WorldWideScience

Sample records for steel-10crninb910

  1. Analysis of a multi pass weld of a thick walled tube made of austenitic stainless steel X6 CrNiNb 18 10

    International Nuclear Information System (INIS)

    Scholtes, B.; Zinn, W.; Ilg, U.; Backfisch, W.; Gibmeier, J.; Kirch, D.

    2006-01-01

    In this paper, microstructure and residual stresses of a multi pass welding of a thick-walled tube made of austenitic stainless steel X6 CrNiNb 18 10 (1.4550) are systematically characterized and assessed. Results of microstructural and phase analyses, residual stress and hardness measurements as well as of a tensile test using micro specimen and SEM analyses are presented. Using these data, plastic deformations occurring during the welding process in the vicinity of the weld seam are evaluated. Finally, consequences of an additional heat treatment at 400 C/24 h are studied. (Abstract Copyright [2006], Wiley Periodicals, Inc.) [de

  2. Strength behaviour of 10CrMo9.10 steel in nonsteady-state applications

    International Nuclear Information System (INIS)

    Seidel, C.

    2 testing runs with cyclic temperature increase were conducted on steel 10CrMo9.10 samples, i.e., at 500 degC and cyclic increase by 10, 25 and 50 degC, and at 550 degC and cyclic increase by 50 degC. Long-term strength was studied under a strain of 6.1 to 25.6 kp/mm 2 for 22,000 hours and the effect of periodical unloading was investigated on long-term strength at 550 degC. Sample loading and unloading proceeded within the range of 8.8 to 24.7 kp/mm 2 at an unloading rate of 8 to 100 %/min. Steel lifetime was not affected by the number of cycles. The effect of the changing load and of constant temperature without load on the long-term strength of the steel at 550 degC is shown graphically. The results showed a clear dependence of steel life on dwell time at the given temperature without load. (J.P.)

  3. The role of Ti, Zr and Ce in shaping of the Cr-Ni-Nb cast steel resistance to carburising

    Directory of Open Access Journals (Sweden)

    G. Tęcza

    2008-08-01

    Full Text Available From the centrifugally cast Cr-Ni-Nb steel pipes, specimens were cut out and subjected to carburising for 100 hours in a mixture of charcoal (90% and Na2CO3 (10% at the temperatures of 950 and 1150°C. The specimens were cut in direction normal to the pipe axis and were examined by optical and scanning microscopy. As a parameter describing the resistance of the examined alloy to the carburising effect, the thickness of a carburised layer was accepted. It has been observed that additions of Ti and Zr, and of Ti+Zr+Ce introduced jointly, increase the thickness of the carburised layer, while the addition of Ce improves the alloy resistance to carburising. On the alloy surface, a layer composed of oxides, mainly of chromium, silicon and iron, has been formed. Changes in the chemical composition of the surface layer were examined by scanning microscopy.

  4. Microstructural aspects of crack formation and propagation in the austenitic steel X6CrNiNb18-10 under low cycle fatigue loading

    International Nuclear Information System (INIS)

    Soppa, E.; Kohler, C.; Roos, E.; Schuler, X.

    2012-01-01

    The understanding of the crack initiation mechanisms and crack growth in apparently monolithic materials like X6CrNiNb18-10 stainless steel under cyclic loading requires the explicit analysis of the phenomena underlying fatigue on both atomistic and microscopic levels. The permanent delivery of mechanical energy through cyclic loading evokes changes in the microstructure that can lead to a martensitic transformation. The transformation of a metastable cubic face centered austenite and formation of a cubic body centered α'-martensite under cyclic loading at room temperature was found, both, in the experiment and in molecular dynamics simulations. The martensite nucleates prevalently at grain boundaries, triple points and at the specimen free surface and forms small (∝ 1 μm) differently oriented grains, also in the same parent austenitic grain. By a combination of interrupted low cycle fatigue tests (LCF) and electron backscatter diffraction (EBSD) measurements the martensitic transformation and subsequent fatigue crack formation were observed at the same area in the microstructure at different stages of the specimen lifetime. The EBSD measurements showed the following crack initiation scenarios: Cracks started (a) at the phase boundary between austenite and α'-martensite, (b) inside fully martensitic areas in the matrix, (c) at broken or debonded coarse NbCs. It is obvious that formation of a hard α'-martensite in a ductile and soft austenite and forming two-phase material causes a heterogeneous stress and strain distribution on the microscopic level. α'-martensite enhances locally the stress amplitude whereas in a soft austenite the plastic strain amplitude increases. Strain concentration in the austenite along the phase boundary is connected with a stress increase along the interface and can initiate fatigue crack there. Also at the crack tip, a permanent martensitic transformation occurs, so that the growth of the fatigue cracks at room temperature seems

  5. 46 CFR 9.10 - Waiting time.

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 1 2010-10-01 2010-10-01 false Waiting time. 9.10 Section 9.10 Shipping COAST GUARD... § 9.10 Waiting time. The same construction should be given the act when charging for waiting time as... for duty the waiting time amounts to at least one hour. ...

  6. Microstructural aspects of crack formation and propagation in the austenitic steel X6CrNiNb18-10 under low cycle fatigue loading

    Energy Technology Data Exchange (ETDEWEB)

    Soppa, E.; Kohler, C.; Roos, E.; Schuler, X. [Stuttgart Univ. (Germany). MPA

    2012-07-01

    The understanding of the crack initiation mechanisms and crack growth in apparently monolithic materials like X6CrNiNb18-10 stainless steel under cyclic loading requires the explicit analysis of the phenomena underlying fatigue on both atomistic and microscopic levels. The permanent delivery of mechanical energy through cyclic loading evokes changes in the microstructure that can lead to a martensitic transformation. The transformation of a metastable cubic face centered austenite and formation of a cubic body centered α'-martensite under cyclic loading at room temperature was found, both, in the experiment and in molecular dynamics simulations. The martensite nucleates prevalently at grain boundaries, triple points and at the specimen free surface and forms small (∝ 1 μm) differently oriented grains, also in the same parent austenitic grain. By a combination of interrupted low cycle fatigue tests (LCF) and electron backscatter diffraction (EBSD) measurements the martensitic transformation and subsequent fatigue crack formation were observed at the same area in the microstructure at different stages of the specimen lifetime. The EBSD measurements showed the following crack initiation scenarios: Cracks started (a) at the phase boundary between austenite and α'-martensite, (b) inside fully martensitic areas in the matrix, (c) at broken or debonded coarse NbCs. It is obvious that formation of a hard α'-martensite in a ductile and soft austenite and forming two-phase material causes a heterogeneous stress and strain distribution on the microscopic level. α'-martensite enhances locally the stress amplitude whereas in a soft austenite the plastic strain amplitude increases. Strain concentration in the austenite along the phase boundary is connected with a stress increase along the interface and can initiate fatigue crack there. Also at the crack tip, a permanent martensitic transformation occurs, so that the growth of the fatigue cracks at room

  7. 22 CFR 9.10 - Mandatory declassification review.

    Science.gov (United States)

    2010-04-01

    ... 22 Foreign Relations 1 2010-04-01 2010-04-01 false Mandatory declassification review. 9.10 Section 9.10 Foreign Relations DEPARTMENT OF STATE GENERAL SECURITY INFORMATION REGULATIONS § 9.10 Mandatory declassification review. All requests to the Department by a member of the public, a government employee, or an...

  8. One-electron reduction of 9,10-anthraquinone, 1-amino-9,10-anthraquinone and 1-hydroxy-9,10-anthraquinone in aqueous-isopropanol-acetone mixed solvent: a pulse radiolysis study

    International Nuclear Information System (INIS)

    Pal, H.; Mukherjee, T.; Mittal, J.P.

    1994-01-01

    The semiquinone radicals produced by one-electron reduction of 9,10-anthraquinone, 1-amino- 9,10-anthraquinone and 1-hydroxy-9,10-anthraquinone have been characterized in aqueous-organic mixed solvent comprising of 30.2 mol dm -3 water, 5 mol dm -3 isopropanol and 1 mol dm -3 acetone, using the pulse radiolysis technique. Spectroscopic characteristics, the kinetic parameters of formation and decay and one acid dissociation constants of the semiquinones and one-electron reduction potentials of the quinones have been estimated. The characteristics of the present semiquinone systems have been compared with those of other similar systems. The observed differences in characteristics of the semiquinones due to different substitutions have been analysed. (Author)

  9. Fatigue behavior of austenitic steels. Subproject. Mechanism oriented investigation of the fatigue behavior of austenitic steel X6CrNiNb1810 in the HCF and VHCF regime. Final report; Ermuedungsverhalten Austenit. Teilprojekt. Mechanismenorientierte Untersuchung des Ermuedungsverhaltens des austenitischen Stahles X6CrNiNb1810 im HCF- und VHCF-Bereich. Abschlussbericht

    Energy Technology Data Exchange (ETDEWEB)

    Sorich, A.; Smaga, M.; Eifler, D.

    2015-01-23

    In addition to load cycles in the Low Cycle Fatigue (LCF)-regime due to start up and shut down procedures of power plants, in some components additional high-frequency loadings in the High Cycle Fatigue (HCF)- and Very High Cycle Fatigue (VHCF)-regime occur. These loadings are induced e.g. by stresses due to thermal cyclic fluctuations and fluid dynamic processes. Therefore it is necessary to characterize experimentally the cyclic deformation behavior of metastable austenitic steels at operating temperature particularly in the HCF- and VHCF-regime and to develop a nondestructive method to detect fatigue processes. This joint research project was conducted in cooperation between the Institute of Materials Science and Engineering (WKK) of the University of Kaiserslautern and the Fraunhofer-Institute for Non-Destructive Testing (IZFP) in Saarbruecken. WKK was focused on experimental investigations to characterize the cyclic deformation behavior of the metastable austenitic steel in the HCF- and VHCF-range, taking into account cyclic hardening and softening processes and in particular to consider fatigue-induced changes in microstructure. The IZFP has focused on the development and application of a testing concept based on electromagnetic ultrasonic measurements. The isothermal cyclic deformation behavior of the metastable austenitic steel X6CrNiNb1810 (1.4550, AISI 347) at 300 C in the HCF-range is characterized by cyclic softening until specimen failure. At strain amplitudes of 0.10 % ≤ ε{sub a,t} ≤ 0.15 % and the stress amplitude σ{sub a} = 160 MPa cyclic softening is followed by cyclic hardening, which results in a significant increase in life time, up to the limiting number of cycles, which was defined at N{sub I} = 10{sup 7} in HCF-regime. The cyclic hardening is determined by a transformation induced phase formation from face-centered cubic (fcc) austenite to body-centered cubic (bcc) α{sup '}-martensite and/or in hexagonal (hcp) ε-martensite. In

  10. 12 CFR 9.10 - Fiduciary funds awaiting investment or distribution.

    Science.gov (United States)

    2010-01-01

    ... distribution. 9.10 Section 9.10 Banks and Banking COMPTROLLER OF THE CURRENCY, DEPARTMENT OF THE TREASURY... has investment discretion, the bank shall obtain for funds awaiting investment or distribution a rate... principal and interest; (ii) Securities that qualify as eligible for investment by national banks pursuant...

  11. The Effect of Heat Treatment Parameters on Mechanical Characteristics of 10CrMo9-10 Steel Tube Bends / Wpływ Parametrów Obróbki Cieplnej Na Charakterystyki Mechaniczne Łuków Rurowych Ze Stali 10CrMo9-10

    Directory of Open Access Journals (Sweden)

    Cieśla M.

    2015-12-01

    Full Text Available The purpose of the paper was to analyse the effect of diverse heat treatment parameters (normalising and tempering on mechanical characteristics of the material used to develop ϕ508x20 tube bends made of the 10CrMo9-10 steel by application of induction heating. The research conducted included tests of basic mechanical properties as well as low cycle fatigue and creep at the temperature of 500°C. With reference to the results thus obtained, it has been established that there is a relationship between mechanical properties of bends and individual features of their microstructure conditional to the heat treatment parameters. Among other conclusions drawn in the research, it has been found that the main structural factor conditioning the mechanical properties of bends was the grain size. Heat treatment parameters characterised by lower temperature and shorter tempering time triggered changes in the material microstructure, such as increased grain comminution. The effects of the said changes included improvement of strength characteristics (Rm, Rp0,2 as well as increased material durability under conditions of fatigue and creep. Main criterion-specific mechanical properties and geometric features of the bends developed conformed with the relevant requirements of reference standards (PN-EN 10216-2, PN-EN 12952.

  12. Vibrational assignments for the Raman and the phosphorescence spectra of 9,10-anthraquinone and 9,10-anthraquinone-d81

    International Nuclear Information System (INIS)

    Lehmann, K.K.; Smolarek, J.; Khalil, O.S.; Goodman, L.

    1979-01-01

    The Raman spectra of 9,10-anthraquinone (AQ) and 9,10-anthraquinone-d/sub 8/ are examined. Raman band assignments are made from this data and from a published normal coordinate analysis. The Raman spectra of AQ at 5K is reported and vibrational assignments for the phosphorescence spectra of AQ in n-hexane at 4.2 K are reexamined in light of new 3 B 1 /sub g/ → 1 A/sub g/ phosphorescence data. Contrary to previous work from this laboratory, it is concluded that although higher order vibronic interactions may be operative between the two closely spaced 3 A/sub u/- 3 B 1 /sub g/ electronic states, these interactions are not manifested in the phosphorescence spectra of AQ in n-hexane at 4.2 K

  13. Convenient synthesis of 6-nor-9,10-dihydrolysergic acid methyl ester.

    Science.gov (United States)

    Crider, A M; Grubb, R; Bachmann, K A; Rawat, A K

    1981-12-01

    6-Nor-9,10-dihydrolysergic acid methyl ester (IV) was prepared by demethylation of 9,10-dihydrolysergic acid methyl ester (II) with 2,2,2-trichloroethyl chloroformate, followed by reduction of the intermediate carbamate (III) with zinc in acetic acid. The 6-ethyl-V and 6-n-propyl-VI derivatives were prepared by alkylation of IV with the appropriate halide. All of the ergoline derivatives were evaluated for stereotyped behavior in rats, with 6-nor-6-ethyl-9,10-dihydrolysergic acid methyl ester (V) being active but much less potent than apomorphine. Compound VI was evaluated for its effect on blood pressure; at a dose of 30 mg/kg ip, it significantly lowered, diastolic pressure in normotensive rats.

  14. Mechanism and kinetic properties for the OH-initiated atmospheric oxidation degradation of 9,10-Dichlorophenanthrene

    Energy Technology Data Exchange (ETDEWEB)

    Dang, Juan; Shi, Xiangli; Zhang, Qingzhu, E-mail: zqz@sdu.edu.cn; Hu, Jingtian; Wang, Wenxing

    2015-02-01

    Chlorinated polycyclic aromatic hydrocarbons (ClPAHs) have become a serious environmental concern due to their widespread occurrence and dioxin-like toxicities. In this work, the mechanism of the OH-initiated atmospheric oxidation degradation of 9,10-dichlorophenanthrene (9,10-Cl{sub 2}Phe) was investigated by using high-accuracy quantum chemistry calculations. The rate constants of the crucial elementary reactions were determined by the Rice–Ramsperger–Kassel–Marcus (RRKM) theory. The theoretical results were compared with the available experimental data. The main oxidation products are a group of ring-retaining and ring-opening compounds including chlorophenanthrols, 9,10-dichlorophenanthrene-3,4-dione, dialdehydes, chlorophenanthrenequinones, nitro-9,10-Cl{sub 2}Phe and epoxides et al. The overall rate constant of the OH addition reaction is 2.35 × 10{sup −12} cm{sup 3} molecule{sup −1} s{sup −1} at 298 K and 1 atm. The atmospheric lifetime of 9,10-Cl{sub 2}Phe determined by OH radicals is about 5.05 days. This study provides a comprehensive investigation of the OH-initiated oxidation degradation of 9,10-Cl{sub 2}Phe and should contribute to clarifying its atmospheric fate. - Highlights: • We studied a comprehensive mechanism of OH-initiated degradation of 9,10-Cl{sub 2}Phe. • The atmospheric lifetime of 9,10-Cl{sub 2}Phe determined by OH radical is about 5.05 d. • The rate constants of the crucial elementary steps were evaluated. • Water plays an important role in the formation of nitro-9,10-Cl{sub 2}Phe.

  15. 9,10-Dioxoanthracene-1,4-diyl bis(4-methylbenzenesulfonate

    Directory of Open Access Journals (Sweden)

    Sirirat Kokpol

    2012-05-01

    Full Text Available The title molecule, C28H20O8S2, has a T-shaped conformation. The central 9,10-anthraquinone moiety is bow-shaped with the two outer aromatic rings being inclined to one another by 13.99 (11°. The benzenesulfonate rings are inclined to one another by 47.35 (12°, and by 34.51 (11 and 17.88 (11° to the bridging aromatic ring of the 9,10-anthraquinone moiety. In the crystal, C—H...O interactions link the molecules into ribbons in [100].

  16. Exposure to 9,10-phenanthrenequinone accelerates malignant progression of lung cancer cells through up-regulation of aldo-keto reductase 1B10

    International Nuclear Information System (INIS)

    Matsunaga, Toshiyuki; Morikawa, Yoshifumi; Haga, Mariko; Endo, Satoshi; Soda, Midori; Yamamura, Keiko; El-Kabbani, Ossama; Tajima, Kazuo; Ikari, Akira; Hara, Akira

    2014-01-01

    Inhalation of 9,10-phenanthrenequinone (9,10-PQ), a major quinone in diesel exhaust, exerts fatal damage against a variety of cells involved in respiratory function. Here, we show that treatment with high concentrations of 9,10-PQ evokes apoptosis of lung cancer A549 cells through production of reactive oxygen species (ROS). In contrast, 9,10-PQ at its concentrations of 2 and 5 μM elevated the potentials for proliferation, invasion, metastasis and tumorigenesis, all of which were almost completely inhibited by addition of an antioxidant N-acetyl-L-cysteine, inferring a crucial role of ROS in the overgrowth and malignant progression of lung cancer cells. Comparison of mRNA expression levels of six aldo-keto reductases (AKRs) in the 9,10-PQ-treated cells advocated up-regulation of AKR1B10 as a major cause contributing to the lung cancer malignancy. In support of this, the elevation of invasive, metastatic and tumorigenic activities in the 9,10-PQ-treated cells was significantly abolished by the addition of a selective AKR1B10 inhibitor oleanolic acid. Intriguingly, zymographic and real-time PCR analyses revealed remarkable increases in secretion and expression, respectively, of matrix metalloproteinase 2 during the 9,10-PQ treatment, and suggested that the AKR1B10 up-regulation and resultant activation of mitogen-activated protein kinase cascade are predominant mechanisms underlying the metalloproteinase induction. In addition, HPLC analysis and cytochrome c reduction assay in in vitro 9,10-PQ reduction by AKR1B10 demonstrated that the enzyme catalyzes redox-cycling of this quinone, by which ROS are produced. Collectively, these results suggest that AKR1B10 is a key regulator involved in overgrowth and malignant progression of the lung cancer cells through ROS production due to 9,10-PQ redox-cycling. - Highlights: • 9,10-PQ promotes invasion, metastasis and tumorigenicity in lung cancer cells. • The 9,10-PQ-elicited promotion is possibly due to AKR1B10 up

  17. Exposure to 9,10-phenanthrenequinone accelerates malignant progression of lung cancer cells through up-regulation of aldo-keto reductase 1B10

    Energy Technology Data Exchange (ETDEWEB)

    Matsunaga, Toshiyuki, E-mail: matsunagat@gifu-pu.ac.jp [Laboratory of Biochemistry, Gifu Pharmaceutical University, Gifu 501-1196 (Japan); Morikawa, Yoshifumi; Haga, Mariko; Endo, Satoshi [Laboratory of Biochemistry, Gifu Pharmaceutical University, Gifu 501-1196 (Japan); Soda, Midori; Yamamura, Keiko [Laboratory of Clinical Pharmacy, School of Pharmacy, Aichi Gakuin University, Nagoya 464-8650 (Japan); El-Kabbani, Ossama [Monash Institute of Pharmaceutical Sciences, Monash University, Victoria 3052 (Australia); Tajima, Kazuo [Faculty of Pharmaceutical Sciences, Hokuriku University, Kanazawa 920-1181 (Japan); Ikari, Akira [Laboratory of Biochemistry, Gifu Pharmaceutical University, Gifu 501-1196 (Japan); Hara, Akira [Faculty of Engineering, Gifu University, Gifu 501-1193 (Japan)

    2014-07-15

    Inhalation of 9,10-phenanthrenequinone (9,10-PQ), a major quinone in diesel exhaust, exerts fatal damage against a variety of cells involved in respiratory function. Here, we show that treatment with high concentrations of 9,10-PQ evokes apoptosis of lung cancer A549 cells through production of reactive oxygen species (ROS). In contrast, 9,10-PQ at its concentrations of 2 and 5 μM elevated the potentials for proliferation, invasion, metastasis and tumorigenesis, all of which were almost completely inhibited by addition of an antioxidant N-acetyl-L-cysteine, inferring a crucial role of ROS in the overgrowth and malignant progression of lung cancer cells. Comparison of mRNA expression levels of six aldo-keto reductases (AKRs) in the 9,10-PQ-treated cells advocated up-regulation of AKR1B10 as a major cause contributing to the lung cancer malignancy. In support of this, the elevation of invasive, metastatic and tumorigenic activities in the 9,10-PQ-treated cells was significantly abolished by the addition of a selective AKR1B10 inhibitor oleanolic acid. Intriguingly, zymographic and real-time PCR analyses revealed remarkable increases in secretion and expression, respectively, of matrix metalloproteinase 2 during the 9,10-PQ treatment, and suggested that the AKR1B10 up-regulation and resultant activation of mitogen-activated protein kinase cascade are predominant mechanisms underlying the metalloproteinase induction. In addition, HPLC analysis and cytochrome c reduction assay in in vitro 9,10-PQ reduction by AKR1B10 demonstrated that the enzyme catalyzes redox-cycling of this quinone, by which ROS are produced. Collectively, these results suggest that AKR1B10 is a key regulator involved in overgrowth and malignant progression of the lung cancer cells through ROS production due to 9,10-PQ redox-cycling. - Highlights: • 9,10-PQ promotes invasion, metastasis and tumorigenicity in lung cancer cells. • The 9,10-PQ-elicited promotion is possibly due to AKR1B10 up

  18. Mechanism and kinetic properties for the OH-initiated atmospheric oxidation degradation of 9,10-Dichlorophenanthrene.

    Science.gov (United States)

    Dang, Juan; Shi, Xiangli; Zhang, Qingzhu; Hu, Jingtian; Wang, Wenxing

    2015-02-01

    Chlorinated polycyclic aromatic hydrocarbons (ClPAHs) have become a serious environmental concern due to their widespread occurrence and dioxin-like toxicities. In this work, the mechanism of the OH-initiated atmospheric oxidation degradation of 9,10-dichlorophenanthrene (9,10-Cl₂Phe) was investigated by using high-accuracy quantum chemistry calculations. The rate constants of the crucial elementary reactions were determined by the Rice-Ramsperger-Kassel-Marcus (RRKM) theory. The theoretical results were compared with the available experimental data. The main oxidation products are a group of ring-retaining and ring-opening compounds including chlorophenanthrols, 9,10-dichlorophenanthrene-3,4-dione, dialdehydes, chlorophenanthrenequinones, nitro-9,10-Cl₂Phe and epoxides et al. The overall rate constant of the OH addition reaction is 2.35 × 10(-12)cm(3) molecule(-1)s(-1) at 298 K and 1 atm. The atmospheric lifetime of 9,10-Cl₂Phe determined by OH radicals is about 5.05 days. This study provides a comprehensive investigation of the OH-initiated oxidation degradation of 9,10-Cl₂Phe and should contribute to clarifying its atmospheric fate. Copyright © 2014 Elsevier B.V. All rights reserved.

  19. A new 9,10-dihydrophenanthrene from Dendrobium moniliforme.

    Science.gov (United States)

    Zhao, Ningdong; Yang, Guangyu; Zhang, Yan; Chen, Lijun; Chen, Yegao

    2016-01-01

    A new 9,10-dihydrophenanthrene,1,5-dihydroxy-3,4,7-trimethoxy-9,10-dihydrophenanthrene (1) was isolated and identified from the whole plants of Dendrobium moniliforme, as well as 24 known compounds including hircinol (2), (2R*,3S*)-3-hydroxymethyl-9-methoxy-2-(4'-hydroxy-3',5'-dimethoxyphenyl)-2,3,6,7-tetrahydro-phenanthro[4,3-b]furan-5,11-diol (3), diospyrosin (4), aloifol I (5), moscatilin (6), 3,4'-dihydroxy-3',4,5-trimethoxybibenzyl (7), gigantol (8), 3,3'-dihydroxy-4,5-dimethoxybibenzyl (9), longicornuol A (10), N-trans-cinnamoyltyramine (11), paprazine (12), N-trans-feruloyl 3'-O-methyldopamine (13), moupinamide (14), dihydroconiferyl dihydro-p-coumarate (15), dihydrosinapyl dihydro-p-coumarate (16), 3-isopropyl-5-acetoxycyclohexene-2-one-1 (17), p-hydroxybenzaldehyde (18), vanillin (19), p-hydroxyphenylpropionic acid (20), vanillic acid (21), protocatechuic acid (22), (+)-syringaresinol (23), β-sitosterol (24) and daucosterol (25). Compounds 3, 4, 13, 16, 17 and 20 were isolated from the Dendrobium genus for the first time, and compounds 2, 5, 7, 9-12, 14, 15, 18, 21 and 22 were originally obtained from D. moniliforme.

  20. Kinetics of steel corrosion in water

    International Nuclear Information System (INIS)

    Vettegren', V.I.; Bashkarev, A.Ya.; Danchukov, K.G.; Morozov, G.I.

    2003-01-01

    Kinetics of corrosion damage accumulation in steels of different composition (Cr-Ni-Mo-Ti, Cr-Ni-Mn-N-V, Cr-Ni-N-Mn-Mo, Cr-Ni-Nb, Cr-Ni-Ti, Cr-Mn-Ni, Mn-Al-Nb-Si, Mn-Cr-Al-Si and Mn-Al-Si) in NaCl solution and in sea water was studied. It is shown that degree of corrosion damage relates to time according to the first order reaction expression. The values of corrosion activation energy and of parameter characterizing protection properties of corrosion film are determined [ru

  1. 75 FR 47199 - Airworthiness Directives; McDonnell Douglas Corporation Model DC-9-10 Series Airplanes, DC-9-30...

    Science.gov (United States)

    2010-08-05

    ... Airworthiness Directives; McDonnell Douglas Corporation Model DC- 9-10 Series Airplanes, DC-9-30 Series... existing airworthiness directive (AD), which applies to all McDonnell Douglas Model DC-9-10 series..., 2010). That AD applies to all McDonnell Douglas Corporation Model DC-9-10 series airplanes, DC-9-30...

  2. Metal complexes with 1,5- and 1,8-dihydroxy-9,10-anthraquinones: electronic absorption spectra and structure of ligands

    International Nuclear Information System (INIS)

    Fajn, V.Ya.; Zajtsev, B.E.; Ryabov, M.A.

    2004-01-01

    By spectrophotometric, quantum-chemical, and correlation methods it is determined that in complexes of metals (Nd, Pr, Sm, Th, UO 2 2+ , V) with 1,5-dihydroxy-9,10-anthraquinone ligand could be in 7 excited states differing not only by ionization degree but primary contribution of tautomeric 9,10-, 1,10-, and 1,5-anthraquinoid structures. On all known complexes with 1,8-dihydroxy-9,10-anthraquinone containing once ionized ligand the last has 1,10-anthraquinoid structure; for complexes containing twofold ionized ligand 9,10-anthraquinoid structure of ligand is the most characteristic. Known complexes are classified in accordance with structure of ligands [ru

  3. Fatigue mechanisms in an austenitic steel under cyclic loading: Experiments and atomistic simulations

    Energy Technology Data Exchange (ETDEWEB)

    Soppa, E.A., E-mail: ewa.soppa@mpa.uni-stuttgart.de; Kohler, C., E-mail: christopher.kohler@mpa.uni-stuttgart.de; Roos, E., E-mail: eberhard.roos@mpa.uni-stuttgart.de

    2014-03-01

    Experimental investigations on the austenitic stainless steel X6CrNiNb18-10 (AISI – 347) and concomitant atomistic simulations of a FeNi nanocrystalline model system have been performed in order to understand the basic mechanisms of fatigue damage under cyclic loading. Using electron backscatter diffraction (EBSD) the influence of deformation induced martensitic transformation and NbC size distribution on the fatigue crack formation has been demonstrated. The martensite nucleates prevalently at grain boundaries, triple points and at the specimen free surface and forms small (∼1 µm sized) differently oriented grains. The atomistic simulations show the role of regions of a high density of stacking faults for the martensitic transformation.

  4. Comparative studies on ultrasonic, friction, laser and resistance pressure welding of NiTi shape memory alloys with high-alloy steels. Final report; Vergleichende Untersuchungen zum Ultraschall-, Reib-, Laserstrahl- und Widerstandspressschweissen von NiTi-Shape-Memory-Metall mit hochlegierten Staehlen. Abschlussbericht

    Energy Technology Data Exchange (ETDEWEB)

    Zuckschwerdt, K.

    2000-04-01

    The suitability of different welding techniques for welding of NiTi shape memory alloys with high-alloy steel (C12CrNi17-7, X5CrNiNb19-9, X20Cr13) was investigated. The quality of the welds was analyzed using mechanical-technological, fractographic, metallographic and electron microscopy analysis. [German] Ziel dieses Forschungsvorhabens ist es, die Eignung der einzelnen Schweissverfahren fuer das Fuegen von NiTi-Formgedaechtnislegierungen mit hochlegiertem Stahl (X12CrNi17-7, X5CrNiNb19-9, X20Cr13) darzustellen und zu beurteilen. Die Qualitaet der Fuegeverbindungen wird mit Hilfe mechanisch-technologischer, fraktographischer, metallographischer und elektronenmikroskopischer Untersuchungen bewertet.

  5. Dual effects of N-acetyl-L-cysteine dependent on NQO1 activity: Suppressive or promotive of 9,10-phenanthrenequinone-induced toxicity

    International Nuclear Information System (INIS)

    Toyooka, Tatsushi; Shinmen, Takuya; Aarts, Jac M.M.J.G.; Ibuki, Yuko

    2012-01-01

    A typical antioxidant, N-acetyl-L-cysteine (NAC) generally protects cells from oxidative damage induced by reactive oxygen species (ROS). 9,10-Phenanthrenequinone (9,10-PQ), a major quinone in diesel exhaust particles, produces ROS in redox cycling following two-electron reduction by NAD(P)H:quinone oxidoreductase 1 (NQO1), which has been considered as a cause of its cyto- and genotoxicity. In this study, we show that NAC unexpectedly augments the toxicity of 9,10-PQ in cells with low NQO1 activity. In four human skin cell lines, the expression and the activity of NQO1 were lower than in human adenocarcinoma cell lines, A549 and MCF7. In the skin cells, the cytotoxicity of 9,10-PQ was significantly enhanced by addition of NAC. The formation of DNA double strand breaks accompanying phosphorylation of histone H2AX, was also remarkably augmented. On the other hand, the cyto- and genotoxicity were suppressed by addition of NAC in the adenocarcinoma cells. Two contrasting experiments: overexpression of NQO1 in CHO-K1 cells which originally expressed low NQO1 levels, and knock‐down of NQO1 in the adenocarcinoma cell line A549 by transfection of RNAi, also showed that NAC suppressed 9,10-PQ-induced toxicity in cell lines expressing high NQO1 activity and enhanced it in cell lines with low NQO1 activity. The results suggested that dual effects of NAC on the cyto- and genotoxicity of 9,10-PQ were dependent on tissue-specific NQO1 activity. -- Highlights: ► NAC augmented the cytotoxicity of 9,10-PQ in skin cell lines. ► 9,10-PQ-induced DSBs accompanying γ-H2AX were also augmented by NAC. ► NAC suppressed the cyto- and genotoxicity of 9,10-PQ in adenocarcinoma cell lines. ► The dual effects of NAC on toxicity of 9,10-PQ were dependent on NQO1 activity.

  6. Results obtained so far with the production of turbine and valve casings made of the new 9% Cr cast steel types G-X 12 CrMoWVNbN 10 11 and G-X 12 CrMoVNbN 91; Erfahrungsbericht ueber die Herstellung von Turbinen- und Ventilgehaeusen aus den neuen 9% Cr-Stahlgusssorten G-X 12 CrMoWVNbN 10 1 1 und G-X 12 CrMoVNbN 91

    Energy Technology Data Exchange (ETDEWEB)

    Schuster, F.; Buberl, A.; Hanus, R. [VOEST-ALPINE STAHL LINZ GmbH, Linz (Austria); Cerjak, H. [Technische Univ., Graz (Austria)

    1996-12-31

    In the course of production start-up of new 9-10% Cr cast steel types, and application of R and D results to practice, the following examinations and modifications have been performed: 1. Reduction of average chromium content from 10.5 to 9.5% in order to suppress delta ferrite segregation, and adjustment of austenite and ferrite stabilizing alloying constituents. 2. Analysis of typical defects in castings, and modification of casting and feeding techniques in compliance with the saturation behaviour of the new 9-10% Cr steels. These measures achieved a reduction of feeding-based flaws (shrinkage) in the last few cast pieces. 3. The good weldability was proven of the new 9-10% Cr steels by means of welding tests and crack-free production and construction welds made in cast pieces. (orig./MM) [Deutsch] Im Zuge der Produktionsaufnahme neuer 9-10% Cr-Stahlgusssorten und der Ueberleitung der F and E Ergebnisse in die betriebliche Praxis wurden folgende Untersuchungen und Anpassungen vorgenommen: 1. Um die Deltaferritausscheidung zu unterdruecken, wurde der mittlere Chromgehalt von 10,5 auf 9,5% abgesenkt und die austenit- und ferritstabilisierenden Legierungselemente besser angepasst. 2. Die Analyse typischer Fehlererscheinungen an Gussstuecken machten eine Anpassung der Giess- und Speisungstechnik an das Saettigungsverhalten der neuen 9-10% Cr-Staehle erforderlich. Diese Massnahmen fuehrten zu einer Verringerung der Speisungsfehler (Lunker) bei den zuletzt abgegossenen Gussstuecken. 3. Bei Schweissversuchen und an Gussstuecken rissfrei ausgefuehrten Fertigungs- und Konstruktionsschweissungen konnte die gute Schweisseignung der neuen 9-10% Cr-Staehle nachgewiesen werden. (orig./MM)

  7. 42 CFR 414.910 - Bidding process.

    Science.gov (United States)

    2010-10-01

    ... 42 Public Health 3 2010-10-01 2010-10-01 false Bidding process. 414.910 Section 414.910 Public Health CENTERS FOR MEDICARE & MEDICAID SERVICES, DEPARTMENT OF HEALTH AND HUMAN SERVICES (CONTINUED... Under Part B § 414.910 Bidding process. (a) Entities may bid to furnish CAP drugs in all competitive...

  8. Rumpictuside A: Unusual 9,10-anthraquinone glucoside from Rumex pictus Forssk.

    Science.gov (United States)

    El-Kashak, Walaa A; Elshamy, Abdelsamed I; Mohamed, Tarik A; El Gendy, Abd El-Nasser G; Saleh, Ibrahim A; Umeyama, Akemi

    2017-08-07

    A new 8-ionized hydroxylated 9,10-anthraquinone namely, 1-hydroxy-3-methyl-9,10-anthraquinone-6-O-β-D-glucopyranoside-8-olate (Rumpictuside A, 1) along with five known flavonoids, apigenin 7-O-β-D-glucoside (2), vitexin (3), quercetin 3-O-β-D-glucouronide (4), orientin (5), and isorientin (6) were isolated from Rumex pictus. The structures of isolated compounds were identified by the extensive spectroscopic techniques such as, UV, FT-IR, 1D, 2D NMR and HR-FAB-ESI-MS. The ionized hydroxyl group in the new anthraquinone (1) was rarely found for anthraquinone glycosides isolated from natural sources. All the isolated compounds were found inactive against influenza A virus infection. Compounds 2-6 exhibited significant antioxidant activity against DPPH and ABTS + . The alcoholic extract exhibited moderate activity while the new anthraquinone 1 showed the lowest activity against both assays. Copyright © 2017 Elsevier Ltd. All rights reserved.

  9. 42 CFR 9.10 - Occupational Health and Safety Program (OHSP) and biosafety requirements.

    Science.gov (United States)

    2010-10-01

    ... 42 Public Health 1 2010-10-01 2010-10-01 false Occupational Health and Safety Program (OHSP) and... SANCTUARY SYSTEM § 9.10 Occupational Health and Safety Program (OHSP) and biosafety requirements. (a) How are employee Occupational Health and Safety Program risks and concerns addressed? The sanctuary shall...

  10. Poly[tetraaqua(μ6-9,10-dioxo-9,10-dihydroanthracene-1,4,5,8-tetracarboxylatodimanganese(II

    Directory of Open Access Journals (Sweden)

    Rui Xu

    2012-07-01

    Full Text Available The title complex, [Mn2(C18H4O10(H2O4]n, was synthesized from manganese(II chloride tetrahydrate and 9,10-dioxo-9,10-dihydroanthracene-1,4,5,8-tetracarboxylic acid (H4AQTC in water. The anthraquinone unit is located about a crystallographic center of inversion. Each asymmetric unit therefore contains one MnII atom, two water ligands and one half AQTC4− anion. The MnII atom is coordinated in a distorted octahedral geometry by four O atoms from three AQTC4− ligands and two water O atoms. Two of the carboxylate groups coordinate one MnII atom in a chelating mode, whereas the others each coordinate two MnII atoms. Each AQTC4− tetra-anion therefore coordinates six different MnII ions and, as a result, a three-dimensional coordination polymer is formed. O—H...O hydrogen bonds, some of them bifurcated, between water ligands and neighboring water or anthraquinone ligands are observed in the crystal structure.

  11. Separation of surface, subsurface and volume fatigue damage effects in AISI 348 steel for power plant applications

    Energy Technology Data Exchange (ETDEWEB)

    Klein, Martin; Nowak, David; Walther, Frank [Technical Univ. Dortmund (Germany). Dept. of Materials Test Engineering (WPT); Starke, Peter [Saarland Univ., Saarbruecken (Germany). Chair of Non-Destructive Testing and Quality Assurance; Boller, Christian [Saarland Univ., Saarbruecken (Germany). Chair of Non-Destructive Testing and Quality Assurance; Fraunhofer IZFP, Saarbruecken (Germany)

    2016-08-01

    A wide range of industries including energy, chemistry, pharmacy, textiles, food and drink, pulp and paper, etc. is using stainless steels. Metastable austenitic steels such as used in power plants and chemical industry are subjected to cyclic mechanical and thermal loading in air as well as under the influence of corrosive media. This paper provides an overview on different nondestructive and electrochemical measurement techniques, which allow differentiating fatigue damage effects in total strain controlled multiple and constant amplitude tests with respect to damage appearance on surface, in subsurface area as well as in volume of specimens or components microstructure. In addition to conventional mechanical stress-strain hysteresis curves, electrical resistance, magnetic and open circuit potential measurements have been applied to characterize the cyclic deformation behavior of the metastable austenitic steel AISI 348 (X10CrNiNb18-9) in laboratory air and in distilled water. Based on these results obtained, the paper provides an outlook on the possibility for an efficient (remaining) fatigue life evaluation approach, which is adapted to the needs of the application areas.

  12. 75 FR 38017 - Airworthiness Directives; McDonnell Douglas Corporation Model DC-9-10 Series Airplanes, DC-9-30...

    Science.gov (United States)

    2010-07-01

    ... Airworthiness Directives; McDonnell Douglas Corporation Model DC- 9-10 Series Airplanes, DC-9-30 Series... previously to all known U.S. owners and operators of the McDonnell Douglas Corporation airplanes identified... INFORMATION: On July 15, 2009, we issued AD 2009-15-16, which applies to all McDonnell Douglas Model DC-9-10...

  13. 46 CFR 154.910 - Inert gas piping: Location.

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 5 2010-10-01 2010-10-01 false Inert gas piping: Location. 154.910 Section 154.910 Shipping COAST GUARD, DEPARTMENT OF HOMELAND SECURITY (CONTINUED) CERTAIN BULK DANGEROUS CARGOES SAFETY... Atmospheric Control in Cargo Containment Systems § 154.910 Inert gas piping: Location. Inert gas piping must...

  14. Planar conjugated polymers containing 9,10-disubstituted phenanthrene units for efficient polymer solar cells.

    Science.gov (United States)

    Li, Guangwu; Kang, Chong; Li, Cuihong; Lu, Zhen; Zhang, Jicheng; Gong, Xue; Zhao, Guangyao; Dong, Huanli; Hu, Wenping; Bo, Zhishan

    2014-06-01

    Four novel conjugated polymers (P1-4) with 9,10-disubstituted phenanthrene (PhA) as the donor unit and 5,6-bis(octyloxy)benzothiadiazole as the acceptor unit are synthesized and characterized. These polymers are of medium bandgaps (2.0 eV), low-lying HOMO energy levels (below -5.3 eV), and high hole mobilities (in the range of 3.6 × 10(-3) to 0.02 cm(2) V(-1) s(-1) ). Bulk heterojunction (BHJ) polymer solar cells (PSCs) with P1-4:PC71 BM blends as the active layer and an alcohol-soluble fullerene derivative (FN-C60) as the interfacial layer between the active layer and cathode give the best power conversion efficiency (PCE) of 4.24%, indicating that 9,10-disubstituted PhA are potential donor materials for high-efficiency BHJ PSCs. © 2014 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

  15. Strain rate effects in nuclear steels at room and higher temperatures

    Energy Technology Data Exchange (ETDEWEB)

    Solomos, G. E-mail: george.solomos@jrc.it; Albertini, C.; Labibes, K.; Pizzinato, V.; Viaccoz, B

    2004-04-01

    An investigation of strain rate, temperature and size effects in three nuclear steels has been conducted. The materials are: ferritic steel 20MnMoNi55 (vessel head), austenitic steel X6CrNiNb1810 (upper internal structure), and ferritic steel 26NiCrMo146 (bolting). Smooth cylindrical tensile specimens of three sizes have been tested at strain rates from 0.001 to 300 s{sup -1}, at room and elevated temperatures (400-600 deg. C). Full stress-strain diagrams have been obtained, and additional parameters have been calculated based on them. The results demonstrate a clear influence of temperature, which amounts into reducing substantially mechanical strengths with respect to RT conditions. The effect of strain rate is also shown. It is observed that at RT the strain rate effect causes up shifting of the flow stress curves, whereas at the higher temperatures a mild downshifting of the flow curves is manifested. Size effect tendencies have also been observed. Some implications when assessing the pressure vessel structural integrity under severe accident conditions are considered.

  16. Energetic effects of ether and ketone functional groups in 9,10-dihydroanthracene compound

    International Nuclear Information System (INIS)

    Freitas, Vera L.S.; Gomes, Jose R.B.; Ribeiro da Silva, Maria D.M.C.

    2010-01-01

    The energetic effects caused by replacing one of the methylene groups in the 9,10-dihydroanthracene by ether or ketone functional groups yielding xanthene and anthrone species, respectively, were determined from direct comparison of the standard (p o = 0.1 MPa) molar enthalpies of formation in the gaseous phase, at T = 298.15 K, of these compounds. The experimental static-bomb combustion calorimetry and Calvet microcalorimetry and the computational G3(MP2)//B3LYP method were used to get the standard molar gas-phase enthalpies of formation of xanthene, (41.8 ± 3.5) kJ . mol -1 , and anthrone, (31.4 ± 3.2) kJ . mol -1 . The enthalpic increments for the substitution of methylene by ether and ketone in the parent polycyclic compound (9,10-dihydroanthracene) are -(117.9 ± 5.5) kJ . mol -1 and -(128.3 ± 5.4) kJ . mol -1 , respectively.

  17. Pulse radiolytic one-electron reduction of 1,4-amino and hydroxy disubstituted 9,10-anthraquinones

    International Nuclear Information System (INIS)

    Pal, H.; Palit, D.K.; Mukherjee, T.; Mittal, J.P.

    1992-01-01

    The semiquinone radicals produced by one-electron reduction of 1-amino-4-hydroxy-9,10-anthraquinone and 1,4-diamino-9,10-anthraquinone have been studied in aqueous-organic mixed solvent using pulse radiolysis technique. Spectroscopic characteristics, kinetic characteristics of formation and decay, acid/base behaviour and redox characteristics of the semiquinones have been investigated and compared with those of some similar systems studied earlier. It has been shown that the variation of the disproportionation equilibria involving the reduced semiquinone radicals, the parent quinone and the fully reduced hydroquinone with pH of the solutions follow a similar trend as observed in the case of other dihydroxy quinones. Stability of the semiquinones over a broad pH range and their thermodynamic properties have been correlated. (Author)

  18. Mechanism of crack initiation and crack growth under thermal and mechanical fatigue loading

    Energy Technology Data Exchange (ETDEWEB)

    Utz, S.; Soppa, E.; Silcher, H.; Kohler, C. [Stuttgart Univ. (Germany). Materials Testing Inst.

    2013-07-01

    The present contribution is focused on the experimental investigations and numerical simulations of the deformation behaviour and crack development in the austenitic stainless steel X6CrNiNb18-10 under thermal and mechanical cyclic loading in HCF and LCF regimes. The main objective of this research is the understanding of the basic mechanisms of fatigue damage and the development of simulation methods, which can be applied further in safety evaluations of nuclear power plant components. In this context the modelling of crack initiation and crack growth inside the material structure induced by varying thermal or mechanical loads are of particular interest. The mechanisms of crack initiation depend among other things on the type of loading, microstructure, material properties and temperature. The Nb-stabilized austenitic stainless steel in the solution-annealed condition was chosen for the investigations. Experiments with two kinds of cyclic loading - pure thermal and pure mechanical - were carried out and simulated. The fatigue behaviour of the steel X6CrNiNb18-10 under thermal loading was studied within the framework of the joint research project [4]. Interrupted thermal cyclic tests in the temperature range of 150 C to 300 C combined with non-destructive residual stress measurements (XRD) and various microscopic investigations, e.g. in SEM (Scanning Electron Microscope), were used to study the effects of thermal cyclic loading on the material. This thermal cyclic loading leads to thermal induced stresses and strains. As a result intrusions and extrusions appear inside the grains (at the surface), at which microcracks arise and evolve to a dominant crack. Finally, these microcracks cause a continuous and significant decrease of residual stresses. The fatigue behaviour of the steel X6CrNiNb18-10 under mechanical loading at room temperature was studied within the framework of the research project [5], [8]. With a combination of interrupted LCF tests and EBSD

  19. Mechanism of crack initiation and crack growth under thermal and mechanical fatigue loading

    International Nuclear Information System (INIS)

    Utz, S.; Soppa, E.; Silcher, H.; Kohler, C.

    2013-01-01

    The present contribution is focused on the experimental investigations and numerical simulations of the deformation behaviour and crack development in the austenitic stainless steel X6CrNiNb18-10 under thermal and mechanical cyclic loading in HCF and LCF regimes. The main objective of this research is the understanding of the basic mechanisms of fatigue damage and the development of simulation methods, which can be applied further in safety evaluations of nuclear power plant components. In this context the modelling of crack initiation and crack growth inside the material structure induced by varying thermal or mechanical loads are of particular interest. The mechanisms of crack initiation depend among other things on the type of loading, microstructure, material properties and temperature. The Nb-stabilized austenitic stainless steel in the solution-annealed condition was chosen for the investigations. Experiments with two kinds of cyclic loading - pure thermal and pure mechanical - were carried out and simulated. The fatigue behaviour of the steel X6CrNiNb18-10 under thermal loading was studied within the framework of the joint research project [4]. Interrupted thermal cyclic tests in the temperature range of 150 C to 300 C combined with non-destructive residual stress measurements (XRD) and various microscopic investigations, e.g. in SEM (Scanning Electron Microscope), were used to study the effects of thermal cyclic loading on the material. This thermal cyclic loading leads to thermal induced stresses and strains. As a result intrusions and extrusions appear inside the grains (at the surface), at which microcracks arise and evolve to a dominant crack. Finally, these microcracks cause a continuous and significant decrease of residual stresses. The fatigue behaviour of the steel X6CrNiNb18-10 under mechanical loading at room temperature was studied within the framework of the research project [5], [8]. With a combination of interrupted LCF tests and EBSD

  20. Synthesis and Electroluminescence Properties of 3-(Trifluoromethylphenyl-Substituted 9,10-Diarylanthracene Derivatives for Blue Organic Light-Emitting Diodes

    Directory of Open Access Journals (Sweden)

    Sang Woo Kwak

    2017-10-01

    Full Text Available Diaryl-substituted anthracene derivatives containing 3-(trifluoromethylphenyl groups, 9,10-diphenyl-2-(3-(trifluoromethylphenylanthracene (1, 9,10-di([1,1′-biphenyl]-4-yl-2-(3-(trifluoromethylphenylanthracene (2, and 9,10-di(naphthalen-2-yl-2-(3-(trifluoromethylphenylanthracene (3 were synthesized and characterized. The compounds 1–3 possessed high thermal stability and proper frontier-energy levels, which make them suitable as host materials for blue organic light-emitting diodes. The electroluminescent (EL emission maximum of the three N,N-diphenylamino phenyl vinyl biphenyl (DPAVBi-doped (8 wt % devices for compounds 1–3 was exhibited at 488 nm (for 1 and 512 nm (for 2 and 3. Among them, the 1-based device displayed the highest device performances in terms of brightness (Lmax = 2153.5 cd·m−2, current efficiency (2.1 cd·A−1, and external quantum efficiency (0.8%, compared to the 2- and 3-based devices.

  1. 47 CFR 76.910 - Franchising authority certification.

    Science.gov (United States)

    2010-10-01

    ... 47 Telecommunication 4 2010-10-01 2010-10-01 false Franchising authority certification. 76.910... MULTICHANNEL VIDEO AND CABLE TELEVISION SERVICE Cable Rate Regulation § 76.910 Franchising authority certification. (a) A franchising authority must be certified by the Commission in order to regulate the basic...

  2. Pulse radiolytic one-electron reduction of 2-hydroxy- and 2,6-dihydroxy-9,10-anthraquinones

    International Nuclear Information System (INIS)

    Pal, Haridas; Mukherjee, Tulsi; Mittal, J.P.

    1994-01-01

    The semiquinone free radicals produced by one-electron reduction of 2-hydroxy-9-10-anthraquinone (2HAQ) and 2,6-dihydroxy-9,10-anthraquinone (26DHAQ) in aqueous formate solution, water-isopropyl alcohol-acetone mixed solvent and isopropyl alcohol have been studied using the pulse radiolysis technique. The absorption characteristics, kinetic parameters of formation and decay, acid-base behaviour and redox characteristics of the semiquinones have been investigated and compared with the corresponding characteristics of a few intramolecularly hydro-bonded anthrasemiquinone derivatives. The non-hydrogen-bonded semiquinones show two pKsub(a) values (4.7 and 10.7 for 2HAQ and 5.4 and 8.7 for 26DHAQ, respectively) within the pH range 1-14, whereas other intramolecularly hydrogen-bonded semiquinones show only one pKsub(a). The one-electron reduction potential (E' 7 ) values for 2HAQ (-440 mV) and 26DHAQ (- 400 mV) are more negative than those of the intramolecularly hydrogen-bonded systems. (Author)

  3. Crystal structure of tetraaquabis(8-chloro-9,10-dioxo-9,10-dihydroanthracene-1-carboxylato-κO1cobalt(II dihydrate

    Directory of Open Access Journals (Sweden)

    Wen-Juan Cai

    2014-10-01

    Full Text Available In the title complex, [Co(C15H6ClO42(H2O4]·2H2O, the CoII ion is bound by two carboxylate O atoms of two 5-chloro-9,10-anthraquinone-1-carboxylate anions and four water O atoms in a trans conformation, forming an irregular octahedral coordination geometry. This arrangement is stabilized by intramolecular O—H...O hydrogen bonds between water and carboxylate. Further O—H...O hydrogen bonds between coordinating and non-coordinating water and carboxylate produce layers of molecules that extend parallel to (001. The organic ligands project above and below the plane. Those ligands of adjacent planes are interdigitated and there are π–π interactions between them with centroid–centroid distances of 3.552 (2 and 3.767 (2 Å that generate a three-dimensional supramolecular structure.

  4. 46 CFR 176.910 - Passenger Ship Safety Certificate.

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 7 2010-10-01 2010-10-01 false Passenger Ship Safety Certificate. 176.910 Section 176... 100 GROSS TONS) INSPECTION AND CERTIFICATION International Convention for Safety of Life at Sea, 1974, as Amended (SOLAS) § 176.910 Passenger Ship Safety Certificate. (a) A vessel, which carries more than...

  5. Association of alkali and alkaline earth metal cations with radical-anions of 9-fluorenone and 9.10-anthraquinone in dimethyl formamide medium

    International Nuclear Information System (INIS)

    Karpinets, A.P.; Bezuglyj, V.D.; Svetlichnaya, T.M.

    1988-01-01

    The polarographic method is used to estimate the stability of associates formed in dimethyl formamide by the products of one-electron reduction of 9-fluorenone and 9.10-anthraquinone with cations of alkali and alkali earth metals. It is shown that the strength of 9-fluorenone and 9.10-anthraquinone radical anion associates studied increases with cation charge increase and decrease of its crystallographic radius

  6. Development of ferritic steels for steam generators of fast breeder reactors

    International Nuclear Information System (INIS)

    Nguyen-Thanh; Vigneron, G.; Vanderschaeghe, A.

    1988-01-01

    STEIN INDUSTRIE, a manufacturer of equipment for the conventional and nuclear power industry, has built up expertise in the use of Cr-Mo steels used at high temperatures. The main ferritic steels developed were 10 CD 9-10 (AFNOR), Z10 CDNb V 9-2 (AFNOR), X 20 Cr Mo V 12-1 (DIN) and ASTM Grade 9.1. For the fast breeder reactor system, STEIN INDUSTRIE proposes the use of these steels in the construction of steam generators. The wide programme of development undertaken by STEIN INDUSTRIE is aimed at the following main subjects: - characterization of materials - welding and bending tests - studies of special junctions. This article reports the results obtained

  7. Crystal structure of 2-bromo-1,4-dihydroxy-9,10-anthraquinone

    Directory of Open Access Journals (Sweden)

    Wataru Furukawa

    2014-10-01

    Full Text Available In an attempt to brominate 1,4-dipropoxy-9,10-anthraquinone, a mixture of products, including the title compound, C14H7BrO4, was obtained. The molecule is essentially planar (r.m.s. deviation = 0.029 Å and two intramolecular O—H...O hydrogen bonds occur. In the crystal, the molecules are linked by weak C—H...O hydrogen bonds, Br...O contacts [3.240 (5 Å], and π–π stacking interactions [shortest centroid–centroid separation = 3.562 (4 Å], generating a three-dimensional network.

  8. Effect of hydrostatic pressure, temperature, and solvent on the rate of the Diels-Alder reaction between 9,10-anthracenedimethanol and maleic anhydride

    Science.gov (United States)

    Kiselev, V. D.; Kornilov, D. A.; Anikin, O. V.; Latypova, L. I.; Konovalov, A. I.

    2017-03-01

    The rate of the reaction between 9,10-anthracenedimethanol and maleic anhydride in 1,4-dioxane, acetonitrile, trichloromethane, and toluene is studied at 25, 35, 45°C in the pressure range of 1-1772 bar. The rate constants, enthalpies, entropies and activation volumes are determined. It is shown that the rate of reaction with 9,10-anthracenedimethanol is approximately one order of magnitude higher than with 9-anthracenemethanol.

  9. 50 CFR 600.910 - Definitions and word usage.

    Science.gov (United States)

    2010-10-01

    ... 50 Wildlife and Fisheries 8 2010-10-01 2010-10-01 false Definitions and word usage. 600.910..., Consultation, and Recommendations § 600.910 Definitions and word usage. (a) Definitions. In addition to the... undertaken by a state agency. (b) Word usage. The terms “must”, “shall”, “should”, “may”, “may not”, “will...

  10. Philostr., Her. XXXV 9-10: ¿un testimonio de Eurísaces de Sófocles?

    Directory of Open Access Journals (Sweden)

    Miryam Librán Moreno

    2005-06-01

    Full Text Available Philostr. Her.. XXXV 9-10 may preserve hints of a rhesis from Sophocles' Eurysaces. Taking that as a departure point, a reconstruction of the general lines of this play is attempted from the evidence supplied by Accius, Pacuvius and Justin, as interpreted through the narrative pattern evinced in Oedipus at Colonus.

  11. Prevalence of overweight, obesity and thinness in 9-10 year old children in Mauritius.

    Science.gov (United States)

    Caleyachetty, Rishi; Rudnicka, Alicja R; Echouffo-Tcheugui, Justin B; Siegel, Karen R; Richards, Nigel; Whincup, Peter H

    2012-07-23

    To document the prevalence of overweight, obesity and thinness in 9-10 year old children in Mauritius. 412 boys and 429 girls aged 9-10 years from 23 primary schools were selected using stratified cluster random sampling. All data was cross-sectional and collected via anthropometry and self-administered questionnaire. Outcome measures were BMI (kg/m2), prevalence of overweight, obesity (International Obesity Task Force definitions) and thinness (low BMI for age). Linear and logistic regression analyses, accounting for clustering at the school level, were used to assess associations between gender, ethnicity, school location, and school's academic performance (average) to each outcome measure. The distribution of BMI was marginally skewed with a more pronounced positive tail in the girls. Median BMI was 15.6 kg/m2 in boys and 15.4 kg/m2 in girls, respectively. In boys, prevalence of overweight was 15.8% (95% CI: 12.6, 19.6), prevalence of obesity 4.9% (95% CI: 3.2, 7.4) and prevalence of thinness 12.4% (95% CI: 9.5, 15.9). Among girls, 18.9% (95% CI: 15.5, 22.9) were overweight, 5.1% (95% CI: 3.4, 7.7) were obese and 13.1% (95% CI: 10.2, 16.6) were thin. Urban children had a slightly higher mean BMI than rural children (0.5 kg/m2, 95% CI: 0.01, 1.00) and were nearly twice as likely to be obese (6.7% vs. 4.0%; adjusted odds ratio 1.6; 95% CI: 0.9, 3.5). Creole children were less likely to be classified as thin compared to Indian children (adjusted odds ratio 0.3, 95% CI: 0.2, 0.6). Mauritius is currently in the midst of nutritional transition with both a high prevalence of overweight and thinness in children aged 9-10 years. The coexistence of children representing opposite sides of the energy balance equation presents a unique challenge for policy and interventions. Further exploration is needed to understand the specific causes of the double burden of malnutrition and to make appropriate policy recommendations.

  12. The radiation chemistry of aqueous solutions of sodium 9,10-anthraquinone-2-sulfonate

    International Nuclear Information System (INIS)

    Burchill, C.E.; Smith, D.M.; Charlton, J.L.

    1976-01-01

    The 60 Co γ-radiolysis of aqueous solutions of sodium 9,10-anthraquinone-2-sulfonate has been studied in acidic, unbuffered, and alkaline conditions and with addition of N 2 O and 2-propanol. Mechanisms are proposed to account for the yields of H 2 O 2 and hydroxylated anthraquinone sulfonates. In neutral solution, in the absence of O 2 , the OH and e - adducts undergo preferential cross termination. Reduction of the OH adduct leads to dehydration and regeneration of the quinone. (author)

  13. Cladding nuclear steels - the application of plasma-arc hot wire surfacing

    International Nuclear Information System (INIS)

    Trarbach, K.O.

    1981-01-01

    The effect of one and two layer plasma-arc hot wire cladding on the HAZ microstructure of the fine grained structural steel 22 NiMoCr 3 7, which is similar to ASTM A 508, class 2, and steel 20 MnMoNi 5 5, similar to ASTM A 533, grade B, class 1 is determined. Attention is directed particularly to the behaviour of the susceptible region, and the consumables considered are cladding materials X 2 CrNiNb 19 9, similar to ER 347 Elc, and S-NiCr 20 Nb, similar to ER NiCr-3 (Inconel 82). Results of corrosion resistance tests show that this cladding technique can be recommended for manufacture of equipment for the chemical industry to avoid corrosion failure. Plasma-arc hot wire surfacing is also shown to be capable of depositing single or double clad layers to meet the highest safety requirements and could be applied to nuclear power plants for the special manufacture of wear resistant parts and for protection of equipment subject to a variety of corrosive environments. (U.K.)

  14. Structural and functional cardiac adaptations to a 10-week school-based football intervention for 9-10-year-old children

    DEFF Research Database (Denmark)

    Krustrup, Peter; Hansen, Peter Riis; Nielsen, Claus Malta

    2014-01-01

    -randomized into a control group that maintained their usual activities (CON; two classes, n = 51, 21 boys and 30 girls) and a football training group that performed an additional 3 × 40 min of small-sided football training per week (FT; two classes, n = 46, 23 boys and 23 girls). No baseline differences were observed......The present study investigated the cardiac effects of a 10-week football training intervention for school children aged 9-10 years using comprehensive transthoracic echocardiography as a part of a larger ongoing study. A total of 97 pupils from four school classes were cluster...

  15. One-pot Microwave-Assisted Synthesis of 1H-Phenanthro[9,10- d][1,2,3]triazole

    Directory of Open Access Journals (Sweden)

    Mehrak Faraji

    2008-09-01

    Full Text Available In this study, a fast and good yield one-pot microwave-assisted synthesis (45 seconds of 1H-phenanthro[9,10-d][1,2,3]triazole by a 1,3-dipolar cycloaddition reaction of sodium azide and 9-bromophenanthrene in the presence of potassium tert-butoxide in DMSO as solvent is reported.

  16. Clinical Outcomes for Patients with Gleason Score 9-10 Prostate Adenocarcinoma Treated With Radiotherapy or Radical Prostatectomy: A Multi-institutional Comparative Analysis.

    Science.gov (United States)

    Kishan, Amar U; Shaikh, Talha; Wang, Pin-Chieh; Reiter, Robert E; Said, Jonathan; Raghavan, Govind; Nickols, Nicholas G; Aronson, William J; Sadeghi, Ahmad; Kamrava, Mitchell; Demanes, David Jeffrey; Steinberg, Michael L; Horwitz, Eric M; Kupelian, Patrick A; King, Christopher R

    2017-05-01

    The long natural history of prostate cancer (CaP) limits comparisons of efficacy between radical prostatectomy (RP) and external beam radiotherapy (EBRT), since patients treated years ago received treatments considered suboptimal by modern standards (particularly with regards to androgen deprivation therapy [ADT] and radiotherapy dose-escalation]. Gleason score (GS) 9-10 CaP is particularly aggressive, and clinically-relevant endpoints occur early, facilitating meaningful comparisons. To compare outcomes of patients with GS 9-10 CaP following EBRT, extremely-dose escalated radiotherapy (as exemplified by EBRT+brachytherapy [EBRT+BT]), and RP. Retrospective analysis of 487 patients with biopsy GS 9-10 CaP treated between 2000 and 2013 (230 with EBRT, 87 with EBRT+BT, and 170 with RP). Most radiotherapy patients received ADT and dose-escalated radiotherapy. Kaplan-Meier analysis and multivariate Cox regression estimated and compared 5-yr and 10-yr rates of distant metastasis-free survival, cancer-specific survival (CSS), and overall survival (OS). The median follow-up was 4.6 yr. Local salvage and systemic salvage were performed more frequently in RP patients (49.0% and 30.1%) when compared with either EBRT patients (0.9% and 19.7%) or EBRT+BT patients (1.2% and 16.1%, pRadiotherapy and RP provide equivalent CSS and OS. Extremely dose-escalated radiotherapy with ADT in particular offers improved systemic control when compared with either EBRT or RP. These data suggest that extremely dose-escalated radiotherapy with ADT might be the optimal upfront treatment for patients with biopsy GS 9-10 CaP. While some prostate cancers are slow-growing requiring many years, sometimes decades, of follow-up in order to compare between radiation and surgery, high-risk and very aggressive cancers follow a much shorter time course allowing such comparisons to be made and updated as treatments, especially radiation, rapidly evolve. We showed that radiation-based treatments and surgery

  17. A mouse model of familial ALS has increased CNS levels of endogenous ubiquinol9/10 and does not benefit from exogenous administration of ubiquinol10.

    Directory of Open Access Journals (Sweden)

    Jacopo Lucchetti

    Full Text Available Oxidative stress and mitochondrial impairment are the main pathogenic mechanisms of Amyotrophic Lateral Sclerosis (ALS, a severe neurodegenerative disease still lacking of effective therapy. Recently, the coenzyme-Q (CoQ complex, a key component of mitochondrial function and redox-state modulator, has raised interest for ALS treatment. However, while the oxidized form ubiquinone10 was ineffective in ALS patients and modestly effective in mouse models of ALS, no evidence was reported on the effect of the reduced form ubiquinol10, which has better bioavailability and antioxidant properties. In this study we compared the effects of ubiquinone10 and a new stabilized formulation of ubiquinol10 on the disease course of SOD1(G93A transgenic mice, an experimental model of fALS. Chronic treatments (800 mg/kg/day orally started from the onset of disease until death, to mimic the clinical trials that only include patients with definite ALS symptoms. Although the plasma levels of CoQ10 were significantly increased by both treatments (from <0.20 to 3.0-3.4 µg/mL, no effect was found on the disease progression and survival of SOD1(G93A mice. The levels of CoQ10 in the brain and spinal cord of ubiquinone10- or ubiquinol10-treated mice were only slightly higher (≤10% than the endogenous levels in vehicle-treated mice, indicating poor CNS availability after oral dosing and possibly explaining the lack of pharmacological effects. To further examine this issue, we measured the oxidized and reduced forms of CoQ9/10 in the plasma, brain and spinal cord of symptomatic SOD1(G93A mice, in comparison with age-matched SOD1(WT. Levels of ubiquinol9/10, but not ubiquinone9/10, were significantly higher in the CNS, but not in plasma, of SOD1(G93A mice, suggesting that CoQ redox system might participate in the mechanisms trying to counteract the pathology progression. Therefore, the very low increases of CoQ10 induced by oral treatments in CNS might be not sufficient to

  18. Direct and ketone-sensitized photoconversion of 1-nitro-9,10-anthraquinone to 1-amino-9,10-anthraquinone mediated by donor radicals

    International Nuclear Information System (INIS)

    Goerner, Helmut; Gruen, Henry

    2010-01-01

    The full photoreduction of 1-nitro-2-R-9,10-anthraquinone (R = H: N1, methyl: N2) was studied in benzene, acetonitrile and acetonitrile-water mixtures in the presence of 2-propanol and triethylamine (TEA). The major photoproduct is the fluorescing 1-amino-2-R-AQ (A1, A2). The quantum yield of full reduction increases with the donor concentration, approaching Φ NH 2 =0.1. The intermediates involved are assigned on the basis of spectral and kinetic characteristics. The short-lived triplet state (≤20 ns) of N2 can be intercepted by 2-propanol or TEA, thereby forming the spectroscopically hidden donor radicals and the nitroAQ radicals which absorb at 400 and 540 nm; the latter band is due to the radical anion. The triplet state of N1 was not observed at room temperature, but the radical properties and decay in the nitrosoAQ are similar for N1 and N2. For donors in lower concentrations Φ NH 2 is strongly increased in the presence of benzophenone, acetophenone or acetone, approaching 0.22. The results under direct and sensitized conditions are compared and major dependences and the effects of mixtures of acetonitrile with water are outlined.

  19. Direct and ketone-sensitized photoconversion of 1-nitro-9,10-anthraquinone to 1-amino-9,10-anthraquinone mediated by donor radicals

    Energy Technology Data Exchange (ETDEWEB)

    Goerner, Helmut, E-mail: goerner@mpi-muelheim.mpg.de [Max-Planck-Institut fuer Bioanorganische Chemie, D-45413 Muelheim an der Ruhr (Germany); Gruen, Henry [Max-Planck-Institut fuer Bioanorganische Chemie, D-45413 Muelheim an der Ruhr (Germany)

    2010-02-18

    The full photoreduction of 1-nitro-2-R-9,10-anthraquinone (R = H: N1, methyl: N2) was studied in benzene, acetonitrile and acetonitrile-water mixtures in the presence of 2-propanol and triethylamine (TEA). The major photoproduct is the fluorescing 1-amino-2-R-AQ (A1, A2). The quantum yield of full reduction increases with the donor concentration, approaching {Phi}{sub NH{sub 2}}=0.1. The intermediates involved are assigned on the basis of spectral and kinetic characteristics. The short-lived triplet state ({<=}20 ns) of N2 can be intercepted by 2-propanol or TEA, thereby forming the spectroscopically hidden donor radicals and the nitroAQ radicals which absorb at 400 and 540 nm; the latter band is due to the radical anion. The triplet state of N1 was not observed at room temperature, but the radical properties and decay in the nitrosoAQ are similar for N1 and N2. For donors in lower concentrations {Phi}{sub NH{sub 2}} is strongly increased in the presence of benzophenone, acetophenone or acetone, approaching 0.22. The results under direct and sensitized conditions are compared and major dependences and the effects of mixtures of acetonitrile with water are outlined.

  20. 36 CFR 910.64 - Replication.

    Science.gov (United States)

    2010-07-01

    ... 36 Parks, Forests, and Public Property 3 2010-07-01 2010-07-01 false Replication. 910.64 Section 910.64 Parks, Forests, and Public Property PENNSYLVANIA AVENUE DEVELOPMENT CORPORATION GENERAL... DEVELOPMENT AREA Glossary of Terms § 910.64 Replication. Replication means the process of using modern methods...

  1. Photosensitized Oxidation of 9,10-Dimethylanthracene on Dye-Doped Silica Composites

    Directory of Open Access Journals (Sweden)

    Elim Albiter

    2012-01-01

    Full Text Available A series of cationic dyes, methylene blue (MB, safranin O (SF, toluidine blue (TB, and neutral red (NR, were successfully incorporated into a silica matrix by using ultrasound irradiation during the Stöber process. Several analyses were performed, including scanning dynamic light scattering (DLS, electron microscopy (SEM, nitrogen physisorption, FTIR spectroscopy, UV-vis, and diffuse reflectance spectroscopy. The entrapped dyes on silica were evaluated in singlet oxygen (1O2 generation under visible light irradiation, by means of the photosensitized oxidation of 9,10-dimethylanthracene (DMA. According to the results, the photocatalytic performance of the silica composites was improved, and the leakage of the dye from the particles was suppressed. Among these four different types of dye-doped silica composites, the SiO2-SF composite showed the most efficient delivery of 1O2.

