi, L [CNR-IMEM Institute, Parco delle Scienze 37a, 43100, Parma (Italy); Franchi, S [CNR-IMEM Institute, Parco delle Scienze 37a, 43100, Parma (Italy); Molina, S I [Departamento de Ciencia de los Materiales e I. M. y Q. I., Universidad de Cadiz, Puerto Real, Cadiz (Spain)

    2007-11-28

    A novel peak finding method to map the strain from high resolution transmission electron micrographs, known as the Peak Pairs method, has been applied to In(Ga)As/AlGaAs quantum dot (QD) samples, which present stacking faults emerging from the QD edges. Moreover, strain distribution has been simulated by the finite element method applying the elastic theory on a 3D QD model. The agreement existing between determined and simulated strain values reveals that these techniques are consistent enough to qualitatively characterize the strain distribution of nanostructured materials. The correct application of both methods allows the localization of critical strain zones in semiconductor QDs, predicting the nucleation of defects, and being a very useful tool for the design of semiconductor devices.

  9. Experimental study of the strain state at the area of a surface defect in a steel cylindrical shell subjected to internal pressure

    OpenAIRE

    Бесчетников, Д. А.

    2014-01-01

    Experimental research of stress-strain state at the area of local volumetric surface defects of the pipeline systems is an important goal because results of the measurements are necessary for increasing of effectiveness of existing repair technologies using fiber reinforcement polymer composite materials. In this work the description of experiment carried out by the author is presented with statement of results. The experiment was devoted to strain gauging of a steel cylindrical shell with vo...

  10. Topological defect clustering and plastic deformation mechanisms in functionalized graphene

    Science.gov (United States)

    Nunes, Ricardo; Araujo, Joice; Chacham, Helio

    2011-03-01

    We present ab initio results suggesting that strain plays a central role in the clustering of topological defects in strained and functionalized graphene models. We apply strain onto the topological-defect graphene networks from our previous work, and obtain topological-defect clustering patterns which are in excellent agreement with recent observations in samples of reduced graphene oxide. In our models, the graphene layer, containing an initial concentration of isolated topological defects, is covered by hydrogen or hydroxyl groups. Our results also suggest a rich variety of plastic deformation mechanism in functionalized graphene systems. We acknowledge support from the Brazilian agencies: CNPq, Fapemig, and INCT-Materiais de Carbono.

  11. Comparative genomics analyses revealed two virulent Listeria monocytogenes strains isolated from ready-to-eat food.

    Science.gov (United States)

    Lim, Shu Yong; Yap, Kien-Pong; Thong, Kwai Lin

    2016-01-01

    Listeria monocytogenes is an important foodborne pathogen that causes considerable morbidity in humans with high mortality rates. In this study, we have sequenced the genomes and performed comparative genomics analyses on two strains, LM115 and LM41, isolated from ready-to-eat food in Malaysia. The genome size of LM115 and LM41 was 2,959,041 and 2,963,111 bp, respectively. These two strains shared approximately 90% homologous genes. Comparative genomics and phylogenomic analyses revealed that LM115 and LM41 were more closely related to the reference strains F2365 and EGD-e, respectively. Our virulence profiling indicated a total of 31 virulence genes shared by both analysed strains. These shared genes included those that encode for internalins and L. monocytogenes pathogenicity island 1 (LIPI-1). Both the Malaysian L. monocytogenes strains also harboured several genes associated with stress tolerance to counter the adverse conditions. Seven antibiotic and efflux pump related genes which may confer resistance against lincomycin, erythromycin, fosfomycin, quinolone, tetracycline, and penicillin, and macrolides were identified in the genomes of both strains. Whole genome sequencing and comparative genomics analyses revealed two virulent L. monocytogenes strains isolated from ready-to-eat foods in Malaysia. The identification of strains with pathogenic, persistent, and antibiotic resistant potentials from minimally processed food warrant close attention from both healthcare and food industry.

  12. Antifungal susceptibility profiles of 1698 yeast reference strains revealing potential emerging human pathogens.

    Directory of Open Access Journals (Sweden)

    Marie Desnos-Ollivier

    Full Text Available New molecular identification techniques and the increased number of patients with various immune defects or underlying conditions lead to the emergence and/or the description of novel species of human and animal fungal opportunistic pathogens. Antifungal susceptibility provides important information for ecological, epidemiological and therapeutic issues. The aim of this study was to assess the potential risk of the various species based on their antifungal drug resistance, keeping in mind the methodological limitations. Antifungal susceptibility profiles to the five classes of antifungal drugs (polyens, azoles, echinocandins, allylamines and antimetabolites were determined for 1698 yeast reference strains belonging to 992 species (634 Ascomycetes and 358 Basidiomycetes. Interestingly, geometric mean minimum inhibitory concentrations (MICs of all antifungal drugs tested were significantly higher for Basidiomycetes compared to Ascomycetes (p<0.001. Twenty four strains belonging to 23 species of which 19 were Basidiomycetes seem to be intrinsically "resistant" to all drugs. Comparison of the antifungal susceptibility profiles of the 4240 clinical isolates and the 315 reference strains belonging to 53 shared species showed similar results. Even in the absence of demonstrated in vitro/in vivo correlation, knowing the in vitro susceptibility to systemic antifungal agents and the putative intrinsic resistance of yeast species present in the environment is important because they could become opportunistic pathogens.

  13. Viral forensic genomics reveals the relatedness of classic herpes simplex virus strains KOS, KOS63, and KOS79.

    Science.gov (United States)

    Bowen, Christopher D; Renner, Daniel W; Shreve, Jacob T; Tafuri, Yolanda; Payne, Kimberly M; Dix, Richard D; Kinchington, Paul R; Gatherer, Derek; Szpara, Moriah L

    2016-05-01

    Herpes simplex virus 1 (HSV-1) is a widespread global pathogen, of which the strain KOS is one of the most extensively studied. Previous sequence studies revealed that KOS does not cluster with other strains of North American geographic origin, but instead clustered with Asian strains. We sequenced a historical isolate of the original KOS strain, called KOS63, along with a separately isolated strain attributed to the same source individual, termed KOS79. Genomic analyses revealed that KOS63 closely resembled other recently sequenced isolates of KOS and was of Asian origin, but that KOS79 was a genetically unrelated strain that clustered in genetic distance analyses with HSV-1 strains of North American/European origin. These data suggest that the human source of KOS63 and KOS79 could have been infected with two genetically unrelated strains of disparate geographic origins. A PCR RFLP test was developed for rapid identification of these strains. Copyright © 2016 Elsevier Inc. All rights reserved.

  14. Fracture of vacancy-defected carbon nanotubes and their embedded nanocomposites

    International Nuclear Information System (INIS)

    Xiao Shaoping; Hou Wenyi

    2006-01-01

    In this paper, we investigate effects of vacancy defects on fracture of carbon nanotubes and carbon nanotube/aluminum composites. Our studies show that even a one-atom vacancy defect can dramatically reduce the failure stresses and strains of carbon nanotubes. Consequently, nanocomposites, in which vacancy-defected nanotubes are embedded, exhibit different characteristics from those in which pristine nanotubes are embedded. It has been found that defected nanotubes with a small volume fraction cannot reinforce but instead weaken nanocomposite materials. Although a large volume fraction of defected nanotubes can slightly increase the failure stresses of nanocomposites, the failure strains of nanocomposites are always decreased

  15. The Ptch1DL mouse: a new model to study lambdoid craniosynostosis and basal cell nevus syndrome associated skeletal defects

    OpenAIRE

    Feng, Weiguo; Choi, Irene; Clouthier, David E.; Niswander, Lee; Williams, Trevor

    2013-01-01

    Mouse models provide valuable opportunities for probing the underlying pathology of human birth defects. Employing an ENU-based screen for recessive mutations affecting craniofacial anatomy we isolated a mouse strain, Dogface-like (DL), with abnormal skull and snout morphology. Examination of the skull indicated that these mice developed craniosynostosis of the lambdoid suture. Further analysis revealed skeletal defects related to the pathology of basal cell nevus syndrome (BCNS) including de...

  16. Observation of defects evolution in electronic materials

    Science.gov (United States)

    Jang, Jung Hun

    Advanced characterization techniques have been used to obtain a better understanding of the microstructure of electronic materials. The structural evolution, especially defects, has been investigated during the film growth and post-growth processes. Obtaining the relation between the defect evolution and growth/post-growth parameters is very important to obtain highly crystalline films. In this work, the growth and post-growth related defects in GaN, ZnO, strained-Si/SiGe films have been studied using several advanced characterization techniques. First of all, the growth of related defects in GaN and p-type ZnO films have been studied. The effect of growth parameters, such as growth temperature, gas flow rate, dopants used during the deposition, on the crystalline quality of the GaN and ZnO layers was investigated by high resolution X-ray diffraction (HRXRD) and transmission electron microscopy (TEM). In GaN films, it was found that the edge and mixed type threading dislocations were the dominant defects so that the only relevant figure of merit (FOM) for the crystalline quality should be the FWHM value of o-RC of the surface perpendicular plane which could be determined by a grazing incidence x-ray diffraction (GIXD) technique as shown in this work. The understanding of the relationship between the defect evolution and growth parameters allowed for the growth of high crystalline GaN films. For ZnO films, it was found that the degree of texture and crystalline quality of P-doped ZnO films decreased with increasing the phosphorus atomic percent. In addition, the result from the x-ray diffraction line profile analysis showed that the 0.5 at % P-doped ZnO film showed much higher microstrain than the 1.0 at % P-doped ZnO film, which indicated that the phosphorus atoms were segregated with increasing P atomic percentage. Finally, post-growth related defects in strained-Si/SiGe films were investigated. Postgrowth processes used in this work included high temperature N2

  17. The interaction of H2O with strained uranium metal surfaces

    International Nuclear Information System (INIS)

    Tiferet, E.; Mintz, M. H.; Zalkind, S.; Jacob, I.; Shamir, N.

    2014-01-01

    The interaction of water vapor was studied on uranium metal surfaces, with various degrees of strain (relieved by different degrees of heating). The main features of dissociation, adsorption and initial oxidation for the studied surfaces will be presented. Common to all strained surfaces, on the metal surface a full dissociation occurs, while after oxidation only on most of them the water dissociation is full and on one of them, it is only partial. The oxygen dissociation product adsorbs (with sticking coefficient decreasing with strain relief), forming clusters, for all strains, while the hydrogen product clusters only on the strain relieved and recrystallized surface. The most interesting phenomenon, revealed for these surfaces, is the inhibition of hydrogen adsorption by traces of water vapor , changing from 10% for the mostly strained (defected) surface down to 1% for the strain relieved one. The suggested mechanism for this inhibition will be discussed

  18. Influence of elastic strain on the thermodynamics and kinetics of lithium vacancy in bulk LiCoO2

    Science.gov (United States)

    Moradabadi, Ashkan; Kaghazchi, Payam; Rohrer, Jochen; Albe, Karsten

    2018-01-01

    The influence of elastic strain on the lithium vacancy formation and migration in bulk LiCoO2 is evaluated by means of first-principles calculations within density functional theory (DFT). Strain dependent energies are determined directly from defective cells and also within linear elasticity theory from the elastic dipole tensor (Gi j) for ground state and saddle point configurations. We analyze finite size effects in the calculation of Gi j, compare the predictions of the linear elastic model with those obtained from direct calculations of defective cells under strain, and discuss the differences. Based on our data, we calculate the variations in vacancy concentration and mobility due to the presence of external strain in bulk LiCoO2 cathodes. Our results reveal that elastic in-plane and out-of-plane strains can significantly change the ionic conductivity of bulk LiCoO2 by up to several orders of magnitude and thus strongly affect the performance of Li-secondary batteries.

  19. The effect of ion-beam induced strain on the nucleation density of chemical vapour deposited diamond

    International Nuclear Information System (INIS)

    Weiser, P.S.; Prawer, S.; Nugent, K.W.; Bettiol, A.A.; Kostidis, L.I.; Jamieson, D.N.

    1995-01-01

    The effect of ion implantation on the nucleation of CVD diamond on silicon and diamond substrates has been investigated. The strategy employed is to create laterally confined regions of strain in the substrates by focused MeV implantation of light ions. Raman Microscopy has been employed to obtain spatially resolved maps of the strain in these implanted regions. On diamond substrates a homo-epitaxial CVD diamond film was grown on top of both the implanted and unimplanted regions of the substrate. Raman analysis of the film grown on top of the implanted region revealed it to be under slightly tensile strain as compared to that grown on the unimplanted diamond substrate. The film deposited on the implanted portion of the diamond showed a lower fluorescence background; indicating a lower concentration of incorporated defects. These results suggest that the strain and defects in the diamond substrate material have an important influence on the quality of the homo-epitaxially grown diamond films. 6 refs., 5 figs

  20. Molecular dynamics simulations of irradiation cascades in alpha-zirconium under macroscopic strain

    Energy Technology Data Exchange (ETDEWEB)

    Di, Sali [Department of Mechanical and Materials Engineering, Queen’s University, Kingston, ON, Canada K7L 3N6 (Canada); Yao, Zhongwen, E-mail: yaoz@me.queensu.ca [Department of Mechanical and Materials Engineering, Queen’s University, Kingston, ON, Canada K7L 3N6 (Canada); Daymond, Mark R. [Department of Mechanical and Materials Engineering, Queen’s University, Kingston, ON, Canada K7L 3N6 (Canada); Gao, Fei [Pacific Northwest National Laboratory, Richland, WA 99352 (United States)

    2013-05-15

    Numerous computer simulation studies have been performed on the radiation damage of zirconium. In contrast to most of the work in the literature which has focused on the effects of temperature and recoil energy on defect production and defect clustering, we have developed a computational model to consider the influence of elastic strain field on the formation of defects and their clusters, as strain is commonly present in a real reactor environment. In this work, irradiation induced displacement cascades in alpha-zirconium experiencing a macroscopic strain have been studied by molecular dynamics (MD) simulations using a many-body interatomic potential. The external strain mainly affects the size of defect clusters rather than the total number of defects. The sizes of interstitial and vacancy clusters respond differently to the external strain conditions.

  1. Global mRNA expression analysis in myosin II deficient strains of Saccharomyces cerevisiae reveals an impairment of cell integrity functions

    Directory of Open Access Journals (Sweden)

    Rivera-Molina Félix E

    2008-01-01

    Full Text Available Abstract Background The Saccharomyces cerevisiae MYO1 gene encodes the myosin II heavy chain (Myo1p, a protein required for normal cytokinesis in budding yeast. Myo1p deficiency in yeast (myo1Δ causes a cell separation defect characterized by the formation of attached cells, yet it also causes abnormal budding patterns, formation of enlarged and elongated cells, increased osmotic sensitivity, delocalized chitin deposition, increased chitin synthesis, and hypersensitivity to the chitin synthase III inhibitor Nikkomycin Z. To determine how differential expression of genes is related to these diverse cell wall phenotypes, we analyzed the global mRNA expression profile of myo1Δ strains. Results Global mRNA expression profiles of myo1Δ strains and their corresponding wild type controls were obtained by hybridization to yeast oligonucleotide microarrays. Results for selected genes were confirmed by real time RT-PCR. A total of 547 differentially expressed genes (p ≤ 0.01 were identified with 263 up regulated and 284 down regulated genes in the myo1Δ strains. Gene set enrichment analysis revealed the significant over-representation of genes in the protein biosynthesis and stress response categories. The SLT2/MPK1 gene was up regulated in the microarray, and a myo1Δslt2Δ double mutant was non-viable. Overexpression of ribosomal protein genes RPL30 and RPS31 suppressed the hypersensitivity to Nikkomycin Z and increased the levels of phosphorylated Slt2p in myo1Δ strains. Increased levels of phosphorylated Slt2p were also observed in wild type strains under these conditions. Conclusion Following this analysis of global mRNA expression in yeast myo1Δ strains, we conclude that 547 genes were differentially regulated in myo1Δ strains and that the stress response and protein biosynthesis gene categories were coordinately regulated in this mutant. The SLT2/MPK1 gene was confirmed to be essential for myo1Δ strain viability, supporting that the up

  2. Large-Scale Molecular Simulations on the Mechanical Response and Failure Behavior of a defective Graphene: Cases of 5-8-5 Defects

    Science.gov (United States)

    Wang, Shuaiwei; Yang, Baocheng; Yuan, Jinyun; Si, Yubing; Chen, Houyang

    2015-10-01

    Understanding the effect of defects on mechanical responses and failure behaviors of a graphene membrane is important for its applications. As examples, in this paper, a family of graphene with various 5-8-5 defects are designed and their mechanical responses are investigated by employing molecular dynamics simulations. The dependence of fracture strength and strain as well as Young’s moduli on the nearest neighbor distance and defect types is examined. By introducing the 5-8-5 defects into graphene, the fracture strength and strain become smaller. However, the Young’s moduli of DL (Linear arrangement of repeat unit 5-8-5 defect along zigzag-direction of graphene), DS (a Slope angle between repeat unit 5-8-5 defect and zigzag direction of graphene) and DZ (Zigzag-like 5-8-5 defects) defects in the zigzag direction become larger than those in the pristine graphene in the same direction. A maximum increase of 11.8% of Young’s modulus is obtained. Furthermore, the brittle cracking mechanism is proposed for the graphene with 5-8-5 defects. The present work may provide insights in controlling the mechanical properties by preparing defects in the graphene, and give a full picture for the applications of graphene with defects in flexible electronics and nanodevices.

  3. Elastic interaction energies of defect structures

    International Nuclear Information System (INIS)

    Seitz, E.; de Fontaine, D.

    1976-01-01

    The elastic strain energy between point defects and small disk-shaped clusters of defects are calculated to determine stable configurations. A distortion tensor of tetragonal symmetry is assigned to each impurity atom. The tetragonality ratio t is varied to cover needle-type (t greater than 1), spherical (t = 1) and disk-type (t less than 0) strain fields. To vary the elastic properties of the host material, Fe, Cu, Al, and V were chosen as examples. Computer calculations are based on the microscopic theory of elasticity which emphasizes calculations in discrete Fourier space. Pairs of point defects order along [001] for t less than 1 and along (001) for t = 1 for all host elements. For t greater than 1 fcc lattices and bcc lattices behave differently. It is shown that only certain three dimensional periodic arrangements of parallel and perpendicular disk-like defect clusters are realized for given tetragonality ratio t and host element

  4. Characterization technique for detection of atom-size crystalline defects and strains using two-dimensional fast-Fourier-transform sampling Moiré method

    Science.gov (United States)

    Kodera, Masako; Wang, Qinghua; Ri, Shien; Tsuda, Hiroshi; Yoshioka, Akira; Sugiyama, Toru; Hamamoto, Takeshi; Miyashita, Naoto

    2018-04-01

    Recently, we have developed a two-dimensional (2D) fast-Fourier-transform (FFT) sampling Moiré technique to visually and quantitatively determine the locations of minute defects in a transmission electron microscopy (TEM) image. We applied this technique for defect detection with GaN high electron mobility transistor (HEMT) devices, and successfully and clearly visualized atom-size defects in AlGaN/GaN crystalline structures. The defect density obtained in the AlGaN/GaN structures is ∼1013 counts/cm2. In addition, we have successfully confirmed that the distribution and number of defects closely depend on the process conditions. Thus, this technique is quite useful for a device development. Moreover, the strain fields in an AlGaN/GaN crystal were effectively calculated with nm-scale resolution using this method. We also demonstrated that this sampling Moiré technique is applicable to silicon devices, which have principal directions different from those of AlGaN/GaN crystals. As a result, we believe that the 2D FFT sampling Moiré method has great potential applications to the discovery of new as yet unknown phenomena occurring between the characteristics of a crystalline material and device performance.

  5. Comparative Genomics Revealed Genetic Diversity and Species/Strain-Level Differences in Carbohydrate Metabolism of Three Probiotic Bifidobacterial Species

    Directory of Open Access Journals (Sweden)

    Toshitaka Odamaki

    2015-01-01

    Full Text Available Strains of Bifidobacterium longum, Bifidobacterium breve, and Bifidobacterium animalis are widely used as probiotics in the food industry. Although numerous studies have revealed the properties and functionality of these strains, it is uncertain whether these characteristics are species common or strain specific. To address this issue, we performed a comparative genomic analysis of 49 strains belonging to these three bifidobacterial species to describe their genetic diversity and to evaluate species-level differences. There were 166 common clusters between strains of B. breve and B. longum, whereas there were nine common clusters between strains of B. animalis and B. longum and four common clusters between strains of B. animalis and B. breve. Further analysis focused on carbohydrate metabolism revealed the existence of certain strain-dependent genes, such as those encoding enzymes for host glycan utilisation or certain membrane transporters, and many genes commonly distributed at the species level, as was previously reported in studies with limited strains. As B. longum and B. breve are human-residential bifidobacteria (HRB, whereas B. animalis is a non-HRB species, several of the differences in these species’ gene distributions might be the result of their adaptations to the nutrient environment. This information may aid both in selecting probiotic candidates and in understanding their potential function as probiotics.

  6. Strain amplitude-dependent anelasticity in Cu-Ni solid solution due to thermally activated and athermal dislocation-point obstacle interactions

    Science.gov (United States)

    Kustov, S.; Gremaud, G.; Benoit, W.; Golyandin, S.; Sapozhnikov, K.; Nishino, Y.; Asano, S.

    1999-02-01

    Experimental investigations of the internal friction and the Young's modulus defect in single crystals of Cu-(1.3-7.6) at. % Ni have been performed for 7-300 K over a wide range of oscillatory strain amplitudes. Extensive data have been obtained at a frequency of vibrations around 100 kHz and compared with the results obtained for the same crystals at a frequency of ˜1 kHz. The strain amplitude dependence of the anelastic strain amplitude and the average friction stress acting on a dislocation due to solute atoms are also analyzed. Several stages in the strain amplitude dependence of the internal friction and the Young's modulus defect are revealed for all of the alloy compositions, at different temperatures and in different frequency ranges. For the 100 kHz frequency, low temperatures and low strain amplitudes (˜10-7-10-5), the amplitude-dependent internal friction and the Young's modulus defect are essentially temperature independent, and are ascribed to a purely hysteretic internal friction component. At higher strain amplitudes, a transition stage and a steep strain amplitude dependence of the internal friction and the Young's modulus defect are observed, followed by saturation at the highest strain amplitudes employed. These stages are temperature and frequency dependent and are assumed to be due to thermally activated motion of dislocations. We suggest that the observed regularities in the entire strain amplitude, temperature and frequency ranges correspond to a motion of dislocations in a two-component system of obstacles: weak but long-range ones, due to the elastic interaction of dislocations with solute atoms distributed in the bulk of the crystal; and strong short-range ones, due to the interaction of dislocations with solute atoms distributed close to dislocation glide planes. Based on these assumptions, a qualitative explanation is given for the variety of experimental observations.

  7. Cariogenic properties of Streptococcus mutans clinical isolates with sortase defects.

    Science.gov (United States)

    Lapirattanakul, Jinthana; Takashima, Yukiko; Tantivitayakul, Pornpen; Maudcheingka, Thaniya; Leelataweewud, Pattarawadee; Nakano, Kazuhiko; Matsumoto-Nakano, Michiyo

    2017-09-01

    In Streptococcus mutans, a Gram-positive pathogen of dental caries, several surface proteins are anchored by the activity of sortase enzyme. Although various reports have shown that constructed S. mutans mutants deficient of sortase as well as laboratory reference strains with a sortase gene mutation have low cariogenic potential, no known studies have investigated clinical isolates with sortase defects. Here, we examined the cariogenic properties of S. mutans clinical isolates with sortase defects as well as caries status in humans harboring such defective isolates. Sortase-defective clinical isolates were evaluated for biofilm formation, sucrose-dependent adhesion, stress-induced dextran-dependent aggregation, acid production, and acid tolerance. Additionally, caries indices of subjects possessing such defective isolates were determined. Our in vitro results indicated that biofilm with a lower quantity was formed by sortase-defective as compared to non-defective isolates. Moreover, impairments of sucrose-dependent adhesion and stress-induced dextran-dependent aggregation were found among the isolates with defects, whereas no alterations were seen in regard to acid production or tolerance. Furthermore, glucan-binding protein C, a surface protein anchored by sortase activity, was predominantly detected in culture supernatants of all sortase-defective S. mutans isolates. Although the sortase-defective isolates showed lower cariogenic potential because of a reduction in some cariogenic properties, deft/DMFT indices revealed that all subjects harboring those isolates had caries experience. Our findings suggest the impairment of cariogenic properties in S. mutans clinical isolates with sortase defects, though the detection of these defective isolates seemed not to imply low caries risk in the subjects harboring them. Copyright © 2017 Elsevier Ltd. All rights reserved.

  8. Defects and the optical absorption in nanocrystalline ZnO

    International Nuclear Information System (INIS)

    Dutta, Sreetama; Chattopadhyay, Sanjay; Sutradhar, Manas; Sarkar, Anindya; Chakrabarti, Mahuya; Sanyal, Dirtha; Jana, Debnarayan

    2007-01-01

    The correlation between the structural and optical properties of mechanically milled high purity ZnO powder is reported in the present work. Reduction of average grain size and enhancement of strain as a result of milling have been estimated from the broadening of x-ray powder diffraction patterns. After milling, the optical bandgap, revealed from absorption spectroscopy, has been red-shifted and the width of the localized states, calculated from the analysis of the Urbach tail below the absorption edge, has been extended more and more into the bandgap. Moreover, the band tailing parameter is seen to vary exponentially with the inverse of the grain size. Finally, the positron annihilation technique has been employed to identify the nature of defects present (or generated due to milling) in the system and thereby to correlate the defect mediated modification of optical absorption in ZnO

  9. Defects and the optical absorption in nanocrystalline ZnO

    Energy Technology Data Exchange (ETDEWEB)

    Dutta, Sreetama [Department of Physics, University of Calcutta, 92 Acharya Prafulla Chandra Road, Kolkata 700 009 (India); Chattopadhyay, Sanjay [Department of Physics, Taki Government College, Taki 743429 (India); Sutradhar, Manas [Department of Chemistry, University of Calcutta, 92 Acharya Prafulla Chandra Road, Kolkata 700 009 (India); Sarkar, Anindya [Department of Physics, Bangabasi Morning College, 19 Rajkumar Chakraborty Sarani, Kolkata 700 009 (India); Chakrabarti, Mahuya [Variable Energy Cyclotron Centre, 1/AF, Bidhannagar, Kolkata 700 064 (India); Sanyal, Dirtha [Variable Energy Cyclotron Centre, 1/AF, Bidhannagar, Kolkata 700 064 (India); Jana, Debnarayan [Department of Physics, University of Calcutta, 92 Acharya Prafulla Chandra Road, Kolkata 700 009 (India)

    2007-06-13

    The correlation between the structural and optical properties of mechanically milled high purity ZnO powder is reported in the present work. Reduction of average grain size and enhancement of strain as a result of milling have been estimated from the broadening of x-ray powder diffraction patterns. After milling, the optical bandgap, revealed from absorption spectroscopy, has been red-shifted and the width of the localized states, calculated from the analysis of the Urbach tail below the absorption edge, has been extended more and more into the bandgap. Moreover, the band tailing parameter is seen to vary exponentially with the inverse of the grain size. Finally, the positron annihilation technique has been employed to identify the nature of defects present (or generated due to milling) in the system and thereby to correlate the defect mediated modification of optical absorption in ZnO.

  10. Strain quantification in epitaxial thin films

    International Nuclear Information System (INIS)

    Cushley, M

    2008-01-01

    Strain arising in epitaxial thin films can be beneficial in some cases but devastating in others. By altering the lattice parameters, strain may give a thin film properties hitherto unseen in the bulk material. On the other hand, heavily strained systems are prone to develop lattice defects in order to relieve the strain, which can cause device failure or, at least, a decrease in functionality. Using convergent beam electron diffraction (CBED) and high-resolution transmission electron microscopy (HRTEM), it is possible to determine local strains within a material. By comparing the results from CBED and HRTEM experiments, it is possible to gain a complete view of a material, including the strain and any lattice defects present. As well as looking at how the two experimental techniques differ from each other, I will also look at how results from different image analysis algorithms compare. Strain in Si/SiGe samples and BST/SRO/MgO capacitor structures will be discussed.

  11. Structural defect linked to nonrandom mutations in the matrix gene of Biden strain subacute sclerosing panencephalitis virus defined by cDNA cloning and expression of chimeric genes

    International Nuclear Information System (INIS)

    Ayata, M.; Hirano, A.; Wong, T.C.

    1989-01-01

    Biken strain, a nonproductive measles viruslike agent isolated from a subacute sclerosing panencephalitis (SSPE) patient, contains a posttranscriptional defect affecting matrix (M) protein. A putative M protein was translated in vitro with RNA from Biken strain-infected cells. A similar protein was detected in vivo by an antiserum against a peptide synthesized from the cloned M gene of Edmonston strain measles virus. By using a novel method, full-length cDNAs of the Biken M gene were selectively cloned. The cloned Biken M gene contained an open reading frame which encoded 8 extra carboxy-terminal amino acid residues and 20 amino acid substitutions predicted to affect both the hydrophobicity and secondary structure of the gene product. The cloned gene was expressed in vitro and in vivo into a 37,500 M r protein electrophoretically and antigenically distinct from the M protein of Edmonston strain but identical to the M protein in Biken strain-infected cells. Chimeric M proteins synthesized in vitro and in vivo showed that the mutations in the carboxy-proximal region altered the local antigenicity and those in the amino region affected the overall protein conformation. The protein expressed from the Biken M gene was unstable in vivo. Instability was attributed to multiple mutations. These results offer insights into the basis of the defect in Biken strain and pose intriguing questions about the evolutionary origins of SSPE viruses in general

  12. Effects of various defects on the mechanical properties of black phosphorene

    Science.gov (United States)

    Nguyen, Danh-Truong; Le, Minh-Quy; Nguyen, Van-Trang; Bui, Thanh-Lam

    2017-12-01

    The present work investigates the effects of seven types of defects on the mechanical properties of black phosphorene. Molecular dynamics finite element method with Stillinger-Weber potential is used to simulate the uniaxial tensile tests of the pristine and defective black phosphorene sheets. Young's modulus, fracture stress, and fracture strain of the pristine and defective black phosphorene sheets are estimated. Comparison of the influence of different types of defects on the mechanical response of black phosphorene is considered. Fracture mechanism of various defective black phosphorene sheets is also analyzed. It is found that effect of the defects on Young's modulus of black phosphorene is insignificant. In contrast, due to defects fracture stress and fracture strain can reduce up to 53% and 69%, respectively. Results provide a landscape on the mechanical properties of defective black phosphorene and are useful for the design of nanodevices with black phosphorene in future applications.

  13. Genomic analysis of an attenuated Chlamydia abortus live vaccine strain reveals defects in central metabolism and surface proteins.

    Science.gov (United States)

    Burall, L S; Rodolakis, A; Rekiki, A; Myers, G S A; Bavoil, P M

    2009-09-01

    Comparative genomic analysis of a wild-type strain of the ovine pathogen Chlamydia abortus and its nitrosoguanidine-induced, temperature-sensitive, virulence-attenuated live vaccine derivative identified 22 single nucleotide polymorphisms unique to the mutant, including nine nonsynonymous mutations, one leading to a truncation of pmpG, which encodes a polymorphic membrane protein, and two intergenic mutations potentially affecting promoter sequences. Other nonsynonymous mutations mapped to a pmpG pseudogene and to predicted coding sequences encoding a putative lipoprotein, a sigma-54-dependent response regulator, a PhoH-like protein, a putative export protein, two tRNA synthetases, and a putative serine hydroxymethyltransferase. One of the intergenic mutations putatively affects transcription of two divergent genes encoding pyruvate kinase and a putative SOS response nuclease, respectively. These observations suggest that the temperature-sensitive phenotype and associated virulence attenuation of the vaccine strain result from disrupted metabolic activity due to altered pyruvate kinase expression and/or alteration in the function of one or more membrane proteins, most notably PmpG and a putative lipoprotein.

  14. Mechanical properties and fracture behaviour of defective phosphorene nanotubes under uniaxial tension

    Science.gov (United States)

    Liu, Ping; Pei, Qing-Xiang; Huang, Wei; Zhang, Yong-Wei

    2017-12-01

    The easy formation of vacancy defects and the asymmetry in the two sublayers of phosphorene nanotubes (PNTs) may result in brand new mechanical properties and failure behaviour. Herein, we investigate the mechanical properties and fracture behaviour of defective PNTs under uniaxial tension using molecular dynamics simulations. Our simulation results show that atomic vacancies cause local stress concentration and thus significantly reduce the fracture strength and fracture strain of PNTs. More specifically, a 1% defect concentration is able to reduce the fracture strength and fracture strain by as much as 50% and 66%, respectively. Interestingly, the reduction in the mechanical properties is found to depend on the defect location: a defect located in the outer sublayer has a stronger effect than one located in the inner layer, especially for PNTs with a small diameter. Temperature is also found to strongly influence the mechanical properties of both defect-free and defective PNTs. When the temperature is increased from 0 K to 400 K, the fracture strength and fracture strain of defective PNTs with a defect concentration of 1% are reduced further by 71% and 61%, respectively. These findings are of great importance for the structural design of PNTs as building blocks in nanodevices.

  15. Genetic Diversity among Rhizobium leguminosarum bv. Trifolii Strains Revealed by Allozyme and Restriction Fragment Length Polymorphism Analyses

    Science.gov (United States)

    Demezas, David H.; Reardon, Terry B.; Watson, John M.; Gibson, Alan H.

    1991-01-01

    Allozyme electrophoresis and restriction fragment length polymorphism (RFLP) analyses were used to examine the genetic diversity of a collection of 18 Rhizobium leguminosarum bv. trifolii, 1 R. leguminosarum bv. viciae, and 2 R. meliloti strains. Allozyme analysis at 28 loci revealed 16 electrophoretic types. The mean genetic distance between electrophoretic types of R. leguminosarum and R. meliloti was 0.83. Within R. leguminosarum, the single strain of bv. viciae differed at an average of 0.65 from strains of bv. trifolii, while electrophoretic types of bv. trifolii differed at a range of 0.23 to 0.62. Analysis of RFLPs around two chromosomal DNA probes also delineated 16 unique RFLP patterns and yielded genetic diversity similar to that revealed by the allozyme data. Analysis of RFLPs around three Sym (symbiotic) plasmid-derived probes demonstrated that the Sym plasmids reflect genetic divergence similar to that of their bacterial hosts. The large genetic distances between many strains precluded reliable estimates of their genetic relationships. PMID:16348600

  16. Strength Estimation of Die Cast Beams Considering Equivalent Porous Defects

    Energy Technology Data Exchange (ETDEWEB)

    Park, Moon Shik [Hannam Univ., Daejeon (Korea, Republic of)

    2017-05-15

    As a shop practice, a strength estimation method for die cast parts is suggested, in which various defects such as pores can be allowed. The equivalent porosity is evaluated by combining the stiffness data from a simple elastic test at the part level during the shop practice and the theoretical stiffness data, which are defect free. A porosity equation is derived from Eshelby's inclusion theory. Then, using the Mori-Tanaka method, the porosity value is used to draw a stress-strain curve for the porous material. In this paper, the Hollomon equation is used to capture the strain hardening effect. This stress-strain curve can be used to estimate the strength of a die cast part with porous defects. An elastoplastic theoretical solution is derived for the three-point bending of a die cast beam by using the plastic hinge method as a reference solution for a part with porous defects.

  17. A large ventricular septal defect complicating resuscitation after blunt trauma

    Directory of Open Access Journals (Sweden)

    Henry D I De′Ath

    2012-01-01

    Full Text Available A young adult pedestrian was admitted to hospital after being hit by a car. On arrival to the Accident and Emergency Department, the patient was tachycardic, hypotensive, hypoxic, and acidotic with a Glasgow Coma Scale of 3. Despite initial interventions, the patient remained persistently hypotensive. An echocardiogram demonstrated a traumatic ventricular septal defect (VSD with right ventricular strain and increased pulmonary artery pressure. Following a period of stabilization, open cardiothoracic surgery was performed and revealed an aneurysmal septum with a single large defect. This was repaired with a bovine patch, resulting in normalization of right ventricular function. This case provides a vivid depiction of a large VSD in a patient following blunt chest trauma with hemodynamic compromise. In all thoracic trauma patients, and particularly those poorly responsive to resuscitation, VSDs should be considered. Relevant investigations and management strategies are discussed.

  18. Microscopic View of Defect Evolution in Thermal Treated AlGaInAs Quantum Well Revealed by Spatially Resolved Cathodoluminescence

    Directory of Open Access Journals (Sweden)

    Yue Song

    2018-06-01

    Full Text Available An aluminum gallium indium arsenic (AlGaInAs material system is indispensable as the active layer of diode lasers emitting at 1310 or 1550 nm, which are used in optical fiber communications. However, the course of the high-temperature instability of a quantum well structure, which is closely related to the diffusion of indium atoms, is still not clear due to the system’s complexity. The diffusion process of indium atoms was simulated by thermal treatment, and the changes in the optical and structural properties of an AlGaInAs quantum well are investigated in this paper. Compressive strained Al0.07Ga0.22In0.71As quantum wells were treated at 170 °C with different heat durations. A significant decrement of photoluminescence decay time was observed on the quantum well of a sample that was annealed after 4 h. The microscopic cathodoluminescent (CL spectra of these quantum wells were measured by scanning electron microscope-cathodoluminescence (SEM-CL. The thermal treatment effect on quantum wells was characterized via CL emission peak wavelength and energy density distribution, which were obtained by spatially resolved cathodoluminescence. The defect area was clearly observed in the Al0.07Ga0.22In0.71As quantum wells layer after thermal treatment. CL emissions from the defect core have higher emission energy than those from the defect-free regions. The defect core distribution, which was associated with indium segregation gradient distribution, showed asymmetric character.

  19. Comparative Transcriptome Analysis Reveals Different Silk Yields of Two Silkworm Strains.

    Directory of Open Access Journals (Sweden)

    Juan Li

    Full Text Available Cocoon and silk yields are the most important characteristics of sericulture. However, few studies have examined the genes that modulate these features. Further studies of these genes will be useful for improving the products of sericulture. JingSong (JS and Lan10 (L10 are two strains having significantly different cocoon and silk yields. In the current study, RNA-Seq and quantitative polymerase chain reaction (qPCR were performed on both strains in order to determine divergence of the silk gland, which controls silk biosynthesis in silkworms. Compared with L10, JS had 1375 differentially expressed genes (DEGs; 738 up-regulated genes and 673 down-regulated genes. Nine enriched gene ontology (GO terms were identified by GO enrichment analysis based on these DEGs. KEGG enrichment analysis results showed that the DEGs were enriched in three pathways, which were mainly associated with the processing and biosynthesis of proteins. The representative genes in the enrichment pathways and ten significant DEGs were further verified by qPCR, the results of which were consistent with the RNA-Seq data. Our study has revealed differences in silk glands between the two silkworm strains and provides a perspective for understanding the molecular mechanisms determining silk yield.

  20. Genome-wide study of the defective sucrose fermenter strain of Vibrio cholerae from the Latin American cholera epidemic.

    Directory of Open Access Journals (Sweden)

    Daniel Rios Garza

    Full Text Available The 7th cholera pandemic reached Latin America in 1991, spreading from Peru to virtually all Latin American countries. During the late epidemic period, a strain that failed to ferment sucrose dominated cholera outbreaks in the Northern Brazilian Amazon region. In order to understand the genomic characteristics and the determinants of this altered sucrose fermenting phenotype, the genome of the strain IEC224 was sequenced. This paper reports a broad genomic study of this strain, showing its correlation with the major epidemic lineage. The potentially mobile genomic regions are shown to possess GC content deviation, and harbor the main V. cholera virulence genes. A novel bioinformatic approach was applied in order to identify the putative functions of hypothetical proteins, and was compared with the automatic annotation by RAST. The genome of a large bacteriophage was found to be integrated to the IEC224's alanine aminopeptidase gene. The presence of this phage is shown to be a common characteristic of the El Tor strains from the Latin American epidemic, as well as its putative ancestor from Angola. The defective sucrose fermenting phenotype is shown to be due to a single nucleotide insertion in the V. cholerae sucrose-specific transportation gene. This frame-shift mutation truncated a membrane protein, altering its structural pore-like conformation. Further, the identification of a common bacteriophage reinforces both the monophyletic and African-Origin hypotheses for the main causative agent of the 1991 Latin America cholera epidemics.

  1. Ion channeling study of defects in compound crystals using Monte Carlo simulations

    Science.gov (United States)

    Turos, A.; Jozwik, P.; Nowicki, L.; Sathish, N.

    2014-08-01

    Ion channeling is a well-established technique for determination of structural properties of crystalline materials. Defect depth profiles have been usually determined basing on the two-beam model developed by Bøgh (1968) [1]. As long as the main research interest was focused on single element crystals it was considered as sufficiently accurate. New challenge emerged with growing technological importance of compound single crystals and epitaxial heterostructures. Overlap of partial spectra due to different sublattices and formation of complicated defect structures makes the two beam method hardly applicable. The solution is provided by Monte Carlo computer simulations. Our paper reviews principal aspects of this approach and the recent developments in the McChasy simulation code. The latter made it possible to distinguish between randomly displaced atoms (RDA) and extended defects (dislocations, loops, etc.). Hence, complex defect structures can be characterized by the relative content of these two components. The next refinement of the code consists of detailed parameterization of dislocations and dislocation loops. Defect profiles for variety of compound crystals (GaN, ZnO, SrTiO3) have been measured and evaluated using the McChasy code. Damage accumulation curves for RDA and extended defects revealed non monotonous defect buildup with some characteristic steps. Transition to each stage is governed by the different driving force. As shown by the complementary high resolution XRD measurements lattice strain plays here the crucial role and can be correlated with the concentration of extended defects.

  2. Chinese hamster ovary cell mutants defective in heparan sulfate biosynthesis

    International Nuclear Information System (INIS)

    Bame, K.J.; Kiser, C.S.; Esko, J.D.

    1987-01-01

    The authors have isolated Chinese hamster ovary cell mutants defective in proteoglycan synthesis by radiographic screening for cells unable to incorporate 35 SO 4 into acid-precipitable material. Some mutants did not incorporate 35 SO 4 into acid-precipitable material, whereas others incorporated about 3-fold less radioactivity. HPLC anion exchange chromatographic analysis of radiolabelled glycosaminoglycans isolated from these mutants revealed many are defective in heparan sulfate biosynthesis. Mutants 803 and 677 do not synthesize heparan sulfate, although they produce chondroitin sulfate: strain 803 makes chondroitin sulfate normally, whereas 677 overaccumulates chondroitin sulfate by a factor of three. These mutants fall into the same complementation group, suggesting that the mutations are allelic. A second group of heparan sulfate biosynthetic mutants, consisting of cell lines 625, 668 and 679, produce undersulfated heparan sulfate and normal chondroitin sulfate. Treatment of the chains with nitrous acid should determine the position of the sulfate groups along the chain. These mutants may define a complementation group that is defective in the enzymes which modify the heparan sulfate chain. To increase the authors repertoire of heparan sulfate mutants, they are presently developing an in situ enzyme assay to screen colonies replica plated on filter discs for sulfotransferase defects

  3. Defect dynamics and coarsening dynamics in smectic-C films

    Science.gov (United States)

    Pargellis, A. N.; Finn, P.; Goodby, J. W.; Panizza, P.; Yurke, B.; Cladis, P. E.

    1992-12-01

    We study the dynamics of defects generated in free-standing films of liquid crystals following a thermal quench from the smectic-A phase to the smectic-C phase. The defects are type-1 disclinations, and the strain field between defect pairs is confined to 2π walls. We compare our observations with a phenomenological model that includes dipole coupling of the director field to an external ordering field. This model is able to account for both the observed coalescence dynamics and the observed ordering dynamics. In the absence of an ordering field, our model predicts the defect density ρ to scale with time t as ρ lnρ~t-1. When the dipole coupling of the director field to an external ordering field is included, both the model and experiments show the defect coarsening proceeds as ρ~e-αt with the strain field confined to 2π walls. The external ordering field most likely arises from the director's tendency to align with edge dislocations within the liquid-crystal film.

  4. Anisotropic mechanical properties and Stone-Wales defects in graphene monolayer: A theoretical study

    International Nuclear Information System (INIS)

    Fan, B.B.; Yang, X.B.; Zhang, R.

    2010-01-01

    We investigate the mechanical properties of graphene monolayer via the density functional theoretical (DFT) method. We find that the strain energies are anisotropic for the graphene under large strain. We attribute the anisotropic feature to the anisotropic sp 2 hybridization in the hexagonal lattice. We further identify that the formation energies of Stone-Wales (SW) defects in the graphene monolayer are determined by the defect concentration and also the direction of applied tensile strain, correlating with the anisotropic feature.

  5. Xenon Defects in Uranium Dioxide From First Principles and Interatomic Potentials

    Science.gov (United States)

    Thompson, Alexander

    In this thesis, we examine the defect energetics and migration energies of xenon atoms in uranium dioxide (UO2) from first principles and interatomic potentials. We also parameterize new, accurate interatomic potentials for xenon and uranium dioxide. To achieve accurate energetics and provide a foundation for subsequent calculations, we address difficulties in finding consistent energetics within Hubbard U corrected density functional theory (DFT+U). We propose a method of slowly ramping the U parameter in order to guide the calculation into low energy orbital occupations. We find that this method is successful for a variety of materials. We then examine the defect energetics of several noble gas atoms in UO2 for several different defect sites. We show that the energy to incorporate large noble gas atoms into interstitial sites is so large that it is energetically favorable for a Schottky defect cluster to be created to relieve the strain. We find that, thermodynamically, xenon will rarely ever be in the interstitial site of UO2. To study larger defects associated with the migration of xenon in UO 2, we turn to interatomic potentials. We benchmark several previously published potentials against DFT+U defect energetics and migration barriers. Using a combination of molecular dynamics and nudged elastic band calculations, we find a new, low energy migration pathway for xenon in UO2. We create a new potential for xenon that yields accurate defect energetics. We fit this new potential with a method we call Iterative Potential Refinement that parameterizes potentials to first principles data via a genetic algorithm. The potential finds accurate energetics for defects with relatively low amounts of strain (xenon in defect clusters). It is important to find accurate energetics for these sorts of low-strain defects because they essentially represent small xenon bubbles. Finally, we parameterize a new UO2 potential that simultaneously yields accurate vibrational properties

  6. Comparative genomic analysis of Brucella abortus vaccine strain 104M reveals a set of candidate genes associated with its virulence attenuation.

    Science.gov (United States)

    Yu, Dong; Hui, Yiming; Zai, Xiaodong; Xu, Junjie; Liang, Long; Wang, Bingxiang; Yue, Junjie; Li, Shanhu

    2015-01-01

    The Brucella abortus strain 104M, a spontaneously attenuated strain, has been used as a vaccine strain in humans against brucellosis for 6 decades in China. Despite many studies, the molecular mechanisms that cause the attenuation are still unclear. Here, we determined the whole-genome sequence of 104M and conducted a comprehensive comparative analysis against the whole genome sequences of the virulent strain, A13334, and other reference strains. This analysis revealed a highly similar genome structure between 104M and A13334. The further comparative genomic analysis between 104M and A13334 revealed a set of genes missing in 104M. Some of these genes were identified to be directly or indirectly associated with virulence. Similarly, a set of mutations in the virulence-related genes was also identified, which may be related to virulence alteration. This study provides a set of candidate genes associated with virulence attenuation in B.abortus vaccine strain 104M.

  7. The accuracy of the imaging reformation of cone beam computed tomography for the assessment of bone defect healing

    International Nuclear Information System (INIS)

    Kang, Ho Duk; Kim, Gyu Tae; Choi, Yong Suk; Hwang, Eui Hwan

    2007-01-01

    To evaluate the accuracy of the imaging reformation of cone beam computed tomography for the assessment of bone defect healing in rat model. Sprague-Dawely strain rats weighing about 350 gms were selected. Then critical size bone defects were done at parietal bone with implantation of collagen sponge. The rats were divided into seven groups of 3 days, 1 week, 2 weeks, 3 weeks, 4 weeks, 6 weeks, and 8 weeks. The healing of surgical defect was assessed by multiplanar reconstruction (MPR) images and three-dimensional (3-D) images of cone beam computed tomography, compared with soft X-ray radiograph and histopathologic examination. MPR images and 3-D images showed similar reformation of the healing amount at 3 days, 1 week, 2 weeks, and 8 weeks, however, lower reformation at 3 weeks, 4 weeks, and 6 weeks. According to imaging-based methodologies, MPR images revealed similar reformation of the healing mount than 3-D images compare with soft X-ray image. Among the four threshold values for 3-D images, 400-500 HU revealed similar reformation of the healing amount. Histopathologic examination confirmed the newly formed trabeculation correspond with imaging-based mythologies. MPR images revealed higher accuracy of the imaging reformation of cone beam computed tomography and cone beam computed tomography is a clinically useful diagnostic tool for the assessment of bone defect healing

  8. The Genomic Sequence of the Oral Pathobiont Strain NI1060 Reveals Unique Strategies for Bacterial Competition and Pathogenicity.

    Directory of Open Access Journals (Sweden)

    Youssef Darzi

    Full Text Available Strain NI1060 is an oral bacterium responsible for periodontitis in a murine ligature-induced disease model. To better understand its pathogenicity, we have determined the complete sequence of its 2,553,982 bp genome. Although closely related to Pasteurella pneumotropica, a pneumonia-associated rodent commensal based on its 16S rRNA, the NI1060 genomic content suggests that they are different species thriving on different energy sources via alternative metabolic pathways. Genomic and phylogenetic analyses showed that strain NI1060 is distinct from the genera currently described in the family Pasteurellaceae, and is likely to represent a novel species. In addition, we found putative virulence genes involved in lipooligosaccharide synthesis, adhesins and bacteriotoxic proteins. These genes are potentially important for host adaption and for the induction of dysbiosis through bacterial competition and pathogenicity. Importantly, strain NI1060 strongly stimulates Nod1, an innate immune receptor, but is defective in two peptidoglycan recycling genes due to a frameshift mutation. The in-depth analysis of its genome thus provides critical insights for the development of NI1060 as a prime model system for infectious disease.

  9. Differential lysine acetylation profiles of Erwinia amylovora strains revealed by proteomics

    Science.gov (United States)

    Wu, Xia; Vellaichamy, Adaikkalam; Wang, Dongping; Zamdborg, Leonid; Kelleher, Neil L.; Huber, Steven C.; Zhao, Youfu

    2015-01-01

    Protein lysine acetylation (LysAc) has recently been demonstrated to be widespread in E. coli and Salmonella, and to broadly regulate bacterial physiology and metabolism. However, LysAc in plant pathogenic bacteria is largely unknown. Here we first report the lysine acetylome of Erwinia amylovora, an enterobacterium causing serious fire blight disease of apples and pears. Immunoblots using generic anti-lysine acetylation antibodies demonstrated that growth conditions strongly affected the LysAc profiles in E. amylovora. Differential LysAc profiles were also observed for two E. amylovora strains, known to have differential virulence in plants, indicating translational modification of proteins may be important in determining virulence of bacterial strains. Proteomic analysis of LysAc in two E. amylovora strains identified 141 LysAc sites in 96 proteins that function in a wide range of biological pathways. Consistent with previous reports, 44% of the proteins are involved in metabolic processes, including central metabolism, lipopolysaccharide, nucleotide and amino acid metabolism. Interestingly, for the first time, several proteins involved in E. amylovora virulence, including exopolysaccharide amylovoran biosynthesis- and type III secretion-associated proteins, were found to be lysine acetylated, suggesting that LysAc may play a major role in bacterial virulence. Comparative analysis of LysAc sites in E. amylovora and E. coli further revealed the sequence and structural commonality for LysAc in the two organisms. Collectively, these results reinforce the notion that LysAc of proteins is widespread in bacterial metabolism and virulence. PMID:23234799

  10. SiC substrate defects and III-N heteroepitaxy

    Energy Technology Data Exchange (ETDEWEB)

    Poust, B D [Department of Materials Science and Engineering, University of California, Los Angeles, CA 90095 (United States); Koga, T S [Department of Materials Science and Engineering, University of California, Los Angeles, CA 90095 (United States); Sandhu, R [Department of Materials Science and Engineering, University of California, Los Angeles, CA 90095 (United States); Heying, B [Northrop Grumman Space Technology, Space and Electronics Group, Redondo Beach, CA 90278 (United States); Hsing, R [Northrop Grumman Space Technology, Space and Electronics Group, Redondo Beach, CA 90278 (United States); Wojtowicz, M [Northrop Grumman Space Technology, Space and Electronics Group, Redondo Beach, CA 90278 (United States); Khan, A [Department of Electrical Engineering, University of South Carolina, Columbia, SC (United States); Goorsky, M S [Department of Materials Science and Engineering, University of California, Los Angeles, CA 90095 (United States)

    2003-05-21

    This study addressed how defects in SiC substrates influence the crystallographic properties of AlGaN/GaN layers deposited by metallorganic vapour phase epitaxy and by molecular beam epitaxy. We employed double crystal reflection x-ray topography using symmetric (0008) and (00012) reflections with CuK{alpha} radiation ({lambda} = 1.54 A) to image dislocations, micropipes, and low angle boundaries in SiC substrates. Lattice strain near the core of a micropipe defect was estimated to be of the order of 10{sup -7}. The substrates investigated exhibited radial patterns of strain and, primarily, of tilt of the order of tens of arcsec. After deposition of the AlGaN and GaN layers, DCXRT images were generated from the substrate (0008) or (00012) and GaN epitaxial layer (0004) reflections. Full-width at half-maximum values ranging from {approx}100 to 300 arcsec were typical of the GaN reflections, while those of the 4H-SiC reflections were {approx}20-70 arcsec. Micropipes, tilt boundaries, and inclusions in the SiC were shown to produce structural defects in the GaN layers. A clear correlation between SiC substrate defects and GaN defects has been established.

  11. SiC substrate defects and III-N heteroepitaxy

    International Nuclear Information System (INIS)

    Poust, B D; Koga, T S; Sandhu, R; Heying, B; Hsing, R; Wojtowicz, M; Khan, A; Goorsky, M S

    2003-01-01

    This study addressed how defects in SiC substrates influence the crystallographic properties of AlGaN/GaN layers deposited by metallorganic vapour phase epitaxy and by molecular beam epitaxy. We employed double crystal reflection x-ray topography using symmetric (0008) and (00012) reflections with CuKα radiation (λ = 1.54 A) to image dislocations, micropipes, and low angle boundaries in SiC substrates. Lattice strain near the core of a micropipe defect was estimated to be of the order of 10 -7 . The substrates investigated exhibited radial patterns of strain and, primarily, of tilt of the order of tens of arcsec. After deposition of the AlGaN and GaN layers, DCXRT images were generated from the substrate (0008) or (00012) and GaN epitaxial layer (0004) reflections. Full-width at half-maximum values ranging from ∼100 to 300 arcsec were typical of the GaN reflections, while those of the 4H-SiC reflections were ∼20-70 arcsec. Micropipes, tilt boundaries, and inclusions in the SiC were shown to produce structural defects in the GaN layers. A clear correlation between SiC substrate defects and GaN defects has been established

  12. Strain buildup in GaAs due to 100 MeV Ag ion irradiation

    Energy Technology Data Exchange (ETDEWEB)

    Mishra, Shramana; Bhaumik, Sudipta; Panda, Jaya Kumar [Department of Physics and Meteorology, Indian Institute of Technology, Kharagpur 721 302 (India); Ojha, Sunil [Inter-University Accelerator Center, Aruna Asaf Ali Marg, New Delhi 110 067 (India); Dhar, Achintya [Department of Physics and Meteorology, Indian Institute of Technology, Kharagpur 721 302 (India); Kabiraj, D. [Inter-University Accelerator Center, Aruna Asaf Ali Marg, New Delhi 110 067 (India); Roy, Anushree, E-mail: anushree@phy.iitkgp.ernet.in [Department of Physics and Meteorology, Indian Institute of Technology, Kharagpur 721 302 (India)

    2013-12-01

    The formation of strained layers and a non-monotonic evolution of strain in high energy (100 MeV) silver ion (Ag{sup 7+}) irradiated undoped semi-insulating GaAs are observed and analyzed using Raman scattering and high resolution X-ray diffraction (HRXRD) measurements. At low fluence, compressively strained layers are formed, whereas, with increase in fluence both compressive and tensile strains appear as observed from HRXRD measurements. Further, at low fluence, the change in compressive strain with increase in fluence is found to be sharper than what is observed at higher fluence, thereby suggesting a critical fluence value, beyond which there is a simultaneous generation and annihilation of vacancy type defects. The initial blue shift and subsequent relative red shift beyond above critical fluence in the Raman peak also qualitatively reveal non-monotonic evolution of strain in this case. Finally, we demonstrate the sensitivity of Raman spectroscopy in detecting the decrease in lattice ordering in the crystal in the low fluence regime, below the detection limit of Rutherford back-scattering channeling (c-RBS) measurements.

  13. The genetic basis underlying variation in production of the flavour compound diacetyl by Lactobacillus rhamnosus strains in milk.

    Science.gov (United States)

    Lo, Raquel; Ho, Van Thi Thuy; Bansal, Nidhi; Turner, Mark S

    2018-01-16

    Diacetyl and the closely related compound acetoin impart desirable buttery flavour and odour to many foods including cheese and are generated through the metabolism of citrate by lactic acid bacteria (LAB). To increase the levels of these compounds, adjunct cultures capable of producing them can be added to cheese fermentations. In this study, we compared the diacetyl and acetoin producing abilities of 13 Lactobacillus rhamnosus strains from cheese sources. Diacetyl and acetoin production was found to be a common feature of Lb. rhamnosus grown in milk, with 12 strains producing these compounds. Whole genome sequencing of four strains revealed that genes encoding the citrate metabolising pathway present in other LAB are conserved in Lb. rhamnosus. One strain was, however, totally defective in diacetyl and acetoin production. This was likely due to an inability to produce the diacetyl/acetoin precursor compound acetolactate resulting from a frameshift mutation in the acetolactate synthase (als) gene. Complementation of this defective strain with a complete als gene from a diacetyl producing strain restored production of diacetyl and acetoin to levels equivalent to naturally high producing strains. Introduction of the same als-containing plasmid into the probiotic Lb. rhamnosus strain GG also increased diacetyl and acetoin levels. In model cheesemaking experiments, the als-complemented strain produced very high levels of diacetyl and acetoin over 35days of ripening. These findings identify the genetic basis for natural variation in production of a key cheese flavour compound in Lb. rhamnosus strains. Copyright © 2017 Elsevier B.V. All rights reserved.

  14. Formation Energies of Native Point Defects in Strained layer Superlattices (Postprint)

    Science.gov (United States)

    2017-06-05

    1215 Jefferson Davis Highway, Suite 1204, Arlington, VA 22202-4302. Respondents should be aware that notwithstanding any other provision of law , no...Hamiltonian, tight-binding Hamiltonian, and Green’s function techniques to obtain energy levels arising from native point defects (NPDs) in InAs-GaSb and...GaSb systems and 2 designs of InAs-InAs 0.7 Sb 0.3 systems lattice matched to GaSb substrate. The calculated defect levels not only agree well with

  15. Model of the Evolution of Deformation Defects and Irreversible Strain at Thermal Cycling of Stressed TiNi Alloy Specimen

    Directory of Open Access Journals (Sweden)

    Volkov Aleksandr E.

    2015-01-01

    Full Text Available This microstructural model deals with simulation both of the reversible and irreversible deformation of a shape memory alloy (SMA. The martensitic transformation and the irreversible deformation due to the plastic accommodation of martensite are considered on the microscopic level. The irreversible deformation is described from the standpoint of the plastic flow theory. Isotropic hardening and kinematic hardening are taken into account and are related to the densities of scattered and oriented deformation defects. It is supposed that the phase transformation and the micro plastic deformation are caused by the generalized thermodynamic forces, which are the derivatives of the Gibbs’ potential of the two-phase body. In terms of these forces conditions for the phase transformation and for the micro plastic deformation on the micro level are formulated. The macro deformation of the representative volume of the polycrystal is calculated by averaging of the micro strains related to the evolution of the martensite Bain’s variants in each grain comprising this volume. The proposed model allowed simulating the evolution of the reversible and of the irreversible strains of a stressed SMA specimen under thermal cycles. The results show a good qualitative agreement with available experimental data. Specifically, it is shown that the model can describe a rather big irreversible strain in the first thermocycle and its fast decrease with the number of cycles.

  16. Strain and crystalline defects in epitaxial GaN layers studied by high-resolution X-ray diffraction

    Energy Technology Data Exchange (ETDEWEB)

    Chierchia, Rosa

    2007-07-01

    This thesis treats strain and dislocations in MOVPE GaN layers. The mosaic structure of metalorganic vapour phase epitaxy (MOVPE)-grown GaN layers was studied in dependence on the grain diameter utilizing high-resolution XRD. Different models for the defect structure were analyzed, the edge type TD densities were calculated under the assumption that the dislocations are not randomly distributed but localized at the grain boundaries. Moreover, in situ measurements have shown that the layers are under tension in the c-plane when a nucleation layer is used. The second part of this thesis treats a particular approach to reduce dislocations in MOVPE GaN layers, i.e. maskless pendeo epitaxial growth of MOVPE GAN layers. FE simulations assuming the strain to be completely induced during cooling of the structures after growth agree only partly with experimental data. The strain state of single layers and stripes of GaN grown on SiC was studied to exploit the evolution of the strain in the different phases of the PE growth. The biaxial compressive stress, due to the lattice mismatch between the GaN layer and the AlN nucleation layer is plastically relieved before overgrowth. Temperature dependent measurements show a linear reduction of the wing tilt with increasing temperature varying from sample to sample. Bent TDs have been observed in TEM images of maskless PE samples. Stress induced from the mismatch between the AlN buffer layer and the GaN also contributes to the remaining part of the wing tilt not relieved thermally. It has to be noted that the rest tilt value varies from sample to sample at the growth temperature. In fact some of the data indicate that the wing tilt decreases with increasing V/III ratio. In the last Chapter the application of X-ray techniques for the analysis of strain and composition in layers of inhomogeneous composition is explored. In the first part of the Chapter the strain state and the Al content of AlGaN buffer layers grown directly on (0001

  17. Nomadic lifestyle of Lactobacillus plantarum revealed by comparative genomics of 54 strains isolated from different habitats.

    Science.gov (United States)

    Martino, Maria Elena; Bayjanov, Jumamurat R; Caffrey, Brian E; Wels, Michiel; Joncour, Pauline; Hughes, Sandrine; Gillet, Benjamin; Kleerebezem, Michiel; van Hijum, Sacha A F T; Leulier, François

    2016-12-01

    The ability of bacteria to adapt to diverse environmental conditions is well-known. The process of bacterial adaptation to a niche has been linked to large changes in the genome content, showing that many bacterial genomes reflect the constraints imposed by their habitat. However, some highly versatile bacteria are found in diverse habitats that almost share nothing in common. Lactobacillus plantarum is a lactic acid bacterium that is found in a large variety of habitat. With the aim of unravelling the link between evolution and ecological versatility of L. plantarum, we analysed the genomes of 54 L. plantarum strains isolated from different environments. Comparative genome analysis identified a high level of genomic diversity and plasticity among the strains analysed. Phylogenomic and functional divergence studies coupled with gene-trait matching analyses revealed a mixed distribution of the strains, which was uncoupled from their environmental origin. Our findings revealed the absence of specific genomic signatures marking adaptations of L. plantarum towards the diverse habitats it is associated with. This suggests fundamentally similar trends of genome evolution in L. plantarum, which occur in a manner that is apparently uncoupled from ecological constraint and reflects the nomadic lifestyle of this species. © 2016 The Authors. Environmental Microbiology published by Society for Applied Microbiology and John Wiley & Sons Ltd.

  18. Multiscale crystal defect dynamics: A coarse-grained lattice defect model based on crystal microstructure

    Science.gov (United States)

    Lyu, Dandan; Li, Shaofan

    2017-10-01

    Crystal defects have microstructure, and this microstructure should be related to the microstructure of the original crystal. Hence each type of crystals may have similar defects due to the same failure mechanism originated from the same microstructure, if they are under the same loading conditions. In this work, we propose a multiscale crystal defect dynamics (MCDD) model that models defects by considering its intrinsic microstructure derived from the microstructure or material genome of the original perfect crystal. The main novelties of present work are: (1) the discrete exterior calculus and algebraic topology theory are used to construct a scale-up (coarse-grained) dual lattice model for crystal defects, which may represent all possible defect modes inside a crystal; (2) a higher order Cauchy-Born rule (up to the fourth order) is adopted to construct atomistic-informed constitutive relations for various defect process zones, and (3) an hierarchical strain gradient theory based finite element formulation is developed to support an hierarchical multiscale cohesive (process) zone model for various defects in a unified formulation. The efficiency of MCDD computational algorithm allows us to simulate dynamic defect evolution at large scale while taking into account atomistic interaction. The MCDD model has been validated by comparing of the results of MCDD simulations with that of molecular dynamics (MD) in the cases of nanoindentation and uniaxial tension. Numerical simulations have shown that MCDD model can predict dislocation nucleation induced instability and inelastic deformation, and thus it may provide an alternative solution to study crystal plasticity.

  19. Strain-Dependent Edge Structures in MoS2 Layers.

    Science.gov (United States)

    Tinoco, Miguel; Maduro, Luigi; Masaki, Mukai; Okunishi, Eiji; Conesa-Boj, Sonia

    2017-11-08

    Edge structures are low-dimensional defects unavoidable in layered materials of the transition metal dichalcogenides (TMD) family. Among the various types of such structures, the armchair (AC) and zigzag (ZZ) edge types are the most common. It has been predicted that the presence of intrinsic strain localized along these edges structures can have direct implications for the customization of their electronic properties. However, pinning down the relation between local structure and electronic properties at these edges is challenging. Here, we quantify the local strain field that arises at the edges of MoS 2 flakes by combining aberration-corrected transmission electron microscopy (TEM) with the geometrical-phase analysis (GPA) method. We also provide further insight on the possible effects of such edge strain on the resulting electronic behavior by means of electron energy loss spectroscopy (EELS) measurements. Our results reveal that the two-dominant edge structures, ZZ and AC, induce the formation of different amounts of localized strain fields. We also show that by varying the free edge curvature from concave to convex, compressive strain turns into tensile strain. These results pave the way toward the customization of edge structures in MoS 2 , which can be used to engineer the properties of layered materials and thus contribute to the optimization of the next generation of atomic-scale electronic devices built upon them.

  20. Role of Defects in Swelling and Creep of Irradiated SiC

    Energy Technology Data Exchange (ETDEWEB)

    Szlufarska, Izabela [Univ. of Wisconsin, Madison, WI (United States); Voyles, Paul [Univ. of Wisconsin, Madison, WI (United States); Sridharan, Kumar [Univ. of Wisconsin, Madison, WI (United States); Katoh, Yutai [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)

    2016-01-16

    Silicon carbide is a promising cladding material because of its high strength and relatively good corrosion resistance. However, SiC is brittle and therefore SiC-based components need to be carefully designed to avoid cracking and failure by fracture. In design of SiC-based composites for nuclear reactor applications it is essential to take into account how mechanical properties are affected by radiation and temperature, or in other words, what strains and stresses develop in this material due to environmental conditions. While thermal strains in SiC can be predicted using classical theories, radiation-induced strains are much less understood. In particular, it is critical to correctly account for radiation swelling and radiation creep, which contribute significantly to dimensional instability of SiC under radiation. Swelling typically increases logarithmically with radiation dose and saturates at relatively low doses (damage levels of a few dpa). Consequently, swelling-induced stresses are likely to develop within a few months of operation of a reactor. Radiation-induced volume swelling in SiC can be as high as 2%, which is significantly higher than the cracking strain of 0.1% in SiC. Swelling-induced strains will lead to enormous stresses and fracture, unless these stresses can be relaxed via some other mechanism. An effective way to achieve stress relaxation is via radiation creep. Although it has been hypothesized that both radiation swelling and radiation creep are driven by formation of defect clusters, existing models for swelling and creep in SiC are limited by the lack of understanding of specific defects that form due to radiation in the range of temperatures relevant to fuel cladding in light water reactors (LWRs) (<1000°C). For example, defects that can be detected with traditional transmission electron microscopy (TEM) techniques account only for 10-45% of the swelling measured in irradiated SiC. Here, we have undertaken an integrated experimental and

  1. Role of Defects in Swelling and Creep of Irradiated SiC

    International Nuclear Information System (INIS)

    Szlufarska, Izabela; Voyles, Paul; Sridharan, Kumar; Katoh, Yutai

    2016-01-01

    Silicon carbide is a promising cladding material because of its high strength and relatively good corrosion resistance. However, SiC is brittle and therefore SiC-based components need to be carefully designed to avoid cracking and failure by fracture. In design of SiC-based composites for nuclear reactor applications it is essential to take into account how mechanical properties are affected by radiation and temperature, or in other words, what strains and stresses develop in this material due to environmental conditions. While thermal strains in SiC can be predicted using classical theories, radiation-induced strains are much less understood. In particular, it is critical to correctly account for radiation swelling and radiation creep, which contribute significantly to dimensional instability of SiC under radiation. Swelling typically increases logarithmically with radiation dose and saturates at relatively low doses (damage levels of a few dpa). Consequently, swelling-induced stresses are likely to develop within a few months of operation of a reactor. Radiation-induced volume swelling in SiC can be as high as 2%, which is significantly higher than the cracking strain of 0.1% in SiC. Swelling-induced strains will lead to enormous stresses and fracture, unless these stresses can be relaxed via some other mechanism. An effective way to achieve stress relaxation is via radiation creep. Although it has been hypothesized that both radiation swelling and radiation creep are driven by formation of defect clusters, existing models for swelling and creep in SiC are limited by the lack of understanding of specific defects that form due to radiation in the range of temperatures relevant to fuel cladding in light water reactors (LWRs) (<1000°C). For example, defects that can be detected with traditional transmission electron microscopy (TEM) techniques account only for 10-45% of the swelling measured in irradiated SiC. Here, we have undertaken an integrated experimental and

  2. Defect luminescence and lattice strain in Mn{sup 2+} doped ZnGa{sub 2}O{sub 4}

    Energy Technology Data Exchange (ETDEWEB)

    Somasundaram, K.; Abhilash, K.P. [Department of Physics, Nallamuthu Gounder Mahalingam College, Pollachi, 642001 Coimbatore (India); Sudarsan, V., E-mail: vsudar@barc.gov.in [Chemistry Division, Bhabha Atomic Research Centre, Trombay, Mumbai 400085 (India); Christopher Selvin, P., E-mail: pcsphyngmc@rediffmail.com [Department of Physics, Nallamuthu Gounder Mahalingam College, Pollachi, 642001 Coimbatore (India); Kadam, R.M. [Radiochemistry Division, Bhabha Atomic Research Centre, Trombay, Mumbai 400085 (India)

    2016-06-15

    Undoped and Mn{sup 2+} doped ZnGa{sub 2}O{sub 4} phosphors were prepared by solution combustion method and characterized by XRD, SEM, luminescence and electron paramagnetic resonance (EPR) techniques. Based on XRD results, it is inferred that, strain in ZnGa{sub 2}O{sub 4} host lattice increases with incorporation of Mn{sup 2+} ions in the lattice. Mn{sup 2+} doping at concentration levels investigated, lead to significant reduction in the defect emission and this has been attributed to the formation of higher oxidation states of Mn ions in the lattice. Electron Paramagnetic Resonance studies confirmed that majority of Mn ions exist as Mn{sup 2+} species and they occupy tetrahedral Zn{sup 2+} site in ZnGa{sub 2}O{sub 4} lattice with an average hyperfine coupling constant, A{sub iso}∼82 G.

  3. Tunneling and migration of the dumbbell defect in electron-irradiated aluminum-zinc alloys

    International Nuclear Information System (INIS)

    Wallace, P.W.

