WorldWideScience

Sample records for rubber biological implants

  1. 3D silicone rubber interfaces for individually tailored implants.

    Science.gov (United States)

    Stieghorst, Jan; Bondarenkova, Alexandra; Burblies, Niklas; Behrens, Peter; Doll, Theodor

    2015-01-01

    For the fabrication of customized silicone rubber based implants, e.g. cochlear implants or electrocortical grid arrays, it is required to develop high speed curing systems, which vulcanize the silicone rubber before it runs due to a heating related viscosity drop. Therefore, we present an infrared radiation based cross-linking approach for the 3D-printing of silicone rubber bulk and carbon nanotube based silicone rubber electrode materials. Composite materials were cured in less than 120 s and material interfaces were evaluated with scanning electron microscopy. Furthermore, curing related changes in the mechanical and cell-biological behaviour were investigated with tensile and WST-1 cell biocompatibility tests. The infrared absorption properties of the silicone rubber materials were analysed with fourier transform infrared spectroscopy in transmission and attenuated total reflection mode. The heat flux was calculated by using the FTIR data, emissivity data from the infrared source manufacturer and the geometrical view factor of the system.

  2. EPDM Rubber Modified by Nitrogen Plasma Immersion Ion Implantation.

    Science.gov (United States)

    Kondyurin, Alexey

    2018-04-24

    Ethylene-propylene diene monomer rubber (EPDM) was treated by plasma immersion ion implantation (PIII) with nitrogen ions of 20 keV energy and fluence from 10 13 to 10 16 ions/cm². The Fourier-transform infrared attenuated total reflection spectra, atomic force microscopy and optical microscopy showed significant structure changes of the surface. The analysis of an interface of PIII treated EPDM rubber with polyurethane binder showed a cohesive character of the adhesion joint fracture at the presence of solvent and interpreted as covalent bond network formation between the PIII treated rubber and the adhesive.

  3. EPDM Rubber Modified by Nitrogen Plasma Immersion Ion Implantation

    Directory of Open Access Journals (Sweden)

    Alexey Kondyurin

    2018-04-01

    Full Text Available Ethylene-propylene diene monomer rubber (EPDM was treated by plasma immersion ion implantation (PIII with nitrogen ions of 20 keV energy and fluence from 1013 to 1016 ions/cm2. The Fourier-transform infrared attenuated total reflection spectra, atomic force microscopy and optical microscopy showed significant structure changes of the surface. The analysis of an interface of PIII treated EPDM rubber with polyurethane binder showed a cohesive character of the adhesion joint fracture at the presence of solvent and interpreted as covalent bond network formation between the PIII treated rubber and the adhesive.

  4. Biofunctionalization of silicone rubber with microgroove-patterned surface and carbon-ion implantation to enhance biocompatibility and reduce capsule formation

    Directory of Open Access Journals (Sweden)

    Lei ZY

    2016-10-01

    Full Text Available Ze-yuan Lei, Ting Liu, Wei-juan Li, Xiao-hua Shi, Dong-li Fan Department of Plastic and Cosmetic Surgery, XinQiao Hospital, The Third Military Medical University, ChongQing, People’s Republic of China Purpose: Silicone rubber implants have been widely used to repair soft tissue defects and deformities. However, poor biocompatibility can elicit capsule formation, usually resulting in prosthesis contracture and displacement in long-term usage. To overcome this problem, this study investigated the properties of silicone rubber materials with or without a microgroove-patterned surface and with or without carbon (C-ion implantation. Materials and methods: Atomic force microscopy, X-ray photoelectron spectroscopy, and a water contact angle test were used to characterize surface morphology and physicochemical properties. Cytocompatibility was investigated by a cell adhesion experiment, immunofluorescence staining, a Cell Counting Kit-8 assay, and scanning electron microscopy in vitro. Histocompatibility was evaluated by studying the inflammatory response and fiber capsule formation that developed after subcutaneous implantation in rats for 7 days, 15 days, and 30 days in vivo. Results: Parallel microgrooves were found on the surfaces of patterned silicone rubber (P-SR and patterned C-ion-implanted silicone rubber (PC-SR. Irregular larger peaks and deeper valleys were present on the surface of silicone rubber implanted with C ions (C-SR. The silicone rubber surfaces with microgroove patterns had stable physical and chemical properties and exhibited moderate hydrophobicity. PC-SR exhibited moderately increased dermal fibroblast cell adhesion and growth, and its surface microstructure promoted orderly cell growth. Histocompatibility experiments on animals showed that both the anti-inflammatory and antifibrosis properties of PC-SR were slightly better than those of the other materials, and there was also a lower capsular contracture rate and less

  5. Biological Reclaiming of Recycled Rubber and Its Effect on Mechanical Properties of New Rubber Vulcanizates

    Directory of Open Access Journals (Sweden)

    Maryam Mansourirad

    2014-12-01

    Full Text Available Nowadays, due to environmental concerns, there has been great attention to recycling and reclaiming of tires. Different methods have been used for reclaiming or desulfurization of rubber. One of these methods, in which desulfurization of rubber happens with no damage to the polymer structure, is desulfurization by biological microorganisms. In this research the application and performance of thermophilic and sulfur oxidizing bacteria, Acidianus brierleyi for this purpose was investigated. Ground tire rubber was detoxified with organic solvents, and the optimum conditions for growing microorganisms in the existence of rubber powder in the shaker flasks were determined. In order to accelerate the process, the suitable conditions for growth of bacteria and desulfurization in the bioreactor were adopted. Fourier transfer infrared spectroscopy and scanning electron microscopy were employed to characterize desulfurization of bio-treated powder from bioreactor. The results indicated that morphological changes on powder surface and reduction of sulfur bonds have occurred. Samples from bioreactors, with and without bacteria and also untreated rubber powder were compounded with virgin styrene butadiene rubber. Tensile and dynamic properties were investigated using uni-direction tensile test and dynamic-mechanical-thermal analysis, respectively. Although some differences in dynamic-mechanical-thermal properties of samples pointed to stronger interaction between rubber matrix and treated rubber powder, no significant improvements in the mechanical properties of vulcanizates containing A.brierleyi-treated powder were observed. Low concentration of sulfur in rubber vulcanizates, chemical bonds of sulfur, and low efficiency of A. brierleyi in breaking sulfur bonds and reclaiming rubber were considered as the reasons for low efficiency of this treatment process.

  6. Electrical and optical properties of nitrile rubber modified by ion implantation

    Science.gov (United States)

    S, Najidha; Predeep, P.

    2014-10-01

    Implantation of N+ ion beams are performed on to a non-conjugated elastomer, acrylonirtle butadiene rubber (NBR) with energy 60 keV in the fluence range of 1014 to 1016 ions/cm2. A decrease in the resistivity of the sample by about eight orders of magnitude is observed in the implanted samples along with color changes. The ion exposed specimens were characterized by means of UV/Vis spectroscopy which shows a shift in the absorption edge value for the as deposited polymer towards higher wavelengths. The band gap is evaluated from the absorption spectra and is found to decrease with increasing fluence. This study can possibly throw light on ion induced changes in the polymer surface.

  7. Electrical and optical properties of nitrile rubber modified by ion implantation

    Energy Technology Data Exchange (ETDEWEB)

    S, Najidha [Department of Physics, B.J.M Govt: college, Chavara, Kollam, Kerala (India); Predeep, P. [Laboratory for molecular Photonics and Electronics, Department of Physics, National Institute of Technology, Calicut (India)

    2014-10-15

    Implantation of N{sup +} ion beams are performed on to a non-conjugated elastomer, acrylonirtle butadiene rubber (NBR) with energy 60 keV in the fluence range of 10{sup 14} to 10{sup 16} ions/cm{sup 2}. A decrease in the resistivity of the sample by about eight orders of magnitude is observed in the implanted samples along with color changes. The ion exposed specimens were characterized by means of UV/Vis spectroscopy which shows a shift in the absorption edge value for the as deposited polymer towards higher wavelengths. The band gap is evaluated from the absorption spectra and is found to decrease with increasing fluence. This study can possibly throw light on ion induced changes in the polymer surface.

  8. Toward 3D Printing of Medical Implants: Reduced Lateral Droplet Spreading of Silicone Rubber under Intense IR Curing.

    Science.gov (United States)

    Stieghorst, Jan; Majaura, Daniel; Wevering, Hendrik; Doll, Theodor

    2016-03-01

    The direct fabrication of silicone-rubber-based individually shaped active neural implants requires high-speed-curing systems in order to prevent extensive spreading of the viscous silicone rubber materials during vulcanization. Therefore, an infrared-laser-based test setup was developed to cure the silicone rubber materials rapidly and to evaluate the resulting spreading in relation to its initial viscosity, the absorbed infrared radiation, and the surface tensions of the fabrication bed's material. Different low-adhesion materials (polyimide, Parylene-C, polytetrafluoroethylene, and fluorinated ethylenepropylene) were used as bed materials to reduce the spreading of the silicone rubber materials by means of their well-known weak surface tensions. Further, O2-plasma treatment was performed on the bed materials to reduce the surface tensions. To calculate the absorbed radiation, the emittance of the laser was measured, and the absorptances of the materials were investigated with Fourier transform infrared spectroscopy in attenuated total reflection mode. A minimum silicone rubber spreading of 3.24% was achieved after 2 s curing time, indicating the potential usability of the presented high-speed-curing process for the direct fabrication of thermal-curing silicone rubbers.

  9. Osteopontin (OPN is an important protein to mediate improvements in the biocompatibility of C ion-implanted silicone rubber.

    Directory of Open Access Journals (Sweden)

    Shao-liang Wang

    Full Text Available Medical device implants are drawing increasing amounts of interest from modern medical practitioners. However, this attention is not evenly spread across all such devices; most of these implantable devices can cause adverse reactions such as inflammation, fibrosis, thrombosis, and infection. In this work, the biocompatibility of silicone rubber (SR was improved through carbon (C ion implantation. Scanning electron microscopy (SEM, atomic force microscopy (AFM, X-ray photoelectron spectroscopy (XPS, and X-ray diffraction (XRD results confirmed that these newly generated carbon-implanted silicone rubbers (C-SRs had large, irregular peaks and deep valleys on their surfaces. The water contact angle of the SR surface decreased significantly after C ion implantation. C ion implantation also changed the surface charge distribution, silicone oxygen rate, and chemical-element distribution of SR to favor cell attachment. The dermal fibroblasts cultured on the surface C-SR grew faster and showed more typical fibroblastic shapes. The expression levels of major adhesion proteins, including talin-1, zyxin, and vinculin, were significantly higher in dermal fibroblasts cultured on C-SR coated plates than in dermal fibroblasts cultured on SR. Those same dermal fibroblasts on C-SRs showed more pronounced adhesion and migration abilities. Osteopontin (OPN, a critical extracellular matrix (ECM protein, was up-regulated and secreted from dermal fibroblasts cultured on C-SR. Matrix metalloproteinase-9 (MMP-9 activity was also increased. These cells were highly mobile and were able to adhere to surfaces, but these abilities were inhibited by the monoclonal antibody against OPN, or by shRNA-mediated MMP-9 knockdown. Together, these results suggest that C ion implantation significantly improves SR biocompatibility, and that OPN is important to promote cell adhesion to the C-SR surface.

  10. RTV silicone rubber surface modification for cell biocompatibility by negative-ion implantation

    International Nuclear Information System (INIS)

    Zheng, Chenlong; Wang, Guangfu; Chu, Yingjie; Xu, Ya; Qiu, Menglin; Xu, Mi

    2016-01-01

    Highlights: • The radiation effect has a greater influence than doping effect on the hydrophilicity of RTV SR. • The implanted ions result in a new surface atomic bonding state and morphology. • Generating hydrophilic functional groups is a reason for the improved cell biocompatibility. • The micro roughness makes the hydrophilicity should be reduced due to the lotus effect. • Cell culture demonstrates that negative-ion implantation can improve biocompatibility. - Abstract: A negative cluster ion implantation system was built on the injector of a GIC4117 tandem accelerator. Next, the system was used to study the surface modification of room temperature vulcanization silicone rubber (RTV SR) for cell biocompatibility. The water contact angle was observed to decrease from 117.6° to 99.3° as the C_1"− implantation dose was increased to 1 × 10"1"6 ions/cm"2, and the effects of C_1"−, C_2"− and O_1"− implantation result in only small differences in the water contact angle at 3 × 10"1"5 ions/cm"2. These findings indicate that the hydrophilicity of RTV SR improves as the dose is increased and that the radiation effect has a greater influence than the doping effect on the hydrophilicity. There are two factors influence hydrophilicity of RTV: (1) based on the XPS and ATR-FTIR results, it can be inferred that ion implantation breaks the hydrophobic functional groups (Si−CH_3, Si−O−Si, C−H) of RTV SR and generates hydrophilic functional groups (−COOH, −OH, Si−(O)_x (x = 3,4)). (2) SEM reveals that the implanted surface of RTV SR appears the micro roughness such as cracks and wrinkles. The hydrophilicity should be reduced due to the lotus effect (Zhou Rui et al., 2009). These two factors cancel each other out and make the C-implantation sample becomes more hydrophilic in general terms. Finally, cell culture demonstrates that negative ion-implantation is an effective method to improve the cell biocompatibility of RTV SR.

  11. RTV silicone rubber surface modification for cell biocompatibility by negative-ion implantation

    Energy Technology Data Exchange (ETDEWEB)

    Zheng, Chenlong [Key Laboratory of Beam Technology and Material Modification Ministry of Education, College of Nuclear Science and Technology, Beijing Normal University, 100875 Beijing (China); Wang, Guangfu, E-mail: 88088@bnu.edu.cn [Key Laboratory of Beam Technology and Material Modification Ministry of Education, College of Nuclear Science and Technology, Beijing Normal University, 100875 Beijing (China); Beijing Radiation Center, 100875 Beijing (China); Chu, Yingjie; Xu, Ya; Qiu, Menglin; Xu, Mi [Key Laboratory of Beam Technology and Material Modification Ministry of Education, College of Nuclear Science and Technology, Beijing Normal University, 100875 Beijing (China)

    2016-03-01

    Highlights: • The radiation effect has a greater influence than doping effect on the hydrophilicity of RTV SR. • The implanted ions result in a new surface atomic bonding state and morphology. • Generating hydrophilic functional groups is a reason for the improved cell biocompatibility. • The micro roughness makes the hydrophilicity should be reduced due to the lotus effect. • Cell culture demonstrates that negative-ion implantation can improve biocompatibility. - Abstract: A negative cluster ion implantation system was built on the injector of a GIC4117 tandem accelerator. Next, the system was used to study the surface modification of room temperature vulcanization silicone rubber (RTV SR) for cell biocompatibility. The water contact angle was observed to decrease from 117.6° to 99.3° as the C{sub 1}{sup −} implantation dose was increased to 1 × 10{sup 16} ions/cm{sup 2}, and the effects of C{sub 1}{sup −}, C{sub 2}{sup −} and O{sub 1}{sup −} implantation result in only small differences in the water contact angle at 3 × 10{sup 15} ions/cm{sup 2}. These findings indicate that the hydrophilicity of RTV SR improves as the dose is increased and that the radiation effect has a greater influence than the doping effect on the hydrophilicity. There are two factors influence hydrophilicity of RTV: (1) based on the XPS and ATR-FTIR results, it can be inferred that ion implantation breaks the hydrophobic functional groups (Si−CH{sub 3}, Si−O−Si, C−H) of RTV SR and generates hydrophilic functional groups (−COOH, −OH, Si−(O){sub x} (x = 3,4)). (2) SEM reveals that the implanted surface of RTV SR appears the micro roughness such as cracks and wrinkles. The hydrophilicity should be reduced due to the lotus effect (Zhou Rui et al., 2009). These two factors cancel each other out and make the C-implantation sample becomes more hydrophilic in general terms. Finally, cell culture demonstrates that negative ion-implantation is an effective method

  12. Ion implantation and bio-compatibility

    Energy Technology Data Exchange (ETDEWEB)

    Suzuki, Yoshiaki; Kusakabe, Masahiro [Sony Corp., Tokyo (Japan). Corporate Research Labs.; Iwaki, Masaya

    1992-07-01

    Surface modification of polymers by ion implantation has been carried out to control surface properties such as conductivity, wettability, blood and tissue compatibility. Ion implantation into silicone rubber, polystyrene and segmented polyurethane was performed at 150 keV with doses ranging from 1 x 10[sup 15] to 3 x 10[sup 17] ions/cm[sup 2] to improve bio-compatibility. The platelet accumulation on ion implanted silicone rubber decreased and non-thrombogenicity of ion implanted specimens were improved. The ion implanted polystyrene and segmented polyurethane have been found to exhibit remarkably higher adhesion and spreading of endothelial cells compared to the non-implanted case. It is concluded that ion implantation into polymers is effective in controlling their bio-compatibility. (author).

  13. In-depth proteome analysis of the rubber particle of Hevea brasiliensis (para rubber tree).

    Science.gov (United States)

    Dai, Longjun; Kang, Guijuan; Li, Yu; Nie, Zhiyi; Duan, Cuifang; Zeng, Rizhong

    2013-05-01

    The rubber particle is a special organelle in which natural rubber is synthesised and stored in the laticifers of Hevea brasiliensis. To better understand the biological functions of rubber particles and to identify the candidate rubber biosynthesis-related proteins, a comprehensive proteome analysis was performed on H. brasiliensis rubber particles using shotgun tandem mass spectrometry profiling approaches-resulting in a thorough report on the rubber particle proteins. A total of 186 rubber particle proteins were identified, with a range in relative molecular mass of 3.9-194.2 kDa and in isoelectric point values of 4.0-11.2. The rubber particle proteins were analysed for gene ontology and could be categorised into eight major groups according to their functions: including rubber biosynthesis, stress- or defence-related responses, protein processing and folding, signal transduction and cellular transport. In addition to well-known rubber biosynthesis-related proteins such as rubber elongation factor (REF), small rubber particle protein (SRPP) and cis-prenyl transferase (CPT), many proteins were firstly identified to be on the rubber particles, including cyclophilin, phospholipase D, cytochrome P450, small GTP-binding protein, clathrin, eukaryotic translation initiation factor, annexin, ABC transporter, translationally controlled tumour protein, ubiquitin-conjugating enzymes, and several homologues of REF, SRPP and CPT. A procedure of multiple reaction monitoring was established for further protein validation. This comprehensive proteome data of rubber particles would facilitate investigation into molecular mechanisms of biogenesis, self-homeostasis and rubber biosynthesis of the rubber particle, and might serve as valuable biomarkers in molecular breeding studies of H. brasiliensis and other alternative rubber-producing species.

  14. The use of an ion-beam source to alter the surface morphology of biological implant materials

    Science.gov (United States)

    Weigand, A. J.

    1978-01-01

    An electron-bombardment ion-thruster was used as a neutralized-ion-beam sputtering source to texture the surfaces of biological implant materials. The materials investigated included 316 stainless steel; titanium-6% aluminum, 4% vanadium; cobalt-20% chromium, 15% tungsten; cobalt-35% nickel, 20% chromium, 10% molybdenum; polytetrafluoroethylene; polyoxymethylene; silicone and polyurethane copolymer; 32%-carbon-impregnated polyolefin; segmented polyurethane; silicone rubber; and alumina. Scanning electron microscopy was used to determine surface morphology changes of all materials after ion-texturing. Electron spectroscopy for chemical analysis was used to determine the effects of ion-texturing on the surface chemical composition of some polymers. Liquid contact angle data were obtained for ion-textured and untextured polymer samples. Results of tensile and fatigue tests of ion-textured metal alloys are presented. Preliminary data of tissue response to ion-textured surfaces of some metals, polytetrafluoroethylene, alumina, and segmented polyurethane have been obtained.

  15. Studying of ion implantation effect on the biology in China

    International Nuclear Information System (INIS)

    Yu Zengliang

    1993-04-01

    Since low energy ion effect on the biology was observed, the ion implantation as a new mutagenic source has been widely used in improving crops and modifying microbes in China. The basic phenomenon of ion implantation effect on the biology and analytical results are reported, and the examples of its application and its further development are shown

  16. Piezosurgery applied to implant dentistry: clinical and biological aspects.

    Science.gov (United States)

    Pereira, Cassiano Costa Silva; Gealh, Walter Cristiano; Meorin-Nogueira, Lamis; Garcia-Júnior, Idelmo Rangel; Okamoto, Roberta

    2014-07-01

    Piezosurgery is a new and modern technique of bone surgery in implantology. Selective cutting is possible for different ultrasonic frequencies acting only in hard tissues (mineralized), saving vital anatomical structures. With the piezoelectric osteotomy technique, receptor site preparation for implants, autogenous bone graft acquistition (particles and blocks), osteotomy for alveolar bone crest expansion, maxillary sinus lifting, and dental implant removal can be performed accurately and safely, providing excellent clinical and biological results, especially for osteocyte viability. The aim of this review was, through literature review, to present clinical applications of piezosurgery in implant dentistry and outline their advantages and disadvantages over conventional surgical systems. Moreover, this study addressed the biological aspects related to piezosurgery that differentiate it from those of bone tissue approaches. Overall, piezosurgery enables critical operations in simple and fully executable procedures; and effectively, areas that are difficult to access have less risk of soft tissue and neurovascular tissue damage via piezosurgery.

  17. Piezoelectric ribbons printed onto rubber for flexible energy conversion.

    Science.gov (United States)

    Qi, Yi; Jafferis, Noah T; Lyons, Kenneth; Lee, Christine M; Ahmad, Habib; McAlpine, Michael C

    2010-02-10

    The development of a method for integrating highly efficient energy conversion materials onto stretchable, biocompatible rubbers could yield breakthroughs in implantable or wearable energy harvesting systems. Being electromechanically coupled, piezoelectric crystals represent a particularly interesting subset of smart materials that function as sensors/actuators, bioMEMS devices, and energy converters. Yet, the crystallization of these materials generally requires high temperatures for maximally efficient performance, rendering them incompatible with temperature-sensitive plastics and rubbers. Here, we overcome these limitations by presenting a scalable and parallel process for transferring crystalline piezoelectric nanothick ribbons of lead zirconate titanate from host substrates onto flexible rubbers over macroscopic areas. Fundamental characterization of the ribbons by piezo-force microscopy indicates that their electromechanical energy conversion metrics are among the highest reported on a flexible medium. The excellent performance of the piezo-ribbon assemblies coupled with stretchable, biocompatible rubber may enable a host of exciting avenues in fundamental research and novel applications.

  18. Biology of teeth and implants: Host factors - pathology, regeneration, and the role of stem cells.

    Science.gov (United States)

    Eggert, F-Michael; Levin, Liran

    2018-01-01

    In chronic periodontitis and peri-implantitis, cells of the innate and adaptive immune systems are involved directly in the lesions within the tissues of the patient. Absence of a periodontal ligament around implants does not prevent a biologic process similar to that of periodontitis from affecting osseointegration. Our first focus is on factors in the biology of individuals that are responsible for the susceptibility of such individuals to chronic periodontitis and to peri-implantitis. Genetic factors are of significant importance in susceptibility to these diseases. Genetic factors of the host affect the composition of the oral microbiome in the same manner that they influence other microbiomes, such as those of the intestines and of the lungs. Our second focus is on the central role of stem cells in tissue regeneration, in the functioning of innate and adaptive immune systems, and in metabolism of bone. Epithelial cell rests of Malassez (ERM) are stem cells of epithelial origin that maintain the periodontal ligament as well as the cementum and alveolar bone associated with the ligament. The tissue niche within which ERM are found extends into the supracrestal areas of collagen fiber-containing tissues of the gingivae above the bony alveolar crest. Maintenance and regeneration of all periodontal tissues involves the activity of a variety of stem cells. The success of dental implants indicates that important groups of stem cells in the periodontium are active to enable that biologic success. Successful replantation of avulsed teeth and auto-transplantation of teeth is comparable to placing dental implants, and so must also involve periodontal stem cells. Biology of teeth and biology of implants represents the biology of the various stem cells that inhabit specialized niches within the periodontal tissues. Diverse biologic processes must function together successfully to maintain periodontal health. Osseointegration of dental implants does not involve formation of

  19. Biological Strategies for Improved Osseointegration and Osteoinduction of Porous Metal Orthopedic Implants

    Science.gov (United States)

    Riester, Scott M.; Bonin, Carolina A.; Kremers, Hilal Maradit; Dudakovic, Amel; Kakar, Sanjeev; Cohen, Robert C.; Westendorf, Jennifer J.

    2015-01-01

    The biological interface between an orthopedic implant and the surrounding host tissue may have a dramatic effect upon clinical outcome. Desired effects include bony ingrowth (osseointegration), stimulation of osteogenesis (osteoinduction), increased vascularization, and improved mechanical stability. Implant loosening, fibrous encapsulation, corrosion, infection, and inflammation, as well as physical mismatch may have deleterious clinical effects. This is particularly true of implants used in the reconstruction of load-bearing synovial joints such as the knee, hip, and the shoulder. The surfaces of orthopedic implants have evolved from solid-smooth to roughened-coarse and most recently, to porous in an effort to create a three-dimensional architecture for bone apposition and osseointegration. Total joint surgeries are increasingly performed in younger individuals with a longer life expectancy, and therefore, the postimplantation lifespan of devices must increase commensurately. This review discusses advancements in biomaterials science and cell-based therapies that may further improve orthopedic success rates. We focus on material and biological properties of orthopedic implants fabricated from porous metal and highlight some relevant developments in stem-cell research. We posit that the ideal primary and revision orthopedic load-bearing metal implants are highly porous and may be chemically modified to induce stem cell growth and osteogenic differentiation, while minimizing inflammation and infection. We conclude that integration of new biological, chemical, and mechanical methods is likely to yield more effective strategies to control and modify the implant–bone interface and thereby improve long-term clinical outcomes. PMID:25348836

  20. Rubber industry

    Science.gov (United States)

    Staszak, Maciej

    2018-03-01

    Following chapter presents short introductory description of rubber and rubber industry. The main problem of rubber industry is the way of the usage of spent tires. Furthermore very important group of problems arise considering the metal and nonmetal additives which are significant component of the vulcanized rubber. The key attention is dedicated to typical ways of rubber usage in utilization and recovery of metals from spent rubber materials concentrating specifically on used tires processing. The method of recovery of rare metals from rubber tires was described. The rubber debris finds widest use in the field of waste metal solutions processing. The environmental pollution caused by metals poses serious threat to humans. Several applications of the use of waste rubber debris to remove metals from environmental waters were described. Moreover, the agriculture usage of waste tire rubber debris is described, presenting systems where the rubber material can be useful as a soil replacement.

  1. Study on the properties of blend rubber prepared with grafted rubber and irradiated rubber by Gamma Rays

    International Nuclear Information System (INIS)

    Dafader, N. C.; Haque, M. E.; Islam, K. A.

    2004-05-01

    The blend rubbers were prepared by mixing γ-rays irradiated and monomer grafted rubbers. The monomers, methyl methacrylate (MMA) and styrene were used separately to prepare grafted rubber by exposure to radiation. The physico-chemical properties of the blend rubbers were evaluated. The tensile strength and elongation at break of the blend rubbers decrease whereas modulus at 500% elongation, swelling ratio and permanent set increase with the increased proportion of grafted rubber in the blend. The tear strength of the blend between irradiated and styrene grafted rubbers increases with the increased proportion of grafted rubber but that of the blend of irradiated and MMA grafted rubbers remains almost constant. The blend rubber could be used for special type of application like rubber thread, tube, catheter etc

  2. Developments in rubber technology 2 synthetic rubbers

    CERN Document Server

    Lee, K

    1981-01-01

    This book is intended for those people who have a knowledge or understanding of rubber materials and processes but who wish to update their knowledge. It should be read in conjunction with Developments in Rubber Technology-l as that volume discussed developments in natural rubber and selected special purpose synthetic rubbers as well as additives. The authors have been selected for their expertise in each particular field and we, as editors, would like to express our appreciation to the individual authors and also to their companies. Such a book would be impossible to produce without such active cooperation as we have received. Volumes 1 and 2 of Developments in Rubber Technology cover rubbers which are processed and vulcanised in the traditional manner. It is appreciated that the omission of non-vulcanised rubber materials (the so­ called thermoplastic elastomers) will be unwelcome to many readers but it is intended, because of the size of the subject, to cover these materials in a subsequent volume. A.W. K...

  3. Induced hemocompatibility and bone formation as biological scaffold for cell therapy implant

    Directory of Open Access Journals (Sweden)

    Keng-Liang Ou

    2016-06-01

    Full Text Available Although stem cells can become almost any type of specialized cell in the human body and may have the potential to generate replacement cells for tissues and organs, the transplantation of these cells are hindered by immune rejection and teratoma formation. However, scientists have found a promising solution for these problems-they have discovered the ability to isolate stem cells from a patient’s umbilical cord blood or bone marrow. Even more recently, small stem cells, such as spore-like stem cells, Blastomere-Like Stem Cells (BLSCs, and Very-Small Embryonic-Like stem cells (VSELs isolated directly from the peripheral blood have beeninvestigated as a novel approach to stem cell therapy as they can be isolated directly from the peripheral blood. A newly-discovered population of multipotent stem cells in this class has been dubbed StemBios (SB cells. The potential therapeutic uses of such stem cells have been explored in many ways, one of which includes dental remodeling and construction. Using adult stem cells, scientists have engineered and cultivated teeth in mice that may one day be used for human implantation.It follows that such regeneration may be possible, to a certain degree, in human patients as well. This idea leads to the present study on the effect of SB cell therapy on early osseointegrationof dental implants. Titanium (Ti dental implants have been proven to be a reliable and predictable treatment for restoration of edentulous regions. The osseointegration process can be described in two stages: primary stability (mechanical stability and secondary stability (biological stability. The mechanical stabilization of the implant reflects the interaction between the bone density and the features of the implant designs and can be determined after implant insertion. Alternatively,the biological stabilization of the implant is a physiologic healing process. It is couple to the biological interaction between the external surface of the

  4. Fiscal 1999 achievement report on regional consortium research and development project. Regional consortium research and development of energy (High-quality low-cost metal dies for molding rubber and plastic - 2nd year); 1999 nendo gomu plastic yo kohin'i tei cost kanagata no kenkyu kaihatsu seika hokokusho. 2

    Energy Technology Data Exchange (ETDEWEB)

    NONE

    2000-03-01

    Metal die surfaces are improved in their resistance to abrasion and corrosion and, in particular, in their release from rubber materials and resistance to contamination. In an effort to develop techniques for optimum metal die surface modification, a PBII (plasma based ion implantation) unit is operated to implant ions into various kinds of metal die surfaces by means of nitrogen or fluorine gas plasma, and optimum conditions are studied by analyzing and evaluating the surface layers after treatment. In an effort to develop a novel ion implantation device to work on 3-dimensional shapes, conditions for stable ion implantation are determined, for which PBII gas concentration, arc plasma power, pulse frequency, application voltage, processing time, etc., are allowed to vary. In the quest for suitable conditions for metal die treatment by the PBII unit, tests are conducted involving natural rubber, butadiene rubber, nitrile rubber, chloroprene rubber, and ethylene propylene rubber and studies are conducted about their release from and contamination of metal dies and 3-dimensional metal dies into which ions have been implanted using fluorine plasma. (NEDO)

  5. Nano-reinforcement of tire rubbers: silica-technology for natural rubber : exploring the infuence of non-rubber constituents on the natural rubber-silica system

    NARCIS (Netherlands)

    Sarkawi, S.S.

    2013-01-01

    Natural rubber is a renewable resource material with outstanding properties which offers significant advantages over its counterparts, the fossil-resource synthetic rubbers. In fact, a natural rubber tree is an efficient carbon dioxide sequester. Since natural rubber is a natural product, it is

  6. Replication of microstructures on three-dimensional geometries by injection moulding of liquid silicone rubber

    DEFF Research Database (Denmark)

    Zhang, Yang; Mischkot, Michael; Hansen, Hans Nørgaard

    2015-01-01

    In this paper, liquid silicon rubber (LSR) parts with micro pillars are studied. The LSR parts were produced by injection moulding and are used as anchoring device for electrode implants inside humans. Micro-structures with specific dimension on implant surfaces can reduce encapsulation...... by the human body, thereby improving implant performance. This paper presents a method of applying micro structure on 3D parts. A Ni-plate with micro holes on the surface was cut into inserts and stuck in a cavity for injection moulding. 1000 injection moulding cycles were performed. Key dimensions...

  7. Prediction of heat generation in rubber or rubber-metal springs

    Directory of Open Access Journals (Sweden)

    Banić Milan S.

    2012-01-01

    Full Text Available The temperature of rubber or rubber-metal springs increases under cyclic loading, due to hysteresis losses and low rubber thermal conductivity. Hysteresis losses correspond to energy dissipation from the rubber, which is primarily converted into heat. This well-known phenomenon, called heat build-up, is the primary reason for rubber aging. Increase in temperature within the rubber compound leads to degradation of its physical and chemical properties, increase in stiffness and loss of damping capability. This paper presents a novel procedure of heat generation prediction in rubber or rubber-metal springs. The procedure encompasses the prediction of hysteresis loss, i. e. dissipated energy within the rubber, by finite element analysis and application of a modern visco-plastic rubber constitutive model. The obtained dissipated energy was used as an input for transient thermal analysis. Verification of the proposed procedure was performed by comparison of simulation results with experimentally obtained data during the dynamic loading of the rubber specimen. The proposed procedure is highly computationally efficient and it enables time integration, which can be problematic in coupled mechanical thermal analysis. [Projekat Ministarstva nauke Republike Srbije, br. TR35005: Research and Development of New Generation of Wind Turbines of High Energy Efficiency

  8. Rubber mixing process and its relationship with bound rubber and crosslink density

    Science.gov (United States)

    Hasan, A.; Rochmadi; Sulistyo, H.; Honggokusumo, S.

    2017-06-01

    This research studied the relationship between bound rubber and crosslink density based on rubber mixing process. Bound rubber was obtained after natural rubber was masticated and mixed with rubber chemicals and filler while crosslink density was collected after rubber compound was vulcanized. Four methods are used and each method refers to four ways of incorporating carbon black during mixing. The first method, after rubber was masticated for 5 minutes, the addition of rubber chemicals and filler was done simultaneously. Rubber was masticated for 1 minute and continued mixing of rubber chemicals and filler where mixing was different from first method. This was the second method. The third method was the same as the second method but the filler used N 660 while in the second method N 330. The last method is not the same as the first and second, the rubber is only masticated for 3 minutes and then mixed with filler and followed by rubber chemicals sequentially. The results showed that bound rubber and crosslink density were influenced by mixing and mastication process. Bound rubber dropped and crosslink density was relatively stable in the first three mixing methods for increasing carbon black at the beginning of the mixing process. Bound rubber and crosslink density stated opposite results in the fourth mixing method. The higher the bound rubber the lower the crosslink density. Without regard to mixing methods, there is a non-linear relationship between bound rubber formation and crosslink density determination

  9. Biological effect of nitrogen ion implantation on stevia

    International Nuclear Information System (INIS)

    Wang Cailian; Shen Mei; Chen Qiufang; Shu Shizhen

    1997-10-01

    Dry seed of stevia were implanted by 35∼150 keV nitrogen ions with various doses. The biological effect in M 1 was studied. The results showed that nitrogen ion beam was able to induce variation on chromosome structure in root tip cells. The rate of cells with chromosome aberration was increased with ion beam energy and dose added, but there was on significant linear regression relationship between ion dose and aberration rate. The results indicated the seedling height reduced with the increasing of dose for ion beam. The biological effect of nitrogen ion beam on M 1 stevia was lower than that of γ-rays. (6 refs., 1 fig., 4 tabs.)

  10. How to Choose between the Implant Materials Steel and Titanium in Orthopedic Trauma Surgery: Part 2 - Biological Aspects.

    Science.gov (United States)

    Perren, S M; Regazzoni, P; Fernandez, A A

    2017-01-01

    BIOLOGICAL ASPECTS OF STEEL AND TITANIUM AS IMPLANT MATERIAL IN ORTHOPEDIC TRAUMA SURGERY The following case from the ICUC database, where a titanium plate was implanted into a flourishing infection, represents the clinical experience leading to preferring titanium over steel. (Fig. 1) (6). Current opinions regarding biological aspects of implant function. The "street" opinions regarding the biological aspects of the use of steel versus titanium as a surgical trauma implant material differ widely. Statements of opinion leaders range from "I do not see any difference in the biological behavior between steel and titanium in clinical application" to "I successfully use titanium implants in infected areas in a situation where steel would act as foreign body "sustaining" infection." Furthermore, some comments imply that clinical proof for the superiority of titanium in human application is lacking. The following tries to clarify the issues addressing the different aspects more through a practical clinical approach than a purely scientific one, this includes simplifications. Today's overall biocompatibility of implant materials is acceptable but: As the vast majority of secondary surgeries are elective procedures this allows the selection of implant materials with optimal infection resistance. The different biological reactions of stainless steel and titanium are important for this segment of clinical pathologies. Biological tole - rance (18) depends on the toxicity and on the amount of soluble implant material released. Release, diffusion and washout through blood circulation determine the local concentration of the corrosion products. Alloying components of steel, especially nickel and chromium, are less than optimal in respect to tissue tolerance and allergenicity. Titanium as a pure metal provides excellent biological tolerance (3, 4, 16). Better strength was obtained by titanium alloys like TiAl6V4. The latter found limited application as surgical implants. It

  11. Technological, biological, and acoustical constraints to music perception in cochlear implant users.

    Science.gov (United States)

    Limb, Charles J; Roy, Alexis T

    2014-02-01

    Despite advances in technology, the ability to perceive music remains limited for many cochlear implant users. This paper reviews the technological, biological, and acoustical constraints that make music an especially challenging stimulus for cochlear implant users, while highlighting recent research efforts to overcome these shortcomings. The limitations of cochlear implant devices, which have been optimized for speech comprehension, become evident when applied to music, particularly with regards to inadequate spectral, fine-temporal, and dynamic range representation. Beyond the impoverished information transmitted by the device itself, both peripheral and central auditory nervous system deficits are seen in the presence of sensorineural hearing loss, such as auditory nerve degeneration and abnormal auditory cortex activation. These technological and biological constraints to effective music perception are further compounded by the complexity of the acoustical features of music itself that require the perceptual integration of varying rhythmic, melodic, harmonic, and timbral elements of sound. Cochlear implant users not only have difficulty perceiving spectral components individually (leading to fundamental disruptions in perception of pitch, melody, and harmony) but also display deficits with higher perceptual integration tasks required for music perception, such as auditory stream segregation. Despite these current limitations, focused musical training programs, new assessment methods, and improvements in the representation and transmission of the complex acoustical features of music through technological innovation offer the potential for significant advancements in cochlear implant-mediated music perception. Copyright © 2013 Elsevier B.V. All rights reserved.

  12. Rubber glove wearing device

    International Nuclear Information System (INIS)

    Nozaki, Tatsuo; Takada, Kaoru.

    1994-01-01

    Rubber groves are attached each to an upper end of a glove putting vessel having an air-sucking hole on the bottom by enlarging an opening end of the rubber glove and turning back the inside to the outside. When the sucking device is operated, air in the glove putting device is sucked and the rubber glove is expanded by an atmospheric pressure. After expansion of the rubber glove to some extent, the sucking device is stopped, and presence or absence of failures of the rubber glove is confirmed by shrinkage of the rubber glove and by an indication value of a pressure gauge for detecting the pressure change in the vessel. Then, a hand is inserted to the expanded rubber glove, and a detaching switch in the vessel is pushed by a finger tip. A detaching piece at the upper end of the vessel is protruded outwardly to enlarge the turned-back portion of the rubber glove to easily release the rubber glove from the putting vessel, and the rubber glove is put on. This enables to wear the rubber glove and conduct failure test simultaneously. Further, a user can put on the rubber glove without touching the outside of the rubber glove. (I.N.)

  13. PROPERTIES TYRE TREAD RUBBERS DEPENDING ON PARTICULARITY OF RUBBER COMPOUND

    Directory of Open Access Journals (Sweden)

    Z. S. Shashok

    2014-01-01

    Full Text Available Summary. The results of studies of the elastomeric compositions based on natural rubber containing curatives different ratio "curing agent : vulcanization accelerator" listed in this article. Influence of the composition of the vulcanizing group on stress-strain and elastic- deformation properties of tire tread rubber was installed. It has been shown that a significant effect on thermo-oxidative aging of vulcanizates was the composition of the vulcanizing group. Results of studies resistance tread rubber to exposure to elevated temperatures were presented . Vulcanizates differing type and density by varying the cross-linking ratio of "curing agent : vulcanization accelerator" were obtained . Research results in the formation of rubber resistance and crack growth at different temperatures were presented. Revealed that the best education and resistance to tear propagation under normal conditions characterized by rubber ratio "curing agent : vulcanization accelerator" equal to 1.5:1. It has been established that a dynamic endurance study rubbers depends largely on the nature and concentration of the cross-linking cross-links and movable promote increase efficiency due to the grid and reduce the sulfidity rearrangement. During loading mode alternating deformations at elevated temperatures lability of polysulfide bonds negatively affects the performance of rubber, and the decisive role of providing strength and thermal cross-linking. It is shown that the performance of the spatial grid rubbers allow indirectly judge the dynamic vulcanizates endurance and predict performance rubbers at elevated temperatures under conditions of repeated cyclic deformation. Revealed that the vulcanizing system containing sulfur and vulcanization accelerator TBBS 1:2, promotes the formation of the optimal structure of vulcanized rubber , which provides the best resistance to repeated cyclic deformations in the operating temperatures of the tire.

  14. Fracture behavior of rubber powder modified rubber blends applied for conveying belt top covers

    OpenAIRE

    Euchler, Eric; Stocek, Radek; Gehde, Michael; Bunzel, Jörg-Michael; Saal, Wolfgang; Kipscholl, Reinhold

    2016-01-01

    The aim of this study is concentrated on the experimental investigation of wear resistance of rubber powder modified rubber blends. Styrene-Butadiene-Rubber (SBR) blends applied for conveying belt top covers have been modified by ground rubber (rubber powder) based on SBR. We theoretically described the rubber wear mechanism due to loading conditions occurring at conveyor belts in the field, to simulate wear behavior of top cover rubber materials. An own developed testing equipment based on g...

  15. Biological effects of N+ ion implantation and UV radiation on streptomyces albus

    International Nuclear Information System (INIS)

    Wu Jian; Dai Guifu

    2005-01-01

    The results of both 30 keV N + ion implantation and UV irradiation of Streptomyces albus showed complicate biological effects. The 'saddle shape' pattern of the dose-dependent curve formed by N + ion implantation with low energy was studied, and it proved that vacuum was not the reason, and the fact, the 'saddle shape' curve may be regarded as a HRS/IRR (hyper-radiosensitivity/increased radiaoresistance) effect caused by low dose irradiation. But Streptomyces albus UV irradiated after vacuum treatment only showed IRR effect or hormesis (survival rate >100%). The streptomycin resistance mutation of Streptomyces albus caused by low energy N + ion implantation and UV irradiation was also studied. the results showed that UV radiation is one effective means for streptomyces albus breeding. (authors)

  16. Autologous chondrocyte implantation: superior biologic properties of hyaline cartilage repairs.

    Science.gov (United States)

    Henderson, Ian; Lavigne, Patrick; Valenzuela, Herminio; Oakes, Barry

    2007-02-01

    Information regarding the quality of autologous chondrocyte implantation repair is needed to determine whether the current autologous chondrocyte implantation surgical technology and the subsequent biologic repair processes are capable of reliably forming durable hyaline or hyaline-like cartilage in vivo. We report and analyze the properties and qualities of autologous chondrocyte implantation repairs. We evaluated 66 autologous chondrocyte implantation repairs in 57 patients, 55 of whom had histology, indentometry, and International Cartilage Repair Society repair scoring at reoperation for mechanical symptoms or pain. International Knee Documentation Committee scores were used to address clinical outcome. Maximum stiffness, normalized stiffness, and International Cartilage Repair Society repair scoring were higher for hyaline articular cartilage repairs compared with fibrocartilage, with no difference in clinical outcome. Reoperations revealed 32 macroscopically abnormal repairs (Group B) and 23 knees with normal-looking repairs in which symptoms leading to arthroscopy were accounted for by other joint disorders (Group A). In Group A, 65% of repairs were either hyaline or hyaline-like cartilage compared with 28% in Group B. Autologous chondrocyte repairs composed of fibrocartilage showed more morphologic abnormalities and became symptomatic earlier than hyaline or hyaline-like cartilage repairs. The hyaline articular cartilage repairs had biomechanical properties comparable to surrounding cartilage and superior to those associated with fibrocartilage repairs.

  17. Nitrile rubber and carboxylated nitrile rubber resistance to soybean biodiesel

    Directory of Open Access Journals (Sweden)

    Felipe Nunes Linhares

    2018-03-01

    Full Text Available Abstract Biodiesel has been considered a suitable substitute for petroleum diesel, but their chemical composition differs greatly. For this reason, biodiesel interacts differently than petroleum diesel with various materials, including rubbers. Therefore, the resistance of some elastomers should be thoroughly evaluated, specifically those which are commonly used in automotive industry. Nitrile rubber (NBR is widely used to produce vehicular parts that are constantly in contact with fuels. This paper aimed to assess the resistance of carboxylated nitrile rubber (XNBR with 28% of acrylonitrile content to soybean biodiesel in comparison with non-carboxylated nitrile rubber samples, with high and medium acrylonitrile content (33 and 45%. NBR with medium acrylonitrile content showed little resistance to biodiesel. However, carboxylated nitrile rubber even with low acrylonitrile content had similar performance to NBR with high acrylonitrile content.

  18. Biological effects of low energy nitrogen ion implantation on Jatropha curcas L. seed germination

    International Nuclear Information System (INIS)

    Xu Gang; Wang Xiaoteng; Gan Cailing; Fang Yanqiong; Zhang Meng

    2012-01-01

    Highlights: ► We analyzed biological effects of N + implantation on dry Jatropha curcas seed. ► N + implantation greatly decreased seedling survival rate. ► At doses beyond 15 × 10 16 ion cm −2 , biological repair took place. ► CAT was essential for H 2 O 2 removal. POD mainly functioned as seed was severely hurt. ► HAsA–GSH cycle mainly contributed to the regeneration of HAsA. - Abstract: To explore the biological effects of nitrogen ion beam implantation on dry Jatropha curcas seed, a beam of N + with energy of 25 keV was applied to treat the dry seed at six different doses. N + beam implantation greatly decreased germination rate and seedling survival rate. The doses within the range of 12 × 10 16 to 15 × 10 16 ions cm −2 severely damaged the seeds: total antioxidant capacity (TAC), germination rate, seedling survival rate, reduced ascorbate acid (HAsA) and reduced glutathione (GSH) contents, and most of the tested antioxidases activity (i.e. catalase (CAT), ascorbate peroxidase (APX) and superoxide dismutase (SOD)) reached their lowest levels. At a dose of 18 × 10 16 ion cm −2 , biological repair took place: moderate increases were found in TAC, germination rate, seedling survival rate, HAsA and GSH contents, and some antioxidant enzyme activities (i.e. CAT, APX, SOD and GPX). The dose of 18 × 10 16 ions cm −2 may be the optimum dose for use in dry J. curcas seed mutation breeding. CAT, HAsA and GSH contributed to the increase of TAC, but CAT was the most important. POD performed its important role as seed was severely damaged. The main role of the HAsA–GSH cycle appeared to be for regeneration of HAsA.

  19. Exposure to rubber fume and rubber process dust in the general rubber goods, tyre manufacturing and retread industries.

    Science.gov (United States)

    Dost, A A; Redman, D; Cox, G

    2000-08-01

    This study assesses the current patterns and levels of exposure to rubber fume and rubber process dust in the British rubber industry and compares and contrasts the data obtained from the general rubber goods (GRG), retread tire (RT) and new tire (NT) sectors. A total of 179 rubber companies were visited and data were obtained from 52 general rubber goods, 29 retread tire and 7 new tire manufacturers. The survey was conducted using a questionnaire and included a walk-through inspection of the workplace to assess the extent of use of control measures and the nature of work practices being employed. The most recent (predominantly 1995-97) exposure monitoring data for rubber fume and rubber process dust were obtained from these companies; no additional sampling was conducted for the purpose of this study. In addition to the assessment of exposure data, evaluation of occupational hygiene reports for the quality of information and advice was also carried out.A comparison of the median exposures for processes showed that the order of exposure to rubber fume (E, in mg m(-3)) is: E(moulding) (0.40) approximately E(extrusion) (0.33)>E(milling) (0.18) for GRG; E(press) (0. 32)>E(extrusion) (0.19)>E(autoclave) (0.10) for RT; and E(press) (0. 22) approximately E(all other) (0.22) for NT. The order of exposure to rubber fume between sectors was E(GRG) (0.40)>E(RT) (0.32)>E(NT) (0.22). Median exposures to rubber process dust in the GRG was E(weighing) (4.2)>E(mixing) (1.2) approximately E(milling) (0.8) approximately E(extrusion) (0.8) and no significant difference (P=0. 31) between GRG and NT sectors. The findings compare well with the study carried out in the Netherlands [Kromhout et al. (1994), Annals of Occupational Hygiene 38(1), 3-22], and it is suggested that the factors governing the significant differences noted between the three sectors relate principally to the production and task functions and also to the extent of controls employed. Evaluation of occupational

  20. Preparation of sulfonic acid-containing rubbers from natural rubber vulcanizates

    Science.gov (United States)

    Poonsawat, Worapong; Poompradub, Sirilux; Ngamcharussrivichai, Chawalit

    2014-06-01

    In this work, a series of sulfonic acid-containing rubbers were prepared by aqueous phase oxidation of natural rubber vulcanizates in the presence of hydrogen peroxide (H2O2) and formic acid (HCOOH). The starting vulcanizates were neatly prepared via an efficient vulcanization (EV) system by varying mass ratio of N-cyclohexyl-2-benzothiazole sulfonamide (CBS), as an accelerator, to sulfur. The oxidation conditions were controlled at the molar ratio of H2O2: HCOOH = 1:1, the concentration of H2O2 = 15 wt.%, the temperature = 50 °C, and the reaction time = 3 h. The rubber materials before and after the oxidation were characterized for their physicochemical properties by using Fourier transform infrared spectroscopy, bomb calorimetry, acid-base titration and swelling measurements. The results indicated the presence of sulfonic acid group in the oxidized rubbers, generated by the oxidative cleaves of sulfide crosslinks in the rubber vulcanizates. The oxidation decreased the sulfur content of the rubber in which the level of sulfur loss was determined by the CBS/sulfur ratio. Moreover, the acidity of the oxidized products was correlated with the amount of sulfur remaining.

  1. The Effect of Rubber Mixing Process on The Curing Characteristics of Natural Rubber

    Directory of Open Access Journals (Sweden)

    Abu Hasan

    2013-04-01

    Full Text Available This research is aimed at studying the relationship between rubber mixing processes and curing characteristics of natural rubber. The curing characteristic analysis was carried out through a natural rubber formula having been masticated and mixed, followed by curing. As many as four mastication methods were finely applied; each respected four sequences of rubber mixing process. In the first method, rubber was masticated for 5 minutes and then rubber chemicals and carbon black N 330 were  simultaneously added. In the second and the third methods, rubber was masticated for 1 minute and then carbon blacks and rubber chemicals were also simultaneously added but using different type of fillers. In the fourth method, rubber was masticated for 3 minutes and then rubber chemicals and carbon black were subsequently added. The additions of rubber chemicals and carbon blacks to the masticated rubber were distinguished by the sequence and time allocated for each mixing process. The carbon blacks were added in two stages by which 10 phr was added first and the remaining 40 phr was added later along with oil. In another method, ratios of the carbon blacks addition (as done in the first  and the second stages were 20:30, 30:20, and 40:10. The examination results showed that rubber mixing process gave an impact on the changes of curing characteristics. They were much affected by the method of carbon black addition. The mixing temperature also had an effect on both curing time and curing rate in which the higher the mixing temperature, the lower the curing time and curing rate. Vulcanization temperature also affected the curing time and curing rate in which the higher the vulcanization temperature, the lower the curing time and the higher the curing rate. Lastly, particle size of carbon black also gave an impact on the curing time and curing rate in which the smaller the particle size, the lower the curing time and the higher the curing rate.

  2. Radiation vulcanization of rubbers

    Energy Technology Data Exchange (ETDEWEB)

    Makuuchi, Keizo [Japan Atomic Energy Research Inst., Takasaki, Gunma (Japan). Takasaki Radiation Chemistry Research Establishment

    2002-02-01

    An abstract of the radiation process of polymer materials and the polymer reaction by radiation is explained. Main radiation is 250 keV to 10 MeV of electron rays in the industry. Radiation cross-linked rubber has less the tensile strength than that by sulfur and organic peroxide crosslinking. The main origins of low tensile strength are caused by cut of backbone chain and ozone depend on radiation. Acceleration of crosslinking and short time of radiation are necessary to improve these defects. To accelerate crosslinking, we used crosslinking accelerators, for example, three poly-functional monomers (PFM). The maximum tensile strength of styrene-butadiene rubber (SBR) not added crosslinking accelerators showed 3 MPa at 110 kGy, but SBR added A-TMMT (tetramethylolmethane tetraacrylate) showed 5.5 MPa at 110 kGy. Radiation crosslinking of many kinds of rubber: isoprene (IR), SBR, CR, nitrile rubber (NBR), hydrogenated nitrile rubber (HNBR), butyl rubber (IIR), chlorinated butyl rubber (CIIR), EPM and TPE are explained. (S.Y.)

  3. Radiation vulcanization of rubbers

    International Nuclear Information System (INIS)

    Makuuchi, Keizo

    2002-01-01

    An abstract of the radiation process of polymer materials and the polymer reaction by radiation is explained. Main radiation is 250 keV to 10 MeV of electron rays in the industry. Radiation cross-linked rubber has less the tensile strength than that by sulfur and organic peroxide crosslinking. The main origins of low tensile strength are caused by cut of backbone chain and ozone depend on radiation. Acceleration of crosslinking and short time of radiation are necessary to improve these defects. To accelerate crosslinking, we used crosslinking accelerators, for example, three poly-functional monomers (PFM). The maximum tensile strength of styrene-butadiene rubber (SBR) not added crosslinking accelerators showed 3 MPa at 110 kGy, but SBR added A-TMMT (tetramethylolmethane tetraacrylate) showed 5.5 MPa at 110 kGy. Radiation crosslinking of many kinds of rubber: isoprene (IR), SBR, CR, nitrile rubber (NBR), hydrogenated nitrile rubber (HNBR), butyl rubber (IIR), chlorinated butyl rubber (CIIR), EPM and TPE are explained. (S.Y.)

  4. US rubber markets recover

    International Nuclear Information System (INIS)

    Wood, A.

    1993-01-01

    Synthetic rubber markets in North America bounced back in no uncertain terms last year, with demand climbing an impressive 9.5%, to 2.97 million m.t.; and, according to the International Institute of Synthetic Rubber Producers (IIS-RP; Houston) latest five-year forecast, producers can look forward to a 3.3% increase in demand during 1993. This growth rate outpaced out 1992 forecast and demonstrates the resilience of the synthetic rubber industry, says William E. Tessemer, managing director of IISRP. We expect demand in 1993 to surpass 1992 and level off at a 2%/year growth rate for synthetic rubber - 2.5% including thermoplastic elastomers [TPEs]-over the 1993-97 period. The improvement reflects signs of a recovery in North America, especially the pickup in the auto and tire industry. The two major tire rubbers - styrene butadiene and polybutadiene rubber - notched up double-digit gains, and other materials that have autos uses, such as nitrile rubber and many of the specialty elastomers, also advanced strongly

  5. Rubber molds for investment casting

    International Nuclear Information System (INIS)

    Sibtain, S.N.

    2011-01-01

    The main objective of the project is to investigate different types of molding rubbers used for investment casting. The level of shape complexity which can be achieved by using these rubber molds is also studied. It was almost impossible to make complex shapes molds using metal molds, in that cases rubber molds are very important because they arc flexible and give accurate and precise part dimensions. Turbine blades are hi-tech components with air-foil geometries that have close dimensional tolerances. They are made of super-alloys and manufactured by investment casting. The final blade profile depends upon the dimensional accuracy in each of the processing steps. In the present work experimental study for the production of high quality low cost castings of turbine blades using rubber molds and injected wax patterns is presented. Natural Rubber molds and wax patterns from these molds were made. Different types of molding rubbers were studied including natural rubber, silicone rubber and liquid silicone rubber. It was found that by using rubber molds we can make most complex shape with very less finishing required. The shrinkage was 12% as compared to original master pattern. Rubber molds were made using laboratory hot press. Three layers of rubber above and below the master pattern. After that vulcanization was done by giving temperature and pressure. (author)

  6. In vitro biological outcome of laser application for modification or processing of titanium dental implants.

    Science.gov (United States)

    Hindy, Ahmed; Farahmand, Farzam; Tabatabaei, Fahimeh Sadat

    2017-07-01

    There are numerous functions for laser in modern implant dentistry including surface treatment, surface coating, and implant manufacturing. As laser application may potentially improve osseointegration of dental implants, we systematically reviewed the literature for in vitro biological responses to laser-modified or processed titanium dental implants. The literature was searched in PubMed, ISI Web, and Scopus, using keywords "titanium dental implants," "laser," "biocompatibility," and their synonyms. After screening the 136 references obtained, 28 articles met the inclusion criteria. We found that Nd:YAG laser was the most commonly used lasers in the treatment or processing of titanium dental implants. Most of the experiments used cell attachment and cell proliferation to investigate bioresponses of the implants. The most commonly used cells in these assays were osteoblast-like cells. Only one study was conducted in stem cells. These in vitro studies reported higher biocompatibility in laser-modified titanium implants. It seems that laser radiation plays a vital role in cell response to dental implants; however, it is necessary to accomplish more studies using different laser types and parameters on various cells to offer a more conclusive result.

  7. Natural rubber: leather composites

    OpenAIRE

    Ravichandran,K.; Natchimuthu,N.

    2005-01-01

    Leather is a fibrous protein consisting of collagen in a three dimensionally crosslinked network. Chrome tanning of leather improves the appearance of leather but at the same time emits both solid and liquid chrome leather wastes. Scrap rubber recycling using untreated and neutralized leather fibrous particles in natural rubber has been studied. Vulcanization, mechanical, morphological and swelling properties of the natural rubber - scrap rubber composites containing neutralized leather have ...

  8. Rubber compounding and processing

    CSIR Research Space (South Africa)

    John, MJ

    2014-06-01

    Full Text Available This chapter presents an overview on the compounding and processing techniques of natural rubber compounds. The introductory portion deals with different types of rubbers and principles of rubber compounding. The primary and secondary fillers used...

  9. Biological effects of low energy nitrogen ion implantation on Jatropha curcas L. seed germination

    Energy Technology Data Exchange (ETDEWEB)

    Xu Gang, E-mail: xg335300@yahoo.com.cn [Center for Research and Development of Fine Chemicals, Guizhou University, Guiyang 550025 (China); Institute of Entomology, Guizhou University, Guiyang 550025 (China); Wang Xiaoteng [Department of Agricultural Resources and Environment, College of Agricultural, Guizhou University, Guiyang 550025 (China); Gan Cailing; Fang Yanqiong; Zhang Meng [College of Life Sciences, Guizhou University, Guiyang 550025 (China)

    2012-09-15

    Highlights: Black-Right-Pointing-Pointer We analyzed biological effects of N{sup +} implantation on dry Jatropha curcas seed. Black-Right-Pointing-Pointer N{sup +} implantation greatly decreased seedling survival rate. Black-Right-Pointing-Pointer At doses beyond 15 Multiplication-Sign 10{sup 16} ion cm{sup -2}, biological repair took place. Black-Right-Pointing-Pointer CAT was essential for H{sub 2}O{sub 2} removal. POD mainly functioned as seed was severely hurt. Black-Right-Pointing-Pointer HAsA-GSH cycle mainly contributed to the regeneration of HAsA. - Abstract: To explore the biological effects of nitrogen ion beam implantation on dry Jatropha curcas seed, a beam of N{sup +} with energy of 25 keV was applied to treat the dry seed at six different doses. N{sup +} beam implantation greatly decreased germination rate and seedling survival rate. The doses within the range of 12 Multiplication-Sign 10{sup 16} to 15 Multiplication-Sign 10{sup 16} ions cm{sup -2} severely damaged the seeds: total antioxidant capacity (TAC), germination rate, seedling survival rate, reduced ascorbate acid (HAsA) and reduced glutathione (GSH) contents, and most of the tested antioxidases activity (i.e. catalase (CAT), ascorbate peroxidase (APX) and superoxide dismutase (SOD)) reached their lowest levels. At a dose of 18 Multiplication-Sign 10{sup 16} ion cm{sup -2}, biological repair took place: moderate increases were found in TAC, germination rate, seedling survival rate, HAsA and GSH contents, and some antioxidant enzyme activities (i.e. CAT, APX, SOD and GPX). The dose of 18 Multiplication-Sign 10{sup 16} ions cm{sup -2} may be the optimum dose for use in dry J. curcas seed mutation breeding. CAT, HAsA and GSH contributed to the increase of TAC, but CAT was the most important. POD performed its important role as seed was severely damaged. The main role of the HAsA-GSH cycle appeared to be for regeneration of HAsA.

  10. Natural rubber: leather composites

    Directory of Open Access Journals (Sweden)

    K. Ravichandran

    2005-06-01

    Full Text Available Leather is a fibrous protein consisting of collagen in a three dimensionally crosslinked network. Chrome tanning of leather improves the appearance of leather but at the same time emits both solid and liquid chrome leather wastes. Scrap rubber recycling using untreated and neutralized leather fibrous particles in natural rubber has been studied. Vulcanization, mechanical, morphological and swelling properties of the natural rubber - scrap rubber composites containing neutralized leather have been discussed. Use of chrome leather particles has been found to improve the consumption of scrap rubber powder in natural rubber formulations. Polymer composites based on leather wastes as fillers are reported to be useful for many applications such as in construction materials, automobile interior moldings, heat and sound insulating boards, shoe soles, flooring materials and moldings with good anti-static properties, air permeability and good appearances.

  11. Rubber

    Science.gov (United States)

    Graves, D. F.

    The word "rubber" immediately brings to mind materials that are highly flexible and will snap back to their original shape after being stretched. In this chapter a variety of materials are discussed that possess this odd characteristics. There will also be a discussion on the mechanism of this "elastic retractive force." Originally, rubber meant the gum collected from a tree growing in Brazil. The term "rubber" was coined for this material by the English chemist Joseph Priestley, who noted that it was effective for removing pencil marks from paper. Today, in addition to Priestley's natural product, many synthetic materials are made that possess these characteristics and many other properties. The common features of these materials are that they are made up of long-chain molecules that are amorphous (not crystalline), and the chains are above their glass transition temperature at room temperature.

  12. BEDVH--A method for evaluating biologically effective dose volume histograms: Application to eye plaque brachytherapy implants

    International Nuclear Information System (INIS)

    Gagne, Nolan L.; Leonard, Kara L.; Huber, Kathryn E.; Mignano, John E.; Duker, Jay S.; Laver, Nora V.; Rivard, Mark J.

    2012-01-01

    Purpose: A method is introduced to examine the influence of implant duration T, radionuclide, and radiobiological parameters on the biologically effective dose (BED) throughout the entire volume of regions of interest for episcleral brachytherapy using available radionuclides. This method is employed to evaluate a particular eye plaque brachytherapy implant in a radiobiological context. Methods: A reference eye geometry and 16 mm COMS eye plaque loaded with 103 Pd, 125 I, or 131 Cs sources were examined with dose distributions accounting for plaque heterogeneities. For a standardized 7 day implant, doses to 90% of the tumor volume ( TUMOR D 90 ) and 10% of the organ at risk volumes ( OAR D 10 ) were calculated. The BED equation from Dale and Jones and published α/β and μ parameters were incorporated with dose volume histograms (DVHs) for various T values such as T = 7 days (i.e., TUMOR 7 BED 10 and OAR 7 BED 10 ). By calculating BED throughout the volumes, biologically effective dose volume histograms (BEDVHs) were developed for tumor and OARs. Influence of T, radionuclide choice, and radiobiological parameters on TUMOR BEDVH and OAR BEDVH were examined. The nominal dose was scaled for shorter implants to achieve biological equivalence. Results: TUMOR D 90 values were 102, 112, and 110 Gy for 103 Pd, 125 I, and 131 Cs, respectively. Corresponding TUMOR 7 BED 10 values were 124, 140, and 138 Gy, respectively. As T decreased from 7 to 0.01 days, the isobiologically effective prescription dose decreased by a factor of three. As expected, TUMOR 7 BEDVH did not significantly change as a function of radionuclide half-life but varied by 10% due to radionuclide dose distribution. Variations in reported radiobiological parameters caused TUMOR 7 BED 10 to deviate by up to 46%. Over the range of OAR α/β values, OAR 7 BED 10 varied by up to 41%, 3.1%, and 1.4% for the lens, optic nerve, and lacrimal gland, respectively. Conclusions: BEDVH permits evaluation of the

  13. Enhanced Physicochemical and Biological Properties of Ion-Implanted Titanium Using Electron Cyclotron Resonance Ion Sources

    Directory of Open Access Journals (Sweden)

    Csaba Hegedűs

    2016-01-01

    Full Text Available The surface properties of metallic implants play an important role in their clinical success. Improving upon the inherent shortcomings of Ti implants, such as poor bioactivity, is imperative for achieving clinical use. In this study, we have developed a Ti implant modified with Ca or dual Ca + Si ions on the surface using an electron cyclotron resonance ion source (ECRIS. The physicochemical and biological properties of ion-implanted Ti surfaces were analyzed using various analytical techniques, such as surface analyses, potentiodynamic polarization and cell culture. Experimental results indicated that a rough morphology was observed on the Ti substrate surface modified by ECRIS plasma ions. The in vitro electrochemical measurement results also indicated that the Ca + Si ion-implanted surface had a more beneficial and desired behavior than the pristine Ti substrate. Compared to the pristine Ti substrate, all ion-implanted samples had a lower hemolysis ratio. MG63 cells cultured on the high Ca and dual Ca + Si ion-implanted surfaces revealed significantly greater cell viability in comparison to the pristine Ti substrate. In conclusion, surface modification by electron cyclotron resonance Ca and Si ion sources could be an effective method for Ti implants.

  14. A comparative study of natural rubber modified with ground tire rubber of truck

    OpenAIRE

    Binti Haridan, Ili Liyana

    2016-01-01

    The recycling of waste rubber has considerable significance in term of environmental protection and energy conservation. Considering that most of the relevant literature is concerned with tire recycling, the aim of this work was to develop and characterize the elastomeric samples of natural rubber (NR) composites filled with ground tire rubber of truck (GTR) devulcanized by microwave (DGTR). The tire rubber was ground under ambient conditions and subjected to microwave exposure for 3, 5 and ...

  15. Natural Rubber Modification For Upper Layer Of Rubberized Asphalt Paving Block AS Shock Absorber

    OpenAIRE

    Nasruddin, Nasruddin

    2017-01-01

    The research of rubber compounding modification for upper layer of rubberized asphalt paving block as shock absorber using natural rubber, styrene butadiene rubber (SBR) as synthetic rubber, fly ash as filler and also vegetable oil as plasticizer has been conducted. The research design was varying the filler Si-69, fly ash and palm oil. The five formulas A, B, C, D, and E designed by varying the amount of Si-69 (48.5; 50.75; 53.00; 55.25; and 57.50) phr; coal fly ash (4.75, 7.00, 9.25, 11.50 ...

  16. Biological in situ Dose Painting for Image-Guided Radiation Therapy Using Drug-Loaded Implantable Devices

    International Nuclear Information System (INIS)

    Cormack, Robert A.; Sridhar, Srinivas; Suh, W. Warren; D'Amico, Anthony V.; Makrigiorgos, G. Mike

    2010-01-01

    Purpose: Implantable devices routinely used for increasing spatial accuracy in modern image-guided radiation treatments (IGRT), such as fiducials or brachytherapy spacers, encompass the potential for in situ release of biologically active drugs, providing an opportunity to enhance the therapeutic ratio. We model this new approach for two types of treatment. Methods and Materials: Radiopaque fiducials used in IGRT, or prostate brachytherapy spacers ('eluters'), were assumed to be loaded with radiosensitizer for in situ drug slow release. An analytic function describing the concentration of radiosensitizer versus distance from eluters, depending on diffusion-elimination properties of the drug in tissue, was developed. Tumor coverage by the drug was modeled for tumors typical of lung stereotactic body radiation therapy treatments for various eluter dimensions and drug properties. Six prostate 125 I brachytherapy cases were analyzed by assuming implantation of drug-loaded spacers. Radiosensitizer-induced subvolume boost was simulated from which biologically effective doses for typical radiosensitizers were calculated in one example. Results: Drug distributions from three-dimensional arrangements of drug eluters versus eluter size and drug properties were tabulated. Four radiosensitizer-loaded fiducials provide adequate radiosensitization for ∼4-cm-diameter lung tumors, thus potentially boosting biologically equivalent doses in centrally located stereotactic body treated lesions. Similarly, multiple drug-loaded spacers provide prostate brachytherapy with flexible shaping of 'biologically equivalent doses' to fit requirements difficult to meet by using radiation alone, e.g., boosting a high-risk region juxtaposed to the urethra while respecting normal tissue tolerance of both the urethra and the rectum. Conclusions: Drug loading of implantable devices routinely used in IGRT provides new opportunities for therapy modulation via biological in situ dose painting.

