WorldWideScience

Sample records for nickel-base superalloy inconel

  1. Fiber laser welding of nickel based superalloy Inconel 625

    Science.gov (United States)

    Janicki, Damian M.

    2013-01-01

    The paper describes the application of single mode high power fiber laser (HPFL) for the welding of nickel based superalloy Inconel 625. Butt joints of Inconel 625 sheets 0,8 mm thick were laser welded without an additional material. The influence of laser welding parameters on weld quality and mechanical properties of test joints was studied. The quality and mechanical properties of the joints were determined by means of tensile and bending tests, and micro hardness tests, and also metallographic examinations. The results showed that a proper selection of laser welding parameters provides non-porous, fully-penetrated welds with the aspect ratio up to 2.0. The minimum heat input required to achieve full penetration butt welded joints with no defect was found to be 6 J/mm. The yield strength and ultimate tensile strength of the joints are essentially equivalent to that for the base material.

  2. Phase Transformations in Nickel base Superalloy Inconel 718 during Cyclic Loading at High Temperature

    Directory of Open Access Journals (Sweden)

    Michal Jambor

    2017-06-01

    Full Text Available Nickel base superalloys are hi-tech materials intended for high temperature applications. This property owns a complex microstructure formed by matrix of Ni and variety of precipitates. The type, form and the amount of these phases significantly affect the resulting properties of these alloys. At sufficiently long exposure to high temperatures, the transformation phase can occur, which can lead to degradation of properties of these alloys. A cyclic plastic deformation can accelerate these changes, and they could occur at significantly lower temperatures or in shorter time of exposure. The aim of this study is to describe phase transformation, which can occur by a cyclic plastic deformation at high temperatures in nickel base superalloy Inconel 718.

  3. Studies on the Corrosion Resistance of Laser-Welded Inconel 600 and Inconel 625 Nickel-Based Superalloys

    Directory of Open Access Journals (Sweden)

    Łyczkowska K.

    2017-06-01

    Full Text Available The paper presents the results of the electrochemical corrosion tests of Inconel 600 and Inconel 625 laser-welded superalloys. The studies were conducted in order to assess the resistance to general and pitting corrosion in 3.5% NaCl solution. It was found that Inconel 600 possesses good corrosion resistance, however Inconel 625 is characterized by a greater resistance to general and also to pitting corrosion of the weld as well as the base metal.

  4. Mechanical properties of nanostructured nickel based superalloy Inconel 718

    Energy Technology Data Exchange (ETDEWEB)

    Mukhtarov, Sh; Ermachenko, A, E-mail: shamil@anrb.r [Institute for Metals Superplasticity Problems RAS, 39, Khalturina, Ufa, 450001 (Russian Federation)

    2010-07-01

    This paper will describe the investigations of a nanostructured (NS) state of nickel based INCONEL alloy 718. This structure was generated in bulk semiproducts by severe plastic deformation (SPD) via multiple isothermal forging (MIF) of a coarse-grained alloy. The initial structure consisted of {gamma}-phase grains with disperse precipitations of {gamma}{sup -}phase in the forms of discs, 50-75 nm in diameter and 20 nm in thickness. The MIF generated structures possess a large quantity of non-coherent plates and rounded precipitations of {delta}-phase, primarily along grain boundaries. In the duplex ({gamma}+{delta}) structure the grains have high dislocation density and a large number of nonequilibrium boundaries. Investigations to determine mechanical properties of the alloy in a nanostructured state were carried out. Nanocrystalline Inconel 718 (80 nm) possesses a very high room-temperature strength after SPD. Microcrystalline (MC) and NS states of the alloy were subjected to strengthening thermal treatment, and the obtained results were compared in order to determine their mechanical properties at room and elevated temperatures.

  5. Hot corrosion behavior of Ni based Inconel 617 and Inconel 738 superalloys

    Energy Technology Data Exchange (ETDEWEB)

    El-Awadi, G.A., E-mail: gaberelawdi@yahoo.com [Atomic Energy Authority, NRC, Cyclotron Project, Abo-zabal, 13759 Cairo (Egypt); Abdel-Samad, S., E-mail: salem_abdelsamad@yahoo.com [Atomic Energy Authority, NRC, Cyclotron Project, Abo-zabal, 13759 Cairo (Egypt); Elshazly, Ezzat S. [Atomic Energy Authority, NRC, Metallurgy Dept., Abo-zabal, 13759 Cairo (Egypt)

    2016-08-15

    Highlights: • Supperalloy good resistance to high temperature oxidation. • Ni-base alloy IN738 and Inconel 617 good resistance to hot corrosion. • Corrosion resistance of supperalloys depending on environment of abrasive ions such as (NaCl or NaSO{sub 4}). • Hot corrosion resistance depend on what the oxides phases where formed. - Abstract: Superalloys are extensively used at high temperature applications due to their good oxidation and corrosion resistance properties in addition to their high stability were made at high temperature. Experimental measurements of hot corrosion at high temperature of Inconel 617 and Inconel 738 superalloys. The experiments were carried out at temperatures 700 °C, 800 °C and 900 °C for different exposure times to up to 100 h. The corrosive media was NaCl and Na{sub 2}SO{sub 4} sprayed on the specimens. Seven different specimens were used at each temperature. The corrosion process is endothermic and the spontaneity increased by increasing temperature. The activation energy was found to be Ea = 23.54 and E{sub a} = 25.18 KJ/mol for Inconel 738 and Inconel 617 respectively. X-ray diffraction technique (XRD) was used to analyze the formed scale. The morphology of the specimen and scale were examined by scanning electron microscopy (SEM). The results show that the major corrosion products formed were NiCr{sub 2}O{sub 4}, and Co Cr{sub 2}O{sub 4} spinles, in addition to Cr{sub 2}O{sub 3}.

  6. Preparation of Inconel 740 superalloy by electron beam smelting

    Energy Technology Data Exchange (ETDEWEB)

    You, Xiaogang [School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023 (China); Laboratory for New Energy Material Energetic Beam Metallurgical Equipment Engineering of Liaoning Province, Dalian 116024 (China); Tan, Yi, E-mail: tanyi@dlut.edu.cn [School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023 (China); Laboratory for New Energy Material Energetic Beam Metallurgical Equipment Engineering of Liaoning Province, Dalian 116024 (China); You, Qifan; Shi, Shuang; Li, Jiayan [School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023 (China); Laboratory for New Energy Material Energetic Beam Metallurgical Equipment Engineering of Liaoning Province, Dalian 116024 (China); Ye, Fei [School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023 (China); Wei, Xin [School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023 (China); Laboratory for New Energy Material Energetic Beam Metallurgical Equipment Engineering of Liaoning Province, Dalian 116024 (China)

    2016-08-15

    A novel method, namely electron beam smelting (EBS) technology was used to prepare the Inconel 740 superalloy. The microstructures, hardness and oxidation behavior were characterized and compared with the traditionally prepared Inconel 740 superalloy. The results imply that the solution treatment gives rise to the coarsening of γ′ precipitates, with further aging treatment, the γ′ precipitates with size of less than 30 nm are distributed dispersively in the matrix, leading to a decreasing of the lattice parameters and an increasing of the misfit. The γ′ precipitates result in shearing mechanism of weakly pair coupling. The EBS 740 superalloy produces better properties than that prepared in the traditional method in both precipitation strengthening effect and oxidation resistance. - Highlights: • Electron beam smelting, a new method, was used to prepare the Inconel 740 superalloy. • The EBS 740 shows higher strengthening effect than 740 made in traditional method. • The EBS 740 shows better oxidation resistance than traditional 740. • It shows application prospect of EBS technology in preparing Ni-base superalloys.

  7. Structural Performance of Inconel 625 Superalloy Brazed Joints

    Science.gov (United States)

    Chen, Jianqiang; Demers, Vincent; Cadotte, Eve-Line; Turner, Daniel; Bocher, Philippe

    2017-02-01

    The purpose of this work was to investigate tensile and fatigue behaviors of Inconel 625 superalloy brazed joints after transient liquid-phase bonding process. Brazing was performed in a vacuum furnace using a nickel-based filler metal in a form of paste to join wrought Inconel 625 plates. Mechanical tests were carried out on single-lap joints under various lap distance-to-thickness ratios. The fatigue crack initiation and crack growth modes were examined via metallographic analysis, and the effect of local stress on fatigue life was assessed by finite element simulations. The fatigue results show that fatigue strength and endurance limit increase with overlap distance, leading to a relatively large scatter of results. Fatigue cracks nucleated in the high-stressed region of the weld fillets from brittle eutectic phases or from internal brazing cavities. The present work proposes to rationalize the results by using the local stress at the brazing fillet. When using this local stress, all fatigue-obtained results find themselves on a single S- N curve, providing a design curve for any joint configuration in fatigue solicitation.

  8. Effect of processing on microstructure and physical properties of three nickel-based superalloys with different hardening mechanisms

    Energy Technology Data Exchange (ETDEWEB)

    Strondl, Annika; Frommeyer, Georg [Department of Materials Technology, Max-Planck-Institut fuer Eisenforschung GmbH, Max-Planck-Strasse 1, D-40237 Duesseldorf (Germany); Klement, Uta [Department of Materials and Manufacturing Technology, Chalmers University of Technology, SE-412 96 Gothenburg (Sweden); Milenkovic, Srdjan; Schneider, Andre

    2012-07-15

    The nickel-based superalloys Inconel alloy 600, Udimet alloy 720, and Inconel alloy 718 were produced by electron beam melting (EBM), casting, and directional solidification (DS). The distance between dendrites and the size of the precipitates indicated the difference in solidification rates between the three processes. In this study, the solidification rate was fastest with EBM, closely followed by casting, whereas it was much slower with DS. In the directional solidified materials the <100> direction was the fastest and thus, preferred growth direction. The EBM samples show a sharp (001)[100] texture in the building direction and in the two scanning directions of the electron beam. Macrosegregation was observed in some cast and directionally solidified samples, but not in the EBM samples. The melting temperatures are in good agreement with literature and the narrow melting interval of IN600 compare to UD720 and IN718 might reduce the risk of incipient melting during EBM processing. Porosity was observed in the EBM samples and the reasons are discussed. However, EBM seems to be a feasible process route to produce nickel-based superalloys with well-defined texture, no macrosegregation and a rapidly solidified microstructure. (Copyright copyright 2012 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  9. The interaction of reaction-bonded silicon carbide and inconel 600 with a nickel-based brazing alloy

    Science.gov (United States)

    McDermid, J. R.; Pugh, M. D.; Drew, R. A. L.

    1989-09-01

    The objective of the present research was to join reaction-bonded silicon carbide (RBSC) to INCONEL 600 (a nickel-based superalloy) for use in advanced heat engine applications using either direct brazing or composite interlayer joining. Direct brazing experiments employed American Welding Society (AWS) BNi-5, a commercial nickel-based brazing alloy, as a filler material; composite interlayers consisted of intimate mixtures of α-SiC and BNi-5 powders. Both methods resulted in the liquid filler metal forming a Ni-Si liquid with the free Si in the RBSC, which, in turn, reacted vigorously with the SiC component of the RBSC to form low melting point constituents in both starting materials and Cr carbides at the metal-ceramic interface. Using solution thermodynamics, it was shown that a Ni-Si liquid of greater than 60 at. pct Ni will decompose a-SiC at the experimental brazing temperature of 1200 ‡C; these calculations are consistent with the experimentally observed composition profiles and reaction morphology within the ceramic. It was concluded that the joining of RBSC to INCONEL 600 using a nickel-based brazing alloy is not feasible due to the inevitability of the filler metal reacting with the ceramic, degrading the high-temperature properties of the base materials.

  10. The Formation and Evolution of Shear Bands in Plane Strain Compressed Nickel-Base Superalloy

    Directory of Open Access Journals (Sweden)

    Bin Tang

    2018-02-01

    Full Text Available The formation and evolution of shear bands in Inconel 718 nickel-base superalloy under plane strain compression was investigated in the present work. It is found that the propagation of shear bands under plane strain compression is more intense in comparison with conventional uniaxial compression. The morphology of shear bands was identified to generally fall into two categories: in “S” shape at severe conditions (low temperatures and high strain rates and “X” shape at mild conditions (high temperatures and low strain rates. However, uniform deformation at the mesoscale without shear bands was also obtained by compressing at 1050 °C/0.001 s−1. By using the finite element method (FEM, the formation mechanism of the shear bands in the present study was explored for the special deformation mode of plane strain compression. Furthermore, the effect of processing parameters, i.e., strain rate and temperature, on the morphology and evolution of shear bands was discussed following a phenomenological approach. The plane strain compression attempt in the present work yields important information for processing parameters optimization and failure prediction under plane strain loading conditions of the Inconel 718 superalloy.

  11. Microstructural studies of carbides in MAR-M247 nickel-based superalloy

    Science.gov (United States)

    Szczotok, A.; Rodak, K.

    2012-05-01

    Carbides play an important role in the strengthening of microstructures of nickel-based superalloys. Grain boundary carbides prevent or retard grain-boundary sliding and make the grain boundary stronger. Carbides can also tie up certain elements that would otherwise promote phase instability during service. Various types of carbides are possible in the microstructure of nickel-based superalloys, depending on the superalloy composition and processing. In this paper, scanning electron and scanning transmission electron microscopy studies of carbides occurring in the microstructure of polycrystalline MAR-M247 nickel-based superalloy were carried out. In the present work, MC and M23C6 carbides in the MAR-M247 microstructure were examined.

  12. Dynamic precipitation of nickel-based superalloys undergoing severe deformation below the solvus temperature

    Energy Technology Data Exchange (ETDEWEB)

    Nowotnik, Andrzej; Rokicki, Pawel; Mrowka-Nowotnik, Grazyna; Sieniawski, Jan [Rzeszow Univ. of Technology (Poland). Dept. of Material Science

    2015-07-15

    The authors performed uniaxial compression tests of nickel-based superalloys: single crystal CMSX-4, also precipitation hardened; Inconel 718 and X750, at temperatures below the γ' solvus, in order to study the effect of temperature and strain rate on their flow stress and microstructural development. On the basis of the obtained flow stress values, the activation energy of a high-temperature deformation process was estimated. Microstructural observations of the deformed samples at high temperatures, previously solution heat treated and aged CMSX-4 and Inconel alloys revealed non-uniform deformation effects. Distribution of either molybdenum- or niobium-rich carbides was found to be affected by localized flow within the investigated strain range at relatively low deformation temperatures, 720-850 C. Microstructural examination of the alloys also showed that shear banding and cavity growth were responsible for the decrease in flow stress and a specimen fracture at larger strains.

  13. Surface alloying of nickel based superalloys by laser

    International Nuclear Information System (INIS)

    Rodriguez, G.P.; Garcia, I.; Damborenea, J.J. de

    1998-01-01

    Ni based superalloys present a high oxidation resistance at high temperature as well as good mechanical properties. But new technology developments force to research in this materials to improve their properties at high temperature. In this work, two Ni based superalloys (Nimonic 80A and Inconel 600) were surface alloyed with aluminium using a high power laser. SEM and EDX were used to study the microstructure of the obtained coatings. Alloyed specimens were tested at 1.273 K between 24 and 250 h. Results showed the generation of a protective and continuous coating of alumina on the laser treated specimens surface that can improve oxidation resistance. (Author) 8 refs

  14. Determinants of the quality of brazed joints of nickel-based superalloys

    Directory of Open Access Journals (Sweden)

    Katarzyna Strzelczak

    2017-10-01

    Full Text Available In the aerospace industry, passenger safety depends on proper quality control at each production stage. The main responsibility for the correct operation of the aircraft lies within a gas turbine. A proper and rigorous selection of the gas turbine construction material is required, and in a further step, the method of joining the construction parts. Nickel superalloys due to the high heat resistance, strength and creep resistance at high temperatures, toughness and corrosion resistance, are very often used for the construction of a gas turbine engine. In the next step, the selection of joining method is necessary. This method must be able to achieve high-quality connections, resistant to work at high temperatures and corrosive environments. The most effective bonding method that meets the above conditions is brazing. In this study non-destructive (visual test and destructive (metallographic test of brazed joint of Inconel 718 and Inconel 625 were conducted.

  15. Solid solution strengthening and diffusion in nickel- and cobalt-based superalloys

    Energy Technology Data Exchange (ETDEWEB)

    Rehman, Hamad ur

    2016-07-01

    Nickel and cobalt-based superalloys with a γ-γ{sup '} microstructure are known for their excellent creep resistance at high temperatures. Their microstructure is engineered using different alloying elements, that partition either to the fcc γ matrix or to the ordered γ{sup '} phase. In the present work the effect of alloying elements on their segregation behaviour in nickel-based superalloys, diffusion in cobalt-based superalloys and the temperature dependent solid solution strengthening in nickel-based alloys is investigated. The effect of dendritic segregation on the local mechanical properties of individual phases in the as-cast, heat treated and creep deformed state of a nickel-based superalloy is investigated. The local chemical composition is characterized using Electron Probe Micro Analysis and then correlated with the mechanical properties of individual phases using nanoindentation. Furthermore, the temperature dependant solid solution hardening contribution of Ta, W and Re towards fcc nickel is studied. The room temperature hardening is determined by a diffusion couple approach using nanoindentation and energy dispersive X-ray analysis for relating hardness to the chemical composition. The high temperature properties are determined using compression strain rate jump tests. The results show that at lower temperatures, the solute size is prevalent and the elements with the largest size difference with nickel, induce the greatest hardening consistent with a classical solid solution strengthening theory. At higher temperatures, the solutes interact with the dislocations such that the slowest diffusing solute poses maximal resistance to dislocation glide and climb. Lastly, the diffusion of different technically relevant solutes in fcc cobalt is investigated using diffusion couples. The results show that the large atoms diffuse faster in cobalt-based superalloys similar to their nickel-based counterparts.

  16. Solid solution strengthening and diffusion in nickel- and cobalt-based superalloys

    International Nuclear Information System (INIS)

    Rehman, Hamad ur

    2016-01-01

    Nickel and cobalt-based superalloys with a γ-γ ' microstructure are known for their excellent creep resistance at high temperatures. Their microstructure is engineered using different alloying elements, that partition either to the fcc γ matrix or to the ordered γ ' phase. In the present work the effect of alloying elements on their segregation behaviour in nickel-based superalloys, diffusion in cobalt-based superalloys and the temperature dependent solid solution strengthening in nickel-based alloys is investigated. The effect of dendritic segregation on the local mechanical properties of individual phases in the as-cast, heat treated and creep deformed state of a nickel-based superalloy is investigated. The local chemical composition is characterized using Electron Probe Micro Analysis and then correlated with the mechanical properties of individual phases using nanoindentation. Furthermore, the temperature dependant solid solution hardening contribution of Ta, W and Re towards fcc nickel is studied. The room temperature hardening is determined by a diffusion couple approach using nanoindentation and energy dispersive X-ray analysis for relating hardness to the chemical composition. The high temperature properties are determined using compression strain rate jump tests. The results show that at lower temperatures, the solute size is prevalent and the elements with the largest size difference with nickel, induce the greatest hardening consistent with a classical solid solution strengthening theory. At higher temperatures, the solutes interact with the dislocations such that the slowest diffusing solute poses maximal resistance to dislocation glide and climb. Lastly, the diffusion of different technically relevant solutes in fcc cobalt is investigated using diffusion couples. The results show that the large atoms diffuse faster in cobalt-based superalloys similar to their nickel-based counterparts.

  17. Phase transformation and liquid density redistribution during solidification of Ni-based superalloy Inconel 718

    Directory of Open Access Journals (Sweden)

    Wang Ling

    2012-08-01

    Full Text Available The influences of chemical segregation and phase transformation on liquid density variation during solidification of Ni-based supperalloy Inconel 718 were investigated using SEM and EDS. It was found that significant segregation in liquid prompts high Nb phase to precipitate directly from liquid, which results in the redistribution of alloy elements and liquid density in their vicinity. The term “inter-precipitate liquid density” is therefore proposed and this concept should be applied to determine the solidification behavior of superalloy Inconel 718.

  18. Welding and Weldability of Directionally Solidified Single Crystal Nickel-Base Superalloys

    Energy Technology Data Exchange (ETDEWEB)

    Vitek, J M; David, S A; Reed, R W; Burke, M A; Fitzgerald, T J

    1997-09-01

    Nickel-base superalloys are used extensively in high-temperature service applications, and in particular, in components of turbine engines. To improve high-temperature creep properties, these alloys are often used in the directionally-solidified or single-crystal form. The objective of this CRADA project was to investigate the weldability of both experimental and commercial nickel-base superalloys in polycrystalline, directionally-solidified, and single-crystal forms.

  19. Rafting in single crystal nickel-base superalloys – An overview

    Indian Academy of Sciences (India)

    R. Narasimhan (Krishtel eMaging) 1461 1996 Oct 15 13:05:22

    Page 1 ... aircraft engines as well as land-based power generation applications. Microstruc- ture and high temperature mechanical properties are the major factors controlling the performance of SX ... Single crystal (SX) superalloys are a group of nickel-base superalloys. They exhibit superior high temperatur mechanical ...

  20. Etude des mecanismes de formation des microstructures lors du brasage isotherme de superalliages a base de nickel

    Science.gov (United States)

    Ruiz-Vargas, Jose

    This thesis reports theoretical and experimental investigations carried out to understand the mechanisms of microstructure formation during isothermal brazing, produced by brazing Inconel 625 and MC2 nickel-based superalloys with filler metal BNi-2. Firstly, studies were made on pure Ni to interpret microstructure's formation with simplified alloy chemistry. Microstructure formation have been studied when varying time at constant temperature (isothermal kinetics), but also when varying temperature for constant hold time (isochronal kinetics). The chemical composition and crystallography of the present phases have been identified, with the following results : (i) the fraction of dissolved base metal has been found proportional to the initial thickness of the brazing alloy, so that the composition of the liquid remains homogeneous with a precise initial equilibrium composition during the whole brazing process, (ii) the melting of the joint occurs in two steps : at lower temperature, it involves only partially melting, and boron diffusion in pure Ni leads to the precipitation of fine Ni3B borides at the interface ; in a second stage, at higher temperature, melting is complete and thermodynamic equilibrium requires significant dissolution of nickel, which also involves the dissolution of part of borides already formed. Secondly, nickel plating technique was used on Inconel 625 nickel-based superalloy. A thin layer of Ni with varying thickness, has been electrodeposited to observe the gradual dissolution of Inconel and microstructural features formation due to the presence of superalloy alloying elements. It has been observed that the nickel coating does not prevent precipitation in the base metal as boron diffuse rapidly through the coating width. In the intermediate nickel plating width, fragile precipitates of nickel borides have been observed, because the contribution of Inconel alloying elements to the melt was very limited. In absence of nickel plating on the

  1. Effects of cobalt in nickel-base superalloys

    Science.gov (United States)

    Tien, J. K.; Jarrett, R. N.

    1983-01-01

    The role of cobalt in a representative wrought nickel-base superalloy was determined. The results show cobalt affecting the solubility of elements in the gamma matrix, resulting in enhanced gamma' volume fraction, in the stabilization of MC-type carbides, and in the stabilization of sigma phase. In the particular alloy studied, these microstructural and microchemistry changes are insufficient in extent to impact on tensile strength, yield strength, and in the ductilities. Depending on the heat treatment, creep and stress rupture resistance can be cobalt sensitive. In the coarse grain, fully solutioned and aged condition, all of the alloy's 17% cobalt can be replaced by nickel without deleteriously affecting this resistance. In the fine grain, partially solutioned and aged condition, this resistance is deleteriously affected only when one-half or more of the initial cobalt content is removed. The structure and property results are discussed with respect to existing theories and with respect to other recent and earlier findings on the impact of cobalt, if any, on the performance of nickel-base superalloys.

  2. Precipitation in Powder Metallurgy, Nickel Base Superalloys: Review of Modeling Approach and Formulation of Engineering (Postprint)

    Science.gov (United States)

    2016-12-01

    AFRL-RX-WP-JA-2016-0333 PRECIPITATION IN POWDER- METALLURGY , NICKEL-BASE SUPERALLOYS: REVIEW OF MODELING APPROACH AND FORMULATION OF...PRECIPITATION IN POWDER- METALLURGY , NICKEL- BASE SUPERALLOYS: REVIEW OF MODELING APPROACH AND FORMULATION OF ENGINEERING (POSTPRINT) 5a...and kinetic parameters required for the modeling of γ′ precipitation in powder- metallurgy (PM), nickel-base superalloys are summarized. These

  3. Predictive Analysis for the Thermal Diffusion of the Plasma-Assisted Machining of Superalloy Inconel-718 Based on Exponential Smoothing

    Directory of Open Access Journals (Sweden)

    Chen Shao-Hsien

    2018-01-01

    Full Text Available Nickel base and titanium base materials have been widely applied to engines in aerospace industry, and these engines are essential components of airplanes. The machining characteristics of aerospace materials may cause machining cutters to be worn down in a short time and thus reduce the accuracy of processing. The plasma-assisted machining adopted in the research is a kind of the complex machining method. In the cases of nickel base and titanium base alloys, the method can heat workpieces in an extremely short duration to soften the materials for the ease of cutting so that the cutting force, cutter wear, and machining cost will all be reduced. The research adopted plasma heating to soften parts of the materials and aimed to explore the heating of nickel base alloy. The temperature variation of the materials was investigated and measured by adjusting the current and feed velocity. Moreover, Inconel-718 superalloy was adopted for the comparison with nickel base alloy for the observation of the influence and change brought by heat, and the method of exponential smoothing was adopted to conduct the prediction and analysis of thermal diffusion for understanding the influence and change brought by electric current on nickel base materials. Finally, given the current from 20 A to 80 A and feed velocity from 1,000 mm/min to 3,000 mm/min, the influence of thermal diffusion was investigated and the related model was built.

  4. A Comparison of the Plastic Flow Response of a Powder Metallurgy Nickel Base Superalloy (Postprint)

    Science.gov (United States)

    2017-04-01

    AFRL-RX-WP-JA-2017-0225 A COMPARISON OF THE PLASTIC-FLOW RESPONSE OF A POWDER- METALLURGY NICKEL-BASE SUPERALLOY (POSTPRINT) S.L...COMPARISON OF THE PLASTIC-FLOW RESPONSE OF A POWDER- METALLURGY NICKEL-BASE SUPERALLOY (POSTPRINT) 5a. CONTRACT NUMBER IN-HOUSE 5b. GRANT...behavior at hot-working temperatures and strain rates of the powder- metallurgy superalloy LSHR was determined under nominally-isothermal and transient

  5. Detection of creep damage in a nickel base superalloy using NDE techniques

    International Nuclear Information System (INIS)

    Carreon, H.; Mora, B.; Barrera, G.

    2009-10-01

    Due to elevated temperatures, excessive stresses and severed corrosion conditions, turbine engine components are subject to creep processes that limit the components life such as a turbine bucket. The failure mechanism of a turbine bucket is related primarily to creep and corrosion and secondarily to thermal fatigue. As a result, it is desirable to assess the current conditions of such turbine component. This study uses the eddy current nondestructive evaluation technique in an effort to monitor the creep damage in a nickel base super-alloy, turbine bucket after service. The experimental results show an important electrical conductivity variation in eddy current images on the creep damage zone of nickel base super-alloy samples cut from a turbine bucket. Thermoelectric power measurements were also conducted in order to obtain a direct correlation between the presence of material changes due to creep damage and the electrical conductivity measurements. This research work shows an alternative non-destructive method in order to detect creep damage in a nickel base super-alloy turbine bucket. (Author)

  6. Degradation of creep properties in a long-term thermally exposed nickel base superalloy

    International Nuclear Information System (INIS)

    Zrnik, J.; Strunz, P.; Vrchovinsky, V.; Muransky, O.; Novy, Z.; Wiedenmann, A.

    2004-01-01

    When exposed for long time at elevated temperatures of 430 and 650 deg. C the nickel base superalloy EI 698 VD can experience a significant decrease in creep resistance. The cause of the creep degradation of nickel base superalloy is generally attributed to the microstructural instability at prolonged high temperature exposure. In this article, the creep-life data, generated on long thermally exposed nickel base superalloy EI698 VD were related to the local microstructural changes observed using SEM and TEM analysing techniques. While structure analysis provided supporting evidence concerning the changes associated with grain boundary carbide precipitation, no persuasive evidence of a morphological and/or dimensional gamma prime change was showed. For clarifying of the role of gamma prime precipitates on alloy on creep degradation, the SANS (small angle neutron scattering) experiment was crucial in the characterization of the bulk-averaged gamma prime morphology and its size distribution with respect to the period of thermal exposure

  7. The Effect of Forging Variables on the Supersolvus Heat-Treatment Response of Powder-Metallurgy Nickel-Base Superalloys

    Science.gov (United States)

    2014-12-01

    AFRL-RX-WP-JA-2015-0160 THE EFFECT OF FORGING VARIABLES ON THE SUPERSOLVUS HEAT-TREATMENT RESPONSE OF POWDER - METALLURGY NICKEL-BASE SUPERALLOYS... POWDER - METALLURGY NICKEL- BASE SUPERALLOYS (POSTPRINT) 5a. CONTRACT NUMBER In-house 5b. GRANT NUMBER 5c. PROGRAM ELEMENT NUMBER 62102F 6. AUTHOR...treatment (SSHT) of two powder - metallurgy , gamma–gamma prime superalloys, IN-100 and LSHR, was established. For this purpose, isothermal, hot

  8. Morphology Dependent Flow Stress in Nickel-Based Superalloys in the Multi-Scale Crystal Plasticity Framework

    Directory of Open Access Journals (Sweden)

    Shahriyar Keshavarz

    2017-11-01

    Full Text Available This paper develops a framework to obtain the flow stress of nickel-based superalloys as a function of γ-γ’ morphology. The yield strength is a major factor in the design of these alloys. This work provides additional effects of γ’ morphology in the design scope that has been adopted for the model developed by authors. In general, the two-phase γ-γ’ morphology in nickel-based superalloys can be divided into three variables including γ’ shape, γ’ volume fraction and γ’ size in the sub-grain microstructure. In order to obtain the flow stress, non-Schmid crystal plasticity constitutive models at two length scales are employed and bridged through a homogenized multi-scale framework. The multi-scale framework includes two sub-grain and homogenized grain scales. For the sub-grain scale, a size-dependent, dislocation-density-based finite element model (FEM of the representative volume element (RVE with explicit depiction of the γ-γ’ morphology is developed as a building block for the homogenization. For the next scale, an activation-energy-based crystal plasticity model is developed for the homogenized single crystal of Ni-based superalloys. The constitutive models address the thermo-mechanical behavior of nickel-based superalloys for a large temperature range and include orientation dependencies and tension-compression asymmetry. This homogenized model is used to obtain the morphology dependence on the flow stress in nickel-based superalloys and can significantly expedite crystal plasticity FE simulations in polycrystalline microstructures, as well as higher scale FE models in order to cast and design superalloys.

  9. Process of welding gamma prime-strengthened nickel-base superalloys

    Science.gov (United States)

    Speigel, Lyle B.; White, Raymond Alan; Murphy, John Thomas; Nowak, Daniel Anthony

    2003-11-25

    A process for welding superalloys, and particularly articles formed of gamma prime-strengthened nickel-base superalloys whose chemistries and/or microstructures differ. The process entails forming the faying surface of at least one of the articles to have a cladding layer of a filler material. The filler material may have a composition that is different from both of the articles, or the same as one of the articles. The cladding layer is machined to promote mating of the faying surfaces, after which the faying surfaces are mated and the articles welded together. After cooling, the welded assembly is free of thermally-induced cracks.

  10. A continuum model for the anisotropic creep of single crystal nickel-based superalloys

    International Nuclear Information System (INIS)

    Prasad, Sharat C.; Rajagopal, K.R.; Rao, I.J.

    2006-01-01

    In this paper, we extend the constitutive theory developed by Prasad et al. [Prasad SC, Rao IJ, Rajagopal KR. A continuum model for the creep of single crystal nickel-base superalloys. Acta Mater 2005;53(3):669-79], to describe the creep anisotropy associated with crystallographic orientation in single crystal nickel-based superalloys. The constitutive theory is cast within a general thermodynamic framework that has been developed to describe the response of materials capable of existing in multiple stress free configurations ('natural configurations'). Central to the theory is the prescription of the forms for the stored energy and rate of dissipation functions. The stored energy reflects the fact that the elastic response exhibits cubic symmetry. The model takes into account the fact that the symmetry of single crystals does not change with inelastic deformation. The rate of dissipation function is also chosen to be anisotropic, in that it reflects invariance to transformations that belong to the cubic symmetry group. The model is used to simulate uniaxial creep of single crystal nickel-based superalloy CMSX-4 for loading along the , and orientations. The predictions of the theory agree well with the experimental data

  11. Recovery of creep properties of the nickel-base superalloy nimonic 105

    CSIR Research Space (South Africa)

    Girdwood, RB

    1996-01-01

    Full Text Available Uniaxial constant stress creep tests were performed on the wrought nickel-base superalloy Nimonic 105. Entire creep curves were recorded and curve shapes analysed using the Theta Projection Concept. Rejuventive procedures were applied to pre...

  12. Microstructural evolution of inconel 625 during thermal aging

    Directory of Open Access Journals (Sweden)

    S. Malej

    2017-01-01

    Full Text Available Inconel 625 is due to alloying elements prone to precipitation of different intermetallic phases and secondary carbides during thermal aging. The base of investigation is nickel superalloy Inconel 625 in hot rolled state. Thermal aging was conducted at temperature 650 °C with different duration of treatment for each sample. Microstructural analysis was performed by light microscope and scanning electron microscope. The results of microstructure observation showed the precipitation of intermetallic γ››- Ni3Nb phase in the γ matrix and δ-Ni3Nb phase with M23C6 secondary carbides at the grain boundaries.

  13. Nanosize boride particles in heat-treated nickel base superalloys

    International Nuclear Information System (INIS)

    Zhang, H.R.; Ojo, O.A.; Chaturvedi, M.C.

    2008-01-01

    Grain boundary microconstituents in aged nickel-based superalloys were studied by transmission electron microscopy techniques. A nanosized M 5 B 3 boride phase, possibly formed by intergranular solute desegregation-induced precipitation, was positively identified. The presence of these intergranular nanoborides provides reasonable clarification of a previously reported reduction of grain boundary liquation temperature during the weld heat affected zone thermal cycle

  14. Research on Liquid Forming Process of Nickel Superalloys Thin Sheet Metals

    Directory of Open Access Journals (Sweden)

    Hyrcza-Michalska M.

    2017-12-01

    Full Text Available The paper presents the study of drawability of thin sheet metals made of a nickel superalloy Inconel type. The manufacturing process of axisymmetric cup – cone and a closed section profile in the form of a circular tube were designed and analyzed. In both cases, working fluid-oil was used in place of the rigid tools. The process of forming liquid is currently the only alternative method for obtaining complex shapes, coatings, and especially if we do it with high-strength materials. In the case of nickel superalloys the search for efficient methods to manufacture of the shaped shell is one of the most considerable problems in aircraft industry [1-5]. However, the automotive industries have the same problem with so-called advanced high-strength steels (AHSS. Due to this, both industrial problems have been examined and the emphasis have been put on the process of liquid forming (hydroforming. The study includes physical tests and the corresponding numerical simulations performed, using the software Eta/Dynaform 5.9. Numerical analysis of the qualitative and quantitative forecasting enables the formability of materials with complex and unusual characteristics of the mechanical properties and forming technology. It has been found that only the computer aided design based on physical and numerical modeling, makes efficient plastic processing possible using a method of hydroforming. Drawability evaluation based on the determination of the mechanical properties of complex characteristics is an indispensable element of this design in the best practice of industrial manufacturing products made of thin sheet metals.

  15. Microstructural characteristics of high-temperature oxidation in nickel-base superalloy

    International Nuclear Information System (INIS)

    Khalid, F.A.

    1997-01-01

    Superalloys are used for aerospace and nuclear applications where they can withstand high-temperature and severe oxidizing conditions. High-temperature oxidation behavior of a nickel-base superalloy is examined using optical and scanning electron microscopical techniques. The morphology of the oxide layers developed is examined, and EDX microanalysis reveals diffusion of the elements across the oxide-metal interface. Evidence of internal oxidation is presented, and the role of structural defects is considered. The morphology of the oxide-metal interface formed in the specimens exposed in steam and air is examined to elucidate the mechanism of high-temperature oxidation

  16. Modeling Long-term Creep Performance for Welded Nickel-base Superalloy Structures for Power Generation Systems

    Energy Technology Data Exchange (ETDEWEB)

    Shen, Chen [GE Global Research, NIskayuna, NY (United States); Gupta, Vipul [GE Global Research, NIskayuna, NY (United States); Huang, Shenyan [GE Global Research, NIskayuna, NY (United States); Soare, Monica [GE Global Research, NIskayuna, NY (United States); Zhao, Pengyang [GE Global Research, NIskayuna, NY (United States); Wang, Yunzhi [GE Global Research, NIskayuna, NY (United States)

    2017-02-28

    The goal of this project is to model long-term creep performance for nickel-base superalloy weldments in high temperature power generation systems. The project uses physics-based modeling methodologies and algorithms for predicting alloy properties in heterogeneous material structures. The modeling methodology will be demonstrated on a gas turbine combustor liner weldment of Haynes 282 precipitate-strengthened nickel-base superalloy. The major developments are: (1) microstructure-property relationships under creep conditions and microstructure characterization (2) modeling inhomogeneous microstructure in superalloy weld (3) modeling mesoscale plastic deformation in superalloy weld and (4) a constitutive creep model that accounts for weld and base metal microstructure and their long term evolution. The developed modeling technology is aimed to provide a more efficient and accurate assessment of a material’s long-term performance compared with current testing and extrapolation methods. This modeling technology will also accelerate development and qualification of new materials in advanced power generation systems. This document is a final technical report for the project, covering efforts conducted from October 2014 to December 2016.

  17. Improved nickel plating of Inconel X-750

    Science.gov (United States)

    Farmer, M. E.; Feeney, J. E.; Kuster, C. A.

    1969-01-01

    Electroplating technique with acid pickling provides a method of applying nickel plating on Inconel X-750 tubing to serve as a wetting agent during brazing. Low-stress nickel-plating bath contains no organic wetting agents that cause the nickel to blister at high temperatures.

  18. Residual stresses analysis in ball end milling of nickel-based superalloy Inconel 718

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Junteng; Zhang, Dinghua; Wu, Baohai; Luo, Ming [Key Laboratory of Contemporary Design and Integrated Manufacturing Technology, Northwestern Polytechnical University (China)

    2017-11-15

    Inconel 718 is widely used in the aviation, space, automotive and biomedical industries because of its outstanding properties. Near-surface residual stresses that are induced by ball end milling in Inconel 718 can be crucial for the performance and service time of the machined parts. In this paper, the influences of cutting conditions, including the use of cutting parameters, cutting fluid and spindle angles, on the residual stresses in the ball end milling process of Inconel 718 alloy were investigated experimentally. X-ray diffraction measurements reveal that residual stress distributions are highly influenced by cutting parameters, especially the depth of cut and cutting speed. The milling operation with cooling induces more compressive stresses trend and the magnitude of the residual stresses increases in the tensile direction with the increase of spindle angles. These cutting induced effects were further discussed with respect to thermal- mechanical coupling theory and some observations made by optical microscopy. From this investigation, it is suggested that the machining process parameters are not the smaller the better for the control of residual stresses in the ball end milling process of Inconel 718. (author)

  19. Grinding of Inconel 713 superalloy for gas turbines

    Czech Academy of Sciences Publication Activity Database

    Čapek, J.; Kyncl, J.; Kolařík, K.; Beránek, L.; Pitrmuc, Z.; Medřický, Jan; Pala, Z.

    2016-01-01

    Roč. 16, č. 1 (2016), s. 14-15 ISSN 1213-2489 Institutional support: RVO:61389021 Keywords : Casting defects * Gas turbine * Grinding * Nickel superalloy * Residual stresses Subject RIV: JJ - Other Materials

  20. Cyclic Oxidation and Hot Corrosion Behavior of Nickel-Iron-Based Superalloy

    Science.gov (United States)

    Chellaganesh, D.; Adam Khan, M.; Winowlin Jappes, J. T.; Sathiyanarayanan, S.

    2018-01-01

    The high temperature oxidation and hot corrosion behavior of nickel-iron-based superalloy are studied at 900 ° and 1000 °C. The significant role of alloying elements with respect to the exposed medium is studied in detail. The mass change per unit area was catastrophic for the samples exposed at 1000 °C and gradual increase in mass change was observed at 900 °C for both the environments. The exposed samples were further investigated with SEM, EDS and XRD analysis to study the metallurgical characteristics. The surface morphology has expressed the in situ nature of the alloy and its affinity toward the environment. The EDS and XRD analysis has evidently proved the presence of protective oxides formation on prolonged exposure at elevated temperature. The predominant oxide formed during the exposure at high temperature has a major contribution toward the protection of the samples. The nickel-iron-based superalloy is less prone to oxidation and hot corrosion when compared to the existing alloy in gas turbine engine simulating marine environment.

  1. Relationship of heat treatment-mechanical properties of nickel base superalloys

    International Nuclear Information System (INIS)

    Zamora R, L.

    1997-01-01

    The nickel-base superalloys have high strength, excellent corrosion resistant, and good creep and fatigue resistance. These alloy improved properties at high temperature derive their mechanical and creep behavior on γ precipitate morphology, and the evolution of such morphology during different heat treatment conditions. The main microstructural variable of Nickel-based superalloys, responsible for the mechanical properties are: a) amount and morphology of precipitates; b) size and shape of grains; and c) carbide distribution. In this work, a Nickel-base superalloy Nimonic 80A, modified little with Zr prepared by melting and casting practices of materials electrolytic in vacuum-induction melting (VIM) type Balzers, to obtain five alloys different and ingots of 2 Kg and 1 Kg, with composition in weight % of Nimonic 80-A is: Ni = bal (76.66), C = 0.01, Cr = 19.83, Fe = 2.4, Mn = 0.17, Si 0.47, Al = 0.19, Zr = 0.4. The solidification process is made in a steel mold. After having realized four thermal treatments, the most representative microstructures there were obtained. The results from tensile tests performed on Instron Servohydraulic testing systems at uniaxial dynamic testing, at constant speeds to ,0.2 cm/min, were: the yield strength, the ultimate strength value, percentage elongation and area reduction. Creep tests were performed at in stress of 90 and 129 MPa, at a temperature of 600 and 680 Centigrades at different times and width of specimen of 1 mm. The alloys were analyzed by MEB(JEOL 35CF) at different magnifications. The nucleation and growth of intergranular cavities during creep of alloy Nimonic M3, were investigated. One sample was deformed in creep at 129 MPa and 680 Centigrades during 110 hs. Creep samples were annealing heat treated at 800 Centigrades, during 7 days. After a careful sample preparation procedure, 3100 of cavities were measured in the sample . The cavity size distributions in the sample were obtained. The cavity growth rate, was

  2. Fractography analysis of Inconel 718 fatigued at 700°C

    Directory of Open Access Journals (Sweden)

    Michal Jambor

    2016-12-01

    Full Text Available This work deals with the fractography analysis of nickel-base superalloy Inconel 718 fatigued at 700°C in air atmosphere in the high cycle region. During cyclic loading of this alloy at high temperatures some different mechanisms compared to cyclic loading at ambient temperature take place. Cyclic plastic deformation at high temperatures causes some structural changes, which could have some influence on the fatigue process.

  3. STUDY OF THE MECHANICAL PROPERTIES OF INCONEL 718 SUPERALLOY AFTER HOT TENSILE TESTS

    Directory of Open Access Journals (Sweden)

    Tarcila Sugahara

    2014-10-01

    Full Text Available This research work investigated some important mechanical properties of Inconel 718 superalloy using hot tensile tests like conventional yield strength to 0.2% strain (σe , ultimate strength (σr , and specific elongation (εu . Samples were strained to failure at temperatures of 600°C, 650°C, 700°C, 750°C, 800°C and 850°C and strain rate of 0.5 mm/min (2 × 10–4 s–1 according to ASTM E-8. The results showed higher values σe of yield strength at 700°C, this anomalous behavior can be attributed to the presence of hardening precipitates as observed in the TTT diagram of superalloy Inconel 718. Examination of the sample’s surfaces tensile fracture showed that with increasing temperature test the actuating mechanism changes from intergranular fracture to coalescence of the microcavities.

  4. Analysis of laser beam weldability of Inconel 738 superalloy

    International Nuclear Information System (INIS)

    Egbewande, A.T.; Buckson, R.A.; Ojo, O.A.

    2010-01-01

    The susceptibility of pre-weld heat treated laser beam welded IN 738 superalloy to heat affected zone (HAZ) cracking was studied. A pre-weld heat treatment that produced the minimal grain boundary liquation resulted in a higher level of cracking compared to those with more intergranular liquation. This deviation from the general expectation of influence of intergranular liquation extent on HAZ microfissuring is attributable to the reduction in the ability of the base alloy to accommodate welding tensile stress that accompanied a pre-weld heat treatment condition designed to minimize intergranular liquation. Furthermore, in contrast to what has been generally reported in other nickel-based superalloys, a decrease in laser welding speed resulted in increased HAZ cracking in the IN 738, which can be attributed to exacerbated process instability at lower welding speeds.

  5. Near-surface residual stresses and microstructural changes after turning of a nickel-based superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Schlauer, Christian

    2003-07-01

    Nickel-based superalloys are precipitation hardened alloys with complex compositions. They are used in aircraft engines and land-based gas turbines in load bearing structural components that are exposed to high temperatures. Failure mechanisms in this environment are high and low cycle fatigue, creep, and corrosion. During manufacturing, residual stresses are often introduced into the material due to inhomogeneous plastic deformations, both intentionally and unintentionally. One such manufacturing process is metal cutting, which introduces residual stresses in the surface layer. The stress state in the near-surface zone of components is of special interest as the surface often experiences peak loads and cracks have their starting point there. In this thesis, near-surface residual stress distributions and microstructural changes are studied in the nickel-based superalloy Inconel 718 for two different turning operations, face grooving and facing. Process variables are in both cases cutting speed and feed that have been varied between (10 and 1200) m/min and (0.01 and 0.5) mm, respectively. The first turning technique face grooving, which gives cutting conditions similar to orthogonal cutting, showed a clear dependency of the residual stresses on the cutting speed. The tensile stress at the surface, the maximum compressive stress below the surface, and the thickness of the affected layer increase with increasing cutting speed. The tensile stresses are constrained to a thin surface layer and compressive residual stresses below the surface dominate the depth profile of the residual stresses. Only at low cutting speed, residual stresses were largely avoided. The second turning technique facing confirmed the dependency of the residual stresses on the cutting speed and revealed a similar dependency on the feed. Microstructural investigations of near-surface cross-sections by means of transmission electron microscopy showed a zone where the grains had undergone plastic

  6. Laser aided direct metal deposition of Inconel 625 superalloy: Microstructural evolution and thermal stability

    International Nuclear Information System (INIS)

    Dinda, G.P.; Dasgupta, A.K.; Mazumder, J.

    2009-01-01

    Direct metal deposition technology is an emerging laser aided manufacturing technology based on a new additive manufacturing principle, which combines laser cladding with rapid prototyping into a solid freeform fabrication process that can be used to manufacture near net shape components from their CAD files. In the present study, direct metal deposition technology was successfully used to fabricate a series of samples of the Ni-based superalloy Inconel 625. A high power CO 2 laser was used to create a molten pool on the Inconel 625 substrate into which an Inconel 625 powder stream was delivered to create a 3D object. The structure and properties of the deposits were investigated using optical and scanning electron microscopy, X-ray diffraction and microhardness test. The microstructure has been found to be columnar dendritic in nature, which grew epitaxially from the substrate. The thermal stability of the dendritic morphology was investigated in the temperature range 800-1200 deg. C. These studies demonstrate that Inconel 625 is an attractive material for laser deposition as all samples produced in this study are free from relevant defects such as cracks, bonding error and porosity.

  7. Laser aided direct metal deposition of Inconel 625 superalloy: Microstructural evolution and thermal stability

    Energy Technology Data Exchange (ETDEWEB)

    Dinda, G.P., E-mail: dindag@focushope.edu [Center for Advanced Technologies, Focus: HOPE, Detroit, MI 48238 (United States); Center for Laser Aided Intelligent Manufacturing, University of Michigan, Ann Arbor, MI 48109 (United States); Dasgupta, A.K. [Center for Advanced Technologies, Focus: HOPE, Detroit, MI 48238 (United States); Mazumder, J. [Center for Laser Aided Intelligent Manufacturing, University of Michigan, Ann Arbor, MI 48109 (United States)

    2009-05-25

    Direct metal deposition technology is an emerging laser aided manufacturing technology based on a new additive manufacturing principle, which combines laser cladding with rapid prototyping into a solid freeform fabrication process that can be used to manufacture near net shape components from their CAD files. In the present study, direct metal deposition technology was successfully used to fabricate a series of samples of the Ni-based superalloy Inconel 625. A high power CO{sub 2} laser was used to create a molten pool on the Inconel 625 substrate into which an Inconel 625 powder stream was delivered to create a 3D object. The structure and properties of the deposits were investigated using optical and scanning electron microscopy, X-ray diffraction and microhardness test. The microstructure has been found to be columnar dendritic in nature, which grew epitaxially from the substrate. The thermal stability of the dendritic morphology was investigated in the temperature range 800-1200 deg. C. These studies demonstrate that Inconel 625 is an attractive material for laser deposition as all samples produced in this study are free from relevant defects such as cracks, bonding error and porosity.

  8. Atomic force microscopy imaging to measure precipitate volume fraction in nickel-based superalloys

    International Nuclear Information System (INIS)

    Bourhettar, A.; Troyon, M.; Hazotte, A.

    1995-01-01

    In nickel-based superalloys, quantitative analysis of scanning electron microscopy images fails in providing accurate microstructural data, whereas more efficient techniques are very time-consuming. As an alternative approach, the authors propose to perform quantitative analysis of atomic force microscopy images of polished/etched surfaces (quantitative microprofilometry). This permits the measurement of microstructural parameters and the depth of etching, which is the main source of measurement bias. Thus, nonbiased estimations can be obtained by extrapolation of the measurements up to zero etching depth. In this article, the authors used this approach to estimate the volume fraction of γ' precipitates in a nickel-based superalloy single crystal. Atomic force microscopy images of samples etched for different times show definition, homogeneity, and contrast high enough to perform image analysis. The result after extrapolation is in very good agreement with volume fraction values available from published reports

  9. Experimental Investigation on High-Cycle Fatigue of Inconel 625 Superalloy Brazed Joints

    Science.gov (United States)

    Chen, Jianqiang; Demers, Vincent; Turner, Daniel P.; Bocher, Philippe

    2018-04-01

    The high-cycle fatigue performance and crack growth pattern of transient liquid phase-brazed joints in a nickel-based superalloy Inconel 625 were studied. Assemblies with different geometries and types of overlaps were vacuum-brazed using the brazing paste Palnicro-36M in conditions such as to generate eutectic-free joints. This optimal microstructure provides the brazed assemblies with static mechanical strength corresponding to that of the base metal. However, eutectic micro-constituents were observed in the fillet region of the brazed assembly due to an incomplete isothermal solidification within this large volume of filler metal. The fatigue performance increased significantly with the overlap distance for single-lap joints, and the best performance was found for double-lap joints. It was demonstrated that these apparent changes in fatigue properties according to the specimen geometry can be rationalized when looking at the fatigue data as a function of the local stress state at the fillet radii. Fatigue cracks were nucleated from brittle eutectic phases located at the surface of the fillet region. Their propagation occurred through the bimodal microstructure of fillet and the diffusion region to reach the base metal. High levels of crack path tortuosity were observed, suggesting that the ductile phases found in the microstructure may act as a potential crack stopper. The fillet region must be considered as the critical region of a brazed assembly for fatigue applications.

  10. Synergistic effect of rhenium and ruthenium in nickel-based single-crystal superalloys

    Energy Technology Data Exchange (ETDEWEB)

    Yu, X.X. [Department of Physics, Tsinghua University, Beijing 100084 (China); Department of Materials Science and Engineering, Tsinghua University, Beijing 100084 (China); Wang, C.Y., E-mail: cywang@mail.tsinghua.edu.cn [Department of Physics, Tsinghua University, Beijing 100084 (China); Central Iron and Steel Research Institute, Beijing 100081 (China); Zhang, X.N. [Institute of Microstructure and Property of Advanced Materials, Beijing University of Technology, Beijing 100124 (China); Yan, P. [Central Iron and Steel Research Institute, Beijing 100081 (China); Zhang, Z., E-mail: zezhang@zju.edu.cn [State Key Laboratory of Silicon Materials, Department of Materials Science and Engineering, Zhejiang University, Hangzhou 310027 (China)

    2014-01-05

    Highlights: • Re and Ru synergistic effects in nickel-based superalloys are investigated. • The Al site occupation of Re atom in the γ′ phase is observed directly. • The addition of Ru results in the repartitioning of Re to γ phase. -- Abstract: The microstructures of ternary Ni–Al–Re and quaternary Ni–Al–Re–Ru single-crystal alloys were investigated at atomic and electronic levels to clarify the synergistic effect of Re and Ru in nickel-based single-crystal superalloys. In the Ni–Al–Re alloy, it was directly observed that Re atom occupied the Al site of γ′ phase. In the Ni–Al–Re–Ru alloy, the mechanisms of Re repartition between γ and γ′ phases were proposed. In the dendritic cores, high concentrations of Re exceeded the solubility limit of γ′ phase and partitioned to γ phase, which led to the homogenization. In the interdendritic regions, Ru resulted in the repartitioning of Re to γ phase which was proved by transmission electron microscopy and first-principles calculations.

  11. Kink structures induced in nickel-based single crystal superalloys by high-Z element migration

    Energy Technology Data Exchange (ETDEWEB)

    Sun, Fei; Zhang, Jianxin [Key Laboratory for Liquid Structure and Heredity of Materials, Ministry of Education, Shandong University, Jinan 250061 (China); Mao, Shengcheng [Institute of Microstructure and Property of Advanced Materials, Beijing University of Technology, Beijing 100124 (China); Jiang, Ying [Center of Electron Microscopy and State Key Laboratory of Silicon Materials, Department of Materials Science and Engineering, Zhejiang University, Hangzhou 310027 (China); Feng, Qiang [National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083 (China); State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083 (China); Shen, Zhenju; Li, Jixue; Zhang, Ze [Center of Electron Microscopy and State Key Laboratory of Silicon Materials, Department of Materials Science and Engineering, Zhejiang University, Hangzhou 310027 (China); Han, Xiaodong [Institute of Microstructure and Property of Advanced Materials, Beijing University of Technology, Beijing 100124 (China)

    2015-01-05

    Highlights: • Innovative kink structures generate at the γ/γ′ interfaces in the crept superalloy. • Clusters of heavy elements congregate at the apex of the kinks. • Dislocation core absorbs hexagonal structural high-Z elements. - Abstract: Here, we investigate a new type of kink structure that is found at γ/γ′ interfaces in nickel-based single crystal superalloys. We studied these structures at the atomic and elemental level using aberration corrected high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM). The core of the dislocation absorbs high-Z elements (i.e., Co and Re) that adopt hexagonal arrangements, and it extrudes elements (i.e., Ni and Al) that adopt face centered cubic (fcc) structures. High-Z elements (i.e., Ta and W) and Cr, which is a low-Z element, are stabilized in body centered cubic (bcc) arrangements; Cr tends to behave like Re. High-Z elements, which migrate and adopt a hexagonal structure, induce kink formation at γ/γ′ interfaces. This process must be analyzed to fully understand the kinetics and dynamics of creep in nickel-based single crystal superalloys.

  12. Welding Metallurgy of Nickel-Based Superalloys for Power Plant Construction

    Science.gov (United States)

    Tung, David C.

    Increasing the steam temperature and pressure in coal-fired power plants is a perpetual goal driven by the pursuit of increasing thermal cycle efficiency and reducing fuel consumption and emissions. The next target steam operating conditions, which are 760°C (1400°F) and 35 MPa (5000 psi) are known as Advanced Ultra Supercritical (AUSC), and can reduce CO2 emissions up to 13% but this cannot be achieved with traditional power plant construction materials. The use of precipitation-strengthened Nickel-based alloys (superalloys) is required for components which will experience the highest operating temperatures. The leading candidate superalloys for power plant construction are alloys 740H, 282, and 617. Superalloys have excellent elevated temperature properties due to careful microstructural design which is achieved through very specific heat treatments, often requiring solution annealing or homogenization at temperatures of 1100 °C or higher. A series of postweld heat treatments was investigated and it was found that homogenization steps before aging had no noticeable effect on weld metal microhardness, however; there were clear improvements in weld metal homogeneity. The full abstract can be viewed in the document itself.

  13. On the microstructural origin of primary creep in nickel-base superalloys

    International Nuclear Information System (INIS)

    Heilmaier, M.; Reppich, B.

    1997-01-01

    The nature of primary creep in nickel-base superalloys is strongly correlated to the different hardening species present in the material. In fine-grained single-phase material the classical assumption of a homogeneous dislocation distribution enables the prediction of the transition from normal via sigmoidal to inverse primary creep with decreasing applied stress σ. In coarse-grained material the back stress σ b of hard subgrain boundaries evolving during plastic deformation must be additionally taken into account. Second-phase particles influence creep in a 2-fold manner via reducing the effective stress σ eff , namely directly by the stress σ p * for particle overcoming, and indirectly by increasing the dislocation density ρ. The proposed approach accounts for the observed pronounced normal primary creep in particle-strengthened superalloys. (orig.)

  14. Eddy Current Nondestructive Residual Stress Assessment in Shot-Peened Nickel-Base Superalloys

    International Nuclear Information System (INIS)

    Blodgett, M.P.; Yu, F.; Nagy, P.B.

    2005-01-01

    Shot peening and other mechanical surface enhancement methods improve the fatigue resistance and foreign-object damage tolerance of metallic components by introducing beneficial near-surface compressive residual stresses and hardening the surface. However, the fatigue life improvement gained via surface enhancement is not explicitly accounted for in current engine component life prediction models because of the lack of accurate and reliable nondestructive methods that could verify the presence of compressive near-surface residual stresses in shot-peened hardware. In light of its frequency-dependent penetration depth, the measurement of eddy current conductivity has been suggested as a possible means to allow the nondestructive evaluation of subsurface residual stresses in surface-treated components. This technique is based on the so-called piezoresistivity effect, i.e., the stress-dependence of electrical resistivity. We found that, in contrast with most other materials, surface-treated nickel-base superalloys exhibit an apparent increase in electrical conductivity at increasing inspection frequencies, i.e., at decreasing penetration depths. Experimental results are presented to illustrate that the excess frequency-dependent apparent eddy current conductivity of shot-peened nickel-base superalloys can be used to estimate the absolute level and penetration depth of the compressive residual stress layer both before and after partial thermal relaxation

  15. Precipitate Contribution to the Acoustic Nonlinearity in Nickel-Based Superalloy

    Institute of Scientific and Technical Information of China (English)

    Chung-Seok KIM; Cliff J.LISSENDEN

    2009-01-01

    The influence of γ' precipitate on the acoustic nonlinearity is investigated for a nickel-based superalloy,which is subjected to creep deformation.During creep deformation,the cuboidal γ' precipitate is preferentially coarsened in a direction perpendicular to the applied stress axis.The length and shape factor of the γ' precipitate increase with creep time.The increase of relative acoustic nonlinearity with increasing fraction of creep life is discussed in relation to the rafting of γ' precipitate,which is closely related to the scattering and distortion of the acoustic wave.

  16. Effect of grain structure on phase transformation events in Inconel 718

    International Nuclear Information System (INIS)

    Dahotre, N.B.; McCay, M.H.; McCay, T.D.; Hubbard, C.R.; Porter, W.D.; Cavin, O.B.

    1993-01-01

    Nickel base superalloys generally obtain their maximum strength from γ'[Ni 3 (Al,Ti)] and γ double-prime[Ni 3 (Al,Ti,Nb)] age hardening precipitates. During welding the γ' precipitation is very rapid and can lead to strain age cracking, which limits weldability. Thus, the weldable superalloys are limited in their Al and Ti content and hence in their ultimate strength. One method of increasing the ultimate strength of a superalloy, while avoiding strain age cracking, is the addition of Nb. This produces Ni 3 Nb(δ), and when used in conjunction with a limited amount of γ', results in an increase in strength without strain age cracking problems. The γ double-prime does not lead to strain age cracking because its transformation kinetics are too slow for formation during ordinary welding practice. This combination of γ' and γ double-prime strengthening is incorporated into the Inconel 718 alloys. The research reported herein was undertaken to determine the time-temperature response of Inconel 718 in the as-cast, wrought and wrought-grain-grown states, using differential thermal analysis (DTA). It is essential to locate the temperature regime of each phase transformation event and to study the transformation sequence in order to tailor sound laser welding techniques for Inconel 718. In the present research, a DTA technique was employed to study both the phase transformation events and the phase transformation sequence as a function of the pre-existing condition of the alloy

  17. Correlation Between the Microstructural Defects and Residual Stress in a Single Crystal Nickel-Based Superalloy During Different Creep Stages

    Science.gov (United States)

    Mo, Fangjie; Wu, Erdong; Zhang, Changsheng; Wang, Hong; Zhong, Zhengye; Zhang, Jian; Chen, Bo; Hofmann, Michael; Gan, Weimin; Sun, Guangai

    2018-03-01

    The present work attempts to reveal the correlation between the microstructural defects and residual stress in the single crystal nickel-based superalloy, both of which play the significant role on properties and performance. Neutron diffraction was employed to investigate the microstructural defects and residual stresses in a single crystal (SC) nickel-based superalloy, which was subjected to creeping under 220 MPa and 1000 °C for different times. The measured superlattice and fundamental lattice reflections confirm that the mismatch and tetragonal distortions with c/a > 1 exist in the SC superalloy. At the initially unstrained state, there exists the angular distortion between γ and γ' phases with small triaxial compressive stresses, ensuring the structural stability of the superalloy. After creeping, the tetragonal distortion for the γ phase is larger than that for the γ' phase. With increasing the creeping time, the mismatch between γ and γ' phases increases to the maximum, then decreases gradually and finally remains unchanged. The macroscopic residual stress shows a similar behavior with the mismatch, indicating the correlation between them. Based on the model of shear and dislocations, the evolution of microstructural defects and residual stress are reasonably explained. The effect of shear is dominant at the primary creep stage, which greatly enlarges the mismatch and the residual stress. The dislocations weaken the effect of shear for the further creep stage, resulting in the decrease of the mismatch and relaxation of the residual stress. Those findings add some helpful understanding into the microstructure-performance relationship in the SC nickel-based superalloy, which might provide the insight to materials design and applications.

  18. Microstructural investigation of thermally aged nickel-based superalloy 718Plus

    International Nuclear Information System (INIS)

    Whitmore, Lawrence; Ahmadi, Mohammad Reza; Stockinger, Martin; Povoden-Karadeniz, Erwin; Kozeschnik, Ernst; Leitner, Harald

    2014-01-01

    The effects of thermal aging upon the nickel-based 718Plus superalloy are investigated and modelled. Yield strength and micro-hardness measurements are made after solution annealing and after aging at 788 °C for 4 h. In order to explain the differences in strength and hardness, a detailed investigation of the microstructure is performed using transmission electron microscopy. The size and phase fraction of the γ′ precipitates are measured and related to the measured hardness and yield strength using a theoretical model of precipitation strengthening based on the shearing of precipitates in terms of coherency strengthening and the formation of an antiphase boundary

  19. Identifying and Understanding Environment-Induced Crack propagation Behavior in Ni-based Superalloy INCONEL 617

    Energy Technology Data Exchange (ETDEWEB)

    Ma, Longzhou

    2012-11-30

    The nickel-based superalloy INCONEL 617 is a candidate material for heat exchanger applications in the next-generation nuclear plant (NGNP) system. This project will study the crack propagation process of alloy 617 at temperatures of 650°C-950°C in air under static/cyclic loading conditions. The goal is to identify the environmental and mechanical damage components and to understand in-depth the failure mechanism. Researchers will measure the fatigue crack propagation (FCP) rate (da/dn) under cyclic and hold-time fatigue conditions, and sustained crack growth rates (da/dt) at elevated temperatures. The independent FCP process will be identified and the rate-controlled sustained loading crack process will be correlated with the thermal activation equation to estimate the oxygen thermal activation energy. The FCP-dependent model indicates that if the sustained loading crack growth rate, da/dt, can be correlated with the FCP rate, da/dn, at the full time dependent stage, researchers can confirm stress-accelerated grain-boundary oxygen embrittlement (SAGBOE) as a predominate effect. Following the crack propagation tests, the research team will examine the fracture surface of materials in various cracking stages using a scanning electron microscope (SEM) and an optical microscope. In particular, the microstructure of the crack tip region will be analyzed in depth using high resolution transmission electron microscopy (TEM) and electron energy loss spectrum (EELS) mapping techniques to identify oxygen penetration along the grain boundary and to examine the diffused oxygen distribution profile around the crack tip. The cracked sample will be prepared by focused ion beam nanofabrication technology, allowing researchers to accurately fabricate the TEM samples from the crack tip while minimizing artifacts. Researchers will use these microscopic and spectroscopic results to interpret the crack propagation process, as well as distinguish and understand the environment or

  20. Study on the machinability characteristics of superalloy Inconel 718 during high speed turning

    International Nuclear Information System (INIS)

    Thakur, D.G.; Ramamoorthy, B.; Vijayaraghavan, L.

    2009-01-01

    The present paper is an attempt of an experimental investigation on the machinability of superalloy, Inconel 718 during high speed turning using tungsten carbide insert (K20) tool. The effect of machining parameters on the cutting force, specific cutting pressure, cutting temperature, tool wear and surface finish criteria were investigated during the experimentation. The machining parameters have been optimized by measuring forces. The effect of machining parameters on the tool wear was examined through SEM micrographs. During high speed turning acoustic emission signal were collected and analyzed to understand the effect of cutting parameters during online. The research work findings will also provide useful economic machining solution by utilizing economical tungsten carbide tooling during high speed processing of Inconel 718, which is otherwise usually machined by costly PCD or CBN tools. The present approach and results will be helpful for understanding the machinability of Inconel 718 during high speed turning for the manufacturing engineers

  1. Prediction of recrystallisation in single crystal nickel-based superalloys during investment casting

    Directory of Open Access Journals (Sweden)

    Panwisawas Chinnapat

    2014-01-01

    Full Text Available Production of gas turbines for jet propulsion and power generation requires the manufacture of turbine blades from single crystal nickel-based superalloys, most typically using investment casting. During the necessary subsequent solution heat treatment, the formation of recrystallised grains can occur. The introduction of grain boundaries into a single crystal component is potentially detrimental to performance, and therefore manufacturing processes and/or component geometries should be designed to prevent their occurrence. If the boundaries have very low strength, they can degrade the creep and fatigue properties. The root cause for recrystallisation is microscale plasticity caused by differential thermal contraction of metal, mould and core; when the plastic deformation is sufficiently large, recrystallisation takes place. In this work, numerical and thermo-mechanical modelling is carried out, with the aim of establishing computational methods by which recrystallisation during the heat treatment of single crystal nickel-based superalloys can be predicted and prevented prior to their occurrence. Elasto-plastic law is used to predict the plastic strain necessary for recrystallisation. The modelling result shows that recrystallisation is most likely to occur following 1.5–2.5% plastic strain applied at temperatures between 1000 ∘C and 1300 ∘C; this is validated with tensile tests at these elevated temperatures. This emphasises that high temperature deformation is more damaging than low temperature deformation.

  2. Hot isostatic pressing of single-crystal nickel-base superalloys: Mechanism of pore closure and effect on Mechanical properties

    Directory of Open Access Journals (Sweden)

    Epishin Alexander I.

    2014-01-01

    Full Text Available Pore annihilation was investigated in the single-crystal nickel-base superalloy CMSX-4. HIP tests at 1288 °C/103 MPa were interrupted at different times, then the specimens were investigated by TEM, metallography and density measurements. The kinetics of pore annihilation was determined. The pore closure mechanism was identified as plastic deformation on the octahedral slip systems. A model describing the kinetics of pore closure has been developed on the base of crystal plasticity and large strain theory. Mechanical tests with the superalloy CMSX-4 and the Ru-containing superalloy VGM4 showed, that HIP significantly increases the fatigue life at low temperatures but has no effect on creep strength.

  3. Relating microstructures to SCC in Inconel 718

    International Nuclear Information System (INIS)

    Sheth, N.K.; Sanchez, J.M.; Hendrix, B.C.; Ide, H.; Miglin, M.T.