    1983-01-01

    Ultrasonic attenuation and velocity measurements on irradiated Al-Zn alloys (0.01, 0.1, and 0.5 at %) indicate a tunneling relaxation of the predominant mixed dumbbell defect at low temperatures, and mixed dumbbell migration at the Stage II anneal temperature. The effect of an internal strain varying with the zinc concentration on the measured decrement and modulus change is striking. Evaluated in the framework of a six-level system, this reveals the simultaneous action of resonance and nonclassical relaxation processes. Using Fe as a probe atom, it is shown that mixed dumbbell dissociation is in an insignificant component of the annealing of this defect. The decrease of the annealing temperature at higher zinc concentrations provides evidence that the mixed dumbbell migrates as a unit during annealing. The energies associated with dumbbell migration and interstitial escape are derived. Further evidence for the migration mechanism is obtained from successive irradiation and annealing

  4. Defective recoveryfrom potentially lethal damage in some human fibroblast cell strains

    International Nuclear Information System (INIS)

    Arlett, C.F.; Priestley, A.

    1983-01-01

    The repair of potentially lethal damage following treatment by gamma radiation was investigated in human fibroblasts held in a non-cycling state by maintenance in a medium containing 0.5 per cent foetal calf serum. Variation in their capacity to repair PLD was noted between three normal cell strains. A failure to repair PLD in ataxia-telangiectasia cells (AT5BI) was confirmed. In three cell strains which were intermediate between normals and A-T cells in their sensitivity, XP3BR, 46BR and GB1142, a limited capacity for the repair of PLD was observed. Two other cell strains, 47BR and 67BR, which showed little if any hypersensitivity could be clearly distinguished from normals after a 24 hour period for the repair of PLD. Thus the technique might permit better discrimination between cell strains. One other cell strain, H15617, could be distinguished from normals by proving hypersensitive under all conditions. Here, however, the repair of PLD appeared to be normal. (author)

  5. Comparative transcriptomic analysis reveals similarities and dissimilarities in Saccharomyces cerevisiae wine strains response to nitrogen availability.

    Directory of Open Access Journals (Sweden)

    Catarina Barbosa

    Full Text Available Nitrogen levels in grape-juices are of major importance in winemaking ensuring adequate yeast growth and fermentation performance. Here we used a comparative transcriptome analysis to uncover wine yeasts responses to nitrogen availability during fermentation. Gene expression was assessed in three genetically and phenotypically divergent commercial wine strains (CEG, VL1 and QA23, under low (67 mg/L and high nitrogen (670 mg/L regimes, at three time points during fermentation (12 h, 24 h and 96 h. Two-way ANOVA analysis of each fermentation condition led to the identification of genes whose expression was dependent on strain, fermentation stage and on the interaction of both factors. The high fermenter yeast strain QA23 was more clearly distinct from the other two strains, by differential expression of genes involved in flocculation, mitochondrial functions, energy generation and protein folding and stabilization. For all strains, higher transcriptional variability due to fermentation stage was seen in the high nitrogen fermentations. A positive correlation between maximum fermentation rate and the expression of genes involved in stress response was observed. The finding of common genes correlated with both fermentation activity and nitrogen up-take underlies the role of nitrogen on yeast fermentative fitness. The comparative analysis of genes differentially expressed between both fermentation conditions at 12 h, where the main difference was the level of nitrogen available, showed the highest variability amongst strains revealing strain-specific responses. Nevertheless, we were able to identify a small set of genes whose expression profiles can quantitatively assess the common response of the yeast strains to varying nitrogen conditions. The use of three contrasting yeast strains in gene expression analysis prompts the identification of more reliable, accurate and reproducible biomarkers that will facilitate the diagnosis of deficiency of this

  6. Comparative Transcriptomic Analysis Reveals Similarities and Dissimilarities in Saccharomyces cerevisiae Wine Strains Response to Nitrogen Availability

    Science.gov (United States)

    Barbosa, Catarina; García-Martínez, José; Pérez-Ortín, José E.; Mendes-Ferreira, Ana

    2015-01-01

    Nitrogen levels in grape-juices are of major importance in winemaking ensuring adequate yeast growth and fermentation performance. Here we used a comparative transcriptome analysis to uncover wine yeasts responses to nitrogen availability during fermentation. Gene expression was assessed in three genetically and phenotypically divergent commercial wine strains (CEG, VL1 and QA23), under low (67 mg/L) and high nitrogen (670 mg/L) regimes, at three time points during fermentation (12h, 24h and 96h). Two-way ANOVA analysis of each fermentation condition led to the identification of genes whose expression was dependent on strain, fermentation stage and on the interaction of both factors. The high fermenter yeast strain QA23 was more clearly distinct from the other two strains, by differential expression of genes involved in flocculation, mitochondrial functions, energy generation and protein folding and stabilization. For all strains, higher transcriptional variability due to fermentation stage was seen in the high nitrogen fermentations. A positive correlation between maximum fermentation rate and the expression of genes involved in stress response was observed. The finding of common genes correlated with both fermentation activity and nitrogen up-take underlies the role of nitrogen on yeast fermentative fitness. The comparative analysis of genes differentially expressed between both fermentation conditions at 12h, where the main difference was the level of nitrogen available, showed the highest variability amongst strains revealing strain-specific responses. Nevertheless, we were able to identify a small set of genes whose expression profiles can quantitatively assess the common response of the yeast strains to varying nitrogen conditions. The use of three contrasting yeast strains in gene expression analysis prompts the identification of more reliable, accurate and reproducible biomarkers that will facilitate the diagnosis of deficiency of this nutrient in the grape

  7. Whole-Genome Analysis of Three Yeast Strains Used for Production of Sherry-Like Wines Revealed Genetic Traits Specific to Flor Yeasts

    Science.gov (United States)

    Eldarov, Mikhail A.; Beletsky, Alexey V.; Tanashchuk, Tatiana N.; Kishkovskaya, Svetlana A.; Ravin, Nikolai V.; Mardanov, Andrey V.

    2018-01-01

    Flor yeast strains represent a specialized group of Saccharomyces cerevisiae yeasts used for biological wine aging. We have sequenced the genomes of three flor strains originated from different geographic regions and used for production of sherry-like wines in Russia. According to the obtained phylogeny of 118 yeast strains, flor strains form very tight cluster adjacent to the main wine clade. SNP analysis versus available genomes of wine and flor strains revealed 2,270 genetic variants in 1,337 loci specific to flor strains. Gene ontology analysis in combination with gene content evaluation revealed a complex landscape of possibly adaptive genetic changes in flor yeast, related to genes associated with cell morphology, mitotic cell cycle, ion homeostasis, DNA repair, carbohydrate metabolism, lipid metabolism, and cell wall biogenesis. Pangenomic analysis discovered the presence of several well-known “non-reference” loci of potential industrial importance. Events of gene loss included deletions of asparaginase genes, maltose utilization locus, and FRE-FIT locus involved in iron transport. The latter in combination with a flor-yeast-specific mutation in the Aft1 transcription factor gene is likely to be responsible for the discovered phenotype of increased iron sensitivity and improved iron uptake of analyzed strains. Expansion of the coding region of the FLO11 flocullin gene and alteration of the balance between members of the FLO gene family are likely to positively affect the well-known propensity of flor strains for velum formation. Our study provides new insights in the nature of genetic variation in flor yeast strains and demonstrates that different adaptive properties of flor yeast strains could have evolved through different mechanisms of genetic variation. PMID:29867869

  8. Genetic relationships between clinical and non-clinical strains of Yersinia enterocolitica biovar 1A as revealed by multilocus enzyme electrophoresis and multilocus restriction typing

    Directory of Open Access Journals (Sweden)

    Virdi Jugsharan S

    2010-05-01

    Full Text Available Abstract Background Genetic relationships among 81 strains of Y. enterocolitica biovar 1A isolated from clinical and non-clinical sources were discerned by multilocus enzyme electrophoresis (MLEE and multilocus restriction typing (MLRT using six loci each. Such studies may reveal associations between the genotypes of the strains and their sources of isolation. Results All loci were polymorphic and generated 62 electrophoretic types (ETs and 12 restriction types (RTs. The mean genetic diversity (H of the strains by MLEE and MLRT was 0.566 and 0.441 respectively. MLEE (DI = 0.98 was more discriminatory and clustered Y. enterocolitica biovar 1A strains into four groups, while MLRT (DI = 0.77 identified two distinct groups. BURST (Based Upon Related Sequence Types analysis of the MLRT data suggested aquatic serotype O:6,30-6,31 isolates to be the ancestral strains from which, clinical O:6,30-6,31 strains might have originated by host adaptation and genetic change. Conclusion MLEE revealed greater genetic diversity among strains of Y. enterocolitica biovar 1A and clustered strains in four groups, while MLRT grouped the strains into two groups. BURST analysis of MLRT data nevertheless provided newer insights into the probable evolution of clinical strains from aquatic strains.

  9. Molecular typing of canine distemper virus strains reveals the presence of a new genetic variant in South America.

    Science.gov (United States)

    Sarute, Nicolás; Pérez, Ruben; Aldaz, Jaime; Alfieri, Amauri A; Alfieri, Alice F; Name, Daniela; Llanes, Jessika; Hernández, Martín; Francia, Lourdes; Panzera, Yanina

    2014-06-01

    Canine distemper virus (CDV, Paramyxoviridae, Morbillivirus) is the causative agent of a severe infectious disease affecting terrestrial and marine carnivores worldwide. Phylogenetic relationships and the genetic variability of the hemagglutinin (H) protein and the fusion protein signal-peptide (Fsp) allow for the classification of field strains into genetic lineages. Currently, there are nine CDV lineages worldwide, two of them co-circulating in South America. Using the Fsp-coding region, we analyzed the genetic variability of strains from Uruguay, Brazil, and Ecuador, and compared them with those described previously in South America and other geographical areas. The results revealed that the Brazilian and Uruguayan strains belong to the already described South America lineage (EU1/SA1), whereas the Ecuadorian strains cluster in a new clade, here named South America 3, which may represent the third CDV lineage described in South America.

  10. Revealing differences in metabolic flux distributions between a mutant strain and its parent strain Gluconacetobacter xylinus CGMCC 2955.

    Directory of Open Access Journals (Sweden)

    Cheng Zhong

    Full Text Available A better understanding of metabolic fluxes is important for manipulating microbial metabolism toward desired end products, or away from undesirable by-products. A mutant strain, Gluconacetobacter xylinus AX2-16, was obtained by combined chemical mutation of the parent strain (G. xylinus CGMCC 2955 using DEC (diethyl sulfate and LiCl. The highest bacterial cellulose production for this mutant was obtained at about 11.75 g/L, which was an increase of 62% compared with that by the parent strain. In contrast, gluconic acid (the main byproduct concentration was only 5.71 g/L for mutant strain, which was 55.7% lower than that of parent strain. Metabolic flux analysis indicated that 40.1% of the carbon source was transformed to bacterial cellulose in mutant strain, compared with 24.2% for parent strain. Only 32.7% and 4.0% of the carbon source were converted into gluconic acid and acetic acid in mutant strain, compared with 58.5% and 9.5% of that in parent strain. In addition, a higher flux of tricarboxylic acid (TCA cycle was obtained in mutant strain (57.0% compared with parent strain (17.0%. It was also indicated from the flux analysis that more ATP was produced in mutant strain from pentose phosphate pathway (PPP and TCA cycle. The enzymatic activity of succinate dehydrogenase (SDH, which is one of the key enzymes in TCA cycle, was 1.65-fold higher in mutant strain than that in parent strain at the end of culture. It was further validated by the measurement of ATPase that 3.53-6.41 fold higher enzymatic activity was obtained from mutant strain compared with parent strain.

  11. Proteomic analysis reveals contrasting stress response to uranium in two nitrogen-fixing Anabaena strains, differentially tolerant to uranium

    Energy Technology Data Exchange (ETDEWEB)

    Panda, Bandita; Basu, Bhakti; Acharya, Celin; Rajaram, Hema; Apte, Shree Kumar, E-mail: aptesk@barc.gov.in

    2017-01-15

    Highlights: • Response of two native cyanobacterial strains to uranium exposure was studied. • Anabaena L-31 exhibited higher tolerance to uranium as compared to Anabaena 7120. • Uranium exposure differentially affected the proteome profiles of the two strains. • Anabaena L-31 showed better sustenance of photosynthesis and carbon metabolism. • Anabaena L-31 displayed superior oxidative stress defense than Anabaena 7120. - Abstract: Two strains of the nitrogen-fixing cyanobacterium Anabaena, native to Indian paddy fields, displayed differential sensitivity to exposure to uranyl carbonate at neutral pH. Anabaena sp. strain PCC 7120 and Anabaena sp. strain L-31 displayed 50% reduction in survival (LD{sub 50} dose), following 3 h exposure to 75 μM and 200 μM uranyl carbonate, respectively. Uranium responsive proteome alterations were visualized by 2D gel electrophoresis, followed by protein identification by MALDI-ToF mass spectrometry. The two strains displayed significant differences in levels of proteins associated with photosynthesis, carbon metabolism, and oxidative stress alleviation, commensurate with their uranium tolerance. Higher uranium tolerance of Anabaena sp. strain L-31 could be attributed to sustained photosynthesis and carbon metabolism and superior oxidative stress defense, as compared to the uranium sensitive Anabaena sp. strain PCC 7120. Significance: Uranium responsive proteome modulations in two nitrogen-fixing strains of Anabaena, native to Indian paddy fields, revealed that rapid adaptation to better oxidative stress management, and maintenance of metabolic and energy homeostasis underlies superior uranium tolerance of Anabaena sp. strain L-31 compared to Anabaena sp. strain PCC 7120.

  12. A FeNiMnC alloy with strain glass transition

    Directory of Open Access Journals (Sweden)

    Hui Ma

    2018-02-01

    Full Text Available Recent experimental and theoretical investigations suggested that doping sufficient point defects into a normal ferroelastic/martensitic alloy systems could lead to a frozen disordered state of local lattice strains (nanomartensite domains, thereby suppressing the long-range strain-ordering martensitic transition. In this study, we attempt to explore the possibility of developing novel ferrous Elinvar alloys by replacing nickel with carbon and manganese as dopant species. A nominal Fe89Ni5Mn4.6C1.4 alloy was prepared by argon arc melting, and XRD, DSC, DMA and TEM techniques were employed to characterize the strain glass transition signatures, such as invariance in average structure, frequency dispersion in dynamic mechanical properties (storage modulus and internal friction and the formation of nanosized strain domains. It is indicated that doping of Ni, Mn and C suppresses γ→α long-range strain-ordering martensitic transformation in Fe89Ni5Mn4.6C1.4 alloy, generating randomly distributed nanosized domains by strain glass transition. Keywords: Strain glass transition, Elinvar alloys, Point defects, Nanosized domains

  13. Single-cell transcriptomic reconstruction reveals cell cycle and multi-lineage differentiation defects in Bcl11a-deficient hematopoietic stem cells.

    Science.gov (United States)

    Tsang, Jason C H; Yu, Yong; Burke, Shannon; Buettner, Florian; Wang, Cui; Kolodziejczyk, Aleksandra A; Teichmann, Sarah A; Lu, Liming; Liu, Pentao

    2015-09-21

    Hematopoietic stem cells (HSCs) are a rare cell type with the ability of long-term self-renewal and multipotency to reconstitute all blood lineages. HSCs are typically purified from the bone marrow using cell surface markers. Recent studies have identified significant cellular heterogeneities in the HSC compartment with subsets of HSCs displaying lineage bias. We previously discovered that the transcription factor Bcl11a has critical functions in the lymphoid development of the HSC compartment. In this report, we employ single-cell transcriptomic analysis to dissect the molecular heterogeneities in HSCs. We profile the transcriptomes of 180 highly purified HSCs (Bcl11a (+/+) and Bcl11a (-/-)). Detailed analysis of the RNA-seq data identifies cell cycle activity as the major source of transcriptomic variation in the HSC compartment, which allows reconstruction of HSC cell cycle progression in silico. Single-cell RNA-seq profiling of Bcl11a (-/-) HSCs reveals abnormal proliferative phenotypes. Analysis of lineage gene expression suggests that the Bcl11a (-/-) HSCs are constituted of two distinct myeloerythroid-restricted subpopulations. Remarkably, similar myeloid-restricted cells could also be detected in the wild-type HSC compartment, suggesting selective elimination of lymphoid-competent HSCs after Bcl11a deletion. These defects are experimentally validated in serial transplantation experiments where Bcl11a (-/-) HSCs are myeloerythroid-restricted and defective in self-renewal. Our study demonstrates the power of single-cell transcriptomics in dissecting cellular process and lineage heterogeneities in stem cell compartments, and further reveals the molecular and cellular defects in the Bcl11a-deficient HSC compartment.

  14. Formation of strain-induced quantum dots in gated semiconductor nanostructures

    Directory of Open Access Journals (Sweden)

    Ted Thorbeck

    2015-08-01

    Full Text Available A long-standing mystery in the field of semiconductor quantum dots (QDs is: Why are there so many unintentional dots (also known as disorder dots which are neither expected nor controllable. It is typically assumed that these unintentional dots are due to charged defects, however the frequency and predictability of the location of the unintentional QDs suggests there might be additional mechanisms causing the unintentional QDs besides charged defects. We show that the typical strains in a semiconductor nanostructure from metal gates are large enough to create strain-induced quantum dots. We simulate a commonly used QD device architecture, metal gates on bulk silicon, and show the formation of strain-induced QDs. The strain-induced QD can be eliminated by replacing the metal gates with poly-silicon gates. Thus strain can be as important as electrostatics to QD device operation operation.

  15. Maternal mismatches in farmed tilapia strains (Oreochromis spp.) in the Philippines as revealed by mitochondrial COI gene.

    Science.gov (United States)

    Ordoñez, June Feliciano F; Ventolero, Minerva Fatimae H; Santos, Mudjekeewis D

    2017-07-01

    The introduction of genetically enhanced tilapia has significantly boosted the performance of Philippine aquaculture industry. While enhanced strains contribute to the increase in tilapia production, genetic characterization of present tilapia stocks is critical to maintain their quality and to ensure the genetic gains are sustained. To understand and determine the genetic relationship of the genetically enhanced strains produced in the Philippines, mitochondrial cytochrome oxidase subunit I (COI) gene using DNA barcoding approach was analyzed. Specimens representing 10 genetically enhanced strains (GIFT, FaST, GET-EXCEL, GST, SST, COLD, YY-male, GMT, Molobicus, and BEST), three red tilapia (Taiwan red, Florida red, and FAC-red), and two pure lines (initially identified as O. aureus and O. spilurus) were collected, sequenced, and identified using DNA barcoding. Results revealed that farmed tilapias consisted of four different Oreochromis species. As expected, COI could not distinguish individuals at the strain level but surprisingly, mismatch between the species of maternal origin and present-day offspring was observed. This particular result may pose a question on the genetic purity and integrity of the strains being distributed to farmers and suggests a re-evaluation of the effectiveness of major tilapia breeding centers in maintaining their stocks.

  16. The Peak Pairs algorithm for strain mapping from HRTEM images

    Energy Technology Data Exchange (ETDEWEB)

    Galindo, Pedro L. [Departamento de Lenguajes y Sistemas Informaticos, CASEM, Universidad de Cadiz, Pol. Rio San Pedro s/n. 11510, Puerto Real, Cadiz (Spain)], E-mail: pedro.galindo@uca.es; Kret, Slawomir [Institute of Physics, PAS, AL. Lotnikow 32/46, 02-668 Warsaw (Poland); Sanchez, Ana M. [Departamento de Ciencia de los Materiales e Ing. Metalurgica y Q. Inorganica, Facultad de Ciencias, Universidad de Cadiz, Pol. Rio San Pedro s/n. 11510, Puerto Real, Cadiz (Spain); Laval, Jean-Yves [Laboratoire de Physique du Solide, UPR5 CNRS-ESPCI, Paris (France); Yanez, Andres; Pizarro, Joaquin; Guerrero, Elisa [Departamento de Lenguajes y Sistemas Informaticos, CASEM, Universidad de Cadiz, Pol. Rio San Pedro s/n. 11510, Puerto Real, Cadiz (Spain); Ben, Teresa; Molina, Sergio I. [Departamento de Ciencia de los Materiales e Ing. Metalurgica y Q. Inorganica, Facultad de Ciencias, Universidad de Cadiz, Pol. Rio San Pedro s/n. 11510, Puerto Real, Cadiz (Spain)

    2007-11-15

    Strain mapping is defined as a numerical image-processing technique that measures the local shifts of image details around a crystal defect with respect to the ideal, defect-free, positions in the bulk. Algorithms to map elastic strains from high-resolution transmission electron microscopy (HRTEM) images may be classified into two categories: those based on the detection of peaks of intensity in real space and the Geometric Phase approach, calculated in Fourier space. In this paper, we discuss both categories and propose an alternative real space algorithm (Peak Pairs) based on the detection of pairs of intensity maxima in an affine transformed space dependent on the reference area. In spite of the fact that it is a real space approach, the Peak Pairs algorithm exhibits good behaviour at heavily distorted defect cores, e.g. interfaces and dislocations. Quantitative results are reported from experiments to determine local strain in different types of semiconductor heterostructures.

  17. Heterogeneity of the Epstein-Barr Virus (EBV) Major Internal Repeat Reveals Evolutionary Mechanisms of EBV and a Functional Defect in the Prototype EBV Strain B95-8.

    Science.gov (United States)

    Ba Abdullah, Mohammed M; Palermo, Richard D; Palser, Anne L; Grayson, Nicholas E; Kellam, Paul; Correia, Samantha; Szymula, Agnieszka; White, Robert E

    2017-12-01

    Epstein-Barr virus (EBV) is a ubiquitous pathogen of humans that can cause several types of lymphoma and carcinoma. Like other herpesviruses, EBV has diversified through both coevolution with its host and genetic exchange between virus strains. Sequence analysis of the EBV genome is unusually challenging because of the large number and lengths of repeat regions within the virus. Here we describe the sequence assembly and analysis of the large internal repeat 1 of EBV (IR1; also known as the BamW repeats) for more than 70 strains. The diversity of the latency protein EBV nuclear antigen leader protein (EBNA-LP) resides predominantly within the exons downstream of IR1. The integrity of the putative BWRF1 open reading frame (ORF) is retained in over 80% of strains, and deletions truncating IR1 always spare BWRF1. Conserved regions include the IR1 latency promoter (Wp) and one zone upstream of and two within BWRF1. IR1 is heterogeneous in 70% of strains, and this heterogeneity arises from sequence exchange between strains as well as from spontaneous mutation, with interstrain recombination being more common in tumor-derived viruses. This genetic exchange often incorporates regions of Epstein-Barr virus (EBV) infects the majority of the world population but causes illness in only a small minority of people. Nevertheless, over 1% of cancers worldwide are attributable to EBV. Recent sequencing projects investigating virus diversity to see if different strains have different disease impacts have excluded regions of repeating sequence, as they are more technically challenging. Here we analyze the sequence of the largest repeat in EBV (IR1). We first characterized the variations in protein sequences encoded across IR1. In studying variations within the repeat of each strain, we identified a mutation in the main laboratory strain of EBV that impairs virus function, and we suggest that tumor-associated viruses may be more likely to contain DNA mixed from two strains. The

  18. Experimental single-strain mobilomics reveals events that shape pathogen emergence.

    Science.gov (United States)

    Schoeniger, Joseph S; Hudson, Corey M; Bent, Zachary W; Sinha, Anupama; Williams, Kelly P

    2016-08-19

    Virulence genes on mobile DNAs such as genomic islands (GIs) and plasmids promote bacterial pathogen emergence. Excision is an early step in GI mobilization, producing a circular GI and a deletion site in the chromosome; circular forms are also known for some bacterial insertion sequences (ISs). The recombinant sequence at the junctions of such circles and deletions can be detected sensitively in high-throughput sequencing data, using new computational methods that enable empirical discovery of mobile DNAs. For the rich mobilome of a hospital Klebsiella pneumoniae strain, circularization junctions (CJs) were detected for six GIs and seven IS types. Our methods revealed differential biology of multiple mobile DNAs, imprecision of integrases and transposases, and differential activity among identical IS copies for IS26, ISKpn18 and ISKpn21 Using the resistance of circular dsDNA molecules to exonuclease, internally calibrated with the native plasmids, showed that not all molecules bearing GI CJs were circular. Transpositions were also detected, revealing replicon preference (ISKpn18 prefers a conjugative IncA/C2 plasmid), local action (IS26), regional preferences, selection (against capsule synthesis) and IS polarity inversion. Efficient discovery and global characterization of numerous mobile elements per experiment improves accounting for the new gene combinations that arise in emerging pathogens. © The Author(s) 2016. Published by Oxford University Press on behalf of Nucleic Acids Research.

  19. Sister Dehalobacter Genomes Reveal Specialization in Organohalide Respiration and Recent Strain Differentiation Likely Driven by Chlorinated Substrates

    Directory of Open Access Journals (Sweden)

    Shuiquan eTang

    2016-02-01

    Full Text Available The genomes of two closely related Dehalobacter strains (strain CF and strain DCA were assembled from the metagenome of an anaerobic enrichment culture that reductively dechlorinates chloroform (CF, 1,1,1-trichloroethane (1,1,1-TCA and 1,1-dichloroethane (1,1-DCA. The 3.1 Mbp genomes of strain CF (that dechlorinates CF and 1,1,1-TCA and strain DCA (that dechlorinates 1,1-DCA each contain 17 putative reductive dehalogenase homologous (rdh genes. These two genomes were systematically compared to three other available organohalide-respiring Dehalobacter genomes (Dehalobacter restrictus strain PER-K23, Dehalobacter sp. strain E1 and Dehalobacter sp. strain UNSWDHB, and to the genomes of Dehalococcoides mccartyi strain 195 and Desulfitobacterium hafniense strain Y51. This analysis compared 42 different metabolic and physiological categories. The genomes of strains CF and DCA share 90% overall average nucleotide identity and greater than 99.8% identity over a 2.9 Mbp alignment that excludes large insertions, indicating that these genomes differentiated from a close common ancestor. This differentiation was likely driven by selection pressures around two orthologous reductive dehalogenase genes, cfrA and dcrA, that code for the enzymes that reduce CF or 1,1,1-TCA and 1,1-DCA. The many reductive dehalogenase genes found in the five Dehalobacter genomes cluster into two small conserved regions and were often associated with Crp/Fnr transcriptional regulators. Specialization is on-going on a strain-specific basis, as some strains but not others have lost essential genes in the Wood-Ljungdahl (strain E1 and corrinoid biosynthesis pathways (strains E1 and PER-K23. The gene encoding phosphoserine phosphatase, which catalyzes the last step of serine biosynthesis, is missing from all five Dehalobacter genomes, yet D. restrictus can grow without serine, suggesting an alternative or unrecognized biosynthesis route exists. In contrast to Dehalococcoides mccartyi

  20. Characterization of Transformation-Induced Defects in Nickel Titanium Shape Memory Alloys

    Science.gov (United States)

    Bowers, Matthew L.

    Shape memory alloys have remarkable strain recovery properties that make them ideal candidates for many applications that include devices in the automotive, aerospace, medical, and MEMS industries. Although these materials are widely used today, their performance is hindered by poor dimensional stability resulting from cyclic degradation of the martensitic transformation behavior. This functional fatigue results in decreased work output and cyclic accumulation of permanent strain. To date, few studies have taken a fundamental approach to investigating the interaction between plasticity and martensite growth and propagation, which is vitally important to mitigating functional fatigue in future alloy development. The current work focuses on understanding the interplay of these deformation mechanisms in NiTi-based shape memory alloys under a variety of different thermomechanical test conditions. Micron-scale compression testing of NiTi shape memory alloy single crystals is undertaken in an effort to probe the mechanism of austenite dislocation generation. Mechanical testing is paired with post mortem defect analysis via diffraction contrast scanning transmission electron microscopy (STEM). Accompanied by micromechanics-based modeling of local stresses surrounding a martensite plate, these results demonstrate that the previously existing martensite and resulting austenite dislocation substructure are intimately related. A mechanism of transformation-induced dislocation generation is described in detail. A study of pure and load-biased thermal cycling of bulk polycrystalline NiTi is done for comparison of the transformation behavior and resultant defects to the stress-induced case. Post mortem and in situ STEM characterization demonstrate unique defect configurations in this test mode and STEM-based orientation mapping reveals local crystal rotation with increasing thermal cycles. Changes in both martensite and austenite microstructures are explored. The results for

  1. Comparative genome analysis of pathogenic and non-pathogenic Clavibacter strains reveals adaptations to their lifestyle.

    Science.gov (United States)

    Załuga, Joanna; Stragier, Pieter; Baeyen, Steve; Haegeman, Annelies; Van Vaerenbergh, Johan; Maes, Martine; De Vos, Paul

    2014-05-22

    The genus Clavibacter harbors economically important plant pathogens infecting agricultural crops such as potato and tomato. Although the vast majority of Clavibacter strains are pathogenic, there is an increasing number of non-pathogenic isolates reported. Non-pathogenic Clavibacter strains isolated from tomato seeds are particularly problematic because they affect the current detection and identification tests for Clavibacter michiganensis subsp. michiganensis (Cmm), which is regulated with a zero tolerance in tomato seed. Their misidentification as pathogenic Cmm hampers a clear judgment on the seed quality and health. To get more insight in the genetic features linked to the lifestyle of these bacteria, a whole-genome sequence of the tomato seed-borne non-pathogenic Clavibacter LMG 26808 was determined. To gain a better understanding of the molecular determinants of pathogenicity, the genome sequence of LMG 26808 was compared with that of the pathogenic Cmm strain (NCPPB 382). The comparative analysis revealed that LMG 26808 does not contain plasmids pCM1 and pCM2 and also lacks the majority of important virulence factors described so far for pathogenic Cmm. This explains its apparent non-pathogenic nature in tomato plants. Moreover, the genome analysis of LMG 26808 detected sequences from a plasmid originating from a member of Enterobacteriaceae/Klebsiella relative. Genes received that way and coding for antibiotic resistance may provide a competitive advantage for survival of LMG 26808 in its ecological niche. Genetically, LMG 26808 was the most similar to the pathogenic Cmm NCPPB 382 but contained more mobile genetic elements. The genome of this non-pathogenic Clavibacter strain contained also a high number of transporters and regulatory genes. The genome sequence of the non-pathogenic Clavibacter strain LMG 26808 and the comparative analyses with other pathogenic Clavibacter strains provided a better understanding of the genetic bases of virulence and

  2. Private selective sweeps identified from next-generation pool-sequencing reveal convergent pathways under selection in two inbred Schistosoma mansoni strains.

    Directory of Open Access Journals (Sweden)

    Julie A J Clément

    Full Text Available BACKGROUND: The trematode flatworms of the genus Schistosoma, the causative agents of schistosomiasis, are among the most prevalent parasites in humans, affecting more than 200 million people worldwide. In this study, we focused on two well-characterized strains of S. mansoni, to explore signatures of selection. Both strains are highly inbred and exhibit differences in life history traits, in particular in their compatibility with the intermediate host Biomphalaria glabrata. METHODOLOGY/PRINCIPAL FINDINGS: We performed high throughput sequencing of DNA from pools of individuals of each strain using Illumina technology and identified single nucleotide polymorphisms (SNP and copy number variations (CNV. In total, 708,898 SNPs were identified and roughly 2,000 CNVs. The SNPs revealed low nucleotide diversity (π = 2 × 10(-4 within each strain and a high differentiation level (Fst = 0.73 between them. Based on a recently developed in-silico approach, we further detected 12 and 19 private (i.e. specific non-overlapping selective sweeps among the 121 and 151 sweeps found in total for each strain. CONCLUSIONS/SIGNIFICANCE: Functional annotation of transcripts lying in the private selective sweeps revealed specific selection for functions related to parasitic interaction (e.g. cell-cell adhesion or redox reactions. Despite high differentiation between strains, we identified evolutionary convergence of genes related to proteolysis, known as a key virulence factor and a potential target of drug and vaccine development. Our data show that pool-sequencing can be used for the detection of selective sweeps in parasite populations and enables one to identify biological functions under selection.

  3. Nanometre-scale 3D defects in Cr2AlC thin films.

    Science.gov (United States)

    Chen, Y T; Music, D; Shang, L; Mayer, J; Schneider, J M

    2017-04-20

    MAX-phase Cr 2 AlC containing thin films were synthesized by magnetron sputtering in an industrial system. Nanometre-scale 3D defects are observed near the boundary between regions of Cr 2 AlC and of the disordered solid solution (CrAl) x C y . Shrinkage of the Cr-Cr interplanar distance and elongation of the Cr-Al distance in the vicinity of the defects are detected using transmission electron microscopy. The here observed deformation surrounding the defects was described using density functional theory by comparing the DOS of bulk Cr 2 AlC with the DOS of a strained and unstrained Cr 2 AlC(0001) surface. From the partial density of states analysis, it can be learned that Cr-C bonds are stronger than Cr-Al bonds in bulk Cr 2 AlC. Upon Cr 2 AlC(0001) surface formation, both bonds are weakened. While the Cr-C bonds recover their bulk strength as Cr 2 AlC(0001) is strained, the Cr-Al bonds experience only a partial recovery, still being weaker than their bulk counterparts. Hence, the strain induced bond strengthening in Cr 2 AlC(0001) is larger for Cr d - C p bonds than for Cr d - Al p bonds. The here observed changes in bonding due to the formation of a strained surface are consistent with the experimentally observed elongation of the Cr-Al distance in the vicinity of nm-scale 3D defects in Cr 2 AlC thin films.

  4. Carbon redistribution and precipitation in high temperature ion-implanted strained Si/SiGe/Si multi-layered structures

    DEFF Research Database (Denmark)

    Gaiduk, Peter; Hansen, John Lundsgaard; Nylandsted Larsen, Arne

    2014-01-01

    Graphical abstract Carbon depth profiles after high temperature implantation in strained Si/SiGe/Si multilayered system and induced structural defects.......Graphical abstract Carbon depth profiles after high temperature implantation in strained Si/SiGe/Si multilayered system and induced structural defects....

  5. Symmetry, strain, defects, and the nonlinear optical response of crystalline BaTiO3/silicon

    Science.gov (United States)

    Kormondy, Kristy; Abel, Stefan; Popoff, Youri; Sousa, Marilyne; Caimi, Daniele; Siegwart, Heinz; Marchiori, Chiara; Rossell, Marta; Demkov, Alex; Fompeyrine, Jean

    Recent progress has been made towards exploiting the linear electro-optic or Pockels effect in ferroelectric BaTiO3 (BTO) for novel integrated silicon photonics devices. In such structures, the crystalline symmetry and domain structure of BTO determine which electro-optic tensor elements are accessible under application of an external electric field. For epitaxial thin films of BTO on Si (001), the role of defects in strain relaxation can lead to very different crystalline symmetry even for films of identical thickness. Indeed, through geometric phase analysis of high-resolution scanning transmission electron microscopy images, we map changes of the in-plane and out-of-plane lattice parameters across two 80-nm-thick BTO films. A corresponding 20% difference in the effective electro-optic response was measured by analyzing induced rotation of the polarization of a laser beam (λ = 1550 nm) transmitted through lithographically defined electrodes. Understanding, controlling, and modelling the role of BTO symmetry in nonlinear optics is of fundamental importance for the development of a hybrid BTO/Si photonics platform.. Work supported by the NSF (IRES-1358111), AFOSR (FA9550-12-10494), and European Commission (FP7-ICT-2013-11-619456-SITOGA).

  6. Genotyping of ancient Mycobacterium tuberculosis strains reveals historic genetic diversity.

    Science.gov (United States)

    Müller, Romy; Roberts, Charlotte A; Brown, Terence A

    2014-04-22

    The evolutionary history of the Mycobacterium tuberculosis complex (MTBC) has previously been studied by analysis of sequence diversity in extant strains, but not addressed by direct examination of strain genotypes in archaeological remains. Here, we use ancient DNA sequencing to type 11 single nucleotide polymorphisms and two large sequence polymorphisms in the MTBC strains present in 10 archaeological samples from skeletons from Britain and Europe dating to the second-nineteenth centuries AD. The results enable us to assign the strains to groupings and lineages recognized in the extant MTBC. We show that at least during the eighteenth-nineteenth centuries AD, strains of M. tuberculosis belonging to different genetic groups were present in Britain at the same time, possibly even at a single location, and we present evidence for a mixed infection in at least one individual. Our study shows that ancient DNA typing applied to multiple samples can provide sufficiently detailed information to contribute to both archaeological and evolutionary knowledge of the history of tuberculosis.

  7. Multilocus Sequence Typing Reveals Relevant Genetic Variation and Different Evolutionary Dynamics among Strains of Xanthomonas arboricola pv. juglandis

    Directory of Open Access Journals (Sweden)

    Marco Scortichini

    2010-11-01

    Full Text Available Forty-five Xanthomonas arboricola pv. juglandis (Xaj strains originating from Juglans regia cultivation in different countries were molecularly typed by means of MultiLocus Sequence Typing (MLST, using acnB, gapA, gyrB and rpoD gene fragments. A total of 2.5 kilobases was used to infer the phylogenetic relationship among the strains and possible recombination events. Haplotype diversity, linkage disequilibrium analysis, selection tests, gene flow estimates and codon adaptation index were also assessed. The dendrograms built by maximum likelihood with concatenated nucleotide and amino acid sequences revealed two major and two minor phylotypes. The same haplotype was found in strains originating from different continents, and different haplotypes were found in strains isolated in the same year from the same location. A recombination breakpoint was detected within the rpoD gene fragment. At the pathovar level, the Xaj populations studied here are clonal and under neutral selection. However, four Xaj strains isolated from walnut fruits with apical necrosis are under diversifying selection, suggesting a possible new adaptation. Gene flow estimates do not support the hypothesis of geographic isolation of the strains, even though the genetic diversity between the strains increases as the geographic distance between them increases. A triplet deletion, causing the absence of valine, was found in the rpoD fragment of all 45 Xaj strains when compared with X. axonopodis pv. citri strain 306. The codon adaptation index was high in all four genes studied, indicating a relevant metabolic activity.

  8. Structural defects in cubic semiconductors characterized by aberration-corrected scanning transmission electron microscopy

    Energy Technology Data Exchange (ETDEWEB)

    Arroyo Rojas Dasilva, Yadira; Kozak, Roksolana; Erni, Rolf; Rossell, Marta D., E-mail: marta.rossell@empa.ch

    2017-05-15

    The development of new electro-optical devices and the realization of novel types of transistors require a profound understanding of the structural characteristics of new semiconductor heterostructures. This article provides a concise review about structural defects which occur in semiconductor heterostructures on the basis of micro-patterned Si substrates. In particular, one- and two-dimensional crystal defects are being discussed which are due to the plastic relaxation of epitaxial strain caused by the misfit of crystal lattices. Besides a few selected examples from literature, we treat in particular crystal defects occurring in GaAs/Si, Ge/Si and β-SiC/Si structures which are studied by high-resolution annular dark-field scanning transmission electron microscopy. The relevance of this article is twofold; firstly, it should provide a collection of data which are of help for the identification and characterization of defects in cubic semiconductors by means of atomic-resolution imaging, and secondly, the experimental data shall provide a basis for advancing the understanding of device characteristics with the aid of theoretical modelling by considering the defective nature of strained semiconductor heterostructures. - Highlights: • The heterogeneous integration of high-quality compound semiconductors remains a challenge. • Lattice defects cause severe degradation of the semiconductor device performances. • Aberration-corrected HAADF-STEM allows atomic-scale characterization of defects. • An overview of lattice defects found in cubic semiconductors is presented. • Theoretical modelling and calculations are needed to determine the defect properties.

  9. Caenorhabditis briggsae recombinant inbred line genotypes reveal inter-strain incompatibility and the evolution of recombination.

    Directory of Open Access Journals (Sweden)

    Joseph A Ross

    2011-07-01

    Full Text Available The nematode Caenorhabditis briggsae is an emerging model organism that allows evolutionary comparisons with C. elegans and exploration of its own unique biological attributes. To produce a high-resolution C. briggsae recombination map, recombinant inbred lines were generated from reciprocal crosses between two strains and genotyped at over 1,000 loci. A second set of recombinant inbred lines involving a third strain was also genotyped at lower resolution. The resulting recombination maps exhibit discrete domains of high and low recombination, as in C. elegans, indicating these are a general feature of Caenorhabditis species. The proportion of a chromosome's physical size occupied by the central, low-recombination domain is highly correlated between species. However, the C. briggsae intra-species comparison reveals striking variation in the distribution of recombination between domains. Hybrid lines made with the more divergent pair of strains also exhibit pervasive marker transmission ratio distortion, evidence of selection acting on hybrid genotypes. The strongest effect, on chromosome III, is explained by a developmental delay phenotype exhibited by some hybrid F2 animals. In addition, on chromosomes IV and V, cross direction-specific biases towards one parental genotype suggest the existence of cytonuclear epistatic interactions. These interactions are discussed in relation to surprising mitochondrial genome polymorphism in C. briggsae, evidence that the two strains diverged in allopatry, the potential for local adaptation, and the evolution of Dobzhansky-Muller incompatibilities. The genetic and genomic resources resulting from this work will support future efforts to understand inter-strain divergence as well as facilitate studies of gene function, natural variation, and the evolution of recombination in Caenorhabditis nematodes.

  10. Point defect weakened thermal contraction in monolayer graphene.

    Science.gov (United States)

    Zha, Xian-Hu; Zhang, Rui-Qin; Lin, Zijing

    2014-08-14

    We investigate the thermal expansion behaviors of monolayer graphene and three configurations of graphene with point defects, namely the replacement of one carbon atom with a boron or nitrogen atom, or of two neighboring carbon atoms by boron-nitrogen atoms, based on calculations using first-principles density functional theory. It is found that the thermal contraction of monolayer graphene is significantly decreased by point defects. Moreover, the corresponding temperature for negative linear thermal expansion coefficient with the maximum absolute value is reduced. The cause is determined to be point defects that enhance the mechanical strength of graphene and then reduce the amplitude and phonon frequency of the out-of-plane acoustic vibration mode. Such defect weakening of graphene thermal contraction will be useful in nanotechnology to diminish the mismatching or strain between the graphene and its substrate.

  11. Strain distribution and defect analysis in III-nitrides by dynamical AFM analysis

    International Nuclear Information System (INIS)

    Minj, Albert; Cavalcoli, Daniela; Cavallini, Anna; Gamarra, Piero; Di Forte Poisson, Marie-Antoinette

    2013-01-01

    Here, we report on significant material information provided by semi-contact phase-images in a wide range of hard III-nitride surfaces. We show that the phase contrast, which is fundamentally related to the energy dissipation during tip–surface interaction, is sensitive to the crystalline nature of the material and thus could potentially be used to determine the crystalline quality of thin nitride layers. Besides, we found that the structural defects, especially threading dislocations and cracks, act as selective sites where energy mainly dissipates. Consequently, in nitrides defects with very low dimensions can actually be imaged with phase-contrast imaging. (paper)

  12. In situ AFM study of pitting corrosion and corrosion under strain on a 304L stainless steel

    International Nuclear Information System (INIS)

    Martin, F.A.; Cousty, J.; Masson, J-L.; Bataillon, C.

    2004-01-01

    Our study is centred on surface localised corrosion under strain of a standard stainless steel (304L). The interest we take in these corrosion phenomena is led by the general misunderstanding of its primary initiation steps. The goal of this study is to determine precisely the relationships between local geometrical defects (grain boundaries, dislocation lines, etc) or chemical defects (inclusions) with the preferential sites of corrosion on the strained material. By combining three techniques at the same time: Atomic Force Microscopy, an electrochemical cell and a traction plate, we can observe in situ the effect of localised stress and deformation on the sample surface exposed to a corrosive solution. We managed to build an original set-up compatible with all the requirements of these three different techniques. Furthermore, we prepared the surface of our sample as flat as possible to decrease at maximum the topographical noise in order to observe the smallest defect on the surface. By using a colloidal suspension of SiO 2 , we obtained surfaces with a typical corrugation (RMS) of about 1 A for areas of at least 1 μm 2 . Our experimental study has been organised in two primary investigations: - In situ study of the morphology evolution of the surface under a corrosive chloride solution (borate buffer with NaCl salt). The influence of time, NaCl concentration, and potential was investigated; - In situ exploration of a 304L strained surface. It revealed the first stages of the surface plastic evolutions like activation of sliding dislocations, materialized by parallel steps of about 2 nm high in the same grain. The secondary sliding plane systems were also noticeable for higher deformation rates. Recent results concerning in situ AFM observation of corroded surfaces under strain in a chloride media will be presented. (authors)

  13. In situ AFM study of pitting corrosion and corrosion under strain on a 304L stainless steel

    Energy Technology Data Exchange (ETDEWEB)

    Martin, F.A. [CEA de Saclay, DRECAM/SPCSI, 91191 Gif-sur-Yvette cedex (France); Cousty, J.; Masson, J-L. [CEA de Saclay, DRECAM/SPCSI, 91191 Gif-sur-Yvette cedex (France); Bataillon, C. [CEA de Saclay, DEN/DPC/LECA, 91191 Gif-sur-Yvette cedex (France)

    2004-07-01

    Our study is centred on surface localised corrosion under strain of a standard stainless steel (304L). The interest we take in these corrosion phenomena is led by the general misunderstanding of its primary initiation steps. The goal of this study is to determine precisely the relationships between local geometrical defects (grain boundaries, dislocation lines, etc) or chemical defects (inclusions) with the preferential sites of corrosion on the strained material. By combining three techniques at the same time: Atomic Force Microscopy, an electrochemical cell and a traction plate, we can observe in situ the effect of localised stress and deformation on the sample surface exposed to a corrosive solution. We managed to build an original set-up compatible with all the requirements of these three different techniques. Furthermore, we prepared the surface of our sample as flat as possible to decrease at maximum the topographical noise in order to observe the smallest defect on the surface. By using a colloidal suspension of SiO{sub 2}, we obtained surfaces with a typical corrugation (RMS) of about 1 A for areas of at least 1 {mu}m{sup 2}. Our experimental study has been organised in two primary investigations: - In situ study of the morphology evolution of the surface under a corrosive chloride solution (borate buffer with NaCl salt). The influence of time, NaCl concentration, and potential was investigated; - In situ exploration of a 304L strained surface. It revealed the first stages of the surface plastic evolutions like activation of sliding dislocations, materialized by parallel steps of about 2 nm high in the same grain. The secondary sliding plane systems were also noticeable for higher deformation rates. Recent results concerning in situ AFM observation of corroded surfaces under strain in a chloride media will be presented. (authors)

  14. Defect assessment procedures at high temperature

    International Nuclear Information System (INIS)

    Ainsworth, R.A.

    1991-01-01

    A comprehensive assessment procedure for the high-temperature response of structures is being produced. The procedure is referred to as R5 and is written as a series of step-by-step instructions in a number of volumes. This paper considers in detail those parts of R5 which address the behaviour of defects. The defect assessment procedures may be applied to defects found in service, postulated defects, or defects formed during operation as a result of creep-fatigue loading. In the last case, a method is described for deducing from endurance data the number of cycles to initiate a crack of a specified size. Under steady loading, the creep crack tip parameter C * is used to assess crack growth. Under cyclic loading, the creep crack growth during dwell periods is stiell governed by C * but crack growth due to cyclic excursions must also be included. This cyclic crack growth is described by an effective stress intensity factor range. A feature of the R5 defect assessment procedures in that they are based on simplified methods and approximate reference stress methods are described which enable C * in a component to be evaluated. It is shown by comparison with theoretical calculations and experimental data that reliable estimates of C * and the associated crack growth are obtained provided realistic creep strain rate date are used in the reference stress approximation. (orig./HP)

  15. Antagonistic pleiotropy and fitness trade-offs reveal specialist and generalist traits in strains of canine distemper virus.

    Directory of Open Access Journals (Sweden)

    Veljko M Nikolin

    Full Text Available Theoretically, homogeneous environments favor the evolution of specialists whereas heterogeneous environments favor generalists. Canine distemper is a multi-host carnivore disease caused by canine distemper virus (CDV. The described cell receptor of CDV is SLAM (CD150. Attachment of CDV hemagglutinin protein (CDV-H to this receptor facilitates fusion and virus entry in cooperation with the fusion protein (CDV-F. We investigated whether CDV strains co-evolved in the large, homogeneous domestic dog population exhibited specialist traits, and strains adapted to the heterogeneous environment of smaller populations of different carnivores exhibited generalist traits. Comparison of amino acid sequences of the SLAM binding region revealed higher similarity between sequences from Canidae species than to sequences from other carnivore families. Using an in vitro assay, we quantified syncytia formation mediated by CDV-H proteins from dog and non-dog CDV strains in cells expressing dog, lion or cat SLAM. CDV-H proteins from dog strains produced significantly higher values with cells expressing dog SLAM than with cells expressing lion or cat SLAM. CDV-H proteins from strains of non-dog species produced similar values in all three cell types, but lower values in cells expressing dog SLAM than the values obtained for CDV-H proteins from dog strains. By experimentally changing one amino acid (Y549H in the CDV-H protein of one dog strain we decreased expression of specialist traits and increased expression of generalist traits, thereby confirming its functional importance. A virus titer assay demonstrated that dog strains produced higher titers in cells expressing dog SLAM than cells expressing SLAM of non-dog hosts, which suggested possible fitness benefits of specialization post-cell entry. We provide in vitro evidence for the expression of specialist and generalist traits by CDV strains, and fitness trade-offs across carnivore host environments caused by

  16. Antagonistic Pleiotropy and Fitness Trade-Offs Reveal Specialist and Generalist Traits in Strains of Canine Distemper Virus

    Science.gov (United States)

    Nikolin, Veljko M.; Osterrieder, Klaus; von Messling, Veronika; Hofer, Heribert; Anderson, Danielle; Dubovi, Edward; Brunner, Edgar; East, Marion L.

    2012-01-01

    Theoretically, homogeneous environments favor the evolution of specialists whereas heterogeneous environments favor generalists. Canine distemper is a multi-host carnivore disease caused by canine distemper virus (CDV). The described cell receptor of CDV is SLAM (CD150). Attachment of CDV hemagglutinin protein (CDV-H) to this receptor facilitates fusion and virus entry in cooperation with the fusion protein (CDV-F). We investigated whether CDV strains co-evolved in the large, homogeneous domestic dog population exhibited specialist traits, and strains adapted to the heterogeneous environment of smaller populations of different carnivores exhibited generalist traits. Comparison of amino acid sequences of the SLAM binding region revealed higher similarity between sequences from Canidae species than to sequences from other carnivore families. Using an in vitro assay, we quantified syncytia formation mediated by CDV-H proteins from dog and non-dog CDV strains in cells expressing dog, lion or cat SLAM. CDV-H proteins from dog strains produced significantly higher values with cells expressing dog SLAM than with cells expressing lion or cat SLAM. CDV-H proteins from strains of non-dog species produced similar values in all three cell types, but lower values in cells expressing dog SLAM than the values obtained for CDV-H proteins from dog strains. By experimentally changing one amino acid (Y549H) in the CDV-H protein of one dog strain we decreased expression of specialist traits and increased expression of generalist traits, thereby confirming its functional importance. A virus titer assay demonstrated that dog strains produced higher titers in cells expressing dog SLAM than cells expressing SLAM of non-dog hosts, which suggested possible fitness benefits of specialization post-cell entry. We provide in vitro evidence for the expression of specialist and generalist traits by CDV strains, and fitness trade-offs across carnivore host environments caused by antagonistic

  17. Thermal processing of strained silicon-on-insulator for atomically precise silicon device fabrication

    International Nuclear Information System (INIS)

    Lee, W.C.T.; Bishop, N.; Thompson, D.L.; Xue, K.; Scappucci, G.; Cederberg, J.G.; Gray, J.K.; Han, S.M.; Celler, G.K.; Carroll, M.S.; Simmons, M.Y.

    2013-01-01

    Highlights: ► Strained silicon-on-insulator (sSOI) samples were flash-annealed at high temperature under ultra-high vacuum conditions. ► The extend of surface strain relaxation depends on the annealing temperature with no strain relaxation observed below 1020 °C. ► A 2 × 1 reconstructed surface with low defect density can be achieved. ► The annealed sSOI surface shows enhanced step undulations due to the unique energetics caused by surface strain. - Abstract: We investigate the ability to reconstruct strained silicon-on-insulator (sSOI) substrates in ultra-high vacuum for use in atomic scale device fabrication. Characterisation of the starting sSOI substrate using μRaman shows an average tensile strain of 0.8%, with clear strain modulation in a crosshatch pattern across the surface. The surfaces were heated in ultra-high vacuum from temperatures of 900 °C to 1100 °C and subsequently imaged using scanning tunnelling microscopy (STM). The initial strain modulation on the surface is observed to promote silicon migration and the formation of crosshatched surface features whose height and pitch increases with increasing annealing temperature. STM images reveal alternating narrow straight S A steps and triangular wavy S B steps attributed to the spontaneous faceting of S B and preferential adatom attachment on S B under biaxial tensile strain. Raman spectroscopy shows that despite these high temperature anneals no strain relaxation of the substrate is observed up to temperatures of 1020 °C. Above 1100 °C, strain relaxation is evident but is confined to the surface.

  18. Immunization against Genital Herpes with a Vaccine Virus That has Defects in Productive and Latent Infection

    Science.gov (United States)

    da Costa, Xavier J.; Jones, Cheryl A.; Knipe, David M.

    1999-06-01

    An effective vaccine for genital herpes has been difficult to achieve because of the limited efficacy of subunit vaccines and the safety concerns about live viruses. As an alternative approach, mutant herpes simplex virus strains that are replication-defective can induce protective immunity. To increase the level of safety and to prove that replication was not needed for immunization, we constructed a mutant herpes simplex virus 2 strain containing two deletion mutations, each of which eliminated viral replication. The double-mutant virus induces protective immunity that can reduce acute viral shedding and latent infection in a mouse genital model, but importantly, the double-mutant virus shows a phenotypic defect in latent infection. This herpes vaccine strain, which is immunogenic but has defects in both productive and latent infection, provides a paradigm for the design of vaccines and vaccine vectors for other sexually transmitted diseases, such as AIDS.

  19. Dioxin-induced retardation of development through a reduction in the expression of pituitary hormones and possible involvement of an aryl hydrocarbon receptor in this defect: A comparative study using two strains of mice with different sensitivities to dioxin

    International Nuclear Information System (INIS)

    Takeda, Tomoki; Taura, Junki; Hattori, Yukiko; Ishii, Yuji; Yamada, Hideyuki

    2014-01-01

    We have previously revealed that treating pregnant rats with 2,3,7,8-tetracholorodibenzo-p-dioxin (TCDD) reduces the expression of gonadotropins and growth hormone (GH) in the fetal and neonatal pituitary. A change in gonadotropin expression impairs the testicular expression of steroidogenic proteins in perinatal pups, and imprint defects in sexual behavior after reaching maturity. In this study, we examined whether TCDD also affects the expression of gonadotropin and GH in mice using C57BL/6J and DBA/2J strains which express the aryl hydrocarbon receptor (Ahr) exhibiting a different affinity for TCDD. When pregnant C57BL/6J mice at gestational day (GD) 12 were given oral TCDD (0.2–20 μg/kg), all doses significantly attenuated the pituitary expression of gonadotropin mRNAs in fetuses at GD18. On the other hand, in DBA/2J mice, a much higher dose of TCDD (20 μg/kg) was needed to produce a significant attenuation. Such reduction in the C57BL/6J strain continued until at least postnatal day (PND) 4. In agreement with this, TCDD reduced the testicular expression of steroidogenic proteins in C57BL/6J neonates at PND2 and 4, although the same did not occur in the fetal testis and ovary. Furthermore, TCDD reduced the perinatal expression of GH, litter size and the body weight of newborn pups only in the C57BL/6J strain. These results suggest that 1) also in mice, maternal exposure to TCDD attenuates gonadotropin-regulated steroidogenesis and GH expression leading to the impairment of pup development and sexual immaturity; and 2) Ahr activation during the late fetal and early postnatal stages is required for these defects. - Highlights: • The effect of 2,3,7,8-tetrachlorodibenzo-p-dioxin (TCDD) on mouse growth was studied. • TCDD reduced the levels of luteinizing hormone and growth hormone in perinatal pups. • Maternal exposure to TCDD also attenuated testicular steroidogenesis in pups. • The above effects of TCDD were more pronounced in C57BL/6J than in DBA/2J

  20. Dioxin-induced retardation of development through a reduction in the expression of pituitary hormones and possible involvement of an aryl hydrocarbon receptor in this defect: A comparative study using two strains of mice with different sensitivities to dioxin

    Energy Technology Data Exchange (ETDEWEB)

    Takeda, Tomoki; Taura, Junki; Hattori, Yukiko; Ishii, Yuji; Yamada, Hideyuki, E-mail: hyamada@phar.kyushu-u.ac.jp

    2014-08-01

    We have previously revealed that treating pregnant rats with 2,3,7,8-tetracholorodibenzo-p-dioxin (TCDD) reduces the expression of gonadotropins and growth hormone (GH) in the fetal and neonatal pituitary. A change in gonadotropin expression impairs the testicular expression of steroidogenic proteins in perinatal pups, and imprint defects in sexual behavior after reaching maturity. In this study, we examined whether TCDD also affects the expression of gonadotropin and GH in mice using C57BL/6J and DBA/2J strains which express the aryl hydrocarbon receptor (Ahr) exhibiting a different affinity for TCDD. When pregnant C57BL/6J mice at gestational day (GD) 12 were given oral TCDD (0.2–20 μg/kg), all doses significantly attenuated the pituitary expression of gonadotropin mRNAs in fetuses at GD18. On the other hand, in DBA/2J mice, a much higher dose of TCDD (20 μg/kg) was needed to produce a significant attenuation. Such reduction in the C57BL/6J strain continued until at least postnatal day (PND) 4. In agreement with this, TCDD reduced the testicular expression of steroidogenic proteins in C57BL/6J neonates at PND2 and 4, although the same did not occur in the fetal testis and ovary. Furthermore, TCDD reduced the perinatal expression of GH, litter size and the body weight of newborn pups only in the C57BL/6J strain. These results suggest that 1) also in mice, maternal exposure to TCDD attenuates gonadotropin-regulated steroidogenesis and GH expression leading to the impairment of pup development and sexual immaturity; and 2) Ahr activation during the late fetal and early postnatal stages is required for these defects. - Highlights: • The effect of 2,3,7,8-tetrachlorodibenzo-p-dioxin (TCDD) on mouse growth was studied. • TCDD reduced the levels of luteinizing hormone and growth hormone in perinatal pups. • Maternal exposure to TCDD also attenuated testicular steroidogenesis in pups. • The above effects of TCDD were more pronounced in C57BL/6J than in DBA/2J

  1. Ab initio study of native defects in SnO under strain

    KAUST Repository

    Bianchi Granato, Danilo; Albar, Arwa; Schwingenschlö gl, Udo

    2014-01-01

    Tin monoxide (SnO) has promising properties to be applied as a p-type semiconductor in transparent electronics. To this end, it is necessary to understand the behaviour of defects in order to control them. We use density functional theory to study

  2. Fatal laboratory-acquired infection with an attenuated Yersinia pestis Strain--Chicago, Illinois, 2009.

    Science.gov (United States)

    2011-02-25

    On September 18, 2009, the Chicago Department of Public Health (CDPH) was notified by a local hospital of a suspected case of fatal laboratory-acquired infection with Yersinia pestis, the causative agent of plague. The patient, a researcher in a university laboratory, had been working along with other members of the laboratory group with a pigmentation-negative (pgm-) attenuated Y. pestis strain (KIM D27). The strain had not been known to have caused laboratory-acquired infections or human fatalities. Other researchers in a separate university laboratory facility in the same building had contact with a virulent Y. pestis strain (CO92) that is considered a select biologic agent; however, the pgm- attenuated KIM D27 is excluded from the National Select Agent Registry. The university, CDPH, the Illinois Department of Public Health (IDPH), and CDC conducted an investigation to ascertain the cause of death. This report summarizes the results of that investigation, which determined that the cause of death likely was an unrecognized occupational exposure (route unknown) to Y. pestis, leading to septic shock. Y. pestis was isolated from premortem blood cultures. Polymerase chain reaction (PCR) identified the clinical isolate as a pgm- strain of Y. pestis. Postmortem examination revealed no evidence of pneumonic plague. A postmortem diagnosis of hereditary hemochromatosis was made on the basis of histopathologic, laboratory, and genetic testing. One possible explanation for the unexpected fatal outcome in this patient is that hemochromatosis-induced iron overload might have provided the infecting KIM D27 strain, which is attenuated as a result of defects in its ability to acquire iron, with sufficient iron to overcome its iron-acquisition defects and become virulent. Researchers should adhere to recommended biosafety practices when handling any live bacterial cultures, even attenuated strains, and institutional biosafety committees should implement and maintain effective

  3. RNA-Seq Analyses for Two Silkworm Strains Reveals Insight into Their Susceptibility and Resistance to Beauveria bassiana Infection.

    Science.gov (United States)

    Xing, Dongxu; Yang, Qiong; Jiang, Liang; Li, Qingrong; Xiao, Yang; Ye, Mingqiang; Xia, Qingyou

    2017-02-10

    The silkworm Bombyx mori is an economically important species. White muscardine caused by Beauveria bassiana is the main fungal disease in sericulture, and understanding the silkworm responses to B. bassiana infection is of particular interest. Herein, we investigated the molecular mechanisms underlying these responses in two silkworm strains Haoyue (HY, sensitive to B. bassiana ) and Kang 8 (K8, resistant to B. bassiana ) using an RNA-seq approach. For each strain, three biological replicates for immersion treatment, two replicates for injection treatment and three untreated controls were collected to generate 16 libraries for sequencing. Differentially expressed genes (DEGs) between treated samples and untreated controls, and between the two silkworm strains, were identified. DEGs and the enriched Kyoto Encyclopedia of Genes and Genomes (KEGG) pathways of the two strains exhibited an obvious difference. Several genes encoding cuticle proteins, serine proteinase inhibitors (SPI) and antimicrobial peptides (AMP) and the drug metabolism pathway involved in toxin detoxification were considered to be related to the resistance of K8 to B. bassiana. These results revealed insight into the resistance and susceptibility of two silkworm strains against B. bassiana infection and provided a roadmap for silkworm molecular breeding to enhance its resistance to B. bassiana .

  4. RNA-Seq Analyses for Two Silkworm Strains Reveals Insight into Their Susceptibility and Resistance to Beauveria bassiana Infection

    Directory of Open Access Journals (Sweden)

    Dongxu Xing

    2017-02-01

    Full Text Available The silkworm Bombyx mori is an economically important species. White muscardine caused by Beauveria bassiana is the main fungal disease in sericulture, and understanding the silkworm responses to B. bassiana infection is of particular interest. Herein, we investigated the molecular mechanisms underlying these responses in two silkworm strains Haoyue (HY, sensitive to B. bassiana and Kang 8 (K8, resistant to B. bassiana using an RNA-seq approach. For each strain, three biological replicates for immersion treatment, two replicates for injection treatment and three untreated controls were collected to generate 16 libraries for sequencing. Differentially expressed genes (DEGs between treated samples and untreated controls, and between the two silkworm strains, were identified. DEGs and the enriched Kyoto Encyclopedia of Genes and Genomes (KEGG pathways of the two strains exhibited an obvious difference. Several genes encoding cuticle proteins, serine proteinase inhibitors (SPI and antimicrobial peptides (AMP and the drug metabolism pathway involved in toxin detoxification were considered to be related to the resistance of K8 to B. bassiana. These results revealed insight into the resistance and susceptibility of two silkworm strains against B. bassiana infection and provided a roadmap for silkworm molecular breeding to enhance its resistance to B. bassiana.

  5. Multilocus microsatellite typing (MLMT of strains from Turkey and Cyprus reveals a novel monophyletic L. donovani sensu lato group.

    Directory of Open Access Journals (Sweden)

    Evi Gouzelou

    Full Text Available BACKGROUND: New foci of human CL caused by strains of the Leishmania donovani (L. donovani complex have been recently described in Cyprus and the Çukurova region in Turkey (L. infantum situated 150 km north of Cyprus. Cypriot strains were typed by Multilocus Enzyme Electrophoresis (MLEE using the Montpellier (MON system as L. donovani zymodeme MON-37. However, multilocus microsatellite typing (MLMT has shown that this zymodeme is paraphyletic; composed of distantly related genetic subgroups of different geographical origin. Consequently the origin of the Cypriot strains remained enigmatic. METHODOLOGY/PRINCIPAL FINDINGS: The Cypriot strains were compared with a set of Turkish isolates obtained from a CL patient and sand fly vectors in south-east Turkey (Çukurova region; CUK strains and from a VL patient in the south-west (Kuşadasi; EP59 strain. These Turkish strains were initially analyzed using the K26-PCR assay that discriminates MON-1 strains by their amplicon size. In line with previous DNA-based data, the strains were inferred to the L. donovani complex and characterized as non MON-1. For these strains MLEE typing revealed two novel zymodemes; L. donovani MON-309 (CUK strains and MON-308 (EP59. A population genetic analysis of the Turkish isolates was performed using 14 hyper-variable microsatellite loci. The genotypic profiles of 68 previously analyzed L. donovani complex strains from major endemic regions were included for comparison. Population structures were inferred by combination of bayesian model-based and distance-based approaches. MLMT placed the Turkish and Cypriot strains in a subclade of a newly discovered, genetically distinct L. infantum monophyletic group, suggesting that the Cypriot strains may originate from Turkey. CONCLUSION: The discovery of a genetically distinct L. infantum monophyletic group in the south-eastern Mediterranean stresses the importance of species genetic characterization towards better understanding

  6. The genetic defect in Cockayne syndrome is associated with a defect in repair of UV-induced DNA damage in transcriptionally active DNA

    International Nuclear Information System (INIS)

    Venema, J.; Mullenders, L.H.; Natarajan, A.T.; van Zeeland, A.A.; Mayne, L.V.

    1990-01-01

    Cells from patients with Cockayne syndrome (CS) are hypersensitive to UV-irradiation but have an apparently normal ability to remove pyrimidine dimers from the genome overall. We have measured the repair of pyrimidine dimers in defined DNA sequences in three normal and two CS cell strains. When compared to a nontranscribed locus, transcriptionally active genes were preferentially repaired in all three normal cell strains. There was no significant variation in levels of repair between various normal individuals or between two constitutively expressed genes, indicating that preferential repair may be a consistent feature of constitutively expressed genes in human cells. Neither CS strain, from independent complementation groups, was able to repair transcriptionally active DNA with a similar rate and to the same extent as normal cells, indicating that the genetic defect in CS lies in the pathway for repair of transcriptionally active DNA. These results have implications for understanding the pleiotropic clinical effects associated with disorders having defects in the repair of DNA damage. In particular, neurodegeneration appears to be associated with the loss of preferential repair of active genes and is not simply correlated with reduced levels of overall repair

  7. Probing localized strain in solution-derived YB a2C u3O7 -δ nanocomposite thin films

    Science.gov (United States)

    Guzman, Roger; Gazquez, Jaume; Mundet, Bernat; Coll, Mariona; Obradors, Xavier; Puig, Teresa

    2017-07-01

    Enhanced pinning due to nanoscale strain is unique to the high-Tc cuprates, where pairing may be modified with lattice distortion. Therefore a comprehensive understanding of the defect landscape is required for a broad range of applications. However, determining the type and distribution of defects and their associated strain constitutes a critical task, and for this aim, real-space techniques for atomic resolution characterization are necessary. Here, we use scanning transmission electron microscopy (STEM) to study the atomic structure of individual defects of solution-derived YB a2C u3O7 (YBCO) nanocomposites, where the inclusion of incoherent secondary phase nanoparticles within the YBCO matrix dramatically increases the density of Y1B a2C u4O8 (Y124) intergrowths, the commonest defect in YBCO thin films. The formation of the Y124 is found to trigger a concatenation of strain-derived interactions with other defects and the concomitant nucleation of intrinsic defects, which weave a web of randomly distributed nanostrained regions that profoundly transform the vortex-pinning landscape of the YBCO nanocomposite thin films.

  8. Unique properties associated with normal martensitic transition and strain glass transition – A simulation study

    International Nuclear Information System (INIS)

    Wang, Dong; Ni, Yan; Gao, Jinghui; Zhang, Zhen; Ren, Xiaobing; Wang, Yunzhi

    2013-01-01

    Highlights: ► We model the unique properties of strain glass which is different from that of normal martensite. ► We describe the importance of point defects in the formation of strain glass and related properties. ► The role of point defect can be attributed to global transition temperature effect (GTTE) and local field effect (LFE). -- Abstract: The transition behavior and unique properties associated with normal martensitic transition and strain glass transition are investigated by computer simulations using the phase field method. The simulations are based on a physical model that assumes that point defects alter the thermodynamic stability of martensite and create local lattice distortion. The simulation results show that strain glass transition exhibits different properties from those found in normal martensitic transformations. These unique properties include diffuse scattering pattern, “smear” elastic modulus peak, disappearance of heat flow peak and non-ergodicity. These simulation predictions agree well with the experimental observations

  9. A microdot multilayer oxide device: let us tune the strain-ionic transport interaction.

    Science.gov (United States)

    Schweiger, Sebastian; Kubicek, Markus; Messerschmitt, Felix; Murer, Christoph; Rupp, Jennifer L M

    2014-05-27

    In this paper, we present a strategy to use interfacial strain in multilayer heterostructures to tune their resistive response and ionic transport as active component in an oxide-based multilayer microdot device on chip. For this, fabrication of strained multilayer microdot devices with sideways attached electrodes is reported with the material system Gd0.1Ce0.9O(2-δ)/Er2O3. The fast ionic conducting Gd0.1Ce0.9O(2-δ) single layers are altered in lattice strain by the electrically insulating erbia phases of a microdot. The strain activated volume of the Gd0.1Ce0.9O(2-δ) is investigated by changing the number of individual layers from 1 to 60 while keeping the microdot at a constant thickness; i.e., the proportion of strained volume was systematically varied. Electrical measurements showed that the activation energy of the devices could be altered by Δ0.31 eV by changing the compressive strain of a microdot ceria-based phase by more than 1.16%. The electrical conductivity data is analyzed and interpreted with a strain volume model and defect thermodynamics. Additionally, an equivalent circuit model is presented for sideways contacted multilayer microdots. We give a proof-of-concept for microdot contacting to capture real strain-ionic transport effects and reveal that for classic top-electrode contacting the effect is nil, highlighting the need for sideways electric contacting on a nanoscopic scale. The near order ionic transport interaction is supported by Raman spectroscopy measurements. These were conducted and analyzed together with fully relaxed single thin film samples. Strain states are described relative to the strain activated volumes of Gd0.1Ce0.9O(2-δ) in the microdot multilayer. These findings reveal that strain engineering in microfabricated devices allows altering the ionic conduction over a wide range beyond classic doping strategies for single films. The reported fabrication route and concept of strained multilayer microdots is a promising path

  10. Strain induced room temperature ferromagnetism in epitaxial magnesium oxide thin films

    Energy Technology Data Exchange (ETDEWEB)

    Jin, Zhenghe; Kim, Ki Wook [Department of Electrical and Computer Engineering, North Carolina State University, Raleigh, North Carolina 27695 (United States); Nori, Sudhakar; Lee, Yi-Fang; Narayan, Jagdish [Department of Materials Science and Engineering, North Carolina State University, Raleigh, North Carolina 27695 (United States); Kumar, D. [Department of Mechanical Engineering, North Carolina A & T State University, Greensboro, North Carolina 27411 (United States); Wu, Fan [Princeton Institute for the Science and Technology of Materials (PRISM), Princeton University, Princeton, New Jersey 08540 (United States); Prater, J. T. [Materials Science Division, Army Research Office, Research Triangle Park, North Carolina 27709 (United States)

    2015-10-28

    We report on the epitaxial growth and room-temperature ferromagnetic properties of MgO thin films deposited on hexagonal c-sapphire substrates by pulsed laser deposition. The epitaxial nature of the films has been confirmed by both θ-2θ and φ-scans of X-ray diffraction pattern. Even though bulk MgO is a nonmagnetic insulator, we have found that the MgO films exhibit ferromagnetism and hysteresis loops yielding a maximum saturation magnetization up to 17 emu/cc and large coercivity, H{sub c} = 1200 Oe. We have also found that the saturation magnetization gets enhanced and that the crystallization degraded with decreased growth temperature, suggesting that the origin of our magnetic coupling could be point defects manifested by the strain in the films. X-ray (θ-2θ) diffraction peak shift and strain analysis clearly support the presence of strain in films resulting from the presence of point defects. Based on careful investigations using secondary ion mass spectrometer and X-ray photoelectron spectroscopy studies, we have ruled out the possibility of the presence of any external magnetic impurities. We discuss the critical role of microstructural characteristics and associated strain on the physical properties of the MgO films and establish a correlation between defects and magnetic properties.