  2. 14 CFR 1274.910 - Authority.

    Science.gov (United States)

    2010-01-01

    ... 14 Aeronautics and Space 5 2010-01-01 2010-01-01 false Authority. 1274.910 Section 1274.910... FIRMS Other Provisions and Special Conditions § 1274.910 Authority. Authority July 2002 This is a... authority of 42 U.S.C. 2451, et seq. (the Space Act). [End of provision] ...

  3. Diels-Alder Reactions of 12-Hydroxy-9(10®20-5aH-abeo-abieta-1(10,8(9,12(13-triene-11,14-dione

    Directory of Open Access Journals (Sweden)

    Shougang Hu

    2013-06-01

    Full Text Available 12-Hydroxy-9(10®20-5aH-abeo-abieta-1(10,8(9,12(13-triene-11,14-dione (quinone 2 served as the dienophile in numerous intermolecular Diels-Alder reactions. These cycloadditions were conducted either thermally (including microwave heating or with Lewis acid activation. While most dienes reacted with quinone 2 in good chemical yield, others were incompatible under the experimental conditions used.

  4. Study of interaction between tin dioxide nanoparticle and 1,4-dihydroxy 2,3-dimethyl 9,10-anthraquinone sensitizer

    International Nuclear Information System (INIS)

    Suvetha Rani, J.; Sasirekha, V.; Ramakrishnan, V.

    2013-01-01

    The interaction between 1,4-dihydroxy 2,3-dimethyl 9,10-anthraquinone (DHDMAQ) and tin dioxide nanoparticle (SnO 2 NPs) has been investigated using optical absorption and emission techniques. Tin dioxide nanoparticles have been synthesized by chemical precipitation method. The experimental results reveal that the fluorescence intensity of 1,4-dihydroxy 2,3-dimethyl 9,10-anthraquinone has been quenched as the concentration of the SnO 2 NPs increased. The Stern–Volmer plot indicates that SnO 2 NPs have dynamic quenching efficiency on the fluorescence nature of DHDMAQ. The obtained value of the association constant infers that there is an association between DHDMAQ and the SnO 2 nanoparticles. -- Highlights: • The interaction between DHDMAQ and SnO 2 NPs has been investigated using optical absorption and emission techniques. • The fluorescence intensity of the fluorophore has been quenched as the concentration of the SnO 2 NPs increased. • The Stern–Volmer plot indicates that SnO 2 NPs have dynamic quenching efficiency on the fluorescence nature of DHDMAQ

  5. Efficient and stable single-dopant white OLEDs based on 9,10-bis (2-naphthyl) anthracene

    International Nuclear Information System (INIS)

    Tao Silu; Peng Zhaokuai; Zhang Xiaohong; Wu Shikang

    2006-01-01

    Efficient white organic light-emitting diodes (WOLEDs) are fabricated with a thin layer of 9,10-bis (2-naphthyl) anthracene (ADN) doped with Rubrene as the source of white emission. A device with the structure of ITO/NPB (70nm)/ADN: 0.5% Rubrene (30nm)/Alq 3 (50nm)/MgAg shows a maximum current efficiency of 3.7cd/A, with the CIE coordinates of x=0.33, y=0.43. The EL spectrum of the devices and the CIE coordinates remains almost the same when the voltage is increased from 10 to 15V and the current efficiency remains quite stable with the current density increased from 20 to 250mA/cm 2

  6. Reproducibility and Relative Validity of a Short Food Frequency Questionnaire in 9-10 Year-Old Children.

    Science.gov (United States)

    Saeedi, Pouya; Skeaff, Sheila A; Wong, Jyh Eiin; Skidmore, Paula M L

    2016-05-07

    The aim of this study was to assess the reproducibility and validity of a non-quantitative 28-item food frequency questionnaire (FFQ). Children aged 9-10 years (n = 50) from three schools in Dunedin, New Zealand, completed the FFQ twice and a four-day estimated food diary (4DEFD) over a two-week period. Intraclass correlation coefficients (ICC) and Spearman's correlation coefficients (SCC) were used to determine reproducibility and validity of the FFQ, respectively. Weekly intakes were estimated for each food item and aggregated into 23 food items/groups. More than half of the food items/groups (52.2%) had an ICC ≥0.5. The median SCC between FFQ administrations was 0.66 (ranging from 0.40 for processed meat to 0.82 for sweets and non-dairy drinks). Cross-classification analysis between the first FFQ and 4DEFD for ranking participants into thirds showed that breakfast cereals had the highest agreement (54.0%) and pasta the lowest (34.0%). In validity analyses, 70% of food items/groups had a SCC ≥0.3. Results indicate that the FFQ is a useful tool for ranking children according to food items/groups intake. The low respondent burden and relative simplicity of the FFQ makes it suitable for use in large cohort studies of 9-10 year-old children in New Zealand.

  7. 5 CFR 890.910 - Provider information.

    Science.gov (United States)

    2010-01-01

    ... 5 Administrative Personnel 2 2010-01-01 2010-01-01 false Provider information. 890.910 Section 890.910 Administrative Personnel OFFICE OF PERSONNEL MANAGEMENT (CONTINUED) CIVIL SERVICE REGULATIONS..., and FEHB Benefit Payments § 890.910 Provider information. The hospital provider information used to...

  8. Hydrogenation of 2-ethyl-9,10-anthraquinone on Pd-polyaniline(SiO.sub.2./sub.) composite catalyst. The effect of humidity

    Czech Academy of Sciences Publication Activity Database

    Drelinkiewicz, A.; Waksmundzka-Góra, A.; Sobczak, J.; Stejskal, Jaroslav

    2007-01-01

    Roč. 333, č. 2 (2007), s. 219-228 ISSN 0926-860X Institutional research plan: CEZ:AV0Z40500505 Keywords : 2-ethyl-9,10- anthraquinone * polyaniline * palladium catalysts Subject RIV: CD - Macromolecular Chemistry Impact factor: 3.166, year: 2007

  9. Association between breast milk intake at 9-10 months of age and growth and development among Malawian young children.

    Science.gov (United States)

    Kumwenda, Chiza; Hemsworth, Jaimie; Phuka, John; Ashorn, Ulla; Arimond, Mary; Maleta, Kenneth; Prado, Elizabeth L; Haskell, Marjorie J; Dewey, Kathryn G; Ashorn, Per

    2018-01-19

    World Health Organization recommends exclusive breastfeeding for infants for the first 6 months of life, followed by introduction of nutritious complementary foods alongside breastfeeding. Breast milk remains a significant source of nourishment in the second half of infancy and beyond; however, it is not clear whether more breast milk is always better. The present study was designed to determine the association between amount of breast milk intake at 9-10 months of age and infant growth and development by 12-18 months of age. The study was nested in a randomized controlled trial conducted in Malawi. Regression analysis was used to determine associations between breast milk intake and growth and development. Mean (SD) breast milk intake at 9-10 months of age was 752 (244) g/day. Mean (SD) length-for-age z-score at 12 months and change in length-for-age z-score between 12 and 18 months were -1.69 (1.0) and -0.17 (0.6), respectively. At 18 months, mean (SD) expressive vocabulary score was 32 (24) words and median (interquartile range) skills successfully performed for fine, gross, and overall motor skills were 21 (19-22), 18 (16-19), and 38 (26-40), respectively. Breast milk intake (g/day) was not associated with either growth or development. Proportion of total energy intake from breast milk was negatively associated with fine motor (β = -0.18, p = .015) but not other developmental scores in models adjusted for potential confounders. Among Malawian infants, neither breast milk intake nor percent of total energy intake from breast milk at 9-10 months was positively associated with subsequent growth between 12 and 18 months, or development at 18 months. © 2018 John Wiley & Sons Ltd.

  10. 36 CFR 910.71 - Weather protection.

    Science.gov (United States)

    2010-07-01

    ... 36 Parks, Forests, and Public Property 3 2010-07-01 2010-07-01 false Weather protection. 910.71 Section 910.71 Parks, Forests, and Public Property PENNSYLVANIA AVENUE DEVELOPMENT CORPORATION GENERAL... DEVELOPMENT AREA Glossary of Terms § 910.71 Weather protection. Weather protection means a seasonal or...

  11. Features of the Diels-Alder reaction between 9,10-diphenylanthracene and 4-phenyl-1,2,4-triazoline-3,5-dione

    Science.gov (United States)

    Kiselev, V. D.; Kornilov, D. A.; Kashaeva, E. A.; Potapova, L. N.; Krivolapov, D. B.; Litvinov, I. A.; Konovalov, A. I.

    2014-12-01

    The Diels-Alder reaction between substituted anthracenes 1a-1j and 4-phenyl-1,2,4-triazoline-3,5 ( 2) is studied. In all cases except one, the reaction proceeds on the most active 9,10-atoms of substituted anthracenes. The orthogonality of the two phenyl groups at the 9,10-position of diene 1a is found to shield 9,10-reactive centers. No dienophiles with C=C bonds are shown to participate in the Diels-Alder reaction with 1a; however, the reaction 1a + 2 proceeds with the very active dienophile 2,4-phenyl-1,2,4-triazoline-3,5-dione. It is shown that attachment occurs on the less active but sterically accessible 1,4-reactive center of diene 1a. The structure of adduct 3a is proved by 1H and 13C NMR spectroscopy and X-ray diffraction analysis. The following parameters are obtained for reaction 1a + 2 ⇆ 3a in toluene at 25°C: K eq = 2120 M-1, Δ Hf ≠ = 58.6 kJ/mol, Δ Sf ≠ = -97 J/(mol K), Δ Vf ≠ = -17.2 cm3/mol, Δ Hb ≠ = 108.8 kJ/mol, Δ Sb ≠ = 7.3 J/(mol K), Δ Vb ≠ = -0.8 cm3/mol, Δ H r-n = -50.2 kJ/mol, Δ S r-n = -104.3 J/(mol K), Δ V r-n = -15.6 cm3/mol. It is concluded that the values of equilibrium constants of the reactions 1a-1j + 2 ⇆ 3a-3j vary within 4 × 101-1011 M-1.

  12. 30 CFR 910.845 - Civil penalties.

    Science.gov (United States)

    2010-07-01

    ... 30 Mineral Resources 3 2010-07-01 2010-07-01 false Civil penalties. 910.845 Section 910.845... PROGRAMS FOR THE CONDUCT OF SURFACE MINING OPERATIONS WITHIN EACH STATE GEORGIA § 910.845 Civil penalties. Part 845 of this chapter, Civil Penalties, shall apply when civil penalties are assessed for violations...

  13. 22 CFR 910.6 - Pending grievances.

    Science.gov (United States)

    2010-04-01

    ... 22 Foreign Relations 2 2010-04-01 2010-04-01 true Pending grievances. 910.6 Section 910.6 Foreign Relations FOREIGN SERVICE GRIEVANCE BOARD MISCELLANEOUS § 910.6 Pending grievances. Any grievance pending before the Board prior to February 15, 1981 shall be resolved under the provisions of the Foreign Service...

  14. 36 CFR 910.35 - Fine arts.

    Science.gov (United States)

    2010-07-01

    ... 36 Parks, Forests, and Public Property 3 2010-07-01 2010-07-01 false Fine arts. 910.35 Section 910... DEVELOPMENT AREA Standards Uniformly Applicable to the Development Area § 910.35 Fine arts. Fine arts... of art which are appropriate for the development. For information and guidance, a reasonable...

  15. In vitro antiproliferative activity of 2,3-dihydroxy-9,10-anthraquinone induced apoptosis against COLO320 cells through cytochrome c release caspase mediated pathway with PI3K/AKT and COX-2 inhibition.

    Science.gov (United States)

    Balachandran, C; Emi, N; Arun, Y; Yamamoto, N; Duraipandiyan, V; Inaguma, Yoko; Okamoto, Akinao; Ignacimuthu, S; Al-Dhabi, N A; Perumal, P T

    2016-04-05

    The present study investigated the anticancer activity of 2,3-dihydroxy-9,10-anthraquinone against different cancer cells such as MCF-7, COLO320, HepG-2, Skov-3, MOLM-14, NB-4, CEM, K562, Jurkat, HL-60, U937, IM-9 and Vero. 2,3-dihydroxy-9,10-anthraquinone showed good antiproliferative activity against COLO320 cells when compared to other tested cells. The cytotoxicity results showed 79.8% activity at the dose of 2.07 μM with IC50 value of 0.13 μM at 24 h in COLO320 cells. So we chose COLO320 cells for further anticancer studies. mRNA expression was confirmed by qPCR analysis using SYBR green method. Treatment with 2,3-dihydroxy-9,10-anthraquinone was found to trigger intrinsic apoptotic pathway as indicated by down regulation of Bcl-2, Bcl-xl; up regulation of Bim, Bax, Bad; release of cytochrome c and pro-caspases cleaving to caspases. Furthermore, 2,3-dihydroxy-9,10-anthraquinone stopped at G0/G1 phase with modulation in protein levels of cyclins. On the other hand PI3K/AKT signaling plays an important role in cell metabolism. We found that 2,3-dihydroxy-9,10-anthraquinone inhibits PI3K/AKT activity after treatment. Also, COX-2 enzyme plays a major role in colorectal cancer. Our results showed that the treatment significantly reduced COX-2 enzyme in COLO320 cells. These results indicated antiproliferative activity of 2,3-dihydroxy-9,10-anthraquinone involving apoptotic pathways, mitochondrial functions, cell cycle checkpoint and controlling the over expression genes during the colorectal cancer. Molecular docking studies showed that the compound bound stably to the active sites of Bcl-2, COX-2, PI3K and AKT. This is the first report of anticancer mechanism involving 2,3-dihydroxy-9,10-anthraquinone in COLO320 cells. The present results might provide helpful suggestions for the design of antitumor drugs toward colorectal cancer treatment. Copyright © 2016 Elsevier Ireland Ltd. All rights reserved.

  16. Quantum Mechanical/Molecular Mechanical Free Energy Simulations of the Glutathione S-Transferase (M1-1) Reaction with Phenanthrene 9,10-Oxide

    NARCIS (Netherlands)

    Ridder, L.; Rietjens, I.M.C.M.; Vervoort, J.J.M.; Mulholland, A.J.

    2002-01-01

    Glutathione S-transferases (GSTs) play an important role in the detoxification of xenobiotics in mammals. They catalyze the conjugation of glutathione to a wide range of electrophilic compounds. Phenanthrene 9,10-oxide is a model substrate for GSTs, representing an important group of epoxide

  17. 46 CFR 115.910 - Passenger Ship Safety Certificate.

    Science.gov (United States)

    2010-10-01

    ...) The route specified on the Certificate of Inspection and the SOLAS Passenger Ship Safety Certificate... 46 Shipping 4 2010-10-01 2010-10-01 false Passenger Ship Safety Certificate. 115.910 Section 115... MORE THAN 150 PASSENGERS OR WITH OVERNIGHT ACCOMMODATIONS FOR MORE THAN 49 PASSENGERS INSPECTION AND...

  18. Aggregation-enhanced emission and piezochromic luminescence of 9,10-bis(p-dibutylaminostyryl)-2,6-bis(p-t-butylstyryl)anthracene

    Energy Technology Data Exchange (ETDEWEB)

    Sun, Mingxiao; Zhang, Deteng; Li, Yiping; Wang, Jianfeng; Gao, Yangyang; Yang, Wenjun, E-mail: ywjph2004@qust.edu.cn

    2014-04-15

    A cruciform 9,10-distyrylanthracene-containing luminogen, 9,10-bis(p-dibutylaminostyryl)-2,6-bis(p-t-butylstyryl)anthracene (DDC), has been synthesized and the optical properties investigated. The results show that DDC is an aggregation-induced enhanced emission (AIEE) and piezofluorochromic (PFC) dye. The fluorescence quantum yield in THF/water=1/9 (18.1%) is about 12-fold over that in THF (1.53%). PFC experiment shows that the fluorescence colors (emission spectra) of DDC solid change reversibly between orange-red (602 nm) and red (632 nm) emissions upon pressing and annealing. Wide-angle X-ray diffraction and differential scanning calorimetric analyses reveal that the grinding has induced the phase transition of DDC solid from pristine crystalline to ground amorphous states, and annealing could cause the re-crystallization of amorphized DDC solid. This transformation between crystalline and amorphous states is responsible for the reversible PFC behavior upon external stimuli. Highlights: • A two-dimensional cross-conjugated luminogen (DDC) was synthesized. • DDC exhibits aggregation-enhanced emission and piezofluorochromic behaviors. • DDC emits bluer light in the crystalline phase than in the amorphous phase. • The PFC mechanism is ascribed to grinding-induced amorphization.

  19. Abstracts of the Mini-Symposium on Stability and Bifurcation in Fluid Motions September 9-10, 1994, Tokai, Japan

    International Nuclear Information System (INIS)

    Fujimura, Kaoru

    1995-01-01

    This is the abstracts of the Mini-Symposium on Stability and Bifurcation in Fluid Motions held on September 9-10, 1994 at the Tokai Establishment of JAERI and the Tokai Kaikan. Sixteen talks were given on various important subjects related with stability and bifurcation phenomena in fluids. All of them are theoretical and numerical analyses involving linear stability analysis, weakly nonlinear analysis, bifurcation analysis, and direct computation of nonlinearly equilibrium solutions. (author)

  20. Abstracts of the Mini-Symposium on Stability and Bifurcation in Fluid Motions September 9-10, 1994, Tokai, Japan

    Energy Technology Data Exchange (ETDEWEB)

    Fujimura, Kaoru [ed.; Japan Atomic Energy Research Inst., Tokai, Ibaraki (Japan). Tokai Research Establishment

    1995-01-01

    This is the abstracts of the Mini-Symposium on Stability and Bifurcation in Fluid Motions held on September 9-10, 1994 at the Tokai Establishment of JAERI and the Tokai Kaikan. Sixteen talks were given on various important subjects related with stability and bifurcation phenomena in fluids. All of them are theoretical and numerical analyses involving linear stability analysis, weakly nonlinear analysis, bifurcation analysis, and direct computation of nonlinearly equilibrium solutions. (author).

  1. Novel derivatives of 9,10-anthraquinone are selective algicides against the musty-odor cyanobacterium Oscillatoria perornata.

    Science.gov (United States)

    Schrader, Kevin K; Nanayakkara, N P Dhammika; Tucker, Craig S; Rimando, Agnes M; Ganzera, Markus; Schaneberg, Brian T

    2003-09-01

    Musty "off-flavor" in pond-cultured channel catfish (Ictalurus punctatus) costs the catfish production industry in the United States at least 30 million US dollars annually. The cyanobacterium Oscillatoria perornata (Skuja) is credited with being the major cause of musty off-flavor in farm-raised catfish in Mississippi. The herbicides diuron and copper sulfate, currently used by catfish producers as algicides to help mitigate musty off-flavor problems, have several drawbacks, including broad-spectrum toxicity towards the entire phytoplankton community that can lead to water quality deterioration and subsequent fish death. By use of microtiter plate bioassays, a novel group of compounds derived from the natural compound 9,10-anthraquinone have been found to be much more selectively toxic towards O. perornata than diuron and copper sulfate. In efficacy studies using limnocorrals placed in catfish production ponds, application rates of 0.3 micro M (125 micro g/liter) of the most promising anthraquinone derivative, 2-[methylamino-N-(1'-methylethyl)]-9,10-anthraquinone monophosphate (anthraquinone-59), dramatically reduced the abundance of O. perornata and levels of 2-methylisoborneol, the musty compound produced by O. perornata. The abundance of green algae and diatoms increased dramatically 2 days after application of a 0.3 micro M concentration of anthraquinone-59 to pond water within the limnocorrals. The half-life of anthraquinone-59 in pond water was determined to be 19 h, making it much less persistent than diuron. Anthraquinone-59 appears to be promising for use as a selective algicide in catfish aquaculture.

  2. Novel Derivatives of 9,10-Anthraquinone Are Selective Algicides against the Musty-Odor Cyanobacterium Oscillatoria perornata

    Science.gov (United States)

    Schrader, Kevin K.; Dhammika Nanayakkara, N. P.; Tucker, Craig S.; Rimando, Agnes M.; Ganzera, Markus; Schaneberg, Brian T.

    2003-01-01

    Musty “off-flavor” in pond-cultured channel catfish (Ictalurus punctatus) costs the catfish production industry in the United States at least $30 million annually. The cyanobacterium Oscillatoria perornata (Skuja) is credited with being the major cause of musty off-flavor in farm-raised catfish in Mississippi. The herbicides diuron and copper sulfate, currently used by catfish producers as algicides to help mitigate musty off-flavor problems, have several drawbacks, including broad-spectrum toxicity towards the entire phytoplankton community that can lead to water quality deterioration and subsequent fish death. By use of microtiter plate bioassays, a novel group of compounds derived from the natural compound 9,10-anthraquinone have been found to be much more selectively toxic towards O. perornata than diuron and copper sulfate. In efficacy studies using limnocorrals placed in catfish production ponds, application rates of 0.3 μM (125 μg/liter) of the most promising anthraquinone derivative, 2-[methylamino-N-(1′-methylethyl)]-9,10-anthraquinone monophosphate (anthraquinone-59), dramatically reduced the abundance of O. perornata and levels of 2-methylisoborneol, the musty compound produced by O. perornata. The abundance of green algae and diatoms increased dramatically 2 days after application of a 0.3 μM concentration of anthraquinone-59 to pond water within the limnocorrals. The half-life of anthraquinone-59 in pond water was determined to be 19 h, making it much less persistent than diuron. Anthraquinone-59 appears to be promising for use as a selective algicide in catfish aquaculture. PMID:12957919

  3. Elucidation of the substitution pattern of 9,10-anthraquinones through the chemical shifts of peri-hydroxyl protons

    DEFF Research Database (Denmark)

    Schripsema, Jan; Danigno, Denise

    1996-01-01

    In 9,10-anthraquinones the chemical shift of a peri-hydroxyl proton is affected by the substituents in the other benzenoid ring. These effects are additive. They are useful for the determination of substitution patterns and have been used to revise the structures of six previously reported...... anthraquinones containing methoxyl, hydroxyl, methylenedioxy and beta-methyl substituents. Because the chemical shifts of the other protons are hardly affected by substitutions in the other ring, the characteristic chemical shifts for a wide variety of substitution patterns could be derived....

  4. Hydrogen effect on different melts of steel 03Cr10Ni10Mo2(Ti,Al)

    International Nuclear Information System (INIS)

    Hruby, J.; Novosad, P.; Axamit, R.

    1984-01-01

    The effect of hydrogen on martensitic 03Cr10Ni10Mo2(Ti,Al) steel was studied following vacuum induction melting and electroslag remelting with and without the effect of radiation. Under the influence of hydrogen and under the same parameters of catodic hydrogen charging of steel after vacuum induction melting shows a 20 - 30% reduction in total ductility. Steels after electroslag remelting show a higher reduction in total ductility - within the range of 26 - 33%, i.e., 33 - 43% for different melts, and contraction Z shows a reduction of 23 - 59%. Electroslag remelted steels show a greater reduction in plasticity owing to hydrogen than steels melted in vacuum induction furnaces. The reduction of the yield point and the breaking strength owing to hydrogen are more explicit than in steel after vacuum melting. In non-irradiated hydrogenated samples a higher yield point was evident. (B.S.)

  5. 42 CFR 435.910 - Use of social security number.

    Science.gov (United States)

    2010-10-01

    ... 42 Public Health 4 2010-10-01 2010-10-01 false Use of social security number. 435.910 Section 435... of social security number. (a) The agency must require, as a condition of eligibility, that each... religious objections, refuses to obtain a Social Security Number (SSN). The identification number may be...

  6. Hot cracking of welded joints of the 7CrMoVTiB 10-10 (T/P24) steel

    Energy Technology Data Exchange (ETDEWEB)

    Adamiec, J, E-mail: janusz.adamiec@polsl.pl [Department of Materials Science, Silesian University of Technology, Krasinskiego 8, 40-019 Katowice (Poland)

    2011-05-15

    Bainitic steel 7CrMoVTiB10-10 is one the newest steels for waterwalls of modern industrial boilers. In Europe, attempts have been made to make butt welded joints of pipes made of this steel of the diameter up to 51 mm and thickness up to 8 mm. Many cracks have been observed in the welded joint, both during welding and transport and storage. The reasons of cracking and the prevention methods have not been investigated. No comprehensive research is carried out in Europe in order to automate the welding process of the industrial boiler elements made of modern bainitic steel, such as 7CrMoVTiB10-10. There is no information about its overall, operative and local weldability, influence of heat treatment, as well as about resistance of the joints to cracking during welding and use. The paper presents experience of Energoinstal SA from development of technology and production of waterwalls of boilers made of the 7CrMoVTiB 10-10 steel on a multi-head automatic welder for submerged arc welding.

  7. 13 CFR 120.910 - Borrower contributions.

    Science.gov (United States)

    2010-01-01

    ... 13 Business Credit and Assistance 1 2010-01-01 2010-01-01 false Borrower contributions. 120.910 Section 120.910 Business Credit and Assistance SMALL BUSINESS ADMINISTRATION BUSINESS LOANS Development... percent, if the Project involves the acquisition, construction, conversion, or expansion of a limited or...

  8. 9-Arylvinyl- and 9,10-bis(arylvinyl)-anthracenes with phenyl and naphthyl as aryl moieties: Differential aggregation behaviors and optoelectronic properties

    Energy Technology Data Exchange (ETDEWEB)

    Dong, Jing; Liu, Wei; Ying, Shian; Wu, Yongjin [Key Laboratory of Rubber-Plastics of Ministry of Education/Shandong Province (QUST), School of Polymer Science & Engineering, Qingdao University of Science & Technology, 53-Zhengzhou Road, Qingdao 266042 (China); Xue, Shanfeng, E-mail: sfxue@qust.edu.cn [Key Laboratory of Rubber-Plastics of Ministry of Education/Shandong Province (QUST), School of Polymer Science & Engineering, Qingdao University of Science & Technology, 53-Zhengzhou Road, Qingdao 266042 (China); State Key Laboratory of Luminescent Materials and Devices, Institute of Polymer Optoelectronic Materials and Devices, South China University of Technology, Guangzhou 510640 (China); Yang, Wenjun, E-mail: ywjph2004@qust.edu.cn [Key Laboratory of Rubber-Plastics of Ministry of Education/Shandong Province (QUST), School of Polymer Science & Engineering, Qingdao University of Science & Technology, 53-Zhengzhou Road, Qingdao 266042 (China)

    2016-08-15

    In this paper, we have synthesized our simple twisting arylvinyl anthracene derivatives, 9-styrylanthracene (ASB), 9,10-bis(styryl)anthracene (SB), 9-(2-(naph- thalen-1-yl)vinyl)anthracene (ASN) and 9,10-bis((naphthalen-1-yl)vinyl)anthracene (SN), to demonstrate the effect of skeleton symmetry on optical and optoelectronic properties. The results showed that SB and SN are weak emission with the fluorescence quantum yields (Φ) of ca. 7% but ASB and ASN are highly fluorescent (Φ≈50%) in THF solution, although they all exhibit high solid-state fluorescence efficiencies (22~50%). Grinding could induce about 20 nm of spectral shift of ASB and ASN crystalline fluorescence, but SB and SN crystals hardly exhibit mechano- fluorochromic behavior. Furthermore, the evaporated films of SB and SN are fragile due to re-crystallization soon, but those of ASB and ASN are stable and could be used as the bulk emissive layer exhibiting commendable electroluminescent performances. This finding indicates that the geometric structures of conjugated skeletons could influence the electronic and aggregate structure of organic luminogens, and then alter their optical and optoelectronic properties.

  9. 36 CFR 910.32 - Historic preservation.

    Science.gov (United States)

    2010-07-01

    ... 36 Parks, Forests, and Public Property 3 2010-07-01 2010-07-01 false Historic preservation. 910.32... DEVELOPMENT AREA Standards Uniformly Applicable to the Development Area § 910.32 Historic preservation... Preservation Plan of the Corporation, are specified for preservation, shall be acomplished (a) in accordance...

  10. 36 CFR 910.67 - Square guidelines.

    Science.gov (United States)

    2010-07-01

    ... 36 Parks, Forests, and Public Property 3 2010-07-01 2010-07-01 false Square guidelines. 910.67... GUIDELINES AND UNIFORM STANDARDS FOR URBAN PLANNING AND DESIGN OF DEVELOPMENT WITHIN THE PENNSYLVANIA AVENUE DEVELOPMENT AREA Glossary of Terms § 910.67 Square guidelines. Square Guidelines establish the Corporation's...

  11. 36 CFR 910.12 - Development density.

    Science.gov (United States)

    2010-07-01

    ... 36 Parks, Forests, and Public Property 3 2010-07-01 2010-07-01 false Development density. 910.12... DEVELOPMENT AREA Urban Planning and Design Concerns § 910.12 Development density. (a) Land would be developed... density within the building envelope delineated by specific height restrictions, but shall also establish...

  12. Isolable Triradical Trication of Hexaaza[16]paracyclophane with Embedded 9,10-Anthrylenes: A Frustrated Three-Spin System.

    Science.gov (United States)

    Kurata, Ryohei; Sakamaki, Daisuke; Uebe, Masashi; Kinoshita, Mariko; Iwanaga, Tetsuo; Matsumoto, Takashi; Ito, Akihiro

    2017-08-18

    A new derivative of hexaaza[1 6 ]paracyclophane in which p-phenylenes are alternately replaced by 9,10-anthrylenes was prepared to investigate the impact on overall π-conjugation as well as conformational change of the macrocycle. The charge and spin distribution for one-electron and three-electron oxidation of the macrocycle was elucidated by means of electrochemical, spectroelectrochemical, EPR spectroscopic, and SQUID magnetometric methods. In particular, the triradical trication was successfully isolated as an air-stable salt, and moreover, its structure was disclosed by X-ray analysis. The triradical trication was characterized as a spin-frustrated three-spin system with the antiferromagnetic exchange interaction (J/k B ≃ - 74 K).

  13. Effects of Nitrogen Content on the HAZ Softening of Ti-Containing High Strength Steels Manufactured by Accelerated Cooling

    Energy Technology Data Exchange (ETDEWEB)

    Bang, Kook-soo; Jung, Ho-shin; Park, Chan [Pukyong National University, Busan (Korea, Republic of)

    2017-03-15

    The effects of nitrogen content on the HAZ softening of Ti-containing high strength steels manufactured by accelerating cooling were investigated and interpreted in terms of the microstructures in the softening zone. Regardless of their content, all of the steels investigated showed a softened zone 9-10 mm wide. The minimum hardness in the zone, however, was different, with lower hardness in the higher nitrogen content steel. Microstructural observations of the steel showed that the amount of soft ferrite was increased in the zone with an increase of nitrogen content of the steel, suggesting that microstructural evolution in the HAZ is influenced by the nitrogen content. Measurements of TiN particles showed that the degree of particles coarsening in the HAZ was lower in the higher nitrogen content steel. Therefore, it is believed that finer TiN particles in the HAZ inhibit austenite grain growth more effectively, and lead to an accelerated ferrite transformation in higher nitrogen content steel, resulting in a higher amount of soft ferrite microstructure in the softened zone.

  14. Ocena występowania wad stóp u dzieci w wieku 9-10 lat w środowisku miejskim i wiejskim = Estimate the prevalence the feet defects in children aged 9-10 years in the urban and rural environment

    Directory of Open Access Journals (Sweden)

    Anna Plaskiewicz

    2015-04-01

    3 Wydział Kultury Fizycznej, Zdrowia i Turystyki, Uniwersytet Kazimierza Wielkiego w Bydgoszczy   Streszczenie   Wstęp. Wady stóp u dzieci są powszechnym problemem medyczno–społecznym w Polsce i na Świecie. Styl i szybkie tempo życia współczesnego człowieka wpływają niekorzystnie na postawę ciała, a stopy są szczególnie narażone na niekorzystny wpływ działania czynników środowiska zewnętrznego. Cel pracy. Celem pracy jest ocena występowania wad stóp u dzieci w wieku 9-10 lat w środowisku miejskim i wiejskim. Materiał i metody. Badaniami objęto grupę 40 dzieci w wieku 9-10 lat. Ze względu na miejsce zamieszkania dzieci podzielono na dwie grupy. Analizę stóp wykonano metodą platurograficzną polegającą na sporządzeniu odcisków podporowej powierzchni stopy. Oceniano wskaźniki opisujące wady stóp tj: wskaźnik „Ky” Sztritera-Godunowa, wskaźnik kątowy Clarke’a (CI, wskaźnik Wejsfloga, kąt piętowy oraz kąt koślawości palucha. Wyniki. Wśród przebadanych dzieci najczęstszą wadą stóp było płaskostopie. Zaobserwowano minimalnie mniej wad stóp u dzieci ze wsi w porównaniu z dziećmi mieszkającymi w mieście, jednak różnice nie są istotne statystycznie. Nie zaobserwowano różnic związanych z występowaniem wad stóp pomiędzy dziećmi ze wsi i z miasta. Wnioski. 1. Większość dzieci zarówno z miasta (65% jak i ze wsi (75% ma prawidłowo ukształtowane stopy. 2. Najczęstszą wadą stóp występującą wśród przebadanych dzieci jest płaskostopie. 3. Nie zaobserwowano istotnych różnic statystycznych w ocenie stóp pomiędzy dziećmi mieszkającymi w środowisku miejskim i wiejskim.   Abstract   Introduction. Feet defects in children is a common socio-medical problem in Poland and the world. Lifestyle of modern man adversely affect posture. The feet are particularly vulnerable to the adverse effects factors the external environment. Aim of the study. The aim of the study is to estimate the

  15. 30 CFR 910.819 - Special performance standards-auger mining.

    Science.gov (United States)

    2010-07-01

    ... 30 Mineral Resources 3 2010-07-01 2010-07-01 false Special performance standards-auger mining. 910.819 Section 910.819 Mineral Resources OFFICE OF SURFACE MINING RECLAMATION AND ENFORCEMENT, DEPARTMENT OF THE INTERIOR PROGRAMS FOR THE CONDUCT OF SURFACE MINING OPERATIONS WITHIN EACH STATE GEORGIA § 910...

  16. Chiral synthesis of (Z)-3-cis-6,7-cis-9,10-diepoxyhenicosenes, sex pheromone components of the satin moth, Leucoma salicis.

    Science.gov (United States)

    Wimalaratne, Priyantha D C; Slessor, Keith N

    2004-06-01

    All four isomers of (Z)-3-cis-6,7-cis-9,10-diepoxyhenicosenes, 1-4, have been synthesized using D-xylose as the chirally pure starting material. D-Xylose was first converted to 2-deoxy-4,5-O-isopropylidene-3-t-butyldimethylsilyl-D-threopentose 11, via several steps of selective protection, dehydroxylation, and deprotection. Wittig coupling of 11 with nonyltriphenylphosphonium bromide followed by hydrogenation and acid catalyzed deprotection of hydroxyl groups yielded the chiral (2R,3R)-1,2,3-triol, 14, which was used as the precursor for the C-8 to C-21 unit of the (Z)-3-cis-6,7-cis-9,10-diepoxyhenicosenes. Selective tosylation of 14 followed by stereospecific cyclization yielded (2R,3R)-1,2-epoxytetradecan-3-ol, 16, which was then divergently converted to the t-butyldimethylsilyl ether 17 and tosylate 22, respectively. Establishment of the C-5 through C-7 unit of the target molecules was accomplished via regiospecific coupling of 17 with 1-t-butyldimethylsiloxy-2-propyne to form 18. Stepwise transformation of 18 via the formation of tosylate 19, desilylation, and stereospecific cyclization to form epoxy alcohol 20, followed by P2-Ni reduction yielded a key intermediate, allylic epoxy alcohol (Z)-2-(5S,6R)-cis-5,6-epoxyheptadecen-1-ol, 21. Similarly, the coupling of 22 with 1-t-butyldimethylsiloxy-2-propyne yielded 23, which was stereospecifically cyclized to form 24. Desilylation and P2-Ni reduction of 24 gave the antipodal intermediate, (Z)-2-(5R,6S)-cis-5,6-epoxyheptadecen-1-ol, 26. Asymmetric epoxidation of antipodes 21 and 26 with (L)- or (D)-diethyl tartrates resulted in the formation of diepoxy alcohols 27 and 29 from 21, and 33 and 31 from 26, respectively. Tosylation of these diepoxy alcohols followed by coupling with lithium dibutenyl cuprate yielded the four stereoisomers of (Z)-3-cis-6,7-cis-9,10-diepoxyhenicosenes, 1-4. Analysis of the retention characteristics of these materials revealed that one or both of the S*,R*,S*,R* stereoisomers comprise the

  17. Mechanical And Microstructural Evaluation Of A Wear Resistant Steel

    International Nuclear Information System (INIS)

    Santos, F.L.F. dos; Vieira, A.G.; Correa, E.C.S.; Pinheiro, I.P.

    2010-01-01

    In the present work, the analysis of the mechanical properties and the microstructural features of a high strength low alloy steel, containing chromium, molybdenum and boron, subjected to different heat treatments, was conducted. After austenitizing at 910 deg C for 10 minutes, three operations were carried out: oil quenching, oil quenching followed by tempering at 200 deg C for 120 minutes and austempering at 400 deg C for 5 minutes followed by water cooling. The analysis was performed through tensile and hardness tests, optical microscopy and X-ray diffraction. The bainitic structure led to high strength and toughness, both essential mechanical properties for wear resistant steels. The occurrence of allotriomorphic ferrite and retained austenite in the samples also increased the wear resistance. This phenomenon is related to the fact that both structures are able to be deformed and, in the case of the retained austenite, the transformation induced plasticity TRIP effect may take place as the material is used. (author)

  18. Experimental Investigation on Tool Wear Behavior and Cutting Temperature during Dry Machining of Carbon Steel SAE 1030 Using KC810 and KC910 Coated Inserts

    Directory of Open Access Journals (Sweden)

    Y. Tamerabet

    2018-03-01

    Full Text Available The removal of cutting fluids and lubrication in dry machining operations requires a good knowledge and full control of all the mechanisms that lead to tool damage. In order to optimize dry machining operations, it is necessary to clearly identify the wear patterns, determine the contact conditions and define the relationship between the contact parameters and the operating conditions. The idea is to choose optimal cutting conditions which lead to the best contact conditions limiting the triggering or aggravation of wear phenomena. The purpose of this paper is to determine the impact multilayer coatings and cutting parameters on tool wear and temperature at the tool-chip interface for two types of coated carbides (KC810 and KC910 Commercialized inserts during dry turning operation of carbon steel SAE 1030, in order to determine the ideal parameters and guarantee the best performances of the cutting tools. Cutting temperature, Crater and Flank wear have been systematically recorded in order to determine their influence on tool life time. To ensure the optimum choice of machining conditions; the TAGUCHI method associated to multi-factorial method were applied to plan the experiments. It has been noted that cutting speed was the most influential factor on temperature and wear evolution. We noted also that the KC810 insert was more suitable for machining of SAE 1030 Carbon Steel; where The best life time was registered (T=228 min. The KC810 inserts offer 30 min of additional machining time for the same work conditions.

  19. Selected Abstracts of the 2nd International Workshop “Intensive Care of the Newborn”; Verona (Italy); March 9-10, 2018

    OpenAIRE

    --- Various Authors

    2018-01-01

    Selected Abstracts of the 2nd International Workshop “Intensive Care of the Newborn”; Verona (Italy); March 9-10, 2018CONGRESS PRESIDENTPaolo Biban  Guest Editor: Paolo BibanABS 1. DOES DELAYED CORD CLAMPING (DCC) AFFECT UMBILICAL CORD pH IN PRETERM INFANTS? • V.M. Samedi, L. Irvine, S. Thomas, D. Kowal, J. Rabi, A. Stritzke, N. Singhal, A. Abou MehremABS 2. SNAP-PE SCORE. MORBIDITY AND MOR­TALI­TY INDEX IN NICUs • A. Konstantinidi, R. Sokou, S. Parastatidou, A. Tsantes, N. IacovidouABS 3. EA...

  20. Proceedings of the Special Demonstration Workshop for Integrating Blind Children with Sighted Children into Ongoing Physical Education and Recreation Programs (Cleveland, Ohio, October 9-10, 1969).

    Science.gov (United States)

    Boninger, Walter B., Ed.

    A special education workshop (Cleveland, Ohio, October 9-10, 1969) for integrating blind children with sighted children into ongoing physical education and recreation programs is described. Physical education and blind children from the viewpoint of opthalmology, social and psychological aspects of blindness as they relate to participation in…

  1. A cross-sectional study of frequency and factors associated with dog walking in 9-10 year old children in Liverpool, UK.

    Science.gov (United States)

    Westgarth, Carri; Boddy, Lynne M; Stratton, Gareth; German, Alexander J; Gaskell, Rosalind M; Coyne, Karen P; Bundred, Peter; McCune, Sandra; Dawson, Susan

    2013-09-10

    Owning a pet dog could potentially improve child health through encouraging participation in physical activity, through dog walking. However, evidence to support this is limited and conflicting. In particular, little is known about children's participation in dog walking and factors that may be associated with this. The objective of this study was to describe the participation of children in dog walking, including their own and those belonging to somebody else, and investigate factors associated with regular walking with their own pet dog. Primary school children (n=1021, 9-10 years) from a deprived area of Liverpool were surveyed during a 'fitness fun day' as part of the SportsLinx project. The 'Child Lifestyle and Pets' survey included questions about pet ownership, pet attachment, and dog walking. Multivariable logistic regression models were used to investigate factors associated with walking any dog, or their own dog, several times a day or more, including level of attachment to the dog, dog type, and sociodemographic factors. Overall, 15.4% of children reported walking with any dog (their own or belonging to a friend or family member) ≥ once daily, 14.1% several times a week, 27.6% ≤ once a week, and 42.8% never. Dog owning children (37.1% of the population) more often reported dog walking 'several times a week or more' (OR=12.30, 95% CI=8.10-18.69, Ppet dogs may be an opportunity for increasing physical activity in 9-10 year old children. The identification of stronger attachment to dogs regularly walked is similar to findings in adult studies.

  2. Long-term behaviour of heat-resistant steels and high-temperature materials

    International Nuclear Information System (INIS)

    1987-01-01

    This book contains 10 lectures with the following subjects: On the effect of thermal pretreatment on the structure and creep behaviour of the alloy 800 H (V. Guttmann, J. Timm); Material properties of heat resistant ferritic and austenitic steels after cold forming (W. Bendick, H. Weber); Investigations for judging the working behaviour of components made of alloy 800 and alloy 617 under creep stress (H.J. Penkalla, F. Schubert); Creep behaviour of gas turbine materials in hot gas (K.H. Kloos et al.); Effect of small cold forming on the creep beahviour of gas turbine blades made of Nimonic 90 (K.H. Keienburg et al.); Investigations on creep fatigue alternating load strength of nickel alloys (G. Raule); Change of structure, creep fatigue behaviour and life of X20 Cr Mo V 12 1 (by G. Eggeler et al.); Investigations on thermal fatigue behaviour (K.H. Mayer et al.); Creep behaviour of similar welds of the steels 13 Cr Mo 4 4, 14 MoV 6 3, 10 Cr Mo 910 and GS-17 Cr Mo V 5 11 (K. Niel et al.); Determining the creep crack behaviour of heat resistant steels with samples of different geometry (K. Maile, R. Tscheuschner). (orig.,/MM) [de

  3. The design of steel string crane with lifting capacity 10 tons

    International Nuclear Information System (INIS)

    Syamsurrijal Ramdja

    2007-01-01

    The steel string (sling) used for lift Crane of type of Overhead Travelling Crane, with capacities lifting 10 ton are designed. If compared to other string type, string of steel have some excellence. At this design, election of type of string become primary and the factor of safety become prima facie matter with pursuant to up to date standard. From made of design, is hence got by specification and age of steel string. (author)

  4. Designing Efficient Solar-Thermal Fuels with [n.n](9,10)Anthracene Cyclophanes: A Theoretical Perspective.

    Science.gov (United States)

    Ganguly, Gaurab; Sultana, Munia; Paul, Ankan

    2018-01-18

    Molecular solar thermal storage (MOST) systems have been largely limited to three classes of molecular motifs: azo-benzene, norbornadiene, and transition metal based fulvalene-tetracarbonyl systems. Photodimerization of anthracene has been known for a century; however, this photoprocess has not been successfully exploited for MOST purposes due to its poor energy storage. Using well-calibrated theoretical methods on a series of [n.n](9,10)bis-anthracene cyclophanes, we have exposed that they can store solar energy into chemical bonds and can release in the form of heat energy on demand under mild conditions. The storage is mainly attributed to the strain in the rings formed by the alkyl linkers upon photoexcitation. Our results demonstrate that the gravimetric energy storage density for longer alkyl-chain linkers (n > 3) are comparable to those for the best-known candidates; however, it lacks some of the deleterious attributes of known systems, thus making the proposed molecules desirable targets for MOST applications.

  5. Modeling the effect of creep deterioration on magnetic properties in heat-resistant steels

    Energy Technology Data Exchange (ETDEWEB)

    Zhang, S.Z.; Tu, S.T., E-mail: sttu@ecust.edu.cn

    2014-11-15

    Abstracts: The hysteresis parameters of the Jiles–Atherton model are modified to elucidate the variation of magnetic properties with creep deterioration based on a consideration of the effect of pinning of magnetic domain walls on the grain boundaries, dislocations as well as precipitates in short-term creep process. Experiments are carried out to evaluate the magnetic hysteresis curves of 10CrMo910 specimens with controlled levels of creep-induced damage. An intelligent optimization algorithm is used to determine the hysteresis parameters of Jiles–Atherton model. The microstructure parameters of the crept specimens are determined by a quantitative metallographic analysis. The modified model is applied to correlate the experimental data of both 10CrMo910 and 410 stainless steel creep specimens. The calculated results are in good agreement with the measured data of the hysteresis parameters. - Highlights: • The hysteresis parameters in the Jiles–Atherton model are modified to account for the effect of creep deterioration. • Magnetic properties are greatly affected by the precipitation and dislocations during creep. • Good consistency is obtained between the experimental and theoretical results of hysteresis parameters.

  6. The most luminous z ∼ 9-10 galaxy candidates yet found: The luminosity function, cosmic star-formation rate, and the first mass density estimate at 500 Myr

    International Nuclear Information System (INIS)

    Oesch, P. A.; Illingworth, G. D.; Magee, D.; Bouwens, R. J.; Labbé, I.; Smit, R.; Franx, M.; Van Dokkum, P. G.; Momcheva, I.; Ashby, M. L. N.; Fazio, G. G.; Huang, J.-S.; Willner, S. P.; Gonzalez, V.; Trenti, M.; Brammer, G. B.; Skelton, R. E.; Spitler, L. R.

    2014-01-01

    We present the discovery of four surprisingly bright (H 160 ∼ 26-27 mag AB) galaxy candidates at z ∼ 9-10 in the complete HST CANDELS WFC3/IR GOODS-N imaging data, doubling the number of z ∼ 10 galaxy candidates that are known, just ∼500 Myr after the big bang. Two similarly bright sources are also detected in a reanalysis of the GOODS-S data set. Three of the four galaxies in GOODS-N are significantly detected at 4.5σ-6.2σ in the very deep Spitzer/IRAC 4.5 μm data, as is one of the GOODS-S candidates. Furthermore, the brightest of our candidates (at z = 10.2 ± 0.4) is robustly detected also at 3.6 μm (6.9σ), revealing a flat UV spectral energy distribution with a slope β = –2.0 ± 0.2, consistent with demonstrated trends with luminosity at high redshift. Thorough testing and use of grism data excludes known low-redshift contamination at high significance, including single emission-line sources, but as-yet unknown low redshift sources could provide an alternative solution given the surprising luminosity of these candidates. Finding such bright galaxies at z ∼ 9-10 suggests that the luminosity function for luminous galaxies might evolve in a complex way at z > 8. The cosmic star formation rate density still shows, however, an order-of-magnitude increase from z ∼ 10 to z ∼ 8 since the dominant contribution comes from low-luminosity sources. Based on the IRAC detections, we derive galaxy stellar masses at z ∼ 10, finding that these luminous objects are typically 10 9 M ☉ . This allows for a first estimate of the cosmic stellar mass density at z ∼ 10 resulting in log 10  ρ ∗ =4.7 −0.8 +0.5 M ☉ Mpc –3 for galaxies brighter than M UV ∼ –18. The remarkable brightness, and hence luminosity, of these z ∼ 9-10 candidates will enable deep spectroscopy to determine their redshift and nature, and highlights the opportunity for the James Webb Space Telescope to map the buildup of galaxies at redshifts much earlier than z ∼ 10.

  7. Quinoidal Oligo(9,10-anthryl)s with Chain-Length-Dependent Ground States: A Balance between Aromatic Stabilization and Steric Strain Release

    KAUST Repository

    Lim, Zhenglong

    2015-11-12

    Quinoidal π-conjugated polycyclic hydrocarbons have attracted intensive research interest due to their unique optical/electronic properties and possible magnetic activity, which arises from a thermally excited triplet state. However, there is still lack of fundamental understanding on the factors that determine the electronic ground states. Herein, by using quinoidal oligo(9,10-anthryl)s, it is demonstrated that both aromatic stabilisation and steric strain release play balanced roles in determining the ground states. Oligomers with up to four anthryl units were synthesised and their ground states were investigated by electronic absorption and electron spin resonance (ESR) spectroscopy, assisted by density functional theory (DFT) calculations. The quinoidal 9,10-anthryl dimer 1 has a closed-shell ground state, whereas the tri- (2) and tetramers (3) both have an open-shell diradical ground state with a small singlet-triplet gap. Such a difference results from competition between two driving forces: the large steric repulsion between the anthryl/phenyl units in the closed-shell quinoidal form that drives the molecule to a flexible open-shell diradical structure, and aromatic stabilisation due to the gain of more aromatic sextet rings in the closed-shell form, which drives the molecule towards a contorted quinoidal structure. The ground states of these oligomers thus depend on the overall balance between these two driving forces and show chain-length dependence. © 2015 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

  8. Polyether precursors of molecular recognition systems based on the 9,10-anthraquinone moiety

    Science.gov (United States)

    Wcisło, Anna; Cirocka, Anna; Zarzeczańska, Dorota; Niedziałkowski, Paweł; Nakonieczna, Sandra; Ossowski, Tadeusz

    2015-02-01

    A series of novel polyether derivatives of 9,10-anthraquinone (AQ) was synthesized and characterized by means of UV-Vis spectroscopy, acid-base titration and complexometric titration. The results were compared with 1-NEt2AQ and 1-NHEtAQ - model compounds of alkylaminoanthraquinones. Acetonitrile and methanol were used as solvents for determination of spectroscopic and acid-base properties. Complexometric titrations were carried out exclusively in acetonitrile. Spectral characteristic of these compounds strongly depends on pH. Addition of acid causes the decrease of absorption intensity and in some cases also a shift of the visible range band. The weakest base is the compound (2), and the strongest - compound (1), both in methanol and acetonitrile solution. The introduction of an additional substituent in the position 8 of the anthraquinone compound increases its basicity. The presence of metal ions causes changes in intensity of absorption (decrease for compounds (2) and (3) and increase with bathochromic shift for (1) and (4)). For the determination of the coordination properties aluminum (III) ions were chosen. The highest complex stability constant with Al (III) ions is observed for compound (1), and the weakest for compound (3). The elongation of the polyether chain decreases the stability of the complex formed.

  9. 9,10-Anthraquinone deposit in tea plantation might be one of the reasons for contamination in tea.

    Science.gov (United States)

    Wang, Xuan; Zhou, Li; Luo, Fengjian; Zhang, Xinzhong; Sun, Hezhi; Yang, Mei; Lou, Zhengyun; Chen, Zongmao

    2018-04-01

    9,10-Anthraquinone (AQ) was a new contaminant, with unknown sources, occurred globally in tea. European Union (EU) fixed the maximum residue limit (MRL) of 0.02mg/kg. The pollution source of AQ in tea was traced from the view of AQ deposit on tea crop by simulation. The possible contamination pathway and main factors to decrease AQ were explored in tea cultivation- tea manufacture- tea infusion, on the basis of AQ analytical methods by using solvent extraction and gas chromatography-tandem mass spectrometry (GC-MS/MS) quantification. 58.8-84.6% of AQ degraded in tea processing, and drying played a key role to reduce the AQ contamination. Certain concentration of AQ deposited on tea shoots could resulted in AQ beyond the MRL of 0.02mg/kg in tea. AQ leaching into tea brew (about 10%) could lead to the possible health risk. AQ deposit on tea crop during the tea cultivation might cause the AQ contamination in tea. Copyright © 2017. Published by Elsevier Ltd.

  10. Ductile fracture of two-phase welds under 77K. [Steel-EhP810, steel-EhP666, steel-08Kh18N10T, steel-EhP659-VI, steel-chP810

    Energy Technology Data Exchange (ETDEWEB)

    Yushchenko, K.A.; Voronin, S.A.; Pustovit, A.I.; Shavel' , A.V.

    The effect of the type of welding and fillers on crack resistance of welded joints high-strength steel EhP810 and its various compounds with steels EhP666, 08Kh18N10T has been studied. For the welding of steel EhP810 with steels EhP810, EhP666, 08Kh18N10T electron-beam, automatic, argon tungsten arc with non-consumable electrode with various fillers, as well as argon metal-arc welding with consumable electrode, were used. It is shown, that for a joint, made by electron-beam welding, parameters sigmasub(u), Ksub(IcJ), KCV are higher than for a joint of a similar phase structure made using filler wire EhP659-VI. It is explained by the fact, that during electron-beam welding joint metal refining takes place, which removes gases. In welded joints of chP810 steel, having joints with austenitic structure, characteristic of crack resistance Ssub(c) increases by more than 0.2 mm in contrast to two-phase joints, which conventional yield strength at 77 K exceeds 1000 MPa. It is worth mentioning, that for other classes of steels formation of two-phase structure of joint increases welded joint resistance to brittle fracture. It is possible to obtain the required structure of joint with assigned level of resistance to brittle fracture by means of the use of different fillers, optimum and welding procedure, regulating the part of the basic metal in joint content.

  11. 36 CFR 910.18 - Vehicular circulation and storage systems.

    Science.gov (United States)

    2010-07-01

    ... storage systems. 910.18 Section 910.18 Parks, Forests, and Public Property PENNSYLVANIA AVENUE DEVELOPMENT... storage systems. (a) Improvement of the existing vehicular storage and circulation system is necessary in order to create the balanced transportation system called for in the Plan, which recognizes the need to...

  12. 30 CFR 910.785 - Requirements for permits for special categories of mining.

    Science.gov (United States)

    2010-07-01

    ... of mining. 910.785 Section 910.785 Mineral Resources OFFICE OF SURFACE MINING RECLAMATION AND ENFORCEMENT, DEPARTMENT OF THE INTERIOR PROGRAMS FOR THE CONDUCT OF SURFACE MINING OPERATIONS WITHIN EACH STATE GEORGIA § 910.785 Requirements for permits for special categories of mining. Part 785 of this...

  13. 29 CFR 780.910 - Engagement in transportation and preparation.

    Science.gov (United States)

    2010-07-01

    ... 29 Labor 3 2010-07-01 2010-07-01 false Engagement in transportation and preparation. 780.910... Requirements Under Section 13(b)(16) Exempt Operations on Fruits Or Vegetables § 780.910 Engagement in... activities, an employee who engages in both is performing exempt work. In referring to “the transportation...

  14. Spectrophotometric determination of ruthenium (III) and rhodium (III) with 9,10-phenanthrenequinone monoxime after extraction into molten naphthalene

    International Nuclear Information System (INIS)

    Wasey, A.; Bansal, R.K.; Puri, B.K.; Satake, Masatada.

    1983-01-01

    9,10-Phenanthrenequinone monoxime has been used as a reagent for the spectrophotometric determination of ruthenium(III) and rhodium(III) after extraction into molten naphthalene. The extracted mixture of the metal complex and naphthalene was dissolved in chloroform and ruthenium and rhodium were determined spectrophotometrically. Beer's law holds in the concentration range of 0.2-4.1 μg/cm 3 for ruthenium and 0.3-5.3 μg/cm 3 for rhodium in 10 cm 3 of the final solution. The molar absorptivities and Sandell sensitivities are calculated to be 9.70 x 10 3 l mol -1 cm -1 and 0.01 μg/cmsup(2 ) (660 nm) for ruthenium and 1.13 x 10 4 l mol -1 cm -1 and 0.009 μg/cm 2 (410 nm) for rhodium respectively. Aliquots containing 2.0 μg of ruthenium and 4.1 μg of rhodium give mean absorbances of 0.192 and 0.451 with standard deviations of 0.0017 and 0.0039, respectively. Interference of various ions has been studied and the method has been applied to the determination of ruthenium and rhodium in various synthetic mixtures. This procedure is also applied to the simultaneous determination of ruthenium and rhodium present together in a solution. (author)

  15. Composition and corrosion properties of high-temperature oxide films on steel type 18-10

    International Nuclear Information System (INIS)

    Vakulenko, B.F.; Morozov, O.N.; Chernysheva, M.V.

    1985-01-01

    The composition and propeties of oxide films, formed in the process of tube production of steel type 18-10, as well as the behaviour of the steels coated with oxide films under operating conditions of NPP heat-exchange equipment at the 20-300 deg C temperatures are determined. It is found, that the films have a good adhesion to the steel surface and repeat the metal structure without interfering with, the surface defect determination. Introduction of the NaNO 2 corrosion inhibitor decreases the film destruction rate to the level of the base metal corrosion. It is found acceptable to use tubes of steel 18-10 coated with dense oxide films in the heat-exchange and water supply systems of NPP

  16. The HUPO Brain Proteome project wish list--summary of the 9(th) HUPO BPP Workshop 9-10 January 2008, Barbados.

    Science.gov (United States)

    Hamacher, Michael; Eisenacher, Martin; Tribl, Florian; Stephan, Christian; Marcus, Katrin; Hardt, Tanja; Wiltfang, Jens; Martens, Lennart; Desiderio, Dominic; Gutstein, Howard; Park, Young Mok; Meyer, Helmut E

    2008-06-01

    The Human Brain Proteome Project (HUPO BPP) aims at advancing knowledge and the understanding of neurodiseases and aging with the purpose of identifying prognostic and diagnostic biomarkers, as well as to push new diagnostic approaches and medications. The participating groups meet in semi-annual workshops to discuss the progress, as well as the needs, within the field of proteomics. The 9(th) HUPO BPP workshop took place in Barbados from 9-10 January, 2008. Discussing the future HUPO BPP Roadmap, the attendees drafted the so called HUPO BPP wish list containing timelines, suggestions and missions. This wish list will be updated regularly and will serve as a guideline for the next phase.

  17. Luminescent Study of the Binding Interaction on 1,4-Dihydroxy-2,3-Dimethyl-9,10-Anthraquinone with Titanium Dioxide Nanoparticles

    Science.gov (United States)

    Pushpam, S.; Yamini, D.; Ramakrishnan, V.

    2014-07-01

    The photophysical properties of 1,4-dihydroxy-2,3-dimethyl-9,10-anthroquinone (DHDMAQ) in the absence and presence of titanium dioxide (TiO2) nanoparticles have been studied using UV-visible absorption spectroscopy and steady-state fluorescence spectroscopy. The fluorescence intensity of the DHDMAQ decreases as the concentration of TiO2 nanoparticles increases. The quenching is characterized by a Stern-Volmer plot, which displays a positive deviation from linearity. This could be explained by static quenching models. The Stern-Volmer quenching constant, association constant, and binding constant have been calculated. The distance between DHDMAQ and TiO2 nanoparticles has also been evaluated using Forster's theory of non-radiative energy transfer.

  18. Ductility, strength and hardness relation after prior incremental deformation (ratcheting) of austenitic steel

    International Nuclear Information System (INIS)

    Kussmaul, K.; Diem, H.K.; Wachter, O.

    1993-01-01

    Experimental investigations into the stress/strain behavior of the niobium stabilized austenitic material with the German notation X6 CrNiNb 18 10 proved that a limited incrementally applied prior deformation will reduce the total deformation capability only by the amount of the prior deformation. It could especially be determined on the little changes in the reduction of area that the basically ductile deformation behavior will not be changed by the type of the prior loading. There is a correlation between the amount of deformation and the increase in hardness. It is possible to correlate both the changes in hardness and the material properties. In the case of low cycle fatigue tests with alternating temperature an incremental increase in total strain (ratcheting) was noted to depend on the strain range applied

  19. Nucleoside adducts from the in vitro reaction of benzo[a]pyrene-7,8-dihydrodiol 9,10-oxide or benzo[a]pyrene 4,5-oxide with nucleic acids.

    Science.gov (United States)

    Jennette, K W; Jeffrey, A M; Blobstein, S H; Beland, F A; Harvey, R G; Weinstein, I B

    1977-03-08

    The covalent binding of benzo[a]pyrene 4,5-oxide and benzo[a]pyrene-7,8-dihydrodiol 9,10-oxide isomer I and isomer II to nucleic acids in aqueous acetone solution has been investigated. Benzo[a]pyrene 4,5-oxide reacted preferentially with guanosine residues. On the other hand, benzo[a]pyrene-7,8-dihydrodiol 9,10-oxide isomer I and II reacted extensively with guanosine, adenosine, and cytidine residues. Time course studies showed that the reactivity of isomer I or isomer II with homopolyribonucleotides followed the order poly(G) greater than poly(A) greater than poly(C). Alkaline or enzymatic hydrolysis of the modified nucleic acids and subsequent chromatography on Sephadex LH-20 columns yielded benzo[a]pyrene-nucleotide adducts. These were enzymatically converted to the corresponding nucleosides which were resolved into several distinct components by high-pressure liquid chromatography. Evidence was obtained for the presence of multiple nucleoside adducts of guanosine, adenosine, cytidine, deoxyguanosine, deoxyadenosine, and deoxycytidine. The HPLC profiles of adducts formed with isomer I were different from the corresponding profiles of adducts formed with isomer II. Structural aspects of these nucleoside adducts are discussed.

  20. Improved efficiency in organic light-emitting devices with tris-(8-hydroxyquinoline) aluminium doped 9,10-di(2-naphthyl) anthracene emission layer

    Energy Technology Data Exchange (ETDEWEB)

    Yuan Yongbo; Lian Jiarong; Li Shuang; Zhou Xiang [State Key Lab of Optoelectronic Materials and Technologies, Sun Yat-Sen University, Guangzhou, 510275 (China)], E-mail: stszx@mail.sysu.edu.cn

    2008-11-21

    Organic light-emitting devices with tris-(8-hydroxyquinoline) aluminium (Alq{sub 3}) doped 9,10-di(2-naphthyl) anthracene (ADN) as the emission layer (EML) have been fabricated. These devices exhibit efficient electroluminescence (EL) originated from the Alq{sub 3} as the mass ratio of Alq{sub 3} to ADN was varied from 1 to 50%. The devices with an optimal Alq{sub 3} mass ratio of 10 wt% showed a peak EL efficiency and an external quantum efficiency of 9.1 cd A{sup -1} and 2.7% at a luminance of 1371 cd m{sup -2}, which is improved by a factor of 2.2 compared with 4.1 cd A{sup -1} and 1.2% at a luminance of 3267 cd m{sup -2} for conventional devices with the neat Alq{sub 3} as the EML.

  1. 30 CFR 910.773 - Requirements for permits and permit processing.

    Science.gov (United States)

    2010-07-01

    ... Georgia Water Quality Control Act, section 17-501; the Georgia Solid Waste Management Act, section 43-1681.... 910.773 Section 910.773 Mineral Resources OFFICE OF SURFACE MINING RECLAMATION AND ENFORCEMENT, DEPARTMENT OF THE INTERIOR PROGRAMS FOR THE CONDUCT OF SURFACE MINING OPERATIONS WITHIN EACH STATE GEORGIA...

  2. Enhancement of strength properties of hot rolled 10KHSND steel

    International Nuclear Information System (INIS)

    Nasibov, A.G.; Popova, L.V.; Pikulin, S.A.; Globa, N.I.

    1989-01-01

    To find out the reasons of low hot rolling yield for 10KhSND steel sheets in mechanical properties, titanium effect in the range of 0.008-0.03% concentrations is studied. It is established that the titanium content in a solid solution is conserved within 0.003-0.005%, the rest of titanium is bound to carbonitrides Ti(C, N). It is shown that alloys with 0.025-0.03% titanium content possess the increased values of ultimate and yield strength the necessary level of impact strength and good wealdability. The good steel yield, when the titanium content is sustained at the given level, increases from 40 to 85%

  3. One electron reduction of 1,2 dihydroxy 9,10 anthraquinone and its transition metal complexes in aqueous-isopropanol-acetone mixed solvent: a steady state-state and pulse radiolysis study

    International Nuclear Information System (INIS)

    Das, Saurabh; Mandal, Parikshit C.; Rath, Madhab C.; Mukherjee, Tulsi

    1998-01-01

    One electron reduction of 1,2 dihydroxy 9,10 anthraquinone and its Cu(II) and Ni(II) and Fe(III) complexes have been studied in aqueous-isopropanol-acetone solvent. Results indicate that the reducing ketyl radical generated reacts with the ligand forming semiquinones which undergoes a disproportionation reaction. Formation and decay rates of semiquinones was calculated using pulse radiolysis. (author)

  4. Passive behaviour of alloy corrosion-resistant steel Cr10Mo1 in simulating concrete pore solutions with different pH

    International Nuclear Information System (INIS)

    Ai, Zhiyong; Jiang, Jinyang; Sun, Wei; Song, Dan; Ma, Han; Zhang, Jianchun; Wang, Danqian

    2016-01-01

    Highlights: • A new alloy corrosion-resistant steel Cr10Mo1 is developed for reinforcing rebar of concrete in severe environments. • The effects of pH on the passive behaviour of Cr10Mo1 steel compared with plain carbon steel were studied systematically by electrochemical techniques and surface analysis. • The mechanism for self-reinforcing passivity against carbonation of the corrosion-resistant steel is revealed. - Abstract: The passive behaviour of new alloy corrosion-resistant steel Cr10Mo1 and plain carbon steel (as a comparison) in simulating concrete pore solutions of different pH (ranging from 13.5 to 9.0) under open circuit potential conditions, was evaluated by various electrochemical techniques: potentiodynamic polarization, capacitance measurements and electrochemical impedance spectroscopy. The chemical composition and structure of passive films were investigated by X-ray photoelectron spectroscopy (XPS) and secondary ion mass spectroscopy (SIMS). The electrochemical responses of passive films show that Cr10Mo1 steel has an increasing passivity with pH decreasing while carbon steel dose conversely, revealing carbonation does no negative effect on passivation of the corrosion-resistant steel. SIMS reveals that the passive film on the corrosion-resistant steel presents a bilayer structure: an outer layer mainly consisting of Fe oxides and hydroxides, and an inner layer enriched in Cr species, while only a Fe-concentrated layer for carbon steel. According to the XPS analysis results, as the pH decreases, more stable and protective Cr oxides are enriched in the film on Cr10Mo1 steel while Fe oxides gradually decompose. Higher content of Cr oxides in the film layer provides Cr10Mo1 corrosion-resistant steel more excellent passivity at lower pH.

  5. Passive behaviour of alloy corrosion-resistant steel Cr10Mo1 in simulating concrete pore solutions with different pH

    Energy Technology Data Exchange (ETDEWEB)

    Ai, Zhiyong, E-mail: 230139452@seu.edu.cn [School of Materials Science and Engineering, Southeast University, Nanjing 211189, Jiangsu (China); Jiangsu Key Laboratory of Construction Materials, Nanjing 211189, Jiangsu (China); Jiang, Jinyang, E-mail: jiangjinyang16@163.com [School of Materials Science and Engineering, Southeast University, Nanjing 211189, Jiangsu (China); Jiangsu Key Laboratory of Construction Materials, Nanjing 211189, Jiangsu (China); Sun, Wei, E-mail: sunwei@seu.edu.cn [School of Materials Science and Engineering, Southeast University, Nanjing 211189, Jiangsu (China); Jiangsu Key Laboratory of Construction Materials, Nanjing 211189, Jiangsu (China); Song, Dan, E-mail: songdancharls@hhu.edu.cn [School of Materials Science and Engineering, Southeast University, Nanjing 211189, Jiangsu (China); Jiangsu Key Laboratory of Construction Materials, Nanjing 211189, Jiangsu (China); College of Mechanics and Materials, Hohai University, Nanjing 210098, Jiangsu (China); Ma, Han, E-mail: mahan-iris@shasteel.cn [Research Institute of Jiangsu Shasteel Iron and Steel, Zhangjiagang 215625, Jiangsu (China); Zhang, Jianchun, E-mail: Zhangjc-iris@shasteel.cn [Research Institute of Jiangsu Shasteel Iron and Steel, Zhangjiagang 215625, Jiangsu (China); Wang, Danqian, E-mail: wonderbaba@126.com [School of Materials Science and Engineering, Southeast University, Nanjing 211189, Jiangsu (China); Jiangsu Key Laboratory of Construction Materials, Nanjing 211189, Jiangsu (China)

    2016-12-15

    Highlights: • A new alloy corrosion-resistant steel Cr10Mo1 is developed for reinforcing rebar of concrete in severe environments. • The effects of pH on the passive behaviour of Cr10Mo1 steel compared with plain carbon steel were studied systematically by electrochemical techniques and surface analysis. • The mechanism for self-reinforcing passivity against carbonation of the corrosion-resistant steel is revealed. - Abstract: The passive behaviour of new alloy corrosion-resistant steel Cr10Mo1 and plain carbon steel (as a comparison) in simulating concrete pore solutions of different pH (ranging from 13.5 to 9.0) under open circuit potential conditions, was evaluated by various electrochemical techniques: potentiodynamic polarization, capacitance measurements and electrochemical impedance spectroscopy. The chemical composition and structure of passive films were investigated by X-ray photoelectron spectroscopy (XPS) and secondary ion mass spectroscopy (SIMS). The electrochemical responses of passive films show that Cr10Mo1 steel has an increasing passivity with pH decreasing while carbon steel dose conversely, revealing carbonation does no negative effect on passivation of the corrosion-resistant steel. SIMS reveals that the passive film on the corrosion-resistant steel presents a bilayer structure: an outer layer mainly consisting of Fe oxides and hydroxides, and an inner layer enriched in Cr species, while only a Fe-concentrated layer for carbon steel. According to the XPS analysis results, as the pH decreases, more stable and protective Cr oxides are enriched in the film on Cr10Mo1 steel while Fe oxides gradually decompose. Higher content of Cr oxides in the film layer provides Cr10Mo1 corrosion-resistant steel more excellent passivity at lower pH.