  17. Fundamental studies on dynamic wear behavior of SBR rubber compounds modified by SBR rubber powder

    OpenAIRE

    Euchler, Eric; Heinrich, Gert; Michael, Hannes; Gehde, Michael; Stocek, Radek; Kratina, Ondrej; Kipscholl, Reinhold; Bunzel, Jörg-Michael; Saal, Wolfgang

    2016-01-01

    The aim of this study is focused on the experimental investigation of dynamic wear behavior of carbon black filled rubber compounds comprising pristine styrene butadiene rubber (SBR) together with incorporated SBR ground rubber (rubber powder). We also analyzed and described quantitatively the service conditions of some dynamically loaded rubber products, which are liable to wear (e.g. conveyor belts, tires). Beside the well-known standard test method to characterize wear resistance at steady...

  18. Hardness measurements of silicon rubber and polyurethane rubber cured by ionizing radiation

    International Nuclear Information System (INIS)

    Basfar, A.A.

    1995-01-01

    This work investigates the hardness of both silicon rubber and polyurethane rubber cured by ionizing radiation. Shore A Hardness is used to characterize the subject elastomers in relation to the crosslinking process. Various formulations of both materials have been investigated in order to achieve the optimum cure conditions desired. A small amount of the curing agent has been incorporated in some formulations in order to reduce the required dose to achieve full cure conditions. Silicon rubber has shown improvements in hardness as absorbed dose is increased, whereas hardness remained constant over a range of absorbed doses for polyurethane rubber

  19. The rubber tree genome reveals new insights into rubber production and species adaptation

    OpenAIRE

    Tang, Chaorong; Yang, Meng; Fang, Yongjun; Luo, Yingfeng; Gao, Shenghan; Xiao, Xiaohu; An, Zewei; Zhou, Binhui; Zhang, Bing; Tan, Xinyu; Yeang, Hoong Yeet; Qin, Yunxia; Yang, Jianghua; Lin, Qiang; Mei, Hailiang

    2016-01-01

    The Para rubber tree (Hevea brasiliensis) is an economically important tropical tree species that produces natural rubber, an essential industrial raw material. Here we present a high-quality genome assembly of this species (1.37 Gb, scaffold N50 = 1.28 Mb) that covers 93.8% of the genome (1.47 Gb) and harbours 43,792 predicted protein-coding genes. A striking expansion of the REF/SRPP (rubber elongation factor/small rubber particle protein) gene family and its divergence into several laticif...

  20. Radiation-induced deterioration of natural rubber and isoprene rubber vulcanizates

    International Nuclear Information System (INIS)

    Kohjiya, Shinzo; Matsumura, Yasushige; Yamashita, Shinzo; Matsuyama, Tomochika; Yamaoka, Hitoshi.

    1984-01-01

    Natural rubber (NR) and isoprene rubber (IR) were cured by sulfur and accelerator to give rubber vulcanizates. Both vulcanizates were subject to solvent extraction to purify them, followed by the γ-ray irradiation in air at room temperature. The deterioration by γ-ray (0-20 Mrad) was investigated by the changes of tensile properties, hardness, swelling, and ATR-IR spectra. The tensile strength decreased much by a few Mrad irradiation, which is elucidated due to the difficulty of stretch-induced crystallization of polyisoprene after the irradiation. Modulus at 50 % elongation, network-chain density, and hardness did not show significant variation with the γ-ray dose. These irradiation results suggest both degradation and crosslinking occur comparably in the rubber vulcanizates and the regularity of polyisoprene chains may be somewhat randomized to prevent them from crystallizing on stretching. (author)

  1. Rubber Reclamation

    Science.gov (United States)

    Williams, Kathryn R.

    2007-01-01

    The safety and health hazards related to recycling of used rubber, due to the scarcity and high price of virgin rubber are reported. Various threats like stagnant water pools trapped in tires leading to diseases and ignited tires, which become very difficult to extinguish and generating smoke that is extremely detrimental to the environment, have…

  2. Biologic Agents for Periodontal Regeneration and Implant Site Development

    Directory of Open Access Journals (Sweden)

    Fernando Suárez-López del Amo

    2015-01-01

    Full Text Available The advancement of molecular mediators or biologic agents has increased tremendously during the last decade in periodontology and dental implantology. Implant site development and reconstruction of the lost periodontium represent main fields in which these molecular mediators have been employed and investigated. Different growth factors trigger different reactions in the tissues of the periodontium at various cellular levels. Proliferation, migration, and differentiation constitute the main target areas of these molecular mediators. It was the purpose of this comprehensive review to describe the origin and rationale, evidence, and the most current understanding of the following biologic agents: Recombinant Human Platelet-Derived Growth Factor-BB (rhPDGF-BB, Enamel Matrix Derivate (EMD, Platelet-Rich Plasma (PRP and Platelet-Rich Fibrin (PRF, Recombinant Human Fibroblast Growth Factor-2 (rhFGF-2, Bone Morphogenic Proteins (BMPs, BMP-2 and BMP-7, Teriparatide PTH, and Growth Differential Factor-5 (GDF-5.

  3. Effect of Recycled Rubber Particles and Silica on Tensile and Tear Properties of Natural Rubber Composites

    Directory of Open Access Journals (Sweden)

    Velu CHANDRAN

    2016-05-01

    Full Text Available Application of scrap rubber and worn out tires in natural rubber compounds has been studied. The scrap rubber can, however, be recycled and compounded with natural rubber and thus can be generated as a rubber composite. In this work, recycled rubber particles (RRP were prepared using pulverization process. Then, RRP was blended with natural rubber and silica compounds, and it was synthesized by two- roll mill and hydraulic press at specified operating conditions. The samples ranging from 0 to 40 phr of RRP loaded with silica were used as constant filler. The mechanical properties and morphological analysis were carried out. The results showed that tensile strength and elongation at break gradually decreased with increasing RRP loading in natural rubber and silica compounds. Tensile modulus went down at 10 phr of RRP and then showed an increasing trend. Hardness increased up to 30 phr of RRP and tear strength increased up to 20 phr of RRP. A comparative study was also carried out with virgin natural rubber vulcanizates. The incorporation of RRP and silica up to 20 phr in natural rubber did not lower the performance of rubber articles. Morphological studies revealed that better filler dispersion, interfacial adhesion, and cross link density could increase the tensile and tear strengths.DOI: http://dx.doi.org/10.5755/j01.ms.22.2.7330

  4. Thrombocytopenia following implantation of the stentless biological sorin freedom SOLO valve.

    Science.gov (United States)

    Gersak, Borut; Gartner, Urska; Antonic, Miha

    2011-07-01

    Stentless biological valves have proven advantages in hemodynamic performance and left ventricular function compared to stented biological valves. Following a marked postoperative fall in the platelet count of patients after implantation of the Freedom SOLO valve, the study aim was to confirm clinical observations that this effect was more severe in patients receiving Freedom SOLO valves than in those receiving St. Jude Medical (SJM) mechanical aortic valves. Preoperative and postoperative platelet counts were compared in two groups of patients who underwent aortic valve replacement (AVR) without any concomitant procedures between January and December 2007. Patients received either a Freedom SOLO valve (n = 28) or a SJM mechanical valve (n = 41). Mean values of platelet counts were compared using three multiple linear regression models. Platelet counts were significantly lower in the Freedom SOLO group than in the SJM group from the first postoperative day (POD 1) up to POD 6 (p SOLO group the platelet count fell below 30x10(9)/l, while the lowest level in the SJM group was 75x10(9)/l. Based on multiple linear regression models, the type of valve implanted had a statistically significant influence on postoperative platelet counts on POD 1, POD 3, and POD 5 (p SOLO group.

  5. Low power digital communication in implantable devices using volume conduction of biological tissues.

    Science.gov (United States)

    Yao, Ning; Lee, Heung-No; Sclabassi, R J; Sun, Mingui

    2006-01-01

    This work investigates the data communication problem of implantable devices using fundamental theories in communications. We utilize the volume conduction property of biological tissues to establish a digital communications link. Data obtained through animal experiments are used to analyze the time and frequency response of the volume conduction channel as well as to characterize the biological signals and noises present in the system. A low power bandwidth efficient channel-coded modulation scheme is proposed to conserve battery power and reduce the health risks associated.

  6. Multilayer graphene rubber nanocomposites

    Science.gov (United States)

    Schartel, Bernhard; Frasca, Daniele; Schulze, Dietmar; Wachtendorf, Volker; Krafft, Bernd; Morys, Michael; Böhning, Martin; Rybak, Thomas

    2016-05-01

    Multilayer Graphene (MLG), a nanoparticle with a specific surface of BET = 250 m2/g and thus made of only approximately 10 graphene sheets, is proposed as a nanofiller for rubbers. When homogenously dispersed, it works at low loadings enabling the replacement of carbon black (CB), increase in efficiency, or reduction in filler concentration. Actually the appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing and mechanical properties of different rubbers, as shown for Chlorine-Isobutylene-Isoprene Rubber (CIIR), Nitrile-Butadiene Rubber (NBR), Natural Rubber (NR), and Styrene-Butadiene Rubber (SBR). A mere 3 phr of MLG tripled the Young's modulus of CIIR, an effect equivalent to 20 phr of carbon black. Similar equivalents are observed for MLG/CB mixtures. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards fire behavior. The later shown by the reduction in heat release rate in the cone calorimeter. The higher the nanofiller concentration is (3 phr, 5 phr, and 10 phr was investigated), the greater the improvement in the properties of the nanocomposites. Moreover, the MLG nanocomposites improve stability of mechanical properties against weathering. An increase in UV-absorption as well as a pronounced radical scavenging are proposed and were proved experimentally. To sum up, MLG is interesting as a multifunctional nanofiller and seems to be quite ready for rubber development.

  7. Advances in rubber/halloysite nanotubes nanocomposites.

    Science.gov (United States)

    Jia, Zhixin; Guo, Baochun; Jia, Demin

    2014-02-01

    The research advances in rubber/halloysite nanotubes (rubber/HNTs) nanocomposites are reviewed. HNTs are environmentally-friendly natural nanomaterials, which could be used to prepare the rubber-based nanocomposites with high performance and low cost. Unmodified HNTs could be adopted to prepare the rubber/HNTs composites with improved mechanical properties, however, the rubber/HNTs nanocomposites with fine morphology and excellent properties were chiefly prepared with various modifiers by in situ mixing method. A series of rubber/HNTs nanocomposites containing several rubbers (SBR, NR, xSBR, NBR, PU) and different modifiers (ENR, RH, Si69, SA, MAA, ILs) have been investigated. The results showed that all the rubber/HNTs nanocomposites achieved strong interfacial interaction via interfacial covalent bonds, hydrogen bonds or multiple interactions, realized significantly improved dispersion of HNTs at nanoscale and exhibited excellent mechanical performances and other properties.

  8. Electrospinning of PVC with natural rubber

    Science.gov (United States)

    Othman, Muhammad Hariz; Mohamed, Mahathir; Abdullah, Ibrahim

    2013-11-01

    Polyvinyl chloride (PVC) was mixed with natural rubbers which are liquid natural rubber (LNR), liquid epoxidised natural rubber (LENR) and liquid epoxidised natural rubber acrylate (LENRA) for a preparation of a fine non-woven fiber's mat. PVC and each natural rubbers(PVC:LENR, PVC:LNR and PVC:LENRA) were mixed based on ratio of 70:30. Electrospinning method was used to prepare the fiber. The results show that the spinnable concentration of PVC/ natural rubber/THF solution is 16 wt%. The morphology, diameter, structure and degradation temperature of electrospun fibers were investigated by scanning electron microscopy (SEM) and thermogravimetric analysis (TGA). SEM photos showed that the morphology and diameter of the fibers were mainly affected by the addition of natural rubber. TGA results suggested that PVC electrospun fiber has higher degradation temperature than those electrospun fibers that contain natural rubber.

  9. Electrospinning of PVC with natural rubber

    International Nuclear Information System (INIS)

    Othman, Muhammad Hariz; Abdullah, Ibrahim; Mohamed, Mahathir

    2013-01-01

    Polyvinyl chloride (PVC) was mixed with natural rubbers which are liquid natural rubber (LNR), liquid epoxidised natural rubber (LENR) and liquid epoxidised natural rubber acrylate (LENRA) for a preparation of a fine non-woven fiber’s mat. PVC and each natural rubbers(PVC:LENR, PVC:LNR and PVC:LENRA) were mixed based on ratio of 70:30. Electrospinning method was used to prepare the fiber. The results show that the spinnable concentration of PVC/ natural rubber/THF solution is 16 wt%. The morphology, diameter, structure and degradation temperature of electrospun fibers were investigated by scanning electron microscopy (SEM) and thermogravimetric analysis (TGA). SEM photos showed that the morphology and diameter of the fibers were mainly affected by the addition of natural rubber. TGA results suggested that PVC electrospun fiber has higher degradation temperature than those electrospun fibers that contain natural rubber

  10. Electrospinning of PVC with natural rubber

    Energy Technology Data Exchange (ETDEWEB)

    Othman, Muhammad Hariz; Abdullah, Ibrahim [Department of Chemistry, Faculty of Science and Technology, Universiti Kebangsaan Malaysia, 43600 Bangi, Selangor (Malaysia); Mohamed, Mahathir [Radiation Processing Technology Division (BTS), Malaysian Nuclear Agency, Bangi, 43000, Kajang (Malaysia)

    2013-11-27

    Polyvinyl chloride (PVC) was mixed with natural rubbers which are liquid natural rubber (LNR), liquid epoxidised natural rubber (LENR) and liquid epoxidised natural rubber acrylate (LENRA) for a preparation of a fine non-woven fiber’s mat. PVC and each natural rubbers(PVC:LENR, PVC:LNR and PVC:LENRA) were mixed based on ratio of 70:30. Electrospinning method was used to prepare the fiber. The results show that the spinnable concentration of PVC/ natural rubber/THF solution is 16 wt%. The morphology, diameter, structure and degradation temperature of electrospun fibers were investigated by scanning electron microscopy (SEM) and thermogravimetric analysis (TGA). SEM photos showed that the morphology and diameter of the fibers were mainly affected by the addition of natural rubber. TGA results suggested that PVC electrospun fiber has higher degradation temperature than those electrospun fibers that contain natural rubber.

  11. Degradation of blending vulcanized natural rubber and nitril rubber (NR/NBR) by dimethyl ether through variation of elastomer ratio

    Science.gov (United States)

    Saputra, A. H.; Juneva, S.; Sari, T. I.; Cifriadi, A.

    2018-04-01

    Dimethyl ether can cause degradation of the rubber material seal in some applications. In order to use of natural rubber in industry, research about a blending of natural rubber (NR) and nitrile rubber (NBR) to produce rubber to meet the standard seal material application were conducted. This study will observe the degradation mechanisms that occur in the blending natural rubber and nitrile rubber (NR/NBR) by dimethyl ether. Nitrile rubber types used in this study is medium quality nitrile rubber with 33% of acrylonitrile content (NBR33). The observed parameters are percent change in mass, mechanical properties and surface morphology. This study is limited to see the effect of variation vulcanized blending ratio (NR/NBR33) against to swelling. The increase of nitrile rubber (NBR33) ratio of blending rubber vulcanized can reduce the tensile strength and elongation. The best elastomer variation was obtained after comparing with the standard feasibility material of seal is rubber vulcanized blending (NR/NBR33) with ratio 40:60 NR: NBR.

  12. Robotically enhanced rubber hand illusion.

    Science.gov (United States)

    Arata, Jumpei; Hattori, Masashi; Ichikawa, Shohei; Sakaguchi, Masamichi

    2014-01-01

    The rubber hand illusion is a well-known multisensory illusion. In brief, watching a rubber hand being stroked by a paintbrush while one's own unseen hand is synchronously stroked causes the rubber hand to be attributed to one's own body and to "feel like it's my hand." The rubber hand illusion is thought to be triggered by the synchronized tactile stimulation of both the subject's hand and the fake hand. To extend the conventional rubber hand illusion, we introduce robotic technology in the form of a master-slave telemanipulator. The developed one degree-of-freedom master-slave system consists of an exoskeleton master equipped with an optical encoder that is worn on the subject's index finger and a motor-actuated index finger on the rubber hand, which allows the subject to perform unilateral telemanipulation. The moving rubber hand illusion has been studied by several researchers in the past with mechanically connected rigs between the subject's body and the fake limb. The robotic instruments let us investigate the moving rubber hand illusion with less constraints, thus behaving closer to the classic rubber hand illusion. In addition, the temporal delay between the body and the fake limb can be precisely manipulated. The experimental results revealed that the robotic instruments significantly enhance the rubber hand illusion. The time delay is significantly correlated with the effect of the multisensory illusion, and the effect significantly decreased at time delays over 100 ms. These findings can potentially contribute to the investigations of neural mechanisms in the field of neuroscience and of master-slave systems in the field of robotics.

  13. Structural characterization of rubber from jackfruit and euphorbia as a model of natural rubber.

    Science.gov (United States)

    Mekkriengkrai, Dararat; Ute, Koiichi; Swiezewska, Ewa; Chojnacki, Tadeusz; Tanaka, Yasuyuki; Sakdapipanich, Jitladda T

    2004-01-01

    A structural study of low molecular weight rubbers from Jackfruit (Artocarpus heterophyllus) and Painted spurge (Euphorbia heterophylla) was carried out as model compounds of natural rubber from Hevea brasiliensis. The rubber content of latex from Jackfruit was 0.4-0.7%, which is very low compared with that of 30-35% in the latex from Hevea tree. The rubber from Jackfruit latex was low molecular weight with narrow unimodal molecular weight distribution (MWD), whereas that obtained from E. heterophylla showed very broad MWD. The 1H and 13C NMR analyses showed that Jackfruit rubber consists of a dimethylallyl group and two trans-isoprene units connected to a long sequence of cis-isoprene units. The alpha-terminal group of Jackfruit rubber was presumed to be composed of a phosphate group based on the presence of 1H NMR signal at 4.08 ppm corresponding to the terminal =CH-CH2OP group.

  14. Magnetic rubber inspection (MRI)

    International Nuclear Information System (INIS)

    Carro, L.

    1997-01-01

    Magnetic Rubber Inspection (MRI) was developed to inspect for small cracks and flaws encountered in high performance aircraft. A formula of very fine magnetic particles immersed in a room temperature curing rubber is catalysed and poured into dams (retainers) on the surface of the part to be inspected. Inducing a magnetic field then causes the particles to be drawn to discontinuities in the component under test. These indicating particles are held to the discontinuity by magnetic attraction, as the rubber cures. The solid rubber cast (Replica) is then removed and examined under a microscope for indicating lines of particle concentrations. 3 refs., 6 figs

  15. Comparative studies on the mechanical properties of natural rubber and natural rubber filled with multi-walled carbon nanotubes

    Science.gov (United States)

    Ismail, R.; Ibrahim, A.; Rusop, M.; Adnan, A.

    2018-05-01

    The present article compares the mechanical properties of natural rubber (NR) and carbon nanotubes (CNTs) filled natural rubber composites. Four types of nanocomposite specimens are fabricated with different MWCNT loadings: 0 wt% (pure natural rubber), 1 wt%, 3 wt%, and 5 wt%. The specimens are tested for their mechanical properties. It is observed that the tensile strength, hardness and elongation break of CNTs filled rubber composites are remarkably higher than that of raw rubber indicating the inherent reinforcing potential of CNTs. Percentage of the elongation at break of rubber CNTs composites is lower than that of raw rubber.

  16. The Effect of Gamma Irradiation on the Mechanical Properties of vulcanized Natural Rubber and Natural Rubber-Polyethylene Blends

    International Nuclear Information System (INIS)

    Sudradjat Iskandar

    2008-01-01

    To enhance the quality of vulcanized natural rubber and natural rubber-polyethylene blends, gamma irradiation has been done. The compound of natural rubber and natural rubber-polyethylene blends made by using roll mill machine. The mixed materials were antioxidant, anti ozon, plasticizer and vulcanisator. The natural rubber and natural rubber-polyethylene blends compound were vulcanizer and made a slab (film of sample) using hot and could press machine. The slabs produced were then gamma irradiated at irradiation dose of 75, 150 and 300 kGy. Before and after irradiation, the slab were characterized using strograph R1 machine. The results showed that the modulus 300 and hardness of vulcanized natural rubber and natural rubber-polyethylene blends were increasing; the tensile strength and tear strength were increasing to maximum level then decreasing with gamma irradiation, while the elongation at break was decreasing. The maximum tensile strength of vulcanized natural rubber and natural rubber-polyethylene blends were found at irradiation dose of 75 kGy. At the irradiation dose of 75 kGy, the tensile strength of vulcanized natural rubber increased from 17.6 MN/m 2 to 21.2 MN/m 2 , while the tensile strength of vulcanized natural rubber-polyethylene blends increased slightly from 18.7 MN/m 2 to 19.4 MN/m 2 . (author)

  17. Vulcanization of Rubber

    Indian Academy of Sciences (India)

    Temperature 140 -180°C. Sulfur. 2-3 parts per. 100 parts of rubber (phr). Accelerator 0.5-1.0 phr. ZnO ... out an experiment, he spilt a mixture of rubber and sulfur with other ingredients on a hot .... both carbon-sulfur and sulfur-nitrogen bonds -.

  18. Application of gamma irradiation for incorporation of rubber powder in the formulations of EPDM and natural rubber

    International Nuclear Information System (INIS)

    Kiyan, Ludmila Y.P.; Parra, Duclerc Fernandes; Lugao, Ademar Benevolo

    2013-01-01

    The objective of this work was to study the behavior of the recycling of rubber burrs in form of powder, of the rubber industry from EPDM rubber powder and natural rubber with SBR. The rubber powder was irradiated and reused in rubber artifacts formulations for classical vulcanization. The processed material was irradiated using a 60 Co source in doses of 50, 100, 150 and 200 kGy and a dose rate of 5 kGy s-1 at room temperature. The radiation created devulcanization active sites for subsequent integration of the material (rubber powder) in formulations of commercial use. The processes were compared and their products characterized by analytical methods of the physical properties such as strength and elongation. Satisfactory results were found, noting a major spin-off of EPDM chain demonstrated by increased elongation

  19. Tribology Aspect of Rubber Shock Absorbers Development

    Directory of Open Access Journals (Sweden)

    M. Banić

    2013-09-01

    Full Text Available Rubber is a very flexible material with many desirable properties Which enable its broad use in engineering practice. Rubber or rubber-metal springs are widely used as anti-vibration or anti-shock components in technical systems. Rubber-metal springs are usually realized as a bonded assembly, however especially in shock absorbers, it is possible to realize free contacts between rubber and metal parts. In previous research it authors was observed that friction between rubber and metal in such case have a significant influence on the damping characteristics of shock absorber. This paper analyzes the development process of rubber or rubber-metal shock absorbers realized free contacts between the constitutive parts, starting from the design, construction, testing and operation, with special emphasis on the development of rubber-metal springs for the buffing and draw gear of railway vehicles.

  20. Lifetime Analysis of Rubber Gasket Composed of Methyl Vinyl Silicone Rubber with Low-Temperature Resistance

    Directory of Open Access Journals (Sweden)

    Young-Doo Kwon

    2015-01-01

    Full Text Available Most machines and instruments constantly require elastomeric materials like rubber for the purposes of shock absorption, noise attenuation, and sealing. The material properties and accurate lifetime prediction of rubber are closely related to the quality of machines, especially their durability and reliability. The properties of rubber-like elastomers are influenced by ambient conditions, such as temperature, environment, and mechanical load. Moreover, the initial properties of rubber gaskets must be sustained under working conditions to satisfy their required function. Because of its technical merits, as well as its low cost, the highly accelerated life test (HALT is used by many researchers to predict the long-term lifetime of rubber materials. Methyl vinyl silicone rubber (VMQ has recently been adopted to improve the lifetime of automobile radiator gaskets. A four-parameter method of determining the recovery ability of the gaskets was recently published, and two revised methods of obtaining the recovery were proposed for polyacrylate (ACM rubber. The recovery rate curves for VMQ were acquired using the successive zooming genetic algorithm (SZGA. The gasket lifetime for the target recovery (60% of a compressed gasket was computed somewhat differently depending on the selected regression model.

  1. The role of linked phospholipids in the rubber-filler interaction in carbon nanotube (CNT) filler natural rubber (NR) composites

    NARCIS (Netherlands)

    Le, H.H.; Abhijeet, S.; Ilish, S.; Klehm, J.; Henning, S.; Beiner, M.; Sarkawi, S.S.; Dierkes, Wilma K.; Das, A.; Fischer, D.; Stöckelhuber, K.-W.; Wiessner, S.; Khatiwada, S.P.; Adhikari, R.; Pham, T.; Heinrich, G.; Radusch, H.-J.

    2014-01-01

    The aim of the present work is to evidence the role of the linked phospholipids of natural rubber (NR) in the rubber-carbon nanotube (CNT) interactions in rubber composites. Three rubbers namely NR, deproteinized NR (DPNR) and a synthetic rubber isoprene (IR) were used as matrix for CNTs. The

  2. Silencing the lettuce homologs of small rubber particle protein does not influence natural rubber biosynthesis in lettuce (Lactuca sativa).

    Science.gov (United States)

    Chakrabarty, Romit; Qu, Yang; Ro, Dae-Kyun

    2015-05-01

    Natural rubber, cis-1,4-polyisoprene, is an important raw material in chemical industries, but its biosynthetic mechanism remains elusive. Natural rubber is known to be synthesized in rubber particles suspended in laticifer cells in the Brazilian rubber tree (Hevea brasiliensis). In the rubber tree, rubber elongation factor (REF) and its homolog, small rubber particle protein (SRPP), were found to be the most abundant proteins in rubber particles, and they have been implicated in natural rubber biosynthesis. As lettuce (Lactuca sativa) can synthesize natural rubber, we utilized this annual, transformable plant to examine in planta roles of the lettuce REF/SRPP homologs by RNA interference. Among eight lettuce REF/SRPP homologs identified, transcripts of two genes (LsSRPP4 and LsSRPP8) accounted for more than 90% of total transcripts of REF/SRPP homologs in lettuce latex. LsSRPP4 displays a typical primary protein sequence as other REF/SRPP, while LsSRPP8 is twice as long as LsSRPP4. These two major LsSRPP transcripts were individually and simultaneously silenced by RNA interference, and relative abundance, polymer molecular weight, and polydispersity of natural rubber were analyzed from the LsSRPP4- and LsSRPP8-silenced transgenic lettuce. Despite previous data suggesting the implications of REF/SRPP in natural rubber biosynthesis, qualitative and quantitative alterations of natural rubber could not be observed in transgenic lettuce lines. It is concluded that lettuce REF/SRPP homologs are not critically important proteins in natural rubber biosynthesis in lettuce. Copyright © 2014 Elsevier Ltd. All rights reserved.

  3. Physico-mecha-nical properties of rubber seed shell carbon – filled natural rubber compounds

    Directory of Open Access Journals (Sweden)

    L.O. Ekebafe

    2010-07-01

    Full Text Available Samples of rubber seed shells were carbonized at varying temperatures (100, 200, 300, 400, 500, 600, 700 and 800 °C for three hours each and sieved through a 150 μm screen. The portion of the rubber seed shell carbon that passed through the screen was characterized in terms of loss on ignition, surface area, moisture content, pH, bulk density, and metal content and used in compounding natural rubber. The characterization shows that the pH, conductivity, loss on ignition and the surface area increases with the increases of the heating temperature, unlike the bulk density which decreases. The compound mixes were cured using the efficient vulcanization system. Cure characteristics of compounds and physico-mechanical properties of the vulcanisates were measured as a function of filler loading along with that of N330 carbon-black filled natural rubbers. The results showed that the cure times, scorch times and the torque gradually increased, with increasing the filler content for rubber seed shell carbon-filled natural rubber, with the filler obtained at carbonizing temperature of 600 °C tending to show optimum cure indices. The physicomechanical properties of the vulcanisates increase with filler loading. The reinforcing potential of the carbonized rubber seed shell carbon was found to increase markedly for the filler obtained at the temperature range of 500-600 °C and then decreases with further increase in temperature.

  4. Constructing better roads with asphalt rubber

    Directory of Open Access Journals (Sweden)

    Pais Jorge C.

    2015-12-01

    Full Text Available Brazilians mixtures containing asphalt rubber were evaluated by mechanical laboratory tests. A conventional mixture with asphalt CAP-50/70 was produced as a mixture control. With the aim of compare the Brazilians mixtures performance, a Portuguese asphalt rubber mixture was tested as well. The testing set involved the determination of the mechanical properties, fatigue and permanent deformation, of asphalt rubber produced by wet process through two different systems: continuous blend and terminal blend. The asphalt rubber morphology was evaluated in order to determine the compatibility of the systems. The asphalt rubber mixtures exhibit good resistance to permanent deformation and prolonged fatigue life in relation to mixture control. Therefore it is concluded that the application of asphalt rubber alters the characteristics of asphalt mixture in a very beneficial way.

  5. Rubber modification of asphalt binders and mixes

    Energy Technology Data Exchange (ETDEWEB)

    Morrison, G.; Hesp, S.A.M. [Queen`s Univ., Kingston, ON (Canada). Dept. of Chemistry

    1995-12-31

    The physical properties of asphalt binders and concrete, modified with waste rubber tire, were examined. In an experiment designed to address the concern of waste disposal of scrap rubber, a control asphalt, devulcanized rubber modified asphalt and a crumb rubber modified asphalt were used to make asphalt concrete mixes. The three mixes were subjected to a thermal stress test to determine their low temperature fracture temperatures and strengths. Results were discussed in terms of the binder material used. At high service temperatures, the addition of 10% devulcanized rubber was found to have no beneficial effect, whereas the addition of 10% 80 mesh crumb rubber produced a modest improvement in performance. At low temperatures, the addition of devulcanized rubber produced increased resistance to cracking up to 90%. The addition of 10% 80 mesh crumb rubber increased fracture toughness by a factor of 3.3 times. 12 refs., 3 tabs.

  6. Biological Activation of Inert Ceramics: Recent Advances Using Tailored Self-Assembled Monolayers on Implant Ceramic Surfaces

    Science.gov (United States)

    Böke, Frederik; Schickle, Karolina; Fischer, Horst

    2014-01-01

    High-strength ceramics as materials for medical implants have a long, research-intensive history. Yet, especially on applications where the ceramic components are in direct contact with the surrounding tissue, an unresolved issue is its inherent property of biological inertness. To combat this, several strategies have been investigated over the last couple of years. One promising approach investigates the technique of Self-Assembled Monolayers (SAM) and subsequent chemical functionalization to create a biologically active tissue-facing surface layer. Implementation of this would have a beneficial impact on several fields in modern implant medicine such as hip and knee arthroplasty, dental applications and related fields. This review aims to give a summarizing overview of the latest advances in this recently emerging field, along with thorough introductions of the underlying mechanism of SAMs and surface cell attachment mechanics on the cell side. PMID:28788687

  7. Solubility Study of Curatives in Various Rubbers

    NARCIS (Netherlands)

    Guo, R.; Talma, Auke; Datta, Rabin; Dierkes, Wilma K.; Noordermeer, Jacobus W.M.

    2008-01-01

    The previous works on solubility of curatives in rubbers were mainly carried out in natural rubber. Not too much information available on dissimilar rubbers and this is important because most of the compounds today are blends of dissimilar rubbers. Although solubility can be expected to certain

  8. Nitrile rubber and carboxylated nitrile rubber resistance to soybean biodiesel

    OpenAIRE

    Felipe Nunes Linhares; Cléverson Fernandes Senra Gabriel; Ana Maria Furtado de Sousa; Marcia Christina Amorim Moreira Leite; Cristina Russi Guimarães Furtado

    2018-01-01

    Abstract Biodiesel has been considered a suitable substitute for petroleum diesel, but their chemical composition differs greatly. For this reason, biodiesel interacts differently than petroleum diesel with various materials, including rubbers. Therefore, the resistance of some elastomers should be thoroughly evaluated, specifically those which are commonly used in automotive industry. Nitrile rubber (NBR) is widely used to produce vehicular parts that are constantly in contact with fuels. T...

  9. QENS investigation of filled rubbers

    CERN Document Server

    Triolo, A; Desmedt, A; Pieper, J K; Lo Celso, F; Triolo, R; Negroni, F; Arrighi, V; Qian, H; Frick, B

    2002-01-01

    The polymer segmental dynamics is investigated in a series of silica-filled rubbers. The presence of inert fillers in polymers greatly affects the mechanical and physical performance of the final materials. For example, silica has been proposed as a reinforcing agent of elastomers in tire production. Results from quasielastic neutron scattering and Dynamic Mechanical Thermal Analysis (DMTA) measurements are presented on styrene-ran-butadiene rubber filled with silica. A clear indication is obtained of the existence of a bimodal dynamics, which can be rationalized in terms of the relaxation of bulk rubber and the much slower relaxation of the rubber adsorbed on the filler surface. (orig.)

  10. Carboxy terminated rubber based on natural rubber grafted with acid anhydrides and its adhesion properties

    International Nuclear Information System (INIS)

    Klinpituksa, P; Kongkalai, P; Kaesaman, A

    2014-01-01

    The chemical modification of natural rubber by grafting of various polar functional molecules is an essential method, improving the versatility of rubber in applications. This research investigated the preparation of natural rubber-graft-citraconic anhydride (NR-g-CCA), natural rubber-graft-itaconic anhydride (NR-g-ICA), and natural rubber-graft-maleic anhydride (NR-g-MA), with the anhydrides grafted to natural rubber in toluene using benzoyl peroxide as an initiator. Variations of monomer content, initiator content, temperature and reaction time of the grafting copolymerization were investigated. The maximum degrees of grafting were 1.06% for NR-g-CCA, 4.66% for NR-g-ICA, and 5.03% for NR-g-MA, reached using 10 phr citraconic anhydride, 10 phr of itaconic anhydride, or 8 phr of maleic anhydride, 3 phr benzoyl peroxide, at 85, 80 and 80°C for 2, 2 and 3 hrs, respectively. Solvent-based wood adhesives were formulated from these copolymers with various contents of wood resin in the range 10-40 phr. The maximal 289 N/in cleavage peel and 245.7 KPa shear strength for NR-g-MA (5.03% grafting) were obtained at 40 phr wood resin

  11. Hyundai plans rubber unit despite overcapacity

    International Nuclear Information System (INIS)

    Hyoungjin Kim.

    1993-01-01

    Despite the oversupply of synthetic rubber in South Korea, the government has granted approval to Hyundai Petrochemical (Seoul) to build the country's second synthetic rubber unit, to be located alongside its petrochemical complex at Daesan. The plant is due for startup during second-half 1995, when the local market is expected to be in better balance. Hyundai will use Goodyear Tire ampersand Rubber technology for the plant, which will have annual capacities for 40,000 m.t. of polybutadiene rubber (BR), 30,000 m.t. of styrene butadiene rubber (SBR) and 12,000 m.t. of nitrile rubber (NBR). Styrene and butadiene requirements will be met from Hyundai's own production at Daesan. The current local producer of synthetic rubber is Korea Kumho Petrochemicals (Seoul), which has annual capacities for 150,000 m.t. of SBR, 95,000 m.t. of BR, and 10,000 m.t. of NBR. Korean SBR demand is about 141,000 m.t./year but is expected to increase to 161,000 m.t./year by 1996 and reach 194,000 m.t./year by the end of the decade

  12. Multi-scale, multi-modal analysis uncovers complex relationship at the brain tissue-implant neural interface: new emphasis on the biological interface

    Science.gov (United States)

    Michelson, Nicholas J.; Vazquez, Alberto L.; Eles, James R.; Salatino, Joseph W.; Purcell, Erin K.; Williams, Jordan J.; Cui, X. Tracy; Kozai, Takashi D. Y.

    2018-06-01

    Objective. Implantable neural electrode devices are important tools for neuroscience research and have an increasing range of clinical applications. However, the intricacies of the biological response after implantation, and their ultimate impact on recording performance, remain challenging to elucidate. Establishing a relationship between the neurobiology and chronic recording performance is confounded by technical challenges related to traditional electrophysiological, material, and histological limitations. This can greatly impact the interpretations of results pertaining to device performance and tissue health surrounding the implant. Approach. In this work, electrophysiological activity and immunohistological analysis are compared after controlling for motion artifacts, quiescent neuronal activity, and material failure of devices in order to better understand the relationship between histology and electrophysiological outcomes. Main results. Even after carefully accounting for these factors, the presence of viable neurons and lack of glial scarring does not convey single unit recording performance. Significance. To better understand the biological factors influencing neural activity, detailed cellular and molecular tissue responses were examined. Decreases in neural activity and blood oxygenation in the tissue surrounding the implant, shift in expression levels of vesicular transporter proteins and ion channels, axon and myelin injury, and interrupted blood flow in nearby capillaries can impact neural activity around implanted neural interfaces. Combined, these tissue changes highlight the need for more comprehensive, basic science research to elucidate the relationship between biology and chronic electrophysiology performance in order to advance neural technologies.

  13. Static friction in rubber-metal contacts with application to rubber pad forming processes

    NARCIS (Netherlands)

    Deladi, E.L.

    2006-01-01

    A static friction model suitable for rubber-metal contact is presented in this dissertation. In introduction, the motivation and the aims of the research are introduced together with the background regarding the related industrial application, which is the rubber pad forming process.

  14. Studies on the increased heat effect within the rubber tree rows of man-made rubber-tea community

    International Nuclear Information System (INIS)

    Ma Youxin

    1994-01-01

    Differences in the various components of thermal balance and the microclimatic factors within lower layers of rubber tree rows between a man-made rubber-tea community(RTC)and a pure rubber garden(PRG)in the coldest month were studied in Xishuangbanna,Yun-nan province

  15. Radiation induced graft copolymerization of acrylonitrile on natural rubber

    International Nuclear Information System (INIS)

    Claramma, N.M.; Mathew, N.M.; Thomas, E.V.

    1989-01-01

    Acrylonitrile graft natural rubber was prepared by initiating the polymerization of acrylonitrile in natural rubber field latex using γ-rays. The reaction was carried out at different rubber-monomer concentrations and the properties of the modified rubbers were compared with those of natural rubber and nitrile rubber. (author)

  16. Biodiversity in rubber agroforests

    NARCIS (Netherlands)

    Beukema, Hendrien

    2013-01-01

    Jungle rubber tuinen zijn extensieve rubber agroforests die qua structuur op secundaire bossen lijken, en waarin wilde soorten door de boer worden getolereerd. Met het verdwijnen van het laaglandregenwoud rijst de vraag of de begroeiing die ervoor in de plaats komt een aantal kenmerken en functies

  17. Enzymatic synthesis of rubber polymer in Hevea brasiliensis

    Energy Technology Data Exchange (ETDEWEB)

    Tang, F.; Hu, S.; Benedict, C.R. (Texas A and M Univ., College Station (United States))

    1991-05-01

    Light and Dennis purified serum soluble rubber transferase from Hevea latex to homogeneity. Prenyl transferase co-purified with rubber transferase. In the absence of washed rubber particles (WRP) the prenyl transferase catalyzed the formation of trans FPP from DMAPP and IPP. In the presence of WRP the transferase catalyzed cis additions of IPP to pre-existing rubber chains. Control mixtures of WRP, Mg{sup 2+} and FPP were not included to test for the contributions of the bound rubber transferase on WRP to the incorporation of IPP into polyisoprene. Bound rubber transferase catalyzes the repetitive addition of IPP to allylic-PP starter molecules to form polyisoprene. The order of utilization of allylic-PP starters was GGPP > FPP > GPP > DMAPP. The authors have shown that the polyisoprene enzymatically synthesized on WRP is a bimodal polymer consisting of different mol wt rubber chains similar to the polymeric characteristics of natural rubber. The bound rubber transferase was solubilized with Chaps and purified on DEAE-cellulose. The polymerization reaction catalyzed by the purified preparation showed a 98% requirement for pre-existing rubber chains. Results suggest that the prenyl transferase from Hevea serum may be part of the polymer starter system furnishing allylic-PP for the bound rubber transferase.

  18. Performance of self-compacting rubberized concrete

    Directory of Open Access Journals (Sweden)

    Hamza Bensaci

    2018-01-01

    Full Text Available Used tyre rubber wastes present a serious environmental problem of pollution and storage. The recycling of this waste in the industry of construction could be an appropriate solution to produce an eco-concrete and could contribute to the improvement of some of its properties. This paper aims to study the possibility of using tyre rubber waste as fine aggregate replacement in self-compacting concrete (SCC. Fines rubber particles of 0-2 mm of waste tyres were added SCC mixtures as a partial substitution of the total volume of sand at different percentages (5, 10, 15, 20 and 30%. The influence of fines rubber of used tyres on fresh and hardened properties of the SCC was investigated. The fresh properties of SCC were performed by using slump-flow, T50 flow time, L-box, V-funnel and segregation resistance tests. Characteristics of the hardened state were obtained by compressive strength and thermal conductivity. The experimental results showed that the inclusion of fines rubber in SCC decreases the workability, reduced its passing capacity and increases the possibility of blocking. A decrease in compressive strength is observed with the increase in rubber content. On the other hand, the incorporation of the rubber fines aggregates enhances in a remarkably way the thermal conductivity.

  19. Chlorinated rubbers with advanced properties for tire industry

    Science.gov (United States)

    Mikhaylov, I. A.; Sukhareva, K. V.; Andriasyan, Yu. O.; Popov, A. A.

    2017-12-01

    The paper investigates the production and processing of halide-modified chlorinated rubbers, such as isobutylene isoprene rubber and ethylene-propylene-diene-monomer rubber (IIR and EPDM), which are perspective in terms of application in rubber industry. Prospects for their production and application are determined by the specific properties of these rubbers (low gas permeability of IIR, high heat and ozone resistance of EPDM). These properties are governed by the structure of both initial IIR and EPDM and chlorinated rubbers (ChIIR and ChEPDM). A new alternative technology of obtaining chlorinated elastomers based on solid-phase mechanochemical halide modification is proposed. Novel chlorinated polyolefin rubbers obtained by the developed technology show good technological properties under industrial production conditions due to enhanced covulcanization.

  20. Production and performance of desulfurized rubber asphalt binder

    Directory of Open Access Journals (Sweden)

    Yanping Sheng

    2017-05-01

    Full Text Available Asphalt rubber binder typically exhibits disadvantages like segregation and high viscosity; however, this can be improved by the incorporation of desulfurized rubber powder. This study examined the swelling principle of desulfurized rubber asphalt (DRA. In addition, it evaluated the performance of DRA fabricated with various rubber powder contents under different shear conditions and development time. Superpave binders tests, including Brookfield viscosity, dynamic shear rheometer (DSR and bending beam rheometer (BBR tests, were applied on three control binders (i.e., neat, 20 mesh asphalt rubber binder, 40 mesh asphalt rubber binder and a DRA binder. Binder testing results indicated that rubber powder swelled into the base binder and resulted in enhanced stability. Optimum performance of the DRA binder was achieved by adding 20% (by weight of rubber powder into the base binder at shear rate, shear temperature, shear time and development time of 7000 r/min, 170 °C, 60 min and 45 min, respectively. Modified ranges of production conditions were also provided to widen the application of DRA in field construction. It appeared that DRA binder benefited from the recovered plasticity and viscosity of the rubber and consequently, exhibited superior performance over the neat and conventional asphalt rubber binders. Preliminary mixture evaluation was also conducted and the DRA binder was found to significantly improve the mixture resistance to permanent deformation and water damage. Overall, the DAR binder is encouraged to be used as a modified binder for flexible pavements. Keywords: Desulfurized rubber asphalt, Swelling model, Production process, Asphalt performance, Rubber asphalt

  1. Chemical modifications of liquid natural rubber

    Science.gov (United States)

    Azhar, Nur Hanis Adila; Rasid, Hamizah Md; Yusoff, Siti Fairus M.

    2016-11-01

    Liquid natural rubber (LNR) was synthesized via photosentisized degradation of natural rubber (NR). LNR was modified into epoxidized liquid natural rubber (LENR) and hydroxylated liquid natural rubber (LNR-OH) using Na2WO4/CH3COOH/H2O2 catalytic system. Chemical structures of LNR and modified LNRs were characterized using Attenuated Total Reflectance Fourier Transform Infrared (ATR-FTIR) and 1H Nuclear Magnetic Resonance (NMR) spectroscopies. Integration of 1H NMR was used to calculate the epoxy content (%) of LENR. 1H NMR detected the formation of LNR-OH after prolonged heating and increased of catalyst in oxidation reaction.

  2. The Cyclization of natural rubber

    International Nuclear Information System (INIS)

    Mirzataheri, M.

    2000-01-01

    The effect of solvent, temperature, time, weight percent of catalyst on the rate and mechanism of cyclization of natural rubber was studied in toluene and xylene solutions having tin tetra chloride catalyst (SnCl 4 ). Iodo metric titration show, with 8% SnCl 4 (based on polymer weight) cyclization occurs, leaving 27.4% of the total unsaturation. Infrared spectra of cyclized natural rubber show decreased absorption intensity at 840 and 780 cm -1 which are characteristic bands of the linear polymer and the appearance of absorption band at 890 cm -1 as cycles were formed. By using this chemical modification, natural rubber is transformed into a resinous thermoplastic, hard, non rubbery cyclized material with much less unsaturation than the original rubber, which could find commercial applications ad adhesives, printing inks, industrial and ship paints

  3. Development of rubber-enriched dandelion varieties by metabolic engineering of the inulin pathway.

    Science.gov (United States)

    Stolze, Anna; Wanke, Alan; van Deenen, Nicole; Geyer, Roland; Prüfer, Dirk; Schulze Gronover, Christian

    2017-06-01

    Natural rubber (NR) is an important raw material for a large number of industrial products. The primary source of NR is the rubber tree Hevea brasiliensis, but increased worldwide demand means that alternative sustainable sources are urgently required. The Russian dandelion (Taraxacum koksaghyz Rodin) is such an alternative because large amounts of NR are produced in its root system. However, rubber biosynthesis must be improved to develop T. koksaghyz into a commercially feasible crop. In addition to NR, T. koksaghyz also produces large amounts of the reserve carbohydrate inulin, which is stored in parenchymal root cell vacuoles near the phloem, adjacent to apoplastically separated laticifers. In contrast to NR, which accumulates throughout the year even during dormancy, inulin is synthesized during the summer and is degraded from the autumn onwards when root tissues undergo a sink-to-source transition. We carried out a comprehensive analysis of inulin and NR metabolism in T. koksaghyz and its close relative T. brevicorniculatum and functionally characterized the key enzyme fructan 1-exohydrolase (1-FEH), which catalyses the degradation of inulin to fructose and sucrose. The constitutive overexpression of Tk1-FEH almost doubled the rubber content in the roots of two dandelion species without any trade-offs in terms of plant fitness. To our knowledge, this is the first study showing that energy supplied by the reserve carbohydrate inulin can be used to promote the synthesis of NR in dandelions, providing a basis for the breeding of rubber-enriched varieties for industrial rubber production. © 2016 The Authors. Plant Biotechnology Journal published by Society for Experimental Biology and The Association of Applied Biologists and John Wiley & Sons Ltd.

  4. Use of rubber crumbs in cement concrete

    Science.gov (United States)

    Longvinenko, A. A.

    2018-03-01

    Rubber crumb obtained from worn out tires has been increasingly used over the last 15-20 years, especially in manufacture of asphalt and cement concrete mixtures. This review pays principal attention to application of the rubber crumb to cement concrete mixtures. Use of the rubber crumb in cement concrete is not as successful as in asphalt concrete mixtures, due to incompatibility problems linked to chemical composition and a significant difference in rigidity between the rubber crumb and concrete mixture aggregates. Different methods are proposed and studied to mitigate the adverse influence and increase the beneficial effects of the rubber crumb when added to cement concrete.

  5. A comparative study of two advanced spraying techniques for the deposition of biologically active enzyme coatings onto bone-substituting implants

    International Nuclear Information System (INIS)

    Jonge, Lise T. de; Ju, J.; Leeuwenburgh, S.C.G.; Yamagata, Y.; Higuchi, T.; Wolke, J.G.C.; Inoue, K.; Jansen, J.A.

    2010-01-01

    Surface modification of implant materials with biomolecule coatings is of high importance to improve implant fixation in bone tissue. In the current study, we present two techniques for the deposition of biologically active enzyme coatings onto implant materials. The well-established thin film ElectroSpray Deposition (ESD) technique was compared with the SAW-ED technique that combines high-frequency Surface Acoustic Wave atomization with Electrostatic Deposition. By immobilizing the enzyme alkaline phosphatase (ALP) onto implant surfaces, the influence of both SAW-ED and ESD deposition parameters on ALP deposition efficiency and ALP biological activity was investigated. ALP coatings with preserved enzyme activity were deposited by means of both the SAW-ED and ESD technique. The advantages of SAW-ED over ESD include the possibility to spray highly conductive protein solutions, and the 60-times faster deposition rate. Furthermore, significantly higher deposition efficiencies were observed for the SAW-ED technique compared to ESD. Generally, it was shown that protein inactivation is highly dependent on both droplet dehydration and the applied electrical field strength. The current study shows that SAW-ED is a versatile and flexible technique for the fabrication of functionally active biomolecule coatings.

  6. Natural rubber (NR) biosynthesis: perspectives from polymer chemistry

    Energy Technology Data Exchange (ETDEWEB)

    Barkakaty, Balaka [ORNL

    2014-01-01

    Natural rubber is an important strategic raw material for manufacturing a wide variety of industrial products. There are at least 2,500 different latex-producing plant species; however, only Hevea brasiliensis (the Brazilian rubber tree) is a commercial source. The chemical structure of natural rubber is cis-1,4-polyisoprene, but the exact structure of the head and end groups remains unknown. Since synthetic cis-1,4-polyisoprenes cannot match the superior properties of natural rubber, understanding the chemistry behind the biosynthetic process is key to finding a possible replacement. T his chapter summarizes our current understandings from the perspective of a polymer scientist by comparing synthetic polyisoprenes to natural rubber. The chapter also highlights biomimetic polymerization, research towards a synthetic match of natural rubber and the role of natural rubber in health care.

  7. Improvement of the titanium implant biological properties by coating with poly (ε-caprolactone)-based hybrid nanocomposites synthesized via sol-gel

    Energy Technology Data Exchange (ETDEWEB)

    Catauro, Michelina; Bollino, Flavia; Papale, Ferdinando [Department of Industrial and Information Engineering, Second University of Naples, Via Roma 21, 81031 Aversa (Italy)

    2016-05-18

    When bioactive coatings are applied to medical implants by means of sol-gel dip coating technique, the biological proprieties of the implant surface can be modified to match the properties of the surrounding tissues. In this study organo-inorganic nanocomposites materials were synthesized via sol-gel. They consisted of an inorganic zirconium-based and silica-based matrix, in which a biodegradable polymer (the poly-ε-caprolactone, PCL) was incorporated in different weight percentages. The synthesized materials, in sol phase, were used to dip-coat a substrate of commercially pure titanium grade 4 (CP Ti gr. 4) in order to improve its biological properties. A microstructural analysis of the obtained films was carried out by scanning electron microscopy (SEM) and attenuated total reflectance (ATR) Fourier transform infrared spectroscopy (FT-IR). Biological proprieties of the coated substrates were investigated by means of in vitro tests.

  8. Amphiphilic semi-interpenetrating polymer networks using pulverized rubber

    Science.gov (United States)

    Shahidi, Nima

    Scrap rubber materials provide a significant challenge to either reuse or safe disposal. Every year, millions of tires are discarded to landfills in the United States, consuming a staggering amount of land space, creating a high risk for large fires, breeding mosquitoes that spread diseases, and wasting the planet's natural resources. This situation cannot be sustained. The challenge of reusing scrap rubber materials is mainly due to the crosslinked structure of vulcanized rubber that prevent them from melting and further processing for reuse. The most feasible recycling approach is believed to be a process in which the vulcanized rubber is first pulverized into a fine powder and then incorporated into new products. The production of fine rubber particles is generally accomplished through the use of a cryogenic process that is costly. Therefore, development of a cost effective technology that utilizes a large quantity of the scrap rubber materials to produce high value added materials is an essential element in maintaining a sustainable solution to rubber recycling. In this research, a cost effective pulverization process, solid state shear extrusion (SSSE), was modified and used for continuous pulverization of the rubber into fine particles. In the modified SSSE process, pulverization takes place at high compressive shear forces and a controlled temperature. Furthermore, an innovative particle modification process was developed to enhance the chemical structure and surface properties of the rubber particles for manufacturing of high value added products. Modification of rubber particles was accomplished through the polymerization of a hydrophilic monomer mixture within the intermolecular structure of the hydrophobic rubber particles. The resulting composite particles are considered as amphiphilic particulate phase semi-interpenetrating polymer networks (PPSIPNs). The modified rubber particles are water dispersible and suitable for use in a variety of aqueous media

  9. Characterization of the natural rubber from new rubber tree clones of PB 300 series

    International Nuclear Information System (INIS)

    Silva, Maycon J.; Spinelli, Rafaela O.; Moreno, Rogerio M.B.; Mattoso, Luiz H.C.; Martins, Maria Alice; Scaloppi Junior, Erivaldo J.

    2015-01-01

    The natural rubber (NR) is present in more than 2500 species of plants, being the Hevea brasiliensis the most commercially exploited. It is a raw material of great importance to the Brazilian economy, but the country faces a production's deficit, having to import about 60% of its consumption. In this work , the latex obtained from rubber tree of new clones of PB series 300 (PB 311, PB 312, PB 314 , PB 326, PB 346 and PB 350 ) and RRIM 600 (control) were characterized by dry rubber content (DRC), total solids content, distribution of particle size, Zeta potential, thermogravimetry, differential scanning calorimetry, infrared in the spectroscopy (FTIR), nuclear magnetic resonance (NMR) and technological properties. The DRC values ranged from 33% to 40%, and total solids of 38% to 44%. All of the clones showed average particle diameter between 180.0 to 192.1 nm, excluding clones PB 326 and PB 346 with 150.0 nm and 157.9 nm, respectively. The NMR spectra and FTIR showed that the structure of the natural rubber from all clones studied is cis -1,4- polyisoprene. Natural rubber from the new clones showed good thermal stability up to 285 °C and glass transition temperature of -64 °C. (author)

  10. SUPPLY-CHAIN OF NATURAL RUBBER IN INDONESIA

    Directory of Open Access Journals (Sweden)

    Bustanul Arifin

    2011-08-01

    Full Text Available Normal 0 false false false MicrosoftInternetExplorer4 st1\\:*{behavior:url(#ieooui } /* Style Definitions */ table.MsoNormalTable {mso-style-name:"Table Normal"; mso-tstyle-rowband-size:0; mso-tstyle-colband-size:0; mso-style-noshow:yes; mso-style-parent:""; mso-padding-alt:0cm 5.4pt 0cm 5.4pt; mso-para-margin:0cm; mso-para-margin-bottom:.0001pt; mso-pagination:widow-orphan; font-size:10.0pt; font-family:"Times New Roman"; mso-ansi-language:#0400; mso-fareast-language:#0400; mso-bidi-language:#0400;} The study examines the supply chain of natural rubber production in Indonesia and assessing the transmission of prices to rubber growers and provides recommendations for a suitable scheme that would help to ensure high production standards and a sustainable return for natural rubber production.  The frameworks to examine the performance of supply chain of rubber marketing rely mostly on the efficiency level of marketing system of natural rubbers, including the value chain principles in marketing margin, and revealed price transmission from consumers to growers. The results show that the roles of subdistrict middlemen are extremely crucial in moving up the slabs from the village level to urban areas, where trader-brokers are expecting the slabs to be forwarded directly to crumb-rubber factories.  Changes in world price, hence the profits being accumulated by traders and rubber factories, are not transmitted properly to rubber farmers and/or sharetappers. Information asymmetry, the access over price information, and immediate response of rubber growers to the change in world price could explain this non-cointegration in price data between growers and exporters.  In the near future, the policy reforms in supply chain of natural rubber marketing in Indonesia should carefully address these issues in a more comprehensive manner.  Finally, in order to contribute to the positive environmental and social benefits, the major challenge for natural rubber

  11. 75 FR 38119 - Polychloroprene Rubber From Japan

    Science.gov (United States)

    2010-07-01

    ... Rubber From Japan AGENCY: United States International Trade Commission. ACTION: Institution of a five-year review concerning the antidumping duty finding on polychloroprene rubber from Japan. SUMMARY: The... on polychloroprene rubber from Japan would be likely to lead to continuation or recurrence of...

  12. Zinc Leaching from Tire Crumb Rubber

    Science.gov (United States)

    Rhodes, E. P.; Ren, J.; Mays, D. C.

    2010-12-01

    Recent estimates indicate that more than 2 billion scrap tires are currently stockpiled in the United States and approximately 280 million more tires are added annually. Various engineering applications utilize recycled tires in the form of shredded tire crumb rubber. However, the use of tire crumb rubber may have negative environmental impacts, especially when the rubber comes into contact with water. A review of the literature indicates that leaching of zinc from tire crumb rubber is the most significant water quality concern associated with using this material. Zinc is generally used in tire manufacturing, representing approximately 1.3% of the final product by mass. This study will report results from the U.S. Environmental Protection Agency’s (EPA’s) Synthetic Precipitation Leaching Procedure, batch leaching tests, and column leaching tests performed to quantify the process by which zinc leaches from tire crumb rubber into water. Results are interpreted with a first-order kinetic attachment/detachment model, implemented with the U.S. Agricultural Research Service software HYDRUS-1D, in order to determine the circumstances when zinc leaching from tire crumb rubber would be expected to comply with the applicable discharge limits. One potential application for recycled tires is replacing sand with tire crumb rubber in granular media filters used for stormwater pollution control. For this to be a viable application, the total zinc in the stormwater discharge must be below the EPA’s benchmark value of 0.117 mg/L.

  13. A model for calculating EM field in layered medium with application to biological implants

    International Nuclear Information System (INIS)

    Salehi-Reyhani, S.M.

    2001-01-01

    Modern wireless telecommunication devices (GSM Mobile system) (cellular telephones and wireless modems on laptop computers) have the potential to interfere with implantable medical devices/prostheses and cause possible malfunction. An implant of resonant dimensions within a homogeneous dielectric lossy sphere can enhance local values of SAR (the specific absorption rate). Also antenna radiation pattern and other characteristics are significantly altered by the presence of the composite dielectric entities such as the human body. Besides, the current safety limits do not take into account the possible effect of hot spots arising from metallic implants resonant at mobile phone frequencies. Although considerable attention has been given to study and measurement of scattering from a dielectric sphere, no rigorous treatment using electromagnetic theory has been given to the implanted dielectric spherical head/cylindrical body. This thesis aims to deal with the scattering of a plane electromagnetic wave from a perfectly conducting or dielectric spherical/cylindrical implant of electrically small radius (of resonant length), embedded eccentrically into a dielectric spherical head model. The method of dyadic Green's function (DGF) for spherical vector wave functions is used. Analytical expressions for the scattered fields of both cylindrical and spherical implants as well as layered spherical head and cylindrical torso models are obtained separately in different chapters. The whole structure is assumed to be uniform along the propagation direction. To further check the accuracy of the proposed solution, the numerical results from the analytical expressions computed for the problem of implanted head/body are compared with the numerical results from the Finite-Difference Time-Domain (FDTD) method using the EMU-FDTD Electromagnetic simulator. Good agreement is observed between the numerical results based on the proposed method and the FDTD numerical technique. This research

  14. Bacterial colonization of polymer brush-coated and pristine silicone rubber implanted in infected pockets in mice

    NARCIS (Netherlands)

    Nejadnik, M.R.; Engelsman, A.F.; Fernandez, I.C.S.; Busscher, H.J.; Norde, W.; Mei, van der H.C.

    2008-01-01

    Curing biomaterial-associated infection (BAI) frequently includes antibiotic treatment, implant removal and re-implantation. However, revision implants are at a greater risk of infection as they may attract bacteria from their infected surroundings. Polymer brush-coatings attract low numbers of

  15. 27 CFR 21.125 - Rubber hydrocarbon solvent.

    Science.gov (United States)

    2010-04-01

    ... 27 Alcohol, Tobacco Products and Firearms 1 2010-04-01 2010-04-01 false Rubber hydrocarbon solvent. 21.125 Section 21.125 Alcohol, Tobacco Products and Firearms ALCOHOL AND TOBACCO TAX AND TRADE BUREAU....125 Rubber hydrocarbon solvent. (a) Rubber hydrocarbon solvent is a petroleum derivative. (b...

  16. Porous Titanium for Dental Implant Applications

    Directory of Open Access Journals (Sweden)

    Zena J. Wally

    2015-10-01

    Full Text Available Recently, an increasing amount of research has focused on the biological and mechanical behavior of highly porous structures of metallic biomaterials, as implant materials for dental implants. Particularly, pure titanium and its alloys are typically used due to their outstanding mechanical and biological properties. However, these materials have high stiffness (Young’s modulus in comparison to that of the host bone, which necessitates careful implant design to ensure appropriate distribution of stresses to the adjoining bone, to avoid stress-shielding or overloading, both of which lead to bone resorption. Additionally, many coating and roughening techniques are used to improve cell and bone-bonding to the implant surface. To date, several studies have revealed that porous geometry may be a promising alternative to bulk structures for dental implant applications. This review aims to summarize the evidence in the literature for the importance of porosity in the integration of dental implants with bone tissue and the different fabrication methods currently being investigated. In particular, additive manufacturing shows promise as a technique to control pore size and shape for optimum biological properties.

  17. Application of gamma irradiation for incorporation of rubber powder in the formulations EPDM and NBR rubber

    International Nuclear Information System (INIS)

    Kiyan, Ludmila de Ysasa Pozzo

    2014-01-01

    The natural decomposition of rubber is a very slow process due to its three-dimensional network formed by vulcanized crosslinked structures becoming extremely difficult to reprocess this material. The present work aims to study the application of gamma irradiation as devulcanization process for material reuse/recycling. The interactions of elastomers with ionizing radiation of a gamma source were investigated and the changes in physicochemical properties of the materials were evaluated. Formulations of NBR (acrylonitrile - butadiene) and EPDM (ethylene - propylene - diene terpolymer) from the rubber industry were crosslinked by conventional sulfur-based mixing. Master - batch was processed with rubber powder (industrial waste) and virgin rubber. The raw material (master batch) was irradiated in 60 Co source at doses of 50, 100, 150 kGy and dose rate of 5 kGy h -1 at room temperature. The irradiated material was incorporated in classical sulfur-based formulations. The formulations were characterized by: infrared spectroscopy (FTIR), thermal analysis (TG and DTG), tensile strength, elongation at break, hardness, abrasion resistance, rheometry and swelling. The results showed a predominance of chain scission at a dose of 50 kGy for EPDM rubber. For nitrile predominance of chain scission was observed at a dose of 100 kGy. These results show the possibility of the use of gamma radiation for the reuse/recycling of EPDM and nitrile rubbers. (author)

  18. Comparison of biological characteristics of mesenchymal stem cells grown on two different titanium implant surfaces

    International Nuclear Information System (INIS)

    Wang Chengyue; Zhao Baohong; Ai Hongjun; Wang Yiwei

    2008-01-01

    This study examined the biological characteristics of mesenchymal stem cells (MSCs) grown on sand-blasted, large-grit, acid-etched (SLA) surface and hydroxyapatite (HA) coating on the SLA (HA/SLA) surface of titanium dental implants. The HA/SLA surfaces of titanium dental implants were formed by the ion beam assisted deposition (IBAD) method. Rabbit bone marrow derived mesenchymal stem cells cultured in vitro were seeded onto the surface of SLA and HA/SLA; the growth states of MSCs on the two samples were observed by a scanning electron microscope; the proliferation index, alkaline phosphatase (ALP) activity, osteocalcin (OCN) content of MSCs and mRNA relative expression level of osteopontin (opn) were compared between two groups. MSCs were found to be easier to adhere to the HA/SLA surface compared to the SLA surface. At the same time, the ALP activity and the OCN content of MSCs grown on the HA/SLA surface were obviously higher, and the relative expression level of opn mRNA was 4.78 times higher than that on the SLA surface. The HA coating formed by the IBAD method on the SLA surface of titanium dental implants significantly improves proliferation and well-differentiated osteoblastic phenotype of MSCs, which indicates a promising method for the surface modification of titanium dental implants

  19. Recycling of rubber tires in electric arc furnace steelmaking: simultaneous combustion of metallurgical coke and rubber tyres blends

    Energy Technology Data Exchange (ETDEWEB)

    Magdalena Zaharia; Veena Sahajwalla; Byong-Chul Kim; Rita Khanna; N. Saha-Chaudhury; Paul O' Kane; Jonathan Dicker; Catherine Skidmore; David Knights [University of New South Wales, Sydney, NSW (Australia). School of Materials Science and Engineering

    2009-05-15

    The present study investigates the effect of addition of waste rubber tires on the combustion behavior of its blends with coke for carbon injection in electric arc furnace steelmaking. Waste rubber tires were mixed in different proportions with metallurgical coke (MC) (10:90, 20:80, 30:70) for combustion and pyrolysis at 1473 K in a drop tube furnace (DTF) and thermogravimetric analyzer (TGA), respectively. Under experimental conditions most of the rubber blends indicated higher combustion efficiencies compared to those of the constituent coke. In the early stage of combustion the weight loss rate of the blends is much faster compared to that of the raw coke due to the higher volatile yield of rubber. The presence of rubber in the blends may have had an impact upon the structure during the release and combustion of their high volatile matter (VM) and hence increased char burnout. Measurements of micropore surface area and bulk density of the chars collected after combustion support the higher combustion efficiency of the blends in comparison to coke alone. The surface morphology of the 30% rubber blend revealed pores in the residual char that might be attributed to volatile evolution during high temperature reaction in oxygen atmosphere. Physical properties and VM appear to have a major effect upon the measured combustion efficiency of rubber blends. The study demonstrates that waste rubber tires can be successfully co-injected with metallurgical coke in electric arc furnace steelmaking process to provide additional energy from combustion. 44 refs., 11 figs., 2 tabs.

  20. Natural rubber/nitrile butadiene rubber/hindered phenol composites with high-damping properties

    Directory of Open Access Journals (Sweden)

    Xiuying Zhao

    2015-10-01

    Full Text Available New natural rubber (NR/nitrile butadiene rubber (NBR/hindered phenol (AO-80 composites with high-damping properties were prepared in this study. The morphological, structural, and mechanical properties were characterized by atomic force microscopy (AFM, polarized Fourier transform infrared spectrometer (FTIR, dynamic mechanical thermal analyzer (DMTA, and a tensile tester. Each composite consisted of two phases: the NR phase and the NBR/AO-80 phase. There was partial compatibility between the NR phase and the NBR/AO-80 phase, and the NR/NBR/AO-80 (50/50/20 composite exhibited a co-continuous morphology. Strain-induced crystallization occurred in the NR phase at strains higher than 200%, and strain-induced orientation appeared in the NBR/AO-80 phase with the increase of strain from 100% to 500%. The composites had a special stress–strain behavior and mechanical properties because of the simultaneous strain-induced orientation and strain-induced crystallization. In the working temperature range of a seismic isolation bearing, the composites (especially the NR/NBR/AO-80 (50/50/20 composite presented a high loss factor, high area of loss peak (TA, and high hysteresis energy. Therefore, the NR/NBR/AO-80 rubber composites are expected to have important application as a high-performance damping material for rubber bearing.

  1. Lignocellulosic fiber reinforced rubber composites

    CSIR Research Space (South Africa)

    Jacob John, Maya

    2009-04-01

    Full Text Available Natural Rubber (NR) is a naturally occurring elastomeric polymer of isoprene (2-methyl-1,3-butadiene). It can be extracted from latex of only one kind of tree, the Hevea braziliensis. Hevea rubber is produced in many tropical regions of Southeast...