    1993-01-01

    Inconel 718, a nickel-iron-base superalloy, is used for stressed applications in the nuclear and oil industries. A major concern facing the continued and expanding use of Inconel 718 in these applications has been their susceptibility to Inter-Granular Stress Corrosion Cracking (IGSCC). Efforts to reduce stress corrosion cracking (SCC) have been aimed at reducing the susceptibility in this alloy to the formation of the deleterious delta (Ni 3 Nb) phase. Microstructural evaluation of SCC test specimens of different thermo-mechanical histories shows that inhomogeneities of all types, including carbides, nitrides, and different morphologies of δ phase, worsen the SCC resistance of IN718. Here the authors study five samples of IN718 with measured hardness and SCC growth rates. A preliminary ranking of the factors mentioned above on SCC resistance finds that precipitation of a fine δ phase, due to over-aging, has the most profound effect on SCC susceptibility of IN718

  4. Transformed model fitting. A straightforward approach to evaluation of anisotropic SANS from nickel-base single-crystal superalloys

    International Nuclear Information System (INIS)

    Strunz, P.

    1999-01-01

    Schematic description of a special evaluation procedure for data treatment of anisotropic Small-Angle Neutron Scattering (SANS) is presented. The use of the discussed procedure is demonstrated on a data taken from investigation of precipitation in single-crystal nickel-base superalloys. (author)

  5. The effect of vacuum environment on creep rupture properties of Inconel 617 at 1000 deg C

    International Nuclear Information System (INIS)

    Ohnami, Masateru; Imamura, Riuzo

    1981-01-01

    The creep rupture strength of nickel-base superalloy in weakly acidic gas at high temperature above 1000 deg C lowers remarkably as compared with that in the atmosphere, and this problem is one of the important subjects in connection with the research and development of high temperature heat exchangers for multi-purpose high temperature gas-cooled reactor system being developed in Japan. In the case of Inconel 617, abnormal decarbonization phenomenon occurs in weakly acidic gas, and this is regarded as the cause of lowering the creep strength. In this study, the effects of the decarbonization in weak vacuum at 1000 deg C and the oxidation of Inconel 617 on its crack occurrence and propagation were clarified experimentally with notched plate test pieces. The material used was Inconel 617 nickel-base superalloy made by Huntington Alloys Inc. in the U.S. The creep rupture experiment was carried out with a simple tension creep tester. At the nominal stress of 3.5 kg/mm 2 , the creep rupture time in 0.3 Torr was the shortest when the grain size was 78 μm, and the creep rupture time increased as the grain size became larger. The creep rupture time in 0.3 Torr decreased to a half of that in the atmosphere. In 0.3 Torr, cracks occurred early, and propagated fast as compared with in the atmosphere. This is because the local creep velocity at the bottom of notches and in front of creep cracks is fast owing to the lack of protective oxide film. (Kako, I.)

  6. Optimization of process parameters for WEDM of Inconel 825 using grey relational analysis

    Directory of Open Access Journals (Sweden)

    Pawan Kuma

    2018-09-01

    Full Text Available Inconel 825 is high nickel-chromium-based superalloy which retains its mechanical properties and exhibits good corrosion and oxidation resistance at elevated temperature. Inconel 825 is extensively used for making aircraft engine parts like combustor casing and turbine blades in aero space industry. This research proposed the Response Surface Methodology with GRA to optimize multiple responses during Wire-cut EDM of Inconel 825. At optimum combination of input parameters i.e. A4B1C1D5E4F2, increase in MRR from 36.13 mm2/min to 41.822 mm2/min, decrease in SR from 2.842μm to 2.445μm and decrease in WWR from 0.01832 to 0.01758 was obtained. Experimental results showed that pulse-on time, wire feed, pulse-off time, and peak current significantly affected the MRR, and surface integrity of specimen and electrode with the formation of craters, pockmarks, debris, micro cracks, and recast layer. The optimal parametric combination obtained from the present study will be advantageous for working on high strength; high thermal conductivity and low melting point materials like nickel alloys.

  7. Microstructure of the Nickel-Base Superalloy CMSX-4 Fabricated by Selective Electron Beam Melting

    Science.gov (United States)

    Ramsperger, Markus; Singer, Robert F.; Körner, Carolin

    2016-03-01

    Powder bed-based additive manufacturing (AM) processes are characterized by very high-temperature gradients and solidification rates. These conditions lead to microstructures orders of magnitude smaller than in conventional casting processes. Especially in the field of high performance alloys, like nickel-base superalloys, this opens new opportunities for homogenization and alloy development. Nevertheless, the high susceptibility to cracking of precipitation-hardenable superalloys is a challenge for AM. In this study, electron beam-based AM is used to fabricate samples from gas-atomized pre-alloyed CMSX-4 powder. The influence of the processing strategy on crack formation is investigated. The samples are characterized by optical and SEM microscopy and analyzed by microprobe analysis. Differential scanning calorimetry is used to demonstrate the effect of the fine microstructure on characteristic temperatures. In addition, in situ heat treatment effects are investigated.

  8. Artificial Neural Network-Based Constitutive Relationship of Inconel 718 Superalloy Construction and Its Application in Accuracy Improvement of Numerical Simulation

    Directory of Open Access Journals (Sweden)

    Junya Lv

    2017-01-01

    Full Text Available The application of accurate constitutive relationship in finite element simulation would significantly contribute to accurate simulation results, which play critical roles in process design and optimization. In this investigation, the true stress-strain data of an Inconel 718 superalloy were obtained from a series of isothermal compression tests conducted in a wide temperature range of 1153–1353 K and strain rate range of 0.01–10 s−1 on a Gleeble 3500 testing machine (DSI, St. Paul, DE, USA. Then the constitutive relationship was modeled by an optimally-constructed and well-trained back-propagation artificial neural network (ANN. The evaluation of the ANN model revealed that it has admirable performance in characterizing and predicting the flow behaviors of Inconel 718 superalloy. Consequently, the developed ANN model was used to predict abundant stress-strain data beyond the limited experimental conditions and construct the continuous mapping relationship for temperature, strain rate, strain and stress. Finally, the constructed ANN was implanted in a finite element solver though the interface of “URPFLO” subroutine to simulate the isothermal compression tests. The results show that the integration of finite element method with ANN model can significantly promote the accuracy improvement of numerical simulations for hot forming processes.

  9. Effects of post-weld heat treatment on microstructure and mechanical properties of TLP bonded Inconel718 superalloy

    International Nuclear Information System (INIS)

    Cao, J.; Wang, Y.F.; Song, X.G.; Li, C.; Feng, J.C.

    2014-01-01

    Transient liquid phase bonding of Inconel718 superalloy was carried out using a commercial Ni–Cr–Si–B amorphous interlayer. The interfacial microstructure of Inconel718 joints was analyzed by a scanning electron microscope and a transmission electron microscope. In particular, the effects of post-weld heat treatment on the interfacial microstructure and joining properties of Inconel718 joints were investigated in detail. The results showed that the precipitation of second phases in joints induced by post-weld heat treatment were beneficial to the improvement of joint properties. A tensile strength of 1130 MPa with an elongation percentage of 7% was achieved for a sample bonded at 1050 °C/60 min+1180 °C/60 min followed by the post-weld heat treatment

  10. Low heat input welding of nickel superalloy GTD-111 with Inconel 625 filler metal

    Energy Technology Data Exchange (ETDEWEB)

    Athiroj, Athittaya; Wangyao, Panyawat; Hartung, Fritz; Lothongkum, Gobboon [Chulalongkorn Univ., Bangkok (Thailand). Dept. of Metallurgical Engineering

    2018-03-01

    GTD-111 precipitation-strengthened nickel-based superalloy is widely used in blades of gas turbine engines which operate at high temperature and in a hot localized corrosion atmosphere. After long-term exposure to high temperature, γ' precipitate is known to exhibit catastrophic changes in size and distribution which cause deterioration of its properties and failure of the component. In this study, a damaged blade removed from a land-based gas turbine generator was subjected to nonpre-heat-treated GTAW and laser welding repair with various welding powers in the range of 135 to 295 J x mm{sup -1}, followed by post-weld heat treatment (PWHT) at 1473 K for 7200 s and strain aging at 1118 K for 86 400 s. Results show no significant relationship between welding powers, size and area fraction of the γ' precipitate in the fcc γ matrix in both GTAW and laser-welded specimens. The final γ' precipitate size and distribution depend mainly on PWHT parameters as γ' precipitates in all GTAW and laser welded specimens showed similar size and area fraction independently of the heat input from welding. Unmixed zones are observed in all laser welding specimens which may cause preferential weld corrosion during service. Microcrack occurrence due to welding and PWHT processes is also discussed.

  11. Misorientation related microstructure at the grain boundary in a nickel-based single crystal superalloy

    International Nuclear Information System (INIS)

    Huang, Ming; Zhuo, Longchao; Liu, Zhanli; Lu, Xiaogang; Shi, Zhenxue; Li, Jiarong; Zhu, Jing

    2015-01-01

    The mechanical properties of nickel-based single crystal superalloys deteriorate with increasing misorientation, thus the finished product rate of the casting of single crystal turbine airfoils may be reduced due to the formation of grain boundaries especially when the misorientation angle exceeds to some extent. To this day, evolution of the microstructures at the grain boundaries with misorientation and the relationship between the microstructures and the mechanical properties are still unclear. In this work a detailed characterization of the misorientation related microstructure at the grain boundary in DD6 single crystal superalloy has been carried out using scanning electron microscopy (SEM) and transmission electron microscopy (TEM) techniques; the elemental distribution at the grain boundaries has been analyzed by energy dispersive (EDS) X-ray mapping; and the effect of precipitation of μ phases at the grain boundary on the mechanical property has been evaluated by finite element calculation. It is shown that the proportion of γ phase at the grain boundaries decreases, while the proportion of γ′ phase at the grain boundaries increases with increasing misorientation; the μ phase is precipitated at the grain boundaries when the misorientation angle exceeds about 10° and thus it could lead to a dramatic deterioration of the mechanical properties, as well as that the enrichment of Re and W gradually disappears as the misorientation angle increases. All these factors may result in the degradation of the mechanical properties at the grain boundaries as the misorientation increases. Furthermore, the finite element calculation confirms that precipitation of μ phases at the grain boundary is responsible for the significant deterioration of the mechanical properties when the misorientation exceeds about 10°. This work provides a physical imaging of the microstructure for understanding the relationship between the mechanical properties and the misorientation

  12. Aspectos metalúrgicos de revestimentos dissimilares com a superliga à base de níquel inconel 625 Metallurgical aspects of dissimilar weld overlays of inconel 625 nickel based superalloys

    Directory of Open Access Journals (Sweden)

    Cleiton Carvalho Silva

    2012-09-01

    Full Text Available Prolongar a vida útil e aumentar a confiabilidade de equipamentos e tubulações de plantas de produção e processamento de petróleo é uma busca constante no setor de petróleo e gás. Tais aspectos dependem essencialmente do uso de ligas resistentes à corrosão. Neste contexto, a soldagem de revestimento com superligas à base de níquel tem sido uma alternativa interessante, pois confere aos equipamentos uma alta resistência à corrosão com um custo inferior, se comparado à fabricação de componentes ou tubulações maciças com superligas. Assim, o objetivo do presente trabalho foi investigar o comportamento metalúrgico de revestimento de superliga à base de níquel do tipo Inconel 625 depositados pelo processo TIG com alimentação de arame frio. As soldagens foram realizadas em uma bancada robotizada, empregando uma fonte eletrônica de soldagem com sistema de aquisição de dados para o monitoramento dos sinais de corrente e tensão. A caracterização microestrutural foi realizada através das técnicas de microscopia eletrônica de varredura (MEV e transmissão (MET, espectroscopia de energia dispersiva de raios-X (EDS. Os resultados mostraram que a microestrutura do metal de solda foi constituída por uma matriz γ com fases secundárias ricas em Nb. Foi encontrada a formação de precipitados complexos de carbonetos/nitretos de Ti e Nb.To extend the life and reliability of pipes and equipment in oil & gas production and processing settings is a continuous demand. These aspects are essentially dependent on corrosion resistant alloys used. In this context, the weld overlay with Ni-based superalloys is a great interesting alternative, since improve the corrosion resistance without increase the cost of manufacture when compared to massive equipment. Thus, the objective of this study was to evaluate the metallurgical aspects of Inconel 625 weld overlays deposited by GTAW cold wire feed process. The welds were performed using a

  13. Microstructural response to heat affected zone cracking of prewelding heat-treated Inconel 939 superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Gonzalez, M.A., E-mail: mgonzalez@comimsa.com.mx [Facultad de Ingenieria Mecanica y Electrica (FIME-UANL), Av. Universidad s/n. Ciudad Universitaria, C.P.66451 San Nicolas de los Garza, N.L. (Mexico); Martinez, D.I., E-mail: dorairma@yahoo.com [Facultad de Ingenieria Mecanica y Electrica (FIME-UANL), Av. Universidad s/n. Ciudad Universitaria, C.P.66451 San Nicolas de los Garza, N.L. (Mexico); Perez, A., E-mail: betinperez@hotmail.com [Facultad de Ingenieria Mecanica y Electrica (FIME-UANL), Av. Universidad s/n. Ciudad Universitaria, C.P.66451 San Nicolas de los Garza, N.L. (Mexico); Guajardo, H., E-mail: hguajardo@frisa.com [FRISA Aerospace, S.A. de C.V., Valentin G. Rivero No. 200, Col. Los Trevino, C.P. 66150, Santa Caterina N.L. (Mexico); Garza, A., E-mail: agarza@comimsa.com [Corporacion Mexicana de Investigacion en Materiales S.A. de C.V. (COMIMSA), Ciencia y Tecnologia No.790, Saltillo 400, C.P. 25295 Saltillo Coah. (Mexico)

    2011-12-15

    The microstructural response to cracking in the heat-affected zone (HAZ) of a nickel-based IN 939 superalloy after prewelding heat treatments (PWHT) was investigated. The PWHT specimens showed two different microstructures: 1) spherical ordered {gamma} Prime precipitates (357-442 nm), with blocky MC and discreet M{sub 23}C{sub 6} carbides dispersed within the coarse dendrites and in the interdendritic regions; and 2) ordered {gamma} Prime precipitates in 'ogdoadically' diced cube shapes and coarse MC carbides within the dendrites and in the interdendritic regions. After being tungsten inert gas welded (TIG) applying low heat input, welding speed and using a more ductile filler alloy, specimens with microstructures consisting of spherical {gamma} Prime precipitate particles and dispersed discreet MC carbides along the grain boundaries, displayed a considerably improved weldability due to a strong reduction of the intergranular HAZ cracking associated with the liquation microfissuring phenomena. - Highlights: Black-Right-Pointing-Pointer Homogeneous microstructures of {gamma} Prime spheroids and discreet MC carbides of Ni base superalloys through preweld heat treatments. Black-Right-Pointing-Pointer {gamma} Prime spheroids and discreet MC carbides reduce the intergranular HAZ liquation and microfissuring of Nickel base superalloys. Black-Right-Pointing-Pointer Microstructure {gamma} Prime spheroids and discreet blocky type MC carbides, capable to relax the stress generated during weld cooling. Black-Right-Pointing-Pointer Low welding heat input welding speeds and ductile filler alloys reduce the HAZ cracking susceptibility.

  14. On Post-Weld Heat Treatment of a Single Crystal Nickel-Based Superalloy Joint by Linear Friction Welding

    Directory of Open Access Journals (Sweden)

    T. J. Ma

    2015-09-01

    Full Text Available Three types of post-weld heat treatment (PWHT, i.e. solution treatment + primary aging + secondary aging (I, secondary aging (II, and primary aging + secondary aging (III, were applied to a single crystal nickel-based superalloy joint made with linear friction welding (LFW. The results show that the grains in the thermomechanically affected zone (TMAZ coarsen seriously and the primary γ' phase in the TMAZ precipitates unevenly after PWHT I. The primary γ' phase in the TMAZ and weld zone (WZ precipitates insufficiently and fine granular secondary γ' phase is observed in the matrix after PWHT II. After PWHT III, the primary γ' phase precipitates more sufficiently and evenly compared to PWHTs I and II. Moreover, the grains in the TMAZ have not coarsened seriously and fine granular secondary γ' phase is not found after PWHT III. PWHT III seems more suitable to the LFWed single crystal nickel-based superalloy joints when performing PWHT.

  15. Focused Ion Beam Nanotomography of ruthenium-bearing nickel-base superalloys with focus on cast-microstructure and phase stability

    International Nuclear Information System (INIS)

    Cenanovic, Samir

    2012-01-01

    The influence of rhenium and ruthenium on the multi component system nickel-base superalloy is manifold and complex. An experimental nickel-base superalloy containing rhenium and ruthenium within defined contents, named Astra, was used to investigate the influences of these two elements on the alloy system. The last stage solidification of nickel-base superalloys after Bridgman casting and the high temperature phase stability of these alloys, could be explored with the aid of focused ion beam nanotomography. FIB-nt therefore was introduced and realized at the chair of General Materials Properties of the University Erlangen-Nuremberg. Cast Astra alloys are like other nickel-base superalloys morphologically very inhomogeneous and affected by segregation. In the interdendritic region different structures with huge γ' precipitates are formed. These inhomogeneities and remaining eutectics degrade the mechanical properties, witch makes an understanding of the subsiding processes at solidification of residual melt important for the casting process and the heat treatment. This is why the last stage solidification in the interdendritic region was analyzed. With the help of focused ion beam nanotomography, three different structures identified from 2-D sections could be assigned to one original 3-D structure. It was pointed out, that only the orientation of the plane of the 2-D cut influences the appearance in the 2-D section. The tomography information was used to explain the development during solidification and to create a model of last stage solidification. The interdendritic region is solidifying under the development of eutectic islands. The structure nucleates eutectically epitaxially at primary dendrite arms, with formation of fine γ/γ' precipitates. During solidification the γ' precipitates coarsen in a rod-like structure, and end up in large γ' precipitates. Simulations and other investigations could approve this model. First three

  16. A new method to predict the metadynamic recrystallization behavior in a typical nickel-based superalloy

    International Nuclear Information System (INIS)

    Lin, Y.C.; Chen, Xiao-Min; Chen, Ming-Song; Wen, Dong-Xu; Zhou, Ying; He, Dao-Guang

    2016-01-01

    The metadynamic recrystallization (MDRX) behaviors of a typical nickel-based superalloy are investigated by two-pass hot compression tests and four conventional stress-based conventional approaches (offset stress method, back-extrapolation stress method, peak stress method, and mean stress method). It is found that the conventional stress-based methods are not suitable to evaluate the MDRX softening fractions for the studied superalloy. Therefore, a new approach, 'maximum stress method', is proposed to evaluate the MDRX softening fraction. Based on the proposed method, the effects of deformation temperature, strain rate, initial average grain size, and interpass time on MDRX behaviors are discussed in detail. Results show that MDRX softening fraction is sensitive to deformation parameters. The MDRX softening fraction rapidly increases with the increase of deformation temperature, strain rate, and interpass time. The MDRX softening fraction in the coarse-grain material is lower than that in the fine-grain material. Moreover, the observed microstructures indicate that the initial coarse grains can be effectively refined by MDRX. Based on the experimental results, the kinetics equations are established and validated to describe the MDRX behaviors of the studied superalloy. (orig.)

  17. Microstructural, mechanical and weldability assessments of the dissimilar welds between γ′- and γ″-strengthened nickel-base superalloys

    Energy Technology Data Exchange (ETDEWEB)

    Naffakh Moosavy, Homam, E-mail: homam_naffakh@iust.ac.ir [School of Metallurgy and Materials Engineering, Iran University of Science and Technology (IUST), Tehran 16846-13114 (Iran, Islamic Republic of); Aboutalebi, Mohammad-Reza; Seyedein, Seyed Hossein [School of Metallurgy and Materials Engineering, Iran University of Science and Technology (IUST), Tehran 16846-13114 (Iran, Islamic Republic of); Mapelli, Carlo [Dipartimento di Meccanica, Politecnico di Milano, Via La Massa 34, Milan 20156 (Italy)

    2013-08-15

    Dissimilar welding of γ′- and γ″-strengthened nickel-base superalloys has been investigated to identify the relationship between the microstructure of the welds and the resultant mechanical and weldability characteristics. γ′-Strengthened nickel-base Alloy 500 and γ″-strengthened nickel-base Alloy 718 were used for dissimilar welding. Gas tungsten arc welding operations were utilized for performing the autogenous dissimilar welding. Alloy 500 and Alloy 718 base metals showed various types of phases, carbides, intermetallics and eutectics in their microstructure. The results for Alloy 500 weld metal showed severe segregation of titanium to the interdendritic regions. The Alloy 718 weld metal compositional analysis confirmed the substantial role of Nb in the formation of low-melting eutectic-type morphologies which can reduce the weldability. The microstructure of dissimilar weld metal with dilution level of 65% wt.% displayed semi-developed dendritic structure. The less segregation and less formation of low-melting eutectic structures caused to less susceptibility of the dissimilar weld metal to the solidification cracking. This result was confirmed by analytic modeling achievements. Dissolution of γ″-Ni{sub 3}Nb precipitations took place in the Alloy 718 heat-affected zone leading to sharp decline of the microhardness in this region. Remelted and resolidified regions were observed in the partially-melted zone of Alloy 500 and Alloy 718. Nevertheless, no solidification and liquation cracking happened in the dissimilar welds. Finally, this was concluded that dissimilar welding of γ′- and γ″-strengthened nickel-base superalloys can successfully be performed. - Highlights: • Dissimilar welding of γ′- and γ″-strengthened nickel-base superalloys is studied. • Microstructural, mechanical and weldability aspects of the welds are assessed. • Microstructure of welds, bases and heat-affected zones is characterized in detail. • The type

  18. The microstructure of heat-treated nickel-based superalloy 718Plus

    International Nuclear Information System (INIS)

    Whitmore, Lawrence; Ahmadi, Mohammad Reza; Guetaz, Laure; Leitner, Harald; Povoden-Karadeniz, Erwin; Stockinger, Martin; Kozeschnik, Ernst

    2014-01-01

    The microstructure of thermally aged nickel-based 718Plus superalloy is investigated using transmission electron microscopy (TEM). Solution annealing at 980 °C for 30 min is followed by either the standard quenching to room temperature or quenching directly to 788 °C, before isothermal aging at 788 °C for four hours. Micro-hardness and yield strength are measured to compare the effects of the two variations. The size and phase fraction of γ′ precipitates are measured using dark-field TEM and related to the hardness and yield strength through a theoretical model based on coherency and antiphase boundary effects. A population of very small sub-precipitates is observed and the larger γ′ precipitates are investigated in detail using high resolution scanning TEM to reveal information about the chemical ordering

  19. Additive Manufacturing of Nickel Superalloys: Opportunities for Innovation and Challenges Related to Qualification

    Science.gov (United States)

    Babu, S. S.; Raghavan, N.; Raplee, J.; Foster, S. J.; Frederick, C.; Haines, M.; Dinwiddie, R.; Kirka, M. K.; Plotkowski, A.; Lee, Y.; Dehoff, R. R.

    2018-06-01

    Innovative designs for turbines can be achieved by advances in nickel-based superalloys and manufacturing methods, including the adoption of additive manufacturing. In this regard, selective electron beam melting (SEBM) and selective laser melting (SLM) of nickel-based superalloys do provide distinct advantages. Furthermore, the direct energy deposition (DED) processes can be used for repair and reclamation of nickel alloy components. The current paper explores opportunities for innovation and qualification challenges with respect to deployment of AM as a disruptive manufacturing technology. In the first part of the paper, fundamental correlations of processing parameters to defect tendency and microstructure evolution will be explored using DED process. In the second part of the paper, opportunities for innovation in terms of site-specific control of microstructure during processing will be discussed. In the third part of the paper, challenges in qualification of AM parts for service will be discussed and potential methods to alleviate these issues through in situ process monitoring, and big data analytics are proposed.

  20. Embrittlement of nickel-, cobalt-, and iron-base superalloys by exposure to hydrogen

    Science.gov (United States)

    Gray, H. R.

    1975-01-01

    Five nickel-base alloys (Inconel 718, Udimet 700, Rene 41, Hastelloy X, and TD-NiCr), one cobalt-base alloy (L-605), and an iron-base alloy (A-286) were exposed in hydrogen at 0.1 MN/sq m (15 psi) at several temperatures in the range from 430 to 980 C for as long as 1000 hours. These alloys were embrittled to varying degrees by such exposures in hydrogen. Embrittlement was found to be: (1) sensitive to strain rate, (2) reversible, (3) caused by large concentrations of absorbed hydrogen, and (4) not associated with any detectable microstructural changes in the alloys. These observations are consistent with a mechanism of internal reversible hydrogen embrittlement.

  1. Superior creep strength of a nickel-based superalloy produced by selective laser melting

    Energy Technology Data Exchange (ETDEWEB)

    Pröbstle, M., E-mail: martin.proebstle@fau.de [Department of Materials Science & Engineering Institute I, Friedrich-Alexander-Universität Erlangen-Nürnberg, Martensstraße 5, D-91058 Erlangen (Germany); Neumeier, S.; Hopfenmüller, J.; Freund, L.P. [Department of Materials Science & Engineering Institute I, Friedrich-Alexander-Universität Erlangen-Nürnberg, Martensstraße 5, D-91058 Erlangen (Germany); Niendorf, T. [Institut für Werkstofftechnik (Materials Engineering), Universität Kassel, Mönchebergstr. 3, D-34125 Kassel (Germany); Schwarze, D. [SLM Solutions GmbH, Roggenhorster Straße 9c, D-23556 Lübeck (Germany); Göken, M. [Department of Materials Science & Engineering Institute I, Friedrich-Alexander-Universität Erlangen-Nürnberg, Martensstraße 5, D-91058 Erlangen (Germany)

    2016-09-30

    The creep properties of a polycrystalline nickel-based superalloy produced via selective laser melting were investigated in this study. All heat treatment conditions of the additively manufactured material show superior creep strength compared to conventional cast and wrought material. The process leads to a microstructure with fine subgrains. In comparison to conventional wrought material no Niobium rich δ phase is necessary to control the grain size and thus more Niobium is available for precipitation hardening and solid solution strengthening resulting in improved creep strength.

  2. Experimental Investigation of Principal Residual Stress and Fatigue Performance for Turned Nickel-Based Superalloy Inconel 718.

    Science.gov (United States)

    Hua, Yang; Liu, Zhanqiang

    2018-05-24

    Residual stresses of turned Inconel 718 surface along its axial and circumferential directions affect the fatigue performance of machined components. However, it has not been clear that the axial and circumferential directions are the principle residual stress direction. The direction of the maximum principal residual stress is crucial for the machined component service life. The present work aims to focuses on determining the direction and magnitude of principal residual stress and investigating its influence on fatigue performance of turned Inconel 718. The turning experimental results show that the principal residual stress magnitude is much higher than surface residual stress. In addition, both the principal residual stress and surface residual stress increase significantly as the feed rate increases. The fatigue test results show that the direction of the maximum principal residual stress increased by 7.4%, while the fatigue life decreased by 39.4%. The maximum principal residual stress magnitude diminished by 17.9%, whereas the fatigue life increased by 83.6%. The maximum principal residual stress has a preponderant influence on fatigue performance as compared to the surface residual stress. The maximum principal residual stress can be considered as a prime indicator for evaluation of the residual stress influence on fatigue performance of turned Inconel 718.

  3. Experimental Investigation of Principal Residual Stress and Fatigue Performance for Turned Nickel-Based Superalloy Inconel 718

    Directory of Open Access Journals (Sweden)

    Yang Hua

    2018-05-01

    Full Text Available Residual stresses of turned Inconel 718 surface along its axial and circumferential directions affect the fatigue performance of machined components. However, it has not been clear that the axial and circumferential directions are the principle residual stress direction. The direction of the maximum principal residual stress is crucial for the machined component service life. The present work aims to focuses on determining the direction and magnitude of principal residual stress and investigating its influence on fatigue performance of turned Inconel 718. The turning experimental results show that the principal residual stress magnitude is much higher than surface residual stress. In addition, both the principal residual stress and surface residual stress increase significantly as the feed rate increases. The fatigue test results show that the direction of the maximum principal residual stress increased by 7.4%, while the fatigue life decreased by 39.4%. The maximum principal residual stress magnitude diminished by 17.9%, whereas the fatigue life increased by 83.6%. The maximum principal residual stress has a preponderant influence on fatigue performance as compared to the surface residual stress. The maximum principal residual stress can be considered as a prime indicator for evaluation of the residual stress influence on fatigue performance of turned Inconel 718.

  4. ISOTHERMAL AND THERMOMECHANICAL FATIGUE OF A NICKEL-BASE SUPERALLOY

    Directory of Open Access Journals (Sweden)

    Carlos Carvalho Engler-Pinto Júnior

    2014-06-01

    Full Text Available Thermal gradients arising during transient regimes of start-up and shutdown operations produce a complex thermal and mechanical fatigue loading which limits the life of turbine blades and other engine components operating at high temperatures. More accurate and reliable assessment under non-isothermal fatigue becomes therefore mandatory. This paper investigates the nickel base superalloy CM 247LC-DS under isothermal low cycle fatigue (LCF and thermomechanical fatigue (TMF. Test temperatures range from 600°C to 1,000°C. The behavior of the alloy is strongly affected by the temperature variation, especially in the 800°C-1,000°C range. The Ramberg-Osgood equation fits very well the observed isothermal behavior for the whole temperature range. The simplified non-isothermal stress-strain model based on linear plasticity proposed to represent the thermo-mechanical fatigue behavior was able to reproduce the observed behavior for both in-phase and out-of-phase TMF cycling.

  5. A continuum approach to combined $\\gamma/\\gamma'$ evolution and dislocation plasticity in Nickel-based superalloys

    OpenAIRE

    Wu, Ronghai; Zaiser, Michael; Sandfeld, Stefan

    2017-01-01

    Creep in single crystal Nickel-based superalloys has been a topic of interest since decades, and nowadays simulations are more and more able to complement experiments. In these alloys, the $\\gamma/\\gamma'$ phase microstructure co-evolves with the system of dislocations under load, and understanding the mutual interactions is essential for understanding the resulting creep properties. Predictive modeling thus requires multiphysics frameworks capable of modeling and simulating both the phase an...

  6. Oxidation of Inconel 625 superalloy upon treatment with oxygen or hydrogen plasma at high temperature

    Science.gov (United States)

    Vesel, Alenka; Drenik, Aleksander; Elersic, Kristina; Mozetic, Miran; Kovac, Janez; Gyergyek, Tomaz; Stockel, Jan; Varju, Jozef; Panek, Radomir; Balat-Pichelin, Marianne

    2014-06-01

    Initial stages of Inconel 625 superalloy (Ni60Cr30Mo10Ni4Nb1) oxidation upon short treatment with gaseous plasma at different temperatures up to about 1600 K were studied. Samples were treated for different periods up to a minute by oxygen or hydrogen plasma created with a microwave discharge in the standing-wave mode at a pressure of 40 Pa and a power 500 W. Simultaneous heating of the samples was realized by focusing concentrated solar radiation from a 5 kW solar furnace directly onto the samples. The morphological changes upon treatment were monitored using scanning electron microscopy, compositional depth profiling was performed using Auger electron spectroscopy, while structural changes were determined by X-ray diffraction. The treatment in oxygen plasma caused formation of metal oxide clusters of three dimensional crystallites initially rich in nickel oxide with the increasing chromium oxide content as the temperature was increasing. At about 1100 K iron and niobium oxides prevailed on the surface causing a drop of the material emissivity at 5 μm. Simultaneously the NiCr2O4 compound started growing at the interface between the oxide film and bulk alloy and the compound persisted up to temperatures close to the Inconel melting point. Intensive migration of minority alloying elements such as Fe and Ti was observed at 1600 K forming mixed surface oxides of sub-micrometer dimensions. The treatment in hydrogen plasma with small admixture of water vapor did not cause much modification unless the temperature was close to the melting point. At such conditions aluminum segregated on the surface and formed well-defined Al2O3 crystals.

  7. Effect of Microstructure on Electrical Conductivity of Nickel-Base Superalloys

    Science.gov (United States)

    Nagarajan, Balasubramanian; Castagne, Sylvie; Annamalai, Swaminathan; Fan, Zheng; Chan, Wai Luen

    2017-08-01

    Eddy current spectroscopy is one of the promising non-destructive methods for residual stress evaluation along the depth of subsurface-treated nickel-base superalloys, but it is limited by its sensitivity to microstructure. This paper studies the influence of microstructure on the electrical conductivity of two nickel-base alloys, RR1000 and IN100. Different microstructures were attained using heat treatment cycles ranging from solution annealing to aging, with varying aging time and temperature. Eddy current conductivity was measured using conductivity probes of frequencies ranging between 1 and 5 MHz. Qualitative and quantitative characterization of the microstructure was performed using optical and scanning electron microscopes. For the heat treatment conditions between the solution annealing and the peak aging, the electrical conductivity of RR1000 increased by 6.5 pct, which is duly substantiated by the corresponding increase in hardness (12 pct) and the volume fraction of γ' precipitates (41 pct). A similar conductivity rise of 2.6 pct for IN100 is in agreement with the increased volume fraction of γ' precipitates (12.5 pct) despite an insignificant hardening between the heat treatment conditions. The observed results with RR1000 and IN100 highlight the sensitivity of electrical conductivity to the minor microstructure variations, especially the volume fraction of γ' precipitates, within the materials.

  8. MeCrAl coatings obtained by arc PVD and pack cementation processes on nickel base superalloys

    International Nuclear Information System (INIS)

    Swadzba, L.; Maciejny, A.; Formanek, B.; Mendala, B.

    1997-01-01

    The paper presents the results of researches on obtaining and structure of high temperature resistance coatings on superalloys. The coatings were deposited on nickel and nickel base superalloys in two stages. During the first stage, the NiCr and NiCrHf coatings were obtained by arc-PVD method. Basic technology, bias, arc current, rotation, parameters of deposition of NiCr and MeCrHf coatings were defined. The high efficiency of deposition of both single and two sources was observed. The targets were made by vacuum melting and machining. An influence of targets chemical composition on coating structure and chemical coatings composition was described. The second stage was made by pack cementation HTLA (high temperature low activity) on 1323 K chromoaluminizing process. These arc-PVD and diffusion (pack cementation) connected processes permitted to obtain MeCrAl and MeCrAlHf type of coatings. The morphology, structure and microchemical composition were characterized by scanning electron microscopy, X-ray microanalysis, energy dispersive X-ray spectroscopy and X-ray diffraction methods. (orig.)

  9. The Corrosion Behavior of Nickel and Inconel 600 in Sodium Hydroxide and Hydrochloric Acid Solution at 280 .deg. C

    International Nuclear Information System (INIS)

    Lee, Ihh Chong; Suk, Tae Won

    1980-01-01

    The corrosion behavior of nickel and Inconel 600 has been investigated by the weight change measurement method at pH ranges 3∼13 of the solution. The specimens were exposed to aqueous solutions in a static autoclave at 280 .deg. C for 210 hours. The pH of the solutions was adjusted by hydrochloric acid and sodium hydroxide and the dissolved oxygen concentration was fixed as 10 ppb by using pure nitrogen gas. Weight loss of Inconel 600 was much less than that of nickel over the tested pH ranges. At pH 9.5, nickel and Inconel 600 showed the minimum weight loss phenomenon and the values of weight loss were 1.5mg/dm 2 and 0.9mg/dm 2 , respectively. Microscopic examination showed that nickel surface was attacked uniformly, whereas Inconel 600 surface was not greatly

  10. Effects of cobalt on structure, microchemistry and properties of a wrought nickel-base superalloy

    Science.gov (United States)

    Jarrett, R. N.; Tien, J. K.

    1982-01-01

    The effect of cobalt on the basic mechanical properties and microstructure of wrought nickel-base superalloys has been investigated experimentally by systematically replacing cobalt by nickel in Udimet 700 (17 wt% Co) commonly used in gas turbine (jet engine) applications. It is shown that the room temperature tensile yield strength and tensile strength only slightly decrease in fine-grained (disk) alloys and are basically unaffected in coarse-grained (blading) alloys as cobalt is removed. Creep and stress rupture resistances at 760 C are found to be unaffected by cobalt level in the blading alloys and decrease sharply only when the cobalt level is reduced below 8 vol% in the disk alloys. The effect of cobalt is explained in terms of gamma prime strengthening kinetics.

  11. Tensile behavior of nickel-base single-crystal superalloy DD6

    Energy Technology Data Exchange (ETDEWEB)

    Xiong, Xinhong, E-mail: xiongxh@whut.edu.cn [School of Logistics Engineering, Wuhan University of Technology, Wuhan 430063 (China); Quan, Dunmiao; Dai, Pengdan; Wang, Zhiping [School of Logistics Engineering, Wuhan University of Technology, Wuhan 430063 (China); Zhang, Qiaoxin [School of Mechanical and Electronic Engineering, Wuhan University of Technology, Wuhan 430070 (China); Yue, Zhufeng [School of Mechanics Civil Engineering and Architecture, Northwestern Polytechnical University, Xi' an 710072 (China)

    2015-06-11

    Tensile behavior of the nickel-base single-crystal superalloy DD6 was studied from room temperature to 1020 °C. The plate specimens were along [001] orientation parallel to the loading axis in tension. The microstructures on the surface and fracture morphology were investigated after tensile test to rupture by scanning electron microscopy (SEM). The results of the present investigation indicate that the yield strength at 650 °C is superior to that at room temperature, 850 °C and 1020 °C. Low ductility and serrated flow in stress–strain curves were also observed at 650 °C. The microstructures on the surface of the plate specimens and fracture morphology observation indicated that localized slip which resulted in glide plane decohesion caused the low ductility of DD6 alloy.

  12. Cobalt-free nickel-base superalloys

    International Nuclear Information System (INIS)

    Koizumi, Yutaka; Yamazaki, Michio; Harada, Hiroshi

    1979-01-01

    Cobalt-free nickel-base cast superalloys have been developed. Cobalt is considered to be a beneficial element to strengthen the alloys but should be eliminated in alloys to be used for direct cycle helium turbine driven by helium gas from HTGR (high temp. gas reactor). The elimination of cobalt is required to avoid the formation of radioactive 60 Co from the debris or scales of the alloys. Cobalt-free alloys are also desirable from another viewpoint, i.e. recently the shortage of the element has become a serious problem in industry. Cobalt-free Mar-M200 type alloys modified by the additions of 0.15 - 0.2 wt% B and 1 - 1.5 wt% Hf were found to have a creep rupture strength superior or comparable to that of the original Mar-M200 alloy bearing cobalt. The ductility in tensile test at 800 0 C, as cast or after prolonged heating at 900 0 C (the tensile test was done without removing the surface layer affected by the heating), was also improved by the additions of 0.15 - 0.2% B and 1 - 1.5% Hf. The morphology of grain boundaries became intricated by the additions of 0.15 - 0.2% B and 1 - 1.5% Hf, to such a degree that one can hardly distinguish grain boundaries by microscopes. The change in the grain boundary morphology was considered, as suggested previously by one of the authors (M.Y.), to be the reason for the improvements in the creep rupture strength and tensile ductility. (author)

  13. Inhomogeneous dislocation structure in fatigued INCONEL 713 LC superalloy at room and elevated temperatures

    International Nuclear Information System (INIS)

    Petrenec, Martin; Obrtlik, Karel; Polak, Jaroslav

    2005-01-01

    The dislocations arrangement was studied using transmission electron microscopy in specimens of polycrystalline INCONEL 713 LC superalloy cyclically strained up to failure with constant total strain amplitudes at temperatures 300, 773, 973 and 1073 K. Planar dislocation arrangements in the form of bands parallel to the {1 1 1} planes were observed in specimens cycled at all the temperatures. The bands showed up as thin slabs of high dislocation density cutting both the γ channels and γ' precipitates. Ladder-like bands were observed at room temperature

  14. Ultrasonic Sensor Signals and Optimum Path Forest Classifier for the Microstructural Characterization of Thermally-Aged Inconel 625 Alloy

    Directory of Open Access Journals (Sweden)

    Victor Hugo C. de Albuquerque

    2015-05-01

    Full Text Available Secondary phases, such as laves and carbides, are formed during the final solidification stages of nickel-based superalloy coatings deposited during the gas tungsten arc welding cold wire process. However, when aged at high temperatures, other phases can precipitate in the microstructure, like the γ'' and δ phases. This work presents an evaluation of the powerful optimum path forest (OPF classifier configured with six distance functions to classify background echo and backscattered ultrasonic signals from samples of the inconel 625 superalloy thermally aged at 650 and 950 \\(^\\circ\\C for 10, 100 and 200 h. The background echo and backscattered ultrasonic signals were acquired using transducers with frequencies of 4 and 5 MHz. The potentiality of ultrasonic sensor signals combined with the OPF to characterize the microstructures of an inconel 625 thermally aged and in the as-welded condition were confirmed by the results. The experimental results revealed that the OPF classifier is sufficiently fast (classification total time of 0.316 ms and accurate (accuracy of 88.75% and harmonic mean of 89.52 for the application proposed.

  15. Ultrasonic sensor signals and optimum path forest classifier for the microstructural characterization of thermally-aged inconel 625 alloy.

    Science.gov (United States)

    de Albuquerque, Victor Hugo C; Barbosa, Cleisson V; Silva, Cleiton C; Moura, Elineudo P; Filho, Pedro P Rebouças; Papa, João P; Tavares, João Manuel R S

    2015-05-27

    Secondary phases, such as laves and carbides, are formed during the final solidification stages of nickel-based superalloy coatings deposited during the gas tungsten arc welding cold wire process. However, when aged at high temperatures, other phases can precipitate in the microstructure, like the γ'' and δ phases. This work presents an evaluation of the powerful optimum path forest (OPF) classifier configured with six distance functions to classify background echo and backscattered ultrasonic signals from samples of the inconel 625 superalloy thermally aged at 650 and 950 °C for 10, 100 and 200 h. The background echo and backscattered ultrasonic signals were acquired using transducers with frequencies of 4 and 5 MHz. The potentiality of ultrasonic sensor signals combined with the OPF to characterize the microstructures of an inconel 625 thermally aged and in the as-welded condition were confirmed by the results. The experimental results revealed that the OPF classifier is sufficiently fast (classification total time of 0.316 ms) and accurate (accuracy of 88.75%" and harmonic mean of 89.52) for the application proposed.

  16. Effect of Crystal Orientation on Fatigue Failure of Single Crystal Nickel Base Turbine Blade Superalloys

    Science.gov (United States)

    Arakere, Nagaraj K.; Swanson, Gregory R.

    2000-01-01

    High Cycle Fatigue (HCF) induced failures in aircraft gas-turbine engines is a pervasive problem affecting a wide range of components and materials. HCF is currently the primary cause of component failures in gas turbine aircraft engines. Turbine blades in high performance aircraft and rocket engines are increasingly being made of single crystal nickel superalloys. Single-crystal Nickel-base superalloys were developed to provide superior creep, stress rupture, melt resistance and thermomechanical fatigue capabilities over polycrystalline alloys previously used in the production of turbine blades and vanes. Currently the most widely used single crystal turbine blade superalloys are PWA 1480/1493 and PWA 1484. These alloys play an important role in commercial, military and space propulsion systems. PWA1493, identical to PWA1480, but with tighter chemical constituent control, is used in the NASA SSME (Space Shuttle Main Engine) alternate turbopump, a liquid hydrogen fueled rocket engine. Objectives for this paper are motivated by the need for developing failure criteria and fatigue life evaluation procedures for high temperature single crystal components, using available fatigue data and finite element modeling of turbine blades. Using the FE (finite element) stress analysis results and the fatigue life relations developed, the effect of variation of primary and secondary crystal orientations on life is determined, at critical blade locations. The most advantageous crystal orientation for a given blade design is determined. Results presented demonstrates that control of secondary and primary crystallographic orientation has the potential to optimize blade design by increasing its resistance to fatigue crack growth without adding additional weight or cost.

  17. CYCLIC STRAIN LOCALIZATION IN CAST NICKEL BASED SUPERALLOY INCONEL 792-5A AT ROOM TEMPERATURE

    Czech Academy of Sciences Publication Activity Database

    Petrenec, Martin; Man, Jiří; Obrtlík, Karel; Polák, Jaroslav

    308/2005, č. 86 (2005), s. 269-274 ISSN 1429-6055. [Metody oceny struktury oraz wlasności materialów i wyrobów. Ustroń-Jaszowiec, 07.12.2005-09.12.2005] Institutional research plan: CEZ:AV0Z20410507 Keywords : low cycle fatigue * superalloy * cyclic strain localization Subject RIV: JL - Materials Fatigue, Friction Mechanics

  18. Cyclic plastic response of nickel-based superalloy at room and at elevated temperatures

    International Nuclear Information System (INIS)

    Polak, Jaroslav; Petrenec, Martin; Chlupova, Alice; Tobias, Jiri; Petras, Roman

    2015-01-01

    Nickel-based cast IN 738LC superalloy has been cycled at increasing strain amplitudes at room temperature and at 800 C. Hysteresis loops were analyzed using general statistical theory of the hysteresis loop. Dislocation structures of specimens cycled at these two temperatures were studied. They revealed localization of the cyclic plastic strain in the thin bands which are rich in dislocations. The analysis of the loop shapes yields effective stresses of the matrix and of the precipitates and the probability density function of the critical internal stresses at both temperatures. It allows to find the sources of the high cyclic stress.

  19. A novel unified dislocation density-based model for hot deformation behavior of a nickel-based superalloy under dynamic recrystallization conditions

    International Nuclear Information System (INIS)

    Lin, Y.C.; Wen, Dong-Xu; Chen, Xiao-Min; Chen, Ming-Song

    2016-01-01

    In this study, a novel unified dislocation density-based model is presented for characterizing hot deformation behaviors in a nickel-based superalloy under dynamic recrystallization (DRX) conditions. In the Kocks-Mecking model, a new softening item is proposed to represent the impacts of DRX behavior on dislocation density evolution. The grain size evolution and DRX kinetics are incorporated into the developed model. Material parameters of the developed model are calibrated by a derivative-free method of MATLAB software. Comparisons between experimental and predicted results confirm that the developed unified dislocation density-based model can nicely reproduce hot deformation behavior, DRX kinetics, and grain size evolution in wide scope of initial grain size, strain rate, and deformation temperature. Moreover, the developed unified dislocation density-based model is well employed to analyze the time-variant forming processes of the studied superalloy. (orig.)

  20. A novel unified dislocation density-based model for hot deformation behavior of a nickel-based superalloy under dynamic recrystallization conditions

    Energy Technology Data Exchange (ETDEWEB)

    Lin, Y.C. [Central South University, School of Mechanical and Electrical Engineering, Changsha (China); Light Alloy Research Institute of Central South University, Changsha (China); State Key Laboratory of High Performance Complex Manufacturing, Changsha (China); Wen, Dong-Xu; Chen, Xiao-Min [Central South University, School of Mechanical and Electrical Engineering, Changsha (China); Chen, Ming-Song [Central South University, School of Mechanical and Electrical Engineering, Changsha (China); State Key Laboratory of High Performance Complex Manufacturing, Changsha (China)

    2016-09-15

    In this study, a novel unified dislocation density-based model is presented for characterizing hot deformation behaviors in a nickel-based superalloy under dynamic recrystallization (DRX) conditions. In the Kocks-Mecking model, a new softening item is proposed to represent the impacts of DRX behavior on dislocation density evolution. The grain size evolution and DRX kinetics are incorporated into the developed model. Material parameters of the developed model are calibrated by a derivative-free method of MATLAB software. Comparisons between experimental and predicted results confirm that the developed unified dislocation density-based model can nicely reproduce hot deformation behavior, DRX kinetics, and grain size evolution in wide scope of initial grain size, strain rate, and deformation temperature. Moreover, the developed unified dislocation density-based model is well employed to analyze the time-variant forming processes of the studied superalloy. (orig.)

  1. Experimental study of micro-milling mechanism and surface quality of a nickel-based single crystal superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Gao, Qi; Gong, Yadong; Zhou, Yun Guang; Wen, Xue Long [School of Mechanical Engineering and Automation, Northeastern University, Shenyang (China)

    2017-01-15

    Micro-milling is widely used as a method for machining of micro-parts with high precision and efficiency. Taking the nickel-based single-crystal superalloy DD98 as the research object, the crystal characteristics of single-crystal materials were analysed, and the removal mechanism of single-crystal micro-milled parts was described. Based on molecular dynamics, a simulation model for nickel-based single-crystal superalloy DD98 micro-milling was established. Based on the response surface method of central composite design, the influences of spindle speed, feed rate, and milling depth on the surface roughness were examined, and a second-order regression model of the DD98 surface roughness was established. Using analysis of variance and the residuals of the model, a significant influence on surface roughness was found in the following order from large to small: Feed rate, spindle speed, and milling depth. Comparisons were conducted between the micro-milling experimental values and the predicted model values for different process parameters. The results show that the model fit is relatively high, and the adaptability is good. Scanning electron microscopy analysis of the micro-milling surfaces was performed to verify the slip and the removal mechanism of single-crystal materials. These results offer a theoretical reference and experimental basis for micro-milling of single-crystal materials.

  2. Oxidation of Inconel 625 superalloy upon treatment with oxygen or hydrogen plasma at high temperature

    Energy Technology Data Exchange (ETDEWEB)

    Vesel, Alenka; Drenik, Aleksander; Elersic, Kristina; Mozetic, Miran; Kovac, Janez [Jozef Stefan Institute, Jamova 39, SI-1000 Ljubljana (Slovenia); Gyergyek, Tomaz [University of Ljubljana, Faculty of Electrical Engineering, Trzaska 25, SI-1000 Ljubljana (Slovenia); Stockel, Jan; Varju, Jozef; Panek, Radomir [Institute of Plasma Physics, Academy of Sciences of the Czech Republic, Ze Slovankou 3, Praha 8 (Czech Republic); Balat-Pichelin, Marianne, E-mail: marianne.balat@promes.cnrs.fr [PROMES-CNRS Laboratory, 7 rue du four solaire, 66120 Font Romeu Odeillo (France)

    2014-06-01

    Initial stages of Inconel 625 superalloy (Ni{sub 60}Cr{sub 30}Mo{sub 10}Ni{sub 4}Nb{sub 1}) oxidation upon short treatment with gaseous plasma at different temperatures up to about 1600 K were studied. Samples were treated for different periods up to a minute by oxygen or hydrogen plasma created with a microwave discharge in the standing-wave mode at a pressure of 40 Pa and a power 500 W. Simultaneous heating of the samples was realized by focusing concentrated solar radiation from a 5 kW solar furnace directly onto the samples. The morphological changes upon treatment were monitored using scanning electron microscopy, compositional depth profiling was performed using Auger electron spectroscopy, while structural changes were determined by X-ray diffraction. The treatment in oxygen plasma caused formation of metal oxide clusters of three dimensional crystallites initially rich in nickel oxide with the increasing chromium oxide content as the temperature was increasing. At about 1100 K iron and niobium oxides prevailed on the surface causing a drop of the material emissivity at 5 μm. Simultaneously the NiCr{sub 2}O{sub 4} compound started growing at the interface between the oxide film and bulk alloy and the compound persisted up to temperatures close to the Inconel melting point. Intensive migration of minority alloying elements such as Fe and Ti was observed at 1600 K forming mixed surface oxides of sub-micrometer dimensions. The treatment in hydrogen plasma with small admixture of water vapor did not cause much modification unless the temperature was close to the melting point. At such conditions aluminum segregated on the surface and formed well-defined Al{sub 2}O{sub 3} crystals.

  3. Emission spectral analysis of nickel-base superalloys with fixed time intergration technique

    International Nuclear Information System (INIS)

    Okochi, Haruno; Takahashi, Katsuyuki; Suzuki, Shunichi; Sudo, Emiko

    1980-01-01

    Simultaneous determination of multielements (C, B, Mo, Ta, Co, Fe, Mn, Cr, Nb, Cu, Ti, Zr, and Al) in nickel-base superalloys (Ni: 68 -- 76%) was performed by emission spectral analysis. At first, samples which had various nickel contents (ni: 68 -- 76%) were prepared by using JAERI R9, nickel and other metals (Fe, Co, or Cr). It was confirmed that in the internal standard method (Ni II 227.73 nm), analytical values of all the elements examined decreased with a decrease of the integration time (ca. 3.9 -- 4.6 s), that is, an increase of the nickel content. On the other hand, according to the fixed time integration method, elements except for C, Mo, and Cr were not interfered within the range of nickel contents examined. A series of nickel-base binary alloys (Al, Si, Ti, Cr, Mn, Fe, Co, Nb, Mo, and W series) were prepared by high frequency induction melting and the centrifugal casting method and formulae for correcting interferences with near spectral lines were obtained. Various synthetic samples were prepared and analysed by this method. The equations of calibration curves were derived from the data for standard samples (JAERI R1 -- R6, NBS 1189, 1203 -- 1205, and B.S. 600B) by curve fitting with orthogonal polynomials using a computer. For the assessment of this method studied, the F-test was performed by comparison of variances of both analytical values of standard and synthetic samples. The surfaces of specimens were polished with a belt grinder using No. 80 of alumina or silicon carbide endless-paper. The preburn period and integration one were decided at 5 and 6 s respectively. A few standard samples which gave worse reproducibility in emission spectral analysis was investigated with an optical microscope and an electron probe X-ray microanalyser. (author)

  4. Heat affected zone liquation cracking in electron beam welded third generation nickel base superalloys

    International Nuclear Information System (INIS)

    Ojo, O.A.; Wang, Y.L.; Chaturvedi, M.C.

    2008-01-01

    The weldability of directionally solidified nickel base superalloy TMS-75 and TMS-75+C was investigated by autogenous bead-on-plate electron beam welding. The analysis of microsegregation that occurred during solidification of the as-cast alloys indicated that while W and Re segregated into the γ dendrites of both the alloys, Ta, Hf and C were rejected into the interdendritic liquid in the TMS-75+C. Heat affected zone intergranular liquation cracking was observed in both the materials and was observed to be closely associated with liquated γ-γ' eutectic microconstituent. The TMS-75+C alloy, however, exhibited a reduced extent of HAZ cracking compared to TMS-75. Suppression of terminal solidification reaction involving non-invariant γ-γ' eutectic transformation due to modification of primary solidification path by carbon addition is suggested to be an important factor contributing to reduced susceptibility of TMS-75+C alloy to HAZ liquation cracking relative to the TMS-75 superalloy

  5. Relationship of heat treatment-mechanical properties of nickel base superalloys.; Relacion tratamiento termico-propiedades mecanicas de una superaleacion base niquel.

    Energy Technology Data Exchange (ETDEWEB)

    Zamora R, L

    1997-12-01

    The nickel-base superalloys have high strength, excellent corrosion resistant, and good creep and fatigue resistance. These alloy improved properties at high temperature derive their mechanical and creep behavior on {gamma} precipitate morphology, and the evolution of such morphology during different heat treatment conditions. The main microstructural variable of Nickel-based superalloys, responsible for the mechanical properties are: (a) amount and morphology of precipitates; (b) size and shape of grains; and (c) carbide distribution. In this work, a Nickel-base superalloy Nimonic 80A, modified little with Zr prepared by melting and casting practices of materials electrolytic in vacuum-induction melting (VIM) type Balzers, to obtain five alloys different and ingots of 2 Kg and 1 Kg, with composition in weight % of Nimonic 80-A is: Ni = bal (76.66), C = 0.01, Cr = 19.83, Fe = 2.4, Mn = 0.17, Si 0.47, Al = 0.19, Zr = 0.4. The solidification process is made in a steel mold. After having realized four thermal treatments, the most representative microstructures there were obtained. The results from tensile tests performed on Instron Servohydraulic testing systems at uniaxial dynamic testing, at constant speeds to ,0.2 cm/min, were: the yield strength, the ultimate strength value, percentage elongation and area reduction. Creep tests were performed at in stress of 90 and 129 MPa, at a temperature of 600 and 680 Centigrades at different times and width of specimen of 1 mm. The alloys were analyzed by MEB(JEOL 35CF) at different magnifications. The nucleation and growth of intergranular cavities during creep of alloy Nimonic M3, were investigated. One sample was deformed in creep at 129 MPa and 680 Centigrades during 110 hs. Creep samples were annealing heat treated at 800 Centigrades, during 7 days. After a careful sample preparation procedure, 3100 of cavities were measured in the sample . The cavity size distributions in the sample were obtained. (Abstract Truncated)

  6. Erosion–corrosion behaviour of Ni-based superalloy Superni-75 in ...

    Indian Academy of Sciences (India)

    microscopy/energy-dispersive analysis (SEM/EDAX) and electron probe micro ... gas turbines and they have designated this alloy as superalloy Superni-75. ... The nickel-based superalloy Superni-75 (19·5Cr-3Fe-0·3Ti-0·1C- Balance Ni) was ...

  7. Effects of cutting parameters on machinability characteristics of Ni-based superalloys: a review

    Directory of Open Access Journals (Sweden)

    Kaya Eren

    2017-12-01

    Full Text Available Nickel based superalloys offer high strength, corrosion resistance, thermal stability and superb thermal fatigue properties. However, they have been one of the most difficult materials to machine due to these properties. Although we are witnessing improved machining strategies with the developing machining, tooling and inspection technologies, machining of nickel based superalloys is still a challenging task due to in-process strains and post process part quality demands.

  8. Control of microstructure and mechanical properties of laser solid formed Inconel 718 superalloy by electromagnetic stirring

    Science.gov (United States)

    Liu, Fencheng; Cheng, Hongmao; Yu, Xiaobin; Yang, Guang; Huang, Chunping; Lin, Xin; Chen, Jing

    2018-02-01

    The coarse columnar grains and special interface in laser solid formed (LSFed) Inconel 718 superalloy workpieces seriously affect their mechanical properties. To improve the microstructure and mechanical properties of LSFed Inconel 718 superalloy, electromagnetic stirring (EMS) was introduced to alter the solidification process of the molten pool during LSF. The results show that EMS could not completely eliminate the epitaxially growing columnar grains, however, the strong convection of liquid metals can effectively influence the solid-liquid interface growing mode. The segregation of alloying elements on the front of solid-liquid interface is inhibited and the degree of constitutional supercooling decreases correspondingly. Comparing the microstructures of samples formed under different process parameters, the size and amount of the γ+Laves eutectic phases formed in interdendritic area decrease along with the increasing magnetic field intensity, resulting in more uniformly distributed alloying elements. The residual stress distribution is proved to be more uniform, which is beneficial to the grain refinement after recrystallilzaiton. Mechanical properties testing results show an improvement of 100 MPa in tensile strength and 22% in elongation was obtained after EMS was used. The high cycle fatigue properties at room temperature was also improved from 4.09 × 104 cycles to 8.21 × 104 cycles for the as-deposited samples, and from 5.45 × 104 cycles to 12.73 × 104 cycles for the heat treated samples respectively.

  9. Characterization and Modeling of Microstructure Development in Nickel-base Superalloy Welds

    Energy Technology Data Exchange (ETDEWEB)

    Babu, S.S.; David, S.A.; Miller, M.K.; Vitek, J.M.

    1999-11-01

    Welding is important for economical reuse and reclamation of used and failed nickel-base superalloy blades, respectively [1]. Solidification and solid state decomposition of {gamma} (Face Centered Cubic, FCC) phase into {gamma}{prime} (L1{sub 2}-ordered) phase control the properties of these welds. In previous publications, the microstructure development in electron beam welds of PWA-1480 alloy [2] and laser beam welds of CMSX-4 alloy [3] were presented. These results showed that the weld cracking in these alloys were associated with low melting point eutectic at the dendrite boundaries [1,2]. The eutectic-{gamma}{prime} precipitation was reduced at rapid weld cooling rates and the partitioning between {gamma}-{gamma}{prime} phase was found to be far from equilibrium conditions [3,4]. This observation was related to diffusional growth of {gamma}{prime} precipitate into {gamma} phase. Subsequent to the above work, the precipitation characteristics of {gamma}{prime} phase from {gamma} phase were evaluated during continuous cooling conditions [5]. The results show that the number density of {gamma} precipitates increased with an increase in cooling rate. However, the details of this decomposition and also the fine-scale elemental partitioning characteristics between {gamma}-{gamma}{prime} were not investigated. In this paper, the precipitation characteristics of {gamma}{prime} from {gamma} during continuous cooling conditions were investigated with transmission electron microscopy, and atom probe field ion microscopy. In addition, thermodynamic and kinetic models were used to describe microstructure development in Ni-base superalloy welds.

  10. An assessment of microstructure, mechanical properties and corrosion resistance of dissimilar welds between Inconel 718 and 310S austenitic stainless steel

    International Nuclear Information System (INIS)

    Mortezaie, A.; Shamanian, M.

    2014-01-01

    In the present study, dissimilar welding between Inconel 718 nickel-base superalloy and 310S austenitic stainless steel using gas tungsten arc welding process was performed to determine the relationship between the microstructure of the welds and the resultant mechanical and corrosion properties. For this purpose, three filler metals including Inconel 625, Inconel 82 and 310 stainless steel were used. Microstructural observations showed that weld microstructures for all filler metals were fully austenitic. In tension tests, welds produced by Inconel 625 and 310 filler metals displayed the highest and the lowest ultimate tensile strength, respectively. The results of Charpy impact tests indicated that the maximum fracture energy was related to Inconel 82 weld metal. According to the potentiodynamic polarization test results, Inconel 82 exhibited the highest corrosion resistance among all tested filler metals. Finally, it was concluded that for the dissimilar welding between Inconel 718 and 310S, Inconel 82 filler metal offers the optimum properties at room temperature. - Highlights: • Three filler metals including Inconel 625, Inconel 82 and 310 SS were used. • A columnar to equiaxed dendritic structure was seen for IN-625 weld metal. • A granular austenitic microstructure obtained for Inconel 82 weld metal. • Microstructure of 310 weld metal includes solidification cracks along SSGB. • IN-82 weld metal showed the highest corrosion potential

  11. Homogenization Kinetics of a Nickel-based Superalloy Produced by Powder Bed Fusion Laser Sintering.

    Science.gov (United States)

    Zhang, Fan; Levine, Lyle E; Allen, Andrew J; Campbell, Carelyn E; Lass, Eric A; Cheruvathur, Sudha; Stoudt, Mark R; Williams, Maureen E; Idell, Yaakov

    2017-04-01

    Additively manufactured (AM) metal components often exhibit fine dendritic microstructures and elemental segregation due to the initial rapid solidification and subsequent melting and cooling during the build process, which without homogenization would adversely affect materials performance. In this letter, we report in situ observation of the homogenization kinetics of an AM nickel-based superalloy using synchrotron small angle X-ray scattering. The identified kinetic time scale is in good agreement with thermodynamic diffusion simulation predictions using microstructural dimensions acquired by ex situ scanning electron microscopy. These findings could serve as a recipe for predicting, observing, and validating homogenization treatments in AM materials.

  12. Inconel type resistive alloys based on ultrahigh purity nickel

    International Nuclear Information System (INIS)

    Matsarin, K.A.; Matsarin, S.K.

    2000-01-01

    The new nickel high-ohm alloys (ρ = 1.2-1.4 μOhm · m), containing the W, Al, Mo alloying elements in the quantity, not exceeding their solubility in a solid solution, are developed on the basis of the Inconel-type standard alloy. The optical composition of the alloy was determined by the results of the alloy was determined by the results of the electric resistance measurement and technological effectiveness indices (relative to the pressure and workable metal yield). The following optimal component concentrations were established: 14-17 %Cr; 10-12 %Fe; 0.5-1.0 %Cu; 1.0-1.5 %Mn; 0.1-0.2 %C; 0.4-0.6 %Si; 0.5-3.0 %W; 5-16 %Mo; 0.5-2.0 %Al; the remainder - Ni. The new alloys are recommended as materials for resistive elements of direct-glow cathode nodes of low capacity electron tubes [ru

  13. Improved creep strength of nickel-base superalloys by optimized γ/γ′ partitioning behavior of solid solution strengthening elements

    International Nuclear Information System (INIS)

    Pröbstle, M.; Neumeier, S.; Feldner, P.; Rettig, R.; Helmer, H.E.; Singer, R.F.; Göken, M.

    2016-01-01

    Solid solution strengthening of the γ matrix is one key factor for improving the creep strength of single crystal nickel-base superalloys at high temperatures. Therefore a strong partitioning of solid solution hardening elements to the matrix is beneficial for high temperature creep strength. Different Rhenium-free alloys which are derived from CMSX-4 are investigated. The alloys have been characterized regarding microstructure, phase compositions as well as creep strength. It is found that increasing the Titanium (Ti) as well as the Tungsten (W) content causes a stronger partitioning of the solid solution strengtheners, in particular W, to the γ phase. As a result the creep resistance is significantly improved. Based on these ideas, a Rhenium-free alloy with an optimized chemistry regarding the partitioning behavior of W is developed and validated in the present study. It shows comparable creep strength to the Rhenium containing second generation alloy CMSX-4 in the high temperature / low stress creep regime and is less prone to the formation of deleterious topologically close packed (TCP) phases. This more effective usage of solid solution strengtheners can enhance the creep properties of nickel-base superalloys while reducing the content of strategic elements like Rhenium.

  14. Synchrotron measurement of the 3D shape of X-ray reflections from the {gamma}/{gamma}{sup '}-microstructure of nickel-base superalloys

    Energy Technology Data Exchange (ETDEWEB)

    Epishin, Alexander; Link, Thomas; Ulbricht, Alexander; Bansal, Mamta [Technical Univ. of Berlin (Germany). Inst. of Material Science and Technology; Zizak, Ivo [Helmholtz-Zentrum Berlin for Materials and Energy BESSY II, Berlin (Germany)

    2011-12-15

    The 3D shape of X-ray reflections from the {gamma}/{gamma}{sup '}-microstructure of a nickel-base superalloy was investigated using synchrotron X-ray radiation and a position sensitive area detector. The measurements were performed on the 4{sup th} generation single-crystal nickel-base superalloy TMS138. The results show that X-ray reflections from non-cubic crystallographic planes have a complex 3D shape which changes during rafting. The 3D intensity distributions contain information about the spacing of the planes and their orientation as well. Whereas h00 reflections show the usual splitting into a {gamma}{sup '} and one {gamma}-subreflection, the hh0 and hhh reflections show two and three {gamma}-peaks respectively, resulting from the different types of {l_brace}100{r_brace} matrix channels. Therefore, these 3D diffraction measurements supply additional information about the spatial distribution of microstrains. (orig.)

  15. Repair of Precision Castings Made of the Inconel 713C Alloy

    Directory of Open Access Journals (Sweden)

    Łyczkowska K.

    2017-09-01

    Full Text Available Inconel 713C precision castings are used as aircraft engine components exposed to high temperatures and the aggressive exhaust gas environment. Industrial experience has shown that precision-cast components of such complexity contain casting defects like microshrinkage, porosity, and cracks. This necessitates the development of repair technologies for castings of this type. This paper presents the results of metallographic examinations of melted areas and clad welds on the Inconel 713C nickel-based superalloy, made by TIG, plasma arc, and laser. The cladding process was carried out on model test plates in order to determine the technological and material-related problems connected with the weldability of Inconel 713C. The studies included analyses of the macro- and microstructure of the clad welds, the base materials, and the heat-affected zones. The results of the structural analyses of the clad welds indicate that Inconel 713C should be classified as a low-weldability material. In the clad welds made by laser, cracks were identified mainly in the heat-affected zone and at the melted zone interface, crystals were formed on partially-melted grains. Cracks of this type were not identified in the clad welds made using the plasma-arc method. It has been concluded that due to the possibility of manual cladding and the absence of welding imperfections, the technology having the greatest potential for application is plasma-arc cladding.

  16. Lattice misfit during ageing of a polycrystalline nickel-base superalloy

    International Nuclear Information System (INIS)

    Collins, D.M.; Yan, L.; Marquis, E.A.; Connor, L.D.; Ciardiello, J.J.; Evans, A.D.; Stone, H.J.