  6. Proceedings of 1974 National powder metallurgy conference held at Boston, Massachusetts, April 9--10, 1974

    International Nuclear Information System (INIS)

    Halter, R.F.

    1974-01-01

    Papers given at the conference on process variables in production of P/M parts, properties of 316L steel powder, compacts, properties of highly porous Al powder compacts, properties of Cu infiltrated steel powders, uses of P/M Ti and P/M Al alloys, heat treatment of P/M parts, quality control, safety, ultrasonic testing of P/M parts, P/M sealing, cold pressing P/M, properties of AISI 4027 P/M materials, properties of Ni--Mo steel powders, and state of the industry-1974 are presented

  7. SERS investigations on orientation of 2-bromo-3-methyl-1,4-dimethoxy-9,10-anthraquinone on silver nanoparticles.

    Science.gov (United States)

    Anuratha, M; Jawahar, A; Umadevi, M; Sathe, V G; Vanelle, P; Terme, T; Khoumeri, O; Meenakumari, V; Milton Franklin Benial, A

    2015-01-01

    Silver nanoparticles (Ag NPs) were prepared by solution combustion method with urea as fuel. Silver nanoparticles were characterized by UV-visible spectroscopy, X-ray diffraction (XRD) and scanning electron microscopy (SEM) techniques. Surface-enhanced Raman scattering (SERS) of 2-bromo-3-methyl-1,4-dimethoxy-9,10-anthraquinone (BMDMAQ) adsorbed on silver nanoparticles was investigated. The orientation of BMDMAQ on silver nanoparticles was inferred from nRs and SERS spectral features. Density functional theory (DFT) calculation was also performed to study the theoretical performance. The observed spectral features such as the high intensity of C-H out-of-plane bending mode and ring C-C stretching mode revealed that BMDMAQ adsorbed on silver surface through 'stand-on' orientation. Anthraquinone (AQ) derivatives have wide biomedical application which includes laxatives, antimalarials and antineoplastics used in the treatment of cancer. This present study would help to identify the interaction of drug molecules with DNA. Copyright © 2015 Elsevier B.V. All rights reserved.

  8. Hot ductility testing and weld simulation tests

    International Nuclear Information System (INIS)

    Weber, G.; Schick, M.

    1999-01-01

    The objective of the project was to enhance the insight into the causes of intergranular cracks detected in austenitic circumferential welds at BWR pipes. The susceptibility of a variety of austenitic pipe materials to hot cracking during welding and in-service intergranular crack corrosion was examined. The assumption was cracking in the root area of the HAZ of a multiple-layer weld. Hot-ductility tests and weld simulation tests specifically designed for the project were performed with the austenitic LWR pipe materials 1.4553 (X6 CrNiNb 18 10 S), 1.4550 (X10 CrNiNb 18 9), 1.4533 (X6 CrNiTi 18 9, two weld pools), and a non-stabilized TP 304 (X5 CrNi 18 10). (orig./CB) [de

  9. 25 CFR 11.910 - Expungement.

    Science.gov (United States)

    2010-04-01

    ... INDIAN AFFAIRS, DEPARTMENT OF THE INTERIOR LAW AND ORDER COURTS OF INDIAN OFFENSES AND LAW AND ORDER CODE Children's Court § 11.910 Expungement. When a minor who has been the subject of any proceeding before the children's court attains his or her twenty-first birthday, the children's court magistrate shall order the...

  10. Breast-milk intake of 9-10-mo-old rural infants given a ready-to-use complementary food in South Kivu, Democratic Republic of Congo.

    Science.gov (United States)

    Owino, Victor O; Bahwere, Paluku; Bisimwa, Ghislain; Mwangi, Christine M; Collins, Steve

    2011-06-01

    Lipid-based ready-to-use foods are currently used for infant feeding, but their potential effect on breast-milk intake is not well documented. The objective was to assess the breast-milk intake of 9-10-mo-old infants given either a ready-to-use complementary food (RUCF) paste or a standard corn-soy blend (UNIMIX) porridge in South Kivu, Democratic Republic of Congo. Infants were randomly assigned at 6 mo of age to receive either RUCF (n = 700) or UNIMIX (n = 700) for 6 mo. Breast-milk intake was measured at 9-10 mo in a subsample of 58 infants (29 from each group). Mothers received a dose of ≈30 g deuterium oxide. Predose and postdose saliva samples were collected from both mothers and infants over 2 wk. Breast-milk intake (g/d) was measured from saliva samples by using infrared spectroscopy. Mean (±SD) breast-milk intake was not significantly (P = 0.69) different between the 2 groups: RUCF (705 ± 236 g/d) and UNIMIX (678 ± 285 g/d). Mean (±SD) nonmilk oral water intakes were 338.3 ± 251.1 and 336.4 ± 227.2 g/d for RUCF and UNIMIX, respectively (P = 0.98). No differences in breast-milk intake were observed between infants consuming either RUCF or UNIMIX. The deuterium-dose-to-the-mother dilution technique is an affordable technique that we recommend for periodic evaluation of breast-milk intake in resource-poor settings. This trial is registered at controlled-trials.com as ISRCTN20267635.

  11. The research of axial corrosion fatigue on 10Ni3CrMoV steel

    Science.gov (United States)

    Xie, Xing; Yi, Hong; Xu, Jian; Xie, Kun

    2017-09-01

    Fatigue life had been studied with 10CrNi3MoV steel at different load ratios and in different environmental medias. The microstructure and micro-topography had been observed and analyzed by means of SEM, EDS and TEM. Our findings indicated that, the fatigue life of 10Ni3CrMoV steel in seawater was shorter than in air, the difference in longevity was larger with the decreasing of axis stress. Corrosion pits had a great influence on corrosion fatigue life.

  12. 40 CFR 725.910 - Persons excluded from reporting significant new uses.

    Science.gov (United States)

    2010-07-01

    ... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Persons excluded from reporting significant new uses. 725.910 Section 725.910 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... designated significant new uses, or (2) That the recipient has knowledge of the specific section in subpart M...

  13. Excited-state intramolecular hydrogen transfer (ESIHT) of 1,8-Dihydroxy-9,10-anthraquinone (DHAQ) characterized by ultrafast electronic and vibrational spectroscopy and computational modeling

    KAUST Repository

    Mohammed, Omar F.

    2014-05-01

    We combine ultrafast electronic and vibrational spectroscopy and computational modeling to investigate the photoinduced excited-state intramolecular hydrogen-transfer dynamics in 1,8-dihydroxy-9,10-anthraquinone (DHAQ) in tetrachloroethene, acetonitrile, dimethyl sulfoxide, and methanol. We analyze the electronic excited states of DHAQ with various possible hydrogen-bonding schemes and provide a general description of the electronic excited-state dynamics based on a systematic analysis of femtosecond UV/vis and UV/IR pump-probe spectroscopic data. Upon photoabsorption at 400 nm, the S 2 electronic excited state is initially populated, followed by a rapid equilibration within 150 fs through population transfer to the S 1 state where DHAQ exhibits ESIHT dynamics. In this equilibration process, the excited-state population is distributed between the 9,10-quinone (S2) and 1,10-quinone (S1) states while undergoing vibrational energy redistribution, vibrational cooling, and solvation dynamics on the 0.1-50 ps time scale. Transient UV/vis pump-probe data in methanol also suggest additional relaxation dynamics on the subnanosecond time scale, which we tentatively ascribe to hydrogen bond dynamics of DHAQ with the protic solvent, affecting the equilibrium population dynamics within the S2 and S1 electronic excited states. Ultimately, the two excited singlet states decay with a solvent-dependent time constant ranging from 139 to 210 ps. The concomitant electronic ground-state recovery is, however, only partial because a large fraction of the population relaxes to the first triplet state. From the similarity of the time scales involved, we conjecture that the solvent plays a crucial role in breaking the intramolecular hydrogen bond of DHAQ during the S2/S1 relaxation to either the ground or triplet state. © 2014 American Chemical Society.

  14. Laser induced transient absorptions of the excited triplet state of 9,10-anthraquinone-2-sulfonate. A further study by 248 nm laser photolysis

    International Nuclear Information System (INIS)

    Ma Jianhua; Lin Weizheng; Wang Wenfen; Yao Side; Lin Nianyun

    1999-01-01

    Transient absorption spectrum of triplet state of 9,10-anthraquinone-2-sulfonate (AQS) in aqueous solution has been investigated using 248 nm (KrF) laser photolysis. A whole transient absorption spectrum with absorption maxim at 380 nm and 580 nm has been assigned to triple AQS from detailed kinetic analysis of decay of 380 nm and 580 nm signals, which is the neat characteristic absorption of triplet AQS reported for the first time. In addition, the difference in feature of the spectrum of triplet AQS in H 2 O and that in CH 3 CN was eliminated by further study using 248 nm laser pulses

  15. Study on microstructure and mechanical characteristics of low-carbon steel and ferritic stainless steel joints

    Energy Technology Data Exchange (ETDEWEB)

    Sarkari Khorrami, Mahmoud; Mostafaei, Mohammad Ali; Pouraliakbar, Hesam, E-mail: hpouraliakbar@alum.sharif.edu; Kokabi, Amir Hossein

    2014-07-01

    In this work, examinations on the microstructure and mechanical properties of plain carbon steel and AISI 430 ferritic stainless steel dissimilar welds are carried out. Welding is conducted in both autogenous and using ER309L austenitic filler rod conditions through gas tungsten arc welding process. The results indicate that fully-ferritic and duplex ferritic–martensitic microstructures are formed for autogenous and filler-added welds, respectively. Carbide precipitation and formation of martensite at ferrite grain boundaries (intergranular martensite) as well as grain growth occur in the heat affected zone (HAZ) of AISI 430 steel. It is found that weld heat input can strongly affect grain growth phenomenon along with the amount and the composition of carbides and intergranular martensite. Acquired mechanical characteristics of weld in the case of using filler metal are significantly higher than those of autogenous one. Accordingly, ultimate tensile strength (UTS), hardness, and absorbed energy during tensile test of weld metal are increased from 662 MPa to 910 MPa, 140 Hv to 385 Hv, and 53.6 J m{sup −3} to 79 J m{sup −3}, respectively by filler metal addition. From fracture surfaces, predominantly ductile fracture is observed in the specimen welded with filler metal while mainly cleavage fracture occurs in the autogenous weld metal.

  16. Heavy steel casting components for power plants 'mega-components' made of high Cr-steels

    Energy Technology Data Exchange (ETDEWEB)

    Hanus, Reinhold [voestalpine Giesserei Linz GmbH, Linz (Austria)

    2010-07-01

    Steel castings of creep resistant steels play a key role in fossil fuel fired power plants for highly loaded components in the high and intermediate pressure section of the turbines. Inner and outer casings, valve casings, inlet connections and elbows are examples of such critical components. The most important characteristic in a power plant is the efficiency, which mainly drives the CO2-emission. As a consequence of steadily improving power plant efficiencies and ever stricter emission standards, steam parameters become more critical and the creep resistance of the cast materials must also be constantly improved. The foundries voestalpine Giesserei Linz and voestalpine Giesserei Traisen participated in the development of the new 9-10% Cr-steels for application up to 625 C/650 C and in the THERMIE project where Ni-base alloys for 700 C-power plants were developed. Beside the material development in the European research projects the commercial production had to be established for industrial processes and the newly developed materials have to be transferred from research into the commercial production of heavy cast components. After selecting the most promising alloy from the laboratory melts, welding tests were performed - mostly with matching electrodes also produced within COST/THERMIE. Base material and welds were investigated in respect of microstructure, creep resistance, mechanical properties and weldability. Heat treatment investigations were also necessary for optimization of the mechanical properties. Based on the results of these studies, pilot components and plates for testing welding processes were cast in order to verify the castability and weldability of larger parts and to make any necessary adjustments to chemical composition, heat treatment or welding parameters. Parallel to the ongoing creep tests within COST/THERMIE-program, the newly developed steel grades were introduced into the commercial production of large components. This involved finding

  17. 40 CFR 80.910 - How does a refiner or importer apply for a toxics baseline?

    Science.gov (United States)

    2010-07-01

    ... for a toxics baseline? 80.910 Section 80.910 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY (CONTINUED) AIR PROGRAMS (CONTINUED) REGULATION OF FUELS AND FUEL ADDITIVES Gasoline Toxics Baseline Determination § 80.910 How does a refiner or importer apply for a toxics baseline? (a)(1) A refiner or importer...

  18. Long-term strength and allowable stresses of grade 10Kh9MFB and X10CrMoVNb9-1 (T91/P91) chromium heat-resistant steels

    Science.gov (United States)

    Skorobogatykh, V. N.; Danyushevskiy, I. A.; Schenkova, I. A.; Prudnikov, D. A.

    2015-04-01

    Currently, grade X10CrMoVNb9-1 (T91, P91) and 10Kh9MFB (10Kh9MFB-Sh) chromium steels are widely applied in equipment manufacturing for thermal power plants in Russia and abroad. Compilation and comparison of tensile, impact, and long-term strength tests results accumulated for many years of investigations of foreign grade X10CrMoVNb9-1, T91, P91, and domestic grade 10Kh9MFB (10Kh9MFB-Sh) steels is carried out. The property identity of metals investigated is established. High strength and plastic properties of steels, from which pipes and other products are made, for operation under creep conditions are confirmed. Design characteristics of long-term strength on the basis of tests with more than one million of hour-samples are determined ( and at temperatures of 500-650°C). The table of recommended allowable stresses for grade 10Kh9MFB, 10Kh9MFB-SH, X10CrMoVNb9-1, T91, and P91 steels is developed. The long-time properties of pipe welded joints of grade 10Kh9MFB+10Kh9MFB, 10Kh9MFB-Sh+10Kh9MFB-Sh, X10CrMoVNb9-1+X10CrMoVNb9-1, P91+P91, T91+T91, 10Kh9MFB (10Kh9MFB-Sh)+X10CrMoVNb9-1(T/P91) steels is researched. The welded joint reduction factor is experimentally determined.

  19. Ten-year changes in positive and negative marker food, fruit, vegetables, and salad intake in 9-10 year olds: SportsLinx 2000-2001 to 2010-2011.

    Science.gov (United States)

    Boddy, L M; Abayomi, J; Johnson, B; Hackett, A F; Stratton, G

    2014-06-01

    To investigate changes in intakes of 'negative' and 'positive' foods, fruit, vegetables, and salad in serial cohorts of 9-10-year-old children from 2000-2001 to 2010-2011. For this serial, cross-sectional study, children in school year 5 (9-10 years of age) completed the SportsLinx Lifestyles Survey [n = 30,239 (15,336 boys and 14,903 girls)]. Changes in positive and negative food scores, and the proportion of boys and girls reportedly consuming fruit, vegetables and salad on the previous day to surveying, were investigated annually from 2000 to 2011. The consumption of negative foods declined and positive foods increased significantly compared to baseline. Positive changes in fruit, vegetables and salad consumption were observed over time, with the most recent cohort more likely to consume fruit, vegetables and salad compared to the 2000-2001 baseline. Girls displayed more favourable positive and negative food scores and were more likely to consume fruit, salad and vegetables across several study years compared to boys. The consumption of negative and positive foods, fruit, vegetables, and salad has improved over the last 10 years. In addition, girls appear to have better positive and negative food scores, and were more likely to consume fruit, vegetables and salad, across a number of study years or cohorts compared to boys. These encouraging findings suggest that children's food intake has improved since 2000. Furthermore, the data indicate that boys and girls may require separate or different healthy eating messages to further improve food intake. © 2013 The Authors Journal of Human Nutrition and Dietetics © 2013 The British Dietetic Association Ltd.

  20. Mechanical And Microstructural Evaluation Of A Wear Resistant Steel; Avaliacao mecanica e microestrutural de um aco resistente ao desgaste

    Energy Technology Data Exchange (ETDEWEB)

    Santos, F.L.F. dos; Vieira, A.G.; Correa, E.C.S.; Pinheiro, I.P., E-mail: falletti@hotmail.co [Centro Federal de Educacao Tecnologica de Minas Gerais (CEFET/MG), Belo Horizonte, MG (Brazil). Dept. de Engenharia de Materiais

    2010-07-01

    In the present work, the analysis of the mechanical properties and the microstructural features of a high strength low alloy steel, containing chromium, molybdenum and boron, subjected to different heat treatments, was conducted. After austenitizing at 910 deg C for 10 minutes, three operations were carried out: oil quenching, oil quenching followed by tempering at 200 deg C for 120 minutes and austempering at 400 deg C for 5 minutes followed by water cooling. The analysis was performed through tensile and hardness tests, optical microscopy and X-ray diffraction. The bainitic structure led to high strength and toughness, both essential mechanical properties for wear resistant steels. The occurrence of allotriomorphic ferrite and retained austenite in the samples also increased the wear resistance. This phenomenon is related to the fact that both structures are able to be deformed and, in the case of the retained austenite, the transformation induced plasticity TRIP effect may take place as the material is used. (author)

  1. Strength of 10CR-N martensitic steels

    International Nuclear Information System (INIS)

    Bahrami, F.; Hendry, A.

    1993-01-01

    10Cr stainless steel has been employed to examine the effect of nitrogen on microstructure and strength. Applying Solid state gaseous nitrogenising treatments a whole range of nitrogen martensite structures containing up to 0.45 wt% were obtained. It was found that a linear relationship exists between strength and nitrogen content in precipitate free martensitic structures. Yield strength increased from 705 to 1295 MPa for nitrogen free base material and alloys with 0.35 wt%N respectively. Pronounce secondary hardening was observed at a tempering temperature of 500 C. A linear relationship was also observed between the lattice parameter and nitrogen concentration in these alloys. A model for mechanical behaviour is presented. (orig.)

  2. Microstructural change during creep deformation in a 10%Cr martensitic steel

    International Nuclear Information System (INIS)

    Kim, Sung Ho; Song, B. J.; Ryu, Woo Seog

    2001-01-01

    The relationship between creep deformation and microstructural changes in martensitic 10Cr-MoW steel has been studied. Transmission electron microscopy and image analyser were used to determine the variation of precipitates and martensite lath width size during creep deformation and aging. As precipitates are coarsened during creep deformation, dislocations become easy to move and the recovery proceeds rapidly. This leads to the growth of lath width. The average size of precipitates was linearly increased with creep time. On the other hand the growth rate of lath width is constant until tertiary creep, but the growth of lath width is accelerated during tertiary creep. It has been concluded that the growth behavior of lath width are consistent with creep deformation. Because the growth of lath width is controlled by the coarsening of precipitates it is important to form more stable precipitates in creep condition for improvement of creep properties of martensitic steel. Microstructure of martensitic steel is thermally very stable, so the size of precipitates and martensite lath width are hardly changed during aging

  3. Inhibition of HIV-1 reverse transcriptase-catalyzed synthesis by intercalated DNA Benzo[a]Pyrene 7,8-Dihydrodiol-9,10-Epoxide adducts.

    Directory of Open Access Journals (Sweden)

    Parvathi Chary

    Full Text Available To aid in the characterization of the relationship of structure and function for human immunodeficiency virus type-1 reverse transcriptase (HIV-1 RT, this investigation utilized DNAs containing benzo[a]pyrene-7,8-dihydrodiol-9,10-epoxide (BPDE-modified primers and templates as a probe of the architecture of this complex. BPDE lesions that differed in their stereochemistry around the C10 position were covalently linked to N (6-adenine and positioned in either the primer or template strand of a duplex template-primer. HIV-1 RT exhibited a stereoisomer-specific and strand-specific difference in replication when the BPDE-lesion was placed in the template versus the primer strand. When the C10 R-BPDE adduct was positioned in the primer strand in duplex DNA, 5 nucleotides from the 3΄ end of the primer terminus, HIV-1 RT could not fully replicate the template, producing truncated products; this block to further synthesis did not affect rates of dissociation or DNA binding affinity. Additionally, when the adducts were in the same relative position, but located in the template strand, similar truncated products were observed with both the C10 R and C10 S BPDE adducts. These data suggest that the presence of covalently-linked intercalative DNA adducts distant from the active site can lead to termination of DNA synthesis catalyzed by HIV-1 RT.

  4. Persistence of hepatitis B immune memory until 9-10 years of age following hepatitis B vaccination at birth and DTaP-IPV-HB-PRP∼T vaccination at 2, 4 and 6 months.

    Science.gov (United States)

    Kosalaraksa, Pope; Chokephaibulkit, Kulkanya; Benjaponpitak, Suwat; Pancharoen, Chitsanu; Chuenkitmongkol, Sunate; B'Chir, Siham; Da Costa, Xavier; Vidor, Emmanuel

    2018-01-15

    To evaluate the long-term persistence of anti-hepatitis B surface (HBs) antibodies and the response to a HB challenge re-vaccination in children who had received a primary series of DTaP-IPV-HB-PRP∼T (Hexaxim™) or DTaP-IPV-HB/PRP∼T (Infanrix hexa™). Two cohorts of participants who had previously received HB vaccine at birth followed by either DTaP-IPV-HB-PRP∼T or DTaP-IPV-HB/PRP∼T co-administered with PCV7 at 2, 4, 6 months of age in a randomized, Phase III, observer-blind study in Thailand, were followed up for anti-HBs antibodies (geometric mean concentrations [GMCs] and seroprotection [SP] rate [% of participants with a titer ≥10 mIU/mL]) at 12-18 months of age and 9-10 years of age. A monovalent HB challenge re-vaccination was administered at 9-10 years of age and the anamnestic response was evaluated. Anti-HBs GMCs and SP rates in the DTaP-IPV-HB-PRP∼T and DTaP-IPV-HB/PRP∼T groups were high and similar post-primary vaccination series (2477 mIU/mL and 99.5% and 2442 mIU/mL and 99.5%, respectively) and declined to a similar extent in each group at 12-18 months (154.5 mIU/mL and 90.8% and 162.3 mIU/mL and 96.5%, respectively). Antibody levels further declined at 9-10 years of age (13.3 mIU/mL and 49.3% and 8.0 mIU/mL and 42.9%) and a strong anamnestic response occurred in each group post-HB challenge re-vaccination (92.8% and 98.7%, respectively). The kinetics of long-term anti-HBs antibody persistence were similar following a primary series of DTaP-IPV-HB-PRP∼T or DTaP-IPV-HB/PRP∼T. The response to a subsequent HB challenge re-vaccination was strong and similar in each group, demonstrating persisting immune memory.

  5. Interactions between 9,10-anthraquinone and aromatic amines in homogeneous and micellar media: A laser flash photolysis and magnetic field effect study

    International Nuclear Information System (INIS)

    Chowdhury, Adity; Basu, Samita

    2006-01-01

    The interactions between 9,10-anthraquinone (AQ) and different aromatic amines, N,N-dimethylaniline and 4,4'-bis (dimethylamino) diphenylmethane (DMDPM), have been studied using absorption, steady-state fluorescence, and laser flash photolysis techniques in organic homogeneous and heterogeneous micellar media. In polar organic homogeneous medium, electron transfer (ET) occurs from amines to excited AQ. In micellar medium, similar intermolecular ET is observed. However, in latter medium, ET predominates over hydrogen abstraction from micelles by excited AQ itself. The occurrence of ET has been further supported by the application of an external magnetic field during laser flash photolysis experiments, which modulates the yield of radical ion pairs formed through ET. Another novel feature, which has also been discussed here, is the abnormal behavior of DMDPM in micellar medium pertaining to energy transfer

  6. (4bS,8aS-1-Isopropyl-4b,8,8-trimethyl-4b,5,6,7,8,8a,9,10-octahydrophenanthren-2-yl acetate

    Directory of Open Access Journals (Sweden)

    Radouane Oubabi

    2014-03-01

    Full Text Available The hemisynthesis of the title compound, C22H32O2, was carried out through direct acetylation reaction of the naturally occurring diterpene totarol [systematic name: (4bS,8aS-4b,8,8-trimethyl-1-propan-2-yl-5,6,7,8a,9,10-hexahydrophenanthren-2-ol]. The molecule is built up from three fused six membered rings, one saturated and two unsaturated. The central unsaturated ring has a half-chair conformation, whereas the other unsaturated ring displays a chair conformation. The absolute configuration is deduced from the chemical pathway. The value of the Hooft parameter [−0.10 (6] allowed this absolute configuration to be confirmed.

  7. Effect of rolling temperature on 12Kh18N10T steel tube hardening

    International Nuclear Information System (INIS)

    Yushkevich, P.M.; Stepanovich, V.E.; Manankova, L.V.; Usenko, V.N.; Semenov, I.A.

    1984-01-01

    Mechanical properties and substructure of tubes at the constant reduction degree k(the ratio of deformation over wall thickness to deformation over diameter), depending on strain degree during cold and hot tube rolling, have been studied. The investigations are carried out using hot-rolled tubes with the dimensions 88x8 mm of 12Kh1hN10T steel. With the decrease of strain over the wall of the tube, produced of 12Kh18N10T steel as to strain over diameter the values of yield strength and ultimate strength increase with simultaneous decrease in ductility during warm rolling and yield strength and ultimate strength decrease with the increase in ductility-during cold rolling. During warm rolling of the tubes at 250 deg C the hardening of 12Kh18N10T steel is higher, than at the rolling temperature 150 deg C. The optimum temperature range of warm rolling is 120-150 deg C. Grain orientation in the metal of the tubes and degree of texture perfection increase with the temperature increase of the tube warm drolling as compared with col rolli

  8. Study of the AISI 347 austenitic stainless steel sensitization through the potentiokinetic reactivation method

    International Nuclear Information System (INIS)

    Teodoro, Celso Antonio; Wolynec, Stephan

    1996-01-01

    The sensitization kinetics of AISI 347 austenitic stainless steel samples, removed from a forged bar, was investigated with an electrochemical potentiokinetic reactivation method. After the solution anneal at 1140 deg C, the steel was submitted to sensitization treatments at 550 deg C, 670 deg C, 790 deg C and 910 deg C during times that varied from 1 h to 62 h. It was found that samples treated at 550 deg C, 670 deg C and 790 deg C become sensitized. The activation energy was found to be 124 kJ/mol. The observed behaviour was discussed in terms of both carbon retention in solution after the solution anneal and kinetics of carbon combination with chromium and niobium. (author)

  9. Influence of Ni(II) and Fe(III) complexes of 1,2 dihydroxy 9,10 anthraquinone on the modification in calf thymus DNA upon gamma irradiation

    International Nuclear Information System (INIS)

    Das, Saurabh; Mandal, Parikshit C.

    2009-01-01

    Ionizing radiation when allowed to fall upon cells or DNA, the radicals produced modify the base-pair region of the double strands. Radiation-induced double-strand modifications in calf thymus DNA were detected using Ni(II) and Fe(III) complexes of 1,2 dihydroxy 9,10 anthraquinone (DHA). 60 Co was used as the source for γ-radiation and ethidium bromide (EB) as the fluorescent dye for detecting double-strand modifications caused in DNA. Results show that the Fe(III)-DHA complex is more efficient in modifying the base-pair region in double-stranded DNA in comparison to DHA or the Ni(II)-DHA complex

  10. Effect of temper and hydrogen embrittlement on mechanical properties of 2,25Cr–1Mo steel grades – Application to Minimum Pressurizing Temperature (MPT) issues. Part I: General considerations and materials' properties

    International Nuclear Information System (INIS)

    Pillot, Sylvain; Chauvy, Cédric; Corre, Stéphanie; Coudreuse, Lionel; Gingell, Andrew; Héritier, Déborah; Toussaint, Patrick

    2013-01-01

    Standard and Vanadium-alloyed 2,25Cr–1Mo steel grades (EN 10028-2 12CrMo9-10/ASTM A387 gr. 22 and 13CrMoV9-10/ASTM A542 tp. D) are commonly used for the fabrication of heavy pressure vessels for applications in petroleum refining plants. These reactors are made of heavy plates, forged shells, forged nozzles and fittings. They are subjected to thermal cycles (stop and go) and to severe service conditions (high temperatures and high hydrogen partial pressures). A primary concern for end-users is the definition of the Minimum Pressurizing Temperature (MPT) of the equipment. This temperature is the lowest temperature at which the vessel can be repressurized after shutdown and insures no risk of brittle failure of the containment body. The MPT is defined by fracture mechanics and/or CVN approaches and calculations. This first part of the paper presents the impact of thermal aging and exposure to hydrogen on materials' mechanical properties and consequently on the value of MPT

  11. Microstructural evolution of HFIR-irradiated low activation F82H and F82H-10B steels

    International Nuclear Information System (INIS)

    Wakai, E.; Shiba, K.; Sawai, T.; Hashimoto, N.; Robertson, J.P.; Klueh, R.L.

    1998-01-01

    Microstructures of reduced-activation F82H (8Cr-2W-0.2V-0.04Ta) and the F82H steels doped with 10 B, irradiated at 250 and 300 C to 3 and 57 dpa in the High Flux Isotope Reactor (HFIR), were examined by TEM. In the F82H irradiated at 250 C to 3 dpa, dislocation loops, small unidentified defect clusters with a high number density, and a few MC precipitates were observed in the matrix. The defect microstructure after 300 C irradiation to 57 dpa is dominated by the loops, and the number density of loops was lower than that of the F82H- 10 B steel. Cavities were observed in the F82H- 10 B steels, but the swelling value is insignificant. Small particles of M 6 C formed on the M 23 C 6 carbides that were present in both steels before the irradiation at 300 C to 57 dpa. A low number density of MC precipitate particles formed in the matrix during irradiation at 300 C to 57 dpa

  12. Reaction of a chemotherapeutic agent, 6-mercaptopurine, with a direct-acting, electrophilic carcinogen, benzo[a]pyrene-7,8-diol 9,10-epoxide.

    Science.gov (United States)

    MacLeod, M C; Stewart, E; Daylong, A; Lew, L K; Evans, F E

    1991-01-01

    The chemotherapeutic agent 6-mercaptopurine (6-MP) has been shown to react covalently with the ultimate carcinogenic metabolite of benzo[a]pyrene, 7-r,8-t-dihydroxy-9-t,10-t-oxy-7,8,9,10-tetrahydrobenzo[a]pyrene (BPDE), in aqueous solution, forming a single adduct. NMR studies of the HPLC-purified product were consistent with its identification as 10(S)-(6'-mercaptopurinyl)-7,8,9-trihydroxy-7,8,9,10- tetrahydrobenzo[a]pyrene. Reaction kinetics were analyzed by using both HPLC separation of the products formed and a spectrophotometric assay for adduct formation. A simple model in which direct reaction between 6-MP and BPDE takes place without formation of a physical complex was found to adequately predict the dependence of product ratios on 6-MP concentration. Variations in the observed rate constant for this reaction with changes in temperature, pH, and buffer concentration were determined and compared to the effects of these variables on the observed rate constant for BPDE hydrolysis. In each case, the processes were affected quite differently, suggesting that different rate-determining steps are involved. The data suggest that the reaction mechanism involves SN2 attack of the anion of 6-MP, formed by ionization of the sulfhydryl group, on carbon 10 of BPDE, resulting in a trans-9,10 reaction product.

  13. Effects of Mn addition on microstructures and mechanical properties of 10Cr ODS ferritic/martensitic steels

    International Nuclear Information System (INIS)

    Jin, Hyun Ju; Kim, Tae Kyu

    2014-01-01

    Ferritic/martensitic (FM) steels are very attractive for the structural materials of fast fission reactors such as a sodium cooled fast reactor (SFR) owing to their excellent irradiation resistance to a void swelling, but are known to reveal an abrupt loss of their creep and tensile strengths at temperatures above 600 .deg. C. Accordingly, high temperature strength should be considerably improved for an application of the FM steel to the structural materials of SFR. Oxide dispersion strengthened (ODS) FM steels are considered to be promising candidate materials for high- temperature components operating in severe environments such as nuclear fusion and fission systems due to their excellent high temperature strength and radiation resistance stemming from the addition of extremely thermally stable oxide particles dispersed in the ferritic/martensitic matrix.. To develop an advanced ODS steel for core structural materials for next generation nuclear reactor system applications, it is important to optimize its compositions to improve the high temperature strength and radiation resistance. This study investigates effects of Mn addition on microstructures and mechanical properties of 10Cr ODS FM steel. For this, two 10 Cr ODS FM steels were prepared by mechanical alloying (MA), hot isostatic pressing (HIP), and hot rolling process. Tensile tests were carried out at room temperature and 700 .deg. C to evaluate the influences of the Mn element on the mechanical properties. The microstructures were observed using SEM, electron back-scatter diffraction (EBSD) and transmission electron microscopy (TEM) with energy dispersive spectroscopy (EDS). In the present study, the effects of Mn addition on the microstructure and mechanical properties of ODS FM steels were investigated. The ODS FM steels were manufactured by the MA, HIP and hot-rolling processes

  14. Hydrogen effect on mechanical properties and flake formation in the 10KhSND steel rolled plates

    Energy Technology Data Exchange (ETDEWEB)

    Muradova, R G; Zakharov, V A; Kuzin, A P; Gol' tsov, V A; Podgajskij, M S [Donetskij Politekhnicheskij Inst. (Ukrainian SSR); Donetskij Nauchno-Issledovatel' skij Inst. Chernoj Metallurgii (Ukrainian SSR))

    1982-01-01

    The effect of hydrogen on mechanical properties of the 10KhSND steel rolled plates during natural aging is studied. Optimum period of metal acceptance tests, which are advisable to conduct after 5-7 day natural aging of finished products, are found out. The technique is worked out and a safe hydrogen content to prevent flake formation in the 10KhSND steel is determined. It is shown that a safe hydrogen content is dependent on the experiment conditions (sample dimensions, conditions of cooling, and prehistory).

  15. Hydrogen effect on mechanical properties and flake formation in the 10KhSND steel rolled plates

    International Nuclear Information System (INIS)

    Muradova, R.G.; Zakharov, V.A.; Kuzin, A.P.; Gol'tsov, V.A.; Podgajskij, M.S.

    1982-01-01

    The effect of hydrogen on mechanical properties of the 10KhSND steel rolled plates during natural aging is studied. Optimum period of metal acceptance tests, which are advisable to conduct after 5-7 day natural aging of finished products, are found out. The technique is worked out and a safe hydrogen content to prevent flake formation in the 10KhSND steel is determined. It is shown that a safe hydrogen content is dependent on the experiment conditions (sample dimensions, conditions of cooling, and prehistory)

  16. Zn-10.2% Fe coating over carbon steel atmospheric corrosion resistance. Comparison with zinc coating

    International Nuclear Information System (INIS)

    Arnau, G.; Gimenez, E.; Rubio, M.V.; Saura, J.J.; Suay, J.J.

    1998-01-01

    Zn-10.2% Fe galvanized coating versus hot galvanized coating over carbon steel corrosion performance has been studied. Different periods of atmospheric exposures in various Valencia Community sites, and salt spray accelerated test have been done. Carbon steel test samples have been used simultaneously in order to classify exposure atmosphere corrosivity, and environmental exposure atmosphere characteristics have been analyzed. Corrosion Velocity versus environmental parameters has been obtained. (Author) 17 refs

  17. Non-destructive detection of fatigue in austenitic steel X6CrNiNb1810 in the HCF and VHCF range. Final report; Zerstoerungsfreie Detektion der Ermuedung von austenitischem Stahl X6CrNiNb1810 im HCF- und VHCF-Bereich. Abschlussbericht

    Energy Technology Data Exchange (ETDEWEB)

    Seiler, Georg; Boller, Christian [Univ. des Saarlandes, Saarbruecken (Germany). Lehrstuhl fuer Zerstoerungsfreie Pruefung und Qualitaetsmanagement

    2014-12-31

    In addition to load cycles in the Low Cycle Fatigue (LCF)-regime due to start up and shut down procedures of power plants, in some components additional high-frequency loadings in the High Cycle Fatigue (HCF)- and Very High Cycle Fatigue (VHCF)-regime occur. These loadings are induced e.g. by stresses due to thermal cyclic fluctuations and fluid dynamic processes. Therefore it is necessary to characterize experimentally the cyclic deformation behavior of metastable austenitic steels at operating temperature particularly in the HCF- and VHCF-regime and to develop a nondestructive method to detect fatigue processes. This joint research project was conducted in cooperation between the Institute of Materials Science and Engineering (WKK) of the University of Kaiserslautern and the Chair of Non-Destructive Testing and Quality Assurance of Saarland University (LZfPQ). WKK was focused on experimental investigations of the cyclic deformation behavior of metastable austenitic steel in the HCF- and VHCF-range, taking into account cyclic hardening and softening processes and in particular to consider fatigue-induced changes in microstructure. The samples were taken from a real pressurized water reactor component (surgeline). LZfPQ has focused on the development and application of a testing concept based on electromagnetic ultrasonic measurements. Within this subproject, electromagnetic acoustic transducers (EMATs) for in situ Operation in WKK's fatigue testing equipment have been developed and assembled. Single-step fatigue tests at elevated temperature (300 C) were conducted both with total-stress and strain control. During the test, the fatigue specimens were characterized by EMAT ultrasound in transmission mode. Different sensor types and wavemodes were used. The transmission signal was evaluated in terms of time of flight and amplitude. Both measured values are seen to behave in a characteristic manner depending on the test duration and the mechanical measured value

  18. Electrochemical characterisation of X10CrNi 18-8 steel in artificial plasma

    Directory of Open Access Journals (Sweden)

    J. Przondziono

    2015-01-01

    Full Text Available Quality of applied guide wires conditions the course of treatment and its success to a great extent. In order to simulate conditions that can be found in blood vascular system samples were exposed to artificial blood plasma (T = 37 } 1 oC for the time of 8 h. In order to obtain information regarding physical and chemical properties of modified surface of wire made of X10CrNi 18-8 steel, electrochemical impedance spectroscopy (EIS test and tests of chemical composition of the surface layer X-ray photoelectron spectroscopy (XPS were made. On the ground of performed EIS and XPS tests, favourable impact of steam sterilisation process on corrosion resistance of X10CrNi 18-8 steel was observed only for the case when chemical passivation was applied prior to sterilisation.

  19. The influence of interstitial impurities on temperature ranges of deuterium retention in austenitic stainless steel 18Cr10NiTi

    International Nuclear Information System (INIS)

    Neklyudov, I.M.; Morozov, O.M.; Kulish, V.G.; Zhurba, V.I.; Galytsky, A.G.; Piatenko, E.V.

    2009-01-01

    The influence of nitrogen, oxygen and helium on the temperature range of deuterium retention in 18Cr10NiTi stainless steel (of AISI304L type) has been investigated. It is demonstrated that the introduction of oxygen, nitrogen or helium into 18Cr10NiTi steel extends the upper limit in the high-temperature range of deuterium retention. It has been found that for 18Cr10NiTi stainless steel, pre-irradiated with helium ions, the increase in the temperature range of deuterium retention occurs in steps: on attainment of helium concentration of ∼0.5 at.% He the temperature range increases by ∼100 K, and on attainment of helium concentration of ∼2.5 at.% He the temperature range increases by ∼350 K. The introduction of oxygen into 18Cr10NiTi stainless steel results in the increase of the temperature range of deuterium retention in the direction of rise in temperature. In the deuterium thermodesorption spectrum, this manifests itself by the occurrence of an additional low-amplitude peak with the maximum temperature T m ∼ 560 K. The introduction of nitric impurity into 18Cr10NiTi stainless steel results in the extension of the temperature range of deuterium retention towards higher temperatures.

  20. Changes in mechanical properties and structure of electrolytic plasma treated X 12 CrNi 18 10 Ti stainless steel

    Energy Technology Data Exchange (ETDEWEB)

    Kurbanbekov, Sherzod; Baklanov, Viktor; Karakozov, Batyrzhan [Republican State Enterprise National Nuclear Center of Kazakhstan, Kurchatov (Kazakhstan). Inst. of Atomic Energy Branch; Skakov, Mazhyn [Republican State Enterprise National Nuclear Center of Kazakhstan, Kurchatov (Kazakhstan)

    2017-05-01

    The paper addresses findings regarding the influence of electrolytic plasma treatment on the mechanical properties as well as structural and phase states of X 12 CrNi 18 10 Ti steel. Electrolytic plasma treatment is based on carburizing of stainless steel heated in electrolytes. Treatment of steel samples has been performed as follows: the samples were heated up to a temperature between 850 and 950 C and then they were cured for 7 minutes in an electrolyte of an aqueous solution containing 10 % glycerol (C{sub 3}H{sub 8}O{sub 3}) and 15 % sodium carbonate (Na{sub 2}CO{sub 3}). It is found that, after plasma electrolytic treatment, the surface of X 12 CrNi 18 10 Ti steel had a modified structure and high hardness. Increasing wear resistance of X 12 CrNi 18 10 Ti steel has been observed after carburizing and the coefficient of friction has been reduced. X-ray analysis showed that retained austenite γ-Fe is a main phase, and there are some diffraction lines of orthorhombic Fe{sub 3}C phase as well as Fe{sub 3}O{sub 4} cubic phase. It has been determined, that, after plasma electrolytic treatment, a carbide phase in the modified surface layer, irrespective of the location in the steel structure has the chemical composition Fe{sub 3}C. High concentration of carbon atoms in a solid solution based on γ- and α-iron, a large dislocation density, presence of particles of carbide phase and retained austenite layers have been found.

  1. Investigation of Creep Processes and Microdamages in 10Kh9V2MFBR-Sh High-Chromium Steel

    Science.gov (United States)

    Grin', E. A.; Pchelintsev, A. V.

    2018-01-01

    During the modernization and the new construction of power units at TPPs in Russia, high-chromium martensitic steels with higher heat-resistant properties than the traditional perlite steels are increasingly used as structural materials. High-chromium steels have a necessary regulatory support for their use in domestic power engineering. However, up to the present time, the issue of assessing the quality of these steels at the analysis of their state during long-term operation remains open. The article proposed is one of the first attempts to create a system of quality criteria for martensitic steels based on their microdamage parameters. Tests were carried out on the long-term strength and creep of samples from 10Kh9V2MFBR-Sh steel at high temperatures with the construction of creep curves in relative coordinates "deformation related to the deformation of fracture, current time related to time to failure." For some samples, the tests were interrupted and the metal was subjected to metallographic studies consisting of the analysis of microdamage with reference to the accumulated creep strain. It has been shown experimentally that the deformation curve of high-chromium steel differs from the analogous curve of pearlitic steel by a longer and flat section of steady creep and by a sharper transition to the third accelerated creep stage, which has a very short time period (approximately 10% of the total durability). The tendency to the increase in the microdamage of the structure of steel as the accumulated creep strain increases with time was confirmed. The beginning of transition to the final creep phase is characterized by the formation of contours of future pore chains and by the appearance of individual large pores of up to 6 μm in size, the presence of which in the microstructure of the martensitic steel indicates a very significant accumulation of creep strain, and corresponds to the predestruction stage of metal. It is necessary to continue the research to

  2. H2 EJECTION FROM POLYCYCLIC AROMATIC HYDROCARBONS: INFRARED MULTIPHOTON DISSOCIATION STUDY OF PROTONATED ACENAPHTHENE AND 9,10-DIHYDROPHENANTHRENE

    International Nuclear Information System (INIS)

    Szczepanski, Jan; Vala, Martin T.; Oomens, Jos; Steill, Jeffrey D.

    2011-01-01

    The infrared multiple-photon dissociation (IRMPD) spectra of protonated acenaphthene ([ACN+H] + ) and 9,10-dihydrophenanthrene ([DHP+H] + ) have been recorded using an infrared free electron laser after the compounds were protonated by electrospray ionization and trapped in a Fourier transform ion cyclotron mass spectrometer. In both compounds, the loss of two mass units is predominant. Density functional calculations (B3LYP/6-311++G(d,p)) of the infrared spectra of all possible protonated isomers of each species showed that the observed IRMPD spectra are best fit to the isomer with the largest proton affinity and lowest relative electronic energy. Potential energy surfaces of the most stable isomers of [ACN+H] + and [DHP+H] + have been calculated for H and H 2 loss. The lowest energy barriers are for loss of H 2 , with predicted energies 4.28 and 4.15 eV, respectively. After H 2 ejection, the adjacent aliphatic hydrogens migrate to the bare ejection site and stabilize the remaining fragment. Single H loss may occur from [ACN+H] + but the energy required is higher. No single H loss is predicted from [DHP+H] + , only H migration around the carbon skeleton. The vibrational bands in the parent closed-shell protonated polycyclic aromatic hydrocarbons are compared to bands observed from the interstellar medium.

  3. Welding of high-strength stainless steel 03Kh12N10MT for cryogenic engineering

    International Nuclear Information System (INIS)

    Pustovit, A.I.

    1989-01-01

    Consideration is being given to weld resistance to cold and hot cracking at 93 and 77K and to mechanical properties of welded joints of high-strength stainless steel 03Kh12N10MT, produced under the fluxes AN-17M, AN-18, AN-26, AN-45, ANF-5, 48-OF-6, ANK-45 and ANK-49 in combination with various welding wires. It is shown that welds on 03Kh12N10MT steel meet the requirements only when using 48-OF-6 or ANK-49 flux. It is noted that impact strength of welds at 77K is sufficiently affected by the volume fraction of non-metallic inclusions in weld metal

  4. Effect of partial oxygen pressure on physicochemical properties of Kh18N10T steel at isothermal oxidation

    International Nuclear Information System (INIS)

    Alekseev, V.N.; Oshe, E.K.; Fokin, M.N.; Bogdanova, S.V.; Loskutov, A.I.

    1990-01-01

    Auger-electron spectroscopy, photoelectric polarization, conductometry methods have been used to analyze chemical and defect composition of surface oxide layers, formed on stainless steel Kh18N10T in vacuum (10 -9 - 10 -2 torr) and at temperatures 593-673 K. The boundary conditions of manifestation of extermal behaviour of the dependence of the surface oxide growth rate at isothermal oxidation of this steel are determined. The relation between passivation properties of the surface oxide and the magnitude of the edge angle of the surface wetting with molten tin is revealed

  5. Tandem organic light-emitting diodes with KBH4 doped 9,10-bis(3-(pyridin-3-yl)phenyl) anthracene connected to the charge generation layer.

    Science.gov (United States)

    Duan, Lian; Tsuboi, Taiju; Qiu, Yong; Li, Yanrui; Zhang, Guohui

    2012-06-18

    Tandem organic light emitting diodes (OLEDs) are ideal for lighting applications due to their low working current density at high brightness. In this work, we have studied an efficient electron transporting layer of KBH(4) doped 9,10-bis(3-(pyridin-3-yl)phenyl)anthracene (DPyPA) which is located adjacent to charge generation layer of MoO(3)/NPB. The excellent transporting property of the DPyPA:KBH(4) layer helps the tandem OLED to achieve a lower voltage than the tandem device with the widely used tris-(8-hydroxyquinoline)aluminum:Li. For the tandem white OLED with a fluorescent blue unit and a phosphorescent yellow unit, we've achieved a high current efficiency of 75 cd/A, which can be further improved to 120 cd/A by attaching a diffuser layer.

  6. Influence of the fabrication process parameters on microstructures and mechanical properties of 10Cr-1Mo ODS steel

    International Nuclear Information System (INIS)

    Jin, Hyun Ju; Kim, Ki Baik; Choi, Byoung Kwon; Kang, Suk Hoon; Noh, Sang Hoon; Kim, Ga Eon; Kim, Tae Kyu

    2016-01-01

    Oxide dispersion strengthened (ODS) FM steels have been developed as the most promising core structural material for high- temperature components operating in severe environments such as nuclear fusion and fission systems owing to its excellent elevated temperature strength and radiation resistance stemming from the addition of extremely thermally stable oxide particles dispersed in a ferritic/martensitic matrix. To realize the structural components such as plates, sheets and tubes in SFR, the development of manufacturing processes is an essential issue for the ODS FM steel. While the ODS steel has superior radiation resistance and high temperature strength, in comparison with the existing commercial steels, it is difficult for the ODS steel to obtain sufficient workability for the fabrication due to high hardness and low ductility at room temperature, meaning that the manufacturing of the ODS plate including cladding tube can be complicated by the low cold workability. In order to prevent the ODS steel from any damage during the manufacturing process, thus, the introduction of intermediate heat treatments between cold rolling processes is necessary. This study investigates effects of the fabrication process parameters such as the cold working ratio, the intermediate and final heat treatments on the microstructure and mechanical properties of 10Cr-1Mo ODS steel. In an effort to optimize the manufacturing route of the ODS FM steel, the microstructural and mechanical evolutions for the ODS plate manufactured by a control of the fabrication process parameters were evaluated in the present study. In the present study, the effect of a cold rolling and intermediate heat treatments on microstructures and mechanical properties of 10Cr-1Mo FM ODS steel were investigated. During the manufacturing route the hardness measurements remained below the critical value of 400 Hv. Intermediate heat treatment with slow cooling led to a softened ferritic structures which can be further

  7. PLASTIC DEFORMATION ON THE MACHINED SURFACE OF STEEL Cr20Ni10MoTi AT DRILLING

    Directory of Open Access Journals (Sweden)

    Jozef Jurko

    2009-07-01

    Full Text Available Information about material machinability is very important for the machining technology. Precise and reliable information on the machinability of a material before it enters the machining process is a necessity, and this brings the verification of technological methods in practice. This article presents the conclusions of machinability tests on austenitic stainless steel according to EN-EU (ISO: steel Cr20Ni10MoTi. This article presents the conclusions of VEGA grant agency at the Ministry of Education SR for supporting research work and co-financing the projects: Grant work #01/3173/2006 with the title „Experimental investigation of cutting zones in drilled and milled stainless steels

  8. 30 CFR 910.784 - Underground mining permit applications-minimum requirements for reclamation and operation plan.

    Science.gov (United States)

    2010-07-01

    ... requirements for reclamation and operation plan. 910.784 Section 910.784 Mineral Resources OFFICE OF SURFACE... for reclamation and operation plan. (a) Part 784 of this chapter, Underground Mining Permit Applications—Minimum Requirements for Reclamation and Operation Plan, shall apply to any person who makes...

  9. Ultrasound surface treatment of Kh18N10T steel with different structural state. Ul'trazvukovaya poverkhnostnaya obrabotka stali Kh18N10T s razlichnym strukturnym sostoyaniem

    Energy Technology Data Exchange (ETDEWEB)

    Aksenov, V K; Danilov, P A; Mats, A V; Netesov, V M; Yaes, A A [AN Ukrainskoj SSR, Kharkov (Ukrainian SSR). Fiziko-Tekhnicheskij Inst.

    1989-09-01

    Ultrasound surface treatment (USST) is studied for its effect on the structure and mechanical-and-physical properties of Kh18N10T steel with different prehistory. It is shown that surface treatment may both increase and decrease steel microhardness.

  10. Effect of temper and hydrogen embrittlement on mechanical properties of 2,25Cr–1Mo steel grades – Application to Minimum Pressurizing Temperature (MPT) issues. Part II: Vintage reactors and MPT determination

    International Nuclear Information System (INIS)

    Pillot, Sylvain; Chauvy, Cédric; Corre, Stéphanie; Coudreuse, Lionel; Gingell, Andrew; Héritier, Déborah; Toussaint, Patrick

    2013-01-01

    Standard and Vanadium-alloyed 2,25Cr–1Mo steel grades (EN 10028-2 12CrMo9-10/ASTM A387 gr. 22 and 13CrMoV9-10/ASTM A542 tp. D) are commonly used for the fabrication of heavy pressure vessels for applications in petroleum refining plants. These reactors are made of heavy plates, forged shells, forged nozzles and fittings. They are subjected to thermal cycles (stop and go) and to severe service conditions (high temperatures and high hydrogen partial pressures). A primary concern for end-users is the definition of the Minimum Pressurizing Temperature (MPT) of the equipment. This temperature is the lowest temperature at which the vessel can be repressurized after shutdown and insures no risk of brittle failure of the containment body. The MPT is defined by fracture mechanics and/or CVN approaches and calculations. This second part of the paper presents the methodology of MPT determination and the particular case of vintage reactors. MPT determination methodology is explained by using a virtual pressure vessel representative of vessels found in petroleum refineries. A special focus is also set on the evolution of embedded defects

  11. Effects of heat treatment condition on the mechanical properties and weldability of 10Cr-1Mo-VNbN cast steel

    International Nuclear Information System (INIS)

    Shon, Dae Young; Bang, Kook Soo; Lee, Kyong Woon; Chi, Byung Ha

    2003-01-01

    Mechanical properties and weldability such as HAZ hardness, cold cracking susceptibility and hot ductility of two differently heat treated 10Cr-1Mo-VNbN cast steels were measured and compared. Because of high hardenability of the cast steel, as-annealed cast steel showed martensitic microstructure and thus had higher hardness than annealed-normalized-tempered cast steel which had tempered martensite. Because the welding electrode used resulted in a high hardness weld metal, both cast steels showed same weld metal cold cracking susceptibility even though the as-annealed cast steel had higher HAZ hardness than the annealed-normalized-tempered cast steel. Both cast steels had excellent hot ductility in high temperature range, indicating no risk of grain boundary liquation cracking in the HAZ. However, the as-annealed cast steel showed an inferior ductility in the intermediate temperature range of 1000∼1150 .deg. C because of larger unrecrystallized grain size

  12. Tribocorrosion behaviour of 08CH18N10T steel

    International Nuclear Information System (INIS)

    Kubecka, P.; Tvrdy, M.; Wenger, F.; Ponthiaux, P.

    2000-01-01

    Tribocorrosion of the 08CH18N10T austenitic stainless steel in a potassium sulphate solution was investigated with the help of pin-on-disk tribometer and polarisation curves method. The results indicate the occurrence of synergetic interactions between electrochemical and mechanical conditions: the damaging of the passive film by friction was pointed out, leading to an increase in the dissolution rate of the metal and simultaneously, the occurrence of electrochemical reactions (gas evolution, dissolution, passivation) was found to modify the tribological conditions (friction coefficient). (author)

  13. Influence of local microplastic strains on stress corrosion of 08Kh18N10T steel

    International Nuclear Information System (INIS)

    Moskvin, L.N.; Efimov, A.A.; Sherman, Ya.I.; Fedorova, T.I.

    1987-01-01

    Study on specific features of microhomogeneous strain in the process of plastic strain development and their role in stress corrosion of 08Kh18N10T steel sheet specimens subject to preliminary strain by 1, 3, 6, 16 and 23% and subsequent tests of stress corrosion in magnesium chloride solution at 150 deg C 140 MPa has been carried out. Analysis of test results has shown that microplastic strain is distributed over a specimen nonuniformly and is accompanied with the slip bands formation which are sources of corrosion crack origination and development. 08Kh18N10T steel manifests the highest trend to stress corrosion under 1% microplastic strain

  14. 30 CFR 910.780 - Surface mining permit applications-minimum requirements for reclamation and operation plan.

    Science.gov (United States)

    2010-07-01

    ... requirements for reclamation and operation plan. 910.780 Section 910.780 Mineral Resources OFFICE OF SURFACE... reclamation and operation plan. (a) Part 780 of this chapter, Surface Mining Permit Applications—Minimum Requirement for Reclamation and Operation Plan, shall apply to any person who makes application to conduct...

  15. The effect of refurbishing a UK steel plant on PM10 metal composition and ability to induce inflammation

    Directory of Open Access Journals (Sweden)

    Maynard Robert L

    2005-05-01

    Full Text Available Abstract Background In the year 2000 Corus closed its steel plant operations in Redcar, NE of England temporarily for refurbishment of its blast furnace. This study investigates the impact of the closure on the chemical composition and biological activity of PM10 collected in the vicinity of the steel plant. Methods The metal content of PM10 samples collected before during and after the closure was measured by ICP-MS in order to ascertain whether there was any significant alteration in PM10 composition during the steel plant closure. Biological activity was assessed by instillation of 24 hr PM10 samples into male Wistar rats for 18 hr (n = 6. Inflammation was identified by the cellular and biochemical profile of the bronchoalveolar lavage fluid. Metal chelation of PM10 samples was conducted using Chelex beads prior to treatment of macrophage cell line, J774, in vitro and assessment of pro-inflammatory cytokine expression. Results The total metal content of PM10 collected before and during the closure period were similar, but on reopening of the steel plant there was a significant 3-fold increase (p 10 collected during the reopened period, as well as significant increases in albumin (p 10 from the pre-closure and closure periods did not induce any significant alterations in inflammation or lung damage. The soluble and insoluble extractable PM10 components washed from the reopened period both induced a significant increase in neutrophil cell number (p 10 from the re-opened period stimulated J774 macrophages to generate TNF-α protein and this was significantly prevented by chelating the metal content of the PM10 prior to addition to the cells. Conclusion PM10-induced inflammation in the rat lung was related to the concentration of metals in the PM10 samples tested, and activity was found in both the soluble and insoluble fractions of the particulate pollutant.

  16. 30 CFR 910.702 - Exemption for coal extraction incidental to the extraction of other minerals.

    Science.gov (United States)

    2010-07-01

    ... 30 Mineral Resources 3 2010-07-01 2010-07-01 false Exemption for coal extraction incidental to the extraction of other minerals. 910.702 Section 910.702 Mineral Resources OFFICE OF SURFACE MINING RECLAMATION... minerals. Part 702 of this chapter, Exemption for Coal Extraction Incidental to the Extraction of Other...

  17. Proceedings of the Modeling Evidence in HPV Pre-Conference Workshop in Malmö, Sweden, May 9-10, 2009.

    Science.gov (United States)

    Craig, Benjamin M; Brisson, Marc; Chesson, Harrell; Giuliano, Anna R; Jit, Mark

    2010-08-01

    Prominent published and active human papillomavirus (HPV) modelers from around the world were invited to participate in the inaugural Modeling Evidence in HPV (MEHPV) Pre-Conference Workshop on May 9-10, 2009, in Malmö, Sweden. The workshop took place directly before the 25th International Papillomavirus Conference. The aim of the workshop was to develop an international network of investigators engaged in HPV modeling and to facilitate open discussion about the structure and parameterization of models, as well as other methodologic concerns. Thirty-four participants from more than a dozen countries and a variety of settings, representing the authors or coauthors of 82% of the HPV modeling literature, exchanged ideas on fundamental questions in the field. These proceedings, based on the 217-page transcript, were assembled by the Scientific Committee to summarize the ideas of workshop participants in a deidentified, readable fashion. They represent the work and recorded opinions of session participants and do not constitute the official positions of participants as a whole or individually, the Scientific Committee, or any sponsoring organization or entity. In charting a path forward, 3 topics emerged as most pressing: best practices for HPV modeling, comparative modeling, and modeling in developing countries. This summary of the proceedings of the preconference workshop on HPV modeling characterizes many of the prominent contemporary issues in the field. 2010 Excerpta Medica Inc. All rights reserved.

  18. Susceptibility to stress corrosion in stainless steels type AISI 321 and 12X18H10T used in PWR type reactors (WWER)

    International Nuclear Information System (INIS)

    Matadamas C, N.

    1995-01-01

    Titanium stabilized stainless steels have been utilized in sovietic pressurized water reactors (VVER) for avoid the susceptibility to Intergranular Corrosion (IGC) present in other austenitic stainless steels. However the Intergranular Corrosion resistance of this kind of materials has been questioned because of Intergranular Stress Corrosion Cracking failures (IGSCC) have been reported. This paper study the electrochemical behavior of the AISI 321 stainless steel in a H 3 BO 3 Solution contaminated with chlorides and its susceptibility to Intergranular Corrosion.Electrochemical prediction diagrams of the stainless steels AISI 321 and 12X18H10T (sovietic) sensitized (600 Centigrade, 3 h.) were compared. Cylindrical and conical samples were used in Slow Strain Rate Tests (SSRT), to determine the susceptibility to Stress Corrosion Cracking (SCC) in AISI 321 and 12X18H10T stainless steels. The results obtained showed that the temperature of the solution is a very important factor to detect this susceptibility. Fractography studies on the fracture surfaces of the samples obtained in the SSRT at high temperature were realized. Corrosion velocities of both AISI 321 and 12X18H10T stainless steels were determined using conical samples in the CERT system at high temperature. E.D.A.X. analysis was employed in both AISI 321 and 12X18H10T stainless steels in order to explain the degree of sensitization. (Author)

  19. Microstructural stability of fast reactor irradiated 10 to 12% Cr ferritic-martensitic stainless steels

    International Nuclear Information System (INIS)

    Little, E.A.; Stoter, L.P.

    1982-01-01

    The strength and microstructural stability of three 10 to 12% Cr ferritic-martensitic stainless steels have been characterized following fast reactor irradiation to damage levels of 30 displacements per atom (dpa) at temperatures in the range 380 to 615 0 C. Irradiation results in either increases or decreases in room temperature hardness depending on the irradiation temperature. These strength changes can be qualitatively rationalized in terms of the combined effects of irradiation-induced interstitial dislocation loop formation and recovery of the dislocation networks comprising the initial tempered martensite structures. Precipitate evolution in the irradiated steels is associated with the nonequilibrium segregation of the elements nickel, silicon, molybdenum, chromium and phosphorus, brought about by solute-point defect interactions. The principal irradiation-induced precipitates identified are M 6 X, intermetallic chi and sigma phases and also α' (Cr-rich ferrite). The implications of the observed microstructural changes on the selection of martensitic stainless steels for fast reactor wrapper applications are briefly considered

  20. 30 CFR 910.761 - Areas designated unsuitable for surface coal mining by Act of Congress.

    Science.gov (United States)

    2010-07-01

    ... 30 Mineral Resources 3 2010-07-01 2010-07-01 false Areas designated unsuitable for surface coal mining by Act of Congress. 910.761 Section 910.761 Mineral Resources OFFICE OF SURFACE MINING RECLAMATION... Congress. Part 761 of this chapter, Areas Designated by Act of Congress, shall apply to surface coal mining...

  1. Development of plastic deformations in 12Kh18N10T steel under cyclic symmetrical bending of specimens of various length

    Energy Technology Data Exchange (ETDEWEB)

    Pisarenko, G.S.; Leonets, V.A.; Bega, N.D. (AN Ukrainskoj SSR, Kiev. Inst. Problem Prochnosti)

    1983-08-01

    Effect of specimen length on intensity of plastic deformation development and cyclic strength is studied for annealed 12Kh18N10T steel under cyclic symmetrical bending. The intensity of microplastic deformations and cyclic strength of annealed 12Kh18N10T steel in the considered case is due to self-heating.

  2. Impact of neighbourhood food environment on food consumption in children aged 9-10 years in the UK SPEEDY (Sport, Physical Activity and Eating behaviour: Environmental Determinants in Young people) study.

    Science.gov (United States)

    Skidmore, Paula; Welch, Ailsa; van Sluijs, Esther; Jones, Andrew; Harvey, Ian; Harrison, Flo; Griffin, Simon; Cassidy, Aedín

    2010-07-01

    Poor diet in childhood increases risk of obesity but the relationship between access to food and children's food choice is underexplored. We determined relationships between distance to and density of food outlets on children's food choice. Children (n 1721) aged 9-10 years who participated in a cross-sectional study from a sample of state and private schools across urban and rural areas. Food consumption was reported using a short validated FFQ. A Geographic Information System was used to determine proximity to local food outlets. Multivariable regression analyses were performed to determine associations between food consumption and distance to and density of local food outlets. Norfolk, England. Boys (n 754) and girls (n 967) aged 9-10 years. The impact of distance to or density of food outlets on food choice was small after adjustment. Living further away from a supermarket increased portions of fruit (0.11 portions/week per 1 km increase in distance to nearest supermarket, P < 0.05) and vegetables (0.11 portions/week, P < 0.05) consumed. Living closer to convenience stores was also associated with an increased consumption of crisps, chocolate and white bread. Density of supermarkets was associated with both an increase in vegetable intake (0.31 portions/week, P < 0.05) and unhealthy foods. Distance to and density of food outlets are both associated with children's food choice, although the impact appears to be small and the relationship is complex. However, the effects of individual foods combined could be important, particularly as even small differences in intake can impact on body weight over time.

  3. Fatigue behaviour of the austenitic steel 1.4550 under mechanical and thermal cyclic loading

    Energy Technology Data Exchange (ETDEWEB)

    Siegele, D.; Fingerhuth, J.; Varfolomeev, I.; Moroz, S. [Fraunhofer Institute for Mechanics of Materials (IWM), Freiburg (Germany)

    2014-07-01

    Fatigue behaviour of the austenitic steel 1.4550 (X6CrNiNb18-10) under low-cycle fatigue and high-cycle thermal fatigue was investigated with in two research projects supported by the Federal Ministry of Economic Affairs and Energy and the Ministry of Education and Research. The objectives of the projects were the gain of deep understanding of the damage mechanisms under mechanical and thermal cyclic loading and the development of material models and simulation procedures for an improved lifetime assessment. In comparison to the advanced mechanism based material models engineering computational procedures were proven with respect to their applicability and conservatisms. For thermal cyclic loading, test equipment and technique were developed which allow for cyclic thermal loading with temperature ranges between 1 00 C and 300 C and frequencies between 0.1 and 1 Hz. As a result, tests with a temperature range of 150 C and lower showed no crack formation up to 300,000 cycles. For temperature ranges of 200 C and higher multiple crack patterns were observed with the deepest crack of about 1.3 mm after 1,000,000 cycles, whereas the difference in crack depth between 300,000 and 1,000,000 cycles was negligibly small. To model the fatigue lifetime, the D{sub TMF} damage parameter was applied to the low-cycle fatigue and the thermal, high frequent fatigue tests. For thermal fatigue, the analyses predicted in agreement with the tests crack initiation followed by crack propagation, subsequent retardation and arrest. This behaviour can be explained qualitatively and quantitatively using the methods of linear-elastic fracture mechanics, whereas the consideration of the interaction of multiple cracks is essential to describe the experimentally observed crack retardation. The results for thermal fatigue are in the scatterband of the mechanical p and thermo-mechanical fatigue results and the cycles to failure are 10 times higher than those estimated according to the KTA fatigue

  4. Electrochemical noise measurements of steel corrosion in the molten NaCl-K2SO4 system

    DEFF Research Database (Denmark)

    Cappeln, Frederik Vilhelm; Bjerrum, Niels; Petrushina, Irina

    2005-01-01

    -called active corrosion (i.e., the corrosion proceeds with no passivation due to the influence of chlorine), characterized by the formation of volatile metal chlorides as a primary corrosion product. It was found possible to obtain an empirical separation of general and intergranular corrosion using kurtosis (a......Electrochemical noise measurements have been carried out on AISI347, 10CrMo910, 15Mo3, and X20CrMoV121 steels in molten NaCl-K2SO4 at 630 degrees C. Different types of current noise have been identified for pitting, intergranular and peeling corrosion. The corrosion mechanism was the so...... statistical parameter calculated from the electrochemical noise data). It was found that average kurtosis values above 6 indicated intergranular corrosion and average values below 6 indicated general corrosion. The response time for localized corrosion detection in in-plant monitoring was approximately 90 min...

  5. Chameleonic reactivity of vicinal diazonium salt of acetylenyl-9,10-anthraquinones: synthetic application toward two heterocyclic targets.

    Science.gov (United States)

    Stepanov, A A; Gornostaev, L M; Vasilevsky, S F; Arnold, E V; Mamatyuk, V I; Fadeev, D S; Gold, B; Alabugin, I V

    2011-11-04

    The nature of products in the diazotization of 1-amino-2-acetylenyl-9,10-anthraquinones strongly depends on the nature of substituents at both the alkyne and at the anthraquinone core. Donor substitution (NHAr, OH) at the fourth position stabilizes the diazonium salt at C1, decelerating electrophilic cyclization at the arylethynyl substituent at C2. This effect allows the replacement of the diazonium with azide group and subsequent closure into isoxazole ring with preservation of the alkyne. In contrast, electrophilic 5-exo-dig cyclizations to condensed pyrazoles is observed for the combination of donor substituents at the aryl alkyne moiety and an OAc substituent at C4. The latter process provides a new synthetic route to 3-ethynyl-[1,9-cd]isoxazol-6-ones that are difficult to access otherwise. DFT calculations suggest that donor substituents have only a minor effect on alkyne and diazonium polarization in the reactant but provide specific transition state stabilization by stabilizing the incipient vinyl cation. This analysis provides the first computational data on electrophilic 5-exo-dig cyclization in its parent form and the nucleophile-promoted version. This cyclization is a relatively fast but endothermic process that is rendered thermodynamically feasible by the enol-keto tautomerization with concomitant aromatization in the five-membered heteroaromatic ring. Computations suggest that the importance of nucleophilic assistance in the transition state for a relatively weak nucleophile such as water is minor because the energy gain due to the Lewis base coordination to the carbocationic center is more than compensated for by the unfavorable entropic term for the bimolecular proces.

  6. Influence of Mn contents in 0Cr18Ni10Ti thin wall stainless steel tube on TIG girth weld quality

    Science.gov (United States)

    Liu, Bo

    2017-03-01

    Three kinds of cold worked 0Cr18Ni10Ti thin wall stainless steel tubes with the manganese contents of 1.27%, 1.35% and 1.44% and the cold worked 0Cr18Ni10Ti stainless steel end plug with manganese content of 1.35% were used for TIG girth welding in the present investigation. The effect of different manganese contents in stainless steel tube on weld quality was studied. The results showed that under the same welding conditions, the metallographic performance of the girth weld for the thin wall stainless steel tube with the manganese element content 1.44% welded with end plug was the best. Under the appropriate welding conditions, the quality of the girth weld increased with the increase of the manganese content till 1.44%. It was found that in the case of the Mn content of 1.44%, and under the proper welding condition the welding defects, such as welding cracks were effectively avoided, and the qualified weld penetration can be obtained.. It is concluded that the appropriate increase of the manganese content can significantly improve the TIG girth weld quality of the cold worked 0Cr18Ni10Ti stainless steel tube.

  7. Influence of different amino substituents in position 1 and 4 on spectroscopic and acid base properties of 9,10-anthraquinone moiety.

    Science.gov (United States)

    Wcisło, Anna; Niedziałkowski, Paweł; Wnuk, Elżbieta; Zarzeczańska, Dorota; Ossowski, Tadeusz

    2013-05-01

    A series of novel 1-amino and 1,4-diamino-9,10-anthraquinones, substituted with different alkyl groups, were synthesized as the result of alkylation with amino substituents. All the obtained aminoanthraquinone derivatives were characterized by NMR, IR spectroscopy and mass spectrometry. The spectroscopic properties of these compounds were determined by using UV-Vis spectroscopy in acetonitrile, and in the mixture of acetonitrile and methanol at different pH ranges. The effects of various substituents present in the newly developed anthraquinone derivatives and their ability to form hydrogen bonds between the carbonyl oxygen atom of anthraquinone moiety and nitrogen atom of N-H group in 1-aminoanthraquinone (1-AAQ) and 1,4-diaminoanthraquinone (1,4-DAAQ) were studied. Additionally, the effects of hydrogen bond formation between O-H group in hydroxyethylamino substituent and the carbonyl oxygen atom of anthraquinone were investigated. The spectroscopic behavior of the studied derivatives strongly depended on the solvent-solute interactions and the nature of solvent. The values of pKa for the new anthraquinones were determined by the combined potentiometric and spectrophotometric titration methods. Copyright © 2013 Elsevier B.V. All rights reserved.