  2. A study on creep properties of laminated rubber bearings. Pt. 1. Creep properties and numerical simulations of thick rubber bearings

    International Nuclear Information System (INIS)

    Matsuda, Akihiro; Yabana, Shuichi

    2000-01-01

    In this report, to evaluate creep properties and effects of creep deformation on mechanical properties of thick rubber bearings for three-dimensional isolation system, we show results of compression creep test for rubber bearings of various rubber materials and shapes and development of numerical simulation method. Creep properties of thick rubber bearings were obtained from compression creep tests. The creep strain shows steady creep that have logarithmic relationships between strain and time and accelerated creep that have linear relationships. We make numerical model of a rubber material with nonlinear viscoelastic constitutional equations. Mechanical properties after creep loading test are simulated with enough accuracy. (author)

  3. Treatment of wastewater from rubber industry in Malaysia ...

    African Journals Online (AJOL)

    Treatment of wastewater from rubber industry in Malaysia. ... Discharge of untreated rubber effluent to waterways resulted in water pollution that affected the human health. ... Key words: Rubber industry, effluent, waste management, Malaysia.

  4. Presence of Polycyclic Aromatic Hydrocarbons in Rubber Packaging Materials and in Parenteral Formulations Stored in Bottles With Rubber Stoppers.

    Science.gov (United States)

    Bohrer, Denise; Viana, Carine; Barichello, Marcia M; de Moura, Juliane F; de Carvalho, Leandro M; Nascimento, Paulo C

    2017-08-01

    Rubber closures are the primary packaging material for sterile preparations intended for repeated use. Important features of rubber closures are achieved after additives are added to the elastomeric material that compounds the rubber. Among these additives is carbon black. Because of its origin, carbon black may contain polycyclic aromatic hydrocarbons (PAHs). The U.S. Environmental Protection Agency has identified 16 priority PAHs on the basis of concerns that they cause or might cause cancer in animals and humans. Regulatory agencies impose carbon black purity specifications based on limits for total PAHs (0.5 mg/kg) and benzo[a]pyrene (5 μg/kg) or benzo[a]pyrene only (250 μg/kg). PAHs in rubber packaging used for pharmaceutical formulations and in parenteral products stored in containers with rubber stoppers were investigated. To this end, the method proposed by the National Institute for Occupational Safety and Health-based on high-performance liquid chromatography with ultraviolet and fluorescence detection-was adapted to determine the levels of PAHs in rubber stoppers (gray and red) and in lipid emulsions and amino acid solutions stored in bottles with rubber stoppers. The rubber materials were shown to contain 12 PAHs, in concentrations ranging from 0.25-3.31 µg/g. Only 1 of 18 samples (11 amino acid solutions and 7 lipid emulsions) was uncontaminated. The most prevalent contaminants were pyrene, benzo[a]pyrene, and fluoranthene. The total PAH concentrations in the samples ranged from 0.11-5.96 µg/mL. Components of parenteral nutrition may be contaminated with PAHs, and rubber stoppers represent a potential source of these contaminants.

  5. Rubber friction: role of the flash temperature

    International Nuclear Information System (INIS)

    Persson, B N J

    2006-01-01

    When a rubber block is sliding on a hard rough substrate, the substrate asperities will exert time-dependent deformations of the rubber surface resulting in viscoelastic energy dissipation in the rubber, which gives a contribution to the sliding friction. Most surfaces of solids have roughness on many different length scales, and when calculating the friction force it is necessary to include the viscoelastic deformations on all length scales. The energy dissipation will result in local heating of the rubber. Since the viscoelastic properties of rubber-like materials are extremely strongly temperature dependent, it is necessary to include the local temperature increase in the analysis. At very low sliding velocity the temperature increase is negligible because of heat diffusion, but already for velocities of order 10 -2 m s -1 the local heating may be very important. Here I study the influence of the local heating on the rubber friction, and I show that in a typical case the temperature increase results in a decrease in rubber friction with increasing sliding velocity for v>0.01 m s -1 . This may result in stick-slip instabilities, and is of crucial importance in many practical applications, e.g. for tyre-road friction and in particular for ABS braking systems

  6. Design, Construction, and Evaluation of Rubber Friction Tester

    Directory of Open Access Journals (Sweden)

    Mehdi Razzaghi Kashani

    2012-12-01

    Full Text Available Coeffcient of  friction  (COF  for  rubber parts  is one of  the key parameters in their interaction with solid rough surfaces (micrometer to millimeter scales,  such  as  tire-road  interactions. COF  of  rubber  depends  on  viscoelastic properties of rubber, roughness characteristics of the counter-part surface, and process variables such as contact nominal pressure and sliding speed. Due to the need for measuring COF  for  rubber,  a  new  friction  tester, with  continuous  variation  of nominal pressure and sliding speed, was designed and constructed in order to assess the effect of above mentioned parameters. Tire tread compounds, as the most common rubber part  in  the feld of  rubber  tribology, was used  for  this purpose. Viscoelastic properties of compounds were varied by changing composition of styrene-butadiene rubber (SBR and butadiene rubber (BR in the blend. Effect of surface roughness was evaluated by using silicon-carbide papers with different roughness parameters. By statistical analysis it was shown that the designed friction tester has high accuracy in measuring the coeffcient of friction of rubber and differentiating the effective parameters. Increasing the nominal pressure led to reduction of COF and increase in sliding speed forced it through a maximum. In conclusion, the loss factor of the compound and asymmetry in roughness distribution of the counter-surface are considered as the most effective parameters on COF of rubber.

  7. Cryogenic Deflashing for Rubber Products

    Directory of Open Access Journals (Sweden)

    Abhilash M.

    2018-01-01

    Full Text Available Deflashing is the process of removal of excess flashes from the rubber products. Initially deflashing was a manual operation where dozen of workers, seated at small work stations would take each part and trim the excess rubber off with scissors, knives or by grinding. Still the same method is employed in most of the rubber industry. The drawbacks of this method are demand inconsistent and repeatable quality. Work done by hand is often inconsistent. There are commercially available cryogenic deflashing machine but they are too expensive hence cost effectiveness is also a prime factor. The objective of this paper is to develop a technique, to identify the media through which the flashes can be removed easily and effectively. Based on the test results obtained from testing of five different types of media, ABCUT Steel media gave best results. The testing of the ABCUT Steel media on rubber samples like O-rings, grommet tail door, bottom bush etc. shows good results.

  8. Characterization of crumb rubber modified by gamma radiation

    Energy Technology Data Exchange (ETDEWEB)

    Faldini, Sonia B.; Terence, Mauro C.; Miranda, Leila F.; Munhoz, Antonio H.; Domingues, Leandro S.; Coghetto, Gregory, E-mail: sfaldini@yahoo.com.br, E-mail: mauroterence@yahoo.com.br [Universidade Presbiteriana Mackenzie (UPM), Sao Paulo, SP (Brazil). Escola de Engenharia. Engenharia de Materiais

    2013-07-01

    The use of crumb rubber from scrap tires has become a common practice in the construction of roads, leading to improved properties of the asphalt and decreasing the environmental pollution. In this study, crumb rubber was modified by gamma radiation to eventually incorporate it into the asphalt and verify potential improvements of their properties. The crumb rubber modified by gamma radiation in the dose 500 kGy and 1000kGy was characterized by thermal analysis, infrared spectroscopy and scanning electron microscopy. The dose of radiation used has no effect on degradation temperatures. It is observed that the IV spectra of untreated rubbers and rubbers irradiated have substantially the same profile. The results indicate that despite small morphological changes in the irradiated rubber, they do not influence its degradation temperature and composition. (author)

  9. Characterization of crumb rubber modified by gamma radiation

    International Nuclear Information System (INIS)

    Faldini, Sonia B.; Terence, Mauro C.; Miranda, Leila F.; Munhoz, Antonio H.; Domingues, Leandro S.; Coghetto, Gregory

    2013-01-01

    The use of crumb rubber from scrap tires has become a common practice in the construction of roads, leading to improved properties of the asphalt and decreasing the environmental pollution. In this study, crumb rubber was modified by gamma radiation to eventually incorporate it into the asphalt and verify potential improvements of their properties. The crumb rubber modified by gamma radiation in the dose 500 kGy and 1000kGy was characterized by thermal analysis, infrared spectroscopy and scanning electron microscopy. The dose of radiation used has no effect on degradation temperatures. It is observed that the IV spectra of untreated rubbers and rubbers irradiated have substantially the same profile. The results indicate that despite small morphological changes in the irradiated rubber, they do not influence its degradation temperature and composition. (author)

  10. Silane grafted natural rubber and its compatibilization effect on silica-reinforced rubber tire compounds

    NARCIS (Netherlands)

    Sengloyluan, K.; Sahakaro, K.; Dierkes, W. K.; Noordermeer, J. W.M.

    2017-01-01

    Natural Rubber (NR) grafted with 3-octanoylthio-1-propyltriethoxysilane (NXT) was prepared by melt mixing using 1,1′-di(tert-butylperoxy)-3,3,5-trimethylcyclohexane as initiator at 140 °C with NXT contents of 10 and 20 parts per hundred rubber [phr] and initiator 0.1 phr. The silane grafted on NR

  11. Effect of rubber flooring on dairy cattle stepping behavior and muscle activity.

    Science.gov (United States)

    Rajapaksha, Eranda; Winkler, Christoph; Tucker, Cassandra B

    2015-04-01

    effects of standing. However, additional work, including measurements of blood flow in the leg, is needed to fully understand the biological implications of these changes. Overall, the rubber flooring tested had little effect on standing behavior. Copyright © 2015 American Dairy Science Association. Published by Elsevier Inc. All rights reserved.

  12. Alternative sources of natural rubber

    NARCIS (Netherlands)

    Mooibroek, H.; Cornish, K.

    2000-01-01

    Rubber (cis-1,4-polyisoprene) is one of the most important polymers naturally produced by plants because it is a strategic raw material used in more than 40,000 products, including more than 400 medical devices. The sole commercial source, at present, is natural rubber harvested from the Brazilian

  13. Butyl Rubber: Compound Development and Characterization

    National Research Council Canada - National Science Library

    Sloan, James

    2000-01-01

    ...), to develop the standard butyl rubber compound. The strategy of this work was to compound- and compression-mold high-quality, uniform butyl rubber experimental sheets and to evaluate their cure properties, mechanical properties...

  14. Geotechnical Properties of Rubber Tires and Sediments Mixtures

    Directory of Open Access Journals (Sweden)

    H. Sellaf

    2014-04-01

    Full Text Available An experimental work was undertaken to study the effect of rubber tires on the geotechnical properties of a dredged sediment, using a mixing ratio of large size. For comparison, two types of soil were studied (dredged sediment from Fergoug dam and Tizi Tuff from the north west of Algeria. Taking into account the high compressibility and the low water absorption of the rubber tires, grain size analysis, density, Atterberg limits analysis, chemical composition, direct shear tests, loading-unloading tests, modified Proctor and CBR tests are performed on the two soils and their mixtures with different scrap tire rubber (10, 20, 25 and 50%. The results show that liquid limits and plastic indexes decrease with the scrap tire rubber content and that the decrease is more significant for soil with high plasticity. Cohesion also decreases with scrap tire rubber content when the internal friction angle is vacillating. Compression and recompression indexes increase gradually with the scrap tire rubber content and the variation for compression index is more significant for the two soils. Compaction characteristics and CBR values decrease with scrap tire rubber content. The CBR values for W=3% are important compared to those with W=5% excepted for mixture with (75% tuff and 25% scrap tire rubber. The results show that the scrap tire rubber can be used as a reinforcement material for dredged soil, but with a content that should not highly affect the compressibility.

  15. Crack Velocities in Natural Rubber.

    Science.gov (United States)

    1982-05-01

    vulcanized natural rubber (3). The surprisingly low value for natural rubber was attributed to highly anisotropic elastic behavior at high strains...Dr. R.L. Rabie Hercules Incorporated WX-2, MS-952 Alleghany Ballistic Lab Los Alamos National Lab. P.O. Box 210 P.O. Box 1663 Washington, D.C. 21502

  16. Practical application of thermoreversibly Cross-linked rubber products

    Science.gov (United States)

    Polgar, L. M.; Picchioni, F.; de Ruiter, E.; van Duin, M.

    2017-07-01

    Currently, rubber products cannot simply be reprocessed after their product life, due to the irreversible cross-linking methods traditionally applied. The purpose of this work is to investigate how thermoreversible cross-linking of rubbers via Diels Alder chemistry can be used for the development of recyclable rubber products. Unfortunately, the applicability of the thermoreversible EPM-g-furan/BM system appears to be limited to room temperature applications, because of the rapid deterioration of the compression set at elevated temperatures compared to irreversibly cross-linked EPM. However, the use of EPM rubber modified with thiophene or cyclopentadiene moieties may extend the temperature application range and results in rubber products with acceptable properties. Finally, rubber products generally comprise fillers such as silica, carbon black or fibers. In this context, the reinforcing effect of short cut aramid fibers on the material properties of the newly developed thermoreversibly cross-linked EPM rubbers was also studied. The material properties of the resulting products were found to be comparable to those of a fiber reinforced, peroxide cured reference sample.

  17. Biodiesel production methods of rubber seed oil: a review

    Science.gov (United States)

    Ulfah, M.; Mulyazmi; Burmawi; Praputri, E.; Sundari, E.; Firdaus

    2018-03-01

    The utilization of rubber seed as raw material of biodiesel production is seen highly potential in Indonesia. The availability of rubber seeds in Indonesia is estimated about 5 million tons per annum, which can yield rubber seed oil about 2 million tons per year. Due to the demand of edible oils as a food source is tremendous and the edible oil feedstock costs are far expensive to be used as fuel, production of biodiesel from non-edible oils such as rubber seed is an effective way to overcome all the associated problems with edible oils. Various methods for producing biodiesel from rubber seed oil have been reported. This paper introduces an optimum condition of biodiesel production methods from rubber seed oil. This article was written to be a reference in the selection of methods and the further development of biodiesel production from rubber seed oil. Biodiesel production methods for rubber seed oils has been developed by means of homogeneous catalysts, heterogeneous catalysts, supercritical method, ultrasound, in-situ and enzymatic processes. Production of biodiesel from rubber seed oil using clinker loaded sodium methoxide as catalyst is very interesting to be studied and developed further.

  18. Synergistic effect of plasma-modified halloysite nanotubes and carbon black in natural rubber-butadiene rubber blend

    NARCIS (Netherlands)

    Poikelispaa, Minna; Das, Amit; Dierkes, Wilma K.; Vuorinen, Jyrki

    2013-01-01

    Halloysite nanotubes (HNTs) were investigated concerning their suitability for rubber reinforcement. As they have geometrical similarity with carbon nanotubes, they were expected to impart a significant reinforcement effect on the rubber compounds but the dispersion of the nanofillers is difficult.

  19. Butterfly valve of all rubber lining type

    International Nuclear Information System (INIS)

    Shimada, Shosaku; Nakatsuma, Sumiya; Sasaki, Iwao; Aoki, Naoshi.

    1982-01-01

    The valves used for the circulating water pipes for condensers in nuclear and thermal power stations have become large with the increase of power output, and their specifications have become strict. The materials for the valves change from cast iron to steel plate construction. To cope with sea water corrosion, rubber lining has been applied to the internal surfaces of valve boxes, and the build-up welding of stainless steel has been made on the edges of valves. However, recently it is desired to develop butterfly valves, of which the whole valve disks are lined with hard rubber. For the purpose of confirming the performance of large bore valves, a 2600 mm bore butterfly valve of all rubber lining type was used, and the opening and closing test of 1100 times was carried out by applying thermal cycle and pressure difference and using artifical sea water. Also the bending test of hard rubber lining was performed with test pieces. Thus, it was confirmed that the butterfly valves of all rubber lining type have the performance exceeding that of the valves with build-up welding. The course of development of the valves of all rubber lining type, the construction and the items of confirmation by tests of these valves, and the tests of the valve and the hard rubber lining described above are reported. (Kako, I.)

  20. RoxB Is a Novel Type of Rubber Oxygenase That Combines Properties of Rubber Oxygenase RoxA and Latex Clearing Protein (Lcp).

    Science.gov (United States)

    Birke, Jakob; Röther, Wolf; Jendrossek, Dieter

    2017-07-15

    Only two types of rubber oxygenases, rubber oxygenase (RoxA) and latex clearing protein (Lcp), have been described so far. RoxA proteins (RoxAs) are c -type cytochromes of ≈70 kDa produced by Gram-negative rubber-degrading bacteria, and they cleave polyisoprene into 12-oxo-4,8-dimethyltrideca-4,8-diene-1-al (ODTD), a C 15 oligo-isoprenoid, as the major end product. Lcps are common among Gram-positive rubber degraders and do not share amino acid sequence similarities with RoxAs. Furthermore, Lcps have much smaller molecular masses (≈40 kDa), are b -type cytochromes, and cleave polyisoprene to a mixture of C 20 , C 25 , C 30 , and higher oligo-isoprenoids as end products. In this article, we purified a new type of rubber oxygenase, RoxB Xsp (RoxB of Xanthomonas sp. strain 35Y). RoxB Xsp is distantly related to RoxAs and resembles RoxAs with respect to molecular mass (70.3 kDa for mature protein) and cofactor content (2 c -type hemes). However, RoxB Xsp differs from all currently known RoxAs in having a distinctive product spectrum of C 20 , C 25 , C 30 , and higher oligo-isoprenoids that has been observed only for Lcps so far. Purified RoxB Xsp revealed the highest specific activity of 4.5 U/mg (at 23°C) of all currently known rubber oxygenases and exerts a synergistic effect on the efficiency of polyisoprene cleavage by RoxA Xsp RoxB homologs were identified in several other Gram-negative rubber-degrading species, pointing to a prominent function of RoxB for the biodegradation of rubber in Gram-negative bacteria. IMPORTANCE The enzymatic cleavage of rubber (polyisoprene) is of high environmental importance given that enormous amounts of rubber waste materials are permanently released (e.g., by abrasion of tires). Research from the last decade has discovered rubber oxygenase A, RoxA, and latex clearing protein (Lcp) as being responsible for the primary enzymatic attack on the hydrophobic and water-insoluble biopolymer poly( cis -1,4-isoprene) in Gram

  1. Group D. Initiator paper. Implants--peri-implant (hard and soft tissue) interactions in health and disease: the impact of explosion of implant manufacturers.

    Science.gov (United States)

    Ivanovski, Saso

    2015-01-01

    1. The best-documented implants have a threaded solid screw-type design and are manufactured from commercially pure (grade IV) titanium. There is good evidence to support implants ≥ 6 mm in length, and ≥ 3 mm in diameter. 2. Integrity of the seal between the abutment and the implant is important for several reasons, including minimization of mechanical and biological complications and maintaining marginal bone levels. Although the ideal design features of the implant-abutment connection have not been determined, an internal connection, micro-grooves at the implant collar, and horizontal offset of the implant-abutment junction (platform switch) appear to impart favorable properties. 3. Implants with moderately rough implant surfaces provide advantages over machined surfaces in terms of the speed and extent of osseointegration. While the favorable performances of both minimally and moderately rough surfaces are supported by long-term data, moderately rough surfaces provide superior outcomes in compromised sites, such as the posterior maxilla. 4. Although plaque is critical in the progression of peri-implantitis, the disease has a multi-factorial aetiology, and may be influenced by poor integrity of the abutment/implant connection. Iatrogenic factors, such as the introduction of a foreign body. (e.g., cement) below the mucosal margin, can be important contributors. 5. Clinicians should exercise caution when using a particular implant system, ensuring that the implant design is appropriate and supported by scientific evidence. Central to this is access to and participation in quality education on the impact that implant characteristics can have on clinical outcomes. Caution should be exercised in utilizing non-genuine restorative componentry that may lead to a poor implant-abutment fit and subsequent technical and biological complications.

  2. Biological effects of ion implantation on processing tomato and eggplant seed

    International Nuclear Information System (INIS)

    Mao Peihong; Zeng Xianxian; Jin Xiang

    2004-01-01

    The seed of processing tomato '87-5' (Lycopersicon esculentum Mill) were implanted by the low energy nitrogen ion (N + ) with 6 different doses. The rate of emergence was little reduced in M1 generation, but the fruiting number per plant was increased and it's maturing earlier 20 days than the control. The precocity, disease resistance and stronger growth vigor were shown in M2 generation. Experimental results of two years showed that, according to synthetic analysis in factors such as precocity, disease resistance, high yield and quality, the N + dose of 6 x 10 16 cm -2 (60 times of pulse) for tomato seed '87-5' had been proved to have notable biological effects on M1 and M2 generation. The seed of eggplant 'Wuyeqie' (Solanum melongena L.) was also implanted by the low energy nitrogen ion (N + ) with 2 different doses. Multi-vertical channel fruits were obtained in variable M1 generation, which liked the pomelo without peel. The seed of these variable eggplants was taken and planted in the next year. The meaningful variable fruits, the characters of disease-resistance, purple-peel, small-navel, lantern-form, large-scale, etc. were obtained in beneficial M2 generation. The biggest single-fruit weight reached 1.53 kg, providing valuable germplasm resource for breeding. (authors)

  3. Greenhouse Gas Emissions from Rubber Industry in Thailand

    NARCIS (Netherlands)

    Jawjit, W.; Kroeze, C.; Rattanapan, S.

    2010-01-01

    Rubber production has been taking place in Thailand for many decades. Thailand is currently the world's largest natural rubber producer. We present emissions of greenhouse gases associated with the production of fresh latex, and three primary rubber products, including concentrated latex, block

  4. Development of rubber material for high radiation field

    International Nuclear Information System (INIS)

    Nakatsukasa, Sadayoshi; Tabasaki, Takeshi; Yoshida, Akihiro; Kadowaki, Yoshito

    2013-01-01

    Generally flexible polymeric materials exposed to radiation can't be used because they soften or harden remarkably in high radiation environment. Aromatic polymers such as PEEK, PI, and PES are also known as radiation-proof polymeric materials. Aromatic polymers are very hard, they can't be used for products like a packing where flexibility is required. We developed a new vulcanized rubber compound by the use of various additives and polymer blend. This developed rubber compound has a high radiation-proof performance by reaction balance of cross-linking and decomposition in this rubber. This rubber compound has a rubber elasticity even if exposed to radiation of MGy level, and its radiation proof is more than 5 times as high as conventional polymeric materials. This rubber compound is much more flexible than the aromatic polymers which are the used as conventional radiation-proof polymers. (author)

  5. Characterization of Hexsyn, a polyolefin rubber.

    Science.gov (United States)

    McMillin, C R

    1987-07-01

    Hexsyn is the Goodyear Tire and Rubber Company tradename for a polyolefin rubber synthesized from 1-hexene with 3-5% methylhexadiene as the source of residual double bonds for vulcanization. Under license from Goodyear, this same polymer has been manufactured by Lord Corporation for the hinge portion of finger joint prostheses using the tradename Bion. This rubber is currently licensed to the University of Akron and to the Cleveland Clinic Foundation for use in biomedical applications, and is being used primarily for biocompatible and highly fatigue resistant rubber components in ventricular assist and artificial heart systems. Results are presented from the physical, mechanical, and biological characterization of Hexsyn. Procedures are described for the synthesis, compounding, and post-molding extraction for Hexsyn. The physical testing of Hexsyn reported includes determinations of its density at 23 and 37 degrees C, initial hardness and hardness after aging in oxygen, blood, pseudoextracellular fluid and polyethylene glycol 600, typical molecular weights determined by gel permeation chromatography/low angle laser light scattering and intrinsic viscosity, thermal analyses by differential scanning calorimetry of Hexsyn gum, and vulcanized Hexsyn after exposure to blood and blood/fatigue conditions. Also reported are results of differential thermal analyses, thermomechanical analyses of virgin and annealed samples, and thermogravimetric analyses conducted in helium and in air. Dynamic mechanical analyses of Hexsyn include Clash-Berg and Rheovibron tests. Swelling was conducted to determine lot-to-lot and sheet-to-sheet variation for quality control and also a number of solvents were used so that the polymer-solvent interaction parameters could be determined. The permeability of Hexsyn to water, water vapor, and a variety of gases is reported. The permeability by contact angle measurements, refractive index, residual solvent analyses, migration of blood components

  6. Biological effects of low energy nitrogen ion implantation on Jatropha curcas L. seed germination

    Science.gov (United States)

    Xu, Gang; Wang, Xiao-teng; Gan, Cai-ling; Fang, Yan-qiong; Zhang, Meng

    2012-09-01

    To explore the biological effects of nitrogen ion beam implantation on dry Jatropha curcas seed, a beam of N+ with energy of 25 keV was applied to treat the dry seed at six different doses. N+ beam implantation greatly decreased germination rate and seedling survival rate. The doses within the range of 12 × 1016 to 15 × 1016 ions cm-2 severely damaged the seeds: total antioxidant capacity (TAC), germination rate, seedling survival rate, reduced ascorbate acid (HAsA) and reduced glutathione (GSH) contents, and most of the tested antioxidases activity (i.e. catalase (CAT), ascorbate peroxidase (APX) and superoxide dismutase (SOD)) reached their lowest levels. At a dose of 18 × 1016 ion cm-2, biological repair took place: moderate increases were found in TAC, germination rate, seedling survival rate, HAsA and GSH contents, and some antioxidant enzyme activities (i.e. CAT, APX, SOD and GPX). The dose of 18 × 1016 ions cm-2 may be the optimum dose for use in dry J. curcas seed mutation breeding. CAT, HAsA and GSH contributed to the increase of TAC, but CAT was the most important. POD performed its important role as seed was severely damaged. The main role of the HAsA-GSH cycle appeared to be for regeneration of HAsA.

  7. Thermal endurance tests on silicone rubber specimens

    International Nuclear Information System (INIS)

    Warburton, C.

    1977-07-01

    Thermal endurance tests have been performed on a range of silicone rubber specimens at temperature above 300 0 C. It is suggested that the rubber mix A2426, the compound from which Wylfa sealing rings are manufactured, will fail at temperatures above 300 0 C within weeks. Hardness measurements show that this particular rubber performs in a similar manner to Walker's S.I.L./60. (author)

  8. Crumb Rubber Recycling in Enhancing Damping Properties of Concrete

    Science.gov (United States)

    Sugapriya, P.; Ramkrishnan, R.

    2018-02-01

    Damping plays a major role in the design of roadside structures that gets affected due to vibrations transmitted from moving traffic. In this study, fine aggregates were partially replaced with crumb rubber in concrete, at varying percentages of 5, 10, 15 and 20% by weight. Three different sets of concrete, mixed with crumb rubber were prepared using raw rubber, treated rubber and treated rubber with partial replacement of cement. Cement was partially replaced with Ultra-Fine Ground Granulated Blast furnace Slag (UFGGBS) for this study. Samples were cast, cured and tested for various properties on the 7th and 28th day. The damping ratio and frequency of the peak value from a number of waves in rubber incorporated beams were found out using a FFT Analyser along with its Strength, Damping and Sorptivity characteristics. SEM analysis was conducted to analyse the micro structural bonding between rubber and concrete. The mode shapes of pavement slabs were modelled and analysed using a FEM tool, ANSYS. From the results, the behaviour of the three sets of rubberized concrete were compared and analysed, and an optimum percentage for crumb rubber and UFGGBS was proposed to achieve best possible damping without compromising the strength properties.

  9. Cream concentrated latex for foam rubber products

    Science.gov (United States)

    Suksup, R.; Imkaew, C.; Smitthipong, W.

    2017-12-01

    Fresh natural latex (around 40% rubber and 60% water) can be transformed to concentrated natural latex (around 60% rubber and 40% water) in order to realise economical transportation and easier latex product’s preparation. The concentrated natural latex is an extremely valuable material. It can be applied for many types of products, for example, foam rubber as pillow and mattress, elastic band, etc. Industrially, the concentrated natural latex can be prepared by centrifugation which requires an enormous expensive machine. From the eco-friendly products point of view, most of rubber entrepreneurs in the world try to develop a green rubber product. So, the main objective of this study is to prepare the cream concentrated latex without any sophisticated machine. Thus, we work on a simple, cheap and green method that does not use any expensive machine but uses water-based chemical as sodium alginate to prepare the cream concentrated latex. The optimal amount of sodium alginate in the latex was studied. The main characteristics of the cream concentrated latex were tested by various technics, such as alkalinity, total solid content (TSC), dry rubber content (DRC), etc. We found that there are no significant differences of results between fresh natural latex and cream concentrated latex, except for the TSC and DRC. The TSC and DRC of cream latex are higher than those of fresh natural latex. Finally, we propose a model of natural rubber particle and sodium alginate to form the cream concentrated latex.

  10. Compatibilization efficiency of carboxylated nitrile rubber and epoxy pre-polymer in nitrile/acrylic rubber blends

    Directory of Open Access Journals (Sweden)

    Micheli L. Celestin

    2013-01-01

    Full Text Available An investigation has been made of the effects from a compatibilizer, viz. carboxylated nitrile rubber (XNBR, on several properties of nitrile rubber (NBR and acrylic rubber (ACM blends, including curing characteristics, mechanical, dynamic mechanical and dielectric properties. The presence of XNBR until 10 phr resulted in an improvement of the ultimate tensile properties, especially elongation at break. The mechanical properties associated to the volume fraction of rubber in the network (Vr and torque values suggest the co-vulcanization phenomenon imparted by the compatibilization. The oil resistance of NBR/ACM (50:50 wt. (% blends (compatibilized and non compatibilized was similar to that observed for pure ACM and significantly higher than NBR. The addition of small amounts of epoxy pre-polymer in combination with XNBR resulted in an additional improvement of the tensile properties. The dynamic mechanical and dielectric properties of the blends were also investigated. The loss modulus values of the compatibilized blends were significantly lower indicating an increase of the elastic characteristics. All blends presented two dielectric relaxation peaks confirming the heterogeneity of the compatibilized blends

  11. Proceedings of the Rubber Association of Canada's 7. biennial 2006 rubber recycling symposium : changing concepts

    International Nuclear Information System (INIS)

    2006-01-01

    Rising energy costs and concerns over the environment have contributed to a renewed focus on recycling for many governments and industries. This conference examined recent trends affecting rubber recycling activities as well as the legislative environment and its impacts on future recycling activities. Major rubber recycling markets were reviewed, and emerging product ideas were evaluated. Industry stewardship model and governance models were discussed. The impacts of new advances in tire technology and manufacturing on the rubber recycling industry were also investigated. Issues concerning fixed tipping fees and incentive structures were discussed, and effective management strategies for the recycling of large off-the-road tires were evaluated. Tire-derived fuel (TDF) is the largest market in North America for scrap tires, and TDF may continue to grow as a result of rising fossil fuel costs. Issues and challenges related to the introduction of TDF to new communities were discussed. New developments in tire derived aggregates (TDA) and ground rubber were also reviewed. Twenty-eight presentations were given at this conference, 3 of which were catalogued separately for inclusion in this database. refs., tabs., figs

  12. Evapotranspiration of rubber ( Hevea brasiliensis ) cultivated at two plantation sites in Southeast Asia: RUBBER EVAPOTRANSPIRATION IN SE ASIA

    Energy Technology Data Exchange (ETDEWEB)

    Giambelluca, Thomas W. [Department of Geography, University of Hawai' i at Mānoa, Honolulu Hawai' i USA; Hydrospheric Atmospheric Research Center, Nagoya University, Nagoya Japan; Mudd, Ryan G. [Department of Geography, University of Hawai' i at Mānoa, Honolulu Hawai' i USA; Liu, Wen [Department of Geography, University of Hawai' i at Mānoa, Honolulu Hawai' i USA; Ziegler, Alan D. [Department of Geography, National University of Singapore, Singapore Singapore; Kobayashi, Nakako [Hydrospheric Atmospheric Research Center, Nagoya University, Nagoya Japan; Kumagai, Tomo' omi [Hydrospheric Atmospheric Research Center, Nagoya University, Nagoya Japan; Miyazawa, Yoshiyuki [Department of Geography, University of Hawai' i at Mānoa, Honolulu Hawai' i USA; Research Institute of East Asia Environments, Kyushu University, Fukuoka Japan; Lim, Tiva Khan [Cambodian Rubber Research Institute, Phnom Penh Cambodia; Huang, Maoyi [Atmospheric Sciences and Global Change Division, Pacific Northwest National Laboratory, Richland Washington USA; Fox, Jefferson [East-West Center, Honolulu Hawai' i USA; Yin, Song [Cambodian Rubber Research Institute, Phnom Penh Cambodia; Mak, Sophea Veasna [Cambodian Rubber Research Institute, Phnom Penh Cambodia; Kasemsap, Poonpipope [Department of Horticulture, Kasetsart University, Bangkok Thailand

    2016-02-01

    The expansion of rubber (Hevea brasiliensis) cultivation to higher latitudes and higher elevations in southeast Asia is part of a dramatic shift in the direction of rural land cover change in the region toward more tree covered landscapes. To investigate the possible effects of increasing rubber cultivation in the region on ecosystem services including water cycling, eddy covariance towers were established to measure ecosystem fluxes within two rubber plantations, one each in Bueng Kan, northeastern Thailand, and Kampong Cham, central Cambodia. The results show that evapotranspiration (ET) at both sites is strongly related to variations in available energy and leaf area, and moderately controlled by soil moisture. Measured mean annual ET was 1128 and 1272 mm for the Thailand and Cambodia sites, respectively. After adjustment for energy closure, mean annual was estimated to be 1211 and 1459 mm yr at the Thailand and Cambodia sites, respectively. Based on these estimates and that of another site in Xishuangbanna, southwestern China, it appears that of rubber is higher than that of other tree dominated land covers in the region, including forest. While measurements by others in non rubber tropical ecosystems indicate that at high net radiation sites is at most only slightly higher than for sites with lower net radiation, mean annual rubber increases strongl with increasing net radiation across the three available rubber plantation observation sites. With the continued expansion of tree dominated land covers, including rubber cultivation, in southeast Asia, the possible association between commercially viable, fast growing tree crop species Giambelluca et al. Evapotranspiration of rubber (Havea brasiliensis) cultivated at two sites in southeast Asia and their relatively high water use raises concerns about potential effects on water and food security.

  13. Nylon-6/rubber blends: 6. Notched tensile impact testing of nylon-6(ethylene-propylene rubber) blends

    NARCIS (Netherlands)

    Dijkstra, Krijn; Dijkstra, K.; ter Laak, J.A.; ter Laak, J.; Gaymans, R.J.

    1994-01-01

    The deformation and fracture behaviour of nylon-6/EPR (ethylene-propylene rubber) blends is studied as a function of strain rate and rubber content. Therefore, tensile experiments are conducted on notched specimens over a broad range of draw speeds (including strain rates as encountered in normal

  14. Stimuli-responsive cement-reinforced rubber.

    Science.gov (United States)

    Musso, Simone; Robisson, Agathe; Maheshwar, Sudeep; Ulm, Franz-Josef

    2014-05-14

    In this work, we report the successful development of a cement-rubber reactive composite with reversible mechanical properties. Initially, the composite behaves like rubber containing inert filler, but when exposed to water, it increases in volume and reaches a stiffness that is intermediate between that of hydrogenated nitrile butadiene rubber (HNBR) and hydrated cement, while maintaining a relatively large ductility characteristic of rubber. After drying, the modulus increases even further up to 400 MPa. Wet/drying cycles prove that the elastic modulus can reversibly change between 150 and 400 MPa. Utilizing attenuated total reflection Fourier transform infrared spectroscopy), we demonstrate that the high pH produced by the hydration of cement triggers the hydrolysis of the rubber nitrile groups into carboxylate anions. Thus, the salt bridges, generated between the carboxylate anions of the elastomer and the cations of the filler, are responsible for the reversible variations in volume and elastic modulus of the composite as a consequence of environmental moisture exposure. These results reveal that cement nanoparticles can successfully be used to accomplish a twofold task: (a) achieve an original postpolymerization modification that allows one to work with carboxylate HNBR (HXNBR) not obtained by direct copolymerization of carboxylate monomers with butadiene, and (b) synthesize a stimuli-responsive polymeric composite. This new type of material, having an ideal behavior for sealing application, could be used as an alternative to cement for oil field zonal isolation applications.

  15. Microbial detoxification of waste rubber material by wood-rotting fungi.

    Science.gov (United States)

    Bredberg, Katarina; Andersson, B Erik; Landfors, Eva; Holst, Olle

    2002-07-01

    The extensive use of rubber products, mainly tires, and the difficulties to recycle those products, has resulted in world wide environmental problems. Microbial devulcanisation is a promising way to increase the recycling of rubber materials. One obstacle is that several microorganisms tested for devulcanisation are sensitive to rubber additives. A way to overcome this might be to detoxify the rubber material with fungi prior to the devulcanisation. In this study, 15 species of white-rot and brown-rot fungi have been screened with regard to their capacity to degrade an aromatic model compound in the presence of ground waste tire rubber. The most effective fungus, Resinicium bicolor, was used for detoxification of rubber material. Increase in growth of the desulfurising bacterium Thiobacillus ferrooxidans in presence of the rubber treated with Resinicium bicolor compared to untreated rubber demonstrated that detoxification with fungi is possible.

  16. Natural rubber producing plants: An overview

    African Journals Online (AJOL)

    User

    2013-03-20

    Mar 20, 2013 ... Currently, Hevea brasiliensis has been only one resource for commercial natural rubber production. ...... ADVANTAGES AND DISADVANTAGES ... polymer chain. Combinations of an amine antioxidant and a zinc dialkyldithiocarbamate have been used to counter these effects, improving guayule rubber ...

  17. [Role of different scale structures of titanium implant in the biological behaviors of human umbilical vein endothelial cells].

    Science.gov (United States)

    Liang, N W; Shi, L; Huang, Y; Deng, X L

    2017-02-18

    To study the role of different scale structure of Ti implants on the biological behaviors of human umbilical vein endothelial cell (HUVECs) and to reveal the role of material surface topographical features on peri-implant angiogenesis. Titanium (Ti) discs with different surface structures (Ti discs with smooth surface, Ti discs with nano scale structure, Ti discs with micro scale structure and Ti discs with micro/nano scale structure, named as SM-Ti, Nano-Ti, Micro-Ti and Micro/Nano-Ti, respectively) were prepared and their surface topographical features were confirmed via scanning electron microscopy (SEM) observation. HUVECs were cultured on these Ti discs. Biological outcomes of HUVECs on different surfaces were carried out, including cell adhesive capacity, proliferation, vascular endothelial growth factor (VEGF) production and intracellular expression of Ca(2+). The results of SEM images and immunofluorescence double staining of rhodamine-phalloidin and DAPI showed that compared with the SM-Ti and Nano-Ti group, the adhesive capacity and proliferation behavior of HUVECs on the surfaces of Micro-Ti and Micro/Nano-Ti was decreased. The results of culturing HUVECs on different groups of Ti discs after 24 hours showed that the cells number grew from (18±4) to (42±6)/ vision on SM-Ti, (28±6) to (52±10)/vision on Nano-Ti, (20±4) to (21±6)/vision on Micro-Ti and (16±4) to (18±6)/vision on Micro/Nano-Ti. Moreover, compared with the adhesion and proliferation of HUVECs on SM-Ti group and Nano-Ti, the adhesion and proliferation of HUVECs on Micro-Ti group and Micro/Nano-Ti group was significantly reduced (PMicro-Ti and Micro/Nano-Ti were (690±35) ng/L, (560±20) ng/L, (474±43) ng/L and (517±29) ng/L, respectively. Moreover, compared with the VEGF production of HUVECs on SM-Ti group, the VEGF production of HUVECs on Micro-Ti group and Micro/Nano-Ti group was significantly reduced (PMicro-Ti and Micro/Nano-Ti was significantly higher than that on the surface of

  18. Reshaping and Customization of SMILE-Derived Biological Lenticules for Intrastromal Implantation.

    Science.gov (United States)

    Damgaard, Iben Bach; Riau, Andri Kartasasmita; Liu, Yu-Chi; Tey, Min Li; Yam, Gary Hin-Fai; Mehta, Jodhbir Singh

    2018-05-01

    To evaluate the feasibility of excimer laser reshaping of biological lenticules available after small incision lenticule extraction (SMILE). Fresh and cryopreserved SMILE-derived human lenticules underwent excimer laser ablation for stromal reshaping. The treatment effects in the lasered group were compared with the nonlasered group with respect to changes in surface functional groups (by Fourier transform infrared spectroscopy [FTIR]) and surface morphology (by scanning electron microscopy [SEM] and atomic force microscopy [AFM]). Ten SMILE-derived porcine lenticules, five nonlasered (107-μm thick, -6 diopter [D] spherical power) and five excimer lasered (50% thickness reduction), were implanted into a 120-μm stromal pocket of 10 porcine eyes. Corneal thickness and topography were assessed before and after implantation. FTIR illustrated prominent changes in the lipid profile. The collagen structure was also affected by the laser treatment but to a lesser extent. SEM exhibited a more regular surface for the lasered lenticules, confirmed by the lower mean Rz value (290.1 ± 96.1 nm vs. 380.9 ± 92.6 nm, P = 0.045) on AFM. The lasered porcine lenticules were thinner than the nonlasered controls during overhydration (132 ± 26 μm vs. 233 ± 23 μm, P < 0.001) and after 5 hours in a moist chamber (46 ± 3 μm vs. 57 ± 3 μm, P < 0.001). After implantation, the nonlasered group showed a tendency toward a greater increase in axial keratometry (6.63 ± 2.17 D vs. 5.60 ± 3.79 D, P = 0.613) and elevation (18.6 ± 15.4 vs. 15.2 ± 5.5, P = 0.656) than the lasered group. Excimer laser ablation may be feasible for thinning and reshaping of SMILE-derived lenticules before reimplantation or allogenic transplantation. However, controlled lenticule dehydration before ablation is necessary in order to allow stromal thinning.

  19. Design of Self-Healing Supramolecular Rubbers by Introducing Ionic Cross-Links into Natural Rubber via a Controlled Vulcanization.

    Science.gov (United States)

    Xu, Chuanhui; Cao, Liming; Lin, Baofeng; Liang, Xingquan; Chen, Yukun

    2016-07-13

    Introducing ionic associations is one of the most effective approaches to realize a self-healing behavior for rubbers. However, most of commercial rubbers are nonpolar rubbers without now available functional groups to be converted into ionic groups. In this paper, our strategy was based on a controlled peroxide-induced vulcanization to generate massive ionic cross-links via polymerization of zinc dimethacrylate (ZDMA) in natural rubber (NR) and exploited it as a potential self-healable material. We controlled vulcanization process to retard the formation of covalent cross-link network, and successfully generated a reversible supramolecular network mainly constructed by ionic cross-links. Without the restriction of covalent cross-linkings, the NR chains in ionic supramolecular network had good flexibility and mobility. The nature that the ionic cross-links was easily reconstructed and rearranged facilitating the self-healing behavior, thereby enabling a fully cut sample to rejoin and retain to its original properties after a suitable self-healing process at ambient temperature. This study thus demonstrates a feasible approach to impart an ionic association induced self-healing function to commercial rubbers without ionic functional groups.

  20. Making post-mortem implantable cardioverter defibrillator explantation safe

    DEFF Research Database (Denmark)

    Räder, Sune B E W; Zeijlemaker, Volkert; Pehrson, Steen

    2009-01-01

    that the resting voltage over the operating person would not exceed 50 V. CONCLUSION: The use of intact medical gloves made of latex, neoprene, or plastic eliminates the potential electrical risk during explantation of an ICD. Two gloves on each hand offer sufficient protection. We will recommend the use......AIMS: The aim of this study is to investigate whether protection with rubber or plastic gloves during post-mortem explantation of an implantable cardioverter defibrillator (ICD) offers enough protection for the explanting operator during a worst-case scenario (i.e. ICD shock). METHODS AND RESULTS...

  1. [Total analysis of organic rubber additives].

    Science.gov (United States)

    He, Wen-Xuan; Robert, Shanks; You, Ye-Ming

    2010-03-01

    In the present paper, after middle pressure chromatograph separation using both positive phase and reversed-phase conditions, the organic additives in ethylene-propylene rubber were identified by infrared spectrometer. At the same time, by using solid phase extraction column to maintain the main component-fuel oil in organic additves to avoid its interfering with minor compounds, other organic additves were separated and analysed by GC/Ms. In addition, the remaining active compound such as benzoyl peroxide was identified by CC/Ms, through analyzing acetone extract directly. Using the above mentioned techniques, soften agents (fuel oil, plant oil and phthalte), curing agent (benzoylperoxide), vulcanizing accelerators (2-mercaptobenzothiazole, ethyl thiuram and butyl thiuram), and antiagers (2, 6-Di-tert-butyl-4-methyl phenol and styrenated phenol) in ethylene-propylene rubber were identified. Although the technique was established in ethylene-propylene rubber system, it can be used in other rubber system.

  2. Osteogenesis and Morphology of the Peri-Implant Bone Facing Dental Implants

    Directory of Open Access Journals (Sweden)

    Marco Franchi

    2004-01-01

    tissue showed different results. Around the SS screws, the compact bone with areas of different mineralisation rate appeared very smooth, while around the rougher TPS screws, the bone still showed an irregular surface corresponding to the implant macro/microroughness. Around the Zr-SLA screws, a more regular implant-bone surface and sparse, calcified marrow spaces were detectable.Results from this research suggest that 2 weeks after implantation, trabecular bone represents the calcified healing tissue, which supports the early biological fixation of the implants. The peri-implant marrow spaces, rich in undifferentiated cells and blood vasculature, observed both 2 weeks and 3 months after surgery, favour the biological turnover of both early and mature peri-implant bone. The implant surface morphology strongly influences the rate and the modality of peri-implant osteogenesis, as do the morphology and arrangement of the implant face in peri-implant bone both during early healing (after 2 weeks and when the implant is just osseointegrated; rough surfaces, and in particular Zr-SLA, seem to better favour bone deposition on the metal surface.

  3. Investigation of surface halide modification of nitrile butadiene rubber

    Science.gov (United States)

    Sukhareva, K. V.; Mikhailov, I. A.; Andriasyan, Yu O.; Mastalygina, E. E.; Popov, A. A.

    2017-12-01

    The investigation is devoted to the novel technology of surface halide modification of rubber samples based on nitrile butadiene rubber (NBR). 1,1,2-trifluoro-1,2,2-trichlorethane was used as halide modifier. The developed technology is characterized by production stages reduction to one by means of treating the rubber compound with a halide modifier. The surface halide modification of compounds based on nitrile butadiene rubber (NBR) was determined to result in increase of resistance to thermal oxidation and aggressive media. The conducted research revealed the influence of modification time on chemical resistance and physical-mechanical properties of rubbers under investigation.

  4. Improving rubber concrete by waste organic sulfur compounds.

    Science.gov (United States)

    Chou, Liang-Hisng; Lin, Chun-Nan; Lu, Chun-Ku; Lee, Cheng-Haw; Lee, Maw-Tien

    2010-01-01

    In this study, the use of crumb tyres as additives to concrete was investigated. For some time, researchers have been studying the physical properties of concrete to determine why the inclusion of rubber particles causes the concrete to degrade. Several methods have been developed to improve the bonding between rubber particles and cement hydration products (C-S-H) with the hope of creating a product with an improvement in mechanical strength. In this study, the crumb tyres were treated with waste organic sulfur compounds from a petroleum refining factory in order to modify their surface properties. Organic sulfur compounds with amphiphilic properties can enhance the hydrophilic properties of the rubber and increase the intermolecular interaction forces between rubber and C-S-H. In the present study, a colloid probe of C-S-H was prepared to measure these intermolecular interaction forces by utilizing an atomic force microscope. Experimental results showed that rubber particles treated with waste organic sulfur compounds became more hydrophilic. In addition, the intermolecular interaction forces increased with the adsorption of waste organic sulfur compounds on the surface of the rubber particles. The compressive, tensile and flexural strengths of concrete samples that included rubber particles treated with organic sulfur compound also increased significantly.

  5. Circuit racing, track texture, temperature and rubber friction

    Science.gov (United States)

    Sharp, R. S.; Gruber, P.; Fina, E.

    2016-04-01

    Some general observations relating to tyre shear forces and road surfaces are followed by more specific considerations from circuit racing. The discussion then focuses on the mechanics of rubber friction. The classical experiments of Grosch are outlined and the interpretations that can be put on them are discussed. The interpretations involve rubber viscoelasticity, so that the vibration properties of rubber need to be considered. Adhesion and deformation mechanisms for energy dissipation at the interface between rubber and road and in the rubber itself are highlighted. The enquiry is concentrated on energy loss by deformation or hysteresis subsequently. Persson's deformation theory is outlined and the material properties necessary to apply the theory to Grosch's experiments are discussed. Predictions of the friction coefficient relating to one particular rubber compound and a rough surface are made using the theory and these are compared with the appropriate results from Grosch. Predictions from Persson's theory of the influence of nominal contact pressure on the friction coefficient are also examined. The extent of the agreement between theory and experiment is discussed. It is concluded that there is value in the theory but that it is far from complete. There is considerable scope for further research on the mechanics of rubber friction.

  6. Implant-retained maxillary overdentures.

    Science.gov (United States)

    Eckert, Steven E; Carr, Alan B

    2004-07-01

    Overdentures supported by osseointegrated implants overcome many of the complications observed with overdentures supported by natural teeth. Dental implants are free of biologic consequences associated with natural teeth, such as dental caries and periodontal disease. Bone undercuts adjacent to implants do not mimic those found adjacent to natural tooth roots. Implants are used to provide predictable retention, support, and stability for overdenture prostheses. When lip or facial support is required, the overdenture is the treatment of choice. Likewise the overdenture may improve phonetic deficiencies associated with alveolar bone loss.

  7. Composite Piezoelectric Rubber Band for Energy Harvesting from Breathing and Limb Motion

    International Nuclear Information System (INIS)

    Wang, Jhih-Jhe; Su, Huan-Jan; Hsu, Chang-I; Su, Yu-Chuan

    2014-01-01

    We have successfully demonstrated the design and microfabrication of piezoelectric rubber bands and their application in energy harvesting from human motions. Composite polymeric and metallic microstructures with embedded bipolar charges are employed to realize the desired stretchability and electromechanical sensitivity. In the prototype demonstration, multilayer PDMS cellular structures coated with PTFE films and stretchable gold electrodes are fabricated and implanted with bipolar charges. The composite structures show elasticity of 300∼600 kPa and extreme piezoelectricity of d 33 >2000 pC/N and d 31 >200 pC/N. For a working volume of 2.5cm×2.5cm×0.3mm, 10% (or 2.5mm) stretch results in effective d 31 of >17000 pC/N. It is estimated that electric charge of >0.2 μC can be collected and stored per breath (or 2.5cm deformation). As such, the composite piezoelectric rubber bands (with spring constants of ∼200 N/m) can be mounted on elastic waistbands to harvest the circumferential stretch during breathing, or on pads around joints to harvest the elongation during limb motion. Furthermore, the wearable piezoelectric structures can be spread, stacked and connected to charge energy storages and power micro devices

  8. Composite Piezoelectric Rubber Band for Energy Harvesting from Breathing and Limb Motion

    Science.gov (United States)

    Wang, Jhih-Jhe; Su, Huan-Jan; Hsu, Chang-I.; Su, Yu-Chuan

    2014-11-01

    We have successfully demonstrated the design and microfabrication of piezoelectric rubber bands and their application in energy harvesting from human motions. Composite polymeric and metallic microstructures with embedded bipolar charges are employed to realize the desired stretchability and electromechanical sensitivity. In the prototype demonstration, multilayer PDMS cellular structures coated with PTFE films and stretchable gold electrodes are fabricated and implanted with bipolar charges. The composite structures show elasticity of 300~600 kPa and extreme piezoelectricity of d33 >2000 pC/N and d31 >200 pC/N. For a working volume of 2.5cm×2.5cm×0.3mm, 10% (or 2.5mm) stretch results in effective d31 of >17000 pC/N. It is estimated that electric charge of >0.2 μC can be collected and stored per breath (or 2.5cm deformation). As such, the composite piezoelectric rubber bands (with spring constants of ~200 N/m) can be mounted on elastic waistbands to harvest the circumferential stretch during breathing, or on pads around joints to harvest the elongation during limb motion. Furthermore, the wearable piezoelectric structures can be spread, stacked and connected to charge energy storages and power micro devices.

  9. Determination of the Mechanical Properties of Rubber by FT-NIR

    OpenAIRE

    Pornprasit, Rattapol; Pornprasit, Philaiwan; Boonma, Pruet; Natwichai, Juggapong

    2016-01-01

    Mechanical tests, for example, tensile and hardness tests, are usually used to evaluate the properties of rubber materials. In this work, mechanical properties of selected rubber materials, that is, natural rubber (NR), styrene butadiene rubber (SBR), nitrile butadiene rubber (NBR), and ethylene propylene diene monomer (EPDM), were evaluated using a near infrared (NIR) spectroscopy technique. Here, NR/NBR and NR/EPDM blends were first prepared. All of the samples were then scanned using a FT-...

  10. Ultraviolet curing of acrylated liquid natural rubber for surface coating application

    OpenAIRE

    Kannikar Kwanming; Pairote Klinpituksa; Wae-asae Waehamad

    2009-01-01

    Ultraviolet curable acrylated liquid natural rubber was prepared by grafting of photosensitive molecule onto liquid natural rubber for surface coating application. The liquid natural rubber (LNR) was firstly obtained by degradation of natural rubber latex with hydrogen peroxide and cobalt acetylacetonate at 65oC for 72 hrs. The preparation of acrylated natural rubber was carried out by the reaction of acrylic acid and epoxidized liquid natural rubber (ELNR) prior obtained from LNR with formic...

  11. A lettuce (Lactuca sativa) homolog of human Nogo-B receptor interacts with cis-prenyltransferase and is necessary for natural rubber biosynthesis.

    Science.gov (United States)

    Qu, Yang; Chakrabarty, Romit; Tran, Hue T; Kwon, Eun-Joo G; Kwon, Moonhyuk; Nguyen, Trinh-Don; Ro, Dae-Kyun

    2015-01-23

    Natural rubber (cis-1,4-polyisoprene) is an indispensable biopolymer used to manufacture diverse consumer products. Although a major source of natural rubber is the rubber tree (Hevea brasiliensis), lettuce (Lactuca sativa) is also known to synthesize natural rubber. Here, we report that an unusual cis-prenyltransferase-like 2 (CPTL2) that lacks the conserved motifs of conventional cis-prenyltransferase is required for natural rubber biosynthesis in lettuce. CPTL2, identified from the lettuce rubber particle proteome, displays homology to a human NogoB receptor and is predominantly expressed in latex. Multiple transgenic lettuces expressing CPTL2-RNAi constructs showed that a decrease of CPTL2 transcripts (3-15% CPTL2 expression relative to controls) coincided with the reduction of natural rubber as low as 5%. We also identified a conventional cis-prenyltransferase 3 (CPT3), exclusively expressed in latex. In subcellular localization studies using fluorescent proteins, cytosolic CPT3 was relocalized to endoplasmic reticulum by co-occurrence of CPTL2 in tobacco and yeast at the log phase. Furthermore, yeast two-hybrid data showed that CPTL2 and CPT3 interact. Yeast microsomes containing CPTL2/CPT3 showed enhanced synthesis of short cis-polyisoprenes, but natural rubber could not be synthesized in vitro. Intriguingly, a homologous pair CPTL1/CPT1, which displays ubiquitous expressions in lettuce, showed a potent dolichol biosynthetic activity in vitro. Taken together, our data suggest that CPTL2 is a scaffolding protein that tethers CPT3 on endoplasmic reticulum and is necessary for natural rubber biosynthesis in planta, but yeast-expressed CPTL2 and CPT3 alone could not synthesize high molecular weight natural rubber in vitro. © 2015 by The American Society for Biochemistry and Molecular Biology, Inc.

  12. Some Tribological Characterization of “EPDM” Rubber

    Directory of Open Access Journals (Sweden)

    A. Mukhopadhyay

    2014-06-01

    Full Text Available Ethylene Propylene Diene Monomer (EPDM rubber emerges as a dominant elastomer for major engineering applications. The major properties of EPDM are its outstanding heat, ozone and weather resistance ability. It has a good resistance to polar substances and steam condition too. In automobiles EPDM rubber has a common use as seals. This includes door seals, window seals, trunk seals and sometimes hood seals. Frequently these seals are the source of noise due to the movement of the door versus the car body. This is due to friction between the EPDM rubber parts and the mating surfaces. Thus, the contact iteration between the rubber sealing and the indenting object must be known to optimize the performance of rubber sealing. However, it is need less to mention that the behaviour of any viscoelastic material is very difficult to be predicted. In the present work various tribo-characteristics of EPDM rubber of different hardness have been evaluated utilizing the available laboratory test facilities in the Jadavpur University, Kolkata, India. Compression tests have been carried out using ‘Instron’ to determine the flow behaviour of EPDM rubber of different hardness both in dry as well as under different conditions of lubrication. The flow behaviour like load -vs.- elongation curves, true stress -vs.- elongation curves and true stress -vs.- true strain curves have been drawn from the experimental data. Abrasive wear behaviour has been evaluated using a two-body abrasion tester and the pattern abrasion has been appraised through SEM/EDAX study. Experimental results reveal that the hardness of EPDM rubber has significant effect on the flow behaviour and wear characteristics. The hardness, again, depends on the proportion of carbon black (CB content. Thus it can be stated that the flow behaviour can be governed by controlling the CB concentration in the EPDM rubber. Based on the experimental results conclusion has been drawn accordingly. Some of the

  13. Energy usage in the rubber industry

    Energy Technology Data Exchange (ETDEWEB)

    Soederstroem, M.

    1980-01-01

    The rubber industry has several energy-intensive steps, such as mastication of natural rubber, mixing and extrusion, and vulcanization. Opportunities for energy savings would be available with a continuous mixing process, heat recovery from cooling waters, and abandonment of thermal conduction in vulcanization. 6 figures. (DCK)

  14. Reinforcing effect of plasma modified halloysite nanotubes in a carbon black filled natural rubber-butadien rubber matrix

    NARCIS (Netherlands)

    Poikelispaa, Minna; Das, Amit; Dierkes, Wilma K.; Vuorinen, Jyrki

    2011-01-01

    Rubber composites are generally produced by the direct incorporation of fillers like carbon black and/or silica into the rubber matrix. The incorporation of different types of nanofillers is the subject of recent research with the aim of preparing composites with special compositions and properties.

  15. The enzymatic synthesis of rubber polymer in Parthenium argentatum Gray

    International Nuclear Information System (INIS)

    Benedict, C.R.; Madhavan, S.; Greenblatt, G.A.; Venkatachalam, K.V.; Foster, M.A.

    1990-01-01

    Washed rubber particles isolated from stem homogenates of Parthenium argentatum Gray by ultracentrifugation and gel filtration on columns of LKB Ultrogel AcA34 contain rubber transferase which catalyzes the polymerization of isopentenyl pyrophosphate into rubber polymer. The polymerization reaction requires Mg 2+ isopentenyl pyrophosphate, and an allylic pyrophosphate. The K m values for Mg 2+ , isopentenyl pyrophosphate, and dimethylallyl pyrophosphate were 5.2 x 10 -4 molar, 8.3 x 10 -5 molar, and 9.6 x 10 -5 molar, respectively. The molecular characteristics of the rubber polymer synthesized from [ 14 C]isopentenyl pyrophosphate were examined by gel permeation chromatography. The peak molecular weight of the radioactive polymer increased from 70,000 in 15 minutes to 750,000 in 3 hours. The weight average molecular weight of the polymer synthesized over a 3 hour period was 1.17 x 10 6 compared to 1.49 x 10 6 for the natural rubber polymer extracted from the rubber particles. Over 90% of the in vitro formation of the rubber polymer was de novo from dimethylallyl pyrophosphate and isopentenyl pyrophosphate. Treatment of the washed rubber particles with 3-[(3-cholamidopropyl)dimethylammonio]-1-propanesulfonate solubilized the rubber transferase. The solubilized enzyme(s) catalyzed the polymerization of isopentenyl pyrophosphate into rubber polymer with a peak molecular weight of 1 x 10 5 after 3 hours of incubation with Mg 2+ and dimethylallyl pyrophosphate. The data support the conclusion that the soluble preparation of rubber transferase is capable of catalyzing the formation of a high molecular weight rubber polymer from an allylic pyrophosphate initiator and isopentenyl pyrophosphate monomer

  16. Parasitism of Erythmelus tingitiphagus (Soares) (Hymenoptera: Mymaridae) in Leptopharsa heveae Drake and Poor (Hemiptera: Tingidae) eggs, in rubber tree plantation (Hevea brasiliensis Mueell. Arg.)

    International Nuclear Information System (INIS)

    Santos, Rodrigo S.; Freitas, Sergio de

    2008-01-01

    The rubber tree lace bug, Leptopharsa heveae Drake and Poor occurs in high populations in rubber tree plantations and it is a limiting factor in rubber production due to the loss of photosynthetic tissue. The control of the pest has been made mainly with chemical products, which cause environmental contamination. The alternative would be the use of biological control agents, however, information about L. heveae natural enemies are scarce. The parasitoid Erythmelus tingitiphagus (Soares) parasitize eggs of the rubber tree lace bug. The aim of this study was to verify the occurrence of E. tingitiphagus in plantations of several rubber tree clones, located in Itiquira town, Mato Grosso State. The plant leaflets of the clones RRIM 600, PR 255, GT 1, PB 235 and PB 217 were collected weekly from October 2005 to February 2006. Parasitism was recorded during the entire study period. The parasitism rate of L. heveae eggs in the different clones ranged from 16.8 to 20.6%. (author)

  17. Fabrication of shape memory natural rubber using palmitic acid

    Directory of Open Access Journals (Sweden)

    Jeff Sze-Hua Wee

    2017-10-01

    Full Text Available This paper investigates the practicability of fabricating a shape memory natural rubber with the use of palmitic acid as the swelling agent. Strips of natural rubber samples were swollen in molten palmitic acid at 75 °C. Equilibrium swelling of natural rubber with palmitic acid was found to occur at approximately 50 min of swelling time. Under cooling effect, the palmitic acid crystallized to form a percolated crystalline platelet network. These networks allow fabricated shape memory natural rubber (SMNR to deform and recover its shape at a temperature above the melting point of palmitic acid. Under controlled uniaxial stress, the natural rubber sample with 0 parts per hundred rubber (phr carbon black loading exhibits fixity and recovery of 80 ± 10%. Motivation of this research is primarily on practicability of palmitic acid to be used as a swelling agent for shape memory properties. Results show that palmitic acid is a relatively good swelling agent to induce shape memory properties into natural rubber.

  18. Fabrication of Wood-Rubber Composites Using Rubber Compound as a Bonding Agent Instead of Adhesives

    Directory of Open Access Journals (Sweden)

    Dongwei Shao

    2016-06-01

    Full Text Available Differing from the hot-pressing method in the manufacturing of traditional wood-rubber composites (WRCs, this study was aimed at fabricating WRCs using rubber processing to improve water resistance and mechanical properties. Three steps were used to make WRCs, namely, fiber-rubber mixing, tabletting, and the vulcanization molding process. Ninety-six WRC panels were made with wood fiber contents of 0%–50% at rotor rotational speeds of 15–45 rpm and filled coefficients of 0.55–0.75. Four regression equations, i.e., the tensile strength (Ts, elongation at break (Eb, hardness (Ha and rebound resilience (Rr as functions of fiber contents, rotational speed and filled coefficient, were derived and a nonlinear programming model were developed to obtain the optimum composite properties. Although the Ts, Eb and Rr of the panels were reduced, Ha was considerably increased by 17%–58% because of the wood fiber addition. Scanning electron microscope images indicated that fibers were well embedded in rubber matrix. The 24 h water absorption was only 1%–3%, which was much lower than commercial wood-based composites.

  19. Fabrication of Wood-Rubber Composites Using Rubber Compound as a Bonding Agent Instead of Adhesives.

    Science.gov (United States)

    Shao, Dongwei; Xu, Min; Cai, Liping; Shi, Sheldon Q

    2016-06-14

    Differing from the hot-pressing method in the manufacturing of traditional wood-rubber composites (WRCs), this study was aimed at fabricating WRCs using rubber processing to improve water resistance and mechanical properties. Three steps were used to make WRCs, namely, fiber-rubber mixing, tabletting, and the vulcanization molding process. Ninety-six WRC panels were made with wood fiber contents of 0%-50% at rotor rotational speeds of 15-45 rpm and filled coefficients of 0.55-0.75. Four regression equations, i.e. , the tensile strength ( T s), elongation at break ( E b), hardness ( H a) and rebound resilience ( R r) as functions of fiber contents, rotational speed and filled coefficient, were derived and a nonlinear programming model were developed to obtain the optimum composite properties. Although the T s, E b and R r of the panels were reduced, H a was considerably increased by 17%-58% because of the wood fiber addition. Scanning electron microscope images indicated that fibers were well embedded in rubber matrix. The 24 h water absorption was only 1%-3%, which was much lower than commercial wood-based composites.

  20. Biologically effective dose (BED) for interstitial seed implants containing a mixture of radionuclides with different half-lives

    International Nuclear Information System (INIS)

    Chen Zhe; Nath, Ravinder

    2003-01-01

    Purpose: To develop a tool for evaluating interstitial seed implants that contain a mixture of radionuclides with different half-lives and to demonstrate its utility by examining the clinical implications of prescribing to an isodose surface for such an implant. Methods and Materials: A linear-quadratic model for continuous low dose rate irradiation was developed for permanent implants containing a mixture of radionuclides. Using a generalized equation for the biologically effective dose (BED), the effects of cell proliferation and sublethal damage repair were examined systematically for implants containing a mixture of radionuclides. A head-and-neck permanent seed implant that contained a mixture of 125 I and 103 Pd seeds was used to demonstrate the utility of the generalized BED. Results: An equation of BED for implants containing a mixture of radionuclides with different half-lives was obtained. In such an implant, the effective cell kill was shown to depend strongly on the relative dose contributions from each radionuclide type; dose delivered by radionuclides with shorter half-life always resulted in more cell kill for any given sublethal damage repair and cell proliferation rates. Application of the BED formula to an implant containing a mixture of 125 I and 103 Pd seeds demonstrates that the conventional dose prescription to an isodose surface is not unique for such an implant. When the prescription dose was based on existing clinical experience of using 125 I seeds alone, mixing 103 Pd seeds with 125 I seeds would increase the cell kill. On the other hand, if the prescription dose were based on existing clinical experience of using 103 Pd seeds alone, mixing 125 I seeds with 103 Pd seeds in the same implant would create radiobiologically 'cold' spots (i.e., an increase in cell survival) at locations where a major portion of the prescription dose is contributed by the 125 I seeds. For fast-growing tumors, these 'cold' spots can become significant

  1. Seismic isolation rubber bearings for nuclear facilities

    International Nuclear Information System (INIS)

    Fujita, Takafumi

    1991-01-01

    This paper describes results of biaxial breaking tests by compression and shear and by tension and shear for seismic isolation rubber bearings with bolted-type connections. The bearings used in the tests were low-damping rubber bearings, high-damping rubber bearings, and lead-rubber bearings. Three modes of failure of the bolted-type bearings were observed in the tests. They are the breaking failure by tension and shear; the breaking failure by compression and shear; and the buckling failure by compression and shear. The first and the second modes of failures are almost independent of the types and the sizes of the bearings. The breaking conditions of those failure modes are described in the axial-stress-shear-strain plane. This expression is useful for the evaluation of safety margins of the bearings. The paper outlines the basic design of the nuclear-grade bearings which were used for large-scale rubber bearing tests in a research project for seismic isolation of FBR plants. It also discusses the protection method against aging and the quality control which are important for implementation. (orig./HP)

  2. Seismic isolation rubber bearings for nuclear facilities

    International Nuclear Information System (INIS)

    Fujita, Takafumi

    1989-01-01

    This paper describes results of biaxial breaking tests by compression and shear and by tension and shear for seismic isolation rubber bearings with bolted-type connections. The bearings used in the tests were low-damping rubber bearings, high-damping rubber bearings, and lead-rubber bearings. Three modes of failure of the bolted-type bearings were observed in the tests. They are the breaking failure by tension and shear; the breaking failure by compression and shear; and the buckling failure by compression and shear. The first and the second modes of failures are almost independent of the types and the sizes of the bearings. The breaking conditions of those failure modes are described in the axial stress-shear strain plane. This expression is useful for the evaluation of safety margins of the bearings. The paper outlines the basic design of the nuclear-grade bearings which were used for large-scale rubber bearing tests in a research project for seismic isolation of fast breeder reactor (FBR) plants. The paper also discusses the protection method against aging and the quality control which are important for implementation

  3. Review of food toxicological issues associated in rubber products

    OpenAIRE

    Ng, Mei Xiang; Ong, S.P.; Hii, C.L.; Chuah, L.A.; Law, C.L.

    2014-01-01

    Over the centuries, rubber latex gained its popularity in machinery application due to its unique thermal properties, high elasticity and excellent impact resistance. It is widely accepted in food industry as rubber has good resistance to chemicals, including acids, alkalis and salts. For instance, rubber components comprise of couplings, shields, dust covers, gaskets and seals exist as group or standalone component in food manufacturing equipments or machinery. Even though most of the rubber...