    2013-01-01

    The temporal evolution of the lattice parameters and lattice misfit of an advanced polycrystalline nickel-base superalloy have been studied in situ during an ageing heat treatment using synchrotron X-ray diffraction. During ageing, the γ and γ′ lattice parameters were both observed to decrease, a trend that cannot be attributed to a loss of coherency alone. Phase-extracted γ′ replicated this behaviour. Atom probe tomography was used to measure the compositional changes between the start and end of the ageing heat treatment. Using these data, a thermodynamic assessment was made using the software ThermoCalc of the structural change across the interface between γ and γ′. Subsequently, the unconstrained lattice parameters were estimated and were shown to be in good agreement with the X-ray diffraction measurements. Thus, the observed anomalous lattice misfit behaviour was concluded to be dominated by elemental exchange between the γ and γ′ phases during ageing

  17. A phenomenological creep model for nickel-base single crystal superalloys at intermediate temperatures

    Science.gov (United States)

    Gao, Siwen; Wollgramm, Philip; Eggeler, Gunther; Ma, Anxin; Schreuer, Jürgen; Hartmaier, Alexander

    2018-07-01

    For the purpose of good reproduction and prediction of creep deformation of nickel-base single crystal superalloys at intermediate temperatures, a phenomenological creep model is developed, which accounts for the typical γ/γ‧ microstructure and the individual thermally activated elementary deformation processes in different phases. The internal stresses from γ/γ‧ lattice mismatch and deformation heterogeneity are introduced through an efficient method. The strain hardening, the Orowan stress, the softening effect due to dislocation climb along γ/γ‧ interfaces and the formation of dislocation ribbons, and the Kear–Wilsdorf-lock effect as key factors in the main flow rules are formulated properly. By taking the cube slip in \\{100\\} slip systems and \\{111\\} twinning mechanisms into account, the creep behavior for [110] and [111] loading directions are well captured. Without specific interaction and evolution of dislocations, the simulations of this model achieve a good agreement with experimental creep results and reproduce temperature, stress and crystallographic orientation dependences. It can also be used as the constitutive relation at material points in finite element calculations with complex boundary conditions in various components of superalloys to predict creep behavior and local stress distributions.

  18. Investigation of grain competitive growth during directional solidification of single-crystal nickel-based superalloys

    Energy Technology Data Exchange (ETDEWEB)

    Zhao, Xinbao [National Energy R and D Center of Clean and High-Efficiency Fossil-Fired Power Generation Technology, Xi' an Thermal Power Research Institute Co. Ltd., Xi' an (China); Northwestern Polytechnical University, State Key Laboratory of Solidification Processing, Xi' an (China); Liu, Lin; Zhang, Jun [Northwestern Polytechnical University, State Key Laboratory of Solidification Processing, Xi' an (China)

    2015-08-15

    Grain competitive growth of nickel-based single-crystal superalloys during directional solidification was investigated. A detailed characterization of bi-crystals' competitive growth was performed to explore the competitive grain evolution. It was found that high withdrawal rate improved the efficiency of grain competitive growth. The overgrowth rate was increased when the misorientation increased. Four patterns of grain competitive growth with differently oriented dispositions were characterized. The results indicated that the positive branching of the dendrites played a significant role in the competitive growth process. The effect of crystal orientation and heat flow on the competitive growth can be attributed to the blocking mechanism between the adjacent grains. (orig.)

  19. Predicting the morphologies of {\\gamma}' precipitates in cobalt-based superalloys

    OpenAIRE

    Jokisaari, Andrea M.; Naghavi, Shahab S.; Wolverton, Chris; Voorhees, Peter W.; Heinonen, Olle G.

    2017-01-01

    Cobalt-based alloys with {\\gamma}/{\\gamma}' microstructures have the potential to become the next generation of superalloys, but alloy compositions and processing steps must be optimized to improve coarsening, creep, and rafting behavior. While these behaviors are different than in nickel-based superalloys, alloy development can be accelerated by understanding the thermodynamic factors influencing microstructure evolution. In this work, we develop a phase field model informed by first-princip...

  20. A model for life predictions of nickel-base superalloys in high-temperature low cycle fatigue

    Science.gov (United States)

    Romanoski, Glenn R.; Pelloux, Regis M.; Antolovich, Stephen D.

    1988-01-01

    Extensive characterization of low-cycle fatigue damage mechanisms was performed on polycrystalline Rene 80 and IN100 tested in the temperature range from 871 to 1000 C. Low-cycle fatigue life was found to be dominated by propagation of microcracks to a critical size governed by the maximum tensile stress. A model was developed which incorporates a threshold stress for crack extension, a stress-based crack growth expression, and a failure criterion. The mathematical equivalence between this mechanistically based model and the strain-life low-cycle fatigue law was demonstrated using cyclic stress-strain relationships. The model was shown to correlate the high-temperature low-cycle fatigue data of the different nickel-base superalloys considered in this study.

  1. Non-isothermal irradiation creep of nickel alloys Inconel 706 and PE-16

    International Nuclear Information System (INIS)

    Gilbert, E.R.; Chin, B.A.

    1984-06-01

    The results of in-reactor step temperature change experiments conducted on two nickel alloys, PE-16 and Inconel 706, were evaluated to determine the creep behavior under nonisothermal conditions. The effect of the temperature changes was found to be significantly different for the two alloys. Following a step temperature change, the creep rate of PE-16 adjusted to the rate found in isothermal tests at the new temperature. In contrast for Inconel 706, a reduction in temperature from 540 to 425 0 C produced a 300% increase in creep above that measured at 540 0 C in isothermal tests. The response of in-reactor creep in Inconel 706 to temperature changes was attributed to the dissolution of the gamma double-prime phase and subsequent loss of precipitation-strengthening at temperatures below 500 C

  2. Environmental aspects on LCF-life of Ni-base superalloys during long term operation; Miljoeinverkan paa LCF-egenskaper vid laanga drifttider hos superlegeringar

    Energy Technology Data Exchange (ETDEWEB)

    Moverare, Johan; Leijon, Gunnar; Palmert, Frans

    2012-02-15

    The applicability of fine grain polycrystalline nickel base superalloys in gas or steam turbine applications is often limited by their susceptibility to fast intergranular cracking during fatigue in combination with extended hold times at high temperatures and high tensile stresses. This effect is further enhanced in corrosive environments even at moderate temperatures such as 400-600 deg In this study the negative effect of SO{sub 2} + water vapour on the low cycle fatigue resistance of three different nickel based superalloys (Nimonic 901, Inconel 718 and 718 plus) has been studied at 450 deg and 550 deg. A negative effect was found on both the crack initiation and crack propagation process. The effect increases with increasing temperature and is likely to be influenced by both the chemical composition and the grain size of the material. The negative effect of water vapour + SO{sub 2} is manifested by a decreased resistance to cyclic plastic deformation and a transition from transcrystalline to intercrystalline fracture behaviour. In Nimonic 901 this negative effect increases with the degree of plastic deformation. For lower mechanical strain amplitudes where the number of cycles and the total exposure time is increased the environmental impact is reduced. Similar trends can also be noticed for the other alloys. The surface corrosion in air and in SO{sub 2} + water vapour are found to be rather similar in this study and it is therefore concluded that the surface scale can remain adherent and protective if the strains on the oxide scale are low. However, for LCF tests with higher strain ranges, the oxide scale will rupture preferably at the grain boundaries and intergranular microcracks will initiate which promotes inward diffusion of embritteling elements such as oxygen and sulphur. Inconel 718 seems to be more sensitive to SO{sub 2} + water vapour than Nimonic 901 when tested at 450. The overall resistance to LCF is however still higher in Inconel 718 for the

  3. Creep properties of heat-resistant superalloys for nuclear plants in helium

    International Nuclear Information System (INIS)

    Shimizu, Shigeki; Satoh, Keisuke; Honda, Yoshio; Matsuda, Shozo; Murase, Hirokazu

    1979-01-01

    Creep properties of candidate superalloys for VHTR components in a helium environment at both temperatures of 800 0 C and 900 0 C were compared with those of the same alloys in the atmospheric condition, and the superalloys were contrasted with each other from the viewpoint of high temperature structural design. At 800 0 C, no significant effect of a helium environment on creep properties of the superalloys is observed. At 900 0 C, however, creep strength of Inconel 617, Incoloy 800 and Incoloy 807 in the helium environment decrease more than in the atmospheric environment. In Hastelloy X and Inconel 625, there is no significant difference between creep strengths in helium and those in the atmospheric condition. Concerning So and St values in helium at 900 0 C, Inconel 617 and Hastelloy X are clearly superior to other superalloys. (author)

  4. Recent Advances in Creep Modelling of the Nickel Base Superalloy, Alloy 720Li.

    Science.gov (United States)

    Harrison, William; Whittaker, Mark; Williams, Steve

    2013-03-20

    Recent work in the creep field has indicated that the traditional methodologies involving power law equations are not sufficient to describe wide ranging creep behaviour. More recent approaches such as the Wilshire equations however, have shown promise in a wide range of materials, particularly in extrapolation of short term results to long term predictions. In the aerospace industry however, long term creep behaviour is not critical and more focus is required on the prediction of times to specific creep strains. The current paper illustrates the capability of the Wilshire equations to recreate full creep curves in a modern nickel superalloy. Furthermore, a finite-element model based on this method has been shown to accurately predict stress relaxation behaviour allowing more accurate component lifing.

  5. Ductile Fracture Behaviour of Hot Isostatically Pressed Inconel 690 Superalloy

    Science.gov (United States)

    Cooper, A. J.; Brayshaw, W. J.; Sherry, A. H.

    2018-04-01

    Herein we assess the differences in Charpy impact behavior between Hot Isostatically Pressed and forged Inconel 690 alloy over the temperature range of 300 °C to - 196 °C. The impact toughness of forged 690 exhibited a relatively small temperature dependence, with a maximum difference of ca. 40 J measured between 300 °C and - 196 °C, whereas the HIP'd alloy exhibited a difference of approximately double that of the forged alloy over the same temperature range. We have conducted Charpy impact testing, tensile testing, and metallographic analyses on the as-received materials as well as fractography of the failed Charpy specimens in order to understand the mechanisms that cause the observed differences in material fracture properties. The work supports a recent series of studies which assess differences in fundamental fracture behavior between Hot Isostatically Pressed and forged austenitic stainless steel materials of equivalent grades, and the results obtained in this study are compared to those of the previous stainless steel investigations to paint a more general picture of the comparisons between HIP vs forged material fracture behavior. Inconel 690 was selected in this study since previous studies were unable to completely omit the effects of strain-induced martensitic transformation at the tip of the Chary V-notch from the fracture mechanism; Inconel 690 is unable to undergo strain-induced martensitic transformation due to the alloy's high nickel content, thereby providing a sister study with the omission of any martensitic transformation effects on ductile fracture behavior.

  6. Phase-field modelling of as-cast microstructure evolution in nickel-based superalloys

    International Nuclear Information System (INIS)

    Warnken, N.; Ma, D.; Drevermann, A.; Reed, R.C.; Fries, S.G.; Steinbach, I.

    2009-01-01

    A modelling approach is presented for the prediction of microstructure evolution during directional solidification of nickel-based superalloys. A phase-field model is coupled to CALPHAD thermodynamic and kinetic (diffusion) databases, so that a multicomponent alloy representative of those used in industrial practice can be handled. Dendritic growth and the formation of interdendritic phases in an isothermal (2-D) cross-section are simulated for a range of solidification parameters. The sensitivity of the model to changes in the solidification input parameters is investigated. It is demonstrated that the predicted patterns of microsegregation obtained from the simulations compare well to the experimental ones; moreover, an experimentally observed change in the solidification sequence is correctly predicted. The extension of the model to 3-D simulations is demonstrated. Simulations of the homogenization of the as-cast structure during heat treatment are presented.

  7. Phase-field modelling of as-cast microstructure evolution in nickel-based superalloys

    Energy Technology Data Exchange (ETDEWEB)

    Warnken, N., E-mail: n.warnken@bham.ac.uk [University of Birmingham, Department of Metallurgy and Materials, Edgbaston, Birmingham B15 2TT (United Kingdom); Ma, D. [Foundry Institute of the RWTH-Aachen, Intzestr. 5, 52072 Aachen (Germany); Drevermann, A. [ACCESS e.V., Intzestr. 5, 52072 Aachen (Germany); Reed, R.C. [University of Birmingham, Department of Metallurgy and Materials, Edgbaston, Birmingham B15 2TT (United Kingdom); Fries, S.G. [SGF Consultancy, 52064 Aachen (Germany)] [ICAMS, Ruhr University Bochum, Stiepeler Strasse 129, D-44780 Bochum (Germany); Steinbach, I. [ICAMS, Ruhr University Bochum, Stiepeler Strasse 129, D-44780 Bochum (Germany)

    2009-11-15

    A modelling approach is presented for the prediction of microstructure evolution during directional solidification of nickel-based superalloys. A phase-field model is coupled to CALPHAD thermodynamic and kinetic (diffusion) databases, so that a multicomponent alloy representative of those used in industrial practice can be handled. Dendritic growth and the formation of interdendritic phases in an isothermal (2-D) cross-section are simulated for a range of solidification parameters. The sensitivity of the model to changes in the solidification input parameters is investigated. It is demonstrated that the predicted patterns of microsegregation obtained from the simulations compare well to the experimental ones; moreover, an experimentally observed change in the solidification sequence is correctly predicted. The extension of the model to 3-D simulations is demonstrated. Simulations of the homogenization of the as-cast structure during heat treatment are presented.

  8. Additive Manufacturing of Nickel-Base Superalloy IN100 Through Scanning Laser Epitaxy

    Science.gov (United States)

    Basak, Amrita; Das, Suman

    2018-01-01

    Scanning laser epitaxy (SLE) is a laser powder bed fusion (LPBF)-based additive manufacturing process that uses a high-power laser to consolidate metal powders facilitating the fabrication of three-dimensional objects. In the present study, SLE is used to produce samples of IN100, a high-γ' non-weldable nickel-base superalloy on similar chemistry substrates. A thorough analysis is performed using various advanced material characterization techniques such as high-resolution optical microscopy, scanning electron microscopy, energy dispersive x-ray spectroscopy, and Vickers microhardness measurements to characterize and compare the quality of the SLE-fabricated IN100 deposits with the investment cast IN100 substrates. The results show that the IN100 deposits have a finer γ/γ' microstructure, weaker elemental segregation, and higher microhardness compared with the substrate. Through this study, it is demonstrated that the SLE process has tremendous potential in the repair and manufacture of gas turbine hot-section components.

  9. Influence of the alloy composition on the oxidation and internal-nitridation behaviour of nickel-base superalloys

    International Nuclear Information System (INIS)

    Krupp, U.; Christ, H.-J.

    1999-01-01

    Internal nitridation of nickel-base superalloys takes place as a consequence of the failure of protecting oxide scales (Al 2 O 3 and Cr 2 O 3 , respectively) and leads to a deterioration of the material properties due to near-surface embrittlement caused by the nitrides precipitated (TiN and AlN, respectively) and due to near-surface dissolution of the γ' phase. By using thermogravimetric methods in a temperature range between 800 C and 1100 C supplemented by microstructural examinations, the failure potential due to internal nitridation could be documented. A quantification was carried out by extending the experimental program to thermogravimetric studies in a nearly oxygen-free nitrogen atmosphere which was also applied to various model alloys of the system Ni-Cr-Al-Ti. It could be shown that the nitrogen diffusivity and solubility in nickel-base alloys is influenced particularly by the chromium concentration. An increasing chromium content leads to an enhanced internal-nitridation attack. (orig.)

  10. Effect of tensile holds on the deformation behaviour of a nickel base superalloy subjected to low cycle fatigue

    Energy Technology Data Exchange (ETDEWEB)

    Zrnik, J.; Semenak, J.; Wangyao, P.; Vrchovinsky, V.; Hornak, P. [Dept. of Materials Science, Technical Univ. of Kosice, Kosice (Slovakia)

    2002-07-01

    The deformation behaviour of the wrought nickel base superalloy EI698 VD has been investigated in conditions of low cycle fatigue. The tensile hold periods, imposing a constant stress into the fatigue loading, have been introduced at the maximum stress value. The individual hold periods were in the range of 1 minute to 10 hours. The fatigue tests were of tension-tension type defined by a stress ratio R = 0.027 and were conducted at temperature of 650 C. The tests were performed until fracture. The time to failure, the time to failure corresponding to total load at peak amplitude and the number of cycles to failure have been criteria to evaluate the deformation behaviour of the alloy subjected to complex cyclic creep loading. In order to predict lifetime of alloy, regarding the respective types cyclic test, the Kitagawa's modified the linear cumulative damage criterion has been considered. The two regression functions for applied hold period interval were proposed time to calculate the time to failure. The formulae can be used to predict the life of nickel base superalloy considering the specific conditions of low cycle fatigue with tensile hold period introduced at stress amplitude peaks. The failure analysis of fracture surfaces contributed to evaluation of the role of repeatedly reduced stress in damage process. (orig.)

  11. Friction Freeform Fabrication of Superalloy Inconel 718: Prospects and Problems

    Science.gov (United States)

    Dilip, J. J. S.; Janaki Ram, G. D.

    2014-01-01

    Friction Freeform Fabrication is a new solid-state additive manufacturing process. The present investigation reports a detailed study on the prospects of this process for additive part fabrication in superalloy Inconel 718. Using a rotary friction welding machine and employing alloy 718 consumable rods in solution treated condition, cylindrical-shaped multi-layer friction deposits (10 mm diameter) were successfully produced. In the as-deposited condition, the deposits showed very fine grain size with no grain boundary δ phase. The deposits responded well to direct aging and showed satisfactory room-temperature tensile properties. However, their stress rupture performance was unsatisfactory because of their layered microstructure with very fine grain size and no grain boundary δ phase. The problem was overcome by heat treating the deposits first at 1353 K (1080 °C) (for increasing the grain size) and then at 1223 K (950 °C) (for precipitating the δ phase). Overall, the current study shows that Friction Freeform Fabrication is a very useful process for additive part fabrication in alloy 718.

  12. Comparison the machinability of Inconel 718, Inconel 625 and Monel 400 in hot turning operation

    Directory of Open Access Journals (Sweden)

    Asit Kumar Parida

    2018-06-01

    Full Text Available In the present paper, three nickel base alloys (Inconel 718, Inconel 625 and Monel-400 have been studied for chip formation in the hot turning process using flame heating. Cutting force, tool life, chip morphology, tool wear, and surface integrity (surface roughness and microhardness beneath the machined surface have been determined in both room and hot temperature conditions (300 °C and 600 °C. Flame heating (Liquefied petroleum gas and oxygen along with turning operation has been utilized for machining of three materials. It was observed that significant reduction of cutting force, tool wear, chatter formation, surface roughness and increase tool life, chip tool contact length, etc., for all three nickel base alloys in hot machining compared to room temperature machining. Keywords: Hot turning, Nickel base alloys, Machinability, Cutting forces, Tool wear

  13. Pore annihilation in a single-crystal nickel-base superalloy during hot isostatic pressing: Experiment and modelling

    International Nuclear Information System (INIS)

    Epishin, Alexander; Fedelich, Bernard; Link, Thomas; Feldmann, Titus; Svetlov, Igor L.

    2013-01-01

    Pore annihilation during hot isostatic pressing (HIP) was investigated in the single-crystal nickel-base superalloy CMSX-4 experimentally by interrupted HIP tests at 1288 °C/103 MPa. The kinetics of pore annihilation was determined by density measurement and quantitative metallography. Transmission electron microscopy of a HIPed specimen showed that the pores shrink via dislocation movement on octahedral glide planes. Theoretically pore closure under HIP condition was modelled by the finite element method using crystal plasticity and large strain theories. The modelling gives a similar kinetics of pore annihilation as observed experimentally, however somewhat higher annihilation rate

  14. Laser Cladding of Ultra-Thin Nickel-Based Superalloy Sheets

    Directory of Open Access Journals (Sweden)

    Tobias Gabriel

    2017-03-01

    Full Text Available Laser cladding is a well-established process to apply coatings on metals. However, on substrates considerably thinner than 1 mm it is only rarely described in the literature. In this work 200 µm thin sheets of nickel-based superalloy 718 are coated with a powder of a cobalt-based alloy, Co–28Cr–9W–1.5Si, by laser cladding. The process window is very narrow, therefore, a precisely controlled Yb fiber laser was used. To minimize the input of energy into the substrate, lines were deposited by setting single overlapping points. In a design of experiments (DoE study, the process parameters of laser power, laser spot area, step size, exposure time, and solidification time were varied and optimized by examining the clad width, weld penetration, and alloying depth. The microstructure of the samples was investigated by optical microscope (OM and scanning electron microscopy (SEM, combined with electron backscatter diffraction (EBSD and energy dispersive X-ray spectroscopy (EDX. Similarly to laser cladding of thicker substrates, the laser power shows the highest influence on the resulting clad. With a higher laser power, the clad width and alloying depth increase, and with a larger laser spot area the weld penetration decreases. If the process parameters are controlled precisely, laser cladding of such thin sheets is manageable.

  15. Laser Cladding of Ultra-Thin Nickel-Based Superalloy Sheets.

    Science.gov (United States)

    Gabriel, Tobias; Rommel, Daniel; Scherm, Florian; Gorywoda, Marek; Glatzel, Uwe

    2017-03-10

    Laser cladding is a well-established process to apply coatings on metals. However, on substrates considerably thinner than 1 mm it is only rarely described in the literature. In this work 200 µm thin sheets of nickel-based superalloy 718 are coated with a powder of a cobalt-based alloy, Co-28Cr-9W-1.5Si, by laser cladding. The process window is very narrow, therefore, a precisely controlled Yb fiber laser was used. To minimize the input of energy into the substrate, lines were deposited by setting single overlapping points. In a design of experiments (DoE) study, the process parameters of laser power, laser spot area, step size, exposure time, and solidification time were varied and optimized by examining the clad width, weld penetration, and alloying depth. The microstructure of the samples was investigated by optical microscope (OM) and scanning electron microscopy (SEM), combined with electron backscatter diffraction (EBSD) and energy dispersive X-ray spectroscopy (EDX). Similarly to laser cladding of thicker substrates, the laser power shows the highest influence on the resulting clad. With a higher laser power, the clad width and alloying depth increase, and with a larger laser spot area the weld penetration decreases. If the process parameters are controlled precisely, laser cladding of such thin sheets is manageable.

  16. Microstructure and properties of nickel base superalloy joints brazed with Ni-Cr-Co-B and BNi-1a filler metals

    Energy Technology Data Exchange (ETDEWEB)

    Zhuang, H. [Beijing Univ. of Aeronautics and Astronautics (China); Liu, W. [Dalian Railway Inst. (China). Welding Div.

    1995-12-31

    In this study, the kind and compositions of brittle phases formed in joints of a nickel-base superalloy brazed with the Ni-Cr-Co-B and BNi-1a (Ni-Cr-B-Si) filler metals were investigated. Their brittle-phase-free maximum brazing clearances (MBC) were characterized in dependence on the brazing conditions. The improvement on joint structures by post-braze heat treatment was also examined. (orig./MM)

  17. Erosion–corrosion behaviour of Ni-based superalloy Superni-75

    Indian Academy of Sciences (India)

    The super-heater and re-heater tubes of the boilers used in thermal power plants are ... mechanism, resulting in the tube wall thinning and premature failure. The nickel-based superalloys can be used as boiler tube materials to increase the ...

  18. On the Time-Temperature-Transformation Behavior of a New Dual-Superlattice Nickel-Based Superalloy

    Science.gov (United States)

    Mignanelli, P. M.; Jones, N. G.; Hardy, M. C.; Stone, H. J.

    2018-03-01

    Recent research has identified compositions of nickel-based superalloys with microstructures containing appreciable and comparable volume fractions of γ' and γ″ precipitates. In this work, an alloy capable of forming such a dual-superlattice microstructure was subjected to a range of thermal exposures between 873 K and 1173 K (600 °C and 900 °C) for durations of 1 to 1000 hours. The microstructures and nature of the precipitating phases were characterized using synchrotron X-ray diffraction and electron microscopy. These data have enabled the construction of a T-T-T diagram for the precipitating phases. Hardness measurements following each thermal exposure have identified the age-hardening behavior of this alloy and allowed preliminary mechanical properties to be assessed.

  19. Effect of solution heat treatment on the precipitation behavior and strengthening mechanisms of electron beam smelted Inconel 718 superalloy

    Energy Technology Data Exchange (ETDEWEB)

    You, Xiaogang [School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023 (China); Laboratory for New Energy Material Energetic Beam Metallurgical Equipment Engineering of Liaoning Province, Dalian 116024 (China); Tan, Yi, E-mail: tanyi@dlut.edu.cn [School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023 (China); Laboratory for New Energy Material Energetic Beam Metallurgical Equipment Engineering of Liaoning Province, Dalian 116024 (China); Shi, Shuang [School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023 (China); Laboratory for New Energy Material Energetic Beam Metallurgical Equipment Engineering of Liaoning Province, Dalian 116024 (China); Yang, Jenn-Ming [Department of Materials Science and Engineering, University of California, Los Angeles, CA 90095 (United States); Wang, Yinong [School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023 (China); Li, Jiayan; You, Qifan [School of Materials Science and Engineering, Dalian University of Technology, Dalian 116023 (China); Laboratory for New Energy Material Energetic Beam Metallurgical Equipment Engineering of Liaoning Province, Dalian 116024 (China)

    2017-03-24

    Inconel 718 superalloy was fabricated by electron beam smelting (EBS) technique. The effect of solution heat treatment on the precipitation behavior and mechanical properties of EBS 718 superalloys were studied, the strengthening mechanisms were analyzed and related to the mechanical properties. The results indicate that the optimized microstructures can be acquired by means of EBS, which is attributed to the rapid cooling rate of approximately 280 ℃/min. The solution heat treatment shows a great impact on the microstructures, precipitation behavior and mechanical properties of EBS 718 superalloy. The γ'' phase shows an apt to precipitate at relatively lower solution temperatures followed by aging, while the γ' precipitates are prone to precipitate at higher temperatures. When solution treated at 1150 ℃, the γ' precipitates are dispersively distributed in the matrix with size and volume fraction of 8.43 nm and 21.66%, respectively, a Vickers hardness of approximately 489 HV{sub 0.1} is observed for the aged superalloy. The precipitation strengthening effect of EBS 718 superalloy could be elucidated by considering the interaction between the dislocations and γ''/γ' precipitates. The shearing of γ' is resisted by the coherency strengthening and formation of antiphase boundary (APB), which shows equal effect as weakly coupled dislocation (WCD) model. And for γ'', the strengthening effect is much more prominent with the primary strengthening mechanism of ordering. Moreover, it is interestingly found that the strengthening mechanism of stacking fault (SF) shearing coexists with APB shearing, and SF shearing plays a major role in strengthening of EBS 718 superalloy.

  20. Thermo-Viscoplastic Behavior of Ni-Based Superalloy Haynes 282 and Its Application to Machining Simulation

    Directory of Open Access Journals (Sweden)

    Marcos Rodríguez-Millán

    2017-12-01

    Full Text Available Ni-based superalloys are extensively used in high-responsibility applications in components of aerospace engines and gas turbines with high temperature service lives. The wrought, γ’-strengthened superalloy Haynes 282 has been recently developed for applications similar to other common superalloys, such as Waspaloy or Inconel 718, with improved creep behavior, thermal stability, and fabrication ability. Despite the potential of Haynes 282, there are still important gaps in the knowledge of the mechanical behavior of this alloy. In fact, it was not possible to find information concerning the mechanical behavior of the alloy under impulsive loading. This paper focuses on the mechanical characterization of the Haynes 282 at strain rates ranging from 0.1 to 2800 s−1 and high temperatures ranging from 293 to 523 K using Hopkinson bar compression tests. The experimental results from the thermo-mechanical characterization allowed for calibration of the Johnson–Cook model widely used in modeling metallic alloy’s responses under dynamic loading. Moreover, the behavior of Haynes 282 was compared to that reported for Inconel 718, and the results were used to successfully model the orthogonal cutting of Haynes 282, being a typical case of dynamic loading requiring previous characterization of the alloy.

  1. Metallurgical joining of engine parts. Inertia welding of nickel superalloy HP compressor disks

    International Nuclear Information System (INIS)

    Ferte, J.P.

    1993-01-01

    The main part of this paper describes upside metallurgical and mechanical work done at SNECMA, on inertia welding of powder metallurgy nickel base superalloys ASTROLOY and N18, allowing appliance of this process to engine parts : Inertia welding of superalloys leads to deap microstructural changes in the H.A.Z. which have been, as well as upset, correlated to process parameters, weld geometry and base material microstructure; a full mechanical testing of welds shown properties equivalent to base material ones up to 650 C except for fatigue crack growth behavior under specific conditions (T>600 C-hold time at maximum load) which is drastically reduced for in weld plane propagation. A significant improvement of this later property has been done through post-welding heat treatment and optimization of welding parameters. Last part of this paper summarize the main teachings gained, on the complete welding procedure, from welding of scale one parts. (orig.)

  2. Investigating the Effect of Approach Angle and Nose Radius on Surface Quality of Inconel 718

    Science.gov (United States)

    Kumar, Sunil; Singh, Dilbag; Kalsi, Nirmal S.

    2017-11-01

    This experimental work presents a surface quality evaluation of a Nickel-Cr-Fe based Inconel 718 superalloy, which has many applications in the aero engine and turbine components. However, during machining, the early wear of tool leads to decrease in surface quality. The coating on cutting tool plays a significant role in increasing the wear resistance and life of the tool. In this work, the aim is to study the surface quality of Inconel 718 with TiAlN-coated carbide tools. Influence of various geometrical parameters (tool nose radius, approach angle) and machining variables (cutting velocity, feed rate) on the quality of machined surface (surface roughness) was determined by using central composite design (CCD) matrix. The mathematical model of the same was developed. Analysis of variance was used to find the significance of the parameters. Results showed that the tool nose radius and feed were the main active factors. The present experiment accomplished that TiAlN-coated carbide inserts result in better surface quality as compared with uncoated carbide inserts.

  3. Nickel-base superalloy powder metallurgy: state-of-the-art

    International Nuclear Information System (INIS)

    Allen, M.M.; Athey, R.L.; Moore, J.B.

    1975-01-01

    Development of powder metallurgical methods for fabrication of Ni-base superalloy turbine engine disks is reviewed. Background studies are summarized and current state-of-art is discussed for the F100 jet engine, advanced applications, and forging processes

  4. Advanced Scale Bridging Microstructure Analysis of Single Crystal Ni-Base Superalloys

    Czech Academy of Sciences Publication Activity Database

    Parsa, A. B.; Wollgramm, P.; Buck, H.; Somsen, C.; Kostka, A.; Povstugar, I.; Choi, P.-P.; Raabe, D.; Dlouhý, Antonín; Müller, J.; Spiecker, E.; Demtroder, K.; Schreuer, J.; Neuking, K.; Eggeler, G.

    2015-01-01

    Roč. 17, č. 2 (2015), s. 216-230 ISSN 1438-1656 Institutional support: RVO:68081723 Keywords : High temperature materials * Nickel based superalloys * EPMA * HRTEM Subject RIV: JG - Metallurgy Impact factor: 1.817, year: 2015

  5. Influence of cooling rate on the development of multiple generations of {gamma}' precipitates in a commercial nickel base superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Singh, A.R.P. [Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, TX (United States); Nag, S., E-mail: nag.soumya@gmail.com [Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, TX (United States); Hwang, J.Y. [Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, TX (United States); Viswanathan, G.B.; Tiley, J. [Materials and Manufacturing Directorate, Air Force Research Laboratory, Dayton, OH (United States); Srinivasan, R. [ExxonMobil Research and Engineering Company, Annandale, NJ (United States); Fraser, H.L. [Center for the Accelerated Maturation of Materials and Department of Materials Science and Engineering, The Ohio State University, Columbus, OH (United States); Banerjee, R. [Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, TX (United States)

    2011-09-15

    The compositional and microstructural evolution of different generations of {gamma}' precipitates during the continuous cooling of a commercial nickel base superalloy, Rene88DT, has been characterized by three dimensional atom probe tomography coupled with energy-filtered transmission electron microscopy studies. After solutionizing in the single {gamma} phase field, continuous cooling at a very high rate results in a monomodal size distribution of {gamma}' precipitates with a high nucleation density and non-equilibrium compositions. In contrast, a relatively slower cooling rate ({approx} 24 deg. C/min) results in a multi-modal size distribution of {gamma}' precipitates with the larger first generation primary precipitates exhibiting close to equilibrium composition, along with the smaller scale secondary {gamma}' precipitates, exhibiting non-equilibrium composition (excess of Co and Cr, depleted in Al and Ti). The composition of the {gamma} matrix near these precipitates also exhibits similar trends with the composition being closer to equilibrium near the primary precipitates as compared to the secondary precipitates. - Highlights: {yields} Effect of cooling rate on the precipitation of {gamma}' particles in commercial nickel base superalloy. {yields} Couples EFTEM and 3DAP studies to determine the composition and morphology of {gamma}' precipitates. {yields} Determination of near and far field compositional variations within the gamma matrix leading to subsequent precipitation.

  6. Fatigue crack growth behavior of a new single crystal nickel-based superalloy (CMSX-4) at 650 C

    International Nuclear Information System (INIS)

    Sengupta, A.; Putatunda, S.K.

    1994-01-01

    CMSX-4 is a recently developed rhenium containing single crystal nickel-based superalloy. This alloy has potential applications in many critical high-temperature applications such as turbine blades, rotors, nuclear reactors, etc. The fatigue crack growth rate and the fatigue threshold data of this material is extremely important for accurate life prediction, as well as failure safe design, at elevated temperatures. In this paper, the fatigue crack growth behavior of CMSX-4 has been studied at 650 C. The investigation also examined the influence of γ' precipitates (size and distribution) on the near-threshold fatigue crack growth rate and the fatigue threshold. The influence of load ratio on the fatigue crack growth rate and the fatigue threshold was also examined. Detailed fractographic studies were carried out to determine the crack growth mechanism in fatigue in the threshold region. Compact tension specimens were prepared from the single crystal nickel-based superalloy CMSX-4 with [001] orientation as the tensile loading axis direction. These specimens were given three different heat treatments to produce three different γ' precipitate sizes and distributions. Fatigue crack growth behavior of these specimens was studied at 650 C in air. The results of the present investigation indicate that the near-threshold fatigue crack growth rate decreases and that the fatigue threshold increases with an increase in the γ' precipitate size at 650 C. The fatigue threshold decreased linearly with an increase in load ratio. Fractographs at 650 C show a stage 2 type of crack growth along {100} type of crystal planes in the threshold region, and along {111} type of crystal planes in the high ΔK region

  7. ON THE INFLUENCE OF COLD WORK ON RESISTIVITY VARIATIONS WITH THERMAL EXPOSURE IN IN-718 NICKEL-BASE SUPERALLOY

    International Nuclear Information System (INIS)

    Madhi, Elhoucine; Nagy, Peter B.

    2010-01-01

    In nickel-base superalloys, irreversible electrical conductivity changes occur above a transition temperature where thermally-activated microstructural evolution initiates. The electrical conductivity first decreases above about 450 deg. C then increases above 600 deg. C. However, the presence of plastic deformation results in accelerated microstructure evolution at an earlier transition temperature. It was recently suggested that this well-known phenomenon might explain the notable conductivity difference between the peened near-surface part and the intact part at sufficiently large depth in surface-treated specimens. The influence of cold work on the electrical conductivity change with thermal exposure offers a probable answer to one of the main remaining questions in eddy current residual stress assessment, namely unusually fast and occasionally even non-monotonic decay of the apparent eddy current conductivity (AECC) change that was observed at temperatures as low as 400 deg. C. To validate this explanation, the present study investigates the influence of cold work on low-frequency Alternating Current Potential Drop (ACPD) resistivity variations with thermal exposure. In-situ resistivity monitoring was conducted throughout various heating cycles using the ACPD technique. IN-718 nickel-base superalloy specimens with different levels of cold work were exposed to gradually increasing peak temperatures from 400 deg. C to 800 deg. C. The results indicate that the initial irreversible rise in resistivity is approximately one order of magnitude higher and occurs at about 50 deg. C lower temperature in cold-worked samples of 30% plastic strain than in the intact material.

  8. Effect of heat-treatment on microstructure and high-temperature deformation behavior of a low rhenium-containing single crystal nickel-based superalloy

    International Nuclear Information System (INIS)

    Sun, Nairong; Zhang, Lanting; Li, Zhigang; Shan, Aidang

    2014-01-01

    A low rhenium-containing [001] oriented single crystal nickel-based superalloy with different γ′ morphologies induced by various aging treatments was compressed from room temperature to 1000 °C. All the single crystal samples with different γ′ morphologies exhibit anomalous yield behavior. The sample first aged at 1180 °C has the widest anomalous temperature domain and highest yield strengths. The sample first aged at 1000 °C has the highest anomalous peak stress temperature

  9. Sintering and microstructure evolution of columnar nickel-based superalloy sheets prepared by EB-PVD

    International Nuclear Information System (INIS)

    Chen, S.; Qu, S.J.; Liang, J.; Han, J.C.

    2010-01-01

    Research highlights: → EB-PVD technology is commonly used to deposit thermal barrier coatings (TBCs) and columnar structure is commonly seen in EB-PVD condensates. The unique columnar structure can provide outstanding resistance against thermal shock and mechanical strains for TBCs. However, a number of researchers have found that the columnar structure can affect the mechanical properties of EB-PVD alloy thin sheet significantly. As yet, works on how to reduce this kind of effects are seldom done. In the present article, we tried to reveal the sintering effects on microstructure evolution and mechanical properties of columnar Ni-based superalloy sheet. The results suggests that after sintering, the columnar structure degrades. Degradation depends on sintering temperature and time. Both the ultimate tensile strength and the elongation percentage are effectively improved after sintering. - Abstract: A ∼0.15 mm-thick columnar nickel-based superalloy sheet was obtained by electron beam physical vapor deposition (EB-PVD). The as-deposited alloy sheet was sintered at different conditions. The microstructure of the specimens before and after sintering was characterized by using scanning electron microscopy. An X'Pert texture facility was used to determine the crystallographic orientation of the as-deposited alloy sheet. The phase transformation was investigated by X-ray diffraction. Tensile tests were conducted at room temperature on as-deposited and sintered specimens. The results show that the as-deposited sheet is composed of typical columnar structures. After sintering, however, the columnar structure degrades. The degradation depends on sintering temperature and time. Both the ultimate tensile strength and the elongation percentage are effectively improved after sintering.

  10. Effect of temperature on the elastic-plastic fracture toughness behavior of Inconel X-750

    International Nuclear Information System (INIS)

    Mills, W.J.

    1977-09-01

    The elastic-plastic J/sub Ic/ fracture toughness response of precipitation heat treated Inconel X-750 has been evaluated by the multi-specimen resistance curve (R-curve) technique at room temperature, 800 0 F (427 0 C), and 1000 0 F (538 0 C). The value of J/sub Ic/ for this nickel-base superalloy was found to be relatively independent of temperature over the test temperature range. On the other hand, the slopes of the fracture toughness R-curves were steeper at 800 and 1000 0 F (427 and 538 0 C) than at 75 0 F (24 0 C), thereby indicating that the resistance to crack extension was considerably greater at elevated temperatures, Metallographic and electron fractographic examination of the Inconel X-750 fracture surfaces revealed that this slope change phenomenon was associated with an intergranular to transgranular fracture mechanism transition. Under room temperature conditions, crack extension occurred primarily by an intergranular dimple rupture mechanism attributed to microvoid coalescence along a grain boundary denuded region. In the 800 to 1000 0 F (427 to 538 0 C) regime, the fracture surface was dominated by a faceted transgranular morphology

  11. Application of laser ultrasonics to monitor microstructure evolution in Inconel 718 superalloy

    Directory of Open Access Journals (Sweden)

    Garcin Thomas

    2014-01-01

    Full Text Available Laser ultrasonics for metallurgy is an innovative sensor dedicated to the measurement of microstructure evolution during thermomechanical processing. In this technique, broadband ultrasound pulses are generated and detected with lasers. The properties of the ultrasounds are then related to the characteristics of the microstructure. Ultrasound attenuation is primary originated by the scattering at grain boundaries and its frequency dependence can be related to the grain size. The present work aims to introduce this technology as an exciting tool for metallurgists. As an illustration of its capability, the evolution of the grain size during isothermal annealing from a fine grained structure is in-situ monitored in an Inconel 718 superalloy. Laser ultrasonic measurements are compared with ex-situ metallography observations. Indication of heterogeneous grain growth is observed, correlated to the dissolution of δ-phase particles present in the initial structure. This preliminary study illustrates the potential of this new technique to monitor microstructure evolution in more complex scenarios including recrystallization during simulation of hot forging processes.

  12. Microstructural evolution of cold-sprayed Inconel 625 superalloy coatings on low alloy steel substrate

    International Nuclear Information System (INIS)

    Chaudhuri, Atanu; Raghupathy, Y.; Srinivasan, Dheepa; Suwas, Satyam; Srivastava, Chandan

    2017-01-01

    This study illustrates microstructural evolution of INCONEL 625 superalloy coatings cold-sprayed on a 4130 chrome alloy steel with medium carbon content. INCONEL 625 powder (5–25 μm) were successfully cold sprayed without any oxidation. The comprehensive microstructure analysis of the as-sprayed coatings and of the substrate-coating interface was carried out using EBSD, TEM, and XRD. The coating microstructure at the substrate-coating interface was markedly different from the microstructure away from the interface. The coating microstructure at steel-coating interface consisted of a fine layer of small grains. The microstructure beyond this fine layer can be divided into splats, inter splat and intra splat boundaries. Both splat and splat boundaries exhibited deformation induced dislocations. Dynamic recovery of dislocations-ridden regions inside the splat was responsible for the development of sub grain structure inside a splat with both low and high angle grain boundaries. Splat-splat (inter splat) boundary consisted of a relatively high density of dislocations and shear bands as a result of adiabatic shear flow localisation. This flow instability is believed to enhance the microstructural integrity by eliminating porosity at splat-splat boundaries. Based on the microstructural analysis using electron microscopy, a plausible mechanism for the development of microstructure has been proposed in this work. Cold spray technique can thus be deployed to develop high quality coatings of commercial importance. - Graphical abstract: Schematics of the evolution of microstructure at the 4130 steel substrate close to interface. i) initial deformation close to interface. ii) Accumulation of dislocation in the substrate. iii) Formation of cell structure due to dislocation tangling and arrangement. iv) Dislocation rearrangement and subgrain formation. v.a) Formation HAGB from dislocation accumulation into LAGB. v.b) HAGB formation through DRX by progressive lattice rotation

  13. Superalloy applications in the nuclear field

    International Nuclear Information System (INIS)

    Ramanathan, L.V.; Padilha, A.F.

    1984-01-01

    The process conditions in the areas of nuclear fuel processing, fabrication, utilization, reprocessing and disposal are severe, demanding therefore the use of materials with high temperature mechanical strength and corrosion resistance. A number of refractory metal containing superalloys have found application in the diferrent areas of the nuclear field. The main aspects of the microstructure, strengthening mechanisms and corrosion resistance of 3 superalloys, namely Incoloy 825, Inconel 718 and Hastelloy C have been discussed. The role of the refractory metal elements in influencing the mechanical strength and corrosion resistance of superalloys has been emphasised. (Author) [pt

  14. Forging Oxide-Dispersion-Strengthened Superalloys

    Science.gov (United States)

    Harf, F. H.; Glasgow, T. K.; Moracz, D. J.; Austin, C. M.

    1986-01-01

    Cladding of mild steel prevents surface cracking when alloy contacts die. Continual need for improvements in properties of alloys capable of withstanding elevated temperatures. Accomplished by using oxide-dispersion-strengthed superalloys such as Inconel Alloy MA 6000. Elevated tensile properties of forged alloy equal those of hot-rolled MA 6000 bar. Stress-rupture properties somewhat lower than those of bar stock but, at 1,100 degrees C, exceed those of strongest commercial single crystal, directionally solidified and conventionally cast superalloys.

  15. The effects of thermomechanical history on the microstructure of a nickel-base superalloy during forging

    Energy Technology Data Exchange (ETDEWEB)

    Gardner, S., E-mail: 485354@swansea.ac.uk [College of Engineering, Bay Campus, Swansea University, Swansea SA1 8EN (United Kingdom); Li, W. [Rolls-Royce plc, PO Box 31, Derby DE24 8BJ (United Kingdom); Coleman, M. [College of Engineering, Bay Campus, Swansea University, Swansea SA1 8EN (United Kingdom); Johnston, R., E-mail: r.johnston@swansea.ac.uk [College of Engineering, Bay Campus, Swansea University, Swansea SA1 8EN (United Kingdom)

    2016-06-21

    The effect of thermo-mechanical history on hot compression behaviour and resulting microstructures of a nickel base superalloy is presented. Hot compression tests were carried out on HAYNES® 282® specimens to varying strains from 0.1 to 0.8. Both single pass and multi-pass tests were completed. 60 min inter-pass times were utilized to accurately replicate industrial forging practices. The effect of dynamic, metadynamic and static recrystallization during inter-pass times on flow stress was investigated. The resulting microstructures were analysed using scanning electron, optical microscopy and EBSD to relate grain size and homogeneity with flow stress data. The study showed a negligible difference between multi-pass and single pass tests for strain increments above 0.2. Therefore, when modelling similar low strain and strain rate forging processes in HAYNES® 282®, previous forging steps can be ignored.

  16. Investigation of the Mechanical Properties and Microstructure of Nickel Superalloys Processed in Shear Forming / Identyfikacja Właściwości Mechanicznych Oraz Mikrostruktury Superstopów Niklu Przetwarzanych W Procesie Kształtowania Obrotowego

    Directory of Open Access Journals (Sweden)

    Żaba K.

    2015-12-01

    Full Text Available The paper presents the research results of the mechanical properties and microstructure of the material in initial state and parts made from nickel superalloy Inconel®718 in the rotary forming process with laser heating. In the first step was carried out basic research of chemical composition, mechanical properties, hardness and microstructure of sheet in initial state. Then from the metal sheet, in industrial conditions, was made axisymmetric parts in the flow and shear forming with laser heating. Parts were subjected to detailed studies focused on the analysis of changes in the mechanical properties and microstructure in the relation to the material in initial state. The analysis was based on the tests results of strength and plastic properties, hardness, microstructural observations and X-ray microanalysis in the areas where defects appear and beyond. The results are presented in the form of tables, charts, and photographs of the microstructure.

  17. Nickel base alloys

    International Nuclear Information System (INIS)

    Gibson, R.C.; Korenko, M.K.

    1980-01-01

    Nickel based alloy, the characteristic of which is that it mainly includes in percentages by weight: 57-63 Ni, 7-18 Cr, 10-20 Fe, 4-6 Mo, 1-2 Nb, 0.2-0.8 Si, 0.01-0.05 Zr, 1.0-2.5 Ti, 1.0-2.5 Al, 0.02-0.06 C and 0.002-0.015 B. The aim is to create new nickel-chromium alloys, hardened in a solid solution and by precipitation, that are stable, exhibit reduced swelling and resistant to plastic deformation inside the reactor. These alloys of the gamma prime type have improved mechanical strengthm swelling resistance, structural stability and welding properties compared with Inconel 625 [fr

  18. Fatigue crack initiation in nickel-based superalloys studied by microstructure-based FE modeling and scanning electron microscopy

    Directory of Open Access Journals (Sweden)

    Fried M.

    2014-01-01

    Full Text Available In this work stage I crack initiation in polycrystalline nickel-based superalloys is investigated by analyzing anisotropic mechanical properties, local stress concentrations and plastic deformation on the microstructural length scale. The grain structure in the gauge section of fatigue specimens was characterized by EBSD. Based on the measured data, a microstructure-based FE model could be established to simulate the strain and stress distribution in the specimens during the first loading cycle of a fatigue test. The results were in fairly good agreement with experimentally measured local strains. Furthermore, the onset of plastic deformation was predicted by identifying shear stress maxima in the microstructure, presumably leading to activation of slip systems. Measurement of plastic deformation and observation of slip traces in the respective regions of the microstructure confirmed the predicted slip activity. The close relation between micro-plasticity, formation of slip traces and stage I crack initiation was demonstrated by SEM surface analyses of fatigued specimens and an in-situ fatigue test in a large chamber SEM.

  19. TOPSIS based parametric optimization of laser micro-drilling of TBC coated nickel based superalloy

    Science.gov (United States)

    Parthiban, K.; Duraiselvam, Muthukannan; Manivannan, R.

    2018-06-01

    The technique for order of preference by similarity ideal solution (TOPSIS) approach was used for optimizing the process parameters of laser micro-drilling of nickel superalloy C263 with Thermal Barrier Coating (TBC). Plasma spraying was used to deposit the TBC and a pico-second Nd:YAG pulsed laser was used to drill the specimens. Drilling angle, laser scan speed and number of passes were considered as input parameters. Based on the machining conditions, Taguchi L8 orthogonal array was used for conducting the experimental runs. The surface roughness and surface crack density (SCD) were considered as the output measures. The surface roughness was measured using 3D White Light Interferometer (WLI) and the crack density was measured using Scanning Electron Microscope (SEM). The optimized result achieved from this approach suggests reduced surface roughness and surface crack density. The holes drilled at an inclination angle of 45°, laser scan speed of 3 mm/s and 400 number of passes found to be optimum. From the Analysis of variance (ANOVA), inclination angle and number of passes were identified as the major influencing parameter. The optimized parameter combination exhibited a 19% improvement in surface finish and 12% reduction in SCD.

  20. Comparison of corrosion behavior between fusion cladded and explosive cladded Inconel 625/plain carbon steel bimetal plates

    International Nuclear Information System (INIS)

    Zareie Rajani, H.R.; Akbari Mousavi, S.A.A.; Madani Sani, F.

    2013-01-01

    Highlights: ► Both explosive and fusion cladding aggravate the corrosion resistance of Inconel 625. ► Fusion cladding is more detrimental to nonuniform corrosion resistance. ► Single-layered fusion coat does not show any repassivation ability. ► Adding more layers enhance the corrosion resistance of fusion cladding Inconel 625. ► High impact energy spoils the corrosion resistance of explosive cladding Inconel 625. -- Abstract: One of the main concerns in cladding Inconel 625 superalloy on desired substrates is deterioration of corrosion resistance due to cladding process. The present study aims to compare the effect of fusion cladding and explosive cladding procedures on corrosion behavior of Inconel 625 cladding on plain carbon steel as substrate. Also, an attempt has been made to investigate the role of load ratio and numbers of fusion layers in corrosion behavior of explosive and fusion cladding Inconel 625 respectively. In all cases, the cyclic polarization as an electrochemical method has been applied to assess the corrosion behavior. According to the obtained results, both cladding methods aggravate the corrosion resistance of Inconel 625. However, the fusion cladding process is more detrimental to nonuniform corrosion resistance, where the chemical nonuniformity of fusion cladding superalloy issuing from microsegregation, development of secondary phases and contamination of clad through dilution hinders formation of a stable passive layer. Moreover, it is observed that adding more fusion layers can enhance the nonuniform corrosion resistance of fusion cladding Inconel 625, though this resistance still remains weaker than explosive cladding superalloy. Also, the results indicate that raising the impact energy in explosive cladding procedure drops the corrosion resistance of Inconel 625.

  1. Low-cycle fatigue and damage of an uncoated and coated single crystal nickel-base superalloy SCB

    International Nuclear Information System (INIS)

    Stekovic, S.; Ericsson, T.

    2007-01-01

    This paper presents low-cycle fatigue (LCF) behaviour and damage mechanisms of uncoated and coated specimens of a single crystal nickel-base superalloy SCB tested at 500 C and 900 C. Four coatings were deposited on the base material, an overlay coating AMDRY997, a platinum-modified aluminide diffusion coating RT22 and two innovative coatings called IC1 and IC3 with a NiW diffusion barrier in the interface. AMDRY997 and RT22 were used as reference coatings. The LCF tests were performed at three strain amplitudes, 1.0, 1.2 and 1.4%, with R = -1, in laboratory air and without any dwell time. The LCF life of the specimens is determined by crack initiation and propagation. Crack data are presented for different classes of crack size in the form of crack density, that is, the number of cracks normalised to the investigated interface length. Micrographs of damage of the coatings are also shown. The effect of the coatings on the LCF life of the superalloy was dependent on the test temperature and deposited coating. At 500 C all coatings had a detrimental effect on the LCF life of the superalloy. At 900 C both AMDRY997 and IC1 prolonged the fatigue life of the superalloy by factors ranging between 1.5 and 4 while RT22 and IC3 shortened the life of the coating-substrate system. Specimens coated with RT22 exhibited generally more damage than other tested coatings at 900 C. Most of the cracks observed initiated at the coating surface and a majority were arrested in the interdiffusion zone between the base material and the coating. No topologically close-packed phases were found. Delamination was only found in AMDRY997 at higher strains. Surface roughness or rumpling was found in the overlay coating AMDRY997 with some cracks initiating from the rumples. The failure morphology at 900 C reflected the role of oxidation in the fatigue life, the crack initiation and propagation of the coated specimens. The wake of the cracks grown into the substrate was severely oxidised leading to

  2. Effect of Sulfur and Chlorine on Fireside Corrosion Behavior of Inconel 740 H Superalloy

    Science.gov (United States)

    Jin-tao, Lu; Yan, Li; Zhen, Yang; Jin-yang, Huang; Ming, Zhu; Gu, Y.

    2018-03-01

    Fireside corrosion behavior of Inconel 740H superalloy was studied at 750 °C in simulated coal ash/flue gas environments by means of XRD, SEM and EDS. The results indicated that the corrosion behavior was strongly related to the SO2 levels and was significantly affected by NaCl additions. In presence of the atmospheres with 0.1 % SO2, the alloy exhibited the highest corrosion resistance due to formation of a stable and dense Cr2O3 film. In presence of the atmosphere with 1.5 % SO2, however, a non-coherent and porous Cr2O3 film was formed. The thickness of film and internal sulfides were substantially increased. The NaCl additions significantly accelerated the corrosion process. A non-protective outer oxide film was formed, composed by multiple layers with serious inner sulfide and spallation. The depths of internal oxidizing and sulfuration zones were significantly increased. The mechanism of ash corrosion formation was also discussed.

  3. The Precipitation Processes and Mechanical Properties of Aged Inconel 718 Alloy After Annealing

    Directory of Open Access Journals (Sweden)

    Maj P.

    2017-09-01

    Full Text Available Inconel 718 is a precipitation hardenable nickel-iron based superalloy. It has exceptionally high strength and ductility compared to other metallic materials. This is due to intense precipitation of the γ’ and γ” strengthening phases in the temperature range 650-850°C. The main purpose of the authors was to analyze the aging process in Inconel 718 obtained in accordance with AMS 5596, and its effect on the mechanical properties. Tensile and hardness tests were used to evaluate the mechanical properties, in the initial aging process and after reheating, as a function of temperature and time respectively in the ranges 650°-900°C and 5-480 min. In addition, to link the mechanical properties with the microstructure transmission microscopy observations were carried out in selected specimens. As a result, factors influencing the microstructure changes at various stages of strengthening were observed. The authors found that the γ’’ phase nucleates mostly homogenously in the temperature range 650-750°C, causing the greatest increase in strength. On the other hand, the γ’ and δ phases are formed heterogeneously at 850°C or after longer annealing in 800°C, which may weaken the material.

  4. Comparative Analysis of Properties and Microstructure of the Plastically Deformed Alloy Inconel®718, Manufactured by Plastic Working and Direct Metal Laser Sintering

    Directory of Open Access Journals (Sweden)

    Żaba K.

    2016-03-01

    Full Text Available Nickel superalloys as Inconel® are materials widely used in the aerospace industry among others for diffusers, combustion chamber, shells of gas generators and other. In most cases, manufacturing process of those parts are used metal strips, produced by conventional plastic processing techniques, and thus by hot or cold rolling. An alternative technology allowing for manufacturing components for jet engines is the technique of 3D printing (additive manufacturing, and most of all Direct Metal Laser Sintering, which is one of the latest achievement in field of additive technologies.

  5. Development and Characterization of a Metal Injection Molding Bio Sourced Inconel 718 Feedstock Based on Polyhydroxyalkanoates

    Directory of Open Access Journals (Sweden)

    Alexandre Royer

    2016-04-01

    Full Text Available The binder plays the most important role in the metal injection molding (MIM process. It provides fluidity of the feedstock mixture and adhesion of the powder to keep the molded shape during injection molding. The binder must provide strength and cohesion for the molded part and must be easy to remove from the molded part. Moreover, it must be recyclable, environmentally friendly and economical. Also, the miscibility between polymers affects the homogeneity of the injected parts. The goal of this study is to develop a feedstock of superalloy Inconel 718 that is environmentally friendly. For these different binders, formulations based on polyethylene glycol (PEG, because of his water solubility property, and bio sourced polymers were studied. Polyhydroxyalkanoates (PHA were investigated as a bio sourced polymer due to its miscibility with the PEG. The result is compared to a standard formulation using polypropylene (PP. The chemical and rheological behavior of the binder formulation during mixing, injection and debinding process were investigated. The feedstock was characterized in the same way as the binders and the interactions between the powder and the binders were also studied. The results show the well adapted formulation of polymer binder to produce a superalloy Inconel 718 feedstock.

  6. Focused Ion Beam Nanotomography of ruthenium-bearing nickel-base superalloys with focus on cast-microstructure and phase stability; Focused Ion Beam Nanotomographie von rutheniumhaltigen Nickelbasis-Superlegierungen mit Fokus auf Gussgefuege und Phasenstabilitaet

    Energy Technology Data Exchange (ETDEWEB)

    Cenanovic, Samir

    2012-12-03

    The influence of rhenium and ruthenium on the multi component system nickel-base superalloy is manifold and complex. An experimental nickel-base superalloy containing rhenium and ruthenium within defined contents, named Astra, was used to investigate the influences of these two elements on the alloy system. The last stage solidification of nickel-base superalloys after Bridgman casting and the high temperature phase stability of these alloys, could be explored with the aid of focused ion beam nanotomography. FIB-nt therefore was introduced and realized at the chair of General Materials Properties of the University Erlangen-Nuremberg. Cast Astra alloys are like other nickel-base superalloys morphologically very inhomogeneous and affected by segregation. In the interdendritic region different structures with huge γ' precipitates are formed. These inhomogeneities and remaining eutectics degrade the mechanical properties, witch makes an understanding of the subsiding processes at solidification of residual melt important for the casting process and the heat treatment. This is why the last stage solidification in the interdendritic region was analyzed. With the help of focused ion beam nanotomography, three different structures identified from 2-D sections could be assigned to one original 3-D structure. It was pointed out, that only the orientation of the plane of the 2-D cut influences the appearance in the 2-D section. The tomography information was used to explain the development during solidification and to create a model of last stage solidification. The interdendritic region is solidifying under the development of eutectic islands. The structure nucleates eutectically epitaxially at primary dendrite arms, with formation of fine γ/γ' precipitates. During solidification the γ' precipitates coarsen in a rod-like structure, and end up in large γ' precipitates. Simulations and other investigations could approve this model. First three

  7. Comparison of Inconel 625 and Inconel 600 in resistance to cavitation erosion and jet impingement erosion

    International Nuclear Information System (INIS)

    Hu, H.X.; Zheng, Y.G.; Qin, C.P.

    2010-01-01

    Liquid droplet erosion (LDE), which often occurs in bellows made of nickel-based alloys, threatens the security operation of the nuclear power plant. As the candidate materials of the bellows, Inconel 600 and Inconel 625 were both tested for resistance to cavitation erosion (CE) and jet impingement erosion (JIE) through vibratory cavitation equipment and a jet apparatus for erosion-corrosion. Cumulative mass loss vs. exposure time was used to evaluate the erosion rate of the two alloys. The surface and cross-sectional morphologies before and after the erosion tests were observed by scanning electron microscopy (SEM), the inclusions were analyzed by an energy dispersive spectroscopy (EDS), and the surface roughness was also measured by surface roughness tester to illustrate the evolution of erosion process. The results show that the cumulative mass loss of CE of Inconel 625 is about 1/6 that of Inconel 600 and the CE incubation period of the Inconel 625 is 4 times as long as that of the Inconel 600. The micro-morphology evolution of CE process illustrates that the twinning and hardness of the Inconel 625 plays a significant role in CE. In addition, the cumulative mass loss of JIE of Inconel 625 is about 2/3 that of Inconel 600 at impacting angle of 90 o , and almost equal to that of the Inconel 600 at impacting angle of 30 o . Overall, the resistance to CE and JIE of Inconel 625 is much superior to that of Inconel 600.

  8. Changes in the properties of superalloys by long term heating

    International Nuclear Information System (INIS)

    Susukida, H.; Tsuji, I.; Kawai, H.

    1976-01-01

    A laboratory study was conducted in order to determine the effect of long term heating (max. 10000h at 850 0 and 950 0 C) on the microstructure, tensile properties, hardness and stress rupture properties of four kinds of superalloys. These superalloys are two kinds of solid solution hardened Ni-base superalloys Hastelloy X and Inconel 617 and two kinds of dispersion strengthened Ni-base superalloys TD-Ni and TD-NiCr. The result of the study can be summarized as follows: (1) Solid solution hardened superalloys: Many precipitates were observed in the grains and on the grain boundaries after 100 hours of heating, and the precipitates became coarse-grained by over 1000 hours of heating. This tendency was remarkable when they were heated at 950 0 C. With the change of their microstructure, their mechanical properties also changed, particularly their tensile ductility decreased remarkably. (2) Dispersion strengthened superalloys: Their microstructure and mechanical properties were almost unchanged by long term heating. (3) The authors proposed ''solid solution hardening value'' in order to grasp quantitatively the solid solution hardening which has been discussed by the content of each element hitherto. (auth.)

  9. Development of welding technology for improving the metallurgical and mechanical properties of 21st century nickel based superalloy 686

    Energy Technology Data Exchange (ETDEWEB)

    Arulmurugan, B. [School of Mechanical Engineering, VIT University, Vellore 632014 (India); KPR Institute of Engineering and Technology, Coimbatore (India); Manikandan, M., E-mail: mano.manikandan@gmail.com [School of Mechanical Engineering, VIT University, Vellore 632014 (India)

    2017-04-13

    Alloy 686 is a highly corrosion resistant 21st-Century Nickel based superalloy derived from Ni-Cr-Mo ternary system. The alloying elements chromium (Cr) and molybdenum (Mo) are added to improve the resistance to corrosion in the broad range of service environment. The presence of a higher percentage of alloying elements Cr and Mo lead to microsegregation and end up with hot cracking in the fusion zone of Nickel-based superalloys. However, there is scanty of information regarding the welding of alloy 686 with respect to the microsegregation of alloying elements. The present study investigates the possibility of bringing down the microsegregation to cut down the formation of secondary phases in the fusion zone. The weld joints were fabricated by Gas Tungsten Arc Welding (GTAW) and Pulsed current gas tungsten arc welding (PCGTAW) with ERNiCrMo-10 filler and without filler wire (autogenous) mode. The microstructural properties of the weld joints were studied with optical and Scanning Electron Microscope (SEM). The joints fabricated by pulsed current (PC) technique shows refined microstructure, narrower weld bead and practically no heat affected zone (HAZ). Scanning Electron Microscope demonstrates the presence of secondary phases in the interdendritic regions of GTAW case. Energy Dispersive X-ray Spectroscopy (EDS) analysis was carried out to evaluate the microsegregation of alloying element. The results show that the segregation of Mo noticed in the interdendritic zone of GTAW both autogenous and filler wire. Tensile and Impact tests were done to evaluate the strength, ductility, and toughness of the weld joints. The results show that the PCGTA helps to obtain improved strength, ductility and toughness of the weld joints compared to their respective GTAW. Bend test did not lead to cracking irrespective of the type of welding adopted in the present study.

  10. Computer aided design of nickel-base superalloys

    International Nuclear Information System (INIS)

    Lawrence, P.J.

    1988-01-01

    This paper describes a computer aided design process for Ni-base superalloys developed and employed at ASEA Brown Boveri. The technique involves a series of modules each of which predicts a particular property of a hypothetical new composition. In the first stage of the development of this design techniques modules were produced to predict phase stability, using PHACOMP, and high temperature creep strength and hot corrosion resistance, using multiple linear regression equations derived from the data in the literature. Alloys designed using these technique are also discussed and, in particular, shortcomings of the design process are highlighted. This information was then used to produce a revamped design methodology involving extra modules, including prediction of an alloy's gamma-prime content. (orig.)

  11. Fatigue Crack Growth Behavior of Nickel-base Superalloy Haynes 282 at 550-750 °C

    Science.gov (United States)

    Rozman, K. A.; Kruzic, J. J.; Hawk, J. A.

    2015-08-01

    The fatigue crack growth rates for nickel-based superalloy Haynes 282 were measured at temperatures of 550, 650, and 750 °C using compact tension specimens with a load ratio of 0.1 and cyclic loading frequencies of 25 Hz and 0.25 Hz. Increasing the temperature from 550 to 750 °C caused the fatigue crack growth rates to increase from ~20 to 60% depending upon the applied stress intensity level. The effect of reducing the applied loading frequency increased the fatigue crack growth rates from ~20 to 70%, also depending upon the applied stress intensity range. The crack path was observed to be transgranular for the temperatures and frequencies used during fatigue crack growth rate testing. At 750 °C, there were some indications of limited intergranular cracking excursions at both loading frequencies; however, the extent of intergranular crack growth was limited and the cause is not understood at this time.

  12. Fatigue Crack Growth Mechanisms for Nickel-based Superalloy Haynes 282 at 550-750 °C

    Science.gov (United States)

    Rozman, Kyle A.; Kruzic, Jamie J.; Sears, John S.; Hawk, Jeffrey A.

    2015-10-01

    The fatigue crack growth rates for nickel-based superalloy Haynes 282 were measured at 550, 650, and 750 °C using compact tension specimens with a load ratio of 0.1 and cyclic loading frequencies of 25 and 0.25 Hz. The crack path was observed to be primarily transgranular for all temperatures, and the observed effect of increasing temperature was to increase the fatigue crack growth rates. The activation energy associated with the increasing crack growth rates over these three temperatures was calculated less than 60 kJ/mol, which is significantly lower than typical creep or oxidation mechanisms; therefore, creep and oxidation cannot explain the increase in fatigue crack growth rates. Transmission electron microscopy was done on selected samples removed from the cyclic plastic zone, and a trend of decreasing dislocation density was observed with increasing temperature. Accordingly, the trend of increasing crack growth rates with increasing temperature was attributed to softening associated with thermally assisted cross slip and dislocation annihilation.

  13. Machinability of nickel based alloys using electrical discharge machining process

    Science.gov (United States)

    Khan, M. Adam; Gokul, A. K.; Bharani Dharan, M. P.; Jeevakarthikeyan, R. V. S.; Uthayakumar, M.; Thirumalai Kumaran, S.; Duraiselvam, M.

    2018-04-01

    The high temperature materials such as nickel based alloys and austenitic steel are frequently used for manufacturing critical aero engine turbine components. Literature on conventional and unconventional machining of steel materials is abundant over the past three decades. However the machining studies on superalloy is still a challenging task due to its inherent property and quality. Thus this material is difficult to be cut in conventional processes. Study on unconventional machining process for nickel alloys is focused in this proposed research. Inconel718 and Monel 400 are the two different candidate materials used for electrical discharge machining (EDM) process. Investigation is to prepare a blind hole using copper electrode of 6mm diameter. Electrical parameters are varied to produce plasma spark for diffusion process and machining time is made constant to calculate the experimental results of both the material. Influence of process parameters on tool wear mechanism and material removal are considered from the proposed experimental design. While machining the tool has prone to discharge more materials due to production of high energy plasma spark and eddy current effect. The surface morphology of the machined surface were observed with high resolution FE SEM. Fused electrode found to be a spherical structure over the machined surface as clumps. Surface roughness were also measured with surface profile using profilometer. It is confirmed that there is no deviation and precise roundness of drilling is maintained.

  14. Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting

    International Nuclear Information System (INIS)

    Muñoz-Moreno, R.; Divya, V.D.; Driver, S.L.; Messé, O.M.D.M.; Illston, T.; Baker, S.; Carpenter, M.A.; Stone, H.J.

    2016-01-01

    Selective laser melting (SLM) of nickel-based superalloys is of great interest for the aerospace industry due to its capability for producing components with complex geometries. However, an improved understanding of the effect of SLM and subsequent post deposition heat treatments on the microstructure and mechanical properties is required to ensure that components with good structural integrity are produced. In this study, the microstructure, texture and elastic anisotropy of the nickel-based superalloy, CM247LC, in the as-SLM and heat-treated states have been analysed. The as-SLM microstructure showed fine elongated cells with a preferential alignment of <001> along the build direction and a significant intercellular misorientation. Heat treatments at temperatures below 1230 °C resulted in a progressive recovery of the microstructure, whilst heat treatments above this temperature gave rise to a recrystallised microstructure. The extent to which nucleation and growth of the γ′ precipitates and secondary particles were affected by increasing the heat treatment temperature was also characterised. The bulk elastic anisotropy of all samples was measured by resonant ultrasound spectroscopy (RUS) and was found to be consistent with the local textures obtained by electron backscatter diffraction (EBSD). It was observed that the initially strong elastic anisotropy exhibited by the as-SLM material was significantly reduced in the recrystallised samples, although some anisotropy was retained as a result of their elongated grain microstructures.