  8. Efficacy of krypton laser photodynamic therapy for oral mucosa dysplasia in 9,10-dimethyl-1,2-benzanthracene-treated hamsters.

    Science.gov (United States)

    Shen, Lingyue; Xu, Qing; Li, Pingping; Zhou, Guoyu

    2013-11-01

    The present study aimed to evaluate the efficacy of krypton laser photodynamic therapy (PDT) with PsD-007 for the treatment of oral mucosa dysplasia in 9,10-dimethyl-1,2-benzanthracene (DMBA)-treated hamsters. A DMBA-induced hamster cheek pouch model of precancerous lesions was created and the resultant 25 hamsters were divided into five groups. The right side was treated with PDT and the left side was used as the positive control. Following systemic anesthesia, an incision was made in the groin area to expose the femoral vein. PsD-007 was administered intravenously through the femoral vein. Various doses of photosensitizer were used to treat groups A-E. Subsequent to closing the incision, the right side of the buccal mucosa was irradiated with light using the krypton laser at a wavelength of 413 nm, a power density of 150 mW/cm 2 and an irradiation time of 20 min. At six weeks post-surgery, the response was analyzed using histological examinations of the buccal pouch mucosa. A total of 24 hamsters completed the six-week observation period, as one hamster from group C died in the second week following the PDT. Of all 24 irradiated sides, 15 formed normal mucosal tissues and nine demonstrated mild dysplasia. Of the total control sides, six developed moderate dysplasia, five developed severe dysplasia and 13 progressed to carcinoma in situ or squamous cell carcinoma (SCC). The results revealed a significant difference between the two sides (P10 mg/kg, there was no statistical difference (P>0.05). PsD-007-mediated krypton laser PDT is effective for the treatment of oral mucosa dysplasia in hamsters.

  9. Pet ownership, dog types and attachment to pets in 9-10 year old children in Liverpool, UK.

    Science.gov (United States)

    Westgarth, Carri; Boddy, Lynne M; Stratton, Gareth; German, Alexander J; Gaskell, Rosalind M; Coyne, Karen P; Bundred, Peter; McCune, Sandra; Dawson, Susan

    2013-05-13

    Little is known about ethnic, cultural and socioeconomic differences in childhood ownership and attitudes to pets. The objective of this study was to describe the factors associated with living with different pet types, as well as factors that may influence the intensity of relationship or 'attachment' that children have to their pet. Data were collected using a survey of 1021 9-10 year old primary school children in a deprived area of the city of Liverpool, UK. Dogs were the most common pet owned, most common 'favourite' pet, and species most attached to. Twenty-seven percent of dog-owning children (10% of all children surveyed) reported living with a 'Bull Breed' dog (which includes Pit Bulls and Staffordshire Bull Terriers), and the most popular dog breed owned was the Staffordshire Bull Terrier. Multivariable regression modelling identified a number of variables associated with ownership of different pets and the strength of attachment to the child's favourite pet. Girls were more likely to own most pet types, but were no more or less attached to their favourite pet than boys. Children of white ethnicity were more likely to own dogs, rodents and 'other' pets but were no more or less attached to their pets than children of non-white ethnicity. Single and youngest children were no more or less likely to own pets than those with younger brothers and sisters, but they showed greater attachment to their pets. Children that owned dogs lived in more deprived areas than those without dogs, and deprivation increased with number of dogs owned. 'Pit Bull or cross' and 'Bull Breed' dogs were more likely to be found in more deprived areas than other dog types. Non-whites were also more likely to report owning a 'Pit Bull or cross' than Whites. Gender, ethnicity and socioeconomic status were associated with pet ownership, and sibling status with level of attachment to the pet. These are important to consider when conducting research into the health benefits and risks of the

  10. Morphology-Controlled 9,10-Diphenylanthracene Nanoblocks as Electrochemiluminescence Emitters for MicroRNA Detection with One-Step DNA Walker Amplification.

    Science.gov (United States)

    Liu, Jia-Li; Tang, Zhi-Ling; Zhang, Jia-Qi; Chai, Ya-Qin; Zhuo, Ying; Yuan, Ruo

    2018-04-17

    The electrochemiluminescence (ECL) properties of polycyclic aromatic hydrocarbons (PAHs) are excellent on account of the high photoluminescence quantum yield. However, the poor solubility and radical instability of PAHs in the aqueous solution severely restricted further biological application. Here 9,10-diphenylanthracene (DPA) nanoblocks (NBs) with good dispersibility and stability in aqueous solution were prepared according to morphology-controlled technology employing water-soluble polymers as a protectant. Furthermore, an ECL "off-on" switch biosensor was developed based on a novel ECL ternary system with DPA NBs as luminophore, dissolved O 2 as coreactant, and Pt-Ag alloy nanoflowers as the coreaction accelerator, which achieved a high-intense initial ECL signal. Subsequently, the Fc-DNA as ECL signal quencher was assembled on the electrode surface to quench the initial ECL signal for a "signal-off" state. Meanwhile, DNA swing arm was modified on the electrode surface for one-step DNA walker amplification. Interestingly, in the presence of miRNA-141 and T7 Exo, the one-step DNA walker amplification was executed to recover a strong ECL signal as a "signal-on" state by the digestion of Fc-DNA. Thus the developed ECL "off-on" switch biosensor possesses a detection limit down to 29.5 aM for ultrasensitive detection of miRNA-141, which is expected to be applicable to the detection of miRNA in clinic tumor cells.

  11. Protective effect of KhOSP-10 inhibitor during corrosion, hydrogenadsorption and corrosion cracking of a steel in sulfuric acid

    Energy Technology Data Exchange (ETDEWEB)

    Mindyuk, A K; Svist, E I; Savitskaya, O P; Goyan, E B; Gopanenko, A N [AN Ukrainskoj SSR, Lvov. Fiziko-Mekhanicheskij Inst.

    1975-01-01

    The protective propeties of inhibitor KhOSP-10 in the time of corrosion and corrosive cracking of steel 40Kh are higher then those of inhibitors KPI-1, KI-1, I-I-V etc. Its ability to reduce steel hydrogenation is the same as in the case of KPI-1 inhibitor i.e. below that of KI-1. HCl additives enhance the efficiency of inhibitors KPI-1, KI-1, I-1-V etc. up to the protective ability of KhOSP-10. Kinetics of the electrode processes was estimated from polarization curves.

  12. Low-Cycle Fatigue Behavior of 10CrNi3MoV High Strength Steel and Its Undermatched Welds.

    Science.gov (United States)

    Song, Wei; Liu, Xuesong; Berto, Filippo; Razavi, S M J

    2018-04-24

    The use of high strength steel allows the design of lighter, more slender and simpler structures due to high strength and favorable ductility. Nevertheless, the increase of yield strength does not guarantee the corresponding improvement of fatigue resistance, which becomes a major concern for engineering structure design, especially for the welded joints. The paper presents a comparison of the low cycle fatigue behaviors between 10CrNi3MoV high strength steel and its undermatched weldments. Uniaxial tension tests, Push-pull, strain-controlled fatigue tests were conducted on base metal and weldments in the strain range of 0.2⁻1.2%. The monotonic and cyclic stress-strain curves, stress-life, strain-life and energy-life in terms of these materials were analyzed for fatigue assessment of materials discrepancy. The stress-life results of base metal and undermatched weld metal exhibit cyclic softening behaviors. Furthermore, the shapes of 10CrNi3MoV steel hysteresis loops show a satisfactory Masing-type behavior, while the weld metal shows a non-Masing type behavior. Strain, plastic and total strain energy density amplitudes against the number of reversals to failure results demonstrate that the undermatched weld metal presents a higher resistance to fatigue crack initiation than 10CrNi3MoV high strength steel. Finally, fatigue fracture surfaces of specimens were compared by scanning electron microscopy to identify the differences of crack initiation and the propagation between them.

  13. Low-Cycle Fatigue Behavior of 10CrNi3MoV High Strength Steel and Its Undermatched Welds

    Directory of Open Access Journals (Sweden)

    Wei Song

    2018-04-01

    Full Text Available The use of high strength steel allows the design of lighter, more slender and simpler structures due to high strength and favorable ductility. Nevertheless, the increase of yield strength does not guarantee the corresponding improvement of fatigue resistance, which becomes a major concern for engineering structure design, especially for the welded joints. The paper presents a comparison of the low cycle fatigue behaviors between 10CrNi3MoV high strength steel and its undermatched weldments. Uniaxial tension tests, Push-pull, strain-controlled fatigue tests were conducted on base metal and weldments in the strain range of 0.2–1.2%. The monotonic and cyclic stress-strain curves, stress-life, strain-life and energy-life in terms of these materials were analyzed for fatigue assessment of materials discrepancy. The stress-life results of base metal and undermatched weld metal exhibit cyclic softening behaviors. Furthermore, the shapes of 10CrNi3MoV steel hysteresis loops show a satisfactory Masing-type behavior, while the weld metal shows a non-Masing type behavior. Strain, plastic and total strain energy density amplitudes against the number of reversals to failure results demonstrate that the undermatched weld metal presents a higher resistance to fatigue crack initiation than 10CrNi3MoV high strength steel. Finally, fatigue fracture surfaces of specimens were compared by scanning electron microscopy to identify the differences of crack initiation and the propagation between them.

  14. Passivation Characteristics of Alloy Corrosion-Resistant Steel Cr10Mo1 in Simulating Concrete Pore Solutions: Combination Effects of pH and Chloride.

    Science.gov (United States)

    Ai, Zhiyong; Sun, Wei; Jiang, Jinyang; Song, Dan; Ma, Han; Zhang, Jianchun; Wang, Danqian

    2016-09-01

    The electrochemical behaviour for passivation of new alloy corrosion-resistant steel Cr10Mo1 immersed in alkaline solutions with different pH values (13.3, 12.0, 10.5, and 9.0) and chloride contents (0.2 M and 1.0 M), was investigated by various electrochemical techniques: linear polarization resistance, electrochemical impedance spectroscopy and capacitance measurements. The chemical composition and structure of passive films were determined by XPS. The morphological features and surface composition of the immersed steel were evaluated by SEM together with EDS chemical analysis. The results evidence that pH plays an important role in the passivation of the corrosion-resistant steel and the effect is highly dependent upon the chloride contents. In solutions with low chloride (0.2 M), the corrosion-resistant steel has notably enhanced passivity with pH falling from 13.3 to 9.0, but does conversely when in presence of high chloride (1.0 M). The passive film on the corrosion-resistant steel presents a bilayer structure: an outer layer enriched in Fe oxides and hydroxides, and an inner layer, rich in Cr species. The film composition varies with pH values and chloride contents. As the pH drops, more Cr oxides are enriched in the film while Fe oxides gradually decompose. Increasing chloride promotes Cr oxides and Fe oxides to transform into their hydroxides with little protection, and this is more significant at lower pH (10.5 and 9.0). These changes annotate passivation characteristics of the corrosion-resistant steel in the solutions of different electrolyte.

  15. 30 CFR 910.827 - Special performance standards-coal processing plants and support facilities not located at or...

    Science.gov (United States)

    2010-07-01

    ... mining and reclamation operations which includes the operation of coal processing plants and support... plants and support facilities not located at or near the minesite or not within the permit area for a mine. 910.827 Section 910.827 Mineral Resources OFFICE OF SURFACE MINING RECLAMATION AND ENFORCEMENT...

  16. Damage development - effects of multiaxial loads on creep pore formation and fatigue damage in typical power plant steels. Final report

    International Nuclear Information System (INIS)

    Lenk, P.; Proft, D.; Kussmaul, A.; Fischer, R.

    2000-01-01

    The influence of multiaxial stress on creep pore formation in the steels 14MoV6-3 10CrMo9-10 and X10CrMoVNb9-1 was investigated on the basis of internal pressure experiments on smooth and notched hollow cylinders. In some cases, additional axial forces were applied in order to reproduce component-relevant multiaxial stresses. Local elongation during loading was investigated and analyzed using applied HT-DMS. When different strain levels had been reached, the samples were removed, analyzed, and characterized with regard to different damage parameters. It was found that no interdependence between the surface damage pattern and the deep damage pattern can be derived across the wall thickness if no information on the load state is available. Parallel to the experiments, inelastic FEA were carried out using the ABAQUS program system. The creep law of Graham and Walles was used for calculating flow and creep via a user-defined subroutine CREEP. The parameters of the creep law could be identified by adaptation to monoaxial creep tests [de

  17. Structural changes in surface layer of steel 08Kh18N10T during machining

    International Nuclear Information System (INIS)

    Palenik, J.; Vodarek, V.

    1989-01-01

    The results are reported of a study of the surface layer of steel 08Kh18N10T affected by machining. Structural changes were studied caused by finish turning and by additional roller burnishing. Multiple deformation bands were observed to occur under the given cutting conditions; they mainly consisted of deformation doublets and only in isolated cases of ε-martensite. The presence of α'-martensite was not shown in the specimen surface layer following finish turning. The deformation shear bands in the roller-burnished specimen consisted of both ε-martensite and of deformation doublets. The amount of ε-martensite in the structure was significantly higher than in the specimen worked by turning. Local presence of α'-martensite formations was observed inside the deformation bands. It thus follows that roller burnishing is unsuitable as part of the manufacture of components from steel 08Kh18N10T. (J.B.). 5 figs., 1 tab., 9 refs

  18. Extracts from Kang-T'ieh (Steel), Issue Number 10 - Communist China

    National Research Council Canada - National Science Library

    1960-01-01

    .... Big Drop in Pig Iron Consumption for converter steel production, 3. Surpass the Open-Hearth Furnace, Catch up with the electric furnace and struggle for high quality and varieties of products in converter steel production, 4...

  19. 32 CFR 37.910 - How long must I require participants to keep records related to the TIA?

    Science.gov (United States)

    2010-07-01

    ... records related to the TIA? 37.910 Section 37.910 National Defense Department of Defense OFFICE OF THE... require participants to keep records related to the TIA? Your TIA must require participants to keep records related to the TIA (for which the agreement provides Government access under § 37.915) for a...

  20. Technology development and production of elongated shell for reactor vessel active zone of WWER-TOI project from steel 15Cr2NiMoVN class 1

    International Nuclear Information System (INIS)

    Shklyaev, S.Eh.; Titova, T.I.; Ratushev, D.V.; Shul'gan, N.A.; Eroshkin, S.B.; Durynin, V.A.; Efimov, S.V.; Dub, V.S.; Kulikov, A.P.; Romashkin, A.N.

    2015-01-01

    Production process for the elongated shell blank of the active zone of the reactor pressure vessel made from steel 15Cr2NiMoVN Class 1 with finished sizes Dext=4.655 mm, Dint=4.240 mm, H=4.910 mm (height for heat treatment – 5.750 mm) is presented. For the first time in Russia in production site of OMZ-Special steel LLC a unique elongated shell blank of the reactor vessel active zone was made from ingot 420.0 t for WWER-TOI project fully meeting the specified requirements in terms of metallurgical quality and set of service properties [ru

  1. The rupture strength of dissimilar joints in high temperature

    International Nuclear Information System (INIS)

    Groenwall, B.

    1992-05-01

    In dissimilar joints between austenitic stainless steels and ferritic steels the heat affected zone in the ferritic steel always is the weakest link. Two different joints where the ferritic steel has been 10CrMo910 (2.25Cr1Mo) and X20CrMoV121 respectively (162Cr1Mo0.3V) has been investigated through thermal cycling and isothermal creep testing. In this case the purpose has been to investigate the weakest link and therefore both 10CrMo910 and X20CrMoV121 have been welded to themselves using the TIG-method with Inconel 82 (70Cr20Cr3Mn2). 5Nb as filler wire. Crossweld specimens have been taken from the joints. To accelerate the testing the tip temperature at thermal cycling and the temperature at isothermal creep testing has been in the region 600-650 degrees C. Low ductile fracture, which is typical for failures in practice, has been obtained by using a moderate tensile stress, 63 N/mm 2 . In the high temperature range, 650 degrees C, the thermal cycling compared to the isothermal testing had no influence but in lower temperatures the cycling caused decreased time to rupture. The time to rupture in thermal cycling as well as in isothermal testing as a function of testing temperature can be fitted to exponential curve of type t = a x e bT (where t and T are time and temperature respectively). Through extrapolation of the measured data it has been found that 10CrMo910 in hard conditions that is thermal cycling has a life time at 500 degrees C of about 100 000 h. If the operational temperature is constant the life time will be about four times longer. The X20CrMoV121 on the other hand has a life time at thermal cycling at 500 degrees C and moderate tensile stress of about 3 000 000 h. This means that the tensile stress can be increased considerably. The cracks appear in 10CrMo910 closely to the fusion line but in the X20CrMoV121 steel cracking and fracture arise in the heat affected zone some millimeters from the fusion line. (au)

  2. Spectroscopic, computational and electrochemical studies on the formation of the copper complex of 1-amino-4-hydroxy-9,10-anthraquinone and effect of it on superoxide formation by NADH dehydrogenase.

    Science.gov (United States)

    Roy, Sanjay; Mondal, Palash; Sengupta, Partha Sarathi; Dhak, Debasis; Santra, Ramesh Chandra; Das, Saurabh; Guin, Partha Sarathi

    2015-03-28

    A 1 : 2 copper(II) complex of 1-amino-4-hydroxy-9,10-anthraquinone (QH) having the molecular formula CuQ2 was prepared and characterized by elemental analysis, NMR, FTIR, UV-vis and mass spectroscopy. The powder diffraction of the solid complex, magnetic susceptibility and ESR spectra were also recorded. The presence of the planar anthraquinone moiety in the complex makes it extremely difficult to obtain a single crystal suitable for X-ray diffraction studies. To overcome this problem, density functional theory (DFT) was used to evaluate an optimized structure of CuQ2. In the optimized structure, it was found that there is a tilt of the two planar aromatic anthraquinone rings of the complex with respect to each other in the two planes containing the O-Cu(II)-O plane. The present study is an important addition to the understanding of the structural aspects of metal-anthracyclines because there are only a few reports on the actual structures of metal-anthracyclines. The theoretical vibrational spectrum of the complex was assigned with the help of vibrational energy distribution analysis (VEDA) using potential energy distribution (PED) and compared with experimental results. Being important in producing the biochemical action of this class of molecules, the electrochemical behavior of the complex was studied in aqueous and non-aqueous solvents to find certain electrochemical parameters. In aqueous media, reduction involves a kinetic effect during electron transfer at an electrode surface, which was characterized very carefully using cyclic voltammetry. Electrochemical studies showed a significant modification in the electrochemical properties of 1-amino-4-hydroxy-9,10-anthraquinone (QH) when bound to Cu(II) in the complex compared to those observed for free QH. This suggests that the copper complex might be a good choice as a biologically active molecule, which was reflected in the lack of stimulated superoxide generation by the complex.

  3. Creep oceli L360NB za normálních teplot

    Czech Academy of Sciences Publication Activity Database

    Gajdoš, Lubomír; Šperl, Martin; Náprstek, Jiří; Pavelková, M.

    2016-01-01

    Roč. 96, 9/10 (2016), s. 202-211 ISSN 0032-1761 R&D Projects: GA TA ČR(CZ) TE02000162 Institutional support: RVO:68378297 Keywords : L360NB steel * creep deformation * normal temperatures Subject RIV: JL - Materials Fatigue, Friction Mechanics

  4. 9,10-phenanthrenesemiquinone radical complexes of ruthenium(III), osmium(III) and rhodium(III) and redox series.

    Science.gov (United States)

    Biswas, Manas Kumar; Patra, Sarat Chandra; Maity, Amarendra Nath; Ke, Shyue-Chu; Weyhermüller, Thomas; Ghosh, Prasanta

    2013-05-14

    Reactions of 9,10-phenanthrenequinone (PQ) in toluene with [M(II)(PPh3)3X2] at 298 K afford green complexes, trans-[M(PQ)(PPh3)2X2] (M = Ru, X = Cl, 1; M = Os, X = Br, 2) in moderate yields. Reaction of anhydrous RhCl3 with PQ and PPh3 in boiling ethanol affords the dark brown paramagnetic complex, cis-[Rh(PQ)(PPh3)2Cl2] (3) in good yields. Diffusion of iodine solution in n-hexane to the trans-[Os(PQ) (PPh3)2(CO)(Br)] solution in CH2Cl2 generates the crystals of trans-[Os(PQ)(PPh3)2(CO)(Br)](+)I3(-), (4(+))I3(-)), in lower yields. Single crystal X-ray structure determinations of 1·2toluene, 2·CH2Cl2 and 4(+)I3(-), UV-vis/NIR absorption spectra, EPR spectra of 3, electrochemical activities and DFT calculations on 1, 2, trans-[Ru(PQ)(PMe3)2Cl2] (1Me), trans-[Os(PQ)(PMe3)2Br2] (2Me), cis-[Rh(PQ)(PMe3)2Cl2] (3Me) and their oxidized and reduced analogues including trans-[Os(PQ)(PMe3)2(CO)(Br)](+) (4Me(+)) substantiated that 1-3 are the 9,10-phenanthrenesemiquinone radical (PQ(˙-)) complexes of ruthenium(III), osmium(III) and rhodium(III) and are defined as trans/cis-[M(III)(PQ(˙-))(PPh3)2X2] with a minor contribution of the resonance form trans/cis-[M(II)(PQ)(PPh3)2X2]. Two comparatively longer C-O (1.286(4) Å) and the shorter C-C lengths (1.415(7) Å) of the OO-chelate of 1·2toluene and 2·CH2Cl2 and the isotropic fluid solution EPR signal at g = 1.999 of 3 are consistent with the existence of the reduced PQ(˙-) ligand in 1-3 complexes. Anisotropic EPR spectra of the frozen glasses (g11 = g22 = 2.0046 and g33 = 1.9874) and solids (g11 = g22 = 2.005 and g33 = 1.987) instigate the contribution of the resonance form, cis-[Rh(II)(PQ)(PPh3)2Cl2] in 3. DFT calculations established that the closed shell singlet (CSS) solutions of 1Me and 2Me are unstable due to open shell singlet (OSS) perturbation. However, the broken symmetry (BS) (1,1) Ms = 0 solutions of 1Me and 2Me are respectively 22.6 and 24.2 kJ mole(-1) lower in energy and reproduced the experimental bond

  5. 20 W continuous-wave cladding-pumped Nd-doped fiber laser at 910 nm.

    Science.gov (United States)

    Laroche, M; Cadier, B; Gilles, H; Girard, S; Lablonde, L; Robin, T

    2013-08-15

    We demonstrate a double-clad fiber laser operating at 910 nm with a record power of 20 W. Laser emission on the three-level scheme is enabled by the combination of a small inner cladding-to-core diameter ratio and a high brightness pump source at 808 nm. A laser conversion efficiency as high as 44% was achieved in CW operating regime by using resonant fiber Bragg reflectors at 910 nm that prevent the lasing at the 1060 nm competing wavelength. Furthermore, in a master oscillator power-amplifier scheme, an amplified power of 14.8 W was achieved at 914 nm in the same fiber.

  6. Self-protective powder wire for semiautomatic welding of corrosion resistant chromium-nickel type 18-10 steels

    International Nuclear Information System (INIS)

    Lipodaev, V.N.; Kakhovskij, N.I.; Fadeeva, G.V.

    1977-01-01

    Self-protecting NP-ANV1 powder wire has been developed for welding 18-10 type stainless steels. The use of the wire provides for the same running properties of the welds as the TsL-11 electrodes, the welding being 3-5 times more efficient

  7. Influence of ion implanted helium on deuterium trapping in Kh18N10T stainless steel

    International Nuclear Information System (INIS)

    Tolstolutskaya, G.D.; Ruzhitskij, V.V.; Kopanets, I.E.

    2004-01-01

    The results are presented on evolution of distribution profiles and helium and deuterium thermal desorption ion implanted in steel 18Cr10NiTi. Accumulation, trapping, retention and microstructure evolution are studied; effect helium and hydrogen simultaneous implantation on these processes is also studied

  8. The unbound isotopes {sup 9,10}He

    Energy Technology Data Exchange (ETDEWEB)

    Johansson, H.T. [Fundamental Fysik, Chalmers Tekniska Hoegskola, S-412 96 Goeteborg (Sweden); Aksyutina, Yu. [Fundamental Fysik, Chalmers Tekniska Hoegskola, S-412 96 Goeteborg (Sweden); GSI Helmholtzzentrum fuer Schwerionenforschung GmbH, D-64291 Darmstadt (Germany); Aumann, T.; Boretzky, K. [GSI Helmholtzzentrum fuer Schwerionenforschung GmbH, D-64291 Darmstadt (Germany); Borge, M.J.G. [Instituto Estructura de la Materia, CSIC, E-28006 Madrid (Spain); Chatillon, A. [GSI Helmholtzzentrum fuer Schwerionenforschung GmbH, D-64291 Darmstadt (Germany); Chulkov, L.V. [GSI Helmholtzzentrum fuer Schwerionenforschung GmbH, D-64291 Darmstadt (Germany); Kurchatov Institute, RU-123182 Moscow (Russian Federation); Cortina-Gil, D. [GSI Helmholtzzentrum fuer Schwerionenforschung GmbH, D-64291 Darmstadt (Germany); University of Santiago de Compostela, 15706 Santiago de Compostela (Spain); Datta Pramanik, U. [Saha Institute of Nuclear Physics, 1/AF Bidhannagar, Kolkata 700064 (India); Emling, H. [GSI Helmholtzzentrum fuer Schwerionenforschung GmbH, D-64291 Darmstadt (Germany); Forssen, C. [Fundamental Fysik, Chalmers Tekniska Hoegskola, S-412 96 Goeteborg (Sweden); Fynbo, H.O.U. [Department of Physics and Astronomy, University of Aarhus, DK-8000 Aarhus C (Denmark); Geissel, H.; Ickert, G. [GSI Helmholtzzentrum fuer Schwerionenforschung GmbH, D-64291 Darmstadt (Germany); Jonson, B., E-mail: Bjorn.Jonson@chalmers.s [Fundamental Fysik, Chalmers Tekniska Hoegskola, S-412 96 Goeteborg (Sweden); Physics Department, CERN, CH-1211 Geneve 23 (Switzerland); Kulessa, R. [Instytut Fizyki, Universytet Jagiellonski, PL-30-059 Krakow (Poland); Langer, C. [GSI Helmholtzzentrum fuer Schwerionenforschung GmbH, D-64291 Darmstadt (Germany); Lantz, M. [Fundamental Fysik, Chalmers Tekniska Hoegskola, S-412 96 Goeteborg (Sweden); LeBleis, T.; Mahata, K. [GSI Helmholtzzentrum fuer Schwerionenforschung GmbH, D-64291 Darmstadt (Germany)

    2010-10-15

    The unbound nuclei {sup 9}He and {sup 10}He have been produced in proton-knockout reactions from a 280 MeV/u {sup 11}Li beam impinging on a liquid hydrogen target at the ALADIN-LAND setup at GSI. Information on their nuclear structure has been obtained from the relative-energy spectra, {sup 8}He+n and {sup 8}He+2n, employing reaction models incorporating the structure of {sup 11}Li. The {sup 8}He+n relative-energy spectrum is dominated by a strong peak-like structure at low energy, which may be interpreted within the effective-range approximation as the result of an s-wave interaction with a neutron scattering length of -3.17(66) fm. This spectrum also shows evidence for resonance states at 1.33(8) MeV and at 2.4 MeV above the {sup 8}He+n threshold. It is argued that the s-state might not be the {sup 9}He ground state. For {sup 8}He+n+n, the analysis of the relative-energy spectrum gives two alternative possibilities for an interpretation: either a narrow resonance at 1.42(10) MeV ({Gamma}=1.11(76) MeV) superimposed on a correlated background, or two overlapping resonances, a ground state at 1.54(11) MeV ({Gamma}=1.91(41) MeV) together with an excited state at 3.99(26) MeV ({Gamma}=1.64(89) MeV). The two possible interpretations are discussed.

  9. Metallographical procedure for detecting carburized layer in the 12Kh18N10T steel tubes

    International Nuclear Information System (INIS)

    Najmark, S.I.; Shmalenyuk, R.P.

    1977-01-01

    The various causes of the tendency to intercrystalline corrosion of stainless steel tubing were studied. 12Kh18N10T steel tube specimens were metallographically investigated to reveal the presence and depth of the carburized layer. Unlubricated specimens and specimens with the graphite-saltpeter lubrication applied on them were austenized in the temperature range from 950 to 1250 deg C and then exposed to a provoking anneal at 650 deg C for 24 h. All the lubricated specimens showed a carbide network along grain boundaries and intercrystalline cracks. The specimens treated without lubrication had no cracks. The method offered can differentiate poor tube cleaning and the undesirable effect of other processing steps on the tubes

  10. On the protective effect of KhOSP-10 inhibitor during corrosion, hydrogenadsorption and corrosion cracking of a steel in sulfuric acid

    International Nuclear Information System (INIS)

    Mindyuk, A.K.; Svist, E.I.; Savitskaya, O.P.; Goyan, E.B.; Gopanenko, A.N.

    1975-01-01

    The protective propeties of inhibitor KhOSP-10 in the time of corrosion and corrosive cracking of steel 40Kh are higher then those of inhibitors KPI-1, KI-1, I-I-V etc. Its ability to reduce steel hydrogenation is the same as in the case of KPI-1 inhibitor i.e. below that of KI-1. HCl additives enhance the efficiency of inhibitors KPI-1, KI-1, I-1-V etc. up to the protective ability of KhOSP-10. Kinetics of the electrode processes was estimated from polarization curves

  11. Determination of susceptibility to intergranular corrosion of stainless steels type X5CrNi18-10 in field

    Directory of Open Access Journals (Sweden)

    Bore V. Jegdic

    2016-12-01

    Full Text Available In this paper, the DL EPR method (electrochemical potentiokinetic reactivation with double loop was modified and used to study the susceptibility to intergranular corrosion and stress corrosion cracking of a stainless steel type X5CrNi18-10. The tests were performed in a special electrochemical cell, with the electrolyte in the gel form. Modified DL EPR method is characterized by simple and high accuracy measurements as well as repeatability of the test results. The indicator of susceptibility to intergranular corrosion (Qr/QpGBA obtained by modified DL EPR method is in a very good agreement with the same indicator obtained by standard DL EPR method. The modified DL EPR method is quantitative and highly selective method. Small differences in the susceptibility of the stainless steel type CrNi18-10 to intergranular corrosion and stress corrosion cracking can be determined. Test results can be obtained in a short time. The cost of tests performed by modified DL EPR method is much lower than the cost of tests by conventional chemical methods. Modified DL EPR method can be applied in the field on the stainless steels constructions.

  12. Anti-factor IXa/X bispecific antibody ACE910 prevents joint bleeds in a long-term primate model of acquired hemophilia A

    Science.gov (United States)

    Yoshihashi, Kazutaka; Takeda, Minako; Kitazawa, Takehisa; Soeda, Tetsuhiro; Igawa, Tomoyuki; Sampei, Zenjiro; Kuramochi, Taichi; Sakamoto, Akihisa; Haraya, Kenta; Adachi, Kenji; Kawabe, Yoshiki; Nogami, Keiji; Shima, Midori; Hattori, Kunihiro

    2014-01-01

    ACE910 is a humanized anti-factor IXa/X bispecific antibody mimicking the function of factor VIII (FVIII). We previously demonstrated in nonhuman primates that a single IV dose of ACE910 exerted hemostatic activity against hemophilic bleeds artificially induced in muscles and subcutis, and that a subcutaneous (SC) dose of ACE910 showed a 3-week half-life and nearly 100% bioavailability, offering support for effective prophylaxis for hemophilia A by user-friendly SC dosing. However, there was no direct evidence that such SC dosing of ACE910 would prevent spontaneous bleeds occurring in daily life. In this study, we newly established a long-term primate model of acquired hemophilia A by multiple IV injections of an anti-primate FVIII neutralizing antibody engineered in mouse-monkey chimeric form to reduce its antigenicity. The monkeys in the control group exhibited various spontaneous bleeding symptoms as well as continuous prolongation of activated partial thromboplastin time; notably, all exhibited joint bleeds, which are a hallmark of hemophilia. Weekly SC doses of ACE910 (initial 3.97 mg/kg followed by 1 mg/kg) significantly prevented these bleeding symptoms; notably, no joint bleeding symptoms were observed. ACE910 is expected to prevent spontaneous bleeds and joint damage in hemophilia A patients even with weekly SC dosing, although appropriate clinical investigation is required. PMID:25274508

  13. The effects of adding molybdenum and niobium on the creep strength of 18Cr-10Ni-20Co austenitic steel

    International Nuclear Information System (INIS)

    Tomono, Yutaka

    1987-01-01

    The decrease in the creep strength of structural materials during service at elevated temperatures is a very important problem that affects the security of plants and machinery. The improvement in the creep strength of 18Cr-10Ni-20Co austenitic steel achieved through the addition of molybdenum and niobium was studied in tests carried out at 973K and 1,073K. The creep strengthening mechanism was examined using transmission electron micrographs, X-ray diffraction, etc. The results obtained are summarized as follows: (1) The creep strength of low C-18Cr-10Ni-20Co austenitic steel with molybdenum was greatly improved by the addition of niobium up to 1% by weight. In the case of long-term creep, no trend toward decreasing creep strength was observed. (2) The creep strength of austenitic steel possessing a matrix strengthened with molybdenum can be improved through the addition of niobium combined with precipitation hardening with fine carbides precipitated in the grains. (author)

  14. Selected Lectures of the 2nd International Workshop “Intensive Care of the Newborn”; Verona (Italy; March 9-10, 2018

    Directory of Open Access Journals (Sweden)

    --- Various Authors

    2018-03-01

    Full Text Available Selected Lectures of the 2nd International Workshop “Intensive Care of the Newborn”; Verona (Italy; March 9-10, 2018 CONGRESS PRESIDENT Paolo Biban  Guest Editor: Paolo BibanLECT 1. RESUSCITATION OF EXTREMELY PREMATURE INFANTS: HOW TO IMPROVE EVEN FURTHER • J.M. PerlmanLECT 2. MAINTAINING NORMAL TEMPERATURE IN THE NEWLY BORN: NOT A TRIVIAL GAME • J. WyllieLECT 3. PRESENT AND FUTURE OF SURFACTANT AD­MINISTRATION IN PRETERM INFANTS WITH RESPIRATORY DISTRESS SYNDROME (RDS • A. KribsLECT 4. CONTINUOUS POSITIVE AIRWAY PRES­SURE (CPAP, SURFACTANT, OR BOTH? A DILEMMA STILL WAITING TO BE SOLVED • D. De LucaLECT 5. NON-INVASIVE RESPIRATORY SUPPORT AND RESPIRATORY DISTRESS SYNDROME (RDS: IS NASAL CONTINUOUS POSITIVE AIRWAY PRESSURE (nCPAP ALWAYS ENOUGH? • G. Lista, I. BresestiLECT 6. NEURALLY ADJUSTED VENTILATORY ASSIST (NAVA IN THE NEWBORN: A NEW STANDARD OF CARE? • H. SteinLECT 7. HIGH-FREQUENCY, MULTI-FREQUENCY OSCIL­LA­TION, JET VENTILATION: WHERE ARE WE? • J.J. PillowLECT 8. SURVIVAL AND NEURODEVELOPMENTAL OUT­COME IN PERIVIABLE INFANTS • N. YoungeLECT 9. PATHOPHYSIOLOGY AND TREATMENT OF SEPTIC SHOCK IN NEONATES • H.R. WongLECT 10. CLINICAL METABOLOMICS IN NEONATAL SEPSIS • V. FanosLECT 11. OPTIMIZING EARLY NUTRITION SUPPORT IN VERY LOW BIRTH WEIGHT (VLBW INFANTS • T. SenterreLECT 12. LONG-TERM ADVERSE EFFECTS OF EARLY GROWTH ACCELERATION OR CATCH-UP GROWTH • A. SinghalLECT 13. ROLE OF NEAR INFRARED SPECTROSCOPY DURING NEONATAL TRANSITION • B. UrlesbergerLECT 14. HEART RATE CHARACTERISTICS AS PHYSIO­MARKERS FOR DETECTION OF SEPSIS AND OTHER DISEASES • K.D. FairchildLECT 15. ENHANCED CARDIORESPIRATORY MONI­TORING OF THE PRETERM INFANT DURING STABILIZA­TION IN THE DELIVERY ROOM • E. Dempsey

  15. Serum Level of Antibody against Benzo[a]pyrene-7,8-diol-9,10-epoxide-DNA Adducts in People Dermally Exposed to PAHs

    Directory of Open Access Journals (Sweden)

    Lenka Borska

    2014-01-01

    Full Text Available Some specific antibodies indicate the presence of antigenic structures on DNA (DNA adducts that can play an important role in the process of mutagenesis and/or carcinogenesis. They indicate the presence of increased genotoxic potential (hazard prior to the formation of disease (primary prevention. The present study was focused on the serum level of benzo[a]pyrene 7,8-diol-9,10-epoxide-DNA adducts antibodies (anti-BPDE-DNA in psoriatic patients (n=55 dermally exposed to different levels of polycyclic aromatic hydrocarbons (PAHs. The general goal of the study was to contribute to better understanding of the value of the assumed biomarker (anti-BPDE-DNA for evaluation of the organism's answer to genotoxic exposure to PAHs. Elevated level of exposure to PAHs resulted in the increased level of anti-BPDE-DNA. However, almost all levels of anti-BPDE-DNA ranged within the field of low values. Both variants of GT (CCT-3% and CCT-5% induced higher expression of anti-BPDE-DNA in the group of nonsmokers. Significant relations between the level of anti-BPDE-DNA and PASI score, total duration of the therapy, or time of UVR exposure were not found. Further studies are needed to reduce interpretation uncertainty of this promising bioindicator.

  16. Ground and excited state behavior of 1,4-dimethoxy-3-methyl-anthracene-9,10-dione in silver nanoparticles: Spectral and computational investigations

    Energy Technology Data Exchange (ETDEWEB)

    Umadevi, M., E-mail: ums10@yahoo.com [Department of Physics, Mother Teresa Women' s University, Kodaikanal 624101, Tamil Nadu (India); Kavitha, S.R. [Department of Physics, Mother Teresa Women' s University, Kodaikanal 624101, Tamil Nadu (India); Vanelle, P.; Terme, T.; Khoumeri, O. [Laboratoire de Pharmaco-Chimie Radicalaire, Faculté de Pharmacie, Aix-Marseille Univ, CNRS, Institut de Chimie Radicalaire ICR, UMR 7273, 27 Boulevard Jean Moulin, 13385 Marseille Cedex 05 (France)

    2013-10-15

    Silver nanoparticles (Ag NPs) of various sizes have been successfully synthesized by the simple and convenient Creighton method using sodium borohydride as the reducing agent under microwave irradiation. Optical absorption and fluorescence emission spectroscopic techniques were employed to investigate the effect of silver nanoparticles on the ground and excited state of 1,4-dimethoxy-3-methylanthracene-9,10-dione (DMMAD). The surface plasmon resonance (SPR) peak of the prepared silver colloidal solution was observed at 400 nm. Fluorescence quenching of DMMAD by silver nanoparticles has been found to increase with increase in the size of Ag. The fluorescence quenching has been explained by Forster Resonance Energy Transfer (FRET) theory between DMMAD and silver nanoparticles. The Stern–Volmer quenching constant and Benesi–Hildebrand association constant for the above system were calculated. DFT calculations were also performed to study the charge distribution of DMMAD in Ag both in ground and excited states. -- Highlights: • Silver nanoparticles (Ag NPs) have been synthesized using the Creighton method. • Effect of Ag NPs on the ground state of DMMAD was studied. • Influence of Ag NPs on the excited state of DMMAD was investigated. • Fluorescence quenching has been explained by Forster Resonance Energy Transfer. • Quenching and binding constants were also calculated.

  17. N,N′-Diphenyl-9,10-dioxo-9,10-dihydroanthracene-2,7-disulfonamide

    Directory of Open Access Journals (Sweden)

    Wei-Guan Yuan

    2013-07-01

    Full Text Available The title molecule, C26H18N2O6S2, has an overall Z-shaped conformation, in which the benzene rings are inclined to the anthraquinone mean plane by 60.60 (9 and 50.66 (13°. In the crystal, N—H...O and C—H...O hydrogen bonds link the molecules into layers parallel to the bc plane.

  18. 44 CFR 9.10 - Identify impacts of proposed actions.

    Science.gov (United States)

    2010-10-01

    ... 44 Emergency Management and Assistance 1 2010-10-01 2010-10-01 false Identify impacts of proposed... impacts of proposed actions. (a) Purpose. The purpose of this section is to ensure that the effects of... adverse impacts associated with the occupancy and modification of floodplains and wetlands and the...

  19. Investigations on the ratchetting behaviour of austenitic pipes

    International Nuclear Information System (INIS)

    Kraemer, D.; Krolop, S.; Scheffold, A.; Stegmeyer, R.

    1994-01-01

    Reversed bending tests at room temperature with pipes with and without internal pressure were carried out. The pipes were manufactured from the austenitic steel X10 CrNiNb 18 9. Under internal pressure ratchetting was observed in circumferential direction. The component tests were accompanied by numerical computations using a nonlinear kinematic hardening rule and superposed isotropic hardening. In total the constitutive model needed 13 parameters to be fitted when isotropic hardening resulted in a cyclic saturation. Uniaxial monotonic and cyclic loading tests served for characterizing the material. A reasonable parameter fitting with respect to describe ratchetting required load controlled nonzero mean-stress tests. On condition, that the loading will lead to cyclic saturation, ratchetting could be well predicted in the pipe with the found set of parameters. An extension of the isotropic hardening rule in the constitutive model was proposed allowing to describe various types of isotropic hardening. In a first step it was shown that under uniaxial conditions the extension reproduces continuous isotropic hardening up to incipient cracking quite well. (orig.)

  20. Effects of Intercritical Annealing Temperature on Mechanical Properties of Fe-7.9Mn-0.14Si-0.05Al-0.07C Steel

    Directory of Open Access Journals (Sweden)

    Xianming Zhao

    2014-12-01

    Full Text Available A medium Mn steel has been designed to achieve an excellent combination of strength and ductility based on the TRIP (Transformation Induced Plasticity concept for automotive applications. Following six passes of hot rolling at 850 °C, the Fe-7.9Mn-0.14Si-0.05Al-0.07C (wt.% steel was warm-rolled at 630 °C for seven passes and subsequently air cooled to room temperature. The sample was subsequently intercritically annealed at various temperatures for 30 min to promote the reverse transformation of martensite into austenite. The obtained results show that the highest volume fraction of austenite is 39% for the sample annealed at 600 °C. This specimen exhibits a yield stress of 910 MPa and a high ultimate tensile stress of 1600 MPa, with an elongation-to-failure of 0.29 at a strain rate of 1 × 10−3/s. The enhanced work-hardening ability of the investigated steel is closely related to martensitic transformation and the interaction of dislocations. Especially, the alternate arrangement of acicular ferrite (soft phase and ultrafine austenite lamellae (50–200 nm, strong and ductile phase is the key factor contributing to the excellent combination of strength and ductility. On the other hand, the as-warm-rolled sample also exhibits the excellent combination of strength and ductility, with elongation-to-failure much higher than those annealed at temperatures above 630 °C.

  1. Effects of Intercritical Annealing Temperature on Mechanical Properties of Fe-7.9Mn-0.14Si-0.05Al-0.07C Steel.

    Science.gov (United States)

    Zhao, Xianming; Shen, Yongfeng; Qiu, Lina; Liu, Yandong; Sun, Xin; Zuo, Liang

    2014-12-09

    A medium Mn steel has been designed to achieve an excellent combination of strength and ductility based on the TRIP (Transformation Induced Plasticity) concept for automotive applications. Following six passes of hot rolling at 850 °C, the Fe-7.9Mn-0.14Si-0.05Al-0.07C (wt.%) steel was warm-rolled at 630 °C for seven passes and subsequently air cooled to room temperature. The sample was subsequently intercritically annealed at various temperatures for 30 min to promote the reverse transformation of martensite into austenite. The obtained results show that the highest volume fraction of austenite is 39% for the sample annealed at 600 °C. This specimen exhibits a yield stress of 910 MPa and a high ultimate tensile stress of 1600 MPa, with an elongation-to-failure of 0.29 at a strain rate of 1 × 10 -3 /s. The enhanced work-hardening ability of the investigated steel is closely related to martensitic transformation and the interaction of dislocations. Especially, the alternate arrangement of acicular ferrite (soft phase) and ultrafine austenite lamellae (50-200 nm, strong and ductile phase) is the key factor contributing to the excellent combination of strength and ductility. On the other hand, the as-warm-rolled sample also exhibits the excellent combination of strength and ductility, with elongation-to-failure much higher than those annealed at temperatures above 630 °C.

  2. 12 CFR 609.910 - Compliance with the Electronic Signatures in Global and National Commerce Act (Public Law 106-229...

    Science.gov (United States)

    2010-01-01

    ... Global and National Commerce Act (Public Law 106-229) (E-SIGN). 609.910 Section 609.910 Banks and Banking... with the Electronic Signatures in Global and National Commerce Act (Public Law 106-229) (E-SIGN). (a) General. E-SIGN makes it easier to conduct E-commerce. With some exceptions, E-SIGN permits the use and...

  3. Effect of load ratio and saltwater corrosive environment on the initiation life of fatigue of 10Ni5CrMoV steel

    Science.gov (United States)

    Xie, Xing; Yi, Hong; Xu, Jian; Gen, Liming; Chen, Luyun

    2017-09-01

    Fatigue initiation life has been studied with 10CrNi5MoV steel for use in ocean engineering at different load ratios and in different environmental media. The microstructure and micro-topography have been observed and analyzed by means of SEM, EDS and EBSD. Our findings indicate that, the initiation life of 10Ni5CrMoV steel in seawater is shorter than that in air, and the difference in longevity is larger with the increasing of load ratio. Corrosion pits had a great influence on initial corrosion fatigue life.

  4. Atom-Probe Tomographic Investigations of a Precipitation-Strengthened HSLA-115 Steel and a Ballistic-Resistant 10 wt. % Ni Steel for Naval Applications

    Science.gov (United States)

    Jain, Divya

    High performance structural materials are needed for Naval applications which require an excellent combination of yield strength, low-temperature impact toughness, ductility, ballistic-resistance, and weldability. This research investigates precipitation-strengthened HSLA-115 steels and ballistic-resistant 10 wt. % Ni steels, which have emerged as promising alternatives to the widely used HSLA-100 steels for Naval applications. HSLA-115 is a Cu-bearing high-strength low-carbon martensitic steel and has been used in the flight deck of the recently built U.S. Navy CVN-78 aircraft carrier. It is typically used in conditions with overaged Cu precipitates, to obtain acceptable impact toughness and ductility at 115 ksi (793 MPa) yield strength. However, overaging of Cu precipitates limits its strength and applications. This research demonstrates that aging at 550 °C facilitates the co-precipitation of sub-nanometer sized M2C carbides and Cu precipitates in high number density (˜1023 m-3) in HSLA-115. 3-D atom-probe tomography (APT) investigation reveals that Cu precipitates form first, followed by the nucleation of M2C carbides, which are co-located with Cu precipitates and are distributed heterogeneously at lath-boundaries and dislocations, indicating heterogeneous nucleation of M2C. Carbon redistribution during quenching (following the austenitization) and subsequent aging at 550 °C is followed using APT. Segregation of C (3-6 at. % C) is observed at martensitic lath-boundaries in the as-quenched and 0.12 h aged conditions. On further aging, C redistributes, forming cementite and M 2C carbides, whose composition and morphology evolves with aging time. Precipitation kinetics of M2C carbides is intertwined with Cu precipitates; temporal evolution of Cu precipitates and M2C carbides is characterized in terms of their mean radii, number densities, and volume fractions and correlated with the bulk mechanical properties. Precipitation of M2C carbides offsets the softening

  5. Electrochemical Corrosion Behavior of Carbon Steel and Hot Dip Galvanized Steel in Simulated Concrete Solution with Different pH Values

    Directory of Open Access Journals (Sweden)

    Wanchen XIE

    2017-08-01

    Full Text Available Hot dip galvanizing technology is now widely used as a method of protection for steel rebars. The corrosion behaviors of Q235 carbon steel and hot galvanized steel in a Ca(OH2 solution with a pH from 10 to 13 was investigated by electrode potential and polarization curves testing. The results indicated that carbon steel and hot galvanized steel were all passivated in a strong alkaline solution. The electrode potential of hot dip galvanized steel was lower than that of carbon steel; thus, hot dip galvanized steel can provide very good anodic protection for carbon steel. However, when the pH value reached 12.5, a polarity reversal occurred under the condition of a certain potential. Hot dip galvanized coating became a cathode, and the corrosion of carbon steel accelerated. The electrochemical behaviors and passivation abilities of hot dip galvanized steel and carbon steel were affected by pH. The higher the pH value was, the more easily they were passivated.DOI: http://dx.doi.org/10.5755/j01.ms.23.3.16675

  6. Iptycene synthesis: A new method for attaching a 2,3-anthracene moiety to the 9,10-positions of another anthracene moiety - Exceptional conditions for a Lewis acid catalyzed Diels-Alder reaction

    Science.gov (United States)

    Chen, Yong-Shing; Hart, Harold

    1989-01-01

    An efficient three-step method for appending a 2,3-anthracene moiety to the 9,10-positions of an existing anthracene moiety is described. The first step uses excess 1,4-anthraquinone (3 equiv) and aluminum chloride (6 equiv) to obtain the anthracene-quinone cycloadduct (omission of the AlCl3 resulted in no adduct). The resulting diketone was reduced to the corresponding diol (excess LiAlH4), which was dehydrated to the arene with phosphorus oxychloride and pyridine. Specific examples include the preparation of heptipycene 8 from pentiptycene 6 (66 percent overall yield) and a similar conversion of 8 to the noniptycene 13 (75 percent overall yield). The methodology led to a markedly improved synthesis of tritriptycene 9 and the first synthesis of undecaiptycene 14.

  7. Pulse radiolysis of 9,10-anthraquinone in methanol

    International Nuclear Information System (INIS)

    Mayer, J.; Krasiukianis, R.

    1990-01-01

    The reactions of anthraquinone with intermediates in methanol (e 2 - , . CH 2 O - , . CH 2 OH) were investigated using γ-radiolysis and pulse radiolysis method. The anthraquinone radical anions are reactive towards O 2 (ca 3 x 10 8 mol -1 dm 3 s -1 ) and can disproportionate giving corresponding dianion. (author)

  8. Mechanical properties of Fe -10Ni -7Mn martensitic steel subjected to severe plastic deformation via cold rolling and wire drawing

    Energy Technology Data Exchange (ETDEWEB)

    Ghasemi-Nanesa, H; Shirazi, H [School of Metallurgy and Materials Engineering, Faculty of Engineering, University of Tehran, P.O. Box 14395-731 (Iran, Islamic Republic of); Nili-Ahmadabadi, M, E-mail: sut.caster.81710018@gmail.co, E-mail: nili@ut.ac.i [School of Metallurgy and Materials Engineering, Faculty of Engineering, University of Tehran, P.O. Box 14395-731 (Iran, Islamic Republic of) and Center of Excellence for High Performance Materials, University of Tehran, P.O. Box 14395-731, Tehran (Iran, Islamic Republic of)

    2010-07-01

    Fe-Ni-Mn martensitic steels are one of the major groups of ultra-high strength steels that have good mechanical properties and ductility in as annealed condition but they suffer from severe inter-granular embitterment after aging. In this paper, the effect of heavy shaped cold rolling and wire drawing on the mechanical properties of Fe-Ni-Mn steel was investigated. This process could provide a large strain deformation in this alloy. The total strain was {epsilon} {approx}7. Aging behavior and tensile properties of Fe-10Ni-7Mn were studied after aging at 753 K. The results showed that the ultimate tensile strength and ductility after cold rolling, wire drawing and aging increased up to 2540 MPa and 7.1 %, respectively, while the conventional steels show a premature fracture stress of 830 MPa with about zero ductility after aging.

  9. Mechanical properties of Fe -10Ni -7Mn martensitic steel subjected to severe plastic deformation via cold rolling and wire drawing

    Science.gov (United States)

    Ghasemi-Nanesa, H.; Nili-Ahmadabadi, M.; Shirazi, H.

    2010-07-01

    Fe-Ni-Mn martensitic steels are one of the major groups of ultra-high strength steels that have good mechanical properties and ductility in as annealed condition but they suffer from severe inter-granular embitterment after aging. In this paper, the effect of heavy shaped cold rolling and wire drawing on the mechanical properties of Fe-Ni-Mn steel was investigated. This process could provide a large strain deformation in this alloy. The total strain was epsilon ~7. Aging behavior and tensile properties of Fe-10Ni-7Mn were studied after aging at 753 K. The results showed that the ultimate tensile strength and ductility after cold rolling, wire drawing and aging increased up to 2540 MPa and 7.1 %, respectively, while the conventional steels show a premature fracture stress of 830 MPa with about zero ductility after aging.

  10. Effect of cold deformation on latent energy value and high-temperature mechanical properties of 12Cr18Ni10Ti steel

    International Nuclear Information System (INIS)

    Maksimkin, O.P.; Shiganakov, Sh.B.; Gusev, M.N.

    1997-01-01

    Energetic and magnetic characteristics and also the high-temperature mechanical properties depending on the preliminary cold deformation of 12Cr18Ni10Ti steel are presented. It is shown that the value of storage energy in the steel has being grown with increase of the deformation. The rate of its growth has been increased after beginning of martensitic γ→α'- transformation when value of comparative storage energy at first decreased and then has been stay practically constant. Level of mechanical properties of the steel at 1073 K has been determined not only by value of cold deformation but and structural reconstruction corresponding to deformations 35-45% and accompanying with α'-phase martensite formation and change of energy accumulating rate. Preliminary cold deformation (40-60 %) does not improve high- temperature plasticity of steel samples implanted by helium. refs. 7, figs. 2

  11. Creep performance of welded pipe material made of 7CrMoVTiB10-10 (T/P24) steel

    Energy Technology Data Exchange (ETDEWEB)

    Rantala, Juhani; Auerkari, Pertti; Salonen, Jorma; Holmstroem, Stefan; Nevasmaa, Pekka [VTT Technical Research Centre of Finland, Espoo (Finland); Haekkilae, Juha [Foster Wheeler Energia, Varkaus (Finland)

    2010-07-01

    The creep strength of welded low-alloy ferritic steels is typically somewhat lower than that for parent metal, but this is generally due to an inherent weakness of the heat affected zone and accounted for in the common design codes. However, the parent material strength is much higher in certain modern low alloy steels such as 7CrMoVTiB10-10 (P24), and then it can be a significant challenge to develop weld metals (welding consumables) to match this strength. Acceptable weld performance has been previously demonstrated for thin-wall tubes where sufficient mixing with the base material can occur. The objective of this work was to achieve satisfactory properties for a thick-wall welded pipe by using an Nb-modified consumable to avoid weld metal weakening due to arc losses of Ti of a consumable composition approximately matching the base material. A considerable improvement was indeed noted in comparison with earlier experience using matching electrode composition. All short term test results for weld qualification showed acceptable properties, the cross-weld creep strength remain very close to the -20% band from the parent metal creep strength. However, creep testing at lowest stress levels approaching those expected in service resulted in weld metal failure. Although a clear improvement is evident from the previous generation of weld metals, there appears to be some further scope of development of the welding consumables, to improve the long term creep ductility of the welded joints particularly when applying production-like welding parameters. (orig.)

  12. 18 CFR 367.9100 - Account 910, Miscellaneous customer service and informational expenses.

    Science.gov (United States)

    2010-04-01

    ..., Miscellaneous customer service and informational expenses. 367.9100 Section 367.9100 Conservation of Power and... Account 910, Miscellaneous customer service and informational expenses. (a) This account must include the cost of labor, materials used and expenses incurred in connection with customer service and...

  13. Serum Level of Antibodies (IgG, IgM Against Benzo[a]pyrene-7,8-diol-9,10-epoxide-DNA Adducts in Children Dermatologically Exposed to Coal Tar

    Directory of Open Access Journals (Sweden)

    Pavel Borský

    2017-06-01

    Full Text Available Crude coal tar (CCT contains polycyclic aromatic hydrocarbons (PAHs. Benzo[a]pyrene (BaP is metabolized into a highly reactive metabolite benzo[a]pyrene-7,8-diol-9,10-epoxide (BPDE that is able to bind to DNA and creates BPDE-DNA adducts. Adducted DNA becomes immunogenic and induces immune response by production of antibodies against BPDE-DNA adducts (Ab-BPDE-DNA. Circulating Ab-BPDE-DNA was proposed as potential biomarker of genotoxic exposure to BaP (PAHs. Goeckerman therapy (GT of psoriasis uses dermal application of CCT ointment (PAHs. In presented study (children with psoriasis treated by GT; n = 19 the therapy significantly increased the level of Ab-BPDE-DNA (EI = 0.29/0.19–0.34 vs. 0.31/0.25–0.40; median/lower–upper quartile; p < 0.01. The results support the idea of Ab-BPDE-DNA level as a possible tentative indicator of exposure, effects and susceptibility of the organism to the exposure of BaP (PAHs.

  14. The steel scrap age.

    Science.gov (United States)

    Pauliuk, Stefan; Milford, Rachel L; Müller, Daniel B; Allwood, Julian M

    2013-04-02

    Steel production accounts for 25% of industrial carbon emissions. Long-term forecasts of steel demand and scrap supply are needed to develop strategies for how the steel industry could respond to industrialization and urbanization in the developing world while simultaneously reducing its environmental impact, and in particular, its carbon footprint. We developed a dynamic stock model to estimate future final demand for steel and the available scrap for 10 world regions. Based on evidence from developed countries, we assumed that per capita in-use stocks will saturate eventually. We determined the response of the entire steel cycle to stock saturation, in particular the future split between primary and secondary steel production. During the 21st century, steel demand may peak in the developed world, China, the Middle East, Latin America, and India. As China completes its industrialization, global primary steel production may peak between 2020 and 2030 and decline thereafter. We developed a capacity model to show how extensive trade of finished steel could prolong the lifetime of the Chinese steelmaking assets. Secondary steel production will more than double by 2050, and it may surpass primary production between 2050 and 2060: the late 21st century can become the steel scrap age.

  15. Investigation into the Cyclic Strength of the Bodies of Steam Shutoff Valves from 10Kh9MFB-Sh Steel

    Science.gov (United States)

    Skorobogatykh, V. N.; Kunavin, S. A.; Prudnikov, D. A.; Shchenkova, I. A.; Bazhenov, A. M.; Zadoinyi, V. A.; Starkovskii, G. L.

    2018-02-01

    Steam shutoff valves are operated under complex loading conditions at thermal and nuclear power stations. In addition to exposure to high temperature and stresses resulting in fatigue, these valves are subjected to cyclic loads in heating-up-cooling down, opening-closing, etc. cycles. The number of these cycles to be specified in designing the valves should not exceed the maximum allowable value. Hence, the problem of cyclic failure rate of steam shutoff valve bodies is critical. This paper continues the previous publications about properties of the construction material for steam shutoff valve bodies (grade 10Kh9MFB-Sh steel) produced by electroslag melting and gives the results of investigation into the cyclic strength of this material. Fatigue curves for the steal used for manufacturing steam shutoff valve bodies are presented. The experimental data are compared with the calculated fatigue curves plotted using the procedures outlined in PNAE G-002-986 and RD 10-249-98. It is confirmed that these procedures may be used in designing valve bodies from 10Kh9MFB-Sh steel. The effect of the cyclic damage after preliminary cyclic loading of the specimens according to the prescribed load conditions on the high-temperature strength of the steel is examined. The influence of cyclic failure rate on the long-term strength was investigated using cylindrical specimens with a smooth working section in the as-made conditions and after two regimes of preliminary cyclic loading (training) at a working temperature of 570°C and the number of load cycles exceeding the design value, which was 2 × 103 cycles. The experiments corroborated that the material (10Kh9MFB-Sh steel) of the body manufactured by the method of electroslag melting had high resistance to cyclic failure rate. No effect of cyclic damages in the metal of the investigated specimens on the high-temperature strength has been found.

  16. Verwendung von Polypropylen/Polyglactin 910- (PP910- und Polypropylen/Polyglecapron 25 (PP25- Netzen bei Beckenbodenprolaps - eine retrospektive Analyse

    Directory of Open Access Journals (Sweden)

    Schwegler Ch

    2009-01-01

    Full Text Available Die Entwicklung von Polypropylen- Implantaten zur Behandlung von Bauchwandhernien stellt einen Meilenstein in der Geschichte der Chirurgie dar. Mit einigen Jahren Verzug folgten die Urogynäkologen den Chirurgen und begannen, Polypropylen-Netze zur Behebung von Beckenbodenvorfällen einzusetzen. PP910-Netze (Vypro II®, Ethicon und PP25-Netze (Ultrapro®, Ethicon werden seit Langem mit gutem Erfolg bei Hernien-Operationen eingesetzt. Das Ziel dieser Studie war herauszufinden, inwieweit sich diese beiden Netze auch für den Einsatz beim Beckenbodenprolaps eignen. Hierzu wurden Fragebögen an Patientinnen versandt, denen in den Jahren 2003 und 2004 diese Netze im Beckenboden implantiert wurden. Die Hauptfragestellungen waren hierbei, inwiefern sich die Symptome des Vorfalles nach der Behandlung verändert hatten und welche Komplikationen nach der Operation aufgetreten waren. Beide Gruppen zeigten nach dem Netzeinsatz deutliche Verbesserungen der Symptomatik bei einer geringen Komplikationsquote. Beim Einsatz von PP910 zeigten sich in 6 % der Fälle Komplikationen, die auf die Implantation des Netzes zurückgeführt werden konnten. Beim Einsatz von PP25 zeigten sogar nur 1,5 % der operierten Frauen netzbedingte Komplikationen. Somit hat sich gezeigt, dass beide Netze gut für die Verwendung im Beckenboden geeignet sind. Vergleicht man die beiden Netze mit anderen Produkten, die derzeit als Implantate im Beckenboden genutzt werden, so zeigt sich ein sehr positives Ergebnis mit signifikant weniger postoperativen Komplikationen unter der Verwendung von PP25-Netzen. Im Rahmen dieser Analyse konnte festgestellt werden, dass PP25 ein sehr sicheres Netz mit ausgesprochen guten Ergebnissen für die Therapie des Beckenbodenprolaps ist.

  17. Prevention of Internalising Disorders in 9-10 year old children: Efficacy of the Aussie Optimism Positive Thinking Skills Program at 30-month follow-up

    Directory of Open Access Journals (Sweden)

    David eMorrison

    2013-12-01

    Full Text Available The Aussie Optimism: Positive Thinking Skills Program (AOPTP is a school-based prevention program aimed at addressing anxious and depressive symptoms in children aged 9-10 years. Nine-hundred and ten students from 22 Australian primary schools situated in low socio-economic areas were randomly assigned to either an intervention or control group, and assessed at a 30-month follow up. Those in the intervention group received the AOPTP program, where the control group continued to receive the regular health education course. Students completed self-report measures regarding their levels of depression, anxiety, and attribution style. Parents also reported on their children’s externalising and internalising problems outside of school. There were no significant differences between groups in regard to anxiety or depression, as well as no significant differences in attributional styles. Parents reported significantly less hyperactive behaviours from children in the intervention group. This finding suggests that AOP-PTS has the capacity to treat externalising problems at a medium term effect. The decrease in the externalising problems provides evidence of a partial medium term intervention effect. Future studies should continue to evaluate the program at a long term follow up.

  18. Association between diet and physical activity and sedentary behaviours in 9-10-year-old British White children.

    Science.gov (United States)

    Vissers, P A J; Jones, A P; van Sluijs, E M F; Jennings, A; Welch, A; Cassidy, A; Griffin, S J

    2013-03-01

    To examine the association between diet and physical activity and sedentary behaviours in 9-10-year-old children. A cross-sectional study using data from the SPEEDY (Sport, Physical activity and Eating behaviour: Environmental Determinants in Young People) study undertaken in Norfolk, UK. Data from 4-day food diaries and 7 days of accelerometery were matched on concurrent days. Time spent in moderate-to-vigorous physical activity (MVPA), time spent in sedentary behaviour and various measures of dietary intake were collected. Covariates included age, sex, weight status, family socio-economic status, and energy intake reporting quality. Multivariable regression models, adjusted for clustering of children by school and stratified by sex, were fitted to examine the associations between dietary measures and physical activity and sedentary outcomes. In total, 1317 children (584 boys and 733 girls) provided concurrent data. Boys in the highest quartile of energy percentage from protein spent approximately 6 min [95% confidence interval (CI) 0-12] less in MVPA compared with boys in the lowest quartile. Those in the highest quartiles of fruit and vegetable intake and fruit juice intake had respective average activity counts per minute that were 56 above (95% CI 8-105) and 48 below (95% CI 2-95) those in the lowest quartiles, whilst those in the highest quartile of fizzy drink consumption spent approximately 7 min (95% CI 2-13) more in MVPA and approximately 14 min (95% CI 5-24 min) less in sedentary behaviour. Boys in the highest quartile of savoury snack consumption spent approximately 8 min (95% CI 2-13 min) more in MVPA per day, and approximately 12 min (95% CI 2-23) less in sedentary behaviour. No significant associations were apparent among girls. Few associations were detected, and the directions of those that were apparent were mainly counterintuitive. The extent to which this reflects a true lack of association or is associated with the measurement methods used for

  19. Baseline coastal oblique aerial photographs collected from Calcasieu Lake, Louisiana, to Brownsville, Texas, September 9-10, 2008

    Science.gov (United States)

    Morgan, Karen L. M.; Karen A. Westphal,

    2016-04-28

    The U.S. Geological Survey (USGS), as part of the National Assessment of Coastal Change Hazards project, conducts baseline and storm-response photography missions to document and understand the changes in vulnerability of the Nation's coasts to extreme storms (Morgan, 2009). On September 9-10, 2008, the USGS conducted an oblique aerial photographic survey from Calcasieu Lake, Louisiana, to Brownsville, Texas, aboard a Cessna C-210 (aircraft) at an altitude of 500 feet (ft) and approximately 1,000 ft offshore. This mission was flown to collect baseline data for assessing incremental changes of the beach and nearshore area, and the data can be used in the assessment of future coastal change.The photographs provided in this report are Joint Photographic Experts Group (JPEG) images. ExifTool was used to add the following to the header of each photo: time of collection, Global Positioning System (GPS) latitude, GPS longitude, keywords, credit, artist (photographer), caption, copyright, and contact information. The photograph locations are an estimate of the position of the aircraft at the time the photograph was taken and do not indicate the location of any feature in the images (see the Navigation Data page). These photographs document the state of the barrier islands and other coastal features at the time of the survey. Pages containing thumbnail images of the photographs, referred to as contact sheets, were created in 5-minute segments of flight time. These segments can be found on the Photos and Maps page. Photographs can be opened directly with any JPEG-compatible image viewer by clicking on a thumbnail on the contact sheet.In addition to the photographs, a Google Earth Keyhole Markup Language (KML) file is provided and can be used to view the images by clicking on the marker and then clicking on either the thumbnail or the link above the thumbnail. The KML file was created using the photographic navigation files. The KML file can be found in the kml folder.

  20. TR-ESR Investigation on Reaction of Vitamin C with Excited Triplet of 9,10-phenanthrenequinone in Reversed Micelle Solutions

    Science.gov (United States)

    Xu, Xin-sheng; Shi, Lei; Liu, Yi; Ji, Xue-han; Cui, Zhi-feng

    2011-04-01

    Time-resolved electron spin resonance has been used to study quenching reactions between the antioxidant Vitamin C (VC) and the triplet excited states of 9,10-phenanthrenequinone (PAQ) in ethylene glycol-water (EG-H2O) homogeneous and inhomogeneous reversed micelle solutions. Reversed micelle solutions were used to be the models of physiological environment of biological cell and tissue. In PAQ/EG-H2O homogeneous solution, the excited triplet of PAQ (3PAQ*) abstracts hydrogen atom from solvent EG. In PAQ/VC/EG-H2O solution, 3PAQ* abstracts hydrogen atom not only from solvent EG but also from VC. The quenching rate constant of 3PAQ* by VC is close to the diffusion-controlled value of 1.41 × 108 L/(mol ·s). In hexadecyltrimethylammonium bromide (CTAB)/EG-H2O and aerosol OT (AOT)/EG-H2O reversed micelle solutions, 3PAQ* and VC react around the water-oil interface of the reversed micelle. Exit of 3PAQ* from the lipid phase slows down the quenching reaction. For Triton X-100 (TX-100)/EG-H2O reversed micelle solution, PAQ and VC coexist inside the hydrophilic polyethylene glycol core, and the quenching rate constant of 3PAQ* by VC is larger than those in AOT/EG-H2O and CTAB/EG-H2O reversed micelle solutions, even a little larger than that in EG-H2O homogeneous solution. The strong emissive chemically induced dynamic electron polarization of As.- resulted from the effective TM spin polarization transfer in hydrogen abstraction of 3PAQ* from VC.

  1. Variation of martensite lath width and precipitate size during creep deformation in a 10Cr-Mo steel

    International Nuclear Information System (INIS)

    Kim, S. H.; Song, B. Z.; Lu, W. S.