  4. Rubber friction and tire dynamics

    International Nuclear Information System (INIS)

    Persson, B N J

    2011-01-01

    We propose a simple rubber friction law, which can be used, for example, in models of tire (and vehicle) dynamics. The friction law is tested by comparing numerical results to the full rubber friction theory (Persson 2006 J. Phys.: Condens. Matter 18 7789). Good agreement is found between the two theories. We describe a two-dimensional (2D) tire model which combines the rubber friction model with a simple mass-spring description of the tire body. The tire model is very flexible and can be used to accurately calculate μ-slip curves (and the self-aligning torque) for braking and cornering or combined motion (e.g. braking during cornering). We present numerical results which illustrate the theory. Simulations of anti-blocking system (ABS) braking are performed using two simple control algorithms.

  5. Rubber friction and tire dynamics.

    Science.gov (United States)

    Persson, B N J

    2011-01-12

    We propose a simple rubber friction law, which can be used, for example, in models of tire (and vehicle) dynamics. The friction law is tested by comparing numerical results to the full rubber friction theory (Persson 2006 J. Phys.: Condens. Matter 18 7789). Good agreement is found between the two theories. We describe a two-dimensional (2D) tire model which combines the rubber friction model with a simple mass-spring description of the tire body. The tire model is very flexible and can be used to accurately calculate μ-slip curves (and the self-aligning torque) for braking and cornering or combined motion (e.g. braking during cornering). We present numerical results which illustrate the theory. Simulations of anti-blocking system (ABS) braking are performed using two simple control algorithms.

  6. Forecasting Natural Rubber Price In Malaysia Using Arima

    Science.gov (United States)

    Zahari, Fatin Z.; Khalid, Kamil; Roslan, Rozaini; Sufahani, Suliadi; Mohamad, Mahathir; Saifullah Rusiman, Mohd; Ali, Maselan

    2018-04-01

    This paper contains introduction, materials and methods, results and discussions, conclusions and references. Based on the title mentioned, high volatility of the price of natural rubber nowadays will give the significant risk to the producers, traders, consumers, and others parties involved in the production of natural rubber. To help them in making decisions, forecasting is needed to predict the price of natural rubber. The main objective of the research is to forecast the upcoming price of natural rubber by using the reliable statistical method. The data are gathered from Malaysia Rubber Board which the data are from January 2000 until December 2015. In this research, average monthly price of Standard Malaysia Rubber 20 (SMR20) will be forecast by using Box-Jenkins approach. Time series plot is used to determine the pattern of the data. The data have trend pattern which indicates the data is non-stationary data and the data need to be transformed. By using the Box-Jenkins method, the best fit model for the time series data is ARIMA (1, 1, 0) which this model satisfy all the criteria needed. Hence, ARIMA (1, 1, 0) is the best fitted model and the model will be used to forecast the average monthly price of Standard Malaysia Rubber 20 (SMR20) for twelve months ahead.

  7. Fatigue life of automotive rubber jounce bumper

    International Nuclear Information System (INIS)

    Sidhu, R S; Ali, Aidy

    2010-01-01

    It is evident that most rubber components in the automotive industry are subjected to repetitive loading. Vigorous research is needed towards improving the safety and reliability of the components. The study was done on an automotive rubber jounce bumper with a rubber hardness of 60 IRHD. The test was conducted in displacement-controlled environment under compressive load. The existing models by Kim, Harbour, Woo and Li were adopted to predict the fatigue life. The experimental results show strong similarities with the predicted models.

  8. Determination of the Mechanical Properties of Rubber by FT-NIR

    Directory of Open Access Journals (Sweden)

    Rattapol Pornprasit

    2016-01-01

    Full Text Available Mechanical tests, for example, tensile and hardness tests, are usually used to evaluate the properties of rubber materials. In this work, mechanical properties of selected rubber materials, that is, natural rubber (NR, styrene butadiene rubber (SBR, nitrile butadiene rubber (NBR, and ethylene propylene diene monomer (EPDM, were evaluated using a near infrared (NIR spectroscopy technique. Here, NR/NBR and NR/EPDM blends were first prepared. All of the samples were then scanned using a FT-NIR spectrometer and fitted with an integration sphere working in a diffused reflectance mode. The spectra were correlated with hardness and tensile properties. Partial least square (PLS calibration models were built from the spectra datasets with preprocessing techniques, that is, smoothing and second derivative. This indicated that reasonably accurate models, that is, with a coefficient of determination [R2] of the validation greater than 0.9, could be achieved for the hardness and tensile properties of rubber materials. This study demonstrated that FT-NIR analysis can be applied to determine hardness and tensile values in rubbers and rubber blends effectively.

  9. Application of gamma irradiation for incorporation of rubber powder in the formulations of acrylonitrile-butadiene rubber (NBR)

    International Nuclear Information System (INIS)

    Kiyan, Ludmila Y.P.; Parra, Duclerc Fernandes

    2013-01-01

    Full text: Polymeric materials do not decompose easily, disposal of waste polymers is a major environmental problem of global character. Recycling is an economical alternative and environmentally recommended for polymers consumed and discarded by society. As regards the rubber in object, its natural decomposition is much slower due to their highly crosslinked, in three-dimensional networks, structures which makes it an infusible and insoluble material. Moreover, these three dimensional structures entails several problems for their recovery and reprocessing. The aim of this paper was to study the behavior of NBR rubber recycle. It was used rubber powder from industry. The powder was irradiated in master-batch composition and used directly in classical formulations for rubber vulcanization. The master-batch processed was irradiated at doses of 50, 100 and 150kGy in 60 Co source at 5 kGy s -1 rate, at room temperature. Gamma radiation created active sites during devulcanization that promoted further integration of the rubber powder in formulations for commercial use. The processes were compared and their products were characterized by analytical methods of the physical properties such as tensile strength and elongation. The greatest change in the properties of polymeric materials by exposure to ionizing radiation resulted mainly of two main reactions occurring in the polymer molecule: chains scission (degradation) and crosslinking. Although these two processes occur simultaneously in all the polymers, the predominance of one or other effect depends mainly of the chemical structure of each polymer, and the irradiation conditions. In the results was observed the behavior of nitrile rubber under different doses and radiation improvement of the mechanical properties. (author)

  10. Application of gamma irradiation for incorporation of rubber powder in the formulations of acrylonitrile-butadiene rubber (NBR)

    Energy Technology Data Exchange (ETDEWEB)

    Kiyan, Ludmila Y.P.; Parra, Duclerc Fernandes, E-mail: ludmilapozzo@gmail.com [Instituto de Pesquisas Energeticas e Nucleares (IPEN/CNEN-SP), Sao Paulo, SP (Brazil). Centro de Quimica e Meio Ambiente (CQMA)

    2013-07-01

    Full text: Polymeric materials do not decompose easily, disposal of waste polymers is a major environmental problem of global character. Recycling is an economical alternative and environmentally recommended for polymers consumed and discarded by society. As regards the rubber in object, its natural decomposition is much slower due to their highly crosslinked, in three-dimensional networks, structures which makes it an infusible and insoluble material. Moreover, these three dimensional structures entails several problems for their recovery and reprocessing. The aim of this paper was to study the behavior of NBR rubber recycle. It was used rubber powder from industry. The powder was irradiated in master-batch composition and used directly in classical formulations for rubber vulcanization. The master-batch processed was irradiated at doses of 50, 100 and 150kGy in {sup 60}Co source at 5 kGy s{sup -1} rate, at room temperature. Gamma radiation created active sites during devulcanization that promoted further integration of the rubber powder in formulations for commercial use. The processes were compared and their products were characterized by analytical methods of the physical properties such as tensile strength and elongation. The greatest change in the properties of polymeric materials by exposure to ionizing radiation resulted mainly of two main reactions occurring in the polymer molecule: chains scission (degradation) and crosslinking. Although these two processes occur simultaneously in all the polymers, the predominance of one or other effect depends mainly of the chemical structure of each polymer, and the irradiation conditions. In the results was observed the behavior of nitrile rubber under different doses and radiation improvement of the mechanical properties. (author)

  11. Properties of tire rubber with zinc-containing technological additives

    Directory of Open Access Journals (Sweden)

    S. N. Kayushnikov

    2017-01-01

    Full Text Available In this paper, we studied the influence of zinc-containing technological additives on partial replacement of zinc oxide and stearic acid on deformation-strength and performance properties of tire elastomeric compositions based on polyisoprene rubber and combination of oil-filled butadiene-styrene and polybutadiene rubbers. It was revealed that partial replacement of zinc oxide and stearic acid with zinc-containing technological additives does not significantly affect the basic physico-mechanical properties of rubbers based on synthetic rubbers of general use. It was determined that the introduction of zinc-containing technological additives SCC2 in combination with zinc oxide in all the studied ratios and SCC3 in combination with zinc oxide in 4: 1 and 3: 1 ratios leads to increase (up to 10.4% of the resistance of these rubbers under the action of temperature-force fields, which is probably due to a more even distribution of polar components of curing system in non-polar elastomeric matrix, as well as the type of cross-links formed during vulcanization under the action of surface-active additives. It has been found that the introduction of zinc-containing additives into the elastomeric compositions based on SRMS-30 ARKM-15 + SRD in combination with zinc oxide leads to increase to 6.3% of wear resistance of rubbers, which may be due to a lower defectiveness of vulcanization structure of these rubbers, concentration of stress centers in the material. For rubbers based on SRI-3, preservation of bond strength of rubber with a textile cord at a sufficiently high level is shown.

  12. Development of rubberized geopolymer interlocking bricks

    Directory of Open Access Journals (Sweden)

    Bashar S Mohammed

    2018-06-01

    Full Text Available Waste tires contribute badly to the environment on a huge scale as they are bulky, non-biodegradable, and prone to fire and being a shelter for mosquitos and other insects. This paper reports on a novel approach towards the development of rubberized brick by utilizing crumb rubber as the sole fine aggregate in the production of geopolymer interlocking bricks. The response surface methodology (RSM from Design Experts software has been used to determine the numbers of trial mixes and their corresponding ingredients. A total of thirteen trial mixes were carried out and tested for compressive strength and the RSM model was developed to predict the design mix based on the targeted compressive strength. The mix design was obtained to be an 18 M for NaOH and 0.8 solution to fly ash ratio. The geopolymer interlocking rubberized bricks were then produced and tested for compressive strength, dimension, modulus of rupture, water absorption, initial rate of absorption, and efflorescence. The geopolymer interlocking rubberised bricks presented a low compressive and flexural strength and a high-water absorption capacity. The bricks were rated as non-effloresced and classified as 3rd class bricks which can be used as non-load bearing material. It is recommended to utilize nano silica in order to increase the strength of the brick. Keywords: Rubberized bricks, Crumb rubber, Interlocking bricks, Geopolymer, Response surface methodology

  13. Modification of rubber surface by UV surface grafting

    International Nuclear Information System (INIS)

    Shanmugharaj, A.M.; Kim, Jin Kuk; Ryu, Sung Hun

    2006-01-01

    Rubber surface is subjected to ultraviolet radiation (UV) in the presence of allylamine and radiation sensitizer benzophenone (BP). Fourier transform infrared spectral studies reveal the presence of allylamine on the surface. The presence of irregular needle shapes on the surface as observed in scanning electron micrographs also confirms the polymerized allylamine on the surface. Allylamine coatings have been further confirmed from atomic force microscopy (AFM) analysis. Thermogravimetric analysis (TGA) reveals that allylamine coating on the rubber surface lowers the thermal degradation rate. The contact angle between the water and rubber surface decreases for the modified rubber surface confirming the surface modification due to UV surface grafting

  14. Life assessment of rubber articles in fuels

    OpenAIRE

    Selldén, Emmy

    2013-01-01

    The choice of rubber material for use in sealings and hoses in the fuel system is of great importance. If a wrong type of rubber is used, premature failure during service may occur. This impacts the environmental performance, the safety during driving, uptime and economy of the transport. In this diploma work, rubbers for use in sealing and hoses in the fuel system have been evaluated to assess which materials have the potential to be used under long-term use in contact with commercial fuels....

  15. Research Progress in Graphene/Rubber Conducting Nanocomposites

    Directory of Open Access Journals (Sweden)

    DONG Hui-min

    2017-03-01

    Full Text Available The conductive mechanism of graphene/rubber nanocomposites was introduced.Advances in the synthesis and properties of graphene and its derivatives, modifications of graphene, along with its hybrid fillers, as well as fabrication of related rubber conducting nanocomposites were reviewed.Many factors affecting the electrical properties, such as fabrication method, vulcanization, temperature, pressure, frequency and media etc. were also summarized.It was pointed out that the further research should be focused on multi-component graphene/rubber nanocomposites and its double percolation phenomenon.

  16. Boron-Loaded Silicone Rubber Scintillators

    Energy Technology Data Exchange (ETDEWEB)

    Bell, Z.W.; Maya, L.; Brown, G.M.; Sloop, F.V.Jr

    2003-05-12

    Silicone rubber received attention as an alternative to polyvinyltoluene in applications in which the scintillator is exposed to high doses because of the increased resistance of the rubber to the formation of blue-absorbing color centers. Work by Bowen, et al., and Harmon, et al., demonstrated their properties under gamma/x-ray irradiation, and Bell, et al. have shown their response to thermal neutrons. This last work, however, provided an example of a silicone in which both the boron and the scintillator were contained in the rubber as solutes, a formulation which led to the precipitation of solids and sublimation of the boron component. In the present work we describe a scintillator in which the boron is chemically bonded to the siloxane and so avoids the problem of precipitation and loss of boron to sublimation. Material containing up to 18% boron, by weight, was prepared, mounted on photomultipliers, and exposed to both neutron and gamma fluxes. Pulse height spectra showing the neutron and photon response were obtained, and although the light output was found to be much poorer than from samples in which boron was dissolved, the higher boron concentrations enabled essentially 100% neutron absorption in only a few millimeters' thickness of rubber.

  17. Trends in prosthetic biomaterials in implant dentistry

    Directory of Open Access Journals (Sweden)

    Saranjit Singh Bhasin

    2015-01-01

    Full Text Available The most important criterion for the success of dental implants is the selection of a suitable implant biomaterial. To improve the biologic performance of an implant, it is necessary to select a material that does not elicit any negative biological response and at the same time maintains adequate function. It is mandatory for a dentist to have a comprehensive knowledge of various biomaterials used for dental implants. The material of choice for fabrication of the dental implant till date is titanium. With the advancements in the field of implants, zirconia seems to be propitious in the future. However, more advanced in vitro and in vivo studies are required before reaching any such conclusion. To increase the success of zirconia implants, care should be taken to reduce the incidence of mechanical failures. Such failures can be taken care of by having a thorough technical knowledge of implant designing and manufacturing defects. This article attempts to compare the advantages and disadvantages of various dental implant biomaterials. Focus is placed on the recent advances in this field with the recently introduced zirconia and its comparison to conventional titanium.

  18. Asphalt concrete modified by rubber crumbs in transport construction.

    Science.gov (United States)

    Duhovny, G. S.; Karpenko, AV

    2018-03-01

    High-temperature and low-temperature characteristics of the rubber-bitumen binder and rubber asphalt concrete based on it are researched. The determination method of binder’s low-temperature characteristics is offered. The estimation of binder’s and pavement’s stability against technological and operational aging is evaluated. Estimation of environmental and economic aspects of using rubber crumbs is made. The possibility of using rubber crumbs as modifier of organic binder for production of asphalt concrete on its base is justified.

  19. FY 2000 report on the results of the regional consortium R and D project - Regional consortium energy R and D. Third year report. R and D of high grade/low cost mold for rubber/plastic; 2000 nendo chiiki consortium kenkyu kaihatsu jigyo - chiiki consortium energy kenkyu kaihatsu. Gomu plastic yo kohin'i tei cost kanagata no kenkyu kaihatsu (dai 3 nendo) seika hokokusho

    Energy Technology Data Exchange (ETDEWEB)

    NONE

    2001-05-01

    The development was proceeded with of technology to reform the surface of rubber/plastic use mold by ion engineering technology so that the product can be easily taken out without being stained by the material. Concretely, PBII (plasma-based ion implantation) device with high ion implantation efficiency was developed, and surface reforming conditions were studied. Then, from the test using the actual device, the surface reforming technology optimum to mold releasing and mold staining resistance as rubber molding was established. Studies were made of the following: 1) establishment of the optimum mold surface reforming technology; 2) establishment of the mold surface treatment technology using PBII device; 3) improvement of PBII device and optimization of implantation method. In 2), by the surface treatment by implanting nitrogen and fluorine ions into hard chromium plating and aluminum alloys using PBII device, treatment effects were recognized in implantation ability into 3D shape, mold staining resistance and mold releasing in the hard chromium plating treated mold. (NEDO)

  20. On the response of rubbers at high strain rates.

    Energy Technology Data Exchange (ETDEWEB)

    Niemczura, Johnathan Greenberg (University of Texas-Austin)

    2010-02-01

    In this report, we examine the propagation of tensile waves of finite deformation in rubbers through experiments and analysis. Attention is focused on the propagation of one-dimensional dispersive and shock waves in strips of latex and nitrile rubber. Tensile wave propagation experiments were conducted at high strain-rates by holding one end fixed and displacing the other end at a constant velocity. A high-speed video camera was used to monitor the motion and to determine the evolution of strain and particle velocity in the rubber strips. Analysis of the response through the theory of finite waves and quantitative matching between the experimental observations and analytical predictions was used to determine an appropriate instantaneous elastic response for the rubbers. This analysis also yields the tensile shock adiabat for rubber. Dispersive waves as well as shock waves are also observed in free-retraction experiments; these are used to quantify hysteretic effects in rubber.

  1. Biodiesel Production from Rubber Seed Oil via Esterification Process

    Directory of Open Access Journals (Sweden)

    W Widayat

    2012-07-01

    Full Text Available One promise source of alternative energy is biodiesel from rubber seed oil, because the raw materials available in plentiful quantities and can be renewed. In addition, the rubber seed is still lack of utilization, and Indonesia is one of the largest rubbers producing country in the world. The objective of this research is to studied on biodiesel production by esterification process. Parameters used in this study are the ratio of catalyst and temperature and its influence on the characteristics of the resulting biodiesel product. Characterization of rubber seed include acid content number analysis, saponification numbers, density, viscosity, iodine number, type of free fatty acids and triglyceride oils. The results of analysis showed that rubber seed oil content obtained is 50.5%. The results of the GCMS analysis showed that a free fatty acid level in rubber seed is very high. Conversion into bio-diesel oil is obtained by at most 59.91% and lowest 48.24%.

  2. The Rubber Hand Illusion Revisited: Visuotactile Integration and Self-Attribution

    Science.gov (United States)

    Tsakiris, Manos; Haggard, Patrick

    2005-01-01

    Watching a rubber hand being stroked, while one's own unseen hand is synchronously stroked, may cause the rubber hand to be attributed to one's own body, to "feel like it's my hand." A behavioral measure of the rubber hand illusion (RHI) is a drift of the perceived position of one's own hand toward the rubber hand. The authors investigated (a) the…

  3. Research on a haptic sensor made using MCF conductive rubber

    International Nuclear Information System (INIS)

    Zheng Yaoyang; Shimada, Kunio

    2008-01-01

    To provide a new composite material having a high electrical sensitivity in the fields of robotics and sensing, a magnetic rubber having network-like magnetic clusters was developed by utilizing a magnetic compound fluid (MCF). MCF rubber with small deformations can provide an effective sensor. In this paper, we report many experiments in which changes of the MCF rubber's resistance were observed when the rubber was compressed and a deformation was generated; we then made a trial haptic sensor using the MCF conductive rubber and performed many experiments to observe changes of the electrical resistance of the sensor. The results of experiments showed that the proposed sensor made with MCF conductive rubber is useful for sensing small amounts of pressure or small deformations

  4. Research on a haptic sensor made using MCF conductive rubber

    Energy Technology Data Exchange (ETDEWEB)

    Zheng Yaoyang; Shimada, Kunio [Faculty of Symbiotic Systems Science Fukushima University, 1 Kanayakawa, Fukushima 960-1296 (Japan)], E-mail: tei@sss.fukushima-u.ac.jp, E-mail: shimadakun@sss.fukushima-u.ac.jp

    2008-05-21

    To provide a new composite material having a high electrical sensitivity in the fields of robotics and sensing, a magnetic rubber having network-like magnetic clusters was developed by utilizing a magnetic compound fluid (MCF). MCF rubber with small deformations can provide an effective sensor. In this paper, we report many experiments in which changes of the MCF rubber's resistance were observed when the rubber was compressed and a deformation was generated; we then made a trial haptic sensor using the MCF conductive rubber and performed many experiments to observe changes of the electrical resistance of the sensor. The results of experiments showed that the proposed sensor made with MCF conductive rubber is useful for sensing small amounts of pressure or small deformations.

  5. Research on a haptic sensor made using MCF conductive rubber

    Science.gov (United States)

    Zheng, Yaoyang; Shimada, Kunio

    2008-05-01

    To provide a new composite material having a high electrical sensitivity in the fields of robotics and sensing, a magnetic rubber having network-like magnetic clusters was developed by utilizing a magnetic compound fluid (MCF). MCF rubber with small deformations can provide an effective sensor. In this paper, we report many experiments in which changes of the MCF rubber's resistance were observed when the rubber was compressed and a deformation was generated; we then made a trial haptic sensor using the MCF conductive rubber and performed many experiments to observe changes of the electrical resistance of the sensor. The results of experiments showed that the proposed sensor made with MCF conductive rubber is useful for sensing small amounts of pressure or small deformations.

  6. Contact allergy to rubber accelerators remains prevalent

    DEFF Research Database (Denmark)

    Schwensen, J F; Menné, T; Johansen, J D

    2016-01-01

    several clinical cases with allergic facial dermatitis to rubber. OBJECTIVES: To evaluate temporal trends of contact allergy to rubber accelerators from the European baseline series in a tertiary patch test clinic in Denmark, and examine associations with anatomical locations of dermatitis. METHODS: Patch...... test and clinical data collected in a Danish tertiary dermatology clinic in Gentofte, Herlev, Copenhagen between 1 January 2005 and 31 December 2014 were analysed. The following rubber accelerators or mixtures in petrolatum from the European baseline patch test series were included: thiuram mix 1.......0%, mercaptobenzothiazole 2.0% and mercapto mix 1.0%. RESULTS: The overall prevalence of contact allergy to rubber accelerators was 3.1% with no significant change during the study period (Ptrend = 0.667). Contact allergy to thiuram mix was the most prevalent and was significantly associated with occupational contact...

  7. Study for the degumming pretreatment of rubber seed oil

    Science.gov (United States)

    Li, X. Y.; Chen, Y. B.; Zhang, X.; Souliyathai, D.; Yang, S. P.; Wang, Q.

    2017-11-01

    With the rapid development of the aviation industry, appearing of the aviation carbon tax and the increasingly serious environmental problems have forced the world to research the development of renewable bio-aviation fuel. Renewable biological aviation fuel contains phosphorus that could reduce the synthesis of noble metal catalysts such as Pd, Pt activity. In order to get low content of phosphorus in degummed oil of non-edible vegetable oil, in this paper, with rubber seed oil as raw material, making the experiment of single factor at the influence of temperature, stirring speed, adding amount of monoethanolamine (MEA) and water amount. The experimental results show that the added amount of MEA is 2.5% in the weight of oil, and temperature is 60°C, while the amount of added water is 2% in the weight of oil, reaction time is 40 min, and stirring speed is 200 r/min. Under these conditions, the phosphorus content of rubber seed oil can be reduced to below 3 mg/kg, degumming rate is 91.37%, and the degumming effects are obvious, which also provides some foundation for follow-up studies.

  8. Sugarcane bagasse ash: new filler to natural rubber composite

    Directory of Open Access Journals (Sweden)

    Renivaldo José dos Santos

    2014-12-01

    Full Text Available Waste recycling has been the subject of numerous scientific researches regarding the environmental care. This paper reports the redirecting of sugarcane bagasse ash (SBA as new filler to natural rubber (NR/SBA. The NR/SBA composites were prepared using an opened cylinder mixer to incorporate the vulcanization agents and different proportions of residue (SBA. The ash contains about 70-90% of inorganic compounds, with silica (SiO2 being the main compound. The SBA incorporation improved the mechanical properties of the vulcanized rubber. Based on these results, a new use is proposed for the agro-industry organic waste to be implemented in the rubber vulcanization process, aimed at improving the rubber physical properties as well as decreasing the prices of natural rubber composites.

  9. Research and Application Progress of Silicone Rubber Materials in Aviation

    Directory of Open Access Journals (Sweden)

    HUANG Yanhua

    2016-06-01

    Full Text Available The research progress of heat resistance, cold resistance, electrical conductivity and damping properties of aviation silicone rubber were reviewed in this article. The heat resistance properties of silicone rubber can be enhanced by changing the molecular structure (main chain, end-group, side chain and molecular weight of the gum and adding special heat-resistance filler. The cold resistance of aviation silicone rubber can be enhanced by adjusting the side chain molecular structure of the gum and the content of different gum chain. The electrical conductivity of silicone rubber can be improved by optimizing, blending and dispersing of conductive particles. The damping property of silicone rubber can be improved by designing and synthesizing of high-molecular polysiloxane damping agent. Furthermore, the application of aviation silicone rubber used in high-low temperature seal, electrical conduction and vibration damping technology are also summarized, and the high performance (for example long-term high temperature resistance, ultralow temperature resistance, high electromagnetic shelding, long-term fatigue resistance vibration damping, quasi constant modulus and so on of special silicone rubber is the future direction of aviation silicone rubber.

  10. Thermal properties of hydrogenated liquid natural rubber

    Science.gov (United States)

    Jamaluddin, Naharullah; Abdullah, Ibrahim; Yusoff, Siti Fairus M.

    2015-09-01

    Natural rubber (NR) was modified to form liquid natural rubber (LNR) via photooxidative degradation. Hydrogenated liquid natural rubber (HLNR) was synthesized by using diimide as source of hydrogen which the diimide is produced by thermolysis of p-toluenesulfonyl hydrazide (TSH). The structure of HLNR was characterized by determining the changes of main peaks in Fourier Transform infrared and nuclear magnetic resonance spectra after hydrogenation. Thermogravimetric analysis showed that the HLNR had higher decomposition temperature compared to LNR and the decomposition temperature is directly proportional to the percentage of conversion.

  11. Thermal properties of hydrogenated liquid natural rubber

    International Nuclear Information System (INIS)

    Jamaluddin, Naharullah; Abdullah, Ibrahim; Yusoff, Siti Fairus M.

    2015-01-01

    Natural rubber (NR) was modified to form liquid natural rubber (LNR) via photooxidative degradation. Hydrogenated liquid natural rubber (HLNR) was synthesized by using diimide as source of hydrogen which the diimide is produced by thermolysis of p-toluenesulfonyl hydrazide (TSH). The structure of HLNR was characterized by determining the changes of main peaks in Fourier Transform infrared and nuclear magnetic resonance spectra after hydrogenation. Thermogravimetric analysis showed that the HLNR had higher decomposition temperature compared to LNR and the decomposition temperature is directly proportional to the percentage of conversion

  12. Thermal properties of hydrogenated liquid natural rubber

    Energy Technology Data Exchange (ETDEWEB)

    Jamaluddin, Naharullah; Abdullah, Ibrahim; Yusoff, Siti Fairus M. [School of Chemical Sciences and Food Technology, Faculty of Science and Technology, Universiti Kebangsaan Malaysia, 43600 Bangi, Selangor (Malaysia)

    2015-09-25

    Natural rubber (NR) was modified to form liquid natural rubber (LNR) via photooxidative degradation. Hydrogenated liquid natural rubber (HLNR) was synthesized by using diimide as source of hydrogen which the diimide is produced by thermolysis of p-toluenesulfonyl hydrazide (TSH). The structure of HLNR was characterized by determining the changes of main peaks in Fourier Transform infrared and nuclear magnetic resonance spectra after hydrogenation. Thermogravimetric analysis showed that the HLNR had higher decomposition temperature compared to LNR and the decomposition temperature is directly proportional to the percentage of conversion.

  13. Natural rubber producing plants: An overview | Venkatachalam ...

    African Journals Online (AJOL)

    ... Hevea and also other natural rubber producing species for alternative source of latex production in the near future. Keywords: Alternative rubber sources, biotechnology, breeding, Hevea brasiliensis, Parthenium argentatum, Taraxacum koksaghyz, Ficus bengalensis, Lactuca serriola. African Journal of Biotechnology Vol.

  14. UTILISATION OF RUBBER SEED OL IN THE

    African Journals Online (AJOL)

    Thermal degradation studies on polyvinyl chloride in the presence of rubber seed oil, epoxidized rubber seed oil and metal ... Epoxidation of RSO was carried out at 29°C using peractic acid ..... impurities such as pigments, Vitamins, sterols ...

  15. Interfacial interaction between the epoxidized natural rubber and silica in natural rubber/silica composites

    Science.gov (United States)

    Xu, Tiwen; Jia, Zhixin; Luo, Yuanfang; Jia, Demin; Peng, Zheng

    2015-02-01

    The epoxidized natural rubber (ENR) as an interfacial modifier was used to improve the mechanical and dynamical mechanical properties of NR/silica composites. In order to reveal the interaction mechanism between ENR and silica, the ENR/Silica model compound was prepared by using an open mill and the interfacial interaction of ENR with silica was investigated by Fourier transform infrared spectroscopy (FTIR), X-ray photoelectron spectroscopy (XPS), transmission electron microscopy (TEM), X-ray diffraction (XRD) and stress-strain testing. The results indicated that the ring-opening reaction occurs between the epoxy groups of ENR chains and Si-OH groups on the silica surfaces and the covalent bonds are formed between two phases, which can improve the dispersion of silica in the rubber matrix and enhance the interfacial combination between rubber and silica. The ring-opening reaction occurs not only in vulcanization process but also in mixing process, meanwhile, the latter seems to be more important due to the simultaneous effects of mechanical force and temperature.

  16. Mechanistic study of the rubber-brass adhesion interphase

    Science.gov (United States)

    Ashirgade, Akshay

    Brass-plated steel tire cords form an essential strengthening component of a radial automobile tire. Adhesion between rubber compound and brass-plated steel tire cord is crucial in governing the overall performance of tires. The rubber-brass interfacial adhesion is influenced by the chemical composition and thickness of the interfacial layer. It has been shown that the interfacial layer consists mainly of sulfides and oxides of copper and zinc. This thesis discusses the effect of changes in the chemical composition and the structure of the interfacial layers due to addition of adhesion promoter resins. Grazing incidence X-Ray Diffraction (GIXRD) experiments were run on sulfidized polished brass coupons previously bonded to six experimental rubber compounds. It was confirmed that heat and humidity conditions lead to physical and chemical changes of the rubber-steel tire cord interfacial layer, closely related to the degree of rubber-brass adhesion. Morphological transformation of the interfacial layer led to loss of adhesion after aging. The adhesion promoter resins inhibit unfavorable morphological changes in the interfacial layer thus stabilizing it during aging and prolonging failure. Tire cord adhesion tests illustrated that the one-component resins improved adhesion after aging using a rubber compound with lower cobalt loading. Based on the acquired diffraction profiles, these resins were also found to impede crystallization of the sulfide layer after aging leading to improved adhesion. Secondary Ion Mass Spectrometry (SIMS) depth profiles, SEM micrographs and AFM images strongly corroborated the findings from GIXRD. FTIR was utilized in a novel way to understand the degradation mechanism due to aging. A model for rubber and interfacial layer degradation is proposed to illustrate the effect of aging and the one-component resins. This interfacial analysis adds valuable new information to our understanding of the complex nature of the rubber-brass bonding

  17. 75 FR 57980 - Polychloroprene Rubber From Japan

    Science.gov (United States)

    2010-09-23

    ... INTERNATIONAL TRADE COMMISSION [Investigation No. AA1921-129 (Third Review)] Polychloroprene Rubber From Japan AGENCY: United States International Trade Commission. ACTION: Termination of five-year... of the antidumping duty finding on polychloroprene rubber from Japan would be likely to lead to...

  18. Experimental Investigation of the Mechanical and Durability Properties of Crumb Rubber Concrete.

    Science.gov (United States)

    Liu, Hanbing; Wang, Xianqiang; Jiao, Yubo; Sha, Tao

    2016-03-07

    Recycling waste tire rubber by incorporating it into concrete has become the preferred solution to dispose of waste tires. In this study, the effect of the volume content of crumb rubber and pretreatment methods on the performances of concrete was evaluated. Firstly, the fine aggregate and mixture were partly replaced by crumb rubber to produce crumb rubber concrete. Secondly, the mechanical and durability properties of crumb rubber concrete with different replacement forms and volume contents had been investigated. Finally, the crumb rubber after pretreatment by six modifiers was introduced into the concrete mixture. Corresponding tests were conducted to verify the effectiveness of pretreatment methods as compared to the concrete containing untreated crumb rubber. It was observed that the mechanical strength of crumb rubber concrete was reduced, while durability was improved with the increasing of crumb rubber content. 20% replacement of fine aggregate and 5% replacement of the total mixture exhibited acceptable properties for practical applications. In addition, the results indicated that the modifiers had a positive impact on the mechanical and durability properties of crumb rubber concrete. It avoided the disadvantage of crumb rubber concrete having lower strength and provides a reference for the production of modified crumb rubber concrete.

  19. Experimental Investigation of the Mechanical and Durability Properties of Crumb Rubber Concrete

    Directory of Open Access Journals (Sweden)

    Hanbing Liu

    2016-03-01

    Full Text Available Recycling waste tire rubber by incorporating it into concrete has become the preferred solution to dispose of waste tires. In this study, the effect of the volume content of crumb rubber and pretreatment methods on the performances of concrete was evaluated. Firstly, the fine aggregate and mixture were partly replaced by crumb rubber to produce crumb rubber concrete. Secondly, the mechanical and durability properties of crumb rubber concrete with different replacement forms and volume contents had been investigated. Finally, the crumb rubber after pretreatment by six modifiers was introduced into the concrete mixture. Corresponding tests were conducted to verify the effectiveness of pretreatment methods as compared to the concrete containing untreated crumb rubber. It was observed that the mechanical strength of crumb rubber concrete was reduced, while durability was improved with the increasing of crumb rubber content. 20% replacement of fine aggregate and 5% replacement of the total mixture exhibited acceptable properties for practical applications. In addition, the results indicated that the modifiers had a positive impact on the mechanical and durability properties of crumb rubber concrete. It avoided the disadvantage of crumb rubber concrete having lower strength and provides a reference for the production of modified crumb rubber concrete.

  20. Simulation work of fatigue life prediction of rubber automotive components

    International Nuclear Information System (INIS)

    Samad, M S A; Ali, Aidy

    2010-01-01

    The usage of rubbers has always been so important, especially in automotive industries. Rubbers have a hyper elastic behaviour which is the ability to withstand very large strain without failure. The normal applications for rubbers are used for shock absorption, sound isolation and mounting. In this study, the predictions of fatigue life of an engine mount of rubber automotive components were presented. The finite element analysis was performed to predict the critical part and the strain output were incorporated into fatigue model for prediction. The predicted result shows agreement in term of failure location of rubber mount.

  1. Performance Study of the Natural Rubber Composite with Clay Minerals

    International Nuclear Information System (INIS)

    Nyo Nyo Myint; Tin Tin Aye; Kyaw Myo Naing; Nyunt Wynn

    2008-03-01

    The preparation, characterization and some applications of natural rubber clay composite have been studied. This study investigated the possibility of natural rubber latex to replace some part of natural clays. In formulation of rubber clay composite from natural rubber latex and various clay minerals, three main steps were involved (i) preparation of latex cream (ii) prevulcanization of latex cream (iii) mixing vulcanized latex compound, with other ingredients. In each step, several parameters have been carefully investigated to optimize the performance of natural rubber clay composite production. The composite products were of better quality and can be considered to be more cost effective.

  2. Use of rubber crumb for preparation of asphalt-concrete mixtures

    Directory of Open Access Journals (Sweden)

    Yerbol Tileuberdi

    2012-03-01

    Full Text Available In this article use of rubber crumb from spent tire for preparation of rubber-bitumen compounds is investigated. Then the rubber-bitumen compositions are used in composition of asphalt concrete mixes .

  3. Proceedings of the Rubber Association of Canada's 7. biennial 2006 rubber recycling symposium : changing concepts

    Energy Technology Data Exchange (ETDEWEB)

    NONE

    2006-07-01

    Rising energy costs and concerns over the environment have contributed to a renewed focus on recycling for many governments and industries. This conference examined recent trends affecting rubber recycling activities as well as the legislative environment and its impacts on future recycling activities. Major rubber recycling markets were reviewed, and emerging product ideas were evaluated. Industry stewardship model and governance models were discussed. The impacts of new advances in tire technology and manufacturing on the rubber recycling industry were also investigated. Issues concerning fixed tipping fees and incentive structures were discussed, and effective management strategies for the recycling of large off-the-road tires were evaluated. Tire-derived fuel (TDF) is the largest market in North America for scrap tires, and TDF may continue to grow as a result of rising fossil fuel costs. Issues and challenges related to the introduction of TDF to new communities were discussed. New developments in tire derived aggregates (TDA) and ground rubber were also reviewed. Twenty-eight presentations were given at this conference, 3 of which were catalogued separately for inclusion in this database. refs., tabs., figs.

  4. The water-food nexus of natural rubber production

    Science.gov (United States)

    Chiarelli, D. D.; Rosa, L.; Rulli, M. C.; D'Odorico, P.

    2017-12-01

    The increasing global demand for natural rubber (100% increase in the last 15 years) is for most part met by Malaysia and Indonesia, and - to a lesser extent - other countries in south-east Asia and Africa. The consequent expansion of rubber plantation has often occurred at the expenses of agricultural land for staple food, particularly in southeast Asia, where most of the land suitable for agriculture is already harvested for food crops or other uses. Here we investigate the extent to which the ongoing increase in rubber production is competing with the food system and affecting the livelihoods of rural communities in the areas of production and their appropriation of natural resources, such as water. We also investigate to what extent the expansion of rubber plantations is taking place through large scale land acquisitions (LSLAs) and evaluate the impacts on rural communities. Our results show how rubber production has strong environmental, social and economic impacts. Despite their ability to bring employment and increase the average income of economically disadvantaged areas, rubber plantations may threaten the local water and food security and induce a loss of rural livelihoods, particularly when the new plantations result from LSLAs that displace semi-subsistence forms of production thereby forcing the local populations to depend on global markets.

  5. Aging Depth Test of Rubber Blocks by Accelerated Thermal Oxidation Test

    International Nuclear Information System (INIS)

    Park, Junhee; Choun, Young-Sun; Kim, Min Kyu

    2015-01-01

    In this study, the accelerated thermal oxidation tests of rubber block were performed to investigate the aging depth of rubber bearing. From the tests, it was found the critical aging depth in rubber block. Also the property variation of rubber was investigated along the depth. The deterioration pattern from the aging depth tests was found from surface to inside and the critical aging depth was to be about 10 mm. The analytical model for rubber bearing with aging can be developed based on the relationship between the property variation and aging depth investigated from this study. The mechanical properties of rubber bearings were changed with time. Because the aging effect of rubber material was generally higher than that of other structure materials it is needed that the aging properties of seismically isolators should be evaluated to ensure the safety of seismically isolated nuclear power plants (NPPs) over the lifetime. NRC and ASCE required the tests of seismically isolators for investigating the aging properties. JNES also required the seismic response analysis for the seismically isolated NPPs when the properties of seismically isolators were extremely changed. If the aging properties of seismically isolators such as rubber bearings are evaluated by analysis the analytical model of seismically isolators should be developed considering aging effect of rubber material. From the previous research, it was reported that the behavior of aged rubber material mainly affected by temperature and oxidation. The material properties between surface and inside can be different by the oxidation of rubber. Therefore, the aging depth should be investigated for exactly evaluating the seismic behavior of aged rubber bearing. The aging depth of rubber baring was not influenced by the size of seismically isolators but environment condition. Therefore, the detail analysis considering aging depth was not required for NPPs with large seismically isolators. But the seismic response

  6. 30 CFR 77.606-1 - Rubber gloves; minimum requirements.

    Science.gov (United States)

    2010-07-01

    ... 30 Mineral Resources 1 2010-07-01 2010-07-01 false Rubber gloves; minimum requirements. 77.606-1... COAL MINES Trailing Cables § 77.606-1 Rubber gloves; minimum requirements. (a) Rubber gloves (lineman's gloves) worn while handling high-voltage trailing cables shall be rated at least 20,000 volts and shall...

  7. Recycling of rubber tires in asphalt paving materials

    Energy Technology Data Exchange (ETDEWEB)

    Piggott, M.R.; Woodhams, R.T.

    1979-01-01

    It has been known that the addition of rubber to asphalt used in paving will produced markedly superior road surfaces. Partly because of cost and because of the nonconventional paving techniques necessary, rubber has been largely ignored as a practical paving additive except in special cases. However, the large accumulation of old tires existing today provides a ready source for suitable rubber. If ground into a fine powder, this rubber can be mixed in a conventional pug mill along with sand, stone and asphalt to produce a hot mix which can be aplied in the normal manner without any special techniques. The extra cost of such modification is only 1% of a typical paving contract, whereas the advantages include lower maintenance cost, more durable road surface, and elimination of unwanted waste tires. This report has been prepared to assist civic and other authorities in the development of improved road surfacing formulations through the reuse of old tires. It includes the results of paving trials in Toronto and laboratory evaluations. These tests show that the addition of powdered rubber to asphalt paving materials markedly improves the durability and crack resistance, particularly at low temperatures. Additives in the rubber impart good strength retention in the presence of moisture. The toughness increases with age due to a slow interaction of the rubber with the asphalt which is accompanied by an increase in viscosity. As a result, performance is also enhanced at high temperatures and helps to minimize pavement distortions due to hot weather and traffic. 16 refs., 18 figs., 2 tabs.

  8. Studies on biological effects of nitrogen ion implantation in different genotype rice

    International Nuclear Information System (INIS)

    Xie Jiahua; Xia Yingwu; Shu Qingyao

    1994-01-01

    The biological effects of nitrogen ion implantation on different genotype rice (Oryza sativa L) were studied. The results showed that there were obvious differences in physiological damages for the M 1 generation, mutation frequencies and mutagenic efficiencies of chlorophyll, heading date and plant height for M 2 generation of different genotypes. Treated by nitrogen ions, the varieties with high mutation frequency and mutagenic efficiency of chlorophyll in the M 2 generation were not necessarily high in those of heading date and plant height. Moreover, the radiation sensitivity of Fu8530 and Fuxian No.6 which were bred by using early maturing and semidwarf mutants as maternal plant was low. The early maturing and high stature mutation were not induced with these two varieties

  9. Chrome-tanned leather shavings as a filler of butadiene-acrylonitrile rubber.

    Science.gov (United States)

    Przepiórkowska, A; Chrońska, K; Zaborski, M

    2007-03-06

    The noxious wastes from the tanning industry such as chrome-tanned leather shavings were used as the only filler of rubber mixes containing carboxylated butadiene-acrylonitrile rubber (XNBR) or butadiene-acrylonitrile rubber (NBR), and a dispersing agent Limanol PEV (Schill & Seilacher). The best form addition of leather powder to the rubber mixes is mixed the waste protein with zinc oxide. The leather powder added to the rubber mixes improves the mechanical properties: tensile strength (T(s)), elongation at break (epsilon(b)) and increase the cross-linking density of carboxylated XNBR and NBR rubber mixes. Satisfactory results of these studies are presented in this work.

  10. Soft matter: rubber and networks

    Science.gov (United States)

    McKenna, Gregory B.

    2018-06-01

    Rubber networks are important and form the basis for materials with properties ranging from rubber tires to super absorbents and contact lenses. The development of the entropy ideas of rubber deformation thermodynamics provides a powerful framework from which to understand and to use these materials. In addition, swelling of the rubber in the presence of small molecule liquids or solvents leads to materials that are very soft and ‘gel’ like in nature. The review covers the thermodynamics of polymer networks and gels from the perspective of the thermodynamics and mechanics of the strain energy density function. Important relationships are presented and experimental results show that the continuum ideas contained in the phenomenological thermodynamics are valid, but that the molecular bases for some of them remain to be fully elucidated. This is particularly so in the case of the entropic gels or swollen networks. The review is concluded with some perspectives on other networks, ranging from entropic polymer networks such as thermoplastic elastomers to physical gels in which cross-link points are formed by glassy or crystalline domains. A discussion is provided for other physical gels in which the network forms a spinodal-like decomposition, both in thermoplastic polymers that form a glassy network upon phase separation and for colloidal gels that seem to have a similar behavior.

  11. Optical and Thermal Stability of Oligofluorene/Rubber Luminescent Blend.

    Science.gov (United States)

    Barbosa, Camila G; Faez, Roselena; Péres, Laura O

    2016-09-01

    This paper proposes to obtain homogeneous and stable blends of oligo(9,9-dioctylfluorene)-co-phenylene (OF), a conjugated oligomer with strong tendency of formation of excimers in the solid state, and nitrile rubber (NBR). This rubber protection reduces the formation of polymer excimers in the films. The fluorene oligomer was synthesized via Suzuki reaction and incorporated in the nitrile rubber. The films were formed by spin coating and casting techniques on the proportions of 1, 5, 10, 20 and 50 % (w/w) of OF in the nitrile rubber (NBR). The structural, optical and thermal properties of the films were evaluated with infrared, UV-Vis, fluorescence and thermogravimetry, respectively. The nitrile rubber proved to be essential for the preparation of homogeneous and stable films, since it was not possible to obtain films with only fluorene using the above-mentioned techniques. Furthermore, luminescent properties of OF are unchanged and the excimers formation in the solid state decrease suggesting the efficiency of nitrile rubber as the matrix for making films.

  12. Gamma-radiation effect on thermal ageing of butyl rubber compounds

    Energy Technology Data Exchange (ETDEWEB)

    Scagliusi, Sandra R.; Cardoso, Elizabeth C.L.; Lugao, Ademar B., E-mail: srscagliusi@ipen.br [Instituto de Pesquisas Energeticas e Nucleares (IPEN/CNEN-SP), Sao Paulo, SP (Brazil)

    2015-07-01

    Butyl rubber has a comprehensive use in sealing systems, especially in tires inner tubes, due to their low permeability to gases. So, it is required that butyl rubber compounds show a better performance, more and more. Butyl rubber is provided with excellent mechanical properties and oxidation resistance. Besides showing these properties, radiation exposures impart modifications in physical-chemical and morphological properties on butyl rubber materials. When exposed to gamma-radiation, rubbers suffer changes in their mechanical and physical properties, caused by material degradation. The major radiation effect in butyl rubbers is chain scission; besides, ageing promotes too the same effect with further build-up of free radicals. This work aims to the study of gamma-radiation in physical-chemical properties of butyl rubber subjected to thermal ageing. Doses used herein were: 25 kGy, 50 kGy, 100 kGy, 150 kGy and 200 KGy. Samples were evaluated before and after ageing according to traditional essays, such as: hardness, tensile strength and elongation at break. From accomplished assessments it is possible to affirm that at doses higher than 50 kGy it was observed a sharp decreasing in butyl rubber physical-chemical properties, before and after exposure to ageing. (author)

  13. Gamma-radiation effect on thermal ageing of butyl rubber compounds

    International Nuclear Information System (INIS)

    Scagliusi, Sandra R.; Cardoso, Elizabeth C.L.; Lugao, Ademar B.

    2015-01-01

    Butyl rubber has a comprehensive use in sealing systems, especially in tires inner tubes, due to their low permeability to gases. So, it is required that butyl rubber compounds show a better performance, more and more. Butyl rubber is provided with excellent mechanical properties and oxidation resistance. Besides showing these properties, radiation exposures impart modifications in physical-chemical and morphological properties on butyl rubber materials. When exposed to gamma-radiation, rubbers suffer changes in their mechanical and physical properties, caused by material degradation. The major radiation effect in butyl rubbers is chain scission; besides, ageing promotes too the same effect with further build-up of free radicals. This work aims to the study of gamma-radiation in physical-chemical properties of butyl rubber subjected to thermal ageing. Doses used herein were: 25 kGy, 50 kGy, 100 kGy, 150 kGy and 200 KGy. Samples were evaluated before and after ageing according to traditional essays, such as: hardness, tensile strength and elongation at break. From accomplished assessments it is possible to affirm that at doses higher than 50 kGy it was observed a sharp decreasing in butyl rubber physical-chemical properties, before and after exposure to ageing. (author)

  14. Preparation of vinyl acetate grafted natural rubber by irradiation method

    Energy Technology Data Exchange (ETDEWEB)

    Porntrairat, A.; Pattamaprom, C. [Center of Excellence on Natural Rubber Technology, Department of Chemical Engineering, Faculty of Engineering, Thammasat University, Pathumthani 12120 (Thailand)

    2016-03-09

    Improvement in properties of natural rubber could be done by several methods. In this research, gamma radiation technique, which is simple, accurate, easy to control and clean, was applied to enhance the properties of natural rubber (NR) in latex state. The purpose of this research is to study the appropriate condition for preparing grafted natural rubber latex by using irradiation method. Vinyl acetate monomers (VAc) were grafted onto natural rubber latex (NR-g-PVAc) at 0-10 kGys by gamma radiation from Cobalt-60 source at room temperature. Physical properties of grafted natural rubber such as chloroform number, swelling ratio and gel content were measured. The VAc content of NR-g-PVAc was investigated by titration and visualized by FTIR spectroscopy. The FTIR spectra of NR-g-PVAc prepared at 0-10 kGys showed characteristic peaks of the vinyl acetate confirming that VAc could be grafted onto natural rubber molecular chains effectively under appropriate irradiation conditions. From the result, radiation grafting was found to be a useful technique for grafting of vinyl acetate onto natural rubber.

  15. Rheological testing of crumb rubber modified bitumen

    CSIR Research Space (South Africa)

    Mturi, GAJ

    2011-08-01

    Full Text Available used to analyse crumb rubber modified (CRM) bitumen is that the specified gap setting in the configuration of the DSR between the upper and lower test platens is too small to accommodate crumb rubber particles. DSR testing of CRM bitumen therefore...

  16. Implant Stability of Biological Hydroxyapatites Used in Dentistry

    Directory of Open Access Journals (Sweden)

    Maria Piedad Ramírez Fernández

    2017-06-01

    Full Text Available The aim of the present study was to monitor implant stability after sinus floor elevation with two biomaterials during the first six months of healing by resonance frequency analysis (RFA, and how physico-chemical properties affect the implant stability quotient (ISQ at the placement and healing sites. Bilateral maxillary sinus augmentation was performed in 10 patients in a split-mouth design using a bobine HA (BBM as a control and porcine HA (PBM. Six months after sinus lifting, 60 implants were placed in the posterior maxilla. The ISQ was recorded on the day of surgery from RFA at T1 (baseline, T2 (three months, and T3 (six months. Statistically significant differences were found in the ISQ values during the evaluation period. The ISQ (baseline was 63.8 ± 2.97 for BBM and 62.6 ± 2.11 for PBM. The ISQ (T2 was ~73.5 ± 4.21 and 67 ± 4.99, respectively. The ISQ (T3 was ~74.65 ± 2.93 and 72.9 ± 2.63, respectively. All of the used HAs provide osseointegration and statistical increases in the ISQ at baseline, T2 and T3 (follow-up, respectively. The BBM, sintered at high temperature with high crystallinity and low porosity, presented higher stability, which demonstrates that variations in the physico-chemical properties of a bone substitute material clearly influence implant stability.

  17. New type of liquid rubber and compositions based on it.

    Science.gov (United States)

    Semikolenov, S V; Nartova, A V; Voronchikhin, V D; Dubkov, K A

    2014-11-01

    The new method for producing the functionalized polymers and oligomers containing carbonyl C=O groups is developed. The method is based on the noncatalytic oxidation of unsaturated rubbers by nitrous oxide (N2O) at 180-230 °С. The proposed method allows obtaining the new type of functionalized rubbers-liquid unsaturated polyketones with regulated molecular weight and concentration of C=O groups. The influence of the liquid polyketone addition on properties of rubber-based composites is investigated. The study indicates good prospects of using the liquid polyketones for the improvement of properties and operating characteristics of the various types of rubbers and the rubber-cord systems.

  18. Adaptive neuro-fuzzy inference system for forecasting rubber milk production

    Science.gov (United States)

    Rahmat, R. F.; Nurmawan; Sembiring, S.; Syahputra, M. F.; Fadli

    2018-02-01

    Natural Rubber is classified as the top export commodity in Indonesia. Its high production leads to a significant contribution to Indonesia’s foreign exchange. Before natural rubber ready to be exported to another country, the production of rubber milk becomes the primary concern. In this research, we use adaptive neuro-fuzzy inference system (ANFIS) to do rubber milk production forecasting. The data presented here is taken from PT. Anglo Eastern Plantation (AEP), which has high data variance and range for rubber milk production. Our data will span from January 2009 until December 2015. The best forecasting result is 1,182% in term of Mean Absolute Percentage Error (MAPE).

  19. Shear modulus and damping ratio of natural rubber containing carbon nanotubes

    Science.gov (United States)

    Ismail, R.; Ibrahim, A.; Rusop, M.; Adnan, A.

    2018-05-01

    This paper presents the results of an investigation into the potential application of Natural rubber (NR) containing Carbon Nanotubes (CNTs) by measuring its shear modulus and damping ratio. Four different types of rubber specimens which fabricated with different MWCNT loadings: 0 wt% (pure natural rubber), 1 wt%, 3 wt%, and 5 wt%. It is observed that the shear modulus and damping ratio of CNTs filled rubber composites are remarkably higher than that of raw rubber indicating the inherent reinforcing potential of CNTs.

  20. The team approach to managing dental implant complications: strategies for treating peri-implantitis.

    Science.gov (United States)

    Rosen, Paul S

    2013-10-01

    Practitioners who are knowledgeable about the risk factors identified by the Consensus Report of the Sixth European Workshop on Periodontology and who are trained in techniques to eliminate or reduce them may be able to significantly improve long-term implant outcomes. A careful review of the literature suggests that this will include treatment planning, restoring a patient to periodontal heath before initiating care, appropriate implant selection, complete cement removal, and diligent recordkeeping that will track changes and enable early intervention should complications arise. In the case of the biologic complication of peri-implantitis, recent reports suggest that regenerative care may restore implants back to health.

  1. Mecanobiología de la interfase hueso-implante dental Mechanobiology of bone-dental implant interphase

    Directory of Open Access Journals (Sweden)

    Juan Carlos Vanegas Acosta

    2010-03-01

    Full Text Available La osteointegración es la conexión estructural y funcional entre el hueso y un implante. Cuando un implante se inserta en el hueso, se crea la denominada interfase hueso-implante, una zona de unión entre la superficie del biomaterial del implante y el hueso circundante. La cicatrización de esta interfase depende de las condiciones biológicas del hueso, las características de diseño del implante y la distribución de cargas entre hueso e implante. En este artículo se hace una revisión del proceso de cicatrización de la interfase hueso-implante para el caso de un implante dental. El objetivo es describir la secuencia de eventos biológicos iniciados con la lesión causada por la inserción del implante y que concluyen con la formación de nuevo hueso en la interfase. Esta descripción incluye una novedosa clasificación de los fenómenos mecánicos que intervienen durante el proceso de cicatrización de los tejidos lesionados. Esta descripción mecanobiológica de la interfase hueso-implante dental se utiliza para determinar las características más relevantes a tener en cuenta en la formulación de un modelo matemático de la osteointegración de implantes dentales.The osteointegration is the structural and functional connection between bone and implant. When an implant is inserted in bone, it creates the so-called bone-implant interphase, a joint zone between implant biomaterial surface and the surrounding bone. The healing of this interphase depends on bone biological conditions, characteristic of implant design and the distribution of loads between bone and implant. The aim of present article is to review of healing process of bone-implant interphase for a dental implant and also to describe the sequence of biological events beginning with lesion caused by implant insertion and leading to the formation of a new bone in the interphase. This description includes a novel classification of mechanical phenomena present in the healing

  2. Use of Diels-Alder Chemistry for Thermoreversible Cross-Linking of Rubbers : The Next Step toward Recycling of Rubber Products?

    NARCIS (Netherlands)

    Polgar, L. M.; van Duin, M.; Broekhuis, A. A.; Picchioni, F.

    2015-01-01

    A proof of principle for the use of Diels-Alder chemistry as a thermoreversible cross-linking tool for rubber products is demonstrated. A commercial ethylene-propylene rubber grafted with maleic anhydride has been thermoreversibly cross-linked in two steps. The pending anhydride rings were first

  3. Evaluation of rubber seal products for gamma facilities

    International Nuclear Information System (INIS)

    Sobhy, M.S.; Shafy, M.A.; Shahin, F.

    2005-01-01

    Ageing behavior by employing the prolonged exposures of high-energy radiation such as gamma-rays on the physicomechanical properties of some rubber seal products are studied. The proposed binary-rubber blends, SBR/NBR, EPDM/NBR and EPDM/EPM. have overcome their problem of inhomogeneity and incompatibility between the two rubber phases. Such enhancements are acquired by either the replacement of part of NBR by SBR during mastication, or the incorporation of maleic anhydride. Results show that the EPDM/EPM rubber blend has possessed the radiation resistance property towards the deterioration due to higher gamma-irradiation dose. The SEM images have c early observed the role of the used antioxidant, where a thin film is usually produced, degraded; with the appearance of surface cracks, and repaired with further gamma-irradiation up to high doses. Such enhancement is necessary for the definition of the requirements to be put on rubber seal materials. Finally, these products ought to assure the quality control in production and evaluate their application suitability that may employ in the pneumatic system in gamma facility

  4. Radiation cured silicone rubber articles

    International Nuclear Information System (INIS)

    DuPont, J.G.; Goodwin, P.A.

    1984-01-01

    A process for making radiation cured silicone rubber articles is disclosed wherein a hydroxyl-terminated polysilaxane having a molecular weight from about 50,000 to about 2,000,000, optionally modified by mixing with up to 85% of an end-stopped silicone rubber, is mixed with from about 10 to about 70 parts per hundred of rubber of a finely divided silica filler with a particle size in the reinforcing range and other inert fillers as determined by desired final properties; the composition so prepared is formed into the desired shape at room temperature; the article so formed is precured to improve the mechanical properties of the material with which it is made by exposure to ammonia gas, ammonium hydroxide, or to the vapors or solutions of a volatile amine at room temperature; and the precured article is irradiated with high energy electrons or gamma radiation to effect a permanent cure of the material from which the article is formed

  5. Strength of mortar containing rubber tire particle

    Science.gov (United States)

    Jusoh, M. A.; Abdullah, S. R.; Adnan, S. H.

    2018-04-01

    The main focus in this investigation is to determine the strength consist compressive and tensile strength of mortar containing rubber tire particle. In fact, from the previous study, the strength of mortar containing waste rubber tire in mortar has a slightly decreases compare to normal mortar. In this study, rubber tire particle was replacing on volume of fine aggregate with 6%. 9% and 12%. The sample were indicated M0 (0%), M6 (6%), M9 (9%) and M12 (12%). In this study, two different size of sample used with cube 100mm x 100mm x 100mm for compressive strength and 40mm x 40mm x 160mm for flexural strength. Morphology test was conducted by using Scanning electron microscopic (SEM) were done after testing compressive strength test. The concrete sample were cured for day 3, 7 and 28 before testing. Results compressive strength and flexural strength of rubber mortar shown improved compare to normal mortar.

  6. Antimicrobial and Osseointegration Properties of Nanostructured Titanium Orthopaedic Implants.

    Science.gov (United States)

    Jäger, Marcus; Jennissen, Herbert P; Dittrich, Florian; Fischer, Alfons; Köhling, Hedda Luise

    2017-11-13

    The surface design of titanium implants influences not only the local biological reactions but also affects at least the clinical result in orthopaedic application. During the last decades, strong efforts have been made to improve osteointegration and prevent bacterial adhesion to these surfaces. Following the rule of "smaller, faster, cheaper", nanotechnology has encountered clinical application. It is evident that the hierarchical implant surface micro- and nanotopography orchestrate the biological cascades of early peri-implant endosseous healing or implant loosening. This review of the literature gives a brief overview of nanostructured titanium-base biomaterials designed to improve osteointegration and prevent from bacterial infection.

  7. Effects of preparation process on performance of rubber modified asphalt

    Science.gov (United States)

    Liu, Hanbing; Luo, Guobao; Wang, Xianqiang; Jiao, Yubo

    2015-06-01

    The rational utilization of waste rubber tire is essential for the environmental protection. Utilizing rubber particles to modify asphalt can not only improve asphalt performance, but also help the recycling of waste materials. Considering the effect of different preparation process parameters on the performance of rubber modified asphalt, this paper analyzes the effects of the shear temperature, shear time and shear rate on the performance of rubber modified asphalt, and provided a reference for its preparation.

  8. Characterizing Tire Crumb Rubber for Exposure Assessment

    Science.gov (United States)

    Tire crumb rubber derived from recycled tires is widely used as infill material in synthetic turf fields in the United States. An estimated 95% of the over 12,000 installed fields in the U.S. use tire crumb rubber infill alone or mixed with sand or alternative materials. Concerns...

  9. Endurance test report of rubber sealing materials for the containment vessel

    International Nuclear Information System (INIS)

    Yamamoto, R.; Watanabe, K.; Hanashima, K.

    2015-01-01

    In the event of a nuclear power plant accident such as a core meltdown and a cooling system failure, the containment contains radioactive materials released from the reactor pressure vessel to reduce the activity of the radioactive materials and the effects of radiation in the vicinity of the plant. Since high sealing performance and high pressure resistance are required of the containment, a silicone or EPDM rubber gasket with high heat and radiation resistance is used for the sealing of the sealing boundary of the containment. In recent years, it has been shown that a large amount of steam is released into the containment in the case of a severe accident. Consequently, radiation resistance at high temperature as well as steam resistance is required of the rubber gasket placed at the sealing boundary. However, the steam resistance of silicone rubber is not necessarily as good as that of EPDM rubber. Therefore, it is necessary to evaluate the sealing characteristics of rubber gaskets in such a degrading environment in a severe accident. O. Kato et al. [1] conducted a study on the degradation status of rubber gaskets and their application limits at high temperature. However, few studies have evaluated rubber gaskets in high-temperature radiation and steam environments. In this study, we degraded silicone rubber and EPDM rubber used for the containment in the high-temperature radiation and steam environments expected to occur in a severe accident and evaluated the useful life of the rubber as a sealing material by estimating the change in its performance as a sealing material from the change in permanent compressive strain in the rubber. (author)

  10. Review of recent publications on bone implant interactions

    International Nuclear Information System (INIS)

    Moseke, C.

    2001-01-01

    Review of recent development in bone implant manufacturing and properties have been reported. The desirable implant mechanical, chemical, biological and surface properties have been discussed. Implant materials as well as their surface treatment and coating for achievement of best therapeutic results have been also presented

  11. Caltrans use of scrap tires in asphalt rubber products: a comprehensive review

    Directory of Open Access Journals (Sweden)

    Haiping Zhou

    2014-02-01

    Full Text Available The California Department of Transportation (Caltrans has been using scrap tire rubber in asphalt pavements since the 1970s in chip seals and the 1980s in rubberized hot mix asphalt(RHMA. Both the wet (field blend and dry processes were used in early trials. Caltrans has also used rubber modified binders containing both crumb rubber modifier and polymer modifier that could be manufactured at a refinery facility, a terminal blend wet process. Since the beginning of this century, Caltrans increased the use of scrap tire rubber in paving projects and invested considerable resources in developing technically sound, cost effective, and environmentally friendly strategies for using scrap tire rubber in roadway applications. By the end of year 2010, approximately 31%of all hot mix asphalt (HMA placed by Caltrans was rubberized HMA, roughly 1.2 million tons. Caltrans efforts in using asphalt rubber products were also demonstrated in its research and technology development. These included the construction of two full-scale field experiments, five warranty projects, and an accelerated pavement study using a heavy vehicle simulator. Additionally, terminal blend asphalt rubber and rubberized warm mix asphalts began to be experimented on trial basis. This paper provides a comprehensive review of Caltrans experience over four decades with asphalt rubber products. Current practices and future outlook are also discussed.

  12. Devulcanization of Waste Tire Rubber Using Amine Based Solvents and Ultrasonic Energy

    Directory of Open Access Journals (Sweden)

    Walvekar Rashmi

    2018-01-01

    Full Text Available This research project focuses on an alternative pathway of devulcanizing waste tire rubber by using amine based chemicals. Waste tire rubbers are known to be as toxic, non-degradable material due to their vulcanized crosslink carbon structure, and disposing of such waste could impose hazardous impacts on the environment. The current rubber recycling methods that are practiced today are rather uneconomical, non-environmentally friendly, and also producing recycled rubber with low quality due to the alteration in the main polymeric chains of waste rubber. This project aims to answer the question of whether the usage of amine can produce high quality rubber, where the properties of recycled rubber is almost the same as new/virgin rubber. With known potential of amine, it is a challenge for the chemical to selectively cleave the sulfur bonds without affecting the main carbon backbone chain in the rubber structure and diminishing much of the rubber properties. To study this research, amine-treated rubber must undergo devulcanisation process by applying heat and sonication energy. Then, the properties of the amine-treated rubber were determined through a set of characterization tests and analysis which are: gel content test to determine the weight of rubber before and after devulcanization, the thermogravimetric analysis (TGA to determine the thermal degradation and stability of rubber, and Fourier Transform Infrared Spectroscopy (FTIR to determine any structural change of the rubber. In this research so far, the first two preliminary analysis tests have been performed. The gel content test has shown that tertiary amine samples possessed a lower gel content (% of (77 – 63 %, compared to primary amine samples (falls within the range of 80%, as well as the TGA test in which tertiary amine samples degrade faster than primary amine samples (suggesting a higher degree of rubber structure breakdown. For each type of amine, the concertation of amine did

  13. Effect of Graphite on the Properties of Natural Rubber

    Directory of Open Access Journals (Sweden)

    Auda jabber Braihi

    2016-09-01

    Full Text Available Natural rubber-graphite composites (0, 1, 2, 3, 4 pphr graphite were prepared on a laboratory two-roll mill. Swelling measurements were used to evaluate the impacts of graphite on the properties of natural rubber. Swelling results showed that the volume fraction of natural rubber in the swollen gel, the interaction parameter, and the cross-link density decreased by increasing graphite loadings, while the average molecular weight of natural rubber between cross-links increased. Vulcanization results showed that only scorch time parameter increased with increasing graphite loadings, while other parameters (Max. torque, Min. torque, cure rate and cure rate index decreased. Both thermal and AC conductivities increased.

  14. Rheological Properties of Rubber Compounds with Finely Divided Carbon Additives

    Science.gov (United States)

    Shashok, Zh. S.; Prokopchuk, N. R.; Vishnevskii, K. V.; Krauklis, A. V.; Borisevich, K. O.; Borisevich, I. O.

    2018-01-01

    A study has been made of the influence of three different nanomaterials: of the starting material, and also of those functionalized by amine and oxygen-containing groups, on the properties of elastomer compositions based on rubbers for special purposes. As the elastomer matrix, use was made in one case of a rubber compound based on BNKS-18 butadiene-nitrile rubber and in the other, of a combination of two grades of butadiene-nitrile rubber (BNKS-18 + BNKS-28 in a 50:50 ratio), which differed by the amount of the bound nitrile of acrylic acid. To determine the degree of interaction between the additives and the elastomer matrix, the authors carried out multiple tests of the rubber compounds. The indices of plastoelastic properties of the rubber compounds and the qualitative characteristics of distribution of the filler (elastic modulus at small deformation amplitudes and the shear modulus under large deformation) and the difference in these indices (complex dynamic modulus) alike have been determined.

  15. Comparative Proteomics of Rubber Latex Revealed Multiple Protein Species of REF/SRPP Family Respond Diversely to Ethylene Stimulation among Different Rubber Tree Clones

    Directory of Open Access Journals (Sweden)

    Zheng Tong

    2017-05-01

    Full Text Available Rubber elongation factor (REF and small rubber particle protein (SRPP are two key factors for natural rubber biosynthesis. To further understand the roles of these proteins in rubber formation, six different genes for latex abundant REF or SRPP proteins, including REF138,175,258 and SRPP117,204,243, were characterized from Hevea brasiliensis Reyan (RY 7-33-97. Sequence analysis showed that REFs have a variable and long N-terminal, whereas SRPPs have a variable and long C-terminal beyond the REF domain, and REF258 has a β subunit of ATPase in its N-terminal. Through two-dimensional electrophoresis (2-DE, each REF/SRPP protein was separated into multiple protein spots on 2-DE gels, indicating they have multiple protein species. The abundance of REF/SRPP proteins was compared between ethylene and control treatments or among rubber tree clones with different levels of latex productivity by analyzing 2-DE gels. The total abundance of each REF/SRPP protein decreased or changed a little upon ethylene stimulation, whereas the abundance of multiple protein species of the same REF/SRPP changed diversely. Among the three rubber tree clones, the abundance of the protein species also differed significantly. Especially, two protein species of REF175 or REF258 were ethylene-responsive only in the high latex productivity clone RY 8-79 instead of in RY 7-33-97 and PR 107. Some individual protein species were positively related to ethylene stimulation and latex productivity. These results suggested that the specific protein species could be more important than others for rubber production and post-translational modifications might play important roles in rubber biosynthesis.