  15. Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting

    Energy Technology Data Exchange (ETDEWEB)

    Muñoz-Moreno, R., E-mail: rociomunozmoreno@gmail.com [Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge CB3 0FS (United Kingdom); Divya, V.D. [Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge CB3 0FS (United Kingdom); Driver, S.L. [Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge CB3 0FS (United Kingdom); Department of Earth Sciences, University of Cambridge, Downing Street, Cambridge CB2 3EQ (United Kingdom); Messé, O.M.D.M. [Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge CB3 0FS (United Kingdom); Illston, T.; Baker, S. [Materials Solutions, Unit 8, Great Western Business Park, McKenzie Way, Worcester WR4 9GN (United Kingdom); Carpenter, M.A. [Department of Earth Sciences, University of Cambridge, Downing Street, Cambridge CB2 3EQ (United Kingdom); Stone, H.J. [Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge CB3 0FS (United Kingdom)

    2016-09-30

    Selective laser melting (SLM) of nickel-based superalloys is of great interest for the aerospace industry due to its capability for producing components with complex geometries. However, an improved understanding of the effect of SLM and subsequent post deposition heat treatments on the microstructure and mechanical properties is required to ensure that components with good structural integrity are produced. In this study, the microstructure, texture and elastic anisotropy of the nickel-based superalloy, CM247LC, in the as-SLM and heat-treated states have been analysed. The as-SLM microstructure showed fine elongated cells with a preferential alignment of <001> along the build direction and a significant intercellular misorientation. Heat treatments at temperatures below 1230 °C resulted in a progressive recovery of the microstructure, whilst heat treatments above this temperature gave rise to a recrystallised microstructure. The extent to which nucleation and growth of the γ′ precipitates and secondary particles were affected by increasing the heat treatment temperature was also characterised. The bulk elastic anisotropy of all samples was measured by resonant ultrasound spectroscopy (RUS) and was found to be consistent with the local textures obtained by electron backscatter diffraction (EBSD). It was observed that the initially strong elastic anisotropy exhibited by the as-SLM material was significantly reduced in the recrystallised samples, although some anisotropy was retained as a result of their elongated grain microstructures.

  16. Effect of long-term aging at 8150C on the tensile properties and microstructural stability of four cobalt- and nickel-base superalloys

    International Nuclear Information System (INIS)

    Hammond, J.P.

    1976-08-01

    Two heats of Haynes alloy 25 and one heat each of Haynes alloy 188, Hastelloy N, and Inconel 625 were tensile tested after aging for 11,000 h at 816 0 C. Yield strength, ultimate tensile strength, and elongation were determined 24, 316, 760, and 982 0 C and compared with typical properties for these materials in the solution annealed condition. Toughness values were determined for these materials from their engineering stress-strain curves. The long-term aging treatment degraded ductility and toughness at room temperature but, contrary to behavior expected for overaging, enhanced them over those for the solution annealed condition in tests at 760 0 C. The tensile properties of the aged superalloys were correlated with mode of fracture and the amounts, identity, and morphology of the precipitates. Aging substantially depleted the hardener tungsten from the matrix in the cobalt-base alloys

  17. Comparison of Inconel 625 and Inconel 600 in resistance to cavitation erosion and jet impingement erosion

    Energy Technology Data Exchange (ETDEWEB)

    Hu, H.X. [State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Science, 62 Wencui Road, Shenyang 110016 (China); Zheng, Y.G., E-mail: ygzheng@imr.ac.c [State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Science, 62 Wencui Road, Shenyang 110016 (China); Qin, C.P. [State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Science, 62 Wencui Road, Shenyang 110016 (China)

    2010-10-15

    Liquid droplet erosion (LDE), which often occurs in bellows made of nickel-based alloys, threatens the security operation of the nuclear power plant. As the candidate materials of the bellows, Inconel 600 and Inconel 625 were both tested for resistance to cavitation erosion (CE) and jet impingement erosion (JIE) through vibratory cavitation equipment and a jet apparatus for erosion-corrosion. Cumulative mass loss vs. exposure time was used to evaluate the erosion rate of the two alloys. The surface and cross-sectional morphologies before and after the erosion tests were observed by scanning electron microscopy (SEM), the inclusions were analyzed by an energy dispersive spectroscopy (EDS), and the surface roughness was also measured by surface roughness tester to illustrate the evolution of erosion process. The results show that the cumulative mass loss of CE of Inconel 625 is about 1/6 that of Inconel 600 and the CE incubation period of the Inconel 625 is 4 times as long as that of the Inconel 600. The micro-morphology evolution of CE process illustrates that the twinning and hardness of the Inconel 625 plays a significant role in CE. In addition, the cumulative mass loss of JIE of Inconel 625 is about 2/3 that of Inconel 600 at impacting angle of 90{sup o}, and almost equal to that of the Inconel 600 at impacting angle of 30{sup o}. Overall, the resistance to CE and JIE of Inconel 625 is much superior to that of Inconel 600.

  18. Studies of Standard Heat Treatment Effects on Microstructure and Mechanical Properties of Laser Net Shape Manufactured INCONEL 718

    Science.gov (United States)

    Qi, H.; Azer, M.; Ritter, A.

    2009-10-01

    Laser net shape manufacturing (LNSM) is a laser cladding/deposition based technology, which can fabricate and repair near-net-shape high-performance components directly from metal powders. Characterizing mechanical properties of the laser net shape manufactured components is prerequisite to the applications of LNSM in aircraft engine industrial productions. Nickel-based superalloys such as INCONEL 718 are the most commonly used metal materials in aircraft engine high-performance components. In this study, the laser deposition process is optimized through a set of designed experiments to reduce the porosity to less than 0.03 pct. It is found that the use of plasma rotating electrode processed (PREP) powder and a high energy input level greater than 80 J/mm are necessary conditions to minimize the porosity. Material microstructure and tensile properties of laser-deposited INCONEL 718 are studied and compared under heat treatment conditions of as deposited, direct aged, solution treatment and aging (STA), and full homogenization followed by STA. Tensile test results showed that the direct age heat treatment produces the highest tensile strength equivalent to the wrought material, which is followed by the STA-treated and the homogenization-treated tensile strengths, while the ductility exhibits the reverse trend. Finally, failure modes of the tensile specimens were analyzed with fractography.

  19. Zinc-induced embrittlement in nickel-base superalloys by simulation and experiment

    Science.gov (United States)

    Otis, Richard; Waje, Mahesh; Lindwall, Greta; Jefferson, Tiffany; Lange, Jeremy; Liu, Zi-Kui

    2017-09-01

    The high cost of Re has driven interest in processes for recovering Re from scrap superalloy parts. In this work thermodynamic modelling is used to study Zn-induced embrittlement of a superalloy and to direct experiments. Treating superalloy powder with Zn vapour reduces the average particle size after milling from approximately ?m to 0.5-10 ?m, vs. ?m for untreated powder. Simulations predict the required treatment time to increase with temperature. Agreement between predictions and experiments suggests that an embrittling liquid forms in less than an hour of Zn vapour treatment between 950-1000 ?C and partial pressures of Zn between 14-34 kPa (2-5 psi).

  20. Microstructural evolution of hydroformed Inconel 625 bellows

    Energy Technology Data Exchange (ETDEWEB)

    Pavithra, E., E-mail: epavithrasenthil@gmail.com; Senthil Kumar, V.S., E-mail: vsskumar@annauniv.edu

    2016-06-05

    Fatigue cycle tests of Inconel 625 superalloy bellows expansion joints were conducted using a Fatigue testing machine at both room and elevated (650 °C) temperatures. Optical Microscope, Scanning Electron Microscope (SEM) and Energy Dispersive X-ray Spectroscopy (EDS) were employed to investigate the microstructure evolution of grains and its boundaries. The intermetallic phases like γ″ were found and carbide precipitates were observed on the grain boundaries at elevated temperature. The recrystallization of the grains and its growth at the elevated temperature is characterized. - Highlights: • The fatigue test is conducted for Inconel 625 bellows in both room and elevated (650 °C) temperatures. • The investigation on the microstructural study of Fatigue behaviour of Inconel 625 Bellows Expansion joints. • The characterisation studies were done by Optical microscope and SEM/EDAS.

  1. Microstructural evolution of hydroformed Inconel 625 bellows

    International Nuclear Information System (INIS)

    Pavithra, E.; Senthil Kumar, V.S.

    2016-01-01

    Fatigue cycle tests of Inconel 625 superalloy bellows expansion joints were conducted using a Fatigue testing machine at both room and elevated (650 °C) temperatures. Optical Microscope, Scanning Electron Microscope (SEM) and Energy Dispersive X-ray Spectroscopy (EDS) were employed to investigate the microstructure evolution of grains and its boundaries. The intermetallic phases like γ″ were found and carbide precipitates were observed on the grain boundaries at elevated temperature. The recrystallization of the grains and its growth at the elevated temperature is characterized. - Highlights: • The fatigue test is conducted for Inconel 625 bellows in both room and elevated (650 °C) temperatures. • The investigation on the microstructural study of Fatigue behaviour of Inconel 625 Bellows Expansion joints. • The characterisation studies were done by Optical microscope and SEM/EDAS.

  2. Effect of refining techniques on stress corrosion cracking behaviour of Inconel X-750

    International Nuclear Information System (INIS)

    Mishra, B.; Moore, J.J.

    1988-01-01

    High-strength age-hardenable nickel-base superalloy Inconel X-750, is susceptible to severe intergranular stress corrosion cracking (IGSCC) when used in the triple heat-treated condition. In this research, the slow strain-rate technique has been employed to evaluate the stress corrosion cracking susceptibility of alloy X-750 under simulated nuclear pressurized water reactor (PWR) conditions, using an automated autoclave system at 8 x 10 6 N m -2 pressure and 289 0 C temperature. The alloys produced via electroslag refining (ESR) or vacuum arc refining (VAR) processing routes containing 0.004% and 0.011% sulphur, respectively, were solution annealed at either 1075 or 1240 0 C for 2 h and water quenched followed by ageing in the 704 to 871 0 C temperature range for up to 200 h, followed by air cooling or furnace cooling. The scanning electron microscopy performed on fractured surfaces revealed that Inconel X-750 processed through the ESR route, solution annealed at 1240 0 C for 2 h and water quenched, aged at 871 0 C for 200 h and furnace cooled provided the best combination of strength, ductility and resistance to SCC. A less sensitized area adjacent to the grain boundary was responsible for the improvement in properties and the alloy X-750 is recommended for PWR applications in the above conditions of processing and heat treatment. (author)

  3. An overview of advanced high-strength nickel-base alloys for LWR applications

    International Nuclear Information System (INIS)

    Prybylowski, J.; Ballinger, R.G.

    1989-01-01

    This paper reviews our current understanding of the behavior of high strength nickel base alloys used in light water reactor (LWR) applications. Emphasis is placed on understanding the fundamental mechanisms controlling crack propagation in these environments. To provide a foundation for this survey, general mechanisms of stress corrosion cracking and hydrogen embrittlement are first reviewed. The behavior of high strength nickel base alloys in LWR environments, as well as in other relevant environments is then reviewed. Suggested mechanisms of crack propagation are discussed. Alternate alloys and microstructural modifications that may result in improved behavior are presented. It is now clear that, at temperatures near 100C, alloy X-750, the predominant high strength nickel base alloy used today in LWR applications, is susceptible to hydrogen embrittlement. A review of published data from hydrogen embrittlement studies of nickel base superalloys during electrolytic charging and in hydrogen sulfide/brine solutions suggests that other nickel base superalloys are available possessing resistance to hydrogen embrittlement superior to that of alloy X-750. Available results of tests in gaseous hydrogen suggest that reduced grain boundary precipitation and a fine distribution of intragranular precipitates that act as irreversible hydrogen traps is the optimum microstructure for hydrogen embrittlement resistance. 42 refs., 2 figs., 5 tabs

  4. Experimental Design for Evaluation of Co-extruded Refractory Metal/Nickel Base Superalloy Joints

    International Nuclear Information System (INIS)

    ME Petrichek

    2005-01-01

    a critical thickness (0.0005 in.). A diffusion barrier that exceeded this thickness would likely fail. The joint fabrication method must therefore mechanically bond the two materials causing little or no interdiffusion upon formation. Co-extrusion fits this description since it forms a mechanical joint between two materials by using heat and pressure. The two materials to be extruded are first assembled and sealed within a co-extrusion billet which is subsequently heated and then extruded through a die. For a production application, once the joint is formed, it is dejacketed to remove the outer canister. The remaining piece consists of two materials bonded together with a thin diffusion barrier. Therefore, the long-term stability of the joint is determined primarily by the kinetics of interdiffusion reaction between the two materials. An experimental design for co-extrusion of refractory metals and nickel-based superalloys was developed to evaluate this joining process and determine the long-term stability of the joints

  5. Evaluation of gamma prime volume fractions and lattice misfits in a nickel base superalloy using the external standard X-ray diffraction method

    Energy Technology Data Exchange (ETDEWEB)

    Tiley, J., E-mail: jaimie.tiley@wpafb.af.mil [Air Force Research Laboratory, Materials and Manufacturing Directorate, WPAFB, OH (United States); Viswanathan, G.B. [Air Force Research Laboratory, Materials and Manufacturing Directorate, WPAFB, OH (United States); Hwang, J.Y. [Materials Engineering Department, University of North Texas, Denton, TX (United States); Shiveley, A. [Air Force Research Laboratory, Materials and Manufacturing Directorate, WPAFB, OH (United States); Banerjee, R. [Materials Engineering Department, University of North Texas, Denton, TX (United States)

    2010-11-25

    The unconstrained lattice parameters and volume fractions of {gamma}' for a low misfit nickel based superalloy were evaluated using X-ray diffraction techniques. Extraction techniques were used to provide unconstrained {gamma}' powders for both water quenched and slow cooled samples that were aged at 760 deg. C for 0, 25, 50, 100, and 200 h. The external standard method was used to determine the volume fraction for the unaged water quenched sample and the slow cooled sample aged for 200 h. These two extremes in processing conditions provided an increase in the total volume fraction of {gamma}'.

  6. Mechanical Behavior of Three-Dimensional Braided Nickel-Based Superalloys Synthesized via Pack Cementation

    Science.gov (United States)

    Lippitz, Nicolas; Erdeniz, Dinc; Sharp, Keith W.; Dunand, David C.

    2018-03-01

    Braided tubes of Ni-based superalloys are fabricated via three-dimensional (3-D) braiding of ductile Ni-20Cr (wt pct) wires followed by post-textile gas-phase alloying with Al and Ti to create, after homogenization and aging, γ/ γ' strengthened lightweight, porous structures. Tensile tests reveal an increase in strength by 100 MPa compared to as-braided Ni-20Cr (wt pct). An interrupted tensile test, combined with X-ray tomographic scans between each step, sheds light on the failure behavior of the braided superalloy tubes.

  7. The Study of the Impact of Surface Preparation Methods of Inconel 625 and 718 Nickel-Base Alloys on Wettability by BNi-2 and BNi-3 Brazing Filler Metals

    Directory of Open Access Journals (Sweden)

    Lankiewicz K.

    2015-04-01

    Full Text Available The article discusses the impact of surface preparation method of Inconel 625 and 718 nickel-base alloys in the form of sheets on wettability of the surface. The results of the investigations of surface preparation method (such as nicro-blasting, nickel plating, etching, degreasing, abrasive blasting with grit 120 and 220 and manually grinding with grit 120 and 240 on spreading of BNi-2 and BNi-3 brazing filler metals, widely used in the aerospace industry in high temperature vacuum brazing processes, are presented. Technological parameters of vacuum brazing process are shown. The macro- and microscopic analysis have shown that nicro-blasting does not bring any benefits of wettability of the alloys investigated.

  8. The Study Of The Impact Of Surface Preparation Methods Of Inconel 625 And 718 Nickel-Base Alloys On Wettability By BNi-2 And BNi-3 Brazing Filler Metals

    Directory of Open Access Journals (Sweden)

    Lankiewicz K.

    2015-06-01

    Full Text Available The article discusses the impact of surface preparation method of Inconel 625 and 718 nickel-base alloys in the form of sheets on wettability of the surface. The results of the investigations of surface preparation method (such as nicro-blasting, nickel plating, etching, degreasing, abrasive blasting with grit 120 and 220 and manually grinding with grit 120 and 240 on spreading of BNi-2 and BNi-3 brazing filler metals, widely used in the aerospace industry in high temperature vacuum brazing processes, are presented. Technological parameters of vacuum brazing process are shown. The macro- and microscopic analysis have shown that nicro-blasting does not bring any benefits of wettability of the alloys investigated.

  9. High Speed Finish Turning of Inconel 718 Using PCBN Tools under Dry Conditions

    Directory of Open Access Journals (Sweden)

    José Luis Cantero

    2018-03-01

    Full Text Available Inconel 718 is a superalloy, considered one of the least machinable materials. Tools must withstand a high level of temperatures and pressures in a very localized area, the abrasiveness of the hard carbides contained in the Inconel 718 microstructure and the adhesion tendency during its machining. Mechanical properties along with the low thermal conductivity become an important issue for the tool wear. The finishing operations for Inconel 718 are usually performed after solution heat treatment and age hardening of the material to give the superalloy a higher level of hardness. Carbide tools, cutting fluid (at normal or high pressures and low cutting speed are the main recommendations for finish turning of Inconel 718. However, dry machining is preferable to the use of cutting fluids, because of its lower environmental impact and cost. Previous research has concluded that the elimination of cutting fluid in these processes is feasible when using hard carbide tools. Recent development of new PCBN (Polycrystalline Cubic Boron Nitride grades for cutting tools with higher tenacity has allowed the application of these tool grades in the finishing operations of Inconel 718. This work studies the performance of commercial PCBN tools from four different tool manufacturers as well as an additional grade with equivalent performance during finish turning of Inconel 718 under dry conditions. Wear tests were carried out with different cutting conditions, determining the evolution of machining forces, surface roughness and tool wear. It is concluded that it is not industrially viable the high-speed finishing of Inconel 718 in a dry environment.

  10. Fatigue of superalloys and intermetallics

    International Nuclear Information System (INIS)

    Stoloff, N.S.

    1993-01-01

    The fatigue behavior of intermetallic alloys and their composites is contrasted to that of nickel-base superalloys. The roles of microstructure and slip planarity are emphasized. Obstacles to use of intermetallics under cyclic loading conditions are described and future research directions are suggested

  11. ANALYSIS OF PITTING CORROSION ON AN INCONEL 718 ALLOY SUBMITTED TO AGING HEAT TREATMENT

    Directory of Open Access Journals (Sweden)

    Felipe Rocha Caliari

    2014-10-01

    Full Text Available Inconel 718 is one of the most important superalloys, and it is mainly used in the aerospace field on account of its high mechanical strength, good resistance to fatigue and creep, good corrosion resistance and ability to operate continuously at elevated temperatures. In this work the resistance to pitting corrosion of a superalloy, Inconel 718, is analyzed before and after double aging heat treatment. The used heat treatment increases the creep resistance of the alloy, which usually is used up to 0.6 Tm. Samples were subjected to pitting corrosion tests in chloride-containing aqueous solution, according to ASTM-F746-04 and the procedure described by Yashiro et al. The results of these trials show that after heat treatment the superalloy presents higher corrosion resistance, i.e., the pitting corrosion currents of the as received surfaces are about 6 (six times bigger (~0.15 mA than those of double aged surfaces (~0.025 mA.

  12. The structure and properties of a nickel-base superalloy produced by osprey atomization-deposition

    Science.gov (United States)

    Bricknell, Rodger H.

    1986-04-01

    The production of a nickel-base superalloy, René* 80, by the Osprey atomization-deposition process has been investigated. Dense (>99 pct) material with a fine-grained equiaxed microstructure was deposited using either argon or nitrogen as the atomizing gas. Defects present in the material included a chill region at the collector plate interface, entrapped recirculated particles, porosity, and ceramic particles from the melting and dispensing system. In contrast to other rapid solidification techniques, low oxygen pick-ups are noted in the current technique. Tensile strengths above those displayed by castings are found in both nitrogen and argon atomized material, and in both the as-deposited and heat treated conditions. In addition, no profound mid-temperature ductility loss is displayed by this low oxygen material, in contrast to results on other rapidly solidified material with high oxygen contents. These results are explained in terms of oxygen embrittlement. In view of the excellent properties measured, the attractive economics of the process, and the fact that fine control of the gas/metal flow ratio is shown to be unnecessary, it is concluded that atomization-deposition presents an attractive potential production route for advanced alloys.

  13. Solidification phenomena in nickel base brazes containing boron and silicon

    International Nuclear Information System (INIS)

    Tung, S.K.; Lim, L.C.; Lai, M.O.

    1996-01-01

    Nickel base brazes containing boron and/or silicon as melting point depressants are used extensively in the repair and joining of aero-engine hot-section components. These melting point depressants form hard and brittle intermetallic compounds with nickel which are detrimental to the mechanical properties of brazed joints. The present investigation studied the microstructural evolution in nickel base brazes containing boron and/or silicon as melting point depressant(s) in simple systems using nickel as the base metal. The basic metallurgical reactions and formation of intermetallic compounds uncovered in these systems will be useful as a guide in predicting the evolution of microstructures in similar brazes in more complex systems involving base metals of nickel base superalloys. The four filler metal systems investigated in this study are: Ni-Cr-Si; Ni-Cr-B; Ni-Si-B and Ni-Cr-Fe-Si-B

  14. Microstructure and Mechanical Properties of Laser Welded Joints of DZ125L and IN718 Nickel Base Superalloys

    Science.gov (United States)

    Liang, Taosha; Wang, Lei; Liu, Yang; Song, Xiu

    2018-05-01

    The microstructure and mechanical properties of the laser welded joint of DZ125L and IN718 nickel base superalloys were investigated. The results show that the fusion zone (FZ) mainly consists of fine dendrite structure with fine γ', Laves phases and MC carbides inhomogeneously distributed. The high welding temperature induces the partial dissolution of γ' in the heat-affected zone (HAZ) of DZ125L and liquation of grain boundaries in both of the HAZs. After post-weld heat treatment (PWHT), fine γ″ and γ' phases precipitate in the FZ, IN718 HAZ and IN718 base metal (BM), and fine γ' precipitate in the γ channel of the HAZ and BM of DZ125L. With tensile testing, the joints after PWHT show higher strengths than that of the weaker DZ125L alloy. Plastic deformation mainly concentrates in the weaker DZ125L and the joint finally fails in the DZ125L BM.

  15. The effect of heat treatment on the micro-structure and the mechanical properties of high-temperature nickel-base-superalloys

    International Nuclear Information System (INIS)

    Schubert, R.; Horn, E.

    1974-01-01

    General review of heat treatment applied to high-temperature nickel-base-superalloys as a function of the volume percent of the γ'-phase. Heat treatment schedule. γ'-morphology and γ'-distribution as well as their effect on mechanical properties. Values obtained from tensile tests up to 1,000 0 C. Results obtained from creep tests. Limitation for the heat treatment of alloys having an unstable γ'-phase. Alloys X 5 NiCrTi 26 15, ATS 270 (approximately INCO 718), NiCr 20 TiAl, NiCr 20 Co 18 Ti, ATS 342 (approximately Waspaloy), ATS 354 (approximately Udimet 520), NiCo 20 Cr 15 MoAlTi, ATS 382 (approximately Udimet 710), ATS 381-G (approximately Mar M 246), FIS 145 and ATS 391-G (aproximately IN 100). (orig.) [de

  16. Galvanic corrosion resistance of welded dissimilar nickel-base alloys

    International Nuclear Information System (INIS)

    Corbett, R.A.; Morrison, W.S.; Snyder, R.J.

    1986-01-01

    A program for evaluating the corrosion resistance of various dissimilar welded nickel-base alloy combinations is outlined. Alloy combinations included ALLCORR, Hastelloy C-276, Inconel 72 and Inconel 690. The GTAW welding process involved both high and minimum heat in-put conditions. Samples were evaluated in the as-welded condition, as well as after having been aged at various condtions of time and temperature. These were judged to be most representative of process upset conditions which might be expected. Corrosion testing evaluated resistance to an oxidizing acid and a severe service environment in which the alloy combinations might be used. Mechanical properties are also discussed

  17. A high-throughput search for new ternary superalloys

    Science.gov (United States)

    Nyshadham, Chandramouli; Hansen, Jacob; Oses, Corey; Curtarolo, Stefano; Hart, Gus

    In 2006 an unexpected new superalloy, Co3[Al,W], was discovered. This new alloy is cobalt-based, in contrast to conventional superalloys, which are nickel-based. Inspired by this new discovery, we performed first-principles calculations, searching through 2224 ternary metallic systems of the form A3[B0.5C0.5], where A = Ni/Co/Fe and [B, C] = all binary combinations of 40 different elements chosen from the periodic table. We found 175 new systems that are better than the Co3[Al, W] superalloy. 75 of these systems are brand new--they have never been reported in experimental literature. These 75 new potential superalloys are good candidates for further experiments. Our calculations are consistent with current experimental literature where data exists. Work supported under: ONR (MURI N00014-13-1-0635).

  18. Effect of laser shock on tensile deformation behavior of a single crystal nickel-base superalloy

    International Nuclear Information System (INIS)

    Lu, G.X.; Liu, J.D.; Qiao, H.C.; Zhou, Y.Z.; Jin, T.; Zhao, J.B.; Sun, X.F.; Hu, Z.Q.

    2017-01-01

    This investigation focused on the tensile deformation behavior of a single crystal nickel-base superalloy, both in virgin condition and after laser shock processing (LSP) with varied technology parameters. Nanoindention tests were carried out on the sectioned specimens after LSP treatment to characterize the surface strengthening effect. Stress strain curves of tensile specimens were analyzed, and microstructural observations of the fracture surface and the longitudinal cross-sections of ruptured specimens were performed via scanning electron microscope (SEM), in an effort to clarify the fracture mechanisms. The results show that a surface hardening layer with the thickness of about 0.3–0.6 mm was gained by the experimental alloys after LSP treatment, but the formation of surface hardening layer had not affected the yield strength. Furthermore, fundamental differences in the plastic responses at different temperatures due to LSP treatment had been discovered. At 700 °C, the slip deformation was held back when it extended to the surface hardening layer and the ensuing slip steps improved the plasticity; however, at 1000 °C, surface hardening layer hindered the macro necking, which resulted in the relatively lower plasticity.

  19. Effect of laser shock on tensile deformation behavior of a single crystal nickel-base superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Lu, G.X. [Institute of Metal Research, Chinese Academy of Sciences, 72 Wenhua Road, Shenyang 110016 (China); University of Chinese Academy of Sciences, 19 Yuquan Road, Beijing 100049 (China); Liu, J.D., E-mail: jdliu@imr.ac.cn [Institute of Metal Research, Chinese Academy of Sciences, 72 Wenhua Road, Shenyang 110016 (China); Qiao, H.C. [Shenyang Institute of Automation, Chinese Academy of Sciences, 114 Nanta Road, Shenyang 110016 (China); Zhou, Y.Z. [Institute of Metal Research, Chinese Academy of Sciences, 72 Wenhua Road, Shenyang 110016 (China); Jin, T., E-mail: tjin@imr.ac.cn [Institute of Metal Research, Chinese Academy of Sciences, 72 Wenhua Road, Shenyang 110016 (China); Zhao, J.B. [Shenyang Institute of Automation, Chinese Academy of Sciences, 114 Nanta Road, Shenyang 110016 (China); Sun, X.F.; Hu, Z.Q. [Institute of Metal Research, Chinese Academy of Sciences, 72 Wenhua Road, Shenyang 110016 (China)

    2017-02-16

    This investigation focused on the tensile deformation behavior of a single crystal nickel-base superalloy, both in virgin condition and after laser shock processing (LSP) with varied technology parameters. Nanoindention tests were carried out on the sectioned specimens after LSP treatment to characterize the surface strengthening effect. Stress strain curves of tensile specimens were analyzed, and microstructural observations of the fracture surface and the longitudinal cross-sections of ruptured specimens were performed via scanning electron microscope (SEM), in an effort to clarify the fracture mechanisms. The results show that a surface hardening layer with the thickness of about 0.3–0.6 mm was gained by the experimental alloys after LSP treatment, but the formation of surface hardening layer had not affected the yield strength. Furthermore, fundamental differences in the plastic responses at different temperatures due to LSP treatment had been discovered. At 700 °C, the slip deformation was held back when it extended to the surface hardening layer and the ensuing slip steps improved the plasticity; however, at 1000 °C, surface hardening layer hindered the macro necking, which resulted in the relatively lower plasticity.

  20. Effect of Notches on Creep-Fatigue Behavior of a P/M Nickel-Based Superalloy

    Science.gov (United States)

    Telesman, Jack; Gabb, Timothy P.; Ghosn, Louis J.; Gayda, John, Jr.

    2015-01-01

    A study was performed to determine and model the effect of high temperature dwells on notched low cycle fatigue (NLCF) and notch stress rupture behavior of a fine grain LSHR powder metallurgy (PM) nickel-based superalloy. It was shown that a 90 second dwell applied at the minimum stress (min dwell) was considerably more detrimental to the NLCF lives than similar dwell applied at the maximum stress (max dwell). The short min dwell NLCF lives were shown to be caused by growth of small oxide blisters which caused preferential cracking when coupled with high concentrated notch root stresses. The cyclic max dwell notch tests failed mostly by a creep accumulation, not by fatigue, with the crack origin shifting internally to a substantial distance away from the notch root. The classical von Mises plastic flow model was unable to match the experimental results while the hydrostatic stress profile generated using the Drucker-Prager plasticity flow model was consistent with the experimental findings. The max dwell NLCF and notch stress rupture tests exhibited substantial creep notch strengthening. The triaxial Bridgman effective stress parameter was able to account for the notch strengthening by collapsing the notched and uniform gage geometry test data into a singular grouping.

  1. Optimising mechanical properties of hot forged nickel superalloy 625 components

    Science.gov (United States)

    Singo, Nthambe; Coles, John; Rosochowska, Malgorzata; Lalvani, Himanshu; Hernandez, Jose; Ion, William

    2018-05-01

    Hot forging and subsequent heat treatment were resulting in substandard mechanical properties of nickel superalloy, Alloy 625, components. The low strength was found to be due to inadequate deformation during forging, excessive grain growth and precipitation of carbides during subsequent heat treatment. Experimentation in a drop forging company and heat treatment facility led to the establishment of optimal parameters to minimise grain size and mitigate the adverse effects of carbide precipitation, leading to successful fulfilment of mechanical property specifications. This was achieved by reducing the number of operations, maximising the extent of deformation by changing the slug dimensions and its orientation in the die, and minimising the time of exposure to elevated temperatures in both the forging and subsequent heat treatment processes to avoid grain growth.

  2. Application of Finite Element, Phase-field, and CALPHAD-based Methods to Additive Manufacturing of Ni-based Superalloys.

    Science.gov (United States)

    Keller, Trevor; Lindwall, Greta; Ghosh, Supriyo; Ma, Li; Lane, Brandon M; Zhang, Fan; Kattner, Ursula R; Lass, Eric A; Heigel, Jarred C; Idell, Yaakov; Williams, Maureen E; Allen, Andrew J; Guyer, Jonathan E; Levine, Lyle E

    2017-10-15

    Numerical simulations are used in this work to investigate aspects of microstructure and microseg-regation during rapid solidification of a Ni-based superalloy in a laser powder bed fusion additive manufacturing process. Thermal modeling by finite element analysis simulates the laser melt pool, with surface temperatures in agreement with in situ thermographic measurements on Inconel 625. Geometric and thermal features of the simulated melt pools are extracted and used in subsequent mesoscale simulations. Solidification in the melt pool is simulated on two length scales. For the multicomponent alloy Inconel 625, microsegregation between dendrite arms is calculated using the Scheil-Gulliver solidification model and DICTRA software. Phase-field simulations, using Ni-Nb as a binary analogue to Inconel 625, produced microstructures with primary cellular/dendritic arm spacings in agreement with measured spacings in experimentally observed microstructures and a lesser extent of microsegregation than predicted by DICTRA simulations. The composition profiles are used to compare thermodynamic driving forces for nucleation against experimentally observed precipitates identified by electron and X-ray diffraction analyses. Our analysis lists the precipitates that may form from FCC phase of enriched interdendritic compositions and compares these against experimentally observed phases from 1 h heat treatments at two temperatures: stress relief at 1143 K (870 °C) or homogenization at 1423 K (1150 °C).

  3. Nanoscale Origins of the Size Effect in the Compression Response of Single Crystal Ni-Base Superalloy Micro-Pillars

    Directory of Open Access Journals (Sweden)

    Siqi Ying

    2018-04-01

    Full Text Available Nickel superalloys play a pivotal role in enabling power-generation devices on land, sea, and in the air. They derive their strength from coherent cuboidal precipitates of the ordered γ’ phase that is different from the γ matrix in composition, structure and properties. In order to reveal the correlation between elemental distribution, dislocation glide and the plastic deformation of micro- and nano-sized volumes of a nickel superalloy, a combined in situ nanoindentation compression study was carried out with a scanning electron microscope (SEM on micro- and nano-pillars fabricated by focused ion beam (FIB milling of Ni-base superalloy CMSX4. The observed mechanical response (hardening followed by softening was correlated with the progression of crystal slip that was revealed using FIB nano-tomography and energy-dispersive spectroscopy (EDS elemental mapping. A hypothesis was put forward that the dependence of material strength on the size of the sample (micropillar diameter is correlated with the characteristic dimension of the structural units (γ’ precipitates. By proposing two new dislocation-based models, the results were found to be described well by a new parameter-free Hall–Petch equation.

  4. Thermal stability of the superalloys Inconel 625 and Nimonic 86

    International Nuclear Information System (INIS)

    Kohl, H.K.; Peng, K.

    1981-01-01

    The thermal stability of Inconel 625 and Nimonic 86, as received, cold worked (10, 20, and 40%), and solution treated, was investigated in the temperature range 500-900 0 C. The annealing times varied from 0.3 (0.03) to 100 days. Precipitation hardening and recovery (recrystallisation) takes place in cold worked material, beginning after shorter times in cold worked material than in as received material. The temperature interval for precipitation hardening is extended in Nimonic 86, due to cold working, from about 500-600 0 C to about 450-700 0 C. It is possible to suppress or retard the precipitation hardening in solution treated Inconel 625 and Nimonic 86 by fast cooling after solution annealing. Hardness was measured at room temperature with five different loads, so that the parameters k and n from Meyer's-law, and the Brinell hardness number (for F / D 2 = 30) could be determined. The lattice contraction of Inconel 625 due to ageing was investigated with X-ray measurements. The change of intensities of the diffractometer traces due to recovery was also determined. (orig.)

  5. Effect of modified mold shell on the microstructure and tensile fracture morphology of single-crystal nickel-base superalloy

    Science.gov (United States)

    Xu, Weitai; Zhao, Yutao; Sun, Shaochun; Liu, Manping; Ma, Dexin; Liang, Xiangfeng; Wang, Cunlong; Tao, Ran

    2018-04-01

    The mold shell used for single-crystal turbine blades preparation was modified from conventional process to fiber reinforcement technology. The wall thickness was decreased by 32.3 percent (pct) than the conventional process. Then these two mold shells were used to produce single crystal samples of nickel-base superalloy in a Bridgman furnace. The local temperature curves were recorded in the process. The results show that the modified mold shell can increase the temperature gradient in the mushy zone than the conventional mold shell. The primary and secondary dendrite arm space were reduced by 8 pct and 12 pct, respectively. Moreover, both the area fraction and mean size of the γ‧/γ eutectic were declined, as well as the dendritic segregation tendency. Therefore it contributed to the lower residual eutectic and micro-porosity in the heat-treated microstructure. Further, fracture surface of the samples made by modified mold shell exhibited smaller facets and more uniform dimples in the size and shape.

  6. 3D imaging and characterisation of strengthening particles in inconel 718 using FIB tomography

    Energy Technology Data Exchange (ETDEWEB)

    Kruk, Adam; Gruszczynski, Adam; Czyrska-Filemonowicz, Aleksandra [AGH University of Science and Technology, Faculty of Metals Engineering and Industrial Computer Science, Al. A. Mickiewicza 30, 30-059 Krakow (Poland)

    2011-07-01

    The Inconel 718 is a commercial nickel-base superalloy, widely used for critical pieces in turbine engines. Its microstructure consists of the {gamma} matrix and strengthening coherent nanoparticles {gamma}' and {gamma}''. In the present work FIB tomography technique was used for imaging and characterisation of strengthening particles. FIB tomography is based on a serial sectioning procedure using a FIB/SEM dual beam workstation. Repeated removal of layers as thin as several nm for some hundred times allows to investigate at total a volume of some {mu}m3 with a voxel size as 2.5 nm x 2.5 nm x 2.5 nm. 3D mapping of nanoparticles with high Z-resolution by serial FIB slicing (in a distance of about 2.5 nm) and SEM imaging was performed. Ga ion beam at 30 kV was used to perform a precise in-situ milling. The SEM images at accelerating voltage 1.5 kV were taken with using ESB detector. The real 3D-data of precipitates obtained by FIB tomography, open a new possibility for microstructure analysis of materials for industrial applications.

  7. Microstructural Characterization of a Polycrystalline Nickel-Based Superalloy Processed via Tungsten-Intert-Gas-Shaped Metal Deposition

    Science.gov (United States)

    Clark, Daniel; Bache, Martin R.; Whittaker, Mark T.

    2010-12-01

    Recent trials have produced tungsten-inert-gas (TIG)-welded structures of a suitable scale to allow an evaluation of the technique as an economic and commercial process for the manufacture of complex aeroengine components. The employment of TIG welding is shown to have specific advantages over alternative techniques based on metal inert gas (MIG) systems. Investigations using the nickel-based superalloy 718 have shown that TIG induces a smaller weld pool with less compositional segregation. In addition, because the TIG process involves a pulsed power source, a faster cooling rate is achieved, although this rate, in turn, compromises the deposition rate. The microstructures produced by the two techniques differ significantly, with TIG showing an absence of the detrimental delta and Laves phases typically produced by extended periods at a high temperature using MIG. Instead, an anisotropic dendritic microstructure was evident with a preferred orientation relative to the axis of epitaxy. Niobium was segregated to the interdendritic regions. A fine-scale porosity was evident within the microstructure with a maximum diameter of approximately 5 μm. This porosity often was found in clusters and usually was associated with the interdendritic regions. Subsequent postdeposition heat treatment was shown to have no effect on preexisting porosity and to have a minimal effect on the microstructure.

  8. L12-phase cutting during high temperature and low stress creep of a Re-containing Ni-base single crystal superalloy

    Czech Academy of Sciences Publication Activity Database

    Kostka, A.; Maelzer, G. (ed.); Eggeler, G.; Dlouhý, Antonín; Reese, S.; Mack, T.

    2007-01-01

    Roč. 42, č. 11 (2007), s. 3951-3957 ISSN 0022-2461 Institutional research plan: CEZ:AV0Z20410507 Keywords : nickel-base superalloys * single crystals * creep Subject RIV: JG - Metallurgy Impact factor: 1.081, year: 2007

  9. Influence of dwell times on the thermomechanical fatigue behavior of a directionally solidified Ni-base superalloy

    Czech Academy of Sciences Publication Activity Database

    Guth, S.; Petráš, Roman; Škorík, Viktor; Kruml, Tomáš; Man, Jiří; Lang, K. H.; Polák, Jaroslav

    2015-01-01

    Roč. 80, NOV (2015), s. 426-433 ISSN 0142-1123 R&D Projects: GA MŠk(CZ) EE2.3.30.0063 Institutional support: RVO:68081723 Keywords : Nickel base superalloy * Thermomechanical fatigue * Dwell time * Lifetime behavior * Damage mechanisms Subject RIV: JL - Materials Fatigue, Friction Mechanics Impact factor: 2.162, year: 2015

  10. Manufacture of an Inconel pressure vessel

    International Nuclear Information System (INIS)

    Herz, H.; Iversen, K.; Stiefelhagen, B.

    1978-01-01

    The fabrication of a thermo-shock-loaded pressure vessel of high temperature nickel alloys required the individual licensing of the basic and addition materials according to the AD data sheets Contrary to the experience of Duennbleck processars, it was found that the alloy Inconel 718 in its hardened state could not be allowed due to the formation of the brittle daves phase in the welding deposit. Positive experience was acquired however with the non-hardenable alloy Inconel 625 which could be processed as jacket materials without problem. Rods of Inconel 625 were used as similar additive for WIG welding and the same type electrode 112 for E-welding. The heat resistance required of 320 N/cm 2 at 623 0 K and the lowest notch bar value of 35 J/cm 2 at RT were well surpassed. The mixed compounds of Inconel 625 and 718 were also no problem when welding with the non-hardening additives Inconel 625 and 112 and eliminating a thermal treatment. (orig.) [de

  11. Integrated computational microstructure engineering for single-crystal nickel-base superalloys

    Science.gov (United States)

    Wang, Billie

    A methodology that integrates the phase field model with simpler models was developed to study the early stages of microstructural development in nickel base superalloys under non-isothermal conditions, allowing for faster, more comprehensive examination of the experimental system. Additionally, the parameters required for calibrating a phase field model were examined for uncertainty, and a comprehensive method for linking experimental data to a model was developed. The methodology developed was applied to analyze the formation of bimodal particle size distributions during linear continuous cooling. The dynamic competition for supersaturation by growth of existing precipitates and nucleation of new particles was modeled. The nucleation rate was calculated according to classical nucleation theory as function of local supersaturation and temperature. The depletion of matrix super-saturation by growth of existing particles was calculated from fully diffusion-controlled precipitate growth in an infinite matrix. Phase field simulations of gamma' precipitation in a binary Ni-Al alloy were performed under continuous cooling conditions. Then the average and maximum matrix supersaturations were calculated and plotted onto the contours of nucleation rate and growth rate in concentration and temperature space. These methods were used iteratively to identify the window for bimodal particle size distributions. Combining the models of different complexities produced a much more comprehensive understanding of the competing dynamics involved early in microstructure formation. A systemic method for calibrating a model to experimental alloy systems was developed. Calibrated to isothermal aging data along with literature, database and parametric values, a phase field model reproduced the precipitation kinetics. Quantitative phase field modeling techniques were developed to control the influence of uncertainty in the original data sources for model inputs. Using more data sources than

  12. Effect of alumina-silica-zirconia eutectic ceramic thermal barrier coating on the low cycle fatigue behaviour of cast polycrystalline nickel-based superalloy at 900 °C

    Czech Academy of Sciences Publication Activity Database

    Obrtlík, Karel; Čelko, L.; Chráska, Tomáš; Šulák, Ivo; Gejdoš, P.

    2017-01-01

    Roč. 318, MAY (2017), s. 374-381 ISSN 0257-8972. [RIPT - International Meeting on Thermal Spraying /7./. Limoges, 09.12.2015-12.12.2015] R&D Projects: GA ČR(CZ) GA15-20991S Institutional support: RVO:68081723 ; RVO:61389021 Keywords : Thermal barrier coating * Nickel-based superalloy * Plasma spraying * High temperature fatigue * Fatigue life * Cyclic stress-strain curve Subject RIV: JL - Materials Fatigue, Friction Mechanics; JL - Materials Fatigue, Friction Mechanics (UFP-V) OBOR OECD: Audio engineering, reliability analysis; Audio engineering, reliability analysis (UFM-A); Audio engineering, reliability analysis (UFP-V) Impact factor: 2.589, year: 2016

  13. Surface passivity largely governs the bioaccessibility of nickel-based powder particles at human exposure conditions.

    Science.gov (United States)

    Hedberg, Yolanda S; Herting, Gunilla; Latvala, Siiri; Elihn, Karine; Karlsson, Hanna L; Odnevall Wallinder, Inger

    2016-11-01

    The European chemical framework REACH requires that hazards and risks posed by chemicals, including alloys and metals, are identified and proven safe for humans and the environment. Therefore, differences in bioaccessibility in terms of released metals in synthetic biological fluids (different pH (1.5-7.4) and composition) that are relevant for different human exposure routes (inhalation, ingestion, and dermal contact) have been assessed for powder particles of an alloy containing high levels of nickel (Inconel 718, 57 wt% nickel). This powder is compared with the bioaccessibility of two nickel-containing stainless steel powders (AISI 316L, 10-12% nickel) and with powders representing their main pure alloy constituents: two nickel metal powders (100% nickel), two iron metal powders and two chromium metal powders. X-ray photoelectron spectroscopy, microscopy, light scattering, and nitrogen absorption were employed for the particle and surface oxide characterization. Atomic absorption spectroscopy was used to quantify released amounts of metals in solution. Cytotoxicity (Alamar blue assay) and DNA damage (comet assay) of the Inconel powder were assessed following exposure of the human lung cell line A549, as well as its ability to generate reactive oxygen species (DCFH-DA assay). Despite its high nickel content, the Inconel alloy powder did not release any significant amounts of metals and did not induce any toxic response. It is concluded, that this is related to the high surface passivity of the Inconel powder governed by its chromium-rich surface oxide. Read-across from the pure metal constituents is hence not recommended either for this or any other passive alloy. Copyright © 2016 The Author(s). Published by Elsevier Inc. All rights reserved.

  14. Decarburization behavior and mechanical properties of Inconel 617 during high temperature oxidation in He environment

    International Nuclear Information System (INIS)

    Kim, Young Do; Kim, Dae Gun; Jo, Tae Sun; Kim, Hoon Sup; Lim, Jeong Hun

    2010-04-01

    Among Generation IV reactor concepts, high temperature gas-cooled reactors (HTGRs) are high-efficiency systems designed for the economical production of hydrogen and electricity. Inconel 617 is a solid-solution strengthening Ni-based superalloy that shows excellent strength, creep-rupture strength, and oxidation resistance at high temperatures. Thus, it is a desirable candidate for tube material of IHX and HGD in HTGRs. In spite of these excellent properties, aging degradation by long time exposure at high temperature induced to deterioration of mechanical properties and furthermore alloys' lifetime because of Cr-depleted zone and carbide free zone below external scale. Also, machinability of Inconel 617 is a important property for system design. In this study, oxidation and decarbrization behavior were evaluated at various aging temperature and environment. Also, cold rolling was carried out for the machinability evaluation of Inconel 617 and then microstructure change was evaluated

  15. The effect of deformation temperature on the microstructure evolution of Inconel 625 superalloy

    Science.gov (United States)

    Guo, Qingmiao; Li, Defu; Guo, Shengli; Peng, Haijian; Hu, Jie

    2011-07-01

    Hot compression tests of Inconel 625 superalloy were conducted using a Gleeble-1500 simulator between 900 °C and 1200 °C with different true strains and a strain rate of 0.1 s -1. Scanning electron microscope (SEM) and electron backscatter diffraction technique (EBSD) were employed to investigate the effect of deformation temperature on the microstructure evolution and nucleation mechanisms of dynamic recrystallization (DRX). It is found that the relationship between the DRX grain size and the peak stress can be expressed by a power law function. Significant influence of deformation temperatures on the nucleation mechanisms of DRX are observed at different deformation stages. At lower deformation temperatures, continuous dynamic recrystallization (CDRX) characterized by progressive subgrain rotation is considered as the main mechanism of DRX at the early deformation stage. However, discontinuous dynamic recrystallization (DDRX) with bulging of the original grain boundaries becomes the operating mechanism of DRX at the later deformation stage. At higher deformation temperatures, DDRX is the primary mechanism of DRX, while CDRX can only be considered as an assistant mechanism at the early deformation stage. Nucleation of DRX can also be activated by the twinning formation. With increasing the deformation temperature, the effect of DDRX accompanied with twinning formation grows stronger, while the effect of CDRX grows weaker. Meanwhile, the position of subgrain formation shifts gradually from the interior of original grains to the vicinity of the original boundaries.

  16. Nickel based alloys for molten salt applications in pyrochemical reprocessing applications

    International Nuclear Information System (INIS)

    Ningshen, S.; Ravi Shankar, A.; Rao, Ch. Jagadeeswara; Mallika, C.; Kamachi Mudali, U.

    2016-01-01

    Pyrochemical reprocessing route is one of the best option for reprocessing of spent metallic nuclear fuel from future fast breeder in many countries, especially in the US (Integral fast reactor, IFR), Russia (Research Institute of Atomic Reactors, RIAR), Japan, Korea and India. This technology with intrinsic nuclear proliferation resistance is regarded as one of the most promising nuclear fuel cycle technologies of the next-generation. However, the selection of materials of construction for pyrochemical reprocessing plants is challenging because of the extreme environments, i.e., high radiation, corrosive molten salt (LiCl-KCl, LiCl-KCl-CsCl, KCl-NaCl-MgCl 2 , etc.), reactive molten metals, and high temperature. Efforts have been made to develop compatible materials for various unit operations like salt preparation, electrorefining, cathode processing and alloy casting in pyrochemical reprocessing. Nickel and its alloy are the candidate materials for salt purification exposed to molten LiCl-KCl under Cl 2 bubbling, in air or ultra high purity argon environment. In the present study, the corrosion behavior of candidate materials like Inconel 600, Inconel 625, Inconel 690 exposed to molten LiCl-KCl eutectic salt environment at 500 to 600 °C have been carried out. The surface morphology of the exposed samples and scales were examined by SEM/EDX and XRD. The weight loss results indicated that Inconel 600 and Inconel 690 offer better corrosion resistance compared to Inconel 625 in air and chlorine environment. Higher corrosion of Inconel 625 is attributed to development of Mo rich salt layers. However, Ni base alloys exhibited a decreasing trend of weight loss with increasing time of exposure and weight gain was observed under UHP Ar environment. The mechanism of corrosion of Ni base alloys appeared to be due to formation of Cr rich and Ni rich layers of Cr 2 O 3 , NiO and spinel oxides at the surface and subsequent spallation. Based on the present studies, Inconel 690

  17. The influence of cobalt, tantalum, and tungsten on the elevated temperature mechanical properties of single crystal nickel-base superalloys

    Science.gov (United States)

    Nathal, M. V.; Ebert, L. J.

    1985-01-01

    The influence of composition on the tensile and creep strength of 001-line oriented nickel-base superalloy single crystals at temperatures near 1000 C was investigated. Cobalt, tantalum, and tungsten concentrations were varied according to a matrix of compositions based on the single crystal version of MAR-M247. For alloys with the baseline refractory metal level of 3 wt pct Ta and 10 wt pct W, decreases in Co level from 10 to 0 wt pct resulted in increased tensile and creep strength. Substitution of 2 wt pct W for 3 wt pct Ta resulted in decreased creep life at high stresses, but improved life at low stresses. Substitution of Ni for Ta caused large reductions in tensile strength and creep resistance, and corresponding increases in ductility. For these alloys with low Ta-plus-W totals, strength was independent of Co level. The effects of composition on properties were related to the microstructural features of the alloys. In general, high creep strength was associated with high levels of gamma-prime volume fraction, gamma-gamma-prime lattice mismatch, and solid solution hardening.

  18. Fatigue-crack propagation response of two nickel-base alloys in a liquid sodium environment

    International Nuclear Information System (INIS)

    Mills, W.J.; James, L.A.

    1979-01-01

    The elevated temperature fatigue-crack propagation response of Inconel 600 and Inconel 718 was characterized within a linear-elastic fracture mechanics framework in air and low-oxygen liquid sodium environments. The crack growth rates of both nickel-base alloys tested in liquid sodium were found to be considerably lower than those obtained in air. This enhanced fatigue resistance in sodium was attributed to the very low oxygen content in the inert sodium environment. Electron fractographic examination of the Inconel 600 and Inconel 718 fatigue fracture surfaces revealed that operative crack growth mechanisms were dependent on the prevailing stress intensity level. Under low growth rate conditions, Inconel 600 and Inconel 718 fracture surfaces exhibited a faceted, crystallographic morphology in both air and sodium environments. In the higher growth rate regime, fatigue striations were observed; however, striations formed in sodium were rather ill-defined. These indistinct striations were attributed to the absence of oxygen in the liquid sodium environment. Striation spacing measurements were found to be in excellent agreement with macroscopic growth rates in both environments

  19. Corrosion Performance of Inconel 625 in High Sulphate Content

    Science.gov (United States)

    Ismail, Azzura

    2016-05-01

    Inconel 625 (UNS N06625) is a type of nickel-chromium-molybdenum alloy with excellent corrosion resistance in a wide range of corrosive media, being especially resistant to pitting and crevice corrosion. However, in aggressive environment, Inconel 625 will suffer corrosion attack like other metals. This research compared the corrosion performance of Inconel 625 when exposed to higher sulphate content compared to real seawater. The results reveal that Inconel 625 is excellent in resist the corrosion attack in seawater. However, at increasing temperature, the corrosion resistance of this metal decrease. The performance is same in seawater with high sulphate content at increasing temperature. It can be concluded that sulphate promote perforation on Inconel 625 and become aggressive agents that accelerate the corrosion attack.

  20. The effects of ruthenium on the phase stability of fourth generation Ni-base single crystal superalloys

    International Nuclear Information System (INIS)

    Sato, Atsushi; Harada, Hiroshi; Yokokawa, Tadaharu; Murakumo, Takao; Koizumi, Yutaka; Kobayashi, Toshiharu; Imai, Hachiro

    2006-01-01

    The formation of topologically close-packed (TCP) phases in nickel-base single crystal superalloys causes considerable degradation of the mechanical properties. It has recently been found that platinum-group metals can be effective in controlling the precipitation of such phases, and this extent of precipitation control requires further investigation. This study compares Ru-containing and non-Ru-containing single crystal superalloys. Scanning electron microscopy microstructural observations showed that the rate of TCP phase precipitations decreased through Ru addition. Transmission electron microscopy microstructural observations showed that the P phase, one of the TCP phases, was eliminated through the addition of Ru. The occurrence of this phenomenon will be discussed

  1. Coupling effects of tungsten and molybdenum on microstructure and stress-rupture properties of a nickel-base cast superalloy

    Directory of Open Access Journals (Sweden)

    Tongjin Zhou

    2018-02-01

    Full Text Available In order to comprehensively understand the forming mechanism of abnormal phases solidified in a nickel-base cast superalloy with additives of tungsten and molybdenum, the coupling effects of W and Mo on the microstructure and stress-rupture properties were investigated in this paper. The results indicated that the precipitation of primary α-(W, Mo phase depended tremendously on the amount of W and Mo addition. When the total amount of W and Mo was greater than 5.79 at%, α-(W, Mo phase became easily precipitated in the alloy. With increasing of Mo/W ratio, the dendrite-like α-(W, Mo phases were apt to convert into small bars or blocky-like phases at the vicinities of γ′/γ eutectic. The morphological changes of α-(W, Mo phase can be interpreted as the non-equilibrium solidification of W and Mo in the alloy. Since the large sized α-(W, Mo phase has detrimental effects on stress-rupture properties in as-cast conditions, secondary cracks may mainly initiate at and then propagate along the interfaces of brittle phases and soft matrix. During exposing at 1100 ℃ for 1000 h, the α-(W, Mo phases transformed gradually into bigger and harder M6C carbide, which results in decreasing of stress-rupture properties of the alloy. Finally, the alloy with an addition of 14W-1Mo(wt% maintained the longest stress lives at high temperatures and therefore it revealed the best microstructure stability after 1100 ℃/1000 h thermal exposure. Keywords: Superalloy, Tungsten and molybdenum, Cast, Microstructure, Stress-rupture properties

  2. Low cycle fatigue and creep-fatigue interaction behavior of nickel-base superalloy GH4169 at elevated temperature of 650 °C

    Energy Technology Data Exchange (ETDEWEB)

    Chen, G., E-mail: agang@tju.edu.cn [School of Chemical Engineering and Technology, Tianjin University, Tianjin 300072 (China); Zhang, Y. [School of Chemical Engineering and Technology, Tianjin University, Tianjin 300072 (China); Xu, D.K. [Environmental Corrosion Center, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China); Lin, Y.C. [School of Mechanical and Electrical Engineering, Central South University, Changsha 410083 (China); Chen, X. [School of Chemical Engineering and Technology, Tianjin University, Tianjin 300072 (China)

    2016-02-08

    Total strain-controlled low cycle fatigue (LCF) tests of a nickel based superalloy were performed at 650 °C. Various hold times were introduced at the peak tensile strain to investigate the high-temperature creep-fatigue interaction (CFI) effects under the same temperature. A substantial decrease in fatigue life occurred as the total strain amplitude increased. Moreover, tensile strain holding further reduced fatigue life. The saturation phenomenon of holding effect was found when the holding period reached 120 s. Cyclic softening occurred during the LCF and CFI process and it was related to the total strain amplitude and the holding period. The relationship between life-time and total strain amplitude was obtained by combining Basquin equation and Coffin-Manson equation. The surface and fracture section of the fatigued specimens were observed via scanning electronic microscope (SEM) to determine the failure mechanism.

  3. 3D DDD modelling of dislocation-precipitate interaction in a nickel-based single crystal superalloy under cyclic deformation

    Science.gov (United States)

    Lin, Bing; Huang, Minsheng; Zhao, Liguo; Roy, Anish; Silberschmidt, Vadim; Barnard, Nick; Whittaker, Mark; McColvin, Gordon

    2018-06-01

    Strain-controlled cyclic deformation of a nickel-based single crystal superalloy has been modelled using three-dimensional (3D) discrete dislocation dynamics (DDD) for both [0 0 1] and [1 1 1] orientations. The work focused on the interaction between dislocations and precipitates during cyclic plastic deformation at elevated temperature, which has not been well studied yet. A representative volume element with cubic γ‧-precipitates was chosen to represent the material, with enforced periodical boundary conditions. In particular, cutting of superdislocations into precipitates was simulated by a back-force method. The global cyclic stress-strain responses were captured well by the DDD model when compared to experimental data, particularly the effects of crystallographic orientation. Dislocation evolution showed that considerably high density of dislocations was produced for [1 1 1] orientation when compared to [0 0 1] orientation. Cutting of dislocations into the precipitates had a significant effect on the plastic deformation, leading to material softening. Contour plots of in-plane shear strain proved the development of heterogeneous strain field, resulting in the formation of shear-band embryos.

  4. Superalloys. Volume 2. 1977-February 1978 (citations from the NTIS data base). Report for 1977--Feb 78

    International Nuclear Information System (INIS)

    Smith, M.F.

    1978-03-01

    Federally-funded research on cobalt- and nickel-based superalloys is cited. Casting and powder metallurgy of these alloys are covered. Properties such as heat resistance, corrosion resistance, microstructure, fracture, and creep are described. The use of these materials in nuclear reactors, gas turbine parts, and high-temperature equipment is a major part of this compilation

  5. Development of advanced P/M Ni-base superalloys for turbine disks

    Directory of Open Access Journals (Sweden)

    Garibov Genrikh S.

    2014-01-01

    Full Text Available In the process of evolution of powder metallurgy in Russia the task permanently formulated was the following: to improve strength properties of P/M superalloys without application of additional complex HIPed blanks deformation operation. On the other hand development of a turbine disk material structure to ensure an improvement in aircraft engine performance requires the use of special HIP and heat treatment conditions. To ensure maximum strength properties of disk materials it is necessary to form a structure which would have optimum size of solid solution grains, γ′-phases and carbides. Along with that heating of the material up to a temperature determined by solvus of an alloy ensures a stable and reproducible level of mechanical properties of the disks. The above-said can be illustrated by successful mastering of new complex-alloyed VVP-class superalloys with the use of powder size − 100 μm. Application of special HIP and heat treatment conditions for these superalloys to obtain the desired grain size and the strengthening γ′-phase precipitates allowed a noticeable improvement in ultimate tensile strength and yield strength up to ≥1600 MPa and ≥1200 MPa respectively. 100 hrs rupture strength at 650 ∘C and 750 ∘C was improved up to 1140 MPa and 750 MPa respectively. P/M VVP nickel-base superalloys offer higher characteristics in comparison with many superalloys designed for the same purposes. HIPed disc compacts manufactured from PREP-powder have a homogeneous micro- and macrostructure, a stable level of mechanical properties.

  6. Cold Spray Deposition of Freestanding Inconel Samples and Comparative Analysis with Selective Laser Melting

    Science.gov (United States)

    Bagherifard, Sara; Roscioli, Gianluca; Zuccoli, Maria Vittoria; Hadi, Mehdi; D'Elia, Gaetano; Demir, Ali Gökhan; Previtali, Barbara; Kondás, Ján; Guagliano, Mario

    2017-10-01

    Cold spray offers the possibility of obtaining almost zero-porosity buildups with no theoretical limit to the thickness. Moreover, cold spray can eliminate particle melting, evaporation, crystallization, grain growth, unwanted oxidation, undesirable phases and thermally induced tensile residual stresses. Such characteristics can boost its potential to be used as an additive manufacturing technique. Indeed, deposition via cold spray is recently finding its path toward fabrication of freeform components since it can address the common challenges of powder-bed additive manufacturing techniques including major size constraints, deposition rate limitations and high process temperature. Herein, we prepared nickel-based superalloy Inconel 718 samples with cold spray technique and compared them with similar samples fabricated by selective laser melting method. The samples fabricated using both methods were characterized in terms of mechanical strength, microstructural and porosity characteristics, Vickers microhardness and residual stresses distribution. Different heat treatment cycles were applied to the cold-sprayed samples in order to enhance their mechanical characteristics. The obtained data confirm that cold spray technique can be used as a complementary additive manufacturing method for fabrication of high-quality freestanding components where higher deposition rate, larger final size and lower fabrication temperatures are desired.

  7. Microstructure and oxidation behaviour of aluminized coating of inconel 625

    International Nuclear Information System (INIS)

    Khalid, F.A.; Hussain, N.; Shahid, K.A.; Rehman, S.; Qureshi, A.H.; Khan, I.H.

    1999-01-01

    Microstructural and oxidation characteristics of aluminized coated Inconel 625 have been examined using scanning electron microscopy (SEM) and fine-probe spot and linescan EDS microanalysis techniques. The formation of slowly growing adherent metallic coatings is essential for protection against the severe environments. Aluminising of the superalloy samples was carried out by pack cementation process at 900 deg. C. in an argon atmosphere. The samples were subsequently oxidized in air at various temperatures to examine performance of the pack aluminized coated alloy. The microstructural changes that occurred in the aluminized layer at various exposure temperature and time were examined to study the oxidation behavior and formation of different phases in the aluminized coating deposited on Inconel 625. (author)

  8. Effects of cobalt on creep rupture properties and dislocation structures in nickel base superalloys

    International Nuclear Information System (INIS)

    Wang, W.Z.; Jin, T.; Jia, J.H.; Liu, J.L.; Hu, Z.Q.

    2015-01-01

    The influences of cobalt (Co) on creep rupture lives and dislocation structures in nickel base superalloys with and without rhenium (Re) are investigated. The creep rupture test conditions were high temperature low stress (1100 °C/150 MPa), intermediate temperature and stress (982 °C, 1010 °C) and low temperature high stress (850 °C/586 MPa). The results show that increasing Co content could enhance the creep rupture lives at low and intermediate temperature, and does not degrade the creep rupture lives of alloys at high temperature. In Re-containing alloys, at high temperature low stress (1100 °C/150 MPa), the effects of Co on the dislocation structures are negligible, while at low temperature high stress (850 °C/586 MPa), stacking faults are generated in alloy with 12% Co, and in alloy with 3% Co and free of Co, gamma prime particles are sheared by dislocation pairs. In Re-free alloys, at intermediate temperature and stress (1010 °C/248 MPa), large quantities of stacking faults appear in alloy without Co, while in alloy having 12% Co, gamma prime particles are sheared by dislocation pairs coupled by anti-phase boundary (APB). The gamma prime sheared by stacking faults or by dislocation pairs coupled by APB depends on the competition of stacking faults energy and APB energy which is affected by temperature and the interaction of Re and Co

  9. A Study on Ultrasonic Elliptical Vibration Cutting of Inconel 718

    Directory of Open Access Journals (Sweden)

    Zhao Haidong

    2016-01-01

    Full Text Available Inconel 718 is a kind of nickel-based alloys that are widely used in the aerospace and nuclear industry owing to their high temperature mechanical properties. Cutting of Inconel 718 in conventional cutting (CC is a big challenge in modern industry. Few researches have been studied on cutting of Inconel 718 using single point diamond tool applying the UEVC method. This paper shows an experimental study on UEVC of Inconel 718 by using polycrystalline diamond (PCD coated tools. Firstly, cutting tests have been carried out to study the effect of machining parameters in the UEVC in terms of surface finish and flank wear during machining of Inconel 718. The tests have clearly shown that the PCD coated tools in cutting of Inconel 718 by the UEVC have better performance at 0.1 mm depth of cut as compared to the lower 0.05 mm depth of cut and the higher 0.12 or 0.15 mm depth of cut. Secondly, like CC method, the cutting performance in UEVC increases with the decrease of the feed rate and cutting speed. The CC tests have also been carried out to compare performance of CC with UEVC method.

  10. Fatigue studies of superalloys in Japan

    International Nuclear Information System (INIS)

    Kitagawa, Masaki

    1985-01-01

    In the past 15 years, several national projects were advanced to develop high temperature machinery, such as high temperature gas-cooled reactors, gas turbines and fusion reactors. Before, the studies on the strength of superalloys were rarely carried out, however, by the above research works, superalloys are in rapid progress. Because these machinery are subjected to temperature cycles and vibration stress, the fatigue failure is the main concern in the safety analysis of the components. The purpose of this paper is to summarize the present status of the fatigue research on the alloys for high temperature use in Japan. The superalloys used for gas turbine and HTGR components are listed, and the materials tested were mostly the alloys of nickel base, cobalt base or iron base. In the above national projects, the main purpose was to clarify the high temperature properties including fatigue properties, to develop the method of forecasting the life span and to develop better materials. As the topics about the fatigue research on superalloys, the development of the method for forecasting the life span, the effect of directional solidification, coating and HIP process on the fatigue strength of gas turbine materials, the effect of helium and aging on the fatigue strength of HTGR materials, the fatigue strength of weldment of HTGR materials and others are reported. (Kako, I.)

  11. Multiscale modelling of single crystal superalloys for gas turbine blades

    NARCIS (Netherlands)

    Tinga, T.

    2009-01-01

    Gas turbines are extensively used for power generation and for the propulsion of aircraft and vessels. Their most severely loaded parts, the turbine rotor blades, are manufactured from single crystal nickel-base superalloys. The superior high temperature behaviour of these materials is attributed to

  12. Oxygen-induced intergranular fracture of the nickel-base alloy IN718 during mechanical loading at high temperatures

    Directory of Open Access Journals (Sweden)

    Krupp Ulrich

    2004-01-01

    Full Text Available There is a transition in the mechanical-failure behavior of nickel-base superalloys from ductile transgranular crack propagation to time-dependent intergranular fracture when the temperature exceeds about 600 °C. This transition is due to oxygen diffusion into the stress field ahead of the crack tip sufficient to cause brittle decohesion of the grain boundaries. Since very high cracking rates were observed during fixed-displacement loading of IN718, it is not very likely that grain boundary oxidation governs the grain-boundary-separation process, as has been proposed in several studies on the fatigue-damage behavior of the nickel-base superalloy IN718. Further studies on bicrystal and thermomechanically processed specimens of IN718 have shown that this kind of brittle fracture, which has been termed "dynamic embrittlement", depends strongly on the structure of the grain boundaries.

  13. The sectional size effect on the deformation behaviour of Inconel 718 at different temperatures

    Directory of Open Access Journals (Sweden)

    Zhao R.

    2015-01-01

    Full Text Available Inconel 718, as a multiphase super-alloy, is widely used in aeronautics and astronautics industries. In this field, a modified Hall-Petch equation was used to describe the grain size effect on the deformation behaviour of Inconel 718 sheet in uniaxial tension test. There is a piecewise linearity in the σ-d−1 curve: With the thickness t is a constant, the slope changes obviously after a critical t/d ratio, which increases with strain. Moreover, the influence on sectional curve caused by temperature is also an interesting issue. To address that, the sectionalized curve was fitted at different strains and temperatures, and the phenomena of grain size effect in piecewise curve at different temperatures were further explained. A surface model of Inconel 718 was proposed to explain the intrinsic mechanism of different slopes. The research provided an in-depth understanding of the size effect on the deformation behaviour of Inconel 718 at different hot working temperatures.