  11. Influence of weld discontinuities on strain controlled fatigue behavior of 308 stainless steel weld metal

    International Nuclear Information System (INIS)

    Bhanu Sankara Rao, K.; Valsan, M.; Sandhya, R.; Mannan, S.L.; Rodriguez, P.

    1994-01-01

    Detailed investigations have been performed for assessing the importance of weld discontinuities in strain controlled low cycle fatigue (LCF) behavior of 308 stainless steel (SS) welds. The LCF behavior of 308 SS welds containing defects was compared with that of type 304 SS base material and 308 SS sound weld metal. Weld pads were prepared by shielded metal arc welding process. Porosity and slag inclusions were introduced deliberately into the weld metal by grossly exaggerating the conditions normally causing such defects. Total axial strain controlled LCF tests have been conducted in air at 823 K on type 304 SS base and 308 SS sound weld metal employing strain amplitudes in the range from ±0.25 to ±0.8 percent. A single strain amplitude of ±0.25 percent was used for all the tests conducted on weld samples containing defects. The results indicated that the base material undergoes cyclic hardening whereas sound and defective welds experience cyclic softening. Base metal showed higher fatigue life than sound weld metal at all strain amplitudes. The presence of porosity and slag inclusions in the weld metal led to significant reduction in life. Porosity on the specimen surface has been found to be particularly harmful and caused a reduction in life by a factor of seven relative to sound weld metal

  12. Printed strain sensors for early damage detection in engineering structures

    Science.gov (United States)

    Zymelka, Daniel; Yamashita, Takahiro; Takamatsu, Seiichi; Itoh, Toshihiro; Kobayashi, Takeshi

    2018-05-01

    In this paper, we demonstrate the analysis of strain measurements recorded using a screen-printed sensors array bonded to a metal plate and subjected to high strains. The analysis was intended to evaluate the capabilities of the printed strain sensors to detect abnormal strain distribution before actual defects (cracks) in the analyzed structures appear. The results demonstrate that the developed device can accurately localize the enhanced strains at the very early stage of crack formation. The promising performance and low fabrication cost confirm the potential suitability of the printed strain sensors for applications within the framework of structural health monitoring (SHM).

  13. ISC1-dependent metabolic adaptation reveals an indispensable role for mitochondria in induction of nuclear genes during the diauxic shift in Saccharomyces cerevisiae.

    Science.gov (United States)

    Kitagaki, Hiroshi; Cowart, L Ashley; Matmati, Nabil; Montefusco, David; Gandy, Jason; de Avalos, Silvia Vaena; Novgorodov, Sergei A; Zheng, Jim; Obeid, Lina M; Hannun, Yusuf A

    2009-04-17

    Growth of Saccharomyces cerevisiae following glucose depletion (the diauxic shift) depends on a profound metabolic adaptation accompanied by a global reprogramming of gene expression. In this study, we provide evidence for a heretofore unsuspected role for Isc1p in mediating this reprogramming. Initial studies revealed that yeast cells deleted in ISC1, the gene encoding inositol sphingolipid phospholipase C, which resides in mitochondria in the post-diauxic phase, showed defective aerobic respiration in the post-diauxic phase but retained normal intrinsic mitochondrial functions, including intact mitochondrial DNA, normal oxygen consumption, and normal mitochondrial polarization. Microarray analysis revealed that the Deltaisc1 strain failed to up-regulate genes required for nonfermentable carbon source metabolism during the diauxic shift, thus suggesting a mechanism for the defective supply of respiratory substrates into mitochondria in the post-diauxic phase. This defect in regulating nuclear gene induction in response to a defect in a mitochondrial enzyme raised the possibility that mitochondria may initiate diauxic shift-associated regulation of nucleus-encoded genes. This was established by demonstrating that in respiratory-deficient petite cells these genes failed to be up-regulated across the diauxic shift in a manner similar to the Deltaisc1 strain. Isc1p- and mitochondrial function-dependent genes significantly overlapped with Adr1p-, Snf1p-, and Cat8p-dependent genes, suggesting some functional link among these factors. However, the retrograde response was not activated in Deltaisc1, suggesting that the response of Deltaisc1 cannot be simply attributed to mitochondrial dysfunction. These results suggest a novel role for Isc1p in allowing the reprogramming of gene expression during the transition from anaerobic to aerobic metabolism.

  14. High-precision, whole-genome sequencing of laboratory strains facilitates genetic studies.

    Directory of Open Access Journals (Sweden)

    Anjana Srivatsan

    2008-08-01

    Full Text Available Whole-genome sequencing is a powerful technique for obtaining the reference sequence information of multiple organisms. Its use can be dramatically expanded to rapidly identify genomic variations, which can be linked with phenotypes to obtain biological insights. We explored these potential applications using the emerging next-generation sequencing platform Solexa Genome Analyzer, and the well-characterized model bacterium Bacillus subtilis. Combining sequencing with experimental verification, we first improved the accuracy of the published sequence of the B. subtilis reference strain 168, then obtained sequences of multiple related laboratory strains and different isolates of each strain. This provides a framework for comparing the divergence between different laboratory strains and between their individual isolates. We also demonstrated the power of Solexa sequencing by using its results to predict a defect in the citrate signal transduction pathway of a common laboratory strain, which we verified experimentally. Finally, we examined the molecular nature of spontaneously generated mutations that suppress the growth defect caused by deletion of the stringent response mediator relA. Using whole-genome sequencing, we rapidly mapped these suppressor mutations to two small homologs of relA. Interestingly, stable suppressor strains had mutations in both genes, with each mutation alone partially relieving the relA growth defect. This supports an intriguing three-locus interaction module that is not easily identifiable through traditional suppressor mapping. We conclude that whole-genome sequencing can drastically accelerate the identification of suppressor mutations and complex genetic interactions, and it can be applied as a standard tool to investigate the genetic traits of model organisms.

  15. Studies on intrinsic defects related to Zn vacancy in ZnO nanoparticles

    International Nuclear Information System (INIS)

    Singh, V.P.; Das, D.; Rath, Chandana

    2013-01-01

    Graphical abstract: Display Omitted Highlights: ► Williamson–Hall analysis of ZnO indicates strain in the lattice and size is of 20 nm. ► PL shows a broad emission peak in visible range due to native defects. ► Raman active modes corresponding to P6 3 mc and a few additional modes are observed. ► FTIR detects few local vibrational modes of hydrogen attached to zinc vacancies. ► V Zn -H and Zn + O divacancies are confirmed by PAS. -- Abstract: ZnO being a well known optoelectronic semiconductor, investigations related to the defects are very promising. In this report, we have attempted to detect the defects in ZnO nanoparticles synthesized by the conventional coprecipitation route using various spectroscopic techniques. The broad emission peak observed in photoluminescence spectrum and the non zero slope in Williamson–Hall analysis indicate the defects induced strain in the ZnO lattice. A few additional modes observed in Raman spectrum could be due to the breakdown of the translation symmetry of the lattice caused by defects and/or impurities. The presence of impurities can be ruled out as XRD pattern shows pure wurtzite structure. The presence of the vibrational band related to the Zn vacancies (V Zn ), unintentional hydrogen dopants and their complex defects confirm the defects in ZnO lattice. Positron life time components τ 1 and τ 2 additionally support V Zn attached to hydrogen and to a cluster of Zn and O di-vacancies respectively.

  16. Anisotropic chemical strain in cubic ceria due to oxygen-vacancy-induced elastic dipoles.

    Science.gov (United States)

    Das, Tridip; Nicholas, Jason D; Sheldon, Brian W; Qi, Yue

    2018-06-06

    Accurate characterization of chemical strain is required to study a broad range of chemical-mechanical coupling phenomena. One of the most studied mechano-chemically active oxides, nonstoichiometric ceria (CeO2-δ), has only been described by a scalar chemical strain assuming isotropic deformation. However, combined density functional theory (DFT) calculations and elastic dipole tensor theory reveal that both the short-range bond distortions surrounding an oxygen-vacancy and the long-range chemical strain are anisotropic in cubic CeO2-δ. The origin of this anisotropy is the charge disproportionation between the four cerium atoms around each oxygen-vacancy (two become Ce3+ and two become Ce4+) when a neutral oxygen-vacancy is formed. Around the oxygen-vacancy, six of the Ce3+-O bonds elongate, one of the Ce3+-O bond shorten, and all seven of the Ce4+-O bonds shorten. Further, the average and maximum chemical strain values obtained through tensor analysis successfully bound the various experimental data. Lastly, the anisotropic, oxygen-vacancy-elastic-dipole induced chemical strain is polarizable, which provides a physical model for the giant electrostriction recently discovered in doped and non-doped CeO2-δ. Together, this work highlights the need to consider anisotropic tensors when calculating the chemical strain induced by dilute point defects in all materials, regardless of their symmetry.

  17. Automatic classification of defects in weld pipe

    International Nuclear Information System (INIS)

    Anuar Mikdad Muad; Mohd Ashhar Hj Khalid; Abdul Aziz Mohamad; Abu Bakar Mhd Ghazali; Abdul Razak Hamzah

    2000-01-01

    With the advancement of computer imaging technology, the image on hard radiographic film can be digitized and stored in a computer and the manual process of defect recognition and classification may be replace by the computer. In this paper a computerized method for automatic detection and classification of common defects in film radiography of weld pipe is described. The detection and classification processes consist of automatic selection of interest area on the image and then classify common defects using image processing and special algorithms. Analysis of the attributes of each defect such as area, size, shape and orientation are carried out by the feature analysis process. These attributes reveal the type of each defect. These methods of defect classification result in high success rate. Our experience showed that sharp film images produced better results

  18. Automatic classification of defects in weld pipe

    International Nuclear Information System (INIS)

    Anuar Mikdad Muad; Mohd Ashhar Khalid; Abdul Aziz Mohamad; Abu Bakar Mhd Ghazali; Abdul Razak Hamzah

    2001-01-01

    With the advancement of computer imaging technology, the image on hard radiographic film can be digitized and stored in a computer and the manual process of defect recognition and classification may be replaced by the computer. In this paper, a computerized method for automatic detection and classification of common defects in film radiography of weld pipe is described. The detection and classification processes consist of automatic selection of interest area on the image and then classify common defects using image processing and special algorithms. Analysis of the attributes of each defect such area, size, shape and orientation are carried out by the feature analysis process. These attributes reveal the type of each defect. These methods of defect classification result in high success rate. Our experience showed that sharp film images produced better results. (Author)

  19. Size Effect of Defects on the Mechanical Properties of Graphene

    Science.gov (United States)

    Park, Youngho; Hyun, Sangil

    2018-03-01

    Graphene, a two-dimensional material, has been studied and utilized for its excellent material properties. In reality, achieving a pure single-crystalline structure in graphene is difficult, so usually graphene may have various types of defects in it. Vacancies, Stone-Wales defects, and grain boundaries can drastically change the material properties of graphene. Graphene with vacancy defects has been of interest because it is a two-dimensional analogy of three-dimensional porous materials. It has efficient material properties, and can function as a part of modern devices. The mechanical properties have been studied by using molecular dynamics for either a single vacancy defect with various sizes or multiple vacancy defects with same defect ratios. However, it is not clear which one has more influence on the mechanical properties between the size of the defects and the defect ratio. Therefore, we investigated the hole-size effect on the mechanical properties of single-crystalline graphene at various defect ratios. A void defect with large size can have a rather high tensile modulus with a low fracture strain compared to a void defect with small size. We numerically found that the tensile properties of scattered single vacancies is similar to that of amorphous graphene. We suspect that this is due to the local orbital change of the carbon atoms near the boundary of the void defects, so-called the interfacial phase.

  20. Atomic structure of surface defects in alumina studied by dynamic force microscopy: strain-relief-, translation- and reflection-related boundaries, including their junctions

    International Nuclear Information System (INIS)

    Simon, G H; König, T; Heinke, L; Lichtenstein, L; Heyde, M; Freund, H-J

    2011-01-01

    We present an extensive atomic resolution frequency modulation dynamic force microscopy study of ultrathin aluminium oxide on a single crystalline NiAl(110) surface. One-dimensional surface defects produced by domain boundaries have been resolved. Images are presented for reflection domain boundaries (RDBs), four different types of antiphase domain boundaries, a nucleation-related translation domain boundary and also domain boundary junctions. New structures and aspects of the boundaries and their network are revealed and merged into a comprehensive picture of the defect arrangements. The alumina film also covers the substrate completely at the boundaries and their junctions and follows the structural building principles found in its unit cell. This encompasses square and rectangular groups of surface oxygen sites. The observed structural elements can be related to the electronic signature of the boundaries and therefore to the electronic defects associated with the boundaries. A coincidence site lattice predicted for the RDBs is in good agreement with experimental data. With Σ = 19 it can be considered to be of low-sigma type, which frequently coincides with special boundary properties. Images of asymmetric RDBs show points of good contact alternating with regions of nearly amorphous disorder in the oxygen sublattice. (paper)

  1. Multi-gene phylogenetic analysis reveals that shochu-fermenting Saccharomyces cerevisiae strains form a distinct sub-clade of the Japanese sake cluster.

    Science.gov (United States)

    Futagami, Taiki; Kadooka, Chihiro; Ando, Yoshinori; Okutsu, Kayu; Yoshizaki, Yumiko; Setoguchi, Shinji; Takamine, Kazunori; Kawai, Mikihiko; Tamaki, Hisanori

    2017-10-01

    Shochu is a traditional Japanese distilled spirit. The formation of the distinguishing flavour of shochu produced in individual distilleries is attributed to putative indigenous yeast strains. In this study, we performed the first (to our knowledge) phylogenetic classification of shochu strains based on nucleotide gene sequences. We performed phylogenetic classification of 21 putative indigenous shochu yeast strains isolated from 11 distilleries. All of these strains were shown or confirmed to be Saccharomyces cerevisiae, sharing species identification with 34 known S. cerevisiae strains (including commonly used shochu, sake, ale, whisky, bakery, bioethanol and laboratory yeast strains and clinical isolate) that were tested in parallel. Our analysis used five genes that reflect genome-level phylogeny for the strain-level classification. In a first step, we demonstrated that partial regions of the ZAP1, THI7, PXL1, YRR1 and GLG1 genes were sufficient to reproduce previous sub-species classifications. In a second step, these five analysed regions from each of 25 strains (four commonly used shochu strains and the 21 putative indigenous shochu strains) were concatenated and used to generate a phylogenetic tree. Further analysis revealed that the putative indigenous shochu yeast strains form a monophyletic group that includes both the shochu yeasts and a subset of the sake group strains; this cluster is a sister group to other sake yeast strains, together comprising a sake-shochu group. Differences among shochu strains were small, suggesting that it may be possible to correlate subtle phenotypic differences among shochu flavours with specific differences in genome sequences. Copyright © 2017 John Wiley & Sons, Ltd. Copyright © 2017 John Wiley & Sons, Ltd.

  2. Whole genome PCR scanning reveals the syntenic genome structure of toxigenic Vibrio cholerae strains in the O1/O139 population.

    Directory of Open Access Journals (Sweden)

    Bo Pang

    Full Text Available Vibrio cholerae is commonly found in estuarine water systems. Toxigenic O1 and O139 V. cholerae strains have caused cholera epidemics and pandemics, whereas the nontoxigenic strains within these serogroups only occasionally lead to disease. To understand the differences in the genome and clonality between the toxigenic and nontoxigenic strains of V. cholerae serogroups O1 and O139, we employed a whole genome PCR scanning (WGPScanning method, an rrn operon-mediated fragment rearrangement analysis and comparative genomic hybridization (CGH to analyze the genome structure of different strains. WGPScanning in conjunction with CGH revealed that the genomic contents of the toxigenic strains were conservative, except for a few indels located mainly in mobile elements. Minor nucleotide variation in orthologous genes appeared to be the major difference between the toxigenic strains. rrn operon-mediated rearrangements were infrequent in El Tor toxigenic strains tested using I-CeuI digested pulsed-field gel electrophoresis (PFGE analysis and PCR analysis based on flanking sequence of rrn operons. Using these methods, we found that the genomic structures of toxigenic El Tor and O139 strains were syntenic. The nontoxigenic strains exhibited more extensive sequence variations, but toxin coregulated pilus positive (TCP+ strains had a similar structure. TCP+ nontoxigenic strains could be subdivided into multiple lineages according to the TCP type, suggesting the existence of complex intermediates in the evolution of toxigenic strains. The data indicate that toxigenic O1 El Tor and O139 strains were derived from a single lineage of intermediates from complex clones in the environment. The nontoxigenic strains with non-El Tor type TCP may yet evolve into new epidemic clones after attaining toxigenic attributes.

  3. Special Features of Strain Localization and Nanodipoles of Partial Disclinations in the Region of Elastic Distortions

    Science.gov (United States)

    Tyumentsev, A. N.; Ditenberg, I. A.; Sukhanov, I. I.

    2018-02-01

    In the zones of strain localization in the region of elastic distortions and nanodipoles of partial disclinations representing the defects of elastically deformed medium, a theoretical analysis of the elastically stressed state and the energy of these defects, including the cases of their transformation into more complex ensembles of interrelated disclinations, is performed. Using the analytical results, the mechanisms of strain localization are discussed in the stages of nucleation and propagation of the bands of elastic and plastic strain localization formed in these zones (including the cases of nanocrystalline structure formation).

  4. Inducing and manipulating magnetization in 2D zinc–oxide by strain and external voltage

    Science.gov (United States)

    Taivansaikhan, P.; Tsevelmaa, T.; Rhim, S. H.; Hong, S. C.; Odkhuu, D.

    2018-04-01

    Two-dimensional (2D) structures that exhibit intriguing magnetic phenomena such as perpendicular magnetic anisotropy and its switchable feature are of great interests in spintronics research. Herein, the density functional theory studies reveal the critical impacts of strain and external gating on vacancy-induced magnetism and its spin direction in a graphene-like single layer of zinc oxide (ZnO). In contrast to the pristine and defective ZnO with an O-vacancy, the presence of a Zn-vacancy induces significant magnetic moments to its first neighboring O and Zn atoms due to the charge deficit. We further predict that the direction of magnetization easy axis reverses from an in-plane to perpendicular orientation under a practically achievable biaxial compressive strain of only ~1–2% or applying an electric field by means of the charge density modulation. This magnetization reversal is mainly driven by the strain- and electric-field-induced changes in the spin–orbit coupled d states of the first-neighbor Zn atom to a Zn-vacancy. These findings open interesting prospects for exploiting strain and electric field engineering to manipulate magnetism and magnetization orientation of 2D materials.

  5. Spin-wave dispersion of nanostructured magnonic crystals with periodic defects

    Directory of Open Access Journals (Sweden)

    V. L. Zhang

    2016-11-01

    Full Text Available The spin-wave dispersions in nanostructured magnonic crystals with periodic defects have been mapped by Brillouin light scattering. The otherwise perfect crystals are one-dimensional arrays of alternating 460nm-wide Ni80Fe20 stripes and 40nm-wide air gaps, where one in ten Ni80Fe20 stripes is a defect of width other than 460 nm. Experimentally, the defects are manifested as additional Brillouin peaks, lying within the first and second bandgaps of the perfect crystal, whose frequencies decrease with increasing defect stripe width. Finite-element calculations, based on a supercell comprising one defect and nine perfect Py stripes, show that the defect modes are localized about the defects, with the localization exhibiting an approximate U-shaped dependence on defect size. Calculations also reveal extra magnon branches and the opening of mini-bandgaps, within the allowed bands of the perfect crystal, arising from Bragg reflections at the boundaries of the shorter supercell Brillouin zone. Simulated magnetization profiles of the band-edge modes of the major and mini-bandgaps reveal their different symmetries and localization properties. The findings could find application in microwave magnonic devices like single-frequency passband spin-wave filters.

  6. Aquaglyceroporin-null trypanosomes display glycerol transport defects and respiratory-inhibitor sensitivity.

    Directory of Open Access Journals (Sweden)

    Laura Jeacock

    2017-03-01

    Full Text Available Aquaglyceroporins (AQPs transport water and glycerol and play important roles in drug-uptake in pathogenic trypanosomatids. For example, AQP2 in the human-infectious African trypanosome, Trypanosoma brucei gambiense, is responsible for melarsoprol and pentamidine-uptake, and melarsoprol treatment-failure has been found to be due to AQP2-defects in these parasites. To further probe the roles of these transporters, we assembled a T. b. brucei strain lacking all three AQP-genes. Triple-null aqp1-2-3 T. b. brucei displayed only a very moderate growth defect in vitro, established infections in mice and recovered effectively from hypotonic-shock. The aqp1-2-3 trypanosomes did, however, display glycerol uptake and efflux defects. They failed to accumulate glycerol or to utilise glycerol as a carbon-source and displayed increased sensitivity to salicylhydroxamic acid (SHAM, octyl gallate or propyl gallate; these inhibitors of trypanosome alternative oxidase (TAO can increase intracellular glycerol to toxic levels. Notably, disruption of AQP2 alone generated cells with glycerol transport defects. Consistent with these findings, AQP2-defective, melarsoprol-resistant clinical isolates were sensitive to the TAO inhibitors, SHAM, propyl gallate and ascofuranone, relative to melarsoprol-sensitive reference strains. We conclude that African trypanosome AQPs are dispensable for viability and osmoregulation but they make important contributions to drug-uptake, glycerol-transport and respiratory-inhibitor sensitivity. We also discuss how the AQP-dependent inverse sensitivity to melarsoprol and respiratory inhibitors described here might be exploited.

  7. First interim examination of defected BWR and PWR rods tested in unlimited air at 2290C

    International Nuclear Information System (INIS)

    Einziger, R.E.; Cook, J.A.

    1983-01-01

    A five-year whole rod test was initiated to investigate the long-term stability of spent fuel rods under a variety of possible dry storage conditions. Both PWR and BWR rods were included in the test. The first interim examination was conducted after three months of testing to determine if there was any degradation in those defected rods stored in an unlimited air atmosphere. Visual observations, diametral measurements and radiographic smears were used to assess the degree of cladding deformation and particulate dispersal. The PWR rod showed no measurable change from the pre-test condition. The two original artificial defects had not changed in appearance and there was no diametral growth of the cladding. One of the defects in BWR rod showed significant deformation. There was approximately 10% cladding strain at the defect site and a small axial crack had formed. The fuel in the defect did not appear to be friable. The second defect showed no visible change and no cladding strain. Following examination, the test was continued at 230 0 C. Another interim examination is planned during the summer of 1983. This paper discusses the details and meaning of the data from the first interim examination

  8. Electronic and magnetic properties of MoS2 nanoribbons with sulfur line vacancy defects

    International Nuclear Information System (INIS)

    Han, Yang; Zhou, Jian; Dong, Jinming

    2015-01-01

    Highlights: • We performed DFT calculations on Sulfur line defects embedded MoS 2 . • The defects induced bond strains are larger in the zigzag (ZZ) edge ones. • The ZZ ones are metals, having two degenerate ground states FM and AFM. • The armchair ones are nonmagnetic semiconductors. • The defects can induce some defect states in the electronic structures. - Abstract: Motivated by the recent experimental result that single sulfur vacancies in monolayer MoS 2 are mobile under the electron beam and easily agglomerate into the sulfur line vacancy defects [Physical Review B 88, 035301(2013)] , the structural, electronic and magnetic properties of one dimensional zigzag (ZZ) and armchair (AC) edge MoS 2 nanoribbons with single or double staggered sulfur line vacancy defects (hereafter, abbreviated as SV or DV, respectively), parallel to their edges, have been investigated systematically by density functional theory calculations. It is very interesting to find that the bond strains induced by the sulfur line vacancy defect can cause a much larger out-of plane distortions in the ZZ edge MoS 2 nanoribbon than in the AC edge counterpart. Besides, the defective ZZ edge MoS 2 nanoribbons with SV or DV are both metals, having their two respective degenerate ground states with the same energy, among which one is ferromagnetic (FM “ + +”) and the other is antiferromagnetic (AFM “ + −”). But the AC edge MoS 2 nanoribbons with SV or DV are both nonmagnetic semiconductors, having very different gap values. Finally, the sulfur line vacancy defects would induce some defect states in the electronic structures of the defective MoS 2 nanoribbons. All these important results could provide a new route of tuning the electronic properties of MoS 2 nanoribbons and its derivatives for their promising applications in nanoelectronics and optoelectronics

  9. Defect-engineered graphene chemical sensors with ultrahigh sensitivity.

    Science.gov (United States)

    Lee, Geonyeop; Yang, Gwangseok; Cho, Ara; Han, Jeong Woo; Kim, Jihyun

    2016-05-25

    We report defect-engineered graphene chemical sensors with ultrahigh sensitivity (e.g., 33% improvement in NO2 sensing and 614% improvement in NH3 sensing). A conventional reactive ion etching system was used to introduce the defects in a controlled manner. The sensitivity of graphene-based chemical sensors increased with increasing defect density until the vacancy-dominant region was reached. In addition, the mechanism of gas sensing was systematically investigated via experiments and density functional theory calculations, which indicated that the vacancy defect is a major contributing factor to the enhanced sensitivity. This study revealed that defect engineering in graphene has significant potential for fabricating ultra-sensitive graphene chemical sensors.

  10. Fibrous metaphyseal defect (fibrous cortical defect, non-ossifying fibroma)

    International Nuclear Information System (INIS)

    Freyschmidt, J.; Saure, D.; Dammenhain, S.

    1981-01-01

    Fibrous cortical defect and nonossifying fibromas can be classified together as fibrous metaphyseal defects (FMD) since they have the same pahtological substrate, with a tendency to the same localisation around the knee, and occuring at the same age. They have a tendency to spontaneous healing, are clinically silent and are usually discovered accidentally during radiological examination. A radiological survey fo 5.674 metaphyseal regions in the upper and lower extremities of 2.065 unselected patients aged one to 20 years revealed an incidence of 1.8%; exlcusive examination of the distal femur showed an incidence of 2.7%. 96% of all lesions were in the lower extremities and only 4% in the upper. The marked discrepancy in the incidence rate between American and German publications is discussed. (orig.) [de

  11. Annealing effect of H+ -implanted single crystal silicon on strain and crystal structure

    International Nuclear Information System (INIS)

    Duo Xinzhong; Liu Weili; Zhang Miao; Gao Jianxia; Fu Xiaorong; Lin Chenglu

    2000-01-01

    The work focuses on the rocking curves of H + -implanted single silicon crystal detected by Four-Crystal X-ray diffractometer. The samples were annealed under different temperatures. Lattice defect in H + -implanted silicon crystals was detected by Rutherford Backscattering Spectrometry. It appeared that H-related complex did not crush until annealing temperature reached about 400 degree C. At that temperature H 2 was formed, deflated in silicon lattice and strained the lattice. But defects did not come into being in large quantity. The lattice was undamaged. When annealing temperature reached 500 degree C, strain induced by H 2 deflation crashed the silicon lattice. A large number of defects were formed. At the same time bubbles in the crystal and blister/flaking on the surface could be observed

  12. Trichoderma reesei xylanase 5 is defective in the reference strain QM6a but functional alleles are present in other wild-type strains.

    Science.gov (United States)

    Ramoni, Jonas; Marchetti-Deschmann, Martina; Seidl-Seiboth, Verena; Seiboth, Bernhard

    2017-05-01

    Trichoderma reesei is a paradigm for the regulation and industrial production of plant cell wall-degrading enzymes. Among these, five xylanases, including the glycoside hydrolase (GH) family 11 XYN1 and XYN2, the GH10 XYN3, and the GH30 XYN4 and XYN6, were described. By genome mining and transcriptome analysis, a further putative xylanase, encoded by xyn5, was identified. Analysis of xyn5 from the genome-sequenced reference strain T. reesei QM6a shows that it encodes a non-functional, truncated form of XYN5. However, non-truncated orthologues are present in other genome sequenced Trichoderma spp., and sequencing of xyn5 in other T. reesei wild-type isolates shows that they harbor a putative functional xyn5 allele. In silico analysis and 3D modeling revealed that the encoded XYN5 has significant structural similarities to xylanases of the GH11 family, including a GH-typical substrate binding groove and a carboxylate pair in the active site. The xyn5 of wild-type strain TUCIM1282 was recombinantly expressed in a T. reesei strain with a (hemi)cellulase-free background and the corresponding protein purified to apparent homogeneity. The pH and temperature optima and the kinetic parameters of the purified XYN5 were pH 4, 50 °C, and V max  = 2646 nkat/mg with a K m of 9.68 mg/ml. This functional xyn5 allele was used to replace the mutated version which led to an overall increase of the xylanolytic activity. These findings are of particular importance as GH11 xylanases are of high biotechnological relevance, and T. reesei is one of the main industrial producers of such lignocellulose-degrading enzymes.

  13. Strain mapping near a triple junction in strained Ni-based alloy using EBSD and biaxial nanogauges

    Energy Technology Data Exchange (ETDEWEB)

    Clair, A. [Laboratoire Interdisciplinaire Carnot de Bourgogne, UMR 5209 CNRS, Universite de Bourgogne, 9 Avenue Alain Savary, BP 47870, 21078 Dijon Cedex (France); Foucault, M.; Calonne, O. [Areva ANP, Centre Technique Departement Corrosion-Chimie, 30 Bd de l' industrie, BP 181, 71205 Le Creusot (France); Lacroute, Y.; Markey, L.; Salazar, M.; Vignal, V. [Laboratoire Interdisciplinaire Carnot de Bourgogne, UMR 5209 CNRS, Universite de Bourgogne, 9 Avenue Alain Savary, BP 47870, 21078 Dijon Cedex (France); Finot, E., E-mail: Eric.Finot@u-bourgogne.fr [Laboratoire Interdisciplinaire Carnot de Bourgogne, UMR 5209 CNRS, Universite de Bourgogne, 9 Avenue Alain Savary, BP 47870, 21078 Dijon Cedex (France)

    2011-05-15

    Research highlights: > Surface strains measured using nanogauge were compared to the texture obtained by EBSD. > Statistics of the principal strain discern the grains according to the Schmid factor. > Strain hotspots were localized near a triple junction of alloy 600 under tensile loading. > Asymetrical profile of the GB strains is a criterion for surface cracking initiation. - Abstract: A key element for analyzing the crack initiation in strained polycrystalline alloys is the local quantification of the surface strain distribution according to the grain texture. Using electron backscattered diffraction, the local microstructure was determined to both localize a triple junction and deduce the local Schmid factors. Kernel average misorientation (KAM) was also used to map the areas of defect concentration. The maximum principal strain and the in-plane shear strain were quantified using the biaxial nanogauge. Distortions of the array of nanodots used as spot markers were analyzed near the triple junction. The crystallographic orientation and the surface strain were then investigated both statistically for each grain and locally at the grain boundaries. The superimposition of microstructure and strain maps allows the high strain gradient (reaching 3-fold the applied strain) to be localized at preferential grain boundaries near the triple junction. The Schmid factors and the KAM were compared to the maximum principal strain and the in-plane shear strain respectively. The polycrystalline deformation was attributable first to the rotation of some grains, followed by the elongation of all grains along their preferential activated slip systems.

  14. Whole-genome characterization of Uruguayan strains of avian infectious bronchitis virus reveals extensive recombination between the two major South American lineages.

    Science.gov (United States)

    Marandino, Ana; Tomás, Gonzalo; Panzera, Yanina; Greif, Gonzalo; Parodi-Talice, Adriana; Hernández, Martín; Techera, Claudia; Hernández, Diego; Pérez, Ruben

    2017-10-01

    Infectious bronchitis virus (Gammacoronavirus, Coronaviridae) is a genetically variable RNA virus that causes one of the most persistent respiratory diseases in poultry. The virus is classified in genotypes and lineages with different epidemiological relevance. Two lineages of the GI genotype (11 and 16) have been widely circulating for decades in South America. GI-11 is an exclusive South American lineage while the GI-16 lineage is distributed in Asia, Europe and South America. Here, we obtained the whole genome of two Uruguayan strains of the GI-11 and GI-16 lineages using Illumina high-throughput sequencing. The strains here sequenced are the first obtained in South America for the infectious bronchitis virus and provide new insights into the origin, spreading and evolution of viral variants. The complete genome of the GI-11 and GI-16 strains have 27,621 and 27,638 nucleotides, respectively, and possess the same genomic organization. Phylogenetic incongruence analysis reveals that both strains have a mosaic genome that arose by recombination between Euro Asiatic strains of the GI-16 lineage and ancestral South American GI-11 viruses. The recombination occurred in South America and produced two viral variants that have retained the full-length S1 sequences of the parental lineages but are extremely similar in the rest of their genomes. These recombinant virus have been extraordinary successful, persisting in the continent for several years with a notorious wide geographic distribution. Our findings reveal a singular viral dynamics and emphasize the importance of complete genomic characterization to understand the emergence and evolutionary history of viral variants. Copyright © 2017 Elsevier B.V. All rights reserved.

  15. Atrial septal defect in a Korean wild raccoon dog.

    Science.gov (United States)

    Yim, Soomi; Choi, Sooyoung; Kim, Jongtaek; Chung, Jin-Young; Park, Inchul

    2017-10-07

    An approximately two-year-old, male 6.1 kg body weight, Korean wild raccoon dog (Nyctereutes procyonoides koreensis) was captured by the wildlife medical rescue center of Kangwon National University. Upon physical examination, the heart rate was 87 beats per min and there were no clinical signs. The hematological, and blood biochemical profiles revealed no remarkable findings; however, thoracic radiographs showed cardiac enlargement, especially in the right atrium. On electrocardiogram, sinus node dysfunction and bradyarrhythmia were revealed. Echocardiography showed a left-to-right shunting atrial septal defect. Based on these findings, this Korean wild raccoon dog was diagnosed with atrial septal defect. This is the rare case report of atrial septal defect in wildlife.

  16. Electronic and magnetic properties of MoS{sub 2} nanoribbons with sulfur line vacancy defects

    Energy Technology Data Exchange (ETDEWEB)

    Han, Yang [Group of Computational Condensed Matter Physics, National Laboratory of Solid State Microstructures and Department of Physics, Nanjing University, Nanjing 210093 (China); Zhou, Jian [National Laboratory of Solid State Microstructures and Department of Materials Science and Engineering, Nanjing University, Nanjing 210093 (China); Dong, Jinming, E-mail: jdong@nju.edu.cn [Group of Computational Condensed Matter Physics, National Laboratory of Solid State Microstructures and Department of Physics, Nanjing University, Nanjing 210093 (China)

    2015-08-15

    Highlights: • We performed DFT calculations on Sulfur line defects embedded MoS{sub 2}. • The defects induced bond strains are larger in the zigzag (ZZ) edge ones. • The ZZ ones are metals, having two degenerate ground states FM and AFM. • The armchair ones are nonmagnetic semiconductors. • The defects can induce some defect states in the electronic structures. - Abstract: Motivated by the recent experimental result that single sulfur vacancies in monolayer MoS{sub 2} are mobile under the electron beam and easily agglomerate into the sulfur line vacancy defects [Physical Review B 88, 035301(2013)] , the structural, electronic and magnetic properties of one dimensional zigzag (ZZ) and armchair (AC) edge MoS{sub 2} nanoribbons with single or double staggered sulfur line vacancy defects (hereafter, abbreviated as SV or DV, respectively), parallel to their edges, have been investigated systematically by density functional theory calculations. It is very interesting to find that the bond strains induced by the sulfur line vacancy defect can cause a much larger out-of plane distortions in the ZZ edge MoS{sub 2} nanoribbon than in the AC edge counterpart. Besides, the defective ZZ edge MoS{sub 2} nanoribbons with SV or DV are both metals, having their two respective degenerate ground states with the same energy, among which one is ferromagnetic (FM “ + +”) and the other is antiferromagnetic (AFM “ + −”). But the AC edge MoS{sub 2} nanoribbons with SV or DV are both nonmagnetic semiconductors, having very different gap values. Finally, the sulfur line vacancy defects would induce some defect states in the electronic structures of the defective MoS{sub 2} nanoribbons. All these important results could provide a new route of tuning the electronic properties of MoS{sub 2} nanoribbons and its derivatives for their promising applications in nanoelectronics and optoelectronics.

  17. Pupillary anomaly masquerading as a glaucomatous visual field defect: a case report

    Directory of Open Access Journals (Sweden)

    Tey Adrian

    2004-06-01

    Full Text Available Abstract Background Patients are often referred to ophthalmologists with focal visual field defects on routine testing, possibly related to a potential diagnosis of glaucoma. However, examination of the individual patient's ocular characteristics as well as facial characteristics may often reveal a cause of the visual field defect. Case presentation We describe a patient who was found to have a superior visual field defect on routine testing by the optician. Repeat perimetry with pharmacological dilatation of the pupil revealed that the cause of the field defect was related to an eccentric inferiorly displaced pupil, secondary to trauma some years previously. Discussion Individual patient characteristics, including both ocular, as well as facial, need to be considered, when interpreting any visual field defect.

  18. Molecular typing of Brucella melitensis endemic strains and differentiation from the vaccine strain Rev-1.

    Science.gov (United States)

    Noutsios, Georgios T; Papi, Rigini M; Ekateriniadou, Loukia V; Minas, Anastasios; Kyriakidis, Dimitrios A

    2012-03-01

    In the present study forty-four Greek endemic strains of Br. melitensis and three reference strains were genotyped by Multi locus Variable Number Tandem Repeat (ML-VNTR) analysis based on an eight-base pair tandem repeat sequence that was revealed in eight loci of Br. melitensis genome. The forty-four strains were discriminated from the vaccine strain Rev-1 by Restriction Fragment Length Polymorphism (RFLP) and Denaturant Gradient Gel Electrophoresis (DGGE). The ML-VNTR analysis revealed that endemic, reference and vaccine strains are genetically closely related, while most of the loci tested (1, 2, 4, 5 and 7) are highly polymorphic with Hunter-Gaston Genetic Diversity Index (HGDI) values in the range of 0.939 to 0.775. Analysis of ML-VNTRs loci stability through in vitro passages proved that loci 1 and 5 are non stable. Therefore, vaccine strain can be discriminated from endemic strains by allele's clusters of loci 2, 4, 6 and 7. RFLP and DGGE were also employed to analyse omp2 gene and reveled different patterns among Rev-1 and endemic strains. In RFLP, Rev-1 revealed three fragments (282, 238 and 44 bp), while endemic strains two fragments (238 and 44 bp). As for DGGE, the electrophoretic mobility of Rev-1 is different from the endemic strains due to heterologous binding of DNA chains of omp2a and omp2b gene. Overall, our data show clearly that it is feasible to genotype endemic strains of Br. melitensis and differentiate them from vaccine strain Rev-1 with ML-VNTR, RFLP and DGGE techniques. These tools can be used for conventional investigations in brucellosis outbreaks.

  19. Thermodynamics of diffusion under pressure and stress: Relation to point defect mechanisms

    International Nuclear Information System (INIS)

    Aziz, M.J.

    1997-01-01

    A thermodynamic formalism is developed for illuminating the predominant point defect mechanism of self- and impurity diffusion in silicon and is used to provide a rigorous basis for point defect-based interpretation of diffusion experiments in biaxially strained epitaxial layers in the Si endash Ge system. A specific combination of the hydrostatic and biaxial stress dependences of the diffusivity is ±1 times the atomic volume, depending upon whether the predominant mechanism involves vacancies or interstitials. Experimental results for Sb diffusion in biaxially strained Si endash Ge films and ab initio calculations of the activation volume for Sb diffusion by a vacancy mechanism are in quantitative agreement with no free parameters. Key parameters are identified that must be measured or calculated for a quantitative test of interstitial-based mechanisms. copyright 1997 American Institute of Physics

  20. Survival and SOS response induction in ultraviolet B irradiated Escherichia coli cells with defective repair mechanisms.

    Science.gov (United States)

    Prada Medina, Cesar Augusto; Aristizabal Tessmer, Elke Tatjana; Quintero Ruiz, Nathalia; Serment-Guerrero, Jorge; Fuentes, Jorge Luis

    2016-06-01

    Purpose In this paper, the contribution of different genes involved in DNA repair for both survival and SOS induction in Escherichia coli mutants exposed to ultraviolet B radiation (UVB, [wavelength range 280-315 nm]) was evaluated. Materials and methods E. coli strains defective in uvrA, oxyR, recO, recN, recJ, exoX, recB, recD or xonA genes were used to determine cell survival. All strains also had the genetic sulA::lacZ fusion, which allowed for the quantification of SOS induction through the SOS Chromotest. Results Five gene products were particularly important for survival, as follows: UvrA > RecB > RecO > RecJ > XonA. Strains defective in uvrA and recJ genes showed elevated SOS induction compared with the wild type, which remained stable for up to 240 min after UVB-irradiation. In addition, E. coli strains carrying the recO or recN mutation showed no SOS induction. Conclusions The nucleotide excision and DNA recombination pathways were equally used to repair UVB-induced DNA damage in E. coli cells. The sulA gene was not turned off in strains defective in UvrA and RecJ. RecO protein was essential for processing DNA damage prior to SOS induction. In this study, the roles of DNA repair proteins and their contributions to the mechanisms that induce SOS genes in E. coli are proposed.

  1. Tunneling and migration of the dumbbell defect in electron irradiated aluminum-zinc alloys

    International Nuclear Information System (INIS)

    Wallace, P.W.

    1983-01-01

    Ultrasonic attenuation and velocity measurements have been made on irradiated Al-Zn alloys (Zn concentrations of .01%, .1%, and .5% atomic). They provide strong evidence for a tunneling relaxation of the predominant mixed dumbbell defect at low temperatures and for mixed dumbbell migration at the Stage II anneal temperature. The effect of an internal strain varying with the zinc concentration of the measured decrement and modulus change is striking. Evaluated in the framework of a six level system, this reveals the simultaneous action of resonance and non-classical relaxation processes. Using Fe as a probe atom, it is shown that mixed dumbbell dissociation is in an insignificant component of the annealing of this defect. The decrease of the annealing temperature at higher zinc concentrations provides evidence that the mixed dumbbell migrates as a unit during annealing. The energies associated with dumbbell migration and interstitial escape are derived. Further evidence for the migration mechanism is obtained from successive irradiation and annealing measurements on the Al-Zn .01% alloy, and from a comparison of these results with published radiation damage rate measurements of dilute Al-Zn alloys

  2. Effect of strain field on displacement cascade in tungsten studied by molecular dynamics simulation

    Energy Technology Data Exchange (ETDEWEB)

    Wang, D. [Institute of Modern Physics, Chinese Academy of Sciences, Lanzhou 730000 (China); University of Chinese Academy of Sciences, Beijing 100049 (China); Gao, N., E-mail: ning.gao@impcas.ac.cn [Institute of Modern Physics, Chinese Academy of Sciences, Lanzhou 730000 (China); Wang, Z.G., E-mail: zhgwang@impcas.ac.cn [Institute of Modern Physics, Chinese Academy of Sciences, Lanzhou 730000 (China); Gao, X. [Institute of Modern Physics, Chinese Academy of Sciences, Lanzhou 730000 (China); He, W.H. [Institute of Modern Physics, Chinese Academy of Sciences, Lanzhou 730000 (China); University of Chinese Academy of Sciences, Beijing 100049 (China); Cui, M.H.; Pang, L.L.; Zhu, Y.B. [Institute of Modern Physics, Chinese Academy of Sciences, Lanzhou 730000 (China)

    2016-10-01

    Using atomistic methods, the coupling effect of strain field and displacement cascade in body-centered cubic (BCC) tungsten is directly simulated by molecular dynamics (MD) simulations at different temperatures. The values of the hydrostatic and uniaxial (parallel or perpendicular to primary knock-on atom (PKA) direction) strains are from −2% to 2% and the temperature is from 100 to 1000 K. Because of the annealing effect, the influence of strain on radiation damage at low temperature has been proved to be more significant than that at high temperature. When the cascade proceeds under the hydrostatic strain, the Frenkel Pair (FP) production, the fraction of defect in cluster and the average size of the defect cluster, all increase at tensile state and decrease at compressive state. When the cascade is under uniaxial strain, the effect of strain parallel to PKA direction is less than the effect of hydrostatic strain, while the effect of strain perpendicular to PKA direction can be negligible. Under the uniaxial strain along 〈1 1 1〉 direction, the SIA and SIA cluster is observed to orientate along the strain direction at tensile state and the uniaxial compressive strain with direction perpendicular to 〈1 1 1〉 has led to the similar preferred nucleation. All these results indicate that under irradiation, the tensile state should be avoided for materials used in nuclear power plants.

  3. Antisite Defects of the L12 Structure Determined by the Phase Field Microelasticity Model

    International Nuclear Information System (INIS)

    Jing, Zhang; Zheng, Chen; Yan-Li, Lu; Yong-Xin, Wang; Yan, Zhao

    2009-01-01

    A phase field microelasticity simulation is performed to examine the antisite defect of L1 2 -Ni 3 Al in Ni 75 Al 5.3 V 19.7 ternary alloy. Combinimg strain energy with the phase field model leads to an atom configuration change as time proceeds. For the Ni sublattice, the antisite defect Al Ni , the equilibrium occupancy probability (OP) of which declines, precedes Ni Ni and V Ni in reaching equilibrium; subsequently, Ni Ni and V Ni present a phenomenon of symmetrical rise and decline individually. Similarly, for the Al sublattice, the antisite defect Ni Al , the OP of which eventually rises, takes fewer time steps than Al Ai and V Al to attain equilibrium. Thereafter, Al Al rises while V Al declines symmetrically at the axes of the Ni Al MAI curve. Furthermore, the OP for the Al sublattice is much more sensitive to strain energy than that for the Ni sublattice. (condensed matter: structure, mechanical and thermal properties)

  4. Defect studies of thin ZnO films prepared by pulsed laser deposition

    International Nuclear Information System (INIS)

    Vlček, M; Čížek, J; Procházka, I; Novotný, M; Bulíř, J; Lančok, J; Anwand, W; Brauer, G; Mosnier, J-P

    2014-01-01

    Thin ZnO films were grown by pulsed laser deposition on four different substrates: sapphire (0 0 0 1), MgO (1 0 0), fused silica and nanocrystalline synthetic diamond. Defect studies by slow positron implantation spectroscopy (SPIS) revealed significantly higher concentration of defects in the studied films when compared to a bulk ZnO single crystal. The concentration of defects in the films deposited on single crystal sapphire and MgO substrates is higher than in the films deposited on amorphous fused silica substrate and nanocrystalline synthetic diamond. Furthermore, the effect of deposition temperature on film quality was investigated in ZnO films deposited on synthetic diamond substrates. Defect studies performed by SPIS revealed that the concentration of defects firstly decreases with increasing deposition temperature, but at too high deposition temperatures it increases again. The lowest concentration of defects was found in the film deposited at 450° C.

  5. Electronic properties of polycrystalline graphene under large local strain

    International Nuclear Information System (INIS)

    He, Xin; Tang, Ning; Duan, Junxi; Mei, Fuhong; Meng, Hu; Lu, Fangchao; Xu, Fujun; Yang, Xuelin; Gao, Li; Wang, Xinqiang; Shen, Bo; Ge, Weikun

    2014-01-01

    To explore the transport properties of polycrystalline graphene under large tensile strain, a strain device has been fabricated using piezocrystal to load local strain onto graphene, up to 22.5%. Ionic liquid gate whose capability of tuning carrier density being much higher than that of a solid gate is used to survey the transfer characteristics of the deformed graphene. The conductance of the Dirac point and field effect mobility of electrons and holes is found to decrease with increasing strain, which is attributed to the scattering of the graphene grain boundaries, the strain induced change of band structure, and defects. However, the transport gap is still not opened. Our study is helpful to evaluate the application of graphene in stretchable electronics.

  6. An Inducible Operon Is Involved in Inulin Utilization in Lactobacillus plantarum Strains, as Revealed by Comparative Proteogenomics and Metabolic Profiling.

    Science.gov (United States)

    Buntin, Nirunya; Hongpattarakere, Tipparat; Ritari, Jarmo; Douillard, François P; Paulin, Lars; Boeren, Sjef; Shetty, Sudarshan A; de Vos, Willem M

    2017-01-15

    The draft genomes of Lactobacillus plantarum strains isolated from Asian fermented foods, infant feces, and shrimp intestines were sequenced and compared to those of well-studied strains. Among 28 strains of L. plantarum, variations in the genomic features involved in ecological adaptation were elucidated. The genome sizes ranged from approximately 3.1 to 3.5 Mb, of which about 2,932 to 3,345 protein-coding sequences (CDS) were predicted. The food-derived isolates contained a higher number of carbohydrate metabolism-associated genes than those from infant feces. This observation correlated to their phenotypic carbohydrate metabolic profile, indicating their ability to metabolize the largest range of sugars. Surprisingly, two strains (P14 and P76) isolated from fermented fish utilized inulin. β-Fructosidase, the inulin-degrading enzyme, was detected in the supernatants and cell wall extracts of both strains. No activity was observed in the cytoplasmic fraction, indicating that this key enzyme was either membrane-bound or extracellularly secreted. From genomic mining analysis, a predicted inulin operon of fosRABCDXE, which encodes β-fructosidase and many fructose transporting proteins, was found within the genomes of strains P14 and P76. Moreover, pts1BCA genes, encoding sucrose-specific IIBCA components involved in sucrose transport, were also identified. The proteomic analysis revealed the mechanism and functional characteristic of the fosRABCDXE operon involved in the inulin utilization of L. plantarum The expression levels of the fos operon and pst genes were upregulated at mid-log phase. FosE and the LPXTG-motif cell wall anchored β-fructosidase were induced to a high abundance when inulin was present as a carbon source. Inulin is a long-chain carbohydrate that may act as a prebiotic, which provides many health benefits to the host by selectively stimulating the growth and activity of beneficial bacteria in the colon. While certain lactobacilli can catabolize

  7. Factors affecting finite strain estimation in low-grade, low-strain clastic rocks

    Science.gov (United States)

    Pastor-Galán, Daniel; Gutiérrez-Alonso, Gabriel; Meere, Patrick A.; Mulchrone, Kieran F.

    2009-12-01

    The computer strain analysis methods SAPE, MRL and DTNNM have permitted the characterization of finite strain in two different regions with contrasting geodynamic scenarios; (1) the Talas Ala Tau (Tien Shan, Kyrgyzs Republic) and (2) the Somiedo Nappe and Narcea Antiform (Cantabrian to West Asturian-Leonese Zone boundary, Variscan Belt, NW of Iberia). The performed analyses have revealed low-strain values and the regional strain trend in both studied areas. This study also investigates the relationship between lithology (grain size and percentage of matrix) and strain estimates the two methodologies used. The results show that these methods are comparable and the absence of significant finite strain lithological control in rocks deformed under low metamorphic and low-strain conditions.

  8. Implications of permeation through intrinsic defects in graphene on the design of defect-tolerant membranes for gas separation.

    Science.gov (United States)

    Boutilier, Michael S H; Sun, Chengzhen; O'Hern, Sean C; Au, Harold; Hadjiconstantinou, Nicolas G; Karnik, Rohit

    2014-01-28

    Gas transport through intrinsic defects and tears is a critical yet poorly understood phenomenon in graphene membranes for gas separation. We report that independent stacking of graphene layers on a porous support exponentially decreases flow through defects. On the basis of experimental results, we develop a gas transport model that elucidates the separate contributions of tears and intrinsic defects on gas leakage through these membranes. The model shows that the pore size of the porous support and its permeance critically affect the separation behavior, and reveals the parameter space where gas separation can be achieved regardless of the presence of nonselective defects, even for single-layer membranes. The results provide a framework for understanding gas transport in graphene membranes and guide the design of practical, selectively permeable graphene membranes for gas separation.

  9. Defect characterization in compositionally graded InGaAs layers on GaAs(001) grown by MBE

    International Nuclear Information System (INIS)

    Sasaki, Takuo; Takahasi, Masamitu; Norman, Andrew G.; Romero, Manuel J.; Al-Jassim, Mowafak M.; Kojima, Nobuaki; Ohshita, Yoshio; Yamaguchi, Masafumi

    2013-01-01

    Defect characterization in molecular beam epitaxial (MBE) compositionally-graded In x Ga 1-x As layers on GaAs substrates consisting different thickness of overshooting (OS) layers was carried out using cathodoluminescence (CL) and transmission electron microscopy (TEM). We found that the thickness of the OS layer influences not only stress but also lattice defects generated in a top InGaAs layer. While the top InGaAs layer with a thin OS layer is under compression and has mainly threading dislocations, the top layer with a thick OS layer is under tension and exhibits inhomogeneous strain associating with phase separation. We will discuss the mechanisms of defect generation and their in-plane distribution based on strain relaxation at the top and OS layers. (copyright 2013 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim) (orig.)

  10. Atomic-scale Ge diffusion in strained Si revealed by quantitative scanning transmission electron microscopy

    Science.gov (United States)

    Radtke, G.; Favre, L.; Couillard, M.; Amiard, G.; Berbezier, I.; Botton, G. A.

    2013-05-01

    Aberration-corrected scanning transmission electron microscopy is employed to investigate the local chemistry in the vicinity of a Si0.8Ge0.2/Si interface grown by molecular-beam epitaxy. Atomic-resolution high-angle annular dark field contrast reveals the presence of a nonuniform diffusion of Ge from the substrate into the strained Si thin film. On the basis of multislice calculations, a model is proposed to quantify the experimental contrast, showing that the Ge concentration in the thin film reaches about 4% at the interface and decreases monotonically on a typical length scale of 10 nm. Diffusion occurring during the growth process itself therefore appears as a major factor limiting the abruptness of interfaces in the Si-Ge system.

  11. Herpes simplex virus type 1 strain KOS carries a defective US9 and a mutated US8A gene.

    Science.gov (United States)

    Negatsch, Alexandra; Mettenleiter, Thomas C; Fuchs, Walter

    2011-01-01

    The membrane protein encoded by the US9 gene of alphaherpesviruses plays an important role during virion assembly and transport in neurons. Here, we demonstrate that in herpes simplex virus type 1 (HSV-1) strain KOS, due to base substitutions, the predicted TATA-box of US9 is mutated, and a premature stop is present at codon 58 of US9, which contains 91 codons in other HSV-1 strains. The TATA-box mutation also removes the native stop codon of the adjacent US8A gene, leading to extension of the coding region from 160 to 191 codons. Northern blot analyses revealed reduced transcription of US9 in cells infected with HSV-1 KOS. Moreover, a US9-specific antiserum did not detect any gene products in Western blot and immunofluorescence analyses of KOS-infected cells, indicating that the truncated protein is not stable. In contrast, Western blot reactions of a pUS8A-specific antiserum confirmed enlargement of this protein in HSV-1 KOS.

  12. The estimation of defects influence on lifetime of NPP equipment components

    International Nuclear Information System (INIS)

    Ovchinikov, A.V.; Vasilchenko, G.S.; Rivkin, E.Y.

    1998-01-01

    Estimating the influence of defects on NPP components lifetime requires several typical operations: testing the objects without destroying the means of control, scheme of detected defects and performing calculations. The basic methods for revealing defects are ultrasonic, radiographic and visual control. A technique was developed for lifetime calculation of reactor equipment with defects using minimum information about defects and properties of material. The experience obtained during several years has shown good results. Experimental data of tests concerning destruction of construction elements showed good reliability

  13. Characterization of the biocontrol activity of pseudomonas fluorescens strain X reveals novel genes regulated by glucose.

    Directory of Open Access Journals (Sweden)

    Gerasimos F Kremmydas

    Full Text Available Pseudomonas fluorescens strain X, a bacterial isolate from the rhizosphere of bean seedlings, has the ability to suppress damping-off caused by the oomycete Pythium ultimum. To determine the genes controlling the biocontrol activity of strain X, transposon mutagenesis, sequencing and complementation was performed. Results indicate that, biocontrol ability of this isolate is attributed to gcd gene encoding glucose dehydrogenase, genes encoding its co-enzyme pyrroloquinoline quinone (PQQ, and two genes (sup5 and sup6 which seem to be organized in a putative operon. This operon (named supX consists of five genes, one of which encodes a non-ribosomal peptide synthase. A unique binding site for a GntR-type transcriptional factor is localized upstream of the supX putative operon. Synteny comparison of the genes in supX revealed that they are common in the genus Pseudomonas, but with a low degree of similarity. supX shows high similarity only to the mangotoxin operon of Ps. syringae pv. syringae UMAF0158. Quantitative real-time PCR analysis indicated that transcription of supX is strongly reduced in the gcd and PQQ-minus mutants of Ps. fluorescens strain X. On the contrary, transcription of supX in the wild type is enhanced by glucose and transcription levels that appear to be higher during the stationary phase. Gcd, which uses PQQ as a cofactor, catalyses the oxidation of glucose to gluconic acid, which controls the activity of the GntR family of transcriptional factors. The genes in the supX putative operon have not been implicated before in the biocontrol of plant pathogens by pseudomonads. They are involved in the biosynthesis of an antimicrobial compound by Ps. fluorescens strain X and their transcription is controlled by glucose, possibly through the activity of a GntR-type transcriptional factor binding upstream of this putative operon.

  14. Impact of the Botrytis cinerea strain and metabolism on (-)-geosmin production by Penicillium expansum in grape juice.

    Science.gov (United States)

    La Guerche, Stéphane; De Senneville, Laure; Blancard, Dominique; Darriet, Philippe

    2007-10-01

    Geosmin, an off-flavour of some rotten grapes, has been implicated in wine defects. Botrytis cinerea and Penicillium expansum were the most common among the numerous microorganisms isolated from rotten grapes. P. expansum produces geosmin on model media but not healthy grape juice. However, geosmin synthesis by P. expansum was demonstrated in grape juice and on crushed grapes that had been pre-cultured with certain B. cinerea strains. 34 out of 156 B. cinerea strains ([bot +] phenotype) isolated from the centre of grape bunches were able to induce high geosmin production, up to 494 ng/l, by P. expansum in grape juice. A study of the impact of grape juice composition on geosmin synthesis by P. expansum revealed the importance of nitrogen composition, particularly amino-acid deficiency. Metabolism of amino acids by B. cinerea was shown to be favourable to geosmin synthesis by P. expansum. However, the amino-acid and ammonium concentrations in grape juices pre-cultured with B. cinerea [bot -] and [bot +] strains were very similar implying that other factors are involved as well. Indeed, an ethanol-precipitable fraction, probably a polysaccharide, synthesized by B. cinerea [bot -], but not [bot +] strains, inhibited geosmin production by P. expansum.

  15. Tuning thermal conduction via extended defects in graphene

    Science.gov (United States)

    Huang, Huaqing; Xu, Yong; Zou, Xiaolong; Wu, Jian; Duan, Wenhui

    2013-05-01

    Designing materials for desired thermal conduction can be achieved via extended defects. We theoretically demonstrate the concept by investigating thermal transport in graphene nanoribbons (GNRs) with the extended line defects observed by recent experiments. Our nonequilibrium Green's function study excluding phonon-phonon interactions finds that thermal conductance can be tuned over wide ranges (more than 50% at room temperature), by controlling the orientation and the bond configuration of the embedded extended defect. Further transmission analysis reveals that the thermal-conduction tuning is attributed to two fundamentally different mechanisms, via modifying the phonon dispersion and/or tailoring the strength of defect scattering. The finding, applicable to other materials, provides useful guidance for designing materials with desired thermal conduction.

  16. Association between left ventricular perfusion defects and myocardial deformation indexes in heart transplantation recipients.

    Science.gov (United States)

    D'Andrea, Antonello; De Rimini, Maria Luisa; America, Raffaella; Cirillo, Chiara; Riegler, Lucia; Limongelli, Giuseppe; D'Alto, Michele; Salerno, Gemma; Maiello, Ciro; Muto, Pietro; Russo, Maria Giovanna; Calabrò, Raffaele; Bossone, Eduardo; Pacileo, Giuseppe

    2017-10-01

    The aim of the study was to analyze possible correlations between strain echocardiography (STE) and PET myocardial perfusion in a population of heart transplantation (HTx) recipients showing preserved left ventricular (LV) ejection fraction. By STE, LV global longitudinal strain (LV GLS) was lower in HTx. PET showed no transient or chronic ischemia in 83 of 115 HTx (73%). Fixed perfusion defects were observed in 17% of HTx and reversible ischemia in 10%. Significant coronary stenosis was observed only in 10 cases. GLS was independently associated with age at HTx and fixed perfusion defects (HR 0.41; P<.001). Such relationships underline STE ability to early identify HTx pts with subclinical myocardial dysfunction during long-term follow-up. © 2017, Wiley Periodicals, Inc.

  17. Defect Engineering and Interface Phenomena in Tin Oxide

    KAUST Repository

    Albar, Arwa

    2017-04-05

    The advance in transparent electronics requires high-performance transparent conducting oxide materials. The microscopic properties of these materials are sensitive to the presence of defects and interfaces and thus fundamental understanding is required for materials engineering. In this thesis, first principles density functional theory is used to investigate the possibility of tuning the structural, electronic and magnetic properties of tin oxide by means of defects and interfaces. Our aim is to reveal unique properties and the parameters to control them as well as to explain the origin of unique phenomena in oxide materials. The stability of native defect in tin monoxide (SnO) under strain is investigated using formation energy calculations. We find that the conductivity (which is controlled by native defects) can be switched from p-type to either n-type or undoped semiconducting by means of applied pressure. We then target inducing magnetism in SnO by 3d transition metal doping. We propose that V doping is efficient to realize spin polarization at high temperature. We discuss different tin oxide interfaces. Metallic states are found to form at the SnO/SnO2 interface with electronic properties that depend on the interface terminations. The origin of these states is explained in terms of charge transfer caused by chemical bonding and band alignment. For the SnO/SnO2 heterostructure, we observe the formation of a two dimensional hole gas at the interface, which is surprising as it cannot be explained by the standard polar catastrophe model. Thus, we propose a charge density discontinuity model to explain our results. The model can be generalized to other polar-polar interfaces. Motivated by technological applications, the electronic and structural properties of the MgO (100)/SnO2 (110) interface are investigated. Depending on the interface termination, we observe the formation of a two dimensional electron gas or spin polarized hole gas. Aiming to identify further

  18. The effect of point defects on ferroelastic phase transition of lanthanum-doped calcium titanate ceramics

    International Nuclear Information System (INIS)

    Ni, Yan; Zhang, Zhen; Wang, Dong; Wang, Yu; Ren, Xiaobing

    2013-01-01

    Highlights: ► The effect of point defects on phase transitions in Ca (1−x) La 2x/3 TiO 3 was studied. ► When x = 0.45, normal ferroelastic phase transition happens. ► When x = 0.7, a “glassy-like” frozen process appears. ► Point defects weaken the thermodynamic stability of ferroelastic phase. ► Point defects induce a “glassy-like” frozen process. -- Abstract: In the present paper, La-doped CaTiO 3 is studied to investigate the effect of point defects on ferroelastic phase transition of the ceramics. The dynamic mechanical measurements show that the transition temperature of the orthorhombic to tetragonal phase transition of Ca (1−x) La 2x/3 TiO 3 decreases with increasing dopant (La) concentration x. The samples with the dopant content of x = 0.45 and 0.7 exhibit different structure evolution features during their transition processes as revealed by in situ powder X-ray diffraction (XRD) measurement. Moreover, when x = 0.7, the storage modulus shows a frequency-dependent minimum at T g , which can be well fitted with the Vogel–Fulcher relation, and the corresponding internal friction also exhibits a frequency-dependent peak within the same temperature regime. These results thus indicate that doping La suppresses ferroelastic phase transition in CaTiO 3 and induces a “glassy-like” behavior in Ca (1−x) La 2x/3 TiO 3 , which is similar to “strain glass” in Ni-doped Ti 50−x Ni 50+x

  19. Imaging active topological defects in carbon nanotubes

    Science.gov (United States)

    Suenaga, Kazu; Wakabayashi, Hideaki; Koshino, Masanori; Sato, Yuta; Urita, Koki; Iijima, Sumio

    2007-06-01

    A single-walled carbon nanotube (SWNT) is a wrapped single graphene layer, and its plastic deformation should require active topological defects-non-hexagonal carbon rings that can migrate along the nanotube wall. Although in situ transmission electron microscopy (TEM) has been used to examine the deformation of SWNTs, these studies deal only with diameter changes and no atomistic mechanism has been elucidated experimentally. Theory predicts that some topological defects can form through the Stone-Wales transformation in SWNTs under tension at 2,000 K, and could act as a dislocation core. We demonstrate here, by means of high-resolution (HR)-TEM with atomic sensitivity, the first direct imaging of pentagon-heptagon pair defects found in an SWNT that was heated at 2,273 K. Moreover, our in situ HR-TEM observation reveals an accumulation of topological defects near the kink of a deformed nanotube. This result suggests that dislocation motions or active topological defects are indeed responsible for the plastic deformation of SWNTs.

  20. Single ventricle cardiac defect

    International Nuclear Information System (INIS)

    Eren, B.; Turkmen, N.; Fedakar, R.; Cetin, V.

    2010-01-01

    Single ventricle heart is defined as a rare cardiac abnormality with a single ventricle chamber involving diverse functional and physiological defects. Our case is of a ten month-old baby boy who died shortly after admission to the hospital due to vomiting and diarrhoea. Autopsy findings revealed cyanosis of finger nails and ears. Internal examination revealed; large heart, weighing 60 grams, single ventricle, without a septum and upper membranous part. Single ventricle is a rare pathology, hence, this paper aims to discuss this case from a medico-legal point of view. (author)

  1. High Strain Rate and Shock-Induced Deformation in Metals

    Science.gov (United States)

    Ravelo, Ramon

    2012-02-01

    Large-scale non-equilibrium molecular Dynamics (MD) simulations are now commonly used to study material deformation at high strain rates (10^9-10^12 s-1). They can provide detailed information-- such as defect morphology, dislocation densities, and temperature and stress profiles, unavailable or hard to measure experimentally. Computational studies of shock-induced plasticity and melting in fcc and bcc single, mono-crystal metals, exhibit generic characteristics: high elastic limits, large directional anisotropies in the yield stress and pre-melting much below the equilibrium melt temperature for shock wave propagation along specific crystallographic directions. These generic features in the response of single crystals subjected to high strain rates of deformation can be explained from the changes in the energy landscape of the uniaxially compressed crystal lattice. For time scales relevant to dynamic shock loading, the directional-dependence of the yield strength in single crystals is shown to be due to the onset of instabilities in elastic-wave propagation velocities. The elastic-plastic transition threshold can accurately be predicted by a wave-propagation stability analysis. These strain-induced instabilities create incipient defect structures, which can be quite different from the ones, which characterize the long-time, asymptotic state of the compressed solid. With increase compression and strain rate, plastic deformation via extended defects gives way to amorphization associated with the loss in shear rigidity along specific deformation paths. The hot amorphous or (super-cooled liquid) metal re-crystallizes at rates, which depend on the temperature difference between the amorphous solid and the equilibrium melt line. This plastic-amorphous transition threshold can be computed from shear-waves stability analyses. Examples from selected fcc and bcc metals will be presented employing semi-empirical potentials of the embedded atom method (EAM) type as well as

  2. A semi-mechanistic approach to calculate the probability of fuel defects

    International Nuclear Information System (INIS)

    Tayal, M.; Millen, E.; Sejnoha, R.

    1992-10-01

    In this paper the authors describe the status of a semi-mechanistic approach to the calculation of the probability of fuel defects. This approach expresses the defect probability in terms of fundamental parameters such as local stresses, local strains, and fission product concentration. The calculations of defect probability continue to reflect the influences of the conventional parameters like power ramp, burnup and CANLUB. In addition, the new approach provides a mechanism to account for the impacts of additional factors involving detailed fuel design and reactor operation, for example pellet density, pellet shape and size, sheath diameter and thickness, pellet/sheath clearance, and coolant temperature and pressure. The approach has been validated against a previous empirical correlation. AN illustrative example shows how the defect thresholds are influenced by changes in the internal design of the element and in the coolant pressure. (Author) (7 figs., tab., 12 refs.)

  3. Defect Structure of Localized Excitons in a WSe2 Monolayer

    KAUST Repository

    Zhang, Shuai

    2017-07-26

    The atomic and electronic structure of intrinsic defects in a WSe2 monolayer grown on graphite was revealed by low temperature scanning tunneling microscopy and spectroscopy. Instead of chalcogen vacancies that prevail in other transition metal dichalcogenide materials, intrinsic defects in WSe2 arise surprisingly from single tungsten vacancies, leading to the hole (p-type) doping. Furthermore, we found these defects to dominate the excitonic emission of the WSe2 monolayer at low temperature. Our work provided the first atomic-scale understanding of defect excitons and paved the way toward deciphering the defect structure of single quantum emitters previously discovered in the WSe2 monolayer.

  4. Dislocation defect interaction in irradiated Cu

    International Nuclear Information System (INIS)

    Schaeublin, R.; Yao, Z.; Spaetig, P.; Victoria, M.

    2005-01-01

    Pure Cu single crystals irradiated at room temperature to low doses with 590 MeV protons have been deformed in situ in a transmission electron microscope in order to identify the basic mechanisms at the origin of hardening. Cu irradiated to 10 -4 dpa shows at room temperature a yield shear stress of 13.7 MPa to be compared to the 8.8 MPa of the unirradiated Cu. Irradiation induced damage consists at 90% of 2 nm stacking fault tetrahedra, the remaining being dislocation loops and unidentified defects. In-situ deformation reveals that dislocation-defect interaction can take several forms. Usually, dislocations pinned by defects bow out under the applied stress and escape without leaving any visible defect. From the escape angles obtained at 183 K, an average critical stress of 100 MPa is deduced. In some cases, the pinning of dislocations leads to debris that are about 20 nm long, which formation could be recorded during the in situ experiment

  5. Phylogenetic and genome-wide deep-sequencing analyses of canine parvovirus reveal co-infection with field variants and emergence of a recent recombinant strain.

    Directory of Open Access Journals (Sweden)

    Ruben Pérez

    Full Text Available Canine parvovirus (CPV, a fast-evolving single-stranded DNA virus, comprises three antigenic variants (2a, 2b, and 2c with different frequencies and genetic variability among countries. The contribution of co-infection and recombination to the genetic variability of CPV is far from being fully elucidated. Here we took advantage of a natural CPV population, recently formed by the convergence of divergent CPV-2c and CPV-2a strains, to study co-infection and recombination. Complete sequences of the viral coding region of CPV-2a and CPV-2c strains from 40 samples were generated and analyzed using phylogenetic tools. Two samples showed co-infection and were further analyzed by deep sequencing. The sequence profile of one of the samples revealed the presence of CPV-2c and CPV-2a strains that differed at 29 nucleotides. The other sample included a minor CPV-2a strain (13.3% of the viral population and a major recombinant strain (86.7%. The recombinant strain arose from inter-genotypic recombination between CPV-2c and CPV-2a strains within the VP1/VP2 gene boundary. Our findings highlight the importance of deep-sequencing analysis to provide a better understanding of CPV molecular diversity.

  6. Phylogenetic and Genome-Wide Deep-Sequencing Analyses of Canine Parvovirus Reveal Co-Infection with Field Variants and Emergence of a Recent Recombinant Strain

    Science.gov (United States)

    Pérez, Ruben; Calleros, Lucía; Marandino, Ana; Sarute, Nicolás; Iraola, Gregorio; Grecco, Sofia; Blanc, Hervé; Vignuzzi, Marco; Isakov, Ofer; Shomron, Noam; Carrau, Lucía; Hernández, Martín; Francia, Lourdes; Sosa, Katia; Tomás, Gonzalo; Panzera, Yanina

    2014-01-01

    Canine parvovirus (CPV), a fast-evolving single-stranded DNA virus, comprises three antigenic variants (2a, 2b, and 2c) with different frequencies and genetic variability among countries. The contribution of co-infection and recombination to the genetic variability of CPV is far from being fully elucidated. Here we took advantage of a natural CPV population, recently formed by the convergence of divergent CPV-2c and CPV-2a strains, to study co-infection and recombination. Complete sequences of the viral coding region of CPV-2a and CPV-2c strains from 40 samples were generated and analyzed using phylogenetic tools. Two samples showed co-infection and were further analyzed by deep sequencing. The sequence profile of one of the samples revealed the presence of CPV-2c and CPV-2a strains that differed at 29 nucleotides. The other sample included a minor CPV-2a strain (13.3% of the viral population) and a major recombinant strain (86.7%). The recombinant strain arose from inter-genotypic recombination between CPV-2c and CPV-2a strains within the VP1/VP2 gene boundary. Our findings highlight the importance of deep-sequencing analysis to provide a better understanding of CPV molecular diversity. PMID:25365348

  7. X-ray sensitive strains of CHO cells show decreased frequency of stable transfection

    International Nuclear Information System (INIS)

    Jeggo, P.; Smith, J.