  16. FTIR spectra and mechanical strength analysis of some selected rubber derivatives

    Science.gov (United States)

    Gunasekaran, S.; Natarajan, R. K.; Kala, A.

    2007-10-01

    Rubber materials have wide range of commercial applications such as, infant diapers, famine hygiene products, drug delivery devices and incontinency products such as rubber tubes, tyres, etc. In the present work, studies on mechanical properties of some selected rubber materials viz., natural rubber (NR), styrene butadiene rubber (SBR), nitrile butadiene rubber (NBR) and ethylene propylene diene monomer (EPDM) have been carried out in three states viz., raw, vulcanized and reinforced. To enhance the quality of rubber elastomers, an attempt is made to prepare new elastomers called polyblends. In the present study an attempt is made to blend NR with NBR and with EPDM. We here report, a novel approach for the evaluation of various physico-mechanical properties such as mechanical strength, tensile strength, elongation and hardness. The method is simple, direct and fast and involves infrared spectral measurements for the evaluation of these properties. With the applications of modern infrared spectroscopy, the mechanical strength of these rubber materials have been analyzed by calculating the internal standards among the methyl and methylene group vibrational frequencies obtained from FTIR spectroscopy. Also the tensile strength measurements carried out by universal testing machine. The results pertaining physico-mechanical properties of the rubber derivatives undertaken in the present study obtained by IR-based method are in good agreement with data resulted from the standard methods.

  17. Study of the Properties of Polyurethane-waste Rubber Granulate Composites

    Institute of Scientific and Technical Information of China (English)

    W.W.Sulkowski; M.Moczy′ski; A.Sulkowska; A.Danch; J.Borek; S.Mistarz

    2007-01-01

    1 Results The production of rubber is very high and rises every year. Among other things it is directly connected with the growth of car production. Therefore, the processing of waste rubber and its management must be treated as a global problem. Used rubber may replace conventional fuel and, owing to its low price, can improve the economic effectiveness of combustion. Energy recovery by combustion of car tyres allows for rapid management of rubber waste. However, it is well-known that all kinds of wast...

  18. Buffing dust as a filler of carboxylated butadiene-acrylonitrile rubber and butadiene-acrylonitrile rubber.

    Science.gov (United States)

    Chronska, K; Przepiorkowska, A

    2008-03-01

    Buffing dust from chrome tanned leather is one of the difficult tannery wastes to manage. It is also hazardous to both human health and the environment. The scientific literature rarely reports studies on dust management, especially on its utilization as a filler for elastomers. In this connection we have made an attempt to use this leather waste as a filler for rubbers such as XNBR and NBR. The addition of the buffing dust to rubber mixes brought improvement in mechanical properties, and increase in resistance to thermal ageing as well as in electric conductivity and crosslink density of vulcalizates.

  19. Responses of rubber leaf phenology to climatic variations in Southwest China

    Science.gov (United States)

    Zhai, De-Li; Yu, Haiying; Chen, Si-Chong; Ranjitkar, Sailesh; Xu, Jianchu

    2017-11-01

    The phenology of rubber trees (Hevea brasiliensis) could be influenced by meteorological factors and exhibits significant changes under different geoclimates. In the sub-optimal environment in Xishuangbanna, rubber trees undergo lengthy periods of defoliation and refoliation. The timing of refoliation from budburst to leaf aging could be affected by powdery mildew disease (Oidium heveae), which negatively impacts seed and latex production. Rubber trees are most susceptible to powdery mildew disease at the copper and leaf changing stages. Understanding and predicting leaf phenology of rubber trees are helpful to develop effective means of controlling the disease. This research investigated the effect of several meteorological factors on different leaf phenological stages in a sub-optimal environment for rubber cultivation in Jinghong, Yunnan in Southwest China. Partial least square regression was used to quantify the relationship between meteorological factors and recorded rubber phenologies from 2003 to 2011. Minimum temperature in December was found to be the critical factor for the leaf phenology development of rubber trees. Comparing the delayed effects of minimum temperature, the maximum temperature, diurnal temperature range, and sunshine hours were found to advancing leaf phenologies. A comparatively lower minimum temperature in December would facilitate the advancing of leaf phenologies of rubber trees. Higher levels of precipitation in February delayed the light green and the entire process of leaf aging. Delayed leaf phenology was found to be related to severe rubber powdery mildew disease. These results were used to build predictive models that could be applied to early warning systems of rubber powdery mildew disease.

  20. Recycling of Gamma Irradiated Inner Tubes in Butyl Based Rubber Compound

    International Nuclear Information System (INIS)

    Karaagac, B.

    2006-01-01

    Crosslinked elastomeric materials, such as tyres are of great challenge concerning the environmental and ecological reasons. Ionizing radiation seems to offer unique opportunities to tackle the problem of recycling of polymers and rubbers on account of its ability to cause chain scission and/or cross-linking of polymeric materials. There is only limited amount of work reported on the irradiation-induced degradation of rubbers. Unlike the majority of the elastomers with high levels of unsaturation, butyl rubber exhibits significant degradation by ionizing radiation action. In this study, recycling of gamma irradiated inner tubes made of butyl rubber in butyl based rubber compounds was studied. Used inner tubes were irradiated with gamma rays in air at 100 and 120 kGy absorbed doses. The compatibility of irradiated inner tubes with virgin butyl rubber was first investigated. Gamma irradiated inner tube wastes were replaced with butyl rubber up to 15 phr in the compound recipe. Similar recipes were also prepared by using the same quantity of commercial butyl rubber crumbs devulcanized by conventional methods. The rheological and mechanical properties and carbon black dispersion degree for both types of compounds prepared by using inner tubes scraps and commercial butyl crumbs were measured and were compared to the values of virgin butyl rubber compound. It is well known that mechanical properties are deteriorated when rubber crumb is added to the virgin compound. It was observed that the decrease in the mechanical properties was much lower for the compounds prepared from the tubes irradiated at 120 kGy than irradiated at 100 kGy. The better mechanical properties were obtained for the compounds prepared by recycling of irradiated inner tubes at 120 kGy than the compounds prepared by using commercial butyl crumbs. Almost similar carbon black distributions were observed for the all compounds studied. It has been concluded that gamma irradiated inner tubes are compatible

  1. Soil methane and CO2 fluxes in rainforest and rubber plantations

    Science.gov (United States)

    Lang, Rong; Blagodatsky, Sergey; Goldberg, Stefanie; Xu, Jianchu

    2017-04-01

    Expansion of rubber plantations in South-East Asia has been a land use transformation trend leading to losses of natural forest cover in the region. Besides impact on ecosystem carbon stocks, this conversion influences the dynamics of greenhouse gas fluxes from soil driven by microbial activity, which has been insufficiently studied. Aimed to understand how land use change affects the soil CO2 and CH4 fluxes, we measured surface gas fluxes, gas concentration gradient, and 13C signature in CH4 and soil organic matter in profiles in a transect in Xishuangbanna, including a rainforest site and three rubber plantation sites with age gradient. Gas fluxes were measured by static chamber method and open chamber respiration system. Soil gases were sampled from installed gas samplers at 5, 10, 30, and 75cm depth at representative time in dry and rainy season. The soil CO2 flux was comparable in rainforest and old rubber plantations, while young rubber plantation had the lowest rate. Total carbon content in the surface soil well explained the difference of soil CO2 flux between sites. All sites were CH4 sinks in dry season and uptake decreased in the order of rainforest, old rubber plantations and young rubber plantation. From dry season to rainy season, CH4 consumption decreased with increasing CH4 concentration in the soil profile at all depths. The enrichment of methane by 13CH4 shifted towards to lowerδ13C, being the evidence of enhanced CH4 production process while net surface methane flux reflected the consumption in wet condition. Increment of CH4 concentration in the profile from dry to rainy season was higher in old rubber plantation compared to rainforest, while the shifting of δ13CH4 was larger in rainforest than rubber sites. Turnover rates of soil CO2 and CH4 suggested that the 0-5 cm surface soil was the most active layer for gaseous carbon exchange. δ13C in soil organic matter and soil moisture increased from rainforest, young rubber plantation to old

  2. Liquefaction of ground tire rubber at low temperature.

    Science.gov (United States)

    Cheng, Xiangyun; Song, Pan; Zhao, Xinyu; Peng, Zonglin; Wang, Shifeng

    2018-01-01

    Low-temperature liquefaction has been investigated as a novel method for recycling ground tire rubber (GTR) into liquid using an environmentally benign process. The liquefaction was carried out at different temperatures (140, 160 and 180 °C) over variable time ranges (2-24 h) by blending the GTR with aromatic oil in a range from 0 to 100 parts per hundred rubber (phr). The liquefied GTR was separated into sol (the soluble fraction of rubber which can be extracted with toluene) and gel fractions (the solid fraction obtained after extraction) to evaluate the reclaiming efficiency. It was discovered that the percentage of the sol fraction increased with time, swelling ratio and temperature. Liquefied rubber was obtained with a high sol fraction (68.34 wt%) at 140 °C. Simultaneously, separation of nano-sized carbon black from the rubber networks occurred. The separation of carbon black from the network is the result of significant damage to the cross-linked-network that occurs throughout the liquefaction process. During liquefaction, a competitive reaction between main chain scission and cross-link bond breakage takes place. Copyright © 2017 Elsevier Ltd. All rights reserved.

  3. Properties of concrete containing scrap-tire rubber--an overview.

    Science.gov (United States)

    Siddique, Rafat; Naik, Tarun R

    2004-01-01

    Solid waste management is one of the major environmental concerns in the United States. Over 5 billion tons of non-hazardous solid waste materials are generated in USA each year. Of these, more than 270 million scrap-tires (approximately 3.6 million tons) are generated each year. In addition to this, about 300 million scrap-tires have been stockpiled. Several studies have been carried out to reuse scrap-tires in a variety of rubber and plastic products, incineration for production of electricity, or as fuel for cement kilns, as well as in asphalt concrete. Studies show that workable rubberized concrete mixtures can be made with scrap-tire rubber. This paper presents an overview of some of the research published regarding the use of scrap-tires in portland cement concrete. The benefits of using magnesium oxychloride cement as a binder for rubberized concrete mixtures are also presented. The paper details the likely uses of rubberized concrete.

  4. Degrading radiation effects on properties of bromobutyl rubber compounds

    Energy Technology Data Exchange (ETDEWEB)

    Scagliusi, Sandra R.; Cardoso, Elisabeth C.L.; Pozenato, Cristina A.; Lugao, Ademar B., E-mail: srscagliusi@ipen.br [Instituto de Pesquisas Energeticas e Nucleares (IPEN/CNEN-SP), Sao Paulo, SP (Brazil)

    2013-07-01

    The understanding of chemistry involved in degradation induced radiation is becoming more and more relevant in the re-use of polymeric materials, as well in beneficial radiation uses. Degrading radiation effects have been considered from viewpoint of controlled degradation for isoprene/isobutene in rubbers for recycling purposes. Bromobutyl rubber (BIIR) is an isobutylene/isoprene copolymer comprising 1.9 to 2.1% bromine and has a lot of applications including in tires air-chambers. In this work there were evaluated gamma-irradiation effects for re-use or recycling objectives in elastomeric bromobutyl compositions irradiated at 5, 15, 25, 50, 100,150 and 200 kGy. Mechanical properties, hardness and swelling were assessed in non-vulcanized and vulcanized rubber, non-irradiated and irradiated at different doses. The major gamma radiation effect in butyl rubber is the generation of free radicals along changes in mechanical properties. Irradiation effects in bromobutyl rubber compounds were comprehensively investigated, demonstrated and discussed. (author)

  5. Degrading radiation effects on properties of bromobutyl rubber compounds

    International Nuclear Information System (INIS)

    Scagliusi, Sandra R.; Cardoso, Elisabeth C.L.; Pozenato, Cristina A.; Lugao, Ademar B.

    2013-01-01

    The understanding of chemistry involved in degradation induced radiation is becoming more and more relevant in the re-use of polymeric materials, as well in beneficial radiation uses. Degrading radiation effects have been considered from viewpoint of controlled degradation for isoprene/isobutene in rubbers for recycling purposes. Bromobutyl rubber (BIIR) is an isobutylene/isoprene copolymer comprising 1.9 to 2.1% bromine and has a lot of applications including in tires air-chambers. In this work there were evaluated gamma-irradiation effects for re-use or recycling objectives in elastomeric bromobutyl compositions irradiated at 5, 15, 25, 50, 100,150 and 200 kGy. Mechanical properties, hardness and swelling were assessed in non-vulcanized and vulcanized rubber, non-irradiated and irradiated at different doses. The major gamma radiation effect in butyl rubber is the generation of free radicals along changes in mechanical properties. Irradiation effects in bromobutyl rubber compounds were comprehensively investigated, demonstrated and discussed. (author)

  6. HERBERT HOOVER, GREAT BRITAIN, AND THE RUBBER CRISIS, 1923-1926

    Directory of Open Access Journals (Sweden)

    Silvano A. Wueschner

    2000-01-01

    Full Text Available This paper examines the controversy arising out of Great Britain’s decision to implement the Stevenson plan. It examines, in particular, the role played by Herbert Hoover, both behind the scenes and in an effort to affect the repeal of the Stevenson scheme and at the same time to encourage and support the development of new sources of rubber under the control of American producers. During the period 1920-1922 rubber producing countries were confronted by the specter of overproduction. The existence of even a short term oversupply coupled with the business slump, a reaction from the war, led to a decline in the price of rubber. British producers succeeded in inducing the British Colonial authorities to support a scheme whereby rubber exports would be regulated in order to bring about an increase in the price of rubber. This plan, developed by the Stevenson Committee, called for a small minimum tax on all exports. Moreover, it soughtto limit production by establishing a quota based on the actual production of rubber during the 1919-1920 growing season. A progressive tax was applied to exports beyond standard production. American reaction to the scheme was varied. Secretary of Commerce Hoover, while publicly stating that the price of rubber had been low and was supportive of efforts to regulate production, behind the scenes showed a great deal of concern about the actions of the British government in regulating a commodity of which the United States was the single largest consumer. He was also linked, by some, to the idea that Great Britain sought to pay its war debt to the United States through the application of this tax. Much was made in American newspapers and the British press about Hoover’s criticism of British rubber restrictions. He was not opposed to regulating the supply of rubber, but only to the involvement of a government in the process, especially when it affected American producers and consumers. In response he proposed a scheme

  7. A novel implantation model for evaluation of bone healing response to dental implants: the goat iliac crest.

    NARCIS (Netherlands)

    Schouten, C.; Meijer, G.J.; Beucken, J.J.J.P van den; Spauwen, P.H.M.; Jansen, J.A.

    2010-01-01

    OBJECTIVES: Despite the availability of numerous animal models for testing the biological performance of dental and orthopedic implants, the selection of a suitable model is complex. This paper presents a new model for objective and standardized evaluation of bone responses to implants using the

  8. STUDY ON HEAT DYNAMIC LOADING OF RUBBER

    Directory of Open Access Journals (Sweden)

    T. I. Igumenova

    2015-01-01

    Full Text Available A number of studies on heat buildup in tire rubber surface scan method samples using a thermal imaging camera. Investigated the exothermic chemical reaction mechanical destruction rubber when loading designs permanent cyclic stretching with deformation of the working zone 50%. Percentage of deformation of the working zone was chosen on the basis of the actual data on the stretch-compression zone "Rusk" tires, which is the maximum level difference of deformation during run-in. Experiment plan provided for periodic relaxation samples of at least 72 hours for more accurate simulation of operation process of structural products. Created and processed data on temperature changes in samples for bar and line profile for rubber compounds with the introduction of nanomodifiers (fulleren technical carbon in comparison with the control sample without him. The data obtained reflect the nature of heat depending on the composition of the compound. Identified common patterns of thermal nature of physico-chemical process mechanical destruction rubbers. For rubber with nanomodifikatorom there has been an increase in the temperature interval reaction from a minimum to a maximum 2 degrees that is also linked to the rise in the average temperature of the reaction on the histogram also at 2-3 degrees of deformation under the same conditions and the level of cyclic loading. However, the temperature in the control sample that is associated with the beginning of the formation of hardened rubber structures, economies of Mallinz-Petrikeev, occurs with delay twice compared with modified Fullerenes. Measurement of physic-mechanical indicators selected in the course of testing of samples showed the beginning of formation of structure with increased strength of samples in the sample temperature zone that corresponds to the thermal effect of èndotermičeskomu recombination reactions of macromolecules.

  9. Air Abrasive Disinfection of Implant Surfaces in a Simulated Model of Peri-Implantitis

    Science.gov (United States)

    2016-06-01

    may be higher in patients diagnosed with periodontal disease, systemic chronic disease such as diabetes or patients who smoke tobacco.9,10 One of...flora associated with peri-implantitis is similar to that found in chronic periodontitis .14 Gram-positive, facultative bacteria are normally...9):1490-5. 20. Heitz-Mayfield LJ, Lang NP. Comparative biology of chronic and aggressive periodontitis vs. peri-implantitis. Periodontol 2000

  10. Mechanical Properties of Graphene-Rubber Nanocomposites

    Science.gov (United States)

    Anhar, N. A. M.; Ramli, M. M.; Hambali, N. A. M. A.; Aziz, A. A.; Mat Isa, S. S.; Danial, N. S.; Abdullah, M. M. A. B.

    2017-11-01

    This research focused on development of wearable sensor device by using Prevulcanized Natural Rubber (PV) and Epoxidized Natural Rubber (ENR 50) latex incorporated with graphene oxide (GO), graphene paste, graphene powder and reduced graphene oxide (rGO) powder. The compounding formulation and calculation were based on phr (parts per hundred rubber) and all the samples were then tested for mechanical properties using Instron 5565 machine. It was found that the sonication effects on tensile strength may have better quality of tensile strength compared to non-sonicated GO. For PV incorporate GO, the optimum loading was best determined at loading 1.5 phr with or without sonication and similar result was recorded for PV/G. For ENR 50 incorporate graphene paste and rGO powder nanocomposite shows the best optimum was at 3.0 phr with 24 hours’ sonication.

  11. Chemi-microbial processing of waste tire rubber: A project overview

    International Nuclear Information System (INIS)

    Romine, R.A.; Snowden-Swan, L.

    1993-12-01

    PNL is developing a method to use thiophillic microorganisms to devulcanize (biodesulfurize) the surface of ground rubber particles, which will improve the bonding and adhesion of the ground tire rubber into the virgin tire rubber matrix. The Chemi-microbial processing approach, introduced in this paper, is targeted at alleviating the waste tire problem in an environmentally conscious manner; it may also be applied to improve asphaltic materials and rubber and polymeric wastes to facilite their recycling. This paper outlines the logic and technical methods that will be used

  12. Utilization of waste tire rubber in manufacture of oriented strandboard.

    Science.gov (United States)

    Ayrilmis, Nadir; Buyuksari, Umit; Avci, Erkan

    2009-09-01

    Some physical and mechanical properties of oriented strandboards (OSBs) containing waste tire rubber at various addition levels based on the oven-dry strand weight, using the same method as that used in the manufacture of OSB. Two resin types, phenol-formaldehyde (PF) and polyisocyanate, were used in the experiments. The manufacturing parameters were: a specific gravity of 0.65 and waste tire rubber content (10/90, 20/80 and 30/70 by wt.% of waste tire rubber/wood strand). Average internal bond values of PF-bonded OSB panels with rubber chips were between 17.6% and 48.5% lower than the average of the control samples while polyisocyanate bonded OSBs were 16.5-50.6%. However, water resistance and mechanical properties of OSBs made using polyisocyanate resin were found to comply with general-purpose OSB minimum property requirements of EN 300 Type 1 (1997) values for use in dry conditions at the lowest tire rubber loading level (10%) based on the oven-dry panel weight. The tire rubber improved water resistance of the OSB panel due to its almost hydrophobic property. Based on the findings obtained from this study, we concluded that waste tire rubber could be used for general-purpose OSB manufacturing up to 10% ratio based on the oven-dry panel weight.

  13. their use as Accelerator in Curing Process of Rubber Compounds

    Directory of Open Access Journals (Sweden)

    S. taghvaee

    2007-06-01

    Full Text Available In some special cases, rubber compounds with high amounts of unsaturated elastomer are recommended with organic sulfur donors instead of mineral sulfurs. In this condition, activated sulfur is produced in situ and curingprocess is facilitated without accelerators. Organic sulfur donor compounds have low thermal stability and in the vulcanization temperature produce free and activated sulfurs. The advantages of these compounds are:1. High effectiveness of curing agent in low quantities in rubber compounds manufacturing.2. Producing activated sulfurs in controlled condition and avoiding the over curing of rubber compounds.In this report the novel synthesis of some derivatives of diamino-disulfides which can be applied as sulfur donors in vulcanization of special rubber compounds is introduced. The key process is reaction of sulfurmonochloride with amines in petroleum ether as solvent in low temperature. Dithio-dimorpholine(DTDM, dithio-dipipyridyl (DTDP, dithio-bis dibutylamine (DTBDB and dithio-bisdiisopropyl amine (DTBDI were prepared according to this method. All products thus obtained were characterized by 1H and 13C-NMR spectroscopies. The effects of accelerating and sulfur donoring of all prepared agents were detected in rubber compounds with natural and synthetic rubber bases. All physical, chemical, reological and mechanical properties of rubber compounds based on prepared sulfur donors were characterized.

  14. The optimum content of rubber ash in concrete: flexural strength

    Science.gov (United States)

    Senin, M. S.; Shahidan, S.; Shamsuddin, S. M.; Ariffin, S. F. A.; Othman, N. H.; Rahman, R.; Khalid, F. S.; Nazri, F. M.

    2017-11-01

    Discarded scrap tyres have become one of the major environmental problems nowadays. Several studies have been carried out to reuse waste tires as an additive or sand replacement in concrete with appropriate percentages of tire rubber, called as rubberized concrete to solve this problem. The main objectives of this study are to investigate the flexural strength performance of concrete when adding the rubber ash and also to analyse the optimum content of rubber ash in concrete prisms. The performance total of 30 number of concrete prisms in size of 100mm x 100mm x 500 mm were investigated, by partially replacement of rubber ash with percentage of 0%, 3%, 5%, 7% and 9% from the volume of the sand. The flexural strength is increased when percentage of rubber ash is added 3% from control concrete prism, RA 0 for both concrete prism age, 7 days and 28 days with value 1.21% and 0.976% respectively. However, for RA 5, RA 7 and RA 9, the flexural strength was decreased compared to the control for both age, 7 days and 28 days. In conclusion, 3% is the optimum content of rubber ash in concrete prism for both concrete age

  15. Synthesis, characterization and degradation behavior of admicelled polyacrylate-natural rubber

    International Nuclear Information System (INIS)

    Pongpilaipruet, Angkana; Magaraphan, Rathanawan

    2015-01-01

    In order to improve weatherability of the cured natural rubber, the novel introduction of good ozone resistant polymers such as polyacrylates (poly(methyl acrylate) (PMA) or poly(methyl methacrylate) (PMMA)) into natural rubber (NR) by admicellar polymerization was investigated in this work. The admicellar polymerization to synthesize polyacrylate layer over the surface of NR latex particles was performed with varying monomer type (PMA and PMMA) and content (50 and 100 mM). The admicelled PMMA showed higher molecular weight than PMA. Fourier transform infrared spectra of the admicellar synthesized natural rubbers exhibited characteristic peaks of those polyacrylates. Micrographs from transmission electron and field emission scanning electron microscopes (FE-SEM) revealed the coatings of PMA and PMMA over the rubber particles, suggesting a core-shell structure. Thermogravimetric analysis revealed that the admicelled rubbers not only showed an improvement in heat stability but also a single decomposition temperature. After vulcanization, FE-SEM results showed the cured admicelled rubbers had phase transformation from core-shell to phase separation (aggregate domains of polyacrylate-rich phase) with smooth interface. This agreed well to their one glass transition temperature (∼−48 °C) which indicated good miscibility between NR and each polyacrylate. The cracks generated after exposure to ozone found in the admicelled rubbers were smaller than those in NR, suggesting better ozone resistance was achieved. Increasing monomer concentration led to less cracks or much better ozone resistance. Furthermore, changes in mechanical properties after ozone exposure of the admicelled PMA-NR were less than those of the admicelled PMMA-NR (having the same shell content) and the NR, respectively. - Highlights: • We use admicellar technique to add polyacrylates to NR in form of core-shell rubber. • This core-shell structure was physically formed as seen by the phase

  16. Synthesis, characterization and degradation behavior of admicelled polyacrylate-natural rubber

    Energy Technology Data Exchange (ETDEWEB)

    Pongpilaipruet, Angkana; Magaraphan, Rathanawan, E-mail: rathanawan.k@chula.ac.th

    2015-06-15

    In order to improve weatherability of the cured natural rubber, the novel introduction of good ozone resistant polymers such as polyacrylates (poly(methyl acrylate) (PMA) or poly(methyl methacrylate) (PMMA)) into natural rubber (NR) by admicellar polymerization was investigated in this work. The admicellar polymerization to synthesize polyacrylate layer over the surface of NR latex particles was performed with varying monomer type (PMA and PMMA) and content (50 and 100 mM). The admicelled PMMA showed higher molecular weight than PMA. Fourier transform infrared spectra of the admicellar synthesized natural rubbers exhibited characteristic peaks of those polyacrylates. Micrographs from transmission electron and field emission scanning electron microscopes (FE-SEM) revealed the coatings of PMA and PMMA over the rubber particles, suggesting a core-shell structure. Thermogravimetric analysis revealed that the admicelled rubbers not only showed an improvement in heat stability but also a single decomposition temperature. After vulcanization, FE-SEM results showed the cured admicelled rubbers had phase transformation from core-shell to phase separation (aggregate domains of polyacrylate-rich phase) with smooth interface. This agreed well to their one glass transition temperature (∼−48 °C) which indicated good miscibility between NR and each polyacrylate. The cracks generated after exposure to ozone found in the admicelled rubbers were smaller than those in NR, suggesting better ozone resistance was achieved. Increasing monomer concentration led to less cracks or much better ozone resistance. Furthermore, changes in mechanical properties after ozone exposure of the admicelled PMA-NR were less than those of the admicelled PMMA-NR (having the same shell content) and the NR, respectively. - Highlights: • We use admicellar technique to add polyacrylates to NR in form of core-shell rubber. • This core-shell structure was physically formed as seen by the phase

  17. Model fire tests on polyphosphazene rubber and polyvinyl chloride (PVC)/nitrile rubber foams

    Science.gov (United States)

    Widenor, W. M.

    1978-01-01

    A video tape record of model room fire tests was shown, comparing polyphosphazene (P-N) rubber and polyvinyl chloride (PVC)/nitrile rubber closed-cell foams as interior finish thermal insulation under conditions directly translatable to an actual fire situation. Flashover did not occur with the P-N foam and only moderate amounts of low density smoke were formed, whereas with the PVC/nitrile foam, flashover occurred quickly and large volumes of high density smoke were emitted. The P-N foam was produced in a pilot plant under carefully controlled conditions. The PVC/nitrile foam was a commercial product. A major phase of the overall program involved fire tests on P-N open-cell foam cushioning.

  18. Mechanical properties of concrete containing a high volume of tire-rubber particles.

    Science.gov (United States)

    Khaloo, Ali R; Dehestani, M; Rahmatabadi, P

    2008-12-01

    Due to the increasingly serious environmental problems presented by waste tires, the feasibility of using elastic and flexible tire-rubber particles as aggregate in concrete is investigated in this study. Tire-rubber particles composed of tire chips, crumb rubber, and a combination of tire chips and crumb rubber, were used to replace mineral aggregates in concrete. These particles were used to replace 12.5%, 25%, 37.5%, and 50% of the total mineral aggregate's volume in concrete. Cylindrical shape concrete specimens 15 cm in diameter and 30 cm in height were fabricated and cured. The fresh rubberized concrete exhibited lower unit weight and acceptable workability compared to plain concrete. The results of a uniaxial compressive strain control test conducted on hardened concrete specimens indicate large reductions in the strength and tangential modulus of elasticity. A significant decrease in the brittle behavior of concrete with increasing rubber content is also demonstrated using nonlinearity indices. The maximum toughness index, indicating the post failure strength of concrete, occurs in concretes with 25% rubber content. Unlike plain concrete, the failure state in rubberized concrete occurs gently and uniformly, and does not cause any separation in the specimen. Crack width and its propagation velocity in rubberized concrete are lower than those of plain concrete. Ultrasonic analysis reveals large reductions in the ultrasonic modulus and high sound absorption for tire-rubber concrete.

  19. Radiation vulcanization of natural rubber latex sensitized with commercial gases

    International Nuclear Information System (INIS)

    Chirinos, H.; Lugao, A.

    2002-01-01

    The industrial activities using natural rubber latex are fully compatible with rural areas in Amazon and other places in Brazil, as well as in other tropical countries. However the classical sulfur vulcanization presents many occupational problems for the workers in rural areas. Radiation vulcanization of natural rubber latex is a much more friendly process as sulfur compounds are not needed for crosslinking, although chemicals as acrylate monomers, particularly multifunctional acrylates are still used as sensitizers for radiation processes. Two commercial gases, acetylene and butadiene, were selected as sensitizers for the radiation vulcanization of natural rubber latex instead of acrylates. These gases accelerate the crosslinking rates of the cure process and lower the radiation dose required to achieve vulcanization of natural rubber latex and improve the mechanical properties to reduce the tackiness of rubber goods. (author)

  20. Radiation vulcanization of natural rubber latex sensitized with commercial gases

    Energy Technology Data Exchange (ETDEWEB)

    Chirinos, H.; Lugao, A. [Instituto de Pesquisas Energeticas e Nucleares (IPEN), Sao Paulo, SP (Brazil)

    2002-07-01

    The industrial activities using natural rubber latex are fully compatible with rural areas in Amazon and other places in Brazil, as well as in other tropical countries. However the classical sulfur vulcanization presents many occupational problems for the workers in rural areas. Radiation vulcanization of natural rubber latex is a much more friendly process as sulfur compounds are not needed for crosslinking, although chemicals as acrylate monomers, particularly multifunctional acrylates are still used as sensitizers for radiation processes. Two commercial gases, acetylene and butadiene, were selected as sensitizers for the radiation vulcanization of natural rubber latex instead of acrylates. These gases accelerate the crosslinking rates of the cure process and lower the radiation dose required to achieve vulcanization of natural rubber latex and improve the mechanical properties to reduce the tackiness of rubber goods. (author)

  1. Radiation sterilization of polymeric implant materials

    International Nuclear Information System (INIS)

    Bruck, S.D.; Mueller, E.P.

    1988-01-01

    High-energy irradiation sterilization of medical devices and implants composed of polymeric biomaterials that are in contact with tissue and/or blood, may adversely affect their long-term mechanical and/or biological performance (tissue and/or blood compatibility). Since many polymeric implants may contain trace quantities of catalysts and/or other additives, the effect of high-energy radiation on these additives, and possible synergistic effects with the polymer chains under the influence of high-energy radiation, must be considered. It is essential to indicate whether polymeric implants are used in short-term (acute) or long-term (chronic) applications. Relatively small changes in their physicochemical, mechanical, and biological properties may be tolerable in the short term, whereas similar changes may lead to catastrophic failures in long-term applications. Therefore, polymeric implants which are to be sterilized by high-energy irradiation should be carefully evaluated for long-term property changes which may be induced by the radiation

  2. Porous metal for orthopedics implants

    OpenAIRE

    Matassi, Fabrizio; Botti, Alessandra; Sirleo, Luigi; Carulli, Christian; Innocenti, Massimo

    2013-01-01

    Porous metal has been introduced to obtain biological fixation and improve longevity of orthopedic implants. The new generation of porous metal has intriguing characteristics that allows bone healing and high osteointegration of the metallic implants. This article gives an overview about biomaterials properties of the contemporary class of highly porous metals and about the clinical use in orthopaedic surgery.

  3. Ultraviolet curing of acrylated liquid natural rubber for surface coating application

    Directory of Open Access Journals (Sweden)

    Kannikar Kwanming

    2009-01-01

    Full Text Available Ultraviolet curable acrylated liquid natural rubber was prepared by grafting of photosensitive molecule onto liquid natural rubber for surface coating application. The liquid natural rubber (LNR was firstly obtained by degradation of natural rubber latex with hydrogen peroxide and cobalt acetylacetonate at 65oC for 72 hrs. The preparation of acrylated natural rubber was carried out by the reaction of acrylic acid and epoxidized liquid natural rubber (ELNR prior obtained from LNR with formic acid and hydrogen peroxide in the ratio of 2:1 by weight in toluene at 80oC for 6, 9, 12, 18, and 24 hrs. It was found that the percentage of acrylate grafted onto liquid natural rubber depended on the reaction time. Surface coating was performed by using acrylated liquid natural rubber and 1,6-hexanediol diacrylate (HDDA or tripropylene glycol diacrylate (TPGDA as a crosslinker and Irgarcure 184 or Irgarcure 651 as a photoinitiator under UV exposure for 30, 60, and 90 seconds. The hardness test of cured products was investigated using the Pencil hardness test at pencil level of 2B to 6H. It was found that the highest hardness of surface coating was at pencil level of 4H for the product using TPGDA and Irgacure 651 in the ratio of 80:10 parts per hundred of rubber (phr. The cured products were able to resist to 2% H2SO4 and distilled water for more than 24 hrs.

  4. Experimental Investigation on Damping Property of Coarse Aggregate Replaced Rubber Concrete

    Science.gov (United States)

    Sugapriya, P.; Ramkrishnan, R.; Keerthana, G.; Saravanamurugan, S.

    2018-02-01

    Rubber has good damping and vibrational characteristics and can reduce cracking significantly due to its elastic nature. This property of rubber can be incorporated in concrete to control vibrations and create better pavements. Crumb Rubber on being dumped in landfills has serious repercussions and causes soil and land pollution. An innovative use of waste tires is shredding them into small pieces and using them as a replacement for coarse aggregate. Crumb rubber is obtained by chopping scrap tires, and in this study it was added in two different sets named SET 1 - Treated Crumb Rubber and concrete, and SET 2 - Treated Crumb rubber with Ultra Fine GGBS as admixture in concrete. Coarse aggregate replaces Rubber in each of the 2 SET’s in proportions of 5, 10, 15 and 20%. Properties like Compressive Strength, Young’s Modulus, Direct and Semi direct Ultrasonic Pulse Velocity, Sorptivity, Damping ratio and Frequency were found out. Deformation and mode shape were studied with modal analysis and static analysis by applying a uniform pressure corresponding to the highest compressive strength of the slab, using ANSYS.

  5. Rubber-like poly(vinyl alcohol) gel

    Energy Technology Data Exchange (ETDEWEB)

    Nambu, Masao (Nippon Oil Co. Ltd., Yokohama (Japan). Central Technical Research Lab.)

    1990-09-01

    Anomalous poly (vinyl alcohol) gel has been found in our laboratory since 1980. The gel is prepared by repeated freezing (or freeze-dehydration) of aqueous poly (vinyl alcohol). Experiments establish the fact that anomalous gel is never produced in the course of freezing, but during sustained thawing the gelation does occur. Moreover, it was found that the softening point of the gel increases at 37degC. It is assumed that crystal nuclei are generated on freezing, then on thawing, some of them grow to very fine crystals which act as polymer network-knots (cross-linking). Additional freezing provide other seeds, which grow similarly, and these are accumulated until rubber-like gel is produced. The gel was always water-resistant at 37degC, and the potassium permanganate consumption of the extracted water layer remained far below the official restricted value for medical materials. The gel can be sterilized with gamma-rays or chlorhexidine. Moreover, it satisfies the official standards of acute toxicity, pyrogen, intracutaneous reaction, hemolyzation, and intracorporeal implantation, respectively. Applications to adhesion-preventing membrane (for joint or pericardium), tamponade (for jaw defects), electrode (for electroretinogram or artificial inner ear), artificial denture base and phantoms for magnetic resonance imaging were examined. (author) 54 refs.

  6. Laboratory Evaluation of Ground Tire Rubber in Stone Mastic Asphalt

    Directory of Open Access Journals (Sweden)

    R. Muniandy

    2004-12-01

    Full Text Available Stone mastic asphalt (SMA is a gap-graded mix whereby stiffer asphalt cement is required to bind the stone matrix or arrangement of stones together. Although various asphalt additives are traditionally available, the use of rubber crumbs in SMA is still a new rresearch endeavor. Many countries around the world are facing serious problems on what to do with reject or discarded tires. In the present study, commercial truck tires, containing 70% natural rubber, were ground and pre-blended in 80-100 penetration asphalt for use in SMA mixtures. An assessment was made of the laboratory performance of rubberized SMA in terms of stability, resilent modulus, dynamic creep and tensile strength ratio. It was observed that the performance of SMA with ground tire rubber was for superior as compared to SMA mix with unmodified asphalt. Sulfur and Styrene Butadeline Rubber (SBR were used in rubberized SMA mixes as additives to test the sensitivity of SMA mixtures. As standard practice a 0.3% newly developed cellulose oil palm fiber was used in SMA to minimize the asphalt drain-down effects.

  7. Improved properties of dissimilar rubber-rubber blends using plasma polymer encapsulated curatives : a novel surface modification method to improve co-vulcanization

    NARCIS (Netherlands)

    Guo, R.

    2009-01-01

    In industrial applications, different rubber types are often blended to fine-tune or optimize the property portfolio required for successful performance of articles. Considering the complexity of a rubber blend compound, wherein numerous additives are involved, vulcanization or cure mismatch often

  8. Strength and microstructure characteristics of the recycled rubber tire-sand mixtures as lightweight backfill.

    Science.gov (United States)

    Zhang, Tao; Cai, Guojun; Duan, Weihong

    2018-02-01

    The disposal of scrap rubber tires has induced critical environmental issue worldwide due to the rapid increase in the number of vehicles. Recycled scrap tires as a construction material in civil engineering have significant environmental benefits from a waste management perspective. A systematic study that deals with strength and microstructure characteristics of the rubber-sand mixtures is initiated, and mechanical response of the mixtures is discussed in this investigation. Experiments were conducted to evaluate the effects of rubber fraction on the basic properties including mass density (ρ), stress-strain characteristics, shear strength, and unconfined compression strength (q u ) of the rubber-sand mixtures. Additionally, scanning electron microscopy (SEM) was carried out to reveal the microstructure characteristics of the mixtures with various rubber fractions. A discussion on the micromechanics of the mixtures also was conducted. This study demonstrates that the ρ, friction angle, and q u decrease linearly with an increase in rubber fraction, whereas shear strain at peak increases. The stress-strain characteristics of the rubber-sand mixtures shift from brittle to ductile as the rubber fraction increase. These changes are attributed to remarkably lower stiffness and higher compressibility of the rubber particle compared with those of the conventional mineral aggregates. With an increase in the rubber fraction, the mechanical response of rubber-sand mixtures exhibits two types: sand-like material and rubber-like material. Rubber particle possesses the capacity to prevent the contacted sand particles from sliding at lower rubber fraction, whereas it transmits the applied loadings as the rubber fraction increased. This outcome reinforces the practicability of using recycled rubber tire-sand mixtures as a lightweight backfill in subbase/base applications.

  9. A review on fatigue life prediction methods for anti-vibration rubber materials

    Directory of Open Access Journals (Sweden)

    Xiaoli WANG

    2016-08-01

    Full Text Available Anti-vibration rubber, because of its superior elasticity, plasticity, waterproof and trapping characteristics, is widely used in the automotive industry, national defense, construction and other fields. The theory and technology of predicting fatigue life is of great significance to improve the durability design and manufacturing of anti-vibration rubber products. According to the characteristics of the anti-vibration rubber products in service, the technical difficulties for analyzing fatigue properties of anti-vibration rubber materials are pointed out. The research progress of the fatigue properties of rubber materials is reviewed from three angles including methods of fatigue crack initiation, fatigue crack propagation and fatigue damage accumulation. It is put forward that some nonlinear characteristics of rubber under fatigue loading, including the Mullins effect, permanent deformation and cyclic stress softening, should be considered in the further study of rubber materials. Meanwhile, it is indicated that the fatigue damage accumulation method based on continuum damage mechanics might be more appropriate to solve fatigue damage and life prediction problems for complex rubber materials and structures under fatigue loading.

  10. Time series analysis of the behavior of brazilian natural rubber

    Directory of Open Access Journals (Sweden)

    Antônio Donizette de Oliveira

    2009-03-01

    Full Text Available The natural rubber is a non-wood product obtained of the coagulation of some lattices of forest species, being Hevea brasiliensis the main one. Native from the Amazon Region, this species was already known by the Indians before the discovery of America. The natural rubber became a product globally valued due to its multiple applications in the economy, being its almost perfect substitute the synthetic rubber derived from the petroleum. Similarly to what happens with other countless products the forecast of future prices of the natural rubber has been object of many studies. The use of models of forecast of univariate timeseries stands out as the more accurate and useful to reduce the uncertainty in the economic decision making process. This studyanalyzed the historical series of prices of the Brazilian natural rubber (R$/kg, in the Jan/99 - Jun/2006 period, in order tocharacterize the rubber price behavior in the domestic market; estimated a model for the time series of monthly natural rubberprices; and foresaw the domestic prices of the natural rubber, in the Jul/2006 - Jun/2007 period, based on the estimated models.The studied models were the ones belonging to the ARIMA family. The main results were: the domestic market of the natural rubberis expanding due to the growth of the world economy; among the adjusted models, the ARIMA (1,1,1 model provided the bestadjustment of the time series of prices of the natural rubber (R$/kg; the prognosis accomplished for the series supplied statistically adequate fittings.

  11. Application of gamma irradiation for incorporation of rubber powder in the formulations

    International Nuclear Information System (INIS)

    Kiyan, Ludmila Y.P.; Lugao, Ademar B.; Parra, Duclerc F.; Zaharescu, Traian

    2013-01-01

    The aim of this paper was to study the behavior of rubber recycle, in powder form of rubber industry. It was used EPDM rubber powder. The rubber powder was irradiated and used directly in classical formulations of rubber vulcanizate. The master-batch processed material was irradiated at doses of 50, 100 and 150kGy in 60 Co source at 5kGy s -1 rate, at room temperature. Gamma radiation created active sites devulcanization for further integration of the material (rubber powder) with facilities in formulations of commercial use. The processes were compared and their products were characterized by analytical methods of the physical properties such as tensile strength, elongation, hardness, rheology and abrasion tests. (author)

  12. Preparation of Natural Rubber (NR) Based Nano-Sized Materials Using Sol-Gel Technique

    International Nuclear Information System (INIS)

    Dahlan Mohd; Mahathir Mohamed

    2011-01-01

    The objectives of this project are to prepare nano-sized natural rubber-based hybrid coating material by sol-gel technique; to explore the possibility of producing ENR-Si (epoxidized natural rubber-silica) cramer with toughening effects; and to use it in radiation curing of surface coating. Since early 1960s Malaysia has introduced various forms of value-added natural rubber such as Standard Malaysian Rubber (SMR), methylmethacrylate-grafted natural rubber (MG rubber), followed by liquid natural rubber and epoxidized natural rubber (ENR). Products such as liquid epoxidized natural rubber acrylate (LENRA) and thermoplastic natural rubber (TPNR) are still on-going research projects in Nuclear Malaysia. The former has strong possibility to be used as radiation-sensitive comparabilities in TPNR blends, besides its original purpose for example in radiation curing of surface coating. But earlier findings indicated that, to make it (as for surface coating) more effective, reinforcement system is needed to be introduced. Strong candidate is silica by sol-gel technique, since common reinforcement filler for example carbon black has drawbacks in this particular case. This technique was introduced in late 1960s to produce metal oxides such as silica and titanium oxides in solution. (author)

  13. The use of radiotracers in natural rubber research in Malaysia

    International Nuclear Information System (INIS)

    Lai, P.F.; Singh, M.M.

    1981-01-01

    Five main areas where radiotracers have been used in research on natural rubber are on studies on the uptake of plant nutrients by Hevea brasiliensis using 32 P, 86 Rb and 45 Ca as tracers; biosynthesis of Hevea rubber using 14 C or 3 H labelled intermediates; translocation and metabolism of 14 C. Ethephon in Hevea brasiliensis; use of radiotracers as analytical tools and adsorption of labelled fatty acid soaps on natural rubber lattices. These studies are discussed to show the powerful tool that radiotracers provide in agricultural, biochemical and chemical research on natural rubber. (author)

  14. Competitiveness and Exports Sustainability of the Indonesian Natural Rubber

    Directory of Open Access Journals (Sweden)

    Rumbiati Kamaludin

    2018-03-01

    Full Text Available This paper examines Indonesian competitiveness in export of natural rubber commodities by employing set of revealed comparative advantage (RCA and Export competitive index (ECI with respect to global trade. The market structure that is formed on natural rubber commodities is calculated using Herfindahl Index and Concentration Ratio analysis tools shows the oligopoly-shaped market structure. Calculation of comparative advantage with RCA analysis shows that the four countries exporting natural rubber, namely Thailand, Indonesia, Malaysia and Vietnam each have a comparative advantage. Where Indonesia has a better comparative advantage than Thailand in the period 2011 to 2015. This result is different from the calculations made on competitive advantage (ECI in which Indonesia's natural rubber commodities are not more competitive than Thailand

  15. Rubber friction on road surfaces: Experiment and theory for low sliding speeds

    Energy Technology Data Exchange (ETDEWEB)

    Lorenz, B.; Persson, B. N. J. [PGI, FZ Jülich, 52425 Jülich (Germany); Oh, Y. R.; Nam, S. K.; Jeon, S. H. [Hankook Tire Co. LTD., 112 Gajeongbuk-ro, Yuseong-gu, Daejeon 305-725 (Korea, Republic of)

    2015-05-21

    We study rubber friction for tire tread compounds on asphalt road surfaces. The road surface topographies are measured using a stylus instrument and atomic force microscopy, and the surface roughness power spectra are calculated. The rubber viscoelastic modulus mastercurves are obtained from dynamic mechanical analysis measurements and the large-strain effective modulus is obtained from strain sweep data. The rubber friction is measured at different temperatures and sliding velocities, and is compared to the calculated data obtained using the Persson contact mechanics theory. We conclude that in addition to the viscoelastic deformations of the rubber surface by the road asperities, there is an important contribution to the rubber friction from shear processes in the area of contact. The analysis shows that the latter contribution may arise from rubber molecules (or patches of rubber) undergoing bonding-stretching-debonding cycles as discussed in a classic paper by Schallamach.

  16. Effect of electron beam irradiation on the properties of crosslinked rubbers

    Science.gov (United States)

    Banik, Indranil; Bhowmick, Anil K.

    2000-05-01

    Influence of electron beam (EB) irradiation on the mechanical and dynamic mechanical properties of crosslinked fluorocarbon (FKM) rubber, natural rubber (NR), ethylene propylene diene monomer (EPDM) rubber and nitrile rubber (NBR) has been investigated. The modulus, gel fraction, glass transition temperature ( Tg) and storage modulus increased, while the elongation at the break and the loss tangent (tan δ) Tg decreased. FKM and NBR vulcanizates have been shown to have EB radiation resistance up to 1500 kGy.

  17. Particle reinforced composites from acrylamide modified blend of styrene-butadiene and natural rubber

    Science.gov (United States)

    Blends of styrene-butadiene rubber and natural rubber that provide balanced properties were modified with acrylamide and reinforced with soy protein particles. The rubber composites show improved mechanical properties. Both modified rubber and composites showed a faster curing rate. The crosslinking...

  18. A review on the suitability of rubberized concrete for concrete bridge decks

    Science.gov (United States)

    Syamir Senin, Mohamad; Shahidan, Shahiron; Radziah Abdullah, Siti; Anting Guntor, Nickholas; Syazani Leman, Alif

    2017-11-01

    Road authorities manage a large population of ageing bridges, a substantial number of which fail to meet the current requirements either due to deterioration and other structural deficiencies or as a result of the escalating demands imposed by increased traffic. This problem is related to the dynamic load from vehicles. This problem can be solved by producing a type of concrete that can reduce the amplitude of oscillation or vibration such as rubberized concrete. Green construction has been a very important aspect in concrete production field in the last decade. One of the most problematic waste materials is scrap tires. The use of scrap tires in civil engineering is increasing by producing rubberized concrete. Rubberized concrete is a type of concrete that is mixed with rubber. The purpose of this review is to justify the suitability of rubberized concrete for concrete bridge decks. Several parameters named physical, chemical and mechanical properties were measured to ensure the suitability of rubberized concrete for concrete bridge decks. Rubberized concrete has similar workability to normal concrete. The rubber reduced the density and compressive strength of the concrete while increased the flexural strength, water absorption and damping ratio. The used of rubber in concrete beyond 20% is not recommended due to decreasing in compressive strength. Rubberized concrete recommended to be used in circumstances where vibration damping was required such as in bridge construction as shock-wave absorber.

  19. Surface improvement of EPDM rubber by plasma treatment

    Energy Technology Data Exchange (ETDEWEB)

    Moraes, J H [LPP, Physics Department, ITA, CTA, Pca Mal Eduardo Gomes 50, 12228-900 Sao Jose dos Campos, S.P. (Brazil); Silva Sobrinho, A S da [LPP, Physics Department, ITA, CTA, Pca Mal Eduardo Gomes 50, 12228-900 Sao Jose dos Campos, S.P. (Brazil); Maciel, H S [LPP, Physics Department, ITA, CTA, Pca Mal Eduardo Gomes 50, 12228-900 Sao Jose dos Campos, S.P. (Brazil); Dutra, J C N [EBO, Chemistry Division, IAE, CTA, Pca Mal Eduardo Gomes 50, 12228-904 Sao Jose dos Campos, S.P. (Brazil); Massi, M [LPP, Physics Department, ITA, CTA, Pca Mal Eduardo Gomes 50, 12228-900 Sao Jose dos Campos, S.P. (Brazil); Mello, S A C [EBO, Chemistry Division, IAE, CTA, Pca Mal Eduardo Gomes 50, 12228-904 Sao Jose dos Campos, S.P. (Brazil); Schreiner, W H [Physics Department, UFPR, Centro Politecnico, 80060-000 Curitiba, P.R. (Brazil)

    2007-12-21

    The surface of ethylene-propylene-diene monomer (EPDM) rubber was treated in N{sub 2}/Ar and N{sub 2}/H{sub 2}/Ar RF plasmas in order to achieve similar or better adhesion properties than NBR (acrylonitrile-butadiene) rubber, nowadays used as thermal protection of rocket chambers. The surface properties were studied by contact angle measurements and by x-ray photoelectron spectroscopy (XPS). The treated surfaces of the EPDM samples show a significant reduction in the contact angle measurement, indicating an increase in the surface energy. XPS analyses show the incorporation of polar nitrogen- and oxygen-containing groups on the rubber surface. After plasma treatment the presence of oxygen is observed due to surface oxidation which occurs when the samples are exposed to the air. Atomic force microscopy and scanning electron microscopy analyses indicate a decrease in the EPDM rubber surface roughness, promoted by surface etching during the plasma treatment. Strength tests indicate improvement of about 30% and 110% in the adhesion strength for the plasma treated EPDM/polyurethane liner interface and for the EPDM/epoxy adhesive interface, respectively. The adhesion strength of the EPDM/liner is similar to that obtained for the NBR/liner, which indicates that EPDM rubber can safely be used as thermal protection of the solid propellant rocket chamber.

  20. Surface improvement of EPDM rubber by plasma treatment

    International Nuclear Information System (INIS)

    Moraes, J H; Silva Sobrinho, A S da; Maciel, H S; Dutra, J C N; Massi, M; Mello, S A C; Schreiner, W H

    2007-01-01

    The surface of ethylene-propylene-diene monomer (EPDM) rubber was treated in N 2 /Ar and N 2 /H 2 /Ar RF plasmas in order to achieve similar or better adhesion properties than NBR (acrylonitrile-butadiene) rubber, nowadays used as thermal protection of rocket chambers. The surface properties were studied by contact angle measurements and by x-ray photoelectron spectroscopy (XPS). The treated surfaces of the EPDM samples show a significant reduction in the contact angle measurement, indicating an increase in the surface energy. XPS analyses show the incorporation of polar nitrogen- and oxygen-containing groups on the rubber surface. After plasma treatment the presence of oxygen is observed due to surface oxidation which occurs when the samples are exposed to the air. Atomic force microscopy and scanning electron microscopy analyses indicate a decrease in the EPDM rubber surface roughness, promoted by surface etching during the plasma treatment. Strength tests indicate improvement of about 30% and 110% in the adhesion strength for the plasma treated EPDM/polyurethane liner interface and for the EPDM/epoxy adhesive interface, respectively. The adhesion strength of the EPDM/liner is similar to that obtained for the NBR/liner, which indicates that EPDM rubber can safely be used as thermal protection of the solid propellant rocket chamber

  1. Surface improvement of EPDM rubber by plasma treatment

    Science.gov (United States)

    Moraes, J. H.; da Silva Sobrinho, A. S.; Maciel, H. S.; Dutra, J. C. N.; Massi, M.; Mello, S. A. C.; Schreiner, W. H.

    2007-12-01

    The surface of ethylene-propylene-diene monomer (EPDM) rubber was treated in N2/Ar and N2/H2/Ar RF plasmas in order to achieve similar or better adhesion properties than NBR (acrylonitrile-butadiene) rubber, nowadays used as thermal protection of rocket chambers. The surface properties were studied by contact angle measurements and by x-ray photoelectron spectroscopy (XPS). The treated surfaces of the EPDM samples show a significant reduction in the contact angle measurement, indicating an increase in the surface energy. XPS analyses show the incorporation of polar nitrogen- and oxygen-containing groups on the rubber surface. After plasma treatment the presence of oxygen is observed due to surface oxidation which occurs when the samples are exposed to the air. Atomic force microscopy and scanning electron microscopy analyses indicate a decrease in the EPDM rubber surface roughness, promoted by surface etching during the plasma treatment. Strength tests indicate improvement of about 30% and 110% in the adhesion strength for the plasma treated EPDM/polyurethane liner interface and for the EPDM/epoxy adhesive interface, respectively. The adhesion strength of the EPDM/liner is similar to that obtained for the NBR/liner, which indicates that EPDM rubber can safely be used as thermal protection of the solid propellant rocket chamber.

  2. RTV Silicone Rubber Degradation Induced by Temperature Cycling

    Directory of Open Access Journals (Sweden)

    Xishan Wen

    2017-07-01

    Full Text Available Room temperature vulcanized (RTV silicone rubber is extensively used in power system due to its hydrophobicity and hydrophobicity transfer ability. Temperature has been proven to markedly affect the performance of silicone rubbers. This research investigated the degradation of RTV silicone rubber under temperature cycling treatment. Hydrophobicity and its transfer ability, hardness, functional groups, microscopic appearance, and thermal stability were analyzed using the static contact angle method, a Shore A durometer, Fourier transform infrared spectroscopy (FTIR, scanning electron microscopy (SEM, and thermogravimetry (TG, respectively. Some significant conclusions were drawn. After the temperature was cycled between −25 °C and 70 °C, the hydrophobicity changed modestly, but its transfer ability changed remarkably, which may result from the competition between the formation of more channels for the transfer of low molecular weight (LMW silicone fluid and the reduction of LMW silicone fluid in the bulk. A hardness analysis and FTIR analysis demonstrated that further cross-linking reactions occurred during the treatment. SEM images showed the changes in roughness of the RTV silicone rubber surfaces. TG analysis also demonstrated the degradation of RTV silicone rubber by presenting evidence that the content of organic materials decreased during the temperature cycling treatment.

  3. Implant supported overdentures--the Copenhagen experience

    DEFF Research Database (Denmark)

    Gotfredsen, K

    1997-01-01

    OBJECTIVES: To evaluate the functional and biological effect of implant-supported overdenture treatment in the lower jaw. METHODS AND MATERIALS: Thirty-two patients were consecutively treated with Astra Tech implants in the lower jaw for retaining overdentures. All implants had a diameter of 3.5 mm...... and all but two of the implants were longer than 10 mm. For the implant supported overdentures two methods of attachment were used, a bar or a ball. RESULTS: One of 69 fixtures was lost during the 4-5 year observation period. The mean bone loss for all fixtures was less than 0.2 mm per year. Complications...... quality and quantity is sufficient, two implants can support an overdenture in the lower jaw, providing prosthesis which functions well....

  4. Development of rubber gloves by radiation vulcanization

    International Nuclear Information System (INIS)

    Makuuchi, K.; Yoshii, F.; Ishigaki, I.; Mogi, M.; Saito, T.

    1990-01-01

    The processes of radiation vulcanization and production of protective rubber gloves for radioactive contamination are described. A newly developed sensitizing system consisting of 5 phr 2-ethylhexyl acrylate and 1 phr carbon tetrachloride was used to vulcanize natural rubber latex at 12 kGy. Transparent and soft gloves were obtained from the radiation vulcanized latex by a coagulant dipping process. The mechanical properties of the gloves meet Japanese Industrial Standard specification for protective gloves. Combustion analysis of the gloves revealed that the amount of evolved sulfur dioxide and remaining ashes are less than those from commercially available rubber gloves. A trial usage of the gloves at a nuclear power plant showed that the gloves were easy to use for delicate work without undergoing fatigue. (author)

  5. Synthesis and characterization of silver nanoparticles in natural rubber

    International Nuclear Information System (INIS)

    Abu Bakar, N.H.H.; Ismail, J.; Abu Bakar, M.

    2007-01-01

    Silver nanoparticles are formed in natural rubber matrix via photo reduction of film cast from natural rubber latex (NRL) containing silver salt. The resulting NR-Ag nanocomposite is characterized using TEM, XRD and UV spectroscopic techniques. The nanoparticles, diameter ranging between 4 and 10 nm, are dispersed within distinct interfaces which correspond to the inter-particle boundaries of the NRL particles that form the matrix. The average width of the interfaces is 8 nm. X-ray diffraction (XRD) analysis confirms the nanoparticles as metallic silver of the face-centered cubic type. UV-vis absorption spectra show peaks characteristic of the surface plasmon resonance of nano-sized silver. A comparison with the results of formation of silver, obtained under similar reduction condition, in a series of matrices namely de-proteinized natural rubber latex (DNRL), NRL containing sodium dodecyl sulfate (SDS), aqueous solutions of bovain serum albumin and SDS, suggests that the protein in natural rubber is responsible for the formation of stable silver nanoparticles in the natural rubber (NR) matrix

  6. Review on Parameters Influencing the Rice Breakage and Rubber Roll Wear in Sheller

    Directory of Open Access Journals (Sweden)

    Prabhakaran P.

    2017-09-01

    Full Text Available The present review deals with parameters influencing the rice breakage during rice milling operations and the effect of rubber roll Sheller in rice husk removal process. The main objective of rice milling system is to remove the husk and bran layer to produce the white rice. In this process, rubber roll sheller is used to remove husk from the grains by friction process. If the rubber material is too soft, there may not be sufficient shear force to husk the paddy. Wear will be minimum for rubber material with high hardness but indeed it pronounce the breakage of rice. Hence, for efficient husking the rubber roll material should possess the balance of physico-mechanical properties. Rice breakage depends on several other parameters like the type of harvest, drying temperature, drying methods, physical characteristics of paddy, husking characteristics, paddy moisture content, rubber roller speed, rubber roll pressure, paddy feed rate and fissures. Rubber roll wear depends on the type of rubber material attached to the roller, feed rate, roller speed, pressure etc.

  7. Polybutadiene and Styrene-Butadiene rubbers for high-dose dosimetry

    Energy Technology Data Exchange (ETDEWEB)

    Oliveira, Lucas N. [Instituto Federal de Educacao, Ciencia e Tecnologia de Goias-IFG,Campus Goiania, Goiania -GO (Brazil); Instituto de Pesquisas Energeticas e Nucleares -IPEN, Sao Paulo-SP (Brazil); Vieira, Silvio L. [Instituto de Fisica, Universidade Federal de Goias-UFG, Campus Samambaia, Goiania-GO (Brazil); Schimidt, Fernando [Instituto Federal de Educacao, Ciencia e Tecnologia de Goias-IFG,Campus Inhumas, Inhumas-GO (Brazil); Antonio, Patricia L.; Caldas, Linda V.E. [Instituto de Pesquisas Energeticas e Nucleares -IPEN, Sao Paulo-SP (Brazil)

    2015-07-01

    Polybutadiene and Styrene-Butadiene are synthetical rubbers used widely for pneumatic tires manufacturing. In this research, the dosimeter characteristics of those rubbers were studied for application in high-dose dosimetry. The rubber samples were irradiated with doses of 10 Gy up to 10 kGy, using a {sup 60}Co Gamma Cell-220 system (dose rate of 1.089 kGy/h) and their readings were taken on a Fourier Transform Infrared Spectroscopy-FTIR system (model Frontier/Perkin Elmer). The ratios of two absorbance peaks were taken for each kind of rubber spectrum, Polybutadiene (1306/1130 cm{sup -1}) and Styrene-Butadiene (1449/1306 cm{sup -1}). The ratio calculated was used as the response to the irradiation, and is not uniform across the sample. From the results, it can be concluded for both rubbers: a) the dose-response curves may be useful for high-dose dosimetry (greater than 250 Gy); b) their response for reproducibility presented standard deviations lower than 2.5%; c) the relative sensitivity was higher for Styrene-Butadiene (1.86 kGy{sup -1}) than for Polybutadiene (1.81 kGy{sup -1}), d) for doses of 10 kGy to 200 kGy, there was no variation in the dosimetric response. Both types of rubber samples showed usefulness as high-dose dosimeters. (authors)

  8. Study on a Haptic Sensor Using MCF (Magnetic Compound Fluid) Electric Conductive Rubber

    Science.gov (United States)

    Zheng, Yaoyang; Shimada, Kunio

    To provide a new composite material having a high degree of sensitivity regarding both electrical conduction and temperature for the field of robotics or sensing, we have developed magnetic rubber that contains a network-like magnetic cluster. We compared the temperature response of MCF rubber with others rubbers made under various experimental conditions, allowing us to find an optimum condition for making MCF rubber. The temperature response was obtained by an experimental equation. We also compared the electric conductivity of MCF rubber with that of ordinary electric conductive rubber and found that its electric sensitivity was lower at a small deformation, but increased at larger deformations. Therefore, MCF rubber has proven itself effective as a switching sensor when a small deformation is applied.

  9. Rubber lining design for grinding mills: influence on economy and capacity

    Energy Technology Data Exchange (ETDEWEB)

    Nillson, G

    1979-11-01

    There is a difference in design parameters between steel linings and rubber linings for grinding mills. The basic design parameters for rubber are described and a comparison is made between steel and rubber in different applications. If a rubber lining is correctly designed, it will give at least the same capacity as any other type of lining. A rubber lining can often be made thinner than other types of lining and, in such cases, the increased mill diameter will increase the capacity. What has been said above regarding capacity applies equally to grinding efficiency. The grind can sometimes be changed by altering the lifter height and lifter profile. Rubber linings of the correct quality and design will always give improved lining economy, except for large primary ball mills. We trust that new designs and rubber qualities will change the picture in the future. What is said about lining economy is especially true when taking reduced downtime and maintenance into consideration. The lining must be designed to reduce sliding over the shell, which leads to heavy wear. When used for dry grinding, the adverse effects of temperature must be observed.

  10. Effect of electron beam irradiation on the properties of crosslinked rubbers

    Energy Technology Data Exchange (ETDEWEB)

    Banik, Indranil; Bhowmick, Anil K. E-mail: anilkb@rtc.iitkgp.ernet.in

    2000-05-01

    Influence of electron beam (EB) irradiation on the mechanical and dynamic mechanical properties of crosslinked fluorocarbon (FKM) rubber, natural rubber (NR), ethylene propylene diene monomer (EPDM) rubber and nitrile rubber (NBR) has been investigated. The modulus, gel fraction, glass transition temperature (T{sub g}) and storage modulus increased, while the elongation at the break and the loss tangent (tan {delta}){sub T{sub g}} decreased. FKM and NBR vulcanizates have been shown to have EB radiation resistance up to 1500 kGy. (author)

  11. Effect of electron beam irradiation on the properties of crosslinked rubbers

    International Nuclear Information System (INIS)

    Banik, Indranil; Bhowmick, Anil K.

    2000-01-01

    Influence of electron beam (EB) irradiation on the mechanical and dynamic mechanical properties of crosslinked fluorocarbon (FKM) rubber, natural rubber (NR), ethylene propylene diene monomer (EPDM) rubber and nitrile rubber (NBR) has been investigated. The modulus, gel fraction, glass transition temperature (T g ) and storage modulus increased, while the elongation at the break and the loss tangent (tan δ) T g decreased. FKM and NBR vulcanizates have been shown to have EB radiation resistance up to 1500 kGy. (author)

  12. Unraveling the mystery of natural rubber biosynthesis. Part II. Composition and growth of in vitro natural rubber using high-resolution size exclusion chromatography

    Energy Technology Data Exchange (ETDEWEB)

    Chiang, Cheng Ching K. [Univ. of Akron, OH (United States); Barkakaty, Balaka [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States); Puskas, Judit E. [Univ. of Akron, OH (United States); Xie, Wenshuang [The Ohio State Univ., Wooster, OH (United States); Cornish, Katrina [The Ohio State Univ., Wooster, OH (United States); Peruch, Federic [Univ. of Bordeaux, Pessac Cedex (France); Deffieux, Alain [Univ. of Bordeaux, Pessac Cedex (France)

    2014-09-01

    The superior properties of natural rubber (cis-1,4-polyisoprene [NR]) are a function of its structure and composition, properties that still remain a mystery and that are irreplaceable by any synthetic rubber. NR from guayule (Parthenium argentatum) has been gaining special interest for its hypoallergenic properties while maintaining superior mechanical properties that are commonly associated with the Brazilian rubber tree (Hevea brasiliensis), the most common source of NR. Techniques exist to isolate washed rubber particles (WRPs) that contain enzymatically active rubber transferase, to study NR biosynthesis, and previous work on the in vitroNRgrowth in Hevea has demonstrated the presence of around 50wt%of a low molecular weight ([MW], Mn <10 000 g/mol) fraction. Structural and compositional analyses of this low MW fraction in Hevea are challenging due to the high protein content. Here, we discuss the analysis and composition of guayule latex and WRPs using high-resolution Size Exclusion Chromatography. We also discuss the composition of the soluble fraction of inactive guayule latex using matrix-assisted laser desorption ionization/time of flight mass spectrometry.

  13. Effect of Modified Rubber Particles Mixing Amount on Properties of Cement Mortar

    Directory of Open Access Journals (Sweden)

    Gang Xue

    2017-01-01

    Full Text Available The crumb rubber cement mortar is prepared by the crumb rubber aggregates in 60 mesh which are modified by 1% polyvinyl alcohol (PVA solution. Some mechanical properties of cement mortar with different crumb rubber aggregate amounts are researched including compressive strength, flexural strength, the ratio of compressive strength to flexural strength, impact resistance, and dry contraction percentage. In our tests, we consider six kinds of the rubber contents, 0%, 7.5%, 15%, 19%, 22.5%, and 30%, respectively. The optimal mixing amount of crumb rubber is determined by measuring three indices, the ratio of compressive strength to flexural strength, impact resistance, and dry contraction percentage. It is shown by test that the ratio of compressive strength to flexural strength is the smallest when the mixing amount of rubber is 19%; meanwhile high impact resistance and rational drying shrinkage are observed. The optimal mixing amount of the rubber particles is 19% determined by this test.

  14. Evaluation of biological properties of electron beam melted Ti6Al4V implant with biomimetic coating in vitro and in vivo.

    Directory of Open Access Journals (Sweden)

    Xiang Li

    Full Text Available BACKGROUND: High strength porous titanium implants are widely used for the reconstruction of craniofacial defects because of their similar mechanical properties to those of bone. The recent introduction of electron beam melting (EBM technique allows a direct digitally enabled fabrication of patient specific porous titanium implants, whereas both their in vitro and in vivo biological performance need further investigation. METHODS: In the present study, we fabricated porous Ti6Al4V implants with controlled porous structure by EBM process, analyzed their mechanical properties, and conducted the surface modification with biomimetic approach. The bioactivities of EBM porous titanium in vitro and in vivo were evaluated between implants with and without biomimetic apatite coating. RESULTS: The physical property of the porous implants, containing the compressive strength being 163 - 286 MPa and the Young's modulus being 14.5-38.5 GPa, is similar to cortical bone. The in vitro culture of osteoblasts on the porous Ti6Al4V implants has shown a favorable circumstance for cell attachment and proliferation as well as cell morphology and spreading, which were comparable with the implants coating with bone-like apatite. In vivo, histological analysis has obtained a rapid ingrowth of bone tissue from calvarial margins toward the center of bone defect in 12 weeks. We observed similar increasing rate of bone ingrowth and percentage of bone formation within coated and uncoated implants, all of which achieved a successful bridging of the defect in 12 weeks after the implantation. CONCLUSIONS: This study demonstrated that the EBM porous Ti6Al4V implant not only reduced the stress-shielding but also exerted appropriate osteoconductive properties, as well as the apatite coated group. The results opened up the possibility of using purely porous titanium alloy scaffolds to reconstruct specific bone defects in the maxillofacial and orthopedic fields.