  14. Computational and Experimental Design of Fe-Based Superalloys for Elevated-Temperature Applications

    Energy Technology Data Exchange (ETDEWEB)

    Liaw, Peter K. [Univ. of Tennessee, Knoxville, TN (United States); Fine, Morris E. [Northwestern Univ., Evanston, IL (United States); Ghosh, Gautam [Northwestern Univ., Evanston, IL (United States); Asta, Mark D. [Univ. of California, Berkeley, CA (United States); Liu, Chain T. [Auburn Univ., AL (United States); Sun, Zhiqian [Univ. of Tennessee, Knoxville, TN (United States); Huang, Shenyan [Univ. of Tennessee, Knoxville, TN (United States); Teng, Zhenke [Univ. of Tennessee, Knoxville, TN (United States); Wang, Gongyao [Univ. of Tennessee, Knoxville, TN (United States)

    2012-04-13

    Analogous to nickel-based superalloys, Fe-based superalloys, which are strengthened by coherent B2- type precipitates are proposed for elevated-temperature applications. During the period of this project, a series of ferritic superalloys have been designed and fabricated by methods of vacuum-arc melting and vacuum-induction melting. Nano-scale precipitates were characterized by atom-probe tomography, ultrasmall- angle X-ray scattering, and transmission-electron microscopy. A duplex distribution of precipitates was found. It seems that ferritic superalloys are susceptible to brittle fracture. Systematic endeavors have been devoted to understanding and resolving the problem. Factors, such as hot rolling, precipitate volume fractions, alloy compositions, precipitate sizes and inter-particle spacings, and hyperfine cooling precipitates, have been investigated. In order to understand the underlying relationship between the microstructure and creep behavior of ferric alloys at elevated temperatures, in-situ neutron studies have been carried out. Based on the current result, it seems that the major role of β' with a 16%-volume fraction in strengthening ferritic alloys is not load sharing but interactions with dislocations. The oxidation behavior of one ferritic alloy, FBB8 (Fe-6.5Al-10Ni-10Cr-3.4Mo-0.25Zr-0.005B, weight percent), was studied in dry air. It is found that it possesses superior oxidation resistance at 1,023 and 1,123 K, compared with other creep-resistant ferritic steels [T91 (modified 9Cr-1Mo, weight percent) and P92 (9Cr-1.8W-0.5Mo, weight percent)]. At the same time, the calculation of the interfacial energies between the -iron and B2-type intermetallics (CoAl, FeAl, and NiAl) has been conducted.

  15. Microstructure of selective laser melted CM247LC nickel-based superalloy and its evolution through heat treatment

    International Nuclear Information System (INIS)

    Divya, V.D.; Muñoz-Moreno, R.; Messé, O.M.D.M.; Barnard, J.S.; Baker, S.; Illston, T.; Stone, H.J.

    2016-01-01

    The selective laser melting of high temperature alloys is of great interest to the aerospace industry as it offers the prospect of producing more complex geometries than can be achieved with other manufacturing methods. In this study, the microstructure of the nickel-based superalloy, CM247LC, has been characterised following selective laser melting and after a post deposition heat treatment below the γ′ solvus temperature. In the as-deposited state, scanning electron microscopy with electron backscatter diffraction revealed a fine, cellular microstructure with preferential alignment of 〈001〉 along the build direction. A high dislocation density was seen at the periphery of the cells, indicating substantial localised deformation of the material. Fine primary MC carbides were also observed in the inter-cellular regions. High-resolution transmission electron microscopy identified the occurrence of very fine γ′ precipitates, approximately 5 nm in diameter, dispersed within the gamma phase. After heat treatment, the elongated cell colonies were observed to partially coalesce, accompanied by a decrease in dislocation density, producing columnar grains along the build direction. Cuboidal γ′ precipitates approximately 500 nm in diameter were observed to form in the recrystallised grains, accompanied by larger γ′ precipitates on the grain boundaries.

  16. Microstructure of selective laser melted CM247LC nickel-based superalloy and its evolution through heat treatment

    Energy Technology Data Exchange (ETDEWEB)

    Divya, V.D., E-mail: dv272@cam.ac.uk [Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge CB3 0FS (United Kingdom); Muñoz-Moreno, R.; Messé, O.M.D.M.; Barnard, J.S. [Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge CB3 0FS (United Kingdom); Baker, S.; Illston, T. [Materials Solutions, Unit 8, Great Western Business Park, McKenzie Way, Worcester WR4 9GN (United Kingdom); Stone, H.J. [Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge CB3 0FS (United Kingdom)

    2016-04-15

    The selective laser melting of high temperature alloys is of great interest to the aerospace industry as it offers the prospect of producing more complex geometries than can be achieved with other manufacturing methods. In this study, the microstructure of the nickel-based superalloy, CM247LC, has been characterised following selective laser melting and after a post deposition heat treatment below the γ′ solvus temperature. In the as-deposited state, scanning electron microscopy with electron backscatter diffraction revealed a fine, cellular microstructure with preferential alignment of 〈001〉 along the build direction. A high dislocation density was seen at the periphery of the cells, indicating substantial localised deformation of the material. Fine primary MC carbides were also observed in the inter-cellular regions. High-resolution transmission electron microscopy identified the occurrence of very fine γ′ precipitates, approximately 5 nm in diameter, dispersed within the gamma phase. After heat treatment, the elongated cell colonies were observed to partially coalesce, accompanied by a decrease in dislocation density, producing columnar grains along the build direction. Cuboidal γ′ precipitates approximately 500 nm in diameter were observed to form in the recrystallised grains, accompanied by larger γ′ precipitates on the grain boundaries.

  17. The effect of strain distribution on microstructural developments during forging in a newly developed nickel base superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Buckingham, R.C. [Institute of Structural Materials, Swansea University, Bay Campus, Fabian Way, Swansea SA1 8EN (United Kingdom); Argyrakis, C.; Hardy, M.C. [Rolls-Royce plc, PO Box 31, Derby DE24 8BJ (United Kingdom); Birosca, S., E-mail: 522042@swansea.ac.uk [Institute of Structural Materials, Swansea University, Bay Campus, Fabian Way, Swansea SA1 8EN (United Kingdom)

    2016-01-27

    In the current study, the effect of strain distribution in a simple forging geometry on the propensity for recrystallization, and its impact on mechanical properties has been investigated in a newly developed experimental nickel-based superalloy. The new alloy was produced via a Powder Metallurgy (PM) route and was subsequently Hot Isostatic Processed (HIP), isothermally forged, and heat treated to produce a coarse grain microstructure with average grain size of 23–32 μm. The alloy was examined by means of Electron Back-Scatter Diffraction (EBSD) to characterise the microstructural features such as grain orientation and morphology, grain boundary characteristics and the identification of potential Prior Particle Boundaries (PPBs) throughout each stage of the processing route. Results at the central region of the cross-section plane parallel to the loading direction showed significant microstructural differences across the forging depth. This microstructural variation was found to be highly dependent on the value of local strain imparted during forging such that areas of low effective strain showed partial recrystallisation and a necklace grain structure was observed following heat treatment. Meanwhile, a fully recrystallised microstructure with no PPBs was observed in the areas of high strain values, in the central region of the forging.

  18. Strain Amount Dependent Grain Size and Orientation Developments during Hot Compression of a Polycrystalline Nickel Based Superalloy

    Directory of Open Access Journals (Sweden)

    Guoai He

    2017-02-01

    Full Text Available Controlling grain size in polycrystalline nickel base superalloy is vital for obtaining required mechanical properties. Typically, a uniform and fine grain size is required throughout forging process to realize the superplastic deformation. Strain amount occupied a dominant position in manipulating the dynamic recrystallization (DRX process and regulating the grain size of the alloy during hot forging. In this article, the high-throughput double cone specimen was introduced to yield wide-range strain in a single sample. Continuous variations of effective strain ranging from 0.23 to 1.65 across the whole sample were achieved after reaching a height reduction of 70%. Grain size is measured to be decreased from the edge to the center of specimen with increase of effective strain. Small misorientation tended to generate near the grain boundaries, which was manifested as piled-up dislocation in micromechanics. After the dislocation density reached a critical value, DRX progress would be initiated at higher deformation region, leading to the refinement of grain size. During this process, the transformations from low angle grain boundaries (LAGBs to high angle grain boundaries (HAGBs and from subgrains to DRX grains are found to occur. After the accomplishment of DRX progress, the neonatal grains are presented as having similar orientation inside the grain boundary.

  19. Bending of pipes with inconel cladding; Curvamento de tubos revestidos com inconel

    Energy Technology Data Exchange (ETDEWEB)

    Nachpitz, Leonardo; Menezes, Carlos Eduardo B; Vieira, Carlos R. Tavares [PROTUBO, Macae, RJ (Brazil)

    2008-07-01

    The pipes used in offshore equipment, such as wet Christmas trees, sub sea manifolds and rigid platform risers, as well as some pipes for refineries and ships, must have mechanical resistance to high pressure and also be resistant to corrosion from acids. Some special materials, such as stainless steel, duplex and super duplex steel are used to resolve this problem, but the cost is very high. Besides the problem of cost, these materials have other drawbacks, such as the difficulty of welding them, a technology mastered in few countries. As a better alternative, the use has been increasing of carbon steel and API pipes coated internally with inconel by welding deposition. This groundbreaking technology, of proven efficiency, has a far superior cost-benefit relation. Carbon steel and API pipes, besides having better mechanical resistance to high pressure and corrosion resistance, can be fabricated with technology mastered worldwide. Nickel alloys, such as inconel, are highly resistant to corrosion and temperature, and in these aspects are better than stainless steels. The pipes for transportation equipment and for refining hydrocarbons, as mentioned above, require various turns and special geometries, which generally are solved by the use of bends and spools made by high-frequency induction. This technology, already well established for various carbon and stainless steels, was developed to work with pipes coated internally with inconel (inconel cladding). Therefore, our work describes the process of fabricating bends from API steel pipes with inconel cladding, demonstrating the efficacy of this technology along with its quality gains and cost reduction. (author)

  20. Effects of Stress Ratio and Microstructure on Fatigue Failure Behavior of Polycrystalline Nickel Superalloy

    Science.gov (United States)

    Zhang, H.; Guan, Z. W.; Wang, Q. Y.; Liu, Y. J.; Li, J. K.

    2018-05-01

    The effects of microstructure and stress ratio on high cycle fatigue of nickel superalloy Nimonic 80A were investigated. The stress ratios of 0.1, 0.5 and 0.8 were chosen to perform fatigue tests in a frequency of 110 Hz. Cleavage failure was observed, and three competing failure crack initiation modes were discovered by a scanning electron microscope, which were classified as surface without facets, surface with facets and subsurface with facets. With increasing the stress ratio from 0.1 to 0.8, the occurrence probability of surface and subsurface with facets also increased and reached the maximum value at R = 0.5, meanwhile the probability of surface initiation without facets decreased. The effect of microstructure on the fatigue fracture behavior at different stress ratios was also observed and discussed. Based on the Goodman diagram, it was concluded that the fatigue strength of 50% probability of failure at R = 0.1, 0.5 and 0.8 is lower than the modified Goodman line.

  1. Evaluation of the Low Heat Input Process for Weld Repair of Nickel-Base Superalloys

    Science.gov (United States)

    Durocher, J.; Richards, N. L.

    2011-10-01

    The repair of turbine blades and vanes commonly involves gas tungsten arc welding or an equivalent process, but unfortunately these components are often susceptible to heat-affected zone (HAZ) cracking during the weld repair process. This is a major problem especially in cast alloys due to their coarse-grain size and where the (Al + Ti) contents is in excess of 3-4%; vacuum brazing is also used but mainly on low stress non-rotating components such as vanes. Micro-welding has the potential to deposit small amounts of filler at low heat input levels with minimum HAZ and thus is an attractive process for depositing a quality weld. As with conventional fusion processes, the filler alloy is deposited by the generation of a low power arc between a consumable electrode and the substrate. The low heat input of this process offers unique advantages over more common welding processes such as gas tungsten arc, plasma arc, laser, and electron beam welding. In this study, the low heat input characteristic of micro-welding has been used to simulate weld repair using Inconel (IN) (Inconel and IN are trademarks of INCO Alloys International) 625, Rene (Rene is a trademark of General Electric Company) 41, Nimonic (Nimonic is a trademark of INCO Alloys International) 105 and Inconel 738LC filler alloys, to a cast Inconel 738LC substrate. The effect of micro-welding process parameters on the deposition rate, coating quality, and substrate has been investigated.

  2. Inconel 939 processed by selective laser melting: Effect of microstructure and temperature on the mechanical properties under static and cyclic loading

    Energy Technology Data Exchange (ETDEWEB)

    Kanagarajah, P., E-mail: p.kanagarajah@uni-paderborn.de [Lehrstuhl für Werkstoffkunde (Materials Science), University of Paderborn, Pohlweg 47-49, 33098 Paderborn (Germany); Brenne, F. [Lehrstuhl für Werkstoffkunde (Materials Science), University of Paderborn, Pohlweg 47-49, 33098 Paderborn (Germany); Direct Manufacturing Research Center (DMRC), Mersinweg 3, 33098 Paderborn (Germany); Niendorf, T. [Lehrstuhl für Werkstoffkunde (Materials Science), University of Paderborn, Pohlweg 47-49, 33098 Paderborn (Germany); Maier, H.J. [Direct Manufacturing Research Center (DMRC), Mersinweg 3, 33098 Paderborn (Germany); Institut für Werkstoffkunde, Leibniz Universität Hannover, An der Universität 2, 30823 Garbsen (Germany)

    2013-12-20

    Nickel-based superalloys, such as Inconel 939, are a long-established construction material for high-temperature applications and profound knowledge of the mechanical properties for this alloy produced by conventional techniques exists. However, many applications demand for highly complex geometries, e.g. in order to optimize the cooling capability of thermally loaded parts. Thus, additive manufacturing (AM) techniques have recently attracted substantial interest as they provide for an increased freedom of design. However, the microstructural features after AM processing are different from those after conventional processing. Thus, further research is vital for understanding the microstructure-processing relationship and its impact on the resulting mechanical properties. The aim of the present study was to investigate Inconel 939 processed by selective laser melting (SLM) and to reveal the differences to the conventional cast alloy. Thorough examinations were conducted using electron backscatter diffraction, transmission electron microscopy, optical microscopy and mechanical testing. It is demonstrated that the microstructure of the SLM-material is highly influenced by the heat flux during layer-wise manufacturing and consequently anisotropic microstructural features prevail. An epitaxial grain growth accounts for strong bonding between the single layers resulting in good mechanical properties already in the as-built condition. A heat treatment following SLM leads to microstructural features different to those obtained after the same heat treatment of the cast alloy. Still, the mechanical performance of the latter is met underlining the potential of this technique for producing complex parts for high temperature applications.

  3. Effect of microstructure on high-temperature mechanical behavior of nickel-base superalloys for turbine disc applications

    Science.gov (United States)

    Sharpe, Heather Joan

    2007-05-01

    Engineers constantly seek advancements in the performance of aircraft and power generation engines, including, lower costs and emissions, and improved fuel efficiency. Nickel-base superalloys are the material of choice for turbine discs, which experience some of the highest temperatures and stresses in the engine. Engine performance is proportional to operating temperatures. Consequently, the high-temperature capabilities of disc materials limit the performance of gas-turbine engines. Therefore, any improvements to engine performance necessitate improved alloy performance. In order to take advantage of improvements in high-temperature capabilities through tailoring of alloy microstructure, the overall objectives of this work were to establish relationships between alloy processing and microstructure, and between microstructure and mechanical properties. In addition, the projected aimed to demonstrate the applicability of neural network modeling to the field of Ni-base disc alloy development and behavior. The first phase of this work addressed the issue of how microstructure varies with heat treatment and by what mechanisms these structures are formed. Further it considered how superalloy composition could account for microstructural variations from the same heat treatment. To study this, four next-generation Ni-base disc alloys were subjected to various controlled heat-treatments and the resulting microstructures were then quantified. These quantitative results were correlated to chemistry and processing, including solution temperature, cooling rate, and intermediate hold temperature. A complex interaction of processing steps and chemistry was found to contribute to all features measured; grain size, precipitate distribution, grain boundary serrations. Solution temperature, above a certain threshold, and cooling rate controlled grain size, while cooling rate and intermediate hold temperature controlled precipitate formation and grain boundary serrations. Diffusion

  4. High temperature corrosion of nickel-base alloys in environments containing alkali sulphate

    Energy Technology Data Exchange (ETDEWEB)

    Pettersson, Rachel; Flyg, Jesper; Caddeo, Sophie [Corrosion and Metals Research Institute, KIMAB, Stockholm (Sweden); Karlsson, Fredrik [Siemens Industrial Turbomachinery, Finspong (Sweden)

    2007-02-15

    This work is directed towards producing data to assist in lifetime assessment of components in gas turbines run in severely polluted industrial environments where the main corrosive species is SO{sub 2}, which can condense to form alkali sulphates. Corrosion rates have been measured for the base materials, in order to assess the worst-case scenario, in which cracks or other damage has occurred to the protective coating. The information is expected to be of value to manufacturers, owners and inspectors of gas turbines. Six nickel-base superalloys were subject to thermal cycles of 160 hours duration, and 0.8mg/cm{sup 2} of 20 mol % Na{sub 2}SO{sub 4} + 80mol% K{sub 2}SO{sub 4} was applied before each cycle. The test temperatures were 850 deg C and 900 deg C, with maximum test durations of 24 cycles and 12 cycles respectively. The metal loss was assessed by metallography of cross sections and the sulphidation attack was found to be very uneven. Mass change data indicated that the corrosion process was largely linear in character, and probability plots and estimations of the propagation rate of corrosion based on the linear growth assumption were produced. The performance of the alloys increased with increasing chromium content. The single crystal materials CMSX4 and MD2 showed such high corrosion rates that their use in severely contaminated industrial environments is considered inadvisable. The best performance was shown by Inconel 939 and Inconel 6203, so that even if cracks occur in the protective coating, a reasonable remaining lifetime can be expected for these materials. Sulphide formation occurred at the reaction front in all cases and mixed sulphides such as Ta-Ni or Ti-Nb sulphides were often present. The work has news value since very little long-term data is currently available for materials performance in severely sulphidising environments. The project goals in terms of exposures and metrology have been fully realised. Contributions have been made to the

  5. Fabrication of tungsten wire reinforced nickel-base alloy composites

    Science.gov (United States)

    Brentnall, W. D.; Toth, I. J.

    1974-01-01

    Fabrication methods for tungsten fiber reinforced nickel-base superalloy composites were investigated. Three matrix alloys in pre-alloyed powder or rolled sheet form were evaluated in terms of fabricability into composite monotape and multi-ply forms. The utility of monotapes for fabricating more complex shapes was demonstrated. Preliminary 1093C (2000F) stress rupture tests indicated that efficient utilization of fiber strength was achieved in composites fabricated by diffusion bonding processes. The fabrication of thermal fatigue specimens is also described.

  6. Low-Cobalt Powder-Metallurgy Superalloy

    Science.gov (United States)

    Harf, F. H.

    1986-01-01

    Highly-stressed jet-engine parts made with less cobalt. Udimet 700* (or equivalent) is common nickel-based superalloy used in hot sections of jet engines for many years. This alloy, while normally used in wrought condition, also gas-atomized into prealloyed powder-metallurgy (PM) product. Product can be consolidated by hot isostatically pressing (HIPPM condition) and formed into parts such as turbine disk. Such jet-engine disks "see" both high stresses and temperatures to 1,400 degrees F (760 degrees C).

  7. On the Feasibility of Eddy Current Characterization of the Near-Surface Residual Stress Distribution in Nickel-Base Superalloys

    International Nuclear Information System (INIS)

    Blodgett, Mark P.; Nagy, Peter B.

    2004-01-01

    In light of its frequency-dependent penetration depth, the measurement of eddy current conductivity has been suggested as a possible means to allow the nondestructive evaluation of subsurface residual stresses in shot-peened specimens. This technique is based on the so-called electroelastic effect, i.e., the stress-dependence of the electrical conductivity. Unfortunately, the relatively small (∼1%) change in electrical conductivity caused by the presence of compressive residual stresses is often distorted, or even completely overshadowed, by the accompanying conductivity loss caused by cold work and surface roughness effects. Recently, it was observed that, in contrast with most other materials, shot-peened Waspaloy and IN100 specimens exhibit an apparent increase in electrical conductivity at increasing inspection frequencies. This observation by itself indicates that in these materials the measured conductivity change is probably dominated by residual stress effects, since both surface roughness and increased dislocation density are known to decrease rather than increase the conductivity and the presence of crystallographic texture does not affect the electrical conductivity of these materials, which crystallize in cubic symmetry. Our preliminary experiments indicate that probably there exists a unique 'window of opportunity' for eddy current NDE in nickel-base superalloys. We identified five major effects that contribute to this fortunate constellation of material properties, which will be reviewed in this presentation

  8. Initial Mechanical Testing of Superalloy Lattice Block Structures Conducted

    Science.gov (United States)

    Krause, David L.; Whittenberger, J. Daniel

    2002-01-01

    The first mechanical tests of superalloy lattice block structures produced promising results for this exciting new lightweight material system. The testing was performed in-house at NASA Glenn Research Center's Structural Benchmark Test Facility, where small subelement-sized compression and beam specimens were loaded to observe elastic and plastic behavior, component strength levels, and fatigue resistance for hundreds of thousands of load cycles. Current lattice block construction produces a flat panel composed of thin ligaments arranged in a three-dimensional triangulated trusslike structure. Investment casting of lattice block panels has been developed and greatly expands opportunities for using this unique architecture in today's high-performance structures. In addition, advances made in NASA's Ultra-Efficient Engine Technology Program have extended the lattice block concept to superalloy materials. After a series of casting iterations, the nickel-based superalloy Inconel 718 (IN 718, Inco Alloys International, Inc., Huntington, WV) was successfully cast into lattice block panels; this combination offers light weight combined with high strength, high stiffness, and elevated-temperature durability. For tests to evaluate casting quality and configuration merit, small structural compression and bend test specimens were machined from the 5- by 12- by 0.5-in. panels. Linear elastic finite element analyses were completed for several specimen layouts to predict material stresses and deflections under proposed test conditions. The structural specimens were then subjected to room-temperature static and cyclic loads in Glenn's Life Prediction Branch's material test machine. Surprisingly, the test results exceeded analytical predictions: plastic strains greater than 5 percent were obtained, and fatigue lives did not depreciate relative to the base material. These assets were due to the formation of plastic hinges and the redundancies inherent in lattice block construction

  9. Metallurgical and mechanical properties of Inconel 600 and stellite; Estudio del comportamiento mecanico-metalurgico de alceacion inconel 600 y estelita

    Energy Technology Data Exchange (ETDEWEB)

    Cstillo, Martin; Villa, Gabriel; Vite, Manuel [Instituto Politecnico Nacional, Mexico D.F. (Mexico); Palacios, Francisco [Instituto Nacional de Investigacion Nuclear (ININ), Estado de Mexico (Mexico); Hernandez, Luis H; Urriolagoita, Guillermo [Instituto Politecnico Nacional, Mexico D.F. (Mexico)

    2005-01-15

    The present work studies the metallurgical and mechanical properties of two alloys, Inconel 600 and stellite, which are within the group of high hardness alloys or superalloys, which are deposited through the electrical weld process to the metallic arc with coated electrode (SMAW) and thereinafter analyzed through electron microscopy, diffractometry and abrasion, Impact and hardness test. The relationship between the microstructure and the final properties of the coating (hardness and abrasion wear resistance) was observed. [Spanish] Este trabajo presenta el estudio sobre las propiedades metalurgicas y mecanicas de dos aleaciones, inconel 600 y estelita, clasificadas dentro del grupo de aleaciones de alta dureza o superaleaciones; las cuales fueron depositadas mediante el proceso de soldadura electrica al arco metalico con electrodo revestido (SMAW) y fueron analizadas mediante microscopia electronica (SEM), difractometria pruebas de abrasion, impacto y dureza. Se observo la relacion entre la microstructura y las propiedades del recubrimiento, como son: dureza, resistencia a la abrasion, resistencia al impacto, ente otras.

  10. The Role of Cold Work in Eddy Current Residual Stress Measurements in Shot-Peened Nickel-Base Superalloys

    International Nuclear Information System (INIS)

    Yu, F.; Nagy, P. B.

    2006-01-01

    Recently, it was shown that eddy current methods can be adapted to residual stress measurement in shot-peened nickel-base superalloys. However, experimental evidence indicates that the piezoresistivity effect is simply not high enough to account for the observed apparent eddy current conductivity (AECC) increase. At the same time, X-ray diffraction data indicates that 'cold work' lingers even when the residual stress is fully relaxed and the excess AECC is completely gone. It is impossible to account for both observations with a single coherent explanation unless we assume that instead of a single 'cold work' effect, there are two varieties of cold work; type-A and type-B. Type-A cold work (e.g., changes in the microscopic homogeneity of the material) is not detected by X-ray diffraction as it does not significantly affect the beam width, but causes substantial conductivity change and exhibits strong thermal relaxation. Type-B cold work (e.g., dislocations) is detected by X-ray, but causes little or no conductivity change and exhibits weak thermal relaxation. Based on the assumption of two separate cold-work variables and that X-ray diffraction results indicate the presence of type-B, but not type-A, all observed phenomena can be explained. If this working hypothesis is proven right, the separation of residual stress and type-A cold work is less critical because they both relax much earlier and much faster than type-B cold work

  11. The effect of deformation temperature on the microstructure evolution of Inconel 625 superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Guo Qingmiao [General Research Institute for Non-Ferrous Metals, Beijing 100088 (China); Li Defu, E-mail: lide_fu@163.com [General Research Institute for Non-Ferrous Metals, Beijing 100088 (China); Guo Shengli; Peng Haijian; Hu Jie [General Research Institute for Non-Ferrous Metals, Beijing 100088 (China)

    2011-07-31

    Highlights: > The relationship between the stable DRX grain size and peak stress can be expressed by a power law function. > Deformation temperature has a significant influence on the nucleation mechanisms of DRX at different deformation stages. > With increasing the deformation temperature, the effect of DDRX accompanied with twinning formation grows stronger, while the effect of CDRX grows weaker. -- Abstract: Hot compression tests of Inconel 625 superalloy were conducted using a Gleeble-1500 simulator between 900 deg. C and 1200 deg. C with different true strains and a strain rate of 0.1 s{sup -1}. Scanning electron microscope (SEM) and electron backscatter diffraction technique (EBSD) were employed to investigate the effect of deformation temperature on the microstructure evolution and nucleation mechanisms of dynamic recrystallization (DRX). It is found that the relationship between the DRX grain size and the peak stress can be expressed by a power law function. Significant influence of deformation temperatures on the nucleation mechanisms of DRX are observed at different deformation stages. At lower deformation temperatures, continuous dynamic recrystallization (CDRX) characterized by progressive subgrain rotation is considered as the main mechanism of DRX at the early deformation stage. However, discontinuous dynamic recrystallization (DDRX) with bulging of the original grain boundaries becomes the operating mechanism of DRX at the later deformation stage. At higher deformation temperatures, DDRX is the primary mechanism of DRX, while CDRX can only be considered as an assistant mechanism at the early deformation stage. Nucleation of DRX can also be activated by the twinning formation. With increasing the deformation temperature, the effect of DDRX accompanied with twinning formation grows stronger, while the effect of CDRX grows weaker. Meanwhile, the position of subgrain formation shifts gradually from the interior of original grains to the vicinity of the

  12. Increasing the Useful Life of Quench Reliefs with Inconel Bellows

    Energy Technology Data Exchange (ETDEWEB)

    Soyars, W. M. [Fermilab

    1999-01-01

    Reliable quench relief valves are an important part of superconducting magnet systems. Fermilab developed bellows-actuated cryogenic quench reliefs which have been in use since the early l 980's. The original design uses a stainless steel bellows. A high frequency, low amplitude vibration during relieving events has resulted in fatigue failures in the original design. To take advantage of the improved resistance to fatigue of Inconel, a nickel-chromium alloy, reliefs using Inconel 625 bellows were made. Design, development, and testing of the new version reliefs will be discussed. Tests show that relief valve lifetimes using Inconel bellows are more than five times greater than when using the original stainless steel bellows. Inconel bellows show great promise in increasing the lifetime of quench relief valves, and thus the reliability of accelerator cryogenic systems.

  13. Nano-scale characterization of white layer in broached Inconel 718

    Energy Technology Data Exchange (ETDEWEB)

    Chen, Zhe, E-mail: zhe.chen@liu.se [Division of Engineering Materials, Linköping University, 58183 Linköping (Sweden); Colliander, Magnus Hörnqvist; Sundell, Gustav [Department of Physics, Chalmers University of Technology, 41296 Gothenburg (Sweden); Peng, Ru Lin [Division of Engineering Materials, Linköping University, 58183 Linköping (Sweden); Zhou, Jinming [Division of Production and Materials Engineering, Lund University, 22100 Lund (Sweden); Johansson, Sten; Moverare, Johan [Division of Engineering Materials, Linköping University, 58183 Linköping (Sweden)

    2017-01-27

    The formation mechanism of white layers during broaching and their mechanical properties are not well investigated and understood to date. In the present study, multiple advanced characterization techniques with nano-scale resolution, including transmission electron microscopy (TEM), transmission Kikuchi diffraction (TKD), atom probe tomography (APT) as well as nano-indentation, have been used to systematically examine the microstructural evolution and corresponding mechanical properties of a surface white layer formed when broaching the nickel-based superalloy Inconel 718. TEM observations showed that the broached white layer consists of nano-sized grains, mostly in the range of 20–50 nm. The crystallographic texture detected by TKD further revealed that the refined microstructure is primarily caused by strong shear deformation. Co-located Al-rich and Nb-rich fine clusters have been identified by APT, which are most likely to be γ′ and γ′′ clusters in a form of co-precipitates, where the clusters showed elongated and aligned appearance associated with the severe shearing history. The microstructural characteristics and crystallography of the broached white layer suggest that it was essentially formed by adiabatic shear localization in which the dominant metallurgical process is rotational dynamic recrystallization based on mechanically-driven subgrain rotations. The grain refinement within the white layer led to an increase of the surface nano-hardness by 14% and a reduction in elastic modulus by nearly 10% compared to that of the bulk material. This is primarily due to the greatly increased volume fraction of grain boundaries, when the grain size was reduced down to the nanoscale.

  14. Experimental and modeling results of creep fatigue life of Inconel 617 and Haynes 230 at 850 C

    International Nuclear Information System (INIS)

    Chen, Xiang; Sokolov, Mikhail A.; Sham, Sam; Erdman, Donald L. III; Busby, Jeremy T.; Mo, Kun; Stubbins, James

    2013-01-01

    Creep fatigue testing of Ni-based superalloy Inconel 617 and Haynes 230 were conducted in the air at 850 C. Tests were performed with fully reversed axial strain control at a total strain range of 0.5%, 1.0% or 1.5% and hold time at maximum tensile strain for 3, 10 or 30 min. In addition, two creep fatigue life prediction methods, i.e. linear damage summation and frequency-modified tensile hysteresis energy modeling, were evaluated and compared with experimental results. Under all creep fatigue tests, Haynes 230 performed better than Inconel 617. Compared to the low cycle fatigue life, the cycles to failure for both materials decreased under creep fatigue test conditions. Longer hold time at maximum tensile strain would cause a further reduction in both material creep fatigue life. The linear damage summation could predict the creep fatigue life of Inconel 617 for limited test conditions, but considerably underestimated the creep fatigue life of Haynes 230. In contrast, frequency-modified tensile hysteresis energy modeling showed promising creep fatigue life prediction results for both materials.

  15. Hydrogen Annealing Of Single-Crystal Superalloys

    Science.gov (United States)

    Smialek, James L.; Schaeffer, John C.; Murphy, Wendy

    1995-01-01

    Annealing at temperature equal to or greater than 2,200 degrees F in atmosphere of hydrogen found to increase ability of single-crystal superalloys to resist oxidation when subsequently exposed to oxidizing atmospheres at temperatures almost as high. Supperalloys in question are principal constituents of hot-stage airfoils (blades) in aircraft and ground-based turbine engines; also used in other high-temperature applications like chemical-processing plants, coal-gasification plants, petrochemical refineries, and boilers. Hydrogen anneal provides resistance to oxidation without decreasing fatigue strength and without need for coating or reactive sulfur-gettering constituents. In comparison with coating, hydrogen annealing costs less. Benefits extend to stainless steels, nickel/chromium, and nickel-base alloys, subject to same scale-adhesion and oxidation-resistance considerations, except that scale is chromia instead of alumina.

  16. Creep and residual mechanical properties of cast superalloys and oxide dispersion strengthened alloys

    Science.gov (United States)

    Whittenberger, J. D.

    1981-01-01

    Tensile, stress-rupture, creep, and residual tensile properties after creep testing were determined for two typical cast superalloys and four advanced oxide dispersion strengthened (ODS) alloys. The superalloys examined included the nickel-base alloy B-1900 and the cobalt-base alloy MAR-M509. The nickel-base ODS MA-757 (Ni-16CR-4Al-0.6Y2O3 and the iron-base ODS alloy MA-956 (Fe-20Cr-5Al-0.8Y2O3) were extensively studied, while limited testing was conducted on the ODS nickel-base alloys STCA (Ni-16Cr-4.5Al-2Y2O3) with a without Ta and YD-NiCrAl (Ni-16Cr-5Al-2Y2O3). Elevated temperature testing was conducted from 114 to 1477 K except for STCA and YD-NiCrAl alloys, which were only tested at 1366 K. The residual tensile properties of B-1900 and MAR-M509 are not reduced by prior creep testing (strains at least up to 1 percent), while the room temperature tensile properties of ODS nickel-base alloys can be reduced by small amounts of prior creep strain (less than 0.5 percent). The iron-base ODS alloy MA-956 does not appear to be susceptible to creep degradation at least up to strains of about 0.25 percent. However, MA-956 exhibits unusual creep behavior which apparently involves crack nucleation and growth.

  17. Influence of heat treatment on microstructure and tensile behavior of a hot isostatically pressed nickel-based superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Qiu, Chunlei, E-mail: c.qiu@bham.ac.uk [School of Metallurgy and Materials, University of Birmingham, Edgbaston, Birmingham B15 2TT (United Kingdom); Wu, Xinhua; Mei, Junfa [School of Metallurgy and Materials, University of Birmingham, Edgbaston, Birmingham B15 2TT (United Kingdom); Andrews, Paul; Voice, Wayne [Rolls-Royce Plc, Derby DE24 8BJ (United Kingdom)

    2013-11-25

    Highlights: •Post-HIP heat treatment led to refined microstructure and improved tensile properties. •Deformation occurred mainly by forming stacking faults in γ′ at RT and elevated temperature. •Net-shape HIPed RR1000 failed in a transgranular fracture mode. -- Abstract: A nickel-based superalloy powder RR1000 has been hot isostatically pressed (HIPed) and heat treated to produce different microstructures. Microstructures were investigated using a scanning electron microscope (SEM). Tensile testing was performed at room temperature and 700 °C and the deformed samples were examined using SEM and transmission electron microscope (TEM). It was found that in the as-HIPed condition the microstructure consisted of coarse and irregular-shaped primary and secondary γ′ together with a low volume fraction of fine γ′ (<50 nm in diameter). Solution treatment below the γ′ solvus followed by air cooling resulted in the formation of finer cuboidal secondary γ′ (350–750 nm) and medium-sized spherical tertiary γ′ (100–200 nm). This led to an improvement of both the 0.2% yield strength and ultimate tensile strength. Ageing of the solution-treated or of the as-HIPed samples at 760 °C resulted in the precipitation of a high population of fine γ′ (around 50 nm) which further increased the strength. Within the resolution limit of the current TEM analysis, deformation at room temperature seemed to occur mainly by dislocations cutting through secondary γ′ and very fine γ′, accompanied by the formation of stacking faults within these precipitates; most of the medium-sized tertiary γ′ precipitates in solution-treated and aged samples were not cut through but were surrounded by dislocations. Deformation at 700 °C happened by dislocations cutting through γ′ precipitates and γ matrix, leading to the formation of extended stacking faults across both γ and γ′. It is suggested that the optimum treatment of the current powder superalloy is to

  18. Influence of heat treatment on microstructure and tensile behavior of a hot isostatically pressed nickel-based superalloy

    International Nuclear Information System (INIS)

    Qiu, Chunlei; Wu, Xinhua; Mei, Junfa; Andrews, Paul; Voice, Wayne

    2013-01-01

    Highlights: •Post-HIP heat treatment led to refined microstructure and improved tensile properties. •Deformation occurred mainly by forming stacking faults in γ′ at RT and elevated temperature. •Net-shape HIPed RR1000 failed in a transgranular fracture mode. -- Abstract: A nickel-based superalloy powder RR1000 has been hot isostatically pressed (HIPed) and heat treated to produce different microstructures. Microstructures were investigated using a scanning electron microscope (SEM). Tensile testing was performed at room temperature and 700 °C and the deformed samples were examined using SEM and transmission electron microscope (TEM). It was found that in the as-HIPed condition the microstructure consisted of coarse and irregular-shaped primary and secondary γ′ together with a low volume fraction of fine γ′ (<50 nm in diameter). Solution treatment below the γ′ solvus followed by air cooling resulted in the formation of finer cuboidal secondary γ′ (350–750 nm) and medium-sized spherical tertiary γ′ (100–200 nm). This led to an improvement of both the 0.2% yield strength and ultimate tensile strength. Ageing of the solution-treated or of the as-HIPed samples at 760 °C resulted in the precipitation of a high population of fine γ′ (around 50 nm) which further increased the strength. Within the resolution limit of the current TEM analysis, deformation at room temperature seemed to occur mainly by dislocations cutting through secondary γ′ and very fine γ′, accompanied by the formation of stacking faults within these precipitates; most of the medium-sized tertiary γ′ precipitates in solution-treated and aged samples were not cut through but were surrounded by dislocations. Deformation at 700 °C happened by dislocations cutting through γ′ precipitates and γ matrix, leading to the formation of extended stacking faults across both γ and γ′. It is suggested that the optimum treatment of the current powder superalloy is to

  19. Constitutive modeling of a nickel base superalloy -with a focus on gas turbine applications

    Energy Technology Data Exchange (ETDEWEB)

    Almroth, Per

    2003-05-01

    Gas turbines are used where large amounts of energy is needed, typically as engines in aircraft, ferries and power plants. From an efficiency point of view it is desirable to increase the service temperature as much as possible. One of the limiting factors is then the maximum allowable metal temperatures in the turbine stages, primarily in the blades of the first stage, that are exposed to the highest gas temperatures. Specially designed materials are used to cope with these severe conditions, such as the nickel base superalloy IN792. In order to be able to design the components for higher temperatures and tighter tolerances, a detailed understanding and computationel models of the material behaviour is needed. The models presented in this work have been developed with the objective of being physically well motivated, and with the intention of avoiding excessive numbers of parameters. The influence of the parameters should also be as easy as possible to interpret. The models are to describe the behaviour of IN792, under conditions typically found for a gas turbine blade. Specifically the high- and intermediate temperature isothermal modelling of IN792 have been addressed. One main issue when characterising the material and calibrating the models is the use of relevant tests, that are representative of component conditions. Therefore isothermal tests with an eye on the typical environment of a turbine blade have been planned and performed. Using numerical optimization techniques the material parameters for the isothermal behaviour of IN792 at 650 deg and 850 deg have been estimated. The good overall calibration results for these specific temperatures, using the presented modeling concept and nonstandard constitutive tests, suggests that the model can describe the behaviour of IN792 in gas turbine hot part applications.

  20. Creep deformation and microstructural examination of a prior thermally exposed nickel base superalloy

    Czech Academy of Sciences Publication Activity Database

    Zrník, J.; Strunz, Pavel; Vrchovinský, V.; Muránsky, O.; Horňák, P.; Wiedenmann, A.

    2004-01-01

    Roč. 274 (2004), s. 925-930 ISSN 1013-9826 R&D Projects: GA AV ČR KSK1010104 Keywords : superalloy * thermal exposition * creep Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 0.278, year: 2004

  1. A probabilistic-based approach to monitoring tool wear state and assessing its effect on workpiece quality in nickel-based alloys

    Science.gov (United States)

    Akhavan Niaki, Farbod

    The objective of this research is first to investigate the applicability and advantage of statistical state estimation methods for predicting tool wear in machining nickel-based superalloys over deterministic methods, and second to study the effects of cutting tool wear on the quality of the part. Nickel-based superalloys are among those classes of materials that are known as hard-to-machine alloys. These materials exhibit a unique combination of maintaining their strength at high temperature and have high resistance to corrosion and creep. These unique characteristics make them an ideal candidate for harsh environments like combustion chambers of gas turbines. However, the same characteristics that make nickel-based alloys suitable for aggressive conditions introduce difficulties when machining them. High strength and low thermal conductivity accelerate the cutting tool wear and increase the possibility of the in-process tool breakage. A blunt tool nominally deteriorates the surface integrity and damages quality of the machined part by inducing high tensile residual stresses, generating micro-cracks, altering the microstructure or leaving a poor roughness profile behind. As a consequence in this case, the expensive superalloy would have to be scrapped. The current dominant solution for industry is to sacrifice the productivity rate by replacing the tool in the early stages of its life or to choose conservative cutting conditions in order to lower the wear rate and preserve workpiece quality. Thus, monitoring the state of the cutting tool and estimating its effects on part quality is a critical task for increasing productivity and profitability in machining superalloys. This work aims to first introduce a probabilistic-based framework for estimating tool wear in milling and turning of superalloys and second to study the detrimental effects of functional state of the cutting tool in terms of wear and wear rate on part quality. In the milling operation, the

  2. Evaluation of Heat Capacity and Resistance to Cyclic Oxidation of Nickel Superalloys

    Directory of Open Access Journals (Sweden)

    Przeliorz R.

    2014-08-01

    Full Text Available Paper presents the results of evaluation of heat resistance and specific heat capacity of MAR-M-200, MAR-M-247 and Rene 80 nickel superalloys. Heat resistance was evaluated using cyclic method. Every cycle included heating in 1100°C for 23 hours and cooling for 1 hour in air. Microstructure of the scale was observed using electron microscope. Specific heat capacity was measured using DSC calorimeter. It was found that under conditions of cyclically changing temperature alloy MAR-M-247 exhibits highest heat resistance. Formed oxide scale is heterophasic mixture of alloying elements, under which an internal oxidation zone was present. MAR-M-200 alloy has higher specific heat capacity compared to MAR-M-247. For tested alloys in the temperature range from 550°C to 800°C precipitation processes (γ′, γ″ are probably occurring, resulting in a sudden increase in the observed heat capacity.

  3. High-temperature γ (FCC/γ′ (L12 Co-Al-W based superalloys

    Directory of Open Access Journals (Sweden)

    Knop Matthias

    2014-01-01

    Full Text Available Interim results from the development of a polycrystalline Co-Al-W based superalloy are presented. Cr has been added to provide oxidation resistance and Ni has then been added to widen and stabilise the γ′ phase field. The alloy presented has a solvus of 1010 °C and a density of 8.7 g cm−3. The room temperature flow stress is over 1000 MPa and this reduces dramatically above 800 °C. The flow stress anomaly is observed. A microstructure with both ∼ 50 nm γ′ produced on cooling and larger 100–200 nm γ′ can be obtained. Isothermal oxidation at 800 °C in air for 200 h gave a mass gain of 0.96 mg cm−2. After hot deformation in the 650–850 °C temperature range, both anti phase boundaries (APBs and stacking faults could be observed. An APB energy of 71 mJ m−2 was measured, which is comparable to that found in commercial nickel superalloys.

  4. Chatter identification in milling of Inconel 625 based on recurrence plot technique and Hilbert vibration decomposition

    Directory of Open Access Journals (Sweden)

    Lajmert Paweł

    2018-01-01

    Full Text Available In the paper a cutting stability in the milling process of nickel based alloy Inconel 625 is analysed. This problem is often considered theoretically, but the theoretical finding do not always agree with experimental results. For this reason, the paper presents different methods for instability identification during real machining process. A stability lobe diagram is created based on data obtained in impact test of an end mill. Next, the cutting tests were conducted in which the axial cutting depth of cut was gradually increased in order to find a stability limit. Finally, based on the cutting force measurements the stability estimation problem is investigated using the recurrence plot technique and Hilbert vibration decomposition method.

  5. Parametric study of development of Inconel-steel functionally graded materials by laser direct metal deposition

    International Nuclear Information System (INIS)

    Shah, Kamran; Haq, Izhar ul; Khan, Ashfaq; Shah, Shaukat Ali; Khan, Mushtaq; Pinkerton, Andrew J

    2014-01-01

    Highlights: • Functionally graded steel and nickel super-alloy structures have been developed. • Mechanical properties of FGMs can be controlled by process input parameters. • SDAS is strongly dependent on the laser power and powder mass flow rate. • Carbides provide a mechanism to control the hardness and wear resistance of FGM. • Tensile strength of FGM is dependent on the laser power and powder mass flow rate. - Abstract: Laser direct metal deposition (LDMD) has developed from a prototyping to a single and multiple metals manufacturing technique. It offers an opportunity to produce graded components, with differing elemental composition, phase and microstructure at different locations. In this work, continuously graded Stainless Steel 316L and Inconel 718 thin wall structures made by direct laser metal deposition process have been explored. The paper considers the effects of process parameters including laser power levels and powder mass flow rates of SS316L and Inconel 718 during the deposition of the Steel–Ni graded structures. Microstructure characterisation and phase identification are performed by optical microscopy and X-ray diffraction techniques. Mechanical testing, using methods such as hardness, wear resistance and tensile testing have been carried out on the structures. XRD results show the presence of the NbC and Fe 2 Nb phases formed during the deposition. The effect of experimental parameters on the microstructure and physical properties are determined and discussed. Work shows that mechanical properties can be controlled by input parameters and generation of carbides provides an opportunity to selectively control the hardness and wear resistance of the functionally graded material

  6. Novel microstructural growth in the surface of Inconel 625 by the addition of SiC under electron beam melting

    Energy Technology Data Exchange (ETDEWEB)

    Ahmad, M., E-mail: maqomer@yahoo.com [Physics Division, Pakistan Institute of Nuclear Science and Technology (PINSTECH), P.O. Nilore, Islamabad (Pakistan); Ali, G.; Ahmed, Ejaz; Haq, M.A.; Akhter, J.I. [Physics Division, Pakistan Institute of Nuclear Science and Technology (PINSTECH), P.O. Nilore, Islamabad (Pakistan)

    2011-06-15

    Electron beam melting is being used to modify the microstructure of the surfaces of materials due to its ability to cause localized melting and supercooling of the melt. This article presents an experimental study on the surface modification of Ni-based superalloy (Inconel 625) reinforced with SiC ceramic particles under electron beam melting. Scanning electron microscopy, energy dispersive spectroscopy and X-ray diffraction techniques have been applied to characterize the resulted microstructure. The results revealed growth of novel structures like wire, rod, tubular, pyramid, bamboo and tweezers type morphologies in the modified surface. In addition to that fibrous like structure was also observed. Formation of thin carbon sheet has been found at the regions of decomposed SiC. Electron beam modified surface of Inconel 625 alloy has been hardened twice as compared to the as-received samples. Surface hardening effect may be attributed to both the formation of the novel structures as well as the introduction of Si and C atom in the lattice of Inconel 625 alloy.

  7. Novel microstructural growth in the surface of Inconel 625 by the addition of SiC under electron beam melting

    Science.gov (United States)

    Ahmad, M.; Ali, G.; Ahmed, Ejaz; Haq, M. A.; Akhter, J. I.

    2011-06-01

    Electron beam melting is being used to modify the microstructure of the surfaces of materials due to its ability to cause localized melting and supercooling of the melt. This article presents an experimental study on the surface modification of Ni-based superalloy (Inconel 625) reinforced with SiC ceramic particles under electron beam melting. Scanning electron microscopy, energy dispersive spectroscopy and X-ray diffraction techniques have been applied to characterize the resulted microstructure. The results revealed growth of novel structures like wire, rod, tubular, pyramid, bamboo and tweezers type morphologies in the modified surface. In addition to that fibrous like structure was also observed. Formation of thin carbon sheet has been found at the regions of decomposed SiC. Electron beam modified surface of Inconel 625 alloy has been hardened twice as compared to the as-received samples. Surface hardening effect may be attributed to both the formation of the novel structures as well as the introduction of Si and C atom in the lattice of Inconel 625 alloy.

  8. Novel microstructural growth in the surface of Inconel 625 by the addition of SiC under electron beam melting

    International Nuclear Information System (INIS)

    Ahmad, M.; Ali, G.; Ahmed, Ejaz; Haq, M.A.; Akhter, J.I.

    2011-01-01

    Electron beam melting is being used to modify the microstructure of the surfaces of materials due to its ability to cause localized melting and supercooling of the melt. This article presents an experimental study on the surface modification of Ni-based superalloy (Inconel 625) reinforced with SiC ceramic particles under electron beam melting. Scanning electron microscopy, energy dispersive spectroscopy and X-ray diffraction techniques have been applied to characterize the resulted microstructure. The results revealed growth of novel structures like wire, rod, tubular, pyramid, bamboo and tweezers type morphologies in the modified surface. In addition to that fibrous like structure was also observed. Formation of thin carbon sheet has been found at the regions of decomposed SiC. Electron beam modified surface of Inconel 625 alloy has been hardened twice as compared to the as-received samples. Surface hardening effect may be attributed to both the formation of the novel structures as well as the introduction of Si and C atom in the lattice of Inconel 625 alloy.

  9. Application of a multi-component mean field model to the coarsening behaviour of a nickel-based superalloy

    International Nuclear Information System (INIS)

    Anderson, M.J.; Rowe, A.; Wells, J.; Basoalto, H.C.

    2016-01-01

    A multi-component mean field model has been applied to predict the particle evolution of the γ′ particles in the nickel based superalloy IN738LC, capturing the transition from an initial multimodal particle distribution towards a unimodal distribution. Experiments have been performed to measure the coarsening behaviour during isothermal heat treatments using quantitative analysis of micrographs. The three dimensional size of the γ′ particles has been approximated for use in simulation. A coupled thermodynamic/mean field modelling framework is presented and applied to describe the particle size evolution. A robust numerical implementation of the model is detailed that makes use of surrogate models to capture the thermodynamics. Different descriptions of the particle growth rate of non-dilute particle systems have been explored. A numerical investigation of the influence of scatter in chemical composition upon the particle size distribution evolution has been carried out. It is shown how the tolerance in chemical composition of a given alloy can impact particle coarsening behaviour. Such predictive capability is of interest in understanding variation in component performance and the refinement of chemical composition tolerances. It has been found that the inclusion of misfit strain within the current model formulation does not have a significant affect upon predicted long term particle coarsening behaviour. Model predictions show good agreement with experimental data. In particular, the model predicts a reduced growth rate of the mean particle size during the transition from bimodal to unimodal distributions.

  10. Chemical vapor deposition of aluminide coatings on iron, nickel and superalloys

    International Nuclear Information System (INIS)

    John, John T.; De, P.K.; Dubey, Vivekanand; Srinivasa, Raman

    2009-08-01

    Aluminide coatings are a class of intermetallic coatings applied on nickel and cobalt base superalloys and steels to protect them from different forms of environmental degradation at high temperatures. In this report a CVD system that can produce the aluminide coatings on iron, nickel and nickel base alloys has been described and the result of chemical vapor deposition of aluminide coatings on iron specimens, their characterization, and property evaluation have been presented. The CVD system consists of an AlCl 3 bath, a stainless steel retort as a hot-wall reacto, cold traps and vacuum system. Aluminium chloride vapor was carried in a stream of hydrogen gas at a flow rate of 150 SCCM (standard cubic centimeter per minute) into the CVD reactor maintained in the temperature range of 1173 - 1373 K and at a pressure of 1.33 kPa (10 Torr). Aluminum deposition takes place from aluminium subchlorides produced by reaction between AlCl 3 and pure aluminum kept in the CVD reactor. The aluminum diffuses into the iron samples and iron aluminide phases are formed at the surface. The coatings were shining bright and showed good adherence to the substrate. The coatings consisted of FeAl phase over a wide range of experimental conditions. The growth kinetics of the coating followed a parabolic rate law and the mean activation energy was 212 ±16 kJ/mol. Optical microscopic studies on the transverse section of the coating showed that the aluminide coating on iron consisted of two layers. The top layer had a thickness in the range of 20-50 μm, and the under layer had thickness ranging from 35 to 250 μm depending on coating temperature in two hours. The thickness of the aluminide layer increased with coating duration and temperature. Electron microprobe studies (EPMA) showed that the aluminum concentration decreased steadily as distance from the surface increased. TEM studies showed that the outer most layer had a B2 order (of the FeAl phase), which extended even into the under

  11. High temperature deformation mechanisms of L12-containing Co-based superalloys

    Science.gov (United States)

    Titus, Michael Shaw

    Ni-based superalloys have been used as the structural material of choice for high temperature applications in gas turbine engines since the 1940s, but their operating temperature is becoming limited by their melting temperature (Tm =1300degrees C). Despite decades of research, no viable alternatives to Ni-based superalloys have been discovered and developed. However, in 2006, a ternary gamma' phase was discovered in the Co-Al-W system that enabled a new class of Co-based superalloys to be developed. These new Co-based superalloys possess a gamma-gamma' microstructure that is nearly identical to Ni-based superalloys, which enables these superalloys to achieve extraordinary high temperature mechanical properties. Furthermore, Co-based alloys possess the added benefit of exhibiting a melting temperature of at least 100degrees C higher than commercial Ni-based superalloys. Superalloys used as the structural materials in high pressure turbine blades must withstand large thermomechanical stresses imparted from the rotating disk and hot, corrosive gases present. These stresses induce time-dependent plastic deformation, which is commonly known as creep, and new superalloys must possess adequate creep resistance over a broad range of temperature in order to be used as the structural materials for high pressure turbine blades. For these reasons, this research focuses on quantifying high temperature creep properties of new gamma'-containing Co-based superalloys and identifying the high temperature creep deformation mechanisms. The high temperature creep properties of new Co- and CoNi-based alloys were found to be comparable to Ni-based superalloys with respect to minimum creep rates and creep-rupture lives at 900degrees C up to the solvus temperature of the gamma' phase. Co-based alloys exhibited a propensity for extended superlattice stacking fault formation in the gamma' precipitates resulting from dislocation shearing events. When Ni was added to the Co-based compositions

  12. Recrystallization of the ODS superalloy PM-1000

    International Nuclear Information System (INIS)

    Sandim, H.R.Z.; Hayama, A.O.F.; Raabe, D.

    2006-01-01

    The primary recrystallization of a -fiber textured coarse-grained oxide dispersion strengthened nickel-based superalloy (PM-1000) has been investigated by high-resolution electron backscatter diffraction. The annealing behavior of this alloy is quite complex. Even at high annealing temperatures (e.g. 1200 deg. C), recrystallization is only partial. The microstructure of this superalloy in the annealed state consists of a blurred subgrain structure, coarse grains with sizes of about 10-20 μm at the pre-existing grain boundaries and a significant fraction of small crystals in the interior of the recovered grains. These small grains are elongated and display anisotropic growth. In the present paper we present a detailed explanation for this peculiar microstructure. Particular focus is placed on the origin of the new grains in the recovered structure in a [1 0 0]-oriented grain

  13. High temperature properties of polycrystalline γ"'-strengthened cobalt-base superalloys

    International Nuclear Information System (INIS)

    Bauer, Alexander

    2016-01-01

    The recent discovery of a stable γ"'-phase in Co-based superalloys opened up a pathway for the development of a new high temperature material class, which is similar in microstructure and properties to the modern γ"'-hardened Ni-based superalloys. In this work, the first attempt was done to check the influence of several for Ni-based superalloys typical alloying elements on the properties of the new Co-based superalloys. It became clear that the basic characteristics of the first experimental alloys are similar to those of the γ"'-hardened Ni-based alloys. The results of the multinary experimental alloys show that, based on the insight gained so far, targeted alloy development is possible. These materials have the potential to be used as disc materials in turbines.

  14. Mechanical properties and microstructure evaluation of powder bed fused inconel 625 nickel alloy

    Energy Technology Data Exchange (ETDEWEB)

    Brand, Michael J. [Los Alamos National Lab. (LANL), Los Alamos, NM (United States)

    2016-04-19

    The objectives of this report were to optimize and fabricate full density Inconel 625 samples using direct metal laser fusion, an additive manufacturing process; and to compare and evaluate precipitation and solid solution strengthening of Inconel 625 produced by PBF to conventional processed material.

  15. Investigations on the structure – Property relationships of electron beam welded Inconel 625 and UNS 32205

    International Nuclear Information System (INIS)

    Devendranath Ramkumar, K.; Sridhar, R.; Periwal, Saurabh; Oza, Smitkumar; Saxena, Vimal; Hidad, Preyas; Arivazhagan, N.

    2015-01-01

    Highlights: • Joining of dissimilar metals of Inconel 625 and UNS S32205 using electron beam welding. • Detailed structure – property relationship of dissimilar welds. • Improved metallurgical and tensile properties from the EB welding. - Abstract: The metallurgical and mechanical properties of electron beam welded Ni based superalloy Inconel 625 and UNS S32205 duplex stainless steel plates have been investigated in the present study. Interface microstructure studies divulged the absence of any grain coarsening effects or the formation of any secondary phases at the heat affected zone (HAZ) of the electron beam (EB) weldments. Tensile studies showed that the fracture occurred at the weld zone in all the trials and the average weld strength was reported to be 850 MPa. Segregation of Mo rich phases was witnessed at the inter-dendritic arms of the fusion zone. The study recommended the use of EB welding for joining these dissimilar metals by providing detailed structure – property relationships

  16. Response surface modelling of tool electrode wear rate and material removal rate in micro electrical discharge machining of Inconel 718

    DEFF Research Database (Denmark)

    Puthumana, Govindan

    2017-01-01

    Inconel 718 is a corrosion-resistant and high strength nickel-based alloy with wide range of applications includingcomponents for cryogenic tankage, liquid fueled rockets and casings for aircraft engines. The material is characterizedby high hardness, high temperature strength, low thermal...

  17. Grain size refinement of inconel 718 thermomechanical processing

    International Nuclear Information System (INIS)

    Okimoto, P.C.

    1988-01-01

    Inconel 718 is a Ni-Fe precipitation treated superalloy. It presents good thermal fatigue properties when the material has small grain size. The aim of this work is to study the grain size refinement by thermomechanical processing, through observations of the microstructural evolution and the influence of some of the process variables in the final grain size. The results have shown that this refinement occured by static recrystallization. The presence of precipitates have influenced the final grain size if the deformations are below 60%. For greater deformations the grain size is independent of the precipitate distribution in the matrix and tends to a limit size of 5 μm. (author)

  18. Coarsening behaviour and interfacial structure of γ′ precipitates in Co-Al-W based superalloys

    International Nuclear Information System (INIS)

    Vorontsov, V.A.; Barnard, J.S.; Rahman, K.M.; Yan, H.-Y.; Midgley, P.A.; Dye, D.

    2016-01-01

    This work discusses the effects of alloying on the coarsening behaviour of the L1 2 ordered γ ′ phase and the structure of the γ/γ ′ interfaces in three Co-Al-W base superalloys aged at ∼90 °C below the respective solvus temperatures: Co-7Al-7W, Co-10Al-5W-2Ta and Co-7Al-7W-20Ni (at.%). The coarsening kinetics are adequately characterised by the classical Lifshitz-Slyozov-Wagner model for Ostwald ripening. Co-7Al-7W exhibited much slower coarsening than its quaternary derivatives. Alloying can be exploited to modify the coarsening kinetics either by increasing the solvus temperature by adding tantalum, or by adding nickel to shift the rate controlling mechanism towards dependence on the diffusion of aluminium rather than tungsten. Lattice resolution STEM imaging was used to measure the widths of the order-disorder (structural) and Z-contrast (compositional) gradients across the γ/γ ′ interfaces. Similarly to nickel base superalloys, the compositional gradient was found to be wider than the structural. Co-7Al-7W-20Ni had much wider interface gradients than Co-7Al-7W and Co-10Al-5W-2Ta, which suggests that its γ ′ phase stoichiometry is less constrained. A possible correlation between temperature and misfit normalised r vs. t 1/3 coarsening rate coefficients and the structural gradient width has also been identified, whereby alloys with wider interfaces exhibit faster coarsening rates.

  19. SANS investigation of precipitate microstructure in nickel-base superalloys Waspaloy and DT750

    Czech Academy of Sciences Publication Activity Database

    Strunz, Pavel; Zrník, J.; Seliga, T.; Penkalla, H.J.

    2006-01-01

    Roč. 2, č. 23 (2006), s. 363-368 ISSN 0044-2968 R&D Projects: GA ČR GA202/06/0601 Institutional research plan: CEZ:AV0Z10480505 Keywords : small-angle-neutron scattering * superalloys * precipitation Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 1.897, year: 2006

  20. Low temperature gaseous nitriding of Ni based superalloys

    DEFF Research Database (Denmark)

    Eliasen, K. M.; Christiansen, Thomas Lundin; Somers, Marcel A. J.

    2010-01-01

    In the present work the nitriding response of selected Ni based superalloys at low temperatures is addressed. The alloys investigated are nimonic series nos. 80, 90, 95 and 100 and nichrome (Ni/Cr......In the present work the nitriding response of selected Ni based superalloys at low temperatures is addressed. The alloys investigated are nimonic series nos. 80, 90, 95 and 100 and nichrome (Ni/Cr...

  1. Subsurface characterization of an oxidation-induced phase transformation and twinning in nickel-based superalloy exposed to oxy-combustion environments

    International Nuclear Information System (INIS)

    Zhu Jingxi; Holcomb, Gordon R.; Jablonski, Paul D.; Wise, Adam; Li Jia; Laughlin, David E.; Sridhar, Seetharaman

    2012-01-01

    Highlights: ►Oxidation products of Ni-based superalloy were studied in oxy-fuel combustion conditions. ► An oxidation-induced phase transformation occurred in the subsurface region. ► One of the two product phases was not in the Ni database of Thermo-Calc. ► This unknown phase is an ordered derivative of FCC structure of Ni–Ti(–Ta) system. ► This phase is likely detrimental to the mechanical integrity of the alloy in use. - Abstract: In the integration of oxy-fuel combustion to turbine power generation system, turbine alloys are exposed to high temperature and an atmosphere comprised of steam, CO 2 and O 2 . While surface and internal oxidation of the alloy takes place, the microstructure in the subsurface region also changes due to oxidation. In this study, bare metal coupons of Ni-base superalloys were exposed in oxy-fuel combustion environment for up to 1000 h and the oxidation-related microstructures were examined. Phase transformation occurred in the subsurface region in Ni-based superalloy and led to twinning. The transformation product phases were analyzed through thermodynamic equilibrium calculations and various electron microscopy techniques, including scanning electron microscopy (SEM), orientation imaging microscopy (OIM) and transmission electron microscopy (TEM). The mechanism by which the phase transformation and the formation of the microstructure occurred was also discussed. The possible effects of the product phases on the performance of the alloy in service were discussed.

  2. STABILITY ANALYSIS OF RADIAL TURNING PROCESS FOR SUPERALLOYS

    Directory of Open Access Journals (Sweden)

    Alberto JIMÉNEZ

    2017-07-01

    Full Text Available Stability detection in machining processes is an essential component for the design of efficient machining processes. Automatic methods are able to determine when instability is happening and prevent possible machine failures. In this work a variety of methods are proposed for detecting stability anomalies based on the measured forces in the radial turning process of superalloys. Two different methods are proposed to determine instabilities. Each one is tested on real data obtained in the machining of Waspalloy, Haynes 282 and Inconel 718. Experimental data, in both Conventional and High Pressure Coolant (HPC environments, are set in four different states depending on materials grain size and Hard-ness (LGA, LGS, SGA and SGS. Results reveal that PCA method is useful for visualization of the process and detection of anomalies in online processes.

  3. THE EFFECT OF THE CONDITIONS OF SHOT PEENING THE INCONEL 718 NICKEL ALLOY ON THE GEOMETRICAL STRUCTURE OF THE SURFACE

    Directory of Open Access Journals (Sweden)

    Kazimierz Zaleski

    2017-06-01

    Full Text Available The article presents the research results of roughness and topography of the surface of Inconel 718 nickel alloy after shot peening. Evaluation of stereometric properties of the surface layer of the examined material was performed based on the amplitude, height and Abbott-Firestone curve parametres. The shot peening was carried out on the impulse shot peening stand. The impact energy Ej, distance between the traces xs and the ball diameter dk were changed in the range: Ej = 60 ÷ 240 mJ, xs = 0,15 ÷ 0,5 mm, dk = 3,95 ÷ 12,45 mm. The T8000 RC 120-140 device of the Hommel-Etamic company, along with the software, was used for measuring the surface roughness and for determining the material bearing curve. As a result of the machin-ing, the surface roughness was reduced and the selected functional parameters were improved.

  4. Microstructure evolution of a pre-compression nickel-base single crystal superalloy during tensile creep

    International Nuclear Information System (INIS)

    Yu Xingfu; Tian Sugui; Du Hongqiang; Yu Huichen; Wang Minggang; Shang Lijuan; Cui Shusen

    2009-01-01

    By pre-compressive creep treatment, the cubical γ' phase in the nickel-base single crystal superalloy is transformed into the P-type rafted structure along the direction parallel to the applied stress axis. And the microstructure evolution of the P-type γ' rafted alloy during tensile creep is investigated by means of the measurement of the creep curve and microstructure observation. Results show that the P-type γ' rafted phase in the alloy is transformed into the N-type structure along the direction perpendicular to the applied stress axis in the initial stage of the tensile creep. In the role of the tensile stress at high temperature, the change of the element's equilibrium concentration in the different regions of P-type γ' rafted phase occurs, which promotes the inhomogeneous coarsening of the P-type γ' phase. And then, the decomposition of the P-type γ' rafted phase in the alloy occurs to form the groove structure. As of result of the directional diffusion of the elements, the fact that the P-type γ' rafted phase is decomposed to transform into the cubical-like structure is attributed to the increment of the solute elements M(Ta, Al) chemical potential in the groove regions. Further, the lattice constriction in the horizontal interfaces of the cubical-like γ' phase may repel out the Al and Ta atoms with higher radius due to the role of the shearing stress, and the lattice expanding in the upright interfaces of the cubical-like γ' phase, due to the role of the tension stress, may trap the Ta and Al atoms, which promotes the directional growing of γ' phase into the N-type rafted structure. Therefore, the change of the strain energy density in different interfaces of the cubical-like γ' phase is thought to be the driving force of the elements diffusing and the directional coarsening of γ' phase

  5. Microstructural analysis of laser weld fusion zone in Haynes 282 superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Osoba, L.O. [Department of Mechanical and Manufacturing Engineering, University of Manitoba, Winnipeg, Manitoba, R3T 5V6 (Canada); Ding, R.G. [Department of Metallurgy and Materials Engineering, University of Birmingham, Birmingham B15 2TT (United Kingdom); Ojo, O.A., E-mail: ojo@cc.umanitoba.ca [Department of Mechanical and Manufacturing Engineering, University of Manitoba, Winnipeg, Manitoba, R3T 5V6 (Canada)

    2012-03-15

    Analytical electron microscopy and spectroscopy analyses of the fusion zone (FZ) microstructure in autogenous laser beam welded Haynes 282 (HY 282) superalloy were performed. The micro-segregation patterns observed in the FZ indicate that Co, Cr and Al exhibited a nearly uniform distribution between the dendrite core and interdendritic regions while Ti and Mo were rejected into the interdendritic liquid during the weld solidification. Transmission electron diffraction analysis and energy dispersive X-ray microanalysis revealed the second phase particles formed along the FZ interdendritic region to be Ti-Mo rich MC-type carbide particles. Weld FZ solidification cracking, which is sometimes associated with the formation of {gamma}-{gamma}' eutectic in {gamma}' precipitation strengthened nickel-base superalloys, was not observed in the HY 282 superalloy. Modified primary solidification path due to carbon addition in the newly developed superalloy is used to explain preclusion of weld FZ solidification cracking in the material. - Highlights: Black-Right-Pointing-Pointer A newly developed superalloy was welded by CO{sub 2} laser beam joining technique. Black-Right-Pointing-Pointer Electron microscopy characterization of the weld microstructure was performed. Black-Right-Pointing-Pointer Identified interdendritic microconstituents consist of MC-type carbides. Black-Right-Pointing-Pointer Modification of primary solidification path is used to explain cracking resistance.

  6. Microstructural analysis of laser weld fusion zone in Haynes 282 superalloy

    International Nuclear Information System (INIS)

    Osoba, L.O.; Ding, R.G.; Ojo, O.A.

    2012-01-01

    Analytical electron microscopy and spectroscopy analyses of the fusion zone (FZ) microstructure in autogenous laser beam welded Haynes 282 (HY 282) superalloy were performed. The micro-segregation patterns observed in the FZ indicate that Co, Cr and Al exhibited a nearly uniform distribution between the dendrite core and interdendritic regions while Ti and Mo were rejected into the interdendritic liquid during the weld solidification. Transmission electron diffraction analysis and energy dispersive X-ray microanalysis revealed the second phase particles formed along the FZ interdendritic region to be Ti–Mo rich MC-type carbide particles. Weld FZ solidification cracking, which is sometimes associated with the formation of γ–γ' eutectic in γ' precipitation strengthened nickel-base superalloys, was not observed in the HY 282 superalloy. Modified primary solidification path due to carbon addition in the newly developed superalloy is used to explain preclusion of weld FZ solidification cracking in the material. - Highlights: ► A newly developed superalloy was welded by CO 2 laser beam joining technique. ► Electron microscopy characterization of the weld microstructure was performed. ► Identified interdendritic microconstituents consist of MC-type carbides. ► Modification of primary solidification path is used to explain cracking resistance.