    2001-01-01

    The relationship between creep deformation and microstructural changes in martensitic 10Cr-MoW steel has been studied. Transmission electron microscopy and image analyser were used to determine the variation of precipitates and martensite lath width size during creep deformation and aging. As precipitates are coarsened during creep deformation, dislocations become easy to move and the recovery proceeds rapidly. This leads to the growth of lath width. The average size of precipitates was linearly increased with creep time. On the other hand the growth rate of lath width is constant until tertiary creep, but the growth of lath width is accelerated during tertiary creep. It has been concluded that the growth behavior of lath width are consistent with creep deformation. Because the growth of lath width is controlled by the coarsening of precipitates it is important to form more stable precipitates in creep condition for improvement of creep properties of martensitie steel. Microstructure of martensitic steel is thermally very stable, so the size of precipitates and martensite lath width are hardly changed during aging

  2. Long term properties and microstructural evolution of 18Cr-10Ni-3Cu-Ti-Nb austenitic stainless steel for boiler tube application

    Energy Technology Data Exchange (ETDEWEB)

    Minami, Y.; Fukui, T.; Ono, T. [TenarisNKK Tubes, Kawasaki, Kanagawa (Japan); Caminada, S. [TenarisDalmine, Dalmine, BG (Italy)

    2010-07-01

    The allowable tensile stress of 0.1C-18Cr-10Ni-3Cu-Ti-Nb steel (TEMPALOY AA-1; ASME C.C. 2512) is more than 30% higher compared with that of ASME SA-213 Grade TP347H in the temperature range 600-700 C. This high creep rupture strength is obtained by the precipitation of MC and M{sub 23}C{sub 6} carbides, and Cu-rich phase. Long term creep rupture tests over 10{sup 5}h enabled to verify the superior creep rupture strength of this steel. The investigation of microstructural evolution on the creep ruptured and aged specimens has shown the high structural stability of this material. Hardness and impact properties after high temperature aging reveal similar performance as conventional 18-8 stainless steels. Excellent steam oxidation resistance can be achieved by a shot-blasting method. The scale thickness of shot-blasted tube after 1000h at 750 C is below a few micron meters. These results have revealed that the mechanical properties and environmental resistance of this steel enable the use of TEMPALOY AA-1 in the latest generation of advanced USC boiler. (orig.)

  3. INFLUENCE OF MODIFICATION ON THE STRUCTURE AND CHARACTERISTICS OF THE STAINLESS STEEL 12X18H10TL

    Directory of Open Access Journals (Sweden)

    I. V. Zemskov

    2004-01-01

    Full Text Available There are given the results of investigation of influence of modification by ferrocerium, FS30RZM30B, FSMG, modifier MN, developed in BNTU, ferromolybdenum on the structure and characteristics of the steel 12X18H10TL.

  4. Solvatochromism and preferential solvation of 1,4-dihydroxy-2,3-dimethyl-9,10-anthraquinone by UV-vis absorption and laser-induced fluorescence measurements

    Science.gov (United States)

    Sasirekha, V.; Vanelle, P.; Terme, T.; Ramakrishnan, V.

    2008-12-01

    Solvation characteristics of 1,4-dihydroxy-2,3-dimethyl-9,10-anthraquinone ( 1) in pure and binary solvent mixtures have been studied by UV-vis absorption spectroscopy and laser-induced fluorescence techniques. The binary solvent mixtures used as CCl 4 (tetrachloromethane)-DMF ( N, N-dimethylformamide), AN (acetonitrile)-DMSO (dimethylsulfoxide), CHCl 3 (chloroform)-DMSO, CHCl 3-MeOH (methanol), and MeOH-DMSO. The longest wavelength band of 1 has been studied in pure solvents as well as in binary solvent mixtures as a function of the bulk mole fraction. The Vis absorption band maxima show an unusual blue shift with increasing solvent polarity. The emission maxima of 1 show changes with varying the pure solvents and the composition in the case of binary solvent mixtures. Non-ideal solvation characteristics are observed in all binary solvent mixtures. It has been observed that the quantity [ ν-(Xν+Xν)] serves as a measure of the extent of preferential solvation, where ν˜ and X are the position of band maximum in wavenumbers (cm -1) and the bulk mole fraction values, respectively. The preferential solvation parameters local mole fraction ( X2L), solvation index ( δs2), and exchange constant ( k12) are evaluated.

  5. Structural and theoretical study of 1-[1-oxo-3-phenyl-(2-benzosulfonamide)-propyl amido] - anthracene-9,10-dione to be i-motif inhibitor

    Science.gov (United States)

    Vatsal, Manu; Devi, Vandna; Awasthi, Pamita

    2018-04-01

    The 1-[1-oxo-3-phenyl-(2-benzosulfonamide)-propyl amido] - anthracene-9,10-dione (BPAQ) an analogue of anthracenedione class of antibiotic has been synthesized. To characterize molecular functional groups FT-IR and FT-Raman spectrum were recorded and vibrational frequencies were assigned accordingly. The optimized geometrical parameters, vibrational assignments, chemical shifts and thermodynamic properties of title compound were computed by ab initio calculations at Density Functional Theory (DFT) method with 6-31G(d,p) as basis set. The calculated harmonic vibrational frequencies of molecule were then analysed in comparison to experimental FT-IR and Raman spectrum. Gauge independent atomic orbital (GIAO) method was used for determining, (1H) and carbon (13C) nuclear magnetic resonance (NMR) spectra of the molecule. Molecular parameters were calculated along with its periodic boundary conditions calculation (PBC) analysis supported by X-ray diffraction studies. The frontier molecular orbital (HOMO, LUMO) analysis describes charge distribution and stability of the molecule which concluded that nucleophilic substitution is more preferred and the mullikan charge analysis also confirmed the same. Further the title compound showed an inhibitory action at d(TCCCCC), an intermolecular i-motif sequence, hence molecular docking study suggested the inhibitory activity of the compound at these junction.

  6. Topic 1. Steels for light water reactor pressure vessels

    International Nuclear Information System (INIS)

    Brumovsky, M.; Brynda, J.; Kepka, M.; Barackova, L.; Vacek, M.; Havel, S.; Cukr, B.; Protiva, K.; Petrman, I.; Tvrdy, M.; Hyspecka, L.; Mazanec, K.; Kupca, L.; Brezina, M.

    1980-01-01

    Part 1 of the Proceedings consists of papers on the criteria for the selection and comparison of the properties of steel for pressure vessels and on the metallurgy of the said steels, the selection of suitable material for internal tubing systems, the manufacture of high-alloy steels for WWER components, the mechanical and metallurgical properties of steel 22K for WWER 440 pressure components, and of steel 10MnNi2Mo for the WWER primary coolant circuit, and the metallographic assessment of steel 0Kh18N10T. (J.P.)

  7. Round Robin Posttest analysis of a 1/10-scale Steel Containment Vessel Model Test

    International Nuclear Information System (INIS)

    Komine, Kuniaki; Konno, Mutsuo

    1999-01-01

    NUPEC and U.S. Nuclear Regulatory Commission (USNRC) have been jointly sponsoring 'Structural Behavior Test' at Sandia National Laboratory (SNL) in Cooperative Containment Research Program'. As one of the test, a test of a mixed scaled SCV model with 1/10 in the geometry and 1/4 in the shell thickness. Round Robin analyses of a 1/10-scale Steel Containment Vessel (SCV) Model Test were carried out to obtain an adequate analytical method among seven organizations belonged to five countries in the world. As one of sponsor, Nuclear Power Engineering Corporation (NUPEC) filled the important role of a posttest analysis of SCV model. This paper describes NUPEC's analytical results in the round robin posttest analysis. (author)

  8. Numerical simulation on temperature field of TIG welding for 0Cr18Ni10Ti steel cladding and experimental verification

    International Nuclear Information System (INIS)

    Luo Hongyi; Tang Xian; Luo Zhifu

    2015-01-01

    Aiming at tungsten inert gas (TIG) for 0Cr18Ni10Ti stainless steel cladding for radioactive source, the numerical calculation of welding pool temperature field was carried out through adopting ANSYS software. The numerical model of non-steady TIG welding pool shape was established, the heat enthalpy and Gaussian electric arc heat source model of surface distribution were introduced, and the effects of welding current and welding speed to temperature field distribution were calculated. Comparing the experimental data and the calculation results under different welding currents and speeds, the reliability and correctness of the model were proved. The welding technological parameters of 0Cr18Ni10Ti stainless steel were optimized based on the calculation results and the welding procedure was established. (authors)

  9. Influence of family and friend smoking on intentions to smoke and smoking-related attitudes and refusal self-efficacy among 9-10 year old children from deprived neighbourhoods: a cross-sectional study.

    Science.gov (United States)

    McGee, Ciara E; Trigwell, Joanne; Fairclough, Stuart J; Murphy, Rebecca C; Porcellato, Lorna; Ussher, Michael; Foweather, Lawrence

    2015-03-07

    Smoking often starts in early adolescence and addiction can occur rapidly. For effective smoking prevention there is a need to identify at risk groups of preadolescent children and whether gender-specific intervention components are necessary. This study aimed to examine associations between mother, father, sibling and friend smoking and cognitive vulnerability to smoking among preadolescent children living in deprived neighbourhoods. Cross-sectional data was collected from 9-10 year old children (n =1143; 50.7% girls; 85.6% White British) from 43 primary schools in Merseyside, England. Children completed a questionnaire that assessed their smoking-related behaviour, intentions, attitudes, and refusal self-efficacy, as well as parent, sibling and friend smoking. Data for boys and girls were analysed separately using multilevel linear and logistic regression models, adjusting for individual cognitions and school and deprivation level. Compared to girls, boys had lower non-smoking intentions (P = 0.02), refusal self-efficacy (P = 0.04) and were less likely to agree that smoking is 'definitely' bad for health (P non-smoking intentions in girls (P non-smoking intentions in girls (P < 0.01) but a positive association was found in boys (P = 0.02). Boys who had a smoking friend were less likely to 'definitely' believe that the smoke from other people's cigarettes is harmful (OR 0.57, 95% CI: 0.35 to 0.91, P = 0.02). Further, boys with a smoking friend (OR 0.38, 95% CI: 0.21 to 0.69, P < 0.01) or a smoking sibling (OR 0.45, 95% CI: 0.21 to 0.98) were less likely to 'definitely' believe that smoking is bad for health. This study indicates that sibling and friend smoking may represent important influences on 9-10 year old children's cognitive vulnerability toward smoking. Whilst some differential findings by gender were observed, these may not be sufficient to warrant separate prevention interventions. However, further research is needed.

  10. Features of argon-arc welding of aluminium alloy AD1 to stainless steel 12Kh18N10T

    International Nuclear Information System (INIS)

    Sadov, I.I.

    1982-01-01

    Welding of pipes made of the 12Kh18N10T stainless steel and the AD1 aluminium alloy is proposed to perform using one-sided aluminizing. It is recommended to use shields in order to protect internal and external surfaces of pipes, aluminizing of which is impossible. It is shown that developed technological process for welded joints made of aluminium and stainless steel for cryogenic apparatus permits to create light-duty cryostat assembly using aluminium alloys instead of copper alloys, to increase reliability of apparatus (usage of welded joints instead of soldered ones), and to improve labour conditions

  11. Effect of heat treatment on workability of Cr-Ni-Mo steels

    International Nuclear Information System (INIS)

    Barcal, J.; Macek, K.

    1988-01-01

    The workability was studied of the new development generation of hardenable martensite Cr-Ni-Mo steels of the 10-10-2 and 6-11-3 types whose application is envisaged in future in nuclear engineering. Attention is paid to identification of inclusions and the phase analysis ofthe structure with respect to heat treatment and steel type. Face milling was used in the test of workability. In addition, tensile strength and impact bending strength testing was performed. The results showed that steel of the 6-11-3 type in the quenched condition was best workable. However, this steel showed a significant reduction in workability when in the hardened condition. Reduced workability can also be presumed for type 10-10-2 steel in the hardened condition when life is considered. Microstructure changes leading to softening of steel by aging had a favourable effect on workability, especially in steels of the 10-10-2 type. Hardened steels of the 6-11-3 type are recommended to be re-quenched. (Z.M.). 7 figs., 3 tabs., 9 refs

  12. Effect of partial oxygen pressure on physicochemical properties of Kh18N10T steel at isothermal oxidation. Vliyanie partsial'nogo davleniya kisloroda na fiziko-khimicheskie svojstva poverkhnosti stali Kh18N10T pri izotermicheskom okislenii

    Energy Technology Data Exchange (ETDEWEB)

    Alekseev, V N; Oshe, E K; Fokin, M N; Bogdanova, S V; Loskutov, A I [AN SSSR, Moscow (USSR). Inst. Fizicheskoj Khimii

    1990-10-01

    Auger-electron spectroscopy, photoelectric polarization, conductometry methods have been used to analyze chemical and defect composition of surface oxide layers, formed on stainless steel Kh18N10T in vacuum (10{sup -9} - 10{sup -2} torr) and at temperatures 593-673 K. The boundary conditions of manifestation of extermal behaviour of the dependence of the surface oxide growth rate at isothermal oxidation of this steel are determined. The relation between passivation properties of the surface oxide and the magnitude of the edge angle of the surface wetting with molten tin is revealed.

  13. Development of High Heat Input Welding High Strength Steel Plate for Oil Storage Tank in Xinyu Steel Company

    Science.gov (United States)

    Zhao, Hemin; Dong, Fujun; Liu, Xiaolin; Xiong, Xiong

    This essay introduces the developed high-heat input welding quenched and tempered pressure vessel steel 12MnNiVR for oil storage tank by Xinyu Steel, which passed the review by the Boiler and Pressure Vessel Standards Technical Committee in 2009. The review comments that compared to the domestic and foreign similar steel standard, the key technical index of enterprise standard were in advanced level. After the heat input of 100kJ/cm electro-gas welding, welded points were still with excellent low temperature toughness at -20°C. The steel plate may be constructed for oil storage tank, which has been permitted by thickness range from 10 to 40mm, and design temperature among -20°C-100°C. It studied microstructure genetic effects mechanical properties of the steel. Many production practices indicated that the mechanical properties of products and the steel by stress relief heat treatment of steel were excellent, with pretreatment of hot metal, converter refining, external refining, protective casting, TMCP and heat treatment process measurements. The stability of performance and matured technology of Xinyu Steel support the products could completely service the demand of steel constructed for 10-15 million cubic meters large oil storage tank.

  14. 40 CFR 35.910-5 - Additional allotments of previously withheld sums.

    Science.gov (United States)

    2010-07-01

    ...-Clean Water Act § 35.910-5 Additional allotments of previously withheld sums. (a) A total sum of $9... Kansas 53,794,200 Kentucky 90,430,800 Louisiana 71,712,250 Maine 78,495,200 Maryland 297,705,300... Montana 12,378,200 Nebraska 38,539,500 Nevada 31,839,800 New Hampshire 77,199,350 New Jersey 660,830,500...

  15. 49 CFR 178.512 - Standards for steel or aluminum boxes.

    Science.gov (United States)

    2010-10-01

    ... 49 Transportation 2 2010-10-01 2010-10-01 false Standards for steel or aluminum boxes. 178.512... aluminum boxes. (a) The following are identification codes for steel or aluminum boxes: (1) 4A for a steel box; and (2) 4B for an aluminum box. (b) Construction requirements for steel or aluminum boxes are as...

  16. Round Robin Posttest analysis of a 1/10-scale Steel Containment Vessel Model Test

    Energy Technology Data Exchange (ETDEWEB)

    Komine, Kuniaki [Nuclear Power Engineering Corp., Tokyo (Japan); Konno, Mutsuo

    1999-07-01

    NUPEC and U.S. Nuclear Regulatory Commission (USNRC) have been jointly sponsoring 'Structural Behavior Test' at Sandia National Laboratory (SNL) in Cooperative Containment Research Program'. As one of the test, a test of a mixed scaled SCV model with 1/10 in the geometry and 1/4 in the shell thickness. Round Robin analyses of a 1/10-scale Steel Containment Vessel (SCV) Model Test were carried out to obtain an adequate analytical method among seven organizations belonged to five countries in the world. As one of sponsor, Nuclear Power Engineering Corporation (NUPEC) filled the important role of a posttest analysis of SCV model. This paper describes NUPEC's analytical results in the round robin posttest analysis. (author)

  17. Mechanical properties and fatigue strength of high manganese non-magnetic steel/carbon steel welded joints

    International Nuclear Information System (INIS)

    Nakaji, Eiji; Ikeda, Soichi; Kim, You-Chul; Nakatsuji, Yoshihiro; Horikawa, Kosuke.

    1997-01-01

    The dissimilar materials welded joints of high manganese non-magnetic steel/carbon steel (hereafter referred to as DMW joints), in which weld defects such as hot crack or blowhole are not found, were the good quality. Tensile strength of DMW joints was 10% higher than that of the base metal of carbon steel. In the bend tests, the DMW joints showed the good ductility without crack. Charpy absorbed energy at 0(degC) of the DMW joints was over 120(J) in the bond where it seems to be the lowest. Large hardening or softening was not detected in the heat affected zone. Fatigue strength of the DMW joints is almost the same with that of the welded joints of carbon steel/carbon steel. As the fatigue strength of the DMW joints exceeds the fatigue design standard curve of JSSC for carbon steel welded joints, the DMW joints can be treated the same as the welded joints of carbon steel/carbon steel of which strength is lower than that of high manganese non-magnetic steel, from the viewpoint of the fatigue design. (author)

  18. The effect of cobalt and molybdenum on the creep strength of low C-18Cr-10Ni steel

    International Nuclear Information System (INIS)

    Tomono, Yutaka; Ueda, Jitsuhiko

    1982-01-01

    The improvement of creep strength through the addition of cobalt and molybdenum to low C-18Cr-10Ni steel was studied at a temperature range of between 700 and 800 0 C. Changes in mechanical and physical properties such as lattice parameter and stacking fault energy, related to the additional elements were investigated to estimate the strengthening effect. Dislocation structures corresponding to the various creep stages were observed through a transmission electron microscope to distinguish the solution hardening effect of the added elements from the precipitation hardening effects of carbide. The results obtained are summarized as follows: (1) Addition of cobalt of up to 20% by weight improved the creep strength of austenitic steel. Addition of molybdenum of up to 5% by weight remarkably improved the creep strength of austenitic steel having a cobalt content of 20% by weight. (2) The trend for creep strength to improve with the addition of these elements was closely coincident with increases in lattice parameter and did not necessarily coincide with changes in the stacking fault energy. (author)

  19. Quality of austenite chrome-nickel steel made by gas-oxygen refining

    International Nuclear Information System (INIS)

    Fel'dgandler, Eh.G.; Levin, F.L.; Moshkevich, E.A.; Shifrin, Eh.V.; Movshovich, V.S.; Pargamonov, E.A.

    1991-01-01

    Properties and structure were investigated of austenitic 03Kh18N11 and 08KhN10T steels melted at gas oxygen refining aggregates. It was established that mechanical and corrosion properties of rolling of such steels were in agreement with standard properties of metal of open melting. Sheet 08Kh18N10T steel has the level of strength and plasticity regulated for 12Kh18N10T steel. As steel of 08Kh18N10T holds the complex of high mechanical and corrosion properties, 08Kh18N10T is recommended to be replace by 12Kh18N10T with the aim of decrease of titanium usage and increase of process efficiency

  20. On the corrosion resistance of 01Kh25 ferritic steel

    International Nuclear Information System (INIS)

    Eremeeva, R.A.; Koval', E.K.

    1989-01-01

    Effect of non-ferrous metal ions on corrosion behaviour of 01Kh25 specific low carbon steel as compared to austenitic 12Kh18N10T and 06KhN28MDT steels in boiling solutions of sulfuric and nitric acids and their mixture is studied. Compositions initating commercial ones are chosen the media. It is shown that trough corrosion resistance of 01Kh25 steel in 10% H 2 SO 4 is two order below 06KhN28MDT austenitic steel in presence of Cu 2+ ions as a result of the surface passivation corrosion resistance of ferritic steel is an order higher the austenitic ones. Ferrite steel resistance in the nitric acid and its mixture with sulfuric acid is five timesas much as in 12Kh18N10T austenitic steel

  1. 46 CFR 154.195 - Aluminum cargo tank: Steel enclosure.

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 5 2010-10-01 2010-10-01 false Aluminum cargo tank: Steel enclosure. 154.195 Section... Equipment Hull Structure § 154.195 Aluminum cargo tank: Steel enclosure. (a) An aluminum cargo tank and its... the aluminum cargo tank must meet the steel structural standards of the American Bureau of Shipping...

  2. Plasticity of low carbon stainless steels

    International Nuclear Information System (INIS)

    Bulat, S.I.; Fel'dgandler, Eh.G.; Kareva, E.N.

    1975-01-01

    In the temperature range 800-1200 0 C and with strain rates of from 10 -3 to 3 s -1 , austenitic (000Kh18N12) and austenitic-ferrite (000Kh26N6) very low carbon stainless steels containing 0.02-0.03% C exhibit no higher resilience than corresponding ordinary steels containing 0.10-0.12% C. However, the plasticity of such steels (particularly two-phase steels) at 900-1100 0 C is appreciably inferior owing to the development of intergranular brittle fracture. Pressure treatment preceded by partial cooling of the surface to 850 0 C yields rolled and forged products with acceptable indices but is inconvenient technically. At the Zlatoustovsk and Ashin metallurgical plants successful tests have been performed involving the forging and rolling of such steels heated to 1280-1300 0 C without partial cooling; it was necessary to improve the killing conditions, correct the chemical composition (increasing the proportion of ferrite) and take measures against heat loss. (author)

  3. 1-Hydroxy-3-[(E)-4-(piperazine-diium)but-2-enyloxy]-9,10-anthraquinone ditrifluoroactate induced autophagic cell death in human PC3 cells.

    Science.gov (United States)

    Huang, A-Mei; Lin, Kai-Wei; Lin, Wei-Hong; Wu, Li-Hung; Chang, Hao-Chun; Ni, Chujun; Wang, Danny Ling; Hsu, Hsue-Yin; Su, Chun-Li; Shih, Chiaho

    2018-02-01

    The autophagy of human prostate cancer cells (PC3 cells) induced by a new anthraquinone derivative, 1-Hydroxy-3-[(E)-4-(piperazine-diium)but-2-enyloxy]-9,10-anthraquinone ditrifluoroactate (PA) was investigated, and the relationship between autophagy and reactive oxygen species (ROS) generation was studied. The results indicated that PA induced PC3 cell death in a time- and dose-dependent manner, could inhibit PC3 cell growth by G1 phase cell cycle arrest and corresponding decrease in the G2/M cell population and induced S-phase arrest accompanied by a significant decrease G2/M and G1 phase numbers after PC3 cells treated with PA for 48 h, and increased the accumulation of autophagolysosomes and microtubule-associated protein LC3-ll, a marker of autophagy. However, these phenomenon were not observed in the group pretreated with the autophagy inhibitor 3-MA or Bafilomycin A1 (BAF), suggesting that PA induced PC3 cell autophagy. In addition, we found that PA triggered ROS generation in cells, while the levels of ROS decreased in the N-acetylcysteine (NAC) co-treatment, indicating that PA-mediated autophagy was partly blocked by NAC. In summary, the autophagic cell death of human PC3 cells mediated by PA-triggered ROS generation. Copyright © 2017 Elsevier B.V. All rights reserved.

  4. Influence of cooling rate on the structure and mechanical properties of G17CrMoV5 – 10 cast steel

    Directory of Open Access Journals (Sweden)

    G. Golański

    2009-07-01

    Full Text Available The paper presents results of research on the influence of cooling rate on the structure and properties of G17CrMoV5 – 10 (L17HMF cast steel. The material for research was a section taken out from an outer cylinder of a steam turbine body after about 250 000 hours of operation at the temperature of 535°C and pressure 9 MPa. The investigated cast steel was subjected to heat treatment which consisted in cooling at the rates corresponding to the processes, such as: bainitic hardening, normalizing and full annealing. Tempering after the process of cooling from austenitizing temperature was carried out at the temperatures of: 700, 720 and 740°C. Performed research has proved that structures obtained after bainitic hardening and normalizing are characterized by a large strength margin which allows to apply high temperatures of tempering. It has been shown that the cast steel of bainitic structure, with similar mechanical properties as the cast steel of bainitic – ferritic structure, is characterized by almost twice as high impact energy. Full annealing and tempering of the examined cast steel ensures only the required impact strength, with mechanical properties comparable to those after service.

  5. EAMJ Provider April 10.indd

    African Journals Online (AJOL)

    2010-04-04

    Apr 4, 2010 ... from 14 to 30 days in studies done in Europe and. North America ... to confirmatory laboratory diagnostic test was 56.2 days (n=83, range 1 to 985 days, standard .... (9,10). In a population based study in German, Volker ... risk factors for provider delays (9). ... mammographic reliability for cancer diagnosis at.

  6. Age-hardening susceptibility of high-Cr ODS ferritic steels and SUS430 ferritic steel

    Energy Technology Data Exchange (ETDEWEB)

    Chen, Dongsheng, E-mail: chen.dongsheng85@gmail.com [Graduate School of Energy Science, Kyoto University, Gokasho, Uji, Kyoto 611-0011 (Japan); Kimura, Akihiko; Han, Wentuo; Je, Hwanil [Institute of Advanced Energy, Kyoto University, Gokasho, Uji, Kyoto 611-0011 (Japan)

    2015-10-15

    Highlights: • The role of oxide particles in α/α′ phase decomposition behavior; microstructure of phase decomposition observed by TEM. • The characteristics of ductility loss caused by age-hardening. • Correlation of phase decomposition and age-hardening explained by dispersion strengthened models. • Age-hardening susceptibility of ODS steels and SUS430 steel. - Abstract: The effect of aging on high-Cr ferritic steels was investigated with focusing on the role of oxide particles in α/α′ phase decomposition behavior. 12Cr-oxide dispersion strengthened (ODS) steel, 15Cr-ODS steel and commercial SUS430 steel were isothermally aged at 475 °C for up to 10,000 h. Thermal aging caused a larger hardening in SUS430 than 15Cr-ODS, while 12Cr-ODS showed almost no hardening. A characteristic of the ODS steels is that the hardening was not accompanied by the significant loss of ductility that was observed in SUS430 steel. After aging for 2000 h, SUS430 steel shows a larger ductile–brittle transition temperature (DBTT) shift than 15Cr-ODS steel, which suggests that the age-hardening susceptibility is lower in 15Cr-ODS steel than in conventional SUS430 steel. Thermal aging leaded to a large number of Cr-rich α′ precipitates, which were confirmed by transmission electron microscopy (TEM). Correlation of age-hardening and phase decomposition was interpreted by Orowan type strengthening model. Results indicate that oxide particles cannot only suppress ductility loss, but also may influence α/α′ phase decomposition kinetics.

  7. Susceptibility to stress corrosion in stainless steels type AISI 321 and 12X18H10T used in PWR type reactors (WWER); Susceptibilidad a la corrosion bajo esfuerzo de barras de acero inoxidable AISI 321 y 12X18H10T en ambientes utilizados en reactores VVER

    Energy Technology Data Exchange (ETDEWEB)

    Matadamas C, N

    1996-12-31

    Titanium stabilized stainless steels have been utilized in sovietic pressurized water reactors (VVER) for avoid the susceptibility to Intergranular Corrosion (IGC) present in other austenitic stainless steels. However the Intergranular Corrosion resistance of this kind of materials has been questioned because of Intergranular Stress Corrosion Cracking failures (IGSCC) have been reported. This paper study the electrochemical behavior of the AISI 321 stainless steel in a H{sub 3}BO{sub 3} Solution contaminated with chlorides and its susceptibility to Intergranular Corrosion.Electrochemical prediction diagrams of the stainless steels AISI 321 and 12X18H10T (sovietic) sensitized (600 Centigrade, 3 h.) were compared. Cylindrical and conical samples were used in Slow Strain Rate Tests (SSRT), to determine the susceptibility to Stress Corrosion Cracking (SCC) in AISI 321 and 12X18H10T stainless steels. The results obtained showed that the temperature of the solution is a very important factor to detect this susceptibility. Fractography studies on the fracture surfaces of the samples obtained in the SSRT at high temperature were realized. Corrosion velocities of both AISI 321 and 12X18H10T stainless steels were determined using conical samples in the CERT system at high temperature. E.D.A.X. analysis was employed in both AISI 321 and 12X18H10T stainless steels in order to explain the degree of sensitization. (Author).

  8. One-electron reduction of 1,2-dihydroxy-9,10-anthraquinone and some of its transition metal complexes in aqueous solution and in aqueous isopropanol-acetone-mixed solvent: a steady-state and pulse radiolysis study

    International Nuclear Information System (INIS)

    Das, S.; Bhattacharya, A.; Mandal, P.C.; Rath, M.C.; Mukherjee, T.

    2002-01-01

    One-electron reduction of 1,2-dihydroxy-9,10-anthraquinone (DHA) and its complexes with Cu(II), Ni(II) and Fe(III), by acetone ketyl radical, (CH 3 ) 2 C·OH, was carried out in aqueous solution and in aqueous isopropanol acetone mixed solvent using both steady-state gamma radiolysis and pulse radiolysis techniques. The rate constants for the reduction of DHA at different pH values by the ketyl radical are in the order of ∼10 9 dm 3 mol -1 s -1 , whereas those for the metal complexes are comparatively less. These rate constants are, however, in conformity with the one-electron reduction potentials of the ligand in free DHA and in its metal complexes. Decay kinetics of the one-electron reduced semiquinones of the free ligand and its metal complexes suggest disproportionation of the semiquinone in the case of the free ligand and intermolecular electron transfer from the co-ordinated semiquinone radical to the metal centre in the case of the metal complexes

  9. Stress corrosion (Astm G30-90 standard) in 08x18H10T stainless steel of nuclear fuel storage pool in WWER reactors

    International Nuclear Information System (INIS)

    Herrera, V.; Zamora R, L.

    1997-01-01

    At the water storage of the irradiated nuclear fuel has been an important factor in its management. The actual pools have its walls covered with inoxidable steel and heat exchangers to dissipate the residual heat from fuel. It is essential to control the water purity to eliminate those conditions which aid to the corrosion process in fuel and at related components. The steel used in this research was obtained from an austenitic inoxidizable steel standardized with titanium 08x18H10T (Type 321) similar to one of the two steel coatings used to cover walls and the pools floor. the test consisted in the specimen deformation through an U ply according to the Astm G30-90 standard. The exposition of the deformed specimen it was realized in simulated conditions to the chemical regime used in pools. (Author)

  10. DEVELOPMENT OF SOFTWARE “PRODSP-1.0” FOR OPTIMIZATION OF THE DEPHOSPHORIZATION PROCESSES IN ARC STEEL-FURNACES FOR TECHNOLOGICAL LINE-UP OF RUP “BMZ”

    Directory of Open Access Journals (Sweden)

    A. A. Chichko

    2006-01-01

    Full Text Available The software “ProDSP-1,0” allowing to forecast the dynamics of the dephosphorizaiton process at casting course in arc steel-furnace, is worked out. The examples of working of different program operating regimes, showing the possibilities of phosphorus control in steel-furnace of RUP ‘'BMZ'' are given.

  11. Steel alloys

    International Nuclear Information System (INIS)

    Bloom, E.E.; Stiegler, J.O.; Rowcliffe, A.F.; Leitnaker, J.M.

    1977-01-01

    The invention deals with a fuel element for fast breeder reactors. It consits essentially of a uranium oxide, nitride, or carbide or a mixture of these fuels with a plutonium or thorium oxide, nitride, or carbide. The fuel elements are coated with an austenitic stainless steel alloy. Inside the fuel elements, vacancies or small cavities are produced by neutron effects which causes the steel coating to swell. According to the invention, swelling is prevented by a modification of type 304, 316, 321, or 12 K 72HV commercial steels. They consist mainly of Fe, Cr, and Ni in a ratio determined by a temary diagram. They may also contain 1.8 to 2.3% by weight of Mo and a fraction of Si (0.7 to 2% by weight) and Ti(0.10 to 0.5% by weight) to prevent cavity formation. They are structurally modified by cold working. (IHOE) [de

  12. Food and drink consumption at school lunchtime: the impact of lunch type and contribution to overall intake in British 9-10-year-old children.

    Science.gov (United States)

    Harrison, Flo; Jennings, Amy; Jones, Andy; Welch, Ailsa; van Sluijs, Esther; Griffin, Simon; Cassidy, Aedín

    2013-06-01

    To examine the differences in dietary intakes of children consuming school meals and packed lunches, the contribution of lunchtime intake to overall dietary intake, and how lunchtime intake relates to current food-based recommendations for school meals. Cross-sectional analysis of overall intake of macronutrients and food choice from 4 d food diaries and school lunchtime intake from the two diary days completed while at school. Norfolk, UK. One thousand six hundred and twenty-six children (aged 9-10 years) attending ninety Norfolk primary schools. At school, lunchtime school meal eaters consumed more vegetables, sweet snacks, chips, starchy foods and milk, and less squash/cordial, fruit, bread, confectionery and savoury snacks than packed lunch eaters. These differences were also reflected in the overall diet. On average school meal eaters met the School Food Trust (SFT) food-based standards, while food choices among packed lunch eaters were less healthy. The contribution of food consumed at school lunchtime to overall diet varied by food and lunch type, ranging from 0.8 % (milk intake in packed lunches) to 74.4 % (savoury snack intake in packed lunches). There were significant differences in the foods consumed by school meal and packed lunch eaters, with food choices among school meal eaters generally in line with SFT standards. The food choices made at school lunchtime make a significant contribution to overall diet.

  13. Corrosion behavior of Al-Fe-sputtering-coated steel, high chromium steels, refractory metals and ceramics in high temperature Pb-Bi

    International Nuclear Information System (INIS)

    Abu Khalid, Rivai; Minoru, Takahashi

    2007-01-01

    Corrosion tests of Al-Fe-coated steel, high chromium steels, refractory metals and ceramics were carried out in high temperature Pb-Bi at 700 C degrees. Oxygen concentrations in this experiment were 6.8*10 -7 wt.% for Al-Fe-coated steels and 5*10 -6 wt.% for high chromium steels, refractory metals and ceramics. All specimens were immersed in molten Pb-Bi in a corrosion test pot for 1.000 hours. Coating was done with using the unbalanced magnetron sputtering (UBMS) technique to protect the steel from corrosion. Sputtering targets were Al and SUS-304. Al-Fe alloy was coated on STBA26 samples. The Al-Fe alloy-coated layer could be a good protection layer on the surface of steel. The whole of the Al-Fe-coated layer still remained on the base surface of specimen. No penetration of Pb-Bi into this layer and the matrix of the specimen. For high chromium steels i.e. SUS430 and Recloy10, the oxide layer formed in the early time could not prevent the penetration of Pb-Bi into the base of the steels. Refractory metals of tungsten (W) and molybdenum (Mo) had high corrosion resistance with no penetration of Pb-Bi into their matrix. Penetration of Pb-Bi into the matrix of niobium (Nb) was observed. Ceramic materials were SiC and Ti 3 SiC 2 . The ceramic materials of SiC and Ti 3 SiC 2 had high corrosion resistance with no penetration of Pb-Bi into their matrix. (authors)

  14. High - speed steel for precise cased tools

    International Nuclear Information System (INIS)

    Karwiarz, J.; Mazur, A.

    2001-01-01

    The test results of high-vanadium high - speed steel (SWV9) for precise casted tools are presented. The face -milling cutters of NFCa80A type have been tested in industrial operating conditions. An average life - time of SWV9 steel tools was 3-10 times longer compare to the conventional high - speed milling cutters. Metallography of SWB9 precise casted steel revealed beneficial for tool properties distribution of primary vanadium carbides in the steel matrix. Presented results should be a good argument for wide application of high - vanadium high - speed steel for precise casted tools. (author)

  15. Corrosion mechanism of Z3 CN18.10 stainless steel in the presence of nitric acid condensates

    International Nuclear Information System (INIS)

    Balbaud, Fanny

    1998-01-01

    In installations handling concentrated boiling nitric acid, a severe intergranular corrosion can sometimes occur in condensation zones constituted of non-sensitized Z3 CN 18.10 stainless steel. Corrosion tests in reactors and in a specific loop, CIRCE, allowed to specify the conditions of occurrence of this type of corrosion and showed the similitude with the corrosion in non-renewed liquid nitric acid: the specific parameters linked to the condensate phase are the high ratio metallic surface area to volume of condensate and the low renewing rate which induce a concentration of oxidation products of the metal and of reduction products of nitric acid. The initiation of the intergranular corrosion is attributed to the increase in the reduction rate of nitric acid by an autocatalytic mechanism which was demonstrated by electrochemical measurements on platinum and on stainless steel. The reduction mechanism involves a charge transfer step where nitrous acid, the electro-active species, is reduced into nitrogen monoxide and a chemical regeneration reaction of nitrous acid. The thermodynamic study led to a representation of the chemical and electrochemical properties of nitric acid. This study allowed also to determine the Gibbs free energy of formation of nitrous acid in solution in concentrated nitric acid at 100 deg. C. The diagram, constructed in coordinates log(P O 2 ) / [-log(P HNO 3 )] or E eXperimental / [-log(P HNO 3 )], shows that the final reduction product of nitric acid depends on the concentration of nitric acid: at 100 deg. C, NO is obtained for concentrations lower than 8 mol.L -1 and NO 2 is obtained for higher concentrations. All these results allowed to propose a corrosion mechanism of Z3 CN 18.10 stainless steel in the presence of nitric acid condensates. [fr

  16. Simulation of Microdamage and Evaluation of Remaining Life of Steam Conduit Components from New-Generation Refractory Steel 10Kh9MF-Sh

    Science.gov (United States)

    Gladshtein, V. I.

    2018-03-01

    The effects of microdamage on the remaining life of high-temperature components of steam conduits from high-chromium steel 10Kh9MF-Sh and low-alloy steel 12Kh1M1F are compared. To simulate the microdamage, specimens with a circular notch and different relative diameters are fabricated. Specimens with a notch simulating the highest degree of microdamage and smooth specimens are tested for long-term strength. The coefficient of the remaining life of a conduit is computed for the range of relative damage presenting practical interest.

  17. Larson-Miller Constant of Heat-Resistant Steel

    Science.gov (United States)

    Tamura, Manabu; Abe, Fujio; Shiba, Kiyoyuki; Sakasegawa, Hideo; Tanigawa, Hiroyasu

    2013-06-01

    Long-term rupture data for 79 types of heat-resistant steels including carbon steel, low-alloy steel, high-alloy steel, austenitic stainless steel, and superalloy were analyzed, and a constant for the Larson-Miller (LM) parameter was obtained in the current study for each material. The calculated LM constant, C, is approximately 20 for heat-resistant steels and alloys except for high-alloy martensitic steels with high creep resistance, for which C ≈ 30 . The apparent activation energy was also calculated, and the LM constant was found to be proportional to the apparent activation energy with a high correlation coefficient, which suggests that the LM constant is a material constant possessing intrinsic physical meaning. The contribution of the entropy change to the LM constant is not small, especially for several martensitic steels with large values of C. Deformation of such martensitic steels should accompany a large entropy change of 10 times the gas constant at least, besides the entropy change due to self-diffusion.

  18. Compatibility tests of steels in flowing liquid lead-bismuth

    International Nuclear Information System (INIS)

    Barbier, F.; Benamati, G.; Fazio, C.; Rusanov, A.

    2001-01-01

    The behaviour of steels exposed to flowing Pb-55Bi was evaluated. The materials tested are the two austenitic steels AISI 316L and 1.4970, and the six martensitic steels Optifer IVc, T91, Batman 27, Batman 28, EP823 and EM10 which were exposed to flowing Pb-55Bi for 1000, 2000 and 3000 h and at two temperatures (573 and 743 K). The corrosion tests were conducted in the non-isothermal loop of IPPE-Obninsk under a controlled oxygen level (10 -6 wt%). The compatibility study showed that at a lower temperature, a very thin oxide layer (<1 μm) was formed on the steels. At higher temperature, austenitic steels also exhibited a thin oxide layer sufficient to prevent their dissolution in the melt. A thicker oxide, which grew according to a parabolic law, was observed on the surface of the martensitic steels. The oxidation resistance behaviour of the martensitic steels was correlated with their alloying elements

  19. Irradiation embrittlement of pressure vessel steels

    International Nuclear Information System (INIS)

    Brumovsky, M.; Vacek, M.

    1975-01-01

    A Standard Research Programme on Irradiation Embrittlement of Pressure Vessel Steels was approved by the Coordinating Meeting on the 12th May 1972 at the Working Group on Engineering Aspects of Irradiation Embrittlement of Pressure Vessel Steels. This Working Group was set up by the International Atomic Energy Agency in Vienna. Seven countries with their research institutes agreed on doing irradiation experiments according to the approved programme on steel A533 B from the U.S. HSST Programme. The Czechoslovak contribution covering tensile and impact testing of non-irradiated steel and steel irradiated at 280degC to 1.3 x 10 23 n/m 2 (E above 1 MeV) is presented in this report. As an additional part the same set of experiments was carried out on two additional steels - A 542 and A 543, made in SKODA Works for comparison of their irradiation embrittlement and hardening with A533 B steel. (author)

  20. Irradiation creep in ferritic steels

    International Nuclear Information System (INIS)

    Vandermeulen, W.; Bremaecker, A. de; Burbure, S. de; Huet, J.J.; Asbroeck, P. van

    Pressurized and non-pressurized capsules of several ferritic steels have been irradiated in Rapsodie between 400 and 500 0 C up to 3.7 x 10 22 n/cm 2 (E>0.1 MeV). Results of the diameter measurements are presented and show that the total in-pile deformation is lower than for austenitic steels

  1. Comparison of extrapolation methods for creep rupture stresses of 12Cr and 18Cr10NiTi steels

    International Nuclear Information System (INIS)

    Ivarsson, B.

    1979-01-01

    As a part of a Soviet-Swedish research programme the creep rupture properties of two heat resisting steels namely a 12% Cr steel and an 18% Cr12% Ni titanium stabilized steel have been studied. One heat from each country of both steels were creep tested. The strength of the 12% Cr steels was similar to earlier reported strength values, the Soviet steel being some-what stronger due to a higher tungsten content. The strength of the Swedish 18/12 Ti steel agreed with earlier results, while the properties of the Soviet steel were inferior to those reported from earlier Soviet creep testings. Three extrapolation methods were compared on creep rupture data collected in both countries. Isothermal extrapolation and an algebraic method of Soviet origin gave in many cases rather similar results, while the parameter method recommended by ISO resulted in higher rupture strength values at longer times. (author)

  2. Early detection of critical material degradation by means of electromagnetic multi-parametric NDE

    Science.gov (United States)

    Szielasko, Klaus; Tschuncky, Ralf; Rabung, Madalina; Seiler, Georg; Altpeter, Iris; Dobmann, Gerd; Herrmann, Hans-Georg; Boller, Christian

    2014-02-01

    With an increasing number of power plants operated in excess of their original design service life an early recognition of critical material degradation in components will gain importance. Many years of reactor safety research allowed for the identification and development of electromagnetic NDE methods which detect precursors of imminent damage with high sensitivity, at elevated temperatures and in a radiation environment. Regarding low-alloy heat-resistant steel grade WB 36 (1.6368, 15NiCuMoNb5), effects of thermal and thermo-mechanical aging on mechanical-technological properties and several micromagnetic parameters have been thoroughly studied. In particular knowledge regarding the process of copper precipitation and its acceleration under thermo-mechanical load has been enhanced. Whilst the Cu-rich WB 36 steel is an excellent model material to study and understand aging effects related to neutron radiation without the challenge of handling radioactive specimens in a hot cell, actually neutron-irradiated reactor pressure vessel materials were investigated as well. The neutron fluence experienced and the resulting shift of the ductile-brittle transition temperature were determined electromagnetically, and it was shown that weld and base material can be distinguished from the cladded side of the RPV wall. Low-cycle fatigue of the austenitic stainless steel AISI 347 (1.4550, X6CrNiNb18-10) has been characterized with electromagnetic acoustic transducers (EMATs) at temperatures of up to 300 °C. Time-of-flight and amplitude of the transmitted ultrasound signal were evaluated against the number of load cycles applied and observed as an indication of the imminent material failure significantly earlier than monitoring stresses or strains.

  3. Early detection of critical material degradation by means of electromagnetic multi-parametric NDE

    Energy Technology Data Exchange (ETDEWEB)

    Szielasko, Klaus; Tschuncky, Ralf; Rabung, Madalina; Altpeter, Iris; Dobmann, Gerd [Fraunhofer Institute for Nondestructive Testing (IZFP), Campus E3 1, 66123 Saarbrücken (Germany); Seiler, Georg; Herrmann, Hans-Georg; Boller, Christian [Fraunhofer Institute for Nondestructive Testing (IZFP), Campus E3 1, 66123 Saarbrücken, Germany and Saarland University, Chair of NDT and Quality Assurance, Campus E3 1, 66123 Saarbrücken (Germany)

    2014-02-18

    With an increasing number of power plants operated in excess of their original design service life an early recognition of critical material degradation in components will gain importance. Many years of reactor safety research allowed for the identification and development of electromagnetic NDE methods which detect precursors of imminent damage with high sensitivity, at elevated temperatures and in a radiation environment. Regarding low-alloy heat-resistant steel grade WB 36 (1.6368, 15NiCuMoNb5), effects of thermal and thermo-mechanical aging on mechanical-technological properties and several micromagnetic parameters have been thoroughly studied. In particular knowledge regarding the process of copper precipitation and its acceleration under thermo-mechanical load has been enhanced. Whilst the Cu-rich WB 36 steel is an excellent model material to study and understand aging effects related to neutron radiation without the challenge of handling radioactive specimens in a hot cell, actually neutron-irradiated reactor pressure vessel materials were investigated as well. The neutron fluence experienced and the resulting shift of the ductile-brittle transition temperature were determined electromagnetically, and it was shown that weld and base material can be distinguished from the cladded side of the RPV wall. Low-cycle fatigue of the austenitic stainless steel AISI 347 (1.4550, X6CrNiNb18-10) has been characterized with electromagnetic acoustic transducers (EMATs) at temperatures of up to 300 °C. Time-of-flight and amplitude of the transmitted ultrasound signal were evaluated against the number of load cycles applied and observed as an indication of the imminent material failure significantly earlier than monitoring stresses or strains.

  4. Early detection of critical material degradation by means of electromagnetic multi-parametric NDE

    International Nuclear Information System (INIS)

    Szielasko, Klaus; Tschuncky, Ralf; Rabung, Madalina; Altpeter, Iris; Dobmann, Gerd; Seiler, Georg; Herrmann, Hans-Georg; Boller, Christian

    2014-01-01

    With an increasing number of power plants operated in excess of their original design service life an early recognition of critical material degradation in components will gain importance. Many years of reactor safety research allowed for the identification and development of electromagnetic NDE methods which detect precursors of imminent damage with high sensitivity, at elevated temperatures and in a radiation environment. Regarding low-alloy heat-resistant steel grade WB 36 (1.6368, 15NiCuMoNb5), effects of thermal and thermo-mechanical aging on mechanical-technological properties and several micromagnetic parameters have been thoroughly studied. In particular knowledge regarding the process of copper precipitation and its acceleration under thermo-mechanical load has been enhanced. Whilst the Cu-rich WB 36 steel is an excellent model material to study and understand aging effects related to neutron radiation without the challenge of handling radioactive specimens in a hot cell, actually neutron-irradiated reactor pressure vessel materials were investigated as well. The neutron fluence experienced and the resulting shift of the ductile-brittle transition temperature were determined electromagnetically, and it was shown that weld and base material can be distinguished from the cladded side of the RPV wall. Low-cycle fatigue of the austenitic stainless steel AISI 347 (1.4550, X6CrNiNb18-10) has been characterized with electromagnetic acoustic transducers (EMATs) at temperatures of up to 300 °C. Time-of-flight and amplitude of the transmitted ultrasound signal were evaluated against the number of load cycles applied and observed as an indication of the imminent material failure significantly earlier than monitoring stresses or strains

  5. Normal Force Influence on 3D Texture Parameters Characterizing the Friction Couple Steel – PBT + 10 % PTFE

    Directory of Open Access Journals (Sweden)

    C. Georgescu

    2014-03-01

    Full Text Available This study presents the influence of the normal force on the surface quality of the friction couple steel – polybutylene terephthalate (PBT + 10 % polytetrafluoroethylene (PTFE. There were calculated the average values of the amplitude and functional parameters, as obtained from investigating square areas on the wear tracks, with the help of a proposed methodology, for initial and tested surfaces generated on the blocks and on counterpart ring made of rolling bearing steel, for the following test conditions: three normal forces (F = 1 N, F = 2.5 N and F =5 N, three sliding speeds (v = 0.25 m/s, v = 0.50 m/s and v = 0.75 m/s and a sliding distance of L = 7500 m. The conclusion of the research study was that the tested normal force range has an insignificant influence on the surface quality for the tested materials and parameters. This friction couple could be recommended for variable conditions (speed and load in dry regimes.

  6. Pion production in 3He-nucleus interactions at 910 MeV

    International Nuclear Information System (INIS)

    Aslanides, E.; Baumann, P.; Bergdolt, G.; Engelstein, P.; Fassnacht, P.; Hibou, F.; Bressani, T.; Puddu, G.A.

    1983-01-01

    The ( 3 He, πsup(+-)X) reaction has been studied at 910 MeV using the 3 He ++ beam of the CERN SC, Complete π - spectra on CH 2 , CD 2 , 9 Be, 12 C, 27 Al, Cd and Pb, and π + spectra on CH 2 , CD 2 and 12 C targets have been measured at 0 0 , up or close to the kinematic limit xsub(F)=1. The results are compared to various theoretical calculations. (orig.)

  7. Changes of structure and properties of cast steels GX10NiCrNb32-20 and GX10NiCrNb3-25 after long-term tempering at 600-1000 C

    International Nuclear Information System (INIS)

    Gommans, R.; Schrijen, H.; Sundermann, J.; Steinkusch, W.; Hering, W.

    2001-01-01

    Low-alloy cast steels of type GX 10NiCrNb 32.20 are commonly used for the outlet section of reformer and cracker tubes for the temperature range of 600-1000 C. There was a lack of data on the ductility of the 25%Cr alloyed cast steel GX10NiCrNb 35.25 at room temperature after tempering, which was investigated in a joint project of Pose-Marre and DSM. Mechanical tests were carried out at room temperature and at elevated temperatures. Apart from light microscopy, also SEM/EDX, SAM and TEM analyses were carried out. The 25% alloy has lower ductility than the 20% alloy, owing primarily to the more pronounced development of M 6 C carbide from primary NbC carbide, which takes up Ni and Si during tempering. The microstructure and composition of the M 6 C carbide wre not fully clarified. Information is presented on the potential application of low-carbon materials of the type GX10NiCrNb35.25 [de

  8. EFEK INTERVENSI PENDIDIKAN BERBASIS SEKOLAH TERHADAP TINGKAT PENGETAHUAN TENTANG PENCEHAGAN KEGEMUKAN DI ANTARA ANAK-ANAK USIA 9-10 TAHUN Di KOTA BANDUNG

    Directory of Open Access Journals (Sweden)

    Hermina Hermina

    2012-11-01

    Full Text Available Effect of School-Based Educational Interventions On The Level of Obesity Prevention's Knowledge Among 9-10 Year-Old Children In Bandung City.Background: The prevalence of obesity in Indonesia shows an increasing trend. A survey among adults in 12 major cities in Indonesia shows the prevalence of obesity in adult is more then 20%. The prevalence among school age children is 6.0%. Obesity in childhood is known to be an independent risk factor for adult obesity.Objectives: To assess the effect of school-based educational intervention on the level of obesity prevention's knowledge, among elementary school-aged children.Methods: This study having non-control group pre- and post-test design was based in three Bandung's Elementary Schools in 112 children aged 9 to 10 years. The three schools were selected from six Bandung's Elementary Schools having both high socio-economic status and more obese children based on the Office of Basic Education. The intervention schools drawn from SDN M5 included 39 children gave the Obesity Prevention's booklet by their teacher for their parent (Group A, SD P1 36 children gave the booklet for themselves (Group B, and SD P2 37 children gave the booklet for their parent and themselves (Group C. All children were measured their weight and height and were interviewed using structured questionnaire that covered their characteristics and the five topics about obesity (definition, causes, consequences, how to identify, and how to weight control. Data were analyzed descriptively and tested by Chi-square and t-tests.Results: At baseline, most of children (>90% had less of knowledge in the obesity prevention. After intervention, only the Group B & C had significantly increase in the knowledge (p<0.05. However, between the two groups, the Group C was more effective in increasing the knowledge.Conclusion: Educational intervention giving the Obesity Prevention's booklet by teacher to school children and their parents was more

  9. Transformation and Precipitation Kinetics in 30Cr10Ni Duplex Stainless Steel

    Science.gov (United States)

    Fazarinc, Matevz; Terčelj, Milan; Bombač, David; Kugler, Goran

    2010-09-01

    To improve the microstructure during casting, hot forming, and heat treatment of 30Cr10Ni duplex stainless steel, accurate data on the precipitation and transformation processes at high temperatures are needed. In this article, the precipitation and transformation processes at various aging times in the temperature range 873 K to 1573 K (600 °C to 1300 °C) were studied. The 30Cr10Ni ferrous alloy contains a relatively large amount of Cr, Ni, and C, which results in a complex microstructure. In addition to the ferrite, austenite, and sigma phase, the M23C6 and MC carbides were also observed in the microstructure. The precipitation of the sigma phase was observed after just 3 minutes of aging, and after 30 minutes of aging at approximately 1053 K (780 °C), its fraction exceeded 40 pct. An intensive austenite-to-ferrite transformation was observed above 1423 K (1150 °C). Optical microscopy, energy-dispersive X-ray spectroscopy (EDS), electron backscattered diffraction (EBSD), and X-ray diffraction (XRD), as well as micro-indentation hardness, hardness, impact toughness, and tensile tests, were carried out to evaluate the obtained microstructures of aged samples.

  10. 46 CFR 154.170 - Outer hull steel plating.

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 5 2010-10-01 2010-10-01 false Outer hull steel plating. 154.170 Section 154.170... STANDARDS FOR SELF-PROPELLED VESSELS CARRYING BULK LIQUEFIED GASES Design, Construction and Equipment Hull Structure § 154.170 Outer hull steel plating. (a) Except as required in paragraph (b) of this section, the...

  11. 46 CFR 154.172 - Contiguous steel hull structure.

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 5 2010-10-01 2010-10-01 false Contiguous steel hull structure. 154.172 Section 154.172... STANDARDS FOR SELF-PROPELLED VESSELS CARRYING BULK LIQUEFIED GASES Design, Construction and Equipment Hull Structure § 154.172 Contiguous steel hull structure. (a) Except as allowed in paragraphs (b) and (c) of this...

  12. SCC growth behavior of cast stainless steels in high-temperature water. Influences of corrosion potential, steel type, thermal aging and cold-work

    International Nuclear Information System (INIS)

    Yamada, Takuyo; Terachi, Takumi; Miyamoto, Tomoki; Arioka, Koji

    2011-01-01

    Recent studies on crack growth rate (CGR) measurement in oxygenated high-temperature pure water conditions, such as normal water chemistry (NWC) in BWRs, using compact tension (CT) type specimens have shown that stainless steel weld metal are susceptible to stress corrosion cracking (SCC). On the other hand, the authors reported that no significant SCC growth was observed on stainless steel weld metals in PWR primary water at temperatures from 250degC to 340degC. Cast austenitic stainless steels are widely used in light water reactors, and there is a similarity between welded and cast stainless steels in terms of the microstructure of the ferrite/austenite duplex structure. However, there are a few reports giving CGR data on cast stainless steels in the BWRs and PWRs. The principal purpose of this study was to examine the SCC growth behavior of cast stainless steels in simulated PWR primary water. A second objective was to examine the effects on SCC growth in hydrogenated and oxygenated water environments at 320degC of: (1) corrosion potential; (2) steels type (Mo in alloy); (3) thermal-aging (up to 400degC x 40 kh); and (4) cold-working (10%). The results were as follows: (1) No significant SCC growth was observed on all types of cast stainless steels: aged (400degC x 40 kh) of SCS14A and SCS13A and 10% cold-working, in hydrogenated (low-potential) water at 320degC. (2) Aging at 400degC x 40 kh SCS14A (10%CW) markedly accelerated the SCC growth of cast material in high-potential water at 320degC, but no significant SCC growth was observed in the hydrogenated water, even after long-term thermal aging (400degC x 40 kh). (3) Thus, cast stainless steels have excellent SCC resistance in PWR primary water. (4) On the other hand, significant SCC growth was observed on all types of cast stainless steels: 10%CW SCS14A and SCS13A, in 8 ppm-oxygenated (high-potential) water at 320degC. (5) No large difference in SCC growth was observed between SCS14A (Mo) and SCS13A. (6) No

  13. Mechanism of creep in stainless steel

    International Nuclear Information System (INIS)

    Monteiro, S.N.; Silveira, T.L.

    In the present work the creep criterions to identify the deformation mechanisms through the exponent of the strain rate versus stress relationship are presented. When applied to several stainless steels these criterions show an apparent contradiction for the proper mechanism acting at Σ/D above 10 9 /cm 2 . Microstructural aspects interfering in different manners with the fracture of these steels could be a reason for rationalizing the contradictory behavior. This is discussed in suggested deformation maps for the steels investigated [pt

  14. 40 CFR 35.910-12 - Reallotment of deobligated funds of Fiscal Year 1978.

    Science.gov (United States)

    2010-07-01

    ...-Clean Water Act § 35.910-12 Reallotment of deobligated funds of Fiscal Year 1978. (a) Of the 4.5 billion... 1,312,681 Indiana 699,465 Iowa 327,345 Kansas 222,494 Kentucky 369,430 Louisiana 319,073 Maine 189... Missouri 630,710 Montana 118,190 Nebraska 139,138 Nevada 118,190 New Hampshire 222,653 New Jersey 902,590...

  15. Utilization of structural steel in buildings.

    Science.gov (United States)

    Moynihan, Muiris C; Allwood, Julian M

    2014-08-08

    Over one-quarter of steel produced annually is used in the construction of buildings. Making this steel causes carbon dioxide emissions, which climate change experts recommend be reduced by half in the next 37 years. One option to achieve this is to design and build more efficiently, still delivering the same service from buildings but using less steel to do so. To estimate how much steel could be saved from this option, 23 steel-framed building designs are studied, sourced from leading UK engineering firms. The utilization of each beam is found and buildings are analysed to find patterns. The results for over 10 000 beams show that average utilization is below 50% of their capacity. The primary reason for this low value is 'rationalization'-providing extra material to reduce labour costs. By designing for minimum material rather than minimum cost, steel use in buildings could be drastically reduced, leading to an equivalent reduction in 'embodied' carbon emissions.

  16. Random cyclic constitutive models of 0Cr18Ni10Ti pipe steel

    International Nuclear Information System (INIS)

    Zhao Yongxiang; Yang Bing

    2004-01-01

    Experimental study is performed on the random cyclic constitutive relations of a new pipe stainless steel, 0Cr18Ni10Ti, by an incremental strain-controlled fatigue test. In the test, it is verified that the random cyclic constitutive relations, like the wide recognized random cyclic strain-life relations, is an intrinsic fatigue phenomenon of engineering materials. Extrapolating the previous work by Zhao et al, probability-based constitutive models are constructed, respectively, on the bases of Ramberg-Osgood equation and its modified form. Scattering regularity and amount of the test data are taken into account. The models consist of the survival probability-strain-life curves, the confidence strain-life curves, and the survival probability-confidence-strain-life curves. Availability and feasibility of the models have been indicated by analysis of the present test data

  17. performance of steel slag performance of steel slag as fine

    African Journals Online (AJOL)

    eobe

    Suitability of using steel slag (SS) as substitute for sand in concrete was ... The strength of SS concrete increased with increase in proporti. 10 mm. .... additives used. All other oxides ..... low lime coal fly ash in foamed concrete”, Fuel, Vol. 84,.

  18. Examination of influencing factors on cyclic crack growth behaviour of cracked components. Final report; Untersuchung von Einflussfaktoren auf das zyklische Risswachstum angerissener Bauteile. Abschlussbericht

    Energy Technology Data Exchange (ETDEWEB)

    Soppa, Ewa Anna; Silcher, Horst

    2015-01-31

    Fatigue crack growth of short and long cracks was investigated for both materials: the Nb-stabilized austenitic stainless steel X6 CrNiNb 18-10 and the ferritic-bainitic steel 22 NiMoCr 3-7. These both steels belong to the materials in the primary circuit of german power plants. For a reliable estimation of the lifetime of components subject to cyclic fatigue a detailed knowledge of the phenomena accompanying fatigue processes and which cause both - initiation and growth of fatigue cracks is essential. The deformation induced transformation of austenite into α'-martensite at room temperature is thus very important in the initiation and growth of fatigue cracks. Because these processes are manifest at first at the microlevel, the use of methods which reveal information at high resolution is of significant importance. In order to study the initiation and growth of short cracks, cylindrical smooth specimens, compact tension C(T)- and modified C(T)-specimens have been used. Cyclic crack propagation of long cracks was investigated on compact tension C(T)-specimens with W=50 mm and B=10 mm. The SEM, TEM and EBSD technique are powerful methods for determining crystallographic orientation, for the identification of individual phases and for recealing plastic deformation. They were used for analyses of microcracks in combination with interrupted cyclic tests. The impact of crack closure on the threshold parameter ΔK{sub th} and the crack growth rate da/dN was investigated experimentally for the growth of long cracks under cyclic loading for different R-values at room temperature. Additional tests were performed at T=288 C in order to investigate the role of temperature on crack growth rates. The effect of overloads in tension and compression as another factor influencing the crack growth was also studied. Measured crack growth curves were fitted using Paris and Erdogan-Ratwani law as well as the NASGRO-equation. Fracture surfaces of selected specimens for both steels

  19. Microstructural characterization of second phases in X10CrMoVNb9-1 and 12CrMoWCuVNb steels after long steam exposure time at 550 C

    International Nuclear Information System (INIS)

    Rodak, Kinga; Hernas, Adam; Vodarek, Vlastimil

    2015-01-01

    Microstructural changes in high alloy (9-12% Cr) creep resistant martensitic X10CrMoVNb9-1 and 12CrMoW . CuVNb steels after 100 000 h of steam exposure at 550 C have been studied using scanning transmission electron microscopy. Precipitates were identified using electron diffraction patterns and energy dispersive X-ray spectroscopy analysis. After long time exposure, a significant coarsening of M 23 C 6 carbides, and intensive precipitation of the coarse Laves phase were observed. Moreover, in the 12CrMoW . CuVNb steel, a low amount of the modified Z-phase particles was detected. The microstructures of the X10Cr . MoVNb9-1 and 12CrMoWCuVNb steels after 100 000 h of exposure differ in several aspects.

  20. Microstructural characterization of second phases in X10CrMoVNb9-1 and 12CrMoWCuVNb steels after long steam exposure time at 550 C

    Energy Technology Data Exchange (ETDEWEB)

    Rodak, Kinga; Hernas, Adam [Silesian Univ. of Technology, Inst. of Materials Science, Katowice (Poland); Vodarek, Vlastimil [VSB-Technical Univ. of Ostrava (Czech Republic)

    2015-07-15

    Microstructural changes in high alloy (9-12% Cr) creep resistant martensitic X10CrMoVNb9-1 and 12CrMoW . CuVNb steels after 100 000 h of steam exposure at 550 C have been studied using scanning transmission electron microscopy. Precipitates were identified using electron diffraction patterns and energy dispersive X-ray spectroscopy analysis. After long time exposure, a significant coarsening of M{sub 23}C{sub 6} carbides, and intensive precipitation of the coarse Laves phase were observed. Moreover, in the 12CrMoW . CuVNb steel, a low amount of the modified Z-phase particles was detected. The microstructures of the X10Cr . MoVNb9-1 and 12CrMoWCuVNb steels after 100 000 h of exposure differ in several aspects.

  1. Microstructure and susceptibility to HIBC of 10H2M steel exposed to service conditions of boilers in fossil power plants

    International Nuclear Information System (INIS)

    Lunarska, E.; Nikiforow, K.; Zielinski, W.; Kurzydlowski, K.J.

    2004-01-01

    Mechanical properties, microstructure and hydrogen permeation through 10H2M ferrite pearlite steel from boilers of power station being in-service for up to 100000 hours have been systematically analysed in order to correlate the change in susceptibility to HIBC with microstructure features. The change of the pearlite volume fraction, the carbide morphology and the ferrite dislocation structure as a function of in-service time has been evaluated by SEM and TEM analysis. Susceptibility to HIBC has been estimated in the especially elaborated electrochemical measurements of hydrogen permeation. The correlation has been found between the microstructure features and the hydrogen permeation parameters describing the susceptibility to hydrogen induced cracking of steel exploited in water-steam environment. (author)

  2. Biaxial Loading Tests for steel containment vessel

    Energy Technology Data Exchange (ETDEWEB)

    Miyagawa, T. [Nuclear Power Engineering Corp., Tokyo (Japan); Wright, D.J.; Arai, S.

    1999-07-01

    The Nuclear Power Engineering Corporation (NUPEC) has conducted a 1/10 scale of the steel containment vessel (SCV) test for the understanding of ultimate structural behavior beyond the design pressure condition. Biaxial Loading Tests were supporting tests for the 1/10 scale SCV model to evaluate the method of estimating failure conditions of thin steel plates under biaxial loading conditions. The tentative material models of SGV480 and SPV490 were obtained. And the behavior of SGV480 and SPV490 thin steel plates under biaxial loading conditions could be well simulated by FE-Analyses with the tentative material models and Mises constitutive law. This paper describes the results and the evaluations of these tests. (author)

  3. Biaxial Loading Tests for steel containment vessel

    International Nuclear Information System (INIS)

    Miyagawa, T.; Wright, D.J.; Arai, S.

    1999-01-01

    The Nuclear Power Engineering Corporation (NUPEC) has conducted a 1/10 scale of the steel containment vessel (SCV) test for the understanding of ultimate structural behavior beyond the design pressure condition. Biaxial Loading Tests were supporting tests for the 1/10 scale SCV model to evaluate the method of estimating failure conditions of thin steel plates under biaxial loading conditions. The tentative material models of SGV480 and SPV490 were obtained. And the behavior of SGV480 and SPV490 thin steel plates under biaxial loading conditions could be well simulated by FE-Analyses with the tentative material models and Mises constitutive law. This paper describes the results and the evaluations of these tests. (author)

  4. Strength of low-carbon rotor steel

    International Nuclear Information System (INIS)

    Voropaev, V.I.; Filimonov, O.V.; Borisov, I.A.

    1988-01-01

    The results of studying the effect of chemical composition and thermal treatment regimes on the structural strength of steels of the 25KhN3MFA type are presented. It is shown that alloying with niobium from 0.01 to 0.08% steels with the increased nickel content (4.2-4.5%) contributes to the increase of structural strength and reduction of semibrittleness temperature. To obtain high values of strength and plastic properties cooling with the rate of 10 3 -10 5 K/hr is recommended

  5. ITER ITA newsletter. No. 10, November 2003

    International Nuclear Information System (INIS)

    2003-12-01

    This issue of ITER ITA (ITER transitional Arrangements) newsletter contains concise information about an ITER related meeting, namely, the Ninth ITER Negotiations Meeting (N-9), which was held on 9-10 November 2003 at the Fragrant Hill Golden Resources Commerce Hotel in Beijing and information about research on magnetic confinement fusion (MCF) in China

  6. Consequences of Globalisation for the Belgian Steel Industry

    OpenAIRE

    DE GROOTE, Patrick

    2008-01-01

    Since a few years the worldwide steel industry has been under the spell of a great consolidation wave and enhanced competition. 2006 was a peak year with the merger of the European group Arcellor Mittal Steel to ArcellorMittal. With this merger, ArcellorMittal became the greatest steel group in the world with a market share of more than 10%. Thanks to the consolidation trend, the steel industry has changed from an obsolete and loss-making industry to a modern, attractive and profitable busine...

  7. 49 CFR 661.6 - Certification requirements for procurement of steel or manufactured products.

    Science.gov (United States)

    2010-10-01

    ... § 661.6 Certification requirements for procurement of steel or manufactured products. If steel, iron, or... 49 Transportation 7 2010-10-01 2010-10-01 false Certification requirements for procurement of steel or manufactured products. 661.6 Section 661.6 Transportation Other Regulations Relating to...

  8. 46 CFR 154.188 - Membrane tank: Inner hull steel.

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 5 2010-10-01 2010-10-01 false Membrane tank: Inner hull steel. 154.188 Section 154.188... STANDARDS FOR SELF-PROPELLED VESSELS CARRYING BULK LIQUEFIED GASES Design, Construction and Equipment Hull Structure § 154.188 Membrane tank: Inner hull steel. For a vessel with membrane tanks, the inner hull...

  9. A spectrophotometric method of determining nobium, ranging from 0,01 to 0,10% Nb, in steel with xylene orange after precipitation by tannin

    International Nuclear Information System (INIS)

    Jurczyk, J.; Capalla, K.; Szeja, K.

    1980-01-01

    A spectrophotometric method is presented of determining 0,1 to 0,10% niobium content in steel. The dissolution of steel was made by means of a mixture of hydrochloric and nitric acids. Niobium was precipitated by hydrolysis in the presence of tannin, gelatine and ascorbic acid and then was determined in the form of a coloured complex compound at pH 3. The concentration of niobium in the examined solution cannot exceed 1,6 μg/cm 3 . Standard deviation for niobium content 0,017% Nb is 0,0007% and for 0,100% Nb - 0,0025%. (author)

  10. Optimum conditions for aging of stainless maraging steels

    International Nuclear Information System (INIS)

    Mironenko, P.A.; Krasnikova, S.I.; Drobot, A.V.

    1980-01-01

    Aging kinetics of two 0Kh11N10M2T type steels in which 3 % Mo (steel 1), and 3 % Mo and 11 % Co (steel 2) had been additionally introduced instead of titanium were investigated. Electron microscopy and X-ray methods were used. It was ascertained that the process of steel aging proceeded in 3 stages. Steel 2 was hardened more intensively during the aging, had a higher degree of hardness and strength after the aging, weakened more slowly if overaged than steel 1. The intermetallide hcp-phase Fe 2 Mo was the hardening phase on steels extended aging. Optimum combination of impact strength and strength was was achieved using two-stage aging: the first stage - maximum strength aging was achieved, the second stage - aging at minimum temperatures of two-phase α+γ region

  11. Corrosion fatigue crack growth in clad low-alloy steels: Part 1, medium-sulfur forging steel

    International Nuclear Information System (INIS)

    James, L.A.; Poskie, T.J.; Auten, T.A.; Cullen, W.H.