  15. Radiation modification of silicone rubber with glycidylmethacrylate

    International Nuclear Information System (INIS)

    Segura, Tania; Burillo, Guillermina

    2013-01-01

    The grafting of glycidilmethacrylate(GMA) was grafted onto silicone rubber (SR) by using the γ-ray pre-irradiation grafting method under different conditions. The effect of reaction time, total dose, reaction temperature and monomer concentration on the graft yield was studied. It was found that the degree of grafting can be controlled by adjusting these parameters. The chemical structure of SR before and after grafting was characterized using FTIR-ATR and SEM–EDS. The analysis revealed that the surface of the SR was uniformly covered by GMA and the cross-section analysis indicated that the grafting occurred in the bulk. Thermogravimetric analysis (TGA) showed that the graft copolymer was more thermally stable than polyglycidylmethacrylate but less stable than SR, and the DSC confirmed that the GMA was grafting onto silicone rubber. - Highlights: • A graft copolymer with silicone rubber was synthesized by gamma pre-irradiation method. • SEM–EDS analysis showed that the surface and the bulk of the new copolymer were grafted. • The thermal properties of the silicone rubber used were modified with grafting. • The new copolymer could be used to immobilize nucleophilic biomolecules

  16. Rubber hand illusion under delayed visual feedback.

    Directory of Open Access Journals (Sweden)

    Sotaro Shimada

    Full Text Available BACKGROUND: Rubber hand illusion (RHI is a subject's illusion of the self-ownership of a rubber hand that was touched synchronously with their own hand. Although previous studies have confirmed that this illusion disappears when the rubber hand was touched asynchronously with the subject's hand, the minimum temporal discrepancy of these two events for attenuation of RHI has not been examined. METHODOLOGY/PRINCIPAL FINDINGS: In this study, various temporal discrepancies between visual and tactile stimulations were introduced by using a visual feedback delay experimental setup, and RHI effects in each temporal discrepancy condition were systematically tested. The results showed that subjects felt significantly greater RHI effects with temporal discrepancies of less than 300 ms compared with longer temporal discrepancies. The RHI effects on reaching performance (proprioceptive drift showed similar conditional differences. CONCLUSIONS/SIGNIFICANCE: Our results first demonstrated that a temporal discrepancy of less than 300 ms between visual stimulation of the rubber hand and tactile stimulation to the subject's own hand is preferable to induce strong sensation of RHI. We suggest that the time window of less than 300 ms is critical for multi-sensory integration processes constituting the self-body image.

  17. On some peculiarities of oil-resisting rubbers production from nitrile rubber of different composition by the use of Co60 gamma irradiation

    International Nuclear Information System (INIS)

    Mamedov, Sh.M.; Nelikzade, M.M.; Mamedov, A.A.

    1976-01-01

    The physicomechanical properties and swelling of vulcanizates were studied by means of radiation vulcanization. The test samples were preheated and formed by a press at 154 deg C for 3 min. Irradiation was performed in atmosphere on 60 Co (dosage 0.48 Mrad/hr). Irradiation caused decrease in tensile strength, as well as relative and permanent elongation; at the same time it considerably strengthened rubber hardness. All the rubber samples showed greater strength after irradiation under 5.7-13.8 Mrad. Depending on the dosage (3.6-13.8 Mrad), the relative and permanent elongation of vulcanizates obtained with the aid of altax was found to decrease, while strength and swelling increased. The swelling of rubber samples obtained with thiurad and thiuradaltax compounds decreased. Hence the advisability of using that rubber for manufacture of petroleum-resistant products

  18. Effects of forests, roads and mistletoe on bird diversity in monoculture rubber plantations.

    Science.gov (United States)

    Sreekar, Rachakonda; Huang, Guohualing; Yasuda, Mika; Quan, Rui-Chang; Goodale, Eben; Corlett, Richard T; Tomlinson, Kyle W

    2016-02-23

    Rising global demand for natural rubber is expanding monoculture rubber (Hevea brasilensis) at the expense of natural forests in the Old World tropics. Conversion of forests into rubber plantations has a devastating impact on biodiversity and we have yet to identify management strategies that can mitigate this. We determined the life-history traits that best predict bird species occurrence in rubber plantations in SW China and investigated the effects of surrounding forest cover and distance to roads on bird diversity. Mistletoes provide nectar and fruit resources in rubber so we examined mistletoe densities and the relationship with forest cover and rubber tree diameter. In rubber plantations, we recorded less than half of all bird species extant in the surrounding area. Birds with wider habitat breadths and low conservation value had a higher probability of occurrence. Species richness and diversity increased logarithmically with surrounding forest cover, but roads had little effect. Mistletoe density increased exponentially with rubber tree diameters, but was unrelated to forest cover. To maximize bird diversity in rubber-dominated landscapes it is therefore necessary to preserve as much forest as possible, construct roads through plantations and not forest, and retain some large rubber trees with mistletoes during crop rotations.

  19. Electromechanical responses of poly(3-thiopheneacetic acid/acrylonitrile-butadiene rubbers

    Directory of Open Access Journals (Sweden)

    2008-12-01

    Full Text Available Acrylonitrile-butadiene rubber (NBR and blends of poly(3-thiopheneacetic acid/ acrylonitrile-butadiene rubber, P3TAA/NBR, were fabricated, and the electrorheological properties, dielectric, and electrical conductivities were investigated . The electrorheological properties were determined under an oscillatory shear mode in a frequency range of 0.1 to 100 rad/s at various electric field strengths, from 0 to 2 kV/mm, at a fixed 27°C to observe the effects of acrylonitrile content (ACN in the rubber systems and the conductive particle concentration in the blends. For the pure rubber systems, the storage modulus response (ΔG′ is linearly dependent on its dielectric constant (ε′, and increases with the ACN content. For the NBR/P3TAA blends, the storage modulus response varies nonlinearly with the dielectric constant. The bending responses of the rubbers and the blends were investigated in a vertical cantilever fixture. For the pure rubber system, the bending angle and the dielectrophoresis force vary linearly with electric field strength. For the blend system, the bending angle and the dielectrophoresis force vary nonlinearly with electric field strength.

  20. Long rotation swidden systems maintain higher carbon stocks than rubber plantations

    DEFF Research Database (Denmark)

    Bruun, Thilde Bech; Berry, Nicholas; De Neergaard, Andreas

    2018-01-01

    in fallows were 1.5 ± 0.12 Mg C ha−1 yr−1 and 1.9 ± 0.14 Mg C ha−1 yr−1 in rubber plantations. When comparing time-averaged carbon stocks of swidden systems to rubber plantations with 30 year rotation periods, the stocks of swidden systems with rotation times of 5 and 10 years were 19% and 13% lower......Conversion of shifting cultivation to rubber (Hevea brasiliensis) plantations is one of the dominant land use changes in montane mainland areas of Southeast Asia, with the area of rubber expected to quadruple by 2050. However, the impacts of this transition on total ecosystem carbon stocks...... are poorly quantified. We undertook a chronosequence study to quantify changes in ecosystem carbon stocks following conversion from swidden agriculture to rubber plantations in Northern Laos. We measured above-ground biomass stocks and collected volume specific soil samples across rubber plantations...

  1. Control Systems of Rubber Dryer Machinery Components Using Programmable Logic Control (PLC)

    Science.gov (United States)

    Hendra; Yulianto, A. S.; Indriani, A.; Hernadewita; Hermiyetti

    2018-02-01

    Application of programmable logic control (PLC) is widely used on the control systems in the many field engineering such as automotive, aviation, food processing and other industries [1-2]. PLC is simply program to control many automatic activity, easy to use, flexible and others. PLC using the ladder program to solve and regulated the control system component. In previous research, PLC was used for control system of rotary dryer machine. In this paper PLC are used for control system of motion component in the rubber dryer machinery. Component of rubber dryer machine is motors, gearbox, sprocket, heater, drying chamber and bearing. Principle working of rubber dryer machinery is wet rubber moving into the drying chamber by sprocket. Sprocket is driven by motors that conducted by PLC to moving and set of wet rubber on the drying chamber. Drying system uses greenhouse effect by making hanger dryer design in the form of line path. In this paper focused on motion control system motors and sensors drying rubber using PLC. The results show that control system of rubber dryer machinery can work in accordance control input and the time required to dry the rubber.

  2. The main features of electrical stimulation of biological tissues by implant electrodes: study from engineering perspective and equipment development to produce

    International Nuclear Information System (INIS)

    Suarez Bagnasco, D.; Alvarez Alonso, J.; Suarez Antola, R.

    2004-08-01

    The main features of electrical stimulation of biological tissues by implant electrodes are studied.These electrodes are applied in neural prostheses and cardiac pacing.Threshold phenomena are stressed and some aspects related with implant electrode design are discussed. A fairly through theoretical research about the optimal pulse shape for electrical stimulation of biological tissues is done.The excitation functional is introduced as a criterium to identify threshold pulses of electric current. We obtain the optimal pulse shapes that minimize the energy dissipated in tissues, or the energy taken by the load seen by the pulse generator, amongst other criteria.We show how these pulse shapes can be determined from experimentally measured strength-duration (S-D) curves using rectangular pulses of current. The development of a prototype of a new equipment is described.The equipment may be used to measure S-D curves and with this information it is able to syntetize the abovementioned optimal pulse shapes. The top-down design process is presented, involving both hardware and software.The construction and assembling of the prototype, as well as the implementation of software are described.Some testing and measures with the prototype, including test with biological tissues are described and assessed

  3. Utilization of surface-treated rubber particles from waste tires

    Energy Technology Data Exchange (ETDEWEB)

    Smith, F.G. [Argonne National Lab., IL (United States). Energy Systems Div.]|[Environmental Technologies Alternatives, Inc., Lima, OH (United States)

    1994-12-01

    During a 12-month program, the author successfully demonstrated commercial applications for surface-treated rubber particles in two major markets: footwear (shoe soles and components) and urethane-foam carpet underlay (padding). In these markets, he has clearly demonstrated the ease of using R-4080 and R-4030 surface-treated rubber particles in existing manufacturing plants and processes and have shown that the material meets or exceeds existing standards for performance, quality, and cost-effectiveness. To produce R-4080 and R-4030, vulcanized rubber, whole-tire material is finely ground to particles of nominal 80 and mesh size respectively. Surface treatment is achieved by reacting these rubber particles with chlorine gas. In this report, the author describes the actual test and evaluations of the participant companies, and identifies other potential end uses.

  4. Biological Evaluation of Implant Drill Made from Zirconium Dioxide.

    Science.gov (United States)

    Akiba, Yosuke; Eguchi, Kaori; Akiba, Nami; Uoshima, Katsumi

    2017-04-01

    Zirconia is a good candidate material in the dental field. In this study, we evaluated biological responses against a zirconia drill using a bone cavity healing model. Zirconia drills, stainless steel drills, and the drilled bone surface were observed by scanning electron microscopy (SEM), before and after cavity preparation. For the bone cavity healing model, the upper first and second molars of Wistar rats were extracted. After 4 weeks, cavities were prepared with zirconia drills on the left side. As a control, a stainless steel drill was used on the right side. At 3, 7, and 14 days after surgery, micro-CT images were taken. Samples were prepared for histological staining. SEM images revealed that zirconia drills maintained sharpness even after 30 drilling procedures. The bone surface was smoother with the zirconia drill. Micro-CT images showed faster and earlier bone healing in the zirconia drill cavity. On H-E staining, at 7 days, the zirconia drill defect had a smaller blank lacunae area. At 14 days, the zirconia drill defect was filled with newly formed bone. The zirconia drill induces less damage during cavity preparation and is advantageous for bone healing. (197 words). © 2016 The Authors Clinical Implant Dentistry and Related Research Published by Wiley Periodicals, Inc.

  5. New rubber qualification for the igniter adapter

    Science.gov (United States)

    Humpherys, Mark A.

    1994-01-01

    Kirkhill Rubber Company (KRC) has informed Thiokol Corporation that two raw materials used in the asbestos and silica filled acrylonitrile butadience rubber (NBR) formulation per STW 2621 are no longer available from their vendors. Agerite White (Di-beta-naphthyl-paraphenylene diamine), manufactured by B. F. Goodrich, is an antioxidant used in NBR. This raw material makes up roughly 1-2 percent of the finished product. KRC proposed that this raw material be replaced by Agerite Stalite S (mixture of octylated diphenylamines) distributed by R. T. Vanderbilt Co. Protox-166 zinc oxide, manufactured by Zinc Corporation of America, is an activator currently used in NBR. This material also makes up about 1-2 percent of the finished material. Protox-166 is an American process grade zinc oxide. It is proposed by KRC to replace Protox-166 with Kadox-930C, a French process grade zinc oxide. American process grades have an ASTM minimum purity of 99.0 percent; the French process grades have a minimum purity of 99.5 percent. Previous testing per WTP-0270 has demonstrated that the mechanical and thermal properties of the rubber with the new ingredients are comparable to the 'old' rubber. The test results are reported in TWR-61790. One igniter adapter, Part no. 7U77562-02 serial no. 2 was insulated per ETP-1206 using the new rubber formulation and a modified lay up and cure method to demonstrate that there is no impact on this process. The results of this demonstration are reported.

  6. Aspects of the political economy of development and synthetic biology.

    Science.gov (United States)

    Wellhausen, Rachel; Mukunda, Gautam

    2009-12-01

    What implications might synthetic biology's potential as a wholly new method of production have for the world economy, particularly developing countries? Theories of political economy predict that synthetic biology can shift terms of trade and displace producers in developing countries. Governments, however, retain the ability to mitigate negative changes through social safety nets and to foster adaptation to some changes through research, education and investment. We consider the effects the synthetic production of otherwise naturally derived molecules are likely to have on trade and investment, particularly in developing countries. Both rubber in Malaysia and indigo dyes in India provide historical examples of natural molecules that faced market dislocations from synthetic competitors. Natural rubber was able to maintain significant market share, while natural indigo vanished from world markets. These cases demonstrate the two extremes of the impact synthetic biology might have on naturally derived products. If developing countries can cushion the pain of technological changes by providing producers support as they retool or exit, the harmful effects of synthetic biology can be mitigated while its benefits can still be captured.

  7. Natural rubber/high density polyethylene/ground rubber composites vulcanized by gamma irradiation

    International Nuclear Information System (INIS)

    Shaltout, N.A.; Abou zeid, M.M.; Khalil, A.M.; El Miligy, A.A.

    2010-01-01

    Natural rubber (NR) was blended mechanically with 50 phr high density polyethylene (HDPE). the mechanical, physical and thermal properties of NR/HDPE blend and its composites with different contents of ground tire rubber (GTR) before and after exposure to gamma irradiation to various doses up to 250 kGy were studied. Also, the change in structure morphology of irradiated NR/HDPE blend as well as NR/HDPE/GTR composites was examined by scanning electron microscope (SEM). The results showed that the substitution of a part of virgin NR with GTR decreases the mechanical and physical properties but not to the extent of deterioration . However, it was found that the mechanical and physical properties were improved after gamma irradiation . Composite of NR/GTR/HDPE (75/25/50) showed good properties. Scanning electron microscope showed homogeneity between the irradiated composites ingredients.

  8. Performance of carbon fiber reinforced rubber composite armour against shaped charge jet penetration

    Directory of Open Access Journals (Sweden)

    Yue Lian-yong

    2016-01-01

    Full Text Available Natural rubber is reinforced with carbon fiber; the protective performances of the carbonfiber reinforced rubber composite armour to shaped charge jet have been studied based on the depth of penetration experiments. The craters on the witness blocks, the nature rubber based composite plates’ deformation and the Scanning Electron Microscopy for the hybrid fiber reinforced rubber plate also is analyzed. The results showed that the composite armour can affect the stability of the jet and made part of the jet fracture. The carbon fiber reinforced rubber composite armour has good defence ablity especially when the nature rubber plate hybrid 15% volume percentage carbonfiber and the obliquity angle is 68°. The hybrid fiber reinforced rubber composite armour can be used as a new kind of light protective armour.

  9. Functionalization of Liquid Natural Rubber via Oxidative Degradation of Natural Rubber

    Directory of Open Access Journals (Sweden)

    Suhawati Ibrahim

    2014-12-01

    Full Text Available Natural rubber (NR is a high molecular weight natural polymer and can be degraded to liquid natural rubber (LNR leaving certain functional groups at the end of chains. In this study, LNR samples prepared via oxidative degradation using H2O2 and NaNO2 as reagents were found to have different end groups depending on the pH of the reaction medium. In an acidic medium, LNR with hydroxyl terminal groups was formed as the degradation reaction was initiated by hydroxyl radicals produced from decomposition of peroxynitrite acid. In contrast, a redox reaction took place in an alkaline medium to yield LNR with carbonyl terminal groups. The mechanisms of reaction are discussed and proposed to explain the formation of different end groups when reaction carried out in acidic and alkaline media. Chain degradation in an acidic medium seems to be more effective than in an alkaline medium, and thus yields LNR with lower Mn.

  10. Effect of rubber polarity on selective wetting of carbon nanotubes in ternary blends

    OpenAIRE

    Le, H.H.; Parsaker, M.; Sriharish, M.N.; Henning, S.; Menzel, M.; Wiessner, S.; Das, A.; Do, Q.K.; Heinrich, G.; Radusch, H.J.

    2015-01-01

    Based on atomic force microscopy (AFM) and Fourier transform infrared spectroscopy (FTIR) analysis of the rubber-filler gel (wetting concept) the kinetics of selective wetting of carbon nanotubes (CNTs) in ternary styrene butadiene rubber (SBR)/butadiene rubber (BR)/natural rubber (NR) blends was qualitatively and quantitatively characterized. Almost all CNTs are found to be wetted by the non-polar NR but not by the other non-polar rubber like BR or weakly polar SBR. It was proposed that phos...

  11. [Rubber band ligation in treatment of hemorrhoids: our experience].

    Science.gov (United States)

    Gaj, F; Biviano, I; Sportelli, G; Candeloro, L

    2015-01-01

    Hemorrhoids are a very common condition. The treatment depends upon persistence and severity of symptoms. For hemorrhoids of II and III grade the rubber band ligation may be therapeutic. Our aim is to report the outcomes of rubber band ligation of hemorrhoids, with a follow up of 6 months. A total of 50 patients underwent rubber band ligation for symptomatic hemorrhoids (grade II and III) without prolapse, between June 2012 and June 2014. All patients underwent plug test to rule out presence of rectal mucosal prolapse and were classified according to PATE classification (1). Each hemorrhoid was ligated with one rubber band through a ligator. All patients were evaluated immediately at the end of the procedure, after ten days and six months after the treatment. Patient's demographic and operative data were collected and analyzed. The mean patients age was 47.6±12.3 years (range 24-72). All procedures were performed without complications. Before rubber band ligation, 42 patients had rectal bleeding, 38 had perineal discomfort and 27 had itching. Ten days after the treatment, 12 patients presented self-limited rectal bleeding, but 10 of these had more hemorrhoids and underwent a second rubber band ligation. No patients complained perineal discomfort, and 8 patients had itching; 78% and 16% of patients respectively, experienced feeling of a foreign body inside the canal anal and anal pain. After 6 months, only 13 patients were occasionally symptomatic: 4 patients had rectal bleeding, 2 had perineal discomfort and 4 had itching. Three more patients presented both perineal discomfort and hitching. None had the feeling of a foreign body in anal canal or anal pain. Rubber band ligation is an efficacious, cost-effective and simple treatment for the second and third degree hemorrhoids without rectal mucosal prolapsed. In our hands, no severe complications developed and minor complications could be handled with ease.

  12. Use of rubber asphalt binder with graded aggregate for seal coats

    Energy Technology Data Exchange (ETDEWEB)

    1979-01-01

    It has been known that incorporating rubber particles into asphalt can improve highway pavement performance. This paper describes a test program on pavement construction using asphalts containing recycled rubber. During the summer 1978, eight test sections were constructed in parts of the Saskatchewan road system to evaluate seal coats using rubber-asphalt as a binder membrane and a graded aggregate as protective cover. Test sections were chosen to represent typical road surface types and different states of repair for each type. These types included prime subgrade, cold-mix on subgrade, primed granular base course, asphaltic concrete on granular base, and full depth asphaltic concrete. Problems with construction materials, techniques, and equipment are discussed. Performance and economics were evaluated to determine whether low cost cold mix and current seal coat surfaces could be replaced successfully and economically by this method of construction. It was shown that use of reclaimed rubber for rubberized asphalt seal coats on Saskatechewan highways is a practical construction application. The economic justification for rubber asphalt seals will be determined after a full assessment of performance. Initial indications are that Saskatchewan graded aggregates are a suitable cover material for the rubberized asphalt membranes used in the trials. 8 refs., 16 figs., 7 tabs.

  13. Polymer Electrolyte Prepared from Highly Deproteinized Natural Rubber Having Epoxy Group

    Science.gov (United States)

    Klinklai, W.; Kawahara, S.; Isono, Y.; Mizumo, T.; Yoshizawa, M.; Ohno, H.

    Deproteinized natural rubber having epoxy group (EDPNR) was applied to transport Li+ as a solid polymer electrolyte. The deproteinized natural rubber, incubated with proteolytic enzyme and surfactant, was subjected to epoxidation followed by oxidative depolymerization in latex stage. The resulting rubber was proved to be a liquid deproteinized natural rubber (LEDPNR) having polar epoxy groups, low Tg, low Mn and well-defined terminal units. Ionic conductivity of LEDPNR mixed with alkali metal salts was investigated through impedance analysis to clarify an effect of proteins present in the rubber. The ionic conductivity of the resulting LEDPNR depended on the kind of salts, their concentrations and temperature. The ionic conductivity of LEDPNR/lithium bis(trifluoromethan sulfonyl)imide (LiTFSI) was higher than that of LEDPNR/ lithium perchlorate (LiClO4). The difference in the ionic conductivity was attributed to the solubility of the salts as results of both high-resolution solid-state 13C-NMR spectroscopy and measurements of spin-lattice relaxation time. The conductivity of LEDPNR/LiTFSI was also dependent upon concentrations of LiTFSI and it reached the highest value at 20 wt%, which was different from the monotonic increase in the Li+ conductivity of liquid epoxidized natural rubber prepared from untreated natural rubber.

  14. Neutrophil Responses to Sterile Implant Materials.

    Directory of Open Access Journals (Sweden)

    Siddharth Jhunjhunwala

    Full Text Available In vivo implantation of sterile materials and devices results in a foreign body immune response leading to fibrosis of implanted material. Neutrophils, one of the first immune cells to be recruited to implantation sites, have been suggested to contribute to the establishment of the inflammatory microenvironment that initiates the fibrotic response. However, the precise numbers and roles of neutrophils in response to implanted devices remains unclear. Using a mouse model of peritoneal microcapsule implantation, we show 30-500 fold increased neutrophil presence in the peritoneal exudates in response to implants. We demonstrate that these neutrophils secrete increased amounts of a variety of inflammatory cytokines and chemokines. Further, we observe that they participate in the foreign body response through the formation of neutrophil extracellular traps (NETs on implant surfaces. Our results provide new insight into neutrophil function during a foreign body response to peritoneal implants which has implications for the development of biologically compatible medical devices.

  15. Flexible diamond-like carbon film coated on rubber

    NARCIS (Netherlands)

    Pei, Y.T.; Bui, X.L.; Pal, J.P. van der; Martinez-Martinez, D.; Hosson, J.Th.M. De

    2013-01-01

    Dynamic rubber seals are major sources of friction of lubrication systems and bearings, which may take up to 70% of the total friction. The solution we present is to coat rubbers with diamond-like carbon (DLC) thin films by which the coefficient of friction is reduced to less than one tenth. Coating

  16. Studies on biological effects of low energy N+ on ion beam implantation rice

    International Nuclear Information System (INIS)

    Wang Songli; Huang Qunce; Wang Tiegu; Qin Guangyong

    2006-01-01

    Dry seeds of five varieties of rice were implanted by 25 KeV low energy N + with doses of 2.0 x 10 17 , 2.5 x 10 17 and 3.0 x 10 17 N + /cm 2 , respectively. Mutant plants were selected from their progenies and the biological effects of the mutant plants were studied. The results showed that chlorophyll content of mutant plants was higher than that of the control, and one of those is as high as 148.67% of chlorophyll content compared with the control. Isoenzyme activities (POD, CAT and SOD) of mutant plants were different from the control plants. And AFLP analysis showed that the similarity between variant plants and feminine control plants was higher than that between variant plants and masculine control plants. (authors)

  17. Effect of concentrated epoxidised natural rubber and silica masterbatch for tyre application

    Energy Technology Data Exchange (ETDEWEB)

    Azira, A. A., E-mail: azira@lgm.gov.my; Kamal, M. M., E-mail: mazlina@lgm.gov.my [High Value Added Rubber Products and Nanostructured Materials, Stesen Penyelidikan RRIM, LGM 47000 Sungai Buloh, Selangor (Malaysia); Verasamy, D., E-mail: devaraj@lgm.gov.my [Environmental Technology & Sustainability, Technology & Engineering Division, Malaysian Rubber Board, Stesen Penyelidikan RRIM, LGM 47000 Sungai Buloh, Selangor (Malaysia)

    2016-07-06

    The availability of concentrated epoxidised natural rubber (ENR-LC) has provided a better opportunity for using epoxidised natural rubber (ENR) with silica to reinforce natural rubber for tyre application. ENR-LC mixed directly with silica to rubber by high speed stirrer without using any coupling agent. Some rubber compounds were prepared by mixing a large amount of precipitated amorphous white silica with natural rubber. The silica was prepared in aqueous dispersion and the filler was perfectly dispersed in the ENR-LC. The performance of the composites was evaluated in this work for the viability of ENR-LC/Si in tyre compounding. Compounding was carried out on a two roll mill, where the additives and curing agents was later mixed. Characterization of these composites was performed by Field Emission Scanning Electron Microscopy (FESEM) and Transmission Electron Microscopy (TEM) for dispersion as well as mechanical testing. C-ENR/Si showed efficient as primary reinforcing filler in ENR with regard to modulus and tensile strength, resulting on an increase in the stiffness of the rubbers compared to ENR latex. Overall improvement in the mechanical properties for the ENR-LC over the control crosslinked rubber sample was probably due to synergisms of silica reinforcement and crosslinking of the polymeric matrix phase.

  18. USE OF CRUMB RUBBER FROM USED CAR TIRES IN MINERAL ASPHALT MIXES

    Directory of Open Access Journals (Sweden)

    Andrzej Plewa

    2014-11-01

    Full Text Available With the development of the automotive industry the disposal of used tires is constantly growing problem. Storage of waste rubber is associated with a very long period of decomposition of rubber in the natural conditions. Simultaneously new technologies are developed every year, which in the future may significantly promote recycling of this type of materials. The crumb rubbery modification of the road bitumen is the one of the environmentally safe solutions of rubbery decomposition. Improvement of resistance of the crumb rubbery modification of the road asphalt mixtures is the very important ecological aspect of the future. The article presents the results of research on the fatigue life resistance of asphalt concretes AC16P and AC22P with asphalt-rubber binders. The above analyses have been based on the results of tests of fatigue life of mineral-rubber-asphalt mixes determined by the method of prismatic four-point bending (4PB-PR. Mineral-rubber -asphalt mixes have been diversified according to the amount of the additive of rubber fines in asphalt-rubber binder. On the basis of the test results have been proven improvements functional properties mineral-rubber-asphalt mixes compared with mineral-asphalt mixes with unmodified asphalt.

  19. Ground rubber: Sorption media for ground water containing benzene and O-xylene

    International Nuclear Information System (INIS)

    Kershaw, D.S.; Pamukcu, S.

    1997-01-01

    The purpose of the current study is to examine the ability of ground rubber to sorb benzene and O-xylene from water contained with aromatic hydrocarbons. The study consisted of running both batch and packed bed column tests to determine the sorption capacity, the required sorption equilibration time, and the flow through utilization efficiency of ground rubber under various contact times when exposed to water contaminated with various amounts of benzene or O-xylene. Initial batch test results indicate that ground rubber can attain equilibrium sorption capacities up to 1.3 or 8.2 mg of benzene or O-xylene, respectively, per gram of tire rubber at solution equilibrium concentrations of 10 mg/L. Packed bed column tests indicate that ground tire rubber has on the average a 40% utilization rate when a hydraulic residence time of 15 min is used. Possible future uses of round rubber as a sorption media could include, but are not limited to, the use of ground rubber as an aggregate in slurry cutoff walls that are in contact with petroleum products. Ground rubber could also be used as a sorption media in pump-and-treat methodologies or as a sorption media in in-situ reactive permeable barriers

  20. Effect of concentrated epoxidised natural rubber and silica masterbatch for tyre application

    International Nuclear Information System (INIS)

    Azira, A. A.; Kamal, M. M.; Verasamy, D.

    2016-01-01

    The availability of concentrated epoxidised natural rubber (ENR-LC) has provided a better opportunity for using epoxidised natural rubber (ENR) with silica to reinforce natural rubber for tyre application. ENR-LC mixed directly with silica to rubber by high speed stirrer without using any coupling agent. Some rubber compounds were prepared by mixing a large amount of precipitated amorphous white silica with natural rubber. The silica was prepared in aqueous dispersion and the filler was perfectly dispersed in the ENR-LC. The performance of the composites was evaluated in this work for the viability of ENR-LC/Si in tyre compounding. Compounding was carried out on a two roll mill, where the additives and curing agents was later mixed. Characterization of these composites was performed by Field Emission Scanning Electron Microscopy (FESEM) and Transmission Electron Microscopy (TEM) for dispersion as well as mechanical testing. C-ENR/Si showed efficient as primary reinforcing filler in ENR with regard to modulus and tensile strength, resulting on an increase in the stiffness of the rubbers compared to ENR latex. Overall improvement in the mechanical properties for the ENR-LC over the control crosslinked rubber sample was probably due to synergisms of silica reinforcement and crosslinking of the polymeric matrix phase.

  1. Radioisotopic determination methods of sulphur dispersion and sulphur blooming in rubber compounds

    International Nuclear Information System (INIS)

    Goraczka, W.; Koczorowska, E.

    1997-01-01

    It is well known that the concentration of sulphur in rubber compounds essentially effects the structure of the vulkanizate network. But there are no efficient and accurate methods to estimate the dispersion and migration (blooming) of curatives in raw rubber. In the work radioisotope methods have been analyzed to study the dispersion of curatives, physical and chemical processes in rubber and to optimize technical conditions of tire production. The radioactivity of the 35 S isotope introduced into rubber compounds has been measured by volumetric and surface methods. It was proved that the radioisotopic methods can be used in the studies. Experimental data of the effect of selected technological factors on these processes are presented. Rubber compounds containing soluble sulphur were made for such investigations. These methods permit detection of concentrations 10 -6 g of the radioactive isotope per 0.1 g of rubber compound. The sensitivity of these methods enables the investigation of radioisotope behaviour in rubber compounds during processing on an industrial scale without any hazards for workers

  2. Enhancing the thermal stability of natural rubber/recycled ethylene–propylene–diene rubber blends by means of introducing pre-vulcanised ethylene–propylene–diene rubber and electron beam irradiation

    International Nuclear Information System (INIS)

    Nabil, H.; Ismail, H.

    2014-01-01

    Highlights: • New route of processing was introduced to optimise the thermal stability of NR/R-EPDM blends. • Pre-vulcanised EPDM and EB irradiation were introduced into NR/R-EPDM blends. • Thermal stability is obviously enhanced by applying these two techniques. • Applying new route of processing methods is clearly successful to NR/R-EPDM blends. - Abstract: Most rubber materials are subjected to oxidation. The rate of oxidation depends on the type of rubber, processing method, and end-use conditions. The oxidation of rubber can result in the loss of physical properties, such as tensile strength, elongation, and flexibility. Hence, the service life is determined by oxidation stability. Thermal properties are relevant to the potential use of polymeric materials in many consumer oriented applications. Thermo-oxidative ageing and thermogravimetric analysis (TGA) have been proven to be successful techniques in determining the thermal stability of polymers and polymer blends. In this article, preparation of a series of natural rubber/recycled ethylene–propylene–diene rubber (NR/R-EPDM) blends is described. Processing of the blends, by means of introducing pre-vulcanised EPDM and electron beam (EB) irradiation, was carried out. Two thermal analysis methods, namely thermo-oxidative ageing and thermogravimetric analysis, were conducted. The results indicated that pre-vulcanising EPDM for 1.45 min (ts − 2) is sufficient to gain the optimum retained tensile and elongation at break. It was simultaneously observed that the introduction of pre-vulcanised EPDM increased decomposition temperature and activation energy by showing optimum values at a pre-vulcanising time of 3.45 min (ts). In the latter study, the retained properties increased after EB irradiation. The results can be verified by the thermal decomposition temperature and their activation energy. The obtained TG profiles and the calculated kinetic parameters indicated that introducing EB irradiation

  3. A Review on Using Crumb Rubber in Reinforcement of Asphalt Pavement

    Science.gov (United States)

    Mashaan, Nuha Salim; Ali, Asim Hassan; Karim, Mohamed Rehan; Abdelaziz, Mahrez

    2014-01-01

    An immense problem affecting environmental pollution is the increase of waste tyre vehicles. In an attempt to decrease the magnitude of this issue, crumb rubber modifier (CRM) obtained from waste tyre rubber has gained interest in asphalt reinforcement. The use of crumb rubber in the reinforcement of asphalt is considered as a smart solution for sustainable development by reusing waste materials, and it is believed that crumb rubber modifier (CRM) could be an alternative polymer material in improving hot mix asphalt performance properties. In this paper, a critical review on the use of crumb rubber in reinforcement of asphalt pavement will be presented and discussed. It will also include a review on the effects of CRM on the stiffness, rutting, and fatigue resistance of road pavement construction. PMID:24688369

  4. A Review on Using Crumb Rubber in Reinforcement of Asphalt Pavement

    Directory of Open Access Journals (Sweden)

    Nuha Salim Mashaan

    2014-01-01

    Full Text Available An immense problem affecting environmental pollution is the increase of waste tyre vehicles. In an attempt to decrease the magnitude of this issue, crumb rubber modifier (CRM obtained from waste tyre rubber has gained interest in asphalt reinforcement. The use of crumb rubber in the reinforcement of asphalt is considered as a smart solution for sustainable development by reusing waste materials, and it is believed that crumb rubber modifier (CRM could be an alternative polymer material in improving hot mix asphalt performance properties. In this paper, a critical review on the use of crumb rubber in reinforcement of asphalt pavement will be presented and discussed. It will also include a review on the effects of CRM on the stiffness, rutting, and fatigue resistance of road pavement construction.

  5. Devulcanization of Waste Tire Rubber Using Amine Based Solvents and Ultrasonic Energy

    OpenAIRE

    Walvekar Rashmi; Afiq Zulkefly Mohammad.; Ramarad Suganti; Khalid Siddiqui

    2018-01-01

    This research project focuses on an alternative pathway of devulcanizing waste tire rubber by using amine based chemicals. Waste tire rubbers are known to be as toxic, non-degradable material due to their vulcanized crosslink carbon structure, and disposing of such waste could impose hazardous impacts on the environment. The current rubber recycling methods that are practiced today are rather uneconomical, non-environmentally friendly, and also producing recycled rubber with low quality due t...

  6. Waste tyre rubberized concrete: properties at fresh and hardened state.

    Science.gov (United States)

    Aiello, M A; Leuzzi, F

    2010-01-01

    The main objective of this paper is to investigate the properties of various concrete mixtures at fresh and hardened state, obtained by a partial substitution of coarse and fine aggregate with different volume percentages of waste tyres rubber particles, having the same dimensions of the replaced aggregate. Workability, unit weight, compressive and flexural strength and post-cracking behaviour were evaluated and a comparison of the results for the different rubcrete mixtures were proposed in order to define the better mix proportions in terms of mechanical properties of the rubberized concrete. Results showed in this paper were also compared to data reported in literature. Moreover, a preliminary geometrical, physical and mechanical characterization on scrap tyre rubber shreds was made. The rubberized concrete mixtures showed lower unit weight compared to plain concrete and good workability. The results of compressive and flexural tests indicated a larger reduction of mechanical properties of rubcrete when replacing coarse aggregate rather than fine aggregate. On the other hand, the post-cracking behaviour of rubberized concrete was positively affected by the substitution of coarse aggregate with rubber shreds, showing a good energy absorption and ductility indexes in the range observed for fibrous concrete, as suggested by standard (ASTM C1018-97, 1997). 2010 Elsevier Ltd. All rights reserved.

  7. Effect of vulcanization temperature and humidity on the properties of RTV silicone rubber

    Science.gov (United States)

    Wu, Xutao; Li, Xiuguang; Hao, Lu; Wen, Xishan; Lan, Lei; Yuan, Xiaoqing; Zhang, Qingping

    2017-06-01

    In order to study the difference in performance of room temperature vulcanized (RTV) silicone rubber in vulcanization environment with different temperature and humidity, static contact angle method, FTIR and TG is utilized to depict the properties of hydrophobicity, transfer of hydrophobicity, functional groups and thermal stability of RTV silicone rubber. It is found that different vulcanization conditions have effects on the characteristics of RTV silicone rubber, which shows that the hydrophobicity of RTV silicone rubber changes little with the vulcanization temperature but a slight increase with the vulcanization humidity. Temperature and humidity have obvious effects on the hydrophobicity transfer ability of RTV silicone rubber, which is better when vulcanization temperature is 5°C or vulcanization humidity is 95%. From the Fourier transform infrared spectroscopy, it can be concluded that humidity and temperature of vulcanization conditions have great effect on the functional groups of silicone rubber, and vulcanization conditions also have effect on thermal stability of RTV silicone rubber. When vulcanization temperature is 5°C or vulcanization humidity is 15% or 95%, the thermal stability of silicone rubber becomes worse.

  8. Development of design method of thick rubber bearings for three-dimensional base isolation

    International Nuclear Information System (INIS)

    Yabana, Shuichi; Matuda, Akihiro

    2000-01-01

    Thick rubber bearings as 3-dimensional base isolators have been developed to reduce both horizontal and vertical seismic loads especially for equipment in Fast Breeder Reactors. In this report, a design method of thick rubber bearings is presented. To consider nonlinearity of vertical stiffness affected by vertical stress in the design of thick rubber bearings, Lindley's evaluation method of vertical stiffness is modified as an explicit form of vertical stress. We confirm that the presented method is efficient for design of the thick rubber bearings from comparing between test results and predicted values. Furthermore, rubber bearing tests are conducted with 1/3 scale models to evaluate mechanical properties of thick rubber bearings including ultimate limits. In the tests, horizontal and vertical characteristics of 1/3 scale model are compared with those of 1/6 scale model to discuss scale effect of test specimen. Ultimate limits such as failure shear strain of thick rubber bearings are obtained under various loading conditions. From the test results, we confirm that full scale thick rubber bearing to satisfy requirements is feasible. (author)

  9. Study on heat under dynamic loading of rubber

    Directory of Open Access Journals (Sweden)

    T. I. Igumenova

    2016-01-01

    Full Text Available A number of studies on heat buildup in tire rubber surface scan method samples using a thermal imaging camera. Investigated the exothermic chemical reaction mechanical destruction rubber when loading designs permanent cyclic stretching with deformation of the working zone 50%. Percentage of deformation of the working zone was chosen on the basis of the actual data on the stretch-compression zone "Rusk" tires, which is the maximum level difference of deformation during run-in. Experiment plan provided for periodic relaxation samples of at least 72 hours for more accurate simulation of operation process of structural products. Created and processed data on temperature changes in samples for bar and line profile for rubber compounds with the introduction of nanomodificator (fullerene-containing technical carbon in comparison with the control sample without him. The data obtained reflect the nature of heat depending on the composition of the compound. Identified common patterns of thermal nature of physicochemical process mechanical destruction rubbers. For rubber with nanomodifikatorom there has been an increase in the temperature interval reaction from a minimum to a maximum 2 degrees that is also linked to the rise in the average temperature of the reaction on the histogram also at 2-3 degrees of deformation under the same conditions and the level of cyclic loading. However, the temperature in the control sample that is associated with the beginning of the formation of hardened rubber structures, economies of Mallinza-Petrikeeva, occurs with delay twice compared with modified Fullerenes. Measurement of physic-mechanical indicators selected in the course of testing of samples showed the beginning of formation of structure with increased strength of samples in the sample temperature zone that corresponds to the thermal effect of èndotermičeskomu recombination reactions of macromolecules.

  10. Impact Resistance of Rubberized Self-Compacting Concrete

    Directory of Open Access Journals (Sweden)

    Eehab Khalil

    2015-04-01

    Full Text Available Impact loads due to ship collision on irrigation structures is significantly decreasing their durability. Loss of material and degradation are quite common problems facing lock walls and piers. In the current research, rubberized self-compacting concrete (SCC was used to investigate problems associated with impact. SCC with cement kiln dust cement replacement was used for that purpose. Concrete specimens were prepared with different crumb rubber ratios of 10% (RSCC-10, 20% (RSCC-20, 30% (RSCC-30, and 40% (RSCC-40 sand replacement by volume. Standard compressive, flexure, and splitting strength tests were conducted to monitor the effect of the added rubber on concrete behavior. Moreover, impact testing program was applied to specific specimens, cylinder of diameter 200 mm and thickness 50 mm, according to ACI committee 544 procedures. The number of blows to first and ultimate cracks was determined. The relationship between the mechanical properties and impact resilience is also presented. With the increase in rubber percentage the resistance to impact increased, but there was a decrease in specimen strength and modulus of elasticity. The variation in results was discussed and mix RSCC-30 exhibited the best impact resistance, 3 times over control mix with 40% reduction of compressive strength.

  11. The cross linking of EPDM and NBR rubber

    Directory of Open Access Journals (Sweden)

    Samardžija-Jovanović Suzana

    2005-01-01

    Full Text Available In the process of macromolecule cross linking, the choice of type and quantity of the components and the experimental conditions are important to obtain the new cross linked materials with better mechanical and chemical characteristics. The cross linking method depends on the rubber type and structure. Intermolecular cross linking results in the formation elastomer network. The basis of the cross linking process, between ethylene propylene diene rubber (EPDM and acrylonitrile butadiene rubber (NBR, is a chemical reaction. Fillers and other additives are present in different mass ratios in the material. The exploitation properties of the cross linked materials depend on the quantity of additive in the cross linked systems.

  12. Mapping Deciduous Rubber Plantation Areas and Stand Ages with PALSAR and Landsat Images

    Directory of Open Access Journals (Sweden)

    Weili Kou

    2015-01-01

    Full Text Available Accurate and updated finer resolution maps of rubber plantations and stand ages are needed to understand and assess the impacts of rubber plantations on regional ecosystem processes. This study presented a simple method for mapping rubber plantation areas and their stand ages by integration of PALSAR 50-m mosaic images and multi-temporal Landsat TM/ETM+ images. The L-band PALSAR 50-m mosaic images were used to map forests (including both natural forests and rubber trees and non-forests. For those PALSAR-based forest pixels, we analyzed the multi-temporal Landsat TM/ETM+ images from 2000 to 2009. We first studied phenological signatures of deciduous rubber plantations (defoliation and foliation and natural forests through analysis of surface reflectance, Normal Difference Vegetation Index (NDVI, Enhanced Vegetation Index (EVI, and Land Surface Water Index (LSWI and generated a map of rubber plantations in 2009. We then analyzed phenological signatures of rubber plantations with different stand ages and generated a map, in 2009, of rubber plantation stand ages (≤5, 6–10, >10 years-old based on multi-temporal Landsat images. The resultant maps clearly illustrated how rubber plantations have expanded into the mountains in the study area over the years. The results in this study demonstrate the potential of integrating microwave (e.g., PALSAR and optical remote sensing in the characterization of rubber plantations and their expansion over time.

  13. Ground tire rubber as a stabilizer for subgrade soils.

    Science.gov (United States)

    2014-05-01

    Over 250 million scrap tires are generated annually in the U.S. Historically, a significant portion of these tires : have been processed into finely ground tire rubber (GTR), or crumb rubber, for use as an additive in hot mix asphalt : (HMA) pavement...

  14. Oxygen Plasma Treatment of Rubber Surface by the Atmospheric Pressure Cold Plasma Torch

    DEFF Research Database (Denmark)

    Lee, Bong-ju; Kusano, Yukihiro; Kato, Nobuko

    1997-01-01

    adhesive. The adhesion property was improved by treatment of the rubber compound with plasma containing oxygen radicals. Physical and chemical changes of the rubber surface as a result of the plasma treatment were analyzed by field emission scanning electron microscopy (FE-SEM) and fourier transform......A new application of the atmospheric cold plasma torch has been investigated. Namely, the surface treatment of an air-exposed vulcanized rubber compound. The effect of plasma treatment was evaluated by the bondability of the treated rubber compound with another rubber compound using a polyurethane...

  15. Effect of gamma irradiation on the properties of natural rubber/styrene butadiene rubber blends

    Directory of Open Access Journals (Sweden)

    A.B. Moustafa

    2016-09-01

    Full Text Available Blends of natural rubber (NR with styrene butadiene rubber (SBR with varying ratios have been prepared. Vulcanization of the prepared blends has been induced by irradiation of gamma rays with varying doses up to 250 kGy. Mechanical properties, namely tensile strength, tensile modulus at 100% elongation, elongation at break have been followed up as a function of irradiation dose as well as blend composition. Physical properties, namely gel fraction and swelling number have been followed up using benzene as a solvent. Thermal measurements namely thermogravimetric analysis were carried out. The results indicated that the addition of NR has improved the properties of NR / SBR blends. Also NR/SBR blend is thermally stable than NR alone.

  16. Influence the Rubber Seed Type and Altitude on Characteristic of Seed, Oil and Biodiesel

    Directory of Open Access Journals (Sweden)

    Salni Salni

    2017-06-01

    Full Text Available This research studies the influence of the type of rubber seed that is superior and local, altitude plant in South Sumatra province to the characteristic of seed, oil and biodiesel (methyl ester. Rubber plants planted from local rubber seed by seeds seedlings and superior rubber seed by selected clones. In the study, rubber plants planted at a different altitude, namely in Banyuasin district (18 m above sea level, Prabumulih District (176 m above sea level and Lahat District (627 m above sea level. The results showed that the weight of the flour, the water content and ash content in the local rubber seeds larger than the superior rubber seed for all altitude, but oil content a large in the superior rubber seeds. The major of fatty acids in the rubber seed oil in all types and altitude are a linoleic acid with a different percentage except local rubber seed oil from Lahat district with the large percentage of octadecanoic acid. Free fatty acids in the oil from the superior seeds rubber of 13.897-15.494 % large than local rubber seed oil was found 9.786-10.399 % for all altitude. By esterification process using sulfuric acid catalyst, Free Fatty Acid (FFA can be reduced to ≤ 2 %. The methyl ester made from the transesterification process of rubber seed oil after esterification using methanol and sodium hydroxide as catalyst. Analysis of methyl esters includes cetane index, flash point, kinematic viscosity, carbon residue, density, moisture content, water and sediment content and distillation compared with SNI 7182 and ASTM 6751-02.  The result indicated that the quality of methyl ester from superior rubber seed oil in the Banyuasin and Prabumulih district better than another methyl ester. The types of rubber seed altitude affect the characteristics of the seed, oil and methyl ester  but the altitude are not significantly different. Keywords: rubber seed, type, altitude, oil, biodiesel Article History: Received March 21st 2017; Received in

  17. Behavior of Rubber Materials under Exposure to High Electric Fields

    DEFF Research Database (Denmark)

    Candela Garolera, Anna; Holbøll, Joachim; Henriksen, M,

    2013-01-01

    The effect of high electrical stress on rubber materials is investigated by performing breakdown tests and tracking resistance tests on selected samples. The study is focused on the relationship between the dielectric strength and the thickness of the samples, as well as the influence of the inte......The effect of high electrical stress on rubber materials is investigated by performing breakdown tests and tracking resistance tests on selected samples. The study is focused on the relationship between the dielectric strength and the thickness of the samples, as well as the influence...... of the interfaces between different layers of material. Tracking resistance tests are also performed on the rubber material. The purpose is to provide a complete study of the applicability of the rubber material in thunderstorm environments....

  18. High damping properties of magnetic particles doped rubber composites at wide frequency

    Energy Technology Data Exchange (ETDEWEB)

    Tian, Ye, E-mail: schtiany@163.com [Research Center for Engineering Technology of Polymeric Composites of Shanxi Province, North University of China, Taiyuan 030051 (China); College of Material Science and Engineering, North University of China, Taiyuan 030051 (China); Liu, Yaqing, E-mail: lyq@nuc.edu.cn [Research Center for Engineering Technology of Polymeric Composites of Shanxi Province, North University of China, Taiyuan 030051 (China); College of Material Science and Engineering, North University of China, Taiyuan 030051 (China); He, Minhong; Zhao, Guizhe; Sun, Youyi [Research Center for Engineering Technology of Polymeric Composites of Shanxi Province, North University of China, Taiyuan 030051 (China); College of Material Science and Engineering, North University of China, Taiyuan 030051 (China)

    2013-05-15

    Highlights: ► A new kind of permanent magnetic rubber was prepared. ► The microstructure and magnetic properties were investigated. ► The mechanical and damping properties were discussed. ► The new material is expected to be an isolator material to a changed frequency. - Abstract: A new kind of rubber composite was prepared by doping SrFe{sub 12}O{sub 19} nanoparticles coated with silane coupling agents (Si-69) into nitrile butadiene rubber (NBR) matrix, which was characterized by the scanning electron microscopy and X-ray spectroscopy. The results showed that the SrFe{sub 12}O{sub 19} nanoparticles were well dispersed in rubber matrix. Furthermore, the mechanical and magnetic properties of the rubber composites were investigated, in which the high tensile strength (15.8 MPa) and high saturation magnetization (22.9 emu/g) were observed. What is more, the high loss factor of the rubber composites was also obtained in a wide frequency range (0–100 Hz) at high loading (80 phr). The result is attributed to that the permanent magnetic field in rubber nanocomposites can absorb shock energy. These results indicate that the new kind of permanent magnetic rubber is expected to be a smart isolator material, in which the isolator will be able to adapt to a changed frequency.

  19. Comparison of mechanical and biological properties of zirconia and titanium alloy orthodontic micro-implants.

    Science.gov (United States)

    Choi, Hae Won; Park, Young Seok; Chung, Shin Hye; Jung, Min Ho; Moon, Won; Rhee, Sang Hoon

    2017-07-01

    The aim of this study was to compare the initial stability as insertion and removal torque and the clinical applicability of novel orthodontic zirconia micro-implants made using a powder injection molding (PIM) technique with those parameters in conventional titanium micro-implants. Sixty zirconia and 60 titanium micro-implants of similar design (diameter, 1.6 mm; length, 8.0 mm) were inserted perpendicularly in solid polyurethane foam with varying densities of 20 pounds per cubic foot (pcf), 30 pcf, and 40 pcf. Primary stability was measured as maximum insertion torque (MIT) and maximum removal torque (MRT). To investigate clinical applicability, compressive and tensile forces were recorded at 0.01, 0.02, and 0.03 mm displacement of the implants at angles of 0°, 10°, 20°, 30°, and 40°. The biocompatibility of zirconia micro-implants was assessed via an experimental animal study. There were no statistically significant differences between zirconia micro-implants and titanium alloy implants with regard to MIT, MRT, or the amount of movement in the angulated lateral displacement test. As angulation increased, the mean compressive and tensile forces required to displace both types of micro-implants increased substantially at all distances. The average bone-to-implant contact ratio of prototype zirconia micro-implants was 56.88 ± 6.72%. Zirconia micro-implants showed initial stability and clinical applicability for diverse orthodontic treatments comparable to that of titanium micro-implants under compressive and tensile forces.

  20. Irradiating rubber laminate containing sensitive agent in layer

    International Nuclear Information System (INIS)

    Bohm, G.G.A.

    1979-01-01

    Rubber compounds may be sensitized to cure or partially cure when subjected to irradiation. If certain layers of a rubber laminate are treated with sensitizing materials and other layers wth densensitizing materials a composite is produced having cured and uncured layers after it has been subjected to irradiation. This technique enables the production of composite laminates in which predetermined layers have predetermined physical characteristics which are desirable in the manufacture of the ultimate end product, for example, automotive tires. Several chemicals have been found to accelerate the cure of rubber compounds by irradiation and several have been found which inhibit the cure. Paradichlorobenzene (PDCB) and certain of the thioetherpolythiols are effective cure promotors. Effective retarders include aromatic oils, sulfur, sulfur cure accelerators and some rubber antioxidants and/or antiozonants of the substituted diphenylamine type. The dosage of irradiation is dependent upon several variables: the type of rubber, the promotor or retarder utilized, the level of the promotor or retarder, the thickness of the layer of material, the thickness of adjacent layers of materials, the sequence of the layers of material, the number of the layers of material and whether the irradiation is applied to one or both sides of the composite strip. The dosage may be controlled by the amount of energy employed so that the electrons do not completely penetrate the entire strip. This results in the irradiaton of part of the strip, but not the entire strip. (LL)

  1. No pain relief with the rubber hand illusion.

    Directory of Open Access Journals (Sweden)

    Rahul Mohan

    Full Text Available The sense of body ownership can be easily disrupted during illusions and the most common illusion is the rubber hand illusion. An idea that is rapidly gaining popularity in clinical pain medicine is that body ownership illusions can be used to modify pathological pain sensations and induce analgesia. However, this idea has not been empirically evaluated. Two separate research laboratories undertook independent randomized repeated measures experiments, both designed to detect an effect of the rubber hand illusion on experimentally induced hand pain. In Experiment 1, 16 healthy volunteers rated the pain evoked by noxious heat stimuli (5 s duration; interstimulus interval 25 s of set temperatures (47°, 48° and 49°C during the rubber hand illusion or during a control condition. There was a main effect of stimulus temperature on pain ratings, but no main effect of condition (p = 0.32, nor a condition x temperature interaction (p = 0.31. In Experiment 2, 20 healthy volunteers underwent quantitative sensory testing to determine heat and cold pain thresholds during the rubber hand illusion or during a control condition. Secondary analyses involved heat and cold detection thresholds and paradoxical heat sensations. Again, there was no main effect of condition on heat pain threshold (p = 0.17, nor on cold pain threshold (p = 0.65, nor on any of the secondary measures (p<0.56 for all. We conclude that the rubber hand illusion does not induce analgesia.

  2. The effects of cosmic radiation on implantable medical devices

    International Nuclear Information System (INIS)

    Bradley, P.

    1996-01-01

    Metal oxide semiconductor (MOS) integrated circuits, with the benefits of low power consumption, represent the state of the art technology for implantable medical devices. Three significant sources of radiation are classified as having the ability to damage or alter the behavior of implantable electronics; Secondary neutron cosmic radiation, alpha particle radiation from the device packaging and therapeutic doses(up to 70 Gγ) of high energy radiation used in radiation oncology. The effects of alpha particle radiation from the packaging may be eliminated by the use of polyimide or silicone rubber die coatings. The relatively low incidence of therapeutic radiation incident on an implantable device and the use of die coating leaves cosmic radiation induced secondary neutron single event upset (SEU) as the main pervasive ionising radiation threat to the reliability of implantable devices. A theoretical model which predicts the susceptibility of a RAM cell to secondary neutron cosmic radiation induced SEU is presented. The model correlates well within the statistical uncertainty associated with both the theoretical and field estimate. The predicted Soft Error Rate (SER) is 4.8 x l0 -12 upsets/(bit hr) compared to an observed upset rate of 8.5 x 10 -12 upsets/(bit hr) from 20 upsets collected over a total of 284672 device days. The predicted upset rate may increase by up to 20% when consideration is given to patients flying in aircraft The upset rate is also consistent with the expected geographical variations of the secondary cosmic ray neutron flux, although insufficient upsets precluded a statistically significant test. This is the first clinical data set obtained indicating the effects of cosmic radiation on implantable devices. Importantly, it may be used to predict the susceptibility of future to the implantable device designs to the effects of cosmic radiation

  3. Implantation of β-emitters on biomedical implants: 32 P isotropic ion implantation using a coaxial plasma reactor

    International Nuclear Information System (INIS)

    Fortin, M.A.; Paynter, R.W.; Sarkissian, A.; Stansfield, B.L.; Terreault, B.; Dufresne, V.

    2003-01-01

    The development of endovascular brachytherapy and the treatment of certain types of cancers (liver, lung, prostate) often require the use of beta-emitters, sometimes in the form of radioisotope-implanted devices. Among the most commonly used isotopes figures 32 P, a pure beta-emitter (maximum energy: 1.7 MeV), of which the path in biological tissues is of a few cm, restricting the impact of electron bombardment to the immediate environment of the implant. Several techniques and processes have been tried to elaborate surfaces and devices showing strongly bonded, or implanted 32 P. Anodizing, vapor phase deposition, grafting of oligonucleotides, as well as ion implantation processes have been investigated by several research groups as methods to implant beta-radioisotopes into surfaces. A coaxial plasma reactor was developed at INRS to implant radioisotopes into cylindrical metallic objects, such as coronary stents commonly used in angioplasty procedures. The dispersion of 32 P atoms on the interior surfaces of the chamber can be investigated using radiographs, contributing to image the plasma ion transport mechanisms that guide the efficiency of the implantation procedure. The amount of radioactivity on the wall liner, on the internal components, and on the biomedical implants are quantified using a surface barrier detector. A comparative study establishes a relationship between the gray scale of the radiographs, and dose measurements. A program was developed to convert the digitized images into maps showing surface dose density in mCi/cm 2 . An integration process allows the quantification of the doses on the walls and components of the reactor. Finally, the resulting integral of the 32 P dose is correlated to the initial amount of radioactivity inserted inside the implanter before the dismantling procedure. This method could be introduced as a fast and reliable way to test, qualify and assess the amount of radioactivity present on the as-produced implants

  4. GRAFT COPOLYMERIZATION OF OLYGOESTERACRYLATES WITH LIQUID RUBBER AND COPOLYMER’S CHARACTERISTICS

    Directory of Open Access Journals (Sweden)

    Y. A. Anisimov

    2015-02-01

    Full Text Available The kinetic of graft copolymerization of threeethyleneglicoldimethacrylate and di threeethyleneglicolftalatedimethacrylate with liquid buthadiene rubber have been studied as a function of the olygomers composition. The experimental constants of copolymerization rate and efficiency olygoesteracrylates graft to liquid rubber were determined. The ihfluence of olygoesteracrylates’ nature on the grafting efficiency to olygomer rubber is determined and the strength characteristics are found.

  5. Development of SBR-Nano clay Composites with Epoxidized Natural Rubber as Compatibilizer

    International Nuclear Information System (INIS)

    Rajasekar, R.; Das, Ch.K.; Gert Heinrich, G.; Das, A.

    2009-01-01

    The significant factor that determines the improvement of properties in rubber by the incorporation of nano clay is its distribution in the rubber matrix. The simple mixing of nonpolar rubber and organically modified nano clay will not contribute for the good dispersion of nano filler in the rubbery matrix. Hence a polar rubber like epoxidized natural rubber (ENR) can be used as a compatibilizer in order to obtain a better dispersion of the nano clay in the matrix polymer. Epoxidized natural rubber and organically modified nano clay composites (EC) were prepared by solution mixing. The nano clay employed in this study is Cloisite 20A. The obtained nano composites were incorporated in styrene butadiene-rubber (SBR) compounds with sulphur as a curing agent. The morphology observed through X-ray diffraction (XRD) and high-resolution transmission electron microscopy (HR-TEM) shows that the nano clay is highly intercalated in ENR, and further incorporation of EC in SBR matrix leads to partial exfoliation of the nano clay. Dynamic mechanical thermal analysis showed an increase in storage modulus and lesser damping characteristics for the compounds containing EC loading in SBR matrix. In addition, these compounds showed improvement in the mechanical properties.

  6. Study on mechanical properties of laminated rubber bearing with small shape factor

    International Nuclear Information System (INIS)

    Mazda, T.; Ootori, Y.; Yabana, S.; Hirata, K.; Ishida, K.

    1995-01-01

    Laminated rubber bearings with a small shape factor are regarded as one of the most promising isolation devices to reduce the vertical seismic load of a nuclear power plant. In this study, three types of natural rubber bearings with different aspect ratios (diameter/total thickness of rubber) and one high-damping rubber bearing are tested under varied loading conditions. Basic characteristics and ultimate characteristics of the bearings are made clear, and applicability of estimation formula and analysis method are verified

  7. Viscoelasticity evaluation of rubber by surface reflection of supersonic wave.

    Science.gov (United States)

    Omata, Nobuaki; Suga, Takahiro; Furusawa, Hirokazu; Urabe, Shinichi; Kondo, Takeru; Ni, Qing-Qing

    2006-12-22

    The main characteristic of rubber is a viscoelasticity. So it is important to research the characteristic of the viscoelasticity of the high frequency band for the friction between a rubber material and the hard one with roughness, for instance, the tire and the road. As for the measurement of the viscoelasticity of rubber, DMA (dynamic mechanical analysis) is general. However, some problems are pointed out to the measurement of the high frequency band by DMA. Then, we evaluated the viscoelasticity characteristic by the supersonic wave measurement. However, attenuation of rubber is large, and when the viscoelasticity is measured by the supersonic wave therefore, it is inconvenient and limited in a past method by means of bottom reflection. In this report, we tried the viscoelasticity evaluation by the method of using complex surface reflection coefficient and we compared with the friction coefficient under wide-range friction velocity. As a result, some relationships had been found for two properties. We report the result that character of viscoelasticity of rubber was comparable to friction coefficient.

  8. Microclimate and development of 'Conilon' coffee intercropped with rubber trees

    Directory of Open Access Journals (Sweden)

    Fábio Luiz Partelli

    2014-11-01

    Full Text Available The objective of this work was to evaluate the influence of intercropping 'Conilon' coffee (Coffea canephora with rubber trees on coffee tree microclimate, nutrition, growth, and yield. Rubber trees were planted in two double rows 33 m apart, with 4x2.3 m spacing between plants. Treatments consisted of the distances from the coffee plants to the rubber trees: 3, 6, 9, 12, and 15 m. Measurements of atmospheric variables (temperature, irradiance, and relative humidity, leaf nutrient concentration, internode length of plagiotropic and orthotropic branches, individual leaf area, chlorophyll content, and yield were performed. Intercropping promotes changes in the microclimatic conditions of coffee plants close to rubber trees, with reduction of temperature and irradiance level and increase in air relative humidity. The proximity of the coffee tree to the rubber trees promotes the elongation of the plagiotropic and orthotropic branches and increases the individual leaf area; however, it does not affect leaf concentrations of N, K, Mg, Fe, Zn, and B in 'Conilon' coffee and does not have a negative impact on yield.

  9. Vulcanization Kinetics of Natural Rubber Based On Free Sulfur Determination

    Directory of Open Access Journals (Sweden)

    Abu Hasan

    2013-05-01

    Full Text Available The determination of free sulfur in the rubber vulcanizates provided significant representation of vulcanization reaction. In this research, the effects of vulcanization temperature, the mixing method of carbon black into rubber, the ingredients mixing sequence and the type of carbon black were studied on masticated and milled natural rubber in which the reaction was observed by un-reacted sulfur determination. The results showed that higher vulcanization temperature provided faster vulcanization reaction and greater reaction rate constant. Similarly, the mixing sequence of ingredient and carbon black into rubber influenced the rate of vulcanization reaction. The subsequent ingredients mixing sequence, in this case, resulted in higher vulcanization rate compared to that of the simultaneous one. However, the mixing method of carbon black into rubber brought small effect on the rate of vulcanization reaction. The type of carbon black applied was observed to influence the reaction rate of vulcanization. Smaller particle sizes of carbon black gave larger reaction rate constant. In this case, the type of carbon black N 330 gave faster vulcanization rate than that of N 660.

  10. Effect of rubber polarity on selective wetting of carbon nanotubes in ternary blends

    Directory of Open Access Journals (Sweden)

    H. H. Le

    2015-11-01

    Full Text Available Based on atomic force microscopy (AFM and Fourier transform infrared spectroscopy (FTIR analysis of the rubber-filler gel (wetting concept the kinetics of selective wetting of carbon nanotubes (CNTs in ternary styrene butadiene rubber (SBR/butadiene rubber (BR/natural rubber (NR blends was qualitatively and quantitatively characterized. Almost all CNTs are found to be wetted by the non-polar NR but not by the other non-polar rubber like BR or weakly polar SBR. It was proposed that phospholipids, which are linked to the α-terminal of NR can interact with the CNT surface through cation-π interactions forming strong bonding between NR and CNTs. Using the corrected surface tension value of NR, which involves the effect of phospholipids found in our previous work the selective wetting of CNTs in ternary rubber blends can be well predicted using the Z-model for a thermodynamic equilibrium state. By replacing the non-polar BR by a polar rubber like nitrile butadiene rubber (NBR as a blend component CNTs are wetted by NBR slightly more than by NR thanks to the strong interaction between CNTs and nitrile groups of NBR. SBR remains unbound to CNTs in both blends.

  11. EVALUATION OF TIRE RUBBER DISPOSAL IN CONCRETE FOR PAVEMENTS

    Directory of Open Access Journals (Sweden)

    Rosa Cristina Cecche Lintz

    2009-01-01

    Full Text Available The production of waste by the tire industry has been a growing problem, indicating the need for its reuse. More than thirty million tires are discharged per year in Brazil, where regulation for the environment states that for each four new tires, five unusable ones must be adequately disposed by manufacturers and importers. Paving consumes an extremely large quantity of materials, which can be the source of rational application of waste and rejected materials. Research shows that tire rubber can be added to asphalt, which increases its durability and improves pavement quality and safety conditions by absorbing the rubber elastic properties, and also be used for architectural applications, among others. This study deals with the addition of rubber fibers from tire crushing in concrete for roadway pavements in order to provide proper indication about the alternative material disposal through an evaluation of the mechanical behavior of the modified concrete. Different concrete mixes were produced, within which, part of fine aggregates were substituted by tire rubber and mechanical experiment tests were performed, which show that, due to great resistance losses, the disposal of this alternative material in concrete should be considered for light traffic pavements, with the addition of rubber ranging up to 10% in mass.

  12. EVALUATION OF TIRE RUBBER DISPOSAL IN CONCRETE FOR PAVEMENTS

    Directory of Open Access Journals (Sweden)

    Rosa Cristina Cecche Lintz

    2009-12-01

    Full Text Available The production of waste by the tire industry has been a growing problem, indicating the need for its reuse. More than thirty million tires are discharged per year in Brazil, where regulation for the environment states that for each four new tires, five unusable ones must be adequately disposed by manufacturers and importers. Paving consumes an extremely large quantity of materials, which can be the source of rational application of waste and rejected materials. Research shows that tire rubber can be added to asphalt, which increases its durability and improves pavement quality and safety conditions by absorbing the rubber elastic properties, and also be used for architectural applications, among others. This study deals with the addition of rubber fibers from tire crushing in concrete for roadway pavements in order to provide proper indication about the alternative material disposal through an evaluation of the mechanical behavior of the modified concrete. Different concrete mixes were produced, within which, part of fine aggregates were substituted by tire rubber and mechanical experiment tests were performed, which show that, due to great resistance losses, the disposal of this alternative material in concrete should be considered for light traffic pavements, with the addition of rubber ranging up to 10% in mass.

  13. Behaviour of Steel Fibre Reinforced Rubberized Continuous Deep Beams

    Science.gov (United States)

    Sandeep, MS; Nagarajan, Praveen; Shashikala, A. P.

    2018-03-01

    Transfer girders and pier caps, which are in fact deep beams, are critical structural elements present in high-rise buildings and bridges respectively. During an earthquake, failure of lifeline structures like bridges and critical structural members like transfer girders will result in severe catastrophes. Ductility is the key factor that influences the resistance of any structural member against seismic action. Structural members cast using materials having higher ductility will possess higher seismic resistance. Previous research shows that concrete having rubber particles (rubcrete) possess better ductility and low density in comparison to ordinary concrete. The main hindrance to the use of rubcrete is the reduction in compressive and tensile strength of concrete due to the presence of rubber. If these undesirable properties of rubcrete can be controlled, a new cementitious composite with better ductility, seismic performance and economy can be developed. A combination of rubber particles and steel fibre has the potential to reduce the undesirable effect of rubcrete. In this paper, the effect of rubber particles and steel fibre in the behaviour of two-span continuous deep beams is studied experimentally. Based on the results, optimum proportions of steel fibre and rubber particles for getting good ductile behaviour with less reduction in collapse load is found out.