  7. High temperature oxidation and corrosion behavior of Ni-base superalloy in He environment

    International Nuclear Information System (INIS)

    Lee, Gyoeng Geun; Park, Ji Yeon; Jung, Su jin

    2010-11-01

    Ni-base superalloy is considered as a IHX (Intermediate Heat Exchanger) material for VHTR (Very High Temperature Gas-Cooled Reactor). The helium environment in VHTR contains small amounts of impure gases, which cause oxidation, carburization, and decarburization. In this report, we conducted the literature survey about the high temperature behavior of Ni-base superalloys in air and He environments. The basic information of Ni-base superalloy and the basic metal-oxidation theory were briefly stated. The He effect on the corrosion of Ni-base superalloy was also summarized. This works would provide a brief suggestion for the next research topic for the application of Ni-base superalloy to VHTR

  8. Strengthening mechanisms in an inertia friction welded nickel-base superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Tiley, J.S., E-mail: Jaimie.Tiley@us.af.mil [Air Force Research Laboratory, Wright Patterson Air Force Base, OH 45433 (United States); Mahaffey, D.W. [Air Force Research Laboratory, Wright Patterson Air Force Base, OH 45433 (United States); Alam, T.; Rojhirunsakool, T. [Department of Materials Engineering, University of North Texas, Denton, TX 76203 (United States); Senkov, O.; Parthasarthy, T. [Air Force Research Laboratory, Wright Patterson Air Force Base, OH 45433 (United States); UES, Inc., Dayton, OH 45433 (United States); Banerjee, R. [Department of Materials Engineering, University of North Texas, Denton, TX 76203 (United States)

    2016-04-26

    This research investigated the strengthening mechanisms associated with the as-welded microstructure developed during inertia friction welding of dissimilar superalloys LHSR and Mar-M247. The weld interface and heat affected regions of the sample were analyzed using hardness indentation techniques and subsequently characterized using SEM, TEM and advanced atom probe tomography. The yield strength of the welded joint was modeled to determine the impact of the gradients in the as-welded microstructure on strengthening mechanisms within the LSHR material. Characterization centered on formation of γ′, γ grain size and chemical segregation within the heat affected regions. Results indicate an increased hardness in the vicinity of the weld interface, resulting from the refined dispersion of γ′ and γ grains.

  9. Characterization of Phase Chemistry and Partitioning in a Family of High-Strength Nickel-Based Superalloys

    Science.gov (United States)

    Lapington, M. T.; Crudden, D. J.; Reed, R. C.; Moody, M. P.; Bagot, P. A. J.

    2018-06-01

    A family of novel polycrystalline Ni-based superalloys with varying Ti:Nb ratios has been created using computational alloy design techniques, and subsequently characterized using atom probe tomography and electron microscopy. Phase chemistry, elemental partitioning, and γ' character have been analyzed and compared with thermodynamic predictions created using Thermo-Calc. Phase compositions and γ' volume fraction were found to compare favorably with the thermodynamically predicted values, while predicted partitioning behavior for Ti, Nb, Cr, and Co tended to overestimate γ' preference over the γ matrix, often with opposing trends vs Nb concentration.

  10. Segregation in welded nickel-base alloys

    International Nuclear Information System (INIS)

    Akhtar, J.I.; Shoaib, K.A.; Ahmad, M.; Shaikh, M.A.

    1990-05-01

    Segregation effects have been investigated in nickel-base alloys monel 400, inconel 625, hastelloy C-276 and incoloy 825, test welded under controlled conditions. Deviations from the normal composition have been observed to varying extents in the welded zone of these alloys. Least effect of this type occurred in Monel 400 where the content of Cu increased in some of the areas. Enhancement of Al and Ti has been found over large areas in the other alloys which has been attributed to the formation of low melting slag. Another common feature is the segregation of Cr, Fe or Ti, most likely in the form of carbides. Enrichment of Al, Ti, Nb, Mb, Mo, etc., to different amounts in some of the areas of these materials is in- terpretted in terms of the formation of gamma prime precipitates or of Laves phases. (author)

  11. High Temperature Deformation Mechanisms in a DLD Nickel Superalloy

    Directory of Open Access Journals (Sweden)

    Sean Davies

    2017-04-01

    Full Text Available The realisation of employing Additive Layer Manufacturing (ALM technologies to produce components in the aerospace industry is significantly increasing. This can be attributed to their ability to offer the near-net shape fabrication of fully dense components with a high potential for geometrical optimisation, all of which contribute to subsequent reductions in material wastage and component weight. However, the influence of this manufacturing route on the properties of aerospace alloys must first be fully understood before being actively applied in-service. Specimens from the nickel superalloy C263 have been manufactured using Powder Bed Direct Laser Deposition (PB-DLD, each with unique post-processing conditions. These variables include two build orientations, vertical and horizontal, and two different heat treatments. The effects of build orientation and post-process heat treatments on the materials’ mechanical properties have been assessed with the Small Punch Tensile (SPT test technique, a practical test method given the limited availability of PB-DLD consolidated material. SPT testing was also conducted on a cast C263 variant to compare with PB-DLD derivatives. At both room and elevated temperature conditions, differences in mechanical performances arose between each material variant. This was found to be instigated by microstructural variations exposed through microscopic and Energy Dispersive X-ray Spectroscopy (EDS analysis. SPT results were also compared with available uniaxial tensile data in terms of SPT peak and yield load against uniaxial ultimate tensile and yield strength.

  12. Strength and structure during hot deformation of nickel-base superalloys

    International Nuclear Information System (INIS)

    Ribeiro, N.D.; Sellars, C.M.

    1984-01-01

    The effect of deformational variables on the flow stress and microstructure developed by plane strain compression testing and experimental rolling of three otherwise well characterized nickel-base super alloys, Nimonic 80A, Nimonic 90 and Waspaloy are presented. Rolled or tested samples were sectioned longitudinally at mid-width and were prepared for optical metallography. X-ray analysis of particles observed in several samples was carried out on polished and lightly etehed surfaces using a diffractometer with CoKα radiation. For other samples, energy dispersive x-ray analysis was also carried out in a scanning microscope. (E.G.) [pt

  13. Mathematical modelling of brittle phase precipitation in complex ruthenium containing nickel-based superalloys

    International Nuclear Information System (INIS)

    Rettig, Ralf

    2010-01-01

    A new model has been developed in this work which is capable of simulating the precipitation kinetics of brittle phases, especially TCP-phases (topologically close packed phases) in ruthenium containing superalloys. The model simultaneously simulates the nucleation and the growth stage of precipitation for any number of precipitating phases. The CALPHAD method (Calculation of Phase Diagrams) is employed to calculate thermodynamic properties, such as the driving force or phase compositions in equilibrium. For calculation of diffusion coefficients, kinetic mobility databases which are also based on the CALPHAD-method are used. The model is fully capable of handling multicomponent effects, which are common in complex superalloys. Metastable phases can be treated and will automatically be dissolved if they get unstable. As the model is based on the general CALPHAD method, it can be applied to a broad range of precipitation processes in different alloys as long as the relevant thermodynamic and kinetic databases are available. The developed model proves that the TCP-phases precipitate in a sequence of phases. The first phase that is often formed is the metastable σ-phase because it has the lowest interface energy due to low-energy planes at the interface between matrix and precipitate. After several hundred hours the stable μ- and P-phases start to precipitate by nucleating at the σ-phase which is energetically favourable. During the growth of these stable phases the sigma-phase is continuously dissolved. It can be shown by thermodynamic CALPHAD calculations that the sigma-phase has a lower Gibbs free enthalpy than the μ- and P-phase. All required parameters of the model, such as interface energy and nucleate densities, have been estimated. The mechanisms of suppression of TCP-phase precipitation in the presence of ruthenium in superalloys were investigated with the newly developed model. It is shown by the simulations that ruthenium mostly affects the nucleation

  14. Cyclic plastic response of nickel-based superalloy at room and at elevated temperatures

    Czech Academy of Sciences Publication Activity Database

    Polák, Jaroslav; Petrenec, Martin; Chlupová, Alice; Tobiáš, Jiří; Petráš, Roman

    2015-01-01

    Roč. 57, č. 2 (2015), s. 119-125 ISSN 0025-5300 R&D Projects: GA ČR(CZ) GA13-23652S; GA MŠk(CZ) ED1.1.00/02.0068 Institutional support: RVO:68081723 Keywords : cyclic plasticity * elevat ed temperature * superalloys * hysteresis loop * statistical theory Subject RIV: JL - Materials Fatigue, Friction Mechanics Impact factor: 0.266, year: 2015

  15. The Effect of Boron and Zirconium on the Structure and Tensile Properties of the Cast Nickel-Based Superalloy ATI 718Plus

    Science.gov (United States)

    Hosseini, Seyed Ali; Abbasi, Seyed Mehdi; Madar, Karim Zangeneh

    2018-04-01

    The effects of boron and zirconium on cast structure, hardness, and tensile properties of the nickel-based superalloy 718Plus were investigated. For this purpose, five alloys with different contents of boron and zirconium were cast via vacuum induction melting and then purified via vacuum arc remelting. Microstructural analysis by light-optical microscope and scanning electron microscope equipped with energy-dispersive x-ray spectroscopy and phase studies by x-ray diffraction analysis were performed. The results showed that boron and zirconium tend to significantly reduce dendritic arm spacing and increase the amount of Laves, Laves/gamma eutectic, and carbide phases. It was also found that boron led to the formation of B4C and (Cr, Fe, Mo, Ni, Ti)3B2 phases and zirconium led to the formation of intermetallic phases and ZrC carbide. In the presence of boron and zirconium, the hardness and its difference between dendritic branches and inter-dendritic spaces increased by concentrating such phases as Laves in the inter-dendritic spaces. These elements had a negative effect on tensile properties of the alloy, including ductility and strength, mainly because of the increase in the Laves phase. It should be noted that the largest degradation of the tensile properties occurred in the alloys containing the maximum amount of zirconium.

  16. The Influence of the Coating Deposition Process on the Interdiffusion Behavior Between Nickel-Based Superalloys and MCrAlY Bond Coats

    Science.gov (United States)

    Elsaß, M.; Frommherz, M.; Oechsner, M.

    2018-02-01

    In this work, interdiffusion between two nickel-based superalloys and two MCrAlY bond coats is investigated. The MCrAlY bond coats were applied using two different spraying processes, high velocity oxygen fuel spraying (HVOF) and low-pressure plasma spraying. Of primary interest is the evolution of Kirkendall porosity, which can form at the interface between substrate and bond coat and depends largely on the chemical compositions of the coating and substrate. Experimental evidence further suggested that the formation of Kirkendall porosity depends on the coating deposition process. Formation of porosity at the interface causes a degradation of the bonding strength between substrate and coating. After coating deposition, the samples were annealed at 1050 °C for up to 2000 h. Microstructural and compositional analyses were performed to determine and evaluate the Kirkendall porosity. The results reveal a strong influence of both the coating deposition process and the chemical compositions. The amount of Kirkendall porosity formed, as well as the location of appearance, is largely influenced by the coating deposition process. In general, samples with bond coats applied by means of HVOF show accelerated element diffusion. It is hypothesized that recrystallization of the substrate material is a main root cause for these observations.

  17. Analysis of Effective and Internal Cyclic Stress Components in the Inconel Superalloy Fatigued at Elevated Temperature

    Czech Academy of Sciences Publication Activity Database

    Šmíd, Miroslav; Petrenec, Martin; Polák, Jaroslav; Obrtlík, Karel; Chlupová, Alice

    2011-01-01

    Roč. 278, 4 July (2011), s. 393-398 ISSN 1022-6680. [European Symposium on Superalloys and their Application. Wildbad Kreuth, 25.5.2010-28.5.2010] R&D Projects: GA ČR GA106/08/1631 Institutional research plan: CEZ:AV0Z20410507 Keywords : low cycle fatigue * superalloys * high temperature * hysteresis loop * effective and internal stresses Subject RIV: JL - Materials Fatigue, Friction Mechanics; JL - Materials Fatigue, Friction Mechanics (UFM-A)

  18. Effect of carbon content on the microstructure and creep properties of a 3rd generation single crystal nickel-base superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Li, X.W.; Liu, T. [Superalloys Division, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China); Wang, L., E-mail: wangli@imr.ac.cn [Superalloys Division, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China); Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China); Liu, X.G.; Lou, L.H. [Superalloys Division, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China); Zhang, J. [Superalloys Division, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China); Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China)

    2015-07-15

    Effect of carbon content on the microstructure and creep properties of a 3rd generation single crystal nickel-base superalloy has been investigated by the scanning electron microscope, X-ray computed tomography and electron probe microanalyzer. With the increase of the carbon content, MC carbides evolve from octahedral to well-developed dendrite, which promotes the formation of microporosity. Moreover, the volume fraction of porosity increases in the experimental alloys after solution heat treatment. As a result, the increase in the size of MC carbides and the porosity has a detrimental effect on the low temperature and high stress creep behavior of the alloys. The specimen crept at 850 °C and 586 MPa with the carbon content of 430 ppm shows the shortest rupture life due to the largest primary creep strain. However, the creep behavior of the alloy at 1120 °C and 140 MPa gets better as the carbon content increases from 88 to 430 ppm. TCP phase is observed near the fracture surfaces of the alloys, which explores as a potential cause for the creep rupture. However, the formation of TCP phase is effectively suppressed for decreasing segregation of the alloying elements, which results in the improvement of the creep life in the alloy with 430 ppm carbon at 1120 °C and 140 MPa.

  19. Additive Manufacturing of IN100 Superalloy Through Scanning Laser Epitaxy for Turbine Engine Hot-Section Component Repair: Process Development, Modeling, Microstructural Characterization, and Process Control

    Science.gov (United States)

    Acharya, Ranadip; Das, Suman

    2015-09-01

    This article describes additive manufacturing (AM) of IN100, a high gamma-prime nickel-based superalloy, through scanning laser epitaxy (SLE), aimed at the creation of thick deposits onto like-chemistry substrates for enabling repair of turbine engine hot-section components. SLE is a metal powder bed-based laser AM technology developed for nickel-base superalloys with equiaxed, directionally solidified, and single-crystal microstructural morphologies. Here, we combine process modeling, statistical design-of-experiments (DoE), and microstructural characterization to demonstrate fully metallurgically bonded, crack-free and dense deposits exceeding 1000 μm of SLE-processed IN100 powder onto IN100 cast substrates produced in a single pass. A combined thermal-fluid flow-solidification model of the SLE process compliments DoE-based process development. A customized quantitative metallography technique analyzes digital cross-sectional micrographs and extracts various microstructural parameters, enabling process model validation and process parameter optimization. Microindentation measurements show an increase in the hardness by 10 pct in the deposit region compared to the cast substrate due to microstructural refinement. The results illustrate one of the very few successes reported for the crack-free deposition of IN100, a notoriously "non-weldable" hot-section alloy, thus establishing the potential of SLE as an AM method suitable for hot-section component repair and for future new-make components in high gamma-prime containing crack-prone nickel-based superalloys.

  20. Influence of Support Configurations on the Characteristics of Selective Laser-Melted Inconel 718

    Science.gov (United States)

    Nadammal, Naresh; Kromm, Arne; Saliwan-Neumann, Romeo; Farahbod, Lena; Haberland, Christoph; Portella, Pedro Dolabella

    2018-03-01

    Samples fabricated using two different support configurations by following identical scan strategies during selective laser melting of superalloy Inconel 718 were characterized in this study. Characterization methods included optical microscopy, electron back-scattered diffraction and x-ray diffraction residual stress measurement. For the scan strategy considered, microstructure and residual stress development in the samples were influenced by the support structures. However, crystallographic texture intensity and the texture components formed within the core part of the samples were almost independent of the support. The formation of finer grains closer to the support as well as within the columnar grain boundaries resulted in randomization and texture intensity reduction by nearly half for the sample built on a lattice support. Heat transfer rates dictated by the support configurations in addition to the scan strategy influenced the microstructure and residual stress development in selective laser-melted Inconel 718 samples.

  1. Thermal analysis of silicon carbide coating on a nickel based superalloy substrate and thickness measurement of top layers by lock-in infrared thermography

    Energy Technology Data Exchange (ETDEWEB)

    Ranjit, Shrestha; Kim, Won Tae [Kongju National University, Cheonan (Korea, Republic of)

    2017-04-15

    In this paper, we investigate the capacity of the lock-in infrared thermography technique for the evaluation of non-uniform top layers of a silicon carbide coating with a nickel based superalloy sample. The method utilized a multilayer heat transfer model to analyze the surface temperature response. The modelling of the sample was done in ANSYS. The sample consists of three layers, namely, the metal substrate, bond coat and top coat. A sinusoidal heating at different excitation frequencies was imposed upon the top layer of the sample according to the experimental procedures. The thermal response of the excited surface was recorded, and the phase angle image was computed by Fourier transform using the image processing software, MATLAB and Thermofit Pro. The correlation between the coating thickness and phase angle was established for each excitation frequency. The most appropriate excitation frequency was found to be 0.05 Hz. The method demonstrated potential in the evaluation of coating thickness and it was successfully applied to measure the non-uniform top layers ranging from 0.05 mm to 1 mm with an accuracy of 0.000002 mm to 0.045 mm.

  2. Development of a Ni-based superalloy with cellular structure and interconnected micro porosity

    International Nuclear Information System (INIS)

    Bernabe, A.; Lopez, E.; Gil-Sevillano, J.

    1998-01-01

    A cellular metallic material with interconnected porosity of controlled size of an order of 10 μm has been developed by electrochemical dissolution of tungsten grains in a W-Ni-Fe heavy alloy. The nickel superalloy with sponge structure and high surface/volume ratio can also be processed recycling chips from heavy metal machining (Patent number p9700191, 1997). Applications for the new materials could be found as support for catalysts, high temperature filters for corrosive fluids, burners, etc. (Author) 10 refs

  3. The machinability of nickel-based alloys in high-pressure jet assisted (HPJA turning

    Directory of Open Access Journals (Sweden)

    D. Kramar

    2013-10-01

    Full Text Available Due to their mechanical, thermal and chemical properties, nickel-based alloys are generally included among materials that are hard to machine. An experimental study has been performed to investigate the capabilities of conventional and high-pressure jet assisted (HPJA turning of hard-to-machine materials, namely Inconel 718. The capabilities of different hard turning procedures are compared by means of chip breakability. The obtained results show that HPJA method offers a significant increase in chip breakability, under the same cutting conditions (cutting speed, feed rate, depth of cut.

  4. Study of the influence of temperature and time on the electroplating nickel layer in Inconel 718 strips used in spacer grid of Pressurized Water Cooled nuclear reactors (PWR)

    Energy Technology Data Exchange (ETDEWEB)

    Rezende, Renato; Abati, Amanda; Verne, Júlio; Panossian, Zehbour, E-mail: amanda.abati@marinha.mil.br, E-mail: jvernegropp@gmail.com, E-mail: renato.rezende@marinha.mil.br, E-mail: zep@ipt.br [Centro Tecnológico da Marinha em São Paulo (CTMSP), São Paulo, SP (Brazil). Laboratório de Desenvolvimento e Instrumentação de Combustível Nuclear; Instituto de Pesquisas Tecnológicas (IPT), São Paulo, SP (Brazil)

    2017-07-01

    The Inconel 718 (UNS N07718: Ni-{sup 19}Cr-{sup 18}Fe-{sup 5}Nb-3 Mo) is a precipitation hardenable nickel alloy that has good corrosion resistance and high mechanical strength. These strips are used for assembling the spacer grid of fuel element of pressurized water cooled nuclear reactors (PWR). The spacer grid is a structural component of fundamental importance in fuel elements of PWR reactors, maintaining the position and necessary spacing of the fuel rods within the arrangement of the fuel element. The spacer grid is formed by joining the points of intersection of the strips, by a joint process called brazing. For this process, these strips are stamped and plated with a thin layer of nickel by means of electroplating in order to protect against oxidation and allow a better flowability and wettability of the addition metal in the strips during brazing. Oxidation at the surface of the base material harms wettability and inhibits spreading of the liquid addition metal on the substrate surface during the brazing process. The use of coatings such as nickel plating is used to ensure such conditions. The results showed that there is a process of diffusion de some chemical elements such as chromium, iron, titanium and aluminum from the substrate to the nickel layer and nickel from the layer to the substrate. These chemical elements are responsible for the oxidation at the surface of the strip. (author)

  5. Degradation modes of nickel-base alternate waste package overpack materials

    International Nuclear Information System (INIS)

    Pitman, S.G.

    1988-07-01

    The suitability of Ti Grade 12 for waste package overpacks has been questioned because of its observed susceptibility to crevice corrosion and hydrogen-assisted crack growth. For this reason, materials have been selected for evaluation as alternatives to Ti Grade 12 for use as waste package overpacks. These alternative materials, which are based on the nickel-chromium-molybdenum (Ni-Cr-Mo) alloy system, are Inconel 625, Hastelloy C-276, and Hastelloy C-22. The degradation modes of the Ni-base alternate materials have been examined at Pacific Northwest Laboratory to determine the suitability of these materials for waste package overpack applications in a salt repository. Degradation modes investigated included general corrosion, crevice corrosion, pitting, stress-corrosion cracking, and hydrogen embrittlement

  6. Some observations on the physical metallurgy of nickel alloy weld metals

    International Nuclear Information System (INIS)

    Skillern, C.G.; Lingenfelter, A.C.

    1982-01-01

    Numerous nickel alloys play critical roles in various energy-related applications. Successful use of these alloys is almost always dependent on the availability of acceptable welding methods and welding products. An understanding of the physical metallurgy of these alloys and their weld metals and the interaction of weld metal and base metal is essential to take full advantage of the useful properties of the alloys. To illustrate this point, this paper presents data for two materials: INCONEL alloy 718 and INCONEL Welding Electrode 132. 8 figures, 9 tables

  7. Thermomechanical behavior of different Ni-base superalloys during cyclic loading at elevated temperatures

    Directory of Open Access Journals (Sweden)

    Huber Daniel

    2014-01-01

    Full Text Available The material behavior of three Ni-base superalloys (Inconel® 718, Allvac® 718PlusTM and Haynes® 282® during in-phase cyclic mechanical and thermal loading was investigated. Stress controlled thermo-mechanical tests were carried out at temperatures above 700 ∘C and different levels of maximum compressive stress using a Gleeble® 3800 testing system. Microstructure investigations via light optical microscopy (LOM and field emission gun scanning electron microscopy (FEG-SEM as well as numerical precipitation kinetics simulations were performed to interpret the obtained results. For all alloys, the predominant deformation mechanism during deformation up to low plastic strains was identified as dislocation creep. The main softening mechanism causing progressive increase of plastic strain after preceding linear behavior is suggested to be recrystallization facilitated by coarsening of grain boundary precipitates. Furthermore, coarsening and partial transformation of strengthening phases was observed. At all stress levels, Haynes® 282® showed best performance which is attributable to its stable microstructure containing a high phase fraction of small, intermetallic precipitates inside grains and different carbides evenly distributed along grain boundaries.

  8. Quantitative characterization and comparison of precipitate and grain shape in Nickel -base superalloys using moment invariants

    Science.gov (United States)

    Callahan, Patrick Gregory

    A fundamental objective of materials science and engineering is to understand the structure-property-processing-performance relationship. We need to know the true 3-D microstructure of a material to understand certain geometric properties of a material, and thus fulfill this objective. Focused ion beam (FIB) serial sectioning allows us to find the true 3-D microstructure of Ni-base superalloys. Once the true 3-D microstructure is obtained, an accurate quantitative description and characterization of precipitate and/or grain shapes is needed to understand the microstructure and describe it in an unbiased way. In this thesis, second order moment invariants, the shape quotient Q, a convexity measure relating the volume of an object to the volume of its convex hull, V/Vconv, and Gaussian curvature have been used to compare an experimentally observed polycrystalline IN100 microstructure to three synthetic microstructures. The three synthetic microstructures used different shape classes to produce starting grain shapes. The three shape classes are ellipsoids, superellipsoids, and the shapes generated when truncating a cube with an octahedron. The microstructures are compared using a distance measure, the Hellinger distance. The Hellinger distance is used to compare distributions of shape descriptors for the grains in each microstructure. The synthetic microstructure that has the smallest Hellinger distance, and so best matched the experimentally observed microstructure is the microstructure that used superellipsoids as a starting grain shape. While it has the smallest Hellinger distance, and is approaching realistic grain morphologies, the superellipsoidal microstructure is still not realistic. Second order moment invariants, Q, and V/V conv have also been used to characterize the γ' precipitate shapes from four experimental Ru-containing Ni-base superalloys with differences in alloying additions. The superalloys are designated UM-F9, UM-F18, UM-F19, and UM-F22. The

  9. Thermal stability and environmental compatibility of Inconel 617

    International Nuclear Information System (INIS)

    Kimball, O.F.

    1989-01-01

    The thermal stability and environmental compatibility of Inconel 617, a prime nuclear process heat steam reformer candidate alloy, are described in this paper. This commercially available wrought nickel-base alloy has excellent high-temperature strength but is subject to loss of toughness and ductility due to thermal instability. Work done to improve the thermal stability of this alloy is discussed. Room-temperature tensile and toughness data and microstructural information for Inconel 617 specimens exposed at elevated temperatures are presented. Preliminary data indicate that controlling the chemistry of Inconel 617 can provide a substantial improvement in thermal stability. Preliminary work to define the range of high-temperature gas-cooled reactor (HTGR) primary coolant compositions within which minimal deleterious gas/metal reactions occur with Inconel 617 is described. Within this gas chemistry range a stable surface oxide forms and only slight carburization occurs. In other gas chemistry ranges, rapid carburization or decarburization can occur. The gas corrosion experiments discussed are part of a series of relatively short-term exposures to HTGR helium in which the effects of different H 2 O concentrations (0.01 to 1.0 Pa) were determined as a function of the systematic variation of a second constituent (CO and CH 4 for this work) in the test gas. The composition of the basic HTGR helium was 40 Pa H 2 , 4 Pa CO, 0.02 Pa CO 2 , 2 Pa CH 4 in helium at 0.2 MPa. Two other CO levels (1 and 12 Pa) and one additional CH 4 level (0.63 Pa) were used in these experiments. Experimental exposure methods are discussed and the results of gas-metal interaction studies are presented. These results include carbon analyses and optical and scanning electron microscopy to determine the morphology and type of surface and subsurface microstructures. (author). 15 refs, 6 figs, 5 tabs

  10. Influence Of The Laser Cladding Strategies On The Mechanical Properties Of Inconel 718

    International Nuclear Information System (INIS)

    Lamikiz, A.; Tabernero, I.; Ukar, E.; Lopez de Lacalle, L. N.; Delgado, J.

    2011-01-01

    This work presents different experimental results of the mechanical properties of Inconel registered 718 test parts built-up by laser cladding. Recently, turbine manufacturers for aeronautical sector have presented high interest on laser cladding processes. This process allows building fully functional structures on superalloys, such as Inconel registered 718, with high flexibility on complex shapes. However, there is limited data on mechanical properties of the laser cladding structures. Moreover, the available data do not include the influence of process parameters and laser cladding strategies. Therefore, a complete study of the influence of the laser cladding parameters and mainly, the variation of the tensile strength with the laser cladding strategy is presented. The results show that there is a high directionality of mechanical properties, depending on the strategies of laser cladding process. In other words, the test parts show a fiber -like structure that should be considered on the laser cladding strategy selection.

  11. Niobium-base superalloys via powder metallurgy technology

    International Nuclear Information System (INIS)

    Loria, E.A.

    1987-01-01

    This paper provides some insight into an area that has been neglected, namely the possibility of developing high-strength, niobium-base alloys by improved oxidation resistance via the consolidation of rapidly solidified powders. Powder metallurgy (P/M) is an attractive processing technique because of its flexibility and versatility, and it may provide the alloys with properties and workability not obtainable via metal casting. A critical review of both U.S. and Russian literature is presented along with suggestions on the most promising compositions and processing techniques available to meet these competing goals. Previous work on many niobium alloys reveals that long term properties are retained well above those obtained on nickel-base superalloys. Cast and wrought alloys extend specific strength beyond 1200 0 C (2200 0 F), but lack oxidation resistance. Remarkable oxidation resistance is obtained, however, on miniature castings of certain ternary alloys which are too brittle for any processing. A better understanding of the oxidation mechanism is necessary before the proper P/M (RST) approach is taken on compositions which could provide compatibility between the two competing goals through grain refinement and a homogeneous distribution of the contributory phases. Finally, ways to up-scale production of Nb powder are discussed, including thermodynamic feasibility for the direct reduction of NbCl/sub 5/ in a 1.5 MW plasma reactor

  12. Study on the hot corrosion behavior of a cast Ni-base superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Wang, W.; Guo, J.T.; Zhang, J.; Yuan, C.; Zhou, L.Z.; Hu, Z.Q. [Chinese Academy of Sciences, Shenyang (China). Inst. of Metal Research

    2010-07-01

    Hot corrosion behavior of Nickel-base cast superalloy K447 in 90% Na{sub 2}SO{sub 4} + 10% NaCl melting salt at 850 C and 900 C was studied. The hot corrosion kinetic of the alloy follows parabolic rate law under the experimental conditions. The external layer is mainly Cr{sub 2}O{sub 3} scale which is protective to the alloy, the intermediate layer is the Ti-rich phase, and the internal layer is mainly the international oxides and sulfides. With increased corrosion time and temperature, the oxide scales are gradually dissolved in the molten salt and then precipitate as a thick and non-protective scale. Chlorides cause the formation of volatile species, which makes the oxide scale disintegrate and break off. The corrosion kinetics and morphology examinations tend to support the basic dissolution model for hot corrosion mechanisms. (orig.)

  13. TEM microstructural analysis of creep deformed CM186LC single crystal Ni-base superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Dubiel, B.; Czyrska-Filemonowicz, A. [AGH Univ. of Science and Technology, Krakow (Poland); Blackler, M. [Howmet Ltd., Exeter (United Kingdom); Barnard, P.M. [ALSTOM Power Turbo-Systems Technology Centre, Rugby (United Kingdom)

    2006-07-01

    The nickel based single crystal superalloy CM186LC was extensively investigated as a potential low cost material for industrial gas turbine vanes within the COST522 programme. The alloy exhibits inhomogeneous structure consisting of dendritic regions and eutectic colonies. In the present work attention is focused on microstructural changes observed in single crystal CM186LC following creep deformation at 750 C. Creep tests were conducted at 750 C with an applied stress of 560 or 675 MPa for up to 11440 hours. The microstructure o ruptured and terminated specimens was investigated by scanning (SEM) and transmission (TEM) electron microscopy. TEM analysis revealed the microstructural changes in the CM186LC at primary and secondary creep as well as after creep rupture. (orig.)

  14. Solute redistribution and Rayleigh number in the mushy zone during directional solidifi cation of Inconel 718

    Directory of Open Access Journals (Sweden)

    Wang Ling

    2009-08-01

    Full Text Available The interdendritic segregation along the mushy zone of directionally solidifi ed superalloy Inconel 718 has been measured by scanning electron microscope (SEM and energy dispersion analysis spectrometry (EDAXtechniques and the corresponding liquid composition profile was presented. The liquid density and Rayleigh number (Ra profi les along the mushy zone were calculated as well. It was found that the liquid density difference increased from top to bottom in the mushy zone and there was no density inversion due to the segregation of Nb and Mo. However carbide formation in the freezing range and the preferred angle of the orientated dendrite array could prompt the fl uid fl ow in the mushy zone although there was no liquid density inversion. The largest relative Rayleigh number appeared at 1,326 篊 for Inconel 718 where the fl uid fl ow most easily occurred.

  15. Microstructural causes of negative creep in cast superalloys

    International Nuclear Information System (INIS)

    Frank, G.

    1990-01-01

    The dissertation examines by means of microstructural investigations and modelling calculations two types of superalloys: the nickel-base cast alloy IN 738 LC (γ'-hardened, containing MC and M 23 C 6 carbides), and the cobalt-base cast alloy FSX 414 (containing M 23 C 6 carbides, solid solution-hardened). The task was to determine the causes of microstructural volume contraction, in order to improve and facilitate explanation and extrapolation of the materials' long-term behaviour at high temperatures, and to derive if possible information on appropriate measures preventing negative creep, which may lead to critical damage of bolted joints, for instance. (orig./MM) [de

  16. Structure and Properties of the Aluminide Coatings on the Inconel 625 Superalloy

    Science.gov (United States)

    Adamiak, Stanisław; Bochnowski, Wojciech; Dziedzic, Andrzej; Filip, Ryszard; Szeregij, Eugeniusz

    2016-01-01

    The research samples used in this study were based on the Inconel 625 alloy; the examined samples were coated with aluminide films deposited in a low-activity chemical vapor deposition (CVD) process. The samples' microstructure was investigated with optical and electron microscopy and energy dispersive X-ray spectroscopy analysis. Hardness measurements were performed using Vickers and Berkovich test methods. The adhesion of the aluminide coating was determined by fractography. It was shown that the fracture mechanism was different for the respective zones of the aluminide coating and the substrate material. The outer zone of the aluminide coating is characterized by an intercrystalline fracture, with a small contribution of transcrystalline fracture within individual grains (large crystallites in the bottom of the zone, composed of smaller crystallites, also show an intercrystalline fracture). The substrate material exhibited a ductile intercrystalline fracture. Based on this investigation, an increase of the microhardness of the material occurring at loads below 0.2 N was observed. When determining microhardness of aluminide coating it is necessary to take into account the optimal choice of the indentation tip.

  17. Creep Behaviour of Modified Mar-247 Superalloy

    Directory of Open Access Journals (Sweden)

    Cieśla M.

    2016-06-01

    Full Text Available The paper presents the results of analysis of creep behaviour in short term creep tests of cast MAR-247 nickel-based superalloy samples made using various modification techniques and heat treatment. The accelerated creep tests were performed under temperature of 982 °C and the axial stresses of σ = 150 MPa (variant I and 200 MPa (variant II. The creep behaviour was analysed based on: creep durability (creep rupture life, steady-state creep rate and morphological parameters of macro- and microstructure. It was observed that the grain size determines the creep durability in case of test conditions used in variant I, durability of coarse-grained samples was significantly higher.

  18. Aleación superficial de superaleaciones base níquel mediante láser

    OpenAIRE

    Rodríguez, G. P.; García, I.; Damborenea, J. J.

    1998-01-01

    Ni based superalloys present a high oxidation resistance at high temperature as well as good mechanical properties. But new tecnhology developments forcé to research in this materials to improve their properties at high temperature. In this work, two Ni based superalloys (Nimonic 80A and Inconel 600) were surface alloyed with aluminium using a high power laser. SEM and EDX were used to study the microstructure of the obtained coatings. Alloyed specimens were tested at 1.273 K between 24 and 2...

  19. A Review on Inertia and Linear Friction Welding of Ni-Based Superalloys

    Science.gov (United States)

    Chamanfar, Ahmad; Jahazi, Mohammad; Cormier, Jonathan

    2015-04-01

    Inertia and linear friction welding are being increasingly used for near-net-shape manufacturing of high-value materials in aerospace and power generation gas turbines because of providing a better quality joint and offering many advantages over conventional fusion welding and mechanical joining techniques. In this paper, the published works up-to-date on inertia and linear friction welding of Ni-based superalloys are reviewed with the objective to make clarifications on discrepancies and uncertainties reported in literature regarding issues related to these two friction welding processes as well as microstructure, texture, and mechanical properties of the Ni-based superalloy weldments. Initially, the chemical composition and microstructure of Ni-based superalloys that contribute to the quality of the joint are reviewed briefly. Then, problems related to fusion welding of these alloys are addressed with due consideration of inertia and linear friction welding as alternative techniques. The fundamentals of inertia and linear friction welding processes are analyzed next with emphasis on the bonding mechanisms and evolution of temperature and strain rate across the weld interface. Microstructural features, texture development, residual stresses, and mechanical properties of similar and dissimilar polycrystalline and single crystal Ni-based superalloy weldments are discussed next. Then, application of inertia and linear friction welding for joining Ni-based superalloys and related advantages over fusion welding, mechanical joining, and machining are explained briefly. Finally, present scientific and technological challenges facing inertia and linear friction welding of Ni-based superalloys including those related to modeling of these processes are addressed.

  20. Numerical multi-criteria optimization methods for alloy design. Development of new high strength nickel-based superalloys and experimental validation

    Energy Technology Data Exchange (ETDEWEB)

    Rettig, Ralf; Mueller, Alexander; Ritter, Nils C.; Singer, Robert F. [Institute of Science and Technology of Metals, Department of Materials Science and Engineering, University of Erlangen (Germany)

    2016-07-01

    A new approach for the design of optimum balanced metallic alloys is presented. It is based on a mathematical multi-criteria optimization method which uses different property models to predict the alloy behavior in dependency of composition. These property models are mostly based on computational thermodynamics (CALPHAD-method). The full composition range of the alloying elements can be considered using these models. In alloy design usually several contradicting goals have to be fulfilled. This is handled by the calculation of so-called Pareto-fronts. The aim of our approach is to guide the experimental research towards new alloy compositions that have a high probability of having very good properties. Consequently the number of required test alloys can be massively reduced. The approach will be demonstrated for the computer-aided design of a new Re-free superalloy with nearly identical creep strength as that of Re-containing superalloys. Our starting point for the design was to maintain the good properties of the gamma prime-phase in well-known alloys like CMSX-4 and to maximize the solid solution strengthening of W and Mo. The presented experimental measurements proof the excellent properties.

  1. X-ray phase analysis of nickel superalloys

    International Nuclear Information System (INIS)

    Khayutin, S.G.

    2004-01-01

    An X-ray diffraction technique for determining phase composition is proposed for an intermetallic system of NiAl-Ni 3 Al and is based on the comparison of X-ray interference line intensity for two phases. Its application to heat resistant intermetallic coatings of nickel base alloys has restrictions associated with coatings nonhomogeneity in thickness. These restrictions are noted to be not essential if the reflecting layer thickness does not exceed the thickness of a chemically homogeneous layer in the coating [ru

  2. Characterisation of As-deformed microstructure of ODS NI-Base superalloy and ODS ferritic steel prior to directional recrystallisation

    International Nuclear Information System (INIS)

    Baloch, M.M.; Memon, S.A.

    2007-01-01

    The materials studied are unusual in the sense that they have been prepared from mechanically alloyed procedures, including compaction and hot extrusion. It was felt necessary to characterise the initial microstructure thoroughly prior to directional recrystallisation of the alloys. Following consolidation by hot extrusion, dispersion strengthened superalloys appear to display a very fine sub-micron grain size consisting of both dislocation free recrystallised material and un- recrystallised regions of high dislocation density. It is found that there is a very fine dislocation cell structure in the ODS (Oxide Dispersion Strengthened) Ferritic stainless Steel prior to recrystallisation treatment, which shows that alloy is in old-deformed condition after mechanical alloying, extrusion I hot-working. This is in contrast to the mechanically alloyed Nickel Base Superalloy, which have consistently been found to be in primary recrystallisation state following extrusion. In order to understand the recrystallisation behaviour of the two mechanically illoyed materials with commercial designations MA6000 and MA956, a measurement of the orientation relationship between adjacent grains in the as- deformed ODS alloys has also been carried out using Transmission Electron microscope. (author)

  3. Mechanical characterization of superalloys for space reactors

    International Nuclear Information System (INIS)

    Duchesne, J.

    1989-01-01

    The aim of this work is the selection of structural materials that can be used in the temperature range 600-900 0 C for a gas cooled space reactor producing electricity. Superalloys fit best the temperature range required. Five nickel base alloys are chosen for their good mechanical behaviour: HAYNES 230, HASTELLOY S, HASTELLOY X, HASTELLOY XR and PYRAD 38D. Metallography, tensile and hardness tests are realized. Sample contraction is evidenced for some creep tests, under low stress: 20MPa at 800 0 C, on HAYNES 230 and HASTELLOY X, probably related to the structural evolution of these materials corresponding to a decrease of the crystal parameter [fr

  4. Microstructural study of weld fusion zone of TIG welded IN 738LC nickel-based superalloy

    International Nuclear Information System (INIS)

    Ojo, O.A.; Richards, N.L.; Chaturvedi, M.C.

    2004-01-01

    The weld fusion zone microstructure of a commercial aerospace superalloy IN 738 was examined. Elemental segregation induced interdendritic microconstituents were identified to include terminal solidification product M 3 B 2 and Ni 7 Zr 2 in association with γ-γ' eutectic constituent, which require proper consideration during the development of optimum post weld heat treatment

  5. An Abnormal Increase of Fatigue Life with Dwell Time during Creep-Fatigue Deformation for Directionally Solidified Ni-Based Superalloy DZ445

    Science.gov (United States)

    Ding, Biao; Ren, Weili; Deng, Kang; Li, Haitao; Liang, Yongchun

    2018-03-01

    The paper investigated the creep-fatigue behavior for directionally solidified nickel-based superalloy DZ445 at 900 °C. It is found that the fatigue life shows an abnormal increase when the dwell time exceeds a critical value during creep-fatigue deformation. The area of hysteresis loop and fractograph explain the phenomenon quite well. The shortest life corresponds to the maximal area of hysteresis loop, i. e. the maximum energy to be consumed during the creep-fatigue cycle. The fractographic observation of failed samples further supports the abnormal behavior of fatigue life.

  6. σ and η Phase formation in advanced polycrystalline Ni-base superalloys

    Energy Technology Data Exchange (ETDEWEB)

    Antonov, Stoichko, E-mail: santonov@hawk.iit.edu [Illinois Institute of Technology, 10 W. 32nd Street, Chicago, IL 60616 (United States); Huo, Jiajie; Feng, Qiang [State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083 (China); Isheim, Dieter; Seidman, David N. [Department of Materials Science and Engineering, Northwestern University, 2220 Campus Drive, Evanston, IL 60208 (United States); Northwestern University Center for Atom Probe Tomography (NUCAPT), 2220 Campus Drive, Evanston, IL 60208 (United States); Helmink, Randolph C.; Sun, Eugene [Rolls-Royce Corporation, 450 S. Meridian Street, Indianapolis, IN 46225 (United States); Tin, Sammy [Illinois Institute of Technology, 10 W. 32nd Street, Chicago, IL 60616 (United States)

    2017-02-27

    In polycrystalline Ni-base superalloys, grain boundary precipitation of secondary phases can be significant due to the effects they pose on the mechanical properties. As new alloying concepts for polycrystalline Ni-base superalloys are being developed to extend their temperature capability, the effect of increasing levels of Nb alloying additions on long term phase stability and the formation of topologically close packed (TCP) phases needs to be studied. Elevated levels of Nb can result in increased matrix supersaturation and promote the precipitation of secondary phases. Long term thermal exposures on two experimental powder processed Ni-base superalloys containing various levels of Nb were completed to assess the stability and precipitation of TCP phases. It was found that additions of Nb promoted the precipitation of η-Ni{sub 6}AlNb along the grain boundaries in powder processed, polycrystalline Ni-base superalloys, while reduced Nb levels favored the precipitation of blocky Cr and Mo – rich σ phase precipitates along the grain boundary. Evaluation of the thermodynamic stability of these two phases in both alloys using Thermo-calc showed that while σ phase predictions are fairly accurate, predictions of the η phase are limited.

  7. Erosion-corrosion behaviour of Ni-based superalloy Superni-75 in the real service environment of the boiler

    Energy Technology Data Exchange (ETDEWEB)

    Sidhu, T.S.; Prakash, S.; Agrawal, R.D.; Bhagat, R. [Shaheed Bhagat Singh College of Engineering & Technology, Ferozepur (India)

    2009-04-15

    The super-heater and re-heater tubes of the boilers used in thermal power plants are subjected to unacceptable levels of surface degradation by the combined effect of erosion-corrosion mechanism, resulting in the tube wall thinning and premature failure. The nickel-based superalloys can be used as boiler tube materials to increase the service life of the boilers, especially for the new generation ultra-supercritical boilers. The aim of the present investigation is to evaluate the erosion-corrosion behaviour of Ni-based superalloy Superni-75 in the real service environment of the coal-fired boiler of a thermal power plant. The cyclic experimental study was performed for 1000 h in the platen superheater zone of the coal-fired boiler where the temperature was around 900{sup o}C. The corrosion products have been characterized with respect to surface morphology, phase composition and element concentration using the combined techniques of X-ray diffractometry (XRD), scanning electron microscopy/energy-dispersive analysis (SEM/EDAX) and electron probe micro analyser (EPMA). The Superni-75 performed well in the coal-fired boiler environment, which has been attributed mainly to the formation of a thick band of chromium in scale due to selective oxidation of the chromium.

  8. Evolution of precipitate in nickel-base alloy 718 irradiated with argon ions at elevated temperature

    International Nuclear Information System (INIS)

    Jin, Shuoxue; Luo, Fengfeng; Ma, Shuli; Chen, Jihong; Li, Tiecheng; Tang, Rui; Guo, Liping

    2013-01-01

    Alloy 718 is a nickel-base superalloy whose strength derives from γ′(Ni 3 (Al,Ti)) and γ″(Ni 3 Nb) precipitates. The evolution of the precipitates in alloy 718 irradiated with argon ions at elevated temperature were examined via transmission electron microscopy. Selected-area electron diffraction indicated superlattice spots disappeared after argon ion irradiation, which showing that the ordered structure of the γ′ and γ″ precipitates became disordered. The size of the precipitates became smaller with the irradiation dose increasing at 290 °C

  9. Effect of tensile mean stress on fatigue behavior of single-crystal and directionally solidified superalloys

    Science.gov (United States)

    Kalluri, Sreeramesh; Mcgaw, Michael A.

    1990-01-01

    Two nickel base superalloys, single crystal PWA 1480 and directionally solidified MAR-M 246 + Hf, were studied in view of the potential usage of the former and usage of the latter as blade materials for the turbomachinery of the space shuttle main engine. The baseline zero mean stress (ZMS) fatigue life (FL) behavior of these superalloys was established, and then the effect of tensile mean stress (TMS) on their FL behavior was characterized. At room temperature these superalloys have lower ductilities and higher strengths than most polycrystalline engineering alloys. The cycle stress-strain response was thus nominally elastic in most of the fatigue tests. Therefore, a stress range based FL prediction approach was used to characterize both the ZMS and TMS fatigue data. In the past, several researchers have developed methods to account for the detrimental effect of tensile mean stress on the FL for polycrystalline engineering alloys. However, the applicability of these methods to single crystal and directionally solidified superalloys has not been established. In this study, these methods were applied to characterize the TMS fatigue data of single crystal PWA 1480 and directionally solidified MAR-M 246 + Hf and were found to be unsatisfactory. Therefore, a method of accounting for the TMS effect on FL, that is based on a technique proposed by Heidmann and Manson was developed to characterize the TMS fatigue data of these superalloys. Details of this method and its relationship to the conventionally used mean stress methods in FL prediction are discussed.

  10. The contrasting roles of creep and stress relaxation in the time-dependent deformation during in-situ cooling of a nickel-base single crystal superalloy.

    Science.gov (United States)

    Panwisawas, Chinnapat; D'Souza, Neil; Collins, David M; Bhowmik, Ayan

    2017-09-11

    Time dependent plastic deformation in a single crystal nickel-base superalloy during cooling from casting relevant temperatures has been studied using a combination of in-situ neutron diffraction, transmission electron microscopy and modelling. Visco-plastic deformation during cooling was found to be dependent on the stress and constraints imposed to component contraction during cooling, which mechanistically comprises creep and stress relaxation. Creep results in progressive work hardening with dislocations shearing the γ' precipitates, a high dislocation density in the γ channels and near the γ/γ' interface and precipitate shearing. When macroscopic contraction is restricted, relaxation dominates. This leads to work softening from a decreased dislocation density and the presence of long segment stacking faults in γ phase. Changes in lattice strains occur to a similar magnitude in both the γ and γ' phases during stress relaxation, while in creep there is no clear monotonic trend in lattice strain in the γ phase, but only a marginal increase in the γ' precipitates. Using a visco-plastic law derived from in-situ experiments, the experimentally measured and calculated stresses during cooling show a good agreement when creep predominates. However, when stress relaxation dominates accounting for the decrease in dislocation density during cooling is essential.

  11. Control of the kerf size and microstructure in Inconel 738 superalloy by femtosecond laser beam cutting

    Energy Technology Data Exchange (ETDEWEB)

    Wei, J.; Ye, Y.; Sun, Z. [Department of Mechanical Engineering, Tsinghua University, Beijing (China); Liu, L., E-mail: liulei@tsinghua.edu.cn [The State Key Laboratory of Tribology, Tsinghua University, Beijing (China); Zou, G., E-mail: sunzhg@tsinghua.edu.cn [Department of Mechanical Engineering, Tsinghua University, Beijing (China)

    2016-05-01

    Highlights: • Effects of processing parameters on the kerf size in Inconel 738 are investigated. • Defocus is a key parameter affecting the kerf width due to the intensity clamping. • The internal surface microstructures with different scanning speed are presented. • The material removal mechanism contains normal vaporization and phase explosion. • Oxidation mechanism is attributed to the trapping effect of the dangling bonds. - Abstract: Femtosecond laser beam cutting is becoming widely used to meet demands for increasing accuracy in micro-machining. In this paper, the effects of processing parameters in femtosecond laser beam cutting on the kerf size and microstructure in Inconel 738 have been investigated. The defocus, pulse width and scanning speed were selected to study the controllability of the cutting process. Adjusting and matching the processing parameters was a basic enhancement method to acquire well defined kerf size and the high-quality ablation of microstructures, which has contributed to the intensity clamping effect. The morphology and chemical compositions of these microstructures on the cut surface have been characterized by a scanning electron microscopy equipped with an energy dispersive X-ray spectroscopy, X-ray diffraction and X-ray photoelectron spectroscopy. Additionally, the material removal mechanism and oxidation mechanism on the Inconel 738 cut surface have also been discussed on the basis of the femtosecond laser induced normal vaporization or phase explosion, and trapping effect of the dangling bonds.

  12. Comparative Thermal Aging Effects on PM-HIP and Forged Inconel 690

    Science.gov (United States)

    Bullens, Alexander L.; Bautista, Esteban; Jaye, Elizabeth H.; Vas, Nathaniel L.; Cain, Nathan B.; Mao, Keyou; Gandy, David W.; Wharry, Janelle P.

    2018-03-01

    This study compares thermal aging effects in Inconel 690 (IN690) produced by forging and powder metallurgy with hot isostatic pressing (PM-HIP). Isothermal aging is carried out over 400-800°C for up to 1000 h and then metallography and nanoindentation are utilized to relate grain microstructure with hardness and yield strength. The PM-HIP IN690 maintains a constant grain size through all aging conditions, while the forged IN690 exhibits limited grain growth at the highest aging temperature and longest aging time. The PM-HIP IN690 exhibits comparable mechanical integrity as the forged material throughout aging: hardness and yield strength are unchanged with 100 h aging, but increase after 1000 h aging at all temperatures. In both the PM-HIP and forged IN690, the Hall-Petch relationship for Ni-based superalloys predicts yield strength for 0-100 h aged specimens, but underestimates yield strength in the 1000 h aged specimens because of thermally induced precipitation.

  13. Identification of acoustic emission sources in early stages of fatigue process of Inconel 713LC

    Energy Technology Data Exchange (ETDEWEB)

    Bartkova, Denisa; Vlasic, Frantisek; Mazal, Pavel [Brno Univ. of Technology, Brno (Czech Republic). Faculty of Mechanical Engineering

    2014-11-01

    Inconel 713LC is low carbon variant of Inconel 713 nickel-based cast alloy. The biggest advantage of these alloys is their ability to resist a wide variety of operating conditions (corrosive environment, high temperature, high stresses). Main area of applications is aircraft, energetic, chemical and petrochemical industry etc. In many applications, components undergo cyclic stresses. This study presents results of acoustic emission response of Inconel 713LC during high-cycle fatigue testing. In comparison with low-cycle fatigue, stage of initiation of micro cracks is in high-cycle region much more significant and can take several tens of percent of whole fatigue life. This work is focused on comparison of selected parameters of acoustic emission signal in pre-initiation and initiation stage of fatigue crack creation. Signal data were specified by linear location technique, hence only signal from shallow notch was analysed. Acoustic emission signal was correlated with frequency of load reversals which is a function of specimen's rigidity (modulus). Acoustic emission hits with higher stress were detected in pre-initiation stage whereas initiation stage hits exhibited low stress. Acoustic emission signal measurements are supplemented by fractographic and metallographic analysis.

  14. Thermal cycling influence on microstructural characterization of alloys with high nickel content

    International Nuclear Information System (INIS)

    Abrudeanu, M.; Gradin, O.; Vulpe, S. C.; Ohai, D.

    2013-01-01

    The IV nuclear energy generation systems are aimed at making revolutionary improvements in economics, safety and reliability, and sustainability. To achieve these goals, Generation IV systems will operate at higher temperatures and in higher radiation fields. This paper shows the thermal cycling influences on microstructure and hardness of nickel based alloys: Incoloy 800 HT and Inconel 617. These alloys were meekly at a thermal cycling of 25, 50, 75 and 100 cycles. The temperature range of a cycle was between 400 O C and 700 O C. Nickel base alloys develop their properties by solid solution and/or precipitation strengthening. (authors)

  15. Effect of Squareness of Initial γ' Precipitates on Creep-Rupture Life of a Ni-Base Single Crystal Superalloy at 760/982 °C

    Science.gov (United States)

    Shi, Zhenbin; Peng, Zhifang; Luo, Yushi; Xie, Hongji; Jin, Haipeng; Zhao, Yunsong; Mei, Qingsong

    2018-05-01

    An approach to determination of squareness of initial γ' precipitates (S 2D) is proposed to evaluate its effect on creep-rupture life (t r) of nickel-base single crystal (SC) superalloys. It is found that the 760/982 °C rupture life varied with the change in regional S 2D caused by redistribution of W when 1st-step aging temperature changed in full heat treatment on superalloy DD83 investigated. The longest creep-rupture life occurred at the highest value/the lowest difference in S 2D in the interdendritic regions/between the typical dendritic regions in DD83. It is also found that S 2D is a weighted function of the area fraction (F 2D), spacing (h), and size (d) of γ' precipitates and is closely related to t r in a series of SC superalloys. In addition, the variation of S 2D with F 2D (here, thermodynamic mole fraction is approximately expressed by F 2D) through lattice misfit (δ) in the SC superalloys with F 2D ranging from 60 to 75 pct is well correlated. Therefore, to reveal and to better understand these relationships and correlations may help to optimize the phase variables in order to achieve a long rupture life of SC superalloys. In addition, functions to reveal the interrelationships of F 2D, volume fraction (F 3D), S 2D, and cuboidness (S 3D) of initial γ' precipitates are derived considering their shape changes. All of these are hoped to be helpful in practical applications and in understanding the true meaning of the related variables.

  16. Design criteria for rhenium-reduced nickel-based single-crystal alloys. Identification and computer-assisted conversion

    International Nuclear Information System (INIS)

    Goehler, Thomas

    2016-01-01

    In the present work, design criteria and property models for the creep strength optimization of rhenium-free nickel based single crystal Superalloys are investigated. The study focuses on a typical load condition of 1050 C and 150 MPa, which is representative for flight engine applications. Thereby the key aspect is to link chemical composition, manufacturing processes, microstructure formation and mechanistic understanding of dislocation creep through a computational materials engineering approach. Beside the positive effect of rhenium on solid solution hardening, a second mechanism in which rhenium increases high temperature creep strength is identified. It indirectly stabilizes precipitation hardening by reducing the coarsening kinetics of γ'-rafting. Five 1st and 2nd generation technical Superalloys show a comparable microstructure evolution for up to 2 % plastic elongation, while creep times differ by a factor of five. The application of a microstructure sensitive creep model shows that these coarsening processes can activate γ-cutting and thus lead to an increasing creep rate. Based on these calculations a threshold value of φ γ/γ' > 2,5 at 150 MPa is estimated. This ratio of matrix channel to raft thickness has been proofed for multiple positions by microstructure analysis of interrupted creep tests. The mechanism described previously can be decelerated by the enrichment of the γ-matrix with slow diffusing elements. The same principle also increases the solid solution strength of the γ-matrix. Therefore, the present work delivers an additional mechanistic explanation why creep properties of single phase nickel based alloys can be transferred to two phase technical Superalloys with rafted γ'-structure. Following, the best way to substitute both rhenium fundamental properties, namely a slow diffusion coefficient and a small solubility in g', has been investigated by means of CALPHAD-modeling. Only molybdenum and especially tungsten

  17. Modeling Long-term Creep Performance for Welded Nickel-base Superalloy Structures for Power Generation Systems

    Energy Technology Data Exchange (ETDEWEB)

    Shen, Chen

    2015-01-01

    We report here a constitutive model for predicting long-term creep strain evolution in’ strengthened Ni-base superalloys. Dislocation climb-bypassing’, typical in intermediate’ volume fraction (~20%) alloys, is considered as the primary deformation mechanism. Dislocation shearing’ to anti-phase boundary (APB) faults and diffusional creep are also considered for high-stress and high-temperature low-stress conditions, respectively. Additional damage mechanism is taken into account for rapid increase in tertiary creep strain. The model has been applied to Alloy 282, and calibrated in a temperature range of 1375-1450°F, and stress range of 15-45ksi. The model parameters and a MATLAB code are provided. This report is prepared by Monica Soare and Chen Shen at GE Global Research. Technical discussions with Dr. Vito Cedro are greatly appreciated. This work was supported by DOE program DE-FE0005859

  18. The metallurgy of superalloys part 1

    International Nuclear Information System (INIS)

    Abdelazim, M.E.; Hammad, F.H.

    1990-01-01

    This is part I of the report titled 'the metallurgy of superalloys'. In this part the structure, phases and systems of superalloys are reviewed. The role of alloying elements in the design of superalloys and the mechanical properties of superalloys are also reviewed. Superalloys are important in high temperature technology, especially above 700 degree c. They are 'super' mainly because their creep and stress rupture resistances are very high. Superalloys are based on an austenitic matrix including secondary phases, mainly gamma precipitates, inter and intragranular carbides mainly M 23 C 6 and M 6 C. They are classified into three systems, Ni-base, Fe-Ni base and Ce-base alloys. Different alloying elements mainly Cr, Mo, Al, Ti are added to increase the strength either by solid solution hardening (Cr, Mo, Al), precipitation hardening (A 1, Ti to produce gamma) or by dispersion hardening (Cr, Mo to form M 23 C 6 and M 6 C carbides) and to increase the oxidation resistance (Cr, Al). 3 tab., 2 fig

  19. Selective laser melting of Inconel super alloy-a review

    Science.gov (United States)

    Karia, M. C.; Popat, M. A.; Sangani, K. B.

    2017-07-01

    Additive manufacturing is a relatively young technology that uses the principle of layer by layer addition of material in solid, liquid or powder form to develop a component or product. The quality of additive manufactured part is one of the challenges to be addressed. Researchers are continuously working at various levels of additive manufacturing technologies. One of the significant powder bed processes for met als is Selective Laser Melting (SLM). Laser based processes are finding more attention of researchers and industrial world. The potential of this technique is yet to be fully explored. Due to very high strength and creep resistance Inconel is extensively used nickel based super alloy for manufacturing components for aerospace, automobile and nuclear industries. Due to law content of Aluminum and Titanium, it exhibits good fabricability too. Therefore the alloy is ideally suitable for selective laser melting to manufacture intricate components with high strength requirements. The selection of suitable process for manufacturing for a specific component depends on geometrical complexity, production quantity, and cost and required strength. There are numerous researchers working on various aspects like metallurgical and micro structural investigations and mechanical properties, geometrical accuracy, effects of process parameters and its optimization and mathematical modeling etc. The present paper represents a comprehensive overview of selective laser melting process for Inconel group of alloys.

  20. Use of indexed sensitivity factors in the analysis of nickel and iron based alloys: study of the decalibration of sheathed Chromel/Alumel thermocouples

    International Nuclear Information System (INIS)

    Christie, W.H.

    1978-01-01

    Sheathed Chromel versus Alumel thermocouples decalibrate when exposed to temperatures in excess of 1100 0 C. Thermocouples sheathed in Inconel-600 and type 304 stainless steel were studied in this work. Quantified SIMS data showed that the observed decalibrations were due to significant alterations that took place in the Chromel and Alumel thermoelements. The amount of alteration was different for each thermocouple and was influenced by the particular sheath material used in the thermocouple construction. Relative sensitivity factors, indexed by a matrix ion species ratio, were used to quantify SIMS data for three nickel-based alloys, Chromel, Alumel, and Inconel-600, and an iron-based alloy, type 304 stainless steel. Oxygen pressure >2 x 10 -6 torr in the sputtering region gave enhanced sensitivity and superior quantitative results as compared to data obtained at instrumental residual pressure

  1. Crack initiation modeling of a directionally-solidified nickel-base superalloy

    Science.gov (United States)

    Gordon, Ali Page

    Combustion gas turbine components designed for application in electric power generation equipment are subject to periodic replacement as a result of cracking, damage, and mechanical property degeneration that render them unsafe for continued operation. In view of the significant costs associated with inspecting, servicing, and replacing damaged components, there has been much interest in developing models that not only predict service life, but also estimate the evolved microstructural state of the material. This thesis explains manifestations of microstructural damage mechanisms that facilitate fatigue crack nucleation in a newly-developed directionally-solidified (DS) Ni-base superalloy components exposed to elevated temperatures and high stresses. In this study, models were developed and validated for damage and life prediction using DS GTD-111 as the subject material. This material, proprietary to General Electric Energy, has a chemical composition and grain structure designed to withstand creep damage occurring in the first and second stage blades of gas-powered turbines. The service conditions in these components, which generally exceed 600°C, facilitate the onset of one or more damage mechanisms related to fatigue, creep, or environment. The study was divided into an empirical phase, which consisted of experimentally simulating service conditions in fatigue specimens, and a modeling phase, which entailed numerically simulating the stress-strain response of the material. Experiments have been carried out to simulate a variety of thermal, mechanical, and environmental operating conditions endured by longitudinally (L) and transversely (T) oriented DS GTD-111. Both in-phase and out-of-phase thermo-mechanical fatigue tests were conducted. In some cases, tests in extreme environments/temperatures were needed to isolate one or at most two of the mechanisms causing damage. Microstructural examinations were carried out via SEM and optical microscopy. A continuum

  2. High temperature creep properties of directionally solidified CM-247LC Ni-based superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Chiou, Mau-Sheng [Department of Materials Science and Engineering, I-Shou University, Kaohsiung 840, Taiwan (China); Jian, Sheng-Rui, E-mail: srjian@gmail.com [Department of Materials Science and Engineering, I-Shou University, Kaohsiung 840, Taiwan (China); Yeh, An-Chou [Department of Materials Science and Engineering, National Tsing Hua University, Hsinchu 300, Taiwan (China); Kuo, Chen-Ming [Department of Mechanical and Automation Engineering, I-Shou University, Kaohsiung 840, Taiwan (China); Juang, Jenh-Yih [Department of Electrophysics, National Chiao Tung University, Hsinchu 300, Taiwan (China)

    2016-02-08

    This study explores the effects of cooling rate after solution heat treatment on the high temperature/low stress (982 °C/200 MPa) creep properties of CM-247LC Nickel base superalloy. Cooling rate was controlled by blowing argon gas, air cooling, and furnace cooling, which, in turn, gave rise to corresponding cooling rates (from 1260 °C to 800 °C) of 18.7, 7.4, and 0.19 °C/s, respectively. The results indicated that higher cooling rate from the solution heat treatment temperature led to finer γ′ precipitates and much improved tertiary creep as well as rupture life time in high-temperature creep test. The microstructural analyses using both scanning electron microscopy (SEM) and transmission electron microscopy (TEM) revealed that finer γ′ precipitates and narrower γ channel width could result in denser rafting structure which might have hindered the climb of dislocations across the precipitates rafts.

  3. Microstructural characterization of thermal barrier coating on Inconel 617 after high temperature oxidation

    Directory of Open Access Journals (Sweden)

    Mohammadreza Daroonparvar

    2013-06-01

    Full Text Available A turbine blade was protected against high temperature corrosion and oxidation by thermal barrier coatings (TBCsusing atmospheric plasma spraying technique (APS on a Ni-based superalloy (Inconel 617. The coatings (NiCr6AlY/ YSZ and NiCr10AlY/YSZ consist of laminar structure with substantial interconnected porosity transferred oxygen from Yittria stabilized Zirconia (YSZ layer toward the bond coat (NiCrAlY. Hence, a thermally grown oxide layer (TGO was formed on the metallic bond coat and internal oxidation of the bond coat occurred during oxidation. The TBC systems were oxidized in a normal electrically heated furnace at 1150 °C for 18, 22, 26, 32 and 40h.Microstructural characterization of coatings demonstrated that the growth of the TGO layer on the nickel alloy with 6wt. % Al is more rapid than TGO with 10wt. % Al. In addition, many micro-cracks were observed at the interface of NiCr6AlY/YSZ. X-ray diffraction analysis (XRD showed the existence of detrimental oxides such as NiCr2O4, NiCrO3 and NiCrO4 in the bond coat containing 6wt. % Al, accompanied by rapid volume expansion causing the destruction of TBC. In contrast, in the bond coat with 10wt. % Al, NiO, Al2O3and Cr2O3 oxides were formed while very low volume expansion occurred. The oxygen could not penetrate into the TGO layer of bond coat with 10 wt. % Al during high temperature oxidation and the detrimental oxides were not extensively formed within the bond coat as more oxygen was needed. The YSZ with higher Al content showed higher oxidation resistance.

  4. An experimental assessment on the performance of different lubrication techniques in grinding of Inconel 751.

    Science.gov (United States)

    Balan, A S S; Vijayaraghavan, L; Krishnamurthy, R; Kuppan, P; Oyyaravelu, R

    2016-09-01

    The application of emulsion for combined heat extraction and lubrication requires continuous monitoring of the quality of emulsion to sustain a desired grinding environment; this is applicable to other grinding fluids as well. Thus to sustain a controlled grinding environment, it is necessary to adopt an effectively lubricated wheel-work interface. The current study was undertaken to assess experimentally the ​ effects of different grinding environments such as dry, minimum quantity lubrication (MQL) and Cryo-MQL on performance, such as grinding force, temperature, surface roughness and chip morphology on Inconel 751, a higher heat resistance material posing thermal problems and wheel loading. The results show that grinding with the combination of both liquid nitrogen (LN2) and MQL lowers temperature, cutting forces, and surface roughness as compared with MQL and dry grinding. Specific cutting energy is widely used as an inverse measure of process efficiency in machining. It is found from the results that specific cutting energy of Cryo-MQL assisted grinding is 50-65% lower than conventional dry grinding. The grindability of Inconel 751 superalloy can be enhanced with Cryo-MQL condition.

  5. Time-temperature influence on the corrosion resistance of Ni-Cr-Nb superalloys in contact with Na2SO4-V2O5 molten mixtures

    International Nuclear Information System (INIS)

    Otero, E.; Pardo, A.; Hernaez, J.; Hierro, P.

    1990-01-01

    Corrosion rate data obtained by the polarization resistance method in nickel-base superalloys in contact with Na 2 SO 4 -V 2 O 5 molten mixtures are presented. The instrumental technique is also described. Time-temperature influence on the corrosion kinetics in the described conditions is discussed (Author)

  6. High Temperature Degradation of Powder-processed Ni-based Superalloy

    Czech Academy of Sciences Publication Activity Database

    Luptáková, Natália; Pizúrová, Naděžda; Roupcová, Pavla; Dymáček, Petr

    2015-01-01

    Roč. 22, č. 2 (2015), s. 85-94 ISSN 1335-0803 Institutional support: RVO:68081723 Keywords : powder materials * polycrystalline Ni-based superalloy * creep machine grips * oxidation Subject RIV: JG - Metallurgy

  7. Thermal Analysis in the Technological “Step” Test of H282 Nickel Alloy

    Directory of Open Access Journals (Sweden)

    Pirowski Z.

    2015-03-01

    Full Text Available Superalloys show a good combination of mechanical strength and resistance to surface degradation under the influence of chemically active environments at high temperature. They are characterized by very high heat and creep resistance. Their main application is in gas turbines, chemical industry, and in all those cases where resistance to creep and the aggressive corrosion environment is required. Modern jet engines could never come into use if not for progress in the development of superalloys. Superalloys are based on iron, nickel and cobalt. The most common and the most interesting group includes superalloys based on nickel. They carry loads at temperatures well in excess of the eighty percent of the melting point. This group includes the H282 alloy, whose nominal chemical composition is as follows (wt%: Ni - base, Fe - max. 1.5%, Al - 1.5% Ti - 2.1%, C - 0.06% Co - 10% Cr - 20% Mo - 8.5%. This study shows the results of thermal analysis of the H282 alloy performed on a cast step block with different wall thickness. Using the results of measurements, changes in the temperature of H282 alloy during its solidification were determined, and the relationship dT / dt = f (t was derived. The results of the measurements taken at different points in the cast step block allowed identifying a number of thermal characteristics of the investigated alloy and linking the size of the dendrites formed in a metal matrix (DAS with the thermal effect of solidification. It was found that the time of solidification prolonged from less than ome minute at 10 mm wall thickness to over seven minutes at the wall thickness of 44 mm doubled the value of DAS.