    1987-01-01

    Six X-ray sensitive (xrs) strains of the Chinese hamster ovary cell line have previously been isolated and shown to have a defect in double strand break rejoining. In this study, these strains have been investigated for their ability to take up and integrate foreign DNA. All the xrs strains investigated so far have shown a decreased frequency of stable transfectants compared to their parent line, in experiments using the plasmid pSV2gpt, which contains the selectable bacterial gene, guanine phosphoribosyl transferase. This decreased frequency is observed over a wide range of DNA concentrations (0.1 to 20 μg DNA) but is more pronounced at higher DNA concentrations. In contrast, these xrs strains show the same level of transfection proficiency as the wild type parent using a transient transfection system with a plasmid containing the bacterial CAT (chloramphenicol acetyl transferase) gene. Since the level of CAT activity does not depend on integration of foreign DNA, this suggests that the xrs strains are able to take up the same amount of DNA as the parent strains, but have a defect in the integration of foreign DNA. Since this integration of foreign DNA probably occurs by non-homologous recombination, this may indicate a role of the xrs gene product in this process

  8. Point defects in ZnO crystals grown by various techniques

    International Nuclear Information System (INIS)

    Čížek, J; Vlček, M; Hruška, P; Lukáč, F; Melikhova, O; Anwand, W; Selim, F; Hugenschmidt, Ch; Egger, W

    2017-01-01

    In the present work point defects in ZnO crystals were characterized by positron lifetime spectroscopy combined with back-diffusion measurement of slow positrons. Defects in ZnO crystals grown by various techniques were compared. Hydrothermally grown ZnO crystals contain defects characterized by lifetime of ≈181 ps. These defects were attributed to Zn vacancies associated with hydrogen. ZnO crystals prepared by other techniques (Bridgman, pressurized melt growth, and seeded chemical vapour transport) exhibit shorter lifetime of ≈165 ps. Positron back-diffusion studies revealed that hydrothermally grown ZnO crystals contain higher density of defects than the crystals grown by other techniques. The lowest concentration of defects was detected in the crystal grown by seeded chemical vapor transport. (paper)

  9. Paediatric post-traumatic cortical defects of the distal radius

    International Nuclear Information System (INIS)

    Roach, Richard T.; Summers, Bruce N.; Cassar-Pullicino, Victor

    2002-01-01

    Paediatric post-traumatic cortical defects, although rare, are predominately seen affecting the distal radius following a greenstick or torus fracture. We review the literature and present a further two cases supported by CT and MRI. Images from an acute greenstick fracture are also presented to help understand the pathogenesis. Defects are typically solitary on plain radiographs and are usually noticed late, proximal to the site of compression. They are non-expansile in an otherwise healthy child. CT and MRI may reveal smaller multiple subperiosteal defects. Typical defects require no further management other than reassurance and advice that they may occasionally cause discomfort but resolve with time. (orig.)

  10. Cytoskeletal defects in Bmpr2-associated pulmonary arterial hypertension.

    Science.gov (United States)

    Johnson, Jennifer A; Hemnes, Anna R; Perrien, Daniel S; Schuster, Manfred; Robinson, Linda J; Gladson, Santhi; Loibner, Hans; Bai, Susan; Blackwell, Tom R; Tada, Yuji; Harral, Julie W; Talati, Megha; Lane, Kirk B; Fagan, Karen A; West, James

    2012-03-01

    The heritable form of pulmonary arterial hypertension (PAH) is typically caused by a mutation in bone morphogenic protein receptor type 2 (BMPR2), and mice expressing Bmpr2 mutations develop PAH with features similar to human disease. BMPR2 is known to interact with the cytoskeleton, and human array studies in PAH patients confirm alterations in cytoskeletal pathways. The goal of this study was to evaluate cytoskeletal defects in BMPR2-associated PAH. Expression arrays on our Bmpr2 mutant mouse lungs revealed cytoskeletal defects as a prominent molecular consequence of universal expression of a Bmpr2 mutation (Rosa26-Bmpr2(R899X)). Pulmonary microvascular endothelial cells cultured from these mice have histological and functional cytoskeletal defects. Stable transfection of different BMPR2 mutations into pulmonary microvascular endothelial cells revealed that cytoskeletal defects are common to multiple BMPR2 mutations and are associated with activation of the Rho GTPase, Rac1. Rac1 defects are corrected in cell culture and in vivo through administration of exogenous recombinant human angiotensin-converting enzyme 2 (rhACE2). rhACE2 reverses 77% of gene expression changes in Rosa26-Bmpr2(R899X) transgenic mice, in particular, correcting defects in cytoskeletal function. Administration of rhACE2 to Rosa26-Bmpr2(R899X) mice with established PAH normalizes pulmonary pressures. Together, these findings suggest that cytoskeletal function is central to the development of BMPR2-associated PAH and that intervention against cytoskeletal defects may reverse established disease.

  11. Influence of defect mobility on electrostrain in acceptor-doped Ba0.80Sr0.20TiO3

    Directory of Open Access Journals (Sweden)

    K. Vani

    2012-12-01

    Full Text Available This study reports significant differences in the defect-mediated electrostrain in B-site trivalent ions (Fe3+ and Mn3+ doped Barium titanate based system. Electron Paramagnetic Resonance (EPR Spectroscopy has been employed as a structural probe for understanding the symmetry of defects. Differences in the reorientation of the defect dipoles have been correlated with the electrostrain. Mechanism for the higher strain in Mn-doped system has also been explained.

  12. Extended defects and hydrogen interactions in ion implanted silicon

    Science.gov (United States)

    Rangan, Sanjay

    The structural and electrical properties of extended defects generated because of ion implantation and the interaction of hydrogen with these defects have been studied in this work. Two distinct themes have been studied, the first where defects are a detrimental and the second where they are useful. In the first scenario, transient enhanced diffusion of boron has been studied and correlated with defect evolution studies due to silicon and argon ion implants. Spreading resistance profiles (SRP) correlated with deep level transient spectroscopy (DLTS) measurements, reveal that a low anneal temperatures (TED at low anneal temperatures (550°C, the effect of hydrogen is lost, due to its out-diffusion. Moreover, due to catastrophic out-diffusion of hydrogen, additional damage is created resulting in deeper junctions in hydrogenated samples, compared to the non-hydrogenated ones. Comparing defect evolution due to Si and Ar ion implants at different anneal temperatures, while the type of defects is the same in the two cases, their (defect) dissolution occurs at lower anneal temperatures (˜850°C) for Si implants. Dissolution for Ar implants seems to occur at higher anneal temperatures. The difference has been attributed to the increased number of vacancies created by Ar to that of silicon implant. In second aspect, nano-cavity formation due to vacancy agglomeration has been studied by helium ion implantation and furnace anneal, where the effect of He dose, implant energy and anneal time have been processing parameters that have been varied. Cavities are formed only when the localized concentration of He is greater than 3 x 1020 cm-3. While at high implant doses, a continuous cavity layer is formed, at low implant doses a discontinuous layer is observed. The formation of cavities at low doses has been observed for the first time. Variation of anneal times reveal that cavities are initially facetted (for short anneal times) and tend to become spherical when annealed for

  13. Defects and defect processes in nonmetallic solids

    CERN Document Server

    Hayes, W

    2004-01-01

    This extensive survey covers defects in nonmetals, emphasizing point defects and point-defect processes. It encompasses electronic, vibrational, and optical properties of defective solids, plus dislocations and grain boundaries. 1985 edition.

  14. Metamorphosis of strain/stress on optical band gap energy of ZAO thin films via manipulation of thermal annealing process

    International Nuclear Information System (INIS)

    Malek, M.F.; Mamat, M.H.; Musa, M.Z.; Soga, T.; Rahman, S.A.; Alrokayan, Salman A.H.; Khan, Haseeb A.; Rusop, M.

    2015-01-01

    We report on the growth of Al-doped ZnO (ZAO) thin films prepared by the sol–gel technique associated with dip-coating onto Corning 7740 glass substrates. The influence of varying thermal annealing (T a ) temperature on crystallisation behaviour, optical and electrical properties of ZAO films has been systematically investigated. All films are polycrystalline with a hexagonal wurtzite structure with a preferential orientation according to the direction 〈0 0 2〉. The metamorphosis of strain/stress effects in ZAO thin films has been investigated using X-ray diffraction. The as growth films have a large compressive stress of 0.55 GPa, which relaxed to 0.25 GPa as the T a was increased to 500 °C. Optical parameters such as optical transmittance, absorption coefficient, refractive index and optical band gap energy have been studied and discussed with respect to T a . All films exhibit a transmittance above 80–90% along the visible–NIR range up to 1500 nm and a sharp absorption onset below 400 nm corresponding to the fundamental absorption edge of ZnO. Experimental results show that the tensile stress in the films reveals an incline pattern with the optical band gap energy, while the compressive stress shows opposite relation. - Highlights: • Minimum stress of highly c-axis oriented ZAO was grown at suitable T a temperature. • The ZAO crystal orientation was influenced by strain/stress of the film. • Minimum stress/strain of ZAO film leads to lower defects. • Bandgap and defects were closely intertwined with strain/stress. • We report additional optical and electrical properties based on T a temperature

  15. Metamorphosis of strain/stress on optical band gap energy of ZAO thin films via manipulation of thermal annealing process

    Energy Technology Data Exchange (ETDEWEB)

    Malek, M.F., E-mail: firz_solarzelle@yahoo.com [NANO-ElecTronic Centre (NET), Faculty of Electrical Engineering, Universiti Teknologi MARA (UiTM), 40450 Shah Alam, Selangor (Malaysia); NANO-SciTech Centre (NST), Institute of Science (IOS), Universiti Teknologi MARA UiTM, 40450 Shah Alam, Selangor (Malaysia); Mamat, M.H. [NANO-ElecTronic Centre (NET), Faculty of Electrical Engineering, Universiti Teknologi MARA (UiTM), 40450 Shah Alam, Selangor (Malaysia); Musa, M.Z. [NANO-ElecTronic Centre (NET), Faculty of Electrical Engineering, Universiti Teknologi MARA (UiTM), 40450 Shah Alam, Selangor (Malaysia); Faculty of Electrical Engineering, Universiti Teknologi MARA (UiTM) Pulau Pinang, Jalan Permatang Pauh, 13500 Permatang Pauh, Pulau Pinang (Malaysia); Soga, T. [Department of Frontier Materials, Nagoya Institute of Technology (NITech), Nagoya 466-8555 (Japan); Rahman, S.A. [Low Dimensional Materials Research Centre (LDMRC), Department of Physics, Faculty of Science, Universiti Malaya (UM), 50603 Kuala Lumpur (Malaysia); Alrokayan, Salman A.H.; Khan, Haseeb A. [Department of Biochemistry, College of Science, King Saud University (KSU), Riyadh 11451 (Saudi Arabia); Rusop, M. [NANO-ElecTronic Centre (NET), Faculty of Electrical Engineering, Universiti Teknologi MARA (UiTM), 40450 Shah Alam, Selangor (Malaysia); NANO-SciTech Centre (NST), Institute of Science (IOS), Universiti Teknologi MARA UiTM, 40450 Shah Alam, Selangor (Malaysia)

    2015-04-15

    We report on the growth of Al-doped ZnO (ZAO) thin films prepared by the sol–gel technique associated with dip-coating onto Corning 7740 glass substrates. The influence of varying thermal annealing (T{sub a}) temperature on crystallisation behaviour, optical and electrical properties of ZAO films has been systematically investigated. All films are polycrystalline with a hexagonal wurtzite structure with a preferential orientation according to the direction 〈0 0 2〉. The metamorphosis of strain/stress effects in ZAO thin films has been investigated using X-ray diffraction. The as growth films have a large compressive stress of 0.55 GPa, which relaxed to 0.25 GPa as the T{sub a} was increased to 500 °C. Optical parameters such as optical transmittance, absorption coefficient, refractive index and optical band gap energy have been studied and discussed with respect to T{sub a}. All films exhibit a transmittance above 80–90% along the visible–NIR range up to 1500 nm and a sharp absorption onset below 400 nm corresponding to the fundamental absorption edge of ZnO. Experimental results show that the tensile stress in the films reveals an incline pattern with the optical band gap energy, while the compressive stress shows opposite relation. - Highlights: • Minimum stress of highly c-axis oriented ZAO was grown at suitable T{sub a} temperature. • The ZAO crystal orientation was influenced by strain/stress of the film. • Minimum stress/strain of ZAO film leads to lower defects. • Bandgap and defects were closely intertwined with strain/stress. • We report additional optical and electrical properties based on T{sub a} temperature.

  16. Revealing the properties of defects formed by CH3NH2 molecules in organic-inorganic hybrid perovskite MAPbBr3

    Science.gov (United States)

    Wang, Ji; Zhang, Ao; Yan, Jun; Li, Dan; Chen, Yunlin

    2017-03-01

    The properties of defects in organic-inorganic hybrid perovskite are widely studied from the first-principles calculation. However, the defects of methylamine (methylamine = CH3NH2), which would be easily formed during the preparation of the organic-inorganic hybrid perovskite, are rarely investigated. Thermodynamic properties as well as defect states of methylamine embedded MAPbX3 (MA = methyl-ammonium = CH3NH3, X = Br, I) are studied based on first-principles calculations of density functional theory. It was found that there is a shallow defect level near the highest occupied molecular orbital, which induced by the interstitial methylamine defect in MAPbBr3, will lead to an increase of photoluminescence. The calculation results showed that interstitial defect states of methylamine may move deeper due to the interaction between methylamine molecules and methyl-ammonium cations. It was also showed that the interstitial methylamine defect is stable at room temperature, and the defect can be removed easily by annealing.

  17. Human fibroblast strain with normal survival but abnormal postreplication repair after ultraviolet light irradiation

    International Nuclear Information System (INIS)

    Doniger, J.; Barrett, S.F.; Robbins, J.H.

    1980-01-01

    Postreplication repair has been studied in ultraviolet light (UV-irradiated) fibroblast strains derived from eight apparently normal control donors and seven xeroderma pigmentosum patients. One control donor strain had an intermediate defect in postreplication repair similar to that in excision-deficient xeroderma pigmentosum fibroblasts. However, unlike the xeroderma pigmentosum strains, this control donor strain had normal UV-induced unscheduled DNA synthesis and normal survival after irradiation with UV. This unique fibroblast strain should be useful in studies designed to elucidate the possible role of postreplication repair in UV-induced carcinogenesis and mutagenesis

  18. Occipital Proton Magnetic Resonance Spectroscopy ((1)H-MRS) Reveals Normal Metabolite Concentrations in Retinal Visual Field Defects

    NARCIS (Netherlands)

    Boucard, Christine C.; Hoogduin, Johannes M.; van der Grond, Jeroen; Cornelissen, Frans W.

    2007-01-01

    Background. Progressive visual field defects, such as age-related macular degeneration and glaucoma, prevent normal stimulation of visual cortex. We investigated whether in the case of visual field defects, concentrations of metabolites such as N-acetylaspartate (NAA), a marker for degenerative

  19. Laboratory-Cultured Strains of the Sea Anemone Exaiptasia Reveal Distinct Bacterial Communities

    KAUST Repository

    Herrera Sarrias, Marcela; Ziegler, Maren; Voolstra, Christian R.; Aranda, Manuel

    2017-01-01

    Exaiptasia is a laboratory sea anemone model system for stony corals. Two clonal strains are commonly used, referred to as H2 and CC7, that originate from two genetically distinct lineages and that differ in their Symbiodinium specificity. However, little is known about their other microbial associations. Here, we examined and compared the taxonomic composition of the bacterial assemblages of these two symbiotic Exaiptasia strains, both of which have been cultured in the laboratory long-term under identical conditions. We found distinct bacterial microbiota for each strain, indicating the presence of host-specific microbial consortia. Putative differences in the bacterial functional profiles (i.e., enrichment and depletion of various metabolic processes) based on taxonomic inference were also detected, further suggesting functional differences of the microbiomes associated with these lineages. Our study contributes to the current knowledge of the Exaiptasia holobiont by comparing the bacterial diversity of two commonly used strains as models for coral research.

  20. Laboratory-Cultured Strains of the Sea Anemone Exaiptasia Reveal Distinct Bacterial Communities

    KAUST Repository

    Herrera Sarrias, Marcela

    2017-05-02

    Exaiptasia is a laboratory sea anemone model system for stony corals. Two clonal strains are commonly used, referred to as H2 and CC7, that originate from two genetically distinct lineages and that differ in their Symbiodinium specificity. However, little is known about their other microbial associations. Here, we examined and compared the taxonomic composition of the bacterial assemblages of these two symbiotic Exaiptasia strains, both of which have been cultured in the laboratory long-term under identical conditions. We found distinct bacterial microbiota for each strain, indicating the presence of host-specific microbial consortia. Putative differences in the bacterial functional profiles (i.e., enrichment and depletion of various metabolic processes) based on taxonomic inference were also detected, further suggesting functional differences of the microbiomes associated with these lineages. Our study contributes to the current knowledge of the Exaiptasia holobiont by comparing the bacterial diversity of two commonly used strains as models for coral research.

  1. Analysis of cagA in Helicobacter pylori strains from Colombian populations with contrasting gastric cancer risk reveals a biomarker for disease severity

    Science.gov (United States)

    Loh, John T.; Shaffer, Carrie L.; Piazuelo, M. Blanca; Bravo, Luis E.; McClain, Mark S.; Correa, Pelayo; Cover, Timothy L.

    2011-01-01

    BACKGROUND Helicobacter pylori infection is a risk factor for the development of gastric cancer, and the bacterial oncoprotein CagA contributes to gastric carcinogenesis. METHODS We analyzed H. pylori isolates from persons in Colombia and observed that there was marked variation among strains in levels of CagA expression. To elucidate the basis for this variation, we analyzed sequences upstream from the CagA translational initiation site in each strain. RESULTS A DNA motif (AATAAGATA) upstream of the translational initiation site of CagA was associated with high levels of CagA expression. Experimental studies showed that this motif was necessary but not sufficient for high-level CagA expression. H. pylori strains from a region of Colombia with high gastric cancer rates expressed higher levels of CagA than did strains from a region with lower gastric cancer rates, and Colombian strains of European phylogeographic origin expressed higher levels of CagA than did strains of African origin. Histopathological analysis of gastric biopsy specimens revealed that strains expressing high levels of CagA or containing the AATAAGATA motif were associated with more advanced precancerous lesions than those found in persons infected with strains expressing low levels of CagA or lacking the AATAAGATA motif. CONCLUSIONS CagA expression varies greatly among H. pylori strains. The DNA motif identified in this study is associated with high levels of CagA expression, and may be a useful biomarker to predict gastric cancer risk. IMPACT These findings help to explain why some persons infected with cagA-positive H. pylori develop gastric cancer and others do not. PMID:21859954

  2. Strain and Defect Engineering for Tailored Electrical Properties in Perovskite Oxide Thin Films and Superlattices

    Science.gov (United States)

    Hsing, Greg Hsiang-Chun

    Functional complex-oxides display a wide spectrum of physical properties, including ferromagnetism, piezoelectricity, ferroelectricity, photocatalytic and metal-insulating transition (MIT) behavior. Within this family, oxides with a perovskite structure have been widely studied, especially in the form of thin films and superlattices (heterostructures), which are strategically and industrially important because they offer a wide range of opportunities for electronic, piezoelectric and sensor applications. The first part of my thesis focuses on understanding and tuning of the built-in electric field found in PbTiO3/SrTiO3 (PTO/STO) ferroelectric superlattices and other ferroelectric films. The artificial layering in ferroelectric superlattices is a potential source of polarization asymmetry, where one polarization state is preferred over another. One manifestation of this asymmetry is a built-in electric field associated with shifted polarization hysteresis. Using off-axis RF-magnetron sputtering, we prepared several compositions of PTO/STO superlattice thin films; and for comparison PbTiO3/SrRuO 3 (PTO/SRO) superlattices, which have an additional intrinsic compositional asymmetry at the interface. Both theoretical modeling and experiments indicate that the layer-by-layer superlattice structure aligns the Pb-O vacancy defect dipoles in the c direction which contributes significantly to the built-in electric field; however the preferred polarization direction is different between the PTO/STO and PTO/SRO interface. By designing a hybrid superlattice that combines PTO/STO and PTO/SRO superlattices, we show the built-in electric field can be tuned to zero by changing the composition of the combo-superlattice. The second part of my thesis focuses on the epitaxial growth of SrCrO 3 (SCO) films. The inconsistent reports regarding its electrical and magnetic properties through the years stem from the compositionally and structurally ill-defined polycrystalline samples, but

  3. A model for the formation of lattice defects at silicon oxide precipitates in silicon

    International Nuclear Information System (INIS)

    Vanhellemont, J.; Gryse, O. de; Clauws, P.

    2003-01-01

    The critical size of silicon oxide precipitates and the formation of lattice defects by the precipitates are discussed. An expression is derived allowing estimation of self-interstitial emission by spherical precipitates as well as strain build-up during precipitate growth. The predictions are compared with published experimental data. A model for stacking fault nucleation at oxide precipitates is developed based on strain and self-interstitial accumulation during the thermal history of the wafer. During a low-temperature treatment high levels of strain develop. During subsequent high-temperature treatment, excess strain energy in the precipitate is released by self-interstitial emission leading to favourable conditions for stacking fault nucleation

  4. Effect of tin doping on oxygen- and carbon-related defects in Czochralski silicon

    International Nuclear Information System (INIS)

    Chroneos, A.; Londos, C. A.; Sgourou, E. N.

    2011-01-01

    Experimental and theoretical techniques are used to investigate the impact of tin doping on the formation and the thermal stability of oxygen- and carbon-related defects in electron-irradiated Czochralski silicon. The results verify previous reports that Sn doping reduces the formation of the VO defect and suppresses its conversion to the VO 2 defect. Within experimental accuracy, a small delay in the growth of the VO 2 defect is observed. Regarding carbon-related defects, it is determined that Sn doping leads to a reduction in the formation of the C i O i , C i C s , and C i O i (Si I ) defects although an increase in their thermal stability is observed. The impact of strain induced in the lattice by the larger tin substitutional atoms, as well as their association with intrinsic defects and carbon impurities, can be considered as an explanation to account for the above observations. The density functional theory calculations are used to study the interaction of tin with lattice vacancies and oxygen- and carbon-related clusters. Both experimental and theoretical results demonstrate that tin co-doping is an efficient defect engineering strategy to suppress detrimental effects because of the presence of oxygen- and carbon-related defect clusters in devices.

  5. Resiliency to social defeat stress relates to the inter-strain social interaction and is influenced by season variation.

    Science.gov (United States)

    Han, Qiuqin; Yang, Liu; Liu, Yan; Lv, Ning; Yu, Jin; Wu, Gencheng; Zhang, Yuqiu

    2014-02-21

    Exposure to social defeat (SD) stress exerts social avoidance and depressive disorders. Little is known about the relationship between resiliency to stressors and the inter-strain social interaction (SI) level. We hypothesized that SD resiliency is correlated with a high SI between the same strain. C57BL/6J mice experienced a 10-day period of SD stress by repeated CD-1 mice offensive. The susceptible mice exhibited significant social-avoidance behaviors with less time in interaction-zone (IZ) and lower social interaction ratio (SIR) toward the Target (CD-1 mice), while resilient ones exhibited similar social interaction to control mice. When the Target was C57BL/6J mouse, either susceptible or resilient mice spent more time in IZ and the inter-strain SI in the resilient group was significantly higher than the susceptible. Correlation analysis revealed a significantly non-zero slope of the linear relationship between SIRs toward two strains. But different groups had a similar baseline of the inter-strain SI before stress, indicating a SD-induced defect in both types of SI. In addition, in four different seasons, animals exhibited a significant resiliency to the stress in summer. These data suggest that SD resiliency is related to a higher SI toward the same-strain, and may be regulated by seasonal variations. Copyright © 2013 Elsevier Ireland Ltd. All rights reserved.

  6. Nonpolar ZnO film growth and mechanism for anisotropic in-plane strain relaxation

    International Nuclear Information System (INIS)

    Pant, P.; Budai, J.D.; Narayan, J.

    2010-01-01

    Using high-resolution transmission electron microscopy (HRTEM) and X-ray diffraction, we investigated the strain relaxation mechanisms for nonpolar (1 1 -2 0) a-plane ZnO epitaxy on (1 -1 0 2) r-plane sapphire, where the in-plane misfit ranges from -1.5% for the [0 0 0 1]ZnO-parallel [1 -1 0 -1]sapphire to -18.3% for the [-1 1 0 0]ZnO-parallel [-1 -1 2 0]sapphire direction. For the large misfit [-1 1 0 0]ZnO direction the misfit strains are fully relaxed at the growth temperature, and only thermal misfit and defect strains, which cannot be relaxed fully by slip dislocations, remain on cooling. For the small misfit direction, lattice misfit is not fully relaxed at the growth temperature. As a result, additive unrelaxed lattice and thermal misfit and defect strains contribute to the measured strain. Our X-ray diffraction measurements of lattice parameters show that the anisotropic in-plane biaxial strain leads to a distortion of the hexagonal symmetry of the ZnO basal plane. Based on the anisotropic strain relaxation observed along the orthogonal in-plane [-1 1 0 0] and [0 0 0 1]ZnO stress directions and our HRTEM investigations of the interface, we show that the plastic relaxation occurring in the small misfit direction [0 0 0 1]ZnO by dislocation nucleation is incomplete. These results are consistent with the domain-matching paradigm of a complete strain relaxation for large misfits and a difficulty in relaxing the film strain for small misfits.

  7. Atypical patterns of neural infection produced in mice by drug-resistant strains of herpes simplex virus.

    Science.gov (United States)

    Field, H J; Anderson, J R; Wildy, P

    1982-03-01

    Mice inoculated intracerebrally (i.c.) with a mutant strain of HSV were found to develop cataracts 1 to 2 months after inoculation. Cataract formation was subsequently shown to follow an acute retinitis which commenced within 1 week of inoculation. The mutant had been selected for high resistance to the nucleoside analogue acyclovir and has been shown previously to be defective in the induction of thymidine kinase and also to express an altered DNA polymerase. The LD50 for mice inoculated i.c. was greater than 10(5) p.f.u. compared with approx 7 p.f.u. for the parental strain. Studies of virus replication following i.c. inoculation with a sublethal dose of the mutant revealed that only small amounts of infectious virus were produced in the brain, but during a period from 6 to 12 days after inoculation vigorous replication occurred in retinal tissue, producing very high titres of virus.

  8. Optimization of Soft Tissue Management, Spacer Design, and Grafting Strategies for Large Segmental Bone Defects using the Chronic Caprine Tibial Defect Model

    Science.gov (United States)

    2015-12-01

    for this animal revealed an abscess at the defect site with cultures identifying Staphylococcus aureus infection . Another animal (15G11) developed...foreign body reaction and expose a bleeding vascular surface significantly increased bone formation in the defect site. Adding texture to a smooth...ACHIEVEMENTS: Nothing to report 10. REFERENCES: 1. Johnson, E.N., et al., Infectious complications of open type III tibial fractures among combat

  9. Unconventional strain-dependent conductance oscillations in pristine phosphorene.

    Science.gov (United States)

    Ray, S J; Kamalakar, M Venkata

    2018-05-16

    Phosphorene is a single elemental, two-dimensional semiconductor that has quickly emerged as a high mobility material for transistors and optoelectronic devices. In addition, being a 2D material it can sustain high levels of strain, enabling sensitive modification of its electronic properties. In this paper, we investigate the strain dependent electronic properties of phosphorene nanocrystals. By performing extensive calculations we determine the electrical conductance as a function of uniaxial, as well as biaxial strain stimuli and uncover a unique zone phase diagram. This enables us to uncover conductance oscillations in pristine phosphorene for the first time, by the simple application of strain. We show that such unconventional current-voltage behaviour is tuneable by the nature of strain, and that an additional gate voltage can modulate the amplitude (peak to valley ratio) of the observed phenomena and its switching efficiency. Furthermore, we show that the switching is highly robust against doping and defects. Our detailed results present new leads for innovation in strain based gauging and high-frequency nanoelectronic switches of phosphorene.

  10. First-principles study of lithium adsorption and diffusion on graphene: the effects of strain

    International Nuclear Information System (INIS)

    Hao, Feng; Chen, Xi

    2015-01-01

    Large strain is produced within graphene sheets, which serve as a critical component in lithium-ion batteries, due to the expansion of the electrodes. First-principles calculations are therefore employed to investigate the interaction of Li with strained single-layer graphene. It is found that tensile strain enhances Li binding on graphene and significantly reduces the formation energy of divacancies. In addition, Li diffusion through graphene with defects is facilitated by tensile strain, whereas diffusion parallel to the plane of pristine graphene is slightly hindered. (paper)

  11. Implementation of ZnO/ZnMgO strained-layer superlattice for ZnO heteroepitaxial growth on sapphire

    Science.gov (United States)

    Petukhov, Vladimir; Bakin, Andrey; Tsiaoussis, Ioannis; Rothman, Johan; Ivanov, Sergey; Stoemenos, John; Waag, Andreas

    2011-05-01

    The main challenge in fabrication of ZnO-based devices is the absence of reliable p-type material. This is mostly caused by insufficient crystalline quality of the material and not well-enough-developed native point defect control of ZnO. At present high-quality ZnO wafers are still expensive and ZnO heteroepitaxial layers on sapphire are the most reasonable alternative to homoepitaxial layers. But it is still necessary to improve the crystalline quality of the heteroepitaxial layers. One of the approaches to reduce defect density in heteroepitaxial layers is to introduce a strained-layer superlattice (SL) that could stop dislocation propagation from the substrate-layer interface. In the present paper we have employed fifteen periods of a highly strained SL structure. The structure was grown on a conventional double buffer layer comprising of high-temperature MgO/low-temperature ZnO on sapphire. The influence of the SLs on the properties of the heteroepitaxial ZnO layers is investigated. Electrical measurements of the structure with SL revealed very high values of the carrier mobility up to 210 cm2/Vs at room temperature. Structural characterization of the obtained samples showed that the dislocation density in the following ZnO layer was not reduced. The high mobility signal appears to come from the SL structure or the SL/ZnO interface.

  12. Rapid transitions between defect configurations in a block copolymer melt.

    Science.gov (United States)

    Tsarkova, Larisa; Knoll, Armin; Magerle, Robert

    2006-07-01

    With in situ scanning force microscopy, we image the ordering of cylindrical microdomains in a thin film of a diblock copolymer melt. Tracking the evolution of individual defects reveals elementary steps of defect motion via interfacial undulations and repetitive transitions between distinct defect configurations on a time scale of tens of seconds. The velocity of these transitions suggests a cooperative movement of clusters of chains. The activation energy for the opening/closing of a connection between two cylinders is estimated.

  13. Effect of uniaxial stress on the electrochemical properties of graphene with point defects

    Science.gov (United States)

    Szroeder, Paweł; Sagalianov, Igor Yu.; Radchenko, Taras M.; Tatarenko, Valentyn A.; Prylutskyy, Yuriy I.; Strupiński, Włodzimierz

    2018-06-01

    We report a calculational study of electron states and the resulting electrochemical properties of uniaxially strained graphene with point defects. For this study the reduction of ferricyanide to ferrocyanide serves as a benchmark electrochemical reaction. We find that the heterogeneous electron transfer activity of the perfect graphene electrode rises under uniaxial strain. However, evolution of the cathodic reaction rate depends on the direction of strain. For moderate lattice deformations, the zigzag strain improves electrochemical performance better than the armchair strain. Standard rate constant increases by 50% at the zigzag strain of 10%. Vacancies, covalently bonded moieties, charged adatoms and substitutional impurities in the zigzag strained graphene induce changes in the shape of the curve of the cathodic reaction rate. However, this changes do not translate into the electrocatalytic activity. Vacancies and covalently bonded moieties at concentration of 0.1% do not affect the electrochemical performance. Charged adatoms and substitutional impurities give a slight increase in the standard rate constant by, respectively, 2.2% and 3.4%.

  14. Defective TFH Cell Function and Increased TFR Cells Contribute to Defective Antibody Production in Aging.

    Science.gov (United States)

    Sage, Peter T; Tan, Catherine L; Freeman, Gordon J; Haigis, Marcia; Sharpe, Arlene H

    2015-07-14

    Defective antibody production in aging is broadly attributed to immunosenescence. However, the precise immunological mechanisms remain unclear. Here, we demonstrate an increase in the ratio of inhibitory T follicular regulatory (TFR) cells to stimulatory T follicular helper (TFH) cells in aged mice. Aged TFH and TFR cells are phenotypically distinct from those in young mice, exhibiting increased programmed cell death protein-1 expression but decreased ICOS expression. Aged TFH cells exhibit defective antigen-specific responses, and programmed cell death protein-ligand 1 blockade can partially rescue TFH cell function. In contrast, young and aged TFR cells have similar suppressive capacity on a per-cell basis in vitro and in vivo. Together, these studies reveal mechanisms contributing to defective humoral immunity in aging: an increase in suppressive TFR cells combined with impaired function of aged TFH cells results in reduced T-cell-dependent antibody responses in aged mice. Copyright © 2015 The Authors. Published by Elsevier Inc. All rights reserved.

  15. Fracture Mechanics Analyses of Subsurface Defects in Reinforced Carbon-Carbon Joggles Subjected to Thermo-Mechanical Loads

    Science.gov (United States)

    Knight, Norman F., Jr.; Raju, Ivatury S.; Song, Kyongchan

    2011-01-01

    Coating spallation events have been observed along the slip-side joggle region of the Space Shuttle Orbiter wing-leading-edge panels. One potential contributor to the spallation event is a pressure build up within subsurface voids or defects due to volatiles or water vapor entrapped during fabrication, refurbishment, or normal operational use. The influence of entrapped pressure on the thermo-mechanical fracture-mechanics response of reinforced carbon-carbon with subsurface defects is studied. Plane-strain simulations with embedded subsurface defects are performed to characterize the fracture mechanics response for a given defect length when subjected to combined elevated-temperature and subsurface-defect pressure loadings to simulate the unvented defect condition. Various subsurface defect locations of a fixed-length substrate defect are examined for elevated temperature conditions. Fracture mechanics results suggest that entrapped pressure combined with local elevated temperatures have the potential to cause subsurface defect growth and possibly contribute to further material separation or even spallation. For this anomaly to occur, several unusual circumstances would be required making such an outcome unlikely but plausible.

  16. Hypomorphic Smn knockdown C2C12 myoblasts reveal intrinsic defects in myoblast fusion and myotube morphology

    International Nuclear Information System (INIS)

    Shafey, Dina; Cote, Patrice D.; Kothary, Rashmi

    2005-01-01

    Dosage of the survival motor neuron (SMN) protein has been directly correlated with the severity of disease in patients diagnosed with spinal muscular atrophy (SMA). It is also clear that SMA is a neurodegenerative disorder characterized by the degeneration of the α-motor neurons in the anterior horn of the spinal cord and atrophy of the associated skeletal muscle. What is more controversial is whether it is neuronal and/or muscle-cell-autonomous defects that are responsible for the disease per se. Although motor neuron degeneration is generally accepted as the primary event in SMA, intrinsic muscle defects in this disease have not been ruled out. To gain a better understanding of the influence of SMN protein dosage in muscle, we have generated a hypomorphic series of myoblast (C2C12) stable cell lines with variable Smn knockdown. We show that depletion of Smn in these cells resulted in a decrease in the number of nuclear 'gems' (gemini of coiled bodies), reduced proliferation with no increase in cell death, defects in myoblast fusion, and malformed myotubes. Importantly, the severity of these abnormalities is directly correlated with the decrease in Smn dosage. Taken together, our work supports the view that there is an intrinsic defect in skeletal muscle cells of SMA patients and that this defect contributes to the overall pathogenesis in this devastating disease

  17. Non-aflatoxigenicity of commercial Aspergillus oryzae strains due to genetic defects compared to aflatoxigenic Aspergillus flavus.

    Science.gov (United States)

    Tao, Lin; Chung, Soo Hyun

    2014-08-01

    Aspergillus oryzae is generally recognized as safe, but it is closely related to A. flavus in morphology and genetic characteristics. In this study, we tested the aflatoxigenicity and genetic analysis of nine commercial A. oryzae strains that were used in Korean soybean fermented products. Cultural and HPLC analyses showed that none of the commercial strains produced detectable amount of aflatoxins. According to the molecular analysis of 17 genes in the aflatoxin (AF) biosynthetic pathway, the commercial strains could be classified into three groups. The group I strains contained all the 17 AF biosynthetic genes tested in this study; the group II strains deleted nine AF biosynthetic genes and possessed eight genes, including aflG, aflI, aflK, aflL, aflM, aflO, aflP, and aflQ; the group III strains only had six AF biosynthetic genes, including aflG, aflI, aflK, aflO, aflP, and aflQ. With the reverse transcription polymerase chain reaction, the group I A. oryzae strains showed no expression of aflG, aflQ and/or aflM genes, which resulted in the lack of AF-producing ability. Group II and group III strains could not produce AF owing to the deletion of more than half of the AF biosynthetic genes. In addition, the sequence data of polyketide synthase A (pksA) of group I strains of A. oryzae showed that there were three point mutations (two silent mutations and one missense mutation) compared with aflatoxigenic A. flavus used as the positive control in this study.

  18. A study on the healing process of bone defect-examination of healing stages of bone defect in the irradiated mandibular rim by microradiography and autoradiography

    International Nuclear Information System (INIS)

    Shimoyama, Tetsuo

    1980-01-01

    The mandibular rim of 150 female Donryu strain rats was exposed to 2000 rads (B group) or to 3000 rads (C group), and a bone defect of 1 x 1 x 2 mm in size was formed in the madibular rim. Cure process of this bone defect was observed periodically by microradiography and autoradiography using 45 Ca as a tracer, compared with that in the control group (A group, non-irradiated). Irradiated rats having bone defects recovered smoothly. Microradiographic findings of the A group showed that new bone was formed on the surface of the perosteum of the mandible on the 7th days after the irradiation. Bone defects in all rats were repaired completely by the 49th days after the irradiation. Microradiographic findings of the B and C groups showed that new bone was formed on the tongue side surface of the periosteum of the mandible in the early stage after the irradiation. However, after that, osteogenesis became slower, and the edge of bone defects or a part of the mandible became smaller. Bone defects were not repaired and became larger. These findings were more marked in the C group than in the B group. Autoradiographic findings showed marked uptake of 45 Ca into new bone in the A group. Rats of which bone defects were repaired showed the uptake of 45 Ca in accordance with the shape of the mandibular rim. The edge of bone defect of the B and C groups where new bone was not formed was destroyed since the 14th day after the irradiation. There were some cases in which the uptake of 45 Ca into the surface of the periosteum of the mandible near bone defect was observed even when bone defect was enlarged. (Tsunoda, M.)

  19. Dissociation and diffusion of hydrogen on defect-free and vacancy defective Mg (0001) surfaces: A density functional theory study

    Energy Technology Data Exchange (ETDEWEB)

    Han, Zongying [College of Chemical and Environmental Engineering, Shandong University of Science and Technology, Qingdao 266590 (China); Union Research Center of Fuel Cell, School of Chemical and Environmental Engineering, China University of Mining and Technology, Beijing 100083 (China); Chen, Haipeng [College of Chemical and Environmental Engineering, Shandong University of Science and Technology, Qingdao 266590 (China); College of Mechanical and Electronic Engineering, Shandong University of Science and Technology, Qingdao 266590 (China); Zhou, Shixue, E-mail: zhoushixue66@163.com [College of Chemical and Environmental Engineering, Shandong University of Science and Technology, Qingdao 266590 (China); College of Mechanical and Electronic Engineering, Shandong University of Science and Technology, Qingdao 266590 (China)

    2017-02-01

    Highlights: • Clarify the effect of vacancy defect on H{sub 2} dissociation on Mg (0001) surface. • Demonstrate the effects of vacancy defect on H atom diffusion. • Reveal the minimum energy diffusion path of H atom from magnesium surface into bulk. - Abstract: First-principles calculations with the density functional theory (DFT) have been carried out to study dissociation and diffusion of hydrogen on defect-free and vacancy defective Mg (0001) surfaces. Results show that energy barriers of 1.42 eV and 1.28 eV require to be overcome for H{sub 2} dissociation on defect-free and vacancy defective Mg (0001) surfaces respectively, indicating that reactivity of Mg (0001) surface is moderately increased due to vacancy defect. Besides, the existence of vacancy defect changes the preferential H atom diffusion entrance to the subsurface and reduces the diffusion energy barrier. An interesting remark is that the minimum energy diffusion path of H atom from magnesium surface into bulk is a spiral channel formed by staggered octahedral and tetrahedral interstitials. The diffusion barriers computed for H atom penetration from the surface into inner-layers are all less than 0.70 eV, which is much smaller than the activation energy for H{sub 2} dissociation on the Mg (0001) surface. This suggests that H{sub 2} dissociation is more likely than H diffusion to be rate-limiting step for magnesium hydrogenation.

  20. Investigation of the impact of defect models on Monte Carlo simulations of RBS/C spectra

    International Nuclear Information System (INIS)

    Kovac, D.; Hobler, G.

    2006-01-01

    We compare the impact on the RBS/C spectra of defect configurations in silicon obtained from either empirical interatomic potentials or ab initio calculations. Using the Tersoff potential as the empirical potential and the VASP code for ab initio calculations we have determined the coordinates of the split- interstitial, of the di-, tri- and four-interstitial cluster, and of the tetrahedral interstitial as well as the strain on neighboring atoms induced by the presence of these defects. Using these coordinates in binary collision RBS/C simulations we find differences in the RBS/C yields of up to 30%. The dependence of the backscattering yield on the assumed defect type is larger with the defect coordinates obtained by the empirical potential than by the ab initio calculations

  1. Electronically active defects in the Cu2ZnSn(Se,S)4 alloys as revealed by transient photocapacitance spectroscopy

    Science.gov (United States)

    Miller, D. Westley; Warren, Charles W.; Gunawan, Oki; Gokmen, Tayfun; Mitzi, David B.; Cohen, J. David

    2012-10-01

    Transient photocapacitance (TPC) spectra were obtained on a series of Cu2ZnSn(Se,S)4 absorber devices with varying Se:S ratios, providing bandgaps (Eg) between 1 eV and 1.5 eV. Efficiencies varied between 8.3% and 9.3% for devices with Eg ≤ 1.2 eV and were near 6.5% for devices with Eg ≥ 1.4 eV. The TPC spectra revealed a band-tail region with Urbach energies at or below 18 meV for the first group, but in the 25-30 meV range for the higher band-gap samples. A deeper defect band centered near 0.8 eV was also observed in most samples. We identified a correlation between the Urbach energies and the voltage deficit in these devices.

  2. Critical defect size assessment in pipelines on a nuclear power plant

    Directory of Open Access Journals (Sweden)

    Dimova Galya

    2018-01-01

    Full Text Available In many energy industry structures, pipeline systems are subject to the impact of mechanical forces, moments of forces and fluid flows of high pressure and temperature. These load factors cause defects in the pipeline metal. As the years of operation increase, defects may occur and grow, which may lead to the destruction of pipeline walls. Special measures have been planned and implemented to ensure the safe operation of high-energy facilities. This study focused on pipelines and nozzles of nuclear power plant equipment with bimetal welded joints on which the size of critical defects was assessed. The base of assessment covers material properties, temperature and stress fields, fracture mechanics calculations. This study involves developing of finite element models and implementing simulations on them in order to obtain temperature fields and determine the stress-strain state of the component.

  3. Defective quiescence entry promotes the fermentation performance of bottom-fermenting brewer's yeast.

    Science.gov (United States)

    Oomuro, Mayu; Kato, Taku; Zhou, Yan; Watanabe, Daisuke; Motoyama, Yasuo; Yamagishi, Hiromi; Akao, Takeshi; Aizawa, Masayuki

    2016-11-01

    One of the key processes in making beer is fermentation. In the fermentation process, brewer's yeast plays an essential role in both the production of ethanol and the flavor profile of beer. Therefore, the mechanism of ethanol fermentation by of brewer's yeast is attracting much attention. The high ethanol productivity of sake yeast has provided a good basis from which to investigate the factors that regulate the fermentation rates of brewer's yeast. Recent studies found that the elevated fermentation rate of sake Saccharomyces cerevisiae species is closely related to a defective transition from vegetative growth to the quiescent (G 0 ) state. In the present study, to clarify the relationship between the fermentation rate of brewer's yeast and entry into G 0 , we constructed two types of mutant of the bottom-fermenting brewer's yeast Saccharomyces pastorianus Weihenstephan 34/70: a RIM15 gene disruptant that was defective in entry into G 0 ; and a CLN3ΔPEST mutant, in which the G 1 cyclin Cln3p accumulated at high levels. Both strains exhibited higher fermentation rates under high-maltose medium or high-gravity wort conditions (20° Plato) as compared with the wild-type strain. Furthermore, G 1 arrest and/or G 0 entry were defective in both the RIM15 disruptant and the CLN3ΔPEST mutant as compared with the wild-type strain. Taken together, these results indicate that regulation of the G 0 /G 1 transition might govern the fermentation rate of bottom-fermenting brewer's yeast in high-gravity wort. Copyright © 2016 The Society for Biotechnology, Japan. Published by Elsevier B.V. All rights reserved.

  4. Plant root transcriptome profiling reveals a strain-dependent response during Azospirillum-rice cooperation

    Directory of Open Access Journals (Sweden)

    Benoît eDrogue

    2014-11-01

    Full Text Available Cooperation involving Plant Growth-Promoting Rhizobacteria results in improvements of plant growth and health. While pathogenic and symbiotic interactions are known to induce transcriptional changes for genes related to plant defence and development, little is known about the impact of phytostimulating rhizobacteria on plant gene expression. This study aims at identifying genes significantly regulated in rice roots upon Azospirillum inoculation, considering possible favored interaction between a strain and its original host cultivar. Genome-wide analyses of Oryza sativa japonica cultivars Cigalon and Nipponbare were performed, by using microarrays, seven days post inoculation with A. lipoferum 4B (isolated from Cigalon or Azospirillum sp. B510 (isolated from Nipponbare and compared to the respective non-inoculated condition. A total of 7,384 genes were significantly regulated, which represent about 16 % of total rice genes. A set of 34 genes is regulated by both Azospirillum strains in both cultivars, including a gene orthologous to PR10 of Brachypodium, and these could represent plant markers of Azospirillum-rice interactions. The results highlight a strain-dependent response of rice, with 83 % of the differentially expressed genes being classified as combination-specific. Whatever the combination, most of the differentially expressed genes are involved in primary metabolism, transport, regulation of transcription and protein fate. When considering genes involved in response to stress and plant defence, it appears that strain B510, a strain displaying endophytic properties, leads to the repression of a wider set of genes than strain 4B. Individual genotypic variations could be the most important driving force of rice roots gene expression upon Azospirillum inoculation. Strain-dependent transcriptional changes observed for genes related to auxin and ethylene signalling highlight the complexity of hormone signalling networks in the Azospirillum

  5. Strain engineered pyrochlore at high pressure

    Energy Technology Data Exchange (ETDEWEB)

    Rittman, Dylan R.; Turner, Katlyn M.; Park, Sulgiye; Fuentes, Antonio F.; Park, Changyong; Ewing, Rodney C.; Mao, Wendy L.

    2017-05-22

    Strain engineering is a promising method for next-generation materials processing techniques. Here, we use mechanical milling and annealing followed by compression in diamond anvil cell to tailor the intrinsic and extrinsic strain in pyrochlore, Dy2Ti2O7 and Dy2Zr2O7. Raman spectroscopy, X-ray pair distribution function analysis, and X-ray diffraction were used to characterize atomic order over short-, medium-, and long-range spatial scales, respectively, under ambient conditions. Raman spectroscopy and X-ray diffraction were further employed to interrogate the material in situ at high pressure. High-pressure behavior is found to depend on the species and concentration of defects in the sample at ambient conditions. Overall, we show that defects can be engineered to lower the phase transformation onset pressure by ~50% in the ordered pyrochlore Dy2Zr2O7, and lower the phase transformation completion pressure by ~20% in the disordered pyrochlore Dy2Zr2O7. These improvements are achieved without significantly sacrificing mechanical integrity, as characterized by bulk modulus.

  6. Recovery of strain-hardening rate in Ni-Si alloys

    Science.gov (United States)

    Yang, C. L.; Zhang, Z. J.; Cai, T.; Zhang, P.; Zhang, Z. F.

    2015-10-01

    In this study, the recovery of strain-hardening rate (RSHR) was discovered for the first time in polycrystalline materials (Ni-Si alloys) that have only dislocation activities during tensile test. Detailed microstructure characterizations show that the activation of dislocations in the secondary slip systems during tensile deformation is the major reason for this RSHR. By taking into account other metals that also exhibit RSHR during tension, a more general mechanism for the RSHR was proposed, i.e. the occurrence of a sharp decrease of dislocation mean free path (Λ) during plastic deformation, caused by either planar defects or linear defects.

  7. The influence of gouge defects on failure pressure of steel pipes

    International Nuclear Information System (INIS)

    Alang, N A; Razak, N A; Zulfadli, M R

    2013-01-01

    Failure pressure of API X42 steel pipes with gouge defects was estimated through a nonlinear finite element (FE) analysis. The effect of gouge length on failure pressure of different pipe diameters was investigated. Stress modified critical strain (SMCS) model was applied as in predicting the failure of the pipe. The model uses strain based criteria to predict the failure. For validation of the model, the FE results were compared to experimental data in literature showing overall good agreement. The results show that the gouge length has significant influence on failure pressure. A smaller pipe diameter gives highest value of failure pressure

  8. Strain-Compensated InGaAsP Superlattices for Defect Reduction of InP Grown on Exact-Oriented (001 Patterned Si Substrates by Metal Organic Chemical Vapor Deposition

    Directory of Open Access Journals (Sweden)

    Ludovico Megalini

    2018-02-01

    Full Text Available We report on the use of InGaAsP strain-compensated superlattices (SC-SLs as a technique to reduce the defect density of Indium Phosphide (InP grown on silicon (InP-on-Si by Metal Organic Chemical Vapor Deposition (MOCVD. Initially, a 2 μm thick gallium arsenide (GaAs layer was grown with very high uniformity on exact oriented (001 300 mm Si wafers; which had been patterned in 90 nm V-grooved trenches separated by silicon dioxide (SiO2 stripes and oriented along the [110] direction. Undercut at the Si/SiO2 interface was used to reduce the propagation of defects into the III–V layers. Following wafer dicing; 2.6 μm of indium phosphide (InP was grown on such GaAs-on-Si templates. InGaAsP SC-SLs and thermal annealing were used to achieve a high-quality and smooth InP pseudo-substrate with a reduced defect density. Both the GaAs-on-Si and the subsequently grown InP layers were characterized using a variety of techniques including X-ray diffraction (XRD; atomic force microscopy (AFM; transmission electron microscopy (TEM; and electron channeling contrast imaging (ECCI; which indicate high-quality of the epitaxial films. The threading dislocation density and RMS surface roughness of the final InP layer were 5 × 108/cm2 and 1.2 nm; respectively and 7.8 × 107/cm2 and 10.8 nm for the GaAs-on-Si layer.

  9. Charged defects during alpha-irradiation of actinide oxides as revealed by Raman and luminescence spectroscopy

    International Nuclear Information System (INIS)

    Mohun, R.; Desgranges, L.; Léchelle, J.; Simon, P.; Guimbretière, G.; Canizarès, A.; Duval, F.; Jegou, C.; Magnin, M.; Clavier, N.; Dacheux, N.; Valot, C.; Vauchy, R.

    2016-01-01

    We have recently evidenced an original Raman signature of alpha irradiation-induced defects in UO 2 . In this study, we aim to determine whether the same signature also exists in different actinide oxides, namely ThO 2 and PuO 2 . Sintered UO 2 and ThO 2 were initially irradiated with 21 MeV He 2+ ions using a cyclotron device and were subjected to an in situ luminescence experiment followed by Raman analysis. In addition, a PuO 2 sample which had accumulated self-irradiation damage due to alpha particles was investigated only by Raman measurement. Results obtained for the initially white ThO 2 showed that a blue color appeared in the irradiated areas as well as luminescence signals during irradiation. However, Raman spectroscopic analysis showed the absence of Raman signature in ThO 2 . In contrast, the irradiated UO 2 and PuO 2 confirmed the presence of the Raman signature but no luminescence peaks were observed. The proposed mechanism involves electronic defects in ThO 2 , while a coupling between electronic defects and phonons is required to explain the Raman spectra for UO 2 and PuO 2 .

  10. Comparative genome analysis of VSP-II and SNPs reveals heterogenic variation in contemporary strains of Vibrio cholerae O1 isolated from cholera patients in Kolkata, India.

    Science.gov (United States)

    Imamura, Daisuke; Morita, Masatomo; Sekizuka, Tsuyoshi; Mizuno, Tamaki; Takemura, Taichiro; Yamashiro, Tetsu; Chowdhury, Goutam; Pazhani, Gururaja P; Mukhopadhyay, Asish K; Ramamurthy, Thandavarayan; Miyoshi, Shin-Ichi; Kuroda, Makoto; Shinoda, Sumio; Ohnishi, Makoto

    2017-02-01

    Cholera is an acute diarrheal disease and a major public health problem in many developing countries in Asia, Africa, and Latin America. Since the Bay of Bengal is considered the epicenter for the seventh cholera pandemic, it is important to understand the genetic dynamism of Vibrio cholerae from Kolkata, as a representative of the Bengal region. We analyzed whole genome sequence data of V. cholerae O1 isolated from cholera patients in Kolkata, India, from 2007 to 2014 and identified the heterogeneous genomic region in these strains. In addition, we carried out a phylogenetic analysis based on the whole genome single nucleotide polymorphisms to determine the genetic lineage of strains in Kolkata. This analysis revealed the heterogeneity of the Vibrio seventh pandemic island (VSP)-II in Kolkata strains. The ctxB genotype was also heterogeneous and was highly related to VSP-II types. In addition, phylogenetic analysis revealed the shifts in predominant strains in Kolkata. Two distinct lineages, 1 and 2, were found between 2007 and 2010. However, the proportion changed markedly in 2010 and lineage 2 strains were predominant thereafter. Lineage 2 can be divided into four sublineages, I, II, III and IV. The results of this study indicate that lineages 1 and 2-I were concurrently prevalent between 2007 and 2009, and lineage 2-III observed in 2010, followed by the predominance of lineage 2-IV in 2011 and continued until 2014. Our findings demonstrate that the epidemic of cholera in Kolkata was caused by several distinct strains that have been constantly changing within the genetic lineages of V. cholerae O1 in recent years.

  11. Pyrosequencing Analysis Reveals Changes in Intestinal Microbiota of Healthy Adults Who Received a Daily Dose of Immunomodulatory Probiotic Strains

    Directory of Open Access Journals (Sweden)

    Julio Plaza-Díaz

    2015-05-01

    Full Text Available The colon microbiota plays a crucial role in human gastrointestinal health. Current attempts to manipulate the colon microbiota composition are aimed at finding remedies for various diseases. We have recently described the immunomodulatory effects of three probiotic strains (Lactobacillus rhamnosus CNCM I-4036, Lactobacillus paracasei CNCM I-4034, and Bifidobacterium breve CNCM I-4035. The goal of the present study was to analyze the compositions of the fecal microbiota of healthy adults who received one of these strains using high-throughput 16S ribosomal RNA gene sequencing. Bacteroides was the most abundant genus in the groups that received L. rhamnosus CNCM I-4036 or L. paracasei CNCM I-4034. The Shannon indices were significantly increased in these two groups. Our results also revealed a significant increase in the Lactobacillus genus after the intervention with L. rhamnosus CNCM I-4036. The initially different colon microbiota became homogeneous in the subjects who received L. rhamnosus CNCM I-4036. While some orders that were initially present disappeared after the administration of L. rhamnosus CNCM I-4036, other orders, such as Sphingobacteriales, Nitrospirales, Desulfobacterales, Thiotrichales, and Synergistetes, were detected after the intervention. In summary, our results show that the intake of these three bacterial strains induced changes in the colon microbiota.

  12. Investigation on the effect of atomic defects on the breaking behaviors of gold nanowires

    International Nuclear Information System (INIS)

    Wang Fenying; Sun Wei; Wang Hongbo; Zhao Jianwei; Kiguchi, Manabu; Sun Changqing

    2012-01-01

    The mechanical properties and breaking behaviors of the [100]-oriented single-crystal gold nanowires containing a set of defect ratios have been studied at different temperatures using molecular dynamics simulations. The size of the nanowire is 10a × 10a × 30a (a stands for lattice constant, 0.408 nm for gold). The mechanical strengths of the nanowires decrease with the increasing temperature. However, the defects that enhance the local thermal energy have improved the nanowire mechanical strength under a wide range of temperature. Comparing to the single-crystal nanowire, the existence of the atomic defects extends the elastic deformation showing a larger yield strain. By summarizing 300 samples at each temperature, the statistical breaking position distribution shows that the nanowire breaking behavior is sensitive to the atomic defects when the defect ratio is 5 % at 100 K, whereas the ratio is 1 % when temperatures are 300 and 500 K.

  13. A rapid NMR-based method for discrimination of strain-specific cell wall teichoic acid structures reveals a third backbone type in Lactobacillus plantarum.

    Science.gov (United States)

    Tomita, Satoru; Tanaka, Naoto; Okada, Sanae

    2017-03-01

    The lactic acid bacterium Lactobacillus plantarum is capable of producing strain-specific structures of cell wall teichoic acid (WTA), an anionic polysaccharide found in the Gram-positive bacterial cell wall. In this study, we established a rapid, NMR-based procedure to discriminate WTA structures in this species, and applied it to 94 strains of L. plantarum. Six previously reported glycerol- and ribitol-containing WTA subtypes were successfully identified from 78 strains, suggesting that these were the dominant structures. However, the level of structural variety differed markedly among bacterial sources, possibly reflecting differences in strain-level microbial diversity. WTAs from eight strains were not identified based on NMR spectra and were classified into three groups. Structural analysis of a partial degradation product of an unidentified WTA produced by strain TUA 1496L revealed that the WTA was 1-O-β-d-glucosylglycerol. Two-dimensional NMR analysis of the polymer structure showed phosphodiester bonds between C-3 and C-6 of the glycerol and glucose residues, suggesting a polymer structure of 3,6΄-linked poly(1-O-β-d-glucosyl-sn-glycerol phosphate). This is the third WTA backbone structure in L. plantarum, following 3,6΄-linked poly(1-O-α-d-glucosyl-sn-glycerol phosphate) and 1,5-linked poly(ribitol phosphate). © FEMS 2017. All rights reserved. For permissions, please e-mail: journals.permissions@oup.com.

  14. Genetic Screen Reveals the Role of Purine Metabolism in Staphylococcus aureus Persistence to Rifampicin

    Directory of Open Access Journals (Sweden)

    Rebecca Yee

    2015-12-01

    Full Text Available Chronic infections with Staphylococcus aureus such as septicemia, osteomyelitis, endocarditis, and biofilm infections are difficult to treat because of persisters. Despite many efforts in understanding bacterial persistence, the mechanisms of persister formation in S. aureus remain elusive. Here, we performed a genome-wide screen of a transposon mutant library to study the molecular mechanisms involved in persistence of community-acquired S. aureus. Screening of the library for mutants defective in persistence or tolerance to rifampicin revealed many genes involved in metabolic pathways that are important for antibiotic persistence. In particular, the identified mutants belonged to metabolic pathways involved in carbohydrate, amino acid, lipid, vitamin and purine biosynthesis. Five mutants played a role in purine biosynthesis and two mutants, purB, an adenylosuccinate lyase, and purM, a phosphoribosylaminoimidazole synthetase, were selected for further confirmation. Mutants purB and purM showed defective persistence compared to the parental strain USA300 in multiple stress conditions including various antibiotics, low pH, and heat stress. The defect in persistence was restored by complementation with the wildtype purB and purM gene in the respective mutants. These findings provide new insights into the mechanisms of persistence in S. aureus and provide novel therapeutic targets for developing more effective treatment for persistent infections due to S. aureus.

  15. In Situ Observation of Antisite Defect Formation during Crystal Growth

    International Nuclear Information System (INIS)

    Kramer, M. J.; Napolitano, R. E.; Mendelev, M. I.

    2010-01-01

    In situ x-ray diffraction (XRD) coupled with molecular dynamics (MD) simulations have been used to quantify antisite defect trapping during crystallization. Rietveld refinement of the XRD data revealed a marked lattice distortion which involves an a axis expansion and a c axis contraction of the stable C11b phase. The observed lattice response is proportional in magnitude to the growth rate, suggesting that the behavior is associated with the kinetic trapping of lattice defects. MD simulations demonstrate that this lattice response is due to incorporation of 1% to 2% antisite defects during growth.

  16. Strengthening of defected beam–column joints using CFRP

    Directory of Open Access Journals (Sweden)

    Mohamed H. Mahmoud

    2014-01-01

    Full Text Available This paper presents an experimental study for the structural performance of reinforced concrete (RC exterior beam–column joints rehabilitated using carbon-fiber-reinforced polymer (CFRP. The present experimental program consists of testing 10 half-scale specimens divided into three groups covering three possible defects in addition to an adequately detailed control specimen. The considered defects include the absence of the transverse reinforcement within the joint core, insufficient bond length for the beam main reinforcement and inadequate spliced implanted column on the joint. Three different strengthening schemes were used to rehabilitate the defected beam–column joints including externally bonded CFRP strips and sheets in addition to near surface mounted (NSM CFRP strips. The failure criteria including ultimate capacity, mode of failure, initial stiffness, ductility and the developed ultimate strain in the reinforcing steel and CFRP were considered and compared for each group for the control and the CFRP-strengthened specimens. The test results showed that the proposed CFRP strengthening configurations represented the best choice for strengthening the first two defects from the viewpoint of the studied failure criteria. On the other hand, the results of the third group showed that strengthening the joint using NSM strip technique enabled the specimen to outperform the structural performance of the control specimen while strengthening the joints using externally bonded CFRP strips and sheets failed to restore the strengthened joints capacity.

  17. Strengthening of defected beam-column joints using CFRP.

    Science.gov (United States)

    Mahmoud, Mohamed H; Afefy, Hamdy M; Kassem, Nesreen M; Fawzy, Tarek M

    2014-01-01

    This paper presents an experimental study for the structural performance of reinforced concrete (RC) exterior beam-column joints rehabilitated using carbon-fiber-reinforced polymer (CFRP). The present experimental program consists of testing 10 half-scale specimens divided into three groups covering three possible defects in addition to an adequately detailed control specimen. The considered defects include the absence of the transverse reinforcement within the joint core, insufficient bond length for the beam main reinforcement and inadequate spliced implanted column on the joint. Three different strengthening schemes were used to rehabilitate the defected beam-column joints including externally bonded CFRP strips and sheets in addition to near surface mounted (NSM) CFRP strips. The failure criteria including ultimate capacity, mode of failure, initial stiffness, ductility and the developed ultimate strain in the reinforcing steel and CFRP were considered and compared for each group for the control and the CFRP-strengthened specimens. The test results showed that the proposed CFRP strengthening configurations represented the best choice for strengthening the first two defects from the viewpoint of the studied failure criteria. On the other hand, the results of the third group showed that strengthening the joint using NSM strip technique enabled the specimen to outperform the structural performance of the control specimen while strengthening the joints using externally bonded CFRP strips and sheets failed to restore the strengthened joints capacity.

  18. Mechanism of fast lattice diffusion of hydrogen in palladium: Interplay of quantum fluctuations and lattice strain

    Science.gov (United States)

    Kimizuka, Hajime; Ogata, Shigenobu; Shiga, Motoyuki

    2018-01-01

    Understanding the underlying mechanism of the nanostructure-mediated high diffusivity of H in Pd is of recent scientific interest and also crucial for industrial applications. Here, we present a decisive scenario explaining the emergence of the fast lattice-diffusion mode of interstitial H in face-centered cubic Pd, based on the quantum mechanical natures of both electrons and nuclei under finite strains. Ab initio path-integral molecular dynamics was applied to predict the temperature- and strain-dependent free energy profiles for H migration in Pd over a temperature range of 150-600 K and under hydrostatic tensile strains of 0.0%-2.4%; such strain conditions are likely to occur in real systems, especially around the elastic fields induced by nanostructured defects. The simulated results revealed that, for preferential H location at octahedral sites, as in unstrained Pd, the activation barrier for H migration (Q ) was drastically increased with decreasing temperature owing to nuclear quantum effects. In contrast, as tetrahedral sites increased in stability with lattice expansion, nuclear quantum effects became less prominent and ceased impeding H migration. This implies that the nature of the diffusion mechanism gradually changes from quantum- to classical-like as the strain is increased. For H atoms in Pd at the hydrostatic strain of ˜2.4 % , we determined that the mechanism promoted fast lattice diffusion (Q =0.11 eV) of approximately 20 times the rate of conventional H diffusion (Q =0.23 eV) in unstrained Pd at a room temperature of 300 K.

  19. Enzyme markers in inbred rat strains: genetics of new markers and strain profiles.

    Science.gov (United States)

    Adams, M; Baverstock, P R; Watts, C H; Gutman, G A

    1984-08-01

    Twenty-six inbred strains of the laboratory rat (Rattus norvegicus) were examined for electrophoretic variation at an estimated 97 genetic loci. In addition to previously documented markers, variation was observed for the enzymes aconitase, aldehyde dehydrogenase, and alkaline phosphatase. The genetic basis of these markers (Acon-1, Ahd-2, and Akp-1) was confirmed. Linkage analysis between 35 pairwise comparisons revealed that the markers Fh-1 and Pep-3 are linked. The strain profiles of the 25 inbred strains at 11 electrophoretic markers are given.

  20. Genetic analysis of Saccharomyces cerevisiae strains isolated from palm wine in eastern Nigeria. Comparison with other African strains.

    Science.gov (United States)

    Ezeronye, O U; Legras, J-L

    2009-05-01

    To study the yeast diversity of Nigerian palm wines by comparison with other African strains. Twenty-three Saccharomyces cerevisiae strains were obtained from palm wine samples collected at four locations in eastern Nigeria, and characterized using different molecular techniques: internal transcribed spacer restriction fragment length polymorphism and sequence analysis, pulsed field gel electrophoresis, inter delta typing and microsatellite multilocus analysis. These techniques revealed that palm wine yeasts represent a group of closely related strains that includes other West African isolates (CBS400, NCYC110, DVPG6044). Population analysis revealed an excess of homozygote strains and an allelic richness similar to wine suggestive of local domestication. Several other African yeast strains were not connected to this group. Ghana sorghum beer strains and other African strains (DBVPG1853 and MUCL28071) displayed strikingly high relatedness with European bread, beer or wine strains, and the genome of strain MUCL30909 contained African and wine-type alleles, indicating its hybrid origin. Nigerian palm wine yeast represents a local specific yeast flora, whereas a European origin or hybrid was suspected for several other Africa isolates. This study presents the first genetic characterization of an autochthonous African palm wine yeast population and confirms the idea that human intervention has favoured yeast migration.

  1. Mutagenesis at the ad-3A and ad-3B loci in haploid UV-sensitive strains of Neurospora crassa. Pt. 6

    International Nuclear Information System (INIS)

    De Serres, F.J.; Inoue, H.; Schuepbach, M.E.

    1983-01-01

    Genetic characterization of ad-3B mutants induced in wild-type and UV-sensitive strains has revealed qualitative differences between the spectra of genetic alterations at the molecular level. Ad-3B mutants induced in the two nucleotide excision-repair-deficient strains upr-1 and uvs-2 had significantly lower frequencies of nonpolarized complementation patterns and higher frequencies of noncomplementing mutants than ad-3B mutants induced in the wild-type strain in samples induced by either UV, #betta#-rays, 4NQO or MNNG. In these same samples ad-3B mutants induced in uvs-4, uvs-5 or uvs-6 did not differ significantly from those induced in the wild-type strain. After ICR-170 treatment, ad-3B mutants induced in the UV-sensitive strains did not differ significantly from those induced in wild-type. The comparisons in the present and previous studies demonstrate that the process of mutation-induction in the ad-3 region is under the control of other loci that not only alter mutant recovery quantitatively but also qualitatively. These data have important implications for comparative chemical mutagenesis, since the spectrum of genetic alterations produced by a given agent can be modified markedly as a result of defects in DNA repair. (orig./AJ)

  2. Porosity Defect Remodeling and Tensile Analysis of Cast Steel

    Directory of Open Access Journals (Sweden)

    Linfeng Sun

    2016-02-01

    Full Text Available Tensile properties on ASTM A216 WCB cast steel with centerline porosity defect were studied with radiographic mapping and finite element remodeling technique. Non-linear elastic and plastic behaviors dependent on porosity were mathematically described by relevant equation sets. According to the ASTM E8 tensile test standard, matrix and defect specimens were machined into two categories by two types of height. After applying radiographic inspection, defect morphologies were mapped to the mid-sections of the finite element models and the porosity fraction fields had been generated with interpolation method. ABAQUS input parameters were confirmed by trial simulations to the matrix specimen and comparison with experimental outcomes. Fine agreements of the result curves between simulations and experiments could be observed, and predicted positions of the tensile fracture were found to be in accordance with the tests. Chord modulus was used to obtain the equivalent elastic stiffness because of the non-linear features. The results showed that elongation was the most influenced term to the defect cast steel, compared with elastic stiffness and yield stress. Additional visual explanations on the tensile fracture caused by void propagation were also given by the result contours at different mechanical stages, including distributions of Mises stress and plastic strain.

  3. Maxillectomy defects: a suggested classification scheme.

    Science.gov (United States)

    Akinmoladun, V I; Dosumu, O O; Olusanya, A A; Ikusika, O F

    2013-06-01

    The term "maxillectomy" has been used to describe a variety of surgical procedures for a spectrum of diseases involving a diverse anatomical site. Hence, classifications of maxillectomy defects have often made communication difficult. This article highlights this problem, emphasises the need for a uniform system of classification and suggests a classification system which is simple and comprehensive. Articles related to this subject, especially those with specified classifications of maxillary surgical defects were sourced from the internet through Google, Scopus and PubMed using the search terms maxillectomy defects classification. A manual search through available literature was also done. The review of the materials revealed many classifications and modifications of classifications from the descriptive, reconstructive and prosthodontic perspectives. No globally acceptable classification exists among practitioners involved in the management of diseases in the mid-facial region. There were over 14 classifications of maxillary defects found in the English literature. Attempts made to address the inadequacies of previous classifications have tended to result in cumbersome and relatively complex classifications. A single classification that is based on both surgical and prosthetic considerations is most desirable and is hereby proposed.

  4. Longitudinal genotyping of Candida dubliniensis isolates reveals strain maintenance, microevolution, and the emergence of itraconazole resistance.

    LENUS (Irish Health Repository)

    Fleischhacker, M

    2010-05-01

    We investigated the population structure of 208 Candida dubliniensis isolates obtained from 29 patients (25 human immunodeficiency virus [HIV] positive and 4 HIV negative) as part of a longitudinal study. The isolates were identified as C. dubliniensis by arbitrarily primed PCR (AP-PCR) and then genotyped using the Cd25 probe specific for C. dubliniensis. The majority of the isolates (55 of 58) were unique to individual patients, and more than one genotype was recovered from 15 of 29 patients. A total of 21 HIV-positive patients were sampled on more than one occasion (2 to 36 times). Sequential isolates recovered from these patients were all closely related, as demonstrated by hybridization with Cd25 and genotyping by PCR. Six patients were colonized by the same genotype of C. dubliniensis on repeated sampling, while strains exhibiting altered genotypes were recovered from 15 of 21 patients. The majority of these isolates demonstrated minor genetic alterations, i.e., microevolution, while one patient acquired an unrelated strain. The C. dubliniensis strains could not be separated into genetically distinct groups based on patient viral load, CD4 cell count, or oropharyngeal candidosis. However, C. dubliniensis isolates obtained from HIV-positive patients were more closely related than those recovered from HIV-negative patients. Approximately 8% (16 of 194) of isolates exhibited itraconazole resistance. Cross-resistance to fluconazole was only observed in one of these patients. Two patients harboring itraconazole-resistant isolates had not received any previous azole therapy. In conclusion, longitudinal genotyping of C. dubliniensis isolates from HIV-infected patients reveals that isolates from the same patient are generally closely related and may undergo microevolution. In addition, isolates may acquire itraconazole resistance, even in the absence of prior azole therapy.