    1996-01-01

    Corrosion fatigue crack propagation tests were conducted on a medium- sulfur ASTM A508-2 forging steel overlaid with weld-deposited Alloy EN82H cladding. The specimens featured semi-elliptical surface cracks penetrating approximately 6.3 mm of cladding into the underlying steel. The initial crack sizes were relatively large with surface lengths of 30.3--38.3 mm, and depths of 13.1--16.8 mm. The experiments were conducted in a quasi-stagnant low-oxygen (O 2 < 10 ppb) aqueous environment at 243 degrees C, under loading conditions (ΔK, R, and cyclic frequency) conductive to environmentally-assisted cracking (EAC) in higher-sulfur steels under quasi-stagnant conditions. Earlier experiments on unclad compact tension specimens of this heat of steel did not exhibit EAC, and the present experiments on semi-elliptical surface cracks penetrating cladding also did not exhibit EAC

  12. Microstructure and Nano-Hardness of 10 MeV Cl-Ion Irradiated T91 Steel

    International Nuclear Information System (INIS)

    Hu Jing; Wang Xianping; Gao Yunxia; Zhuang Zhong; Zhang Tao; Fang Qianfeng; Liu Changsong

    2015-01-01

    Hardening and elemental segregation of T91 martenstic steel irradiated by 10 MeV Cl ions to doses from 0.06 dpa to 0.83 dpa were investigated with the nanoindentation technique and transmission electron microscopy (TEM). The results demonstrated that the irradiation hardening was closely related with irradiation dose. By increasing the dose, the hardness increased rapidly at first from the initial value of 3.15 GPa before irradiation, and then tended to saturate at a value of 3.58 GPa at the highest dose of 0.83 dpa. Combined with TEM observation, the mechanism of hardening was preliminary attributed to the formation of M(Fe,Cr) 2 3C 6 carbides induced by the high energy Cl-ion irradiation. (paper)

  13. 25 CFR 166.910 - What happens if I do not fulfill my obligation to the BIA?

    Science.gov (United States)

    2010-04-01

    ... GRAZING PERMITS Agriculture Education, Education Assistance, Recruitment, and Training § 166.910 What... under agriculture education programs with an obligated service requirement, and who does not accept employment or unreasonably terminates employment must repay us in accordance with the following table: If you...

  14. Effect of agressive medium movement of local corrosion of the steel - 12Kh18N10T

    International Nuclear Information System (INIS)

    Makartsev, V.V.; Pakhomov, V.S.; Abramova, I.M.

    1980-01-01

    The effect of agressive medium movement on the formation of pitting corrosion of the 12Kh18N10T stainless steel in the acidic chloride-nitrate solution at room temperature is studied. It is established that the agressive medium movement hinders the formation of pitting corrosion at potentials more negative than +0.4 V and practically does not affect it at more positive potentials. The investigations have been carried out on a disc electrode rotating at a speed from 0 to 2000 rot./min

  15. Local corrosion of high alloy steels under biodeposits

    International Nuclear Information System (INIS)

    Korovyakova, M.D.; Nikitin, V.M.; Speshneva, N.V.

    1999-01-01

    Impact of the bacteriozenosis different structural-functional state under biodeposits on corrosion resistance of the 12Kh18N10T and Kh18N10T high-alloy steels in the natural seawater is studied. It is shown that saturation of natural micro communities by separate aerobic and facultative-anaerobic bacterial monocultures increases corrosion resistance of these steels by their overgrow with biodeposits [ru

  16. The IkappaB kinase family phosphorylates the Parkinson's disease kinase LRRK2 at Ser935 and Ser910 during Toll-like receptor signaling.

    Directory of Open Access Journals (Sweden)

    Nicolas Dzamko

    Full Text Available Mutations in leucine-rich repeat kinase 2 (LRRK2 are strongly associated with late-onset autosomal dominant Parkinson's disease. LRRK2 is highly expressed in immune cells and recent work points towards a link between LRRK2 and innate immunity. Here we demonstrate that stimulation of the Toll-Like Receptor (TLR pathway by MyD88-dependent agonists in bone marrow-derived macrophages (BMDMs or RAW264.7 macrophages induces marked phosphorylation of LRRK2 at Ser910 and Ser935, the phosphorylation sites that regulate the binding of 14-3-3 to LRRK2. Phosphorylation of these residues is prevented by knock-out of MyD88 in BMDMs, but not the alternative TLR adaptor protein TRIF. Utilising both pharmacological inhibitors, including a new TAK1 inhibitor, NG25, and genetic models, we provide evidence that both the canonical (IKKα and IKKβ and IKK-related (IKKε and TBK1 kinases mediate TLR agonist induced phosphorylation of LRRK2 in vivo. Moreover, all four IKK members directly phosphorylate LRRK2 at Ser910 and Ser935 in vitro. Consistent with previous work describing Ser910 and Ser935 as pharmacodynamic biomarkers of LRRK2 activity, we find that the TLR independent basal phosphorylation of LRRK2 at Ser910 and Ser935 is abolished following treatment of macrophages with LRRK2 kinase inhibitors. However, the increased phosphorylation of Ser910 and Ser935 induced by activation of the MyD88 pathway is insensitive to LRRK2 kinase inhibitors. Finally, employing LRRK2-deficient BMDMs, we present data indicating that LRRK2 does not play a major role in regulating the secretion of inflammatory cytokines induced by activation of the MyD88 pathway. Our findings provide the first direct link between LRRK2 and the IKKs that mediate many immune responses. Further work is required to uncover the physiological roles that phosphorylation of LRRK2 by IKKs play in controlling macrophage biology and to determine how phosphorylation of LRRK2 by IKKs impacts upon the use of Ser

  17. Dynamic characteristics of automotive steel sheets

    Directory of Open Access Journals (Sweden)

    M. Mihaliková

    2016-10-01

    Full Text Available The aim of this experimental research was to perform an analysis of deformation characteristics on two different types of steel: IF steel, and micro-alloyed steel were used automotive industry. For that purpose changes of properties of these materials were carried out by static 10-3 · s-1 and dynamic 103 · s-1 strain rate assess its plastic properties. Vickers micro hardness test was carried out by the static and dynamic loading condition and describes different hardness distribution. The higher strain hardening of materials was obtained too that was confirmed by distribution of dislocations.

  18. Study of the effect of an increase in phosphorus content on the corrosion resistance of austenitic stainless steels type 18-10

    International Nuclear Information System (INIS)

    Charbonnier, J.C.; Thomas, B.

    1982-01-01

    The work is carried out on Z 6 CN 18-10 steels with P concentrations in the range of 0.004 to 0.127%, to examine intercrystalline corrosion, pitting corrosion and cavern corrosion. It is concluded that a slight increase in the P content above 0.04% is compatible with an acceptable corrosion behaviour [fr

  19. Effect of hydrogen charging on the stability of SAE 10B22 steel surface in alkaline solutions

    International Nuclear Information System (INIS)

    Modiano, S.; Carreno, J.A.; Fugivara, C.S.; Benedetti, A.V.; Mattos, O.R.

    2005-01-01

    The influence of hydrogen charging into a quenched and tempered boron steel membrane electrode (SAE 10B22) was studied using borate buffer (pH 8.4) and NaOH solutions (pH 12.7), with or without the addition of 0.01 M EDTA. At the hydrogen input side, hydrogen charging influenced cyclic voltammograms increasing the anodic charge of iron(II) hydroxide formation, and decreasing the donor density of passive films. These results suggest that the hydrogen ingress caused instability of metallic surface, increasing the surface area activity

  20. Corrosion behavior of 2205 duplex stainless steel.

    Science.gov (United States)

    Platt, J A; Guzman, A; Zuccari, A; Thornburg, D W; Rhodes, B F; Oshida, Y; Moore, B K

    1997-07-01

    The corrosion of 2205 duplex stainless steel was compared with that of AISI type 316L stainless steel. The 2205 stainless steel is a potential orthodontic bracket material with low nickel content (4 to 6 wt%), whereas the 316L stainless steel (nickel content: 10 to 14 wt%) is a currently used bracket material. Both stainless steels were subjected to electrochemical and immersion (crevice) corrosion tests in 37 degrees C, 0.9 wt% sodium chloride solution. Electrochemical testing indicates that 2205 has a longer passivation range than 316L. The corrosion rate of 2205 was 0.416 MPY (milli-inch per year), whereas 316L exhibited 0.647 MPY. When 2205 was coupled to 316L with equal surface area ratio, the corrosion rate of 2205 reduced to 0.260 MPY, indicating that 316L stainless steel behaved like a sacrificial anode. When 316L is coupled with NiTi, TMA, or stainless steel arch wire and was subjected to the immersion corrosion test, it was found that 316L suffered from crevice corrosion. On the other hand, 2205 stainless steel did not show any localized crevice corrosion, although the surface of 2205 was covered with corrosion products, formed when coupled to NiTi and stainless steel wires. This study indicates that considering corrosion resistance, 2205 duplex stainless steel is an improved alternative to 316L for orthodontic bracket fabrication when used in conjunction with titanium, its alloys, or stainless steel arch wires.

  1. Hot flow behavior of boron microalloyed steels

    International Nuclear Information System (INIS)

    Lopez-Chipres, E.; Mejia, I.; Maldonado, C.; Bedolla-Jacuinde, A.; El-Wahabi, M.; Cabrera, J.M.

    2008-01-01

    This research work studies the effect of boron contents on the hot flow behavior of boron microalloyed steels. For this purpose, uniaxial hot-compression tests were carried out in a low carbon steel microalloyed with four different amounts of boron over a wide range of temperatures (950, 1000, 1050 and 1100 deg. C) and constant true strain rates (10 -3 , 10 -2 and 10 -1 s -1 ). Experimental results revealed that both peak stress and peak strain tend to decrease as boron content increases, which indicates that boron additions have a solid solution softening effect. Likewise, the flow curves show a delaying effect on the kinetics of dynamic recrystallization (DRX) when increasing boron content. Deformed microstructures show a finer austenitic grain size in the steel with higher boron content (grain refinement effect). Results are discussed in terms of boron segregation towards austenitic grain boundaries during plastic deformation, which increases the movement of dislocations, enhances the grain boundary cohesion and modificates the grain boundary structure

  2. Formed electroslag welded joint from austenitic steel 18/10 CrNi

    International Nuclear Information System (INIS)

    Jilek, L.; Kusak, L.; Martinak, A.

    1987-01-01

    The electroslag welded joint from titanium stabilized steel 18/10 CrNi of 150 mm in thickness showed positive results for both nondestructive and destructive testing. Czechoslovak flux VUZ-4F and the optimized welding mode were completely proven. The weldment was subject to deformation by forging with a removal of 20 to 50% and to bending deformation. A 40% to 50% deformation was necessary for breaking the coarse-grain casting structure. The bending deformation resulted in breaking the coarse-grain casting structure in the entire cross-section, it was, however, only acting in a narrow band corresponding to the largest curvature. At the same time, the heat affected zone decayed. Following heat treatment, especially forming, the delta ferrite content in the weld metal decreased, the mechanical properties of the weld metal and the welded joint following welding and heat treatment showed a relatively large scatter. Forming reduced the scatter and improved plastic properties. Machining within 40 and 50% resulted in good echogenicity of the welded joint in ultrasound testing. The welded joint showed equal properties as the base material of the weldment. (author). 15 figs., 2 tabs., 16 refs

  3. Validation and Application of Computed Radiography (CR) Tangential Technique for Wall Thickness Measurement of 10 Inch Carbon Steel Pipe

    International Nuclear Information System (INIS)

    Norhazleena Azaman; Khairul Anuar Mohd Salleh; Amry Amin Abas; Arshad Yassin; Sukhri Ahmad

    2016-01-01

    Oil and gas industry requires Non Destructive Testing (NDT) to ensure each components, in-service and critical, are fit-for-purpose. Pipes that are used to transfer oil or gas are amongst the critical component that needs to be well maintained and inspected. Typical pipe discontinuities that may lead to unintended incidents are erosion, corrosion, dent, welding defects, etc. Wall thickness assessment, with Radiography Testing (RT) is normally used to inspect such discontinuities and can be performed with two approaches; (a) center line beam tangential technique (b) offset from the centre pipe tangential technique. The latter is a method of choice for this work because of the pipe dimension and limited radiation safe distance at site. Two successful validation approaches (simulation and experimental) were performed to determine the probability of successfulness before the actual RT work with tangential technique is carried out. The pipe was a 10 inch diameter in-service wrapped carbon steel. A 9 Ci Ir-192 and white Imaging Plate (IP) were used as a gamma radiation source and to record the radiographic image. Result of this work suggest that RT with tangential technique for 10 inch wrapped in-service carbon steel pipe can be successfully performed. (author)

  4. Internal Friction of Pressure Vessel Steel Embrittlement

    International Nuclear Information System (INIS)

    Van Ouytsel, K.

    2001-01-01

    The contribution consists of an abstract of a PhD thesis. The thesis contains a literature study, a description of the construction details of a new inverted torsion pendulum. This device was designed to investigate pressure-vessel steels at high amplitudes (10 -4 to 10 -2 ) and over a wide temperature range (90-700K) at approximately 1 Hz in the irradiated condition. Results of measurements on a variety of reactor pressure vessel steels by means of the torsion penduli are reported and interpreted

  5. Effect of smelt aluminium on mechanical properties of steels

    International Nuclear Information System (INIS)

    Ryabov, V.R.; Dykhno, I.S.; Deev, G.F.; Karikh, V.V.

    1987-01-01

    Effect of smelt aluminium on mechanical properties of armco-iron and 12 Kh18N10T steel is studied. It is stated that in smelt aluminium and aluminium alloy contact with armco-iron the sample ductility is decreased. Corrosion effect of smelt alluminium on (18Kh15N5AM3) steel in the form of reinforced wire in aluminium-steel KAS-1A composite material is investigted. It is stated in experiment that during smelt alluminium-steel contact interaction of heterogeneous phases takes place

  6. Anodized Steel Electrodes for Supercapacitors.

    Science.gov (United States)

    Sagu, Jagdeep S; Wijayantha, K G Upul; Bohm, Mallika; Bohm, Siva; Kumar Rout, Tapan

    2016-03-09

    Steel was anodized in 10 M NaOH to enhance its surface texture and internal surface area for application as an electrode in supercapacitors. A mechanism was proposed for the anodization process. Field-emission gun scanning electron microscopy (FEGSEM) studies of anodized steel revealed that it contains a highly porous sponge like structure ideal for supercapacitor electrodes. X-ray photoelectron spectroscopy (XPS) measurements showed that the surface of the anodized steel was Fe2O3, whereas X-ray diffraction (XRD) measurements indicated that the bulk remained as metallic Fe. The supercapacitor performance of the anodized steel was tested in 1 M NaOH and a capacitance of 18 mF cm(-2) was obtained. Cyclic voltammetry measurements showed that there was a large psueudocapacitive contribution which was due to oxidation of Fe to Fe(OH)2 and then further oxidation to FeOOH, and the respective reduction of these species back to metallic Fe. These redox processes were found to be remarkably reversible as the electrode showed no loss in capacitance after 10000 cycles. The results demonstrate that anodization of steel is a suitable method to produce high-surface-area electrodes for supercapacitors with excellent cycling lifetime.

  7. Effect of N+Cr alloying on the microstructures and tensile properties of Hadfield steel

    International Nuclear Information System (INIS)

    Chen, C.; Zhang, F.C.; Wang, F.; Liu, H.; Yu, B.D.

    2017-01-01

    The microstructures and tensile behaviors of traditional Hadfield steel, named Mn12 steel, and Hadfield steel alloyed with N+Cr, named Mn12CrN steel were studied through optical microscopy, transmission electron microscopy, and scanning electron microscopy, among others. Three different tensile strain rates of 5×10 −4 , 5×10 −3 , and 5×10 −2 s −1 were selected in the tensile test. The deformation microstructures and fracture morphologies of the two steels after fracture in the tensile test were observed to analyze the tensile deformation response to different tensile strain rates. Results showed that the grain size of Mn12CrN steel was evidently refined after alloying with N+Cr. The grain would not become abnormally coarse even with increasing austenitizing temperature. During tensile deformation, the strength and plasticity of Mn12CrN steel were superior to those of Mn12 steel at the same strain rate. With increasing the strain rate, the changes in strength and plasticity of Mn12CrN steel were less sensitive to tensile strain rate compared with Mn12 steel. The effects of grain refinement and N+Cr alloying on dynamic strain aging and deformation twining behaviors were responsible for this lack of sensitivity to strain rate.

  8. Aerosol measurements from plasma torch cuts on stainless steel, carbon steel, and aluminum

    International Nuclear Information System (INIS)

    Novick, V.J.; Brodrick, C.J.; Crawford, S.; Nasiatka, J.; Pierucci, K.; Reyes, V.; Sambrook, J.; Wrobel, S.; Yeary, J.

    1996-01-01

    The main purpose of this project is to quantify aerosol particle size and generation rates produced by a plasma torch whencutting stainless steel, carbon steel and aluminum. the plasma torch is a common cutting tool used in the dismantling of nuclear facilities. Eventually, other cutting tools will be characterized and the information will be compiled in a user guide to aid in theplanning of both D ampersand D and other cutting operations. The data will be taken from controlled laboratory experiments on uncontaminated metals and field samples taken during D ampersand D operations at ANL nuclear facilities. The plasma torch data was collected from laboratory cutting tests conducted inside of a closed, filtered chamber. The particle size distributions were determined by isokinetically sampling the exhaust duct using a cascade impactor. Cuts on different thicknesses showed there was no observable dependence of the aerosol quantity produced as a function of material thickness for carbon steel. However, data for both stainless steel and aluminum revealed that the aerosol mass produced for these materials appear to have some dependance on thickness, with thinner materials producing tmore aerosols. The results of the laboratory cutting tests show that most measured particle size distributions are bimodal with one mode at about 0.2 μm and the other at about 10 μm. The average Mass Median Aerodynamic Diameters (MMAD's) for these tests are 0.36 ±0.08 μm for stainless steel, 0.48 ±0.17μm for aluminum and 0.52±0.12 μm for carbon steel

  9. 46 CFR 54.25-25 - Welding of quenched and tempered steels (modifies UHT-82).

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 2 2010-10-01 2010-10-01 false Welding of quenched and tempered steels (modifies UHT-82... ENGINEERING PRESSURE VESSELS Construction With Carbon, Alloy, and Heat Treated Steels § 54.25-25 Welding of quenched and tempered steels (modifies UHT-82). (a) The qualification of welding procedures, welders, and...

  10. Changes in structure and phase composition of chromium diffusion layer on stainless steels after long annealing

    International Nuclear Information System (INIS)

    Knyazev, E.V.; Voshedchenko, B.M.; Voskresenskij, Yu.A.

    1985-01-01

    A study was made on the effect of elevated temperatures UU and long holdings at heat on structure, phase composition and properties of chromium diffusion layer on austenitic chromium-nickel stainless steels 10Kh18N10TVD, 10Kh15N30M4B, 10Kh11N23T3MR, 10Kh21N28V6M3. The following mechanism of processes taking place in diffusion chromium layer is presented. The steady drop of chromium concentrations is observed after diffusion saturation. Chromium redistribution related with system transformation to more equilibrium state and simultaneous decarburization of steel surfaces takes place in diffusion layers of 10Kh15N30M4B and 10Kh21N28V6M3 steels after annealing at different temperatures and holdings at heat. Decarburization of steel surface layers is practically excluded in diffusion layers of 10Kh18N10T-VD and 10Kh11N23T3MR steels. Diffusion chromium-saturated layer stays effective only on 10Kh18N10T-VD and 10Kh11N23T3MR steels on heating up to 1000 deq C with holding up to 250 h

  11. Improved corrosion resistance of cast carbon steel in sulphur oxides by Alonizing

    International Nuclear Information System (INIS)

    Holtzer, M.; Dzioba, Z.

    1992-01-01

    The results of studies on the Alonizing of cast steel and of testing the corrosion resistance of this cast steel in an atmosphere containing 5 to 6% SO 2 + 50% SO 3 at 853 K are described and compared with the results obtained with unalonized cast carbon steel and high-alloy 23Cr-8Ni-2Mo cast steel. The duration of the corrosion tests was 336 hours. The aluminium diffusion layer on cast carbon steel was obtained by holding the specimens in a mixture containing 99% of powered Fe-Al and 1% of NH 4 Cl at 1323 ± 20 K. The holding time was 10 and 20 hours, respectively. The aluminium layer formed on the cast carbon steel was examined by optical microscopy and an X-ray microanalysis. After Alonizing for 10 h the layer had reached a thickness of 950 μm, and contained up to 35% Al. In a mixture of sulphur oxides corrosion rate of the alonized cast carbon steel was by about 600 times lower than of the unalonized cast carbon steel, and by about 50 times lower than that of the 23Cr-8Ni-2Mo cast steel. (orig.) [de

  12. Microbial-Influenced Corrosion of Corten Steel Compared with Carbon Steel and Stainless Steel in Oily Wastewater by Pseudomonas aeruginosa

    Science.gov (United States)

    Mansouri, Hamidreza; Alavi, Seyed Abolhasan; Fotovat, Meysam

    2015-07-01

    The microbial corrosion behavior of three important steels (carbon steel, stainless steel, and Corten steel) was investigated in semi petroleum medium. This work was done in modified nutrient broth (2 g nutrient broth in 1 L oily wastewater) in the presence of Pseudomonas aeruginosa and mixed culture (as a biotic media) and an abiotic medium for 2 weeks. The behavior of corrosion was analyzed by spectrophotometric and electrochemical methods and at the end was confirmed by scanning electron microscopy. The results show that the degree of corrosion of Corten steel in mixed culture, unlike carbon steel and stainless steel, is less than P. aeruginosa inoculated medium because some bacteria affect Corten steel less than other steels. According to the experiments, carbon steel had less resistance than Corten steel and stainless steel. Furthermore, biofilm inhibits separated particles of those steels to spread to the medium; in other words, particles get trapped between biofilm and steel.

  13. Prevalence of undiagnosed cardiovascular risk factors and 10-year CVD risk in male steel industry workers.

    Science.gov (United States)

    Gray, Benjamin J; Bracken, Richard M; Turner, Daniel; Morgan, Kerry; Mellalieu, Stephen D; Thomas, Michael; Williams, Sally P; Williams, Meurig; Rice, Sam; Stephens, Jeffrey W

    2014-05-01

    To assess the prevalence of undiagnosed cardiovascular disease (CVD) in a cohort of male steelworkers in South Wales, UK. Male steel industry workers (n = 221) with no prior diagnosis of CVD or diabetes accepted a CVD risk assessment within the work environment. Demographic, anthropometric, family, and medical histories were all recorded and capillary blood samples obtained. The 10-year CVD risk was predicted using the QRISK2-2012 algorithm. Up to 81.5% of workers were either overweight or obese. More than 20% of workers were found to have diastolic hypertension, high total cholesterol, and/or a total cholesterol/high-density lipoprotein ratio of six or more. Over one quarter of workers assessed had an increased 10-year CVD risk. Despite a physically demanding occupation, risk assessment in the workplace uncovered significant occult factors in CVD risk in a sample of male heavy industry workers.

  14. Aging degradation of cast stainless steel

    International Nuclear Information System (INIS)

    Chopra, O.K.; Chung, H.M.

    1985-10-01

    A program is being conducted to investigate the significance of in-service embrittlement of cast-duplex stainless steels under light-water reactor operating conditions. Data from room-temperature Charpy-impact tests for several heats of cast stainless steel aged up to 10,000 h at 350, 400, and 450 0 C are presented and compared with results from other studies. Microstructures of cast-duplex stainless steels subjected to long-term aging either in the laboratory or in reactor service have been characterized. The results indicate that at least two processes contribute to the low-temperature embrittleent of duplex stainless steels, viz., weakening of the ferrite/austenite phase boundary by carbide precipitation and embrittlement of ferrite matrix by the formation of additional phases such as G-phase, Type X, or the α' phase. Carbide precipitation has a significant effect on the onset of embrittlement of CF-8 and -8M grades of stainless steels aged at 400 or 450 0 C. The existing correlations do not accurately represent the embrittlement behavior over the temperature range 300 to 450 0 C. 18 refs., 13 figs

  15. Low-temperature cyclic cracking resistance of Fe-Cr-Ni and Fe-Cr-Mn steels welded joints

    International Nuclear Information System (INIS)

    Ostash, O.P.; Zhmur-Klimenko, V.T.; Yarema, S.Ya.; Yushchenko, K.A.; Strok, L.P.; Belotserkovets, V.I.

    1983-01-01

    Results of further investigations into regularities of development of low-temperature fatigue fracture of welded oints in 07Kh13G20AN4 steel are presented, they are compared with analogous data traditional cryogenic 0Kh18N10T and 03Kh13AG19 steels. Welded joints have been prepared by means of automatic V-like level arc Welding of plates; 0Kh18N10T and 07Kh13G20AN4 steels have been welded by means of sv-04Kh19N9 wire, 03Kh13AG19 steel-by means of sv-07Kh13AG19 wire. Tests at almost zero (asymmetry coefficient R=0.05) cycle of extension at 15-20 Hz frequency have been conducted on 5 mm thick disk samples at 20 deg C and - 160 deg C according to the given methods. It is shown that by cyclic crack resistance of welded joint zones of 0Kh18N10T steel and chromium-manganese steels at normal temperature the 07Kh13G20AN4 steel exceeds 0Kh18N10T steel, at low temperature it yields to 0Kh18N10T only by fracture toughness of heat affected zones HAZ and weld metal (ne). 07Kh13G20AN4 steel and its welded joints as most hardened and cheap may be a good substituent for 0Kh18N10T steel. Optimization of WM alloying for increase of its cyclic fracture toughness at cryogenic temperatures is necessary

  16. Mass spectrometric analysis of helium in stainless steel

    International Nuclear Information System (INIS)

    Isagawa, Hiroto; Wada, Yukio; Asakura, Yoshiro; Tsuji, Nobuo; Sato, Hitoshi; Tsutsumi, Kenichi

    1974-01-01

    Vacuum fusion mass-spectrometry was adopted for the analysis of helium in stainless steel. Samples were heated in a vacuum crucible, and helium in the samples was extracted and collected into a reservoir tank. The gas was then introduced through an orifice into a mass spectrometer, where the amount of helium was determined. The maspeq 070 quadrupole type mass spectrometer made by Shimazu Seisakusho, Ltd. was used. The resolving power was 150, and the mass range of the apparatus was 0-150. The determination limit of helium was about 2 x 10 -3 μg when standard helium gas was analyzed, and was about 10 -2 μg when the helium in stainless steel was analyzed. The relative standard deviation of helium intensity in repetitive measurement was about 2% in the amount of helium of 0.05 μg. Helium was injected into stainless steel by means of alpha particle irradiation with a cyclotron. The amount of helium in stainless steel was then determined. The energy of alpha particles was 34 MeV, and the beam area was 10 mm x 10 mm. The experimental data were higher than the expected value in one case, and were lower in the other case. This difference was attributable to the fluctuation of alpha particle beam, misplacement of sample plates, and unevenness of the alpha beam. (Fukutomi, T.)

  17. Aircraft Steels

    Science.gov (United States)

    2009-02-19

    component usage. PH 13-8Mo is a precipitation-hardenable martensitic stainless steel combining excellent corrosion resistance with strength. Custom 465 is...a martensitic , age-hardenable stainless steel capable of about 1,724 MPa (250 ksi) UTS when peak-aged (H900 condition). Especially, this steel can...NOTES 14. ABSTRACT Five high strength steels (4340, 300M, AerMet 100, Ferrium S53, and Hy-Tuf) and four stainless steels (High Nitrogen, 13

  18. Stainless steels in boiling water reactors. Corrosion problems and possible solutions

    International Nuclear Information System (INIS)

    Combrade, P.; Desestret, A.; Leroy, F.; Coriou, H.

    1977-01-01

    In boiling water reactors, the heat-carrying water may have an up to 0.1 or even 0.2 ppm oxygen content, which can make it highly agressive at operating temperature for stainless steels subject to high physical stresses. Several metallurgical solutions can be considered, and in particular the use of stainless steels having a mixed austenitic-ferritic structure or of standard austenitic steels (18.10 or 18.10 Mo, such as AISI 304 and 316) with carefully controlled carbon and alloy element contents. The behavior of these steels during prolonged tests in water at 288 0 C with a 30 and even 100 ppm oxygen content turned out to be quite satisfactory [fr

  19. Translation of satellite tobacco necrosis virus RNA modified by (not equal to)-r-7,t-8-dihydroxy-t-9,10-epoxy-7,8,9,10-tetrahydrobenzo[a]pyrene is inhibited in a wheat germ cell-free system

    International Nuclear Information System (INIS)

    Haas, R.; Pulkrabek, P.; Takanami, Y.; Grunberger, D.

    1983-01-01

    It has been shown that (not equal to)-r-7-,t-8-dihydroxy-t-9,10-epoxy-7,8,9,10-tetrahydrobenzo[a]pyrene (BPDE) modification of rabbit globin mRNA results in inhibition of translational initiation. In order to explore the possibility that modification of the 5' cap structure was responsible for this inhibition, the naturally non-capped mRNA from satellite tobacco necrosis virus (STNV) was reacted with BPDE and translated in a wheat germ cell-free system. The extent of modification was 1.3 and 2.9 BPDE residues/molecule. High performance liquid chromatography of the modified nucleosides from enzymatically hydrolyzed STNV RNA revealed that greater than 90% of the nucleoside adducts were substituted at the exocyclic amino group of guanosine. The translational ability of the lower and higher modified STNV, measured by incorporation of [ 14 C]amino acids into acid-precipitable polypeptides is inhibited by 55% and 63%, respectively. Polyacrylamide gel electrophoretic analyses of the translation products indicate that predominantly full-length coat proteins are synthesized but with the carcinogen-modified STNV the amount is reduced. On the other hand, 80S initiation complex formation is not inhibited as measured by binding of the BPDE-modified STNV to ribosomes and followed by glycerol gradient centrifugation. Under these conditions, aurintricarboxylic acid completely inhibits 80S initiation complex formation in the presence of either modified or native STNV. These results suggest that inhibition of in vitro translation of BPDE-modified STNV, in contrast to that of globin mRNA, is not at the level of initiation complex formation but possibly by premature termination of growing polypeptides

  20. Steel making

    CERN Document Server

    Chakrabarti, A K

    2014-01-01

    "Steel Making" is designed to give students a strong grounding in the theory and state-of-the-art practice of production of steels. This book is primarily focused to meet the needs of undergraduate metallurgical students and candidates for associate membership examinations of professional bodies (AMIIM, AMIE). Besides, for all engineering professionals working in steel plants who need to understand the basic principles of steel making, the text provides a sound introduction to the subject.Beginning with a brief introduction to the historical perspective and current status of steel making together with the reasons for obsolescence of Bessemer converter and open hearth processes, the book moves on to: elaborate the physiochemical principles involved in steel making; explain the operational principles and practices of the modern processes of primary steel making (LD converter, Q-BOP process, and electric furnace process); provide a summary of the developments in secondary refining of steels; discuss principles a...

  1. The Structure of the Silumin Coat on Alloy Cast Steels

    Directory of Open Access Journals (Sweden)

    T. Szymczak

    2012-04-01

    Full Text Available The work presents the analysis results of the structure of the coat obtained by dipping in silumin AlSi5 of two grades of alloy cast steel: GX6CrNiTi18-10 (LH18N9T and GX39Cr13 (LH14. The temperature of the silumin bath was 750±5°C, and the hold-up time of the cast steel element τ = 180 s. The absolute thickness of the coat obtained in the given conditions was g = 104 μm on cast steel GX6CrNiTi18-10 and g = 132 μm on GX39Cr13. The obtained coat consisted of three layers of different phase structure. The first layer from the base “g1`” was constructed of the phase AlFe including Si and alloy additives of the tested cast steel grades: Cr and Ni (GX6CrNiTi18-10 and Cr (GX39Cr13. The second layer “g1``” of intermetallic phases AlFe which also contains Si and Cr crystallizes on it. The last, external layer “g2” of the coat consists of the silumin containing the intermetallic phases AlFeSi which additionally can contain alloy additives of the cast steel. It was shown that there were no carbides on the coat of the tested cast steels which are the component of their microstructure, as it took place in the case of the coat on the high speed steels.

  2. Reaustenitisation of steels with different initial microstructures

    International Nuclear Information System (INIS)

    Garcia-Caballero, F.; Capdevila, C.; San Martin, D.; Garcia-de Andre, C.

    2004-01-01

    During the last years, physical mathematical models concerning continuous cooling and isothermal phase transformations valid for a wide range of steel have been attained. However, the modelling of continuous heating transformations has not undergone the same development than in cooling. This investigation concerns with the study and Modelization of continuous heating phase transformations to study the process which is generally referred to as austenitisation of the steel. Therefore, our main aim is to describe those processes which control the non-isothermal formation of austenite in steel with initial microstructures of ferrite and/or pearlite. (Author) 10 refs

  3. 78 FR 16252 - Certain Hot-Rolled Carbon Steel Flat Products From India, Indonesia, and Thailand: Final Results...

    Science.gov (United States)

    2013-03-14

    ... Indonesia P.T. Krakatau Steel 10.21 All Others 10.21 Thailand Sahaviriya Steel Industries Public Company...] Certain Hot-Rolled Carbon Steel Flat Products From India, Indonesia, and Thailand: Final Results of... products (``HR steel'') from India, Indonesia, and Thailand pursuant to section 751(c) of the Tariff Act of...

  4. Effect of N+Cr alloying on the microstructures and tensile properties of Hadfield steel

    Energy Technology Data Exchange (ETDEWEB)

    Chen, C. [State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao 066004 (China); Zhang, F.C., E-mail: zfc@ysu.edu.cn [State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao 066004 (China); National Engineering Research Center for Equipment and Technology of Cold Strip Rolling, Yanshan University, Qinhuangdao 066004 (China); Wang, F. [State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao 066004 (China); Liu, H.; Yu, B.D. [China Railway Shanhaiguan Bridge Group Co. LTD, Qinhuangdao 066205 (China)

    2017-01-02

    The microstructures and tensile behaviors of traditional Hadfield steel, named Mn12 steel, and Hadfield steel alloyed with N+Cr, named Mn12CrN steel were studied through optical microscopy, transmission electron microscopy, and scanning electron microscopy, among others. Three different tensile strain rates of 5×10{sup −4}, 5×10{sup −3}, and 5×10{sup −2} s{sup −1} were selected in the tensile test. The deformation microstructures and fracture morphologies of the two steels after fracture in the tensile test were observed to analyze the tensile deformation response to different tensile strain rates. Results showed that the grain size of Mn12CrN steel was evidently refined after alloying with N+Cr. The grain would not become abnormally coarse even with increasing austenitizing temperature. During tensile deformation, the strength and plasticity of Mn12CrN steel were superior to those of Mn12 steel at the same strain rate. With increasing the strain rate, the changes in strength and plasticity of Mn12CrN steel were less sensitive to tensile strain rate compared with Mn12 steel. The effects of grain refinement and N+Cr alloying on dynamic strain aging and deformation twining behaviors were responsible for this lack of sensitivity to strain rate.

  5. Experimental Investigation on Friction and Wear Properties of Different Steel Materials

    OpenAIRE

    M.A. Chowdhury; D.M. Nuruzzaman

    2013-01-01

    Friction coefficient and wear rate of different steel materials are investigated and compared in this study. In order to do so, a pin on disc apparatus is designed and fabricated. Experiments are carried out when different types of disc materials such as stainless steel 314 (SS 314), stainless steel 202 (SS 202) and mild steel slide against stainless steel 314 (SS 314) pin. Experiments are conducted at normal load 10, 15 and 20 N, sliding velocity 1, 1.5 and 2 m/s and relative humidity 70%. A...

  6. Mechanical and wear behaviour of steel chips reinforced Zn27Al composites

    Directory of Open Access Journals (Sweden)

    Kenneth Kanayo ALANEME

    2016-12-01

    Full Text Available The mechanical and wear behaviour of Zn27Al alloy reinforced with steel machining chips (an industrial waste was investigated. Two step stir casting process was used to produce the Zn27Al based composites consisting of 5, 7.5 and 10 wt.% of the steel machining chips while unreinforced Zn27Al alloy and a composition consisting of 5 wt.% alumina were also prepared as control samples. Microstrutural analysis; mechanical and wear behaviour were assessed for these composites. The results show that the hardness and wear resistance of the composites increased with increase in weight percent of the steel chips from 5 to 10 wt.%. The UTS, strain to fracture, and the fracture toughness were however highest for the 5 wt.% steel chips reinforced composite grade; and decreased with increase in the weight percent of the steel chips from 5 to 10 wt.%. Generally the Zn27Al alloy based composites reinforced with steel machining chips, exhibited superior mechanical and wear properties in comparison to the unreinforced Zn27Al alloy and the 5 wt.% alumina reinforced Zn27Al alloy composite.

  7. Mechanical properties of irradiated 9Cr-2WVTa steel

    International Nuclear Information System (INIS)

    Klueh, R.L.; Alexander, D.J.; Rieth, M.

    1998-01-01

    An Fe-9Cr-2W-0.25V-0.07Ta-0.1C (9Cr-2WVTa) steel has excellent strength and impact toughness before and after irradiation in the Fast Flux Test Facility and the High Flux Reactor (HFR). The ductile-brittle transition temperature (DBTT) increased only 32 C after 28 dpa at 365 C in FFTF, compared to a shift of ∼60 C for a 9Cr-2WV steel--the same as the 9Cr-2WVTa steel but without tantalum. This difference occurred despite the two steels having similar tensile but without tantalum. This difference occurred despite the two steels having similar tensile properties before and after irradiation. The 9Cr-2WVTa steel has a smaller prior-austenite grain size, but otherwise microstructures are similar before irradiation and show similar changes during irradiation. The irradiation behavior of the 9Cr-2WVTa steel differs from the 9Cr-2WV steel and other similar steels in two ways: (1) the shift in DBTT of the 9Cr-2WVTa steel irradiated in FFTF does not saturate with fluence by ∼28 dpa, whereas for the 9Cr-2WV steel and most similar steels, saturation occurs at <10 dpa, and (2) the shift in DBTT for 9Cr-2WVTa steel irradiated in FFTF and HFR increased with irradiation temperature, whereas it decreased for the 9Cr-2WV steel, as it does for most similar steels. The improved properties of the 9Cr-2WVTa steel and the differences with other steels were attributed to tantalum in solution

  8. Reaction of uranium and plutonium carbides with austenitic steels

    International Nuclear Information System (INIS)

    Mouchnino, M.

    1967-01-01

    The reaction of uranium and plutonium carbides with austenitic steels has been studied between 650 and 1050 deg. C using UC, steel and (UPu)C, steel diffusion couples. The steels are of the type CN 18.10 with or without addition of molybdenum. The carbides used are hyper-stoichiometric. Tests were also carried out with UCTi, UCMo, UPuCTi and UPuCMo. Up to 800 deg. C no marked diffusion of carbon into stainless steel is observed. Between 800 and 900 deg. C the carbon produced by the decomposition of the higher carbides diffuses into the steel. Above 900 deg. C, decomposition of the monocarbide occurs according to a reaction which can be written schematically as: (U,PuC) + (Fe,Ni,Cr) → (U,Pu) Fe 2 + Cr 23 C 6 . Above 950 deg. C the behaviour of UPuCMo and that of the titanium (CN 18.12) and nickel (NC 38. 18) steels is observed to be very satisfactory. (author) [fr

  9. Effect of nitrogen alloying of stainless steels on their corrosion stability

    International Nuclear Information System (INIS)

    Chigal, V.; Knyazheva, V.M.; Pitter, Ya.; Babich, S.G.; Bogolyubskij, S.D.

    1986-01-01

    Results of corrosion tests and structural investigations of 03Cr18Ni10 and 03Cr18Ni10Mo3 steels without nitrogen and with nitrogen content of 0.15-0.3% are presented. Corrosion-electrochemical behaviour of Cr20Ni20 steel with ultralow carbon content (0.004-0.006%) and nitrogen content with 0-0.5% as well as Cr 2 N nitride behaviour are investigated. A conclusion is made on nitrogen and excessive nitride phase effect on corrosion stability of steel in corrosive media with different reduction-oxidation properties

  10. Steel for nuclear applications

    International Nuclear Information System (INIS)

    Zorev, N.N.; Astafiev, A.A.; Loboda, A.S.

    1978-01-01

    A steel contains, in percent by weight, the following constituents: carbon from 0.13 to 0.18, silicon from 0.17 to 0.37, manganese from 0.30 to 0.60, chromium from 1.7 to 2.4, nickel from 1.0 to 1.5, molybdenum from 0.5 to 0.7, vanadium from 0.05 to 0.12, aluminium from 0.01 to 0.035, nitrogen from 0.05 to 0.012, copper from 0.11 to 0.20, arsenic from 0.0035 to 0.0055, iron and impurities, the balance. This steel is preferable for use in the manufacture of nuclear reactors. 1 table

  11. Corrosion behavior of steels in liquid lead bismuth with low oxygen concentrations

    Science.gov (United States)

    Kurata, Yuji; Futakawa, Masatoshi; Saito, Shigeru

    2008-02-01

    Corrosion tests in pots were conducted to elucidate corrosion behavior of various steels in liquid lead-bismuth for 3000 h under the condition of an oxygen concentration of 5 × 10 -8 wt% at 450 °C and an oxygen concentration of 3 × 10 -9 wt% at 550 °C, respectively. Significant corrosion was not observed at 450 °C for ferritic/martensitic steels, F82H, Mod.9Cr-1Mo steel, 410SS, 430SS except 2.25Cr-1Mo steel. Pb-Bi penetration into steels and dissolution of elements into Pb-Bi were severe at 550 °C even for ferritic/martensitic steels. Typical dissolution attack occurred for pure iron both at 550 °C without surface Fe 3O 4 and at 450 °C with a thin Fe 3O 4 film. Ferritization due to dissolution of Ni and Cr, and Pb-Bi penetration were recognized for austenitic stainless steels, 316SS and 14Cr-16Ni-2Mo steel at both temperatures of 450 °C and 550 °C. The phenomena were mitigated for 18Cr-20Ni-5Si steel. In some cases oxide films could not be a corrosion barrier in liquid lead-bismuth.

  12. Annealing effect on restoration of irradiation steel properties

    International Nuclear Information System (INIS)

    Vishkarev, O.M.; Kolesova, T.N.; Myasnikova, K.P.; Pecherin, A.M.; Shamardin, V.K.

    1986-01-01

    The effect of temperature and annealing time on the restoration of properties of the 15Kh2NMFAA and 15Kh2MFA steels after irradiation at 285 deg with the fluence of 6x10 23 neutr/m 2 (E>0.5 MeV) is studied. Microhardness (H μ ) restoration in the irradiated 15Kh2NMFAA steel is shown to start from 350 deg C annealing temperature. The complete microhardness restoration is observed at the annealing temperature of 500 deg C for 10 hours

  13. A two-stage constitutive model of X12CrMoWVNbN10-1-1 steel during elevated temperature

    Science.gov (United States)

    Zhu, Luobei; He, Jianli; Zhang, Ying

    2018-02-01

    In order to clarify the competition between work hardening (WH) caused by dislocation movements and the dynamic softening result from dynamic recovery (DRV) and dynamic recrystallization (DRX), a new two-stage flow stress model of X12CrMoWVNbN10-1-1 (X12) ferrite heat-resistant steel was established to describe the whole hot deformation behavior. And the parameters were determined by the experimental data operated on a Gleeble-3800 thermo- mechanical simulation. In this constitutive model, a single internal variable dislocation density evolution model is used to describe the influence of WH and DRV to flow stress. The DRX kinetic dynamic model can express accurately the contribution of DRX to the decline of flow stress, which was established on the Avrami equation. Furthermore, The established new model was compared with Fields-Bachofen (F-B) model and experimental data. The results indicate the new two-stage flow stress model can more accurately represent the hot deformation behavior of X12 ferrite heat-resistant steel, and the average error is only 0.0995.

  14. Anomaly in the dynamic strength of austenitic stainless steel 12Cr19Ni10Ti under shock wave loading

    Science.gov (United States)

    Garkushin, G. V.; Kanel, G. I.; Razorenov, S. V.; Savinykh, A. S.

    2017-07-01

    Measurement results for the shock wave compression profiles of 12Cr19Ni10Ti steel and its dynamic strength in the strain rate range 105-106 s-1 are presented. The protracted viscous character of the spall fracture is revealed. With the previously obtained data taken into account, the measurement results are described by a polynomial relation, which can be used to construct the fracture kinetics. On the lower boundary of the range, the resistance to spall fracture is close to the value of the true strength of the material under standard low-rate strain conditions; on the upper boundary, the spall strength is more than twice greater than this quantity. An increase in the temperature results in a decrease in both the dynamic limit of elasticity and the spall fracture strength of steel. The most interesting result is the anomaly in the dependence of the spall fracture strength on the duration of the shock wave compression pulse, which is related to the formation of deformation martensite near the growing discontinuities.

  15. Kinetics of atmospheric corrosion of mild steel, zinc, galvanized iron and aluminium at 10 exposure stations in India

    International Nuclear Information System (INIS)

    Natesan, M.; Venkatachari, G.; Palaniswamy, N.

    2006-01-01

    As a part of updating Corrosion Map of India project, atmospheric corrosion behaviour of commercially available engineering materials such as mild steel, galvanized iron, zinc and aluminium metals was studied in marine, industrial, urban, and rural environments by weight loss method at 10 exposure stations in India over a period of 5 years. The results of these studies demonstrated that galvanized iron, zinc and aluminium metals were several times more durable than mild steel. Compared to galvanized iron and zinc, aluminium provided superior protection in industrial and marine environment except at Mormugao Port Trust (MPT). It also offered much better resistance to corrosion in rural environments. At certain places, galvanized iron proved to be more durable than aluminium. The results obeyed well with the empirical kinetics equation of the form C = Kt n , where K and C are the corrosion losses in μm after 1 and 't' years of the exposure, respectively, and 'n' is a constant. Based on 'n' values, the corrosion mechanisms of these metals are predicted. The corrosion products formed on the metal samples in Chennai marine atmosphere were identified by X-ray diffraction analysis

  16. X-ray diffraction study of slags forming during corrosion resistant steel production

    International Nuclear Information System (INIS)

    Slavov, V.I.; Zadorozhnaya, V.N.; Shurygina, A.V.

    1990-01-01

    Using X-ray diffraction analysis slags, forming during corrosion-resistant 12Kh18N10T grade steel production by two flowsheets, are studied. Standard two-slag technology of steel production does not provide efficient disintegration of chromospinelides in slags, gives high steel contamination with respect to nonmetallic impurities, coarse structure and, as a consequence, presence of macrodefects on rolled products surface. One-slag steel melting technology with titanium alloying of the steel at vacuum causes fast removal of chromospinelides at the beginning of reduction period, promotes titanium absorption by the steel, refines nonmetallic inclusions, provides more fine structure and steel plasticity, removes surface defects

  17. 78 FR 25422 - Antidumping or Countervailing Duty Order, Finding, or Suspended Investigation; Advance...

    Science.gov (United States)

    2013-05-01

    ... China (A-570-910) (1st 482-5047. Review). Carbon and Certain Alloy Steel Wire Rod from Jennifer Moats... Jennifer Moats (202) Mexico (A-201-830) (2nd Review). 482-5047. Carbon and Certain Alloy Steel Wire Rod... of China (C-570-911) (1st 482-4136. Review). [[Page 25423

  18. Effect of welding thermal cycles on the structure and properties of simulated heat-affected zone areas in X10CrMoVNb9-1 (T91) steel at a state after 100,000 h of operation

    Energy Technology Data Exchange (ETDEWEB)

    Łomozik, Mirosław, E-mail: miroslaw.lomozik@is.gliwice.pl [Instytut Spawalnictwa, Testing of Materials Weldability and Welded Constructions Department, 44-100 Gliwice, Bł. Czesława 16-18 (Poland); Hernas, Adam, E-mail: adam.hernas@polsl.pl [Silesian University of Technology, Faculty of Materials Engineering and Metallurgy, 40-019 Katowice, Krasińskiego 8 str. (Poland); Zeman, Marian L., E-mail: marian.zeman@is.gliwice.pl [Instytut Spawalnictwa, Testing of Materials Weldability and Welded Constructions Department, 44-100 Gliwice, Bł. Czesława 16-18 (Poland)

    2015-06-18

    The article presents results of structural tests (light, scanning electron and scanning transmission electron microscopy) of X10CrMoVNb9-1 (T91) creep-resisting steel after approximately 100,000 h of operation. It was ascertained that the parent metal of T91 steel is characterized by the microstructure of tempered martensite with M{sub 23}C{sub 6} carbide precipitates and few dispersive precipitates of MX-type niobium and vanadium carbonitrides. The most inconvenient change in T91 steel precipitate morphology due to long-term operation is the appearance of the Laves Fe{sub 2}Mo phase which along with M{sub 23}C{sub 6} carbide particles forms elongated blocks and conglomerates on grain boundaries. The article also presents results of tests related to the effect of simulated welding thermal cycles on selected properties of X10CrMoVNb9-1 (T91) grade steel at a state after approximately 100,000 h of operation. The tests involved the determination of the chemical composition of the steel tested as well as impact tests, hardness measurements and microscopic metallographic examination (based on light microscopy) of simulated heat-affected zone (HAZ) areas for a cooling time (t{sub 8/5}) restricted within a range between 3 s and 120 s, with and without heat treatment. The tests revealed that, among other results, hardness values of simulated HAZ areas in X10CrMoVNb9-1 (T91) steel do not guarantee cold crack safety of the steel at the state without additional heat treatment. It was also observed that simulated welding thermal cycles of cooling times t{sub 8/5}=3, 12, 60 and 120 s do not significantly affect the toughness and hardness of simulated HAZ areas of the steel tested.

  19. Modeling irradiation embrittlement in reactor pressure vessel steels

    International Nuclear Information System (INIS)

    Odette, G.R.

    1998-01-01

    As a result of the popularity of the Agencies report 'Neutron Irradiation Embrittlement of Reactor Pressure Vessel Steels' of 1975, it was decided that another report on this broad subject would be of use. In this report, background and contemporary views on specially identified areas of the subject are considered as self-contained chapters, written by experts. In chapter 10, numerical modeling of irradiation embrittlement in reactor vessel steels are introduced. Physically-based models are developed and their role in advancing the state-of-the-art of predicting irradiation embrittlement of RPV steels is stressed

  20. Radiation induced microstructural evolution in ferritic/martensitic steels

    International Nuclear Information System (INIS)

    Kohno, Y.; Kohyama, A.; Asakura, K.; Gelles, D.S.

    1993-01-01

    R and D of ferritic/martensitic steels as structural materials for fusion reactor is one of the most important issues of fusion technology. The efforts to characterize microstructural evolution under irradiation in the conventional Fe-Cr-Mo steels as well as newly developed Fe-Cr-Mn or Fe-Cr-W low activation ferritic/ martensitic steels have been continued. This paper provides some of the recent results of heavy irradiation effects on the microstructural evolution of ferritic/martensitic steels neutron irradiated in the FFTF/MOTA (Fast Flux Test Facility/Materials Open Test Assembly). Materials examined are Fe-10Cr-2Mo dual phase steel (JFMS: Japanese Ferritic/Martensitic Steel), Fe-12Cr-XMn-1Mo manganese stabilized martensitic steels and Fe-8Cr-2W Tungsten stabilized low activation martensitic steel (F82H). JFMS showed excellent void swelling resistance similar to 12Cr martensitic steel such as HT-9, while the manganese stabilized steels and F82H showed less void swelling resistance with small amount of void swelling at 640-700 K (F82H: 0.14% at 678 K). As for irradiation response of precipitate behavior, significant formation of intermetallic χ phase was observed in the manganese stabilized steels along grain boundaries which is though to cause mechanical property degradation. On the other hand, precipitates identified were the same type as those in unirradiated condition in F82H with no recognition of irradiation induced precipitates, which suggested satisfactory mechanical properties of F82H after the irradiation. (author)

  1. Apo-10'-lycopenoic acid inhibits cancer cell migration and angiogenesis and induces peroxisome proliferator-activated receptor gamma

    Science.gov (United States)

    Scope: We have previously shown that apo-10'-lycopenoic acid (ALA), a derivative of lycopene through cleavage by carotene-9',10'-oxygenase, inhibits tumor progression and metastasis in both liver and lung cancer animal models. The underlying mechanism remains unknown. We hypothesized that ALA inhibi...

  2. Steel corrosion in tributyl phosphate in the presence of water and ethyl mercaptan

    International Nuclear Information System (INIS)

    Pischik, L.M.; Tsinman, A.I.

    1979-01-01

    Studied is the corrosion of steels St3, 15Kh5M, 08Kh13, 10Kh14G14N4T, 08Kh18G8N2T, 10Kh17N13M2T in TBP, in mixtures of TBP with ethyl mercaptan (EM) and two-phase systems TBP-water and TBP-water-EM at 50-150 deg. In pure TBP St3 corrosion rate is low even at 150 deg. In the presence of water St 3 strongly corrodes at above 50 deg temperature in organic and water layers and also in gas phase. The steel-08Kh18G8N2T at 90 deg in acid TBP is passive and its corrosion rate is lower than 0.01 mm/year. In identical conditions the resistance of stainless steels increases together with chromium content but in TBP with acid number 100 and above at 150 deg all tested steels including steel-10Kh17N13M2T are slightly resistant. Thus, even in absence of corrosion active additions of EM the mixture of TBP-water at higher temperature is agressive in relation not only to carbon steel but also to stainless steels

  3. Hot Ductility Behaviors in the Weld Heat-Affected Zone of Nitrogen-Alloyed Fe-18Cr-10Mn Austenitic Stainless Steels

    Science.gov (United States)

    Moon, Joonoh; Lee, Tae-Ho; Hong, Hyun-Uk

    2015-04-01

    Hot ductility behaviors in the weld heat-affected zone (HAZ) of nitrogen-alloyed Fe-18Cr-10Mn austenitic stainless steels with different nitrogen contents were evaluated through hot tension tests using Gleeble simulator. The results of Gleeble simulations indicated that hot ductility in the HAZs deteriorated due to the formation of δ-ferrite and intergranular Cr2N particles. In addition, the amount of hot ductility degradation was strongly affected by the fraction of δ-ferrite.

  4. Research and tests of steel-concrete-steel sandwich composite shear wall in reactor containment of HTR-PM

    International Nuclear Information System (INIS)

    Sun Yunlun; Huang Wen; Zhang Ran; Zhang Pei; Tian Chunyu

    2014-01-01

    By quasi-static test of 8 specimens of steel-concrete-steel sandwich composite shear wall, the bearing capacity, hysteretic behavior, failure mode of the specimens was studied. So was the effect of the shear-span ratios, steel ratios and spacing of studs on the properties of the specimens. The failure patterns of all specimens with different shear-span ratios between 1.0 and 1.5 were compression-bending failure. The hysteretic curves of all specimens were relatively plump, which validated the well deformability and energy dissipation capacity of the specimens. When shear-span ratio less than 1.5, the shear property of the steel plate was well played, and so was the deformability of the specimens. The bigger the steel ratio was, the better the lateral resistance capacity and the deformability was. Among the spacing of studs in the test, the spacing of studs had no significant effect on the bearing capacity, deformability and ductility of the specimens. Based on the principle of superposition an advised formula for the compression-bending capacity of the shear wall was proposed, which fitted well with the test result and had a proper safety margin. (author)

  5. Effect of helium ion bombardment on hydrogen behaviour in stainless steel

    International Nuclear Information System (INIS)

    Guseva, M.I.; Stolyarova, V.G.; Gorbatov, E.A.

    1987-01-01

    The effect of helium ion bombardment on hydrogen behaviour in 12Kh18N10T stainless steel is investigated. Helium and hydrogen ion bombardment was conducted in the ILU-3 ion accelerator; the fluence and energy made up 10 16 -5x10 17 cm -2 , 30 keV and 10 16 -5x10 18 cm -2 , 10 keV respectively. The method of recoil nuclei was used for determination of helium and hydrogen content. Successive implantation of helium and hydrogen ions into 12Kh18N10T stainless steel results in hydrogen capture by defects formed by helium ions

  6. A review of temperature measurement in the steel reheat furnace

    International Nuclear Information System (INIS)

    Martocci, A.P.; Mihalow, F.A.

    1985-01-01

    The incentive for conducting research and development on reheat furnaces is substantial; the domestic steel industry spent approximately one billion dollars on fuel in reheat furnaces in 1981. Bethlehem Steel Corp. spent /145 million of that total, and neither figure includes fuel consumed in soaking pits or annealing furnaces. If the authors set a goal to save 10% of these annual fuel costs, that translates into /100 million for the domestic steel industry and /14.5 million for Bethlehem Steel. These large sums of money are significant incentives. The purpose of this paper is to review the historical heating practices and equipment at steel reheat furnaces along with current practices and instrumentation

  7. Academic Training Lectures | The Art of Way Finding | 9-10 December

    CERN Multimedia

    2015-01-01

    Please note that the next series of Academic Training Lectures will take place on 9 and 10 December. The lectures will be given by John Huth (Harvard University (US)).   The Art of Way Finding (1/2) on Wednesday, 9 December from 11 a.m. to 12 p.m. https://indico.cern.ch/event/436443/ The Art of Way Finding (2/2) on Thursday, 10 December from 11 a.m. to 12 p.m. http://indico.cern.ch/event/436444/ at CERN, Council Chamber (503-1-001)  Description: In the modern era we've become accustomed to the instantaneous transfer of information filtered by applications that act as a kind of guardian of information. In the realm of finding one’s way, we use GPS and devices that take us from point A to point B without giving it a second thought. Are we slowly losing the cognitive processes that our ancestors had, and at what price? I use the theme of navi...

  8. Research of Technological Properties of Steel X6CRNITI18-10 Welded Joints Exploited in Nitric Acid Medium

    Directory of Open Access Journals (Sweden)

    Gediminas Mikalauskas

    2016-04-01

    Full Text Available The repair of chemical industry equipments often requires to replace long time operated pipes or welded inserts with the simi-lar chemical composition. During the study the joints from corro-sion resistant steel X6CrNiTi18-10 were welded by manual metal arc welding with covered electrodes (MMA process 111 and tungsten inert gas welding (TIG process 141 at different welding parameters. The visual, radiographic, penetrant control and ferrite content analysis were carried out. The transverse tensile and bending samples were produced from welded samples; also the macroscopic and microscopic analyse were carried out.

  9. Apparent embrittlement saturation and radiation mechanisms of reactor pressure vessel steels

    International Nuclear Information System (INIS)

    Pachur, D.

    1981-01-01

    The irradiation and annealing results of three different reactor pressure vessel steels are reported. Steel A, a basic material according to ASTM A-533 B having 0.15 percent vanadium; and Steel C contained 3.2 percent nickel. The steels were irradiated at 150, 300, and 400 degree C with neutron fluxes of 6 multiplied by 10 11 and 3 multiplied by 10 13 neutrons (n)/cm 2 /s. An apparent saturation-in-irradiation effect was found within certain neutron fluence ranges. During the annealing, various recovery processes occur in different temperature ranges. These are characterized by various activation energies. The individual processes were determined by the different time dependencies at various temperatures. Two causes for the apparent saturation were discovered from the behavior of the annealing curves

  10. Work-hardening of dual-phase steel

    Energy Technology Data Exchange (ETDEWEB)

    Rieger, Florian

    2016-07-01

    Exhibiting good mechanical properties for cold-sheet forming, low-alloyed dual-phase (DP) steels are nowadays widely used for automotive applications. The composite-like microstructure of DP steels is composed of a low-carbon ductile ferrite-matrix and 10 - 60 vol.% hard martensitic inclusions. A nonlinear mean-field model and full-field finite-element simulations are applied to investigate three major topics: the influence of grain-size distribution, grain-level plasticity and derivation of an original material-model. The plastic behavior of polycrystals is assumed to be grain-size dependent in this work. The distribution of grain-sizes is taken to be lognormal. It is found that grain-size dispersion leads to a decrease of the material strength, in particular for small mean diameters around one micron. The numerical results from the mean-field model are confirmed notably well by means of a simple analytical expression. The micromechanical behavior of DP steels is investigated by full-field RVE simulations with a crystal-plasticity based ferrite-matrix and von Mises-type martensite inclusions. To examine the martensite influence, full-field simulation results of DP steels have been compared to an RVE in which martensite is substituted by ferrite. After quenching, a higher grain-boundary area covered by martensite facilitates an increased average dislocation-density. For uniaxial deformations above ∝10%, however, the grain-size dependent relation reverses. With more surrounding martensite, the local crystal-plasticity material-model exhibits hardening at a slower rate. A nonlinear mean-field model of Hashin-Shtrikman type is employed as framework for the original material-model for DP steels. The model incorporates the interaction of ferrite and martensite via incompatibility-induced long-range stresses in an averaged sense. The proposed model combines works of Ashby (1970) and Brown and Stobbs (1971a) to simulate the ferrite behavior. Based on the composite model

  11. Improving composition of protective coatings for steel casting

    International Nuclear Information System (INIS)

    Kuz'kina, N.N.; Pegov, V.G.; Bogatenkov, V.F.; Shub, L.G.; Raspopova, N.A.

    1983-01-01

    A radically new fuel-free slag-forming mixture used as protective coating for steel casting is introduced. The lack of combustible powders precludes explosion and fire Lazard in mixture preparation. Usage of the new mixture in stainless steel casting of Kh18N10T type permitted to improve the ingot surface quality and reduce spoilage from 1.16 to 0.66%

  12. APT characterization of high nickel RPV steels

    International Nuclear Information System (INIS)

    Miller, M.K.; Russell, K.F

    2004-01-01

    Full text: The microstructures of several high nickel content pressure vessel steels have been characterized by atom probe tomography. The purposes of this study were to investigate the influence of high nickel levels on the response to neutron irradiation of high and low copper pressure vessel steels and to establish whether any additional phases were present after neutron irradiation. The nickel levels in these steels were at least twice that typically found in Western pressure vessel steels. Two different types of pressure vessel steels with low and high copper contents were selected for this study. The first set of alloys was low copper (∼0.05% Cu) base (15Ch2NMFAA) and weld (12Ch2N2MAA) materials used in a VVER-1000 reactor. The composition of the lower nickel VVER-1000 base material was Fe- 0.17 wt% C, 0.30% Si, 0.46% Mn, 2.2% Cr, 1.26% Ni, 0.05% Cu, 0.01% S, 0.008% P, 0.10% V and 0.50% Mo. The composition of the higher nickel VVER-1000 weld material was Fe- 0.06 wt % C, 0.33% Si, 0.80% Mn, 1.8% Cr, 1.78% Ni, 0.07% Cu, 0.009% S, 0.005% P, and 0.63% Mo. The VVER-1000 steels were irradiated in the HSSI Program's irradiation facilities at the University of Michigan, Ford Nuclear Reactor at a temperature of 288 o C for 2,137 h at an average flux of 7.08 x 10 11 cm 2 s -1 for a fluence of 5.45 x 10 18 n cm -2 (E >1 MeV) and for 5,340 h at an average flux of 4.33 x 10 11 cm -2 s -1 for a fluence of 8.32 x 10 1 28 n cm -2 (E >1 MeV). Therefore, the total fluence was 1.38 x 10 19 n cm -2 (E >1 MeV). The second type of pressure vessel steel was a high copper (0.20% Cu) weld from the Palisades reactor. The average composition of the Palisades weld was Fe- 0.11 wt% C, 0.18% Si, 1.27% Mn, 0.04% Cr, 1.20% Ni, 0.20% Cu, 0.017% S, 0.014% P, 0.003% V and 0.55% Mn. The Palisades weld, designated weldment 'B' from weld heat 34B009, was irradiated at a temperature of 288 o C and a flux of ∼7 x 10 11 cm -2 s -1 to a fast fluence of 1.4 x 10 19 n cm -2 (E >1 MeV). These three

  13. Doubly coherent production of π- by 3He ions of 910 MeV

    International Nuclear Information System (INIS)

    Aslanides, E.; Fassnacht, P.; Hibou, F.; Chiavassa, E.; Dellacasa, G.; Gallio, M.; Musso, A.; Bressani, T.; Puddu, G.

    1979-01-01

    The inclusive pion spectrum from the reaction 3 He+ 6 Li → π - +X at 910 MeV was measured at 0 0 with moderate resolution up to the kinematic limit of the two-body final-state reaction. A first analysis shows that the production of high-energy pions cannot be explained by the NN → NNπ process using conventional nucleon momentum distributions. At the end of the spectrum a clear deviation from the general falloff slope is observed and attributed to the doubly coherent reaction 3 He+ 6 Li → 9 C+π -

  14. 46 CFR 42.09-30 - Additional survey requirements for steel-hull vessels.

    Science.gov (United States)

    2010-10-01

    ... 46 Shipping 2 2010-10-01 2010-10-01 false Additional survey requirements for steel-hull vessels...-30 Additional survey requirements for steel-hull vessels. (a) In addition to the requirements in § 42...) When the vessel is in drydock, the hull plating, etc., shall be examined. (c) The holds, 'tween decks...

  15. Elevated temperature mechanical properties of line pipe steels

    Science.gov (United States)

    Jacobs, Taylor Roth

    The effects of test temperature on the tensile properties of four line pipe steels were evaluated. The four materials include a ferrite-pearlite line pipe steel with a yield strength specification of 359 MPa (52 ksi) and three 485 MPa (70 ksi) yield strength acicular ferrite line pipe steels. Deformation behavior, ductility, strength, strain hardening rate, strain rate sensitivity, and fracture behavior were characterized at room temperature and in the temperature range of 200--350 °C, the potential operating range for steels used in oil production by the steam assisted gravity drainage process. Elevated temperature tensile testing was conducted on commercially produced as-received plates at engineering strain rates of 1.67 x 10 -4, 8.33 x 10-4, and 1.67 x 10-3 s-1. The acicular ferrite (X70) line pipe steels were also tested at elevated temperatures after aging at 200, 275, and 350 °C for 100 h under a tensile load of 419 MPa. The presence of serrated yielding depended on temperature and strain rate, and the upper bound of the temperature range where serrated yielding was observed was independent of microstructure between the ferrite-pearlite (X52) steel and the X70 steels. Serrated yielding was observed at intermediate temperatures and continuous plastic deformation was observed at room temperature and high temperatures. All steels exhibited a minimum in ductility as a function of temperature at testing conditions where serrated yielding was observed. At the higher temperatures (>275 °C) the X52 steel exhibited an increase in ductility with an increase in temperature and the X70 steels exhibited a maximum in ductility as a function of temperature. All steels exhibited a maximum in flow strength and average strain hardening rate as a function of temperature. The X52 steel exhibited maxima in flow strength and average strain hardening rate at lower temperatures than observed for the X70 steels. For all steels, the temperature where the maximum in both flow

  16. Effect of Explosion Bulge Test Parameters on the Measurement of Deformation Resistance for Steel

    Science.gov (United States)

    2014-02-01

    solidification cracking in steels and stainless steels . He has also undertaken extensive work on improving the weld zone toughness of high strength steels ...Chatterjee and H. Bhadeshia, ‘TRIP-assisted steels : cracking of high carbon martensite ’, Journal of Materials Science and Technology, 2006, 22, pp. 645...649. [10] S. Chaatterjee and H.K.D.H. Bhadeshia, ‘Transformation induced plasticity assisted steels : stress or strain affected martensitic

  17. Residual stress relief in MAG welded joints of dissimilar steels

    International Nuclear Information System (INIS)

    Seodek, P.; Brozda, J.; Wang, L.; Withers, P.J.

    2003-01-01

    This paper addresses the relief of residual stress in welded joints between austenitic and non-alloyed ferritic-pearlitic steels. A series of similar and dissimilar steel joints based on the 18G2A (ferritic-pearlitic) and 1H18N10T (austenitic) steels were produced, some of which were stress relieved by annealing and some by mechanical prestressing. For the as-welded and stress relieved test joints the residual stresses were measured by trepanning. To aid the interpretation of these results, 2D plane stress finite element analysis has been performed to simulate the residual stress relieving methods. Analysis of the results has shown that thermal stress relieving of welded joints between dissimilar steels is not effective and may even increase residual stresses, due to the considerable difference in thermal expansion of the joined steels. It was found that, for the loads imposed, the effectiveness of the mechanical stress relieving of dissimilar steel welded joints was much lower than that of similar steel joints

  18. Stainless steels for cryogenic bolts and nuts

    International Nuclear Information System (INIS)

    Leroy, F.; Rabbe, P.; Odin, G.

    1975-01-01

    Stainless steel for cryogenic applications are generally austenitic steels which, under the effect of cold-drawing, can or cannot undergo a partial martensitic transformation according to their composition. It has been shown that very high ductility and endurance characteristics at low temperatures, together with very high yield strength and resistances values, can be attained with grades of nitrogenous steels of types Z2CN18-10N and Z3CMN18-8-6N. Optimum ductility values are obtained by employing to the best possible, the martensitic transformations which develop during cold-drawing. From the plotting of the rational traction curves, it is possible to analyse very simply the influence of the composition on the martensitic transformations [fr

  19. Mapping the global flow of steel: from steelmaking to end-use goods.

    Science.gov (United States)

    Cullen, Jonathan M; Allwood, Julian M; Bambach, Margarita D

    2012-12-18

    Our society is addicted to steel. Global demand for steel has risen to 1.4 billion tonnes a year and is set to at least double by 2050, while the steel industry generates nearly a 10th of the world's energy related CO₂ emissions. Meeting our 2050 climate change targets would require a 75% reduction in CO₂ emissions for every tonne of steel produced and finding credible solutions is proving a challenge. The starting point for understanding the environmental impacts of steel production is to accurately map the global steel supply chain and identify the biggest steel flows where actions can be directed to deliver the largest impact. In this paper we present a map of global steel, which for the first time traces steel flows from steelmaking, through casting, forming, and rolling, to the fabrication of final goods. The diagram reveals the relative scale of steel flows and shows where efforts to improve energy and material efficiency should be focused.

  20. Microstructure and tensile properties of yttrium nitride dispersion-strengthened 14Cr–3W ferritic steels

    Energy Technology Data Exchange (ETDEWEB)

    Huang, Liqing [State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083 (China); School of Mechanical and Mining Engineering, University of Queensland, Brisbane 4067, QLD (Australia); Liu, Zuming, E-mail: lzm@csu.edu.cn [State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083 (China); Chen, Shiqi; Guo, Yang [State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083 (China)

    2015-12-15

    Highlights: • Innovative nano yttrium nitride dispersion strengthened steels were fabricated. • Higher content of additives accelerate the steel-ceramic powder milling process more. • Steel with high content (3%) of YN dispersoids can obtain good performance at 500 °C. - Abstract: 14Cr–3W ferritic steel powders were mechanically milled with microscale yttrium nitride (YN) particles to fabricate particle dispersion-strengthened ferritic steels. After hot consolidation and annealing, the steel matrix was homogeneously dispersed with nano-scale YN particles. The steel containing 0.3 wt.% YN particles exhibited a yield strength of 1445 MPa at room temperature. Its total elongation was 10.3%, and the fracture surface exhibited mixed ductile and quasi-cleavage fracture morphologies. The steel with a much higher content of YN particles (3 wt.%) in its matrix was much stronger (1652 MPa) at room temperature at the cost of ductility. In particular, it exhibited a high yield strength (1350 MPa) with applicable ductility (total elongation > 10%) at 500 °C. This study has developed a new kind of reinforcement particle to fabricate high-performance ferritic steels.