  8. Oxidation of Inconel 625 superalloy upon treatment with oxygen or hydrogen plasma at high temperature

    Czech Academy of Sciences Publication Activity Database

    Vesel, A.; Drenik, A.; Elersic, K.; Mozetič, M.; Kovač, J.; Gyergyek, T.; Stöckel, Jan; Varju, Jozef; Pánek, Radomír; Balat-Pichelin, M.

    2014-01-01

    Roč. 305, June (2014), s. 674-682 ISSN 0169-4332 R&D Projects: GA MŠk(CZ) LM2011021 Institutional support: RVO:61389021 Keywords : Inconel * Oxidation * High temperature * Oxygen plasma * Hydrogen plasma Subject RIV: BL - Plasma and Gas Discharge Physics OBOR OECD: Fluids and plasma physics (including surface physics) Impact factor: 2.711, year: 2014 https://www.sciencedirect.com/science/article/pii/S0169433214007119

  9. Phase-transformation and subgrain-deformation characteristics in a cobalt-based superalloy

    International Nuclear Information System (INIS)

    Benson, M.L.; Reetz, B.; Liaw, P.K.; Reimers, W.; Choo, H.; Brown, D.W.; Saleh, T.A.; Klarstrom, D.L.

    2011-01-01

    Research highlights: → The mechanical behavior of a cobalt-based superalloy was investigated. → Two diffraction techniques were used to study deformation mechanisms of materials. → In-situ neutron diffraction provides the volume-averaged information. → The peak-profile analysis reveals the information on a subgrain level. → The material exhibited a transformation texture for the HCP phase under loading. - Abstract: A complimentary set of experiments, in situ neutron diffraction and ex situ synchrotron X-ray diffraction, were used to study the phase-transformation and subgrain-deformation characteristics of a cobalt-based superalloy. The neutron diffraction indicated a strain-induced phase transformation in the cobalt-based superalloy under uniaxial tension and compression. The synchrotron X-ray diffraction revealed stacking-fault accumulation and twinning under the same loading conditions. The extent of transformation was found to be greater under tension than under compression. Tensile plastic strains below 2% were accommodated by the stacking-fault creation, while those greater than 2% were accommodated by the phase transformation. Twinning was found to be more active under compressive loading than under tensile loading.

  10. MC Carbide Characterization in High Refractory Content Powder-Processed Ni-Based Superalloys

    Science.gov (United States)

    Antonov, Stoichko; Chen, Wei; Huo, Jiajie; Feng, Qiang; Isheim, Dieter; Seidman, David N.; Sun, Eugene; Tin, Sammy

    2018-04-01

    Carbide precipitates in Ni-based superalloys are considered to be desirable phases that can contribute to improving high-temperature properties as well as aid in microstructural refinement of the material; however, they can also serve as crack initiation sites during fatigue. To date, most of the knowledge pertaining to carbide formation has originated from assessments of cast and wrought Ni-based superalloys. As powder-processed Ni-based superalloys are becoming increasingly widespread, understanding the different mechanisms by which they form becomes increasingly important. Detailed characterization of MC carbides present in two experimental high Nb-content powder-processed Ni-based superalloys revealed that Hf additions affect the resultant carbide morphologies. This morphology difference was attributed to a higher magnitude of elastic strain energy along the interface associated with Hf being soluble in the MC carbide lattice. The composition of the MC carbides was studied through atom probe tomography and consisted of a complex carbonitride core, which was rich in Nb and with slight Hf segregation, surrounded by an Nb carbide shell. The characterization results of the segregation behavior of Hf in the MC carbides and the subsequent influence on their morphology were compared to density functional theory calculations and found to be in good agreement, suggesting that computational modeling can successfully be used to tailor carbide features.

  11. Failure mechanisms of superhard materials when cutting superalloys

    International Nuclear Information System (INIS)

    Focke, A.E.; Westermann, F.E.; Ermi, A.; Yavelak, J.; Hoch, M.

    1975-01-01

    The present research studies the reasons for the failure of tungsten carbide tools while cutting superalloys. There is a continuous layer of the superalloy in the bottom of the crater which from time to time is torn away locally, taking tungsten carbide crystal with it. Under recommended cutting conditions a plateau (unworn cutting surface) separates the crater from the cutting edge of the tool when cutting AISI 4340. This plateau is totally absent in all cutting of Inconel 718, even in short, two-minute tests. The crater intersects the cutting edge--only a thin wedge of carbide is left which either breaks off or deforms and wears very rapidly. Temperature measurements carried out by use of an infrared detector aimed on the corner of the tungsten carbide indicate at recommended speeds a sharp rise of the temperature at the beginning of the cutting operation, then a steady-state very slow increase as the cutting continues, and finally just before tool failure a very rapid increase in the temperature again. Scanning and replica electron microscopy through the crater and flank face shows that both under the crater and in the back of the cutting edge a fairly deep layer of ''disturbed metal'' exists in which the tungsten carbide grains are much smaller and have much more rounded edges than in the original material. 10 figures, 4 tables

  12. MGI-oriented High-throughput Measurement of Interdiffusion Coefficient Matrices in Ni-based Superalloys

    Directory of Open Access Journals (Sweden)

    TANG Ying

    2017-01-01

    Full Text Available One of the research hotspots in the field of high-temperature alloys was to search the substitutional elements for Re in order to prepare the single-crystal Ni-based superalloys with less or even no Re addition. To find the elements with similar or even lower diffusion coefficients in comparison with that of Re was one of the effective strategies. In multicomponent alloys, the interdiffusivity matrix were used to comprehensively characterize the diffusion ability of any alloying elements. Therefore, accurate determination of the composition-dependant and temperature-dependent interdiffusivities matrices of different elements in γ and γ' phases of Ni-based superalloys was high priority. The paper briefly introduces of the status of the interdiffusivity matrices determination in Ni-based superalloys, and the methods for determining the interdiffusivities in multicomponent alloys, including the traditional Matano-Kirkaldy method and recently proposed numerical inverse method. Because the traditional Matano-Kirkaldy method is of low efficiency, the experimental reports on interdiffusivity matrices in ternary and higher order sub-systems of the Ni-based superalloys were very scarce in the literature. While the numerical inverse method newly proposed in our research group based on Fick's second law can be utilized for high-throughput measurement of accurate interdiffusivity matrices in alloys with any number of components. After that, the successful application of the numerical inverse method in the high-throughput measurement of interdiffusivity matrices in alloys is demonstrated in fcc (γ phase of the ternary Ni-Al-Ta system. Moreover, the validation of the resulting composition-dependant and temperature-dependent interdiffusivity matrices is also comprehensively made. Then, this paper summarizes the recent progress in the measurement of interdiffusivity matrices in γ and γ' phases of a series of core ternary Ni-based superalloys achieved in

  13. Requirements of Inconel 718 alloy for aeronautical applications

    Science.gov (United States)

    Ghiban, Brandusa; Elefterie, Cornelia Florina; Guragata, Constantin; Bran, Dragos

    2018-02-01

    The main requirements imposed by aviation components made from super alloys based on Nickel are presented in present paper. A significant portion of fasteners, locking lugs, blade retainers and inserts are manufactured from Inconel 718 alloy. The thesis describes environmental factors (corrosion), conditions of external aggression (salt air, intense heat, heavy industrial pollution, high condensation, high pressure), mechanical characteristics (tensile strength, creep, density, yield strength, fracture toughness, fatigue resistance) and loadings (tensions, compression loads) that must be satisfied simultaneously by Ni-based super alloy, compared to other classes of aviation alloys (as egg. Titanium alloys, Aluminum alloys). For this alloy the requirements are strength, durability, damage tolerance, fail safety and so on. The corrosion can be an issue, but the fatigue under high-magnitude cyclic tensile loading it what limits the lifetime of the airframe. The excellent malleability and weldability characteristics of the 718 system make the material physical properties tolerant of manufacturing processes. These characteristics additionally continue to provide new opportunities for advanced manufacturing methods.

  14. Comparative Studies on Microstructure, Mechanical and Pitting Corrosion of Post Weld Heat Treated IN718 Superalloy GTA and EB Welds

    Science.gov (United States)

    Dilkush; Mohammed, Raffi; Madhusudhan Reddy, G.; Srinivasa Rao, K.

    2018-03-01

    In the present study, an attempt has been made to weld Inconel 718 nickel-base superalloy (IN718 alloy) using gas tungsten arc welding (GTAW) and electron beam welding (EBW) processes. Both the weldments were subjected to post-weld heat treatment condition as follows -980°C / 20 min followed by direct aging condition (DA) as 720°C/8 h/FC followed by 620°C/8 h/AC. The GTA and EB welds of IN718 alloy were compared in two conditions as-received and 980STA conditions. Welds were characterized to observe mechanical properties, pitting corrosion resistance by correlating with observed microstructures. The rate of higher cooling ranges, the fusion zone of EBW exhibited discrete and relative finer lave phases whereas the higher niobium existed laves with coarser structure were observed in GTAW. The significant dissolution of laves were observed at 980STA of EBW. Due to these effects, the EBW of IN718 alloy showed the higher mechanical properties than GTAW. The electrochemical potentiostatic etch test was carried out in 3.5wt% sodium chloride (NaCl) solution to study the pitting corrosion behaviour of the welds. Results of the present investigation established that mechanical properties and pitting corrosion behaviour are significantly better in post weld heat treated condition. The comparative studies showed that the better combination of mechanical properties and pitting corrosion resistance were obtained in 980STA condition of EBW than GTAW.

  15. Innovative technologies for powder metallurgy-based disk superalloys: Progress and proposal

    Science.gov (United States)

    Chong-Lin, Jia; Chang-Chun, Ge; Qing-Zhi, Yan

    2016-02-01

    Powder metallurgy (PM) superalloys are an important class of high temperature structural materials, key to the rotating components of aero engines. In the purview of the present challenges associated with PM superalloys, two novel approaches namely, powder preparation and the innovative spray-forming technique (for making turbine disk) are proposed and studied. Subsequently, advanced technologies like electrode-induction-melting gas atomization (EIGA), and spark-plasma discharge spheroidization (SPDS) are introduced, for ceramic-free superalloy powders. Presently, new processing routes are sought after for preparing finer and cleaner raw powders for disk superalloys. The progress of research in spray-formed PM superalloys is first summarized in detail. The spray-formed superalloy disks specifically exhibit excellent mechanical properties. This paper reviews the recent progress in innovative technologies for PM superalloys, with an emphasis on new ideas and approaches, central to the innovation driving techniques like powder processing and spray forming. Project supported by the National Natural Science Foundation of China (Grant Nos. 50974016 and 50071014).

  16. Life Prediction of Low Cycle Fatigue for Ni-base Superalloy GTD111 DS at Elevated Temperature

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Jin Yeol; Yoon, Dong Hyun; Kim, Jae Hoon [Chungnam Nat’l Univ., Daejeon (Korea, Republic of); Bae, Si Yeon; Chang, Sung Yong; Chang, Sung Ho [KEPCO Research Institute, Daejeon (Korea, Republic of)

    2017-08-15

    GTD111 DS of nickel base superalloy has been used for gas turbine blades. In this study, low cycle fatigue test was conducted on the GTD111 DS alloy by setting conditions similar to the real operating environment. The low cycle fatigue tests were conducted at room temperature, 760 °C, 870 °C, and various strain amplitudes. Test results showed that fatigue life decreased with increasing total strain amplitude. Cyclic hardening response was observed at room temperature and 760 °C; however, tests conducted at 870 °C showed cyclic softening response. Stress relaxation was observed at 870 °C because creep effects occurred from holding time. A relationship between fatigue life and total strain range was obtained from the Coffin-Manson method. The fratography using a SEM was carried out at the crack initiation and propagation regions.

  17. Microstructural Changes during High Temperature Service of a Cobalt-Based Superalloy First Stage Nozzle

    Directory of Open Access Journals (Sweden)

    A. Luna Ramírez

    2016-01-01

    Full Text Available Superalloys are a group of alloys based on nickel, iron, or cobalt, which are used to operate at high temperatures (T > 540°C and in situations involving very high stresses like in gas turbines, particularly in the manufacture of blades, nozzles, combustors, and discs. Besides keeping its high resistance to temperatures which may approach 85% of their melting temperature, these materials have excellent corrosion resistance and oxidation. However, after long service, these components undergo mechanical and microstructural degradation; the latter is considered a major cause for replacement of the main components of gas turbines. After certain operating time, these components are very expensive to replace, so the microstructural analysis is an important tool to determine the mode of microstructure degradation, residual lifetime estimation, and operating temperature and most important to determine the method of rehabilitation for extending its life. Microstructural analysis can avoid catastrophic failures and optimize the operating mode of the turbine. A case study is presented in this paper.

  18. Effect of homogenization heat treatments on the cast structure and tensile properties of nickel-base superalloy ATI 718Plus in the presence of boron and zirconium additions

    Energy Technology Data Exchange (ETDEWEB)

    Hosseini, Seyed Ali, E-mail: saliho3ini@gmail.com; Madar, Karim Zangeneh; Abbasi, Seyed Mehdi

    2017-03-24

    The effect of homogenization heat treatment on cast structure, hardness, and tensile properties of the nickel-based superalloy 718plus in the presence of boron and zirconium additives were investigated. For this purpose, five alloys with different contents of boron (0.00–0.016 wt%) and zirconium (0.0–0.1 wt%) were cast by double vacuum process VIM/VAR and then were homogenized at 1075–1175 °C for 5–25 h. Microstructural investigation by OM and SEM and phase analysis by XRD were done and then hardness and high temperature tensile tests were performed on the homogenized alloys. The results show that the amount of the Laves phase is reduced by increases in time and temperature of homogenization. It was also found that increases in duration of homogenization at 1075 °C results in improving strength and ductility, while duration increase at 1175 °C is accompanied with degradation of them, which caused the reduction of needle-like delta phase on grain boundaries. Boron and zirconium had negative effects on the strength and ductility of the alloy by increasing the amount of Laves in the cast structure. By increasing these elements in alloy composition, more time is needed in order to fully eliminate the Laves by homogenization treatment.

  19. Effect of standard heat treatment on the microstructure and mechanical properties of hot isostatically pressed superalloy inconel 718

    International Nuclear Information System (INIS)

    Rao, G. Appa; Kumar, Mahendra; Srinivas, M.; Sarma, D.S.

    2003-01-01

    Ni-Fe base superalloy, Inconel 718, was processed through powder metallurgy (P/M) hot isostatic pressing (HIP) route. In order to balance the strength and ductility, the HIPed material was given the standard heat treatment, viz. solution treatment at 980 deg. C for 1 h/water quenched (WQ) to room temperature and a two-step ageing treatment consisting of 720 deg. C for 8 h/furnace cooling (FC) at 55 deg. C h -1 to 620 deg. C and holding at 620 deg. C for 8 h before air cooling (AC) to room temperature. Optical microscopy and scanning electron microscopy (SEM) studies on the heat treated alloy have shown a homogeneous microstructure with fine grain size (25 μm) along with the presence of prior particle boundary (PPB) networks. Transmission electron microscopy (TEM) on the heat treated material has revealed the presence of oxides, MC carbides and δ-precipitates at the grain boundaries and a uniform precipitation of fine γ'' and γ' strengthening phases in the matrix. Tensile and stress rupture tests were performed on the heat treated material. While the yield strength (YS) and ultimate tensile strength (UTS) of the HIPed and heat treated alloy at room temperature and 650 deg. C were comparable to those of conventionally processed wrought IN 718, its ductility was lower. The stress rupture life of the HIPed alloy improved marginally due to heat treatment and met the minimum specification requirement of life hours but the rupture ductility was found to be inferior to that of the wrought material. The fractography of the failed samples has revealed the transgranular ductile mode of fracture in the as-solution treated alloy, while intergranular mode of failure with the decohesion of PPBs occurred more predominantly in the aged condition. This change of fracture mode with ageing treatment shows the ductility dependence on the relative strength of the matrix and PPBs. The TEM studies on the deformed alloy have revealed that the brittle oxides and carbides at the prior

  20. The effect of thermal processing on microstructure and mechanical properties in a nickel-iron alloy

    Science.gov (United States)

    Yang, Ling

    The correlation between processing conditions, resulted microstructure and mechanical properties is of interest in the field of metallurgy for centuries. In this work, we investigated the effect of thermal processing parameters on microstructure, and key mechanical properties to turbine rotor design: tensile yield strength and crack growth resistance, for a nickel-iron based superalloy Inconel 706. The first step of the designing of experiments is to find parameter ranges for thermal processing. Physical metallurgy on superalloys was combined with finite element analysis to estimate variations in thermal histories for a large Alloy 706 forging, and the results were adopted for designing of experiments. Through the systematic study, correlation was found between the processing parameters and the microstructure. Five different types of grain boundaries were identified by optical metallography, fractography, and transmission electron microscopy, and they were found to be associated with eta precipitation at the grain boundaries. Proportions of types of boundaries, eta size, spacing and angle respect to the grain boundary were found to be dependent on processing parameters. Differences in grain interior precipitates were also identified, and correlated with processing conditions. Further, a strong correlation between microstructure and mechanical properties was identified. The grain boundary precipitates affect the time dependent crack propagation resistance, and different types of boundaries have different levels of resistance. Grain interior precipitates were correlated with tensile yield strength. It was also found that there is a strong environmental effect on time dependent crack propagation resistance, and the sensitivity to environmental damage is microstructure dependent. The microstructure with eta decorated on grain boundaries by controlled processing parameters is more resistant to environmental damage through oxygen embrittlement than material without eta

  1. Implementation of a structural dependent model for the superalloy IN738LC in ABAQUS-code

    International Nuclear Information System (INIS)

    Wolters, J.; Betten, J.; Penkalla, H.J.

    1994-05-01

    Superalloys, mainly consisting of nickel, are used for applications in aerospace as well as in stationary gas turbines. In the temperature range above 800 C the blades, which are manufactured of these superalloys, are subjected to high centrifugal forces and thermal induced loads. For computer based analysis of the thermo-mechanical behaviour of the blades models for the stress-strain behaviour are necessary. These models have to give a reliable description of the stress-strain behaviour, with emphasis on inelastic affects. The implementation of the model in finite element codes requires a numerical treatment of the constitutive equations with respect to the given interface of the used code. In this paper constitutive equations for the superalloy IN738LC are presented and the implementation in the finite element code ABAQUS with the numerical preparation of the model is described. In order to validate the model calculations were performed for simple uniaxial loading conditions as well as for a complete cross section of a turbine blade under combined thermal and mechanical loading. The achieved results were compared with those of additional calculations by using ABAQUS, including Norton's law, which was already implemented in this code. (orig.) [de

  2. Anisotropic constitutive equations for the viscoplastic behaviour of the single crystal superalloy CMSX-4

    International Nuclear Information System (INIS)

    Fleury, G.; Schubert, F.

    1997-09-01

    Nickel-base superalloy blades of the first rotor stage in a gas turbine have to withstand extremely severe thermomechanical loading conditions. Single crystal blades exhibit a highly anisotropic deformation behaviour and are subjected to triaxial stress fields induced by complex cooling systems. Consequently the prediction of their deformation behaviour requires constitutive equations based on multiaxial formulations. The microstructural evolution of γ/γ' superalloys during the service time modifies the material properties and has therefore to be taken into account in the constitutive equations. For the modelling of the anisotropic, viscoplastic behaviour of single crystal blades taking into account the evolution of the microstructure, a microstructure-dependent, orthotropic Hills potential, whose anisotropy coefficients are connected to the edge length of the γ'-particles, is applied. The prediction was validated by investigating the deformation behaviour of the superalloy CMSX-4 in the range of temperatures [750 C-950 C]. If the shape of γ'-particles remain cubic, for example, in creep testing at low temperatures (up to about 850 C), the microstructure-dependent potential leads to the cubic version of the Hills potential. The prediction is in good agreement with creep results for left angle 001 right angle - and left angle 111 right angle - orientated specimens but overestimates the creep resistance of left angle 011 right angle - orientated specimens. (orig.)

  3. Evaluation of the material’s damage in gas turbine rotors by instrumented spherical indentation

    Directory of Open Access Journals (Sweden)

    D. Nappini

    2014-10-01

    Full Text Available Experimental indentations are carried out on items of two different materials, taken in several location of various components from high pressure gas turbine rotor which have seen an extensive service. The components object of investigation consisted in 1st and 2nd high pressure turbine wheels made in nickel-base superalloy (Inconel 718, the spacer ring (Inconel 718 and the compressor shaft made in CrMoV low alloy steel (ASTM A471 type10. Aim of the work is to set up the capability of the instrumented spherical indentation testing system to evaluate variations in the material properties due to damage, resulting from temperature field and stresses acting on components during service. To perform this task load-indentation depth curves will be acquired in various zones of the above mentioned components. The analysis of the results has allowed to identify an energy parameter which shows a linear evolution with the mean temperature acting on the components.

  4. Framatome technologies awarded nickel plating contract at St. Lucie

    International Nuclear Information System (INIS)

    Anon.

    1997-01-01

    Framatome Technologies is to perform nickel plating on 120 pressurizer heater sleeves at Florida Power and Light's St. Lucie unit 1 during the fall 1997 outage; replacement heaters, fabricated by Framatome, that use stainless steel for the heather sheath, will be installed. The nickel layer is deposited on the inside surface of the heater sleeves, which protects the Inconel 600 material and significantly reduces the intergranular stress-corrosion cracking, as proved in other US and European plants

  5. Microstructure and mechanical properties of the superalloy ATI Allvac 718Plus

    International Nuclear Information System (INIS)

    Zickler, Gerald A.; Schnitzer, Ronald; Radis, Rene; Hochfellner, Rainer; Schweins, Ralf; Stockinger, Martin; Leitner, Harald

    2009-01-01

    ATI Allvac 718Plus is a novel nickel-based superalloy, which was designed for heavy-duty applications in aerospace turbines. In the present study the high-resolution investigation techniques, atom probe tomography, electron microscopy and in situ high-temperature small-angle neutron scattering were used for a comprehensive microstructural characterization. The alloy contains nanometer-sized spherical γ' phase precipitates (Ni 3 (Al,Ti)) and plate-shaped δ phase precipitates (Ni 3 Nb) of micrometer size. The precipitation kinetics of the γ' phase can be described by a classical model for coarsening. The precipitation strongly influences the mechanical properties and is of high scientific and technological interest.

  6. An experimental assessment on the performance of different lubrication techniques in grinding of Inconel 751

    Directory of Open Access Journals (Sweden)

    A.S.S. Balan

    2016-09-01

    Full Text Available The application of emulsion for combined heat extraction and lubrication requires continuous monitoring of the quality of emulsion to sustain a desired grinding environment; this is applicable to other grinding fluids as well. Thus to sustain a controlled grinding environment, it is necessary to adopt an effectively lubricated wheel-work interface. The current study was undertaken to assess experimentally the ​ effects of different grinding environments such as dry, minimum quantity lubrication (MQL and Cryo-MQL on performance, such as grinding force, temperature, surface roughness and chip morphology on Inconel 751, a higher heat resistance material posing thermal problems and wheel loading. The results show that grinding with the combination of both liquid nitrogen (LN2 and MQL lowers temperature, cutting forces, and surface roughness as compared with MQL and dry grinding. Specific cutting energy is widely used as an inverse measure of process efficiency in machining. It is found from the results that specific cutting energy of Cryo-MQL assisted grinding is 50–65% lower than conventional dry grinding. The grindability of Inconel 751 superalloy can be enhanced with Cryo-MQL condition.

  7. An Analysis of Rheological Properties of Inconel 625 Superalloy Feedstocks Formulated with Backbone Binder Polypropylene System for Powder Injection Molding

    Directory of Open Access Journals (Sweden)

    Gökmen U.

    2017-12-01

    Full Text Available Binder formula is one of the most significant factors which has a considerable influence on powder injection molding (PIM processes. In the study, rheological behaviors and properties of different binder systems containing PIM feedstocks, Inconel 625 powder commonly used in space industry, were investigated. The feedstocks were prepared 59%-69% (volume powder loading ratios with three diversified binder systems by use of Polypropylene as backbone binder. The average particle size of the Inconel 625 powder used was 12.86 microns. Components used in the binder were mixed for 30 minutes as dry in three dimensional mixing to prepare binder systems. Rheological features of the feedstock were characterized by using a capillary rheometer. Viscosities of the feedstocks were calculated within the range of 37.996-1900 Pa.s based on the shear rate, shear stress, binder formula and temperature. “n” parameters for PIM feedstocks were determined to be less than 1. Influences of temperature on the viscosities of the feedstocks were also studied and “Ea” under various shear stresses were determined within the range of 24.41-70.89 kJ/mol.

  8. Low Cycle Fatigue of Single Crystal Nickel-based Superalloy DD6 at 1100℃

    Directory of Open Access Journals (Sweden)

    ZHANG Shichao

    2018-02-01

    Full Text Available The total strain-controlled low cycle fatigue(LCF behaviors of a single crystal superalloy DD6 at 1100℃ for R=-1 and 0.05 were investigated. The results of LCF tests indicated that the cyclic hardening/softening behavior of the alloy not only has the relationship with the microstructure of the material, but also the loading status. The mean stress relaxation occurred under asymmetric straining. The rate of mean stress relaxation increased with the increasing of strain amplitude; when R=-1, the alloy shows tension-compression asymmetry behavior. All the LCF data obtain under various ratios were well correlated by three models for lifetime prediction, the precision rates predicted are fallen into the factor of±2 times scatter band.

  9. Precipitate microstructure evolution in exposed IN738LC superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Strunz, Pavel, E-mail: strunz@ujf.cas.cz [Nuclear Physics Institute ASCR, CZ-25068 Řež near Prague (Czech Republic); Petrenec, Martin [Institute of Physics of Materials of the AS CR, Brno (Czech Republic); Gasser, Urs [Laboratory for Neutron Scattering, PSI, CH-5232 Villigen (Switzerland); Tobiáš, Jiří; Polák, Jaroslav [Institute of Physics of Materials of the AS CR, Brno (Czech Republic); Šaroun, Jan [Nuclear Physics Institute ASCR, CZ-25068 Řež near Prague (Czech Republic)

    2014-03-15

    Highlights: • Evolution of γ′-phase morphology in IN738LC Ni-base superalloy was examined by SANS. • In situ tests at high temperatures revealed trimodal precipitate distribution. • Formation, dissolution and (slow) kinetics of small γ′ precipitates was determined. • Equilibrium volume fraction of γ′ phase is significantly higher than 45%. • The small γ′ precipitates arise regardless the application of the mechanical load. -- Abstract: Nickel base superalloy IN738LC has been studied after low-cycle fatigue by Small Angle Neutron Scattering (SANS). Samples subjected to high-temperature low-cycle fatigue were annealed at various temperatures to change the size and the distribution of precipitates. Ex and in situ SANS and TEM studies were performed. It was found that additional precipitates are formed either during slow cooling from high temperatures or after reheating above 570 °C. Their size and distribution were evaluated. The precipitates arise regardless the application of the mechanical load. Nevertheless, these small precipitates influence low-cycle fatigue resistance. From the SANS data, it can be also deduced that the equilibrium volume fraction of γ′-precipitates at temperatures from room temperature to 825 °C is significantly higher than 45%. The kinetics of formation of small and medium-size γ′ precipitates at 700 and 800 °C was determined as well.

  10. Alloying effects of refractory elements in the dislocation of Ni-based single crystal superalloys

    Directory of Open Access Journals (Sweden)

    Shiyu Ma

    2016-12-01

    Full Text Available The alloying effects of W, Cr and Re in the [100] (010 edge dislocation cores (EDC of Ni-based single crystal superalloys are investigated using first-principles based on the density functional theory (DFT. The binding energy, Mulliken orbital population, density of states, charge density and radial distribution functions are discussed, respectively. It is clearly demonstrated that the addition of refractory elements improves the stability of the EDC systems. In addition, they can form tougher bonds with their nearest neighbour (NN Ni atoms, which enhance the mechanical properties of the Ni-based single crystal superalloys. Through comparative analysis, Cr-doped system has lower binding energy, and Cr atom has evident effect to improve the systemic stability. However, Re atom has the stronger alloying effect in Ni-based single crystal superalloys, much more effectively hindering dislocation motion than W and Cr atoms.

  11. Swelling in neutron irradiated nickel-base alloys

    International Nuclear Information System (INIS)

    Brager, H.R.; Bell, W.L.

    1972-01-01

    Inconel 625, Incoloy 800 and Hastelloy X were neutron irradiated at 500 to 700 0 C. It was found that of the three alloys investigated, Inconel 625 offers the greatest swelling resistance. The superior swelling resistance of Inconel 625 relative to that of Hastelloy-X is probably related to differences in the concentrations of the minor rather than major alloy constituents, and can involve (a) enhanced recombination of defects in the Inconel 625 and (b) preferential attraction of vacancies to incoherent precipitates. (U.S.)

  12. Evaluation of High Temperature Corrosion Resistance of Finned Tubes Made of Austenitic Steel And Nickel Alloys

    Directory of Open Access Journals (Sweden)

    Turowska A.

    2016-06-01

    Full Text Available The purpose of the paper was to evaluate the resistance to high temperature corrosion of laser welded joints of finned tubes made of austenitic steel (304,304H and nickel alloys (Inconel 600, Inconel 625. The scope of the paper covered the performance of corrosion resistance tests in the atmosphere of simulated exhaust gases of the following chemical composition: 0.2% HCl, 0.08% SO2, 9.0% O2 and N2 in the temperature of 800°C for 1000 hours. One found out that both tubes made of austenitic steel and those made of nickel alloy displayed good resistance to corrosion and could be applied in the energy industry.

  13. Stress corrosion cracking of several high strength ferrous and nickel alloys

    Science.gov (United States)

    Nelson, E. E.

    1971-01-01

    The stress corrosion cracking resistance of several high strength ferrous and nickel base alloys has been determined in a sodium chloride solution. Results indicate that under these test conditions Multiphase MP35N, Unitemp L605, Inconel 718, Carpenter 20Cb and 20Cb-3 are highly resistant to stress corrosion cracking. AISI 410 and 431 stainless steels, 18 Ni maraging steel (250 grade) and AISI 4130 steel are susceptible to stress corrosion cracking under some conditions.

  14. Evaluation of surface integrity of WEDM processed inconel 718 for jet engine application

    Science.gov (United States)

    Sharma, Priyaranjan; Tripathy, Ashis; Sahoo, Narayan

    2018-03-01

    A unique superalloy, Inconel 718 has been serving for aerospace industries since last two decades. Due to its attractive properties such as high strength at elevated temperature, improved corrosion and oxidation resistance, it is widely employed in the manufacturing of jet engine components. These components require complex shape without affecting the parent material properties. Traditional machining methods seem to be ineffective to fulfil the demand of aircraft industries. Therefore, an advanced feature of wire electrical discharge machining (WEDM) has been utilized to improve the surface features of the jet engine components. With the help of trim-offset technology, it became possible to achieve considerable amount of residual stresses, lower peak to valley height, reduced density of craters and micro globules, minimum hardness alteration and negligible recast layer formation.

  15. A Multiscale Understanding of the Thermodynamic and Kinetic Mechanisms of Laser Additive Manufacturing

    Directory of Open Access Journals (Sweden)

    Dongdong Gu

    2017-10-01

    Full Text Available Selective laser melting (SLM additive manufacturing (AM technology has become an important option for the precise manufacturing of complex-shaped metallic parts with high performance. The SLM AM process involves complicated physicochemical phenomena, thermodynamic behavior, and phase transformation as a high-energy laser beam melts loose powder particles. This paper provides multiscale modeling and coordinated control for the SLM of metallic materials including an aluminum (Al-based alloy (AlSi10Mg, a nickel (Ni-based super-alloy (Inconel 718, and ceramic particle-reinforced Al-based and Ni-based composites. The migration and distribution mechanisms of aluminium nitride (AlN particles in SLM-processed Al-based nanocomposites and the in situ formation of a gradient interface between the reinforcement and the matrix in SLM-processed tungsten carbide (WC/Inconel 718 composites were studied in the microscale. The laser absorption and melting/densification behaviors of AlSi10Mg and Inconel 718 alloy powder were disclosed in the mesoscale. Finally, the stress development during line-by-line localized laser scanning and the parameter-dependent control methods for the deformation of SLM-processed composites were proposed in the macroscale. Multiscale numerical simulation and experimental verification methods are beneficial in monitoring the complicated powder-laser interaction, heat and mass transfer behavior, and microstructural and mechanical properties development during the SLM AM process.

  16. Precipitation in solid solution and structural transformations in single crystals of high rhenium ruthenium-containing nickel superalloys at high-temperature creep

    Energy Technology Data Exchange (ETDEWEB)

    Alekseev, A.A.; Petrushin, N.V.; Zaitsev, D.V.; Treninkov, I.A.; Filonova, E.V. [All-Russian Scientific Research Institute of Aviation Materials (VIAM), Moscow (Russian Federation)

    2010-07-01

    The phase composition and structure of single crystals of two superalloys (alloy 1 and alloy 2) were investigated in this work. For alloy 1 (Re - 9 wt%) the kinetics of precipitation in solid solution at heat treatment (HT) was investigated. TEM and X-Ray examinations have revealed that during HT rhombic phase (R-phase) precipitation (Immm class (BCR)) occurs. The TTT diagram is plotted, it contains the time-temperature area of the existence of R-phase particles. The element content of R-phase is identified (at. %): Re- 51.5; Co- 23.5; Cr- 14.8; Mo- 4.2; W- 3.3; Ta- 2.7. For alloy 2 (Re - 6.5 wt %, Ru - 4 wt %) structural transformations at high-temperature creep are investigated. By dark-field TEM methods it is established, that in alloy 2 the additional phase with a rhombic lattice is formed during creep. Particles of this phase precipitate in {gamma}-phase and their quantity increases during high-temperature creep. It is revealed that during creep 3-D dislocation network is formed in {gamma}-phase. At the third stage of creep the process of inversion structure formation is observed in the alloy, i.e. {gamma}'-phase becomes a matrix. Thus during modeling creep the volume fraction of {gamma}'-phase in the samples increases from 30% (at creep duration of 200 hrs) up to 55% (at 500 hrs). The processes of structure formation in Re and Ru-containing nickel superalloys are strongly affected by decomposition of solid solution during high-temperature creep that includes precipitation of additional TCP-phases. (orig.)

  17. Fatigue Resistance of the Grain Size Transition Zone in a Dual Microstructure Superalloy Disk

    Science.gov (United States)

    Gabb, T. P.; Kantzos, P. T.; Telesman, J.; Gayda, J.; Sudbrack, C. K.; Palsa, B. S.

    2010-01-01

    Mechanical property requirements vary with location in nickel-based superalloy disks. To maximize the associated mechanical properties, heat treatment methods have been developed for producing tailored microstructures. In this study, a specialized heat treatment method was applied to produce varying grain microstructures from the bore to the rim portions of a powder metallurgy processed nickel-based superalloy disk. The bore of the contoured disk consisted of fine grains to maximize strength and fatigue resistance at lower temperatures. The rim microstructure of the disk consisted of coarse grains for maximum resistance to creep and dwell crack growth at high temperatures up to 704 C. However, the fatigue resistance of the grain size transition zone was unclear, and needed to be evaluated. This zone was located as a band in the disk web between the bore and rim. Specimens were extracted parallel and transverse to the transition zone, and multiple fatigue tests were performed at 427 and 704 C. Mean fatigue lives were lower at 427 C than for 704 C. Specimen failures often initiated at relatively large grains, which failed on crystallographic facets. Grain size distributions were characterized in the specimens, and related to the grains initiating failures as well as location within the transition zone. Fatigue life decreased with increasing maximum grain size. Correspondingly, mean fatigue resistance of the transition zone was slightly higher than that of the rim, but lower than that of the bore. The scatter in limited tests of replicates was comparable for all transition zone locations examined.

  18. Intermediate Co/Ni-base model superalloys — Thermophysical properties, creep and oxidation

    International Nuclear Information System (INIS)

    Zenk, Christopher H.; Neumeier, Steffen; Engl, Nicole M.; Fries, Suzana G.; Dolotko, Oleksandr; Weiser, Martin; Virtanen, Sannakaisa; Göken, Mathias

    2016-01-01

    The mechanical properties of γ′-strengthened Co–Ni–Al–W–Cr model superalloys extending from pure Ni-base to pure Co-base superalloys have been assessed. Differential scanning calorimetry measurements and thermodynamic calculations match well and show that the γ′ solvus temperature decreases with increasing Co-content. The γ/γ′ lattice misfit is negative on the Ni- and positive on the Co-rich side. High Ni-contents decelerate the oxidation kinetics up to a factor of 15. The creep strength of the Ni-base alloy increases by an order of magnitude with additions of Co before it deteriorates strongly upon higher additions despite an increasing γ′ volume fraction.

  19. Effect of Powder-Suspended Dielectric on the EDM Characteristics of Inconel 625

    Science.gov (United States)

    Talla, Gangadharudu; Gangopadhyay, S.; Biswas, C. K.

    2016-02-01

    The current work attempts to establish the criteria for powder material selection by investigating the influence of various powder-suspended dielectrics and machining parameters on various EDM characteristics of Inconel 625 (a nickel-based super alloy) which is nowadays regularly used in aerospace, chemical, and marine industries. The powders include aluminum (Al), graphite, and silicon (Si) that have significant variation in their thermo-physical characteristics. Results showed that powder properties like electrical conductivity, thermal conductivity, density, and hardness play a significant role in changing the machining performance and the quality of the machined surface. Among the three powders, highest material removal rate was observed for graphite powder due to its high electrical and thermal conductivities. Best surface finish and least radial overcut (ROC) were attained using Si powder. Maximum microhardness was found for Si due to its low thermal conductivity and high hardness. It is followed by graphite and aluminum powders. Addition of powder to the dielectric has increased the crater diameter due to expansion of plasma channel. Powder-mixed EDM (PMEDM) was also effective in lowering the density of surface cracks with least number of cracks obtained with graphite powder. X-ray diffraction analysis indicated possible formation of metal carbides along with grain growth phenomenon of Inconel 625 after PMEDM.

  20. Effect of tensile dwell on high-temperature low-cycle fatigue and fracture behaviour of cast superalloy MAR-M247

    Czech Academy of Sciences Publication Activity Database

    Šulák, Ivo; Obrtlík, Karel

    2017-01-01

    Roč. 185, NOV (2017), s. 92-100 ISSN 0013-7944. [ICMFM 2016 - International Colloquium on Mechanical Fatigue of Metals /18./. Gijón, 05.09.2016-07.09.2016] R&D Projects: GA ČR(CZ) GA15-20991S Institutional support: RVO:68081723 Keywords : Nickel-based superalloy * High-temperature low-cycle fatigue * Tensile dwell * Fatigue life * Damage mechanisms Subject RIV: JL - Materials Fatigue, Friction Mechanics OBOR OECD: Audio engineering , reliability analysis Impact factor: 2.151, year: 2016

  1. Formation of carbides and their effects on stress rupture of a Ni-base single crystal superalloy

    International Nuclear Information System (INIS)

    Liu, L.R.; Jin, T.; Zhao, N.R.; Sun, X.F.; Guan, H.R.; Hu, Z.Q.

    2003-01-01

    Creep tests of a nickel-base single crystal superalloy with minor C addition and non-carbon were carried out at different temperatures and stresses. Correlations between microstructural change and testing temperature and stress were enabled through scanning electron microscopy (SEM) and transmission electron microscopy (TEM), detailing the rafting microstucture and carbides precipitation. The results showed that minor carbon addition prolonged the second stage of creep strain curves and improved creep properties. Some carbide was precipitated during creep tests in modified alloy. M 23 C 6 carbide precipitated at lower temperature (871-982 deg. C), while (M 6 C) 2 carbide precipitated at higher temperature (>1000 deg. C), all of which was considered to be beneficial to creep properties. A small amount of MC carbide formed during solidification and its decomposition product (M 6 C) 1 were detrimental to mechanical properties, which together with micropores provided the site of initiation of cracks and led to the final fracture

  2. Hot Corrosion of Yttrium Stabilized Zirconia Coatings Deposited by Air Plasma Spray on a Nickel-Based Superalloy

    Science.gov (United States)

    Vallejo, N. Diaz; Sanchez, O.; Caicedo, J. C.; Aperador, W.; Zambrano, G.

    In this research, the electrochemical impedance spectroscopy (EIS) and Tafel analysis were utilized to study the hot corrosion performance at 700∘C of air plasma-sprayed (APS) yttria-stabilized zirconia (YSZ) coatings with a NiCrAlY bond coat grown by high velocity oxygen fuel spraying (HVOF), deposited on an INCONEL 625 substrate, in contact with corrosive solids salts as vanadium pentoxide V2O5 and sodium sulfate Na2SO4. The EIS data were interpreted based on proposed equivalent electrical circuits using a suitable fitting procedure performed with Echem AnalystTM Software. Phase transformations and microstructural development were examined using X-ray diffraction (XRD), with Rietveld refinement for quantitative phase analysis, scanning electron microscopy (SEM) was used to determinate the coating morphology and corrosion products. The XRD analysis indicated that the reaction between sodium vanadate (NaVO3) and yttrium oxide (Y2O3) produces yttrium vanadate (YVO4) and leads to the transformation from tetragonal to monoclinic zirconia phase.

  3. Total hemispherical emissivity of Inconel 718

    Energy Technology Data Exchange (ETDEWEB)

    Keller, Benjamin P.; Nelson, Shawn E.; Walton, Kyle L.; Ghosh, Tushar K.; Tompson, Robert V.; Loyalka, Sudarshan K., E-mail: LoyalkaS@missouri.edu

    2015-06-15

    Highlights: • We have measured the total hemispherical emissivity for Inconel 718 from about 600–1250 K. • Oxidation in air at 1073 K resulted in an increase in emissivity. • Sandblasting of Inconel 718 was also observed to increase the emissivity. • Coating of graphite powder onto the ‘as-received’ Inconel 718 showed no increase in the emissivity. • Coating of graphite powder onto the 220 grit sandblasted Inconel 718 did show an increase in emissivity. - Abstract: Total hemispherical emissivity for Inconel 718 was measured in anticipation of its application in Very High Temperature Gas Reactors (VHTRs). A majority of current emissivity data for Inconel 718 is in the form of spectral measurements. The data presented here were obtained with an experimental apparatus based on the standard ASTM C835-06 for total hemispherical emittance. Measurements of Inconel 718 were made for four different surface types including: (i) ‘as-received’ from the manufacturer, (ii) oxidized in air and humidified helium, (iii) sandblasted with aluminum oxide powder, and (iv) with a thin coating of nuclear grade graphite powder (grade NGB-18). The emissivity for the ‘as-received’ sample ranged from 0.21 to 0.28 in the temperature interval from 760 K to 1275 K. Oxidation in air at 1073 K resulted in an increase in emissivity into the range from 0.2 at 650 K to 0.52 at 1200 K. There was no dependence on the oxidation times studied here. Oxidation with humidified helium at 1073 K produced less of an increase in emissivity than the oxidation in air but there was an increase up to the range from 0.2 at 600 K to 0.35 at 1200 K. Sandblasting of Inconel 718 was also observed to increase the emissivity up to the range from 0.43 at 780 K to 0.53 at 1270 K when 60 grit sized powder was used and up to the range from 0.45 at 683 K to 0.57 at 1267 K when 120 and 220 grit sized powders were used. Coating of graphite powder onto the ‘as-received’ Inconel 718 showed no increase

  4. High-cycle fatigue behavior of Co-based superalloy 9CrCo at elevated temperatures

    OpenAIRE

    Wan, Aoshuang; Xiong, Junjiang; Lyu, Zhiyang; Li, Kuang; Du, Yisen; Chen, Kejiao; Man, Ziyu

    2016-01-01

    A modified model is developed to characterize and evaluate high-cycle fatigue behavior of Co-based superalloy 9CrCo at elevated temperatures by considering the stress ratio effect. The model is informed by the relationship surface between maximum nominal stress, stress ratio and fatigue life. New formulae are derived to deal with the test data for estimating the parameters of the proposed model. Fatigue tests are performed on Co-based superalloy 9CrCo subjected to constant amplitude loading a...

  5. Double minimum creep of single crystal Ni-base superalloys

    Czech Academy of Sciences Publication Activity Database

    WU, X.; Wollgramm, P.; Somsen, C.; Dlouhý, Antonín; Kostka, A.; Eggeler, G.

    2016-01-01

    Roč. 112, JUN (2016), s. 242-260 ISSN 1359-6454 R&D Projects: GA ČR(CZ) GA14-22834S Institutional support: RVO:68081723 Keywords : Single crystal Ni-base superalloys * Primary creep * Transmission electron microscopy * Dislocations * Stacking faults Subject RIV: JG - Metallurgy Impact factor: 5.301, year: 2016

  6. Nickel: makes stainless steel strong

    Science.gov (United States)

    Boland, Maeve A.

    2012-01-01

    Nickel is a silvery-white metal that is used mainly to make stainless steel and other alloys stronger and better able to withstand extreme temperatures and corrosive environments. Nickel was first identified as a unique element in 1751 by Baron Axel Fredrik Cronstedt, a Swedish mineralogist and chemist. He originally called the element kupfernickel because it was found in rock that looked like copper (kupfer) ore and because miners thought that "bad spirits" (nickel) in the rock were making it difficult for them to extract copper from it. Approximately 80 percent of the primary (not recycled) nickel consumed in the United States in 2011 was used in alloys, such as stainless steel and superalloys. Because nickel increases an alloy's resistance to corrosion and its ability to withstand extreme temperatures, equipment and parts made of nickel-bearing alloys are often used in harsh environments, such as those in chemical plants, petroleum refineries, jet engines, power generation facilities, and offshore installations. Medical equipment, cookware, and cutlery are often made of stainless steel because it is easy to clean and sterilize. All U.S. circulating coins except the penny are made of alloys that contain nickel. Nickel alloys are increasingly being used in making rechargeable batteries for portable computers, power tools, and hybrid and electric vehicles. Nickel is also plated onto such items as bathroom fixtures to reduce corrosion and provide an attractive finish.

  7. Effect of grain defects on the mechanical behavior of nickel-based single crystal superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Tang, Haibin; Guo, Haiding [Nanjing Univ. of Aeronautics and Astronautics (China). Jiangsu Province Key Lab. of Aerospace Power System

    2017-03-15

    In this paper, a single crystal (SC) partition model, consisting of primary grains and grain defects, is proposed to simulate the weakening effect of grain defects generated at geometric discontinuities of SC materials. The plastic deformation of SC superalloy is described with the modified yield criterion, associated flow rule and hardening law. Then a bicrystal model containing only one group of misoriented grains under uniaxial loading is constructed and analyzed in the commercial finite element software ABAQUS. The simulation results indicate that the yield strength and elastic modulus of misoriented grains, which are determined by the crystallographic orientation, have a significant effect on the stress distribution of the bicrystal model. A critical stress, which is calculated by the stress state at critical regions, is proposed to evaluate the local stress rise at the sub-boundary of primary and misoriented grains.

  8. Effect of grain defects on the mechanical behavior of nickel-based single crystal superalloy

    International Nuclear Information System (INIS)

    Tang, Haibin; Guo, Haiding

    2017-01-01

    In this paper, a single crystal (SC) partition model, consisting of primary grains and grain defects, is proposed to simulate the weakening effect of grain defects generated at geometric discontinuities of SC materials. The plastic deformation of SC superalloy is described with the modified yield criterion, associated flow rule and hardening law. Then a bicrystal model containing only one group of misoriented grains under uniaxial loading is constructed and analyzed in the commercial finite element software ABAQUS. The simulation results indicate that the yield strength and elastic modulus of misoriented grains, which are determined by the crystallographic orientation, have a significant effect on the stress distribution of the bicrystal model. A critical stress, which is calculated by the stress state at critical regions, is proposed to evaluate the local stress rise at the sub-boundary of primary and misoriented grains.

  9. High temperature properties of polycrystalline γ{sup '}-strengthened cobalt-base superalloys; Hochtemperatureigenschaften polykristalliner γ{sup '}-gehaerteter Kobaltbasis-Superlegierungen

    Energy Technology Data Exchange (ETDEWEB)

    Bauer, Alexander

    2016-07-01

    The recent discovery of a stable γ{sup '}-phase in Co-based superalloys opened up a pathway for the development of a new high temperature material class, which is similar in microstructure and properties to the modern γ{sup '}-hardened Ni-based superalloys. In this work, the first attempt was done to check the influence of several for Ni-based superalloys typical alloying elements on the properties of the new Co-based superalloys. It became clear that the basic characteristics of the first experimental alloys are similar to those of the γ{sup '}-hardened Ni-based alloys. The results of the multinary experimental alloys show that, based on the insight gained so far, targeted alloy development is possible. These materials have the potential to be used as disc materials in turbines.

  10. Caustic stress corrosion cracking of Inconel-600, Incoloy-800, and Type 304 stainless steel

    International Nuclear Information System (INIS)

    Theus, G.J.

    1976-01-01

    High-temperature electrochemical tests have resulted in the stress corrosion cracking of Inconel-600 and Incoloy-800 (registered trademarks, International Nickel Company), and Type 304 stainless steel in caustic solutions. Results show that stress corrosion cracking of these alloys can be prevented or accelerated by varying their electrochemical potential. To a certain extent, the same effect can be achieved by altering the gas atmosphere above the test solution from a pure nitrogen cover gas to a mixture of 5 percent H 2 and 95 percent N 2 . The effect of the cover gas can then be negated by adjusting the specimen's electrochemical potential either to cause or to inhibit stress corrosion cracking. Some specifics of the test results reveal that in deoxygenated caustic solutions, Inconel-600 cracks intergranularly at mildly anodic potentials; Incoloy-800 cracks transgranularly at reduced potentials (at or near the open circuit potential) and intergranularly at highly oxidizing potentials; and cracking is mixed (transgranular/intergranular) for Type 304 stainless steel at or near the open circuit potential. The severity of cracking for both Inconel-600 and Incoloy-800 in deoxygenated caustic solutions is reduced by giving the materials a simulated post-weld heat treatment (1150 0 F for 18 h). Test results on Inconel-600 show that high-carbon (0.06 percent) material cracks less severely than low-carbon (0.02 percent) material, in both the simulated post-weld heat-treated condition and the mill-annealed condition

  11. Solidification behaviors of a single-crystal superalloy under lateral constraints

    International Nuclear Information System (INIS)

    Zhuangqi Hu; Huaming Wang

    1993-01-01

    The effect of lateral constraints ahead of solidification interface on the solidification behaviors of a newly developed hot corrosion resistant single-crystal nickel-base superalloy was investigated under commercial single-crystal production conditions. The lateral constraints or section variations ahead of solidification front were found to have drastic influences both on the modes of solidification and the profiles of solute segregation. As lateral constraints were imposed ahead of the directionally solidifying interface, the solidification microstructure of the single-crystal superalloy changed suddenly, through a γ/γ' eutectic-free zone which is characterized by an extremely-fine and highly-developed dendrite network, from the original well-branched dendritic structure to a fine cellular-dendrite or regular cell structure, accompanying which the primary arm spacing, the severity of segregation and the amount of microporosity decreased remarkably. The newly formed cellular dendrite or cell structure transforms always gradually to the initial coarse dendrite structure as the lateral constraint is finally released whether gradually or sharply. Moreover, an abnormal porosity zone was readily observed in the initial section beneath and away from the eutectic-free zone. The solidification microstructural changes were attributed to the drastic dynamical changes in local solidification cooling conditions and in momentum transport during solidification due to the presence of lateral constraint

  12. Effect of thermal exposure on microstructure and nano-hardness of broached Inconel 718

    Directory of Open Access Journals (Sweden)

    Chen Zhe

    2014-01-01

    Full Text Available Inconel 718 is a high strength, heat resistant superalloy that is used extensively for components in hot sections of gas turbine engines. This paper presents an experimental study on the thermal stability of broached Inconel 718 in terms of microstructure and nano-hardness. The broaching process used in this study is similar to that used in gas turbine industries for machining fir-tree root fixings on turbine discs. Severe plastic deformation was found under the broached surface. The plastic deformation induces a work-hardened layer in the subsurface region with a thickness of ∼50 μm. Thermal exposure was conducted at two temperatures, 550 ∘C and 650 ∘C respectively, for 300 h. Recrystallization occurs in the surface layer during thermal exposure at 550 ∘C and α-Cr precipitates as a consequence of the growth of recrystallized δ phases. More recrystallized grains with a larger size form in the surface layer and the α-Cr not only precipitates in the surface layer, but also in the sub-surface region when the thermal exposure temperature goes up to 650 ∘C. The thermal exposure leads to an increase in nano-hardness both in the work-hardened layer and in the bulk material due to the coarsening of the main strengthening phase γ′′.

  13. Strain-induced γ{sup '}-coarsening during aging of Ni-based superalloys under uniaxial load. Modeling and analysis

    Energy Technology Data Exchange (ETDEWEB)

    Mushongera, Leslie T.

    2016-07-28

    Turbine blades which are used in the hot paths of aerospace or industrial gas turbines are usually manufactured as casted single crystalline parts. However, even though grain boundaries are excluded, the degradation behavior of respectively developed single crystal nickel-base superalloys, is still quite complex involving a number of very different microscopic effects. One of these is the diffusion-limited coarsening of the γ{sup '}-precipitates. Long-term aging or creep loading along the <100> crystallographic orientation results in the anisotropic coarsening of the γ{sup '}-precipitates. In the end, the microstructure contains quite large, irregularly shaped precipitates or plate-like precipitates aligned either parallel (P-type rafts) or perpendicular (N-type rafts) to the loading direction. This behavior is detrimental for the properties of these materials since their superior properties emanate from the size, morphology and distribution of the γ{sup '}-precipitates [R. Reed: Cambridge University Press, (2006)]. In order to efficiently design these materials, the phenomenon of coarsening should be known in detail to optimize the materials accurately. On this background, the general objective of this thesis is to develop an integrated computational approach for simulating morphological evolution in single crystal Ni-base superalloys. As a first step towards that aim, a multi-component phase field model coupled to inputs from CALPHAD-type and kinetic databases for the relevant driving forces was developed based on the grand-potential formalism similar to Plapp [Phys. Rev. E, 84: 031601 (2011)]. The thermodynamic formulation of the model was validated by comparisons to ThermoCalc equilibrium calculations and DICTRA sharp-interface simulations. Phase field approaches that allow for anisotropies of the interfacial energy sufficiently high so that the interface develops sharp corners due to missing crystallographic orientations were formulated. This

  14. Analysis of grinding of superalloys and ceramics for off-line process optimization

    Science.gov (United States)

    Sathyanarayanan, G.

    The present study has compared the performances of resinoid, vitrified, and electroplated CBN wheels in creep feed grinding of M42 and D2 tool steels. Responses such as a specific energy, normal and tangential forces, and surface roughness were used as measures of performance. It was found that creep feed grinding with resinoid, vitrified, and electroplated CBN wheels has its own advantages, but no single wheel could provide good finish, lower specific energy, and high material removal rates simultaneously. To optimize the CBN grinding with different bonded wheels, a Multiple Criteria Decision Making (MCDM) methodology was used. Creep feed grinding of superalloys, Ti-6Al-4V and Inconel 718, has been modeled by utilizing neural networks to optimize the grinding process. A parallel effort was directed at creep feed grinding of alumina ceramics with diamond wheels to investigate the influence of process variables on responses based on experimental results and statistical analysis. The conflicting influence of variables was observed. This led to the formulation of ceramic grinding process as a multi-objective nonlinear mixed integer problem.

  15. Design of a braze alloy for fast epitaxial brazing of superalloys

    Science.gov (United States)

    Piegert, S.; Laux, B.; Rösier, J.

    2012-07-01

    For the repair of directionally solidified turbine components made of nickel-based superalloys, a new high-temperature brazing method has been developed. Utilising heterogeneous nucleation on the crack surface, the microstructure of the base material can be reproduced, i.e. single crystallinity can be maintained. In contrast to commonly used eutectic braze alloys, such as nickel-boron or nickel-silicon systems, the process is not diffusion controlled but works with a consolute binary base system. The currently applied epitaxial brazing methods rely on isothermal solidification diffusing the melting point depressants into the base material until their concentration is reduced so that the liquid braze solidifies. Contrary, the identified Ni-Mn consolute system enables a temperature driven epitaxial solidification resulting in substantially reduced process duration. The development of the braze alloys was assisted using the CALPHAD software Thermo-Calc. The solidification behaviour was estimated by kinetic calculations with realistic boundary conditions. Finally, the complete system, including braze alloy as well as substrate material, was modelled by means of DICTRA. Subsequently, the thermodynamic properties of the braze alloys were experimentally analysed by DSC measurements. For brazing experiments 300 μm wide parallel gaps were used. Complete epitaxial solidification, i.e. the absence of high-angle grain boundaries, could be achieved within brazing times being up to two orders of magnitude shorter compared to diffusion brazing processes. Theoretically and experimentally evaluated process windows reveal similar shapes. However, a distinct shift has to be stated which can be ascribed to the limited accuracy of the underlying thermodynamic databases.

  16. Modelling and simulation of superalloys. Book of abstracts

    Energy Technology Data Exchange (ETDEWEB)

    Rogal, Jutta; Hammerschmidt, Thomas; Drautz, Ralf (eds.)

    2014-07-01

    Superalloys are multi-component materials with complex microstructures that offer unique properties for high-temperature applications. The complexity of the superalloy materials makes it particularly challenging to obtain fundamental insight into their behaviour from the atomic structure to turbine blades. Recent advances in modelling and simulation of superalloys contribute to a better understanding and prediction of materials properties and therefore offer guidance for the development of new alloys. This workshop will give an overview of recent progress in modelling and simulation of materials for superalloys, with a focus on single crystal Ni-base and Co-base alloys. Topics will include electronic structure methods, atomistic simulations, microstructure modelling and modelling of microstructural evolution, solidification and process simulation as well as the modelling of phase stability and thermodynamics.

  17. Conductivity Profile Determination by Eddy Current for Shot Peened Superalloy Surfaces Toward Residual Stress Assessment

    International Nuclear Information System (INIS)

    Shen, Y.; Lo, C. C. H.; Frishman, A. M.; Lee, C.; Nakagawa, N.

    2007-01-01

    This paper describes an eddy current model-based method for inverting near-surface conductivity deviation profiles of surface treated materials from swept-high frequency eddy current (SHFEC) data. This work forms part of our current research directed towards the development of an electromagnetic nondestructive technique for assessing residual stress of shot-peened superalloy components. The inversion procedure is based on the use of a parameterized function to describe the near-surface conductivity as a function of depth for a shot-peened surface, and the laterally uniform multi-layer theory of Cheng, Dodd and Deeds to calculate the resulting coil impedance deviations. The convergence of the inversion procedure has been tested against synthesized eddy current data. As a demonstration, the conductivity deviation profiles of a series of Inconel 718 specimens, shot peened at various Almen intensities, have been obtained by inversion. Several consistency tests were conducted to examine the reliability of the inverted conductivity profiles. The results show that conductivity deviation profiles can be reliably determined from SHFEC data within the accuracy of the current measurement system

  18. Mechanism of formation of corrosion layers on nickel and nickel-based alloys in melts containing oxyanions--a review

    International Nuclear Information System (INIS)

    Tzvetkoff, Tzvety; Gencheva, Petia

    2003-01-01

    A review of the corrosion of Ni and Ni-based alloys in melts containing oxyanions (nitrate, sulphate, hydroxide and carbonate) is presented, emphasising the mechanism of growth, the composition and structure of the passivating oxide films formed on the material in such conditions. First, the thermodynamical background involving solubility and point defect chemistry calculations for oxides formed on Ni, Cr and Ni-Cr alloys in molten salt media is briefly commented. The main passivation product on the Ni surface has been reported to be cubic NiO. In the transition stage, further oxidation of the compact NiO layer has been shown to take place in which Ni(III) ions and nickel cation vacancies are formed. Transport of nickel cation vacancies has been proposed to neutralise the charges of the excess oxide ions formed in the further oxidation reaction. Ex situ analysis studies reported in the literature indicated the possible formation of Ni 2 O 3 phase in the anodic layer. During the third stage of oxidation, a survey of the published data indicated that oxygen evolution from oxyanion melts is the predominant reaction taking place on the Ni/NiO electrode. This has been supposed to lead to a further accumulation of oxygen ions in the oxide lattice presumably as oxygen interstitials, and a NiO 2 phase formation has been also suggested. Literature data on the composition of the oxide film on industrial Ni-based alloys and superalloys in melts containing oxyanions are also presented and discussed. Special attention is paid to the effect of the composition of the alloy, the molten salt mixture and the gas atmosphere on the stability and protective ability of corrosion layers

  19. First-principles calculations for the elastic properties of Ni-base model superalloys: Ni/Ni3Al multilayers

    International Nuclear Information System (INIS)

    Yun-Jiang, Wang; Chong-Yu, Wang

    2009-01-01

    A model system consisting of Ni[001](100)/Ni 3 Al[001](100) multi-layers are studied using the density functional theory in order to explore the elastic properties of single crystal Ni-based superalloys. Simulation results are consistent with the experimental observation that rafted Ni-base superalloys virtually possess a cubic symmetry. The convergence of the elastic properties with respect to the thickness of the multilayers are tested by a series of multilayers from 2γ'+2γ to 10γ'+10γ atomic layers. The elastic properties are found to vary little with the increase of the multilayer's thickness. A Ni/Ni 3 Al multilayer with 10γ'+10γ atomic layers (3.54 nm) can be used to simulate the mechanical properties of Ni-base model superalloys. Our calculated elastic constants, bulk modulus, orientation-dependent shear modulus and Young's modulus, as well as the Zener anisotropy factor are all compatible with the measured results of Ni-base model superalloys R1 and the advanced commercial superalloys TMS-26, CMSX-4 at a low temperature. The mechanical properties as a function of the γ' phase volume fraction are calculated by varying the proportion of the γ and γ' phase in the multilayers. Besides, the mechanical properties of two-phase Ni/Ni 3 Al multilayer can be well predicted by the Voigt–Reuss–Hill rule of mixtures. (classical areas of phenomenology)

  20. Iron and silicon effect on the phase composition of nickel-beryllium bronzes

    International Nuclear Information System (INIS)

    Zakharov, A.M.; Zakharov, M.V.; Ajvaz'yan, N.G.

    1977-01-01

    In order to specify phase composition and strengthening heat treatment conditions for nickel beryllium bronzes that are promising electrode materials for welding of high strength steels and nickel-base superalloys, the primary section of the quinternary Cu-Ni-Be-Fe-S system was studied at constant nickel and beryllium concentration and varying silicon and iron concentration (max. 4% of every element). The study was made using the metallographic and x-ray phase techniques, determination of alloy solidus temperature, and exessphase microhardness testing. Silicon additions are shown to decrease abruptly and those of iron, in contrast, somewhat to raise the solidus temperature of ternary Cu + 2% Ni + 0.3% Be alloy. When added concurrently, iron compensates for the damaging silicon effect on the solidus temperature of Cu-Ni-Be alloys. The excess phases formed can be used as strengthening agents of Cu-Ni-Be-Si-Fe alloys during quenching and subsequent aging

  1. Metallurgical and mechanical examinations of steel–copper joints arc welded using bronze and nickel-base superalloy filler materials

    International Nuclear Information System (INIS)

    Velu, M.; Bhat, Sunil

    2013-01-01

    Highlights: ► Optical and scanning electron microscopy show defect free weld interfaces. ► Energy dispersive spectroscopy shows low dilution level of the weld by Fe. ► XRD studies show no brittle intermetallic phases in the weld interfaces. ► Weld interfaces did not fail during tensile, transverse bending and impact tests. ► The joint exhibits superior strength properties than that of bronze filler. - Abstract: The paper presents metallurgical and mechanical examinations of joints between dissimilar metals viz. copper (UNSC11000) and alloy steel (En31) obtained by Shielded Metal Arc Welding (SMAW) using two different filler materials, bronze and nickel-base super alloy. The weld bead of the joint with bronze-filler displayed porosity, while that with nickel-filler did not. In tension tests, the weldments with bronze-filler fractured in the centre of the weld, while those with nickel-filler fractured in the heat affected zone (HAZ) of copper. Since the latter exhibited higher strength than the former, all the major tests were undertaken over the joints with nickel-filler alone. Scanning Electron Microscopy (SEM) coupled with Energy Dispersive Spectroscopy (EDS) indicated corrugated weld interfaces and favorable elemental diffusions across them. X-ray diffraction (XRD) studies around the weld interfaces did not reveal any detrimental intermetallic compounds. Transverse bending tests showed that flexural strengths of the weldments were higher than the tensile strengths. Transverse side bend tests confirmed good ductility of the joints. Shear strength of the weld-interface (Cu–Ni or Ni–steel) was higher than the yield strength of weaker metal. Microhardness and Charpy impact values were measured at all the important zones across the weldment

  2. Investigation on the Effects of Process Parameters on Laser Percussion Drilling Using Finite Element Methodology; Statistical Modelling and Optimization

    Directory of Open Access Journals (Sweden)

    Mahmoud Moradi

    Full Text Available Abstract In the present research, the simulation of the Nickel-base superalloy Inconel 718 fiber-laser drilling process with the thickness of 1mm is investigated through the Finite Element Method. In order to specify the appropriate Gaussian distribution of laser beam, the results of an experimental research on glass laser drilling were simulated using three types of Gaussian distribution. The DFLUX subroutine was used to implement the laser heat sources of the models using the Fortran language. After the appropriate Gaussian distribution was chosen, the model was validated with the experimental results of the Nickel-base superalloy Inconel 718 laser drilling process. The negligible error percentage among the experimental and simulation results demonstrates the high accuracy of this model. The experiments were performed based on the Response Surface Methodology (RSM as a statistical design of experiment (DOE approach to investigate the influence of process parameters on the responses, obtaining the mathematical regressions and predicting the new results. Four parameters i.e. laser pulse frequency (150 to 550 Hz, laser power (200 to 500 watts, laser focal plane position (-0.5 to +0.5 mm and the duty cycle (30 to 70% were considered to be the input variables in 5 levels and four external parameters i.e. the hole's entrance and exit diameters, hole taper angle and the weight of mass removed from the hole, were observed to be the process output responses of this central composite design. By performing the statistical analysis, the input and output parameters were found to have a direct relation with each other. By an increase in each of the input variables, the entrance and exit hole diameters, the hole taper angel, and the weight of mass removed from the hole increase. Finally, the results of the conducted simulations and statistical analyses having been used, the laser drilling process was optimized by means of the desire ability approach. Good

  3. Oxidation assisted intergranular cracking under loading at dynamic strain aging temperatures in Inconel 718 superalloy

    Energy Technology Data Exchange (ETDEWEB)

    Rezende, M.C., E-mail: monica_crezende@hotmail.com [Universidade Federal do Rio de Janeiro, Departamento de Engenharia Metalúrgica e de Materiais, C.P. 68505, Rio de Janeiro 21945-970 (Brazil); Araújo, L.S.; Gabriel, S.B. [Universidade Federal do Rio de Janeiro, Departamento de Engenharia Metalúrgica e de Materiais, C.P. 68505, Rio de Janeiro 21945-970 (Brazil); Dille, J. [Université Libre de Bruxelles, 4MAT Department, Av. F. Roosevelt 50, C.P. 194/03, Brussels (Belgium); Almeida, L.H. de [Universidade Federal do Rio de Janeiro, Departamento de Engenharia Metalúrgica e de Materiais, C.P. 68505, Rio de Janeiro 21945-970 (Brazil)

    2015-09-15

    Highlights: • Mechanical properties are controlled by DSA, precipitation hardening and OAIC. • Between 600 and 700 °C the critical strain for serrations increases with temperature. • This is related to the consumption of matrix elements (especially Nb: for γ′ and γ″). • A reduction in ductility occurs (related to the OAIC) when the DSA is no longer effective. • This reduction is accompanied by an increase in intergranular brittle fracture. - Abstract: It is well established that 718 superalloy exhibits brittle intergranular cracking when deformed under tension at temperatures above 600 °C. This embrittlement effect is related with grain boundary penetration by oxygen (Oxygen Assisted Intergranular Cracking – OAIC). Simultaneously, impacting on its mechanical properties, the precipitation of coherent γ′ and γ″ phases occur above 650 °C and Dynamic Strain Aging (DSA) occurs in the temperature range between 200 and 800 °C. Although literature indicates that OAIC is the mechanism that controls mechanical properties at high temperatures, its interactions with DSA and precipitation are still under discussion. The objective of this work is to investigate the interactions between the embrittlement phenomena (OAIC and DSA) and the hardening mechanism of γ′ and γ″ precipitation on the mechanical properties of an annealed 718 superalloy. Tensile tests were performed at a strain rate of 3.2 × 10{sup −4} s{sup −1} under secondary vacuum, in temperatures ranging from 200 to 800 °C. Fracture surfaces were observed by scanning electron microscopy (SEM) and precipitation by transmission electron microscopy (TEM). The effect of DSA and precipitation on the strength and of OAIC on the ductility was verified.