  5. Influence of defect mobility on electrostrain in acceptor-doped Ba{sub 0.80}Sr{sub 0.20}TiO{sub 3}

    Energy Technology Data Exchange (ETDEWEB)

    Vani, K.; Kumar, Viswanathan, E-mail: vkumar10@yahoo.com [Center for Materials for Electronics Technology, Scientific Society, Department of Information Technology, Ministry of Communications and Information Technology, Government of India, Thrissur 680 581, Kerala (India)

    2012-12-15

    This study reports significant differences in the defect-mediated electrostrain in B-site trivalent ions (Fe{sup 3+} and Mn{sup 3+}) doped Barium titanate based system. Electron Paramagnetic Resonance (EPR) Spectroscopy has been employed as a structural probe for understanding the symmetry of defects. Differences in the reorientation of the defect dipoles have been correlated with the electrostrain. Mechanism for the higher strain in Mn-doped system has also been explained.

  6. Edge dislocations as sinks for sub-nanometric radiation induced defects in α-iron

    Science.gov (United States)

    Anento, N.; Malerba, L.; Serra, A.

    2018-01-01

    The role of edge dislocations as sinks for small radiation induced defects in bcc-Fe is investigated by means of atomistic computer simulation. In this work we investigate by Molecular Statics (T = 0K) the interaction between an immobile dislocation line and defect clusters of small sizes invisible experimentally. The study highlights in particular the anisotropy of the interaction and distinguishes between absorbed and trapped defects. When the considered defect intersects the dislocation glide plane and the distance from the dislocation line to the defect is on the range between 2 nm and 4 nm, either total or partial absorption of the cluster takes place leading to the formation of jogs. Residual defects produced during partial absorption pin the dislocation. By the calculation of stress-strain curves we have assessed the strength of those residues as obstacles for the motion of the dislocation, which is reflected on the unpinning stresses and the binding energies obtained. When the defect is outside this range, but on planes close to the dislocation glide plane, instead of absorption we have observed a capture process. Finally, with a view to introducing explicitly in kinetic Monte Carlo models a sink with the shape of a dislocation line, we have summarized our findings on a table presenting the most relevant parameters, which define the interaction of the dislocation with the defects considered.

  7. Study of a radiation point defects ensemble in thin GaAs layers implanted by Be+ and Se+ ions

    International Nuclear Information System (INIS)

    Shcherbachev, K.D.; Bublik, V.T.; Kuripyatnik, A.V.; Yurchuk, S.Yu.

    2001-01-01

    The behaviour of a radiation point defects ensemble in SI-GaAs(100) wafers implanted by Be + (a dose of 1x10 14 at/cm 2 , an energy of 50 and 150 keV) and Se + (a dose of 5x10 14 at/cm 2 , an energy of 150, 180 and 240 keV) ions are studied by a triple-crystal diffractometry method. The strain profile and a number of residual radiation point defects are shown to be determined by defects annihilation, their sink to the surface and rechanneling during the implantation [ru

  8. Sequence analysis of measles virus strains collected during the pre- and early-vaccination era in Denmark reveals a considerable diversity of ancient strains

    DEFF Research Database (Denmark)

    Christensen, Laurids Siig; Schöller, S.; Schierup, M. H.

    2002-01-01

    A total of 199 serum samples from patients with measles collected in Denmark, Greenland and the Faroe Islands from 1964 to 1983 were analysed by PCR. Measles virus (MV) RNA could be detected in 38 (19%) of the samples and a total of 18 strains were subjected to partial sequence analysis of the he......A total of 199 serum samples from patients with measles collected in Denmark, Greenland and the Faroe Islands from 1964 to 1983 were analysed by PCR. Measles virus (MV) RNA could be detected in 38 (19%) of the samples and a total of 18 strains were subjected to partial sequence analysis...... of the hemagglutinin gene. The strains exhibited a considerable genomic diversity, which is at odds with the assumption that one genome type prevailed among globally circulating MV strains prior to the advent of live-attenuated vaccines. Our data indicate that the similarity of the various vaccine strains...... is attributed to their having originated from the same primary isolate. Consequently, it is implied that a small number of clinical manifestations of MV worldwide from which strains similar to the vaccine strain were identified were vaccine related rather than being caused by members of a persistently...

  9. Electrical Characterisation of electron beam exposure induced Defects in silicon

    Energy Technology Data Exchange (ETDEWEB)

    Danga, Helga T., E-mail: helga.danga@up.ac.za; Auret, Francois D.; Coelho, Sergio M.M.; Diale, Mmantsae

    2016-01-01

    The defects introduced in epitaxially grown p-type silicon (Si) during electron beam exposure were electrically characterised using deep level transient spectroscopy (DLTS) and high resolution Laplace-DLTS. In this process, Si samples were first exposed to the conditions of electron beam deposition (EBD) without metal deposition. This is called electron beam exposure (EBE) herein. After 50 minutes of EBE, nickel (Ni) Schottky contacts were fabricated using the resistive deposition method. The defect level observed using the Ni contacts had an activation energy of H(0.55). This defect has an activation energy similar to that of the I-defect. The defect level is similar to that of the HB4, a boron related defect. DLTS depth profiling revealed that H(0.55) could be detected up to a depth of 0.8 μm below the junction. We found that exposing the samples to EBD conditions without metal deposition introduced a defect which was not introduced by the EBD method. We also observed that the damage caused by EBE extended deeper into the material compared to that caused by EBD.

  10. Strain Pattern in Supercooled Liquids

    Science.gov (United States)

    Illing, Bernd; Fritschi, Sebastian; Hajnal, David; Klix, Christian; Keim, Peter; Fuchs, Matthias

    2016-11-01

    Investigations of strain correlations at the glass transition reveal unexpected phenomena. The shear strain fluctuations show an Eshelby-strain pattern [˜cos (4 θ ) /r2 ], characteristic of elastic response, even in liquids, at long times. We address this using a mode-coupling theory for the strain fluctuations in supercooled liquids and data from both video microscopy of a two-dimensional colloidal glass former and simulations of Brownian hard disks. We show that the long-ranged and long-lived strain signatures follow a scaling law valid close to the glass transition. For large enough viscosities, the Eshelby-strain pattern is visible even on time scales longer than the structural relaxation time τ and after the shear modulus has relaxed to zero.

  11. Polymorphism of Paramecium pentaurelia (Ciliophora, Oligohymenophorea) strains revealed by rDNA and mtDNA sequences.

    Science.gov (United States)

    Przyboś, Ewa; Tarcz, Sebastian; Greczek-Stachura, Magdalena; Surmacz, Marta

    2011-05-01

    Paramecium pentaurelia is one of 15 known sibling species of the Paramecium aurelia complex. It is recognized as a species showing no intra-specific differentiation on the basis of molecular fingerprint analyses, whereas the majority of other species are polymorphic. This study aimed at assessing genetic polymorphism within P. pentaurelia including new strains recently found in Poland (originating from two water bodies, different years, seasons, and clones of one strain) as well as strains collected from distant habitats (USA, Europe, Asia), and strains representing other species of the complex. We compared two DNA fragments: partial sequences (349 bp) of the LSU rDNA and partial sequences (618 bp) of cytochrome B gene. A correlation between the geographical origin of the strains and the genetic characteristics of their genotypes was not observed. Different genotypes were found in Kraków in two types of water bodies (Opatkowice-natural pond; Jordan's Park-artificial pond). Haplotype diversity within a single water body was not recorded. Likewise, seasonal haplotype differences between the strains within the artificial water body, as well as differences between clones originating from one strain, were not detected. The clustering of some strains belonging to different species was observed in the phylogenies. Copyright © 2010 Elsevier GmbH. All rights reserved.

  12. Potential of anticlostridial Lactobacillus isolated from cheese to prevent blowing defects in semihard cheese

    DEFF Research Database (Denmark)

    Christiansen, Pia; Vogensen,, F. K.; Nielsen, E. W

    2010-01-01

    Five anticlostridial Lactobacillus strains isolated from cheese were selected for a mixed adjunct culture. Cheese with the mixed adjunct culture (experimental) and without (control) was made in triplicate and ripened as vacuum-packed and surface-ripened cheese. Cheese gross composition was similar....... Excessive gas formation occurred only in control cheeses. In contrast to control cheeses, the experimental cheeses were dominated by the added adjunct Lactobacillus strains (repetitive-PCR). Casein breakdown was not influenced, however, the total amount of amino acids and pH was slightly lower...... in the experimental cheeses. Anticlostridial nonstarter Lactobacillus strains have potential as protective adjunct cultures against blowing defects in cheese....

  13. Vertebral defect, anal atresia, cardiac defect, tracheoesophageal fistula/esophageal atresia, renal defect, and limb defect association with Mayer-Rokitansky-Küster-Hauser syndrome in co-occurrence

    DEFF Research Database (Denmark)

    Bjørsum-Meyer, Thomas; Herlin, Morten; Qvist, Niels

    2016-01-01

    Background: The vertebral defect, anal atresia, cardiac defect, tracheoesophageal fistula/esophageal atresia, renal defect, and limb defect association and Mayer-Rokitansky-Küster-Hauser syndrome are rare conditions. We aimed to present two cases with the vertebral defect, anal atresia, cardiac...... defect, tracheoesophageal fistula/esophageal atresia, renal defect, and limb defect association and Mayer-Rokitansky-Küster-Hauser co-occurrence from our local surgical center and through a systematic literature search detect published cases. Furthermore, we aimed to collect existing knowledge...... in the embryopathogenesis and genetics in order to discuss a possible link between the vertebral defect, anal atresia, cardiac defect, tracheoesophageal fistula/esophageal atresia, renal defect, and limb defect association and Mayer-Rokitansky-Küster-Hauser syndrome. Case presentation: Our first case was a white girl...

  14. Defects and Disorder in the Drosophila Eye

    Science.gov (United States)

    Kim, Sangwoo; Carthew, Richard; Hilgenfeldt, Sascha

    Cell division and differentiation tightly control the regular pattern in the normal eye of the Drosophila fruit fly while certain genetic mutations introduce disorder in the form of topological defects. Analyzing data from pupal retinas, we develop a model based on Voronoi construction that explains the defect statistics as a consequence of area variation of individual facets (ommatidia). The analysis reveals a previously unknown systematic long-range area variation that spans the entire eye, with distinct effects on topological disorder compared to local fluctuations. The internal structure of the ommatidia and the stiffness of their interior cells also plays a crucial role in the defect generation. Accurate predictions of the correlation between the area variation and the defect density in both normal and mutant animals are obtained without free parameters. This approach can potentially be applied to cellular systems in many other contexts to identify size-topology correlations near the onset of symmetry breaking. This work has been supported by the NIH (GM098077) and the NSF (Grant No. 1504301).

  15. Aggregation of endosomal-vacuolar compartments in the Aovps24-deleted strain in the filamentous fungus Aspergillus oryzae

    International Nuclear Information System (INIS)

    Tatsumi, Akinori; Shoji, Jun-ya; Kikuma, Takashi; Arioka, Manabu; Kitamoto, Katsuhiko

    2007-01-01

    Previously, we found that deletion of Aovps24, an ortholog of Saccharomyces cerevisiae VPS24, that encodes an ESCRT (endosomal sorting complex required for transport)-III component required for late endosomal function results in fragmented and aggregated vacuoles. Although defective late endosomal function is likely responsible for this phenotype, critical lack of our knowledge on late endosomes in filamentous fungi prevented us from further characterization. In this study, we identified late endosomes of Aspergillus oryzae, by expressing a series of fusion proteins of fluorescent proteins with orthologs of late endosomal proteins. Using these fusion proteins as markers, we observed late endosomes in the wild type strain and the Aovps24 disruptant and demonstrated that late endosomes are aberrantly aggregated in the Aovps24 disruptant. Moreover, we revealed that the aggregated late endosomes have features of vacuoles as well. As deletion of another ESCRT-III component-encoding gene, Aovps2, resulted in similar phenotypes to that in the Aovps24 disruptant, phenotypes of the Aovps24 disruptant are probably due to defective late endosomal function

  16. Thermal annealing of carbon nanotubes reveals a toxicological impact of the structural defects

    Energy Technology Data Exchange (ETDEWEB)

    Figarol, Agathe, E-mail: figarol@emse.fr [Ecole Nationale Supérieure des Mines, SPIN-EMSE, CNRS: UMR 5307, LGF (France); Pourchez, Jérémie, E-mail: pourchez@emse.fr [Ecole Nationale Supérieure des Mines, CIS-EMSE, EA 4624, SFR IFRESIS, LINA (France); Boudard, Delphine [Université Jean Monnet Saint-Etienne, EA 4624, SFR IFRESIS, LINA (France); Forest, Valérie [Ecole Nationale Supérieure des Mines, CIS-EMSE, EA 4624, SFR IFRESIS, LINA (France); Berhanu, Sarah [Armines - Mines ParisTech, Centre des Matériaux, CNRS UMR 7633 (France); Tulliani, Jean-Marc [Politecnico di Torino, Department of Applied Science and Technology (Italy); Lecompte, Jean-Pierre [Centre Européen de la céramique CNRS: UMR 7315, SPCTS (France); Cottier, Michèle [Université Jean Monnet Saint-Etienne, EA 4624, SFR IFRESIS, LINA (France); Bernache-Assollant, Didier [Ecole Nationale Supérieure des Mines, CIS-EMSE, EA 4624, SFR IFRESIS, LINA (France); Grosseau, Philippe [Ecole Nationale Supérieure des Mines, SPIN-EMSE, CNRS: UMR 5307, LGF (France)

    2015-04-15

    The biological response to pristine and annealed multi-walled carbon nanotubes (MWCNT) was assessed on murine macrophages (RAW 264.7). First, the physicochemical features of the as-produced MWCNT and annealed at 2125 °C for 1 h were fully characterized. A decrease in structural defects, hydrophobicity and catalytic impurities was detected after annealing. Thereafter, their impact on cytotoxicity, oxidative stress, and pro-inflammatory response was investigated at concentrations ranging from 15 to 120 µg mL{sup −1}. No effect of the 2125 °C treatment was detected on the cytotoxicity. In contrast, the annealed carbon nanotubes showed a significant increase of the pro-inflammatory response. We assumed that this behavior was due to the reduction in structural defects that may modify the layer of adsorbed biomolecules. Surprisingly, the purification of metallic catalysts did not have any significant impact on the oxidative stress. We suggested that the structural improvements from the 2125 °C treatment can decrease the carbon nanotube scavenging capacity and thus allow a higher free radical release which may counterbalance the decrease of oxidative stress due to a lower content of metallic impurities.

  17. High-Resolution Typing Reveals Distinct Chlamydia trachomatis Strains in an At-Risk Population in Nanjing, China

    NARCIS (Netherlands)

    Bom, Reinier J. M.; van den Hoek, Anneke; Wang, Qianqiu; Long, Fuquan; de Vries, Henry J. C.; Bruisten, Sylvia M.

    2013-01-01

    We investigated Chlamydia trachomatis strains from Nanjing, China, and whether these strains differed from Amsterdam, the Netherlands. C. trachomatis type was determined with multilocus sequence typing. Most strains were specific to Nanjing, but some clustered with strains from Amsterdam. This

  18. Investigation of a weld defect, reactor vessel head Ringhals 2

    International Nuclear Information System (INIS)

    Embring, G.; Pers-Anderson, E.B.

    1994-01-01

    During the summer-outage 1993 Ringhals unit 2 vessel head was inspected at weld-area of Alloy 182. One major defect was found Two plus two ''boat-samples'' were taken out from the zone between the weld and the stainless cladding. All samples were sent to Studsviks laboratories for detailed investigations. The metallographic and fractographic investigations revealed that the major weld-defect had been there from manufacturing. The defect was located between the Alloy 182-buttering and the pressure vessel steel SA 533 grB cl 1. No indications of PWSCC or IDSCC were found. An inspection programme was defined. Different types of reference blocks were provided by Ringhals in cooperation with ABB TRC. Reference reflectors of type flat bottom hole (FBH) and eroded notches (EDM), with different sizes and separation were manufactured. One weld sample with manufacturing defects -lack of fusion and slag was inclusions- was present. ABB TRC performed UT inspection in the gap between the penetration and the thermal sleeve. Inspection results like defect identification, defect separation and defect sizing accuracy were compared with result from the destructive inspection. No relevant additional defects were found. An analysing and repair program was performed. A special designed disc sealed off the defect area. (authors). 5 figs., 3 refs

  19. Perception of color emotions for single colors in red-green defective observers.

    Science.gov (United States)

    Sato, Keiko; Inoue, Takaaki

    2016-01-01

    It is estimated that inherited red-green color deficiency, which involves both the protan and deutan deficiency types, is common in men. For red-green defective observers, some reddish colors appear desaturated and brownish, unlike those seen by normal observers. Despite its prevalence, few studies have investigated the effects that red-green color deficiency has on the psychological properties of colors (color emotions). The current study investigated the influence of red-green color deficiency on the following six color emotions: cleanliness, freshness, hardness, preference, warmth, and weight. Specifically, this study aimed to: (1) reveal differences between normal and red-green defective observers in rating patterns of six color emotions; (2) examine differences in color emotions related to the three cardinal channels in human color vision; and (3) explore relationships between color emotions and color naming behavior. Thirteen men and 10 women with normal vision and 13 men who were red-green defective performed both a color naming task and an emotion rating task with 32 colors from the Berkeley Color Project (BCP). Results revealed noticeable differences in the cleanliness and hardness ratings between the normal vision observers, particularly in women, and red-green defective observers, which appeared mainly for colors in the orange to cyan range, and in the preference and warmth ratings for colors with cyan and purple hues. Similarly, naming errors also mainly occurred in the cyan colors. A regression analysis that included the three cone-contrasts (i.e., red-green, blue-yellow, and luminance) as predictors significantly accounted for variability in color emotion ratings for the red-green defective observers as much as the normal individuals. Expressly, for warmth ratings, the weight of the red-green opponent channel was significantly lower in color defective observers than in normal participants. In addition, the analyses for individual warmth ratings in

  20. Perception of color emotions for single colors in red-green defective observers

    Directory of Open Access Journals (Sweden)

    Keiko Sato

    2016-12-01

    Full Text Available It is estimated that inherited red-green color deficiency, which involves both the protan and deutan deficiency types, is common in men. For red-green defective observers, some reddish colors appear desaturated and brownish, unlike those seen by normal observers. Despite its prevalence, few studies have investigated the effects that red-green color deficiency has on the psychological properties of colors (color emotions. The current study investigated the influence of red-green color deficiency on the following six color emotions: cleanliness, freshness, hardness, preference, warmth, and weight. Specifically, this study aimed to: (1 reveal differences between normal and red-green defective observers in rating patterns of six color emotions; (2 examine differences in color emotions related to the three cardinal channels in human color vision; and (3 explore relationships between color emotions and color naming behavior. Thirteen men and 10 women with normal vision and 13 men who were red-green defective performed both a color naming task and an emotion rating task with 32 colors from the Berkeley Color Project (BCP. Results revealed noticeable differences in the cleanliness and hardness ratings between the normal vision observers, particularly in women, and red-green defective observers, which appeared mainly for colors in the orange to cyan range, and in the preference and warmth ratings for colors with cyan and purple hues. Similarly, naming errors also mainly occurred in the cyan colors. A regression analysis that included the three cone-contrasts (i.e., red-green, blue-yellow, and luminance as predictors significantly accounted for variability in color emotion ratings for the red-green defective observers as much as the normal individuals. Expressly, for warmth ratings, the weight of the red-green opponent channel was significantly lower in color defective observers than in normal participants. In addition, the analyses for individual warmth

  1. Strain relaxation of CdTe on Ge studied by medium energy ion scattering

    Energy Technology Data Exchange (ETDEWEB)

    Pillet, J.C., E-mail: jean-christophe.pillet@cea.fr [Univ. Grenoble Alpes, CEA, LETI, MINATEC campus, F38000 Grenoble (France); CEA, LETI, Département Optique et Photonique, F38054 Grenoble (France); Pierre, F. [Univ. Grenoble Alpes, CEA, LETI, MINATEC campus, F38000 Grenoble (France); CEA, LETI, Service de Caractérisation des Matériaux et Composants, F38054 Grenoble (France); Jalabert, D. [Univ. Grenoble Alpes, CEA, LETI, MINATEC campus, F38000 Grenoble (France); CEA-INAC/UJF-Grenoble 1 UMR-E, SP2M, LEMMA, Minatec Grenoble F-38054 (France)

    2016-10-01

    We have used the medium energy ion scattering (MEIS) technique to assess the strain relaxation in molecular-beam epitaxial (MBE) grown CdTe (2 1 1)/Ge (2 1 1) system. A previous X-ray diffraction study, on 10 samples of the same heterostructure having thicknesses ranging from 25 nm to 10 μm has allowed the measurement of the strain relaxation on a large scale. However, the X-ray diffraction measurements cannot achieve a stress measurement in close proximity to the CdTe/Ge interface at the nanometer scale. Due to the huge lattice misfit between the CdTe and Ge, a high degree of disorder is expected at the interface. The MEIS in channeling mode is a good alternative in order to profile defects with a high depth resolution. For a 21 nm thick CdTe layer, we observed, at the interface, a high density of Cd and/or Te atoms moved from their expected crystallographic positions followed by a rapid recombination of defects. Strain relaxation mechanisms in the vicinity of the interface are discussed.

  2. Birth Defects

    Science.gov (United States)

    A birth defect is a problem that happens while a baby is developing in the mother's body. Most birth defects happen during the first 3 months of ... in the United States is born with a birth defect. A birth defect may affect how the ...

  3. Physical nature of strain rate sensitivity of metals and alloys at high strain rates

    Science.gov (United States)

    Borodin, E. N.; Gruzdkov, A. A.; Mayer, A. E.; Selyutina, N. S.

    2018-04-01

    The role of instabilities of plastic flow at plastic deformation of various materials is one of the important cross-disciplinary problems which is equally important in physics, mechanics and material science. The strain rate sensitivities under slow and high strain rate conditions of loading have different physical nature. In the case of low strain rate, the sensitivity arising from the inertness of the defect structures evolution can be expressed by a single parameter characterizing the plasticity mechanism. In our approach, this is the value of the characteristic relaxation time. In the dynamic case, there are additional effects of “high-speed sensitivity” associated with the micro-localization of the plastic flow near the stress concentrators. In the frames of mechanical description, this requires to introduce additional strain rate sensitivity parameters, which is realized in numerous modifications of Johnson–Cook and Zerilli–Armstrong models. The consideration of both these factors is fundamental for an adequate description of the problems of dynamic deformation of highly inhomogeneous metallic materials such as steels and alloys. The measurement of the dispersion of particle velocities on the free surface of a shock-loaded material can be regarded as an experimental expression of the effect of micro-localization. This is also confirmed by our results of numerical simulation of the propagation of shock waves in a two-dimensional formulation and analytical estimations.

  4. Sequencing of bovine herpesvirus 4 v.test strain reveals important genome features

    Directory of Open Access Journals (Sweden)

    Gillet Laurent

    2011-08-01

    Full Text Available Abstract Background Bovine herpesvirus 4 (BoHV-4 is a useful model for the human pathogenic gammaherpesviruses Epstein-Barr virus and Kaposi's Sarcoma-associated Herpesvirus. Although genome manipulations of this virus have been greatly facilitated by the cloning of the BoHV-4 V.test strain as a Bacterial Artificial Chromosome (BAC, the lack of a complete genome sequence for this strain limits its experimental use. Methods In this study, we have determined the complete sequence of BoHV-4 V.test strain by a pyrosequencing approach. Results The long unique coding region (LUR consists of 108,241 bp encoding at least 79 open reading frames and is flanked by several polyrepetitive DNA units (prDNA. As previously suggested, we showed that the prDNA unit located at the left prDNA-LUR junction (prDNA-G differs from the other prDNA units (prDNA-inner. Namely, the prDNA-G unit lacks the conserved pac-2 cleavage and packaging signal in its right terminal region. Based on the mechanisms of cleavage and packaging of herpesvirus genomes, this feature implies that only genomes bearing left and right end prDNA units are encapsulated into virions. Conclusions In this study, we have determined the complete genome sequence of the BAC-cloned BoHV-4 V.test strain and identified genome organization features that could be important in other herpesviruses.

  5. Influence of damages caused by surface defects upon the oxydation mechanism of inconel 600

    International Nuclear Information System (INIS)

    Rousselet, J.M.; Moulin, G.; Huntz, A.M.

    1985-01-01

    The influence of thermochemical and mechanical treatments on the oxidation mechanism of Ni 76 Cr 16 Fe 8 alloys (Inconel 600) was studied from a kinetic and analytical point of view, in order to clarify the role of defects either due to a prestrain or related to impurities such as S, C. for example to overcome sulfur pollution of steam generator tubes of nuclear power plant. For unstrained alloys, the oxidation process is controlled by the diffusion of alloy elements in the metallic substrate. But, beyond a critical strain value, the diffusion rate in the alloy is sufficiently accelerated by the strain induced defects to involve an oxidation control by the diffusion of base-elements (Cr, Ni, Fe) in the oxide scale. Sulfides present in the alloy (due to a pre-sulphidation treatment) strongly accelerate the oxidation kinetics owing to the fact that a first oxidation step, controlled by a chemical process of sulphide decomposition, takes place simultaneously to an internal oxidation; then, a second step related to sulphur diffusion through the oxide scale appears; sulphur in the oxide scale creates defects which accelerate cationic diffusion in the oxides. The baneful influence of sulphur can be balanced by prestraining the material [fr

  6. Life Stress, Strain, and Deviance Across Schools: Testing the Contextual Version of General Strain Theory in China.

    Science.gov (United States)

    Zhang, Jinwu; Liu, Jianhong; Wang, Xin; Zou, Anquan

    2017-08-01

    General Strain Theory delineates different types of strain and intervening processes from strain to deviance and crime. In addition to explaining individual strain-crime relationship, a contextualized version of general strain theory, which is called the Macro General Strain Theory, has been used to analyze how aggregate variables influence aggregate and individual deviance and crime. Using a sample of 1,852 students (Level 1) nested in 52 schools (Level 2), the current study tests the Macro General Strain Theory using Chinese data. The results revealed that aggregate life stress and strain have influences on aggregate and individual deviance, and reinforce the individual stress-deviance association. The current study contributes by providing the first Macro General Strain Theory test based on Chinese data and offering empirical evidence for the multilevel intervening processes from strain to deviance. Limitations and future research directions are discussed.

  7. Sequencing of emerging canine distemper virus strain reveals new distinct genetic lineage in the United States associated with disease in wildlife and domestic canine populations.

    Science.gov (United States)

    Riley, Matthew C; Wilkes, Rebecca P

    2015-12-18

    Recent outbreaks of canine distemper have prompted examination of strains from clinical samples submitted to the University of Tennessee College of Veterinary Medicine (UTCVM) Clinical Virology Lab. We previously described a new strain of CDV that significantly diverged from all genotypes reported to date including America 2, the genotype proposed to be the main lineage currently circulating in the US. The aim of this study was to determine when this new strain appeared and how widespread it is in animal populations, given that it has also been detected in fully vaccinated adult dogs. Additionally, we sequenced complete viral genomes to characterize the strain and determine if variation is confined to known variable regions of the genome or if the changes are also present in more conserved regions. Archived clinical samples were genotyped using real-time RT-PCR amplification and sequencing. The genomes of two unrelated viruses from a dog and fox each from a different state were sequenced and aligned with previously published genomes. Phylogenetic analysis was performed using coding, non-coding and genome-length sequences. Virus neutralization assays were used to evaluate potential antigenic differences between this strain and a vaccine strain and mixed ANOVA test was used to compare the titers. Genotyping revealed this strain first appeared in 2011 and was detected in dogs from multiple states in the Southeast region of the United States. It was the main strain detected among the clinical samples that were typed from 2011-2013, including wildlife submissions. Genome sequencing demonstrated that it is highly conserved within a new lineage and preliminary serologic testing showed significant differences in neutralizing antibody titers between this strain and the strain commonly used in vaccines. This new strain represents an emerging CDV in domestic dogs in the US, may be associated with a stable reservoir in the wildlife population, and could facilitate vaccine

  8. Amino acids interacting with defected carbon nanotubes: ab initio calculations

    Directory of Open Access Journals (Sweden)

    M. Darvish Ganji

    2016-09-01

    Full Text Available The adsorption of a number of amino acids on a defected single-walled carbon nanotube (SWCNT is investigated by using the density-functional theory (DFT calculations. The adsorption energies and equilibrium distances are calculated for various configurations such as amino acid attaching to defect sites heptagon, pentagon and hexagon in defective tube and also for several molecular orientations with respect to the nanotube surface. The results showed that amino acids prefer to be physisorbed on the outer surface of the defected nanotube with different interaction strength following the hierarchy histidine > glycine > phenylalanine > cysteine. Comparing these findings with those obtained for perfect SWCNTs reveals that the adsorption energy of the amino acids increase for adsorption onto defected CNTs. The adsorption nature has also been evaluated by means of electronics structures analysis within the Mulliken population and DOS spectra for the interacting entities.

  9. Comparative genome analysis of Prevotella intermedia strain isolated from infected root canal reveals features related to pathogenicity and adaptation.

    Science.gov (United States)

    Ruan, Yunfeng; Shen, Lu; Zou, Yan; Qi, Zhengnan; Yin, Jun; Jiang, Jie; Guo, Liang; He, Lin; Chen, Zijiang; Tang, Zisheng; Qin, Shengying

    2015-02-25

    Many species of the genus Prevotella are pathogens that cause oral diseases. Prevotella intermedia is known to cause various oral disorders e.g. periodontal disease, periapical periodontitis and noma as well as colonize in the respiratory tract and be associated with cystic fibrosis and chronic bronchitis. It is of clinical significance to identify the main drive of its various adaptation and pathogenicity. In order to explore the intra-species genetic differences among strains of Prevotella intermedia of different niches, we isolated a strain Prevotella intermedia ZT from the infected root canal of a Chinese patient with periapical periodontitis and gained a draft genome sequence. We annotated the genome and compared it with the genomes of other taxa in the genus Prevotella. The raw data set, consisting of approximately 65X-coverage reads, was trimmed and assembled into contigs from which 2165 ORFs were predicted. The comparison of the Prevotella intermedia ZT genome sequence with the published genome sequence of Prevotella intermedia 17 and Prevotella intermedia ATCC25611 revealed that ~14% of the genes were strain-specific. The Preveotella intermedia strains share a set of conserved genes contributing to its adaptation and pathogenic and possess strain-specific genes especially those involved in adhesion and secreting bacteriocin. The Prevotella intermedia ZT shares similar gene content with other taxa of genus Prevotella. The genomes of the genus Prevotella is highly dynamic with relative conserved parts: on average, about half of the genes in one Prevotella genome were not included in another genome of the different Prevotella species. The degree of conservation varied with different pathways: the ability of amino acid biosynthesis varied greatly with species but the pathway of cell wall components biosynthesis were nearly constant. Phylogenetic tree shows that the taxa from different niches are scarcely distributed among clades. Prevotella intermedia ZT

  10. Bremsstrahlung-induced highly penetrating probes for nondestructive assay and defect analysis

    CERN Document Server

    Selim, F A; Harmon, J F; Kwofie, J; Spaulding, R; Erickson, G; Roney, T

    2002-01-01

    Nondestructive assay and defect analysis probes based on bremsstrahlung-induced processes have been developed to identify elements and probe defects in large volume samples. Bremsstrahlung beams from (electron accelerators) with end-point energies both above and below neutron emission threshold have been used. Below neutron emission threshold these beams (from 6 MeV small pulsed linacs), which exhibit high penetration, create positrons via pair production inside the material and produce X-ray fluorescence (XRF) radiation. Chemical assays of heavy elements in thick samples up to 10 g/cm sup 2 thick are provided by energy dispersive XRF measurements. The pair-produced positrons annihilate within the material, thereby emitting 511 keV gamma radiation. Doppler broadening spectroscopy of the 511 keV radiation can be performed to characterize the material and measure defects in samples of any desired thickness. This technique has successfully measured induced strain due to tensile stress in steel samples of 0.64 cm...

  11. Percutaneous closure of a post-traumatic ventricular septal defect with a patent ductus arteriosus occluder

    Directory of Open Access Journals (Sweden)

    Er-Ping Xi

    2012-11-01

    Full Text Available OBJECTIVE: Ventricular septal defects resulting from post-traumatic cardiac injury are very rare. Percutaneous closure has emerged as a method for treating this disorder. We wish to report our experience in three patients who underwent percutaneous closure of a post-traumatic ventricular septal defect with a patent ductus arteriosus occluder. METHODS: We treated three patients with post-traumatic ventricular septal defects caused by stab wounds with knives. After the heart wound was repaired, patient examinations revealed ventricular septal defects with pulmonary/systemic flow ratios (Qp/Qs of over 1.7. The post-traumatic ventricular septal defects were closed percutaneously with a patent ductus arteriosus occluder (Lifetech Scientific (Shenzhen Co., LTD, Guangdong, China utilizing standard techniques. RESULTS: Post-operative transthoracic echocardiography revealed no residual left-to-right shunt and indicated normal ventricular function. In addition, 320-slice computerized tomography showed that the occluder was well placed and exhibited normal morphology. CONCLUSION: Our experiences indicate that closure of a post-traumatic ventricular septal defect using a patent ductus arteriosus occluder is feasible, safe, and effective.

  12. Percutaneous closure of a post-traumatic ventricular septal defect with a patent ductus arteriosus occluder.

    Science.gov (United States)

    Xi, Er-Ping; Zhu, Jian; Zhu, Shui-Bo; Yin, Gui-Lin; Liu, Yong; Dong, Yong-Qiang; Zhang, Yu; Xia, Feng

    2012-11-01

    Ventricular septal defects resulting from post-traumatic cardiac injury are very rare. Percutaneous closure has emerged as a method for treating this disorder. We wish to report our experience in three patients who underwent percutaneous closure of a post-traumatic ventricular septal defect with a patent ductus arteriosus occluder. We treated three patients with post-traumatic ventricular septal defects caused by stab wounds with knives. After the heart wound was repaired, patient examinations revealed ventricular septal defects with pulmonary/systemic flow ratios (Qp/Qs) of over 1.7. The post-traumatic ventricular septal defects were closed percutaneously with a patent ductus arteriosus occluder (Lifetech Scientific (Shenzhen) Co., LTD, Guangdong, China) utilizing standard techniques. Post-operative transthoracic echocardiography revealed no residual left-to-right shunt and indicated normal ventricular function. In addition, 320-slice computerized tomography showed that the occluder was well placed and exhibited normal morphology. Our experiences indicate that closure of a post-traumatic ventricular septal defect using a patent ductus arteriosus occluder is feasible, safe, and effective.

  13. Feasibility and Accuracy of Digitizing Edentulous Maxillectomy Defects: A Comparative Study.

    Science.gov (United States)

    Elbashti, Mahmoud E; Hattori, Mariko; Patzelt, Sebastian Bm; Schulze, Dirk; Sumita, Yuka I; Taniguchi, Hisashi

    The aim of this study was to evaluate the feasibility and accuracy of using an intraoral scanner to digitize edentulous maxillectomy defects. A total of 20 maxillectomy models with two defect types were digitized using cone beam computed tomography. Conventional and digital impressions were made using silicone impression material and a laboratory optical scanner as well as a chairside intraoral scanner. The 3D datasets were analyzed using 3D evaluation software. Two-way analysis of variance revealed no interaction between defect types and impression methods, and the accuracy of the impression methods was significantly different (P = .0374). Digitizing edentulous maxillectomy defect models using a chairside intraoral scanner appears to be feasible and accurate.

  14. Optical properties of a defective one-dimensional photonic crystal containing graphene nanaolayers

    International Nuclear Information System (INIS)

    Entezar, S. Roshan; Saleki, Z.; Madani, A.

    2015-01-01

    The transmission properties of a defective one-dimensional photonic crystal containing graphene nanolayers have been investigated using the transfer matrix method. It is shown that two kinds of the defect modes can be found in the band gaps of the structure. One kind is the traditional defect mode which is created in the Bragg gaps of the structure and is due to the breaking of the periodicity of the dielectric lattice. The other one is created in the graphene induced band gap. Such a defect mode which we call it the graphene induced defect mode is due to the breaking of the periodicity of the graphene lattice. However, our investigations reveal that only in the case of wide defect layers one can obtain the graphene induced defect modes. The effects of many parameters such as the incident angle, the state of polarization and the chemical potential of the graphene nanolayers on the properties of the graphene induced defect modes are discussed. Moreover, the possibility of external control of the graphene induced defect modes using a gate voltage is shown.

  15. Defect Characterization, Imaging, and Control in Wide-Bandgap Semiconductors and Devices

    Science.gov (United States)

    Brillson, L. J.; Foster, G. M.; Cox, J.; Ruane, W. T.; Jarjour, A. B.; Gao, H.; von Wenckstern, H.; Grundmann, M.; Wang, B.; Look, D. C.; Hyland, A.; Allen, M. W.

    2018-03-01

    Wide-bandgap semiconductors are now leading the way to new physical phenomena and device applications at nanoscale dimensions. The impact of defects on the electronic properties of these materials increases as their size decreases, motivating new techniques to characterize and begin to control these electronic states. Leading these advances have been the semiconductors ZnO, GaN, and related materials. This paper highlights the importance of native point defects in these semiconductors and describes how a complement of spatially localized surface science and spectroscopy techniques in three dimensions can characterize, image, and begin to control these electronic states at the nanoscale. A combination of characterization techniques including depth-resolved cathodoluminescence spectroscopy, surface photovoltage spectroscopy, and hyperspectral imaging can describe the nature and distribution of defects at interfaces at both bulk and nanoscale surfaces, their metal interfaces, and inside nanostructures themselves. These features as well as temperature and mechanical strain inside wide-bandgap device structures at the nanoscale can be measured even while these devices are operating. These advanced capabilities enable several new directions for describing defects at the nanoscale, showing how they contribute to device degradation, and guiding growth processes to control them.

  16. Elimination of active tad elements during the sexual phase of the Neurospora crassa life cycle.

    Science.gov (United States)

    Anderson, C; Tang, Q; Kinsey, J A

    2001-06-01

    Tad is an active LINE-like retrotransposon isolated from the Adiopodoumé strain of Neurospora crassa. Extensive analysis of other Neurospora strains has revealed no other strain with active Tad, but all strains tested have multiple copies of defective Tad elements. We have examined the ability of Tad to survive during the sexual cycle of Neurospora and find that active Tad is rapidly eliminated. The characteristics of this elimination suggest that the repeat-induced point mutation (RIP) mechanism was responsible. By the use of transformation to switch the mating type of the Adiopodoumé strain we concluded that this strain is not defective in the RIP process. Analysis of defective Tad elements isolated from a variety of strains indicates that the major difference between these elements and active Tad is due to the presence of a large number of G-C to A-T transition mutations. This would be expected if the changes were due primarily to the RIP process. Mapping of a selection of defective Tad elements reveals that they are present on all of the chromosomes; however, many of the elements are not widely shared among strains. This suggests that repeated introduction and elimination of Tad elements has occurred. Mechanisms that might be responsible for this repeated introduction are discussed. Copyright 2001 Academic Press.

  17. Development of an embedded thin-film strain-gauge-based SHM network into 3D-woven composite structure for wind turbine blades

    Science.gov (United States)

    Zhao, Dongning; Rasool, Shafqat; Forde, Micheal; Weafer, Bryan; Archer, Edward; McIlhagger, Alistair; McLaughlin, James

    2017-04-01

    Recently, there has been increasing demand in developing low-cost, effective structure health monitoring system to be embedded into 3D-woven composite wind turbine blades to determine structural integrity and presence of defects. With measuring the strain and temperature inside composites at both in-situ blade resin curing and in-service stages, we are developing a novel scheme to embed a resistive-strain-based thin-metal-film sensory into the blade spar-cap that is made of composite laminates to determine structural integrity and presence of defects. Thus, with fiberglass, epoxy, and a thinmetal- film sensing element, a three-part, low-cost, smart composite laminate is developed. Embedded strain sensory inside composite laminate prototype survived after laminate curing process. The internal strain reading from embedded strain sensor under three-point-bending test standard is comparable. It proves that our proposed method will provide another SHM alternative to reduce sensing costs during the renewable green energy generation.

  18. Prevention of congenital defects induced by prenatal alcohol exposure (Conference Presentation)

    Science.gov (United States)

    Sheehan, Megan M.; Karunamuni, Ganga; Pedersen, Cameron J.; Gu, Shi; Doughman, Yong Qiu; Jenkins, Michael W.; Watanabe, Michiko; Rollins, Andrew M.

    2017-02-01

    Over 500,000 women per year in the United States drink during pregnancy, and 1 in 5 of this population also binge drink. Up to 40% of live-born children with prenatal alcohol exposure (PAE) present with congenital heart defects (CHDs) including life-threatening outflow and valvuloseptal anomalies. Previously we established a PAE model in the avian embryo and used optical coherence tomography (OCT) imaging to assay looping-stage (early) cardiac function/structure and septation-stage (late) cardiac defects. Early-stage ethanol-exposed embryos had smaller cardiac cushions (valve precursors) and increased retrograde flow, while late-stage embryos presented with gross head/body defects, and exhibited smaller atrio-ventricular (AV) valves, interventricular septae, and aortic vessels. However, supplementation with the methyl donor betaine reduced gross defects, prevented cardiac defects such as ventricular septal defects and abnormal AV valves, and normalized cardiac parameters. Immunofluorescent staining for 5-methylcytosine in transverse embryo sections also revealed that DNA methylation levels were reduced by ethanol but normalized by co-administration of betaine. Furthermore, supplementation with folate, another methyl donor, in the PAE model appeared to normalize retrograde flow levels which are typically elevated by ethanol exposure. Studies are underway to correlate retrograde flow numbers for folate with associated cushion volumes. Finally, preliminary findings have revealed that glutathione, a key endogenous antioxidant which also regulates methyl group donation, is particularly effective in improving alcohol-impacted survival and gross defect rates. Current investigations will determine whether glutathione has any positive effect on PAE-related CHDs. Our studies could have significant implications for public health, especially related to prenatal nutrition recommendations.

  19. Atomistic simulations of divacancy defects in armchair graphene nanoribbons: Stability, electronic structure, and electron transport properties

    Energy Technology Data Exchange (ETDEWEB)

    Zhao, Jun [College of Physical Science and Technology, Yangtze University, Jingzhou, Hubei 434023 (China); Zeng, Hui, E-mail: zenghui@yangtzeu.edu.cn [College of Physical Science and Technology, Yangtze University, Jingzhou, Hubei 434023 (China); Wei, Jianwei [College of Optoelectronic Information, Chongqing University of Technology, Chongqing 400054 (China); Li, Biao; Xu, Dahai [College of Physical Science and Technology, Yangtze University, Jingzhou, Hubei 434023 (China)

    2014-01-17

    Using the first principles calculations associated with nonequilibrium Green's function, we have studied the electronic structures and quantum transport properties of defective armchair graphene nanoribbon (AGNR) in the presence of divacancy defects. The triple pentagon–triple heptagon (555–777) defect in the defective AGNR is energetically more favorable than the pentagon–octagon–pentagon (5–8–5) defect. Our calculated results reveal that both 5–8–5-like defect and 555–777-like defect in AGNR could improve the electron transport. It is anticipated that defective AGNRs can exhibit large range variations in transport behaviors, which are strongly dependent on the distributions of the divacancy defect.

  20. Case history of a 94 MVA turbo-generator retired after 190.000 hours of service by defects revealed by boresonic in-service inspection

    International Nuclear Information System (INIS)

    Porro, F.; Santoro, M.

    1990-01-01

    The case-history of a turbogenerator manufactured by Ansaldo on 1957 and turned on operation on 1958 then retired after 30 years of operation, with a total of 190.000 hours of service, by defects revealed trough boresonic inspections, will be presented. The rotor was inspected a first time after 130.000 hours of service and was overbored in order to allow further service operations. After other 60.000 hours of service operation the rotor underwent to a new in-service inspection that showed an unacceptable condition. The rotor, retired from service, has been destined to destructive tests in order to verify non-destructive predictions

  1. Defect driven tailoring of colossal dielectricity of Reduced Graphene Oxide

    Energy Technology Data Exchange (ETDEWEB)

    Sarkar, S.; Mondal, A. [Department of Physics, Jadavpur University, Kolkata 700 032 (India); Dey, K. [Department of Solid State Physics, Indian Association for the Cultivation of Science, Jadavpur, Kolkata 700 032 (India); Ray, R., E-mail: juphyruma@gmail.com [Department of Physics, Jadavpur University, Kolkata 700 032 (India)

    2016-02-15

    Highlights: • Reduced graphene oxides (RGO) are prepared by two chemical routes. • Defects in RGO are characterized by Raman, FTIR and XPS studies. • Defects tailor colossal dielectricity in RGO. - Abstract: Reduced graphene oxide (RGO) is prepared in two different chemical routes where reduction of graphene oxide is performed by hydrazine hydrate and through high pressure in hydrothermal reactor. Samples are characterized by X-ray powdered diffraction (XRD), thermo gravimetric analysis (TGA), field emission scanning electron microscopy (FESEM) and tunneling electron microscopy (TEM). Types of defects are probed by Raman, FTIR spectroscopy and X-ray photoelectron spectroscopy (XPS). UV–vis absorption reveals different optical band gaps of the two RGOs. Conductivity mechanism is studied through I–V measurements displaying different characteristic features which are addressed due to the presence of defects appeared in different synthesis. Significantly high value (∼10{sup 4}) of dielectric permittivity at 10 MHz is attractive for technological application which could be tuned by the defects present in RGO.

  2. Regularities of radiation defects build up on oxide materials surface

    International Nuclear Information System (INIS)

    Bitenbaev, M.I.; Polyakov, A.I.; Tuseev, T.

    2005-01-01

    Analysis of experimental data by radiation defects study on different oxide elements (silicon, beryllium, aluminium, rare earth elements) irradiated by the photo-, gamma-, neutron-, alpha- radiation, protons and helium ions show, that gas adsorption process on the surface centers and radiation defects build up in metal oxide correlated between themselves. These processes were described by the equivalent kinetic equations for analysis of radiation defects build up in the different metal oxides. It was revealed in the result of the analysis: number of radiation defects are droningly increasing up to limit value with the treatment temperature growth. Constant of radicals death at ionizing radiation increases as well. Amount of surface defects in different oxides defining absorbing activity of these materials looks as: silicon oxide→beryllium oxide→aluminium oxide. So it was found, that most optimal material for absorbing system preparation is silicon oxide by it power intensity and berylium oxide by it adsorption efficiency

  3. Origin of the strain glass transition in Ti_5_0(Ni_5_0_−_x D_x) alloys

    International Nuclear Information System (INIS)

    Wang, Xu; Shang, Jia-Xiang; Wang, Fu-He; Chen, Yue

    2016-01-01

    Direct evidence was recently discovered for the unique strain glass (STG) transition, which breaks the local symmetries (PRL 112, 025701 (2014)). To understand the origin of the STG transition, the effects of doping point defects on Ti_5_0(Ni_5_0_−_x D_x) are investigated using first-principle calculations. The experimental observation that STG only exists in a limited range of chemical composition x is successfully rationalized. The mechanisms that correspond to the division of a system into domains with distinctly different compositions are found to be directly related to a dip in the defect formation energy. - Highlights: • The strain glass transition phenomenon in Ti−Ni-based alloys is rationalized. • The electronic-structure origins of the strain glass transition are uncovered. • The separation of domains with different compositions is explained.

  4. Strain release in metastable CdSe/CdS quantum dots

    Energy Technology Data Exchange (ETDEWEB)

    Gong, Ke; Beane, Gary; Kelley, David F., E-mail: dfkelley@ucmerced.edu

    2016-06-01

    Highlights: • We have synthesized CdSe/CdS core/shell quantum dots in the “stable” and “metastable” regimes. • Annealing of metastable particles causes lattice strain release, producing hole-trapping defects. • Electron microscopy imaging is relatively insensitive to defects that result in rapid radiationless decay. - Abstract: It has recently been shown (J. Phys. Chem. Lett., 2015, 6, 1559) that high quantum yields (QYs) in zincblende CdSe/CdS quantum dots can be achieved when the lattice strain energy density is in the stable (0–0.59 eV/nm{sup 2}) or metastable (0.59–0.85 eV/nm{sup 2}) regime. Annealing of metastable particles causes a dramatic reduction in the observed QY and a red shift of the absorbance and photoluminescence. In this work we demonstrate that the decline in QY upon annealing is due to the formation of hole traps. These traps, while dramatically affecting the observed QY, produce no significant changes in either morphology or crystallinity as determined by high resolution transmission electron microscopy (HRTEM).

  5. Influence of an uniaxial stress on point defects

    International Nuclear Information System (INIS)

    Beuneu, B.

    1984-03-01

    We study two effects of an elastic external uniaxial stress on point defects (created by electron irradiation): 1.- We measure the linear variation of their resistivity rhosub(D) under the elastic strain epsilon in Copper. It gives the specific elastoresistivity (E.R.S.) chisub(D)=delta rhosub(D)/epsilon. With the help of the results of VON STEBUT (fast neutrons) we show that the E.R.S. is characteristic of a defect and of its configuration. 2.- By means of resistivity measurements in molybdenum, we observe a paraelastic phenomenon. It is thermally activated (νsub(0) approximately= 10 12 s -1 and E approximately= 72 meV) and we attribute it to the reorientation of a dumbell interstitial under the uniaxial stress. The resistivity of this dumbbell is higher along its axis than perpendicularly to it. We have completed these results with some configuration energy calculations for the dumbbell and with a simple kinetic model [fr

  6. The complete genome sequence of Bacillus velezensis strain GH1-13 reveals agriculturally beneficial properties and a unique plasmid.

    Science.gov (United States)

    Kim, Sang Yoon; Song, Hajin; Sang, Mee Kyung; Weon, Hang-Yeon; Song, Jaekyeong

    2017-10-10

    The bacterial strain Bacillus velezensis GH1-13, isolated from rice paddy soil in Korea, has been shown to promote plant growth and have strong antagonistic activities against pathogens. Here, we report the complete genome sequence of GH1-13, revealing that it possesses a single 4,071,980-bp circular chromosome with 46.2% GC-content. The chromosome encodes 3,930 genes, and we have also identified a unique plasmid in the strain that encodes a further 104 genes (71,628bp and 31.7% GC-content). The genome was found to contain various enzyme-encoding operons, including indole-3-acetic acid (IAA) biosynthesis proteins, 2,3-butanediol dehydrogenase, various non-ribosomal peptide synthetases, and several polyketide synthases. These properties are responsible for the promotion of plant growth and the biosynthesis of secondary metabolites. They therefore have multiple beneficial effects that could be applied to agriculture. Through curing, we found that the unique plasmid of GH1-13 has important roles in the production of phytohormones, such as IAA, and in shaping phenotypic and physiological characteristics. The plasmid therefore likely influences the biological activities of GH1-13. The complete genome sequence of B. velezensis GH1-13 contributes to our understanding of this beneficial strain and will encourage research into its development for agricultural or biotechnological applications, enhancing productivity and crop quality. Copyright © 2017 Elsevier B.V. All rights reserved.

  7. Transcriptomic profiling of diverse Aedes aegypti strains reveals increased basal-level immune activation in dengue virus-refractory populations and identifies novel virus-vector molecular interactions.

    Directory of Open Access Journals (Sweden)

    Shuzhen Sim

    Full Text Available Genetic variation among Aedes aegypti populations can greatly influence their vector competence for human pathogens such as the dengue virus (DENV. While intra-species transcriptome differences remain relatively unstudied when compared to coding sequence polymorphisms, they also affect numerous aspects of mosquito biology. Comparative molecular profiling of mosquito strain transcriptomes can therefore provide valuable insight into the regulation of vector competence. We established a panel of A. aegypti strains with varying levels of susceptibility to DENV, comprising both laboratory-maintained strains and field-derived colonies collected from geographically distinct dengue-endemic regions spanning South America, the Caribbean, and Southeast Asia. A comparative genome-wide gene expression microarray-based analysis revealed higher basal levels of numerous immunity-related gene transcripts in DENV-refractory mosquito strains than in susceptible strains, and RNA interference assays further showed different degrees of immune pathway contribution to refractoriness in different strains. By correlating transcript abundance patterns with DENV susceptibility across our panel, we also identified new candidate modulators of DENV infection in the mosquito, and we provide functional evidence for two potential DENV host factors and one potential restriction factor. Our comparative transcriptome dataset thus not only provides valuable information about immune gene regulation and usage in natural refractoriness of mosquito populations to dengue virus but also allows us to identify new molecular interactions between the virus and its mosquito vector.

  8. Whole genome sequencing reveals complex evolution patterns of multidrug-resistant Mycobacterium tuberculosis Beijing strains in patients.

    Directory of Open Access Journals (Sweden)

    Matthias Merker

    Full Text Available Multidrug-resistant (MDR Mycobacterium tuberculosis complex (MTBC strains represent a major threat for tuberculosis (TB control. Treatment of MDR-TB patients is long and less effective, resulting in a significant number of treatment failures. The development of further resistances leads to extensively drug-resistant (XDR variants. However, data on the individual reasons for treatment failure, e.g. an induced mutational burst, and on the evolution of bacteria in the patient are only sparsely available. To address this question, we investigated the intra-patient evolution of serial MTBC isolates obtained from three MDR-TB patients undergoing longitudinal treatment, finally leading to XDR-TB. Sequential isolates displayed identical IS6110 fingerprint patterns, suggesting the absence of exogenous re-infection. We utilized whole genome sequencing (WGS to screen for variations in three isolates from Patient A and four isolates from Patient B and C, respectively. Acquired polymorphisms were subsequently validated in up to 15 serial isolates by Sanger sequencing. We determined eight (Patient A and nine (Patient B polymorphisms, which occurred in a stepwise manner during the course of the therapy and were linked to resistance or a potential compensatory mechanism. For both patients, our analysis revealed the long-term co-existence of clonal subpopulations that displayed different drug resistance allele combinations. Out of these, the most resistant clone was fixed in the population. In contrast, baseline and follow-up isolates of Patient C were distinguished each by eleven unique polymorphisms, indicating an exogenous re-infection with an XDR strain not detected by IS6110 RFLP typing. Our study demonstrates that intra-patient microevolution of MDR-MTBC strains under longitudinal treatment is more complex than previously anticipated. However, a mutator phenotype was not detected. The presence of different subpopulations might confound phenotypic and

  9. Defect of Fe-S cluster binding by DNA polymerase δ in yeast suppresses UV-induced mutagenesis, but enhances DNA polymerase ζ - dependent spontaneous mutagenesis.

    Science.gov (United States)

    Stepchenkova, E I; Tarakhovskaya, E R; Siebler, H M; Pavlov, Y I

    2017-01-01

    Eukaryotic genomes are duplicated by a complex machinery, utilizing high fidelity replicative B-family DNA polymerases (pols) α, δ and ε. Specialized error-prone pol ζ, the fourth B-family member, is recruited when DNA synthesis by the accurate trio is impeded by replication stress or DNA damage. The damage tolerance mechanism dependent on pol ζ prevents DNA/genome instability and cell death at the expense of increased mutation rates. The pol switches occurring during this specialized replication are not fully understood. The loss of pol ζ results in the absence of induced mutagenesis and suppression of spontaneous mutagenesis. Disruption of the Fe-S cluster motif that abolish the interaction of the C-terminal domain (CTD) of the catalytic subunit of pol ζ with its accessory subunits, which are shared with pol δ, leads to a similar defect in induced mutagenesis. Intriguingly, the pol3-13 mutation that affects the Fe-S cluster in the CTD of the catalytic subunit of pol δ also leads to defective induced mutagenesis, suggesting the possibility that Fe-S clusters are essential for the pol switches during replication of damaged DNA. We confirmed that yeast strains with the pol3-13 mutation are UV-sensitive and defective in UV-induced mutagenesis. However, they have increased spontaneous mutation rates. We found that this increase is dependent on functional pol ζ. In the pol3-13 mutant strain with defective pol δ, there is a sharp increase in transversions and complex mutations, which require functional pol ζ, and an increase in the occurrence of large deletions, whose size is controlled by pol ζ. Therefore, the pol3-13 mutation abrogates pol ζ-dependent induced mutagenesis, but allows for pol ζ recruitment for the generation of spontaneous mutations and prevention of larger deletions. These results reveal differential control of the two major types of pol ζ-dependent mutagenesis by the Fe-S cluster present in replicative pol δ. Copyright © 2016

  10. Post-UV colony-forming ability of normal fibroblast strains and of the xeroderma pigmentosum group G strain

    International Nuclear Information System (INIS)

    Barrett, S.F.; Tarone, R.E.; Moshell, A.N.; Ganges, M.B.; Robbins, J.H.

    1981-01-01

    In xeroderma pigmentosum, an inherited disorder of defective DNA repair, post-uv colony-forming ability of fibroblasts from patients in complementation groups A through F correlates with the patients' neurological status. The first xeroderma pigmentosum patient assigned to the recently discovered group G had the neurological abnormalities of XP. Researchers have determined the post-uv colony-forming ability of cultured fibroblasts from this patient and from 5 more control donors. Log-phase fibroblasts were irradiated with 254 nm uv light from a germicidal lamp, trypsinized, and replated at known densities. After 2 to 4 weeks' incubation the cells were fixed, stained and scored for colony formation. The strains' post-uv colony-forming ability curves were obtained by plotting the log of the percent remaining post-uv colony-forming ability as a function of the uv dose. The post-uv colony-forming ability of 2 of the 5 new normal strains was in the previously defined control donor zone, but that of the other 3 extended down to the level of the most resistant xeroderma pigmentosum strain. The post-uv colony-forming ability curve of the group G fibroblasts was not significantly different from the curves of the group D fibroblast strains from patients with clinical histories similar to that of the group G patient

  11. Significant strain accumulation between the deformation front and landward out-of-sequence thrusts in accretionary wedge of SW Taiwan revealed by cGPS and SAR interferometry

    Science.gov (United States)

    Tsai, M. C.

    2017-12-01

    High strain accumulation across the fold-and-thrust belt in Southwestern Taiwan are revealed by the Continuous GPS (cGPS) and SAR interferometry. This high strain is generally accommodated by the major active structures in fold-and-thrust belt of western Foothills in SW Taiwan connected to the accretionary wedge in the incipient are-continent collision zone. The active structures across the high strain accumulation include the deformation front around the Tainan Tableland, the Hochiali, Hsiaokangshan, Fangshan and Chishan faults. Among these active structures, the deformation pattern revealed from cGPS and SAR interferometry suggest that the Fangshan transfer fault may be a left-lateral fault zone with thrust component accommodating the westward differential motion of thrust sheets on both side of the fault. In addition, the Chishan fault connected to the splay fault bordering the lower-slope and upper-slope of the accretionary wedge which could be the major seismogenic fault and an out-of-sequence thrust fault in SW Taiwan. The big earthquakes resulted from the reactivation of out-of-sequence thrusts have been observed along the Nankai accretionary wedge, thus the assessment of the major seismogenic structures by strain accumulation between the frontal décollement and out-of-sequence thrusts is a crucial topic. According to the background seismicity, the low seismicity and mid-crust to mantle events are observed inland and the lower- and upper- slope domain offshore SW Taiwan, which rheologically implies the upper crust of the accretionary wedge is more or less aseimic. This result may suggest that the excess fluid pressure from the accretionary wedge not only has significantly weakened the prism materials as well as major fault zone, but also makes the accretionary wedge landward extension, which is why the low seismicity is observed in SW Taiwan area. Key words: Continuous GPS, SAR interferometry, strain rate, out-of-sequence thrust.

  12. Thermal conductivity of graphene with defects induced by electron beam irradiation

    Science.gov (United States)

    Malekpour, Hoda; Ramnani, Pankaj; Srinivasan, Srilok; Balasubramanian, Ganesh; Nika, Denis L.; Mulchandani, Ashok; Lake, Roger K.; Balandin, Alexander A.

    2016-07-01

    We investigate the thermal conductivity of suspended graphene as a function of the density of defects, ND, introduced in a controllable way. High-quality graphene layers are synthesized using chemical vapor deposition, transferred onto a transmission electron microscopy grid, and suspended over ~7.5 μm size square holes. Defects are induced by irradiation of graphene with the low-energy electron beam (20 keV) and quantified by the Raman D-to-G peak intensity ratio. As the defect density changes from 2.0 × 1010 cm-2 to 1.8 × 1011 cm-2 the thermal conductivity decreases from ~(1.8 +/- 0.2) × 103 W mK-1 to ~(4.0 +/- 0.2) × 102 W mK-1 near room temperature. At higher defect densities, the thermal conductivity reveals an intriguing saturation-type behavior at a relatively high value of ~400 W mK-1. The thermal conductivity dependence on the defect density is analyzed using the Boltzmann transport equation and molecular dynamics simulations. The results are important for understanding phonon - point defect scattering in two-dimensional systems and for practical applications of graphene in thermal management.We investigate the thermal conductivity of suspended graphene as a function of the density of defects, ND, introduced in a controllable way. High-quality graphene layers are synthesized using chemical vapor deposition, transferred onto a transmission electron microscopy grid, and suspended over ~7.5 μm size square holes. Defects are induced by irradiation of graphene with the low-energy electron beam (20 keV) and quantified by the Raman D-to-G peak intensity ratio. As the defect density changes from 2.0 × 1010 cm-2 to 1.8 × 1011 cm-2 the thermal conductivity decreases from ~(1.8 +/- 0.2) × 103 W mK-1 to ~(4.0 +/- 0.2) × 102 W mK-1 near room temperature. At higher defect densities, the thermal conductivity reveals an intriguing saturation-type behavior at a relatively high value of ~400 W mK-1. The thermal conductivity dependence on the defect density is

  13. Effect of Simvastatin collagen graft on wound healing of defective bone

    International Nuclear Information System (INIS)

    Kang, Jun Ho; Kim, Gyu Tae; Choi, Yong Suk; Lee, Hyeon Woo; Hwang, Eui Hwan

    2008-01-01

    To observe and evaluate the effects of Simvastatin-induced osteogenesis on the wound healing of defective bone. 64 defective bones were created in the parietal bone of 32 New Zealand White rabbits. The defects were grafted with collagen matrix carriers mixed with Simvastatin solution in the experimental group of 16 rabbits and with collagen matrix carriers mixed with water in the controlled group. The rabbits were terminated at an interval of 3, 5, 7, and 9 days, 2, 4, 6, and 8 weeks after the formation of defective bone. The wound healing was evaluated by soft X-ray radiography. The tissues within defective bones were evaluated through the analysis of flow cytometry for the manifestation of Runx2 and Osteocalcin, and observed histopathologically by using H-E stain and Masson's trichrome stain. Results : 1. In the experimental group, flow cytometry revealed more manifestation of Runx2 at 5, 7, and 9 days and Osteocalcin at 2 weeks than in the controlled groups, but there was few difference in comparison with the controlled group. 2. In the experimental group, flow cytometry revealed considerably more cells and erythrocytes at 5, 7, and 9 days in comparison with the controlled group. 3. In the experimental group, soft x-ray radiography revealed the extended formation of trabeculation at 2, 4, 6, and 8 weeks. 4. Histopathological features of the experimental group showed more fibroblasts and newly formed vessels at 5 and 7 days, and the formation of osteoid tissues at 9 days, and the newly formed trabeculations at 4 and 6 weeks. As the induced osteogenesis by Simvastatin, there was few contrast of the manifestation between Runx2 and Osteocalcin based on the differentiation of osteoblasts. But it was considered that the more formation of cells and erythrocytes depending on newly formed vessels in the experimental group obviously had an effect on the bone regeneration.

  14. Ambiguous Role of Growth-Induced Defects on the Semiconductor-to-Metal Characteristics in Epitaxial VO2/TiO2 Thin Films.

    Science.gov (United States)

    Mihailescu, Cristian N; Symeou, Elli; Svoukis, Efthymios; Negrea, Raluca F; Ghica, Corneliu; Teodorescu, Valentin; Tanase, Liviu C; Negrila, Catalin; Giapintzakis, John

    2018-04-25

    Controlling the semiconductor-to-metal transition temperature in epitaxial VO 2 thin films remains an unresolved question both at the fundamental as well as the application level. Within the scope of this work, the effects of growth temperature on the structure, chemical composition, interface coherency and electrical characteristics of rutile VO 2 epitaxial thin films grown on TiO 2 substrates are investigated. It is hereby deduced that the transition temperature is lower than the bulk value of 340 K. However, it is found to approach this value as a function of increased growth temperature even though it is accompanied by a contraction along the V 4+ -V 4+ bond direction, the crystallographic c-axis lattice parameter. Additionally, it is demonstrated that films grown at low substrate temperatures exhibit a relaxed state and a strongly reduced transition temperature. It is suggested that, besides thermal and epitaxial strain, growth-induced defects may strongly affect the electronic phase transition. The results of this work reveal the difficulty in extracting the intrinsic material response to strain, when the exact contribution of all strain sources cannot be effectively determined. The findings also bear implications on the limitations in obtaining the recently predicted novel semi-Dirac point phase in VO 2 /TiO 2 multilayer structures.

  15. Use of Multidimensional Fiber Grating Strain Sensors for Damage Detection in Composite Pressure Vessels

    National Research Council Canada - National Science Library

    Kunzler, Marley

    2004-01-01

    ... during curing and pressure cycling near cut tow and Teflon tape defects. These changes in the multi-axis strain due to four pressure cycles and repeated impacts are measured and compared to ultrasonic and eddy current scans...

  16. Transport properties through graphene grain boundaries: strain effects versus lattice symmetry

    Science.gov (United States)

    Hung Nguyen, V.; Hoang, Trinh X.; Dollfus, P.; Charlier, J.-C.

    2016-06-01

    As most materials available at the macroscopic scale, graphene samples usually appear in a polycrystalline form and thus contain grain boundaries. In the present work, the effect of uniaxial strain on the electronic transport properties through graphene grain boundaries is investigated using atomistic simulations. A systematic picture of transport properties with respect to the strain and lattice symmetry of graphene domains on both sides of the boundary is provided. In particular, it is shown that strain engineering can be used to open a finite transport gap in all graphene systems where the two domains are arranged in different orientations. This gap value is found to depend on the strain magnitude, on the strain direction and on the lattice symmetry of graphene domains. By choosing appropriately the strain direction, a large transport gap of a few hundred meV can be achieved when applying a small strain of only a few percents. For a specific class of graphene grain boundary systems, strain engineering can also be used to reduce the scattering on defects and thus to significantly enhance the conductance. With a large strain-induced gap, these graphene heterostructures are proposed to be promising candidates for highly sensitive strain sensors, flexible electronic devices and p-n junctions with non-linear I-V characteristics.

  17. Designing defect-based qubit candidates in wide-gap binary semiconductors for solid-state quantum technologies

    Science.gov (United States)

    Seo, Hosung; Ma, He; Govoni, Marco; Galli, Giulia

    2017-12-01

    The development of novel quantum bits is key to extending the scope of solid-state quantum-information science and technology. Using first-principles calculations, we propose that large metal ion-vacancy pairs are promising qubit candidates in two binary crystals: 4 H -SiC and w -AlN. In particular, we found that the formation of neutral Hf- and Zr-vacancy pairs is energetically favorable in both solids; these defects have spin-triplet ground states, with electronic structures similar to those of the diamond nitrogen-vacancy center and the SiC divacancy. Interestingly, they exhibit different spin-strain coupling characteristics, and the nature of heavy metal ions may allow for easy defect implantation in desired lattice locations and ensure stability against defect diffusion. To support future experimental identification of the proposed defects, we report predictions of their optical zero-phonon line, zero-field splitting, and hyperfine parameters. The defect design concept identified here may be generalized to other binary semiconductors to facilitate the exploration of new solid-state qubits.

  18. Breaking strain of neutron star crust and gravitational waves.

    Science.gov (United States)

    Horowitz, C J; Kadau, Kai

    2009-05-15

    Mountains on rapidly rotating neutron stars efficiently radiate gravitational waves. The maximum possible size of these mountains depends on the breaking strain of the neutron star crust. With multimillion ion molecular dynamics simulations of Coulomb solids representing the crust, we show that the breaking strain of pure single crystals is very large and that impurities, defects, and grain boundaries only modestly reduce the breaking strain to around 0.1. Because of the collective behavior of the ions during failure found in our simulations, the neutron star crust is likely very strong and can support mountains large enough so that their gravitational wave radiation could limit the spin periods of some stars and might be detectable in large-scale interferometers. Furthermore, our microscopic modeling of neutron star crust material can help analyze mechanisms relevant in magnetar giant flares and microflares.

  19. Studies on defect detectability in banded stainless steel tubes

    International Nuclear Information System (INIS)

    Shyamsunder, M.T.; Rao, B.P.C.; Babu Rao, C.; Jayakumar, T.; Kalyanasundaram, P.; Baldev Raj

    1996-01-01

    During inspection of one batch of stainless steel cladding tubes, a few of the tubes gave rise to continuous large amplitude indications throughout the length of the tube. It was observed that the presence of any defects in such tubes would be impossible to detect, due to the poor signal-to-noise ratio. Detailed investigations regarding the surface profile of the tubes were carried out using a novel technique called the projected interferometry method revealed periodic diametral variations and the same were further confirmed by cross sectional profiling. The feasibility of detecting defects in such banded tubes, using eddy current testing were carried out on tubes with artificial defects. This paper discusses the use of three different eddy current methods and their relative performances for inspection. The specific advantages of the phased array eddy current testing method in unambiguous defect detection in situations similar to the one encountered during the present investigations are also discussed. (author)

  20. Application of triple-crystal diffractometry for study of ion implanted layer defects

    International Nuclear Information System (INIS)

    Shcherbachev, K.D.; Bublik, V.T.

    2000-01-01

    Application of a triple-crystal arrangement, unlike traditionally used double-crystal one, allowed one to separate coherent and incoherent scattering components and to improve a resolution significantly. Advantages of the triple-crystal X-ray diffractometry to study defects in ion-implanted layers are demonstrated by example of characterisation of Si-GaAs(100) wafers doped by Si + with energy of 50 keV and does of 1x10 15 and 1x10 14 cm -2 . To explain a behaviour of point defects after implantation and annealing the analysis of strain depth profile was used. Two processes are shown to play a key role in formation of the distorted layer during implantation. The first one is an annihilation of Frenkel pairs components that decreases the total point defects concentration. Another one is a sink of more mobile interstitials to the surface that leads to formation of the thin subsurface layer enriched by vacancies [ru

  1. Optimizing the hydrogen storage in boron nitride nanotubes by defect engineering

    Energy Technology Data Exchange (ETDEWEB)

    Oezdogan, Kemal; Berber, Savas [Physics Department, Gebze Institute of Technology, Cayirova Kampusu, Gebze, 41400 Kocaeli (Turkey)

    2009-06-15

    We use ab initio density functional theory calculations to study the interaction of hydrogen with vacancies in boron nitride nanotubes to optimize the hydrogen storage capacity through defect engineering. The vacancies reconstruct by forming B-B and N-N bonds across the defect site, which are not as favorable as heteronuclear B-N bonds. Our total energy and structure optimization results indicate that the hydrogen cleaves these reconstructing bonds to form more stable atomic structures. The hydrogenated defects offer smaller charge densities that allow hydrogen molecule to pass through the nanotube wall for storing hydrogen inside the nanotubes. Our optimum reaction pathway search revealed that hydrogen molecules could indeed go through a hydrogenated defect site with relatively small energy barriers compared to the pristine nanotube wall. The calculated activation energies for different diameters suggest a preferential diameter range for optimum hydrogen storage in defective boron nitride nanotubes. (author)

  2. Defects improved photocatalytic ability of TiO2

    International Nuclear Information System (INIS)

    Li, Lei; Tian, Hong-Wei; Meng, Fan-Ling; Hu, Xiao-Ying; Zheng, Wei-Tao; Sun, Chang Q.