  14. Nutrient cycling in a RRIM 600 clone rubber plantation

    Directory of Open Access Journals (Sweden)

    Murbach Marcos Roberto

    2003-01-01

    Full Text Available Few reports have been presented on nutrient cycling in rubber tree plantations (Hevea brasiliensis Muell. Arg.. This experiment was carried out to evaluate: the effect of K rates on the amount of nutrients transfered to the soil in a 13-year old Hevea brasilensis RRIM 600 clone plantation, nutrient retranslocation from the leaves before falling to the soil, and nutrient loss by dry rubber export. The experiment started in 1998 and potassium was applied at the rates of 0, 40, 80 and 160 kg ha-1 of K2O under the crowns of 40 rubber trees of each plot. Literfall collectors, five per plot, were randomly distributed within the plots under the trees. The accumulated literfall was collected monthly during one year. The coagulated rubber latex from each plot was weighed, and samples were analyzed for nutrient content. Increasing K fertilization rates also increased the K content in leaf literfall. Calcium and N were the most recycled leaf nutrients to the soil via litterfall. Potassium, followed by P were the nutrients with the highest retranslocation rates. Potassium was the most exported nutrient by the harvested rubber, and this amount was higher than that transfered to the soil by the leaf literfall.

  15. Alexithymia Modulates the Experience of the Rubber Hand Illusion

    Directory of Open Access Journals (Sweden)

    Delphine eGrynberg

    2015-06-01

    Full Text Available Alexithymia is associated with lower awareness of emotional and non-emotional internal bodily signals. However, evidence suggesting that alexithymia modulates body awareness at an external level is scarce. This study aimed to investigate whether alexithymia is associated with disrupted multisensory integration by using the rubber hand illusion task.Fifty healthy individuals completed the Toronto Alexithymia Scale and underwent the rubber hand illusion measure. In this measure, one watches a rubber hand being stroked synchronously or asynchronously with one’s own hand, which is hidden from view. Compared to the asynchronous stimulation, the synchronous stimulation results in the illusion that the rubber hand and the participant’s hand are closer together than they really are and that the rubber hand belongs to them. Results revealed that higher levels of alexithymia are associated with a lower ownership illusion. In conclusion, our findings demonstrate that high alexithymia scorers integrate two simultaneous sensory and proprioceptive events into a single experience (lower multisensory integration to a lesser extent than low alexithymia scorers. Higher susceptibility to the illusion in high alexithymia scorers may -indicate that alexithymia is associated with impaired multisensory integration and that this association results from an abnormal focus of one's own body.

  16. EB-promoted recycling of waste tire rubber with polyolefins

    International Nuclear Information System (INIS)

    Mészáros, László; Bárány, Tamás; Czvikovszky, Tibor

    2012-01-01

    Despite the fact that more and more methods and solutions are used in the recycling of polymers, there are still some problems, especially in the recycling of cross-linked materials such as rubber. Usually the biggest problem is the lack of compatibility between the cross-linked rubber and the thermoplastic matrix. In this study we applied ground tire rubber (GTR) as recycled material. The GTR was embedded into polyethylene (PE) and polyethylene/ethylene-vinyl acetate copolymer (PE/EVA) matrices. In order to increase the compatibility of the components electron beam (EB) irradiation was applied. The results showed that the irradiation has a beneficial effect on the polymer–GTR interfacial connection. The EB treatment increased not only the tensile strength but also the elongation at break. The irradiation had also positive effect on the impact strength properties. - Highlights: ► In this study ground tire rubber was incorporated into polyethylene (LDPE) matrix. ► Compatibilizing effects of irradiation and ethylene-vinyl acetate were investigated. ► The samples were manufactured by twin-screw extrusion and injection molding. ► Both compatibilizing methods improved the rubber-like properties of the blends. ► This improvement was especially significant when they were applied together.

  17. The effect of melatonin implants administered from December until ...

    African Journals Online (AJOL)

    Administrator

    2016-06-28

    Jun 28, 2016 ... implantation had no effect on the growth rate of cashmere, except from ... The treated goats received subcutaneous melatonin implants (Beijing Kangtai Biological Technology .... 2 Litter size = mean number of kids per birth.

  18. Effect of Rubber Nanoparticle Agglomeration on Properties of Thermoplastic Vulcanizates during Dynamic Vulcanization

    Directory of Open Access Journals (Sweden)

    Hanguang Wu

    2016-04-01

    Full Text Available We previously reported that the dispersed rubber microparticles in ethylene-propylene-diene monomer (EPDM/polypropylene (PP thermoplastic vulcanizates (TPVs are actually agglomerates of rubber nanoparticles. In this study, based on this new understanding of the microstructure of TPV, we further revealed the microstructure-properties relationship of EPDM/PP TPV during dynamic vulcanization, especially the effect of the size of rubber nanoparticle agglomerates (dn, the thicknesses of PP ligaments (IDpoly and the rubber network on the properties of EPDM/PP TPV. We were able to simultaneously obtain a high tensile strength, elongation at break, elastic modulus, and elasticity for the EPDM/PP TPV by the achievement of a smaller dn, a thinner IDpoly and a denser rubber network. Interestingly, the effect of dn and IDpoly on the elastic modulus of EPDM/PP TPV composed of rubber nanoparticle agglomerates is different from that of EPDM/PP TPVs composed of rubber microparticles reported previously. The deformation behavior of the TPVs during stretching was studied to understand the mechanism for the achievement of good mechanical properties. Interestingly, the rubber nanoparticle agglomerates are oriented along the tensile direction during stretching. The TPV samples with smaller and more numerous rubber nanoparticle agglomerates can slow down the development of voids and cracks more effectively, thus leading to increase in tensile strength and elongation at break of the EPDM/PP TPV.

  19. Case study of rutting performance of HMA modified with waste rubber powder

    Directory of Open Access Journals (Sweden)

    G.H. Shafabakhsh

    2014-01-01

    Full Text Available Low resistance against dynamic loads and short service life of pavement are the most significant problems in the conservation and maintenance of roads, to the extent that, annually enormous costs are spent in order to improve capabilities of road services in the country. Research shows that the use of some wastes such as waste rubber powder in asphalt mixtures not only increase its serves life but also cause to reduce production costs; furthermore, recycling the crumb rubber has also considerably environmental benefits environmental benefits such as reduced need for landfill, less atmospheric pollution from burning. In this paper, the effect of adding waste rubber powder on the rutting performance of asphalt mixtures has been studied. In order to compare the performance of rubberized asphalt mixtures and conventional asphalt, wheel track test has been used. The results of this study show that the use of rubber powder caused a significant decrease in the rate of rutting depth of rubber asphalt mixtures compared to control samples.

  20. Rubber friction: The contribution from the area of real contact.

    Science.gov (United States)

    Tiwari, A; Miyashita, N; Espallargas, N; Persson, B N J

    2018-06-14

    There are two contributions to the friction force when a rubber block is sliding on a hard and rough substrate surface, namely, a contribution F ad = τ f A from the area of real contact A and a viscoelastic contribution F visc from the pulsating forces exerted by the substrate asperities on the rubber block. Here we present experimental results obtained at different sliding speeds and temperatures, and we show that the temperature dependency of the shear stress τ f , for temperatures above the rubber glass transition temperature T g , is weaker than that of the bulk viscoelastic modulus. The physical origin of τ f for T > T g is discussed, and we propose that its temperature dependency is determined by the rubber molecule segment mobility at the sliding interface, which is higher than in the bulk because of increased free-volume effect due to the short-wavelength surface roughness. This is consistent with the often observed reduction in the glass transition temperature in nanometer-thick surface layers of glassy polymers. For temperatures T contact regions and the contact area is determined by the rubber penetration hardness. For this case, we propose that the frictional shear stress is due to slip at the interface between the rubber and a transfer film adsorbed on the concrete surface.

  1. Rubber and Land-Cover Land-Use Change in Mainland Southeast Asia

    Science.gov (United States)

    Fox, J. M.; Hurni, K.

    2017-12-01

    Over the past half century, the five countries of Mainland Southeast Asia (MSEA) - Cambodia, Laos, Myanmar, Thailand, and Vietnam - have witnessed major shifts from predominantly subsistence agrarian economies to increasingly commercialized agriculture. Major drivers of change include policy initiatives that fostered regional economic integration and promoted among other changes rapid expansion of boom-crop plantations. Among the many types of commercial boom crops promoted and grown in MSEA are numerous tree-based products such as rubber, coffee, tree species for pulp and paper (particularly eucalyptus and acacia), cashews, and fruits such as oranges, lychees, and longans. The project proposal hypothesized that most (but not all) tree crops replaced swidden cultivation fields and hence are not necessarily accompanied by deforestation. We used MODIS EVI and SWIR time-series from 2001-2014 to classify changes in tree cover across MSEA; a total of 6849 sample points were used to train the classifier (75%) and verification (25%). The classification consists of 24 classes and 17 classes represent tree crops. Project results suggest that 4.4 m ha of rubber have been planted since 2003; 50% of rubber is planted on former evergreen forest land, 18% on deciduous forest land, and 32% on low vegetation area (former crop lands, bushes, scrub). Tree crops occupy about 8% of the landscape (half of that is rubber). Due to the differences in their political and economic histories these countries display different LCLUCs. In northern Laos, smallholder rubber plantations dominate and shifting cultivation is common in the upland. In southern Laos, large-scale plantations of rubber, coffee, eucalyptus, and sugarcane are widespread. In Thailand, vast areas are covered by annual agriculture; fruit trees and rubber are the prevailing tree crops and are mostly planted by smallholders. In Cambodia, large-scale rubber plantations have expanded in recent years on forest lands; smallholder

  2. Interfacial interaction between the epoxidized natural rubber and silica in natural rubber/silica composites

    Energy Technology Data Exchange (ETDEWEB)

    Xu, Tiwen [College of Materials Science and Engineering, South China University of Technology, Guangzhou 510640 (China); Jia, Zhixin, E-mail: zxjia@scut.edu.cn [College of Materials Science and Engineering, South China University of Technology, Guangzhou 510640 (China); Luo, Yuanfang; Jia, Demin [College of Materials Science and Engineering, South China University of Technology, Guangzhou 510640 (China); Peng, Zheng [Agricultural Product Processing Research Institute, Chinese Academy of Tropical Agriculture Sciences, Zhanjiang 524001 (China)

    2015-02-15

    Highlights: • Substantiate the ring open reaction between Si-OH of silica and epoxy groups of ENR. • ENR can act as a bridge between NR and silica to enhance the interfacial interaction. • As a modifier, ENR gets the potential to be used in the tread of green tire for improving the wet skid resistance apparently. - Abstract: The epoxidized natural rubber (ENR) as an interfacial modifier was used to improve the mechanical and dynamical mechanical properties of NR/silica composites. In order to reveal the interaction mechanism between ENR and silica, the ENR/Silica model compound was prepared by using an open mill and the interfacial interaction of ENR with silica was investigated by Fourier transform infrared spectroscopy (FTIR), X-ray photoelectron spectroscopy (XPS), transmission electron microscopy (TEM), X-ray diffraction (XRD) and stress–strain testing. The results indicated that the ring-opening reaction occurs between the epoxy groups of ENR chains and Si-OH groups on the silica surfaces and the covalent bonds are formed between two phases, which can improve the dispersion of silica in the rubber matrix and enhance the interfacial combination between rubber and silica. The ring-opening reaction occurs not only in vulcanization process but also in mixing process, meanwhile, the latter seems to be more important due to the simultaneous effects of mechanical force and temperature.

  3. Soft tissue wound healing around teeth and dental implants.

    Science.gov (United States)

    Sculean, Anton; Gruber, Reinhard; Bosshardt, Dieter D

    2014-04-01

    To provide an overview on the biology and soft tissue wound healing around teeth and dental implants. This narrative review focuses on cell biology and histology of soft tissue wounds around natural teeth and dental implants. The available data indicate that: (a) Oral wounds follow a similar pattern. (b) The tissue specificities of the gingival, alveolar and palatal mucosa appear to be innately and not necessarily functionally determined. (c) The granulation tissue originating from the periodontal ligament or from connective tissue originally covered by keratinized epithelium has the potential to induce keratinization. However, it also appears that deep palatal connective tissue may not have the same potential to induce keratinization as the palatal connective tissue originating from an immediately subepithelial area. (d) Epithelial healing following non-surgical and surgical periodontal therapy appears to be completed after a period of 7–14 days. Structural integrity of a maturing wound between a denuded root surface and a soft tissue flap is achieved at approximately 14-days post-surgery. (e) The formation of the biological width and maturation of the barrier function around transmucosal implants requires 6–8 weeks of healing. (f) The established peri-implant soft connective tissue resembles a scar tissue in composition, fibre orientation, and vasculature. (g) The peri-implant junctional epithelium may reach a greater final length under certain conditions such as implants placed into fresh extraction sockets versus conventional implant procedures in healed sites. © 2014 John Wiley & Sons A/S. Published by John Wiley & Sons Ltd.

  4. Preparation and Characterisation of Crosslinked Natural Rubber (SMR CV 60 and Epoxidised Natural Rubber (ENR-50 Blends

    Directory of Open Access Journals (Sweden)

    M. SASITARAN

    2018-04-01

    Full Text Available In this sudy, the influenceof di(tert-butylperoxyisopropylbenzene (DTBPIB on the properties of natural rubber (NR blend with epoxidized natural rubber (ENR was determined. Fourier transform infrared spectroscopy with attenuated total refletance analysis and gel content confired crosslinking occurred in the rubber blends in the presence of peroxide DTBPIB percentage. Studies including tensile properties, dynamic mechanical properties, thermogravimetric analysis (TGA and water absorptivity showed the changes in properties of the crosslinked NR/ENR blends. Tensile properties analysis disclosed the improvements in the modulus at 300% elongation and tensile stength with increasing NR ratios. Dynamic mechanical analysis revealed the blends to be incompatible and immiscible, with ENR showing a more viscous behaviour compared to the polymer blends. Thermal properties improved by blending NR with ENR as the onset temperature of NR/ENR: 50/50 was higher than pure NR by approximately 10oC and ENR by approximately 2oC. Water absorptivity experiment revealed a two-fold reduction in the presence of crosslinking for all blend ratios.

  5. Study on the Secant Segmentation Algorithm of Rubber Tree

    Science.gov (United States)

    Li, Shute; Zhang, Jie; Zhang, Jian; Sun, Liang; Liu, Yongna

    2018-04-01

    Natural rubber is one of the most important materials in the national defense and industry, and the tapping panel dryness (TPD) of the rubber tree is one of the most serious diseases that affect the production of rubber. Although considerable progress has been made in the more than 100 years of research on the TPD, there are still many areas to be improved. At present, the method of artificial observation is widely used to identify TPD, but the diversity of rubber tree secant symptoms leads to the inaccurate judgement of the level of TPD. In this paper, image processing technology is used to separate the secant and latex, so that we can get rid of the interference factors, get the exact secant and latex binary image. By calculating the area ratio of the corresponding binary images, the grade of TPD can be classified accurately. and can also provide an objective basis for the accurate identification of the tapping panel dryness (TPD) level.

  6. Nanostructured magnesium oxide as cure activator for polychloroprene rubber.

    Science.gov (United States)

    Kar, Sritama; Bhowmick, Anil K

    2009-05-01

    The aim of this research was to synthesize magnesium oxide nanoparticles and to use them as cure activator for polychloroprene rubber (CR). The effects of counterions of magnesium salts on the homogeneous phase precipitation reaction to control size, monodispersity, crystallinity, and morphology of Mg(OH)2 nanoparticles were also investigated. Magnesium oxide nanoparticles were synthesized by optimizing the calcination temperature of Mg(OH)2 nanoparticles. Finally, the MgO nanoparticles were dispersed in polychloroprene rubber (CR) solution along with zinc oxide (ZnO) powder. The influence of MgO nanoparticles on the mechanical, dynamic mechanical and thermal properties of the resulting nanocomposites was quantified. The modulus and strength of ZnO-cured polychloroprene rubber with 4% MgO nanoparticles appeared to be superior to those with ZnO particles or ZnO with rubber grade MgO particles. These composites were further characterized by transmission electron microscopy and infrared spectroscopy in order to understand the morphology of the resulting system and the load transfer mechanism.

  7. Physical, mechanical and thermal properties of Crushed Sand Concrete containing Rubber Waste

    Directory of Open Access Journals (Sweden)

    Mohamed Guendouz

    2018-01-01

    Full Text Available Over the past twenty years, the rubber wastes are an important part of municipal solid waste. This work focuses on the recycling of rubber waste, specifically rubber waste of used shoes discharged into the nature and added in the mass of crushed sand concrete with percentage (10%, 20%, 30% and 40%. The physical (workability, fresh density, mechanical (compressive and flexural strength and thermal (thermal conductivity of different crushed sand concrete made are analyzed and compared to the respective controls. The use of rubber waste in crushed sand concrete contributes to reduce the bulk density and performance of sand concrete. Nevertheless, the use of rubber aggregate leads to a significant reduction in thermal conductivity, which improves the thermal insulation of crushed sand concrete.

  8. A 3D Printed Implantable Device for Voiding the Bladder Using Shape Memory Alloy (SMA) Actuators.

    Science.gov (United States)

    Hassani, Faezeh Arab; Peh, Wendy Yen Xian; Gammad, Gil Gerald Lasam; Mogan, Roshini Priya; Ng, Tze Kiat; Kuo, Tricia Li Chuen; Ng, Lay Guat; Luu, Percy; Yen, Shih-Cheng; Lee, Chengkuo

    2017-11-01

    Underactive bladder or detrusor underactivity (DU) is defined as a reduction of contraction strength or duration of the bladder wall. Despite the serious healthcare implications of DU, there are limited solutions for affected individuals. A flexible 3D printed implantable device driven by shape memory alloys (SMA) actuators is presented here for the first time to physically contract the bladder to restore voluntary control of the bladder for individuals suffering from DU. This approach is used initially in benchtop experiments with a rubber balloon acting as a model for the rat bladder to verify its potential for voiding, and that the operating temperatures are safe for the eventual implantation of the device in a rat. The device is then implanted and tested on an anesthetized rat, and a voiding volume of more than 8% is successfully achieved for the SMA-based device without any surgical intervention or drug injection to relax the external sphincter.

  9. Preparation of irradiated natural rubber latex-styrene copolymer for electrical gloves

    International Nuclear Information System (INIS)

    Made Sumarti Kardha

    2010-01-01

    Research on irradiated natural rubber latex-styrene copolymer to prepare electrical glove have been done. Vulcanization of natural rubber latex (NRL) was done by mixing 2 phr (per hundred of rubber) of normal butyl acrylate (n-BA) emulsion then irradiated with ã-ray "6"0Co at the dose of 30 kGy producing irradiated natural rubber latex (INRL). Natural rubber latex-styrene copolymers (SC) were prepared by mixing NRL and styrene monomer at styrene concentrations of 50 phr, 75 phr, 100 phr, 500 phr and irradiated at the doses of 15 kGy, 30 kGy and 45 kGy, then characterized their latex and film properties to obtain optimum SC of SC50. This optimum SC, SC50 then mixed with IRNL at the weight ratio of 0/100, 30/70, 50/50, 70/30 and 100/0, to produce irradiated natural rubber latex-styrene copolymer. The properties of copolymer rubber films made by dipping process i.e., % conversion, total solid content, latex viscosity, tensile strength, modulus 300 %, elongation at break, electrical resistance and dielectric constant were then characterized. Characterization result showed that (INRL-SC50) with 50/50 ratio irradiated at the dose of 30 kGy, have % conversion of 80.93 %, electrical resistivity of 1.73 x 10"1"4 Ohm cm and dielectric constant of 2.76 which fulfill the requirement as material for electrical gloves. (author)

  10. Influence the Rubber Seed Type and Altitude on Characteristic of Seed, Oil and Biodiesel

    OpenAIRE

    Salni Salni; Poedji Loekitowati Hariani; Hanifa Marisa Hanifa

    2017-01-01

    This research studies the influence of the type of rubber seed that is superior and local, altitude plant in South Sumatra province to the characteristic of seed, oil and biodiesel (methyl ester). Rubber plants planted from local rubber seed by seeds seedlings and superior rubber seed by selected clones. In the study, rubber plants planted at a different altitude, namely in Banyuasin district (18 m above sea level), Prabumulih District (176 m above sea level) and Lahat District (627 m above s...

  11. From rubber tree homeland to rubber tree plantation: Jacques Huber and his studies on the culture of heveas in the East (1911-1912

    Directory of Open Access Journals (Sweden)

    Anna Raquel de Matos Castro

    2009-12-01

    Full Text Available The paper deals with the trip of the Swiss botanist Jacques Huber (1867-1914 to the main eastern rubber producing countries between 1911 and 1912. This trip was intended to develop studies on the cultivation of Hevea brasiliensis in that region. Huber was commissioned with the task by the State of Pará governor João Coelho, who wanted to find solutions to the downfall of the regional economy. The economy of Amazonia was primarily based on rubber extractivism and was seriously endangered due the market controlled by England from eastern plantations. Back to Brazil, Huber published a report with information about the society, economy and environment where the rubber trees were cultivated. The report compiles scientific observations and the topics that motivated the regional elites in that context. In addition to the brief analyses of the report, photographs took by Huber in the East of rubber trees plantations, tree tapping and local workers are published.

  12. Factors affecting Thai rubber farmer production and marketing in the western province of Kanchanaburi

    Directory of Open Access Journals (Sweden)

    Narisa Thongtrai

    2016-04-01

    Full Text Available This research aimed to study the factors affecting the production and marketing of rubber farmers in the western Thai province of Kanchanaburi. The sample group included 30 farmers involved in rubber production. From the questionnaire and statistical analysis by SPSS, 15 observed variables were determined to be factors affecting the production and marketing of rubber farmers. The conclusion from the researchers determined that 1 The area planted is not appropriate and is still expanding plantations without any control was found that the rubber plantations are expanding at high plains area flooding. 2 Farmers of rubber technology farmers are not valid and do not conform to the instructions of the Rubber Research Institute study found that the cause is the opportunity to access technology and lack of knowledge regarding the management, production, and marketing. 3 Use rubber tree tapping of the system to high frequency screaming systems correctly. Does not comply with the instructions of the Rubber Research Institute found that of rubber farmers and farmers opening tapped the tire rubber accelerator before opening a huge size tapped that affect productivity and the income of farmers depressed farmers. 4 Problems with the labor of producing rubber of the household. It was found that labor households in the production system are lower 5 Farmers of Thailand are not yet aware of the concept of livelihood along the sufficiency economy as should farmers be life according to the way of life that is not adjusted to prepare 6 Group integration it was found that is not yet strong.

  13. Mechanical Characterisation and Biomechanical and Biological Behaviours of Ti-Zr Binary-Alloy Dental Implants

    Directory of Open Access Journals (Sweden)

    Aritza Brizuela-Velasco

    2017-01-01

    Full Text Available The objective of the study is to characterise the mechanical properties of Ti-15Zr binary alloy dental implants and to describe their biomechanical behaviour as well as their osseointegration capacity compared with the conventional Ti-6Al-4V (TAV alloy implants. The mechanical properties of Ti-15Zr binary alloy were characterised using Roxolid© implants (Straumann, Basel, Switzerland via ultrasound. Their biomechanical behaviour was described via finite element analysis. Their osseointegration capacity was compared via an in vivo study performed on 12 adult rabbits. Young’s modulus of the Roxolid© implant was around 103 GPa, and the Poisson coefficient was around 0.33. There were no significant differences in terms of Von Mises stress values at the implant and bone level between both alloys. Regarding deformation, the highest value was observed for Ti-15Zr implant, and the lowest value was observed for the cortical bone surrounding TAV implant, with no deformation differences at the bone level between both alloys. Histological analysis of the implants inserted in rabbits demonstrated higher BIC percentage for Ti-15Zr implants at 3 and 6 weeks. Ti-15Zr alloy showed elastic properties and biomechanical behaviours similar to TAV alloy, although Ti-15Zr implant had a greater BIC percentage after 3 and 6 weeks of osseointegration.

  14. Advantages of Concrete Mixing with Tyre Rubber

    OpenAIRE

    Mazyad Al-Fadhli *

    2017-01-01

    Strong waste administration is one of the major natural concerns everywhere throughout the world. Tire-rubber particles made out of tire chips, piece elastic, and a mix of tire chips and scrap elastic, where utilized to supplant mineral totals in cement. These particles were utilized to supplant 10% , 15% , 20%, and 25% of the aggregate mineral totals volume in cement.Using rubber aggregates in such applications can help to prevent pollution and overcome the problem of storing used tyres. Adv...

  15. The use of styrene-butadiene rubber waste as a potential filler in nitrile rubber: order of addition and size of waste particles

    Directory of Open Access Journals (Sweden)

    D. A. Baeta

    2009-03-01

    Full Text Available Styrene-butadiene rubber (SBR has large applications in the shoe industry, especially as expanded sheets used to produce insoles and inner soles. According to TG analysis, the rubber content in SBR residues (SBR-r was found to be around 26-wt%. Based on that data, a cost-effective technique for the reuse of SBR-r in Nitrile rubber (NBR was developed. Later, the effect of SBR-r on the cure behavior, mechanical performance, swelling, and crosslink density of reused rubber was investigated, with more emphasis placed on the effect of both particle size and loading of waste filler. Cure characteristics such as optimum cure time and scorch time were then reduced by the increasing amount of SBR-r filler. Owing to the reinforced nature of the largest particle size SBR-r, the best results for the mechanical properties of NBR were those in which SBR-r was added at the end of the cure process. The study has thus shown that SBR residue (SBR-r can be used as an economical alternative filler in NBR.

  16. Studies of chemical interactions between chlorosulphonated polyethylene and nit rile rubber

    Directory of Open Access Journals (Sweden)

    Marković Gordana

    2005-01-01

    Full Text Available Highly polar rubbers interact with each other through their active functional groups via condensation or substitution reactions at high temperature. Chlorosulphonated polyethylene (CSM rubber is a highly reactive rubber, the reactivity of with is due to the -SO2CI groups. When CSM reacts with nit rile rubber (NBR, a chemical reaction takes place between the two rubbers at high temperature. Fourier transform infrared (FTIR studies support that CSM/NBR (50/50 w/w isothermally induces a self cross-linking blend, when cross-linking takes place via the acrylonitrile groups of NBR and the SO2CI groups or the insitu generated allyl chloride moieties of CSM. There is a loss of some -CN groups during cross-linking. This may be due to an attack on the -CN groups by HCI (produced during the heating of CSM in the presence of inherent moisture in the polymers. Amid type of linkage is formed due to cross-linking.

  17. Study on cord/rubber interface at elevated temperatures by H-pull test method

    Science.gov (United States)

    Jamshidi, M.; Afshar, F.; Mohammadi, N.; Pourmahdian, S.

    2005-08-01

    Cords are used as reinforcing materials in rubber compounds. To increase cord/rubber interfacial adhesion, they are coated by an adhesive (usually based on resorcinol-formaldehyde-latex). These composites are used in many sectors such as tire and belt industries. Cord/rubber adhesion strength is an important aspect to determine the durability of system. Due to temperature increase during running tires, the adhesion energy becomes different from initial one. To study cord/rubber interface at elevated temperatures, H-adhesion test method was used. H-pull test is a simple method for adhesion evaluation at ambient temperature, so it is usually used for material quality control. In this research, cord/rubber systems were vulcanized at different temperatures and H-adhesion of samples were evaluated at elevated temperatures. Also cord/rubber interface was studied by ATR analyze to determine interfacial interactions kind.

  18. Experience of rubber band ligation for haemorrhoidal disease

    International Nuclear Information System (INIS)

    Hadi, A.; Aman, Z.; Anwar, F.; Khan, M.; Iqbal, Z.

    2011-01-01

    Objectives: To assess symptomatic relief in haemorrhoidal disease using rubber band ligation. Settings and duration: Surgical unit, Hayatabad Medical Complex, Peshawar from July 2007 to June 2009. Patients and Methods: All patients presenting with rectal bleeding or prolapse underwent proto copy to determine the cause of bleeding. Only patients with first, second and third degree haemorrhoids (bleeding and prolapse) were selected for the study and they underwent rubber band ligation in two sessions, 6 weeks apart. Patients were followed in the OPD at 3 months and one year when their subjective and objective symptoms were noted followed by rectal examination and proctoscopy. Therapeutic response was assessed by symptomatic improvement in bleeding and prolapse of hemorrhoids and any complications. Results: A total of 105 patients underwent rubber band ligation. There were 65(62%) males and 40(38%) females with a male to female ratio of 1.6:1. Age of the patients ranged from 21-65 years (+- 2.4 SD). Twenty three (21.9%) patients had first degree, 50(47.6%) had second degree and 32(30.5%) had third degree haemorrhoids. Forty-eight patients (45.7%) presented with degree, 50(47.6%) had second prolapse, 33(31.4%) had both bleeding and prolapse and 23(21.9%) had bleeding only. At 3 months of follow up rubber band ligation cured 76(72.4%) patients, improved 13(12.4%) and failed in 7(6.7%) patients. At one year follow up, recurrence of bleeding and prolapse occurred in 16(15.2%) patients having third degree haemorrhoids. Overall success was third achieved in 89(84.8%) cases. Complications were seen in 20(19.1%) patients which were of mild to moderate nature and no serious/ life threatening complications were noted. Conclusion: Rubber band legislation is a rapid and safe procedure for testing first, second and and early third degree Conclusions: Rubber band ligation is a rapid and safe non operative procedure for treating first, second and third degree haemorrhoids on out

  19. Influence of the surface treatment of tire rubber residues added in mortars

    Directory of Open Access Journals (Sweden)

    A. C. Marques

    Full Text Available In this work it was evaluated the influence tire rubber addition in mortars in order to replace part of the sand (12% by volume. It was also intended to verify if the tire rubber treatment with NaOH saturated aqueous solution causes interference on the mechanical properties of the mixture. Compressive strength, splitting tensile strength, water absorption, modulus of elasticity, and flow test were made in specimens of 5cmx10cm and the tests were carried out to 7, 28, 56, 90, and 180 days. The results show reduction on mechanical properties values after addition of tire rubber and decrease of the workability. It was also observed that the tire rubber treatment does not cause any alteration on the results compared to the rubber without treatment.

  20. Load Absorption Characteristics of Tyre Production Waste Rubber for Playground Floor Systems

    Directory of Open Access Journals (Sweden)

    Abdul Ghani A.N.

    2014-01-01

    Full Text Available The floor surfaces where slides and swings are placed in parks and playrooms should be soft and thick to ensure that whenever a child falls, the surface can withstand the impact and minimize injuries to the child. Shredded tyres from waste tyres or waste rubber from tyre manufacturing could become beneficial as shock absorber material which can be used as a playground floor. In this study, rubber cubes and rubber pads with 5%, 8% and 10% SBR mixes were prepared for mechanical testing. Two types of floor design surfaces with and without plywood on the surface were assembled for the shock test. Gmax and HIC of this waste rubber flooring system were investigated using the compression test for the rubber cube and the drop test for the rubber pad. The criteria of general protection standards are 200g for optimum acceleration and 1000 for HIC. The Gmax and HIC results indicated that the material and system could ensure a safe fall from up to 1.0m height.

  1. Fundamentals of the knowledge about chemical additives present in rubber gloves.

    Science.gov (United States)

    Oliveira, Hegles Rosa de; Alchorne, Alice de Oliveira de Avelar

    2011-01-01

    One of the most frequent causes of allergic contact dermatitis of occupational origin are rubber additives, which are present in Personal Protective Equipment (PPE). The most allergenic additives of natural and synthetic gloves are thiurams, carbamates and mercapto group. To investigate the state of knowledge about the chemical additives used in the manufacture of synthetic rubber gloves. This was a qualitative research study in which professionals working in the manufacture, research, prescription and commercialization of gloves answered an open questionnaire. 30 individuals were interviewed: 4 researchers in occupational medicine, 5 occupational physicians, 2 occupational safety technicians, a rubber workers' union physician, an occupational safety engineer, a pro duction engineer of rubber gloves, 4 importers of gloves, a manufacturer of gloves, 3 businessmen who sell PPE, 3 salesclerks working in stores that sell PPE, 2 businessmen who own stores that sell products for allergic individuals, and 3 dermatologists. Knowledge of the chemical composition of rubber gloves is scant. The labeling of gloves, with the description of their chemical composition, would facilitate choosing the best type of glove for each person. This low-cost action to businesses would be a gain from the standpoint of public health, with huge repercussions for users of rubber gloves.

  2. Exposure to aged crumb rubber reduces survival time during a stress test in earthworms (Eisenia fetida).

    Science.gov (United States)

    Pochron, Sharon; Nikakis, Jacqueline; Illuzzi, Kyra; Baatz, Andrea; Demirciyan, Loriana; Dhillon, Amritjot; Gaylor, Thomas; Manganaro, Alexa; Maritato, Nicholas; Moawad, Michael; Singh, Rajwinder; Tucker, Clara; Vaughan, Daniel

    2018-04-01

    Solid waste management struggles with the sustainable disposal of used tires. One solution involves shredding used tires into crumb rubber and using the material as infill for artificial turf. However, crumb rubber contains hydrocarbons, organic compounds, and heavy metals, and it travels into the environment. Earthworms living in soil contaminated with virgin crumb rubber gained 14% less body weight than did earthworms living in uncontaminated soil, but the impact of aged crumb rubber on the earthworms is unknown. Since many athletic fields contain aged crumb rubber, we compared the body weight, survivorship, and longevity in heat and light stress for earthworms living in clean topsoil to those living in topsoil contaminated with aged crumb rubber. We also characterized levels of metals, nutrients, and micronutrients of both soil treatments and compared those to published values for soil contaminated with virgin crumb rubber. Consistent with earlier research, we found that contaminated soil did not inhibit microbial respiration rates. Aged crumb rubber, like new crumb rubber, had high levels of zinc. However, while exposure to aged crumb rubber did not reduce earthworm body weight as did exposure to new crumb rubber, exposure to aged crumb rubber reduced earthworm survival time during a stress test by a statistically significant 38 min (16.2%) relative to the survival time for worms that had lived in clean soil. Aged crumb rubber and new crumb rubber appear to pose similar toxic risks to earthworms. This study suggests an environmental cost associated with the current tire-recycling solution.

  3. A rare case report of peri-implant bone necrosis: Mapping the distance of initial peri-implant complication toward a path of success

    Directory of Open Access Journals (Sweden)

    S K Salaria

    2011-01-01

    Full Text Available In the past decade, science of implant placement has greatly advanced and at the same time much success has been experienced with the endosseous implant. Despite the long-term predictability of the implants, however, biological, technical and esthetic complications do occur. The use of osseointegrated implants as a foundation for prosthetic replacement of missing teeth has been highly predictable, but still at present, there is no consensus of how to best manage the complications occurring after implant placement. In this report, we discuss post-insertion complication of bone necrosis and its successful management.

  4. Performance of carbon fiber reinforced rubber composite armour against shaped charge jet penetration

    OpenAIRE

    Yue Lian-yong; Li Wei; Zu Xu-dong; Huang Zheng-xiang; Gao Zhen-yu

    2016-01-01

    Natural rubber is reinforced with carbon fiber; the protective performances of the carbonfiber reinforced rubber composite armour to shaped charge jet have been studied based on the depth of penetration experiments. The craters on the witness blocks, the nature rubber based composite plates’ deformation and the Scanning Electron Microscopy for the hybrid fiber reinforced rubber plate also is analyzed. The results showed that the composite armour can affect the stability of the jet and made pa...

  5. Supply of Rubber Wood Log in Malaysia

    OpenAIRE

    Noraida, A. W.; Abdul-Rahim, A. S.

    2014-01-01

    Issue on shortage of raw material for wood processing solved by discovery of rubber wood log as one of the substitutes the natural log. This paper examines the supply of rubber wood log in Malaysia. We employ ARDL Bound Approach Test and time series data from 1980 to 2010 which represented the whole Malaysia are used to achieve the established objectives. The result shown, in the long run harvested area and wages have 1% and 10% significant level respectively. While in the short run, there wa...

  6. Chimeric Peptides as Implant Functionalization Agents for Titanium Alloy Implants with Antimicrobial Properties

    Science.gov (United States)

    Yucesoy, Deniz T.; Hnilova, Marketa; Boone, Kyle; Arnold, Paul M.; Snead, Malcolm L.; Tamerler, Candan

    2015-04-01

    Implant-associated infections can have severe effects on the longevity of implant devices and they also represent a major cause of implant failures. Treating these infections associated with implants by antibiotics is not always an effective strategy due to poor penetration rates of antibiotics into biofilms. Additionally, emerging antibiotic resistance poses serious concerns. There is an urge to develop effective antibacterial surfaces that prevent bacterial adhesion and proliferation. A novel class of bacterial therapeutic agents, known as antimicrobial peptides (AMPs), are receiving increasing attention as an unconventional option to treat septic infection, partly due to their capacity to stimulate innate immune responses and for the difficulty of microorganisms to develop resistance towards them. While host and bacterial cells compete in determining the ultimate fate of the implant, functionalization of implant surfaces with AMPs can shift the balance and prevent implant infections. In the present study, we developed a novel chimeric peptide to functionalize the implant material surface. The chimeric peptide simultaneously presents two functionalities, with one domain binding to a titanium alloy implant surface through a titanium-binding domain while the other domain displays an antimicrobial property. This approach gains strength through control over the bio-material interfaces, a property built upon molecular recognition and self-assembly through a titanium alloy binding domain in the chimeric peptide. The efficiency of chimeric peptide both in-solution and absorbed onto titanium alloy surface was evaluated in vitro against three common human host infectious bacteria, Streptococcus mutans, Staphylococcus epidermidis, and Escherichia coli. In biological interactions such as occur on implants, it is the surface and the interface that dictate the ultimate outcome. Controlling the implant surface by creating an interface composed chimeric peptides may therefore

  7. Additive manufacturing technologies of porous metal implants

    Directory of Open Access Journals (Sweden)

    Yang Quanzhan

    2014-06-01

    Full Text Available Biomedical metal materials with good corrosion resistance and mechanical properties are widely used in orthopedic surgery and dental implant materials, but they can easily cause stress shielding due to the significant difference in elastic modulus between the implant and human bones. The elastic modulus of porous metals is lower than that of dense metals. Therefore, it is possible to adjust the pore parameters to make the elastic modulus of porous metals match or be comparable with that of the bone tissue. At the same time, the open porous metals with pores connected to each other could provide the structural condition for bone ingrowth, which is helpful in strengthening the biological combination of bone tissue with the implants. Therefore, the preparation technologies of porous metal implants and related research have been drawing more and more attention due to the excellent features of porous metals. Selective laser melting (SLM and electron beam melting technology (EBM are important research fields of additive manufacturing. They have the advantages of directly forming arbitrarily complex shaped metal parts which are suitable for the preparation of porous metal implants with complex shape and fine structure. As new manufacturing technologies, the applications of SLM and EBM for porous metal implants have just begun. This paper aims to understand the technology status of SLM and EBM, the research progress of porous metal implants preparation by using SLM and EBM, and the biological compatibility of the materials, individual design and manufacturing requirements. The existing problems and future research directions for porous metal implants prepared by SLM and EBM methods are discussed in the last paragraph.

  8. Potential of scrap tire rubber as lightweight aggregate in flowable fill.

    Science.gov (United States)

    Pierce, C E; Blackwell, M C

    2003-01-01

    Flowable fill is a self-leveling and self-compacting material that is rapidly gaining acceptance and application in construction, particularly in transportation and utility earthworks. When mixed with concrete sand, standard flowable fill produces a mass density ranging from 1.8 to 2.3 g/cm(3) (115-145 pcf). Scrap tires can be granulated to produce crumb rubber, which has a granular texture and ranges in size from very fine powder to coarse sand-sized particles. Due to its low specific gravity, crumb rubber can be considered a lightweight aggregate. This paper describes an experimental study on replacing sand with crumb rubber in flowable fill to produce a lightweight material. To assess the technical feasibility of using crumb rubber, the fluid- and hardened-state properties of nine flowable fill mixtures were measured. Mixture proportions were varied to investigate the effects of water-to-cement ratio and crumb rubber content on fill properties. Experimental results indicate that crumb rubber can be successfully used to produce a lightweight flowable fill (1.2-1.6 g/cm(3) [73-98 pcf]) with excavatable 28-day compressive strengths ranging from 269 to 1194 kPa (39-173 psi). Using a lightweight fill reduces the applied stress on underlying soils, thereby reducing the potential for bearing capacity failure and minimizing soil settlement. Based on these results, a crumb rubber-based flowable fill can be used in a substantial number of construction applications, such as bridge abutment fills, trench fills, and foundation support fills.

  9. Pemanfaatan Silika Abu Sekam Padi sebagai Bahan Pengisi Rubber Membrane Filter Press untuk Memisahkan Minyak Inti Sawit

    OpenAIRE

    Nasruddin

    2012-01-01

    This research was aimed to obtain rubber membrane filter press (RMFP) from natural rubber (NR) as well as synthetic rubber (chloroprene rubber and nytrike butadiene rubber). The research method was done my vulcanizing natural rubber, synthetic rubber, and filler to shape RMFP. Research formulation was done with 8 units of experiments using variations of mixers that have been pre-determined. The examination to the RMFP was done with ASTM test methods that cover parameters such as viscometer mo...

  10. Mechanical properties of irradiated rubber-blends

    International Nuclear Information System (INIS)

    Nasr, G.M.; Madani, M.

    2005-01-01

    A study has been made on blend ratios of natural rubber (NR) and acrylonitrile butadiene rubber (NBR) that are loaded with general purpose furnace (GPE) carbon black and irradiated at different gamma radiation doses. It was fount that the mechanical properties of such blend are highly affected by γ- irradiation dose and the composition ratios of its constituents. The elongation at break for blends was found to increase slightly with increasing NBR loafing which is mainly due to the stiffness of blending matrix formation between NR and GPF carbon black particles. The hysteresis loss, extension ratio and shape factor have been calculated for the different un-irradiated and irradiated samples

  11. Nanocomposites of nitrile (NBR) rubber with multi-walled carbon nanotubes

    Science.gov (United States)

    Warasitthinon, Nuthathai

    Nanotechnology offers the promise of creating new materials with enhanced performance. There are different kinds of fillers used in rubber nanocomposites, such as carbon black, silica, carbon fibers, and organoclays. Carbon nanotube reinforced elastomers have potential for improved rubber properties in aggressive environments. The first chapter is an introduction to the literature. The second chapter investigated the incorporation of multi-walled carbon nanotubes (MWCNTs) into rubber matrix for potential use in high temperature applications. The vulcanization kinetics of acrylonitrile butadiene rubber (NBR) reinforced with multi-walled carbon nanotubes was investigated. The vulcanized NBR rubber with different loading percentages of MWCNTs was also compared to NBR reinforced with carbon black N330. The optimum curing time at 170°C (T90) was found to decrease with increasing content of MWCNTs. Increased filler loading of both carbon black and MWCNTs gave higher modulus and strength. The MWCNTs filled materials gave better retention of modulus and tensile strength at high temperatures, but lower strength as compared to the carbon black filled samples. In the third chapter, carbon black (CB, 50phr) content in nitrile rubber (NBR) nanocomposites was partially replaced by multi-walled carbon nanotubes (MWCNTs). NBR/CB/CNTs nanocomposites with varying ratio of CB/CNTs (50/0 phr to 40/10 phr) were formulated via the melt-mixing method using an internal mixer. The reinforcing effect of single filler (CB) and mixture of fillers (CB and CNTs) on the properties of NBR nanocomposites was investigated. The cure kinetics and bound rubber content were analyzed using rheometry and solvent swelling method. In addition, mechanical behavior at both room temperature and high temperature (350°F/ 121°C) were examined. The scorch time and curing time values showed that there was no significant effect on the curing behavior of NBR nanocomposites after the partial replacement of CB with

  12. Scaling green rubber cultivation in Southwest China—An integrative analysis of stakeholder perspectives

    NARCIS (Netherlands)

    Wigboldus, Seerp; Hammond, Jim; Xu, Jianchu; Yi, Zhuang-Fang; He, Jun; Klerkx, Laurens; Leeuwis, Cees

    2017-01-01

    The rubber boom across much of Southeast Asia has led to environmental destruction, and the resultant crash in the price of rubber has destabilised livelihoods. We investigated the necessary factors required to enable a transition towards a more sustainable model for rubber cultivation in Southwest

  13. Analysis of asphalt mix surface-tread rubber interaction by using finite element method

    Directory of Open Access Journals (Sweden)

    Santosh Kumar Srirangam

    2017-08-01

    Full Text Available The surface texture of the pavement plays a very important role in driving the frictional properties at the tire rubber-pavement interface. Particularly, the hysteretic friction due to viscoelastic deformations of rubber depends mainly on the pavement surface texture. In the present paper, the effect of micromechanical pavement surface morphology on rubber block friction was brought in by comparing the friction results for three different asphalt mix morphological surfaces, named stone mastic asphalt (SMA, ultra-thin surfacing (UTS and porous asphalt (PA. The asphalt surface morphologies of these mixes were captured by using an X-ray tomographer, from which the resulting images micromechanical finite element (FE meshes for SMA, UTS and PA pavements were developed by means of the SimpleWare software. In the FE model, the rubber and asphalt binder were modeled as viscoelastic (VE materials and the formulation was given in the large deformation framework. FE simulations were then carried out by using contact algorithm between rubber and the road surface. It was observed that the rubber friction inversely varies with the sliding speed and positively varies with the pressure for all the pavement morphological and stiffness conditions. Furthermore, it was observed that the highly porous pavement surface results in large dissipation of energy, hence, large rubber friction which shows that the mix characteristics of pavements have a significant effect on rubber friction.

  14. The use of gamma radiation in preparing rubber materials for purification of waste water

    International Nuclear Information System (INIS)

    Abdel-Hamid, M.M.H.

    1997-01-01

    Waste rubber originates from rejected worn-out tyres and other waste rubber materials. To eliminate or reduce waste rubber from the environment and to reduce costs of some rubber goods, attempts are being made to reuse waste rubber. In the present work rubber powder is going to be subjected to graft copolymerization with different vinyl monomers such as acrylamide (A Am), acrylic acid (A Ac) and acrylonitrile (A N). Graft copolymerization of these monomers onto rubber powder will be carried out using gamma radiation. The effects of different parameters such as monomer concentration, radiation dose, inhibitor concentration and type of solvent used in the reaction mixture on the graft yield will be studied. The recovery of different metal ions and the parameters affecting the recovery efficiency will be studied. These parameters include the type of the metal ions such as copper, lead, cobalt, and nickel, organic pollutant such as phenol, temperature of surrounding and the type of monomers used as well as some of their derivatives

  15. Reinforcement of natural rubber/high density polyethylene blends with electron beam irradiated liquid natural rubber-coated rice husk

    Energy Technology Data Exchange (ETDEWEB)

    Chong, E.L.; Ahmad, Ishak [Polymer Research Center (PORCE), School of Chemical Science and Food Technology, Universiti Kebangsaan Malaysia 4, 43600 UKM Bangi, Selangor Darul Ehsan (Malaysia); Dahlan, H.M. [Radiation Processing Technology Division, Malaysian Nuclear Agency (Nuclear Malaysia), Bangi, 43000 Kajang, Selangor Darul Ehsan (Malaysia); Abdullah, Ibrahim, E-mail: dia@ukm.m [Polymer Research Center (PORCE), School of Chemical Science and Food Technology, Universiti Kebangsaan Malaysia 4, 43600 UKM Bangi, Selangor Darul Ehsan (Malaysia)

    2010-08-15

    Coating of rice husk (RH) surface with liquid natural rubber (LNR) and exposure to electron beam irradiation in air were studied. FTIR analysis on the LNR-coated RH (RHR) exposed to electron beam (EB) showed a decrease in the double bonds and an increase in hydroxyl and hydrogen bonded carbonyl groups arising from the chemical interaction between the active groups on RH surface with LNR. The scanning electron micrograph showed that the LNR formed a coating on the RH particles which transformed to a fine and clear fibrous layer at 20 kGy irradiation. The LNR film appeared as patches at 50 kGy irradiation due to degradation of rubber. Composites of natural rubber (NR)/high density polyethylene (HDPE)/RHR showed an optimum at 20-30 kGy dosage with the maximum stress, tensile modulus and impact strength of 6.5, 79 and 13.2 kJ/m{sup 2}, respectively. The interfacial interaction between the modified RH and TPNR matrix had improved on exposure of RHR to e-beam at 20-30 kGy dosage.

  16. Application of gamma irradiation for incorporation of rubber powder in the formulations of EPDM and natural rubber; Aplicacao da radiacao gama para incorporacao do po de borracha em formulacoes de borracha natural e EPDM

    Energy Technology Data Exchange (ETDEWEB)

    Kiyan, Ludmila Y.P.; Parra, Duclerc Fernandes; Lugao, Ademar Benevolo, E-mail: ludmilapozzo@gmail.com [Instituto de Pesquisas Energeticas e Nucleares (IPEN/CNEN-SP/CQMA), Sao Paulo, SP (Brazil). Centro de Quimica e Meio Ambiente

    2013-07-01

    The objective of this work was to study the behavior of the recycling of rubber burrs in form of powder, of the rubber industry from EPDM rubber powder and natural rubber with SBR. The rubber powder was irradiated and reused in rubber artifacts formulations for classical vulcanization. The processed material was irradiated using a {sup 60}Co source in doses of 50, 100, 150 and 200 kGy and a dose rate of 5 kGy s-1 at room temperature. The radiation created devulcanization active sites for subsequent integration of the material (rubber powder) in formulations of commercial use. The processes were compared and their products characterized by analytical methods of the physical properties such as strength and elongation. Satisfactory results were found, noting a major spin-off of EPDM chain demonstrated by increased elongation.

  17. Rubber - application of radiation to tire manufacture

    International Nuclear Information System (INIS)

    Hunt, J.D.; Alliger, G.

    1979-01-01

    Since the advent of commercial accelerators during the last several years capable of producing controllable electron beams of high energy, Firestone has devoted a considerable effort to the better understanding of the possible applications of such radiation to the production of tires or tire components. A number of chemical reactions can occur when elastomeric compounds are exposed to high energy waves, but crosslinking and degradation are the most important. The degree to which the crosslinking reaction predominates depends upon the nature of the rubber, compounding ingredients and the dosage. In general then, the effects achieved by the radiation of a rubber are quite similar to those resulting from heat. However, radiation cure or precure of compounds offers the advantage that the degree of crosslinking can be better controlled. Uniform crosslinking is possible since the high speed electrons penetrate uniformly throughout the sample. Curing with heat on the other hand may result in a greater degree of crosslinking on the surface of the sample than the center because of low heat conductivity. In general, radiation can be used to advantage to crosslink partially rubber tire components so that they retain better their shape and dimension during tire assembly and final cure or vulcanization. Added advantages of radiation precure include: a reduction of material usage, substitution of synthetic for natural rubber without loss in strength and the fact that partially crosslinked components will not thin out or become displaced during construction and vulcanization of the tire. (author)

  18. Rheological behavior of raw natural rubber coagulated by microorganisms

    Directory of Open Access Journals (Sweden)

    Zhifen Wang

    2014-01-01

    Full Text Available Tests of the strain sweep, frequency sweep and stress relaxation for raw natural rubber coagulated by microorganisms (NR-m and raw natural rubber coagulated by acid (NR-a were carried out with the use of a rubber process analyzer (RPA. The results showed that the storage torque, complex viscosity of NR-m were higher than those of NR-a while the loss factor was lower. The effect of temperature on viscosity of raw NR was studied following the Arrhenious-Frenkel-Eyring model. The viscous flow behavior of NR-m was poorer than those of NR-a. Furthermore, stress relaxation measurements of raw NR showed a longer period of relaxation for NR-m.

  19. Ground tire rubber as a stabilizer for subgrade soils : [summary].

    Science.gov (United States)

    2014-05-01

    Over 250 million scrap tires are generated : annually in the U.S. Historically, a significant : portion of these tires have been processed into : finely ground tire rubber (GTR), or crumb rubber, : for use as an additive in hot mix asphalt (HMA) : pa...

  20. Effects of leachate from crumb rubber and zinc in green roofs on the survival, growth, and resistance characteristics of Salmonella enterica subsp. enterica serovar Typhimurium.

    Science.gov (United States)

    Crampton, Mollee; Ryan, Allayna; Eckert, Cori; Baker, Katherine H; Herson, Diane S

    2014-05-01

    The use of green roofs is a growing practice worldwide, particularly in densely populated areas. In an attempt to find new methods for recycling crumb rubber, incorporation of crumb rubber into artificial medium for plant growth in green roofs and similar engineered environments has become an attractive option for the recycling of waste tires. Though this approach decreases waste in landfills, there are concerns about the leaching of zinc and other heavy metals, as well as nutrient and organic compounds, into the environment. The present study analyzed the impact of leachate from crumb rubber and zinc on the growth and viability of Salmonella enterica subsp. enterica serovar Typhimurium. Zinc was chosen for further studies since it has been previously implicated with other biological functions, including biofilm formation, motility, and possible cross-resistance to antimicrobial agents. The study showed that Salmonella can colonize crumb rubber and that crumb rubber extract may provide nutrients that are usable by this bacterium. Salmonella strains with reduced susceptibility (SRS) to zinc were obtained after subculturing in increasing concentrations of zinc. The SRS exhibited differences in gene expression of flux pump genes zntA and znuA compared to that of the parent when exposed to 20 mM added zinc. In biofilm formation studies, the SRS formed less biofilm but was more motile than the parental strain.

  1. Verification of Interactions between Silica and Epoxidized Squalene as a Model for Epoxidized Natural Rubber

    NARCIS (Netherlands)

    Kaewsakul, Wisut; Sahakaro, Kannika; Dierkes, Wilma K.; Noordermeer, Jacobus W.M.

    2014-01-01

    Unmodified squalene (Sq) and epoxidised squalene (ESq), as models for natural rubber and epoxidised natural rubber, were mixed with silica in a reactor at 140 – 145ºC, which corresponds to the optimal mixing dump temperature of silica-filled natural rubber or epoxidised natural rubber compounds. The

  2. Anodized dental implant surface

    Directory of Open Access Journals (Sweden)

    Sunil Kumar Mishra

    2017-01-01

    Full Text Available Purpose: Anodized implants with moderately rough surface were introduced around 2000. Whether these implants enhanced biologic effect to improve the environment for better osseointegration was unclear. The purpose of this article was to review the literature available on anodized surface in terms of their clinical success rate and bone response in patients till now. Materials and Methods: A broad electronic search of MEDLINE and PubMed databases was performed. A focus was made on peer-reviewed dental journals. Only articles related to anodized implants were included. Both animal and human studies were included. Results: The initial search of articles resulted in 581 articles on anodized implants. The initial screening of titles and abstracts resulted in 112 full-text papers; 40 animal studies, 16 studies on cell adhesion and bacterial adhesion onto anodized surfaced implants, and 47 human studies were included. Nine studies, which do not fulfill the inclusion criteria, were excluded. Conclusions: The long-term studies on anodized surface implants do favor the surface, but in most of the studies, anodized surface is compared with that of machined surface, but not with other surfaces commercially available. Anodized surface in terms of clinical success rate in cases of compromised bone and immediately extracted sockets has shown favorable success.

  3. Monitoring rubber plantation expansion using Landsat data time series and a Shapelet-based approach

    Science.gov (United States)

    Ye, Su; Rogan, John; Sangermano, Florencia

    2018-02-01

    The expansion of tree plantations in tropical forests for commercial rubber cultivation threatens biodiversity which may affect ecosystem services, and hinders ecosystem productivity, causing net carbon emission. Numerous studies refer to the challenge of reliably distinguishing rubber plantations from natural forest, using satellite data, due to their similar spectral signatures, even when phenology is incorporated into an analysis. This study presents a novel approach for monitoring the establishment and expansion of rubber plantations in Seima Protection Forest (SPF), Cambodia (1995-2015), by detecting and analyzing the 'shapelet' structure in a Landsat-NDVI time series. This paper introduces a new classification procedure consisting of two steps: (1) an exhaustive-searching algorithm to detect shapelets that represent a period for relatively low NDVI values within an image time series; and (2) a t-test used to determine if NDVI values of detected shapelets are significantly different than their non-shapelet trend, thereby indicating the presence of rubber plantations. Using this approach, historical rubber plantation events were mapped over the twenty-year timespan. The shapelet algorithm produced two types of information: (1) year of rubber plantation establishment; and (2) pre-conversion land-cover type (i.e., agriculture, or natural forest). The overall accuracy of the rubber plantation map for the year of 2015 was 89%. The multi-temporal map products reveal that more than half of the rubber planting activity (57%) took place in 2010 and 2011, following the granting of numerous rubber concessions two years prior. Seventy-three percent of the rubber plantations were converted from natural forest and twenty-three percent were established on non-forest land-cover. The shapelet approach developed here can be used reliably to improve our understanding of the expansion of rubber production beyond Seima Protection Forest of Cambodia, and likely elsewhere in the

  4. The computer-aided design of rubber-metal products

    Directory of Open Access Journals (Sweden)

    Pavlo S. Shvets

    2015-12-01

    Full Text Available The important problem in design of rubber-metal products is the optimization of their mass without sacrificing of proportionality factor is in the limits of standard. Aim: The aim of this work is to improve the computer-aided systems by development and implementation of improved optimization method in rubber-metal CAD systems for designers based on the reverse optimization. Materials and Methods: The paper studies the matters of computer-aided structural design of technical composite products composed of anisotropic materials that are essentially different in properties. Results: The structure of CAD systems for designers solving the problems of such design is offered and the work principles of its subsystems are described. It is shown that complicated systems optimization in CAD systems must consider as restrictions the entitative connection between separate elements of these systems within the area of the optimizing arguments. Conclusions: The problem of the “reverse” optimization when objective functions are the connectivity area parameters is considered. In many cases, this allows receiving solutions that are more effective during the computer-aided design process. The developed CAD system for designers was used during the production of rubber-metal shock absorbers at the Odessa Rubber Technical Articles Plant. The positive technical and economic effect was obtained.

  5. Tear energy and strain-induced crystallization of natural rubber/styrene-butadiene rubber blend

    International Nuclear Information System (INIS)

    Noguchi, F; Akabori, K; Yamamoto, Y; Kawahara, S; Kawazura, T

    2009-01-01

    Strain-induced crystallization of natural rubber (NR), dispersed in styrene-butadiene rubber (SBR), was investigated in relation to dimensional feature of a dispersoid and crosslink density of NR by measuring tear energy (G) of crosslinked NR/SBR blends. The crosslinked NR/SBR blends in ratios of 1/9 and 3/7 by weight were prepared by mixing masticated NR and SBR with an internal mixer at a rotor speed of 30 rpm, followed by crosslinking with dicumyl peroxide on a hot press at 444 K for 60 min. The G, measured in wide-ranges of temperature and tear rate, was superposed into a master curve with a Williams-Landel-Ferry shift factor. The G of the NR/SBR(3/7) blend abruptly decreased to a level comparable to that of SBR at about melting temperature of NR crystals formed on straining. The temperature, at which the dramatic decrease in the G occurred, was associated with the dimensional feature of the NR dispersoid and the crosslink density.

  6. Rubber Composites Based on Polar Elastomers with Incorporated Modified and Unmodified Magnetic Filler

    Directory of Open Access Journals (Sweden)

    Ján Kruželák

    2016-01-01

    Full Text Available Rubber magnetic composites were prepared by incorporation of unmodified and surface modified strontium ferrite into rubber matrices based on NBR and NBR/PVC. Strontium ferrite was dosed to the rubber matrices in concentration scale ranging from 0 to 100 phr. The main goal was to investigate the influence of the type of ferrite on the curing process, physical-mechanical and magnetic properties of composites. The mutual interactions between the filler and rubber matrices were investigated by determination of cross-link density and SEM analysis. The incorporation of magnetic fillers leads to the increase of cross-link density and remanent magnetic induction of composites. Moreover, the improvement of physical-mechanical properties was achieved in dependence on the content of magnetic fillers. Surface modification of ferrite contributed to the enhancement of adhesion on the interphase filler-rubber. It can be stated that ferrite exhibits reinforcing effect in the composite materials and this reinforcing behavior was emphasized with the increase in polarity of the rubber matrix.

  7. Wear mechanisms in ceramic hip implants.

    Science.gov (United States)

    Slonaker, Matthew; Goswami, Tarun

    2004-01-01

    The wear in hip implants is one of the main causes for premature hip replacements. The wear affects the potential life of the prosthesis and subsequent removals of in vivo implants. Therefore, the objective of this article is to review various joints that show lower wear rates and consequently higher life. Ceramics are used in hip implants and have been found to produce lower wear rates. This article discusses the advantages and disadvantages of ceramics compared to other implant materials. Different types of ceramics that are being used are reviewed in terms of the wear characteristics, debris released, and their size together with other biological factors. In general, the wear rates in ceramics were lower than that of metal-on-metal and metal-on-polyethylene combinations.

  8. Development of radiation-curable resin based on natural rubber

    Energy Technology Data Exchange (ETDEWEB)

    Mohd, Dahlan; Harun, Abdul Ghani [Nuclear Energy Unit, Bangi, Selangor (Malaysia)

    1994-12-31

    A new radiation curable resin based on natural rubber has been developed. The resin was based on the reaction between low molecular weight epoxidised natural rubber and acrylic acid. When formulated with reactive monomers and photoinitiator, it solidified upon irradiation with UV light. The resin may find applications in coating for cellulosic-based substrates and pressure-sensitive adhesive.

  9. Development of radiation-curable resin based on natural rubber

    International Nuclear Information System (INIS)

    Dahlan Mohd; Abdul Ghani Harun

    1993-01-01

    A new radiation curable resin based on natural rubber has been developed. The resin was based on the reaction between low molecular weight epoxidised natural rubber and acrylic acid. When formulated with reactive monomers and photoinitiator, it solidified upon irradiation with UV light. The resin may find applications in coating for cellulosic-based substrates and pressure-sensitive adhesive

  10. Fabrication of a Biologically-Implantable, Multiplexed, Multielectrode Array of JFETS for Cortical Implantation.

    Science.gov (United States)

    1984-12-01

    which could be implanted at the surface of the brain. Electrodes of microfine dimensions I-1 . ..6...to check the operation of the diffusion furnace oxidation tube by comparing measured thicknesses of the oxide against calculated values. Oxide Growth...faster rate than that of Eq ), (11-2). Initial adjustments made prior to using the diffusion furnace included: (1) profiling the oxidation tube to

  11. Recovering/recycling of butyl and halogenated butyl rubber via ionizing radiation

    International Nuclear Information System (INIS)

    Martin, Sandra Regina Scagliusi

    2013-01-01

    Polymeric materials (plastics and rubbers) attain a continuous and raising proportion of urban and industrial scraps discarded in landfills; their impact on environment are more and more concerning. The implementation of new technologies in order to reduce impacts of plastic waste on the environment, at an effective cost, proved to be a great problem, due to inherent complexity for polymers re-using. Ionizing radiation is capable to modify structure and properties of polymeric material. Butyl and halobutyl rubbers have been used within a comprehensive scale, applications such as tires spare parts and diverse artifacts. The major high energy photon effect, as gamma-rays in butyl and halo butyl rubbers consists in free-radicals generation along changes in mechanical properties.This work aims to the development of controlled degradation processes (devulcanization) of butyl and halo butyl (chlorine and bromine) rubbers, in order to characterize their availability for transformation and modification of properties. Experimental results obtained showed that butyl and halobutyl rubbers,irradiated at 25 kGy and further sheared, are able to be used as an initial point for mixtures with pristine. (author)

  12. The Key Points of Maintenance Therapy for Dental Implants: A Literature Review.

    Science.gov (United States)

    Pirc, Miha; Dragan, Irina F

    2017-04-01

    Dental implants require lifelong maintenance and care. Success is defined by biologic factors (presence of inflamed soft tissues surrounding dental implants and radiographic changes in the crestal bone levels) and mechanical factors (stability of the implant fixture and implant supported restoration, etc). Most implant failures are initiated by incipient stages of inflammatory processes, which lead to peri-mucositis and peri-implantitis. The evidence regarding the value of maintenance protocol regarding implants is sparse compared with the one for teeth. This article addresses the existing literature on processes for oral hygiene for implant care.

  13. Possibility of using waste tire rubber and fly ash with Portland cement as construction materials.

    Science.gov (United States)

    Yilmaz, Arin; Degirmenci, Nurhayat

    2009-05-01

    The growing amount of waste rubber produced from used tires has resulted in an environmental problem. Recycling waste tires has been widely studied for the last 20 years in applications such as asphalt pavement, waterproofing systems and membrane liners. The aim of this study is to evaluate the feasibility of utilizing fly ash and rubber waste with Portland cement as a composite material for masonry applications. Class C fly ash and waste automobile tires in three different sizes were used with Portland cement. Compressive and flexural strength, dry unit weight and water absorption tests were performed on the composite specimens containing waste tire rubber. The compressive strength decreased by increasing the rubber content while increased by increasing the fly ash content for all curing periods. This trend is slightly influenced by particle size. For flexural strength, the specimens with waste tire rubber showed higher values than the control mix probably due to the effect of rubber fibers. The dry unit weight of all specimens decreased with increasing rubber content, which can be explained by the low specific gravity of rubber particles. Water absorption decreased slightly with the increase in rubber particles size. These composite materials containing 10% Portland cement, 70% and 60% fly ash and 20% and 30% tire rubber particles have sufficient strength for masonry applications.

  14. Biorefinery methods for separation of protein and oil fractions from rubber seed kernel

    NARCIS (Netherlands)

    Widyarani, R.; Ratnaningsih, E.; Sanders, J.P.M.; Bruins, M.E.

    2014-01-01

    Biorefinery of rubber seeds can generate additional income for farmers, who already grow rubber trees for latex production. The aim of this study was to find the best method for protein and oil production from rubber seed kernel, with focus on protein recovery. Different pre-treatments and oil

  15. Neutron absorbing room temperature vulcanizable silicone rubber compositions

    International Nuclear Information System (INIS)

    Zoch, H.L.

    1979-01-01

    A neutron absorbing composition is described and consists of a one-component room temperature vulcanizable silicone rubber composition or a two-component room temperature vulcanizable silicone rubber composition in which the composition contains from 25 to 300 parts by weight based on the base silanol or vinyl containing diorganopolysiloxane polymer of a boron compound or boron powder as the neutron absorbing ingredient. An especially useful boron compound in this application is boron carbide. 20 claims

  16. Accelerated thermal aging of rubber modified epoxy encapsulants

    International Nuclear Information System (INIS)

    Sayre, J.A.

    1979-01-01

    A program is outlined to enable prediction of physical properties of rubber modified epoxy encapsulants over the life time of the extended life neutron generators. Preliminary results show that the chief aging phenomenon occurring is increased crosslink density of the epoxy matrix. No changes in the rubber phase have been detected. The effect of increased epoxy crosslink density has been higher volume resistivity at 66 0 C, increased tensile strength, and decreased ultimate elongation

  17. Influence of Plasma Treatments on the Frictional Performance of Rubbers

    NARCIS (Netherlands)

    Wolthuizen, D.J.; Martinez-Martinez, D.; Pei, Y.T.; Hosson, J.Th.M. De

    The frictional performance of several rubbers after pulsed-DC plasma treatments has been examined. In all cases, the treated rubbers showed better performance than the corresponding untreated ones. Stronger treatments, in terms of longer process time and/or higher substrate bias voltage, led to

  18. Swelling behaviour of isora/natural rubber composites in oils used

    Indian Academy of Sciences (India)

    Natural rubber/isora fibre composites were cured at various temperatures. The solvent swelling characteristics of natural rubber composites containing both untreated and alkali treated fibres were investigated in aromatic and aliphatic solvents like toluene, and -hexane. The diffusion experiments were conducted by the ...

  19. Mesoscopic Numerical Computation of Compressive Strength and Damage Mechanism of Rubber Concrete

    Directory of Open Access Journals (Sweden)

    Z. H. Xie

    2015-01-01

    Full Text Available Evaluations of both macroscopic and mesoscopic strengths of materials have been the topic of a great deal of recent research. This paper presents the results of a study, based on the Walraven equation of the production of a mesoscopic random aggregate structure containing various rubber contents and aggregate sizes. On a mesoscopic scale, the damage mechanism in the rubber concrete and the effects of the rubber content and aggregate-mortar interface on the rubber concrete’s compressive resistance property were studied. The results indicate that the random aggregate structural model very closely approximates the experimental results in terms of the fracture distribution and damage characteristics under uniaxial compression. The aggregate-mortar interface mechanical properties have a substantial impact on the test sample’s strength and fracture distribution. As the rubber content increases, the compressive strength and elastic modulus of the test sample decrease proportionally. This paper presents graphics of the entire process from fracture propagation to structural failure of the test piece by means of the mesoscopic finite-element method, which provides a theoretical reference for studying the damage mechanism in rubber concrete and performing parametric calculations.