  1. Investigation of alteration behaviour of compacted bentonite contracted with carbon steel for 10 years

    International Nuclear Information System (INIS)

    Suyama, Tadahiro; Ueno, Kenichi; Sasamoto, Hiroshi

    2008-03-01

    To evaluate long term behavior of corrosion for carbon steel in compacted bentonite, and to evaluate long term stability of bentonite, corrosion experiments were conducted using synthetic sea water and synthetic groundwater at 50 and 80degC for 10 years under anaerobic atmosphere. In the present study, the samples of compacted bentonite after experiments were investigated to understand the alteration behavior of bentonite by iron-bentonite interactions. Results were summarized below. Iron generated by corrosion of carbon steel was migrated into compacted bentonite further in the synthetic seawater case than in the synthetic groundwater case. Result of TEM observation for the sample of synthetic sea water case at 80degC showed that the original layer structure for clay minerals was maintained and the layer distance was about 12[A] which was similar to the layer distance of normal 2:1 smectite. Thus, it was suggested that there was no change in smectite before and after experiments. Iron generated by corrosion of carbon steel was migrated into compacted bentonite in anaerobic condition case but scarcely migrated in aerobic condition case. Results of EPMA analysis indicated that the maximum migration depth of iron in compacted bentonite was about 0.2 mm for sample in synthetic sea water at 80degC under anaerobic condition. Results of XRD analysis for the sample in which iron migration in compacted bentonite was observed showed that there was no corrosion product in compacted bentonite and the structure of clay mineral in bentonite was di-octahedral. Furthermore, the result of XRD analysis under relative humidity controlled condition suggested that the swelling property of sample after experiment was similar to that of initial Na-type smectite. Therefore, it was supposed that the initial Na-type smectite did not change during the experiment. Batch type experiments with different temperature, solutions and duration have been conducted to understand the alteration

  2. European development of ferritic-martensitic steels for fast reactor wrapper applications

    International Nuclear Information System (INIS)

    Bagley, K.; Little, E.A.; Levy, V.; Alamo, A.

    1987-01-01

    9-12%Cr ferritic-martensitic stainless steels are under development in Europe for fast reactor sub-assembly wrapper applications. Within this class of alloys, attention is focussed on three key specifications, viz. FV448 and DIN 1.4914 (both 10-12%CrMoVNb steels) and EM10 (an 8-10%Cr-0.15%C steel), which can be optimized to give acceptably low ductile-brittle transition characteristics. The results of studies on these steels, and earlier choices, covering heat treatment and compositional optimization, evolution of wrapper fabrication routes, pre and post-irradiation mechanical property and fracture toughness behaviour, microstructural stability, void swelling and in-reactor creep characteristics are reviewed. The retention of high void swelling to displacement doses in excess of 100 dpa in reactor irradiations reaffirms the selection of 9-12%Cr steels for on-going wrapper development. Moreover, irradiation-induced changes in mechanical properties (e.g. in-reactor creep and impact behaviour), measured to intermediate doses, do not give cause for concern; however, additional data to higher doses and at the lower irradiation temperatures of 370 0 -400 0 C are needed in order to fully endorse these alloys for high burnup applications in advanced reactor systems

  3. Effects of DK-002, a synthesized (6aS,cis)-9,10-Dimethoxy-7,11b-dihydro-indeno[2,1-c]chromene-3,6a-diol, on platelet activity.

    Science.gov (United States)

    Lee, Ki-Seon; Khil, Lee-Yong; Chae, Sang-Ho; Kim, Deukjoon; Lee, Byung-Hoon; Hwang, Gwi-Seo; Moon, Chang-Hyun; Chang, Tong-Shin; Moon, Chang-Kiu

    2006-02-02

    In the present study, the mechanism of antiplatelet activity of DK-002, a synthesized (6aS,cis)-9,10-Dimethoxy-7,11b-dihydro-indeno[2,1-c]chromene-3,6a-diol, was investigated. DK-002 inhibited the thrombin, collagen, and ADP-induced rat platelet aggregation in a concentration-dependent manner, with IC50 values of 120, 27, and 47 microM, respectively. DK-002 also inhibited thrombin-induced dense granule secretion, thromboxane A2 synthesis, and [Ca2+]i elevation in platelets. DK-002 did not show any significant effect on ADP-induced inhibition of cyclic AMP elevation by prostaglandin E1, but DK-002 was confirmed to inhibit ADP-induced [Ca2+]i elevation and shape change. DK-002 inhibited 4-bromo-A23187-induced [Ca2+]i elevation in the presence of creatine phosphate/creatine phosphokinase (CP/CPK, a ADP scavenging system) and indomethacin (a specific inhibitor of cyclooxygenase). DK-002 also inhibited Ca2+ mobilization in thrombin- or 4-bromo-A23187-stimulated platelets through its inhibitory effects on both Ca2+ release from intracellular stores and Ca2+ influx, in the presence of CP/CPK and indomethacin. Taken together, the present study shows that DK-002 has inhibitory effects on stimulation of platelets, and suggests that its antiplatelet activity might be related to the inhibitory mechanism on Ca2+ mobilization in stimulated platelets.

  4. Investigation of hot ductility in Al-killed boron steels

    International Nuclear Information System (INIS)

    Chown, L.H.; Cornish, L.A.

    2008-01-01

    The influence of boron to nitrogen ratio, strain rate and cooling rate on hot ductility of aluminium-killed, low carbon, boron microalloyed steel was investigated. Hot tensile testing was performed on steel samples reheated in argon to 1300 deg. C, cooled at rates of 0.3, 1.2 and 3.0 deg. C s -1 to temperatures in the range 750-1050 deg. C, and then strained to failure at initial strain rates of 1 x 10 -4 or 1 x 10 -3 s -1 . It was found that the steel with a B:N ratio of 0.19 showed deep hot ductility troughs for all tested conditions; the steel with a B:N ratio of 0.47 showed a deep ductility trough for a high cooling rate of 3.0 deg. C s -1 and the steel with a near-stoichiometric B:N ratio of 0.75 showed no ductility troughs for the tested conditions. The ductility troughs extended from ∼900 deg. C (near the Ae 3 temperature) to ∼1000 or 1050 deg. C in the single-phase austenite region. The proposed mechanism of hot ductility improvement with increase in B:N ratio in these steels is that the B removes N from solution, thus reducing the strain-induced precipitation of AlN. Additionally, BN co-precipitates with sulphides, preventing precipitation of fine MnS, CuS and FeS, and forming large, complex precipitates that have no effect on hot ductility

  5. The Study on Weldability of Boron Steel and Hot-Stamped Steel by Using Laser Heat Source (Ⅲ) - Comparison on Laser Weldability of Boron Steel and Hot -Stamped Steel-

    Energy Technology Data Exchange (ETDEWEB)

    Choi, So Young; Kim, Jong Do [Korea Maritime and Ocean University, Busan (Korea, Republic of); Kim, Jong Su [Korea Institute of Machinery and Materials, Daejeon (Korea, Republic of)

    2015-01-15

    This study was conducted to compare the laser weldability of boron steel and hot-stamped steel. In general, boron steel is used in the hot-stamping process. Hot-stamping is a method for simultaneously forming and cooling boron steel in a press die after heating it to the austenitizing temperature. Hot-stamped steel has a strength of 1500 MPa or more. Thus, in this study, the laser weldability of boron steel and that of hot-stamped steel were investigated and compared. A continuous wave disk laser was used to produce butt and lap joints. In the butt welding, the critical cooling speed at which full penetration was obtained in the hot-stamped steel was lower than that of boron steel. In the lap welding, the joint widths were similar regardless of the welding speed when full penetration was obtained.

  6. The Study on Weldability of Boron Steel and Hot-Stamped Steel by Using Laser Heat Source (Ⅲ) - Comparison on Laser Weldability of Boron Steel and Hot -Stamped Steel-

    International Nuclear Information System (INIS)

    Choi, So Young; Kim, Jong Do; Kim, Jong Su

    2015-01-01

    This study was conducted to compare the laser weldability of boron steel and hot-stamped steel. In general, boron steel is used in the hot-stamping process. Hot-stamping is a method for simultaneously forming and cooling boron steel in a press die after heating it to the austenitizing temperature. Hot-stamped steel has a strength of 1500 MPa or more. Thus, in this study, the laser weldability of boron steel and that of hot-stamped steel were investigated and compared. A continuous wave disk laser was used to produce butt and lap joints. In the butt welding, the critical cooling speed at which full penetration was obtained in the hot-stamped steel was lower than that of boron steel. In the lap welding, the joint widths were similar regardless of the welding speed when full penetration was obtained

  7. The crack growth resistance of thin steel sheets under eccentric ...

    Indian Academy of Sciences (India)

    Ľ AMBRIŠKO

    2018-03-10

    Mar 10, 2018 ... of zinc-coated automotive steel sheets (IF – deep drawing interstitial free steel ..... to determine; therefore, the Ji was determined for observ- able crack initiation .... M R S, da Silva L F M and de Castro P M S T 2011. Analysis of ...

  8. 12C(3He,3He n)11C cross section at 910 MeV

    International Nuclear Information System (INIS)

    Aslanides, E.; Fassnacht, P.; Dellacasa, G.; Gallio, M.; Tuyn, J.W.N.

    1981-01-01

    The 12 C( 3 He, 3 He n) 11 C cross section at 910 MeV was measured by using a Ge(Li) gamma spectrometer to determine the disintegration rate and measuring the incident flux by means of a scintillator telescope. Cross sections for the production of 7 Be in C and Al and for the production of 24 Na in Al are then determined using the measured cross section as a monitor

  9. Atom-Probe Tomographic Investigation of Austenite Stability and Carbide Precipitation in a TRIP-Assisted 10 Wt Pct Ni Steel and Its Weld Heat-Affected Zones

    Science.gov (United States)

    Jain, Divya; Seidman, David N.; Barrick, Erin J.; DuPont, John N.

    2018-04-01

    Newly developed low-carbon 10 wt pct Ni-Mo-Cr-V martensitic steels rely on the Ni-enriched, thermally stable austenite [formed via multistep intercritical Quench-Lamellarization-Tempering ( QLT)-treatment] for their superior mechanical properties, specifically ballistic resistance. Critical to the thermal stability of austenite is its composition, which can be severely affected in the weld heat-affected zones (HAZs) and thus needs investigations. This article represents the first study of the nanoscale redistributions of C, Ni, and Mn in single-pass HAZ microstructures of QLT-treated 10 wt pct Ni steels. Local compositions of Ni-rich regions (representative of austenite compositions) in the HAZs are determined using site-specific 3-D atom-probe tomography (APT). Martensite-start temperatures are then calculated for these compositions, employing the Ghosh-Olson thermodynamic and kinetics approach. These calculations predict that austenite (present at high temperatures) in the HAZs is susceptible to a martensitic transformation upon cooling to room temperature, unlike the austenite in the QLT-treated base-metal. While C in the QLT-treated base-metal is consumed primarily in MC and M2C-type carbide precipitates (M is Mo, Cr, V), its higher concentration in the Ni-rich regions in the HAZs indicates the dissolution of carbide precipitates, particularly M2C carbide precipitates. The role of M2C carbide precipitates and austenite stability is discussed in relation to the increase in microhardness values observed in the HAZs, relative to the QLT-treated base-metal. Insights gained from this research on austenite stability and carbide precipitation in the single-pass HAZ microstructures will assist in designing multiple weld cycles for these novel 10 wt pct Ni steels.

  10. Pitting Corrosion Susceptibility of AISI 301 Stainless Steel in ...

    African Journals Online (AJOL)

    The susceptibility of austenitic (AISI 301) stainless steel to pitting corrosion was evaluated in sodium chloride (NaCl) solutions - 0.1M, 0.2M, 0.3M, 0.5M and 0.7M and 1.0M. Tensile tests and microscopic examinations were performed on samples prepared from the steel after exposure in the various environments.

  11. Hydrogen trapping energy levels and hydrogen diffusion at high and low strain rates (~10{sup 5} s{sup −1} and 10{sup −7} s{sup −1}) in lean duplex stainless steel

    Energy Technology Data Exchange (ETDEWEB)

    Silverstein, R., E-mail: barrav@post.bgu.ac.il; Eliezer, D.

    2016-09-30

    Duplex stainless steels (DSS) alloys are high strength steels combined with ductility and excellent resistance to stress corrosion cracking, which makes them attractive for the pressure vessels or underwater pipelines industries. Hydrogen embrittlement (HE) is caused by the action of hydrogen in combination with residual or applied stress and can lead to the mechanical degradation of a material. Dynamic and quasi-static experiments were conducted at room temperature and strain rates of 10{sup 5} s{sup −1} and 10{sup −7} s{sup −1} on gas-phase hydrogen charged DSS. Hydrogen trapping in the various defects and its effect on the mechanical properties are discussed in details. A linear model of Lee and Lee was applied to calculate the trap activation energies. It was found that lower strain rates (~10{sup −7} s{sup −1}) will create less deep hydrogen trapping energies values; ~40% lower than in non-loaded sample. In addition, higher dynamic pressure will create higher trapping energy sites for hydrogen. Based on our experimental studies we developed an analytical model for hydrogen trapping. We have found that the strain rate has a direct influence on both hydrogen diffusion and hydrogen potential trapping sites. During deformation processes created at low strain rates (~10{sup −7} s{sup −1}) hydrogen has enough time to migrate with dislocations from deeper potential trapping sites to lower potential trapping sites.

  12. Connections: Superplasticity, Damascus Steels, Laminated Steels, and Carbon Dating

    Science.gov (United States)

    Wadsworth, Jeffrey

    2016-12-01

    In this paper, a description is given of the connections that evolved from the initial development of a family of superplastic plain carbon steels that came to be known as Ultra-High Carbon Steels (UHCS). It was observed that their very high carbon contents were similar, if not identical, to those of Damascus steels. There followed a series of attempts to rediscover how the famous patterns found on Damascus steels blades were formed. At the same time, in order to improve the toughness at room temperature of the newly-developed UHCS, laminated composites were made of alternating layers of UHCS and mild steel (and subsequently other steels and other metals). This led to a study of ancient laminated composites, the motives for their manufacture, and the plausibility of some of the claims relating to the number of layers in the final blades. One apparently ancient laminated composite, recovered in 1837 from the great pyramid of Giza which was constructed in about 2750 B.C., stimulated a carbon dating study of ancient steels. The modern interest in "Bladesmithing" has connections back to many of these ancient weapons.

  13. 1,5-Diamido-9,10-anthraquinone, a Centrosymmetric Redox-Active Bridge with Two Coupled β-Ketiminato Chelate Functions: Symmetric and Asymmetric Diruthenium Complexes.

    Science.gov (United States)

    Ansari, Mohd Asif; Mandal, Abhishek; Paretzki, Alexa; Beyer, Katharina; Fiedler, Jan; Kaim, Wolfgang; Lahiri, Goutam Kumar

    2016-06-06

    The dinuclear complexes {(μ-H2L)[Ru(bpy)2]2}(ClO4)2 ([3](ClO4)2), {(μ-H2L)[Ru(pap)2]2}(ClO4)2 ([4](ClO4)2), and the asymmetric [(bpy)2Ru(μ-H2L)Ru(pap)2](ClO4)2 ([5](ClO4)2) were synthesized via the mononuclear species [Ru(H3L)(bpy)2]ClO4 ([1]ClO4) and [Ru(H3L)(pap)2]ClO4 ([2]ClO4), where H4L is the centrosymmetric 1,5-diamino-9,10-anthraquinone, bpy is 2,2'-bipyridine, and pap is 2-phenylazopyridine. Electrochemistry of the structurally characterized [1]ClO4, [2]ClO4, [3](ClO4)2, [4](ClO4)2, and [5](ClO4)2 reveals multistep oxidation and reduction processes, which were analyzed by electron paramagnetic resonance (EPR) of paramagnetic intermediates and by UV-vis-NIR spectro-electrochemistry. With support by time-dependent density functional theory (DFT) calculations the redox processes could be assigned. Significant results include the dimetal/bridging ligand mixed spin distribution in 3(3+) versus largely bridge-centered spin in 4(3+)-a result of the presence of Ru(II)-stabilizig pap coligands. In addition to the metal/ligand alternative for electron transfer and spin location, the dinuclear systems allow for the observation of ligand/ligand and metal/metal site differentiation within the multistep redox series. DFT-supported EPR and NIR absorption spectroscopy of the latter case revealed class II mixed-valence behavior of the oxidized asymmetric system 5(3+) with about equal contributions from a radical bridge formulation. In comparison to the analogues with the deprotonated 1,4-diaminoanthraquinone isomer the centrosymmetric H2L(2-) bridge shows anodically shifted redox potentials and weaker electronic coupling between the chelate sites.

  14. Surface modification of hydroturbine steel using friction stir processing

    Science.gov (United States)

    Grewal, H. S.; Arora, H. S.; Singh, H.; Agrawal, A.

    2013-03-01

    Friction stir processing (FSP) has proved to be a viable tool for enhancing the mechanical properties of materials, however, the major focus has been upon improving the bulk properties of light metals and their alloys. Hydroturbines are susceptible to damage owing to slurry and cavitation erosion. In this study, FSP of a commonly employed hydroturbine steel, 13Cr4Ni was undertaken. Microstructural characterization of the processed steel was conducted using optical microscopy (OM), scanning electron microscopy (SEM) equipped with energy dispersive spectroscopy (EDS), X-ray diffraction (XRD) and electron back scatter diffraction (EBSD) techniques. Mechanical characterization of the steel was undertaken in terms of microhardness and resistance to cavitation erosion (CE). FSP resulted in the refinement of the microstructure with reduction in grain size by a factor of 10. EBSD results confirmed the existence of submicron and ultrafine grained microstructure. The microhardness of the steel was found to enhance by 2.6 times after processing. The processed steel also showed 2.4 times higher resistance against cavitation erosion in comparison to unprocessed steel. The primary erosion mechanism for both the steels was identical in nature, with plastic deformation responsible for the loss of material.

  15. Quest for steel quality: the role of metallurgical chemistry

    Energy Technology Data Exchange (ETDEWEB)

    McLean, A. [Toronto Univ., ON (Canada). Dept. of Metallurgy and Materials Science

    2000-10-01

    Improvements in the quality of steels and the role played by metallurgical chemistry to bring about those improvements are discussed. The particular emphasis is on the chemical behaviour of solutes in molten steel and the reaction between steel, slag and refractory materials and the manner in which they influence the physical properties and performance of the steel product. As an illustration of the contribution of chemistry to steel making the case of the steel plates used in the construction of the Titanic is cited. In 1911 when the Titanic was constructed by Harland and Wolff at their Belfast shipyard, the steel plates used in the hull met all then current specifications. In 1992 when a number of steel samples recovered from the Titanic were examined, it was found that the hull of the vessel was constructed of low carbon, semi-killed steel, produced in the open-hearth process. Microstructural analysis showed extensive carbon banding, typical of hot rolled 0.2 per cent carbon steel. Also found were long manganese sulphide inclusions elongated in the rolling direction, some of which exceeded 25 mm in length. It was determined that as a consequence of these inclusions, at a seawater temperature of 0 degree C, the hull plates of the Titanic had essentially no resistance to fracture. Today's high quality steels used in applications such as Arctic pipelines, offshore platforms, icebreakers and ships for the transportation of natural gas, oxygen and sulphur concentrations are frequently less than 10 ppm. These elements have a profound influence of the quality of the final steel products by virtue of their effect of hindering the formation of inclusions. 2 refs., 3 figs.

  16. Modification of steel surface by plasma electrolytic saturation with nitrogen and carbon

    Energy Technology Data Exchange (ETDEWEB)

    Kusmanov, S.A., E-mail: sakusmanov@yandex.ru; Kusmanova, Yu.V., E-mail: yulia.kusmanova@yandex.ru; Smirnov, A.A., E-mail: sciencealexsm@gmail.com; Belkin, P.N., E-mail: belkinp@yandex.ru

    2016-06-01

    The effect of the electrolyte composition with ammonia, acetone, and ammonium chloride on the structure and properties of low carbon steel was studied in anode plasma electrolytic nitrocarburising. An X-ray diffractometer, a scanning electron microscopy (SEM) and an optical microscope were used to characterize the phase composition of the modified layer and its surface morphology. Surface roughness was studied with a profilometer–profilograph. The hardness of the treated and untreated samples was measured using a microhardness tester. The sources of nitrogen and carbon are shown to be the products of evaporation and thermal decomposition of the electrolyte components. It is established that the influence of concentration of ammonia, acetone, and ammonium chloride on the size of the structural components of the hardened layer is explained by the competition of the anode dissolution, high-temperature oxidation and diffusion of the saturating component. The electrolyte composition (10–12.5% ammonium chloride, 5% acetone, 5% ammonia) and processing mode (800 °C, 5–10 min) of low carbon steels allowing to obtain the hardened surface layer up to 0.2 mm with microhardness 930 HV and with decrease in the roughness (R{sub a}) from 1.013 to 0.054 μm are proposed. The anode plasma electrolytic nitricarburising is able to decrease friction coefficient of the treated low carbon steel from 0.191 to 0.169 and wear rate from 13.5 mg to 1.0 mg. - Highlights: • Aqueous solution (12.5% NH{sub 4}Cl, 5% ammonia, 5% acetone) is proposed for PEN/C steels. • Microhardness of steel (0.2% C) is 930 HV due to PEN/C for 5–10 min at 800 °C. • Anode PEN/C of low carbon steel decreases its roughness (R{sub a}) from 1.013 to 0.054 μm. • Anode PEN/C decreases friction coefficient of low carbon steel from 0.191 to 0.169 • Anode PEN/C decreases wear loss of low carbon steel from 13.5 mg to 1.0 mg.

  17. Current status of stainless steel industry and development of stainless steel

    International Nuclear Information System (INIS)

    Lee, Yong Deuk; Lee, Chan Soo; Kim Kwang Tae

    2000-01-01

    Stainless steel is not only clean and smooth in its surface, but also it is superior in quality in terms of corrosion resistance and strength. So that, it is widely in use in the field of construction, chemical installations, and other industries. Growth of stainless steel industry started since the steel technology was developed for mass production in 1960s. Since then stainless steel industry grew rapidly on account of diversified development in this field and growth rate went up to 5.8% per year comparable to 2.3% of steel growth. The rapid growth is attributed to significant industry developments in Europe and Japan in the years of 1970s and 1980s. In addition to these the expansion of stainless steel industry in Korea and Taiwan. Presently Korea produces about 120,000 tons of stainless steel and occupies about 8% of international market. This means Korea become the second largest single country in world in stainless steel production. Moreover Korea is to reinforce its domestic production line by affiliating production companies, increasing of production capability, and specializing in types of stainless steel. This paper is to describe activity of material development, and types of stainless steel for industry use. (Hong, J. S.)

  18. Energy and materials flows in the iron and steel industry

    Energy Technology Data Exchange (ETDEWEB)

    Sparrow, F.T.

    1983-06-01

    Past energy-consumption trends and future energy-conservation opportunities are investigated for the nation's iron and steel industry. It is estimated that, in 1980, the industry directly consumed approximately 2.46 x 10/sup 15/ Btu of energy (roughly 3% of total US energy consumption) to produce 111 million tons of raw steel and to ship 84 million tons of steel products. Direct plus indirect consumption is estimated to be about 3.1 x 10/sup 15/ Btu. Of the set of conservation technologies identified, most are judged to be ready for commercialization if and when the industry's capital formation and profitability problems are solved and the gradual predicted increase in energy prices reduces the payback periods to acceptable levels.

  19. Outlook of the world steel cycle based on the stock and flow dynamics.

    Science.gov (United States)

    Hatayama, Hiroki; Daigo, Ichiro; Matsuno, Yasunari; Adachi, Yoshihiro

    2010-08-15

    We present a comprehensive analysis of steel use in the future compiled using dynamic material flow analysis (MFA). A dynamic MFA for 42 countries depicted the global in-use stock and flow up to the end of 2005. On the basis of the transition of steel stock for 2005, the growth of future steel stock was then estimated considering the economic growth for every country. Future steel demand was estimated using dynamic analysis under the new concept of "stocks drive flows". The significant results follow. World steel stock reached 12.7 billion t in 2005, and has doubled in the last 25 years. The world stock in 2005 mainly consisted of construction (60%) and vehicles (10%). Stock in these end uses will reach 55 billion t in 2050, driven by a 10-fold increase in Asia. Steel demand will reach 1.8 billion t in 2025, then slightly decrease, and rise again by replacement of buildings. The forecast of demand clearly represents the industrial shift; at first the increase is dominated by construction, and then, after 2025, demand for construction decreases and demand for vehicles increases instead. This study thus provides the dynamic mechanism of steel stock and flow toward the future, which contributes to the design of sustainable steel use.

  20. Wear properties of metal ion implanted 4140 steel

    International Nuclear Information System (INIS)

    Evans, P.J.; Paoloni, F.J.

    1994-01-01

    AISI type 4140 (high tensile) steel has been implanted with tungsten and titanium using a metal vapour vacuum arc ion source. Doses in the range (1-5)x10 16 ionscm -2 were implanted to a depth of approximately 30nm. The relative wear resistance between non-implanted and implanted specimens has been estimated using pin-on-disc and abrasive wear tests. Implantation of titanium decreased the area of wear tracks by a factor of 5 over unimplanted steel. In some cases the steel was also hardened by a liquid carburization treatment before implantation. Abrasion tests revealed a further improvement in wear resistance on this material following ion irradiation. ((orig.))

  1. Dislocation structures in cyclically strained X10CrAl24 ferritic steel

    Czech Academy of Sciences Publication Activity Database

    Petrenec, Martin; Polák, Jaroslav; Obrtlík, Karel; Man, Jiří

    2006-01-01

    Roč. 54, č. 13 (2006), s. 3429-3443 ISSN 1359-6454. [Micromechanics and Microstructure Evolution : Modeling Simulation and Experiments. Madrid, 11.09.2005-16.09.2006] R&D Projects: GA ČR(CZ) GP106/05/P521 Institutional research plan: CEZ:AV0Z20410507 Keywords : Transmission electron microscopy * Ferritic steel * Fatigue Subject RIV: JL - Materials Fatigue, Friction Mechanics Impact factor: 3.549, year: 2006

  2. Non-destructive automated express method for determining the inclination of chromium-nickel steels IGC

    International Nuclear Information System (INIS)

    Nazarov, A.A.; Kamenev, Yu.B.; Kuusk, L.V.; Kormin, E.G.; Vasil'ev, A.N.; Sumbaeva, T.E.

    1986-01-01

    Methods of automated control of 18-10-type steel inclination to IGC are developed and a corresponding automated testing complex (ATS) is created. 08Kh18N10T steel samples had two variants of thermal treatment: 1) 1200 deg (5 h), 600 deg (50 h); 2) 1200 deg (5 h). Methods of non-destructive automated control of 18-10-type steel inclination to IGC are developed on the basis of potentiodynamic reactivation (PR) principle. Automated testing complex is developed, which has undergone experimental running and demonstrated a high confidence of results, reliability and easy operation

  3. Johnson - Cook Strength Models for Mild and DP 590 Steels

    International Nuclear Information System (INIS)

    Vedantam, K.; Brar, N. S.; Bajaj, D.; Hill, S.

    2006-01-01

    Automotive steels, Mild and Dual Phase590 (DP590) are characterized in tension at room temperature, using the quasi-static and split Hopkinson bar techniques at various strain rates ranging from ∼10-3/s to ∼1800/s. Tension stress-strain data for both the steels are analyzed to determine the Johnson-Cook Strength model constants, J-C strength model constants for mild steel are A=217 MPa, B = 234 MPa, n = 0.643 and C = 0.076 and for DP590 steel are A = 430 MPa, B = 824 MPa, n = 0.510 and C = 0.017. Higher value of strain rate sensitivity constant C for mild steel (0.076) compared to DP 590 (0.017) is also reflected in the stress- strain data at various strain rates

  4. Strengthening Hadfield steel welds by nitrogen alloying

    International Nuclear Information System (INIS)

    Efstathiou, C.; Sehitoglu, H.

    2009-01-01

    Strengthening Hadfield steel weld repairs by introducing nitrogen into the weld region was proven to be feasible via two welding techniques. The first technique required a pure Hadfield steel filler material to be diffusion treated in a high pressure nitrogen gas environment, and subsequently used during tungsten inert gas welding with a pure argon shielding gas. The second technique used a Hadfield steel filler material, and a 10% nitrogen containing argon shielding gas during tungsten inert gas welding. Both techniques increased the yield strength, the hardening rate, and the ultimate strength of the weld region. Using optical microscopy, scanning electron microscopy, and Auger spectroscopy, we determined that the increased strength of the weld region resulted from a combination of nitrogen alloying and microstructural refinement

  5. Thermally Stable Ni-rich Austenite Formed Utilizing Multistep Intercritical Heat Treatment in a Low-Carbon 10 Wt Pct Ni Martensitic Steel

    Science.gov (United States)

    Jain, Divya; Isheim, Dieter; Zhang, Xian J.; Ghosh, Gautam; Seidman, David N.

    2017-08-01

    Austenite reversion and its thermal stability attained during the transformation is key to enhanced toughness and blast resistance in transformation-induced-plasticity martensitic steels. We demonstrate that the thermal stability of Ni-stabilized austenite and kinetics of the transformation can be controlled by forming Ni-rich regions in proximity of pre-existing (retained) austenite. Atom probe tomography (APT) in conjunction with thermodynamic and kinetic modeling elucidates the role of Ni-rich regions in enhancing growth kinetics of thermally stable austenite, formed utilizing a multistep intercritical ( Quench- Lamellarization- Tempering (QLT)-type) heat treatment for a low-carbon 10 wt pct Ni steel. Direct evidence of austenite formation is provided by dilatometry, and the volume fraction is quantified by synchrotron X-ray diffraction. The results indicate the growth of nm-thick austenite layers during the second intercritical tempering treatment (T-step) at 863 K (590 °C), with austenite retained from first intercritical treatment (L-step) at 923 K (650 °C) acting as a nucleation template. For the first time, the thermal stability of austenite is quantified with respect to its compositional evolution during the multistep intercritical treatment of these steels. Austenite compositions measured by APT are used in combination with the thermodynamic and kinetic approach formulated by Ghosh and Olson to assess thermal stability and predict the martensite-start temperature. This approach is particularly useful as empirical relations cannot be extrapolated for the highly Ni-enriched austenite investigated in the present study.

  6. Structural transformations in austenitic stainless steel induced by deuterium implantation: irradiation at 100 K.

    Science.gov (United States)

    Morozov, Oleksandr; Zhurba, Volodymyr; Neklyudov, Ivan; Mats, Oleksandr; Rud, Aleksandr; Chernyak, Nikolay; Progolaieva, Viktoria

    2015-01-01

    Deuterium thermal desorption spectra were investigated on the samples of austenitic stainless steel 18Cr10NiTi preimplanted at 100 K with deuterium ions in the dose range from 3 × 10(15) to 5 × 10(18) D/cm(2). The kinetics of structural transformation development in the implantation steel layer was traced from deuterium thermodesorption spectra as a function of implanted deuterium concentration. At saturation of austenitic stainless steel 18Cr10NiTi with deuterium by means of ion implantation, structural-phase changes take place, depending on the dose of implanted deuterium. The maximum attainable concentration of deuterium in steel is C = 1 (at.D/at.met. = 1/1). The increase in the implanted dose of deuterium is accompanied by the increase in the retained deuterium content, and as soon as the deuterium concentration attains C ≈ 0.5 the process of shear martensitic structural transformation in steel takes place. It includes the formation of bands, body-centered cubic (bcc) crystal structure, and the ferromagnetic phase. Upon reaching the deuterium concentration C > 0.5, the presence of these molecules causes shear martensitic structural transformations in the steel, which include the formation of characteristic bands, bcc crystal structure, and the ferromagnetic phase. At C ≥ 0.5, two hydride phases are formed in the steel, the decay temperatures of which are 240 and 275 K. The hydride phases are formed in the bcc structure resulting from the martensitic structural transformation in steel.

  7. The structure of the alphinizing coat on alloy steels

    Directory of Open Access Journals (Sweden)

    S. Pietrowski

    2008-12-01

    Full Text Available In this paper results of the structure of the coat alphinizing in AlSi5 silumin on alloy steels: acid-proof 1H18N9T (X6CrNiTi18-10 and high speed SW18 (HS18-0-1 were presented. The temperature of the alphinizing bath was amounts to750±5°C, and immersion time of the element τ = 180s. It was shown, that there is the different “g” coat thickness on testing steels. On the 1H18N9T steel it amounts to g = 52μm, and on the SW18 steel – g = 203μm. Regardless of a grade of testing alloy steels the coat consist of three layers with diversified phasic structure. There is different chemical composition of coat layers on testing steels. The first layer from the base consist of AlFe phase containing alloy addictions of steels: Cr and Ni (1H18N9T and W, V and Cr (SW18. On this layer crystallize the second layer of intermetallic phases. It is the phase containing the main alloy addiction of steels: AlFeCr (1H18N9T and AlFeW (SW18. The last, outside layer consist of silumin containing AlFeNi intermetallic phases on the 1H18N9T steel and AlFeW on the SW18 steel. Regardless of the grade of testing steels there is Si element in all layers of the coat. There are morphological differences in tested layers. The second layer (AlFeW phase inside the coat on the SW18 steel consist of faced crystals growing into in outside silumin layer. On the 1H18N9T steel a boundary between transient and outside layer is more uniform. Free separations of intermetallic phases inside silumin layer on the 1H18N9T steel have lamellar and on the SW18 steel – faced form.

  8. Ratcheting deformation of advanced 316 steel under creep-plasticity condition

    Energy Technology Data Exchange (ETDEWEB)

    Kawashima, Fumiko; Ishikawa, Akiyoshi; Asada, Yasuhide [Tokai Univ., Tokyo (Japan). Dept. of Mechanical Engineering

    1998-11-01

    Tension-torsion biaxial ratcheting tests have been conducted with Advanced 316 Steel (316FR Steel) at 650 C under a cyclic strain rate of 10{sup -3} to 10{sup -5} s{sup -1}. Accumulation of ratcheting strain has been measured. Accumulated ratchet strain has shown to be much larger than predicted based on a usual method of the linear superposition of strains due to creep and plasticity. The result shows there observed the creep-plasticity interaction in the observation. (orig.)

  9. Influence of shock induced polymorphic transition on penetration in steel

    International Nuclear Information System (INIS)

    Hereil, P.L.; Fanget, A.

    1994-01-01

    The effects of polymorphic transition for the impact of a 27NCD10 steel projectile on a 27NCD10 steel target at 1280 m/s is presented. Comparisons between results of 2D numerical calculations performed with and without polymorphic transition show the influence of this phenomenon on stress distribution and tension zones in the target and in the projectile. Good agreement between experimental and calculated free surface velocity profiles is obtained with polymorphic transition and damage models taken into account. (orig.)

  10. Corrosion of stainless steels in lead-bismuth eutectic up to 600 °C

    Science.gov (United States)

    Soler, L.; Martín, F. J.; Hernández, F.; Gómez-Briceño, D.

    2004-11-01

    An experimental program has been carried out to understand the differences in the corrosion behaviour between different stainless steels: the austenitic steels 304L and 316L, the martensitic steels F82Hmod, T91 and EM10, and the low alloy steel P22. The influence of oxygen level in Pb-Bi, temperature and exposure time is studied. At 600 °C, the martensitic steels and the P22 steel exhibit thick oxide scales that grow with time, following a linear law for the wet environment and a parabolic law for the dry one. The austenitic stainless steels show a better corrosion behaviour, especially AISI 304L. Under reducing conditions, the steels exhibit dissolution, more severe for the austenitic stainless steels. At 450 °C, all the materials show an acceptable behaviour provided a sufficient oxygen level in the Pb-Bi. At reducing conditions, the martensitic steels and the P22 steel have a good corrosion resistance, while the austenitic steels exhibit already dissolution at the longer exposures.

  11. Corrosion of stainless steels in lead-bismuth eutectic up to 600 deg. C

    International Nuclear Information System (INIS)

    Soler, L.; Martin, F.J.; Hernandez, F.; Gomez-Briceno, D.

    2004-01-01

    An experimental program has been carried out to understand the differences in the corrosion behaviour between different stainless steels: the austenitic steels 304L and 316L, the martensitic steels F82Hmod, T91 and EM10, and the low alloy steel P22. The influence of oxygen level in Pb-Bi, temperature and exposure time is studied. At 600 deg. C, the martensitic steels and the P22 steel exhibit thick oxide scales that grow with time, following a linear law for the wet environment and a parabolic law for the dry one. The austenitic stainless steels show a better corrosion behaviour, especially AISI 304L. Under reducing conditions, the steels exhibit dissolution, more severe for the austenitic stainless steels. At 450 deg. C, all the materials show an acceptable behaviour provided a sufficient oxygen level in the Pb-Bi. At reducing conditions, the martensitic steels and the P22 steel have a good corrosion resistance, while the austenitic steels exhibit already dissolution at the longer exposures

  12. [Factors influencing electrocardiogram results in workers exposed to noise in steel-making and steel-rolling workshops of an iron and steel plant].

    Science.gov (United States)

    Li, Y H; Yu, S F; Gu, G Z; Chen, G S; Zhou, W H; Wu, H; Jiao, J

    2016-02-20

    To investigate the factors influencing the electrocardiogram results in the workers exposed to noise in steel-making and steel rolling workshops of an iron and steel plant. From September to December, 2013, cluster sampling was used to select 3 150 workers exposed to noise in the steel-making and steel-rolling workshops of an iron and steel plant, and a questionnaire survey and physical examinations were performed. The number of valid workers was 2 915, consisting of 1 606 workers in the steel-rolling workshop and 1 309 in the steel-making workshop. The electrocardiogram results of the workers in steel-making and steel-rolling workshops were analyzed. The overall abnormal rate of electrocardiogram was 26.35%, and the workers in the steel-making workshop had a significantly higher abnormal rate of electrocardiogram than those in the steel-rolling workshop(32.24% vs 21.54%, Pelectrocardiogram than female workers(27.59% vs 18.61%, Pelectrocardiogram than those who did not drink(28.17% vs 23.75%, Pelectrocardiogram than those who were not exposed to high temperature(29.43% vs 20.14%, Pelectrocardiogram in the workers with cumulative noise exposure levels of electrocardiogram results. High cumulative noise exposure, alcohol consumption, and high temperature may affect the abnormal rate of electrocardiogram in the workers exposed to noise in steel-making and steel-rolling workshops.

  13. 75 FR 36678 - Prestressed Concrete Steel Wire Strand From China; Determinations

    Science.gov (United States)

    2010-06-28

    ... prestressed concrete steel wire strand (PC strand), provided for in subheading 7312.10.30 of the Harmonized... Publication 4162 (June 2010), entitled Prestressed Concrete Steel Wire Strand from China: Investigation Nos... INTERNATIONAL TRADE COMMISSION [Investigation Nos. 701-TA-464 and 731-TA-1160 (Final)] Prestressed...

  14. Compactibility of atomized high-speed steel and steel 3 powders

    International Nuclear Information System (INIS)

    Kulak, L.D.; Gavrilenko, A.P.; Pikozh, A.P.; Kuz'menko, N.N.

    1985-01-01

    Spherical powders and powders of lammellar-scaly shape of high-speed R6M5K5 steel and steel 3 produced by the method of centrifugal atomization of a rotating billet under conditions of cold pressing in steel moulds are studied for thier compactability. Compacting pressure dependnences are establsihed for density of cold-pressed compacts of spherical and scaly powders. The powders of lammellar-scaly shape both of high-speed steel and steel 3 are found to possess better compactibility within a wide range of pressures as compared to powders of spherical shape. Compacts of the lammellar-scaly powders possess also higher mechanical strength

  15. Identification of Precipitates in Cr-Mn-N Based Steel After Thermal Exposures

    Directory of Open Access Journals (Sweden)

    Ondruška Michal

    2014-06-01

    Full Text Available The paper deals with the identification of precipitates in the Cr-Mn-N steels after thermal exposure. The purpose of the study is to clarify the M2N precipitation by isothermal annealing at the temperatures of 750 and 900 °C with a holding time of 5, 10, 30 min, 1 hr. and 10 hrs. Microstructure of austenitic steel was characterised by the typical presence of annealing twins. Stepwise etching was observed at the holding time of 5 and 10 minutes, but at the holding time of 30 minutes, secondary particles were precipitated at the grain boundaries. Corrosion tests revealed that holding time significantly affected steel structure. M2N is the dominant precipitate, but the occurrence of σ-phase was occasionally observed especially at the interface of discontinuous precipitation and austenitic matrix. Slight increase of hardness at the grain boundaries was caused due to the precipitation of secondary phases during isothermal holding. The maximum hardness of 294 HV was measured on the sample isothermally annealed at 750 °C and holding for 10 hrs. The research provides theoretical basis for the heat affecting of steels, such as, for example, in welding.

  16. Effect of antimony on the corrosion behavior of low-alloy steel for flue gas desulfurization system

    International Nuclear Information System (INIS)

    Le, D.P.; Ji, W.S.; Kim, J.G.; Jeong, K.J.; Lee, S.H.

    2008-01-01

    The alloying effect of Sb in a new low-alloy steel for the purpose of FGD materials was investigated by potentiodynamic polarization, linear polarization resistance measurement, electrochemical impedance spectroscopy (EIS) and weight loss measurements in an aggressive solution of 16.9 vol.% H 2 SO 4 + 0.35 vol.% HCl (modified green death solution) at 60 deg. C, pH -0.3. All measurements confirmed the marked improvement in the corrosion behavior of the low-alloy steel via the addition of a small amount of Sb, particularly for the 0.10Sb steel. Pitting corrosion was detected by scanning electron microscopy (SEM) on the surface of blank steel and 0.05Sb steel, but not 0.10Sb steel, after weight loss measurements. X-ray photoelectron spectroscopy (XPS) analysis of the corroded surfaces after EIS and linear polarization measurements showed that the decrease in corrosion rates was due to the formation of a protective Sb 2 O 5 oxide film on the surface of the Sb-containing steels. Moreover, the addition of 0.10% Sb stimulated the development of high corrosion inhibiting, Cu-containing compounds which further inhibited the anodic and cathodic reactions

  17. Bond characteristics of steel fiber and deformed reinforcing steel bar embedded in steel fiber reinforced self-compacting concrete (SFRSCC)

    Science.gov (United States)

    Aslani, Farhad; Nejadi, Shami

    2012-09-01

    Steel fiber reinforced self-compacting concrete (SFRSCC) is a relatively new composite material which congregates the benefits of the self-compacting concrete (SCC) technology with the profits derived from the fiber addition to a brittle cementitious matrix. Steel fibers improve many of the properties of SCC elements including tensile strength, ductility, toughness, energy absorption capacity, fracture toughness and cracking. Although the available research regarding the influence of steel fibers on the properties of SFRSCC is limited, this paper investigates the bond characteristics between steel fiber and SCC firstly. Based on the available experimental results, the current analytical steel fiber pullout model (Dubey 1999) is modified by considering the different SCC properties and different fiber types (smooth, hooked) and inclination. In order to take into account the effect of fiber inclination in the pullout model, apparent shear strengths ( τ ( app)) and slip coefficient ( β) are incorporated to express the variation of pullout peak load and the augmentation of peak slip as the inclined angle increases. These variables are expressed as functions of the inclined angle ( ϕ). Furthurmore, steel-concrete composite floors, reinforced concrete floors supported by columns or walls and floors on an elastic foundations belong to the category of structural elements in which the conventional steel reinforcement can be partially replaced by the use of steel fibers. When discussing deformation capacity of structural elements or civil engineering structures manufactured using SFRSCC, one must be able to describe thoroughly both the behavior of the concrete matrix reinforced with steel fibers and the interaction between this composite matrix and discrete steel reinforcement of the conventional type. However, even though the knowledge on bond behavior is essential for evaluating the overall behavior of structural components containing reinforcement and steel fibers

  18. Corrosion resistant steel

    International Nuclear Information System (INIS)

    Zubchenko, A.S.; Borisov, V.P.; Latyshev, V.B.

    1980-01-01

    Corrosion resistant steel for production of sheets and tubes containing C, Mn, Cr, Si, Fe is suggested. It is alloyed with vanadium and cerium for improving tensile properties and ductility. The steel can be melted by a conventional method in electric-arc or induction furnaces. The mentioned steel is intended to be used as a substitute for nickel-bearing austenitic steels

  19. Radiation blistering of stainless steel

    International Nuclear Information System (INIS)

    Yoshii, Naritsugu; Tanabe, Tetsuo; Imoto, Shosuke

    1980-01-01

    Surface blistering of stainless steels due to 20 keV He + ion bombardment has been investigated by examination of surface topography with a scanning electron microscope (SEM) and an optical microscope. Blisters of 0.1 to 2 μm in diameter are observed in all samples irradiated with fluence of about 1 x 10 18 He + /cm 2 at any temperature between -80 0 C and 500 0 C. With increasing the fluence blister covers are ruptured and exfoliated and finally the surface becomes rough surface without traces of blister formation. The surface effect is severer at 500 0 C than at 100 0 C irradiation. Also in double-phase stainless steel DP-3, similar surface topography to 316 SS is observed. But by the difference of the erosion rate by sputtering of the surface between α-phase and γ-phase, a striped pattern appears in DP-3 with heavy irradiation of about 2 x 10 19 He + /cm 2 . (author)

  20. Analysis of Helical Stainless Steel 08X18H10 Spring Relaxation at High Temperature

    Directory of Open Access Journals (Sweden)

    H. Sun

    2015-01-01

    Full Text Available The object of this paper is to study a cylindrical helical spring to be applied at high temperatures. The aim of this work is to study the regularity of relaxation stresses in spring and evaluate its long-term stresses.The work allowed us to establish relaxation dependencies of springs under high temperatures. According to the results of creep tests at 600°, the theoretical equation of steel creep was defined concretely. It was then used for the analysis at 350°.The paper presents a created finite element model of spring relaxation. It is the stainless steel 08Х18Н10 spring to be used at the temperature of 350°.In this paper describes the basic theory of creep, considers the relationship between the creep speed and parameters. The changing compression force of springs is analyzed under fixed compression amount.The paper also analyzes the changing length of springs in the free state after various stages of high-temperature relaxation test. It determines the results of compression forces and free length under different amount of compression.The analysis to compare the theoretical calculation of the compression forces with the experimental results is conducted. Computer modeling is created in Abaqus for calculation. Spring relaxation experiments are carried out under fixed compression amount and at the temperature of 350°. It is shown that the simulation results, which are carried out in Abaqus coincide with experimental results. The study shows that it is possible to use the creep equation parameters, based on the experimental results at high temperatures, to predict creep and relaxation properties of springs, which work at less high temperatures. The work results can be used as a basis in designing the springs working at high temperatures.

  1. Utilization of steel slag for Portland cement clinker production.

    Science.gov (United States)

    Tsakiridis, P E; Papadimitriou, G D; Tsivilis, S; Koroneos, C

    2008-04-01

    The aim of the present research work is to investigate the possibility of adding steel slag, a by-product of the conversion of iron to steel process, in the raw meal for the production of Portland cement clinker. Two samples of raw meals were prepared, one with ordinary raw materials, as a reference sample ((PC)(Ref)), and another with 10.5% steel slag ((PC)(S/S)). Both raw meals were sintered at 1450 degrees C. The results of chemical and mineralogical analyses as well as the microscopic examination showed that the use of the steel slag did not affect the mineralogical characteristics of the so produced Portland cement clinker. Furthermore, both clinkers were tested by determining the grindability, setting times, compressive strengths and soundness. The hydration products were examined by XRD analysis at 2, 7, 28 and 90 days. The results of the physico-mechanical tests showed that the addition of the steel slag did not negatively affect the quality of the produced cement.

  2. Neutron Damage in Steels Containing Small Amounts of Boron

    Energy Technology Data Exchange (ETDEWEB)

    Myers, H P

    1961-05-15

    Certain low alloy steels contain small amounts (0.003 to 0.007 w/o) of boron which element contributes to the development of the air hardening properties of these steels. Such steels appear attractive for reactor pressure vessel construction but the question arises whether they will, due to the (n,{alpha}) reaction in boron, be more susceptible to neutron radiation damage than other steels which do not contain boron. We have attempted to estimate the importance of damage arising through boron fission relative to that caused by fast neutrons by assuming that the two sources of damage will be proportional to the numbers of displaced atoms produced in the two processes when no annealing or re combination of defects occurs. Within the approximations used we conclude that in a neutron spectrum which may be represented by an equivalent thermal flux {phi}{sub t} and an equivalent fast flux at 1 MeV of {phi}{sub f}, then D, the ratio of damage to boron fission to that caused by fast neutrons, is D = 4.5 x 10{sup -2} {phi}{sub t}/{phi}{sub f} (for 0. 003 w/o B). For the conditions at the inside of the reactor tank to R3 this would imply D = 1.2 x 10{sup -2} , i.e. if the R3 tank were built with a steel containing 0.003 w/o B then damage due to boron fission would be only {approx} 1 % of that caused by fast neutrons. Further problems with such steels as here discussed are the probability of embrittlement due to the introduction of boron fission fragments lithium and helium and the possibility of a radiation enhanced diffusion of boron which might lead to accentuated slow strain rate embrittlement. We argue that none of these problems should arise. It is concluded that a constructional steel containing 0.003 to 0.007 w/o B should not on this account be more susceptible to radiation damage than other non boron containing steels.

  3. Engineering Performance of High Strength Concrete Containing Steel Fibre Reinforcement

    Directory of Open Access Journals (Sweden)

    Md Azree Othuman Mydin

    2013-09-01

    Full Text Available The development and utilization of the high strength concrete in the construction industry have been increasing rapidly. Fiber reinforced concrete is introduced to overcome the weakness of the conventional concrete because concrete normally can crack under a low tensile force and it is known to be brittle. Steel fibre is proved to be the popular and best combination in the high strength concrete to result the best in the mechanical and durability properties of high strength concrete with consideration of curing time, steel fibre geometry, concrete grade and else more. The incorporation of steel fibre in the mortar mixture is known as steel fibre reinforced concrete have the potential to produce improvement in the workability, strength, ductility and the deformation of high strength concrete. Besides that, steel fibre also increases the tensile strength of concrete and improves the mechanical properties of the steel fibre reinforced concrete. The range for any high strength concrete is between 60MPa-100MPa. Steel fibre reinforced concrete which contains straight fibres has poorer physical properties than that containing hooked end stainless steel fibre due to the length and the hooked steel fibre provide a better effective aspects ratio. Normally, steel fibre tensile strength is in the range of 1100MPa-1700MPa. Addition of less steel fibre volumes in the range of 0.5% to 1.0% can produce better increase in the flexural fatigue strength. The strength can be increased with addition of steel fibre up to certain percentage. This paper will review and present some basic properties of steel fibre reinforced concrete such as mechanical, workability and durability properties.

  4. Stress corrosion of low alloy steel forgings

    International Nuclear Information System (INIS)

    Thornton, D.V.; Mould, P.B.; Patrick, E.C.

    1976-01-01

    The catastrophic failure of a steam turbine rotor disc at Hinkley Point 'A' Power station was shown to have been caused by the growth of a stress corrosion crack to critical dimensions. This failure has promoted great interest in the stress corrosion susceptibility of medium strength low alloy steel forgings in steam environments. Consequently, initiation and growth of stress corrosion cracks of typical disc steels have been investigated in steam and also in water at 95 0 C. Cracking has been shown to occur, predominantly in an intergranular manner, with growth rates of between 10 -9 and 10 -7 mm sec. -1 . It is observed that corrosion pitting and oxide penetration prior to the establishment of a stress corrosion crack in the plain samples. (author)

  5. Research on reconstruction of steel tube section from few projections

    International Nuclear Information System (INIS)

    Peng Shuaijun; Wu Haifeng; Wang Kai

    2007-01-01

    Most parameters of steel tube can be acquired from CT image of the section so as to evaluate its quality. But large numbers of projections are needed in order to reconstruct the section image, so the collection and calculation of the projections consume lots of time. In order to solve the problem, reconstruction algorithms of steel tube from few projections are researched and the results are validated with simulation data in the paper. Three iterative algorithms, ART, MAP and OSEM, are attempted to reconstruct the section of steel tube by using the simulation model. Considering the prior information distributing of steel tube, we improve the algorithms and get better reconstruction images. The results of simulation experiment indicate that ART, MAP and OSEM can reconstruct accurate section images of steel tube from less than 20 projections and approximate images from 10 projections. (authors)

  6. Corrosion of X65 Pipeline Steel Under Deposit and Effect of Corrosion Inhibitor

    Directory of Open Access Journals (Sweden)

    XU Yun-ze

    2016-10-01

    Full Text Available Effect of the deposit on the electrochemical parameters of X65 pipeline steel in oxygen contained sodium chloride solution was studied by EIS and PDS methods. The galvanic corrosion behavior under deposit and effect of different concentration of corrosion inhibitor PBTCA were studied by electrical resistance (ER method combined with ZRA. The results show that the corrosion potential of X65 steel shifts negatively as SiO2 covering its surface and the corrosion rate becomes lower. When the galvanic couple specimen with deposit is electrically connected with the specimen without deposit, anodic polarization occurs on X65 steel under deposit and the galvanic current density decreases from 120μA/cm2 to 50μA/cm2 and keeps stable. As 5×10-5, 8×10-5 and 3×10-4 PBTCA were introduced into the solution, the galvanic current density reaches the highest 1300μA/cm2 and then decreases to 610μA/cm2 keeping stable around 610μA/cm2, corrosion rate of X65 steel under deposit reaches 6.11mm/a. PBTCA accelerates the corrosion of X65 steel under deposit in oxygen contained solution. Through the investigation on the surface of the specimens, serious local corrosion occurs on the X65 steel surface under deposit.

  7. Influence of tempering temperature on mechanical properties of cast steels

    Directory of Open Access Journals (Sweden)

    G. Golański

    2008-12-01

    Full Text Available The paper presents results of research on the influence of tempering temperature on structure and mechanical properties of bainite hardened cast steel: G21CrMoV4 – 6 (L21HMF and G17CrMoV5 – 10 (L17HMF. Investigated cast steels were taken out from internal frames of steam turbines serviced for long time at elevated temperatures. Tempering of the investigated cast steel was carried out within the temperature range of 690 ÷ 730 C (G21CrMoV4 – 6 and 700 ÷ 740 C (G17CrMoV5 – 10. After tempering the cast steels were characterized by a structure of tempered lower bainite with numerous precipitations of carbides. Performed research of mechanical properties has shown that high temperatures of tempering of bainitic structure do not cause decrease of mechanical properties beneath the required minimum.oo It has also been proved that high-temperature tempering (>720 oC ensures high impact energy at the 20% decrease of mechanical properties.

  8. Fatigue behavior of welded austenitic stainless steel in different environments

    Directory of Open Access Journals (Sweden)

    D.S. Yawas

    2014-01-01

    Full Text Available The fatigue behavior of welded austenitic stainless steel in 0.5 M hydrochloric acid and wet steam corrosive media has been investigated. The immersion time in the corrosive media was 30 days to simulate the effect on stainless steel structures/equipment in offshore and food processing applications and thereafter annealing heat treatment was carried out on the samples. The findings from the fatigue tests show that seawater specimens have a lower fatigue stress of 0.5 × 10−5 N/mm2 for the heat treated sample and 0.1 × 10−5 N/mm2 for the unheat-treated sample compared to the corresponding hydrochloric acid and steam samples. The post-welding heat treatment was found to increase the mechanical properties of the austenitic stainless steel especially tensile strength but it reduces the transformation and thermal stresses of the samples. These findings were further corroborated by the microstructural examination of the stainless steel specimen.

  9. Wear properties of metal ion implanted 4140 steel

    Energy Technology Data Exchange (ETDEWEB)

    Evans, P.J. (Applications of Nuclear Physics, Ansto, Private Mail Bag 1, Menai, NSW 2234 (Australia)); Paoloni, F.J. (Department of Electrical and Computer Engineering, University of Wollongong, GPO Box 1144, Wollongong, NSW 2500 (Australia))

    1994-07-01

    AISI type 4140 (high tensile) steel has been implanted with tungsten and titanium using a metal vapour vacuum arc ion source. Doses in the range (1-5)x10[sup 16]ionscm[sup -2] were implanted to a depth of approximately 30nm. The relative wear resistance between non-implanted and implanted specimens has been estimated using pin-on-disc and abrasive wear tests. Implantation of titanium decreased the area of wear tracks by a factor of 5 over unimplanted steel. In some cases the steel was also hardened by a liquid carburization treatment before implantation. Abrasion tests revealed a further improvement in wear resistance on this material following ion irradiation. ((orig.))

  10. Joining of aluminum and stainless steel using AlSi10 brazing filler: Microstructure and mechanical properties

    Science.gov (United States)

    Fedorov, Vasilii; Uhlig, Thomas; Wagner, Guntram

    2017-07-01

    Joining of dissimilar materials like stainless steel and aluminum is of special interest for automotive applications. Due to the different properties of these materials, suitable joining techniques are required. Brazing offers the possibilities to manufacture high performance joints in one step and at low joining temperatures. However, these joints often need to withstand a high number of high cyclic loads during application. Therefore, in addition to the monotonic properties, the fatigue behavior of the produced joints must be considered and evaluated. In the present work, specimens are manufactured by induction brazing using an AlSi10 filler and a non-corrosive flux. The mechanical properties are determined by tensile shear tests as well as in fatigue tests at ambient and elevated temperatures. The microstructure of the brazed joints and the fracture surfaces of the tested samples are investigated by SEM.

  11. Effect of Cavitation on Surface Damage of 16.7Cr-10Ni-2Mo Stainless Steel in Marine Environment

    Energy Technology Data Exchange (ETDEWEB)

    Chong, Sang-Ok; Han, Min-Su; Kim, Seong-Jong [Mokpo National Maritime University, Mokpo (Korea, Republic of)

    2015-10-15

    Stainless steel is generally known to have characteristics of excellent corrosion resistance and durability, but in a marine environment it can suffer from localized corrosion due to the breakdown of passivity film due to chloride ion in seawater. Furthermore, the damage behaviors are sped up under a cavitation environment because of complex damage from electrochemical corrosion and cavitation-erosion. In this study the characteristics of electrochemical corrosion and cavitation erosion behavior were evaluated on 16.7Cr-10Ni-2Mo stainless steel under a cavitation environment in natural seawater. The electrochemical experiments have been conducted at both static conditions and dynamic conditions inducing cavitation with different current density parameters. The surface morphology and damage behaviors were compared after the experiment. After the cavitation test with time variables morphological examinations on damaged specimens were analyzed by using a scanning electron microscope and a 3D microscope. the galvanostatic experiment gave a cleaner surface morphology presented with less damage depth at high current density regions. It is due to the effect of water cavitation peening under the cavitation condition. In the cavitation experiment, with amplitude of 30 μm and seawater temperature of 25 ℃, weight loss and cavitation-erosion damage depth were dramatically increased after 5 hours inducing cavitation.

  12. Experimental Study on the Utilization of Fine Steel Slag on Stabilizing High Plastic Subgrade Soil

    OpenAIRE

    Hussien Aldeeky; Omar Al Hattamleh

    2017-01-01

    The three major steel manufacturing factories in Jordan dump their byproduct, steel slag, randomly in open areas, which causes many environmental hazardous problems. This study intended to explore the effectiveness of using fine steel slag aggregate (FSSA) in improving the geotechnical properties of high plastic subgrade soil. First soil and fine steel slag mechanical and engineering properties were evaluating. Then 0%, 5%, 10%, 15%, 20%, and 25% dry weight of soil of fine steel slag (FSSA) w...

  13. The compatibility of various austenitic steels with molten sodium (1963)

    International Nuclear Information System (INIS)

    Champeix, L.; Sannier, J.; Darras, R.; Graff, W.; Juste, P.

    1963-01-01

    Various techniques for studying corrosion by molten sodium have been developed and applied to the case of 18/10 austenitic steels. The results obtained are discussed as a function of various parameters: type of steel, temperature, oxygen content of the sodium, surface treatment, welds, mechanical strain. In general, these steels have an excellent resistance to sodium when the oxygen content is limited by a simple purification system of the 'cold trap' type, and when an attempt is made to avoid cavitation phenomena which are particularly dangerous, as is shown by the example given. (authors) [fr

  14. Moessbauer spectroscopic study of rust formed on a weathering steel and a mild steel exposed for a long term in an industrial environment

    International Nuclear Information System (INIS)

    Kamimura, Takayuki; Nasu, Saburo; Tazaki, Takashi; Kuzushita, Kaori; Morimoto, Shotaro

    2002-01-01

    The rusts formed on mild steel (15-year exposure) and weathering steel (32-year exposure) exposed to an industrial environment have been characterized by means of X-ray diffraction technique and 57 Fe Moessbauer spectroscopy. By using an X-ray diffraction method, it is suggested that the rusts formed on both steels consist of the crystalline α-FeOOH, γ-FeOOH and an X-ray amorphous phase, which gives no peak to X-ray diffraction pattern. The amount of the X-ray amorphous phase exceeds 50% of the total amount of the rust. The 57 Fe Moessbauer spectra observed at 10K indicate that the rust contains only α-FeOOH, γ-FeOOH and Fe 3-δ O 4 (γ-Fe 2 O 3 ) for mild steel, and only α-FeOOH and γ-FeOOH for weathering steel. The X-ray amorphous substance in the rust payer formed on mild steel possesses the structures of mainly α-FeOOH showing superparamagnetism owing to its small particle size, and Fe 3-δ O 4 (γ-Fe 2 O 3 ). They are contained both in the inner rust layer and in the outer rust layer. The X-ray amorphous phase in the rust layer formed on weathering steel is mainly α-FeOOH. (author)

  15. 77 FR 14445 - Application for a License To Export Steel Forging

    Science.gov (United States)

    2012-03-09

    ... NUCLEAR REGULATORY COMMISSION Application for a License To Export Steel Forging Pursuant to 10 CFR 110.70(b) ``Public Notice of Receipt of an Application,'' please take notice that the Nuclear... head steel February 7, 2012 forging. forging will be XR175 machined into the 11005983 finished vessel...

  16. Water corrosion test of oxide dispersion strengthened (ODS) steel claddings

    International Nuclear Information System (INIS)

    Narita, Takeshi; Ukai, Shigeharu; Kaito, Takeji; Ohtsuka, Satoshi; Matsuda, Yasushi

    2006-07-01

    As a part of feasibility study of ODS steel cladding, its water corrosion resistance was examined under water pool condition. Although addition of Cr is effective for preventing water corrosion, excessive Cr addition leads to embrittlement due to the Cr-rich α' precipitate formation. In the ODS steel developed by the Japan Atomic Energy Agency (JAEA), the Cr content is controlled in 9Cr-ODS martensite and 12Cr-ODS ferrite. In this study, water corrosion test was conducted for these ODS steels, and their results were compared with that of conventional austenitic stainless steel and ferritic-martensitic stainless steel. Following results were obtained in this study. (1) Corrosion rate of 9Cr-ODS martensitic and 12Cr-ODS ferritic steel are significantly small and no pitting was observed. Thus, these ODS steels have superior resistance for water corrosion under the condition of 60degC and pH8-12. (2) It was showed that 9Cr-ODS martensitic steel and 12Cr-ODS ferritic steel have comparable water corrosion resistance to that of PNC316 and PNC-FMS at 60degC for 1,000h under varying pH of 8, 10. Water corrosion resistance of these alloys is slightly larger than that of PNC316 and PNC-FMS at pH12 without significant difference of appearance and uneven condition. (author)

  17. Peculiarities of cyclic deformation and fracture of heat-resistant steel 10GN2MFA under conditions typical for the steam generator PGV-1000 collector material

    International Nuclear Information System (INIS)

    Giginyak, F.F.

    1998-01-01

    In the present paper, the results are discussed concerning investigations into the regularities of deformation and fracture of steel, 10GN2MFA under conditions close to those of actual operation when used in collectors of PGV-1000-type steam generators, which are in service with WWER-1000-type reactors of nuclear power plants (NPP). (author)

  18. The effect of thermoplastic treatment regimes on the microplastic strain of nitrogen-containing steel Kh21G10N7MBF

    International Nuclear Information System (INIS)

    Bannykh, O.A.; Blinov, V.M.; Kostina, M.V.; Grachev, S.V.; Mal'tseva, L.A.

    2005-01-01

    A study is made into the influence of a percentage reduction during cold rolling and subsequent holdings at heat on development of microplastic deformation when bending sheet specimens of stainless austenitic high-nitrogen steel Kh21G10N7MBF. It is revealed that a maximum value of apparent limit of elasticity (∼1800 MPa) is attained due to plastic deformation by rolling at 20 Deg C with a total percentage reduction of 60 % and subsequent aging at 500 Deg C for 1-4 h [ru

  19. Structural steels for power generating equipment and heat and chemical heat treatments

    International Nuclear Information System (INIS)

    Astaf'ev, A.A.

    1979-01-01

    Development of structural steels for power generating equipment and for reactor engineering, in particular, is elucidated. Noted is utilization of the 15Kh2NMFA steels for the WWER-1000 reactor vessels, the 10GN2MFA steels for steam generators, pressurizers, vessels of the automatic emergency shut down and safety system; the 00Kh12N3DL steel for cast pump vessels and main locking bars. The recommendations on heat treatment of big forgings, for instance, ensuring the necessary complex of mechanical properties are given. Diffusion chromizing with subsequent nitriding of austenitic steels which increase durability of the components in BN reactors more than 4 times, is practised on a large scale

  20. Preparation and characterization of 304 stainless steel/Q235 carbon steel composite material

    Directory of Open Access Journals (Sweden)

    Wenning Shen

    Full Text Available The composite material of 304 stainless steel reinforced Q235 carbon steel has been prepared by modified hot-rolling process. The resulted material was characterized by scanning electron microscope, three-electrode method, fault current impact method, electrochemical potentiodynamic polarization curve measurement and electrochemical impedance spectroscopy. The results showed that metallurgical bond between the stainless steel layer and carbon steel substrate has been formed. The composite material exhibited good electrical conductivity and thermal stability. The average grounding resistance of the composite material was about 13/20 of dip galvanized steel. There has no surface crack and bubbling formed after fault current impact. The composite material led to a significant decrease in the corrosion current density in soil solution, compared with that of hot dip galvanized steel and bare carbon steel. On the basis polarization curve and EIS analyses, it can be concluded that the composite material showed improved anti-corrosion property than hot-dip galvanized steel. Keywords: Stainless steel, Carbon steel, Anti-corrosion, Conductivity, Electrochemical, EIS

  1. Texture evolution of experimental silicon steel grades. Part I: Hot rolling

    Energy Technology Data Exchange (ETDEWEB)

    Sandoval Robles, J.A., E-mail: jsandoval.uanl@yahoo.com [Universidad Autónoma de Nuevo León, Facultad de Ingeniería Mecánica y Eléctrica, Ave. Universidad S/N, Cd. Universitaria, San Nicolás de los Garza, Nuevo León C.P. 66450 (Mexico); Salas Zamarripa, A.; Guerrero Mata, M.P. [Universidad Autónoma de Nuevo León, Facultad de Ingeniería Mecánica y Eléctrica, Ave. Universidad S/N, Cd. Universitaria, San Nicolás de los Garza, Nuevo León C.P. 66450 (Mexico); Cabrera, J. [Universitat Politècnica de Catalunya, Departament de Ciència dels Materials I Enginyeria Metal-lúrgica, Av. Diagonal 647, Barcelona 08028 (Spain)

    2017-05-01

    The metallurgical understanding of the deformation processes during the fabrication of non-oriented electrical steels plays a key role in improving their final properties. Texture control and optimization is critical in these steels for the enhancement of their magnetic properties. The aim of the present work is to study the texture evolution of six non-oriented experimental silicon steel grades during hot rolling. These steels were low carbon steel with a silicon content from 0.5 to 3.0 wt%. The first rolling schedule was performed in the austenitic (γ-Fe) region for the steel with a 0.5 wt% of silicon content, while the 1.0 wt% silicon steel was rolled in the two-phase (α+γ) region. Steels with higher silicon content were rolled in the ferritic (α-Fe) region. The second rolling schedule was performed in the α-Fe region. Samples of each stage were analyzed by means of Electron Backscatter Diffraction (EBSD). Findings showed that the texture was random and heterogeneous in all samples after 60% of rolling reduction, which is due to the low deformation applied during rolling. After the second rolling program, localized deformation and substructured grains near to surface were observed in all samples. The Goss {110}<001>texture-component was found in the 0.5 and 1.0 wt.-%silicon steels. This is due to the thermomechanical conditions and the corresponding hot band microstructure obtained after the first program. Moreover, the α<110>//RD and the γ <111>//ND fiber components of the texture presented a considerable increment as the silicon content increases. Future research to be published soon will be related to the texture evolution during the cold-work rolling process. - Highlights: • We analyze six silicon steel experimental grades alloys trough the rolling process. • Material was subjected to a hot deformation process in the α-γ region. • No recrystalization was observed during-after the rolling schedules. • Rise of the magnetic texture components

  2. Spectroscopic investigation of plasma electrolytic borocarburizing on q235 low-carbon steel

    Energy Technology Data Exchange (ETDEWEB)

    Liu, Run [Key Laboratory for Beam Technology and Materials Modification of Ministry of Education, College of Nuclear Science and Technology, Beijing Normal University, Beijing 100875 (China); Beijing Radiation Center, Beijing 100875 (China); Zhenjiang Watercraft College, Zhenjiang 212000, Jiangsu (China); Wang, Bin; Wu, Jie [Key Laboratory for Beam Technology and Materials Modification of Ministry of Education, College of Nuclear Science and Technology, Beijing Normal University, Beijing 100875 (China); Beijing Radiation Center, Beijing 100875 (China); Xue, Wenbin, E-mail: xuewb@bnu.edu.cn [Key Laboratory for Beam Technology and Materials Modification of Ministry of Education, College of Nuclear Science and Technology, Beijing Normal University, Beijing 100875 (China); Beijing Radiation Center, Beijing 100875 (China); Jin, Xiaoyue; Du, Jiancheng; Hua, Ming [Key Laboratory for Beam Technology and Materials Modification of Ministry of Education, College of Nuclear Science and Technology, Beijing Normal University, Beijing 100875 (China); Beijing Radiation Center, Beijing 100875 (China)

    2014-12-01

    Highlights: • The plasma discharge behaviors for PEB/C on steels were evaluated by OES. • Electron temperature, concentration, atomic ionization degree were calculated. • The decomposition mechanism of electrolyte and was analyzed. - Abstract: A plasma electrolytic borocarburizing process (PEB/C) in borax electrolyte with glycerin additive was employed to fabricate a hardening layer on Q235 low-carbon steel. Optical emission spectroscopy (OES) was utilized to investigate the spectroscopy characteristics of plasma discharge around the steel during PEB/C process. Some plasma parameters were calculated in terms of OES. The electron temperature and electron concentration in plasma discharge zone is about 3000–12,000 K and 2 × 10{sup 22} m{sup −3}–1.4 × 10{sup 23} m{sup −3}. The atomic ionization degrees of iron, carbon and boron are 10{sup −16}–10{sup −3}, and 10{sup −23}–10{sup −6}, 10{sup −19}–10{sup −4}, respectively, which depend on discharge time. The surface morphology and cross-sectional microstructure of PEB/C hardening layer were observed, and the electrolyte decomposition and plasma discharge behaviors were discussed.