    2014-01-01

    Highlights: • Defect improves the photocatalytic ability by band gap narrowing and carrier life prolonging. • Atomic undercoordination shortens the local bonds, entraps, and polarizes electrons. • Polarization lowers the local workfunction and lengthens carrier life. • Entrapment and polarization narrows the band gap tuning the wavelength of absorption. - Abstract: Defect generation forms an important means modulating the photocatalytic ability of TiO 2 with mechanisms that remain yet unclear. Here we show that a spectral distillation clarifies the impact of defect on modulating the band gap, electroaffinity, and work function of the substance. Firstly, by analyzing XPS measurements, we calibrated the 2p 3/2 level of 451.47 eV for an isolated Ti atom and its shifts by 2.14 and 6.94 eV, respectively, upon Ti and TiO 2 bulk formation. Spectral difference between the defected and the un-defected TiO 2 skin revealed then that the 2p 3/2 level shifts further from 6.94 to 9.67 eV due to the defect-induced quantum entrapment. This entrapment is associated with an elevation of the upper edges of both the 2p 3/2 and the conduction band by polarization. The shortening and strengthening of bonds between undercoordinated atoms densify and entrap the core electrons, which in turn polarize the dangling bond electrons of defect atoms. The entrapment and polarization mediate thus the band gap, the electroaffinity, the work function, and the photocatalytic ability of TiO 2

  3. Ultraviolet-endonuclease activity in cell extracts of Saccharomyces cerevisiae mutants defective in excision of pyrimidine dimers

    International Nuclear Information System (INIS)

    Bekker, M.L.; Kaboev, O.K.; Akhmedov, A.T.; Luchkina, L.A.

    1980-01-01

    Cell-free extracts of ultraviolet-sensitive mutants of Saccharomyces cerevisiae defective in excision of pyrimidine dimers, rad1, rad2, rad3, rad4, rad10, and rad16, as well as the extracts of the wild-type strain RAD+, display ultraviolet-endonuclease activity

  4. Ductile failure analysis of API X65 pipes with notch-type defects using a local fracture criterion

    International Nuclear Information System (INIS)

    Oh, Chang-Kyun; Kim, Yun-Jae; Baek, Jong-Hyun; Kim, Young-Pyo; Kim, Woo-Sik

    2007-01-01

    A local failure criterion for API X65 steel is applied to predict ductile failure of full-scale API X65 pipes with simulated corrosion and gouge defects under internal pressure. The local failure criterion is the stress-modified fracture strain as a function of the stress triaxiality (defined by the ratio of the hydrostatic stress to the effective stress). Based on detailed finite element (FE) analyses with the proposed local failure criterion, burst pressures of defective pipes are estimated and compared with experimental data. For pipes with simulated corrosion defects, FE analysis with the proposed local fracture criterion indicates that predicted failure takes place after the defective pipes attain maximum loads for all cases, possibly due to the fact that the material has sufficient ductility. For pipes with simulated gouge defects, on the other hand, it is found that predicted failure takes place before global instability, and the predicted burst pressures are in good agreement with experimental data, providing confidence in the present approach

  5. Benzoate Catabolite Repression of the Phthalate Degradation Pathway in Rhodococcus sp. Strain DK17▿

    OpenAIRE

    Choi, Ki Young; Zylstra, Gerben J.; Kim, Eungbin

    2006-01-01

    Rhodococcus sp. strain DK17 exhibits a catabolite repression-like response when provided simultaneously with benzoate and phthalate as carbon and energy sources. Benzoate in the medium is depleted to detection limits before the utilization of phthalate begins. The transcription of the genes encoding benzoate and phthalate dioxygenase paralleled the substrate utilization profile. Two mutant strains with defective benzoate dioxygenases were unable to utilize phthalate in the presence of benzoat...

  6. Immobile defects in ferroelastic walls: Wall nucleation at defect sites

    Science.gov (United States)

    He, X.; Salje, E. K. H.; Ding, X.; Sun, J.

    2018-02-01

    Randomly distributed, static defects are enriched in ferroelastic domain walls. The relative concentration of defects in walls, Nd, follows a power law distribution as a function of the total defect concentration C: N d ˜ C α with α = 0.4 . The enrichment Nd/C ranges from ˜50 times when C = 10 ppm to ˜3 times when C = 1000 ppm. The resulting enrichment is due to nucleation at defect sites as observed in large scale MD simulations. The dynamics of domain nucleation and switching is dependent on the defect concentration. Their energy distribution follows the power law with exponents during yield between ɛ ˜ 1.82 and 2.0 when the defect concentration increases. The power law exponent is ɛ ≈ 2.7 in the plastic regime, independent of the defect concentration.

  7. Surface phenomena revealed by in situ imaging: studies from adhesion, wear and cutting

    Science.gov (United States)

    Viswanathan, Koushik; Mahato, Anirban; Yeung, Ho; Chandrasekar, Srinivasan

    2017-03-01

    Surface deformation and flow phenomena are ubiquitous in mechanical processes. In this work we present an in situ imaging framework for studying a range of surface mechanical phenomena at high spatial resolution and across a range of time scales. The in situ framework is capable of resolving deformation and flow fields quantitatively in terms of surface displacements, velocities, strains and strain rates. Three case studies are presented demonstrating the power of this framework for studying surface deformation. In the first, the origin of stick-slip motion in adhesive polymer interfaces is investigated, revealing a intimate link between stick-slip and surface wave propagation. Second, the role of flow in mediating formation of surface defects and wear particles in metals is analyzed using a prototypical sliding process. It is shown that conventional post-mortem observation and inference can lead to erroneous conclusions with regard to formation of surface cracks and wear particles. The in situ framework is shown to unambiguously capture delamination wear in sliding. Third, material flow and surface deformation in a typical cutting process is analyzed. It is shown that a long-standing problem in the cutting of annealed metals is resolved by the imaging, with other benefits such as estimation of energy dissipation and power from the flow fields. In closure, guidelines are provided for profitably exploiting in situ observations to study large-strain deformation, flow and friction phenomena at surfaces that display a variety of time-scales.

  8. Study of the irradiation defects in 3C-SiC

    International Nuclear Information System (INIS)

    Lefevre, J.

    2007-01-01

    This work deals with the study of the irradiation defects in the cubic polytype 3C of the n type silicon carbide. Low temperature photoluminescence and electron spin resonance techniques have been used. In situ photoluminescence measurements after irradiation at 10 K by electrons have shown that the nature of the defects induced is identical to those observed after irradiation at ambient temperature with electrons, protons or carbon ions. No regeneration of these defects has been revealed after in situ annealings until 300 K. The electrons Van de Graff accelerator of the Irradiated Solid Laboratory has allowed to irradiate sample of 3C in a range of energies between 190 keV and 1 MeV. It has then been possible to estimate the appearance threshold of the irradiation defects but especially to be able to determine the displacement threshold energy of silicon in this SiC polytype. The found value of 25 eV is in good agreement with the first experimental result proposed by X. Kerbiriou with the use of the ESR. Annealings in the range of high temperatures have been carried out. The evolution of the irradiation defects has been followed in photoluminescence and in ESR. The results show that, in one part, the vacancy of the silicon negatively charged is essentially the only compensating defect in 3C-SiC of n type and that, in another part, the majority of the defects are annealed below 1200 C. Only the D1 defect remains after annealings until 1600 C. The D1 center is in fact a native defect in SiC; indeed, it has been identified alone in non irradiated samples. A systematic study of these last samples show the absence of D1 in samples strongly compensated. The compared results of photoluminescence and of positons annihilation are in good agreement for the possible attribution of D1 to the bi-vacancy V C -V Si . One of the most interesting result of this last work has been obtained using the ESR technique under excitation with a neodymium laser. The measurements, carried

  9. Improvement of heavy metal stress and toxicity assays by coupling a transgenic reporter in a mutant nematode strain

    Energy Technology Data Exchange (ETDEWEB)

    Chu, K.-W. [Department of Biology, Hong Kong University of Science and Technology, Clear Water Bay, Kowloon, Hong Kong (China); Chan, Shirley K.W. [Atmospheric, Marine and Coastal Environment Program, Hong Kong University of Science and Technology, Clear Water Bay, Kowloon, Hong Kong (China); Chow, King L. [Department of Biology, Hong Kong University of Science and Technology, Clear Water Bay, Kowloon, Hong Kong (China) and Atmospheric, Marine and Coastal Environment Program, Hong Kong University of Science and Technology, Clear Water Bay, Kowloon, Hong Kong (China)]. E-mail: bokchow@ust.hk

    2005-09-30

    Previous studies have demonstrated that wild type Caenorhabditis elegans displays high sensitivity to heavy metals in a lethality test at a level comparable to that of other bioindicator organisms. Taking advantage of the genetics of this model organism, we have tested a number of mutant strains for enhanced sensitivity in heavy metal induced lethality and stress response. These mutants are defective in genes controlling dauer formation, longevity or response to reactive oxygen species (ROS). Among the tested mutants, a double mutant daf-16 unc-75 strain was identified to have superior sensitivity. It has a 6-, 3- and 2-fold increase in sensitivity to cadmium, copper and zinc, respectively, as compared with that of wild type animals. When a fluorescent reporter transgene was coupled with this double mutant for stress detection, a 10-fold enhancement of sensitivity to cadmium over the wild type strain was observed. These transgenic animals, superior to most of the model organisms currently used in bioassays for environmental pollutants, offer a fast and economic approach to reveal the bioavailability of toxic substance in field samples. This study also demonstrates that combination of genetic mutations and transgenesis is a viable approach to identify sensitive indicator animals for environmental monitoring.

  10. Improvement of heavy metal stress and toxicity assays by coupling a transgenic reporter in a mutant nematode strain

    International Nuclear Information System (INIS)

    Chu, K.-W.; Chan, Shirley K.W.; Chow, King L.

    2005-01-01

    Previous studies have demonstrated that wild type Caenorhabditis elegans displays high sensitivity to heavy metals in a lethality test at a level comparable to that of other bioindicator organisms. Taking advantage of the genetics of this model organism, we have tested a number of mutant strains for enhanced sensitivity in heavy metal induced lethality and stress response. These mutants are defective in genes controlling dauer formation, longevity or response to reactive oxygen species (ROS). Among the tested mutants, a double mutant daf-16 unc-75 strain was identified to have superior sensitivity. It has a 6-, 3- and 2-fold increase in sensitivity to cadmium, copper and zinc, respectively, as compared with that of wild type animals. When a fluorescent reporter transgene was coupled with this double mutant for stress detection, a 10-fold enhancement of sensitivity to cadmium over the wild type strain was observed. These transgenic animals, superior to most of the model organisms currently used in bioassays for environmental pollutants, offer a fast and economic approach to reveal the bioavailability of toxic substance in field samples. This study also demonstrates that combination of genetic mutations and transgenesis is a viable approach to identify sensitive indicator animals for environmental monitoring

  11. Shallow nitrogen ion implantation: Evolution of chemical state and defect structure in titanium

    Energy Technology Data Exchange (ETDEWEB)

    Manojkumar, P.A., E-mail: manoj@igcar.gov.in [Indira Gandhi Centre for Atomic Research, Kalpakkam 603102 (India); Chirayath, V.A.; Balamurugan, A.K.; Krishna, Nanda Gopala; Ilango, S.; Kamruddin, M.; Amarendra, G.; Tyagi, A.K. [Indira Gandhi Centre for Atomic Research, Kalpakkam 603102 (India); Raj, Baldev [National Institute of Advanced Studies, Bangalore 560 012 (India)

    2016-09-15

    Highlights: • Low energy nitrogen ion implantation in titanium was studied. • Chemical and defect states were analyzed using SIMS, XPS and PAS. • SIMS and depth resolved XPS data showed good agreement. • Depth resolved defect and chemical states information were revealed. • Formation of 3 layers of defect states proposed to fit PAS results. - Abstract: Evolution of chemical states and defect structure in titanium during low energy nitrogen ion implantation by Plasma Immersion Ion Implantation (PIII) process is studied. The underlying process of chemical state evolution is investigated using secondary ion mass spectrometry and X-ray photoelectron spectroscopy. The implantation induced defect structure evolution as a function of dose is elucidated using variable energy positron annihilation Doppler broadening spectroscopy (PAS) and the results were corroborated with chemical state. Formation of 3 layers of defect state was modeled to fit PAS results.

  12. The electronic transport properties of defected bilayer sliding armchair graphene nanoribbons

    Science.gov (United States)

    Mohammadi, Amin; Haji-Nasiri, Saeed

    2018-04-01

    By applying non-equilibrium Green's functions (NEGF) in combination with tight-binding (TB) model, we investigate and compare the electronic transport properties of perfect and defected bilayer armchair graphene nanoribbons (BAGNRs) under finite bias. Two typical defects which are placed in the middle of top layer (i.e. single vacancy (SV) and stone wale (SW) defects) are examined. The results reveal that in both perfect and defected bilayers, the maximum current refers to β-AB, AA and α-AB stacking orders, respectively, since the intermolecular interactions are stronger in them. Moreover it is observed that a SV decreases the current in all stacking orders, but the effects of a SW defect is nearly unpredictable. Besides, we introduced a sequential switching behavior and the effects of defects on the switching performance is studied as well. We found that a SW defect can significantly improve the switching behavior of a bilayer system. Transmission spectrum, band structure, molecular energy spectrum and molecular projected self-consistent Hamiltonian (MPSH) are analyzed subsequently to understand the electronic transport properties of these bilayer devices which can be used in developing nano-scale bilayer systems.

  13. Enamel Defects of Human Primary Dentition as Virtual Memory of Early Developmental Events

    Directory of Open Access Journals (Sweden)

    Naser Asl Aminabadi

    2009-12-01

    Full Text Available Background and aims. The objectives of the present study were to investigate the prevalence and the position of enamel defects of primary teeth and hence to estimate the approximate time of an insult. Material and methods. 121 children aged 3 to 5 years were included in the study. The Modified Developmental Defects of Enamel Index was used to diagnose and classify the defects. The defects were categorized as hypoplasia, hypocalcification or a combination of them. Each tooth was investigated for occlusal/incisal, middle, cervical, incisomiddle, cervicomiddle and complete crown defects. Results. 55.37% of the children were affected by enamel defects, 23.96% being categorized as hypocalcification and 22.31% as hypoplasia. The enamel defects were more abundant in maxillary primary incisors and mandibular primary canines. Minimum involvement was seen in maxillary primary second molars and mandibular primary lateral incisors. The prevalence of cervical defects in maxillary primary incisors was significantly more than the middle or incisal defects (P < 0.05. The prevalence of incisal defects in mandibular primary incisors was significantly more than the middle or cervical defects (P < 0.05. Conclusions. The results revealed a considerable number of enamel defects which are multiple, symmetric and chronologically accordant with the estimated neonatal line in primary teeth of healthy children.

  14. Defect production in simulated cascades: Cascade quenching and short-term annealing

    International Nuclear Information System (INIS)

    Heinisch, H.L.

    1983-01-01

    Defect production in displacement cascades in copper has been modeled using the MARLOWE code to generate cascades and the stochastic annealing code ALSOME to simulate cascade quenching and short-term annealing of isolated cascades. Quenching is accomplished by using exaggerated values for defect mobilities and for critical reaction distances in ALSOME for a very short time. The quenched cascades are then short-term annealed with normal parameter values. The quenching parameter values were empirically determined by comparison with results of resistivity measurements. Throughout the collisional, quenching and short-term annealing phases of cascade development, the high energy cascades continue to behave as a collection of independent lower energy lobes. For recoils above about 30 keV the total number of defects and the numbers of free defects scale with the damage energy. As the energy decreases from 30 keV, defect production varies with the changing nature of the cascade configuration, resulting in more defects per unit damage energy. The simulated annealing of a low fluence of interacting cascades revealed an interstitial shielding effect on depleted zones during Stage I recovery. (orig.)

  15. Exoproteome analysis reveals higher abundance of proteins linked to alkaline stress in persistent Listeria monocytogenes strains.

    Science.gov (United States)

    Rychli, Kathrin; Grunert, Tom; Ciolacu, Luminita; Zaiser, Andreas; Razzazi-Fazeli, Ebrahim; Schmitz-Esser, Stephan; Ehling-Schulz, Monika; Wagner, Martin

    2016-02-02

    The foodborne pathogen Listeria monocytogenes, responsible for listeriosis a rare but severe infection disease, can survive in the food processing environment for month or even years. So-called persistent L. monocytogenes strains greatly increase the risk of (re)contamination of food products, and are therefore a great challenge for food safety. However, our understanding of the mechanism underlying persistence is still fragmented. In this study we compared the exoproteome of three persistent strains with the reference strain EGDe under mild stress conditions using 2D differential gel electrophoresis. Principal component analysis including all differentially abundant protein spots showed that the exoproteome of strain EGDe (sequence type (ST) 35) is distinct from that of the persistent strain R479a (ST8) and the two closely related ST121 strains 4423 and 6179. Phylogenetic analyses based on multilocus ST genes showed similar grouping of the strains. Comparing the exoproteome of strain EGDe and the three persistent strains resulted in identification of 22 differentially expressed protein spots corresponding to 16 proteins. Six proteins were significantly increased in the persistent L. monocytogenes exoproteomes, among them proteins involved in alkaline stress response (e.g. the membrane anchored lipoprotein Lmo2637 and the NADPH dehydrogenase NamA). In parallel the persistent strains showed increased survival under alkaline stress, which is often provided during cleaning and disinfection in the food processing environments. In addition, gene expression of the proteins linked to stress response (Lmo2637, NamA, Fhs and QoxA) was higher in the persistent strain not only at 37 °C but also at 10 °C. Invasion efficiency of EGDe was higher in intestinal epithelial Caco2 and macrophage-like THP1 cells compared to the persistent strains. Concurrently we found higher expression of proteins involved in virulence in EGDe e.g. the actin-assembly-inducing protein ActA and the

  16. Use of porous silicon to minimize oxidation induced stacking fault defects in silicon

    International Nuclear Information System (INIS)

    Shieh, S.Y.; Evans, J.W.

    1992-01-01

    This paper presents methods for minimizing stacking fault defects, generated during oxidation of silicon, include damaging the back of the wafer or depositing poly-silicon on the back. In either case a highly defective structure is created and this is capable of gettering either self-interstitials or impurities which promote nucleation of stacking fault defects. A novel method of minimizing these defects is to form a patch of porous silicon on the back of the wafer by electrochemical etching. Annealing under inert gas prior to oxidation may then result in the necessary gettering. Experiments were carried out in which wafers were subjected to this treatment. Subsequent to oxidation, the wafers were etched to remove oxide and reveal defects. The regions of the wafer adjacent to the porous silicon patch were defect-free, whereas remote regions had defects. Deep level transient spectroscopy has been used to examine the gettering capability of porous silicon, and the paper discusses the mechanism by which the porous silicon getters

  17. Point defects and magnetic properties of neutron irradiated MgO single crystal

    Directory of Open Access Journals (Sweden)

    Mengxiong Cao

    2017-05-01

    Full Text Available (100-oriented MgO single crystals were irradiated to introduce point defects with different neutron doses ranging from 1.0×1016 to 1.0×1020 cm-2. The point defect configurations were studied with X-ray diffuse scattering and UV-Vis absorption spectra. The isointensity profiles of X-ray diffuse scattering caused by the cubic and double-force point defects in MgO were theoretically calculated based on the Huang scattering theory. The magnetic properties at different temperature were measured with superconducting quantum interference device (SQUID. The reciprocal space mappings (RSMs of irradiated MgO revealed notable diffuse scattering. The UV-Vis spectra indicated the presence of O Frenkel defects in irradiated MgO. Neutron-irradiated MgO was diamagnetic at room temperature and became ferromagnetic at low temperature due to O Frenkel defects induced by neutron-irradiation.

  18. Band Structure Characteristics of Nacreous Composite Materials with Various Defects

    Science.gov (United States)

    Yin, J.; Zhang, S.; Zhang, H. W.; Chen, B. S.

    2016-06-01

    Nacreous composite materials have excellent mechanical properties, such as high strength, high toughness, and wide phononic band gap. In order to research band structure characteristics of nacreous composite materials with various defects, supercell models with the Brick-and-Mortar microstructure are considered. An efficient multi-level substructure algorithm is employed to discuss the band structure. Furthermore, two common systems with point and line defects and varied material parameters are discussed. In addition, band structures concerning straight and deflected crack defects are calculated by changing the shear modulus of the mortar. Finally, the sensitivity of band structures to the random material distribution is presented by considering different volume ratios of the brick. The results reveal that the first band gap of a nacreous composite material is insensitive to defects under certain conditions. It will be of great value to the design and synthesis of new nacreous composite materials for better dynamic properties.

  19. Surface defects characterization in a quantum wire by coherent phonons scattering

    Energy Technology Data Exchange (ETDEWEB)

    Rabia, M. S. [Laboratoire de Mécanique des Structures et Energétique, Faculté du Génie de la Construction, Université. Mammeri de Tizi-Ouzou, BP 17 RP Hasnaoua II, Tizi-Ouzou 15000, Algérie m2msr@yahoo.fr (Algeria)

    2015-03-30

    The influence of surface defects on the scattering properties of elastic waves in a quasi-planar crystallographic waveguide is studied in the harmonic approximation using the matching method formalism. The structural model is based on three infinite atomic chains forming a perfect lattice surmounted by an atomic surface defect. Following the Landauer approach, we solve directly the Newton dynamical equation with scattering boundary conditions and taking into account the next nearest neighbour’s interaction. A detailed study of the defect-induced fluctuations in the transmission spectra is presented for different adatom masses. As in the electronic case, the presence of localized defect-induced states leads to Fano-like resonances. In the language of mechanical vibrations, these are called continuum resonances. Numerical results reveal the intimate relation between transmission spectra and localized defect states and provide a basis for the understanding of conductance spectroscopy experiments in disordered mesoscopic systems. The results could be useful for the design of phononic devices.

  20. Surface defects characterization in a quantum wire by coherent phonons scattering

    International Nuclear Information System (INIS)

    Rabia, M. S.

    2015-01-01

    The influence of surface defects on the scattering properties of elastic waves in a quasi-planar crystallographic waveguide is studied in the harmonic approximation using the matching method formalism. The structural model is based on three infinite atomic chains forming a perfect lattice surmounted by an atomic surface defect. Following the Landauer approach, we solve directly the Newton dynamical equation with scattering boundary conditions and taking into account the next nearest neighbour’s interaction. A detailed study of the defect-induced fluctuations in the transmission spectra is presented for different adatom masses. As in the electronic case, the presence of localized defect-induced states leads to Fano-like resonances. In the language of mechanical vibrations, these are called continuum resonances. Numerical results reveal the intimate relation between transmission spectra and localized defect states and provide a basis for the understanding of conductance spectroscopy experiments in disordered mesoscopic systems. The results could be useful for the design of phononic devices

  1. Transition from Spirals to Defect-Mediated Turbulence Driven by a Doppler Instability

    International Nuclear Information System (INIS)

    Ouyang, Qi; Swinney, Harry L.; Li, Ge

    2000-01-01

    A transition from rotating chemical spirals to turbulence is observed in experiments on the Belousov-Zhabotinsky reaction. The transition occurs when the waves near the spiral tip spontaneously break, generating defects. Measurements reveal that this defect-mediated turbulence is caused by the Doppler effect on the traveling waves. The observations are in good accord with numerical simulations and theory. (c) 2000 The American Physical Society

  2. Influence of ion irradiation induced defects on mechanical properties of copper nanowires

    International Nuclear Information System (INIS)

    Li, Weina; Sun, Lixin; Xue, Jianming; Wang, Jianxiang; Duan, Huiling

    2013-01-01

    The mechanical properties of copper nanowires irradiated with energetic ions have been investigated by using molecular dynamics simulations. The Cu ions with energies ranging from 0.2 to 8.0 keV are used in our simulation, and both the elastic properties and yields under tension and compression are analyzed. The results show that two kinds of defects, namely point defects and stacking faults, appear in the irradiated nanowires depending on the incident ion energy. The Young modulus is significantly reduced by the ion irradiation, and the reduction magnitude depends on the vacancy number, which is determined by the ion energy. Moreover, the irradiated nanowires yield at a smaller strain, compared with the unirradiated nanowire. The mechanism for these changes are also discussed

  3. Formate stability and carbonate hydrogenation on strained Cu overlayers on Pt(111)

    DEFF Research Database (Denmark)

    Schumacher, Nana Maria Pii; Andersson, Klas Jerker; Nerlov, Jesper

    2008-01-01

    Formate (HCOO) synthesis, decomposition and the hydrogenation of carbonate (CO3) on Cu overlayers deposited on a Pt(111) single crystal are investigated to examine the reactivity of a Cu surface under tensile strain with defects present. Formate is synthesized from a 0.5 bar mixture of 70% CO2...

  4. Studies of defects and defect agglomerates by positron annihilation spectroscopy

    DEFF Research Database (Denmark)

    Eldrup, Morten Mostgaard; Singh, B.N.

    1997-01-01

    A brief introduction to positron annihilation spectroscopy (PAS), and in particular lo its use for defect studies in metals is given. Positrons injected into a metal may become trapped in defects such as vacancies, vacancy clusters, voids, bubbles and dislocations and subsequently annihilate from...... the trapped state iri the defect. The annihilation characteristics (e.g., the lifetime of the positron) can be measured and provide information about the nature of the defect (e.g., size, density, morphology). The technique is sensitive to both defect size (in the range from monovacancies up to cavities...

  5. Defect modelling

    International Nuclear Information System (INIS)

    Norgett, M.J.

    1980-01-01

    Calculations, drawing principally on developments at AERE Harwell, of the relaxation about lattice defects are reviewed with emphasis on the techniques required for such calculations. The principles of defect modelling are outlined and various programs developed for defect simulations are discussed. Particular calculations for metals, ionic crystals and oxides, are considered. (UK)

  6. Multiple Genome Sequences of Lactobacillus plantarum Strains

    OpenAIRE

    Kafka, Thomas A.; Geissler, Andreas J.; Vogel, Rudi F.

    2017-01-01

    ABSTRACT We report here the genome sequences of four Lactobacillus plantarum strains which vary in surface hydrophobicity. Bioinformatic analysis, using additional genomes of Lactobacillus plantarum strains, revealed a possible correlation between the cell wall teichoic acid-type and cell surface hydrophobicity and provide the basis for consecutive analyses.

  7. Molecular marker studies in riverine buffaloes, for characterization and diagnosis of genetic defects

    International Nuclear Information System (INIS)

    Yadav, B.R.

    2005-01-01

    The buffalo is probably the last livestock species to have been domesticated, with many genetic, physiological and behavioural traits not yet well understood. Molecular markers have been used for characterizing animals and breeds, diagnosing diseases and identifying anatomical and physiological anomalies. RFLP studies showed low heterozygosity, but genomic and oligonucleotide probes showed species-specific bands useful for identification of carcass or other unknown samples. Use of RAPD revealed band frequencies, band sharing frequencies, genetic distances, and genetic and identity indexes in different breeds. Bovine microsatellite primers indicate that 70.9% of bovine loci were conserved in buffalo. Allele numbers, sizes, frequencies, heterozygosity and polymorphism information content showed breed-specific patterns. Different marker types - genomic and oligonucleotide probes, RAPD and microsatellites - are useful in parent identification. Individual specific DNA fingerprinting techniques were applied with twin-born animal (XX/XY) chimerism, sex identification, anatomically defective and XO individuals. Molecular markers are a potential tool for geneticists and breeders to evaluate existing germplasm and to manipulate it to develop character-specific strains and to provide the basis for effective genetic conservation. (author)

  8. Comparative Genomic Analyses of Multiple Pseudomonas Strains Infecting Corylus avellana Trees Reveal the Occurrence of Two Genetic Clusters with Both Common and Distinctive Virulence and Fitness Traits

    Science.gov (United States)

    Marcelletti, Simone; Scortichini, Marco

    2015-01-01

    The European hazelnut (Corylus avellana) is threatened in Europe by several pseudomonads which cause symptoms ranging from twig dieback to tree death. A comparison of the draft genomes of nine Pseudomonas strains isolated from symptomatic C. avellana trees was performed to identify common and distinctive genomic traits. The thorough assessment of genetic relationships among the strains revealed two clearly distinct clusters: P. avellanae and P. syringae. The latter including the pathovars avellanae, coryli and syringae. Between these two clusters, no recombination event was found. A genomic island of approximately 20 kb, containing the hrp/hrc type III secretion system gene cluster, was found to be present without any genomic difference in all nine pseudomonads. The type III secretion system effector repertoires were remarkably different in the two groups, with P. avellanae showing a higher number of effectors. Homologue genes of the antimetabolite mangotoxin and ice nucleation activity clusters were found solely in all P. syringae pathovar strains, whereas the siderophore yersiniabactin was only present in P. avellanae. All nine strains have genes coding for pectic enzymes and sucrose metabolism. By contrast, they do not have genes coding for indolacetic acid and anti-insect toxin. Collectively, this study reveals that genomically different Pseudomonas can converge on the same host plant by suppressing the host defence mechanisms with the use of different virulence weapons. The integration into their genomes of a horizontally acquired genomic island could play a fundamental role in their evolution, perhaps giving them the ability to exploit new ecological niches. PMID:26147218

  9. Development of stress-modified fracture strain criterion for ductile fracture of API X65 steel

    International Nuclear Information System (INIS)

    Oh, Chang Kyun; Kim, Yun Jae; Park, Jin Moo; Kim, Woo Sik; Baek, Jong Hyun

    2005-01-01

    This paper presents a stress-modified fracture strain for API X65 steel used for gas pipeline, as a function of stress triaxiality. To determine the stress-modified fracture strain, tension test of bars with four different notch radii, made of API X65 steel, is firstly performed, from which true fracture strains are determined as a function of notch radius. Then detailed elastic-plastic, large strain Finite Element (FE) analyses are performed to estimate variations of stress triaxiality in the notched bars with load. Combining experimental with FE results provides the true fracture strain as a function of stress triaxiality, which is regarded as a criterion of ductile fracture. Application of the developed stress-modified fracture strain to failure prediction of gas pipes made of API X65 steel with various types of defects is discussed

  10. Adamts18 deletion results in distinct developmental defects and provides a model for congenital disorders of lens, lung, and female reproductive tract development.

    Science.gov (United States)

    Ataca, Dalya; Caikovski, Marian; Piersigilli, Alessandra; Moulin, Alexandre; Benarafa, Charaf; Earp, Sarah E; Guri, Yakir; Kostic, Corinne; Arsenijevic, Yvan; Soininen, Raija; Apte, Suneel S; Brisken, Cathrin

    2016-11-15

    The ADAMTS family comprises 19 secreted metalloproteinases that cleave extracellular matrix components and have diverse functions in numerous disease and physiological contexts. A number of them remain 'orphan' proteases and among them is ADAMTS18, which has been implicated in developmental eye disorders, platelet function and various malignancies. To assess in vivo function of ADAMTS18, we generated a mouse strain with inactivated Adamts18 alleles. In the C57Bl6/Ola background, Adamts18-deficient mice are born in a normal Mendelian ratio, and are viable but show a transient growth delay. Histological examination revealed a 100% penetrant eye defect resulting from leakage of lens material through the lens capsule occurring at embryonic day (E)13.5, when the lens grows rapidly. Adamts18-deficient lungs showed altered bronchiolar branching. Fifty percent of mutant females are infertile because of vaginal obstruction due to either a dorsoventral vaginal septum or imperforate vagina. The incidence of ovarian rete is increased in the mutant mouse strain. Thus, Adamts18 is essential in the development of distinct tissues and the new mouse strain is likely to be useful for investigating ADAMTS18 function in human disease, particularly in the contexts of infertility and carcinogenesis. © 2016. Published by The Company of Biologists Ltd.

  11. Adamts18 deletion results in distinct developmental defects and provides a model for congenital disorders of lens, lung, and female reproductive tract development

    Directory of Open Access Journals (Sweden)

    Dalya Ataca

    2016-11-01

    Full Text Available The ADAMTS family comprises 19 secreted metalloproteinases that cleave extracellular matrix components and have diverse functions in numerous disease and physiological contexts. A number of them remain ‘orphan’ proteases and among them is ADAMTS18, which has been implicated in developmental eye disorders, platelet function and various malignancies. To assess in vivo function of ADAMTS18, we generated a mouse strain with inactivated Adamts18 alleles. In the C57Bl6/Ola background, Adamts18-deficient mice are born in a normal Mendelian ratio, and are viable but show a transient growth delay. Histological examination revealed a 100% penetrant eye defect resulting from leakage of lens material through the lens capsule occurring at embryonic day (E13.5, when the lens grows rapidly. Adamts18-deficient lungs showed altered bronchiolar branching. Fifty percent of mutant females are infertile because of vaginal obstruction due to either a dorsoventral vaginal septum or imperforate vagina. The incidence of ovarian rete is increased in the mutant mouse strain. Thus, Adamts18 is essential in the development of distinct tissues and the new mouse strain is likely to be useful for investigating ADAMTS18 function in human disease, particularly in the contexts of infertility and carcinogenesis.

  12. Temporal dynamics of the developing lung transcriptome in three common inbred strains of laboratory mice reveals multiple stages of postnatal alveolar development

    Directory of Open Access Journals (Sweden)

    Kyle J. Beauchemin

    2016-08-01

    Full Text Available To characterize temporal patterns of transcriptional activity during normal lung development, we generated genome wide gene expression data for 26 pre- and post-natal time points in three common inbred strains of laboratory mice (C57BL/6J, A/J, and C3H/HeJ. Using Principal Component Analysis and least squares regression modeling, we identified both strain-independent and strain-dependent patterns of gene expression. The 4,683 genes contributing to the strain-independent expression patterns were used to define a murine Developing Lung Characteristic Subtranscriptome (mDLCS. Regression modeling of the Principal Components supported the four canonical stages of mammalian embryonic lung development (embryonic, pseudoglandular, canalicular, saccular defined previously by morphology and histology. For postnatal alveolar development, the regression model was consistent with four stages of alveolarization characterized by episodic transcriptional activity of genes related to pulmonary vascularization. Genes expressed in a strain-dependent manner were enriched for annotations related to neurogenesis, extracellular matrix organization, and Wnt signaling. Finally, a comparison of mouse and human transcriptomics from pre-natal stages of lung development revealed conservation of pathways associated with cell cycle, axon guidance, immune function, and metabolism as well as organism-specific expression of genes associated with extracellular matrix organization and protein modification. The mouse lung development transcriptome data generated for this study serves as a unique reference set to identify genes and pathways essential for normal mammalian lung development and for investigations into the developmental origins of respiratory disease and cancer. The gene expression data are available from the Gene Expression Omnibus (GEO archive (GSE74243. Temporal expression patterns of mouse genes can be investigated using a study specific web resource (http://lungdevelopment.jax.org.

  13. Temporal dynamics of the developing lung transcriptome in three common inbred strains of laboratory mice reveals multiple stages of postnatal alveolar development.

    Science.gov (United States)

    Beauchemin, Kyle J; Wells, Julie M; Kho, Alvin T; Philip, Vivek M; Kamir, Daniela; Kohane, Isaac S; Graber, Joel H; Bult, Carol J

    2016-01-01

    To characterize temporal patterns of transcriptional activity during normal lung development, we generated genome wide gene expression data for 26 pre- and post-natal time points in three common inbred strains of laboratory mice (C57BL/6J, A/J, and C3H/HeJ). Using Principal Component Analysis and least squares regression modeling, we identified both strain-independent and strain-dependent patterns of gene expression. The 4,683 genes contributing to the strain-independent expression patterns were used to define a murine Developing Lung Characteristic Subtranscriptome (mDLCS). Regression modeling of the Principal Components supported the four canonical stages of mammalian embryonic lung development (embryonic, pseudoglandular, canalicular, saccular) defined previously by morphology and histology. For postnatal alveolar development, the regression model was consistent with four stages of alveolarization characterized by episodic transcriptional activity of genes related to pulmonary vascularization. Genes expressed in a strain-dependent manner were enriched for annotations related to neurogenesis, extracellular matrix organization, and Wnt signaling. Finally, a comparison of mouse and human transcriptomics from pre-natal stages of lung development revealed conservation of pathways associated with cell cycle, axon guidance, immune function, and metabolism as well as organism-specific expression of genes associated with extracellular matrix organization and protein modification. The mouse lung development transcriptome data generated for this study serves as a unique reference set to identify genes and pathways essential for normal mammalian lung development and for investigations into the developmental origins of respiratory disease and cancer. The gene expression data are available from the Gene Expression Omnibus (GEO) archive (GSE74243). Temporal expression patterns of mouse genes can be investigated using a study specific web resource (http://lungdevelopment.jax.org).

  14. Comparative physicochemical and biological properties of two strains of Kilham rat virus, a non-defective parvovirus

    Energy Technology Data Exchange (ETDEWEB)

    Mitra, S.; Snyder, C.E.; Bates, R.C.; Banerjee, P.T.

    1982-01-01

    Two antigenically indistinguishable strains, 171 and 308, of Kilham rat virus (KRV) have distinct host ranges and contain capsid proteins of identical size, but with different isoelectric points. The single-stranded DNA genomes of the viruses are also the same size but appear to have different secondary and tertiary structures. The genomes of the two strains have nearly identical cleavage maps for 11 restriction endonucleases. However, there is a lack of extended heteroloy in the nucleotide sequence of the two virus genomes, as judged by electron microscopic analysis of the heteroduplex of the two virus DNAs. This suggests that very subtle differences in the sequences of the genome, and possibly of the capsid proteins, may play a role in the host specificity without affecting the antigenic similarity of KRV strains.

  15. Defects of polar, semipolar and nonpolar (In)GaN - a comparison

    Energy Technology Data Exchange (ETDEWEB)

    Schade, Lukas; Schwarz, Ulrich [Department of Microsystems Engeneering, IMTEK, University Freiburg (Germany); Fraunhofer Institute for Applied Solid State Physics (Germany); Wernicke, Tim; Rass, Jens; Ploch, Simon [Institute of Solid State Physics, Technical University Berlin (Germany); Forghani, Kamran [Institute for Optoelectronics, University Ulm (Germany); University of Wisconsin, Madison (United States); Kirste, Lutz [Fraunhofer Institute for Applied Solid State Physics (Germany); Weyers, Markus [Ferdinand-Braun-Institut, Berlin (Germany); Kneissl, Michael [Institute of Solid State Physics, Technical University Berlin (Germany); Ferdinand-Braun-Institut, Berlin (Germany); Scholz, Ferdinand [Institute for Optoelectronics, University Ulm (Germany)

    2013-07-01

    The GaN/InGaN material system is used to realize light emitting diodes from UV-A to the green-yellow spectral region. However, even on quasi bulk GaN substrates threading dislocations (TDs) are present with a density of 10{sup 7} cm{sup -2}. Here, we examine the influence of TDs on the luminescence intensity and transition energy. The impact caused by nonradiative recombination centers and strain fields is analyzed by micro photoluminescence and white light interferometry. We compare TDs in differently oriented GaN layers and InGaN QWs. Three types of burgers vectors are typically observed in GaN: a, c and a+c. When the surface orientation is changed from (0001) c-plane to (10 anti 10) m-plane, their character changes from edge to screw type and vice versa. We studied TDs and V-defects associated to them in polar, semipolar and nonpolar GaN and InGaN QWs. Additionally, we will present the effect of Si doping onto the strain field in (0001) GaN edge dislocations. In undoped GaN, the strain around such a dislocation forms a symmetric dipole. With Si doping, the strain dipole becomes asymmetric.

  16. A novel system for tracking social preference dynamics in mice reveals sex- and strain-specific characteristics.

    Science.gov (United States)

    Netser, Shai; Haskal, Shani; Magalnik, Hen; Wagner, Shlomo

    2017-01-01

    Deciphering the biological mechanisms underlying social behavior in animal models requires standard behavioral paradigms that can be unbiasedly employed in an observer- and laboratory-independent manner. During the past decade, the three-chamber test has become such a standard paradigm used to evaluate social preference (sociability) and social novelty preference in mice. This test suffers from several caveats, including its reliance on spatial navigation skills and negligence of behavioral dynamics. Here, we present a novel experimental apparatus and an automated analysis system which offer an alternative to the three-chamber test while solving the aforementioned caveats. The custom-made apparatus is simple for production, and the analysis system is publically available as an open-source software, enabling its free use. We used this system to compare the dynamics of social behavior during the social preference and social novelty preference tests between male and female C57BL/6J mice. We found that in both tests, male mice keep their preference towards one of the stimuli for longer periods than females. We then employed our system to define several new parameters of social behavioral dynamics in mice and revealed that social preference behavior is segregated in time into two distinct phases. An early exploration phase, characterized by high rate of transitions between stimuli and short bouts of stimulus investigation, is followed by an interaction phase with low transition rate and prolonged interactions, mainly with the preferred stimulus. Finally, we compared the dynamics of social behavior between C57BL/6J and BTBR male mice, the latter of which are considered as asocial strain serving as a model for autism spectrum disorder. We found that BTBR mice ( n  = 8) showed a specific deficit in transition from the exploration phase to the interaction phase in the social preference test, suggesting a reduced tendency towards social interaction. We successfully

  17. Electrical characterization of copper related defect reactions in silicon

    Energy Technology Data Exchange (ETDEWEB)

    Heiser, T. [Centre National de la Recherche Scientifique, 67 - Strasbourg (France). Lab. PHASE; Istratov, A.A.; Flink, C.; Weber, E.R. [Department of Material Science and Mineral Engineering, University of California at Berkeley, 577 Evans Hall, Berkeley, CA 94720 (United States)

    1999-02-12

    Defect reactions involving interstitial copper impurities (Cu{sub i}) in silicon are reviewed. The influence of the Coulomb interaction between positively charged copper and negatively charged defects, such as acceptor states of transition metals and lattice defects, on the complex formation rate is discussed in detail. The diffusivity of interstitial copper and the dissociation kinetics of copper-acceptor pairs are studied using the recently introduced transient ion drift (TID) method. TID results reveal that most interstitial copper impurities remain dissolved immediately after the quench and form pairs with shallow acceptors. It is shown that in moderately and heavily doped silicon the diffusivity of copper is trap limited, while in low B-doped silicon the interstitial copper-acceptor pairing is weak enough to allow the assessment of the copper intrinsic diffusion coefficient. The intrinsic diffusion barrier is estimated to be 0.18{+-}0.01 eV. It is concluded that the Coulomb potential used in previous publications underestimated considerably the acceptor-copper interaction. In light of these results, a general discussion on Cu related defect reactions is given. (orig.) 44 refs.

  18. Identification of 17 hearing impaired mouse strains in the TMGC ENU-mutagenesis screen

    Energy Technology Data Exchange (ETDEWEB)

    Kermany, Mohammad [St. Jude Children' s Research Hospital; Parker, Lisan [St. Jude Children' s Research Hospital; Guo, Yun-Kai [St. Jude Children' s Research Hospital; Miller, Darla R [ORNL; Swanson, Douglas J [ORNL; Yoo, Tai-June [Neuroscience Institute, Memphis, TN; Goldowitz, Daniel [University of Tennessee Health Science Center, Memphis; Zuo, Jian [St. Jude Children' s Research Hospital

    2006-01-01

    The Tennessee Mouse Genome Consortium (TMGC) employed an N-ethyl-N-nitrosourea (ENU)-mutagenesis scheme to identify mouse recessive mutants with hearing phenotypes. We employed auditory brainstem responses (ABR) to click and 8, 16, and 32 kHz stimuli and screened 285 pedigrees (1819 mice of 8-11 weeks old in various mixed genetic backgrounds) each bred to carry a homozygous ENU-induced mutation. To define mutant pedigrees, we measured P12 mice per pedigree in P2 generations and used a criterion where the mean ABR threshold per pedigree was two standard deviations above the mean of all offspring from the same parental strain. We thus identified 17 mutant pedigrees (6%), all exhibiting hearing loss at high frequencies (P16 kHz) with an average threshold elevation of 30-35 dB SPL. Interestingly, four mutants showed sex-biased hearing loss and six mutants displayed wide range frequency hearing loss. Temporal bone histology revealed that six of the first nine mutants displayed cochlear morphological defects: degeneration of spiral ganglia, spiral ligament fibrocytes or inner hair cells (but not outer hair cells) mostly in basal turns. In contrast to other ENU-mutagenesis auditory screens, our screen identified high-frequency, mild and sex-biased hearing defects. Further characterization of these 17 mouse models will advance our understanding of presbycusis and noise-induced hearing loss in humans.

  19. Research on the Phenotypic Characterization of Mrsa Strains Isolated from Animals

    Directory of Open Access Journals (Sweden)

    Iulia Maria BUCUR

    2017-05-01

    Full Text Available Keywords: chromogen, methicillin, MRSA, resistance Introduction: Currently, both in staphylococci isolated from animals with different diseases, as well as in humans, the MRSA strains (Methicillin Resistant S. aureus are monitored, as the methicillin resistance is associated with the resistance to other antibiotic groups. Methicillin resistance is encoded by mec staphylococcal chromosomal cassettes (SCCmec, which are islands of resistance. These strains can be identified by molecular biology tests and tests that reveal several phenotypic characteristics. The research was made in order to characterize and identify phenotypically the MRSA staphylococci strains isolated from animals. Materials and Methods: Researches were made on 240 coagulase positive and coagulase negative strains of staphylococci. Mannitol fermentation was tested on Champan medium, free coagulase was revealed on Baird-Parker medium and to identify S. aureus subsp. aureus was used the chromogenic medium Chromatic Staph. Methicillin-resistant strains were detected by disc diffusion method, using biodiscs with methicillin, oxacillin and cefoxitin. Also, to identify the MRSA strains, was used the chromogenic medium Chromatic MRSA. Results: The isolates were positive to mannitol and produced complete haemolysis or were unhaemolytic. A total of 44 strains produced free coagulase on Baird-Parker medium, considered coagulase positive strains, while 196 were coagulase negative strains. The isolates conducted differently to methicillin: 22,08% of strains were resistant, 51,25% of strains were susceptible and 26,66% had intermediate resistance, while the resistant strains to oxacillin were 42,91%. The increased frequency of methicillin-resistant strains of staphylococci and, particularly, MRSA strains, determined using the cefoxitin disk diffusion test, which is more reliable than methicillin and oxacillin. On the MRSA chromogenic medium, the methicillin-resistant strains of staphylococci

  20. Effects of in-cascade defect clustering on near-term defect evolution

    Energy Technology Data Exchange (ETDEWEB)

    Heinisch, H.L. [Pacific Northwest National Lab., Richland, WA (United States)

    1997-08-01

    The effects of in-cascade defect clustering on the nature of the subsequent defect population are being studied using stochastic annealing simulations applied to cascades generated in molecular dynamics (MD) simulations. The results of the simulations illustrates the strong influence of the defect configuration existing in the primary damage state on subsequent defect evolution. The large differences in mobility and stability of vacancy and interstitial defects and the rapid one-dimensional diffusion of small, glissile interstitial loops produced directly in cascades have been shown to be significant factors affecting the evolution of the defect distribution. In recent work, the effects of initial cluster sizes appear to be extremely important.

  1. Effect of Simvastatin collagen graft on wound healing of defective bone

    Energy Technology Data Exchange (ETDEWEB)

    Kang, Jun Ho; Kim, Gyu Tae [Department of Oral and Maxillofacial Radiology, School of Dentistry, Kyung Hee University, Seoul (Korea, Republic of); Choi, Yong Suk; Lee, Hyeon Woo; Hwang, Eui Hwan [Institute of Oral Biology, School of Dentistry, Kyung Hee University, Seoul (Korea, Republic of)

    2008-09-15

    To observe and evaluate the effects of Simvastatin-induced osteogenesis on the wound healing of defective bone. 64 defective bones were created in the parietal bone of 32 New Zealand White rabbits. The defects were grafted with collagen matrix carriers mixed with Simvastatin solution in the experimental group of 16 rabbits and with collagen matrix carriers mixed with water in the controlled group. The rabbits were terminated at an interval of 3, 5, 7, and 9 days, 2, 4, 6, and 8 weeks after the formation of defective bone. The wound healing was evaluated by soft X-ray radiography. The tissues within defective bones were evaluated through the analysis of flow cytometry for the manifestation of Runx2 and Osteocalcin, and observed histopathologically by using H-E stain and Masson's trichrome stain. Results : 1. In the experimental group, flow cytometry revealed more manifestation of Runx2 at 5, 7, and 9 days and Osteocalcin at 2 weeks than in the controlled groups, but there was few difference in comparison with the controlled group. 2. In the experimental group, flow cytometry revealed considerably more cells and erythrocytes at 5, 7, and 9 days in comparison with the controlled group. 3. In the experimental group, soft x-ray radiography revealed the extended formation of trabeculation at 2, 4, 6, and 8 weeks. 4. Histopathological features of the experimental group showed more fibroblasts and newly formed vessels at 5 and 7 days, and the formation of osteoid tissues at 9 days, and the newly formed trabeculations at 4 and 6 weeks. As the induced osteogenesis by Simvastatin, there was few contrast of the manifestation between Runx2 and Osteocalcin based on the differentiation of osteoblasts. But it was considered that the more formation of cells and erythrocytes depending on newly formed vessels in the experimental group obviously had an effect on the bone regeneration.

  2. Defect-driven inhomogeneities in Ni /4H-SiC Schottky barriers

    Science.gov (United States)

    Tumakha, S.; Ewing, D. J.; Porter, L. M.; Wahab, Q.; Ma, X.; Sudharshan, T. S.; Brillson, L. J.

    2005-12-01

    Nanoscale depth-resolved cathodoluminescence spectroscopy (DRCLS) of Ni diode arrays on 4H-SiC epitaxial wafers reveals a striking correspondence between deep level defects and electrical transport measurements on a diode-by-diode basis. Current-voltage measurements display both ideal and nonideal diode characteristics due to multiple barriers within individual contacts. Near-interface DRCLS demonstrates the presence of three discrete midgap defect levels with 2.2, 2.45, and 2.65eV emission energies whose concentrations vary on a submicron scale among and within individual diodes, correlating with barrier inhomogeneity. These results also suggest that SiC native defect levels can account for the maximum range of n-type barrier heights.

  3. Nature of native defects in ZnO.

    Science.gov (United States)

    Selim, F A; Weber, M H; Solodovnikov, D; Lynn, K G

    2007-08-24

    This study revealed the nature of native defects and their roles in ZnO through positron annihilation and optical transmission measurements. It showed oxygen vacancies are the origin for the shift in the optical absorption band that causes the red or orange coloration. It also revealed experimental evidence that the donor nature of oxygen vacancy is approximately 0.7 eV. In addition, this work showed the Zn interstitial was not the donor in the as-grown ZnO and supported recent calculations that predicted hydrogen in an oxygen vacancy forms multicenter bonds and acts as a shallow donor.

  4. [Congenital skull base defect causing recurrent bacterial meningitis].

    Science.gov (United States)

    Berliner, Elihay; Bar Meir, Maskit; Megged, Orli

    2012-08-01

    Bacterial meningitis is a life threatening disease. Most patients will experience only one episode throughout life. Children who experience bacterial meningitis more than once, require further immunologic or anatomic evaluation. We report a 9 year old child with five episodes of bacterial meningitis due to a congenital defect of the skull base. A two and a half year old boy first presented to our medical center with pneumococcal meningitis. He was treated with antibiotics and fully recovered. Two months later he presented again with a similar clinical picture. Streptococcus pneumoniae grew in cerebrospinal fluid (CSF) culture. CT scan and later MRI of the brain revealed a defect in the anterior middle fossa floor, with protrusion of brain tissue into the sphenoidal sinus. Corrective surgery was recommended but the parents refused. Three months later, a third episode of pneumococcal meningitis occurred. The child again recovered with antibiotics and this time corrective surgery was performed. Five years later, the boy presented once again with clinical signs and symptoms consistent with bacterial meningitis. CSF culture was positive, but the final identification of the bacteria was conducted by broad spectrum 16S ribosomal RNA PCR (16S rRNA PCR) which revealed a sequence of Neisseria lactamica. CT and MRI showed recurrence of the skull base defect with encephalocele in the sphenoid sinus. The parents again refused neurosurgical intervention. A year later the patient presented with bacterial meningitis. CSF culture obtained after initiation of antibiotics was negative, but actinobacillus was identified in the CSF by 16S rRNA PCR. The patient is scheduled for neurosurgical intervention. In patients with recurrent bacterial meningitis caused by organisms colonizing the oropharynx or nasopharynx, an anatomical defect should be carefully sought and surgically repaired.

  5. Photoluminescence and electroluminescence from Ge/strained GeSn/Ge quantum wells

    Energy Technology Data Exchange (ETDEWEB)

    Lin, Chung-Yi; Chang, Chih-Chiang [Department of Electrical Engineering, Graduate Institute of Photonics and Optoelectronics, National Taiwan University, Taipei 10617, Taiwan (China); Huang, Chih-Hsiung; Huang, Shih-Hsien [Department of Electrical Engineering, Graduate Institute of Electronics Engineering, National Taiwan University, Taipei 10617, Taiwan (China); Liu, C. W., E-mail: chee@cc.ee.ntu.edu.tw [Department of Electrical Engineering, Graduate Institute of Photonics and Optoelectronics, National Taiwan University, Taipei 10617, Taiwan (China); Department of Electrical Engineering, Graduate Institute of Electronics Engineering, National Taiwan University, Taipei 10617, Taiwan (China); National Nano Device Labs, Hsinchu 30077, Taiwan (China); Huang, Yi-Chiau; Chung, Hua; Chang, Chorng-Ping [Applied Materials Inc., Sunnyvale, California 94085 (United States)

    2016-08-29

    Ge/strained GeSn/Ge quantum wells are grown on a 300 mm Si substrate by chemical vapor deposition. The direct bandgap emission from strained GeSn is observed in the photoluminescence spectra and is enhanced by Al{sub 2}O{sub 3}/SiO{sub 2} passivation due to the field effect. The electroluminescence of the direct bandgap emission of strained GeSn is also observed from the Ni/Al{sub 2}O{sub 3}/GeSn metal-insulator-semiconductor tunneling diodes. Electroluminescence is a good indicator of GeSn material quality, since defects in GeSn layers degrade the electroluminescence intensity significantly. At the accumulation bias, the holes in the Ni gate electrode tunnel to the strained n-type GeSn layer through the ultrathin Al{sub 2}O{sub 3} and recombine radiatively with electrons. The emission wavelength of photoluminescence and electroluminescence can be tuned by the Sn content.

  6. Atomistic simulation of tantalum nanoindentation: Effects of indenter diameter, penetration velocity, and interatomic potentials on defect mechanisms and evolution

    International Nuclear Information System (INIS)

    Ruestes, C.J.; Stukowski, A.; Tang, Y.; Tramontina, D.R.; Erhart, P.; Remington, B.A.; Urbassek, H.M.; Meyers, M.A.; Bringa, E.M.

    2014-01-01

    Nanoindentation simulations are a helpful complement to experiments. There is a dearth of nanoindentation simulations for bcc metals, partly due to the lack of computationally efficient and reliable interatomic potentials at large strains. We carry out indentation simulations for bcc tantalum using three different interatomic potentials and present the defect mechanisms responsible for the creation and expansion of the plastic deformation zone: twins are initially formed, giving rise to shear loop expansion and the formation of sequential prismatic loops. The calculated elastic constants as function of pressure as well as stacking fault energy surfaces explain the significant differences found in the defect structures generated for the three potentials investigated in this study. The simulations enable the quantification of total dislocation length and twinning fraction. The indenter velocity is varied and, as expected, the penetration depth for the first pop-in (defect emission) event shows a strain rate sensitivity m in the range of 0.037–0.055. The effect of indenter diameter on the first pop-in is discussed. A new intrinsic length-scale model is presented based on the profile of the residual indentation and geometrically necessary dislocation theory

  7. Atomistic simulation of tantalum nanoindentation: Effects of indenter diameter, penetration velocity, and interatomic potentials on defect mechanisms and evolution

    Energy Technology Data Exchange (ETDEWEB)

    Ruestes, C.J., E-mail: cjruestes@hotmail.com [Department of Mechanical and Aerospace Engineering, University of California, San Diego, La Jolla, CA 92093 (United States); Facultad de Ciencias Exactas y Naturales, Univ. Nac. de Cuyo, Mendoza 5500 (Argentina); CONICET, Mendoza 5500 (Argentina); Stukowski, A. [Technische Universität Darmstadt, Darmstadt 64287 (Germany); Tang, Y. [Shanghai Institute of Applied Mathematics and Mechanics, Shanghai University, Shanghai 200072 (China); Tramontina, D.R. [Facultad de Ciencias Exactas y Naturales, Univ. Nac. de Cuyo, Mendoza 5500 (Argentina); Erhart, P. [Chalmers University of Technology, Department of Applied Physics, Gothenburg 41296 (Sweden); Remington, B.A. [Lawrence Livermore National Lab, Livermore, CA 94550 (United States); Urbassek, H.M. [Physics Department and Research Center OPTIMAS, University of Kaiserslautern, Kaiserslautern 67663 (Germany); Meyers, M.A. [Department of Mechanical and Aerospace Engineering, University of California, San Diego, La Jolla, CA 92093 (United States); Bringa, E.M. [Facultad de Ciencias Exactas y Naturales, Univ. Nac. de Cuyo, Mendoza 5500 (Argentina); CONICET, Mendoza 5500 (Argentina)

    2014-09-08

    Nanoindentation simulations are a helpful complement to experiments. There is a dearth of nanoindentation simulations for bcc metals, partly due to the lack of computationally efficient and reliable interatomic potentials at large strains. We carry out indentation simulations for bcc tantalum using three different interatomic potentials and present the defect mechanisms responsible for the creation and expansion of the plastic deformation zone: twins are initially formed, giving rise to shear loop expansion and the formation of sequential prismatic loops. The calculated elastic constants as function of pressure as well as stacking fault energy surfaces explain the significant differences found in the defect structures generated for the three potentials investigated in this study. The simulations enable the quantification of total dislocation length and twinning fraction. The indenter velocity is varied and, as expected, the penetration depth for the first pop-in (defect emission) event shows a strain rate sensitivity m in the range of 0.037–0.055. The effect of indenter diameter on the first pop-in is discussed. A new intrinsic length-scale model is presented based on the profile of the residual indentation and geometrically necessary dislocation theory.

  8. Dirichlet topological defects

    International Nuclear Information System (INIS)

    Carroll, S.M.; Trodden, M.

    1998-01-01

    We propose a class of field theories featuring solitonic solutions in which topological defects can end when they intersect other defects of equal or higher dimensionality. Such configurations may be termed open-quotes Dirichlet topological defects,close quotes in analogy with the D-branes of string theory. Our discussion focuses on defects in scalar field theories with either gauge or global symmetries, in 3+1 dimensions; the types of defects considered include walls ending on walls, strings on walls, and strings on strings. copyright 1998 The American Physical Society

  9. Genome-wide comparison and taxonomic relatedness of multiple Xylella fastidiosa strains reveal the occurrence of three subspecies and a new Xylella species.

    Science.gov (United States)

    Marcelletti, Simone; Scortichini, Marco

    2016-10-01

    A total of 21 Xylella fastidiosa strains were assessed by comparing their genomes to infer their taxonomic relationships. The whole-genome-based average nucleotide identity and tetranucleotide frequency correlation coefficient analyses were performed. In addition, a consensus tree based on comparisons of 956 core gene families, and a genome-wide phylogenetic tree and a Neighbor-net network were constructed with 820,088 nucleotides (i.e., approximately 30-33 % of the entire X. fastidiosa genome). All approaches revealed the occurrence of three well-demarcated genetic clusters that represent X. fastidiosa subspecies fastidiosa, multiplex and pauca, with the latter appeared to diverge. We suggest that the proposed but never formally described subspecies 'sandyi' and 'morus' are instead members of the subspecies fastidiosa. These analyses support the view that the Xylella strain isolated from Pyrus pyrifolia in Taiwan is likely to be a new species. A widely used multilocus sequence typing analysis yielded conflicting results.

  10. MODERNIZATION OF GENEOTIPING OF STRAINS B. PERTUSSIS

    Directory of Open Access Journals (Sweden)

    G. A. Ivashinnikova

    2013-01-01

    Full Text Available The new rapid molecular genotyping method was developed for studying the structure of ptxP promoter of pertussis toxin. Method is based on PCR-RFLP analysis, which allows studying the specific restriction profiles of the B. pertussis strains and allows differentiation of the strains with the ptxP structural particularities. The developed method for genotyping of strains of B. pertussis can be hhelpful when monitoring strains of the causative agent of whooping cough in system of an epidemiological surveillance over pertussis infections, allowing observation over circulating population of B.pertussis, revealing strains of the causative agent of whooping cough with high production of pertussis toxin and to watch their distribution.

  11. Kinetics of interstitial defects in α-Fe: The effect from uniaxial stress

    Energy Technology Data Exchange (ETDEWEB)

    Kang, Changwoo [Department of Nuclear Engineering, Texas A& M University, College Station, TX 77843 (United States); Wang, Qingyu [College of Nuclear Science and Technology, Harbin Engineering University, Harbin 150001 (China); Shao, Lin, E-mail: lshao@tamu.edu [Department of Nuclear Engineering, Texas A& M University, College Station, TX 77843 (United States)

    2017-03-15

    Understanding defect kinetics in a stress field is important for multiscale modeling of materials degradation of nuclear materials. By means of molecular dynamics and molecular statics simulations, we calculate formation and migration energies of self-interstitial atoms (SIA) and SIA clusters (up to size of 5 interstitials) in alpha Fe and identify their stable configurations under uniaxial tensile strains. By applying uniaxial stress along [111], <111> oriented single SIA defects become more stable than <110> oriented SIA, which is opposite to stress-free condition. Diffusion of single SIA defects under [111] tensile stress is facilitated along [111] direction and the diffusion becomes one dimensional (1D). For SIA clusters, their diffusion under zero stress has gradual transition from three dimensional (3D) for small clusters to one dimensional (1D) for large clusters. Under the tensile stress along [111], the 3D to 1D transition is accelerated. For large SIA clusters, the stress effect is quickly saturated with less diffusivity enhancement in comparison with small SIA clusters.

  12. Osteogenic capacity of nanocrystalline bone cement in a weight-bearing defect at the ovine tibial metaphysis.

    Science.gov (United States)

    Harms, Christoph; Helms, Kai; Taschner, Tibor; Stratos, Ioannis; Ignatius, Anita; Gerber, Thomas; Lenz, Solvig; Rammelt, Stefan; Vollmar, Brigitte; Mittlmeier, Thomas

    2012-01-01

    The synthetic material Nanobone(®) (hydroxyapatite nanocrystallines embedded in a porous silica gel matrix) was examined in vivo using a standardized bone defect model in the ovine tibial metaphysis. A standardized 6 × 12 × 24-mm bone defect was created below the articular surface of the medial tibia condyles on both hind legs of 18 adult sheep. The defect on the right side was filled with Nanobone(®), while the defect on the contralateral side was left empty. The tibial heads of six sheep were analyzed after 6, 12, and 26 weeks each. The histological and radiological analysis of the defect on the control side did not reveal any bone formation after the total of 26 weeks. In contrast, the microcomputed tomography analysis of the defect filled with Nanobone(®) showed a 55%, 72%, and 74% volume fraction of structures with bone density after 6, 12, and 26 weeks, respectively. Quantitative histomorphological analysis after 6, and 12 weeks revealed an osteoneogenesis of 22%, and 36%, respectively. Hematoxylin and eosin sections demonstrated multinucleated giant cells on the surface of the biomaterial and resorption lacunae, indicating osteoclastic resorptive activity. Nanobone(®) appears to be a highly potent bone substitute material with osteoconductive properties in a loaded large animal defect model, supporting the potential use of Nanobone(®) also in humans.

  13. Tuning decoherence in superconducting transmon qubits by mechanical strain

    Energy Technology Data Exchange (ETDEWEB)

    Brehm, Jan; Bilmes, Alexander; Weiss, Georg; Ustinov, Alexey; Lisenfeld, Juergen [Karlsruher Institut fuer Technologie, Karlsruhe (Germany)

    2016-07-01

    Two-level tunneling systems (TLS) are formed by structural defects in disordered materials. They gained recent attention as an important decoherence source in superconducting qubits, where they appear on surface oxides and at film interfaces. Although the most advanced qubits do not show avoided level crossings arising from a strong coupling to individual TLS, they commonly display a pronounced frequency dependence of relaxation rates, with distinguishable peaks that may point towards weak resonant coupling to single TLS. Previously, we have shown that TLS are tunable via an applied mechanical strain. Here, we employ this method to test whether the characteristic decoherence spectrum of a transmon qubit sample responds to changes in the applied strain, as it can be expected when the decohering bath is formed of atomic TLS. In our experiment, we will employ a highly coherent X-mon qubit sample and tune the strain by bending the qubit chip via a piezo actuator. Our latest results will be presented.

  14. Studies on Drosophila radiosensitivity strains

    International Nuclear Information System (INIS)

    Varentsova, E.R.; Sharygin, V.I.; Khromykh, Yu.U.

    1985-01-01

    Fertility of radiosensitive mutant drosophila female strain rad (2) 201 61 after irradiation and frequency of dominant lethal mutations (DLM), induced by γ-radiation for 0-5 h and 5-7 days, are investigated. It is shown, that oocytes of the mutant strain are more radiosensitive as compared with cells of mongrel flies as to criterion of DLM appearance over the period of maturing. Early oocytes of stages 2-7 are the most sensitive, i.e. at the stages, corresponding to the manifestation of previously established recombination-defective properties of mutations rad (2) 201 61 . It is also sown, that doses of γ-rays, exceeding 10 Gy produce a strong sterilizing effect on mutant females due to destruction and resorption of egg chambers, irradiated at the stages of previtellogenetic growth of oocytes. In females, carrying mutation of radiosensitivity there is no direct correlation betwen sensitivity of oocytes proper to DLM induction and sensitivity of egg folleicles to resorbing effect of γ-rays. The ways of possible involvement of mutant locus studied into genetic processes in various specialized cells of drosophila

  15. Developmental defects in zebrafish for classification of EGF pathway inhibitors

    Energy Technology Data Exchange (ETDEWEB)

    Pruvot, Benoist; Curé, Yoann; Djiotsa, Joachim; Voncken, Audrey; Muller, Marc, E-mail: m.muller@ulg.ac.be

    2014-01-15

    One of the major challenges when testing drug candidates targeted at a specific pathway in whole animals is the discrimination between specific effects and unwanted, off-target effects. Here we used the zebrafish to define several developmental defects caused by impairment of Egf signaling, a major pathway of interest in tumor biology. We inactivated Egf signaling by genetically blocking Egf expression or using specific inhibitors of the Egf receptor function. We show that the combined occurrence of defects in cartilage formation, disturbance of blood flow in the trunk and a decrease of myelin basic protein expression represent good indicators for impairment of Egf signaling. Finally, we present a classification of known tyrosine kinase inhibitors according to their specificity for the Egf pathway. In conclusion, we show that developmental indicators can help to discriminate between specific effects on the target pathway from off-target effects in molecularly targeted drug screening experiments in whole animal systems. - Highlights: • We analyze the functions of Egf signaling on zebrafish development. • Genetic blocking of Egf expression causes cartilage, myelin and circulatory defects. • Chemical inhibition of Egf receptor function causes similar defects. • Developmental defects can reveal the specificity of Egf pathway inhibitors.

  16. Developmental defects in zebrafish for classification of EGF pathway inhibitors

    International Nuclear Information System (INIS)

    Pruvot, Benoist; Curé, Yoann; Djiotsa, Joachim; Voncken, Audrey; Muller, Marc

    2014-01-01

    One of the major challenges when testing drug candidates targeted at a specific pathway in whole animals is the discrimination between specific effects and unwanted, off-target effects. Here we used the zebrafish to define several developmental defects caused by impairment of Egf signaling, a major pathway of interest in tumor biology. We inactivated Egf signaling by genetically blocking Egf expression or using specific inhibitors of the Egf receptor function. We show that the combined occurrence of defects in cartilage formation, disturbance of blood flow in the trunk and a decrease of myelin basic protein expression represent good indicators for impairment of Egf signaling. Finally, we present a classification of known tyrosine kinase inhibitors according to their specificity for the Egf pathway. In conclusion, we show that developmental indicators can help to discriminate between specific effects on the target pathway from off-target effects in molecularly targeted drug screening experiments in whole animal systems. - Highlights: • We analyze the functions of Egf signaling on zebrafish development. • Genetic blocking of Egf expression causes cartilage, myelin and circulatory defects. • Chemical inhibition of Egf receptor function causes similar defects. • Developmental defects can reveal the specificity of Egf pathway inhibitors

  17. Resistance of Permafrost and Modern Acinetobacter lwoffii Strains to Heavy Metals and Arsenic Revealed by Genome Analysis.

    Science.gov (United States)

    Mindlin, Sofia; Petrenko, Anatolii; Kurakov, Anton; Beletsky, Alexey; Mardanov, Andrey; Petrova, Mayya

    2016-01-01

    We performed whole-genome sequencing of five permafrost strains of Acinetobacter lwoffii (frozen for 15-3000 thousand years) and analyzed their resistance genes found in plasmids and chromosomes. Four strains contained multiple plasmids (8-12), which varied significantly in size (from 4,135 to 287,630 bp) and genetic structure; the fifth strain contained only two plasmids. All large plasmids and some medium-size and small plasmids contained genes encoding resistance to various heavy metals, including mercury, cobalt, zinc, cadmium, copper, chromium, and arsenic compounds. Most resistance genes found in the ancient strains of A . lwoffii had their closely related counterparts in modern clinical A . lwoffii strains that were also located on plasmids. The vast majority of the chromosomal resistance determinants did not possess complete sets of the resistance genes or contained truncated genes. Comparative analysis of various A . lwoffii and of A . baumannii strains discovered a number of differences between them: (i) chromosome sizes in A . baumannii exceeded those in A . lwoffii by about 20%; (ii) on the contrary, the number of plasmids in A . lwoffii and their total size were much higher than those in A . baumannii ; (iii) heavy metal resistance genes in the environmental A . lwoffii strains surpassed those in A . baumannii strains in the number and diversity and were predominantly located on plasmids. Possible reasons for these differences are discussed.

  18. A comparative study on defect estimation using XPS and Raman spectroscopy in few layer nanographitic structures.

    Science.gov (United States)

    Ganesan, K; Ghosh, Subrata; Gopala Krishna, Nanda; Ilango, S; Kamruddin, M; Tyagi, A K

    2016-08-10

    Defects in planar and vertically oriented nanographitic structures (NGSs) synthesized by plasma enhanced chemical vapor deposition (PECVD) have been investigated using Raman and X-ray photoelectron spectroscopy. While Raman spectra reveal the dominance of vacancy and boundary type defects respectively in vertical and planar NGSs, XPS provides additional information on vacancy related defect peaks in the C 1s spectrum, which originate from non-conjugated carbon atoms in the hexagonal lattice. Although an excellent correlation prevails between these two techniques, our results show that estimation of surface defects by XPS is more accurate than Raman analysis. Nuances of these techniques are discussed in the context of assessing defects in nanographitic structures.

  19. Experimental studies of free defect generation during irradiation: Implications for reactor environments

    International Nuclear Information System (INIS)

    Rehn, L.E.; Birtcher, R.C.

    1993-01-01

    Over the past several years, systematic experiments have revealed that irradiations which generate energetically dense cascades are much less effective than light-ion, MeV electron, or thermal neutron irradiations at producing freely-migrating defects. In this paper, the systematic results on freely-migrating defect production from ion irradiation studies are briefly summarized. Difficulties with applying a simple extrapolation of the ion-irradiation results to neutron environments are discussed. This discussion, coupled with our existing knowledge of neutron-induced property changes, indicates that Compton scattering, and the (n,γ), (n,He) and (n,p) nuclear reactions, are considerably more important for producing freely-migrating defects than was previously realized

  20. Dangling-bond defect in a-Si:H : Characterization of network and strain effects by first-principles calculation of the EPR parameters

    NARCIS (Netherlands)

    Pfanner, G.; Freysoldt, C.; Neugebauer, J.; Inam, F.; Drabold, D.; Jarolimek, K.; Zeman, M.