  20. Biomaterials and biologics in craniofacial reconstruction.

    Science.gov (United States)

    Engstrand, Thomas

    2012-01-01

    Complications related to surgery, including infection, wound dehiscence, and implant protrusion, are costly and may cause severe morbidity to patients. The choice of implants materials is critical for a successful outcome, particularly in craniofacial reconstructions. This review discusses the potential benefits and drawbacks of biologically active materials used for craniofacial bone repair as alternatives to inert implant prostheses.

  1. EB-promoted recycling of waste tire rubber with polyolefins

    International Nuclear Information System (INIS)

    Meszaros, L.; Barany, T.; Czvikovszky, T.

    2011-01-01

    Complete text of publication follows. One of the principal problems of common recycling of technical polymers is the thermodynamical incompatibility. The change of the Gibbs 'free energy' during the mixing - determined by the changes of enthalpy and entropy - should be directed towards the miscibility. In most of cases, even between closely related polymers, the compatibility is on low level which leads to phase separation and weak adhesion between the phases. Radiation treatment may help in this problem making the polymers more compatible by creating covalent bonds between the polymer phases. Such problem arises at the recycling of ground tire rubbers (GTR). The rubber properties of GTR could be utilized by mixing the GTR with thermoplastic olefins. With the aid of radiation treatment the rubber-like properties of these types of thermoplastic elastomers can be increased. In this study polyethylene (PE) (50-70 wt%) as thermoplastic olefin, 30 wt% of GTR and ethylene vinyl acetate (EVA) (0-20 wt%) as rubber-like compatibilizing material were used for preparation of a recycled rubber containing blend, processable by thermoplastic processes. The melt-mixing of the samples was made by extrusion and then the test specimens were injection molded. The injection molded samples were than treated by high energy electron beam. On the specimens tensile tests, hysteresis, falling weight impact tests, hardness measurements, and dynamic mechanical thermal analysis (DMA) were carried out. The results proved the benefit of the electron beam treatment.

  2. The Rubber Tail Illusion as Evidence of Body Ownership in Mice.

    Science.gov (United States)

    Wada, Makoto; Takano, Kouji; Ora, Hiroki; Ide, Masakazu; Kansaku, Kenji

    2016-10-26

    The ownership of one's body parts represents a fundamental aspect of self-consciousness. Accumulating empirical evidence supports the existence of this concept in humans and nonhuman primates, but it is unclear whether nonprimate mammals experience similar feelings. Therefore, the present study used rubber tails to investigate body ownership in rodents. When the real tails and rubber tails were synchronously stroked, the mice responded as if their own tails were touched when the rubber tails were grasped. In contrast, when the stimuli were delivered asynchronously, there was a significantly lower mean response rate when the rubber tail was grasped. These findings suggest that mice may experience body ownership of their tails, suggestive of the rubber hand illusion in humans. To explore the manner in which the ownership of body parts is experienced, this study specifically used the rubber hand illusion (RHI), in which self-consciousness can be extended out of one's own body. Accumulating empirical evidence supports the existence of this concept in humans and nonhuman primates, but it remains unclear whether nonprimate mammals experience similar feelings. This study demonstrated for the first time that mice may experience body ownership of their tails, which is suggestive of the RHI in humans and provides evidence that may highlight how humans experience the ownership of body parts. Copyright © 2016 the authors 0270-6474/16/3611133-05$15.00/0.

  3. Radiation vulcanization of Philippine natural rubber latex

    International Nuclear Information System (INIS)

    Dela Rosa, Alumanda M.; Abad, Lucille V.; Sta, Lorna P.; Ana-Relleve; Tranquilan-Aranilla, Charito O.; Pascual, Cristina L.

    1996-01-01

    The response of Philippine natural rubber latex to radiation vulcanization and the stability of the irradiated natural rubber latex (INRL) upon storage and aging were investigated. Commercially available high ammonia (HA) concentrated lattices obtained from various rubber plantations in Mindanao Island were treated with 5 phr of n-butyl acrylate (nBA), and gamma-irradiated at the PNRI sup 60 Co irradiation facility at dose rate of 2.57 KGy/hr. Unirradiated cast latex films gave different green strength which varied from 2 - 11 MPa. Cast films from INRL exhibited maximum tensile strengths of 25 - 32 MPa at a radiation dose of 15 kGy. Higher tensile strengths were obtained from cast films with low Mg and high nitrogen contents. Thermal analysis using thermogravimetry (TG) revealed one major decomposition product at 374 degree C - 377 degree C. Its rate of decomposition decreased to a minimum at 15 kGy, then increased as radiation dose increased. This trend correlated well with the tensile strength measurements. The stability of the INRL upon storage and aging is an essential parameter to the rubber latex industry. For storage studies, INRL was stored for various periods of time. It was found that the pH and total solids content of the stored INRL did not change significantly after 12 months of storage; the MST values remained at above 100 seconds, and the viscosity decreased with time. The cast films exhibited a decline in tensile strength, modulus 300% and crosslinking density upon storage. While there were observed changes in the physical properties of the IRNL during the storage period, the data indicate that these properties were within values acceptable to the latex industry. Tests on the aging properties of INRL film were undertaken. It was shown that among the chemical antioxidants presently used by the latex industry. TNPP demonstrated the highest antioxidant property, followed by Antage DAHQ and Vulcanox BKF. Our data indicate that the natural rubber latex

  4. Psychosis-proneness and the rubber hand illusion of body ownership.

    Science.gov (United States)

    Germine, Laura; Benson, Taylor Leigh; Cohen, Francesca; Hooker, Christine I'lee

    2013-05-15

    Psychosis and psychosis-proneness are associated with abnormalities in subjective experience of the self, including distortions in bodily experience that are difficult to study experimentally due to lack of structured methods. In 55 healthy adults, we assessed the relationship between self-reported psychosis-like characteristics and susceptibility to the rubber hand illusion of body ownership. In this illusion, a participant sees a rubber hand being stroked by a brush at the same time that they feel a brush stroking their own hand. In some individuals, this creates the bodily sense that the rubber hand is their own hand. Individual differences in positive (but not negative) psychosis-like characteristics predicted differences in susceptibility to experiencing the rubber hand illusion. This relationship was specific to the subjective experience of rubber hand ownership, and not other unusual experiences or sensations, and absent when a small delay was introduced between seeing and feeling the brush stroke. This indicates that individual differences in susceptibility are related to visual-tactile integration and cannot be explained by differences in the tendency to endorse unusual experiences. Our findings suggest that susceptibility to body representation distortion by sensory information may be related or contribute to the development of psychosis and positive psychosis-like characteristics. Copyright © 2012 Elsevier Ireland Ltd. All rights reserved.

  5. Influence of the Rubber Seed Type and Altitude on Characteristic of Seed, Oil and Biodiesel

    OpenAIRE

    Salni, Salni; Hariani, Poedji Loekitowati; Hanifa, Hanifa Marisa

    2017-01-01

    This research studies the influence of the type of rubber seed that is superior and local, altitude plant in South Sumatra province to the characteristic of seed, oil and biodiesel (methyl ester). Rubber plants planted from local rubber seed by seeds seedlings and superior rubber seed by selected clones. In the study, rubber plants planted at a different altitude, namely in Banyuasin district (18 m above sea level), Prabumulih District (176 m above sea level) and Lahat District (627 m above s...

  6. Pengaruh Penggunaan Nitril Butadiene Rubber Dan Pale Crepe Pada Pembuatan Sol Karet Untuk Sepatu Pengaman

    OpenAIRE

    Yuniari, Arum

    2010-01-01

    Rubber sole for safety shoes was different on physical specification with general sole, especially on abrasion resistance and oil resistance. The objective of the study was to determine the effect of nitril butadiene rubber and pale crepe on physical properties of vulcanized rubber sole for safety shoes. Rubber sole for safety shoes was produced by blending pale crepe and nitril butadiene rubber with ratio of : 50/50; 60/40; 70/30 and 80/20 phr, respectively. Carbon black as filler was also v...

  7. Pengaruh penggunaan nitril butadiene rubber dan pale crepe pada pembuatan sol karet untuk sepatu pengaman

    OpenAIRE

    Arum Yuniari

    2010-01-01

    Abstract Rubber sole for safety shoes was different on physical specification with general sole, especially on abrasion resistance and oil resistance. The objective of the study was to determine the effect of nitril butadiene rubber and pale crepe on physical properties of vulcanized rubber sole for safety shoes. Rubber sole for safety shoes was produced by blending pale crepe and nitril butadiene rubber with ratio of : 50/50; 60/40; 70/30 and 80/20 phr, respectively. Carbon black as fill...

  8. Study on grafting of different types of acrylic monomers onto natural rubber by γ-rays

    International Nuclear Information System (INIS)

    Dafader, N.C.; Haque, M.E.; Akhtar, F.; Ahmad, M.U.

    2006-01-01

    A comparative study of various acrylic monomers for grafting onto natural rubber was done. The stability of natural rubber latex (NRL) against coagulum with monomer, mechanical properties of grafted rubbers and percent of grafting were investigated. The NRL with monomers, methylacrylate (MA), ethylacrylate (EA) and n-butylacrylate (n-BA), is unstable but it is stable with methyl methacrylate (MMA), n-butyl methacrylate (BMA) and cyclohexyl methacrylate (CHMA). The mechanical properties and degree of grafting attained a maximum at a total radiation dose of 4 kGy. The values of tensile properties of MMA and CHMA grafted rubbers are almost similar, and higher than those of BMA grafted rubbers. On the other hand, the degree of grafting for CHMA is higher than those of MMA and BMA grafted rubbers. The infrared (IR) spectra of monomer grafted natural rubber were also studied

  9. Vulcanization of rubber mixtures by simultaneous electron beam and microwave irradiation

    Energy Technology Data Exchange (ETDEWEB)

    Martin, D. E-mail: martin@ifin.nipne.ro; Ighigeanu, D.; Mateescu, E.; Craciun, G.; Ighigeanu, A

    2002-08-01

    The comparative results obtained by applying separate electron beam (EB) irradiation and simultaneous EB and microwave (MW) irradiation to vulcanization of rubber mixtures based on natural rubber and polybutadiene rubber with carbon black are presented. In the absence of MW, EB irradiation doses of 200-250 kGy are required in order to obtain a higher vulcanization degree. The irradiation doses as well as irradiation times were markedly diminished, from 2 to 6 times, by simultaneous EB and MW irradiation.

  10. Surface Engineering for Bone Implants: A Trend from Passive to Active Surfaces

    Directory of Open Access Journals (Sweden)

    John Jansen

    2012-07-01

    Full Text Available The mechanical and biological properties of bone implants need to be optimal to form a quick and firm connection with the surrounding environment in load bearing applications. Bone is a connective tissue composed of an organic collagenous matrix, a fine dispersion of reinforcing inorganic (calcium phosphate nanocrystals, and bone-forming and -degrading cells. These different components have a synergistic and hierarchical structure that renders bone tissue properties unique in terms of hardness, flexibility and regenerative capacity. Metallic and polymeric materials offer mechanical strength and/or resilience that are required to simulate bone tissue in load-bearing applications in terms of maximum load, bending and fatigue strength. Nevertheless, the interaction between devices and the surrounding tissue at the implant interface is essential for success or failure of implants. In that respect, coatings can be applied to facilitate the process of bone healing and obtain a continuous transition from living tissue to the synthetic implant. Compounds that are inspired by inorganic (e.g., hydroxyapatite crystals or organic (e.g., collagen, extracellular matrix components, enzymes components of bone tissue, are the most obvious candidates for application as implant coating to improve the performance of bone implants. This review provides an overview of recent trends and strategies in surface engineering that are currently investigated to improve the biological performance of bone implants in terms of functionality and biological efficacy.

  11. Thermomyces lanuginosus STm: a source of thermostable hydrolytic enzymes for novel application in extraction of high-quality natural rubber from Taraxacum kok-saghyz (rubber dandelion)

    Science.gov (United States)

    Hydrolytic enzymes from a newly isolated strain of the thermophilic fungus Thermomyces lanuginosus were used to extract rubber from Taraxacum kok-saghyz commonly known as rubber (or Russian or Kazak(h)) dandelion. The fungus was isolated from garden soil and identified as Thermomyces lanuginosus STm...

  12. Rubber Flooring Impact on Production and Herdlife of Dairy Cows

    Science.gov (United States)

    Use of rubber flooring in dairies has become popular because of perceived cow comfort. The overall objective of this longitudinal study was to evaluate production, reproduction, and retention of first and second lactations of cows assigned to either rubber (RUB) or concrete (CON) flooring at the fe...

  13. Best Practice for the Devulcanization of Sulfur-cured SBR Rubber

    NARCIS (Netherlands)

    Saiwari, Sitisaiyidah; Dierkes, Wilma K.; Noordermeer, Jacobus W.M.; Blume, Anke

    2015-01-01

    In the present paper, special attention will be devoted to thermo-chemical devulcanization of sulfur-cured styrene butadiene rubber (SBR) using diphenyldisulfide (DPDS) as devulcanization aid. SBR is the main component in whole passenger car tire rubber and, at the same time, the most critical one

  14. Microwave pre-heating of natural rubber using a rectangular wave guide (MODE: TE10

    Directory of Open Access Journals (Sweden)

    Doo-ngam, N.

    2007-11-01

    Full Text Available This paper presents an application of microwave radiation for pre-heating of natural rubbercompounding with various sulphur contents. The natural rubber-compounding was pre-heated by microwave radiation using a rectangular wave guide system (MODE: TE10 operating at frequency of 2.45 GHz in which the power can vary from 0 to 1500 W. In the present work, the influence of power input, sample thickness, and sulphur content were examined after applying microwave radiation to the rubber samples. Results are discussed regarding the thermal properties, 3-D network, dielectric properties and chemical structures. From the result, firstly, it was found that microwave radiation can be applied to pre-heating natural rubber-compounding before the vulcanization process. Secondly, microwave radiation was very useful for pre-heating natural rubber-compounding that has a thickness greater than 5mm. Thirdly, crosslinking in natural rubber-compounding may occurs after pre-heating by microwave radiation though Fourier Transform Infrared Spectroscopy(FTIR. Finally, there a little effect of sulphur content on temperature profiles after applying microwave radiation to the natural rubber-compounding. Moreover, natural rubber-compounding without carbon black showed a lower heat absorption compared with natural rubbercompounding filled carbon black. This is due to the difference in dielectric loss factor. This preliminary result will be useful information in terms of microwave radiation for pre-heating natural rubber-compounding and rubber processing in industry.

  15. Influence of gamma and e-beam irradiation on microhardness of recycled polyolefin-rubber composites

    International Nuclear Information System (INIS)

    Atabaev, B.G.; Gafurov, U.G.; Fainleib, A.M.; Tolstov, A.

    2006-01-01

    Full text: The dose dependencies of surface Vickers microhardness (H) for gamma and e-beam irradiated (E=5 MeV) recycled polyethylene-rubber and polypropylene-rubber composites has been investigated. The new techniques for measuring of polymer surface microhardness using decoration of indenter imprint under load lower 100g are developed. The measurements under 50g load shown the microhardness sharp decreasing for e-beam irradiation up to dose 50-150 kGy. The optimal dose D opt for improving of viscoelastic properties at minimal microhardness HV for HDPE-rubber blends-100 kGy and PP-rubber blends-75 kGy are defined. The microhardness change depend on irradiation dose can be explained by concurrence of irradiation stimulated chain cross-linking, oxidation and destruction processes. In our work samples of polyolefin powder were irradiated in air to form peroxide and hydroperoxide groups and heated to form polar groups capable of improving the compatibility with the radiation devulcanized rubber particles. The absolute value of microhardness of polyolefin-rubber composites extremely low for polyolefins and close to microhardness of high elastic rubber. The viscoelastic properties can be explained by new model of formation mixing amorphous interface between semicrystalline polyolefin and devulcanized rubber. The work was supported by EC (STCU Project U3009). (author)

  16. Devulcanization of ground tire rubber: Physical and chemical changes after different microwave exposure times

    Directory of Open Access Journals (Sweden)

    P. S. Garcia

    2015-11-01

    Full Text Available Microwave devulcanization is known to be a promising and an efficient rubber recycling method which makes possible for the rubber to regain its fluidity, and makes it capable of being remolded and revulcanized. The focus of this work is to understand the physical and chemical changes that occur in the ground tire rubber after different microwave exposure periods. For this purpose chemical, thermal, rheological and morphological analyses were performed on the tire rubber, which contains natural rubber (NR and styrene-butadiene rubber (SBR as polymeric material. The results showed that the microwave treatment promoted the breaking of sulfur cross-links and consequently increased the rubber fluidity. However, long periods of exposure led to degradation and modification of some properties. At nanoscale, the deformation of the devulcanized NR domain under stress was observed, and the morphology obtained appears to be a droplet dispersion morphology. The most exposed samples presented only one glass transition temperature, and from this it was concluded that the treatment may have played an important role in the compatibilization of the elastomeric blend. Based on the results, it is required to control the microwave exposure time and polymeric degradation in order to achieve a regenerated rubber with satisfactory properties.

  17. The Study of Government’s Role for Welfaring Rubber Farmer in The Globalization Vortex

    Directory of Open Access Journals (Sweden)

    Pahrudin HM

    2017-12-01

    Full Text Available Rubber is a type of plant that has been cultivated by the people of Indonesia for long a time. Until now, farmers have become the largest party to cultivate rubber in Indonesia (85.10% and contribute greatly to the nation’s economy, but are still far from prosperous. Rubber products produced by farmers are priced cheap so that they incomes are very small and create income inequality. As an export commodity, rubber is highly dependent with overseas which determines the price. In this context, the government through the bureaucratic system serves to produce a series of innovative-solutive development program in order to keep the people from the negative impacts of globalization. This effort can be run by the government with adopting The New Public Service Paradigm as part of efforts to better public services for the people. It is implementation in the form of domestic rubber needs priorities, bringing the industry to the center of rubber, training of rubber farmers, and improvement of transportation infrastructures.

  18. Linear motion feed through with thin wall rubber sealing element

    Science.gov (United States)

    Mikhailov, V. P.; Deulin, E. A.

    2017-07-01

    The patented linear motion feedthrough is based on elastic thin rubber walls usage being reinforced with analeptic string fixed in the middle part of the walls. The pneumatic or hydro actuators create linear movement of stock. The length of this movement is two times more the rubber wall length. This flexible wall is a sealing element of feedthrough. The main advantage of device is negligible resistance force that is less then mentioned one in sealing bellows that leads to positioning error decreasing. Nevertheless, the thin wall rubber sealing element (TRE) of the feedthrough is the main unreliable element that was the reason of this element longevity research. The theory and experimental results help to create equation for TRE longevity calculation under vacuum or extra high pressure difference action. The equation was used for TRE longevity determination for hydraulic or vacuum equipment realization also as it helps for gas flow being leaking through the cracks in thin walls of rubber sealing element of linear motion feedthrough calculation.

  19. Novel in situ coordinated cerium salt/acrylonitrile-butadiene rubber composite

    International Nuclear Information System (INIS)

    Han, Jianjun; Lu, Haifeng; Zhang, Jie; Feng, Shengyu

    2012-01-01

    A novel rubber composite of acrylonitrile-butadiene rubber (NBR) filled with cerium salt particles was vulcanized via in situ coordination for the first time. The resulting materials exhibit good mechanical properties. Curing characteristics analysis, differential scanning calorimetry, X-ray photoelectron spectroscopy, tensile testing, and an equilibrium swelling method were used for the characterization of the composite. The results in this paper indicate that the composite is a kind of elastomer based on the in situ coordination crosslinking interactions between the nitrile groups (–CN) of NBR and cerium ions. The mechanical properties of vulcanized cerium salt/ NBR rubber are altered when changing the sorts of cerium salt. Moreover, these materials show good irradiation resistance because of the introduction of the cerium salt. -- Highlights: ► Cerium salts were firstly used to vulcanize the acrylonitrile-butadiene rubber. ► Cerium salts act as not only crosslink agents but also reinforcing fillers in the matrix. ► These materials show good irradiation resistance and mechanical properties at same time.

  20. Experimental Study and Dynamic Modeling of Metal Rubber Isolating Bearing

    International Nuclear Information System (INIS)

    Zhang, Ke; Zhou, Yanguo; Jiang, Jian

    2015-01-01

    In this paper, dynamic shear mechanical properties of a new metal rubber isolating bearing is tested and studied. The mixed damping model is provided for theoretical modeling of MR isolating bearing, the shear stiffness and damping characteristics of the MR bearing can be analyzed separately and easily discussed, and the mixed damping model is proved to be an rather effective approach. The test results indicate that loading frequency bears little impact over shear property of metal rubber isolating bearing, the total energy consumption of metal rubber isolating bearing increases with the increase in loading amplitude. With the increase in loading amplitude, the stiffness of the isolating bearing will reduce showing its “soft property”; and the type of damping force gradually changes to be close to dry friction. The features of “soft property” and dry friction energy consumption of metal rubber isolating bearing are very useful in practical engineering application. (paper)

  1. A Study for Shelf Life Evaluation of Rubber O-ring

    International Nuclear Information System (INIS)

    Jung, Sun Chul; Kim, Jong Seog

    2005-01-01

    Non-metallic materials stored in warehouses in nuclear power plants have shelf life. The shelf life means the maximum storage time allowable such that the install life of the material is not affected. Materials whose shelf lives expire are generally discarded. unless the shelf lives of these materials can be extended by reducing the install life. Examples of this case are rubber materials. Rubber materials are widely used for sealing of various machines. There are various life evaluation methods for rubber material. For example, the compression set is generally used for evaluation the aging condition of rubber materials used for sealing. A compression set value can be calculated according to the ASTM D395. We have tried the compression set test by using specimens with 6.99mm diameter O-ring even when ASTM D 395 recommends the use of bar specimen. Test results and comparison between O-ring and reference data of EPRI NP-6608 are presented below

  2. Physical-chemical characterization and biological assessment of simple and lithium-doped biological-derived hydroxyapatite thin films for a new generation of metallic implants

    Science.gov (United States)

    Popescu, A. C.; Florian, P. E.; Stan, G. E.; Popescu-Pelin, G.; Zgura, I.; Enculescu, M.; Oktar, F. N.; Trusca, R.; Sima, L. E.; Roseanu, A.; Duta, L.

    2018-05-01

    We report on the synthesis by PLD of simple and lithium-doped biological-origin hydroxyapatite (HA) films. The role of doping reagents (Li2CO3, Li3PO4) on the morphology, structure, chemical composition, bonding strength and cytocompatibility of the films was investigated. SEM investigations of the films evidenced a surface morphology consisting of particles with mean diameters of (5-7) μm. GIXRD analyses demonstrated that the synthesized structures consisted of HA phase only, with different degrees of crystallinity, mainly influenced by the doping reagent type. After only three days of immersion in simulated body fluid, FTIR spectra showed a remarkable growth of a biomimetic apatitic film, indicative of a high biomineralization capacity of the coatings. EDS analyses revealed a quasi-stoichiometric target-to-substrate transfer, the values inferred for the Ca/P ratio corresponding to a biological apatite. All synthesized structures displayed a hydrophilic behavior, suitable for attachment of osteoblast cells. In vitro cell viability tests showed that the presence of Li2CO3 and Li3PO4 as doping reagents promoted the hMSC growth on film surfaces. Taking into consideration these enhanced characteristics, corroborated with a low fabrication cost generated by sustainable resources, one should consider the lithium-doped biological-derived materials as promising prospective solutions for a next generation of coated implants with rapid osteointegration.

  3. Effect of high-energy radiation on the rheological characteristics and structure of liquid rubbers

    International Nuclear Information System (INIS)

    Govorkov, A.T.; Zaitseva, V.I.; Muryshkin, D.L.; Safonov, Yu.N.

    1987-01-01

    The effect of high-energy radiation (γ-radiation and accelerated electrons) on liquid polybutadiene and polyisoprene rubbers (SKD, SKD-KTR, SKN) and butyl rubber (BR) was studied by IR and EPR spectroscopy, rheoviscosimetry, and chemical analysis. Newtonian flow was conserved in the rubbers under irradiation. The activation energy of viscous flow was unchanged, evidence of an increase in the contour length of the macromolecules without significant branching and cross-linking at the initial stages of the irradiation. A quantitative relationship was established between the rubber's dynamic viscosity and the absorbed dose, and features of the structure-formation mechanism in the liquid rubbers were determined

  4. High Performance Graphene Oxide Based Rubber Composites

    Science.gov (United States)

    Mao, Yingyan; Wen, Shipeng; Chen, Yulong; Zhang, Fazhong; Panine, Pierre; Chan, Tung W.; Zhang, Liqun; Liang, Yongri; Liu, Li

    2013-01-01

    In this paper, graphene oxide/styrene-butadiene rubber (GO/SBR) composites with complete exfoliation of GO sheets were prepared by aqueous-phase mixing of GO colloid with SBR latex and a small loading of butadiene-styrene-vinyl-pyridine rubber (VPR) latex, followed by their co-coagulation. During co-coagulation, VPR not only plays a key role in the prevention of aggregation of GO sheets but also acts as an interface-bridge between GO and SBR. The results demonstrated that the mechanical properties of the GO/SBR composite with 2.0 vol.% GO is comparable with those of the SBR composite reinforced with 13.1 vol.% of carbon black (CB), with a low mass density and a good gas barrier ability to boot. The present work also showed that GO-silica/SBR composite exhibited outstanding wear resistance and low-rolling resistance which make GO-silica/SBR very competitive for the green tire application, opening up enormous opportunities to prepare high performance rubber composites for future engineering applications. PMID:23974435

  5. Status of surface treatment in endosseous implant: A literary overview

    Directory of Open Access Journals (Sweden)

    Gupta Ankur

    2010-01-01

    Full Text Available The attachment of cells to titanium surfaces is an important phenomenon in the area of clinical implant dentistry. A major consideration in designing implants has been to produce surfaces that promote desirable responses in the cells and tissues. To achieve these requirements, the titanium implant surface can be modified in various ways. This review mainly focuses on the surface topography of dental implants currently in use, emphasizing the association of reported variables with biological outcome.

  6. Implant-supported removable partial dentures in the mandible: A 3-16 year retrospective study.

    Science.gov (United States)

    Jensen, Charlotte; Meijer, Henny J A; Raghoebar, Gerry M; Kerdijk, Wouter; Cune, Marco S

    2017-04-01

    The purpose of this retrospective study was to assess performance, together with biological and technical complications, of implant-supported removable partial dentures (ISRPD) in mandibular Kennedy class I situations with implants placed in the anterior or posterior position. 23 subjects with two endosseous implants to support a bilateral-free-ending mandibular removable denture were examined. Eight subjects had implants in the premolar (anterior) region and 15 subjects implants in the molar (posterior) region. Biological and technical complications were recorded from the patients' medical record. Patients filled out a validated questionnaire regarding their appreciation of oral health related quality of life (OHIP-NL49) and a VAS score on overall satisfaction. Over a mean follow-up period of 8 years (median 8 years, range 3-16 years) the cumulative implant survival rate was 91.7% (SE 0.05). Mean peri-implant bone loss was 0.9mm (SD 1.0mm). Scores for bleeding on probing, plaque and mucosal health were generally low, but significantly worse for posteriorly placed implants. Significantly more biological complications occurred in the posterior group (X 2 (1)=3.9; p=0.048). In 65% of the cases no technical complications were registered. Mean overall OHIP score was 16.1 (SD 18.4) and patients were highly satisfied (VAS: 8.4; SD 2.1). Within the limitations of this retrospective study, in case of a Kennedy class I situation in the mandible, an ISRPD is a viable treatment option with a high implant survival rate and satisfied patients after a maximum of 16 years. Technical and biological complications should be anticipated. Anteriorly placed implants performed slightly better. Copyright © 2016 Japan Prosthodontic Society. Published by Elsevier Ltd. All rights reserved.

  7. Why dentists don't use rubber dam during endodontics and how to promote its usage?

    Science.gov (United States)

    Madarati, Ahmad A

    2016-02-25

    This survey study aimed at investigating the frequency of rubber dam use during root canal treatment, identifying influencing factors for not using it by Saudi general dental practitioners (GDPs) and endodontists. It also aimed at identifying measures that increase rubber dam usage. After obtaining an ethical approval, two pilot studies were conducted on staff members at Taibah University College of Dentistry and a group of GDPs. A final online survey was constructed comprising 17 close-ended questions divided into six categories: demographics, endodontic practice, rubber dam use, alternative isolation methods, reasons for not using rubber dam, and measures and policies that increase its usage. The survey was emailed to 375 GDPs randomly selected from the dental register and all endodontists (n = 53) working in the western province, Saudi Arabia. Data were analyzed using the Chi-square and Linear-by-Linear association tests at p ≤ 0.05. The proportion of endodontists who used rubber dam (84.8 %) was significantly greater than that of GDPs (21.6 %) (p < 0.001). Significantly the highest proportion (40.5 %) did not use rubber dam because of unavailability at working place. Most rubber dam none-users (69.25 %) used a combination of other isolation means. The highest proportion of those who used rubber dam were working in the governmental sector (54.3 %). Among rubber dam users, the greatest proportion graduated from Saudi Arabia (57.8 %) compared to those graduated from Egypt (34.3 %) and Syria (22.4 %). There was a significant correlation between the patterns of rubber dam use during undergraduate training and its usage after graduation (p = 0.001). The highest proportion of participants (48.1 %) reported better undergraduate education as the most important factor that would increase rubber dam use in dental practice. Using of rubber dam was not common in Saudi general dental practice. Dentists must follow the recommended standards of care. Place of work and

  8. Strategies to improve the adhesion of rubbers to adhesives by means of plasma surface modification

    Science.gov (United States)

    Martín-Martínez, J. M.; Romero-Sánchez, M. D.

    2006-05-01

    The surface modifications produced by treatment of a synthetic sulfur vulcanized styrene-butadiene rubber with oxidizing (oxygen, air, carbon dioxide) and non oxidizing (nitrogen, argon) RF low pressure plasmas, and by treatment with atmospheric plasma torch have been assessed by ATR-IR and XPS spectroscopy, SEM, and contact angle measurements. The effectiveness of the low pressure plasma treatment depended on the gas atmosphere used to generate the plasma. A lack of relationship between surface polarity and wettability, and peel strength values was obtained, likely due to the cohesive failure in the rubber obtained in the adhesive joints. In general, acceptable adhesion values of plasma treated rubber were obtained for all plasmas, except for nitrogen plasma treatment during 15 minutes due to the creation of low molecular weight moieties on the outermost rubber layer. A toluene wiping of the N{2 } plasma treated rubber surface for 15 min removed those moieties and increased adhesion was obtained. On the other hand, the treatment of the rubber with atmospheric pressure by means of a plasma torch was proposed. The wettability of the rubber was improved by decreasing the rubber-plasma torch distance and by increasing the duration because a partial removal of paraffin wax from the rubber surface was produced. The rubber surface was oxidized by the plasma torch treatment, and the longer the duration of the plasma torch treatment, the higher the degree of surface oxidation (mainly creation of C O moieties). However, although the rubber surface was effectively modified by the plasma torch treatment, the adhesion was not greatly improved, due to the migration of paraffin wax to the treated rubber-polyurethane adhesive interface once the adhesive joint was produced. On the other hand, the extended treatment with plasma torch facilitated the migration of zinc stearate to the rubber-adhesive interface, also contributing to deteriorate the adhesion in greater extent. Finally

  9. Preparation of composites of national rubber latex (NRL) - portland cement mould. Vol. 3

    International Nuclear Information System (INIS)

    Dessouki, A.M.; Taher, N.H.; El-Nahas, H.H.

    1996-01-01

    The aim of this study is to prepare some polymeric mould using national rubber latex (NRL) - portland cement composites based on a delayed- action mechanism. Factors affecting the preparation process such as concentration, mixing percentage, additives and their effect on what is regarded as a delayed action coacervant combination was studied. Composites of national latex (NRL) - portland cement would were prepared as two separate parts. The stabilized natural rubber latex (NRL) 100 parts with hydroxy ethyl cellulose (HEC) 2 parts as stabilizer and a delayed - action coacervant (sodium meta silicate as a delaying agent) 5 parts on one hand and the dry blend of cement 65 parts soluble in 65 parts of water as a paste on the other hand were mixed thoroughly on site. (HEC) was added to the rubber latex to prevent the coagulation of the rubber latex with the electrolyte (sodium meta silicate) present in the rubber mixture. Two kinds of stabilization occurred in the rubber part, namely steric stabilization and the stabilization against electrolyte. The effect of delayed - action coacervant (sodium meta silicate) on the initial setting time of rubber - cement mould showed that the molding process did not occur at sodium meta silicate concentration less than 2.66 parts per 100 parts of rubber latex (phr), and the optimum concentration used was 5% parts of rubber latex. It was observed that addition of a delaying agent (Sodium meta silicate) to the rubber part enhanced the delaying mechanism in the time needed for the molding process, while the addition of the delaying agent to the cement part did not have any effect on retardation of the molding process. Chemical coacervants function mainly by reducing the ζ potential which is associated with the electrical double layer surrounding the latex particle. This reduction may brought about in at least three distinct ways which take place in the system studied. 5 figs., 3 tabs

  10. Preparation of composites of national rubber latex (NRL) - portland cement mould. Vol. 3

    Energy Technology Data Exchange (ETDEWEB)

    Dessouki, A M; Taher, N H; El-Nahas, H H [National Center for Radiation Research and Technology, Atomic Energy Athority, Cairo (Egypt)

    1996-03-01

    The aim of this study is to prepare some polymeric mould using national rubber latex (NRL) - portland cement composites based on a delayed- action mechanism. Factors affecting the preparation process such as concentration, mixing percentage, additives and their effect on what is regarded as a delayed action coacervant combination was studied. Composites of national latex (NRL) - portland cement would were prepared as two separate parts. The stabilized natural rubber latex (NRL) 100 parts with hydroxy ethyl cellulose (HEC) 2 parts as stabilizer and a delayed - action coacervant (sodium meta silicate as a delaying agent) 5 parts on one hand and the dry blend of cement 65 parts soluble in 65 parts of water as a paste on the other hand were mixed thoroughly on site. (HEC) was added to the rubber latex to prevent the coagulation of the rubber latex with the electrolyte (sodium meta silicate) present in the rubber mixture. Two kinds of stabilization occurred in the rubber part, namely steric stabilization and the stabilization against electrolyte. The effect of delayed - action coacervant (sodium meta silicate) on the initial setting time of rubber - cement mould showed that the molding process did not occur at sodium meta silicate concentration less than 2.66 parts per 100 parts of rubber latex (phr), and the optimum concentration used was 5% parts of rubber latex. It was observed that addition of a delaying agent (Sodium meta silicate) to the rubber part enhanced the delaying mechanism in the time needed for the molding process, while the addition of the delaying agent to the cement part did not have any effect on retardation of the molding process. Chemical coacervants function mainly by reducing the {zeta} potential which is associated with the electrical double layer surrounding the latex particle. This reduction may brought about in at least three distinct ways which take place in the system studied. 5 figs., 3 tabs.

  11. Genomic validation of PB 260 clone of rubber (Hevea brasiliensis) at Cikumpay Plantation by SSR marker

    Science.gov (United States)

    Royani, J. I.; Safarrida, A.; Rachmawati, I.; Khairiyah, H.; Mustika, I. P.; Suyono, A.; Rudiyana, Y.; Kubil; Nurjaya; Arianto, A.

    2017-05-01

    Rubber from Hevea brasiliensis is the only commercial natural rubber in the world. Propagation of rubber trees usually done by grafting and seed germination. BPPT had been producing rubber tree by in vitro technique with embryo somatic methods. Validation of mother plant for in vitro propagation is important to compare between mother plant and propagated plants. The aim for this research was to validation of PB 260 clone that planted at Cikumpay Plantation by SSR marker. Sampling of 10 rubber leaves were done at Cikumpay Plantation based on GPS position from the area of PB 260 clone. Rubber leaves were isolated with CTAB modification method to obtained DNA. Four of SSR primers from rubber, i.e.: hmac 4, hmac 5, hmct 1, and hmct 5, were used as primers to amplification of rubber DNA. The result showed that no band that different from 10 rubber of PB 260 clone at Cikumpay Plantation. This research will continue to compare genomic validation between mother plant and propagated plants that had been produced from BPPT.

  12. Silane grafted natural rubber and its compatibilization effect on silica-reinforced rubber tire compounds

    Directory of Open Access Journals (Sweden)

    K. Sengloyluan

    2017-12-01

    Full Text Available Natural Rubber (NR grafted with 3-octanoylthio-1-propyltriethoxysilane (NXT was prepared by melt mixing using 1,1′-di(tert-butylperoxy-3,3,5-trimethylcyclohexane as initiator at 140 °C with NXT contents of 10 and 20 parts per hundred rubber [phr] and initiator 0.1 phr. The silane grafted on NR molecules was confirmed by Fourier transform infrared (FTIR, proton nuclear magnetic resonance (1H-NMR and scanning electron microscopy/energy dispersive X-ray spectroscopy (SEM-EDX. Based on 1H-NMR, the use of 10 and 20 phr (parts per hundred resin of silane resulted in grafted NXT onto NR of 0.66 and 1.32 mol%, respectively, or a grafting efficiency of approx. 38%. The use of NXT-grafted NR as compatibilizer in silica-filled NR compounds, to give a total amount of NXT in both grafted and non-grafted forms in the range of 0.8–6.1 wt% relative to the silica, decreases the Mooney viscosity and Payne effect of the compounds, improves filler-rubber interaction, and significantly increases the tensile properties of the silica-filled NR-compounds compared to the non-compatibilized one. At the same silane-content, the use of silane-grafted NR gives slightly better properties than the straight use of the same silane. With sulfur compensation, the use of NXT-grafted-NR with about 6 wt% NXT relative to the silica gives technical properties that reach the levels obtained for straight use of bis-(3-triethoxysilyl-propyltetrasulfide (TESPT at 8.6 wt% relative to the silica.

  13. Protecting tropical forests from the rapid expansion of rubber using carbon payments.

    Science.gov (United States)

    Warren-Thomas, Eleanor M; Edwards, David P; Bebber, Daniel P; Chhang, Phourin; Diment, Alex N; Evans, Tom D; Lambrick, Frances H; Maxwell, James F; Nut, Menghor; O'Kelly, Hannah J; Theilade, Ida; Dolman, Paul M

    2018-03-02

    Expansion of Hevea brasiliensis rubber plantations is a resurgent driver of deforestation, carbon emissions, and biodiversity loss in Southeast Asia. Southeast Asian rubber extent is massive, equivalent to 67% of oil palm, with rapid further expansion predicted. Results-based carbon finance could dis-incentivise forest conversion to rubber, but efficacy will be limited unless payments match, or at least approach, the costs of avoided deforestation. These include opportunity costs (timber and rubber profits), plus carbon finance scheme setup (transaction) and implementation costs. Using comprehensive Cambodian forest data, exploring scenarios of selective logging and conversion, and assuming land-use choice is based on net present value, we find that carbon prices of $30-$51 per tCO 2 are needed to break even against costs, higher than those currently paid on carbon markets or through carbon funds. To defend forests from rubber, either carbon prices must be increased, or other strategies are needed, such as corporate zero-deforestation pledges, and governmental regulation and enforcement of forest protection.

  14. Electron beam cross-linking of natural rubber/linear-low density polyethylene blends

    International Nuclear Information System (INIS)

    Ahmad, A.; Mohd, D. H.; Abdullah, I.

    2005-01-01

    Effects of electron beam irradiation on the mechanical properties and morphological structure of natural rubber/linear-low density polyethylene blend was investigated The natural rubber/linear-low density polyethylene blend was prepared by melt blending in a Haake internal mixer at 140 d ig C , rotor speed of 50 rpm, and in 15 min Liquid natural rubber was incorporated into the blend as a compatibilizer Samples in the form of 1 mm sheets were exposed to 50-300 kGy of electron beam irradiation and analyzed for swelling index and gel content, tensile strength, and surface morphology. The result Indicated that gel content and mechanical properties of the samples increased with radiation dosage. The honey-comb structure of the surface morphology in low dosage irradiated samples slowly transformed into a continuous matrix on increasing radiation dose The variation of mechanical and physical properties was due to Increase in cross-linking density in the rubber and plastic phases and rubber-plastic Interaction on irradiation

  15. Allergenicity of latex rubber products used in South African dental ...

    African Journals Online (AJOL)

    Fourteen latex examination gloves (powdered and non-powdered) and five dental rubber dams, representing 6 brands, from five dental academic institutions were analysed for latex allergens and total protein. Total protein content was determined using the BioRad DC protein assay kit and natural rubber allergen levels ...

  16. Rubber band ligation and infrared photocoagulation for the outpatient treatment of hemorrhoidal disease.

    Science.gov (United States)

    Ricci, Maurício Pichler; Matos, Délcio; Saad, Sarhan Sydney

    2008-01-01

    To compare the results of rubber band ligation and infrared photocoagulation for the treatment of hemorrhoidal disease through the analysis of the incidence of complications after each treatment and respective success rate. Forty-eight patients with first, second or third degree hemorrhoidal disease were randomized to receive treatment with either rubber band ligation (n=23) or infrared photocoagulation (n=25). Each patient was assessed at 1 week and 4 week intervals after treatment. We compared the incidence of complications and efficiency of each treatment modality and Qui-square, Fisher's Exact Test and Student's t Test were used to statistical analysis. Bleeding occured in eight (34,7%) patients treated with rubber band ligation and in four (16,0%) after infrared photocoagulation (p=0,243). Thirteen (52,0%) patients felt pain during infrared photocoagulation and 9 (39,1%) after rubber band ligation (p=0,546). After rubber band ligation, 14 (60,8%) required medication for pain relief. One patient (4,0%) required medication after infrared photocoagulation (prubber band ligator and 1 (4,0%) treated with infrared photocoagulation had symptomatic mucosal ulcers. Perianal dermatitis occured in two (8,0%) patients treated with infrared photocoagulation and one patient (4,3%) was observed to have prolapsed thrombosed piles after rubber band ligation. One month after treatment, 17 of 23 patients treated with rubber band ligation (73,9%) and 18 of 25 patients treated with infrared photocoagulation were asymptomatic. Rubber band ligation treated bleeding and prolapse in 90,0% and 82,4% respectively. Infrared photocoagulation treats bleeding and prolapse in 93,7% and 87,5% respectively. Those differences are not significant. Rubber band ligation causes significantly more pain than infrared photocoagulation during the first week after the procedures and their success rate are not different after four weeks of treatment.

  17. Effects of simulant mixed waste on EPDM and butyl rubber

    International Nuclear Information System (INIS)

    Nigrey, P.J.; Dickens, T.G.

    1997-11-01

    The authors have developed a Chemical Compatibility Testing Program for the evaluation of plastic packaging components which may be used in transporting mixed waste forms. In this program, they have screened 10 plastic materials in four liquid mixed waste simulants. These plastics were butadiene-acrylonitrile copolymer (Nitrile) rubber, cross-linked polyethylene, epichlorohydrin rubber, ethylene-propylene (EPDM) rubber, fluorocarbons (Viton and Kel-F trademark), polytetrafluoro-ethylene (Teflon), high-density polyethylene, isobutylene-isoprene copolymer (Butyl) rubber, polypropylene, and styrene-butadiene (SBR) rubber. The selected simulant mixed wastes were (1) an aqueous alkaline mixture of sodium nitrate and sodium nitrite; (2) a chlorinated hydrocarbon mixture; (3) a simulant liquid scintillation fluid; and (4) a mixture of ketones. The screening testing protocol involved exposing the respective materials to approximately 3 kGy of gamma radiation followed by 14-day exposures to the waste simulants at 60 C. The rubber materials or elastomers were tested using Vapor Transport Rate measurements while the liner materials were tested using specific gravity as a metric. The authors have developed a chemical compatibility program for the evaluation of plastic packaging components which may be incorporated in packaging for transporting mixed waste forms. From the data analyses performed to date, they have identified the thermoplastic, polychlorotrifluoroethylene, as having the greatest chemical compatibility after having been exposed to gamma radiation followed by exposure to the Hanford Tank simulant mixed waste. The most striking observation from this study was the poor performance of polytetrafluoroethylene under these conditions. In the evaluation of the two elastomeric materials they have concluded that while both materials exhibit remarkable resistance to these environmental conditions, EPDM has a greater resistance to this corrosive simulant mixed waste

  18. Thermal analysis and microstructure of hexaperrite based magnet composite with natural rubber matrix

    International Nuclear Information System (INIS)

    Sudirman; Ridwan; Jamilah; Trijono, Waluyo

    2000-01-01

    Thermal and microstructure analyse of hexa ferrite based on composite magnets with natural rubber matrix have been done to investigate their performance. Such magnets play an important role in the toy and house-hold industries because of their suitable magnetic properties, low cost, lightness and flexibility. The composite magnets were synthesized by blending the ferrite powder and natural rubber at composition 30%-70% rubber volume. The microstructure and thermal behaviour of the composite were examined by using SEM and OTA/TGA. The result show that the natural rubber swelling is optimally at 181,17 o C, which is the recommended top condition for blending. The performance magnet composite is limited by the change of natural rubber properties which decompose at temperature around 400 o C. In the decomposition process, the natural rubber molecule trapped in a composite system based on BaM is more difficult are more compared to the composite system based on SrM because the BaM system particle microstructure and its distribution more homogeneous

  19. CURING AND MECHANICAL PROPERTIES OF CHLOROSULPHONATED POLYETHYLENE RUBBER BLEND

    Directory of Open Access Journals (Sweden)

    Jaroslava Budinski-Simendić

    2011-09-01

    Full Text Available In this paper, the curing and mechanical properties of two series of prepared blends, i.e., chlorosulphonated polyethylene (CSM/isobutylene-co-isoprene (IIR rubber blends and chlorosulphonated polyethylene (CSM/chlorinated isobutylene-co-isoprene (CIIR rubber blends were carried out. Blends were prepared using a two-roll mill at a temperature of 40-50 °C. The curing was assessed using a Monsanto oscillating disc rheometer R-100. The process of vulcanization accelerated sulfur of pure rubbers and their blends was carried out in an electrically heated laboratory hydraulic press under a pressure of about 4 MPa and 160 °C. The stress-strain experiments were performed using a tensile tester machine (Zwick 1425. Results indicate that the scorch time, ts2, and optimum cure time, tc90, increase with increasing CSM content in both blends. The value of modulus at 100 and 300% elongation and tensile strength increases with increasing CSM content, whereas elongation at break shows a decreasing trend. The enhancement in mechanical properties was supported by data of crosslink density in these samples obtained from swelling measurement and scanning electron microscopy studies of the rubber blends fractured surfaces

  20. Evaluation of high pressure water blast with rotating spray bar for removing paint and rubber deposits from airport runways, and review of runway slipperiness problems created by rubber contamination

    Science.gov (United States)

    Horne, W. B.; Griswold, G. D.

    1975-01-01

    A high pressure water blast with rotating spray bar treatment for removing paint and rubber deposits from airport runways is studied. The results of the evaluation suggest that the treatment is very effective in removing above surface paint and rubber deposits to the point that pavement skid resistance is restored to trafficked but uncontaminated runway surface skid resistance levels. Aircraft operating problems created by runway slipperiness are reviewed along with an assessment of the contributions that pavement surface treatments, surface weathering, traffic polishing, and rubber deposits make in creating or alleviating runway slipperiness. The results suggest that conventional surface treatments for both portland cement and asphaltic concrete runways are extremely vulnerable to rubber deposit accretions which can produce runway slipperiness conditions for aircraft operations as or more slippery than many snow and ice-covered runway conditions. Pavement grooving surface treatments are shown to be the least vulnerable to rubber deposits accretion and traffic polishing of the surface treatments examined.

  1. The influence of temperature and reaction time in the degradation of natural rubber latex

    International Nuclear Information System (INIS)

    Siti Zaleha Isa; Rosiyah Yahya; Aziz Hassan; Mohd Tahir

    2007-01-01

    Liquid natural rubber (LNR /LENR) should be considered as a new material instead of a new type of rubber though they have the same configuration as the rubber used. In this work, thermal degradation of natural rubber latex was carried out to obtain LNR/LENR by varying the reaction time at different temperatures. The degraded polymers were characterized structurally using FTIR and NMR spectroscopies and the average molecular weights were determined by membrane-osmometry and viscometry. (author)

  2. Application of mathematical planning in production of filled emulsion rubbers

    Science.gov (United States)

    Pugacheva, I. N.; Molokanova, L. V.; Popova, L. V.; Repin, P. S.

    2018-05-01

    The applicability of mathematical planning of experiment in the field of chemistry and chemical engineering, in particular in the industrial production of synthetic rubbers, is considered in the article. Possibility of using secondary material resources, which are waste products of light industry, in the production of elastomeric compositions is studied. The method of obtaining a powdered cellulose additive from wastes containing cellulose fiber is described. The best way of introducing the obtained additive into elastomeric compositions based on the emulsion rubber is established. Optimal conditions for obtaining filled emulsion rubber with the help of a powdered cellulose additive were established basing on the mathematical planning of experiment.

  3. Preparation and study of new rubber to steel adhesive systems

    International Nuclear Information System (INIS)

    Labaj, I.; Ondrusova, D.; Dubec, A.; Pajtasova, M.; Kohutiar, M.

    2017-01-01

    The present paper deals with the preparation of new rubber to steel adhesive systems using the steel surface treatment by applying the adhesive coats based on Co (II) and Cu(II) salts. For demonstration of coats chemical composition EDX analysis was used. The topography and microstructure of prepared adhesive coats were investigated using Scanning Electron Microscopy. Finally the efficiency of adhesion between rubber blends and coated metal steel pieces was evaluated according to Test ASTM D429 Rubber to metal adhesion, method A. The adhesive strength resulting values of prepared steel samples with new adhesive coats were compared with samples covered with adhesive systems commonly used in industry. (authors)

  4. Toughening of carbon fibre reinforced polymer composites with rubber nanoparticles for advanced industrial applications

    Directory of Open Access Journals (Sweden)

    N. G. Ozdemir

    2016-05-01

    Full Text Available This study investigates the effects of nano carboxylic acrylonitrile butadiene rubber (CNBR-NP and nano acrylonitrile butadiene rubber (NBR-NP on the interlaminar shear strength and fracture toughness of carbon fibre reinforced polymer composites (CFRP with dicyandiamide-cured epoxy matrix. The results show that nano-size dispersion of rubber significantly improved the Mode I delamination fracture toughness (GIC of the CFRP by 250% and its Mode II delamination fracture toughness (GIIC by 80% with the addition of 20 phr of CNBR-NP. For the NBR-NP system, the GIC and GIIC delamination fracture toughness of the CFRP were increased by 200 and 80% respectively with the addition of 20 phr (parts per hundred rubber of nano rubber to the matrix. Scanning electron microscopy (SEM images of the fracture surface revealed that the toughening was mainly achieved by debonding of the nano rubber, crack path deflection and fibre bridging.

  5. Study on determination of durability analysis process and fatigue damage parameter for rubber component

    International Nuclear Information System (INIS)

    Moon, Seong In; Cho, Il Je; Woo, Chang Su; Kim, Wan Doo

    2011-01-01

    Rubber components, which have been widely used in the automotive industry as anti-vibration components for many years, are subjected to fluctuating loads, often failing due to the nucleation and growth of defects or cracks. To prevent such failures, it is necessary to understand the fatigue failure mechanism for rubber materials and to evaluate the fatigue life for rubber components. The objective of this study is to develop a durability analysis process for vulcanized rubber components, that can predict fatigue life at the initial product design step. The determination method of nonlinear material constants for FE analysis was proposed. Also, to investigate the applicability of the commonly used damage parameters, fatigue tests and corresponding finite element analyses were carried out and normal and shear strain was proposed as the fatigue damage parameter for rubber components. Fatigue analysis for automotive rubber components was performed and the durability analysis process was reviewed

  6. Feasibility study of a soil-based rubberized CLSM.

    Science.gov (United States)

    Wu, Jason Y; Tsai, Mufan

    2009-02-01

    The development of beneficial uses of recycled scrap tires is always in great demand around the world. The disposal of on-site surplus excavated soil and the production of standard engineering aggregates have also been facing increasing environmental and ecological challenges in congested islands, such as Taiwan. This paper presents an experimental study using recycled crumb rubber and native silty sand to produce a lightweight, soil-based, rubberized controlled low strength material (CLSM) for a bridge approach repair. To assess the technical feasibility of this material, the effects of weight ratios of cement-to-water (C/W) and water-to-solid (W/S), and of rubber content on the engineering properties for different mixtures were investigated. The presented test results include flowability, unit weight, strength, settlement potential, and bearing capacity. Based on the findings, we conclude that a soil-based rubberized CLSM with 40% sand by weight and an optimal design ratio of 0.7 for C/W and 0.35 for W/S can be used for the proposed bridge approach repair. Such a mixture has demonstrated acceptable flowability, strength, and bearing capacity. Its lower unit weight, negligible compressibility, and hydrocollapse potential also help ensure that detrimental settlement is unlikely to occur. The results illustrate a novel scheme of CLSM production, and suggest a beneficial alternative for the reduction of scrap tires as well as conservation of resources and environment.

  7. Evapotranspiration of rubber (Hevea brasiliensis) cultivated at two plantation sites in Southeast Asia

    Science.gov (United States)

    Giambelluca, Thomas W.; Mudd, Ryan G.; Liu, Wen; Ziegler, Alan D.; Kobayashi, Nakako; Kumagai, Tomo'omi; Miyazawa, Yoshiyuki; Lim, Tiva Khan; Huang, Maoyi; Fox, Jefferson; Yin, Song; Mak, Sophea Veasna; Kasemsap, Poonpipope

    2016-02-01

    To investigate the effects of expanding rubber (Hevea brasiliensis) cultivation on water cycling in Mainland Southeast Asia (MSEA), evapotranspiration (ET) was measured within rubber plantations at Bueng Kan, Thailand, and Kampong Cham, Cambodia. After energy closure adjustment, mean annual rubber ET was 1211 and 1459 mm yr-1 at the Thailand and Cambodia sites, respectively, higher than that of other tree-dominated land covers in the region, including tropical seasonal forest (812-1140 mm yr-1), and savanna (538-1060 mm yr-1). The mean proportion of net radiation used for ET by rubber (0.725) is similar to that of tropical rainforest (0.729) and much higher than that of tropical seasonal forest (0.595) and savanna (0.548). Plant area index (varies with leaf area changes), explains 88.2% and 73.1% of the variance in the ratio of latent energy flux (energy equivalent of ET) to potential latent energy flux (LE/LEpot) for midday rain-free periods at the Thailand and Cambodia sites, respectively. High annual rubber ET results from high late dry season water use, associated with rapid refoliation by this brevideciduous species, facilitated by tapping of deep soil water, and by very high wet season ET, a characteristic of deciduous trees. Spatially, mean annual rubber ET increases strongly with increasing net radiation (Rn) across the three available rubber plantation observation sites, unlike nonrubber tropical ecosystems, which reduce canopy conductance at high Rn sites. High water use by rubber raises concerns about potential effects of continued expansion of tree plantations on water and food security in MSEA.

  8. High energy radiation effects on mechanical properties of butyl rubber compounds

    International Nuclear Information System (INIS)

    Pozenato, Cristina A.; Scagliusi, Sandra R.; Cardoso, Elisabeth C.L.; Lugao, Ademar B.

    2013-01-01

    The high energy radiation on butyl rubber compounds causes a number of chemical reactions that occur after initial ionization and excitation events. These reactions lead to changes in molecular mass of the polymer through scission and crosslinking of the molecules, being able to affect the physical and mechanical properties. Butyl rubber has excellent mechanical properties and oxidation resistance as well as low gas and water vapor permeability. Due to all these properties butyl rubber is widely used industrially and particularly in tires manufacturing. In accordance with various authors, the major effect of high energy, such as gamma rays in butyl rubber, is the yielding of free-radicals along with changes in mechanical properties. There were evaluated effects imparted from high energy radiation on mechanical properties of butyl rubber compounds, non-irradiated and irradiated with 25 kGy, 50 kGy, 150 kGy and 200 kGy. It was also observed a sharp reducing in stress rupture and elongation at break for doses higher than 50 kGy, pointing toward changes in polymeric chain along build-up of free radicals and consequent degradation. (author)

  9. Geometrical metrology on vacuum cast silicone rubber form using computed tomography

    DEFF Research Database (Denmark)

    Pacurar, Ramona; Müller, Pavel; De Chiffre, Leonardo

    An investigation on geometrical measurements of silicone rubber cake form and polyamide molds using three measuring techniques - CMM, optical scanner and CT scanner - was carried out. The only measurand was diameter of a cone measured at specified levels. An uncertainty budget for all three...... techniques. It was found that when the silicon rubber form was measured on the supported bottom mold or the bottom mold was measured itself, the diameter measurements performed on optical scanner and CT scanner were bigger compared to CMM measurements. On the other hand, the diameter resulted in smaller...... values when the silicon rubber form was measured on the supported top mold or the top mold was measured itself. A procedure for measurement of highly deformable part, such as silicone rubber form, was developed. Uncertainties from measurement on the optical scanner were big. This was mainly connected...

  10. On the stick-slip behaviour of water-lubricated rubber sealings

    Science.gov (United States)

    Thörmann, Stefan; Markiewicz, Marian; von Estorff, Otto

    2017-07-01

    The phenomenon of friction-induced vibration is investigated, focussing on the automobile topic of a car door window in sliding contact with the adjacent rubber seal. Within this study, the influencing parameters on the stick-slip motion are explored experimentally and using FE-simulation. A test rig is established to represent the situation at the car door window under defined and repeatable conditions. It consists of a rotating glass disc in sliding contact with a rubber specimen. The frictional properties of the rubber specimen and the glass disc as well as their vibration response and sound radiation are examined. Parameter studies regarding the influence of the relative sliding velocity and the contact normal force on the vibration response and the sound radiation are carried out experimentally and the results are discussed. A finite element model of the test setup is generated and validated with the spectral results of the recorded sound from experiment. With the use of FE-simulation a detailed analysis on the behaviour of friction-induced vibration of rubber specimen and glass disc is carried out. It can be identified, that the main impact on the spectral results of the friction-induced vibration is derived from the underlying frictional properties. Their influence is demonstrated in detail by picturing the motion of the rubber specimen, represented by the limit cycle, for different friction characteristics.

  11. Properties of Vulcanized Polyisoprene Rubber Composites Filled with Opalized White Tuff and Precipitated Silica

    Directory of Open Access Journals (Sweden)

    Suzana Samaržija-Jovanović

    2014-01-01

    Full Text Available Opalized white tuff (OWT with 40 μm average particle size and 39.3 m2/g specific surface area has been introduced into polyisoprene rubber (NR. Their reinforcing effects were evaluated by comparisons with those from precipitated silica (PSi. The cure characteristic, apparent activation energy of cross-link (Eac and reversion (Ear, and mechanical properties of a variety of composites based on these rubbers were studied. This was done using vulcanization techniques, mechanical testing, and scanning electron microscopy (SEM. The results showed that OWT can greatly improve the vulcanizing process by shortening the time of optimum cure (tc90 and the scorch time (ts2 of cross-linked rubber composites, which improves production efficiency and operational security. The rubber composites filled with 50 phr of OWT were found to have good mechanical and elastomeric properties. The tensile strengths of the NR/OWT composites are close to those of NR/PSi composites, but the tear strength and modulus are not as good as the corresponding properties of those containing precipitated silica. Morphology results revealed that the OWT is poorly dispersed in the rubber matrix. According to that, the lower interactions between OWT and polyisoprene rubber macromolecules are obtained, but similar mechanical properties of NR/OWT (100/50 rubber composites compared with NR/PSi (100/50 rubber composites are resulted.

  12. Study of radiation induced structural changes in nitrile rubber

    International Nuclear Information System (INIS)

    Cardona, F.; Hill, D.J.T.; Pomery, P.J.; Whittaker, A.K.

    1996-01-01

    Full text: Copolymers of butadiene (BD) and acrylonitrile (AN) (NBR rubber), have become important commercial material. NBR rubbers are part of a larger classification of products often referred to as special-purpose rubbers. Oil resistance is the most important property of nitrile rubbers, and refer to the ability of the vulcanised product to retain its original physical properties such as modulus, tensile strength, abrasion resistance and dimensions, while in contact with oils and fuels. Despite these reported advantages very few studies have been conducted on the radiation yields and structural changes in nitrile rubbers during exposure to high energy radiation. In this study we are investigating the stability against gamma and UV radiation, to different doses in vacuum, of butadiene, acrylonitrile and NBR copolymers with different composition ratio BD/AN. The mechanism of radiation induced structural changes is being investigated using experimental techniques such as ESR, NMR (Solid-state), FT-IR, RAMAN and UV spectroscopy. Also is being investigated the effect of irradiation on the mechanical properties of stressed and unstressed samples by TGA, DSC, DMA, Instron and Creep Test measurements. So far the main effect have been a marked radiation-induced loss of unsaturation in the butadiene units, cis to trans isomerization and formation of crosslink structures (intermolecular and intramolecular). One of the main challenges in the studies of NBR polymers is to observe directly the crosslinks produces by the radiation induced chemical reactions. IR spectroscopy is unsuitable because of the low molar absorbity of the peaks related to intermolecular crosslinking and the overlapping of the peaks (1630-1670 cm-1) related to intramolecular crosslinking (cyclization), with conjugated and nonconjugated (-C=C-; -C=N-) double bonds. A. K. Whittaker has shown that crosslink structures in PBD can be detected and measured directly using solid-state 13 C NMR. This technique

  13. Environmental Exposure and Accelerated Testing of Rubber-to-Metal Vulcanized Bonded Assemblies

    Science.gov (United States)

    1974-11-01

    btadiene/acrylonitrile ( NBR ) rubber -to-metat -. canized bonded assemblies at the two exposure sites are shown in Table 5. After exposure for one year...AD-A0-17 368 EN~VIRONMENTAL EXPOSURE AND ACCELERATED TESTING OF RUBBER -TO-METAL VULCANIZED BONDED ASSEMBLIES John A. WilliamsI Rock Island Arseital...COMMERCE 325116 1AD R-TR-75-013 ENViRONMENTAL EXPOSURE AND ACCELERATED TESTING OF RUBBER -TO-METAL VULCANIZED BONDED ASSEMBLIES by __ John A. Williams

  14. Components of Soil Respiration and its Monthly Dynamics in Rubber Plantation Ecosystems

    OpenAIRE

    Zhixiang Wu; Limin Guan; Bangqian Chen; Chuan Yang; Guoyu Lan; Guishui Xie; Zhaode Zhou

    2014-01-01

    Aim: Our objective was to quantify four components and study effect factors of soil respiration in rubber plantation ecosystems. Providing the basic data support for the establishment of the trade of rubber plantation ecosystem carbon source/sink. Methods: We used Li-6400 (IRGA, Li-COR) to quantitate four components of soil respiration in rubber plantation ecosystems at different ages. Soil respiration can be separated as four components: heterotrophic respiration (Rh), Respiration of roots (...

  15. Reinforcement of tire tread and radiator hose rubbers with short aramid fibers

    OpenAIRE

    Shirazi, Morteza; Noordermeer, Jacobus W.M.

    2010-01-01

    Short fiber reinforced rubber composites have gained great importance due to their advantages in processing and low cost, coupled with high strength. Reinforcement with short fibers offers attractive features such as design flexibility, high modulus, tear strength, etc. The degree of reinforcement depends upon many parameters, such as: the nature of the rubber matrix, the type of fiber, the concentration and orientation of the fibers, fiber to rubber adhesion to generate a strong interface, f...

  16. Dielectric properties of perbunan rubber: γ-irradiation effects

    International Nuclear Information System (INIS)

    El-Nour, K.N.A.; Fouda, I.M.; Migahed, M.D.

    1987-01-01

    A systematic dielectric study over a frequency range extending from 200 Hz to 100 kHz and temperature ranging from 20 0 to 60 0 C has been carried out on perbunan rubber. The acrylonitrile content of the rubber samples was 28% and 38%. The effect of 15 MR γ-irradiation on the dielectric properties of both samples was studied and the results are interpreted. The study revealed that NBR-38 is better than NBR-28 for insulating purposes. (author)

  17. Visual nesting system for irregular cutting-stock problem based on rubber band packing algorithm

    Directory of Open Access Journals (Sweden)

    Xiaoping Liao

    2016-05-01

    Full Text Available This article deals with the packing problem of irregular items allocated into a rectangular sheet to minimize the waste. Conventional solution is not visual during the packing process. It obtains a reasonable and relatively satisfactory solution between the nesting time and nesting solution. This article adopts a physical method that uses rubber band packing algorithm to simulate a rubber band wrapping those packing irregular items. The simulation shows a visual and fast packing process. The resultant rubber band force is applied in the packing items to translate, rotate, and slide them to make the area decrease and obtain a high packing density. An improved analogy QuickHull algorithm is presented to obtain extreme points of rubber band convex hull. An adaptive module could set a variable rubber band force and a variable time step to make a proper convergence and no intersection. A quick convex decomposition method is used to solve the problem of concave polygon. A plural vector expression approach is adopted to calculate the resultant vector of the rubber band force. Several cases are compared with the benchmark problems to prove rubber band packing algorithm performance.

  18. Influence of Ultrasonic Vibrations on the Static Friction Characteristics of a Rubber/Aluminum Couple

    International Nuclear Information System (INIS)

    Cheng Ting-Hai; Gao Han; Bao Gang

    2011-01-01

    A novel ultrasonic vibration approach is introduced into a chloroprene rubber/aluminum friction couple for improving the static friction properties between rubber and metal. Compared to the test results without vibrations, the static friction force of a chloroprene rubber/aluminum couple decreases observably, leading to the ultimate displacement of rubber. The values of the static friction force and ultimate displacement can be ultimately reduced to 23.1% and 50% of those without ultrasonic vibrations, respectively. (fundamental areas of phenomenology(including applications))

  19. About the cure kinetics in natural rubber/styrene Butadiene rubber blends at 433 K

    International Nuclear Information System (INIS)

    Mansilla, M.A.; Marzocca, A.J.

    2012-01-01

    Vulcanized blends of elastomers are employed in several goods mainly to improve physical properties and reduce costs. One of the most used blends of this kind is that composed by natural rubber (NR) and styrene butadiene rubber (SBR). The cure kinetic of these blends depends mainly on the compound formulation and the cure temperature and time. The preparation method of the blends can influence the mechanical properties of the vulcanized compounds. In this work the cure kinetic at 433 K of NR/SBR blends vulcanized with the system sulfur/TBBS (N-t-butyl-2-benzothiazole sulfenamide) is analyzed in samples prepared by mechanical mixing and solution blending. The two methods produce elastomer domains of NR and SBR, which present different microstructure due to the cure level attained during vulcanization. The cure kinetics is studied by means of rheometer tests and the model proposed by Kamal and Sourour. The analysis of the cure rate is presented and is related to the structure obtained during the vulcanization process.

  20. About the cure kinetics in natural rubber/styrene Butadiene rubber blends at 433 K

    Energy Technology Data Exchange (ETDEWEB)

    Mansilla, M.A., E-mail: mmansilla@df.uba.ar [Laboratorio de Polimeros y Materiales Compuestos, Departamento de Fisica, Facultad de Ciencias Exactas y Naturales, Universidad de Buenos Aires, Ciudad Universitaria, Pabellon 1, C1428EGA Buenos Aires (Argentina); Marzocca, A.J. [Laboratorio de Polimeros y Materiales Compuestos, Departamento de Fisica, Facultad de Ciencias Exactas y Naturales, Universidad de Buenos Aires, Ciudad Universitaria, Pabellon 1, C1428EGA Buenos Aires (Argentina)

    2012-08-15

    Vulcanized blends of elastomers are employed in several goods mainly to improve physical properties and reduce costs. One of the most used blends of this kind is that composed by natural rubber (NR) and styrene butadiene rubber (SBR). The cure kinetic of these blends depends mainly on the compound formulation and the cure temperature and time. The preparation method of the blends can influence the mechanical properties of the vulcanized compounds. In this work the cure kinetic at 433 K of NR/SBR blends vulcanized with the system sulfur/TBBS (N-t-butyl-2-benzothiazole sulfenamide) is analyzed in samples prepared by mechanical mixing and solution blending. The two methods produce elastomer domains of NR and SBR, which present different microstructure due to the cure level attained during vulcanization. The cure kinetics is studied by means of rheometer tests and the model proposed by Kamal and Sourour. The analysis of the cure rate is presented and is related to the structure obtained during the vulcanization process.