  3. Spectroscopic investigation of plasma electrolytic borocarburizing on q235 low-carbon steel

    International Nuclear Information System (INIS)

    Liu, Run; Wang, Bin; Wu, Jie; Xue, Wenbin; Jin, Xiaoyue; Du, Jiancheng; Hua, Ming

    2014-01-01

    Highlights: • The plasma discharge behaviors for PEB/C on steels were evaluated by OES. • Electron temperature, concentration, atomic ionization degree were calculated. • The decomposition mechanism of electrolyte and was analyzed. - Abstract: A plasma electrolytic borocarburizing process (PEB/C) in borax electrolyte with glycerin additive was employed to fabricate a hardening layer on Q235 low-carbon steel. Optical emission spectroscopy (OES) was utilized to investigate the spectroscopy characteristics of plasma discharge around the steel during PEB/C process. Some plasma parameters were calculated in terms of OES. The electron temperature and electron concentration in plasma discharge zone is about 3000–12,000 K and 2 × 10 22 m −3 –1.4 × 10 23 m −3 . The atomic ionization degrees of iron, carbon and boron are 10 −16 –10 −3 , and 10 −23 –10 −6 , 10 −19 –10 −4 , respectively, which depend on discharge time. The surface morphology and cross-sectional microstructure of PEB/C hardening layer were observed, and the electrolyte decomposition and plasma discharge behaviors were discussed

  4. Control of radioactivity at the Luxembourg steel-making facilities

    International Nuclear Information System (INIS)

    Werner, C.

    1999-01-01

    The Luxembourg steel industry has a yearly capacity of close to 3 million tonnes of raw steel produced from scrap at three electric arc furnace steel-making plants. It has introduced in 1994 a comprehensive system of measuring devices to prevent radioactive material from being introduced into its meltshops. Detection equipment has been installed at the road and railroad accesses to the three plants. Further to the controls of incoming scrap, radioactivity is monitored on both the steel and the slag samples of each heat produced at the plants. This measure is taken in order to detect any incident involving the melting of a radioactive source that might have escaped the controls of incoming material as soon as possible. The triple purpose of these controls is: (i) to protect the personnel of the steel making plants from radiation hazards; (ii) to maintain the integrity of the equipment; and (iii) to assure integrity of the products. The presentation describes the possible origins of radioactive contamination in steel scrap as well as the behaviour in the steel making process of the different radionuclides that can be expected to be introduced into the steel making vessels through steel scrap. Together with the government agency for radiation protection, procedures have been developed for the management of any event of detection of radioactivity in the plants and to assure optimum availability of the measuring equipment. These procedures are described and commented in the presentation. The presentation includes also a report on the experience from 4 years of monitoring, during which more than 10 million tonnes of scrap have passed the gates of the steel-making plants of ProfilARBED and ARES. (author)

  5. Ethnic and gender differences in physical activity levels among 9-10-year-old children of white European, South Asian and African-Caribbean origin: the Child Heart Health Study in England (CHASE Study).

    Science.gov (United States)

    Owen, Christopher G; Nightingale, Claire M; Rudnicka, Alicja R; Cook, Derek G; Ekelund, Ulf; Whincup, Peter H

    2009-08-01

    Ethnic differences in physical activity in children in the UK have not been accurately assessed. We made objective measurements of physical activity in 9-10-year-old British children of South Asian, black African-Caribbean and white European origin. Cross-sectional study of urban primary school children (2006-07). Actigraph-GT1M activity monitors were worn by 2071 children during waking hours on at least 1 full day. Ethnic differences in mean daily activity [counts, counts per minute of registered time (CPM) and steps] were adjusted for age, gender, day of week and month. Multilevel modelling allowed for repeated days within individual and clustering within school. In white Europeans, mean daily counts, CPM and mean daily steps were 394,785, 498 and 10,220, respectively. South Asian and black Caribbean children recorded more registered time per day than white Europeans (34 and 36 min, respectively). Compared with white Europeans, South Asians recorded 18 789 fewer counts [95% confidence interval (CI) 6390-31 187], 41 fewer CPM 95% CI 26-57) and 905 fewer steps (95% CI 624-1187). Black African-Caribbeans recorded 25 359 more counts (95% CI 14 273-36 445), and similar CPM, but fewer steps than white Europeans. Girls recorded less activity than boys in all ethnic groups, with 74 782 fewer counts (95% CI 66 665-82 899), 84 fewer CPM (95% CI 74-95) and 1484 fewer steps (95% CI 1301-1668). British South Asian children have lower objectively measured physical activity levels than European whites and black African-Caribbeans.

  6. Flexural Cracking Behavior Of Steel Fiber Reinforced Concrete Beams

    Directory of Open Access Journals (Sweden)

    Ashraf Abdalkader

    2017-08-01

    Full Text Available Steel fibers are added to concrete due to its ability to improve the tensile strength and control propagation of cracks in reinforced concrete members. Steel fiber reinforced concrete is made of cement fine water and coarse aggregate in addition to steel fibers. In this experimental work flexural cracking behavior of reinforced concrete beams contains different percentage of hooked-end steel fibers with length of 50 mm and equivalent diameter of 0.5 mm was studied. The beams were tested under third-point loading test at 28 days. First cracking load maximum crack width cracks number and load-deflection relations were investigated to evaluate the flexural cracking behavior of concrete beams with 34 MPa target mean strength. Workability wet density compressive and splitting tensile strength were also investigated. The results showed that the flexural crack width is significantly reduced with the addition of steel fibers. Fiber contents of 1.0 resulted in 81 reduction in maximum crack width compared to control concrete without fiber. The results also showed that the first cracking load and maximum load are increased with the addition of steel fibers.

  7. Mechanical and fracture properties at impact loading of selected steels for nuclear power engineering

    International Nuclear Information System (INIS)

    Buchar, J.; Bilek, Z.

    1988-01-01

    The possibilities are briefly characterized of experimental research of mechanical and fracture properties of steels used in nuclear power engineering. Attention is paid to plastic deformation and the assessment of fracture formation during impact loading. The results are reported for steels 15Kh2MFA and 10GN2MFA. For steel 15Kh2MFA the effect was also studied of neutron radiation at different temperatures. From the theory developed for non-irradiated material 10GN2MFA, a prediction is made within the original model of the fracture stress value for steel 15Kh2MFA in both non-irradiated and irradiated states. The conclusion is arrived at that the existing methods of assessing steel properties at impact load allow obtaining knowledge of all significant effects during actual stress, this using only small specimens of the materials. (Z.M.). 4 figs., 8 refs

  8. Microhardness of boron, titanium, and nitrogen implanted steel

    International Nuclear Information System (INIS)

    Sowa, M.; Szyszko, W.; Sielanko, J.; Glusiec, L.

    1989-01-01

    Mechanically polished steel (1H18N9T) and (15GTM) samples are implanted with boron, titanium, and nitrogen ions, with dose ranging from 10 16 to 10 17 ions/cm 2 . The implantation energy varied from 100 to 250 keV. Implanted samples are heat-treated at 400 to 800 0 C in vacuum. The microhardness of implanted samples is measured by using a Hanneman tester with loads ranging from 2 to 40 g. The influence of annealing temperature on microhardness of the implanted layers is determined. The diffusion of boron from the implanted layers is also investigated by using the secondary ion mass spectrometer. The diffusion coefficients of boron in steel are determined. (author)

  9. Aging degradation of cast stainless steel

    International Nuclear Information System (INIS)

    Chopra, O.K.; Chung, H.M.

    1986-10-01

    A program is being conducted to investigate the significance of in-service embrittlement of cast duplex stainless steels under light-water reactor operating conditions. Microstructures of cast materials subjected to long-term aging either in reactor service or in the laboratory have been characterized by TEM, SANS, and APFIM techniques. Two precipitate phases, i.e., the Cr-rich α' and Ni- and Si-rich G phase, have been identified in the ferrite matrix of the aged steels. The results indicate that the low-temperature embrittlement is primarily caused by α' precipitates which form by spinodal decomposition. The relative contribution of G phase to loss of toughness is now known. Microstructural data also indicate that weakening of ferrite/austenite phase boundary by carbide precipitates has a significant effect on the onset and extent of embrittlement of the high-carbon CF-8 and CF-8M grades of stainless steels, particularly after aging at 400 or 450 0 C. Data from Charpy-impact, tensile, and J-R curve tests for several heats of cast stainless steel aged up to 10,000 h at 350, 400, and 450 0 C are presented and correlated with the microstructural results. Thermal aging of the steels results in an increase in tensile strength and a decrease in impact energy, J/sub IC/, and tearing modulus. The fracture toughness results show good agreement with the Charpy-impact data. The effects of compositional and metallurgical variables on loss of toughness are discussed

  10. [Studies on the tolerance of the organism to X 5 CrNiMo 18.10 steel (Königsee). II. Light microscopic studies of the surrounding tissue of metal implants (X 5 CrNiMo 18.10 steel) in guinea pigs].

    Science.gov (United States)

    Höhndorf, H; Drössler, K; Stiehl, P

    1977-06-01

    The tissue around X 5 CrNiMo 18.10-steel implantates with different surfaces was examined in 72 guinea-pigs. Aside from controls, these animals were preoperatively sensibilized against chromium and nickel. The results can be summarized since the histologic findings showed no different peculiarities. The authors describe an intussusception of the implantate in connective tissue which evidently depends on time and surface. Further the spreading of alien material in the surrounding of the implantate, and morphologic findings are reported. The morphologic evidences are described and discussed in detail, since they are interpreted as signs of cell-mediated immune reactions. The presence of lymphocytes, lymphoblasts, histiocytes (mostly carrying alien material), and granulocytes, as well as proliferations at the arterioles suggest an overlapping of immune reactions.

  11. Development of x-ray computed tomographic scanner for iron and steel

    International Nuclear Information System (INIS)

    Taguchi, Isamu; Nakamura, Shigeo.

    1985-01-01

    X-ray computed tomography is extensively used in medicine, but has rarely been applied to non-medical purposes. Steel specimens pose particularly difficult problems-very poor transmission of X-rays and the need for high resolving capability. There has thus been no effective tomographic method of examining steel specimens. Due to the growing need for non-destructive, non-contact methods for observing and analyzing the internal conditions of steel microscopically, however, we have developed an X-ray Computed Tomographic Scanner for Steel (CTS) system, specifically for examination of steel specimens. Its major specifications and functions are as follows. Type: the second-generation CT, 8-channels, Scanning method: 6 0 revolution, 30-times traversing, Slice width: 0.5 mm, Resolving capability: 0.25 x 0.25 mm, X-ray source: 420 kV, 3 mA, X-ray detector: BGO scintillator, Standard specimen shape: 50 mm dia., 100 mm high, Measuring time: 10.5 min. Porosity of a stainless steel (SUS 304) bloom was examined three-dimensionally by the CTS system. Corrosion procedure of a steel slab was also examined. (author)

  12. High temperature fatigue properties of the 316 FR steel

    International Nuclear Information System (INIS)

    Kobayashi, Kazuo; Yamaguchi, Koji; Kato, Seiichi; Nishijima, Satoshi; Fujioka, Terutaka; Nakazawa, Takanori; Koto, Hiroyuki; Date, Shingo

    1998-01-01

    Type 316 FR stainless steel has been developed as a candidate material for fast breeder reactor of next century. For the structural integrity design of high temperature components including reactor vessel, long-term data and analysis method are investigated for the new 316 FR steel especially to evaluate its time-dependent low-cycle fatigue behavior. The present paper reports dependencies of fatigue life on the strain rate from 10 -2 to 10 -5 s -1 , and on the temperature dependencies from 500degC to 600degC. Data are analyzed by a parametric method formerly proposed by the authors. It is shown that the method has a good predictability of the fatigue life up to very low strain rate of 10 -6 s -1 . (author)

  13. 2D magnetization of grain-oriented 3%-Si steel under uniaxial stress

    International Nuclear Information System (INIS)

    Permiakov, V.; Dupre, L.; Pulnikov, A.; Melkebeek, J.

    2005-01-01

    Magnetization in electrical steels is strongly affected by mechanical stress. The stress dependence of magnetic properties of non-oriented steels has been studied at one- and two-dimensional magnetization. This paper deals with the stress effect on one- and two-dimensional magnetization in grain-oriented 3%-Si steel. The special magnetic measurements system is applied to combine uniaxial stress and 2D magnetic measurements. The uniaxial stress ranges from 10 MPa compressive stress to 100 MPa tensile stress. A domain theory is a suitable tool for prediction and a physical explanation of stress dependency in grain-oriented steel

  14. Plasma nitriding of steels

    CERN Document Server

    Aghajani, Hossein

    2017-01-01

    This book focuses on the effect of plasma nitriding on the properties of steels. Parameters of different grades of steels are considered, such as structural and constructional steels, stainless steels and tools steels. The reader will find within the text an introduction to nitriding treatment, the basis of plasma and its roll in nitriding. The authors also address the advantages and disadvantages of plasma nitriding in comparison with other nitriding methods. .

  15. Development of austenitic stainless steel plate (316MN) for fast breeder reactors

    International Nuclear Information System (INIS)

    Nakazawa, Takanori; Abo, Hideo; Tanino, Mitsuru; Komatsu, Hazime.

    1989-01-01

    High creep-fatigue resistance is required for the structural materials for fast breeder reactors. As creep-fatigue life is closely related to creep-rupture ductility, the effects of C, N and Mo on creep-rupture properties were investigated with a view to improving the creep-fatigue resistance of stainless steel. Strengthening by the addition of C has a great adverse effect on rupture ductility, but N can strengthen the steel without decreasing rupture ductility. Strengthening by Mo decreases rupture ductility but this effect is small. The low-C-medium-N (0.01%C - 0.07%N) stainless steel 316 MN developed based on the findings described above exhibits only a small decrease in creep-rupture strength in long-time periods compared with the conventional 316 steel. This steel offers excellent rupture ductility and the 10,000-hour rupture strength which is about 1.2 times that of conventional steel. Moreover, this steel exhibits excellent properties in creep fatigue test. (author)

  16. Steel

    International Nuclear Information System (INIS)

    Zorev, N.N.; Astafiev, A.A.; Loboda, A.S.; Savukov, V.P.; Runov, A.E.; Belov, V.A.; Sobolev, J.V.; Sobolev, V.V.; Pavlov, N.M.; Paton, B.E.

    1977-01-01

    Steels also containing Al, N and arsenic, are suitable for the construction of large components for high-power nuclear reactors due to their good mechanical properties such as good through-hardening, sufficiently low brittleness conversion temperature and slight displacement of the latter with neutron irradiation. Defined steels and their properties are described. (IHOE) [de

  17. Effects of Non-metallic Inclusions on Hot Ductility of High Manganese TWIP Steels Containing Different Aluminum Contents

    Science.gov (United States)

    Wang, Yu-Nan; Yang, Jian; Wang, Rui-Zhi; Xin, Xiu-Ling; Xu, Long-Yun

    2016-06-01

    The characteristics of inclusions in Fe-16Mn- xAl-0.6C ( x = 0.002, 0.033, 0.54, 2.10 mass pct) steels have been investigated and their effects on hot ductility of the high manganese TWIP steels have been discussed. Ductility is very poor in the steel containing 0.54 mass pct aluminum, which is lower than 20 pct in the temperature range of 873 K to 1473 K (600 °C to 1200 °C). For the steels containing 0.002 and 2.10 mass pct aluminum, ductility is higher than 40 pct in the same temperature range. The hot ductility of steel containing 0.033 mass pct aluminum is higher than 30 pct throughout the temperature range under examination. With increasing aluminum content, the main inclusions in the steels change along the route of MnO/(MnO + MnS) → MnS/(Al2O3 + MnS) → AlN/(Al2O3 + MnS)/(MgAl2O4 + MnS) → AlN. The thermodynamic results of inclusion types calculated with FactSage software are in agreement with the experimental observation results. The inclusions in the steels containing 0.002 mass pct aluminum do not deteriorate the hot ductility. MnS inclusions whose average size, number density, and volume ratio are 1.12 μm, 15.62 mm-2, and 2.51 × 10-6 in the steel containing 0.033 mass pct aluminum reduce the ductility. In the steel containing 0.54 mass pct aluminum, AlN inclusions whose average size, number density, and volume ratio are 0.878 μm, 16.28 mm-2 and 2.82 × 10-6 can precipitate at the austenite grain boundaries, prevent dynamic recrystallization and deteriorate the hot ductility. On the contrary, in the steel containing 2.10 mass pct aluminum, the average size, number density and volume ratio of AlN inclusions change to 2.418 μm, 35.95 mm-2, and 2.55 × 10-5. They precipitate in the matrix, which do not inhibit dynamic recrystallization and thereby do not lead to poor hot ductility.

  18. Character evaluation of strength in dispersion strengthened ferritic steel. 5

    International Nuclear Information System (INIS)

    Yoshida, Fuyuki; Nakashima, Hideharu

    1997-03-01

    In order to clarify the high-temperature deformation behaviour and the origin of threshold stress of ODS martensite steel with Y 2 O 3 particles, the stress-strain curves were measured by compression test at 600 to 700degC and at strain rates from 2x10 -5 to 2x10 -3 s -1 , and the threshold stress was measured by stress abruptly loading test (SAL test) at 650degC. Further, the possibility of temperature dependence of threshold stress was discussed by estimating the activation energy for dislocations to detach the Y 2 O 3 particles. The results are summarized as follows. 1) The stress exponents of ODS martensite steel were 22-35. And the activation energy of high-temperature deformation was 742 kJ/mol. Those deformation behaviour of ODS martensite steel agrees with the deformation behaviour of ODS ferritic steel. 2) The Orowan stress and the void-hardening stress calculated from dispersion parameters approximately agreed with the threshold stress obtained by SAL test. It is concluded that the originating mechanism of the threshold stress in ODS martensite steel is the Srolovitz's one. 3) The calculated activation energy for a dislocation to detach the particles was very high compared to the thermal energy. Therefor, the threshold stress is almost independent of temperature. (author)

  19. Tool steels

    DEFF Research Database (Denmark)

    Højerslev, C.

    2001-01-01

    On designing a tool steel, its composition and heat treatment parameters are chosen to provide a hardened and tempered martensitic matrix in which carbides are evenly distributed. In this condition the matrix has an optimum combination of hardness andtoughness, the primary carbides provide...... resistance against abrasive wear and secondary carbides (if any) increase the resistance against plastic deformation. Tool steels are alloyed with carbide forming elements (Typically: vanadium, tungsten, molybdenumand chromium) furthermore some steel types contains cobalt. Addition of alloying elements...... serves primarily two purpose (i) to improve the hardenabillity and (ii) to provide harder and thermally more stable carbides than cementite. Assuming proper heattreatment, the properties of a tool steel depends on the which alloying elements are added and their respective concentrations....

  20. Experimental results of core-concrete interactions using molten steel with zirconium

    International Nuclear Information System (INIS)

    Copus, E.R.; Blose, R.E.; Brockmann, J.E.; Gomez, R.D.; Lucero, D.A.

    1990-07-01

    Four inductively sustained experiments, QT-D, QT-E, SURC-3, and SURC-3A, were performed in order to investigate the additional effects of zirconium metal oxidation on core debris-concrete interactions using molten stainless steel as the core debris simulant. The QT-D experiment ablated 18 cm of concrete axially during 50 minutes of interaction on limestone-common sand concrete using a 10 kg charge of 304 stainless steel to which 2 kg of zirconium metal was added subsequent to the onset of erosion. The QT-E experiment ablated 10 cm of limestone-common sand concrete axially and 10 cm radially during 35 minutes of sustained interaction using 50 kg of stainless steel and 10 kg of zirconium. The SURC-3 experiment had a 45 kg charge of stainless steel to which 1.1 kg of zirconium was subsequently added. SURC-3 axially eroded 33 cm of limestone concrete during two hours of interaction. The fourth experiment, SURC-3A, eroded 25 cm of limestone concrete axially and 9 cm radially during 90 minutes of sustained interaction. It utilized 40 kg of stainless steel and 2.2 kg of added zirconium as the charge material. All four experiments showed in a large increase in erosion rate, gas production, and aerosol release following the addition of Zr metal to the melt. In the SURC-3 and SURC-3A tests the measured erosion rates increased from 14 cm/hr to 27 cm/hr, gas release increased from 50 slpm to 100 slpm, and aerosol release increased from .02 q/sec to .04 q/sec. The effluent gas was composed of 80% CO, 10% CO 2 , and 2% H 2 before Zr addition and 92% CO, 4% CO 2 , 4% H 2 during the Zr interactions which lasted 10--20 minutes. Addition measurements indicated that the melt pool temperature ranged from 1600 degree C--1800 degree and that the aerosols produced were comprised primarily of Te and Fe oxides. 21 refs., 120 figs., 51 tabs

  1. Experimental results of core-concrete interactions using molten steel with zirconium

    Energy Technology Data Exchange (ETDEWEB)

    Copus, E.R.; Blose, R.E.; Brockmann, J.E.; Gomez, R.D.; Lucero, D.A. (Sandia National Labs., Albuquerque, NM (USA))

    1990-07-01

    Four inductively sustained experiments, QT-D, QT-E, SURC-3, and SURC-3A, were performed in order to investigate the additional effects of zirconium metal oxidation on core debris-concrete interactions using molten stainless steel as the core debris simulant. The QT-D experiment ablated 18 cm of concrete axially during 50 minutes of interaction on limestone-common sand concrete using a 10 kg charge of 304 stainless steel to which 2 kg of zirconium metal was added subsequent to the onset of erosion. The QT-E experiment ablated 10 cm of limestone-common sand concrete axially and 10 cm radially during 35 minutes of sustained interaction using 50 kg of stainless steel and 10 kg of zirconium. The SURC-3 experiment had a 45 kg charge of stainless steel to which 1.1 kg of zirconium was subsequently added. SURC-3 axially eroded 33 cm of limestone concrete during two hours of interaction. The fourth experiment, SURC-3A, eroded 25 cm of limestone concrete axially and 9 cm radially during 90 minutes of sustained interaction. It utilized 40 kg of stainless steel and 2.2 kg of added zirconium as the charge material. All four experiments showed in a large increase in erosion rate, gas production, and aerosol release following the addition of Zr metal to the melt. In the SURC-3 and SURC-3A tests the measured erosion rates increased from 14 cm/hr to 27 cm/hr, gas release increased from 50 slpm to 100 slpm, and aerosol release increased from .02 q/sec to .04 q/sec. The effluent gas was composed of 80% CO, 10% CO{sub 2}, and 2% H{sub 2} before Zr addition and 92% CO, 4% CO{sub 2}, 4% H{sub 2} during the Zr interactions which lasted 10--20 minutes. Addition measurements indicated that the melt pool temperature ranged from 1600{degree}C--1800{degree} and that the aerosols produced were comprised primarily of Te and Fe oxides. 21 refs., 120 figs., 51 tabs.

  2. Hot ductility and fracture mechanisms of a structural steel

    International Nuclear Information System (INIS)

    Calvo, J.; Cabrera, J. M.; Prado, J. M.

    2006-01-01

    The hot ductility of a structural steel produced from scrap recycling has been studied to determine the origin of the transverse cracks in the corners that appeared in some billets. Samples extracted both from a billet with transverse cracks and from a billet with no external damage were tested. To evaluate the influence of residual elements and inclusions, the steel was compared to another one impurity free. Reduction in area of the samples tensile tested to the fracture was taken as a measure of the hot ductility. The tests were carried out at temperatures ranging from 1000 degree centigree to 650 degree centigree and at a strain rate of 1.10-3 s-1. The fracture surfaces of the tested samples were observed by scanning electron microscopy in order to determine the embrittling mechanisms that could be acting. The steel with residuals and impurities exhibited lower ductility values for a wider temperature range than the clean steel. The embrittling mechanisms also changed as compared to the impurity free steel. (Author)

  3. Substitution of modified 9 Cr-1 Mo steel for austentic stainless steels

    International Nuclear Information System (INIS)

    Sikka, V.K.

    1982-04-01

    This report describes the current program to develop a high-strength ferritic-martensitic steel. The alloy is essentially Fe-9% Cr-1% Mo with small additions of V and Nb and is known as modifed 9 Cr-1 Mo steel. Its elevated-temperature properties and design allowable stresses match those of type 304 stainless steel for temperatures up to 600 0 C and exceed those of other ferritic steels by factors of 2 to 3. The improved strength of this alloy permits its use in place of stainless steels for many applications

  4. Flexibility and torsional behaviour of rotary nickel-titanium PathFile, RaCe ISO 10, Scout RaCe and stainless steel K-File hand instruments.

    Science.gov (United States)

    Nakagawa, R K L; Alves, J L; Buono, V T L; Bahia, M G A

    2014-03-01

    To assess and compare the flexibility and torsional resistance of PathFile, RaCe ISO 10 and Scout RaCe instruments in relation to stainless steel K-File hand instruments. Rotary PathFile (sizes 13, 16 and 19; .02 taper), Race ISO 10 (size 10; 0.02, 0.04 and 0.06 tapers), Scout RaCe (sizes 10, 15 and 20; 0.02 taper) and hand K-File (sizes 10, 15 and 20; 0.02 taper) instruments were evaluated. Alloy chemical composition, phases present and transformation temperatures were determined for the NiTi instruments. For all instruments, diameters at each millimetre from the tip as well as cross-sectional areas at 3 mm from the tip were measured based on ANSI/ADA Specification No. 101 using image analysis software. Resistance to bending and torsional resistance were determined according to specification ISO 3630-1. Vickers microhardness measurements were also taken in all instruments to assess their strength. Data were analysed using analysis of variance (α = 0.05). The alloys used in the manufacture of the three types of NiTi instruments had approximately the same chemical composition, but the PathFile instruments had a higher Af transformation temperature and contained a small amount of B19' martensite. All instruments had diameter values within the standard tolerance. The bending and torsional resistance values were significantly increased relative to the instrument diameter and cross-sectional area. PathFile instruments were the most flexible and the least torque resistant, whilst the stainless steel instruments were the least flexible although they were more torque resistant than the NiTi instruments. © 2013 International Endodontic Journal. Published by John Wiley & Sons Ltd.

  5. Weldability of Stainless Steels

    International Nuclear Information System (INIS)

    Saida, Kazuyoshi

    2010-01-01

    It gives an outline of metallographic properties of welding zone of stainless steels, generation and mechanisms of welding crack and decreasing of corrosion resistance of welding zone. It consists of seven chapters such as introduction, some kinds of stainless steels and properties, metallographic properties of welding zone, weld crack, toughness of welding zone, corrosion resistance and summary. The solidification modes of stainless steels, each solidification mode on the cross section of Fe-Cr-Ni alloy phase diagram, each solidification mode of weld stainless steels metal by electron beam welding, segregation state of alloy elements at each solidification mode, Schaeffler diagram, Delong diagram, effects of (P + S) mass content in % and Cr/Ni equivalent on solidification cracking of weld stainless steels metal, solidification crack susceptibility of weld high purity stainless steels metal, effects of trace impurity elements on solidification crack susceptibility of weld high purity stainless steels metal, ductile fracture susceptibility of weld austenitic stainless steels metal, effects of H2 and ferrite content on generation of crack of weld 25Cr-5N duplex stainless steels, effects of O and N content on toughness of weld SUS 447J1 metals, effect of ferrite content on aging toughness of weld austenitic stainless steel metal, corrosion morphology of welding zone of stainless steels, generation mechanism of knife line attack phenomenon, and corrosion potential of some kinds of metals in seawater at room temperature are illustrated. (S.Y.)

  6. Stainless steel leaches nickel and chromium into foods during cooking.

    Science.gov (United States)

    Kamerud, Kristin L; Hobbie, Kevin A; Anderson, Kim A

    2013-10-02

    Toxicological studies show that oral doses of nickel and chromium can cause cutaneous adverse reactions such as dermatitis. Additional dietary sources, such as leaching from stainless steel cookware during food preparation, are not well characterized. This study examined stainless steel grades, cooking time, repetitive cooking cycles, and multiple types of tomato sauces for their effects on nickel and chromium leaching. Trials included three types of stainless steels and a stainless steel saucepan, cooking times of 2-20 h, 10 consecutive cooking cycles, and four commercial tomato sauces. After a simulated cooking process, samples were analyzed by ICP-MS for Ni and Cr. After 6 h of cooking, Ni and Cr concentrations in tomato sauce increased up to 26- and 7-fold, respectively, depending on the grade of stainless steel. Longer cooking durations resulted in additional increases in metal leaching, where Ni concentrations increased 34-fold and Cr increased approximately 35-fold from sauces cooked without stainless steel. Cooking with new stainless steel resulted in the largest increases. Metal leaching decreases with sequential cooking cycles and stabilized after the sixth cooking cycle, although significant metal contributions to foods were still observed. The tenth cooking cycle resulted in an average of 88 μg of Ni and 86 μg of Cr leached per 126 g serving of tomato sauce. Stainless steel cookware can be an overlooked source of nickel and chromium, where the contribution is dependent on stainless steel grade, cooking time, and cookware usage.

  7. Heating temperature effect on ferritic grain size of rotor steel

    International Nuclear Information System (INIS)

    Cheremnykh, V.G.; Derevyankin, E.V.; Sakulin, A.A.

    1983-01-01

    The heating temperature effect on ferritic grain size of two steels 13Kh1M1FA and 25Kh1M1FA is evaluated. It is shown that exposure time increase at heating temperatures below 1000 deg C up to 10h changes but slightly the size of the Cr-Mo-V ferritic grain of rotor steel cooled with 25 deg C/h rate. Heating up to 1000 deg C and above leads to substantial ferritic grain growth. The kinetics of ferritic grain growth is determined by the behaviour of phases controlling the austenitic grain growth, such as carbonitrides VCsub(0.14)Nsub(0.78) in 13Kh1M1FA steel and VCsub(0.18)Nsub(0.72) in 25Kh1M1FA steel. Reduction of carbon and alloying elements content in steel composition observed at the liquation over rotor length leads to a certain decrease of ferritic grain resistance to super heating

  8. Studies on A-TIG welding of Low Activation Ferritic/Martensitic (LAFM) steel

    International Nuclear Information System (INIS)

    Vasantharaja, P.; Vasudevan, M.

    2012-01-01

    Low Activation Ferritic–Martensitic steels (LAFM) are chosen as the candidate material for structural components in fusion reactors. The structural components are generally fabricated by welding processes. Activated Tungsten Inert Gas (A-TIG) welding is an emerging process for welding of thicker components. In the present work, attempt was made to develop A-TIG welding technology for LAFM steel plates of 10 mm thick. Activated flux was developed for LAFM steel by carrying out various bead-on-plate TIG welds without flux and with flux. The optimum flux was identified as one which gave maximum depth of penetration at minimum heat input values. With the optimized flux composition, LAFM steel plate of 10 mm thickness was welded in square butt weld joint configuration using double side welding technique. Optical and Scanning Electron Microscopy was used for characterizing the microstructures. Microhardness measurements were made across the weld cross section for as welded and post weld heat treated samples. Tensile and impact toughness properties were determined. The mechanical properties values obtained in A-TIG weld joint were comparable to that obtained in weld joints of LAFM steel made by Electron beam welding process.

  9. Studies on A-TIG welding of Low Activation Ferritic/Martensitic (LAFM) steel

    Science.gov (United States)

    Vasantharaja, P.; Vasudevan, M.

    2012-02-01

    Low Activation Ferritic-Martensitic steels (LAFM) are chosen as the candidate material for structural components in fusion reactors. The structural components are generally fabricated by welding processes. Activated Tungsten Inert Gas (A-TIG) welding is an emerging process for welding of thicker components. In the present work, attempt was made to develop A-TIG welding technology for LAFM steel plates of 10 mm thick. Activated flux was developed for LAFM steel by carrying out various bead-on-plate TIG welds without flux and with flux. The optimum flux was identified as one which gave maximum depth of penetration at minimum heat input values. With the optimized flux composition, LAFM steel plate of 10 mm thickness was welded in square butt weld joint configuration using double side welding technique. Optical and Scanning Electron Microscopy was used for characterizing the microstructures. Microhardness measurements were made across the weld cross section for as welded and post weld heat treated samples. Tensile and impact toughness properties were determined. The mechanical properties values obtained in A-TIG weld joint were comparable to that obtained in weld joints of LAFM steel made by Electron beam welding process.

  10. Strain-tempering of low carbon martensite steel wire by rapid heating

    International Nuclear Information System (INIS)

    Torisaka, Yasunori; Kihara, Junji

    1978-01-01

    In the production of prestressed concrete steel wires, a series of the cold drawing-patenting process are performed to improve the strength. In order to reduce cyclic process, the low carbon martensite steel wire which can be produced only by the process of hot rolling and direct quench has been investigated as strain-tempering material. When strain-tempering is performed on the low carbon martensite steel wire, stress relaxation (Re%) increases and mechanical properties such as total elongation, reduction of area, ultimate tensile strength and proof stress decrease remarkably by annealing. In order to shorten the heating time, the authors performed on the steel wire the strain-tempering with a heating time of 1.0 s using direct electrical resistance heating and examined the effects of rapid heating on the stress relaxation and the mechanical properties. Stress relaxation decreases without impairment of the mechanical properties up to a strain-tempering temperature of 573 K. Re(%) after 10.8 ks is 0% at the testing temperature 301 K, 0.49% at 363 K and 1.39% at 433 K. (auth.)

  11. Corrosion behavior of steels in flowing lead-bismuth under abnormal conditions

    International Nuclear Information System (INIS)

    Doubkova, A.; Di Gabriele, F.; Brabec, P.; Keilova, E.

    2008-01-01

    The project IP EUROTRANS, domain DEMETRA, is primary focused on the study of the technology of the interaction between steels and heavy liquid metals. The characterization of the metal response to sudden changes, simulating accidental conditions in liquid lead-bismuth eutectic was carried out. This paper reports the results of two hot-spot simulations with two different oxygen concentrations (10 -8 wt%, 10 -6 wt%). Each experiment was divided in two main periods: the initial, long period at the standard operating temperature 550 deg. C; the second, short period, at higher temperature, 650 deg. C. The damage that occurs on the austenitic steel AISI 316L and the ferritic-martensitic steel T91 was investigated. The amount of damage for both steels was higher at lower oxygen contents and the short, hot spot simulation, markedly affected the T91. At higher oxygen content the amount of damage decreased. A few, localized pits, were observed; however, there was no visible increment in the amount of damage after the hot spot simulation

  12. austenitic steel corrosion by oxygen-containing liquid sodium

    International Nuclear Information System (INIS)

    Rivollier, Matthieu

    2017-01-01

    France is planning to construct the 4. generation of nuclear reactors. They will use liquid sodium as heat transfer fluid and will be made of 316L(N) austenitic steel as structural materials. To guarantee optimal operation on the long term, the behavior of this steel must be verified. This is why corrosion phenomena of 316L(N) steel by liquid sodium have to be well-understood. Literature points out that several corrosion phenomena are possible. Dissolved oxygen in sodium definitely influences each of the corrosion phenomenon. Therefore, the austenitic steel corrosion in oxygen-containing sodium is proposed in this study. Thermodynamics data point out that sodium chromite formation on 316L(N) steel is possible in sodium containing roughly 10 μg.g -1 of oxygen for temperature lower than 650 C (reactor operating conditions).The experimental study shows that sodium chromite is formed at 650 C in the sodium containing 200 μg.g -1 of oxygen. At the same concentration and at 550 C, sodium chromite is clearly observed only for long immersion time (≥ 5000 h). Results at 450 C are more difficult to interpret. Furthermore, the steel is depleted in chromium in all cases.The results suggest the sodium chromite is dissolved in the sodium at the same time it is formed. Modelling of sodium chromite formation - approached by chromium diffusion in steel (in grain and grain boundaries -, and dissolution - assessed by transport in liquid metal - show that simultaneous formation and dissolution of sodium chromite is a possible mechanism able to explain our results. (author) [fr

  13. Preparation and characterization of 304 stainless steel/Q235 carbon steel composite material

    Science.gov (United States)

    Shen, Wenning; Feng, Lajun; Feng, Hui; Cao, Ying; Liu, Lei; Cao, Mo; Ge, Yanfeng

    The composite material of 304 stainless steel reinforced Q235 carbon steel has been prepared by modified hot-rolling process. The resulted material was characterized by scanning electron microscope, three-electrode method, fault current impact method, electrochemical potentiodynamic polarization curve measurement and electrochemical impedance spectroscopy. The results showed that metallurgical bond between the stainless steel layer and carbon steel substrate has been formed. The composite material exhibited good electrical conductivity and thermal stability. The average grounding resistance of the composite material was about 13/20 of dip galvanized steel. There has no surface crack and bubbling formed after fault current impact. The composite material led to a significant decrease in the corrosion current density in soil solution, compared with that of hot dip galvanized steel and bare carbon steel. On the basis polarization curve and EIS analyses, it can be concluded that the composite material showed improved anti-corrosion property than hot-dip galvanized steel.

  14. Inspection of steel poles; ultrasonic testing of anchor ground rods and cathodic reactions : Corrosion detection : an emerging problem in buried steel structures

    Energy Technology Data Exchange (ETDEWEB)

    Pandey, A.K.; Randle, R.E.; Stewart, A.H. [EDM International Inc., Fort Collins, CO (United States)

    2002-07-01

    A typical inspection of steel utility poles routinely overlooks what is below ground, such as anchor rods, stub angles in lattice towers, and direct embedded steel poles. Stub angles are lap or butt spliced to the tower leg and extend several feet below ground line. A case study concerning stub angles (Oberst 1998) is discussed. An inspection of steel poles erected in 1929 revealed that 40 per cent of legs had complete loss of galvanizing, 10 per cent of legs had greater than 10 per cent loss of cross-section, and 2 per cent of legs had greater than 80 per cent loss of cross-section. All corrosion was found within one foot of ground line. A relatively new concept is direct embedded steel poles. An emerging problem concerns tree induced anchor rod corrosion. A corrosion technique for anchor rods was developed and has been commercially available for the past three years. Its effectiveness was verified at the Montana Power Company 500 kV Colstrip Project, where 3 anchor failures were detected in 1995 due to corrosion wastage. The rods are classified as being in good condition up to 10 per cent loss of cross-section, moderate corrosion for losses between 10 and 25 per cent, and excessive corrosion for losses greater than 25 per cent. The results obtained at the Montana Power Company indicated the technique was 98 per cent accurate. The authors discuss the capabilities and limitations of the technique. It was also applied for the Anchor Rod Inspection Project of the Georgia Power Company (GPC). The technique is evaluated in the laboratory, then optimized. Field prototypes are developed, followed by an evaluation at different test sites. figs.

  15. Corrosion Inhibition of AISI/SAE Steel in a Marine Environment

    Directory of Open Access Journals (Sweden)

    Fatai Olufemi ARAMIDE

    2009-12-01

    Full Text Available Effect of Sodium nitrite as a corrosion inhibitor of mild steel in sea water wasinvestigated, using the conventional weight loss method. Differentpercentages of sodium nitrite were used from 0% to 10% in sea water.Samples of mild steel were exposed to these corrosive media and the weightloss was calculated at intervals of 120 hours, 168 hours, 208 hours, 256 hours,304 hours and 352 hours. It was observed that corrosion rate increases withtime of exposure to the corrosive medium (inhibited or non-inhibited and thatsodium nitrite can be used to retards the corrosion rate of mild steel if theappropriate concentration is used in sea water. It was concluded that theoptimum percentage of sodium nitrate in sea water that gives the optimumcorrosion inhibition of mild steel is 4%.

  16. Fracture-tough, corrosion-resistant bearing steels

    Science.gov (United States)

    Olson, Gregory B.

    1990-01-01

    The fundamental principles allowing design of stainless bearing steels with enhanced toughness and stress corrosion resistance has involved both investigation of basic phenomena in model alloys and evaluation of a prototype bearing steel based on a conceptual design exercise. Progress in model studies has included a scanning Auger microprobe (SAM) study of the kinetics of interfacial segregation of embrittling impurities which compete with the kinetics of alloy carbide precipitation in secondary hardening steels. These results can define minimum allowable carbide precipitation rates and/or maximum allowable free impurity contents in these ultrahigh strength steels. Characterization of the prototype bearing steel designed to combine precipitated austenite transformation toughening with secondary hardening shows good agreement between predicted and observed solution treatment response including the nature of the high temperature carbides. An approximate equilibrium constraint applied in the preliminary design calculations to maintain a high martensitic temperature proved inadequate, and the solution treated alloy remained fully austenitic down to liquid nitrogen temperature rather than transforming above 200 C. The alloy can be martensitically transformed by cryogenic deformation, and material so processed will be studied further to test predicted carbide and austenite precipitation behavior. A mechanistically-based martensitic kinetic model was developed and parameters are being evaluated from available kinetic data to allow precise control of martensitic temperatures of high alloy steels in future designs. Preliminary calculations incorporating the prototype stability results suggest that the transformation-toughened secondary-hardening martensitic-stainless design concept is still viable, but may require lowering Cr content to 9 wt. pct. and adding 0.5 to 1.0 wt. pct. Al. An alternative design approach based on strain-induced martensitic transformation during

  17. Porous stainless steel for biomedical applications

    Directory of Open Access Journals (Sweden)

    Sabrina de Fátima Ferreira Mariotto

    2011-01-01

    Full Text Available Porous 316L austenitic stainless steel was synthesized by powder metallurgy with relative density of 0.50 and 0.30 using 15 and 30 wt. (% respectively of ammonium carbonate and ammonium bicarbonate as foaming agents. The powders were mixed in a planetary ball mill at 60 rpm for 10 minutes. The samples were uniaxially pressed at 287 MPa and subsequently vacuum heat treated in two stages, the first one at 200 ºC for 5 hours to decompose the carbonate and the second one at 1150 ºC for 2 hours to sinter the steel. The sintered samples had a close porous structure and a multimodal pore size distribution that varied with the foaming agent and its concentration. The samples obtained by addition of 30 wt. (% of foaming agents had a more homogeneous porous structure than that obtained with 15 wt. (%. The MTT cytotoxicity test (3-[4,5-dimethylthiazol]-2,5-diphenyltetrazolium bromide was used to evaluate the mitochondrial activity of L929 cells with samples for periods of 24, 48, and 72 hours. The cytotoxicity test showed that the steel foams were not toxic to fibroblast culture. The sample with the best cellular growth, therefore the most suitable for biomedical applications among those studied in this work, was produced with 30 wt. (% ammonium carbonate. In this sample, cell development was observed after 48 hours of incubation, and there was adhesion and spreading on the material after 72 hours. Electrochemical experiments using a chloride-containing medium were performed on steel foams and compared to massive steel. The massive steel had a better corrosion performance than the foams as the porosity contributes to increase the surface area exposed to the corrosive medium.

  18. Compresibility and sinterability of HCx PM steel diluted with stainless steels

    Directory of Open Access Journals (Sweden)

    Elena Gordo

    2003-12-01

    Full Text Available HCx powder metallurgy steel contains in its composition high contents of Cr and C, and significant quantities of alloy elements typical of tool steels (Mo, V, W, to provide the corrosion resistance of stainless steel with wear resistance of tool steels. HCx appears to be a suitable material for applications in aggressive environments, as valve seat inserts in automotive engines. However, this steel presents a low compressibility leading to high production costs. In this work, some results carried out to improve the compressibility of HCx are presented. The way to attempt this improvement is the dilution of base material with two stainless steels, the ferritic 430LHC and the austenitic 316L. The powder mixes prepared were uniaxially pressed to study the compressibility. The sinterability was study by determining of density, hardness, transverse rupture strength (TRS and microstructural evolution after vacuum sintering at different temperatures. As a result, better compressibility is observed in the mixes although not all of them present the properties required.

  19. Boron Steel: An Alternative for Costlier Nickel and Molybdenum Alloyed Steel for Transmission Gears

    Directory of Open Access Journals (Sweden)

    A. Verma

    2010-06-01

    Full Text Available Case Carburized (CC low carbon steels containing Ni, Cr and Mo alloying elements are widely used for transmission gears in automobile, as it possesses desired mechanical properties. In order to cut cost and save scarce materials like Ni and Mo for strategic applications, steel alloyed with Boron has been developed, which gives properties comparable to Ni-Cr-Mo alloyed steel. In the process of steel development, care was taken to ensure precipitation of boron which results in precipitation hardening. The characterization of the developed boron steel had exhibited properties comparable to Ni-Cr-Mo alloyed steel and superior to conventional boron steel.

  20. Nitrogen ion implantation effect on friction coefficient of tool steel

    International Nuclear Information System (INIS)

    Velichko, N.I.; Udovenko, V.F.; Markus, A.M.; Presnyakova, G.N.; Gamulya, G.D.

    1988-01-01

    Effect of nitrogen molecular ion implantation into KhVSG steel on the friction coefficient in the air and vacuum is investigated. Irradiation is carried out by the N 2 + beam with energy 120 keV and flux density 5 μ/cm 2 at room temperature in vacuum 5x10 -4 Pa. The integral dose of irradiation is 10 17 particle/cm 2 . Nitrogen ion implantation is shown to provide the formation of the modified layer changing friction properties of steel. The friction coefficient can either increase or decrease depending on implantation and test conditions. 4 refs.; 2 figs

  1. Microstructure of laser cladded martensitic stainless steel

    CSIR Research Space (South Africa)

    Van Rooyen, C

    2006-08-01

    Full Text Available and martensite with 10% ferrite for Material B. Table 7 - Proposed martensitic stainless steel alloys for laser cladding Material C* Cr Ni Mn Si Mo Co Ms (ºC)* Cr eq Ni eq Material A 0.4 13 - 1 0.5 2.5 5.5 120 16.5 12.5 Material B 0.2 15 2 1 0.7 2.5 5.5 117... dilution, low heat input, less distortion, increased mechanical and corrosion properties excellent repeatability and control of process parameters. Solidification of laser cladded martensitic stainless steel is primarily austenitic. Microstructures...

  2. Anthraquinones with antiplasmodial activity from the roots of Rennellia elliptica Korth. (Rubiaceae).

    Science.gov (United States)

    Osman, Che Puteh; Ismail, Nor Hadiani; Ahmad, Rohaya; Ahmat, Norizan; Awang, Khalijah; Jaafar, Faridahanim Mohd

    2010-10-20

    Dichloromethane root extract of Rennellia elliptica Korth. showed strong inhibition of Plasmodium falciparum growth in vitro with an IC₅₀ value of 4.04 µg/mL. A phytochemical study of the dichloromethane root extract has led to the isolation and characterization of a new anthraquinone, 1,2-dimethoxy-6-methyl-9,10-anthraquinone (1), and ten known anthraquinones: 1-hydroxy-2-methoxy-6-methyl-9,10-anthraquinone (2), nordamnacanthal (3), 2-formyl-3-hydroxy-9,10-anthraquinone (4), damnacanthal (5), lucidin-ω-methyl ether (6), 3-hydroxy-2-methyl-9,10-anthraquinone (7), rubiadin (8), 3-hydroxy-2-methoxy-6-methyl-9,10-anthraquinone (9), rubiadin-1-methyl ether (10) and 3-hydroxy-2-hydroxymethyl-9,10-anthraquinone (11). Structural elucidation of all compounds was accomplished by modern spectroscopic methods, notably 1D and 2D NMR, IR, UV and HREIMS. The new anthraquinone 1, 2-formyl-3-hydroxy-9,10-anthraquinone (4) and 3-hydroxy-2-methyl-9,10-anthraquinone (7) possess strong antiplasmodial activity, with IC₅₀ values of 1.10, 0.63 and 0.34 µM, respectively.

  3. A new steel with good low-temperature sulfuric acid dew point corrosion resistance

    Energy Technology Data Exchange (ETDEWEB)

    Cheng, X.Q.; Li, X.G. [Corrosion and Protection Center, University of Science and Technology Beijing (China); Key Laboratory of Corrosion and Protection (Ministry of Education), Beijing (China); Sun, F.L. [Corrosion and Protection Center, University of Science and Technology Beijing (China); Lv, S.J. [Corrosion and Protection Center, University of Science and Technology Beijing (China); Equipment and Power Department, Shijiazhuang Refine and Chemical Company Limited, SINOPEC, Shijiazhuang (China)

    2012-07-15

    In this work, new steels (1, 2, and 3) were developed for low-temperature sulfuric acid dew point corrosion. The mass loss rate, macro- and micro-morphologies and compositions of corrosion products of new steels in 10, 30, and 50% H{sub 2}SO{sub 4} solutions at its corresponding dew points were investigated by immersion test, scanning electron microscopy (SEM) and energy-dispersive spectrometry (EDS). The results indicated that mass loss rate of all the tested steels first strongly increased and then decreased as H{sub 2}SO{sub 4} concentration increased, which reached maximum at 30%. Corrosion resistance of 2 steel is the best among all specimens due to its fine and homogeneous morphologies of corrosion products. The electrochemical corrosion properties of new steels in 10 and 30% H{sub 2}SO{sub 4} solutions at its corresponding dew points were studied by potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) techniques. The results demonstrated that corrosion resistance of 2 steel is the best among all the experimental samples due to its lowest corrosion current density and highest charge transfer resistance, which is consistent with the results obtained from immersion tests. (Copyright copyright 2012 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  4. Application of the EPR technique in welded couplings in 08X18H10T (AISI 321) stainless steel

    International Nuclear Information System (INIS)

    Fuentes, D.A.; Menendez, C.M.; Dominguez, H.; Sendoya, F.

    1993-01-01

    Stainless steel samples, one AISI 304 and the other 08X18H10T of Soviet origin (equivalent to AISI 320) were welded for the TIG method, submitted to a thermal treatment in order to its sensitization against the intergranular corrosion, then the samples were submitted to the EPR technique in order to establish the sensitization degree which is an indicative of susceptibility to intergranular corrosion. The result were corroborated by two different methodologies, the ASTM A262 standard and the soviet standard GOST 6032-89. The state of the tested surface was analyzed using optical microscopy in order to quantify the number of pricking since its presence disturbs the normalized charge, Pa. (Author)

  5. Hardness of AISI type 410 martensitic steels after high temperature irradiation via nanoindentation

    Science.gov (United States)

    Waseem, Owais Ahmed; Jeong, Jong-Ryul; Park, Byong-Guk; Maeng, Cheol-Soo; Lee, Myoung-Goo; Ryu, Ho Jin

    2017-11-01

    The hardness of irradiated AISI type 410 martensitic steel, which is utilized in structural and magnetic components of nuclear power plants, is investigated in this study. Proton irradiation of AISI type 410 martensitic steel samples was carried out by exposing the samples to 3 MeV protons up to a 1.0 × 1017 p/cm2 fluence level at a representative nuclear reactor coolant temperature of 350 °C. The assessment of deleterious effects of irradiation on the micro-structure and mechanical behavior of the AISI type 410 martensitic steel samples via transmission electron microscopy-energy dispersive spectroscopy and cross-sectional nano-indentation showed no significant variation in the microscopic or mechanical characteristics. These results ensure the integrity of the structural and magnetic components of nuclear reactors made of AISI type 410 martensitic steel under high-temperature irradiation damage levels up to approximately 5.2 × 10-3 dpa.

  6. Mechanical properties of steel 8 CrMoNiNb 9 10 in dependence on the microstructural condition

    International Nuclear Information System (INIS)

    Fabritius, H.; Schnabel, E.

    1976-01-01

    Tension tests at room temperature to 600 0 C and creep-rupture tests at 500 to 600 0 C lasting up to about 75,000 h on two casts of steel 8 CrMoNiNb 9 10 with about 0.08% C, 0.3% Si, 0.7% Mn, 0.012% N, 0.005% Al, 2.34% Cr, 0.95% Mo, 0.8% Nb and 0.64% Ni in bainitic and ferritic microstructural condition. Influence of annealing at 650 to 800 0 C on the properties in the tension test. Influence of aging at 500 to 600 0 C lasting up to 30,000 h with and without mechanical stress on the properties in the tension test at aging temperature and on the toughness behaviour in the notched bar impact bend test at room temperature. (orig.) [de

  7. Heterogeneity of structure and properties of 12Cr18Ni10Ti and 08Cr16Ni11Mo3 stainless steels irradiated up to high damaging doses in reactor Bn-350

    International Nuclear Information System (INIS)

    Maksimkin, O.P.; Tivanova, O.V.; Turubarova, L.G.; Silnyagina, N.S.; Doronina, T.A.

    2006-01-01

    Full text: Earlier, during investigation of post-operating properties and structure of responsible units of fast neutron reactors there was shown /1, 2/ that depending on character of preliminary treatment of austenite stainless steel (austenization, cold deformation, mechanical and thermal treatment) radiation effects could be different. In /2/ one could observe heterogeneity at swelling of cold- worked hexahedral ducts along perimeter, in particular, the swelling of corners was less than plates'. At the same time after mechanical-thermal treatment the corners swell in 3-5 times of magnitude higher than plates. By the present there are several assumptions about nature of this phenomenon. One of them is a difference of deformation degree of material in corners and plates of the duct. It is known that /3/ external effects (including deformation) induce martensitic γ→α transformation in austenitic steels, due to which the structure and properties of steel are changed. In particular, paramagnetic FCC matrix reveals sites with ferromagnetic BCC structure. Steel heating, containing martensitic α-phase higher than ∼ 450-800 deg C, results in reverse γ→α transformation in material, which in its turn leads to formation of phase phase-hardened austenite. We can expect that only peculiarities of processes of direct and reverse martensitic transformations, which took place during preliminary austenitic steel treatment, will predetermine its behavior under irradiation. Taking into account the above mentioned there have been carried out complex material-scientific investigations of 12Cr18Ni10Ti and 08Cr16Ni11Mo3 steel samples cut off from different sites (both adjacent to corners and far from them) of hexagonal ducts of spent fuel assemblies of BN-350 reactor. There were used samples in the form of plates of different sizes: 5x10x2 mm - for metallographic investigations (microscope Neophot-2) and determination of microhardness (PMT-3); 2x20x0,3 mm - for mechanical

  8. The effect of cysteine on the corrosion of 304L stainless steel in sulphuric acid

    International Nuclear Information System (INIS)

    Silva, A.B.; Agostinho, S.M.L.; Barcia, O.E.; Cordeiro, G.G.O.; D'Elia, E.

    2006-01-01

    The effect of cysteine on the corrosion of 304L stainless steel in 1 mol l -1 H 2 SO 4 was studied using open-circuit potential measurements, anodic polarization curves, electrochemical impedance spectroscopy (EIS) and scanning electron microscopy (SEM). All the electrochemical measurements obtained in the presence of low cysteine concentration (10 -6 -10 -5 mol l -1 ) presented the same behaviour as those obtained in the absence of cysteine, a passivated steel surface. However, for higher cysteine concentrations (10 -4 -10 -2 mol l -1 ), a different behaviour was observed: the corrosion potential stabilized at a more negative value; an active region was observed in the anodic polarization curves and the electrochemical impedance diagrams showed an inductive loop at lower frequencies and a much lower polarization resistance. These results show that the presence of cysteine at high concentration turns the surface of 304L stainless steel electrochemically active, probably dissolving the passivation layer and promoting the stainless steel anodic dissolution. SEM experiments performed after immersion experiments at corrosion potential were in good agreement with the electrochemical results

  9. AWWA C303-17 concrete pressure pipe, bar-wrapped, steel-cylinder type

    CERN Document Server

    2017-01-01

    This standard describes the manufacture of concrete pressure pipe, reinforced with a steel cylinder that is helically wrapped with mild steel bar reinforcement, in sizes ranging from 10 in. through 72 in. (250 mm through 1,830 mm), inclusive, and for working pressures up to 400 psi (2,760 kPa).

  10. Fe-Cr-V ternary alloy-based ferritic steels for high- and low-temperature applications

    International Nuclear Information System (INIS)

    Rieth, M.; Materna-Morris, E.; Dudarev, S.L.; Boutard, J.-L.; Keppler, H.; Mayor, J.

    2009-01-01

    The phase stability of alloys and steels developed for application in nuclear fission and fusion technology is one of the decisive factors determining the potential range of operating temperatures and radiation conditions that the core elements of a power plant can tolerate. In the case of ferritic and ferritic-martensitic steels, the choice of the chemical composition is dictated by the phase diagram for binary FeCr alloys where in the 0-9% range of Cr composition the alloy remains in the solid solution phase at and below the room temperature. For Cr concentrations exceeding 9% the steels operating at relatively low temperatures are therefore expected to exhibit the formation of α' Cr-rich precipitates. These precipitates form obstacles for the propagation of dislocations, impeding plastic deformation and embrittling the material. This sets the low temperature limit for the use of of high (14% to 20%) Cr steels, which for the 20% Cr steels is at approximately 600 deg. C. On the other hand, steels containing 12% or less Cr cannot be used at temperatures exceeding ∼600 deg. C due to the occurrence of the α-γ transition (912 deg. C in pure iron and 830 deg. C in 7% Cr alloy), which weakens the steel in the high temperature limit. In this study, we investigate the physical properties of a concentrated ternary alloy system that attracted relatively little attention so far. The phase diagram of ternary Fe-Cr-V alloy shows no phase boundaries within a certain broad range of Cr and V concentrations. This makes the alloy sufficiently resistant to corrosion and suggests that steels and dispersion strengthened materials based on this alloy composition may have better strength and stability at high temperatures. Experimental heats were produced on a laboratory scale by arc melting the material components to pellets, then by melting the pellets in an induction furnace and casting the melt into copper moulds. The compositions in weight percent (iron base) are 10Cr5V, 10Cr

  11. Interaction model of steel ladle of continuous caster in steel works

    Directory of Open Access Journals (Sweden)

    Huang Bang Fu

    2016-01-01

    Full Text Available For further research on the precondition and interoperability model of interaction ladles among continuous caster, this article takes steel ladle of Y steel works as the object of research. On the basis of turnover number calculation model of single cast steel ladle, the relationship between cast number and the turnover number and turnover times and last turnover number are further analyzed. The simulation of steel ladle turnover rules was taken on the 2 continuous casters with Gantt chart. After that, the relationships between turnover number and last turnover number and non-turnover number are researched deeply. Combining with the Gantt chart, the expressions of start casting time and empty ladle ending time and heavy ladle starting time were put forward. The precondition of steel ladle interaction is obtained, which means the exchange ladle should not undertaking transport task in first stop continuous caster, and the empty ladle end time of exchange ladle of first stop continuous caster should early than the heavy ladle start time of last stop continuous caster. After applying the model to practice, 3 steel ladles of No.2 continuous caster can be reduced. This research results is supplying theoretical basis for steel ladle controlling and production organization optimization, and enriches the theory and method of metallurgical process integration.

  12. Partial substitution of vanadium by niobium in AISI H13 steel

    International Nuclear Information System (INIS)

    Itman Filho, A.; Balancin, O.

    1987-01-01

    The aim of this work was to study the tempering resistence in conditions of use of the AISI H13 steel, after partial substitution of vanadium by niobium. Four alloys of this steel were elaborated and in three of them the niobim was added in the contents of 0,2; 0,5 and 1,0%. Metallographic techniques were performed to compare qualitatively the niobium effect in several processing and thermal analisys of the steels. Grain size measurements were made after austenitization of the steels, hardness measurements in prepared samples were made after quenching and tempering, tensile testing at elevated temperature was investigated and yield strength, reduction of area after steel breaking and elongation were calculated. After these studies it was possible to certify that the partial substitution of vanadium by niobium did not alter significantly the basic mechanical properties of the AISI H13. (Author) [pt

  13. Slurry Erosion Behavior of F6NM Stainless Steel and High-Velocity Oxygen Fuel-Sprayed WC-10Co-4Cr Coating

    Science.gov (United States)

    Cui, S. Y.; Miao, Q.; Liang, W. P.; Huang, B. Z.; Ding, Z.; Chen, B. W.

    2017-02-01

    WC-10Co-4Cr coating was applied to the surface of F6NM stainless steel by high-velocity oxygen-fuel spraying. The slurry erosion behavior of the matrix and coating was examined at different rotational speeds using a self-made machine. This experiment effectively simulates real slurry erosion in an environment with high silt load. At low velocity (<6 m/s), the main failure mechanism was cavitation. Small bubbles acted as an air cushion, obstructing direct contact between sand and the matrix surface. However, at velocity above 9 m/s, abrasive wear was the dominant failure mechanism. The results indicate that WC-10Co-4Cr coating significantly improved the slurry resistance at higher velocity, because it created a thin and dense WC coating on the surface.

  14. Water requirements of the iron and steel industry

    Science.gov (United States)

    Walling, Faulkner B.; Otts, Louis Ethelbert

    1967-01-01

    concentrate. Water use in concentration plants is related to the physical state of the ore. The data in this report indicate that grain size of the ore is the most important factor; the very fine grained taconite and jasper required the greatest amount of water. Reuse was not widely practiced in the iron ore industry.Consumption of water by integrated steel plants ranged from 0 to 2,010 gallons per ton of ingot steel and by steel processing plants from 120 to 3,420 gallons per ton. Consumption by a typical integrated steel plant was 681 gallons per ton of ingot steel, about 1.8 percent of the intake and about 1 percent of the gross water use. Consumption by a typical steel processing plant was 646 gallons per ton, 18 percent of the intake, and 3.2 percent of the gross water use. The quality of available water was found not to be a critical factor in choosing the location of steel plants, although changes in equipment and in operating procedures are necessary when poor-quality water is used. The use of saline water having a concentration of dissolved solids as much as 10,400 ppm (parts per million) was reported. This very saline water was used for cooling furnaces and for quenching slag. In operations such as rolling steel in which the water comes into contact with the steel being processed, better quality water is used, although water containing as much as 3,410 ppm dissolved solids has been used for this purpose. Treatment of water for use in the iron and steel industry was not widely practiced. Disinfection and treatment for scale and corrosion control were the most frequently used treatment methods.

  15. Friction stir welding of F/M ODS steel plug and F/M steel tube

    Energy Technology Data Exchange (ETDEWEB)

    Kang, Suk Hoon, E-mail: shkang77@kaeri.re.kr [Nuclear Materials Division, Korea Atomic Energy Research Institute (Korea, Republic of); Vasudevan, M. [Materials Technology Division, Indira Gandhi Centre for Atomic Research, Kalpakkam (India); Noh, Sanghoon; Jin, Hyun Ju; Jang, Jinsung; Kim, Tae Kyu [Nuclear Materials Division, Korea Atomic Energy Research Institute (Korea, Republic of)

    2016-11-01

    Highlights: • Friction stir welding (FSW) was used for joining of oxide dispersion strengthened (ODS) steel plug and F/M steel tube. • The curvature and smaller thickness of tube was the major limitation for applying FSW method, it was solved using specially designed jig. • Considerable hardening occurs in the joint because the cooling rate was sufficient to reproduce a martensitic microstructure. • The measured hoop strength of the FSWed joint was 70–90 MPa, the value was at around 70% of the tube. - Abstract: Friction stir welding (FSW) was used for joining of oxide dispersion strengthened (ODS) steel plug and F/M steel tube. The dimensions of the tube included outer diameter of 7 mm, wall thickness of 0.5 mm. The objective was to find suitable process variables for gaining enough frictional heat from those thin and curved pieces. A specially designed jig was used for stabilization and slow rotation of tube during FSW. Additionally, the plug was designed to overlap the tube. Inconel 718 was used as FSW tool, the diameter was 3.5 mm. The adequate rotation speed of the tool and jig were 1200 rpm and 1.5 rpm, respectively. The joining was successfully accomplished using above combination, showing a good possibility. The hoop stress tests of joint were conducted by blowing Ar gas into the tube, the flow rate of gas was 10 MPa/min. The measured hoop stress was 70–90 MPa, the value was at around 70% of the tube.

  16. Friction stir welding of F/M ODS steel plug and F/M steel tube

    International Nuclear Information System (INIS)

    Kang, Suk Hoon; Vasudevan, M.; Noh, Sanghoon; Jin, Hyun Ju; Jang, Jinsung; Kim, Tae Kyu

    2016-01-01

    Highlights: • Friction stir welding (FSW) was used for joining of oxide dispersion strengthened (ODS) steel plug and F/M steel tube. • The curvature and smaller thickness of tube was the major limitation for applying FSW method, it was solved using specially designed jig. • Considerable hardening occurs in the joint because the cooling rate was sufficient to reproduce a martensitic microstructure. • The measured hoop strength of the FSWed joint was 70–90 MPa, the value was at around 70% of the tube. - Abstract: Friction stir welding (FSW) was used for joining of oxide dispersion strengthened (ODS) steel plug and F/M steel tube. The dimensions of the tube included outer diameter of 7 mm, wall thickness of 0.5 mm. The objective was to find suitable process variables for gaining enough frictional heat from those thin and curved pieces. A specially designed jig was used for stabilization and slow rotation of tube during FSW. Additionally, the plug was designed to overlap the tube. Inconel 718 was used as FSW tool, the diameter was 3.5 mm. The adequate rotation speed of the tool and jig were 1200 rpm and 1.5 rpm, respectively. The joining was successfully accomplished using above combination, showing a good possibility. The hoop stress tests of joint were conducted by blowing Ar gas into the tube, the flow rate of gas was 10 MPa/min. The measured hoop stress was 70–90 MPa, the value was at around 70% of the tube.

  17. Variation of transition temperatures from upper to lower bainites in plain carbon steels

    International Nuclear Information System (INIS)

    Oka, M.; Okamoto, H.

    1995-01-01

    Experimental results and explanations for the transition temperature from upper to lower bainites in carbon steels containing from 0.20 to 1.80 wt%C were presented metallographically and kinematically. The experimental results are summarized as follows: (1) Lower bainite is not formed in steels with less than 0.35 wt%C and no transition from upper to lower bainite occurs. (2) The transition temperature of steels containing from 0.54 to 1.10 %C indicates a constant temperature of 350 C and does not depend on the carbon content. It is important to note that a transition temperature of 350 C corresponds to the Ms temperature of a 0.55%C steel being the boundary of the martensite morphology between a lath and a plate. (3) Transition temperatures of steels with more than 1.10%C decrease along the a line below about 65 C from T 0 -composition line. The bainitic transformation is essentially a kind of the martensitic one and its nucleation site is considered to be a carbon depleted zone in austenite by the thermal fluctuation of carbon atom at an isothermal holding temperature. The supercooling of about 65 C below the T 0 -composition line at the carbon range more than 1.10 wt%C is attributed to the non-chemical free energy for the displacive growth of lower bainite. (orig.)

  18. Effect of nanoprecipitates and grain size on the mechanical properties of advanced structural steels

    International Nuclear Information System (INIS)

    Suarez, M.A.; Alvarez-Perez, M.A.; Alvarez-Fregoso, O.; Juarez-Islas, J.A.

    2011-01-01

    Highlights: → The composition of the steel responded positively to the thermomechanical processing. → Yield strength was increased due to micrometric grain size of 2.2 μm. → Mechanical properties were improved due to nanometric precipitates of 5 nm. → Yield strength values of the API steel were improved up to 877.9 MPa. - Abstract: The microstructure and nanometric precipitates present in advanced structured steel have been studied by high resolution transmission electron microscopy equipped with energy dispersion X-ray microanalysis, in order to relate the nanometric precipitates and grain size with the improvement of the yield strength value of the API steel. The microstructure and nanometric precipitates of the advanced steel were obtained by a combination of thermo-mechanical controlled hot rolling and accelerated cooling procedures. The API steel composition consisted of hot rolled Nb-Ti microalloyed with: 0.07C, 1.40Mn, 0.24Si, 0.020Al, 0.009P, 0.001S, 0.05Mo, 0.5Cr, 0.05Nb, 0.25Ni, 0.10Cu, 0.012Ti, 0.05N in wt%. As a result, this hot rolled steel tested at a strain rate of 5 x 10 -3 s -1 showed an improved yield strength from 798 MPa to 878 MPa due to the micrometric grain size of 2.2 μm and to the nanometric precipitates with a size of around 5 nm in the microstructure of the steel studied.

  19. 1-Amino-4-hydroxy-9,10-anthraquinone - An analogue of anthracycline anticancer drugs, interacts with DNA and induces apoptosis in human MDA-MB-231 breast adinocarcinoma cells: Evaluation of structure-activity relationship using computational, spectroscopic and biochemical studies.

    Science.gov (United States)

    Mondal, Palash; Roy, Sanjay; Loganathan, Gayathri; Mandal, Bitapi; Dharumadurai, Dhanasekaran; Akbarsha, Mohammad A; Sengupta, Partha Sarathi; Chattopadhyay, Shouvik; Guin, Partha Sarathi

    2015-12-01

    The X-ray diffraction and spectroscopic properties of 1-amino-4-hydroxy-9,10-anthraquinone (1-AHAQ), a simple analogue of anthracycline chemotherapeutic drugs were studied by adopting experimental and computational methods. The optimized geometrical parameters obtained from computational methods were compared with the results of X-ray diffraction analysis and the two were found to be in reasonably good agreement. X-ray diffraction study, Density Functional Theory (DFT) and natural bond orbital (NBO) analysis indicated two types of hydrogen bonds in the molecule. The IR spectra of 1-AHAQ were studied by Vibrational Energy Distribution Analysis (VEDA) using potential energy distribution (PED) analysis. The electronic spectra were studied by TDDFT computation and compared with the experimental results. Experimental and theoretical results corroborated each other to a fair extent. To understand the biological efficacy of 1-AHAQ, it was allowed to interact with calf thymus DNA and human breast adino-carcinoma cell MDA-MB-231. It was found that the molecule induces apoptosis in this adinocarcinoma cell, with little, if any, cytotoxic effect in HBL-100 normal breast epithelial cell.

  20. Corrosion of austenitic steels and their components in vanadium-containing chloride melts

    Science.gov (United States)

    Abramov, A. V.; Polovov, I. B.; Rebrin, O. I.; Lisienko, D. G.

    2014-08-01

    The corrosion of austenitic 12Kh18N10T, 10Kh17N13M2T, and 03Kh17N14M3 steels and their components (Cr, Fe, Ni, Mo) in NaCl-KCl-VCl2 melts with 5 wt % V at 750°C is studied. The rates and mechanisms of corrosion of the materials under these conditions are determined. The processes that occur during contact of the metals and steels with vanadium-containing chloride electrolytes are investigated.