    2013-01-01

    The performance of hydrogenated amorphous silicon (a-Si:H) solar cells is severely affected by the light-induced formation of metastable defects in the material (Staebler-Wronski effect). The common notion is that the dangling-bond (db) defect, a threefold coordinated silicon atom, plays a key role

  1. Instrumented hydrostatic testing of pipeline tracts with lamination defects; Ensayos de prueba hidrostatica de oleoductos con defectos de laminacion

    Energy Technology Data Exchange (ETDEWEB)

    Fazzini, Pablo Gabriel [Universidad Nacional de Mar del Plata (Argentina); [Consejo de Investigaciones Cientificas de la Provincia de Buenos Aires (CIC) (Argentina). Instituto de Investigaciones en Ciencia y Tecnologia de Materiales (INTEMA)]. E-mail: pgf@fi.mdp.edu.ar; Otegui, Jose Luis [Universidad Nacional de Mar del Plata (Argentina). Instituto de Investigaciones en Ciencia y Tecnologia de Materiales (INTEMA) (Argentina). CONICET; Motylicki, J [OLDELVAL S.A. (Argentina)

    2003-07-01

    Experimental results from seven hydrostatic tests on ex-service tubes from a 14'' diameter, 6.3 mm thickness ERW (electrical resistance seam welded) oil pipeline are presented. Lamination defects had been detected in these tracts by means of TFI in line inspection and the ultrasonic technique FAST. Of these tests, four were strain gauge instrumented. Five tubes failed in the ERW, burst pressures of defects in base material were larger. The fracture mechanics model of the most representative defect concludes that a lamination defect with an inclination of up to 3 mm in the radial direction, is not critical, test results show that this prediction is conservative. The largest laminations found in base material reduced burst pressure by less than 25%. On the contrary, defects that propagated in the ERW reduced burst resistance up to almost 50 %. These results show that the location of the defects is more important than size, the most important reason being the low toughness of the ERW. The results of this study confirm the validity of the restrictions that imposes section 8 of API 579. (author)

  2. Instrumented hydrostatic testing of pipeline tracts with lamination defects; Ensayos de prueba hidrostatica de oleoductos con defectos de laminacion

    Energy Technology Data Exchange (ETDEWEB)

    Fazzini, Pablo Gabriel [Universidad Nacional de Mar del Plata (Argentina)]|[Consejo de Investigaciones Cientificas de la Provincia de Buenos Aires (CIC) (Argentina). Instituto de Investigaciones en Ciencia y Tecnologia de Materiales (INTEMA)]. E-mail: pgf@fi.mdp.edu.ar; Otegui, Jose Luis [Universidad Nacional de Mar del Plata (Argentina). Instituto de Investigaciones en Ciencia y Tecnologia de Materiales (INTEMA) (Argentina). CONICET]. E-mail: jotegui@fi.mdp.edu.ar; Motylicki, J. [OLDELVAL S.A. (Argentina)]. E-mail: jmotylic@oldelval.com.ar

    2003-07-01

    Experimental results from seven hydrostatic tests on ex-service tubes from a 14'' diameter, 6.3 mm thickness ERW (electrical resistance seam welded) oil pipeline are presented. Lamination defects had been detected in these tracts by means of TFI in line inspection and the ultrasonic technique FAST. Of these tests, four were strain gauge instrumented. Five tubes failed in the ERW, burst pressures of defects in base material were larger. The fracture mechanics model of the most representative defect concludes that a lamination defect with an inclination of up to 3 mm in the radial direction, is not critical, test results show that this prediction is conservative. The largest laminations found in base material reduced burst pressure by less than 25%. On the contrary, defects that propagated in the ERW reduced burst resistance up to almost 50 %. These results show that the location of the defects is more important than size, the most important reason being the low toughness of the ERW. The results of this study confirm the validity of the restrictions that imposes section 8 of API 579. (author)

  3. Molecular characterization of the probiotic strain Bacillus cereus var. toyoi NCIMB 40112 and differentiation from food poisoning strains.

    Science.gov (United States)

    Klein, Günter

    2011-07-01

    Bacillus cereus var. toyoi strain NCIMB 40112 (Toyocerin), a probiotic authorized in the European Union as feed additive for swine, bovines, poultry, and rabbits, was characterized by DNA fingerprinting applying pulsed-field gel electrophoresis and multilocus sequence typing and was compared with reference strains (of clinical and environmental origins). The probiotic strain was clearly characterized by pulsed-field gel electrophoresis using the restriction enzymes Apa I and Sma I resulting in unique DNA patterns. The comparison to the clinical reference strain B. cereus DSM 4312 was done with the same restriction enzymes, and again a clear differentiation of the two strains was possible by the resulting DNA patterns. The use of the restriction enzymes Apa I and Sma I is recommended for further studies. Furthermore, multilocus sequence typing analysis revealed a sequence type (ST 111) that was different from all known STs of B. cereus strains from food poisoning incidents. Thus, a strain characterization and differentiation from food poisoning strains for the probiotic strain was possible. Copyright ©, International Association for Food Protection

  4. Transformation between divacancy defects induced by an energy pulse in graphene.

    Science.gov (United States)

    Xia, Jun; Liu, XiaoYi; Zhou, Wei; Wang, FengChao; Wu, HengAn

    2016-07-08

    The mutual transformations among the four typical divacancy defects induced by a high-energy pulse were studied via molecular dynamics simulation. Our study revealed all six possible mutual transformations and found that defects transformed by absorbing energy to overcome the energy barrier with bonding, debonding, and bond rotations. The reversibility of defect transformations was also investigated by potential energy analysis. The energy difference was found to greatly influence the transformation reversibility. The direct transformation path was irreversible if the energy difference was too large. We also studied the correlation between the transformation probability and the input energy. It was found that the transformation probability had a local maxima at an optimal input energy. The introduction of defects and their structural evolutions are important for tailoring the exceptional properties and thereby performances of graphene-based devices, such as nanoporous membranes for the filtration and desalination of water.

  5. Minimization of Defective Products in The Department of Press Bridge & Rib Through Six Sigma DMAIC Phases

    Science.gov (United States)

    Rochman, YA; Agustin, A.

    2017-06-01

    This study proposes the DMAIC Six Sigma approach of Define, Measure, Analyze, Improve/Implement and Control (DMAIC) to minimizing the number of defective products in the bridge & rib department. There are 5 types of defects were the most dominant are broken rib, broken sound board, strained rib, rib sliding and sound board minori. The imperative objective is to improve the quality through the DMAIC phases. In the define phase, the critical to quality (CTQ) parameters was identified minimization of product defects through the pareto chart and FMEA. In this phase, to identify waste based on the current value stream mapping. In the measure phase, the specified control limits product used to maintain the variations of the product, the calculation of the value of DPMO (Defect Per Million Opportunities) and the calculation of the value of sigma level. In analyze phase, determine the type of defect of the most dominant and identify the causes of defective products. In the improve phase, the existing design was modified through various alternative solutions by conducting brainstorming sessions. In this phase, the solution was identified based on the results of FMEA. Improvements were made to the seven priority causes of disability based on the highest RPN value. In the control phase, focusing on improvements to be made. Proposed improvements include making and define standard operating procedures, improving the quality and eliminate waste defective products.

  6. Structure and flux pinning properties of irradiation defects in YBa2Cu3O7-x

    International Nuclear Information System (INIS)

    Kirk, M.A.

    1992-06-01

    We review our investigations of defects produced in YBa 2 Cu 3 O 7-x by various forms of irradiation. The defect microstructure has been studied by transmission electron microscopy (TEM). Irradiation enhancements of flux pinning have been studied by SQUID magnetometry on single crystals. In many cases the same single crystals were used in both TEM and SQUID investigations. The primary atom recoil spectra for all the irradiations studied have been carefully calculated and used to correlate the TEM and magnetization results for the different types of irradiation. Correlation of annealing experiments, employing both TEM and SQUID measurements, among several types of irradiation has also yielded information on the different defect structures present. Defect densities, sizes and strain field anisotropies have been determined by TEM. Defect flux pinning anisotropies have been determined for two field orientations in twinned single crystals. The temperature dependences of the flux pinning have been measured. The maximum field of irreversibility at 70 K is shown to change markedly upon both neutron and proton irradiations in some crystals and not others. The defect structure, chemistry and location in the unit cell has been determined in some cases. Some interaction with existing defect structure has been observed in proton and electron irradiations. The damage character and directionality has been determined in GeV ion irradiated crystals

  7. Defect forces, defect couples and path integrals in fracture mechanics

    International Nuclear Information System (INIS)

    Roche, R.L.

    1979-07-01

    In this work, it is shown that the path integrals can be introduced without any reference to the material behavior. The method is based on the definition in a continuous medium of a set of vectors and couples having the dimension of a force or a moment. More precisely, definitions are given of volume defect forces, surface defect forces, volume defect couples, and surface defect couples. This is done with the help of the stress working variation of a particule moving through the solid. The most important result is: the resultant of all the defect forces included in a volume V is the J integral on the surface surrounding V and the moment resultant is the L integral. So these integrals are defined without any assumption on the material constitutive equation. Another result is the material form of the virtual work principle - defect forces are acting like conventional forces in the conventional principles of virtual work. This lead to the introduction of the energy momentum tensor and of the associated couple stress. Application of this method is made to fracture mechanics in studying the defect forces distribution around a crack [fr

  8. AC loss characteristics of Bi2223/Ag sheathed tape wires subjected to mechanical strains and stresses

    International Nuclear Information System (INIS)

    Tsukamoto, Osami; Li, Z

    2007-01-01

    losses on the stress-strain are negligibly small when the losses are properly normalized by the stress-strain-dependent critical currents. In the serrated-like plastic region, the AC loss characteristics are different from those in the elastic and continuous plastic regions and can be characterized by defects grown almost tape wide, causing serious degradation of the critical currents. There are various origins of defects causing the degradations of the wire critical currents. However, as a result of this investigation, the influence of the tensile stress-strain on the AC losses can be basically estimated by knowing the degrees of the degradations of the wire critical currents caused by the stress-strain and in which regions the stress-strain characteristics are, regardless of the origins of the defects

  9. Tuning magnetism by biaxial strain in native ZnO.

    Science.gov (United States)

    Peng, Chengxiao; Wang, Yuanxu; Cheng, Zhenxiang; Zhang, Guangbiao; Wang, Chao; Yang, Gui

    2015-07-07

    Magnetic ZnO, one of the most important diluted magnetic semiconductors (DMS), has attracted great scientific interest because of its possible technological applications in optomagnetic devices. Magnetism in this material is usually delicately tuned by the doping level, dislocations, and local structures. The rational control of magnetism in ZnO is a highly attractive approach for practical applications. Here, the tuning effect of biaxial strain on the d(0) magnetism of native imperfect ZnO is demonstrated through first-principles calculations. Our calculation results show that strain conditions have little effect on the defect formation energy of Zn and O vacancies in ZnO, but they do affect the magnetism significantly. For a cation vacancy, increasing the compressive strain will obviously decrease its magnetic moment, while tensile strain cannot change the moment, which remains constant at 2 μB. For a singly charged anion vacancy, however, the dependence of the magnetic moment on strain is opposite to that of the Zn vacancy. Furthermore, the ferromagnetic state is always present, irrespective of the strain type, for ZnO with two zinc vacancies, 2VZns. A large tensile strain is favorable for improving the Curie temperature and realizing room temperature ferromagnetism for ZnO-based native semiconductors. For ZnO with two singly charged oxygen vacancies, 2Vs, no ferromagnetic ordering can be observed. Our work points the way to the rational design of materials beyond ZnO with novel non-intrinsic functionality by simply tuning the strain in a thin film form.

  10. Strain measurements at the HDR-pipe-system under LOCA-load: Effects on elbows and displaced weldings

    International Nuclear Information System (INIS)

    Hunger, H.

    1985-01-01

    This paper characterizes some effects which have been detected during strain gauge measurements on a test piping with feed water check valve oscillating under blowdown-load. The ovalization of a pipe elbow subjected to in-plane-bending affects the connected straight pipe; this is shown by means of circumferential stresses. Very high LOCA-load produces plastic strain and changes the pipe dynamics. Artificial displaced welds increase the local strain but no defects have occurred. One example compares stresses from measurement and post-calculation. Moreover there are given some remarks on the optimization of the comparison of measurement and calculation. (orig.)

  11. Neural Tube Defects

    Science.gov (United States)

    Neural tube defects are birth defects of the brain, spine, or spinal cord. They happen in the ... that she is pregnant. The two most common neural tube defects are spina bifida and anencephaly. In ...

  12. Molecular dynamics simulation of defect formation during energetic Cu deposition

    International Nuclear Information System (INIS)

    Gilmore, Charles M.; Sprague, James A.

    2002-01-01

    The deposition of energetic Cu atoms from 5 to 80 eV onto (0 0 1) Cu was simulated with molecular dynamics. The Cu-Cu interaction potential was a spline of the embedded atom potential developed from equilibrium data, and the universal scattering potential. Incident Cu atoms substituted for first layer substrate atoms by an exchange process at energies as low as 5 eV. Incident Cu atoms of 20 eV penetrated to the second substrate layer, and 20 eV was sufficient energy to produce interstitial defects. Incident atoms of 80 eV penetrated to the third atomic layer, produced interstitials 12 atomic layers into the substrate by focused replacement collision sequences, and produced sputtered atoms with a 16% yield. Interstitial clusters of up to 7 atoms were observed. The observed mechanisms of film growth included: the direct deposition of atoms into film equilibrium atom positions, the exchange of substrate atoms to equilibrium film atoms positions, and the migration of interstitials to equilibrium film atom positions. The relative frequency of each process was a function of incident energy. Since all observed growth mechanisms resulted in film atoms in equilibrium atomic positions, these simulations suggest that stresses in homoepitaxial Cu thin films are due to point defects. Vacancies would produce tensile strain and interstitial atoms would produce compressive strain in the films. It is proposed that immobile interstitial clusters could be responsible for retaining interstitial atoms and clusters in growing metal thin films

  13. Strain field mapping of dislocations in a Ge/Si heterostructure.

    Directory of Open Access Journals (Sweden)

    Quanlong Liu

    Full Text Available Ge/Si heterostructure with fully strain-relaxed Ge film was grown on a Si (001 substrate by using a two-step process by ultra-high vacuum chemical vapor deposition. The dislocations in the Ge/Si heterostructure were experimentally investigated by high-resolution transmission electron microscopy (HRTEM. The dislocations at the Ge/Si interface were identified to be 90° full-edge dislocations, which are the most efficient way for obtaining a fully relaxed Ge film. The only defect found in the Ge epitaxial film was a 60° dislocation. The nanoscale strain field of the dislocations was mapped by geometric phase analysis technique from the HRTEM image. The strain field around the edge component of the 60° dislocation core was compared with those of the Peierls-Nabarro and Foreman dislocation models. Comparison results show that the Foreman model with a = 1.5 can describe appropriately the strain field around the edge component of a 60° dislocation core in a relaxed Ge film on a Si substrate.

  14. Strain field mapping of dislocations in a Ge/Si heterostructure.

    Science.gov (United States)

    Liu, Quanlong; Zhao, Chunwang; Su, Shaojian; Li, Jijun; Xing, Yongming; Cheng, Buwen

    2013-01-01

    Ge/Si heterostructure with fully strain-relaxed Ge film was grown on a Si (001) substrate by using a two-step process by ultra-high vacuum chemical vapor deposition. The dislocations in the Ge/Si heterostructure were experimentally investigated by high-resolution transmission electron microscopy (HRTEM). The dislocations at the Ge/Si interface were identified to be 90° full-edge dislocations, which are the most efficient way for obtaining a fully relaxed Ge film. The only defect found in the Ge epitaxial film was a 60° dislocation. The nanoscale strain field of the dislocations was mapped by geometric phase analysis technique from the HRTEM image. The strain field around the edge component of the 60° dislocation core was compared with those of the Peierls-Nabarro and Foreman dislocation models. Comparison results show that the Foreman model with a = 1.5 can describe appropriately the strain field around the edge component of a 60° dislocation core in a relaxed Ge film on a Si substrate.

  15. Genome-Wide Transcription Study of Cryptococcus neoformans H99 Clinical Strain versus Environmental Strains.

    Directory of Open Access Journals (Sweden)

    Elaheh Movahed

    Full Text Available The infection of Cryptococcus neoformans is acquired through the inhalation of desiccated yeast cells and basidiospores originated from the environment, particularly from bird's droppings and decaying wood. Three environmental strains of C. neoformans originated from bird droppings (H4, S48B and S68B and C. neoformans reference clinical strain (H99 were used for intranasal infection in C57BL/6 mice. We showed that the H99 strain demonstrated higher virulence compared to H4, S48B and S68B strains. To examine if gene expression contributed to the different degree of virulence among these strains, a genome-wide microarray study was performed to inspect the transcriptomic profiles of all four strains. Our results revealed that out of 7,419 genes (22,257 probes examined, 65 genes were significantly up-or down-regulated in H99 versus H4, S48B and S68B strains. The up-regulated genes in H99 strain include Hydroxymethylglutaryl-CoA synthase (MVA1, Mitochondrial matrix factor 1 (MMF1, Bud-site-selection protein 8 (BUD8, High affinity glucose transporter 3 (SNF3 and Rho GTPase-activating protein 2 (RGA2. Pathway annotation using DAVID bioinformatics resource showed that metal ion binding and sugar transmembrane transporter activity pathways were highly expressed in the H99 strain. We suggest that the genes and pathways identified may possibly play crucial roles in the fungal pathogenesis.

  16. Defects detection and non-destructive testing (NDT) techniques in paintings: a unified approach through measurements of deformation

    Science.gov (United States)

    Sfarra, S.; Ibarra-Castanedo, C.; Ambrosini, D.; Paoletti, D.; Bendada, A.; Maldague, X.

    2013-05-01

    The present study is focused on two topics. The first one is a mathematical model, useful to understand the deformation of paintings, which uses straining devices, adjustable and micrometrically controlled via a pin supported in a hollow cylinder. Strains were analyzed by holographic interferometry (HI) technique using an appropriate frame. The second one concerns the need to improve the conservator's knowledge about the defect's detection and defect's propagation in acrylic painting characterized of underdrawings and pentimenti. To fulfill this task, a sample was manufactured to clarify the several uncertainties inherent the influence of external factors on their conservation. Subsurface anomalies were also retrieved by near-infrared reflectography (NIRR) and transmittography (NIRT) techniques, using LED lamps and several narrow-band filters mounted on a CMOS camera, working at different wavelengths each other and in combination with UV imaging. In addition, a sponge glued on the rear side of the canvas was impregnated with a precise amount of water by means of a syringe to verify the "stretcher effect" by the digital speckle photography (DSP) technique (using MatPIV). The same effect also affects the sharp transition of the canvas at the stretcher's edge. In this case, a possible mechanism is a direct mechanical contact between stretcher and canvas that was investigated by HI technique. Finally, advanced algorithms applied to the square heating thermography (SHT) data were very useful to detect three Mylar® inserts simulating different type of defects. These fabricated defects were also identified by optical techniques, while the visual inspection was the only one capable of detecting a biological damage.

  17. Genome sequencing and analysis of BCG vaccine strains.

    Directory of Open Access Journals (Sweden)

    Wen Zhang

    Full Text Available BACKGROUND: Although the Bacillus Calmette-Guérin (BCG vaccine against tuberculosis (TB has been available for more than 75 years, one third of the world's population is still infected with Mycobacterium tuberculosis and approximately 2 million people die of TB every year. To reduce this immense TB burden, a clearer understanding of the functional genes underlying the action of BCG and the development of new vaccines are urgently needed. METHODS AND FINDINGS: Comparative genomic analysis of 19 M. tuberculosis complex strains showed that BCG strains underwent repeated human manipulation, had higher region of deletion rates than those of natural M. tuberculosis strains, and lost several essential components such as T-cell epitopes. A total of 188 BCG strain T-cell epitopes were lost to various degrees. The non-virulent BCG Tokyo strain, which has the largest number of T-cell epitopes (359, lost 124. Here we propose that BCG strain protection variability results from different epitopes. This study is the first to present BCG as a model organism for genetics research. BCG strains have a very well-documented history and now detailed genome information. Genome comparison revealed the selection process of BCG strains under human manipulation (1908-1966. CONCLUSIONS: Our results revealed the cause of BCG vaccine strain protection variability at the genome level and supported the hypothesis that the restoration of lost BCG Tokyo epitopes is a useful future vaccine development strategy. Furthermore, these detailed BCG vaccine genome investigation results will be useful in microbial genetics, microbial engineering and other research fields.

  18. Enhanced radiosensitivity and defective DNA repair in cultured fibroblasts derived from Rothmund Thomson syndrome patients

    Energy Technology Data Exchange (ETDEWEB)

    Smith, P J; Paterson, M C [Atomic Energy of Canada Ltd., Chalk River, Ontario. Radiation Biology Branch

    1982-01-01

    Rothmund Thomson syndrome (RTS) is an oculocutaneous and cancer-prone disorder in which enhanced carcinogen sensitivity, mediated through abnormal DNA metabolism, may be an associated factor. Cultured fibroblasts from 4 RTS patients have been examined for their colony-forming abilities and DNA repair capacities following ..gamma..-irradiation. 2 of the 4 RTS strains showed enhanced sensitivity following hypoxic ..gamma..-irradiation, and 1 of these 2 strains also showed enhanced sensitivity under oxic conditions. Defective DNA repair was implicated in the above abnormal responses to ..gamma..-radiation since both strains displayed reduced levels of repair synthesis and slow removal of radiogenic DNA lesions (assayed by their sensitivity to strand-incising activities present in protein extracts of Micrococcus luteus cells). A hypothesis is presented to rationalize the origin and heterogeneity of these laboratory phenotypes of RTS.

  19. Solitary waves in morphogenesis: Determination fronts as strain-cued strain transformations among automatous cells

    Science.gov (United States)

    Cox, Brian N.; Landis, Chad M.

    2018-02-01

    We present a simple theory of a strain pulse propagating as a solitary wave through a continuous two-dimensional population of cells. A critical strain is assumed to trigger a strain transformation, while, simultaneously, cells move as automata to tend to restore a preferred cell density. We consider systems in which the strain transformation is a shape change, a burst of proliferation, or the commencement of growth (which changes the shape of the population sheet), and demonstrate isomorphism among these cases. Numerical and analytical solutions describe a strain pulse whose height does not depend on how the strain disturbance was first launched, or the rate at which the strain transformation is achieved, or the rate constant in the rule for the restorative cell motion. The strain pulse is therefore very stable, surviving the imposition of strong perturbations: it would serve well as a timing signal in development. The automatous wave formulation is simple, with few model parameters. A strong case exists for the presence of a strain pulse during amelogenesis. Quantitative analysis reveals a simple relationship between the velocity of the leading edge of the pulse in amelogenesis and the known speed of migration of ameloblast cells. This result and energy arguments support the depiction of wave motion as an automatous cell response to strain, rather than as a response to an elastic energy gradient. The theory may also contribute to understanding the determination front in somitogenesis, moving fronts of convergent-extension transformation, and mitotic wavefronts in the syncytial drosophila embryo.

  20. Genome analysis coupled with physiological studies reveals a diverse nitrogen metabolism in Methylocystis sp. strain SC2.

    Directory of Open Access Journals (Sweden)

    Bomba Dam

    Full Text Available BACKGROUND: Methylocystis sp. strain SC2 can adapt to a wide range of methane concentrations. This is due to the presence of two isozymes of particulate methane monooxygenase exhibiting different methane oxidation kinetics. To gain insight into the underlying genetic information, its genome was sequenced and found to comprise a 3.77 Mb chromosome and two large plasmids. PRINCIPAL FINDINGS: We report important features of the strain SC2 genome. Its sequence is compared with those of seven other methanotroph genomes, comprising members of the Alphaproteobacteria, Gammaproteobacteria, and Verrucomicrobia. While the pan-genome of all eight methanotroph genomes totals 19,358 CDS, only 154 CDS are shared. The number of core genes increased with phylogenetic relatedness: 328 CDS for proteobacterial methanotrophs and 1,853 CDS for the three alphaproteobacterial Methylocystaceae members, Methylocystis sp. strain SC2 and strain Rockwell, and Methylosinus trichosporium OB3b. The comparative study was coupled with physiological experiments to verify that strain SC2 has diverse nitrogen metabolism capabilities. In correspondence to a full complement of 34 genes involved in N2 fixation, strain SC2 was found to grow with atmospheric N2 as the sole nitrogen source, preferably at low oxygen concentrations. Denitrification-mediated accumulation of 0.7 nmol (30N2/hr/mg dry weight of cells under anoxic conditions was detected by tracer analysis. N2 production is related to the activities of plasmid-borne nitric oxide and nitrous oxide reductases. CONCLUSIONS/PERSPECTIVES: Presence of a complete denitrification pathway in strain SC2, including the plasmid-encoded nosRZDFYX operon, is unique among known methanotrophs. However, the exact ecophysiological role of this pathway still needs to be elucidated. Detoxification of toxic nitrogen compounds and energy conservation under oxygen-limiting conditions are among the possible roles. Relevant features that may stimulate

  1. Strain distributions and their influence on electronic structures of WSe2-MoS2 laterally strained heterojunctions

    Science.gov (United States)

    Zhang, Chendong; Li, Ming-Yang; Tersoff, Jerry; Han, Yimo; Su, Yushan; Li, Lain-Jong; Muller, David A.; Shih, Chih-Kang

    2018-02-01

    Monolayer transition metal dichalcogenide heterojunctions, including vertical and lateral p-n junctions, have attracted considerable attention due to their potential applications in electronics and optoelectronics. Lattice-misfit strain in atomically abrupt lateral heterojunctions, such as WSe2-MoS2, offers a new band-engineering strategy for tailoring their electronic properties. However, this approach requires an understanding of the strain distribution and its effect on band alignment. Here, we study a WSe2-MoS2 lateral heterojunction using scanning tunnelling microscopy and image its moiré pattern to map the full two-dimensional strain tensor with high spatial resolution. Using scanning tunnelling spectroscopy, we measure both the strain and the band alignment of the WSe2-MoS2 lateral heterojunction. We find that the misfit strain induces type II to type I band alignment transformation. Scanning transmission electron microscopy reveals the dislocations at the interface that partially relieve the strain. Finally, we observe a distinctive electronic structure at the interface due to hetero-bonding.

  2. Finite element approximation of the fields of bulk and interfacial line defects

    Science.gov (United States)

    Zhang, Chiqun; Acharya, Amit; Puri, Saurabh

    2018-05-01

    A generalized disclination (g.disclination) theory (Acharya and Fressengeas, 2015) has been recently introduced that goes beyond treating standard translational and rotational Volterra defects in a continuously distributed defects approach; it is capable of treating the kinematics and dynamics of terminating lines of elastic strain and rotation discontinuities. In this work, a numerical method is developed to solve for the stress and distortion fields of g.disclination systems. Problems of small and finite deformation theory are considered. The fields of a single disclination, a single dislocation treated as a disclination dipole, a tilt grain boundary, a misfitting grain boundary with disconnections, a through twin boundary, a terminating twin boundary, a through grain boundary, a star disclination/penta-twin, a disclination loop (with twist and wedge segments), and a plate, a lenticular, and a needle inclusion are approximated. It is demonstrated that while the far-field topological identity of a dislocation of appropriate strength and a disclination-dipole plus a slip dislocation comprising a disconnection are the same, the latter microstructure is energetically favorable. This underscores the complementary importance of all of topology, geometry, and energetics in understanding defect mechanics. It is established that finite element approximations of fields of interfacial and bulk line defects can be achieved in a systematic and routine manner, thus contributing to the study of intricate defect microstructures in the scientific understanding and predictive design of materials. Our work also represents one systematic way of studying the interaction of (g.)disclinations and dislocations as topological defects, a subject of considerable subtlety and conceptual importance (Aharoni et al., 2017; Mermin, 1979).

  3. Weld defect identification in friction stir welding using power spectral density

    Science.gov (United States)

    Das, Bipul; Pal, Sukhomay; Bag, Swarup

    2018-04-01

    Power spectral density estimates are powerful in extraction of useful information retained in signal. In the current research work classical periodogram and Welch periodogram algorithms are used for the estimation of power spectral density for vertical force signal and transverse force signal acquired during friction stir welding process. The estimated spectral densities reveal notable insight in identification of defects in friction stir welded samples. It was observed that higher spectral density against each process signals is a key indication in identifying the presence of possible internal defects in the welded samples. The developed methodology can offer preliminary information regarding presence of internal defects in friction stir welded samples can be best accepted as first level of safeguard in monitoring the friction stir welding process.

  4. Influence of strain on dislocation core in silicon

    Science.gov (United States)

    Pizzagalli, L.; Godet, J.; Brochard, S.

    2018-05-01

    First principles, density functional-based tight binding and semi-empirical interatomic potentials calculations are performed to analyse the influence of large strains on the structure and stability of a 60? dislocation in silicon. Such strains typically arise during the mechanical testing of nanostructures like nanopillars or nanoparticles. We focus on bi-axial strains in the plane normal to the dislocation line. Our calculations surprisingly reveal that the dislocation core structure largely depends on the applied strain, for strain levels of about 5%. In the particular case of bi-axial compression, the transformation of the dislocation to a locally disordered configuration occurs for similar strain magnitudes. The formation of an opening, however, requires larger strains, of about 7.5%. Furthermore, our results suggest that electronic structure methods should be favoured to model dislocation cores in case of large strains whenever possible.

  5. Effects of strain and age on hepatic gene expression profiles in murine models of HFE-associated hereditary hemochromatosis.

    Science.gov (United States)

    Lee, Seung-Min; Loguinov, Alexandre; Fleming, Robert E; Vulpe, Christopher D

    2015-01-01

    Hereditary hemochromatosis is an iron overload disorder most commonly caused by a defect in the HFE gene. While the genetic defect is highly prevalent, the majority of individuals do not develop clinically significant iron overload, suggesting the importance of genetic modifiers. Murine hfe knockout models have demonstrated that strain background has a strong effect on the severity of iron loading. We noted that hepatic iron loading in hfe-/- mice occurs primarily over the first postnatal weeks (loading phase) followed by a timeframe of relatively static iron concentrations (plateau phase). We thus evaluated the effects of background strain and of age on hepatic gene expression in Hfe knockout mice (hfe-/-). Hepatic gene expression profiles were examined using cDNA microarrays in 4- and 8-week-old hfe-/- and wild-type mice on two different genetic backgrounds, C57BL/6J (C57) and AKR/J (AKR). Genes differentially regulated in all hfe-/- mice groups, compared with wild-type mice, including those involved in cell survival, stress and damage responses and lipid metabolism. AKR strain-specific changes in lipid metabolism genes and C57 strain-specific changes in cell adhesion and extracellular matrix protein genes were detected in hfe-/- mice. Mouse strain and age are each significantly associated with hepatic gene expression profiles in hfe-/- mice. These affects may underlie or reflect differences in iron loading in these mice.

  6. Extended defect related energy loss in CVD diamond revealed by spectrum imaging in a dedicated STEM

    International Nuclear Information System (INIS)

    Bangert, U.; Harvey, A.J.; Schreck, M.; Hoermann, F.

    2005-01-01

    This article aims at investigations of the low EEL region in the wide band gap system diamond. The advent of the UHV Enfina electron energy loss spectrometer combined with Digital Micrograph acquisition and processing software has made reliable detection of absorption losses below 10 eV possible. Incorporated into a dedicated STEM this instrumentation allows the acquisition of spectral information via spectrum maps (spectrum imaging) of sample areas hundreds of nanometers across, with nanometers pixel sizes, adequate spectrum statistics and 0.3 eV energy resolution, in direct correlation with microstructural features in the mapping area. We aim at discerning defect related losses at band gap energies, and discuss different routes to simultaneously process and analyse the spectra in a map. This involves extracting the zero loss peak from each spectrum and constructing ratio maps from the intensities in two energy windows, one defect related and one at a higher, crystal bandstructure dominated energy. This was applied to the residual spectrum maps and their first derivatives. Secondly, guided by theoretical EEL spectra calculations, the low loss spectra were fitted by a series of gaussian distributions. Pixel maps were constructed from amplitude ratios of gaussians, situated in the defect and the unaffected energy regime. The results demonstrate the existence of sp 2 -bonded carbon in the vicinity of stacking faults and partial dislocations in CVD diamond as well as additional states below conduction band, tailing deep into the band gap, at a node in a perfect dislocation. Calculated EEL spectra of shuffle dislocations give similar absorption features at 5-8 eV, and it is thought that this common feature is due to sp 2 -type bonding

  7. Differential stress transcriptome landscape of historic and recently emerged hypervirulent strains of Clostridium difficile strains determined using RNA-seq.

    Directory of Open Access Journals (Sweden)

    Joy Scaria

    Full Text Available C. difficile is the most common cause of nosocomial diarrhea in North America and Europe. Genomes of individual strains of C. difficile are highly divergent. To determine how divergent strains respond to environmental changes, the transcriptomes of two historic and two recently isolated hypervirulent strains were analyzed following nutrient shift and osmotic shock. Illumina based RNA-seq was used to sequence these transcriptomes. Our results reveal that although C. difficile strains contain a large number of shared and strain specific genes, the majority of the differentially expressed genes were core genes. We also detected a number of transcriptionally active regions that were not part of the primary genome annotation. Some of these are likely to be small regulatory RNAs.

  8. Comparison of Quantitative Wall Motion Analysis and Strain For Detection Of Coronary Stenosis With Three-Dimensional Dobutamine Stress Echocardiography

    Science.gov (United States)

    Parker, Katherine M.; Clark, Alexander P.; Goodman, Norman C.; Glover, David K.; Holmes, Jeffrey W.

    2015-01-01

    Background Quantitative analysis of wall motion from three-dimensional (3D) dobutamine stress echocardiography (DSE) could provide additional diagnostic information not available from qualitative analysis. In this study we compare the effectiveness of 3D fractional shortening (3DFS), a measure of wall motion computed from 3D echocardiography (3DE), to strain and strain rate measured with sonomicrometry for detecting critical stenoses during DSE. Methods Eleven open-chest dogs underwent DSE both with and without a critical stenosis. 3DFS was measured from 3DE images acquired at peak stress. 3DFS was normalized by subtracting average 3DFS during control peak stress (Δ3DFS). Strains in the perfusion defect (PD) were measured from sonomicrometry, and PD size and location were measured with microspheres. Results A Δ3DFS abnormality indicated the presence of a critical stenosis with high sensitivity and specificity (88% and 100%, respectively), and Δ3DFS abnormality size correlated with PD size (R2=0.54). The sensitivity and specificity for Δ3DFS was similar to that for area strain (88%, 100%) and circumferential strain and strain rate (88%, 92% and 88%, 86%, respectively), while longitudinal strain and strain rate were less specific. Δ3DFS correlated significantly with both coronary flow reserve (R2=0.71) and PD size (R2=0.97), while area strain correlated with PD size only (R2=0.67), and other measures were not significantly correlated with flow reserve or PD size. Conclusion Quantitative wall motion analysis using Δ3DFS is effective for detecting critical stenoses during DSE, performing similarly to 3D strain, and provides potentially useful information on the size and location of a perfusion defect. PMID:24815588

  9. High strain and strain-rate behaviour of PTFE/aluminium/tungsten mixtures

    International Nuclear Information System (INIS)

    Addiss, John; Walley, Stephen; Proud, William; Cai Jing; Nesterenko, Vitali

    2007-01-01

    Conventional drop-weight techniques were modified to accommodate low-amplitude force transducer signals from low-strength, cold isostatically pressed 'heavy' composites of polytetrafluoroethylene, aluminum and tungsten (W). The failure strength, strain and the post-critical behavior of failed samples were measured for samples of different porosity and tungsten grain size. Unusual phenomenon of significantly higher strength (55 MPa) of porous composites (density 5.9 g/cm 3 ) with small W particles ( 3 ) with larger W particles (44 μm) at the same volume content of components was observed. This is attributed to force chains created by a network of small W particles. Interrupted tests at different levels of strain revealed the mechanisms of fracture under dynamic compression

  10. The activity of catalase and superoxide dismutase in isogenous bacteria strains with different radioresistance

    International Nuclear Information System (INIS)

    Vasil'eva, E.I.; Goncharenko, E.N.; Yudz, T.I.; Samojlenko, I.I.

    1984-01-01

    The catalase and superoxide dismutase activity in isogenous bacterial strains with various radiosensitivity is investigated. In micrococcus radiodurans mutants with defects in the DNA repair systems the superoxide dismutase activity is lower than in the wild type cells. In investigated Escherichia coli strains differing in radiosensitivity, no alteration in catalase and superoxide dismutase activity is found. The conclusion is drawn that viability of bacteria subjected to the effect of ionizing radiations is determined by the efficiency of DNA repair systems whose functional reliability is sometimes connected with the catalase and suferoxide dismutase activity

  11. Strain dependent microstructural modifications of BiCrO{sub 3} epitaxial thin films

    Energy Technology Data Exchange (ETDEWEB)

    Kannan, Vijayanandhini, E-mail: kvnandhini@gmail.com [Max Planck Institute of Microstructure Physics, Weinberg 2, D-06120 Halle (Saale) (Germany); CNRS, University of Bordeaux, ICMCB, UPR 9048, F-33600 Pessac (France); Arredondo, Miryam; Johann, Florian; Hesse, Dietrich [Max Planck Institute of Microstructure Physics, Weinberg 2, D-06120 Halle (Saale) (Germany); Labrugere, Christine [CNRS, University of Bordeaux, ICMCB, UPR 9048, F-33600 Pessac (France); CeCaMA, University of Bordeaux, ICMCB, F-33600 Pessac (France); Maglione, Mario [CNRS, University of Bordeaux, ICMCB, UPR 9048, F-33600 Pessac (France); Vrejoiu, Ionela [Max Planck Institute of Microstructure Physics, Weinberg 2, D-06120 Halle (Saale) (Germany)

    2013-10-31

    Strain-dependent microstructural modifications were observed in epitaxial BiCrO{sub 3} (BCO) thin films fabricated on single crystalline substrates, utilizing pulsed laser deposition. The following conditions were employed to modify the epitaxial-strain: (i) in-plane tensile strain, BCO{sub STO} [BCO grown on buffered SrTiO{sub 3} (001)] and in-plane compressive strain, BCO{sub NGO} [BCO grown on buffered NdGaO{sub 3} (110)] and (ii) varying BCO film thickness. A combination of techniques like X-ray diffraction, X-ray photoelectron spectroscopy (XPS) and high resolution transmission electron microscopy (TEM) was used to analyse the epitaxial growth quality and the microstructure of BCO. Our studies revealed that in the case of BCO{sub STO}, a coherent interface with homogeneous orthorhombic phase is obtained only for BCO film with thicknesses, d < 50 nm. All the BCO{sub STO} films with d ≥ 50 nm were found to be strain-relaxed with an orthorhombic phase showing 1/2 <100> and 1/4 <101> satellite reflections, the latter oriented at 45° from orthorhombic diffraction spots. High angle annular dark field scanning TEM of these films strongly suggested that the satellite reflections, 1/2 <100> and 1/4 <101>, originate from the atomic stacking sequence changes (or “modulated structure”) as reported for polytypes, without altering the chemical composition. The unaltered stoichiometry was confirmed by estimating both valency of Bi and Cr cations by surface and in-depth XPS analysis as well as the stoichiometric ratio (1 Bi:1 Cr) using scanning TEM–energy dispersive X-ray analysis. In contrast, compressively strained BCO{sub NGO} films exhibited monoclinic symmetry without any structural modulations or interfacial defects, up to d ∼ 200 nm. Our results indicate that both the substrate-induced in-plane epitaxial strain and the BCO film thickness are the crucial parameters to stabilise a homogeneous BCO phase in an epitaxially grown film. - Highlights: • Phase pure

  12. Quasi-one-dimensional metals on semiconductor surfaces with defects

    International Nuclear Information System (INIS)

    Hasegawa, Shuji

    2010-01-01

    Several examples are known in which massive arrays of metal atomic chains are formed on semiconductor surfaces that show quasi-one-dimensional metallic electronic structures. In this review, Au chains on Si(557) and Si(553) surfaces, and In chains on Si(111) surfaces, are introduced and discussed with regard to the physical properties determined by experimental data from scanning tunneling microscopy (STM), angle-resolved photoemission spectroscopy (ARPES) and electrical conductivity measurements. They show quasi-one-dimensional Fermi surfaces and parabolic band dispersion along the chains. All of them are known from STM and ARPES to exhibit metal-insulator transitions by cooling and charge-density-wave formation due to Peierls instability of the metallic chains. The electrical conductivity, however, reveals the metal-insulator transition only on the less-defective surfaces (Si(553)-Au and Si(111)-In), but not on a more-defective surface (Si(557)-Au). The latter shows an insulating character over the whole temperature range. Compared with the electronic structure (Fermi surfaces and band dispersions), the transport property is more sensitive to the defects. With an increase in defect density, the conductivity only along the metal atomic chains was significantly reduced, showing that atomic-scale point defects decisively interrupt the electrical transport along the atomic chains and hide the intrinsic property of transport in quasi-one-dimensional systems.

  13. Finite element analysis of Al 2024/Cu-Al-Ni shape memory alloy composites with defects/cracks

    Science.gov (United States)

    Kotresh, M.; Benal, M. M., Dr; Siddalinga Swamy, N. H., Dr

    2018-02-01

    In this work, a numerical approach to predict the stress field behaviour of defect/crack in shape memory alloy (SMA) particles reinforced composite known as the adaptive composite is presented. Simulation is based on the finite element method. The critical stress field approach was used to determine the stresses around defect/crack. Thereby stress amplification issue is being resolved. In this paper, the effect volume % of shape memory alloy and shape memory effect of reinforcement for as-cast and SME trained composites are examined and discussed. Shape memory effect known as training is achieved by pre-straining of reinforcement particles by equivalent changes in their expansion coefficients.

  14. Effect of dose and size on defect engineering in carbon cluster implanted silicon wafers

    Science.gov (United States)

    Okuyama, Ryosuke; Masada, Ayumi; Shigematsu, Satoshi; Kadono, Takeshi; Hirose, Ryo; Koga, Yoshihiro; Okuda, Hidehiko; Kurita, Kazunari

    2018-01-01

    Carbon-cluster-ion-implanted defects were investigated by high-resolution cross-sectional transmission electron microscopy toward achieving high-performance CMOS image sensors. We revealed that implantation damage formation in the silicon wafer bulk significantly differs between carbon-cluster and monomer ions after implantation. After epitaxial growth, small and large defects were observed in the implanted region of carbon clusters. The electron diffraction pattern of both small and large defects exhibits that from bulk crystalline silicon in the implanted region. On the one hand, we assumed that the silicon carbide structure was not formed in the implanted region, and small defects formed because of the complex of carbon and interstitial silicon. On the other hand, large defects were hypothesized to originate from the recrystallization of the amorphous layer formed by high-dose carbon-cluster implantation. These defects are considered to contribute to the powerful gettering capability required for high-performance CMOS image sensors.

  15. N+ ion-implantation-induced defects in ZnO studied with a slow positron beam

    International Nuclear Information System (INIS)

    Chen, Z Q; Sekiguchi, T; Yuan, X L; Maekawa, M; Kawasuso, A

    2004-01-01

    Undoped ZnO single crystals were implanted with multiple-energy N + ions ranging from 50 to 380 keV with doses from 10 12 to 10 14 cm -2 . Positron annihilation measurements show that vacancy defects are introduced in the implanted layers. The concentration of the vacancy defects increases with increasing ion dose. The annealing behaviour of the defects can be divided into four stages, which correspond to the formation and recovery of large vacancy clusters and the formation and disappearance of vacancy-impurity complexes, respectively. All the implantation-induced defects are removed by annealing at 1200 deg. C. Cathodoluminescence measurements show that the ion-implantation-induced defects act as nonradiative recombination centres to suppress the ultraviolet (UV) emission. After annealing, these defects disappear gradually and the UV emission reappears, which coincides with positron annihilation measurements. Hall measurements reveal that after N + implantation, the ZnO layer still shows n-type conductivity

  16. Strain-induced oxygen vacancies in ultrathin epitaxial CaMnO3 films

    Science.gov (United States)

    Chandrasena, Ravini; Yang, Weibing; Lei, Qingyu; Delgado-Jaime, Mario; de Groot, Frank; Arenholz, Elke; Kobayashi, Keisuke; Aschauer, Ulrich; Spaldin, Nicola; Xi, Xiaoxing; Gray, Alexander

    Dynamic control of strain-induced ionic defects in transition-metal oxides is considered to be an exciting new avenue towards creating materials with novel electronic, magnetic and structural properties. Here we use atomic layer-by-layer laser molecular beam epitaxy to synthesize high-quality ultrathin single-crystalline CaMnO3 films with systematically varying coherent tensile strain. We then utilize a combination of high-resolution soft x-ray absorption spectroscopy and bulk-sensitive hard x-ray photoemission spectroscopy in conjunction with first-principles theory and core-hole multiplet calculations to establish a direct link between the coherent in-plane strain and the oxygen-vacancy content. We show that the oxygen vacancies are highly mobile, which necessitates an in-situ-grown capping layer in order to preserve the original strain-induced oxygen-vacancy content. Our findings open the door for designing and controlling new ionically active properties in strongly-correlated transition-metal oxides.

  17. Strain-Driven Stacking Faults in CdSe/CdS Core/Shell Nanorods.

    Science.gov (United States)

    Demortière, Arnaud; Leonard, Donovan N; Petkov, Valeri; Chapman, Karena; Chattopadhyay, Soma; She, Chunxing; Cullen, David A; Shibata, Tomohiro; Pelton, Matthew; Shevchenko, Elena V

    2018-04-19

    Colloidal semiconductor nanocrystals are commonly grown with a shell of a second semiconductor material to obtain desired physical properties, such as increased photoluminescence quantum yield. However, the growth of a lattice-mismatched shell results in strain within the nanocrystal, and this strain has the potential to produce crystalline defects. Here, we study CdSe/CdS core/shell nanorods as a model system to investigate the influence of core size and shape on the formation of stacking faults in the nanocrystal. Using a combination of high-angle annular dark-field scanning transmission electron microscopy and pair-distribution-function analysis of synchrotron X-ray scattering, we show that growth of the CdS shell on smaller, spherical CdSe cores results in relatively small strain and few stacking faults. By contrast, growth of the shell on larger, prolate spheroidal cores leads to significant strain in the CdS lattice, resulting in a high density of stacking faults.

  18. On holographic defect entropy

    International Nuclear Information System (INIS)

    Estes, John; Jensen, Kristan; O’Bannon, Andy; Tsatis, Efstratios; Wrase, Timm

    2014-01-01

    We study a number of (3+1)- and (2+1)-dimensional defect and boundary conformal field theories holographically dual to supergravity theories. In all cases the defects or boundaries are planar, and the defects are codimension-one. Using holography, we compute the entanglement entropy of a (hemi-)spherical region centered on the defect (boundary). We define defect and boundary entropies from the entanglement entropy by an appropriate background subtraction. For some (3+1)-dimensional theories we find evidence that the defect/boundary entropy changes monotonically under certain renormalization group flows triggered by operators localized at the defect or boundary. This provides evidence that the g-theorem of (1+1)-dimensional field theories generalizes to higher dimensions

  19. TEM sample preparation by femtosecond laser machining and ion milling for high-rate TEM straining experiments

    Energy Technology Data Exchange (ETDEWEB)

    Voisin, Thomas; Grapes, Michael D. [Dept. of Materials Science and Engineering, Johns Hopkins University, Baltimore, MD 21218 (United States); Zhang, Yong [Dept. of Mechanical Engineering, Johns Hopkins University, Baltimore, MD 21218 (United States); Lorenzo, Nicholas; Ligda, Jonathan; Schuster, Brian [US Army Research Laboratory, Aberdeen Proving Ground, Aberdeen, MD 21005 (United States); Weihs, Timothy P. [Dept. of Materials Science and Engineering, Johns Hopkins University, Baltimore, MD 21218 (United States)

    2017-04-15

    To model mechanical properties of metals at high strain rates, it is important to visualize and understand their deformation at the nanoscale. Unlike post mortem Transmission Electron Microscopy (TEM), which allows one to analyze defects within samples before or after deformation, in situ TEM is a powerful tool that enables imaging and recording of deformation and the associated defect motion during mechanical loading. Unfortunately, all current in situ TEM mechanical testing techniques are limited to quasi-static strain rates. In this context, we are developing a new test technique that utilizes a rapid straining stage and the Dynamic TEM (DTEM) at the Lawrence Livermore National Laboratory (LLNL). The new straining stage can load samples in tension at strain rates as high as 4×10{sup 3}/s using two piezoelectric actuators operating in bending while the DTEM at LLNL can image in movie mode with a time resolution as short as 70 ns. Given the piezoelectric actuators are limited in force, speed, and displacement, we have developed a method for fabricating TEM samples with small cross-sectional areas to increase the applied stresses and short gage lengths to raise the applied strain rates and to limit the areas of deformation. In this paper, we present our effort to fabricate such samples from bulk materials. The new sample preparation procedure combines femtosecond laser machining and ion milling to obtain 300 µm wide samples with control of both the size and location of the electron transparent area, as well as the gage cross-section and length. - Highlights: • Tensile straining TEM specimens made by femtosecond laser machining and ion milling. • Accurate positioning of the electron transparent area within a controlled gauge region. • Optimization of femtosecond laser and ion milling parameters. • Fast production of numerous samples with a highly repeatable geometry.

  20. Atrial and ventricular septal defect with pulmonary and tricuspid valvular anomalies in a dog

    International Nuclear Information System (INIS)

    Ishikawa, Y.; Wakao, Y.; Watanabe, T.; Minami, T.; Muto, M.; Suzuki, T.; Takahashi, M.; Une, Y.; Nomura, Y.; Ichioka, N.

    1989-01-01

    A 15-month-old male boxer dog weighing 22 kg was referred to Azabu University Animal Hospital for evaluation of the syncopal attack. There was no cardiac murmur, but electrocardiograms revealed an atrial fibrillation. Thoracic radiograph revealed enlargement of the right and left atrial regions. The medical treatment with digitalis and captopril was made for conversion from the atrial fibrillation to the sinus rhythm. By cardiac catheterization, atrial and ventricular septal defect with pulmonary stenosis was demonstrated. The patient died at 20 months from the first medical examination. At autopsy, there were severe enlargement of both atria, atrial defect, and pulmonary and tricuspid valvular anomalies. (author)

  1. Atrial and ventricular septal defect with pulmonary and tricuspid valvular anomalies in a dog

    Energy Technology Data Exchange (ETDEWEB)

    Ishikawa, Y. [Azabu Univ., Sagamihara, Kanagawa (Japan); Wakao, Y.; Watanabe, T.; Minami, T.; Muto, M.; Suzuki, T.; Takahashi, M.; Une, Y.; Nomura, Y.; Ichioka, N.

    1989-12-15

    A 15-month-old male boxer dog weighing 22 kg was referred to Azabu University Animal Hospital for evaluation of the syncopal attack. There was no cardiac murmur, but electrocardiograms revealed an atrial fibrillation. Thoracic radiograph revealed enlargement of the right and left atrial regions. The medical treatment with digitalis and captopril was made for conversion from the atrial fibrillation to the sinus rhythm. By cardiac catheterization, atrial and ventricular septal defect with pulmonary stenosis was demonstrated. The patient died at 20 months from the first medical examination. At autopsy, there were severe enlargement of both atria, atrial defect, and pulmonary and tricuspid valvular anomalies. (author)

  2. Contribution of Metal Defects in the Assembly Induced Emission of Cu Nanoclusters

    KAUST Repository

    Wu, Zhennan

    2017-03-20

    Aggregation/assembly induced emission (AIE) has been observed for metal nanoclusters (NCs), but the origin of the enhanced emission is not fully understood, yet. In this work, the significant contribution of metal defects on AIE is revealed by engineering the self-assembly process of Cu NCs using ethanol. The presence of ethanol leads to a rapid assembly of NCs into ultrathin nanosheets, promoting the formation of metal defects-rich surface. Detailed studies and computer simulation confirm that the metal defects-rich nanosheets possess increased Cu(I)-to-Cu(0) ratio, which greatly influences ligand-to-metal-metal charge transfer and therewith facilitates the radiative relaxation of excitons. Consequently, the Cu NCs self-assembly nanosheets exhibit obvious emission enhancement.

  3. Determining casting defects in near-net shape casting aluminum parts by computed tomography

    Science.gov (United States)

    Li, Jiehua; Oberdorfer, Bernd; Habe, Daniel; Schumacher, Peter

    2018-03-01

    Three types of near-net shape casting aluminum parts were investigated by computed tomography to determine casting defects and evaluate quality. The first, second, and third parts were produced by low-pressure die casting (Al-12Si-0.8Cu-0.5Fe-0.9Mg-0.7Ni-0.2Zn alloy), die casting (A356, Al-7Si-0.3Mg), and semi-solid casting (A356, Al-7Si-0.3Mg), respectively. Unlike die casting (second part), low-pressure die casting (first part) significantly reduced the formation of casting defects (i.e., porosity) due to its smooth filling and solidification under pressure. No significant casting defect was observed in the third part, and this absence of defects indicates that semi-solid casting could produce high-quality near-net shape casting aluminum parts. Moreover, casting defects were mostly distributed along the eutectic grain boundaries. This finding reveals that refinement of eutectic grains is necessary to optimize the distribution of casting defects and reduce their size. This investigation demonstrated that computed tomography is an efficient method to determine casting defects in near-net shape casting aluminum parts.

  4. Plain defects and their vortex configuration in dilute Mo-B alloys in dissipative structure

    International Nuclear Information System (INIS)

    Sofronova, R.M.

    1992-01-01

    Electron microscopic study of single crystal of Mo-0.003 mas.% B alloy after zone melting and annealing at 2373 K was conducted to reveal the nature of planar defects and the role of boron in their formation. It was shown that planar defects should be considered as preprecipitations of MoB nonequilibrous phase out of molybdenum base solid solution. A planar defect was found to constitute a monolayer of boron atoms which consisted of B-B zigzag-like chains. Inturn the chains were surrounded by Mo atoms which formed hexagonal prism. The coherency of planar defects with matrix was due to close lattice parameters of Mo, β-MoB and δ-MoB. The planar defects in molybdenum base alloy were considered as elements of dissipative structure. They determined formation of supercellular dislocation structure under deformation

  5. Influence of coating defects on the corrosion behavior of cold sprayed refractory metals

    International Nuclear Information System (INIS)

    Kumar, S.; Rao, A. Arjuna

    2017-01-01

    Highlights: • Long duration immersion tests reveal inhomogeneous weight losses. • The weight loss for different coatings are well corroborated with the coating defects. • Chemical and micro structural analysis elucidates the reason behind the in homogeneous performance of different type of cold sprayed coatings. • In cold sprayed titanium, formation of oxide along the inter-splat boundary hinders the aggressive attack of the medium. - Abstract: The defects in the cold sprayed coatings are critical in the case of corrosion performances of the coatings in aggressive conditions. To understand the influence of coating defects on corrosion, immersion tests have been carried out in HF solution for the cold sprayed and heat treated Titanium, Tantalum and Niobium coatings. Long duration immersion tests reveal inhomogeneous weight losses of the samples prepared at different heat treatment conditions. The weight loss for different coatings has been well corroborated with the coating defects and microstructures. Chemical and micro structural analysis elucidates the reason behind the inhomogeneous performance of different type of cold sprayed coatings in corrosion medium. In the case of cold sprayed titanium, formation of stable oxide along the inter-splat boundary hinders the aggressive attack of the corrosion medium which is not so in other cases.

  6. Defect mediated van der Waals epitaxy of hexagonal boron nitride on graphene

    Science.gov (United States)

    Heilmann, M.; Bashouti, M.; Riechert, H.; Lopes, J. M. J.

    2018-04-01

    Van der Waals heterostructures comprising of hexagonal boron nitride and graphene are promising building blocks for novel two-dimensional devices such as atomically thin transistors or capacitors. However, demonstrators of those devices have been so far mostly fabricated by mechanical assembly, a non-scalable and time-consuming method, where transfer processes can contaminate the surfaces. Here, we investigate a direct growth process for the fabrication of insulating hexagonal boron nitride on high quality epitaxial graphene using plasma assisted molecular beam epitaxy. Samples were grown at varying temperatures and times and studied using atomic force microscopy, revealing a growth process limited by desorption at high temperatures. Nucleation was mostly commencing from morphological defects in epitaxial graphene, such as step edges or wrinkles. Raman spectroscopy combined with x-ray photoelectron measurements confirm the formation of hexagonal boron nitride and prove the resilience of graphene against the nitrogen plasma used during the growth process. The electrical properties and defects in the heterostructures were studied with high lateral resolution by tunneling current and Kelvin probe force measurements. This correlated approach revealed a nucleation apart from morphological defects in epitaxial graphene, which is mediated by point defects. The presented results help understanding the nucleation and growth behavior during van der Waals epitaxy of 2D materials, and point out a route for a scalable production of van der Waals heterostructures.

  7. X-ray-induced mutations in Escherichia coli K-12 strains with altered DNA polymerase I activities

    International Nuclear Information System (INIS)

    Nagata, Yuki; Kawata, Masakado; Komura, Jun-ichiro; Ono, Tetsuya; Yamamoto, Kazuo

    2003-01-01

    Spectra of ionizing radiation mutagenesis were determined by sequencing X-ray-induced endogenous tonB gene mutations in Escherichia coli polA strains. We used two polA alleles, the polA1 mutation, defective for Klenow domain, and the polA107 mutation, defective for flap domain. We demonstrated that irradiation of 75 and 50 Gy X-rays could induce 3.8- and 2.6-fold more of tonB mutation in polA1 and polA107 strains, respectively, than spontaneous level. The radiation induced spectrum of 51 tonB mutations in polA1 and 51 in polA107 indicated that minus frameshift, A:T→T:A transversion and G:C→T:A transversion were the types of mutations increased. Previously, we have reported essentially the same X-ray-induced tonB mutation spectra in the wild-type strain. These results indicate that (1) X-rays can induce minus frameshift, A:T→T:A transversion and G:C→T:A transversion in E. coli and (2) presence or absence of polymerase I (PolI) of E. coli does not have any effects on the process of X-ray mutagenesis

  8. Use of the piezoelectric film for the determination of cracks and defects - the passive and active electric potential CT method

    International Nuclear Information System (INIS)

    Kubo, S; Sakagami, T; Suzuki, T; Maeda, T; Nakatani, K

    2008-01-01

    The passive and active electric potential CT method was proposed by using piezoelectric film for identification of cracks and defects. This method is based on the principle of mutual conversion between mechanical strains and electric potential of piezoelectric material. A smart-layer was constructed using the piezoelectric film, and attached on a structure with a defect. When the structure was subjected to a mechanical load, the electric potential distribution appeared passively on the piezoelectric film due to the direct piezoelectric effect. The defect can be identified from the distribution with the help of inverse analysis. It was found that the crack could be identified reasonably, although the defect depth was not well estimated for the defects located far from the layer. When the electric signal was input to the smart-layer, acoustic wave was actively emitted from the layer due to the inverse piezoelectric effect, and a reflected wave was received on the layer. It was found that the depth of the defect could be estimated well. The simultaneous use of the passive method and the active method is promising for the identification of the defect.

  9. Comparative genome analysis of pathogenic and non-pathogenic Clavibacter strains reveals adaptations to their lifestyle

    OpenAIRE

    Załuga, Joanna; Stragier, Pieter; Baeyen, Steve; Haegeman, Annelies; Van Vaerenbergh, Johan; Maes, Martine; De Vos, Paul

    2014-01-01

    Background The genus Clavibacter harbors economically important plant pathogens infecting agricultural crops such as potato and tomato. Although the vast majority of Clavibacter strains are pathogenic, there is an increasing number of non-pathogenic isolates reported. Non-pathogenic Clavibacter strains isolated from tomato seeds are particularly problematic because they affect the current detection and identification tests for Clavibacter michiganensis subsp. michiganensis (Cmm), which is reg...

  10. Multiple hypersensitivity to mutagens in a cell strain (46BR) derived from a patient with immuno-deficiencies

    International Nuclear Information System (INIS)

    Teo, I.A.; Arlett, C.F.; Harcourt, S.A.; Priestley, A.; Broughton, B.C.

    1983-01-01

    46BR is a fibroblast cell strain established from an individual with hypogammaglobulinaemia. The cells are unique in showing hypersensitivity to the lethal effects of a wide range of DNA-damaging agents. Thus they are hypersensitive to #betta#- and 254-nm UV-irradiation and show a limited capacity to repair potentially lethal #betta#-irradiation damage when compared with fibroblasts from normal individuals. A slight hypersensitivity to mitomycin C was also revealed but we were not able to discriminate 46BR from normals with 4-nitroquinoline oxide. The cells were hypersensitive to the alkylating agents, dimethyl sulphate, methyl methanesulphonate, ethyl methanesulphonate, N-methyl-N'-nitro-N-nitrosoguanidine and N-methyl-N-nitrosourea but not N-ethyl-N-nitrosourea. A consideration of the spectra of DNA lesions produced by these alkylating agents together with the sensitivity to ionising radiation and mitomycin C suggests that 46BR cells are defective in a repair step that is common to all agents. We suggest that the cells are defective in DNA polymerisation or ligation. Support for this suggestion comes from the absence of any hypersensitivity to N-ethyl-N-nitrosourea since its major reaction products are not removed by excision pathways that require polymerisation and ligation. (orig.)

  11. Nature of oxygen donors and radiation defects in oxygen-doped germanium

    International Nuclear Information System (INIS)

    Fukuoka, Noboru; Atobe, Kozo; Honda, Makoto; Matsuda, Koji.

    1991-01-01

    The nature of oxygen donors and radiation defects in oxygen-doped germanium were studied through measurements of the infrared absorption spectrum, deep level transient spectroscopy spectrum and carrier concentration. It is revealed that a new donor is not formed in oxygen-doped germanium. An A-center (interstitial oxygen-vacancy pair) forms a complex with a thermal donor in its annealing stage at 60degC-140degC. The introduction rate of defects by 1.5 MeV electron irradiation was enhanced in thermal-donor-doped samples. (author)

  12. Defected and Functionalized Germanene based Nanosensors under Sulfur Comprising Gas Exposure

    KAUST Repository

    Hussain, Tanveer; kaewmaraya, thanayut; Chakraborty, Sudip; Vovusha, Hakkim; Amornkitbamrung, Vittaya; Ahuja, Rajeev

    2018-01-01

    by means of DFT based first principles calculations to envisage the structural, electronic and gas sensing properties of pristine, defected and metal substituted Ge-NS. Our initial screening has revealed that although interaction of SO2 on pristine Ge

  13. Strain evolution in Si substrate due to implantation of MeV ion observed by extremely asymmetric x-ray diffraction

    International Nuclear Information System (INIS)

    Emoto, T.; Ghatak, J.; Satyam, P. V.; Akimoto, K.

    2009-01-01

    We studied the strain introduced in a Si(111) substrate due to MeV ion implantation using extremely asymmetric x-ray diffraction and measured the rocking curves of asymmetrical 113 diffraction for the Si substrates implanted with a 1.5 MeV Au 2+ ion at fluence values of 1x10 13 , 5x10 13 , and 1x10 14 /cm 2 . The measured curves consisted of a bulk peak and accompanying subpeak with an interference fringe. The positional relationship of the bulk peak to the subpeak and the intensity variation of those peaks with respect to the wavelengths of the x rays indicated that crystal lattices near the surface were strained; the lattice spacing of surface normal (111) planes near the surface was larger than that of the bulk. Detailed strain profiles along the depth direction were successfully estimated using a curve-fitting method based on Darwin's dynamical diffraction theory. Comparing the shapes of resultant strain profiles, we found that a strain evolution rapidly occurred within a depth of ∼300 nm at fluence values between 1x10 13 and 5x10 13 /cm 2 . This indicates that formation of the complex defects progressed near the surface when the fluence value went beyond a critical value between 1x10 13 and 5x10 13 /cm 2 and the defects brought a large strain to the substrate.

  14. Ceramic Defects in Metal-Ceramic Fixed Dental Prostheses Made from Co-Cr and Au-Pt Alloys: A Retrospective Study.

    Science.gov (United States)

    Mikeli, Aikaterini; Boening, Klaus W; Lißke, Benjamin

    2015-01-01

    Ceramic defects in porcelain-fused-to-metal (PFM) restorations may depend on framework alloy type. This study assessed ceramic defects on cobalt-chromium- (Co-Cr-) and gold-platinum- (Au-Pt-) based PFM restorations. In this study, 147 Co-Cr-based and 168 Au-Pt-based PFM restorations inserted between 1998 and 2010 (139 patients) were examined for ceramic defects. Detected defects were assigned to three groups according to clinical defect relevance. Ceramic defect rates (Co-Cr-based: 12.9%; Au-Pt-based: 7.2%) revealed no significant difference but a strong statistical trend (U test, P = .082). Most defects were of little clinical relevance. Co-Cr PFM restorations may be at higher risk for ceramic defects compared to Au-Pt-based restorations.

  15. Optical defect modes in chiral liquid crystals

    International Nuclear Information System (INIS)

    Belyakov, V. A.; Semenov, S. V.

    2011-01-01

    An analytic approach to the theory of optical defect modes in chiral liquid crystals (CLCs) is developed. The analytic study is facilitated by the choice of the problem parameters. Specifically, an isotropic layer (with the dielectric susceptibility equal to the average CLC dielectric susceptibility) sandwiched between two CLC layers is studied. The chosen model allows eliminating the polarization mixing and reducing the corresponding equations to the equations for light of diffracting polarization only. The dispersion equation relating the defect mode (DM) frequency to the isotropic layer thickness and an analytic expression for the field distribution in the DM structure are obtained and the corresponding dependences are plotted for some values of the DM structure parameters. Analytic expressions for the transmission and reflection coefficients of the DM structure (CLC-defect layer-CLC) are presented and analyzed for nonabsorbing, absorbing, and amplifying CLCs. The anomalously strong light absorption effect at the DM frequency is revealed. The limit case of infinitely thick CLC layers is considered in detail. It is shown that for distributed feedback lasing in a defect structure, adjusting the lasing frequency to the DM frequency results in a significant decrease in the lasing threshold. The DM dispersion equations are solved numerically for typical values of the relevant parameters. Our approach helps clarify the physics of the optical DMs in CLCs and completely agrees with the corresponding results of the previous numerical investigations.

  16. Lattice defect investigation of nanostructured ECAP-Cu by means of x-ray line profile analysis, calorimetry and electrical resistometry

    International Nuclear Information System (INIS)

    Schafler, E.; Steiner, G.; KEXrber, M.; Zehetbauer, M.J.; Korznikova, E.

    2005-01-01

    Full text: Cu rods have been deformed by Equal Channel Angular Pressing (ECAP) up to shear strains γ ∼ 5 while applying various deformation paths A, B c and C. ECAP processed materials show a microstructure with grain sizes in the nanometer range and a high density of lattice defects. X-ray Bragg Profile Analyses (XPA), Differential Scanning Calorimetry (DSC) as well as Residual Electrical Resistivity (RER) measurements have been performed, in order to detect the densities of various deformation induced lattice defects and/or their arrangements. The results have been analyzed in terms of annealing of deformation induced dislocations and vacancies (vacancy agglomerates). Compared to conventional cold work procedures, deformation by ECAP achieves a strongly enhanced concentration of vacancy type defects. (author)

  17. Oxidation behavior of graphene-coated copper at intrinsic graphene defects of different origins.

    Science.gov (United States)

    Kwak, Jinsung; Jo, Yongsu; Park, Soon-Dong; Kim, Na Yeon; Kim, Se-Yang; Shin, Hyung-Joon; Lee, Zonghoon; Kim, Sung Youb; Kwon, Soon-Yong

    2017-11-16

    The development of ultrathin barrier films is vital to the advanced semiconductor industry. Graphene appears to hold promise as a protective coating; however, the polycrystalline and defective nature of engineered graphene hinders its practical applications. Here, we investigate the oxidation behavior of graphene-coated Cu foils at intrinsic graphene defects of different origins. Macro-scale information regarding the spatial distribution and oxidation resistance of various graphene defects is readily obtained using optical and electron microscopies after the hot-plate annealing. The controlled oxidation experiments reveal that the degree of structural deficiency is strongly dependent on the origins of the structural defects, the crystallographic orientations of the underlying Cu grains, the growth conditions of graphene, and the kinetics of the graphene growth. The obtained experimental and theoretical results show that oxygen radicals, decomposed from water molecules in ambient air, are effectively inverted at Stone-Wales defects into the graphene/Cu interface with the assistance of facilitators.

  18. Origin of the Strain Sensitivity for an Organic Heptazole Thin-Film and Its Strain Gauge Application

    Science.gov (United States)

    Bae, Heesun; Jeon, Pyo Jin; Park, Ji Hoon; Lee, Kimoon

    2018-04-01

    The authors report on the origin of the strain sensitivity for an organic C26H16N2 (heptazole) thinfilm and its application for the detection of tensile strain. From the electrical characterization on the thin-film transistor adopting a heptazole channel, heptazole film exhibits p-channel conduction with a relatively low value of field-effect mobility (0.05 cm2/Vs), suggesting a hopping conduction behavior via hole carriers. By analyzing the strain and temperature dependences of the electrical conductivity, we reveal that the electrical conduction for a heptazole thin-film is dominated by the variable range hopping process with quite a large energy separation (224.9 meV) between the localized states under a relatively long attenuation length (10.46 Å). This indicates that a change in the inter-grain spacing that is much larger than the attenuation length is responsible for the reversible modification of electrical conductivity depending on strain for the heptazole film. By utilizing our heptazole thin-film both as a strain sensitive passive resistor and an active semiconducting channel layer, we can achieve a strain gauge device exhibiting reversible endurance for tensile strains up to 2.12%. Consequently, this study advances the understanding of the fundamental strain sensing mechanism in a heptazole thin-film toward finding a promise material with a strain gauge for applications as potential flexible devices and/or wearable electronics.

  19. Defects in semiconductors

    CERN Document Server

    Romano, Lucia; Jagadish, Chennupati

    2015-01-01

    This volume, number 91 in the Semiconductor and Semimetals series, focuses on defects in semiconductors. Defects in semiconductors help to explain several phenomena, from diffusion to getter, and to draw theories on materials' behavior in response to electrical or mechanical fields. The volume includes chapters focusing specifically on electron and proton irradiation of silicon, point defects in zinc oxide and gallium nitride, ion implantation defects and shallow junctions in silicon and germanium, and much more. It will help support students and scientists in their experimental and theoret

  20. Three-dimensional characterization of extreme ultraviolet mask blank defects by interference contrast photoemission electron microscopy.

    Science.gov (United States)

    Lin, Jingquan; Weber, Nils; Escher, Matthias; Maul, Jochen; Han, Hak-Seung; Merkel, Michael; Wurm, Stefan; Schönhense, Gerd; Kleineberg, Ulf

    2008-09-29

    A photoemission electron microscope based on a new contrast mechanism "interference contrast" is applied to characterize extreme ultraviolet lithography mask blank defects. Inspection results show that positioning of interference destructive condition (node of standing wave field) on surface of multilayer in the local region of a phase defect is necessary to obtain best visibility of the defect on mask blank. A comparative experiment reveals superiority of the interference contrast photoemission electron microscope (Extreme UV illumination) over a topographic contrast one (UV illumination with Hg discharge lamp) in detecting extreme ultraviolet mask blank phase defects. A depth-resolved detection of a mask blank defect, either by measuring anti-node peak shift in the EUV-PEEM image under varying inspection wavelength condition or by counting interference fringes with a fixed illumination wavelength, is discussed.

  1. Optimal Fluorescence Waveband Determination for Detecting Defective Cherry Tomatoes Using a Fluorescence Excitation-Emission Matrix

    Directory of Open Access Journals (Sweden)

    In-Suck Baek

    2014-11-01

    Full Text Available A multi-spectral fluorescence imaging technique was used to detect defective cherry tomatoes. The fluorescence excitation and emission matrix was used to measure for defects, sound surface and stem areas to determine the optimal fluorescence excitation and emission wavelengths for discrimination. Two-way ANOVA revealed the optimal excitation wavelength for detecting defect areas was 410 nm. Principal component analysis (PCA was applied to the fluorescence emission spectra of all regions at 410 nm excitation to determine the emission wavelengths for defect detection. The major emission wavelengths were 688 nm and 506 nm for the detection. Fluorescence images combined with the determined emission wavebands demonstrated the feasibility of detecting defective cherry tomatoes with >98% accuracy. Multi-spectral fluorescence imaging has potential utility in non-destructive quality sorting of cherry tomatoes.

  2. Electrical properties of Schottky barrier diodes fabricated on (001) β-Ga2O3 substrates with crystal defects

    Science.gov (United States)

    Oshima, Takayoshi; Hashiguchi, Akihiro; Moribayashi, Tomoya; Koshi, Kimiyoshi; Sasaki, Kohei; Kuramata, Akito; Ueda, Osamu; Oishi, Toshiyuki; Kasu, Makoto

    2017-08-01

    The electrical properties of Schottky barrier diodes (SBDs) on a (001) β-Ga2O3 substrate were characterized and correlated with wet etching-revealed crystal defects below the corresponding Schottky contacts. The etching process revealed etched grooves and etched pits, indicating the presence of line-shaped voids and small defects near the surface, respectively. The electrical properties (i.e., leakage currents, ideality factor, and barrier height) exhibited almost no correlation with the density of the line-shaped voids. This very weak correlation was reasonable considering the parallel positional relation between the line-shaped voids extending along the [010] direction and the (001) basal plane in which the voids are rarely exposed on the initial surface in contact with the Schottky metals. The distribution of small defects and SBDs with unusually large leakage currents showed similar patterns on the substrate, suggesting that these defects were responsible for the onset of fatal leak paths. These results will encourage studies on crystal defect management of (001) β-Ga2O3 substrates for the fabrication of devices with enhanced performance using these substrates.

  3. Frequency Optimization for Enhancement of Surface Defect Classification Using the Eddy Current Technique

    Science.gov (United States)

    Fan, Mengbao; Wang, Qi; Cao, Binghua; Ye, Bo; Sunny, Ali Imam; Tian, Guiyun

    2016-01-01

    Eddy current testing is quite a popular non-contact and cost-effective method for nondestructive evaluation of product quality and structural integrity. Excitation frequency is one of the key performance factors for defect characterization. In the literature, there are many interesting papers dealing with wide spectral content and optimal frequency in terms of detection sensitivity. However, research activity on frequency optimization with respect to characterization performances is lacking. In this paper, an investigation into optimum excitation frequency has been conducted to enhance surface defect classification performance. The influences of excitation frequency for a group of defects were revealed in terms of detection sensitivity, contrast between defect features, and classification accuracy using kernel principal component analysis (KPCA) and a support vector machine (SVM). It is observed that probe signals are the most sensitive on the whole for a group of defects when excitation frequency is set near the frequency at which maximum probe signals are retrieved for the largest defect. After the use of KPCA, the margins between the defect features are optimum from the perspective of the SVM, which adopts optimal hyperplanes for structure risk minimization. As a result, the best classification accuracy is obtained. The main contribution is that the influences of excitation frequency on defect characterization are interpreted, and experiment-based procedures are proposed to determine the optimal excitation frequency for a group of defects rather than a single defect with respect to optimal characterization performances. PMID:27164112

  4. Genomic comparison of invasive and rare non-invasive strains reveals Porphyromonas gingivalis genetic polymorphisms

    Directory of Open Access Journals (Sweden)

    Svetlana Dolgilevich

    2011-03-01

    Full Text Available Porphyromonas gingivalis strains are shown to invade human cells in vitro with different invasion efficiencies, varying by up to three orders of magnitude.We tested the hypothesis that invasion-associated interstrain genomic polymorphisms are present in P. gingivalis and that putative invasion-associated genes can contribute to P. gingivalis invasion.Using an invasive (W83 and the only available non-invasive P. gingivalis strain (AJW4 and whole genome microarrays followed by two separate software tools, we carried out comparative genomic hybridization (CGH analysis.We identified 68 annotated and 51 hypothetical open reading frames (ORFs that are polymorphic between these strains. Among these are surface proteins, lipoproteins, capsular polysaccharide biosynthesis enzymes, regulatory and immunoreactive proteins, integrases, and transposases often with abnormal GC content and clustered on the chromosome. Amplification of selected ORFs was used to validate the approach and the selection. Eleven clinical strains were investigated for the presence of selected ORFs. The putative invasion-associated ORFs were present in 10 of the isolates. The invasion ability of three isogenic mutants, carrying deletions in PG0185, PG0186, and PG0982 was tested. The PG0185 (ragA and PG0186 (ragB mutants had 5.1×103-fold and 3.6×103-fold decreased in vitro invasion ability, respectively.The annotation of divergent ORFs suggests deficiency in multiple genes as a basis for P. gingivalis non-invasive phenotype. Access the supplementary material to this article: Supplement, table (see Supplementary files under Reading Tools online.

  5. Radiation defect production in quartz crystals with various structure perfectness degree; Radiatsionnoe defektoobrazovanie v kristallakh kvartsa s razlichnoj stepen`yu sovershenstva struktury

    Energy Technology Data Exchange (ETDEWEB)

    Khushvakov, O B

    1992-01-01

    Radiation defects production processes in pure and doped quartz crystals with various structure defectness, caused by preliminary irradiation with neutrons, protons, deuterons and {alpha}-particles, during various electron excitation densities were investigated. The distribution of colour centres along the thickness of irradiated quartz crystals was measured. It was supposed that colour centres are produced on account of inelastic energy losses as the result of collective decay of two or more interacting excitons. It was shown that in quartz crystals under the actions of protons with overthreshold energy 18 MeV and electrons with subthreshold energy 100 keV the same structure defects are formed. It was established that radiation defect production process has two stages. The first stage reveals radiation defects produced by preliminary irradiation. The second one reveals additional intrinsic defects formed under the action of gamma-rays and electrons. The probability dependence of defect production on neutron fluence and masses of incident particles was studied. It was supposed that the creation of additional defects in preliminary irradiated crystals is due to non-radiative decay of electron excitations near radiation-induced defects. It was shown that increase of impurity concentration leads to rate growth of accumulation of radiation induced defects. (A.A.D.) 15 refs. 4 figs.

  6. Size Effects on Surface Elastic Waves in a Semi-Infinite Medium with Atomic Defect Generation

    Directory of Open Access Journals (Sweden)

    F. Mirzade

    2013-01-01

    Full Text Available The paper investigates small-scale effects on the Rayleigh-type surface wave propagation in an isotopic elastic half-space upon laser irradiation. Based on Eringen’s theory of nonlocal continuum mechanics, the basic equations of wave motion and laser-induced atomic defect dynamics are derived. Dispersion equation that governs the Rayleigh surface waves in the considered medium is derived and analyzed. Explicit expressions for phase velocity and attenuation (amplification coefficients which characterize surface waves are obtained. It is shown that if the generation rate is above the critical value, due to concentration-elastic instability, nanometer sized ordered concentration-strain structures on the surface or volume of solids arise. The spatial scale of these structures is proportional to the characteristic length of defect-atom interaction and increases with the increase of the temperature of the medium. The critical value of the pump parameter is directly proportional to recombination rate and inversely proportional to deformational potentials of defects.

  7. [Genetic modification of Methylobacterium extorquens G10 producer strain of polyhydroxybutyrate].

    Science.gov (United States)

    Fedorov, D N; Zamakhaeva, S A; Ezhov, V A; Doronina, N V; Trotsenko, Iu A

    2014-01-01

    The effect of the increased copy number of polyhydroxybutyrate (PHB) biosynthesis genes in pink-pigmented methylobacterium Methylobacterium extorquens G10 on properties of the biopolymer was studied. The activity of poly-3-hydroxybutyril-synthase (PHB-synthase) was shown to increase and the molecular weight of synthesized PHB decreases twofold (150 --> 79 kDa) after insertion of extra copies of phaC and phaCAB genes into cells of the producer strain, whereas the physicochemical properties of the plastic changed insignificantly. White mutant M. extorquens G10-W with disrupted synthesis of the carotenoid pigment (defect by the crtI gene, which codes for phytoene desaturase) was established to have the same rate of growth and level of PHB accumulation as the initial strain G10. The G10-W strain is a promising producer of PHB, with decreased expenses for purification and PHB biosynthesis.

  8. Combination of Metabolomic and Proteomic Analysis Revealed Different Features among Lactobacillus delbrueckii Subspecies bulgaricus and lactis Strains While In Vivo Testing in the Model Organism Caenorhabditis elegans Highlighted Probiotic Properties

    Directory of Open Access Journals (Sweden)

    Elena Zanni

    2017-06-01

    Full Text Available Lactobacillus delbrueckii represents a technologically relevant member of lactic acid bacteria, since the two subspecies bulgaricus and lactis are widely associated with fermented dairy products. In the present work, we report the characterization of two commercial strains belonging to L. delbrueckii subspecies bulgaricus, lactis and a novel strain previously isolated from a traditional fermented fresh cheese. A phenomic approach was performed by combining metabolomic and proteomic analysis of the three strains, which were subsequently supplemented as food source to the model organism Caenorhabditis elegans, with the final aim to evaluate their possible probiotic effects. Restriction analysis of 16S ribosomal DNA revealed that the novel foodborne strain belonged to L. delbrueckii subspecies lactis. Proteomic and metabolomic approaches showed differences in folate, aminoacid and sugar metabolic pathways among the three strains. Moreover, evaluation of C. elegans lifespan, larval development, brood size, and bacterial colonization capacity demonstrated that L. delbrueckii subsp. bulgaricus diet exerted beneficial effects on nematodes. On the other hand, both L. delbrueckii subsp. lactis strains affected lifespan and larval development. We have characterized three strains belonging to L. delbrueckii subspecies bulgaricus and lactis highlighting their divergent origin. In particular, the two closely related isolates L. delbrueckii subspecies lactis display different galactose metabolic capabilities. Moreover, the L. delbrueckii subspecies bulgaricus strain demonstrated potential probiotic features. Combination of omic platforms coupled with in vivo screening in the simple model organism C. elegans is a powerful tool to characterize industrially relevant bacterial isolates.

  9. Combination of Metabolomic and Proteomic Analysis Revealed Different Features among Lactobacillus delbrueckii Subspecies bulgaricus and lactis Strains While In Vivo Testing in the Model Organism Caenorhabditis elegans Highlighted Probiotic Properties.

    Science.gov (United States)

    Zanni, Elena; Schifano, Emily; Motta, Sara; Sciubba, Fabio; Palleschi, Claudio; Mauri, Pierluigi; Perozzi, Giuditta; Uccelletti, Daniela; Devirgiliis, Chiara; Miccheli, Alfredo

    2017-01-01

    Lactobacillus delbrueckii represents a technologically relevant member of lactic acid bacteria, since the two subspecies bulgaricus and lactis are widely associated with fermented dairy products. In the present work, we report the characterization of two commercial strains belonging to L. delbrueckii subspecies bulgaricus , lactis and a novel strain previously isolated from a traditional fermented fresh cheese. A phenomic approach was performed by combining metabolomic and proteomic analysis of the three strains, which were subsequently supplemented as food source to the model organism Caenorhabditis elegans , with the final aim to evaluate their possible probiotic effects. Restriction analysis of 16S ribosomal DNA revealed that the novel foodborne strain belonged to L. delbrueckii subspecies lactis . Proteomic and metabolomic approaches showed differences in folate, aminoacid and sugar metabolic pathways among the three strains. Moreover, evaluation of C. elegans lifespan, larval development, brood size, and bacterial colonization capacity demonstrated that L. delbrueckii subsp. bulgaricus diet exerted beneficial effects on nematodes. On the other hand, both L. delbrueckii subsp. lactis strains affected lifespan and larval development. We have characterized three strains belonging to L. delbrueckii subspecies bulgaricus and lactis highlighting their divergent origin. In particular, the two closely related isolates L. delbrueckii subspecies lactis display different galactose metabolic capabilities. Moreover, the L. delbrueckii subspecies bulgaricus strain demonstrated potential probiotic features. Combination of omic platforms coupled with in vivo screening in the simple model organism C. elegans is a powerful tool to characterize industrially relevant bacterial isolates.

  10. Surface Defects in Sheet Metal Forming: a Simulative Laboratory Device and Comparison with FE Analysis

    Science.gov (United States)

    Thuillier, Sandrine; Le Port, Alban; Manach, Pierre-Yves

    2011-08-01

    Surface defects are small concave imperfections that can develop during forming on outer convex panels of automotive parts like doors. They occur during springback steps, after drawing in the vicinity of bending over a curved line and flanging/hemming in the vicinity of the upper corner of a door. They can alter significantly the final quality of the automobile and it is of primary importance to deal with them as early as possible in the design of the forming tools. The aim of this work is to reproduce at the laboratory scale such a defect, in the case of the flanging along a curved edge, made of two orthogonal straight part of length 50 mm and joint by a curved line. A dedicated device has been designed and steel samples were tested. Each sample was measured initially (after laser cutting) and after flanging, with a 3D measuring machine. 2D profiles were extracted and the curvature was calculated. Surface defects were defined between points where the curvature sign changed. Isovalues of surface defect depth could then be plotted, thus displaying also the spatial geometry on the part surface. An experimental database has been created on the influence of process parameters like the flanging height and the flanging radius. Numerical simulations have been performed with the finite element code Abaqus to predict the occurrence of such surface defects and to analyze stress and strain distribution within the defect area.

  11. Fibrous metaphyseal defects

    International Nuclear Information System (INIS)

    Ritschl, P.; Hajek, P.C.; Pechmann, U.

    1989-01-01

    Sixteen patients with fibrous metaphyseal defects were examined with both plain radiography and magnetic resonance (MR) imaging. Depending on the age of the fibrous metaphyseal defects, characteristic radiomorphologic changes were found which correlated well with MR images. Following intravenous Gadolinium-DTPA injection, fibrous metaphyseal defects invariably exhibited a hyperintense border and signal enhancement. (orig./GDG)

  12. Vertebral defect, anal atresia, cardiac defect, tracheoesophageal fistula/esophageal atresia, renal defect, and limb defect association with Mayer-Rokitansky-Küster-Hauser syndrome in co-occurrence: two case reports and a review of the literature.

    Science.gov (United States)

    Bjørsum-Meyer, Thomas; Herlin, Morten; Qvist, Niels; Petersen, Michael B

    2016-12-21

    The vertebral defect, anal atresia, cardiac defect, tracheoesophageal fistula/esophageal atresia, renal defect, and limb defect association and Mayer-Rokitansky-Küster-Hauser syndrome are rare conditions. We aimed to present two cases with the vertebral defect, anal atresia, cardiac defect, tracheoesophageal fistula/esophageal atresia, renal defect, and limb defect association and Mayer-Rokitansky-Küster-Hauser co-occurrence from our local surgical center and through a systematic literature search detect published cases. Furthermore, we aimed to collect existing knowledge in the embryopathogenesis and genetics in order to discuss a possible link between the vertebral defect, anal atresia, cardiac defect, tracheoesophageal fistula/esophageal atresia, renal defect, and limb defect association and Mayer-Rokitansky-Küster-Hauser syndrome. Our first case was a white girl delivered by caesarean section at 37 weeks of gestation; our second case was a white girl born at a gestational age of 40 weeks. A co-occurrence of vertebral defect, anal atresia, cardiac defect, tracheoesophageal fistula/esophageal atresia, renal defect, and limb defect association and Mayer-Rokitansky-Küster-Hauser syndrome was diagnosed in both cases. We performed a systematic literature search in PubMed ((VACTERL) OR (VATER)) AND ((MRKH) OR (Mayer-Rokitansky-Küster-Hauser) OR (mullerian agenesis) OR (mullerian aplasia) OR (MURCS)) without limitations. A similar search was performed in Embase and the Cochrane library. We added two cases from our local center. All cases (n = 9) presented with anal atresia and renal defect. Vertebral defects were present in eight patients. Rectovestibular fistula was confirmed in seven patients. Along with the uterovaginal agenesis, fallopian tube aplasia appeared in five of nine cases and in two cases ovarian involvement also existed. The co-occurrence of the vertebral defect, anal atresia, cardiac defect, tracheoesophageal fistula/esophageal atresia, renal

  13. Density Functional Theory Study on Defect Feature of AsGaGaAs in Gallium Arsenide

    Directory of Open Access Journals (Sweden)

    Deming Ma

    2015-01-01

    Full Text Available We investigate the defect feature of AsGaGaAs defect in gallium arsenide clusters in detail by using first-principles calculations based on the density functional theory (DFT. Our calculations reveal that the lowest donor level of AsGaGaAs defect on the gallium arsenide crystal surface is 0.85 eV below the conduction band minimum, while the lowest donor level of the AsGaGaAs defect inside the gallium arsenide bulk is 0.83 eV below the bottom of the conduction band, consistent with gallium arsenide EL2 defect level of experimental value (Ec-0.82 eV. This suggests that AsGaGaAs defect is one of the possible gallium arsenide EL2 deep-level defects. Moreover, our results also indicate that the formation energies of internal AsGaGaAs and surface AsGaGaAs defects are predicted to be around 2.36 eV and 5.54 eV, respectively. This implies that formation of AsGaGaAs defect within the crystal is easier than that of surface. Our results offer assistance in discussing the structure of gallium arsenide deep-level defect and its effect on the material.

  14. Genetic diversity and population structure of Iranian wild Pleurotus eryngii species-complex strains revealed by URP-PCR markers

    NARCIS (Netherlands)

    Behnamian, Mahdi; Mohammadi, Seyed A.; Sonnenberg, A.S.M.; Goltapeh, Ebrahim M.; Hendrickx, P.M.

    2010-01-01

    In the present study, a set of 68 P. eryngii wild strains collected from nine locations in northwest and west of Iran along with six commercial strains were studied using universal rice primers (URP). The wild strains were isolated from Ferula ovina, F. haussknechtii, Cachrys ferulacea, Kellusia

  15. Strain path and work-hardening behavior of brass

    International Nuclear Information System (INIS)

    Sakharova, N.A.; Fernandes, J.V.; Vieira, M.F.

    2009-01-01

    Plastic straining in metal forming usually includes changes of strain path, which are frequently not taken into account in the analysis of forming processes. Moreover, strain path change can significantly affect the mechanical behavior and microstructural evolution of the material. For this reason, a combination of several simple loading test sequences is an effective way to investigate the dislocation microstructure of sheet metals under such forming conditions. Pure tension and rolling strain paths and rolling-tension strain path sequences were performed on brass sheets. A study of mechanical behavior and microstructural evolution during the simple and the complex strain paths was carried out, within a wide range of strain values. The appearance and development of deformation twinning was evident. It was shown that strain path change promotes the onset of premature twinning. The work-hardening behavior is discussed in terms of the twinning and dislocation microstructure evolution, as revealed by transmission electron microscopy

  16. Diffusive, Structural, Optical, and Electrical Properties of Defects in Semiconductors

    CERN Multimedia

    Wagner, F E

    2002-01-01

    Electronic properties of semiconductors are extremely sensitive to defects and impurities that have localized electronic states with energy levels in the band gap of the semiconductor. Spectroscopic techniques like photoluminescence (PL), deep level transient spectroscopy (DLTS), or Hall effect, that are able to detect and characterize band gap states do not reveal direct information about their microscopic origin. To overcome this chemical "blindness", the present approach is to use radioactive isotopes as a tracer. Moreover, the recoil energies involved in $\\beta$ and $\\gamma$-decays can be used to create intrinsic isolated point defects (interstitials, vacancies) in a controlled way. A microscopic insight into the structure and the thermodynamic properties of complexes formed by interacting defects can be gained by detecting the hyperfine interaction between the nuclear moments of radioactive dopants and the electromagnetic fields present at the site of the radioactive nucleus. The understanding and the co...

  17. ILT based defect simulation of inspection images accurately predicts mask defect printability on wafer

    Science.gov (United States)

    Deep, Prakash; Paninjath, Sankaranarayanan; Pereira, Mark; Buck, Peter

    2016-05-01

    At advanced technology nodes mask complexity has been increased because of large-scale use of resolution enhancement technologies (RET) which includes Optical Proximity Correction (OPC), Inverse Lithography Technology (ILT) and Source Mask Optimization (SMO). The number of defects detected during inspection of such mask increased drastically and differentiation of critical and non-critical defects are more challenging, complex and time consuming. Because of significant defectivity of EUVL masks and non-availability of actinic inspection, it is important and also challenging to predict the criticality of defects for printability on wafer. This is one of the significant barriers for the adoption of EUVL for semiconductor manufacturing. Techniques to decide criticality of defects from images captured using non actinic inspection images is desired till actinic inspection is not available. High resolution inspection of photomask images detects many defects which are used for process and mask qualification. Repairing all defects is not practical and probably not required, however it's imperative to know which defects are severe enough to impact wafer before repair. Additionally, wafer printability check is always desired after repairing a defect. AIMSTM review is the industry standard for this, however doing AIMSTM review for all defects is expensive and very time consuming. Fast, accurate and an economical mechanism is desired which can predict defect printability on wafer accurately and quickly from images captured using high resolution inspection machine. Predicting defect printability from such images is challenging due to the fact that the high resolution images do not correlate with actual mask contours. The challenge is increased due to use of different optical condition during inspection other than actual scanner condition, and defects found in such images do not have correlation with actual impact on wafer. Our automated defect simulation tool predicts

  18. Risk assessment for pipelines with active defects based on artificial intelligence methods

    Energy Technology Data Exchange (ETDEWEB)

    Anghel, Calin I. [Department of Chemical Engineering, Faculty of Chemistry and Chemical Engineering, University ' Babes-Bolyai' , Cluj-Napoca (Romania)], E-mail: canghel@chem.ubbcluj.ro

    2009-07-15

    The paper provides another insight into the pipeline risk assessment for in-service pressure piping containing defects. Beside of the traditional analytical approximation methods or sampling-based methods safety index and failure probability of pressure piping containing defects will be obtained based on a novel type of support vector machine developed in a minimax manner. The safety index or failure probability is carried out based on a binary classification approach. The procedure named classification reliability procedure, involving a link between artificial intelligence and reliability methods was developed as a user-friendly computer program in MATLAB language. To reveal the capacity of the proposed procedure two comparative numerical examples replicating a previous related work and predicting the failure probabilities of pressured pipeline with defects were presented.

  19. Risk assessment for pipelines with active defects based on artificial intelligence methods

    International Nuclear Information System (INIS)

    Anghel, Calin I.

    2009-01-01

    The paper provides another insight into the pipeline risk assessment for in-service pressure piping containing defects. Beside of the traditional analytical approximation methods or sampling-based methods safety index and failure probability of pressure piping containing defects will be obtained based on a novel type of support vector machine developed in a minimax manner. The safety index or failure probability is carried out based on a binary classification approach. The procedure named classification reliability procedure, involving a link between artificial intelligence and reliability methods was developed as a user-friendly computer program in MATLAB language. To reveal the capacity of the proposed procedure two comparative numerical examples replicating a previous related work and predicting the failure probabilities of pressured pipeline with defects were presented.

  20. Packing defects into ordered structures

    DEFF Research Database (Denmark)

    Bechstein, R.; Kristoffersen, Henrik Høgh; Vilhelmsen, L.B.

    2012-01-01

    . With the help of density functional theory calculations we develop a complete structural model for the entire strand and demonstrate these adstructures to be more stable than an equivalent amount of bulk defects such as Ti interstitials. We argue that strands can form particularly easy on stepped surfaces......We have studied vicinal TiO2(110) surfaces by high-resolution scanning tunneling microscopy and density functional theory calculations. On TiO2 surfaces characterized by a high density of ⟨11̅ 1⟩ steps, scanning tunneling microscopy reveals a high density of oxygen-deficient strandlike adstructures...

  1. Defect detection based on extreme edge of defective region histogram

    Directory of Open Access Journals (Sweden)

    Zouhir Wakaf

    2018-01-01

    Full Text Available Automatic thresholding has been used by many applications in image processing and pattern recognition systems. Specific attention was given during inspection for quality control purposes in various industries like steel processing and textile manufacturing. Automatic thresholding problem has been addressed well by the commonly used Otsu method, which provides suitable results for thresholding images based on a histogram of bimodal distribution. However, the Otsu method fails when the histogram is unimodal or close to unimodal. Defects have different shapes and sizes, ranging from very small to large. The gray-level distributions of the image histogram can vary between unimodal and multimodal. Furthermore, Otsu-revised methods, like the valley-emphasis method and the background histogram mode extents, which overcome the drawbacks of the Otsu method, require preprocessing steps and fail to use the general threshold for multimodal defects. This study proposes a new automatic thresholding algorithm based on the acquisition of the defective region histogram and the selection of its extreme edge as the threshold value to segment all defective objects in the foreground from the image background. To evaluate the proposed defect-detection method, common standard images for experimentation were used. Experimental results of the proposed method show that the proposed method outperforms the current methods in terms of defect detection.

  2. Clinical Trichophyton rubrum Strain Exhibiting Primary Resistance to Terbinafine

    Science.gov (United States)

    Mukherjee, Pranab K.; Leidich, Steven D.; Isham, Nancy; Leitner, Ingrid; Ryder, Neil S.; Ghannoum, Mahmoud A.

    2003-01-01

    The in vitro antifungal susceptibilities of six clinical Trichophyton rubrum isolates obtained sequentially from a single onychomycosis patient who failed oral terbinafine therapy (250 mg/day for 24 weeks) were determined by broth microdilution and macrodilution methodologies. Strain relatedness was examined by random amplified polymorphic DNA (RAPD) analyses. Data obtained from both broth micro- and macrodilution assays were in agreement and revealed that the six clinical isolates had greatly reduced susceptibilities to terbinafine. The MICs of terbinafine for these strains were >4 μg/ml, whereas they were terbinafine for all six strains were >128 μg/ml, whereas they were 0.0002 μg/ml for the reference strain. The MIC of terbinafine for the baseline strain (cultured at the initial screening visit and before therapy was started) was already 4,000-fold higher than normal, suggesting that this is a case of primary resistance to terbinafine. The results obtained by the broth macrodilution procedure revealed that the terbinafine MICs and MFCs for sequential isolates apparently increased during the course of therapy. RAPD analyses did not reveal any differences between the isolates. The terbinafine-resistant isolates exhibited normal susceptibilities to clinically available antimycotics including itraconazole, fluconazole, and griseofulvin. However, these isolates were fully cross resistant to several other known squalene epoxidase inhibitors, including naftifine, butenafine, tolnaftate, and tolciclate, suggesting a target-specific mechanism of resistance. This is the first confirmed report of terbinafine resistance in dermatophytes. PMID:12499173

  3. The effects of strain relaxation on the dielectric properties of epitaxial ferroelectric Pb(Zr0.2Ti0.8)TiO3 thin films

    Science.gov (United States)

    Khan, Asif Islam; Yu, Pu; Trassin, Morgan; Lee, Michelle J.; You, Long; Salahuddin, Sayeef

    2014-07-01

    We study the effects of strain relaxation on the dielectric properties of epitaxial 40 nm Pb(Zr0.2Ti0.8)TiO3 (PZT) films. A significant increase in the defect and dislocation density due to strain relaxation is observed in PZT films with tetragonality c/a fatigue in ferroelectric materials.

  4. N{sup +} ion-implantation-induced defects in ZnO studied with a slow positron beam

    Energy Technology Data Exchange (ETDEWEB)

    Chen, Z Q [Japan Atomic Energy Research Institute, 1233 Watanuki, Takasaki, Gunma 370-1292, Japan (Japan); Sekiguchi, T [Nanomaterials Laboratory, National Institute for Materials Science, 1-2-1 Sengen, Tsukuba, Ibaraki 305-0047 (Japan); Yuan, X L [Nanomaterials Laboratory, National Institute for Materials Science, 1-2-1 Sengen, Tsukuba, Ibaraki 305-0047 (Japan); Maekawa, M [Japan Atomic Energy Research Institute, 1233 Watanuki, Takasaki, Gunma 370-1292, Japan (Japan); Kawasuso, A [Japan Atomic Energy Research Institute, 1233 Watanuki, Takasaki, Gunma 370-1292, Japan (Japan)

    2004-01-21

    Undoped ZnO single crystals were implanted with multiple-energy N{sup +} ions ranging from 50 to 380 keV with doses from 10{sup 12} to 10{sup 14} cm{sup -2}. Positron annihilation measurements show that vacancy defects are introduced in the implanted layers. The concentration of the vacancy defects increases with increasing ion dose. The annealing behaviour of the defects can be divided into four stages, which correspond to the formation and recovery of large vacancy clusters and the formation and disappearance of vacancy-impurity complexes, respectively. All the implantation-induced defects are removed by annealing at 1200 deg. C. Cathodoluminescence measurements show that the ion-implantation-induced defects act as nonradiative recombination centres to suppress the ultraviolet (UV) emission. After annealing, these defects disappear gradually and the UV emission reappears, which coincides with positron annihilation measurements. Hall measurements reveal that after N{sup +} implantation, the ZnO layer still shows n-type conductivity.

  5. Dechanneling measurements of defect depth profiles and effective cross-channel distribution of misaligned atoms in ion irradiated gold

    International Nuclear Information System (INIS)

    Pronko, P.P.

    1975-01-01

    Defect depth profiles for self ion and He + irradiated gold are obtained from single and multiple scatter dechanneling analysis in single crystal gold films. Quantitative defect densities are obtained through use of atomic scattering cross sections. Integral damage profiles are extracted from the dechanneling spectra and subsequently differentiated to yield the volume concentration of defects as a function of depth. Results from the self ion irradiations suggest that incident ions produce defect distributions across depths much greater than predicted by random stopping theory. This is in agreement with TEM observations of others. Comparison of the experimental profiles is made with theoretical vacancy distributions predicted by defect diffusion in a radiation environment. Similarities are observed for the low fluence irradiations suggesting that profile characteristics may be controlled by rapid migration and loss of interstitials to the film surfaces during irradiation. Information on the across-channel distribution of misaligned atoms in the damaged films is obtained with the steady increase of transverse energy model applied to the dechanneling spectra. A predominance of slight misalignment is observed with no contribution to dechanneling coming from atoms displaced significantly close to the center of the channels. This is in keeping with what is expected for crystal distortions caused by the strain fields associated with vacancy cluster defects

  6. Dechanneling measurements of defect depth profiles and effective cross-channel distribution of misaligned atoms in ion-irradiated gold

    International Nuclear Information System (INIS)

    Pronko, P.P.

    1976-01-01

    Defect depth profiles for self-ion and He + irradiated gold are obtained from single and multiple scatter dechanneling analysis in single-crystal gold films. Quantitative defect densities are obtained through use of atomic-scattering cross sections. Integral damage profiles are extracted from the dechanneling spectra and subsequently differentiated to yield the volume concentration of defects as a function of depth. Results from the self-ion irradiations suggest that incident ions produce defect distributions across depths much greater than predicted by random stopping theory. This is in agreement with TEM observations of others. Comparison of the experimental profiles is made with theoretical vacancy distributions predicted by defect diffusion in a radiation environment. Similarities are observed for the low-fluence irradiations, suggesting that profile characteristics may be controlled by rapid migration and loss of interstitials to the film surfaces during irradiation. Information on the across-channel distribution of misaligned atoms in the damaged films is obtained with the steady increase of transverse energy model. A predominance of slight misalignment is observed with no contribution to dechanneling coming from atoms displaced significantly close to the center of the channels. This is in keeping with what is expected for crystal distortions caused by the strain fields associated with vacancy cluster defects. (Auth.)

  7. Morphological characterization and molecular fingerprinting of Nostoc strains by multiplex RAPD.

    Science.gov (United States)

    Hillol, Chakdar; Pabbi, Sunil

    2012-01-01

    Morphological parameters studied for the twenty selected Nostoc strains were mostly found to be consistent with the earlier reports. But the shape of akinetes observed in this study was a little deviation from the existing descriptions and heterocyst frequency was also found to be different in different strains in spite of growing in the same nitrogen free media. Multiplex RAPD produced reproducible and completely polymorphic amplification profiles for all the strains including some strain specific unique bands which are intended to be useful for identification of those strains. At least one to a maximum of two unique bands was produced by different dual primer combinations. For ten strains out of twenty, strain specific bands were found to be generated. Cluster analysis revealed a vast heterogeneity among these Nostoc strains and no specific clustering based on geographical origin was found except a few strains. It was also observed that morphological data may not necessarily correspond to the genetic data in most of the cases. CCC92 (Nostoc muscorum) and CCC48 (Nostoc punctiforme) showed a high degree of similarity which was well supported by high bootstrap value. The level of similarity of the strains ranged from 0.15 to 0.94. Cluster analysis based on multiplex RAPD showed a good fit revealing the discriminatory power of this technique.

  8. Intraspecies diversity of Lactobacillus sakei response to oxidative stress and variability of strain performance in mixed strains challenges.

    Science.gov (United States)

    Guilbaud, Morgan; Zagorec, Monique; Chaillou, Stéphane; Champomier-Vergès, Marie-Christine

    2012-04-01

    Lactobacillus sakei is a meat-borne lactic acid bacterium species exhibiting a wide genomic diversity. We have investigated the diversity of response to various oxidative compounds, between L. sakei strains, among a collection representing the genomic diversity. We observed various responses to the different compounds as well as a diversity of response depending on the aeration conditions used for cell growth. A principal component analysis revealed two main phenotypic groups, partially correlating with previously described genomic clusters. We designed strains mixes composed of three different strains, in order to examine the behavior of each strain, when cultured alone or in the presence of other strains. The strains composing the mixtures were chosen as diverse as possible, i.e. exhibiting diverse responses to oxidative stress and belonging to different genomic clusters. Growth and survival rates of each strain were monitored under various aeration conditions, with or without heme supplementation. The results obtained suggest that some strains may act as "helper" or "burden" strains depending on the oxidative conditions encountered during incubation. This study confirms that resistance to oxidative stress is extremely variable within the L. sakei species and that this property should be considered when investigating starter performance in the complex meat bacterial ecosystems. Copyright © 2011 Elsevier Ltd. All rights reserved.

  9. Yersinia enterocolitica YopH-Deficient Strain Activates Neutrophil Recruitment to Peyer's Patches and Promotes Clearance of the Virulent Strain.

    Science.gov (United States)

    Dave, Mabel N; Silva, Juan E; Eliçabe, Ricardo J; Jeréz, María B; Filippa, Verónica P; Gorlino, Carolina V; Autenrieth, Stella; Autenrieth, Ingo B; Di Genaro, María S

    2016-11-01

    Yersinia enterocolitica evades the immune response by injecting Yersinia outer proteins (Yops) into the cytosol of host cells. YopH is a tyrosine phosphatase critical for Yersinia virulence. However, the mucosal immune mechanisms subverted by YopH during in vivo orogastric infection with Y. enterocolitica remain elusive. The results of this study revealed neutrophil recruitment to Peyer's patches (PP) after infection with a YopH-deficient mutant strain (Y. enterocolitica ΔyopH). While the Y. enterocolitica wild-type (WT) strain in PP induced the major neutrophil chemoattractant CXCL1 mRNA and protein levels, infection with the Y. enterocolitica ΔyopH mutant strain exhibited a higher expression of the CXCL1 receptor, CXCR2, in blood neutrophils, leading to efficient neutrophil recruitment to the PP. In contrast, migration of neutrophils into PP was impaired upon infection with Y. enterocolitica WT strain. In vitro infection of blood neutrophils revealed the involvement of YopH in CXCR2 expression. Depletion of neutrophils during Y. enterocolitica ΔyopH infection raised the bacterial load in PP. Moreover, the clearance of WT Y. enterocolitica was improved when an equal mixture of Y. enterocolitica WT and Y. enterocolitica ΔyopH strains was used in infecting the mice. This study indicates that Y. enterocolitica prevents early neutrophil recruitment in the intestine and that the effector protein YopH plays an important role in the immune evasion mechanism. The findings highlight the potential use of the Y. enterocolitica YopH-deficient strain as an oral vaccine carrier. Copyright © 2016, American Society for Microbiology. All Rights Reserved.

  10. Synthetic Defects for Vibrothermography

    Science.gov (United States)

    Renshaw, Jeremy; Holland, Stephen D.; Thompson, R. Bruce; Eisenmann, David J.

    2010-02-01

    Synthetic defects are an important tool used for characterizing the performance of nondestructive evaluation techniques. Viscous material-filled synthetic defects were developed for use in vibrothermography (also known as sonic IR) as a tool to improve inspection accuracy and reliability. This paper describes how the heat-generation response of these VMF synthetic defects is similar to the response of real defects. It also shows how VMF defects can be applied to improve inspection accuracy for complex industrial parts and presents a study of their application in an aircraft engine stator vane.

  11. The effect of temperature on primary defect formation in Ni–Fe alloy

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Chengbin, E-mail: wangchengbin@sinap.ac.cn [Key Laboratory of Interfacial Physics and Technology, Chinese Academy of Sciences, Shanghai 201800 (China); Zhang, Wei; Ren, Cuilan [Key Laboratory of Interfacial Physics and Technology, Chinese Academy of Sciences, Shanghai 201800 (China); Huai, Ping [Key Laboratory of Nuclear Radiation and Nuclear Energy Technology, Chinese Academy of Sciences, Shanghai 201800 (China); Zhu, Zhiyuan [Key Laboratory of Interfacial Physics and Technology, Chinese Academy of Sciences, Shanghai 201800 (China)

    2014-02-15

    Molecular dynamics (MD) simulations have been used to study the influence of temperature on defect generation and evolution in nickel and Ni–Fe alloy (with 15% and 50% Fe content) with a 10-keV primary knock-on atom (PKA) at six different temperatures from 0 to 1500 K. The recently available Ni–Fe potential is used with its repulsive part modified by Vörtler. The temporal evolution and temperature dependence of stable defect formation and in-cascade clustering processes are analysed. The number of stable defect and the interstitial clustering fraction are found to increase with temperature whereas the vacancy clustering fraction decreases with temperature. The alloy composition dependence of the stable defect number is also found for the PKA energy considered here. Additionally, a study of the temperature influence on the cluster size distribution is performed, revealing a systematic change in the cluster size distributions, with higher temperature cascades producing larger interstitial clusters.

  12. Defect-Induced Hedgehog Polarization States in Multiferroics

    Science.gov (United States)

    Li, Linze; Cheng, Xiaoxing; Jokisaari, Jacob R.; Gao, Peng; Britson, Jason; Adamo, Carolina; Heikes, Colin; Schlom, Darrell G.; Chen, Long-Qing; Pan, Xiaoqing

    2018-03-01

    Continuous developments in nanotechnology require new approaches to materials synthesis that can produce novel functional structures. Here, we show that nanoscale defects, such as nonstoichiometric nanoregions (NSNRs), can act as nano-building blocks for creating complex electrical polarization structures in the prototypical multiferroic BiFeO3 . An array of charged NSNRs are produced in BiFeO3 thin films by tuning the substrate temperature during film growth. Atomic-scale scanning transmission electron microscopy imaging reveals exotic polarization rotation patterns around these NSNRs. These polarization patterns resemble hedgehog or vortex topologies and can cause local changes in lattice symmetries leading to mixed-phase structures resembling the morphotropic phase boundary with high piezoelectricity. Phase-field simulations indicate that the observed polarization configurations are mainly induced by charged states at the NSNRs. Engineering defects thus may provide a new route for developing ferroelectric- or multiferroic-based nanodevices.

  13. Healing parameters in a rabbit partial tendon defect following tenocyte/biomaterial implantation.

    Science.gov (United States)

    Stoll, Christiane; John, Thilo; Conrad, Claudia; Lohan, Anke; Hondke, Sylvia; Ertel, Wolfgang; Kaps, Christian; Endres, Michaela; Sittinger, Michael; Ringe, Jochen; Schulze-Tanzil, G

    2011-07-01

    Although rabbits are commonly used as tendon repair model, interpretative tools are divergent and comprehensive scoring systems are lacking. Hence, the aim was to develop a multifaceted scoring system to characterize healing in a partial Achilles tendon defect model. A 3 mm diameter defect was created in the midsubstance of the medial M. gastrocnemius tendon, which remained untreated or was filled with a polyglycolic-acid (PGA) scaffold + fibrin and either left cell-free or seeded with Achilles tenocytes. After 6 and 12 weeks, tendon repair was assessed macroscopically and histologically using self-constructed scores. Macroscopical scoring revealed superior results in the tenocyte seeded PGA + fibrin group compared with the controls at both time points. Histology of all operated tendons after 6 weeks proved extracellular matrix (ECM) disorganization, hypercellularity and occurrence of irregular running elastic fibres with no significance between the groups. Some inflammation was associated with PGA implantation and increased sulphated proteoglycan deposition predominantly with the empty defects. After 12 weeks defect areas became hard to recognize and differences between groups, except for the increased sulphated proteoglycans content in the empty defects, were almost nullified. We describe a partial Achilles tendon defect model and versatile scoring tools applicable for characterizing biomaterial-supported tendon healing. Copyright © 2011 Elsevier Ltd. All rights reserved.

  14. Strain-accelerated dynamics of soft colloidal glasses

    KAUST Repository

    Agarwal, Praveen

    2011-04-11

    We have investigated strain-accelerated dynamics of soft glasses theoretically and experimentally. Mechanical rheology measurements performed on a variety of systems reveal evidence for the speeding-up of relaxation at modest shear strains in both step and oscillatory shear flows. Using the soft glassy rheology (SGR) model framework, we show that the observed behavior is a fundamental, but heretofore unexplored attribute of soft glasses. © 2011 American Physical Society.

  15. Digital volume tomography in the diagnosis of peri-implant defects: an in vitro study on native pig mandibles.

    Science.gov (United States)

    Mengel, Reiner; Kruse, Björn; Flores-de-Jacoby, Lavin

    2006-07-01

    The aim of this study of native pig mandibles was to investigate the accuracy and quality of the representation of peri-implant defects by intraoral radiography (IR), panoramic radiography (PR), computer tomography (CT), and digital volume tomography (DVT). The examination was carried out on 19 native pig mandibles. In the toothless sections of the mandibles, one or two implants were inserted. Following the standardized preparation of peri-implant defects (11 each of dehiscences, fenestrations, and 2- to 3-walled intrabony defects), IR, PR, CT, and DVT were performed. The peri-implant defects were measured using appropriate software on the digitized IR and PR image programs. As a control method, the peri-implant bone defects were measured directly using a reflecting stereomicroscope with measuring ocular. The statistical comparison between the measurements of the radiographic scans and those of the direct readings of the peri-implant defects was performed with Pearson's correlation coefficient. The quality of the radiographic scans was determined through the subjective perception and detectability of the peri-implant defects by five independent observers. In the DVT and CT scans, it was possible to measure all the bone defects in three planes. Comparison with the direct peri-implant defect measurements yielded a mean deviation of 0.17+/-0.11 mm for the DVT scans and 0.18+/-0.12 mm for the CT scans. On the IR and PR images, the defects could be detected only in the mesio-distal and cranio-caudal planes. In comparison with the direct measurements of the peri-implant defects, the IR images revealed a mean deviation of 0.34+/-0.30 mm, and the PR images revealed a mean deviation of 0.41+/-0.35 mm. The quality rating of the radiographic images was highest for the DVT scans. Overall, the CT and DVT scans displayed only a slight deviation in the extent of the peri-implant defects. Both radiographic imaging techniques permitted imaging of peri-implant defects in three

  16. Different distribution patterns of ten virulence genes in Legionella reference strains and strains isolated from environmental water and patients.

    Science.gov (United States)

    Zhan, Xiao-Yong; Hu, Chao-Hui; Zhu, Qing-Yi

    2016-04-01

    Virulence genes are distinct regions of DNA which are present in the genome of pathogenic bacteria and absent in nonpathogenic strains of the same or related species. Virulence genes are frequently associated with bacterial pathogenicity in genus Legionella. In the present study, an assay was performed to detect ten virulence genes, including iraA, iraB, lvrA, lvrB, lvhD, cpxR, cpxA, dotA, icmC and icmD in different pathogenicity islands of 47 Legionella reference strains, 235 environmental strains isolated from water, and 4 clinical strains isolated from the lung tissue of pneumonia patients. The distribution frequencies of these genes in reference or/and environmental L. pneumophila strains were much higher than those in reference non-L. pneumophila or/and environmental non-L. pneumophila strains, respectively. L. pneumophila clinical strains also maintained higher frequencies of these genes compared to four other types of Legionella strains. Distribution frequencies of these genes in reference L. pneumophila strains were similar to those in environmental L. pneumophila strains. In contrast, environmental non-L. pneumophila maintained higher frequencies of these genes compared to those found in reference non-L. pneumophila strains. This study illustrates the association of virulence genes with Legionella pathogenicity and reveals the possible virulence evolution of non-L. pneumophia strains isolated from environmental water.

  17. Random transposon mutagenesis of the Saccharopolyspora erythraea genome reveals additional genes influencing erythromycin biosynthesis

    Science.gov (United States)

    Fedashchin, Andrij; Cernota, William H.; Gonzalez, Melissa C.; Leach, Benjamin I.; Kwan, Noelle; Wesley, Roy K.; Weber, J. Mark

    2015-01-01

    A single cycle of strain improvement was performed in Saccharopolyspora erythraea mutB and 15 genotypes influencing erythromycin production were found. Genotypes generated by transposon mutagenesis appeared in the screen at a frequency of ∼3%. Mutations affecting central metabolism and regulatory genes were found, as well as hydrolases, peptidases, glycosyl transferases and unknown genes. Only one mutant retained high erythromycin production when scaled-up from micro-agar plug fermentations to shake flasks. This mutant had a knockout of the cwh1 gene (SACE_1598), encoding a cell-wall-associated hydrolase. The cwh1 knockout produced visible growth and morphological defects on solid medium. This study demonstrated that random transposon mutagenesis uncovers strain improvement-related genes potentially useful for strain engineering. PMID:26468041

  18. Determination of Burst Pressure of API Steel Pipes using Stress Modified Critical Strain Model

    International Nuclear Information System (INIS)

    Alang, N A; Razak, N A; Sulaiman, A S

    2012-01-01

    This paper presents a technique which can be used to determine the burst pressure of defective steel pipes using non-linear finite element (FE) analysis. The technique uses stress modified critical strain (SMCS) failure criterion to study the effect of gouge defects on maximum working pressure of API X65 steel pipes. The procedures in determining the model parameters using 3-D, homogeneous isotropic elastic-plastic material model with large deformation finite element analyses from notched tensile bars were systematically discussed. The relationship between burst pressure and gouge depth was proposed. The burst pressure estimated then was compared to experimental data from the literature for validation showing overall good agreements.

  19. Genomic and gene variation in Mycoplasma hominis strains

    DEFF Research Database (Denmark)

    Christiansen, Gunna; Andersen, H; Birkelund, Svend

    1987-01-01

    DNAs from 14 strains of Mycoplasma hominis isolated from various habitats, including strain PG21, were analyzed for genomic heterogeneity. DNA-DNA filter hybridization values were from 51 to 91%. Restriction endonuclease digestion patterns, analyzed by agarose gel electrophoresis, revealed...... no identity or cluster formation between strains. Variation within M. hominis rRNA genes was analyzed by Southern hybridization of EcoRI-cleaved DNA hybridized with a cloned fragment of the rRNA gene from the mycoplasma strain PG50. Five of the M. hominis strains showed identical hybridization patterns....... These hybridization patterns were compared with those of 12 other mycoplasma species, which showed a much more complex band pattern. Cloned nonribosomal RNA gene fragments of M. hominis PG21 DNA were analyzed, and the fragments were used to demonstrate heterogeneity among the strains. A monoclonal antibody against...

  20. A DFT study of Cu nanoparticles adsorbed on defective graphene

    International Nuclear Information System (INIS)

    García-Rodríguez, D.E.; Mendoza-Huizar, L.H.; Díaz, C.

    2017-01-01

    Highlights: • Cu_n supported on graphene may be a promising electrode material for DBFC's cells. • Cu_n/graphene interaction is rather local and size independent. • Cu_1_3 anchors strongly to defects in graphene, while keeping its gas-phase properties. - Abstract: Metal nanoparticles adsorbed on graphene are systems of interest for processes relative to catalytic reactions and alternative energy production. Graphene decorated with Cu-nanoparticles, in particular, could be a good alternative material for electrodes in direct borohydride fuel cells. However our knowledge of this system is still very limited. Based on density functional theory, we have analyzed the interaction of Cu_n nanoparticles (n = 4, 5, 6, 7, 13) with pristine and defective-graphene. We have considered two types of defects, a single vacancy (SV), and an extended lineal structural defect (ELSD), formed by heptagon-pentagon pairs. Our analysis has revealed the covalent character of the Cu_n-graphene interaction for pristine- and ELSD-graphene, and a more ionic-like interaction for SV-graphene. Furthermore, our analysis shows that the interaction between the nanoparticles and the graphene is rather local, i.e., only the nanoparticle atoms close to the contact region are involved in the interaction, being the electronic contact region much higher for defective-graphene than for pristine-graphene. Thus, the higher the particle the lower its average electronic and structural distortion.

  1. Bordetella pertussis pertactin knock-out strains reveal immunomodulatory properties of this virulence factor.

    NARCIS (Netherlands)

    Hovingh, Elise Sofie; Mariman, Rob; Solans, Luis; Hijdra, Daniëlle; Hamstra, Hendrik-Jan; Jongerius, Ilse; van Gent, Marjolein; Mooi, Frits; Locht, Camille; Pinelli, Elena

    2018-01-01

    Whooping cough, caused by Bordetella pertussis, has resurged and presents a global health burden worldwide. B. pertussis strains unable to produce the acellular pertussis vaccine component pertactin (Prn), have been emerging and in some countries represent up to 95% of recent clinical isolates.

  2. Detection and quantification of creep strain using process compensated resonance testing (PCRT) sorting modules trained with modeled resonance spectra

    Science.gov (United States)

    Heffernan, Julieanne; Biedermann, Eric; Mayes, Alexander; Livings, Richard; Jauriqui, Leanne; Goodlet, Brent; Aldrin, John C.; Mazdiyasni, Siamack

    2018-04-01

    Process Compensated Resonant Testing (PCRT) is a full-body nondestructive testing (NDT) method that measures the resonance frequencies of a part and correlates them to the part's material and/or damage state. PCRT testing is used in the automotive, aerospace, and power generation industries via automated PASS/FAIL inspections to distinguish parts with nominal process variation from those with the defect(s) of interest. Traditional PCRT tests are created through the statistical analysis of populations of "good" and "bad" parts. However, gathering a statistically significant number of parts can be costly and time-consuming, and the availability of defective parts may be limited. This work uses virtual databases of good and bad parts to create two targeted PCRT inspections for single crystal (SX) nickel-based superalloy turbine blades. Using finite element (FE) models, populations were modeled to include variations in geometric dimensions, material properties, crystallographic orientation, and creep damage. Model results were verified by comparing the frequency variation in the modeled populations with the measured frequency variations of several physical blade populations. Additionally, creep modeling results were verified through the experimental evaluation of coupon geometries. A virtual database of resonance spectra was created from the model data. The virtual database was used to create PCRT inspections to detect crystallographic defects and creep strain. Quantification of creep strain values using the PCRT inspection results was also demonstrated.

  3. Synergistic effects of interstitial impurities and radiation defects on mechanical characteristics of ferritic steels

    International Nuclear Information System (INIS)

    Charit, I.; Seok, C.S.; Murty, K.L.

    2007-01-01

    Ferritic steels are generally used in pressure vessels and various reactor support structures in light water reactors. They are known to exhibit radiation embrittlement in terms of decreased toughness and increased ductile-brittle transition temperature as a result of exposure to neutron radiation. The superimposed effects of strain aging due to interstitial impurity atoms on radiation embrittlement were considered first by Wechsler, Hall and others. Here we summarize some of our efforts on the investigation of synergistic effects between interstitial impurity atoms (IIAs) and radiation-induced point defects, which result in interesting effects at appropriate temperature and strain rate conditions. Two materials, a mild steel and a pressure vessel steel (A516 Gr.70), are evaluated using tensile and three-point bend tests

  4. Atomic-scale structure and properties of highly stable antiphase boundary defects in Fe3O4.

    Science.gov (United States)

    McKenna, Keith P; Hofer, Florian; Gilks, Daniel; Lazarov, Vlado K; Chen, Chunlin; Wang, Zhongchang; Ikuhara, Yuichi

    2014-12-10

    The complex and intriguing properties of the ferrimagnetic half metal magnetite (Fe 3 O 4 ) are of continuing fundamental interest as well as being important for practical applications in spintronics, magnetism, catalysis and medicine. There is considerable speculation concerning the role of the ubiquitous antiphase boundary (APB) defects in magnetite, however, direct information on their structure and properties has remained challenging to obtain. Here we combine predictive first principles modelling with high-resolution transmission electron microscopy to unambiguously determine the three-dimensional structure of APBs in magnetite. We demonstrate that APB defects on the {110} planes are unusually stable and induce antiferromagnetic coupling between adjacent domains providing an explanation for the magnetoresistance and reduced spin polarization often observed. We also demonstrate how the high stability of the {110} APB defects is connected to the existence of a metastable bulk phase of Fe 3 O 4 , which could be stabilized by strain in films or nanostructures.

  5. Detection of defects in electron-irradiated synthetic silica quartz probed by positron annihilation

    International Nuclear Information System (INIS)

    Watauchi, Satoshi; Uedono, Akira; Ujihira, Yusuke; Yoda, Osamu.

    1994-01-01

    Defects in amorphous SiO 2 films, formed on MOS(metal/oxide/semiconductor) devices as gates, perturb its operation. The positron annihilation techniques, were applied to the study of the annealing behavior of the defects, introduced in the high purity synthetic quartz glass by the irradiation of 3-MeV electrons up to the 1x10 18 e - /cm 2 dosage. It was proved that the positron annihilation techniques were sufficiently sensitive to detect the defects in the electron-irradiated silica glasses. Three types of open-space defects were detected by the positron lifetime measurements. These can be attributed to monovacancy or divacancy type defects, vacancy clusters, and open-volume defects. A high formation probability (∼90%) of positroniums(Ps) was found in unirradiated specimens. These Ps were considered to be formed in open-volume defects. The formation probability of Ps was drastically decreased by the electron irradiation. But the size of open-volume defects was kept unchanged by the irradiation. These facts suggest that vacancy-type defects were introduced by the electron irradiation and that positrons were trapped in these defects. By the isochronal annealing in nitrogen atmosphere, the lifetime component (τ 2 ) and its relative intensity (I 2 ), attributed to positrons trapped in monovacancy or divacancy type defects and annihilated there, changed remarkably. τ 2 was constant in the temperature range up to 300degC, getting slightly shorter between 300degC and 700degC, and constant above 700degC. I 2 decreased gradually up to 300degC, constant between 300degC and 550degC, decreased above 550degC, and constant above 700degC. This revealed that the behavior of the defects, in which positrons were trapped, change by the elevation of the annealing temperature. (author)

  6. Mechanical control over valley magnetotransport in strained graphene

    Energy Technology Data Exchange (ETDEWEB)

    Ma, Ning, E-mail: maning@stu.xjtu.edu.cn [Department of Physics, MOE Key Laboratory of Advanced Transducers and Intelligent Control System, Taiyuan University of Technology, Taiyuan 030024 (China); Department of Applied Physics, MOE Key Laboratory for Nonequilibrium Synthesis and Modulation of Condensed Matter, Xi' an Jiaotong University, Xi' an 710049 (China); Zhang, Shengli, E-mail: zhangsl@mail.xjtu.edu.cn [Department of Applied Physics, MOE Key Laboratory for Nonequilibrium Synthesis and Modulation of Condensed Matter, Xi' an Jiaotong University, Xi' an 710049 (China); Liu, Daqing, E-mail: liudq@cczu.edu.cn [School of Mathematics and Physics, Changzhou University, Changzhou 213164 (China)

    2016-05-06

    Recent experiments report that the graphene exhibits Landau levels (LLs) that form in the presence of a uniform strain pseudomagnetic field with magnitudes up to hundreds of tesla. We further reveal that the strain removes the valley degeneracy in LLs, and leads to a significant valley polarization with inversion symmetry broken. This accordingly gives rise to the well separated valley Hall plateaus and Shubnikov–de Haas oscillations. These effects are absent in strainless graphene, and can be used to generate and detect valley polarization by mechanical means, forming the basis for the new paradigm “valleytronics” applications. - Highlights: • We explore the mechanical strain effects on the valley magnetotransport in graphene. • We analytically derive the dc collisional and Hall conductivities under strain. • The strain removes the valley degeneracy in Landau levels. • The strain causes a significant valley polarization with inversion symmetry broken. • The strain leads to the well separated valley Hall and Shubnikov–de Haas effects.

  7. The enhanced UV-sensitivity of Escherichia coli uvr A crp strain

    International Nuclear Information System (INIS)

    Skavronskaya, A.G.; Aleshkin, G.I.

    1979-01-01

    Mutations in genes cya and crp do not affect the UV cell sensitivity of Escherichia coli of wild type in relation to repairs of UV-injuries and UV induced mutations yield. Mutations in gene crp (protein defect of catabolitic activator - cap) result in UV sensitivity decrease of E. coli uvrA strain, imperfect as to the first stage of excision repairs not decreasing the quantity of revertants, induced by the UV-light

  8. Strain distributions and their influence on electronic structures of WSe2–MoS2 laterally strained heterojunctions

    KAUST Repository

    Zhang, Chendong

    2018-01-12

    Monolayer transition metal dichalcogenide heterojunctions, including vertical and lateral p–n junctions, have attracted considerable attention due to their potential applications in electronics and optoelectronics. Lattice-misfit strain in atomically abrupt lateral heterojunctions, such as WSe2–MoS2, offers a new band-engineering strategy for tailoring their electronic properties. However, this approach requires an understanding of the strain distribution and its effect on band alignment. Here, we study a WSe2–MoS2 lateral heterojunction using scanning tunnelling microscopy and image its moiré pattern to map the full two-dimensional strain tensor with high spatial resolution. Using scanning tunnelling spectroscopy, we measure both the strain and the band alignment of the WSe2–MoS2 lateral heterojunction. We find that the misfit strain induces type II to type I band alignment transformation. Scanning transmission electron microscopy reveals the dislocations at the interface that partially relieve the strain. Finally, we observe a distinctive electronic structure at the interface due to hetero-bonding.

  9. Strain distributions and their influence on electronic structures of WSe2–MoS2 laterally strained heterojunctions

    KAUST Repository

    Zhang, Chendong; Li, Ming-yang; Tersoff, Jerry; Han, Yimo; Su, Yushan; Li, Lain-Jong; Muller, David A.; Shih, Chih-Kang

    2018-01-01

    Monolayer transition metal dichalcogenide heterojunctions, including vertical and lateral p–n junctions, have attracted considerable attention due to their potential applications in electronics and optoelectronics. Lattice-misfit strain in atomically abrupt lateral heterojunctions, such as WSe2–MoS2, offers a new band-engineering strategy for tailoring their electronic properties. However, this approach requires an understanding of the strain distribution and its effect on band alignment. Here, we study a WSe2–MoS2 lateral heterojunction using scanning tunnelling microscopy and image its moiré pattern to map the full two-dimensional strain tensor with high spatial resolution. Using scanning tunnelling spectroscopy, we measure both the strain and the band alignment of the WSe2–MoS2 lateral heterojunction. We find that the misfit strain induces type II to type I band alignment transformation. Scanning transmission electron microscopy reveals the dislocations at the interface that partially relieve the strain. Finally, we observe a distinctive electronic structure at the interface due to hetero-bonding.

  10. Links between environmental geochemistry and rate of birth defects: Shanxi Province, China

    Energy Technology Data Exchange (ETDEWEB)

    Yu Haiying [State Key Laboratory of Earth Surface Processes and Resource Ecology, School of Geography, Beijing Normal University, Beijing 100875 (China); College of Resources and Environmental Sciences, Sichuan Agricultural University, Ya' an, Sichuan 625014 (China); Zhang Keli, E-mail: keli@bnu.edu.cn [State Key Laboratory of Earth Surface Processes and Resource Ecology, School of Geography, Beijing Normal University, Beijing 100875 (China)

    2011-01-01

    The rate of birth defects in Shanxi Province is among the highest worldwide. In order to identify the impacts of geochemical and environmental factors on birth defect risk, samples of soil, water and food were collected from an area with an unusually high rate of birth defects (study area) and an area with a low rate of birth defects (control area) in Shanxi Province, China. Element contents were determined by ICP-OES, and the results were analyzed using a non-parametric test and stepwise regression. Differences in the level and distribution of 14 geochemical elements, namely arsenic (As), selenium (Se), molybdenum (Mo), zinc (Zn), strontium (Sr), iron (Fe), tin (Sn), magnesium (Mg), vanadium (V), calcium (Ca), copper (Cu), aluminum (Al), potassium (K) and sulfur (S) were thus compared between the study and control areas. The results reveal that the geochemical element contents in soil, water and food show a significant difference between the study area and control area, and suggest that the study area was characterized by higher S and lower Sr and Al contents. These findings, based on statistical analysis, may be useful in directing further epidemiological investigations identifying the leading causes of birth defects. - Research Highlights: {yields} Environmental geochemistry has an significant impact on birth defects in the regions with an unusually high rate of birth defects. {yields} An excess of S and deficiency of Sr and Al are the distinctive environmental features associated with the high rate of birth defects in the Shanxi Province of China. {yields} Geochemical anomalies is a non-medical basis for effective prevention and cure of birth defects.

  11. Links between environmental geochemistry and rate of birth defects: Shanxi Province, China

    International Nuclear Information System (INIS)

    Yu Haiying; Zhang Keli

    2011-01-01

    The rate of birth defects in Shanxi Province is among the highest worldwide. In order to identify the impacts of geochemical and environmental factors on birth defect risk, samples of soil, water and food were collected from an area with an unusually high rate of birth defects (study area) and an area with a low rate of birth defects (control area) in Shanxi Province, China. Element contents were determined by ICP-OES, and the results were analyzed using a non-parametric test and stepwise regression. Differences in the level and distribution of 14 geochemical elements, namely arsenic (As), selenium (Se), molybdenum (Mo), zinc (Zn), strontium (Sr), iron (Fe), tin (Sn), magnesium (Mg), vanadium (V), calcium (Ca), copper (Cu), aluminum (Al), potassium (K) and sulfur (S) were thus compared between the study and control areas. The results reveal that the geochemical element contents in soil, water and food show a significant difference between the study area and control area, and suggest that the study area was characterized by higher S and lower Sr and Al contents. These findings, based on statistical analysis, may be useful in directing further epidemiological investigations identifying the leading causes of birth defects. - Research Highlights: → Environmental geochemistry has an significant impact on birth defects in the regions with an unusually high rate of birth defects. → An excess of S and deficiency of Sr and Al are the distinctive environmental features associated with the high rate of birth defects in the Shanxi Province of China. → Geochemical anomalies is a non-medical basis for effective prevention and cure of birth defects.

  12. Chemical Profile of Monascus ruber Strains

    Directory of Open Access Journals (Sweden)

    Ahamed M. Moharram

    2012-01-01

    Full Text Available Chemical profile of Monascus ruber strains has been studied using gas chromatography-mass spectrometry (GC/MS analysis. The colour intensity of the red pigment and secondary metabolic products of two M. ruber strains (AUMC 4066 and AUMC 5705 cultivated on ten different media were also studied. Metabolic products can be classified into four categories: anticholesterol, anticancer, food colouring, and essential fatty acids necessary for human health. Using GC/MS, the following 88 metabolic products were detected: butyric acid and its derivatives (25 products, other fatty acids and their derivatives (19 products, pyran and its derivatives (22 products and other metabolites (22 products. Among these, 32 metabolites were specific for AUMC 4066 strain and 34 for AUMC 5705 strain, whereas 22 metabolites were produced by both strains on different tested substrates. Production of some metabolites depended on the substrate used. High number of metabolites was recorded in the red pigment extract obtained by both strains grown on malt broth and malt agar. Also, 42 aroma compounds were recorded (4 alcohols, 2 benzaldehydes, 27 esters, 3 lactones, 1 phenol, 1 terpenoid, 3 thiol compounds and acetate-3-mercapto butyric acid. Thin layer chromatography and GC/MS analyses revealed no mycotoxin citrinin in any media used for the growth of the two M. ruber strains.

  13. Facts about Birth Defects

    Science.gov (United States)

    ... label> Information For… Media Policy Makers Facts about Birth Defects Language: English (US) Español (Spanish) Recommend on ... having a baby born without a birth defect. Birth Defects Are Common Every 4 ½ minutes, a ...

  14. Diagnosis of atrial septal defect using magnetic resonance imaging

    International Nuclear Information System (INIS)

    Sakakibara, Makoto; Kobayashi, Shiro; Imai, Hitoshi; Watanabe, Shigeru; Masuda, Yoshiaki; Inagaki, Yoshiaki

    1987-01-01

    The capability of magnetic resonance imaging (MRI) to detect atrial septal defect (ASD) was evaluated in 28 ASD patients of diagnostic confirmation, including five with complicated anomaly. Findings of MRI obtained from 7 normal volunteers and 142 patients with acquired heart diseases were used as controls. Non-gated MRI, performed in three ASD patients, failed to reveal defect areas ; gated MRI, in the other 25 patients, depicted defects in the interatrial septum corresponding to findings of surgery and cardiac catheterizatioin, which allowed the site and size of ASD to be determined. Other findings of MRI included right atrial dilatation, right ventricular hypertrophy and dilatation, and pulmonary artery dilatation in majority of ASD patients. Complex anomalies associated with ADS were also clearly shown on MRI. The interatrial septum was shown on gated-MRI in 124 control subjects, 17 of whom had an extremely faint signal from the central portion of the interatrial septum. The results indicate that gated MRI is a valuable noninvasive method in the diagnosis of ASD and complicating anomalies. (Namekawa, K.)

  15. The negative binomial distribution as a model for external corrosion defect counts in buried pipelines

    International Nuclear Information System (INIS)

    Valor, Alma; Alfonso, Lester; Caleyo, Francisco; Vidal, Julio; Perez-Baruch, Eloy; Hallen, José M.

    2015-01-01

    Highlights: • Observed external-corrosion defects in underground pipelines revealed a tendency to cluster. • The Poisson distribution is unable to fit extensive count data for these type of defects. • In contrast, the negative binomial distribution provides a suitable count model for them. • Two spatial stochastic processes lead to the negative binomial distribution for defect counts. • They are the Gamma-Poisson mixed process and the compound Poisson process. • A Rogeŕs process also arises as a plausible temporal stochastic process leading to corrosion defect clustering and to negative binomially distributed defect counts. - Abstract: The spatial distribution of external corrosion defects in buried pipelines is usually described as a Poisson process, which leads to corrosion defects being randomly distributed along the pipeline. However, in real operating conditions, the spatial distribution of defects considerably departs from Poisson statistics due to the aggregation of defects in groups or clusters. In this work, the statistical analysis of real corrosion data from underground pipelines operating in southern Mexico leads to conclude that the negative binomial distribution provides a better description for defect counts. The origin of this distribution from several processes is discussed. The analysed processes are: mixed Gamma-Poisson, compound Poisson and Roger’s processes. The physical reasons behind them are discussed for the specific case of soil corrosion.

  16. Superelastic load cycling of Gum Metal

    International Nuclear Information System (INIS)

    Vorontsov, V.A.; Jones, N.G.; Rahman, K.M.; Dye, D.

    2015-01-01

    The superelastic beta titanium alloy, Gum Metal, has been found to accumulate plastic strain during tensile load cycling in the superelastic regime. This is evident from the positive drift of the macroscopic stress vs. strain hysteresis curve parallel to the strain axis and the change in its geometry subsequent to every load–unload cycle. In addition, there is a progressive reduction in the hysteresis loop width and in the stress at which the superelastic transition occurs. In situ synchrotron X-ray diffraction has shown that the lattice strain exhibited the same behaviour as that observed in macroscopic measurements and identified further evidence of plastic strain accumulation. The mechanisms responsible for the observed behaviour have been evaluated using transmission electron microscopy, which revealed a range of different defects that formed during load cycling. The formation of these defects is consistent with the classical mathematical theory for the bcc to orthorhombic martensitic transformation. It is the accumulation of these defects over time that alters its superelastic behaviour

  17. Effect of saddle-point anisotropy on point-defect drift-diffusion into straight dislocations

    International Nuclear Information System (INIS)

    Skinner, B.C.; Woo, C.H.

    1983-02-01

    Effects on point-defect drift-diffusion in the strain fields of edge or screw dislocations, due to the anisotropy of the point defect in its saddle-point configuration, are investigated. Expressions for sink strength and bias that include the saddle-point shape effect are derived, both in the absence and presence of an externally applied stress. These are found to depend on intrinsic parameters such as the relaxation volume and the saddle-point shape of the point defects, and extrinsic parameters such as temperature and the magnitude and direction of the externally applied stress with respect to the line direction and Burgers vector direction of the dislocation. The theory is applied to fcc copper and bcc iron. It is found that screw dislocations are biased sinks and that the stress-induced bias differential for the edge dislocations depends much more on the line direction than the Burgers vector direction. Comparison with the stress-induced bias differential due to the usual SIPA effect is made. It is found that the present effect causes a bias differential that is more than an order of magnitude larger

  18. Fatigue Strength of Titanium Risers - Defect Sensitivity

    Energy Technology Data Exchange (ETDEWEB)

    Babalola, Olusegun Tunde

    2001-07-01

    This study is centred on assessment of the fatigue strength of titanium fusion welds for deep-water riser's applications. Deep-water risers are subjected to significant fatigue loading. Relevant fatigue data for titanium fusion welds are very scarce. Hence there is a need for fatigue data and life prediction models for such weldments. The study has covered three topics: Fatigue testing, Fractography and defect assessment, and Fracture Mechanics modelling of fatigue crack growth. Two series of welded grade of titanium consisting of 14 specimens in each series were fatigue tested under constant amplitude loading. Prior to fatigue testing, strain gauge measurements of some specimens was conducted to enable the definition of stress range in the fatigue assessment procedure. The results were compared with finite solid element analysis and related to fatigue stresses in a riser pipe wall. Distribution and geometry of internal and surface defects both in the as-welded and in the post-weld machined conditions were assessed using fractography. This served as a tool to determine the fatigue initiation point in the welds. Fracture mechanics was applied to model fatigue strength of titanium welds with initiation from weld defects. Two different stress intensity factor formulations for embedded eccentrically placed cracks were used for analysis of elliptical cracks with the major axis parallel and close to one of the free surfaces. The methods were combined to give a satisfactory model for crack growth analysis. The model analyses crack growth of elliptical and semi-elliptical cracks in two directions, with updating of the crack geometry. Fatigue strength assessment was conducted using two crack growth models, the Paris-Erdogan relation with no threshold and the Donahue et al. relation with an implied threshold. The model was validated against experimental data, with a discussion on the choice of crack growth model. (author)

  19. Dual passivation of intrinsic defects at the compound semiconductor/oxide interface using an oxidant and a reductant.

    Science.gov (United States)

    Kent, Tyler; Chagarov, Evgeniy; Edmonds, Mary; Droopad, Ravi; Kummel, Andrew C

    2015-05-26

    Studies have shown that metal oxide semiconductor field-effect transistors fabricated utilizing compound semiconductors as the channel are limited in their electrical performance. This is attributed to imperfections at the semiconductor/oxide interface which cause electronic trap states, resulting in inefficient modulation of the Fermi level. The physical origin of these states is still debated mainly because of the difficulty in assigning a particular electronic state to a specific physical defect. To gain insight into the exact source of the electronic trap states, density functional theory was employed to model the intrinsic physical defects on the InGaAs (2 × 4) surface and to model the effective passivation of these defects by utilizing both an oxidant and a reductant to eliminate metallic bonds and dangling-bond-induced strain at the interface. Scanning tunneling microscopy and spectroscopy were employed to experimentally determine the physical and electronic defects and to verify the effectiveness of dual passivation with an oxidant and a reductant. While subsurface chemisorption of oxidants on compound semiconductor substrates can be detrimental, it has been shown theoretically and experimentally that oxidants are critical to removing metallic defects at oxide/compound semiconductor interfaces present in nanoscale channels, oxides, and other nanostructures.

  20. Defect production in ceramics

    Energy Technology Data Exchange (ETDEWEB)

    Zinkle, S.J. [Oak Ridge National Lab., TN (United States); Kinoshita, C. [Kyushu Univ. (Japan)

    1997-08-01

    A review is given of several important defect production and accumulation parameters for irradiated ceramics. Materials covered in this review include alumina, magnesia, spinel silicon carbide, silicon nitride, aluminum nitride and diamond. Whereas threshold displacement energies for many ceramics are known within a reasonable level of uncertainty (with notable exceptions being AIN and Si{sub 3}N{sub 4}), relatively little information exists on the equally important parameters of surviving defect fraction (defect production efficiency) and point defect migration energies for most ceramics. Very little fundamental displacement damage information is available for nitride ceramics. The role of subthreshold irradiation on defect migration and microstructural evolution is also briefly discussed.