  4. Effect of residual elements on high performance nickel base ...

    Indian Academy of Sciences (India)

    Unknown

    superalloys for gas turbines and strategies for manufacture. O P SINHA*, M ... Superalloys; tramp elements; creep and stress rupture properties; vacuum induction melting. 1. Introduction ... The physical metallurgy of superalloys demands the.

  5. In situ corrosion testing of various nickel alloys at Måbjerg waste incineration plant

    DEFF Research Database (Denmark)

    Montgomery, Melanie; Hansson, A. N.; Jensen, S. A.

    2013-01-01

    overlay material currently being used to give improved corrosion resistance. In order to assess the use of alternative nickel alloys, test panels have been manufactured and inserted into Måbjerg waste incineration plant. Inconel 625 as a 50% weld overlay, two layered weld overlay and as a spiral weld......The majority of waste in Denmark is disposed via waste to energy (WTE) incineration plants which are fabricated from carbon steel. However, due to the increasing corrosiveness of waste over the years, more corrosion resistant alloys are required. In Denmark, Inconel 625 (UNSN06625) is the weld...... overlay was exposed. Other nickel materials exposed were weld overlay Alloy 686, Alloy 50 and Sumitomo Super 625 coextruded tube. Exposure has been undertaken from 2003 to 2009 in the first pass and 2005–2009 in the second pass, and sections have been removed and investigated during this period...

  6. Lubricating Properties of Ceramic-Bonded Calcium Fluoride Coatings on Nickel-Base Alloys from 75 to 1900 deg F

    Science.gov (United States)

    Sliney, Harold E.

    1962-01-01

    The endurance life and the friction coefficient of ceramic-bonded calcium fluoride (CaF2) coatings on nickel-base alloys were determined at temperatures from 75 F to 1900 F. The specimen configuration consisted of a hemispherical rider (3/16-in. rad.) sliding against the flat surface of a rotating disk. Increasing the ambient temperature (up to 1500 F) or the sliding velocity generally reduced the friction coefficient and improved coating life. Base-metal selection was critical above 1500 F. For instance, cast Inconel sliding against coated Inconel X was lubricated effectively to 1500 F, but at 1600 F severe blistering of the coatings occurred. However, good lubrication and adherence were obtained for Rene 41 sliding against coated Rene 41 at temperatures up to 1900 F; no blisters developed, coating wear life was fairly good, and the rider wear rate was significantly lower than for the unlubricated metals. Friction coefficients were 0.12 at 1500 F, 0.15 at 1700 F, and 0.17 at 1800 F and 1900 F. Because of its ready availability, Inconel X appears to be the preferred substrate alloy for applications in which the temperature does not exceed 1500 F. Rene 41 would have to be used in applications involving higher temperatures. Improved coating life was derived by either preoxidizing the substrate metals prior to the coating application or by applying a very thin (less than 0.0002 in.) burnished and sintered overlay to the surface of the coating. Preoxidation did not affect the friction coefficient. The overlay generally resulted in a higher friction coefficient than that obtained without the overlay. The combination of both modifications resulted in longer coating life and in friction coefficients intermediate between those obtained with either modification alone.

  7. On the Influence of Nb/Ti Ratio on Environmentally-Assisted Crack Growth in High-Strength Nickel-Based Superalloys

    Science.gov (United States)

    Németh, A. A. N.; Crudden, D. J.; Collins, D. M.; Kuksenko, V.; Liebscher, C. H.; Armstrong, D. E. J.; Wilkinson, A. J.; Reed, R. C.

    2018-05-01

    The effect of Nb/Ti ratio on environmentally-assisted crack growth of three prototype Ni-based superalloys is studied. For these alloys, the yield strength is unaltered with increasing Nb/Ti ratio due to an increase in grain size. This situation has allowed the rationalization of the factors influencing damage tolerance at 700 °C. Primary intergranular cracks have been investigated using energy-dispersive X-ray spectroscopy in a scanning transmission electron microscope and the analysis of electron back-scatter diffraction patterns. Any possible detrimental effect of Nb on the observed crack tip damage due to Nb-rich oxide formation is not observed. Instead, evidence is presented to indicate that the tertiary γ'-precipitates are dissolving ahead of the crack consistent with the formation of oxides such as alumina and rutile. Our results have implications for alloy design efforts; at any given strength level, both more and less damage-tolerant variants of these alloys can be designed.

  8. Investigation on edge joints of Inconel 625 sheets processed with laser welding

    Science.gov (United States)

    Caiazzo, F.; Alfieri, V.; Cardaropoli, F.; Sergi, V.

    2017-08-01

    Laser welding of Inconel 625 edge joint beads in square groove configuration was investigated. The use of different weld geometries in new aerospace solutions explains research on edge joints. A structured plan was carried out in order to characterize the process defining the influence of laser power and welding speed and to study possible interactions among the governing factors. As weld pool protection is crucial in order to obtain sound joints when processing superalloys, a special glove box for gas supply was designed to upgrade the welding head. Welded joints were characterized referring to bead profile, microstructure and X-rays. It was found that heat input plays an important role as it affects welding stability, porosity content and bead shape. Results suggest operating with low values of heat input to reduce porosity and guarantee stable bead conformation. Furthermore, a decrease in the grain size has been observed as a consequence of decreasing heat input.

  9. Length change of the alloys Waspaloy and Inconel 718 after long-term annealing; Laengenaenderung der Legierungen Waspaloy und Inconel 718 nach Langzeitauslagerung

    Energy Technology Data Exchange (ETDEWEB)

    Kinzel, Svenja

    2016-07-01

    Within the scope of this work the contraction behavior of Ni-based superalloy Waspaloy could in detail be referred to a combination of different microstructural changes and the results could partially be transferred to Ni-Fe-based alloy Inconel 718. Isothermal annealing of sample rods at temperatures between 450 C and 750 C induces an average relative length contraction of about -2.10{sup -4}. It is apparent that contraction is more pronounced for lower temperatures (-3.10{sup -4} at 550 C) than for higher ones (-1.10{sup -4} at 750 C). Within the first 300 hours of annealing the contraction reaches about 70-75% of the value measured after 10,000 hours. This means the major part of the effect takes place at the beginning of long term annealing but even after 10,000 hours no saturation occurs. On the basis of lattice parameter measurements it could be found that within the first 300 hours a significant lattice parameter decrease of matrix and γ{sup '} phase emerged. Longer annealing time does not cause further lattice contraction. This sample behavior can be explained by temperature dependence of phase fractions and phase compositions. Thermodynamic calculations as well as stereological analysis of micrographs show a decrease of stable γ{sup '}-phase content with increasing temperature. In parallel, TEM-EDS measurements and calculated phase fractions show concentration fluctuations due to the different precipitate fraction, which cause contraction of the lattice parameter. Furthermore, within the first 100 hours at temperatures up to 650 C the formation or Ni-Cr rich domains could be observed. As these domains exhibit a smaller lattice parameter than the matrix they contribute to the more pronounced contraction at lower temperatures. While XRD measurements point to the formation of Ni{sub 3}Cr, TEM-EDS measurements reveal a composition of (Ni,Co){sub 2}Cr. Stress relief heat treatment at higher temperatures (815 C) after annealing shows that the effect

  10. Morphological changes of gamma prime precipitates in nickel-base superalloy single crystals

    International Nuclear Information System (INIS)

    Mackay, R.A.

    1984-07-01

    Changes in the morphology of the gamma prime precipitate were examined during tensile creep at temperatures between 927 and 1038 C in 001-oriented single crystals of a Ni-Al-Mo-Ta superalloy. In this alloy, which has a large negative misfit of -0.80%, the gamma prime particles link together during creep to form platelets, or rafts, which are aligned with their broad faces perpendicular to the applied tensile axis. The dimensions of the gamma and gamma prime phases were measured as directional coarsening developed in an attempt to trace the changing morphology under various stress levels. In addition, the effects of initial microstructure, as well as slight compositional variations, were related to raft development and creep properties. The results showed that directional coarsening of gamma prime began during primary creep, and under certain conditions, continued to develop after the onset of steady-state creep. The length of the rafts increased linearly with time up to a plateau region. The thickness of the rafts, however, remained equal to the initial gamma prime size at least up through the onset of tertiary creep this is a clear indication of the stability of the finely-spaced gamma-gamma prime lamellar structure. It was found that the single crystals with the finest gamma prime size exhibited the longest creep lives, because the resultant rafted structure had a larger number of gamma-gamma prime interfaces per unit volume of material

  11. Insoluble Coatings for Stirling Engine Heat Pipe Condenser Surfaces

    Science.gov (United States)

    Dussinger, Peter M.; Lindemuth, James E.

    1997-01-01

    The principal objective of this Phase 2 SBIR program was to develop and demonstrate a practically insoluble coating for nickel-based superalloys for Stirling engine heat pipe applications. Specific technical objectives of the program were: (1) Determine the solubility corrosion rates for Nickel 200, Inconel 718, and Udimet 72OLI in a simulated Stirling engine heat pipe environment, (2) Develop coating processes and techniques for capillary groove and screen wick structures, (3) Evaluate the durability and solubility corrosion rates for capillary groove and screen wick structures coated with an insoluble coating in cylindrical heat pipes operating under Stirling engine conditions, and (4) Design and fabricate a coated full-scale, partial segment of the current Stirling engine heat pipe for the Stirling Space Power Convertor program. The work effort successfully demonstrated a two-step nickel aluminide coating process for groove wick structures and interior wall surfaces in contact with liquid metals; demonstrated a one-step nickel aluminide coating process for nickel screen wick structures; and developed and demonstrated a two-step aluminum-to-nickel aluminide coating process for nickel screen wick structures. In addition, the full-scale, partial segment was fabricated and the interior surfaces and wick structures were coated. The heat pipe was charged with sodium, processed, and scheduled to be life tested for up to ten years as a Phase 3 effort.

  12. Effect of the microstructure on the creep behavior of PM Udimet 720 superalloy--experiments and modeling

    International Nuclear Information System (INIS)

    Dubiez-Le Goff, Sophie; Couturier, Raphaeel; Guetaz, Laure; Burlet, Helene

    2004-01-01

    Powder metallurgy processed Udimet 720 is a high creep strength nickel-based superalloy considered for high temperature turbine disks for nuclear gas cooled reactors working under 700 deg. C. Both fine-grained and coarse-grained microstructures have been obtained by applying respectively a subsolvus or a supersolvus solution treatments, followed by ageing treatments. In both microstructures, the distribution of the strengthening γ' precipitates has been characterized by transmission electron microscopy (TEM). The creep curves of the coarse-grained microstructure show the three usual creep stages. On the contrary, the creep curves of the fine-grained microstructure show a transition directly from primary to apparent tertiary creep without any obvious steady state. According to TEM analyses, Orowan loops surround Udimet 720 CR γ' and U720 HS γ' at high stress whereas U720 HS γ' are sheared at low stress. To describe the behavior of the superalloy Udimet 720, a specific creep model is developed on the basis of McLean and Dyson models including physical damage parameters

  13. Design criteria for rhenium-reduced nickel-based single-crystal alloys. Identification and computer-assisted conversion; Designkriterien fuer rheniumreduzierte Nickelbasis-Einkristalllegierungen. Identifikation und rechnergestuetzte Umsetzung

    Energy Technology Data Exchange (ETDEWEB)

    Goehler, Thomas

    2016-06-17

    In the present work, design criteria and property models for the creep strength optimization of rhenium-free nickel based single crystal Superalloys are investigated. The study focuses on a typical load condition of 1050 C and 150 MPa, which is representative for flight engine applications. Thereby the key aspect is to link chemical composition, manufacturing processes, microstructure formation and mechanistic understanding of dislocation creep through a computational materials engineering approach. Beside the positive effect of rhenium on solid solution hardening, a second mechanism in which rhenium increases high temperature creep strength is identified. It indirectly stabilizes precipitation hardening by reducing the coarsening kinetics of γ'-rafting. Five 1st and 2nd generation technical Superalloys show a comparable microstructure evolution for up to 2 % plastic elongation, while creep times differ by a factor of five. The application of a microstructure sensitive creep model shows that these coarsening processes can activate γ-cutting and thus lead to an increasing creep rate. Based on these calculations a threshold value of φ{sub γ/γ'} > 2,5 at 150 MPa is estimated. This ratio of matrix channel to raft thickness has been proofed for multiple positions by microstructure analysis of interrupted creep tests. The mechanism described previously can be decelerated by the enrichment of the γ-matrix with slow diffusing elements. The same principle also increases the solid solution strength of the γ-matrix. Therefore, the present work delivers an additional mechanistic explanation why creep properties of single phase nickel based alloys can be transferred to two phase technical Superalloys with rafted γ'-structure. Following, the best way to substitute both rhenium fundamental properties, namely a slow diffusion coefficient and a small solubility in g', has been investigated by means of CALPHAD-modeling. Only molybdenum and especially

  14. Anisotropic stress rupture properties of the nickel-base single crystal superalloy SRR99

    International Nuclear Information System (INIS)

    Han, G.M.; Yu, J.J.; Sun, Y.L.; Sun, X.F.; Hu, Z.Q.

    2010-01-01

    The influence of orientation on the stress rupture properties of a single crystal superalloy SRR99 was investigated at temperatures of 760 and 1040 deg. C. It is found that the creep anisotropic behaviour is pronounced at the lower temperature of 760 deg. C and the stress rupture life ranks in the order [0 0 1] > [1 1 1] > [0 1 1]. Despite the anisotropy of stress rupture life is evidently reduced at the higher temperature, the [1 1 1] orientation exhibits the longest life. At 760 deg. C, EBSD (electron back scattered diffraction) was adopted to measure the lattice rotation and the deduced results indicate that the dominant slip systems are {1 1 1} during stress rupture test. At 1040 deg. C, the ranking order of the stress rupture life is [1 1 1] > [0 0 1] > [0 1 1] and the single crystal close to [0 1 1] orientation still shows the poorest life. In the [0 0 1] and [1 1 1] samples, regular γ' raft structure is formed compared with [0 1 1] samples. Further observations made by TEM investigations reveal the underlying deformation mechanisms for crystals with orientations near [0 0 1], [0 1 1] and [1 1 1] under two test conditions.

  15. Intercrystalline and transcrystalline vibration fatigue failure in the inconel 718 nickel-based alloy; Inter- und transkristalliner Schwingbruch in der Nickelbasislegierung Inconel 718

    Energy Technology Data Exchange (ETDEWEB)

    Wanzek, Horst; Fruhner, Annett [Lufthansa Technik AG, Hamburg (Germany). Metallurgical Lab., HAM WR123

    2011-07-01

    The fracture of the turbine rotor disc resulted in the breakdown of the APU and high expenses. The APU is located below the vertical tailplane, at the tail of every major-sized aircraft. The vane receptacle failed in the mode of a vibration fatigue failure of an intercrystalline and transcrystalline progression. The cause of this damage is attributable to the fatigue of the material. This can result from the long service life (21 131 h) and the fact that 9 more vane receptacles exhibited a comparable damage pattern. In INCONEL 718 alloys, cracks propagate in a transcrystalline way when under an alternate bend stress and at temperatures below abt. 600 C. In contrast, cracks propagate because of grain boundary oxidation above abt. 600 C in an intercrystalline way. The phenomenon that the two crack modi occurred alternately on the same fracture area is explained from the fact that the component part was exposed to different temperatures during operation. While the crack progress was transcrystalline in the ''cooler'' starting and stopping phase crack propagation occurred along the grain boundaries (was intercrystalline) in a normal operation above 600 C. Besides a limitation of the running time in its service life, other measures could not be taken for this component part. (orig.)

  16. Castability of Traditionally Wrought Ni-Based Superalloys for USC Steam Turbines

    Energy Technology Data Exchange (ETDEWEB)

    Jablonski, P D; Cowen, C J; Hawk, J A; Evens, N; Maziasz, P

    2011-02-27

    The high temperature components within conventional coal fired power plants are manufactured from ferritic/martensitic steels. In order to reduce greenhouse gas emissions the efficiency of pulverized coal steam power plants must be increased. The proposed steam temperature in the Advanced Ultra Supercritical (A-USC) power plant is high enough (760°C) that ferritic/martensitic steels will not work due to temperature limitations of this class of materials; thus Ni-based superalloys are being considered. The full size castings are quite substantial: ~4in thick, several feet in diameter and weigh 5-10,000lb each half. Experimental castings were quite a bit smaller, but section size was retained and cooling rate controlled in order to produce relevant microstructures. A multi-step homogenization heat treatment was developed in order to better deploy the alloy constituents. The castability of two traditionally wrought Ni-based superalloys to which minor alloy adjustments have been made in order to improve foundry performance is further explored.

  17. Effect of HIP Combined with RHT Process on Creep Damage of DZ125 Superalloy

    Directory of Open Access Journals (Sweden)

    WANG Tian-you

    2017-02-01

    Full Text Available Four different processes of hot isostatic pressing (HIP combined with rejuvenation heat treatments (RHT were adopted to reveal the microstructural evolution of creep damaged DZ125 specimens, finally the mechanical properties were evaluated.The results show that both γ' precipitate degeneration and creep cavities for the creep damaged DZ125 superalloy are found after the pre-endurance damage test.However, the carbided compositions from MC type to M23C6 type or M6C type has not been observed for DZ125.In addition, it is found that the HIP temperature play a dominant role in the cavity healing process for the damaged specimens. The concentrically oriented γ' rafting structure and the incipient melting are observed at 1200℃ and 1250℃ respectively.Meanwhile, it is found that the appropriate HIP schedule adopted can effectively avoid the internal recrystallization for the directionally solidified nickel-based superalloy DZ125. The appropriate HIP schedule combined with RHT process can successfully restore the microstructure induced by creep damage and recover the degraded micro-hardness to the original one, in addition improve the creep rupture life.

  18. Pitting corrosion of Inconel 600 in chloride and sulfate solutions at low temperature

    International Nuclear Information System (INIS)

    Chang Mingyu; Yu Geping

    1993-01-01

    Pitting corrosion of Inconel 600 was examined in chloride and sulfate solutions through usage of potentiodynamic polarization techniques. The effects of chloride and sulfate concentration were investigated in the range of 0.0001 to 0.1 M. Increasing chloride concentrations resulted in active shifts of the pit nucleation potential. Immunity to pitting corrosion was evident at a chloride level below 0.005 M. Increasing sulfate concentrations resulted in improved pitting resistance of Inconel 600 in chloride solutions. Detrimental effects associated with pitting were evident with low-level sulfate being added to dilute chloride media. The density of pits increased with increasing chloride concentrations or temperature between room temperature and 70 C. Systematic trends for the depth of pits were not evident. The observations of pitting corrosion in open immersion were consistent with those in polarization methods. Corrosion products contained in the pits were enriched in nickel, chromium and iron with a small amount of titanium and silicon. The enrichment of chlorine or sulfur was still, however, not found. (orig.)

  19. Introduction to superalloys

    International Nuclear Information System (INIS)

    Li-Chenggong

    1995-01-01

    Throughout history, humans have developed mechanical devices to satisfy their needs, Jet aircraft was thrust into public awareness with the 1937 flight of Hans Von Ohains turbine engine Heinkel in Germany and an independent development, the 1939 flight of Whittle's engine in England. Since that time, progress in jet propulsion and industrial gas turbines has been a growing engineering technology of immense importance. This opened a new era of engineering material called superalloy. Superalloy is an alloy developed for elevated temperature service usually based on group VIIA elements, where relatively severe mechanical stressing is encountered, and where high surface stability is frequently required. The title of the speech is T he Effect of a Changing Environment on the requirements of Engine Materials . In this speech, the author emphasized that may changes in the business environment have occurred in recent years, the aircraft engine business is rapidly changing from a military focus to a commercial one, speed to market will assume greater importance in the engine industry, and greater attention to customer value will be required to remain competitive etc. However the superalloys will continue to be developed in the future. (author) 14 figs

  20. Development of a Refractory High Entropy Superalloy (Postprint)

    Science.gov (United States)

    2016-03-17

    hardened with HfC precipitates [2], Co-Re- or Co-Al-W-based alloys [3] or two-phase ( FCC + L12) refractory superalloys based on platinum group metals...Ni-based superalloys consisting of cuboids with the ordered L12 structure embedded in an FCC solid-solution matrix. Based on this microstructural...and 5). A comparison of the average atomic radii with the measured lattice parameters allows us to conclude that the disordered BCC phase forming

  1. Review of corrosion phenomena on zirconium alloys, niobium, titanium, inconel, stainless steel, and nickel plate under irradiation

    International Nuclear Information System (INIS)

    Johnson, A.B. Jr.

    1975-01-01

    The role of nuclear fluxes in corrosion processes was investigated in ATR, ETR, PRTR, and in Hanford production reactors. Major effort was directed to zirconium alloy corrosion parameter studies. Corrosion and hydriding results are reported as a function of oxygen concentration in the coolant, flux level, alloy composition, surface pretreatment, and metallurgical condition. Localized corrosion and hydriding at sites of bonding to dissimilar metals are described. Corrosion behavior on specimens transferred from oxygenated to low-oxygen coolants in ETR and ATR experiments is compared. Mechanism studies suggest that a depression in the corrosion of the Zr--2.5Nb alloy under irradiation is due to radiation-induced aging. The radiation-induced onset of transition on several alloys is in general a gradual process which nucleates locally, causing areas of oxide prosity which eventually encompass the surface. Examination of Zry-2 process tubes reveals that accelerated corrosion has occurred in low-oxygen coolants. Hydrogen contents are relatively low, but show some localized profiles. Gross hydriding has occurred on process tubes containing aluminum spacers, apparently by a galvanic charging mechanism. Titanium paralleled Zry-2 in corrosion behavior under irradiation. Niobium corrosion was variable, but did not appear to be strongly influenced by radiation. Corrosion rates on Inconel and stainless steel were only slightly higher in-flux than out-of-reactor. Corrosion rates on nickel-plated aluminum appeared to vary substantially with preexposure treatments, but the rates generally were accelerated compared to rates on unirradiated coupons. (59 references, 11 tables, 12 figs.)

  2. On γ and γ' phases composition in IN-100 superalloy after high-temperature exposure

    International Nuclear Information System (INIS)

    Matteazzi, P.; Principi, G.; Ramous, E.

    1981-01-01

    The chemistry and volume fraction of UPSILON' phase in IN-100 superalloy after high-temperature exposure in furnace and in service have been examined. Increasing the time of exposure aluminium plus titanium content remains nearly constant and very close to 25 at.%; the little decrease of nickel together with the increase of iron and molybdenum suggest that the last two elements are preferentially occupying Ni-type sites, according to the pair potential model of UPSILON'. (orig.)

  3. Effect of deposition strategy on the microstructure and mechanical properties of Inconel 625 superalloy fabricated by pulsed plasma arc deposition

    International Nuclear Information System (INIS)

    Xu, F.J.; Lv, Y.H.; Xu, B.S.; Liu, Y.X.; Shu, F.Y.; He, P.

    2013-01-01

    Highlights: ► PPAD Inconel 625 sample deposited with ICS strategy exhibits improved surface quality. ► ICS sample exhibits finer microstructure and improved mechanical properties. ► Higher level γ′ and γ″ phases are precipitated in the ICS sample. ► STA heat treatment reduced the concentration of Nb element. ► STA heat treatment improved the mechanical properties of PPAD Inconel 625. -- Abstract: Pulsed plasma arc deposition (PPAD), which combines pulsed plasma cladding with rapid prototyping, is a promising technology for manufacturing near net shape components due to its superiority in cost and convenience of processing. The aim of this study was to investigate the influences of interpass cooling strategy (ICS) and continuous deposition strategy (CDS) on microstructure and mechanical properties of the PPAD Inconel 625 non-ferrous alloy. The as-deposited samples in the two conditions were subjected to the post heat treatment: 980 °C solution treatment + direct aging (STA). The microstructures and mechanical properties of the samples were characterized by means of scanning electron microscopy (SEM) equipped with energy dispersive spectrometer (EDS), transmission electron microscopy (TEM), micro-hardness and tensile testers. It was found that the as-deposited microstructure exhibited homogenous cellular dendrite structure, which grew epitaxially along the deposition direction. The as-deposited microstructure of ICS sample revealed smaller dendritic arm spacing, less niobium segregation and discontinuous finer Laves phase in the interdendritic regions compared to the case of continuous deposition strategy (CDS). The ICS sample exhibited better mechanical properties than CDS sample. After STA heat treatment, a large amount of Laves particles in the interdendritic regions were dissolved, resulting in the reduction of Nb segregation and the precipitation of needle-like δ (Ni 3 Nb). The tensile and yield strength of the as-deposited samples were

  4. The speed of growth of the gamma phase comes prime in nickel based alloys

    International Nuclear Information System (INIS)

    Peretti, M.M; Ges, A.M; Versaci, R.A

    2004-01-01

    Nickel-based alloys have a high fraction in volume of precipitate phase. This precipitate phase provides the characteristics of high mechanical resistance to high temperatures and, therefore, a study of the growth of this phase can predict the behavior of the components in service. This work studies the speed of growth in the alloy INCONEL 713C at temperatures of 800 o C, 875 o C and 950 o C with different treatment times. The present phase in this alloy is Ni3(AlTi), with a very high fraction in volume. The follow-up on the growth of the phase was carried out using scanning and transmission electron microscopy techniques. The speed of growth presents modifications that increase and decrease as a function of time. These variations in speed are attributed to modifications in the size and morphology of the precipitate particles. The changes in size and morphology directly influence the interfacial energy that produces the change in the speed of growth (CW)

  5. Solidification paths in modified Inconel 625 weld overlay material

    DEFF Research Database (Denmark)

    Chandrasekaran, Karthik; Tiedje, Niels Skat; Hald, John

    2009-01-01

    Inconel 625 is commonly used for overlay welding to protect the base metal against high temperature corrosion. The efficiency of corrosion protection depends on effective mixing of the overlay weld with the base metal and the subsequent segregation of alloy elements during solidification....... Metallographic analysis of solidified samples of Inconel 625 with addition of selected elements is compared with thermodynamic modelling of segregation during solidification. The influence of changes in the melt chemistry on the formation of intermetallic phases during solidification is shown. In particular...

  6. Low Cost Heat Treatment Process for Production of Dual Microstructure Superalloy Disks

    Science.gov (United States)

    Gayda, John; Gabb, Tim; Kantzos, Pete; Furrer, David

    2003-01-01

    There are numerous incidents where operating conditions imposed on a component mandate different and distinct mechanical property requirements from location to location within the component. Examples include a crankshaft in an internal combustion engine, gears for an automotive transmission, and disks for a gas turbine engine. Gas turbine disks are often made from nickel-base superalloys, because these disks need to withstand the temperature and stresses involved in the gas turbine cycle. In the bore of the disk where the operating temperature is somewhat lower, the limiting material properties are often tensile and fatigue strength. In the rim of the disk, where the operating temperatures are higher than those of the bore, because of the proximity to the combustion gases, resistance to creep and crack growth are often the limiting properties.

  7. Hardness and electrochemical behavior of ceramic coatings on Inconel

    Directory of Open Access Journals (Sweden)

    C. SUJAYA

    2012-03-01

    Full Text Available Thin films of ceramic materials like alumina and silicon carbide are deposited on Inconel substrate by pulsed laser deposition technique using Q-switched Nd: YAG laser. Deposited films are characterized using UV-visible spectrophotometry and X-ray diffraction. Composite microhardness of ceramic coated Inconel system is measured using Knoop indenter and its film hardness is separated using a mathematical model based on area-law of mixture. It is then compared with values obtained using nanoindentation method. Film hardness of the ceramic coating is found to be high compared to the substrates. Corrosion behavior of substrates after ceramic coating is studied in 3.5% NaCl solution by potentiodynamic polarization and electrochemical impedance spectroscopy measurements. The Nyquist and the Bode plots obtained from the EIS data are fitted by appropriate equivalent circuits. The pore resistance, the charge transfer resistance, the coating capacitance and the double layer capacitance of the coatings are obtained from the equivalent circuit. Experimental results show an increase in corrosion resistance of Inconel after ceramic coating. Alumina coated Inconel showed higher corrosion resistance than silicon carbide coated Inconel. After the corrosion testing, the surface topography of the uncoated and the coated systems are examined by scanning electron microscopy.

  8. Regenerative heat treatments for the extension of the creep life of the superalloy IN-738

    International Nuclear Information System (INIS)

    Stevens, R.A.; Flewitt, P.E.J.

    1979-01-01

    Uniaxial creep tests have been performed on the cast nickel-base superalloy IN-738 at 1023K and 1123K. Microstructural damage occurring during creep has been characterised using transmission electron microscopy of surface and extraction replicas. Considerable coarsening of the γ' precipitates occurs during creep causing a progressive loss of creep strength. Intermediate heat treatment of interrupted specimens regenerates a microstructure similar to the original, and on re-testing significant creep life extensions are observed. These heat treatments do not completely recover the creep life due to the development of grain boundary cavitation. Additional heat treatments were performed under a superimposed hydrostatic pressure of 138 MPa to remove these cavities. (orig.) [de

  9. Microstructural Evolution of Inconel 625 and Inconel 686CPT Weld Metal for Clad Carbon Steel Linepipe Joints: A Comparator Study

    Science.gov (United States)

    Maltin, Charles A.; Galloway, Alexander M.; Mweemba, Martin

    2014-07-01

    Microstructural evolution of Inconel 625 and Inconel 686CPT filler metals, used for the fusion welding of clad carbon steel linepipe, has been investigated and compared. The effects of iron dilution from the linepipe parent material on the elemental segregation potential of the filler metal chemistry have been considered. The results obtained provide significant evidence to support the view that, in Inconel 686CPT weld metal, the segregation of tungsten is a function of the level of iron dilution from the parent material. The data presented indicate that the incoherent phase precipitated in the Inconel 686CPT weld metal has a morphology that is dependent on tungsten enrichment and, therefore, iron dilution. Furthermore, in the same weld metal, a continuous network of finer precipitates was observed. The Charpy impact toughness of each filler metal was evaluated, and the results highlighted the superior impact toughness of the Inconel 625 weld metal over that of Inconel 686CPT.

  10. ANALYSIS OF THE SURFACE PROFILE AND ITS MATERIAL SHARE DURING THE GRINDING INCONEL 718 ALLOY

    Directory of Open Access Journals (Sweden)

    Martin Novák

    2015-05-01

    Full Text Available Grinding is still an important method for surface finishing. At FPTM JEPU research, which deals with this issue is conducted. Experiments are carried out with grinding various materials under different conditions and then selected components of the surface integrity are evaluated. They include roughness Ra, Rm and Rz, Material ratio curve (Abbott Firestone curve and also the obtained roundness. This article deals with grinding nickel Inconel 718 alloy, when selected cutting grinding conditions were used and subsequently the surface profile and the material ratio curve were measured and evaluated.

  11. Rapid solidification and dynamic compaction of Ni-base superalloy powders

    Science.gov (United States)

    Field, R. D.; Hales, S. J.; Powers, W. O.; Fraser, H. L.

    1984-01-01

    A Ni-base superalloy containing 13Al-9Mo-2Ta (in at. percent) has been characterized in both the rapidly solidified condition and after dynamic compaction. Dynamically compacted specimens were examined in the as-compacted condition and observations related to current theories of interparticle bonding. In addition, the recrystallization behavior of the compacted material at relatively low temperature (about 0.5-0.75 Tm) was investigated.

  12. New Mechanistic Models of Long Term Evolution of Microstructure and Mechanical Properties of Nickel Based Alloys

    Energy Technology Data Exchange (ETDEWEB)

    Kruzic, Jamie J. [Oregon State Univ., Corvallis, OR (United States); Evans, T. Matthew [Oregon State Univ., Corvallis, OR (United States); Greaney, P. Alex [Univ. of California, Riverside, CA (United States)

    2018-05-15

    The report describes the development of a discrete element method (DEM) based modeling approach to quantitatively predict deformation and failure of typical nickel based superalloys. A series of experimental data, including microstructure and mechanical property characterization at 600°C, was collected for a relatively simple, model solid solution Ni-20Cr alloy (Nimonic 75) to determine inputs for the model and provide data for model validation. Nimonic 75 was considered ideal for this study because it is a certified tensile and creep reference material. A series of new DEM modeling approaches were developed to capture the complexity of metal deformation, including cubic elastic anisotropy and plastic deformation both with and without strain hardening. Our model approaches were implemented into a commercially available DEM code, PFC3D, that is commonly used by engineers. It is envisioned that once further developed, this new DEM modeling approach can be adapted to a wide range of engineering applications.

  13. Creep-fatigue behavior of turbine disc of superalloy GH720Li at 650 °C and probabilistic creep-fatigue modeling

    Energy Technology Data Exchange (ETDEWEB)

    Hu, Dianyin [School of Energy and Power Engineering, Beihang University, Beijing 100191 (China); Collaborative Innovation Center of Advanced Aero-Engine, Beijing 100191 (China); Beijing Key Laboratory of Aero-Engine Structure and Strength, Beijing 100191 (China); Ma, Qihang [School of Energy and Power Engineering, Beihang University, Beijing 100191 (China); Shang, Lihong [Mining and Materials Engineering, McGill University, Montreal, QC H3A 0C5 (Canada); Gao, Ye [School of Energy and Power Engineering, Beihang University, Beijing 100191 (China); Wang, Rongqiao, E-mail: wangrq@buaa.edu.cn [School of Energy and Power Engineering, Beihang University, Beijing 100191 (China); Collaborative Innovation Center of Advanced Aero-Engine, Beijing 100191 (China); Beijing Key Laboratory of Aero-Engine Structure and Strength, Beijing 100191 (China)

    2016-07-18

    Creep-fatigue experiments have been conducted in nickel-based superalloy GH720Li at an elevated temperature of 650 °C with a stress ratio of 0.1, based on which, different dwell times at the maximum loading were applied to investigate the effect of dwell time on the creep-fatigue behaviors. The tested specimens were cut from the rim region of an actual turbine disc in the hoop direction. The grain size and precipitates of the GH720Li superalloy were examined through scanning electronic microscope (SEM) and energy-dispersive X-ray spectroscopy (EDS) analyses. Experimental data shows creep-fatigue lifetime decreases as the dwell time prolongs. Further, different scattering was observed in the creep-fatigue lifetime at different dwell times. Then a probabilistic model based on the applied mechanical work density (AMWD), with a linear heteroscedastic function that evaluates the non-constant deviation in the creep-fatigue lifetime, was formulated to describe the dependence of creep-fatigue lifetime on the dwell time. Finally, the possible microscopic mechanism of the creep-fatigue behavior has been discussed by SEM with EDS on the fracture surfaces.

  14. Aluminizing of steel 316L and the nickel-base alloy inconel 625 and followed by a high-temperature oxidation process

    International Nuclear Information System (INIS)

    Skokanova, P.; Glasbrenner, H.; Zimmermann, H.

    1995-03-01

    The supercritical water oxidation process of hazardous waste has to be carried out in a reactor which is resistant against corrosion and high pressure and temperature. Pressure tube materials are coated for protection against corrosion. In this work, the reactor materials Inconel 625 and steel 316L have been powder pack aluminized. These coated specimens were subsequently oxidized. Powder mixtures of different composition were tested, time and temperature of the coating and the oxidation processes were varied. Good results were obtained on the steel 316L in respect to thickness of the layer, composition, and adherence on the steel. (orig.)

  15. Sadhana | Indian Academy of Sciences

    Indian Academy of Sciences (India)

    Home; Journals; Sadhana. M Kamaraj. Articles written in Sadhana. Volume 28 Issue 1-2 February-April 2003 pp 115-128. Rafting in single crystal nickel-base superalloys — An overview · M Kamaraj · More Details Abstract Fulltext PDF. Currently nickel-base single crystal (SX) superalloys are considered for the manufacture ...

  16. High cycle fatigue properties of inconel 690

    International Nuclear Information System (INIS)

    Lee, Young Ho; Lee, Byong Whi; Kim, In Sup; Park, Chi Yong

    1997-01-01

    Inconel 690 is presently used as sleeve material and a replacement alloy in degraded steam generators, as well as the material for new steam generators. But Inconel 690 has low thermal conductivity which are 3-8% less than that of Inconel 600 at operating temperature. For the same power output, conduction area must be increased. As a result, more fluid induced vibration can cause a fatigue damage of Inconel 690. High cycle fatigue ruptures occurred in the U-bend regions of North Anna Unit 1 and Mihama Unit 2 steam generators. At this study, the effect of temperature on fatigue crack growth rate in Inconel 690 steam generator tube was investigated at various temperature in air environment. With increasing temperature, fatigue crack growth rate increased and grain size effect decreased. Chromium carbides which have large size and semi-continuous distribution in the grain boundaries decreased fatigue crack growth rate

  17. Bending of pipes with inconel cladding

    Energy Technology Data Exchange (ETDEWEB)

    Nachpitz, Leonardo; Menezes, Carlos Eduardo B; Vieira, Carlos R. Tavares [Primus Processamento de Tubos S.A. (PROTUBO), Macae, RJ (Brazil)

    2009-07-01

    The high-frequency induction bending process, using API pipes coated with Inconel 625 reconciled to a mechanical transformation for a higher degree of resistance, was developed through a careful specification and control of the manufacturing parameters and inherent heat treatments. The effects of this technology were investigated by a qualification process consisting of a sequence of tests and acceptance criteria typically required by the offshore industry, and through the obtained results was proved the effectiveness of this entire manufacturing process, without causing interference in the properties and the quality of the inconel cladding, adding a gain of resistance to the base material, guaranteed by the requirements of the API 5L Standard. (author)

  18. Estudio del comportamiento en caliente del Inconel 718

    OpenAIRE

    Thomas, Amandine

    2005-01-01

    Las aleaciones Inconel son superaleaciones base níquel-cromo, que cubren un amplio espectro de composiciones y de propiedades. Son superaleaciones que tienen buenas propiedades de resistencia mecánica y a la corrosión que se mantienen a temperaturas altas. Las aplicaciones de estas aleaciones son muy amplias: recipientes para tratamiento térmico, turbinas, aviación, plantas nucleares generadoras de energía, etc... El Inconel 718 en particular es una aleación endurecible por precipitación, ...

  19. Competing fatigue failure behaviors of Ni-based superalloy FGH96 at elevated temperature

    Energy Technology Data Exchange (ETDEWEB)

    Miao, Guolei [School of Energy and Power Engineering, Beihang University, Beijing 100191 (China); Yang, Xiaoguang [School of Energy and Power Engineering, Beihang University, Beijing 100191 (China); Collaborative Innovation Center of Advanced Aero-engine(CICAAE), Beihang University, Beijing 100191 (China); Shi, Duoqi, E-mail: shdq@buaa.edu.cn [School of Energy and Power Engineering, Beihang University, Beijing 100191 (China); Collaborative Innovation Center of Advanced Aero-engine(CICAAE), Beihang University, Beijing 100191 (China)

    2016-06-21

    Fatigue experiments were performed on a polycrystalline P/M processed nickel-based superalloy, FGH96 at 600 °C to investigate competing fatigue failure behaviors of the alloy. The experiments were performed at four levels of stress (from high cycle fatigue to low cycle fatigue) at stress ratio of 0.05. There was large variability in fatigue life at both high and low stresses. Scanning electron microscopy (SEM) was used to analyze the failure surfaces. Three types of competing failure modes were observed (surface, sub-surface and internal initiated failures). Crack initiation sites were gradually changed from the surface to the interior with the decreasing of stress level. Roles of microstructures in competing failure mechanism were analyzed. There were six kinds of fatigue crack initiation modes: (1) surface inclusion initiated; (2) surface facet initiated; (3) sub-surface inclusion initiated; (4) sub-surface facet initiated; (5) internal inclusion initiated; (6) internal facet initiated. Inclusions at surface were the life-limiting microstructures at higher stress levels. The probability of occurrence of inclusions initiated is gradually reduced with decreasing of stress level, simultaneously the probability of occurrence of facets initiated is increasing. The existence of the inclusions resulted in large life variability at higher stress levels, while heterogeneity of material caused by random combinations of grains was the main cause of fatigue variability at lower stress levels.

  20. Competing fatigue failure behaviors of Ni-based superalloy FGH96 at elevated temperature

    International Nuclear Information System (INIS)

    Miao, Guolei; Yang, Xiaoguang; Shi, Duoqi

    2016-01-01

    Fatigue experiments were performed on a polycrystalline P/M processed nickel-based superalloy, FGH96 at 600 °C to investigate competing fatigue failure behaviors of the alloy. The experiments were performed at four levels of stress (from high cycle fatigue to low cycle fatigue) at stress ratio of 0.05. There was large variability in fatigue life at both high and low stresses. Scanning electron microscopy (SEM) was used to analyze the failure surfaces. Three types of competing failure modes were observed (surface, sub-surface and internal initiated failures). Crack initiation sites were gradually changed from the surface to the interior with the decreasing of stress level. Roles of microstructures in competing failure mechanism were analyzed. There were six kinds of fatigue crack initiation modes: (1) surface inclusion initiated; (2) surface facet initiated; (3) sub-surface inclusion initiated; (4) sub-surface facet initiated; (5) internal inclusion initiated; (6) internal facet initiated. Inclusions at surface were the life-limiting microstructures at higher stress levels. The probability of occurrence of inclusions initiated is gradually reduced with decreasing of stress level, simultaneously the probability of occurrence of facets initiated is increasing. The existence of the inclusions resulted in large life variability at higher stress levels, while heterogeneity of material caused by random combinations of grains was the main cause of fatigue variability at lower stress levels.

  1. Comparison of Thermodynamic Predictions and Experimental Observations on B Additions in Powder-Processed Ni-Based Superalloys Containing Elevated Concentrations of Nb

    Science.gov (United States)

    Antonov, Stoichko; Huo, Jiajie; Feng, Qiang; Isheim, Dieter; Seidman, David N.; Sun, Eugene; Tin, Sammy

    2018-03-01

    Boron additions to Ni-based superalloys are considered to be beneficial to the creep properties of the alloy, as boron has often been reported to increase grain boundary cohesion, increase ductility, and promote the formation of stable boride phases. Despite the importance, it is not well understood whether these improvements are associated with the presence of elemental boron or stable borides along the grain boundaries. In this investigation, two experimental powder-processed Ni-based superalloys containing elevated levels of Nb were found to exhibit increased solubility for B in the γ matrix when compared to similar commercial Ni-based superalloys. This resulted in an overall lower B concentration at grain boundaries that suppressed boride formation. As the predictive capability of CALPHAD database models for Ni-based superalloys have improved over the years, some discrepancies may still persist around compositionally heterogeneous features such as grain boundaries. Improved quantification of the characteristic partitioning of B as a function of the bulk alloy composition is required for understanding and predicting the stability of borides.

  2. Aging of vacuum plasma sprayed MCrAlY protective layers and their interaction with nickel- and cobalt-based γ/γ'-superalloys

    International Nuclear Information System (INIS)

    Terberger, Philipp J.

    2015-01-01

    γ/γ' single crystal superalloys with plasma-sprayed thermal barrier coating systems are used as turbine rotor blades in gas turbines if the blades are exposed to high temperatures and high mechanical loads. A bond coat (BC) is part of the thermal barrier coating system. It protects the substrate from oxidation and ensures good bonding of the ceramic coating that serves as a thermal insulator. MCrAlY (M=Ni,Co) alloys are commonly used as BCs. They form a protective Al 2 O 3 layer. This study investigates four different vacuum plasma-sprayed MCrAlY BCs with and without Re after thermal treatment of up to 1000 h at 1044 C in air. The employed substrates are the Ni-based superalloy ERBO1 and the novel Co-based γ/γ' superalloy ERBOCo-1. Additionally, the ternary γ/γ' alloy Co-9Al-9W (in at.%) was aged with a BC for up to 500 h at 900 C. Up to now little is known about the interaction of the Co-based substrates and the BCs. Oxidation and Al depletion of the BC as well as the interdiffusion of BCs and substrates are analysed primarily on the basis of SEM/EDX and XRD. The effect of Y and Hf on the microstructure of the oxide scale is discussed. Rate constants show that Hf results in higher oxidation rates while Re slows down the oxidation. The influence of the alloying elements on the BC microstructure is described. For example, Co prevents the formation of γ' phase, Re slows down diffusion and results in the formation of brittle phases. The choice of substrate material has no measurable influence on the oxidation. Qualitative and quantitative analysis of the interdiffusion zone (IDZ) shows that the choice of substrate surface pre-treatment (grit blasting or grinding) has a major influence on the interdiffusion behaviour with the BC. Grinding results in a thinner IDZ and fewer topologically closed packed (TCP) phases. The reason for this is the recrystallisation of the single crystal substrate. A study of the influence of the substrate crystal

  3. CLASSICAL AREAS OF PHENOMENOLOGY: First-principles calculations for the elastic properties of Ni-base model superalloys: Ni/Ni3Al multilayers

    Science.gov (United States)

    Wang, Yun-Jiang; Wang, Chong-Yu

    2009-10-01

    A model system consisting of Ni[001](100)/Ni3Al[001](100) multi-layers are studied using the density functional theory in order to explore the elastic properties of single crystal Ni-based superalloys. Simulation results are consistent with the experimental observation that rafted Ni-base superalloys virtually possess a cubic symmetry. The convergence of the elastic properties with respect to the thickness of the multilayers are tested by a series of multilayers from 2γ'+2γ to 10γ'+10γ atomic layers. The elastic properties are found to vary little with the increase of the multilayer's thickness. A Ni/Ni3Al multilayer with 10γ'+10γ atomic layers (3.54 nm) can be used to simulate the mechanical properties of Ni-base model superalloys. Our calculated elastic constants, bulk modulus, orientation-dependent shear modulus and Young's modulus, as well as the Zener anisotropy factor are all compatible with the measured results of Ni-base model superalloys R1 and the advanced commercial superalloys TMS-26, CMSX-4 at a low temperature. The mechanical properties as a function of the γ' phase volume fraction are calculated by varying the proportion of the γ and γ' phase in the multilayers. Besides, the mechanical properties of two-phase Ni/Ni3Al multilayer can be well predicted by the Voigt-Reuss-Hill rule of mixtures.

  4. Removal of Non-metallic Inclusions from Nickel Base Superalloys by Electromagnetic Levitation Melting in a Slag

    Science.gov (United States)

    Manjili, Mohsen Hajipour; Halali, Mohammad

    2018-02-01

    Samples of INCONEL 718 were levitated and melted in a slag by the application of an electromagnetic field. The effects of temperature, time, and slag composition on the inclusion content of the samples were studied thoroughly. Samples were compared with the original alloy to study the effect of the process on inclusions. Size, shape, and chemical composition of remaining non-metallic inclusions were investigated. The samples were prepared by Standard Guide for Preparing and Evaluating Specimens for Automatic Inclusion Assessment of Steel (ASTM E 768-99) method and the results were reported by means of the Standard Test Methods for Determining the Inclusion Content of Steel (ASTM E 45-97). Results indicated that by increasing temperature and processing time, greater level of cleanliness could be achieved, and numbers and size of the remaining inclusions decreased significantly. It was also observed that increasing calcium fluoride content of the slag helped reduce inclusion content.

  5. Precipitation and clustering in the early stages of ageing in Inconel 718

    International Nuclear Information System (INIS)

    Alam, Talukder; Chaturvedi, Mahesh; Ringer, Simon P.; Cairney, Julie M.

    2010-01-01

    Research highlights: → IN718 could be age hardened rapidly by secondary phase formation. → Co-located phases were observed in the earliest stage of detection. → Clustering of Ti/Al and Nb atoms was observed prior to precipitation. - Abstract: In this report we investigate the onset and evolution of precipitation in the early stages of ageing in the alloy WE 91, a variant of the Ni-Fe-Cr superalloy Inconel 718 (IN718). Transmission electron microscopy and atom probe tomography were used to study the size and volume fraction of γ' and γ'' precipitates and the extent of pre-precipitate clustering of Al/Ti and Nb. Co-located γ' and γ'' precipitates were observed from the shortest ageing times that precipitates could be visualised using atom probe. At shorter times, prior to the observation of precipitates, clustering of Al/Ti and Nb was shown to occur. The respective volume fraction of the γ' and γ'' precipitates and the clustering of Al/Ti and Nb suggest that γ'' nucleates prior to γ' during ageing at 706 deg. C for this alloy.

  6. Microstructural and mechanical characterization of injection molded 718 superalloy powders

    Energy Technology Data Exchange (ETDEWEB)

    Özgün, Özgür [Bingol University, Faculty of Engineering and Architecture, Mechanical Eng. Dep., 12000 Bingol (Turkey); Gülsoy, H. Özkan, E-mail: ogulsoy@marmara.edu.tr [Marmara University, Technology Faculty, Metallurgy and Materials Eng. Dep., 34722 Istanbul (Turkey); Yılmaz, Ramazan [Sakarya University, Technology Faculty, Metallurgy and Materials Eng. Dep., 54187 Sakarya (Turkey); Fındık, Fehim [Sakarya University, Technology Faculty, Metallurgy and Materials Eng. Dep., 54187 Sakarya (Turkey) and International University of Sarajevo, Faculty of Engineering and Natural Sciences, Department of Mechanical Engineering, 71000 Sarajevo, Bosnia and Herzegovina (Bosnia and Herzegowina)

    2013-11-05

    Highlights: •Microstructural and mechanical properties of injection molded Nickel 718 superalloy were studied. •The maximum sintered density achieved this study was 97.3% at 1290 °C for 3 hours. •Tensile strength of 1022 MPa and elongation of 5.3% were achieved for sintered-heat treated samples. -- Abstract: This study concerns with the determination of optimum production parameters for injection molding 718 superalloy parts. And at the same time, microstructural and mechanical characterization of these produced parts was also carried out. At the initial stage, 718 superalloy powders were mixed with a multi-component binder system for preparing feedstock. Then the prepared feedstock was granulated and shaped by injection molding. Following this operation, the shaped samples were subjected to the debinding process. These samples were sintered at different temperatures for various times. Samples sintered under the condition that gave way to the highest relative density (3 h at 1290 °C) were solution treated and aged respectively. Sintered, solution treated and aged samples were separately subjected to microstructural and mechanical characterization. Microstructural characterization operations such as X-ray diffraction, optical microscope (OM), scanning electron microscope (SEM), transmission electron microscope (TEM) and elemental analysis showed that using polymeric binder system led to plentiful carbide precipitates to be occurred in the injection molded samples. It is also observed that the volume fractions of the intermetallic phases (γ′ and γ″) obtained by aging treatment were decreased due to the plentiful carbide precipitation in the samples. Mechanical characterization was performed by hardness measurements and tensile tests.

  7. Fundamental studies on electron-beam welding of heat-resistant superalloys for nuclear plants: Report 4. Mechanical properties of welded joints

    International Nuclear Information System (INIS)

    Susei, S.; Shimizu, S.; Aota, T.

    1982-04-01

    In this report, electron-beam (EB) welded joints and TIG welded joints of various superalloys to be used for nuclear plants, such as Hastelloy-type, Inconel-type and Incoloy-type, are systematically evaluated in terms of tensile properties, low-cycle fatigue properties at elevated temperatures, creep and creep-rupture properties. It was fully confirmed as conclusion that the EB welded joints are superior to the TIG welded ones in mechanical properties, especially at high temperature. In the evaluation of creep properties, ductility is one of the most important criteria to represent the resistance against fracture due to creep deformation, and this criterion is very useful in evaluating the properties of welded joints. Therefore, the more comparable to the base metal the electron beam welded joint becomes in terms of ductility, the more resistant is it against fracture. From this point of view, the electron beam welded joint is considerably superior to the TIG welded joint [fr

  8. A quantitative approach to study the effect of local texture and heterogeneous plastic strain on the deformation micromechanism in RR1000 nickel-based superalloy

    International Nuclear Information System (INIS)

    Birosca, S.; Di Gioacchino, F.; Stekovic, S.; Hardy, M.

    2014-01-01

    In a weakly textured material with relatively pore-free and homogeneous microstructure, the local texture can influence primary crack propagation and secondary crack initiation, depending on specific microtexture cluster size. Moreover, the plastic strain assessment and strain quantity within individual grains are essential for understanding the material susceptibility to crack initiation and propagation at various loading conditions and temperature ranges. In the current study, electron backscatter diffraction (EBSD) is applied to measure the plastic strain present in RR1000 nickel-based superalloy microstructure following thermo-mechanical fatigue tests. The EBSD plastic strain measurements are evaluated to identify the distinctive deformation mode within individual grains. It was evident from the overall statistical analyses carried out for over 2000 grains that cube (〈0 0 1〉//loading direction) and near cube orientations (φ 1 , Φ, φ 2 : 0, 0–15, 0) behaved as “soft” grains with a high Schmid factor and contained low geometrically necessary dislocation (GND) density as a result of low strain hardening at the early stage of deformation for such grains. The near cube orientation (typically φ 1 , Φ, φ 2 : 0, 9, 0) was the softest orientation among the cube family. While the brass grains (〈1 1 1〉//loading direction) acted as “hard” grains that have the lowest Schmid factor with the highest Taylor factor and GND density compared with other oriented grains. A high GND content was found in the vicinity of the grain boundaries in the soft grains and on slip plane traces within the hard grains. It is concluded that GND absolute value for each grain can vary, as it is interrelated with deformation degree, but the GND locations within the grains give indications of the strain hardening state and deformation stages in hard and soft grains. Furthermore, the areas with random local texture contained high strain incompatibilities between neighbouring

  9. Corrosion properties of plasma deposited nickel and nickel-based alloys

    Czech Academy of Sciences Publication Activity Database

    Voleník, Karel; Pražák, M.; Kalabisová, E.; Kreislová, K.; Had, J.; Neufuss, Karel

    2003-01-01

    Roč. 48, č. 3 (2003), s. 215-226 ISSN 0001-7043 R&D Projects: GA ČR GA106/99/0298 Institutional research plan: CEZ:AV0Z2043910 Keywords : plasma deposits, nickel, nickel-based alloys Subject RIV: JK - Corrosion ; Surface Treatment of Materials

  10. Extrusion and intrusion evolution in cyclically strained cast superalloy Inconel 738LC using confocal laser scanning microscope and AFM

    Czech Academy of Sciences Publication Activity Database

    Obrtlík, Karel; Juliš, M.; Man, Jiří; Podrábský, T.; Polák, Jaroslav

    2010-01-01

    Roč. 241, - (2010), Art. No. 012054 ISSN 1742-6588. [ICSMA-15 (15th International Conference on the Strength of Materials). Dresden, 16.08.2009-21.08.2009] R&D Projects: GA AV ČR 1QS200410502; GA ČR GA106/07/1507 Institutional research plan: CEZ:AV0Z20410507 Keywords : fatigue * persistent slip marking * Inconel 738LC Subject RIV: JL - Materials Fatigue, Friction Mechanics http://iopscience.iop.org/1742-6596/240/1/012054

  11. Refractory metal based superalloys

    International Nuclear Information System (INIS)

    Alonso, Paula R.; Vicente, Eduardo E.; Rubiolo, Gerardo H.

    1999-01-01

    Refractory metals are looked as promising materials for primary circuits in fission reactors and even as fusion reactor components. Indeed, superalloys could be developed which take advantage of their high temperature properties together with the benefits of a two- phase (intermetallic compound-refractory metal matrix) coherent structure. In 1993, researchers of the Office National d'Etudes et de Recherches Aerospatiales of France reported the observation of such a coherent structure in the Ta-Ti-Zr-Al-Nb-Mo system although the exact composition is not reported. The intermetallic compound would be Ti 2 AlMo based. However, the formation of this compound and its possible coexistence with a disordered bcc phase in the ternary system Ti-Al-Mo is a controversial subject in the related literature. In this work we develop a technique to obtain homogeneous alloys samples with 50 Ti-25 Al-25 Mo composition. The resulting specimens were characterized by optical and electronic metallography (SEM), microprobe composition measurements (EPMA) and X-ray diffraction (XRD) analyses. The results show the evidence for a bcc (A2→B2) ordering reaction in the Ti-Al-Mo system in the 50 Ti-25 Al-25 Mo composition. (author)

  12. Influence of composition on precipitation behavior and stress rupture properties in INCONEL RTM740 series superalloys

    Science.gov (United States)

    Casias, Andrea M.

    Increasing demands for energy efficiency and reduction in CO2 emissions have led to the development of advanced ultra-supercritical (AUSC) boilers. These boilers operate at temperatures of 760 °C and pressures of 35 MPa, providing efficiencies close to 50 pct. However, austenitic stainless steels typically used in boiler applications do not have sufficient creep or oxidation resistance. For this reason, nickel (Ni)-based superalloys, such as IN740, have been identified as potential materials for AUSC boiler tube components. However, IN740 is susceptible to heat-affected-zone liquation cracking in the base metal of heavy section weldments. To improve weldability, IN740H was developed. However, IN740H has lower stress rupture ductility compared to IN740. For this reason, two IN740H modifications have been produced by lowering carbon content and increasing boron content. In this study, IN740, IN740H, and the two modified IN740H alloys (modified 1 and 2) were produced with equiaxed grain sizes of 90 ìm (alloys IN740, IN740H, and IN740H modified 1 alloys) and 112 µm (IN740H modified 2 alloy). An aging study was performed at 800 °C on all alloys for 1, 3, 10, and 30 hours to assess precipitation behavior. Stress rupture tests were performed at 760 °C with the goal of attaining stress levels that would yield rupture at 1000 hours. The percent reduction in area was measured after failure as a measure of creep ductility. Light optical, scanning electron, and transmission electron microscopy were used in conjunction with X-ray diffraction to examine precipitation behavior of annealed, aged, and stress rupture tested samples. The amount and type of precipitation that occurred during aging prior to stress rupture testing or in-situ during stress rupture testing influenced damage development, stress rupture life, and ductility. In terms of stress rupture life, IN740H modified 2 performed the best followed by IN740H modified 1 and IN740, which performed similarly, and IN740

  13. Length change of the alloys Waspaloy and Inconel 718 after long-term annealing

    International Nuclear Information System (INIS)

    Kinzel, Svenja

    2016-01-01

    Within the scope of this work the contraction behavior of Ni-based superalloy Waspaloy could in detail be referred to a combination of different microstructural changes and the results could partially be transferred to Ni-Fe-based alloy Inconel 718. Isothermal annealing of sample rods at temperatures between 450 C and 750 C induces an average relative length contraction of about -2.10"-"4. It is apparent that contraction is more pronounced for lower temperatures (-3.10"-"4 at 550 C) than for higher ones (-1.10"-"4 at 750 C). Within the first 300 hours of annealing the contraction reaches about 70-75% of the value measured after 10,000 hours. This means the major part of the effect takes place at the beginning of long term annealing but even after 10,000 hours no saturation occurs. On the basis of lattice parameter measurements it could be found that within the first 300 hours a significant lattice parameter decrease of matrix and γ"' phase emerged. Longer annealing time does not cause further lattice contraction. This sample behavior can be explained by temperature dependence of phase fractions and phase compositions. Thermodynamic calculations as well as stereological analysis of micrographs show a decrease of stable γ"'-phase content with increasing temperature. In parallel, TEM-EDS measurements and calculated phase fractions show concentration fluctuations due to the different precipitate fraction, which cause contraction of the lattice parameter. Furthermore, within the first 100 hours at temperatures up to 650 C the formation or Ni-Cr rich domains could be observed. As these domains exhibit a smaller lattice parameter than the matrix they contribute to the more pronounced contraction at lower temperatures. While XRD measurements point to the formation of Ni_3Cr, TEM-EDS measurements reveal a composition of (Ni,Co)_2Cr. Stress relief heat treatment at higher temperatures (815 C) after annealing shows that the effect of contraction is reversible. It causes an

  14. Microstructural evolution during transient liquid phase bonding of Inconel 617 using Ni-Si-B filler metal

    International Nuclear Information System (INIS)

    Jalilian, F.; Jahazi, M.; Drew, R.A.L.

    2006-01-01

    The influence of process parameters on microstructural characteristics of transient liquid phase (TLP) bonded Inconel 617 alloy was investigated. Experiments were carried out at 1065 deg. C using nickel based filler metal (Ni-4.5% Si-3% B) with B as the melting point depressant (MPD) element. Two different thickness of interlayer and various holding times were employed. The influence of these processing parameters on the characteristics of the joint area particularly size, morphology and composition of precipitates was investigated. The presence of MoB, Mo 2 B, M 23 C 6 , TiC, M 23 (B, C) 6 and Ni 3 B precipitates in the diffusion layer and Ni 3 B, Ni 3 Si and Ni 5 Si 2 precipitates in the interlayer at the interface between the base metal and interlayer were demonstrated using electron back scattered diffraction (EBSD), energy dispersive spectrometry (EDS) and TEM

  15. FLiNaK compatibility studies with Inconel 600 and silicon carbide

    Energy Technology Data Exchange (ETDEWEB)

    Yoder, Graydon L., E-mail: yodergljr@ornl.gov [Oak Ridge National Laboratory, Bldg. 5700, MS 6167 Bethel Valley Rd., Oak Ridge, TN 37831 (United States); Heatherly, Dennis; Wilson, Dane [Oak Ridge National Laboratory, Bldg. 5700, MS 6167 Bethel Valley Rd., Oak Ridge, TN 37831 (United States); Caja, Mario [Electrochemical Systems, Inc. (ESI), 9320 Collingwood Rd., Knoxville, TN 37922 (United States)

    2016-10-15

    Highlights: • A versatile experimental design has been developed to examine liquid fluoride salt materials compatibility behavior. • Samples of silicon carbide and a grafoil/nickel spiral wound gasket were exposed to FLiNaK salt at 700 °C for 90 days and showed no degradation. • Alloy 600 showed material effects penetrating up to 300 μm below the salt interface after exposure to the salt for 90 days at 700 °C. • Comparison of the Alloy 600 corrosion results with existing data indicated that results were comparable to the few corrosion results available for Alloy 600. • Sapphire viewing windows incorporated in the experiment showed fogging by condensed salt components at the highest test temperatures. - Abstract: A small liquid fluoride salt test apparatus has been constructed and testing has been conducted to examine the compatibility of silicon carbide (SiC), Inconel 600 and a spiral wound gasket material in FLiNaK, the ternary eutectic alkaline metal fluoride salt mixture. These tests were conducted to evaluate materials and sealing systems that could be used in fluoride salt systems. Three months of testing at 700 °C was conducted to assure that these materials and seals would be acceptable when operating under prototypic operating conditions. The SiC specimens showed little or no change over the test period, while the spiral wound gasket material did not show any degradation except that salt might have been seeping into the outermost spirals of the gasket. The Inconel 600 specimens showed regions of voiding which penetrated the specimen surface to about 250 μm in depth. Analysis indicated that the salt had leached chrome from the Inconel surface, as was expected for this material.

  16. Quality-productivity decision making when turning of Inconel 718 aerospace alloy: A response surface methodology approach

    Directory of Open Access Journals (Sweden)

    Hamid Tebassi

    2017-06-01

    Full Text Available Inconel 718 is among difficult to machine materials because of its abrasiveness and high strength even at high temperature. This alloy is mainly used in aircraft and aerospace industries. Therefore, it is very important to reveal and evaluate cutting tools behavior during machining of this kind of alloy. The experimental study presented in this research work has been carried out in order to elucidate surface roughness and productivity mathematical models during turning of Inconel 718 superalloy (35 HRC with SiC Whisker ceramic tool at various cutting parameters (depth of cut, feed rate, cutting speed and radius nose. A small central composite design (SCCD including 16 basics runs replicated three times (48 runs, was adopted and graphically evaluated using Fraction of design space (FDS graph, completed by a statistical analysis of variance (ANOVA. Mathematical models for surface roughness and productivity were developed and normality was improved using the Box-Cox transformation. Results show that surface roughness criterion Ra was mainly influenced by cutting speed, radius nose and feed rate, and that the depth of cut had major effect on productivity. Finally, ranges of optimized cutting conditions were proposed for serial industrial production. Industrial benefit was illustrated in terms of high surface quality accompanied with high productivity. Indeed, results show that the use of optimal cutting condition had an industrial benefit to 46.9 % as an improvement in surface quality Ra and 160.54 % in productivity MRR.

  17. Influence of cobalt, tantalum, and tungsten on the microstructure and mechanical properties of superalloy single crystals

    International Nuclear Information System (INIS)

    Nathal, M.V.; Ebert, L.J.

    1982-01-01

    The influence of Co, Ta, and W on the microstructure and mechanical properties of nickel base super-alloy single crystals was investigated. A matrix of alloys was based on Mar-M 247 stripped of C, B, Zr, and Hf. The microstructures of the alloys were examined using optical and electron microscopy, phase extraction, X-ray diffraction, and differential thermal analysis. Tensile and creep-rupture tests were performed at 1000 C. An increase in tensile and creep strength resulted when Co was removed from alloys containing high refractory metal contents, but Co effects were negligible for alloys with lower refractory metal levels. In the composition range studied, W was more effective than Ta in increasing the creep resistance. The mechanical properties are discussed in relation to the microstructures of the alloys

  18. Influence of cobalt, tantalum, and tungsten on the microstructure and mechanical properties of superalloy single crystals

    Science.gov (United States)

    Nathal, M. V.; Ebert, L. J.

    1982-01-01

    The influence of Co, Ta, and W on the microstructure and mechanical properties of nickel base super-alloy single crystals was investigated. A matrix of alloys was based on Mar-M 247 stripped of C, B, Zr, and Hf. The microstructures of the alloys were examined using optical and electron microscopy, phase extraction, X-ray diffraction, and differential thermal analysis. Tensile and creep-rupture tests were performed at 1000 C. An increase in tensile and creep strength resulted when Co was removed from alloys containing high refractory metal contents, but Co effects were negligible for alloys with lower refractory metal levels. In the composition range studied, W was more effective than Ta in increasing the creep resistance. The mechanical properties are discussed in relation to the microstructures of the alloys.

  19. Microstructural characterization, formation mechanism and fracture behavior of the needle δ phase in Fe–Ni–Cr type superalloys with high Nb content

    Energy Technology Data Exchange (ETDEWEB)

    Ning, Yongquan, E-mail: luckyning@nwpu.edu.cn [School of Materials Science & Engineering, Northwestern Polytechnical University, Xi' an 710072 (China); Huang, Shibo [Anshan Iron & Steel Group Corporation Bayuquan Subsidiary Company, Bayuquan 115007 (China); Fu, M.W. [Department of Mechanical Engineering, Hong Kong Polytechnic University, Hung Hom, Kowloon, Hong Kong (China); Dong, Jie [Inspection & Research Institute of Boiler & Pressure Vessel of Jiangxi Province, Nanchang 330029 (China)

    2015-11-15

    Microstructural characterization, formation mechanism and fracture behavior of the needle δ phase in Fe–Ni–Cr type superalloys with high Nb content (GH4169, equivalent to Inconel 718) have been quantitatively investigated in this research. The typical microstructures of δ phases with the stick, mixed and needle shapes obviously present in Inconel 718 after the isothermal upsetting at the temperature of 980–1060 °C with the initial strain rate of 10{sup −3}–10{sup −1} s{sup −1}. It is found that the shape of the δ phase has a great effect on the mechanical properties of the alloy, viz., the stick δ phase behaves good plasticity and the needle δ phase has good strength. In addition, the needle δ phase can be used to control the grain size as it can prevent grain growth. The combined effect of the localized necking and microvoid coalescence leads to the final ductile fracture of the GH4169 components with the needle δ phase. Both dislocation motion and atom diffusion are the root-cause for the needle δ phase to be firstly separated at grain boundary and then at sub-boundary. The formation mechanism of the needle δ phase is the new finding in this research. Furthermore, it is the primary mechanism for controlling the needle δ phase in Fe–Ni–Cr type superalloys with high Nb content. - Highlights: • Shape of the δ phase takes great effect on mechanical property. • Needle δ phase plays a great role to prevent grain growth. • Needle δ phase can enhance the fracture strength. • Microstructure mechanism of the needle δ phase has been investigated. • Fracture behavior of the needle δ phase has been studied.

  20. A Study on Fretting Behavior in Room Temperature for Inconel Alloy 690

    Science.gov (United States)

    Kwon, Jae Do; Chai, Young Suck; Bae, Yong Tak; Choi, Sung Jong

    The initial crack under fretting condition occurs at lower stress amplitude and lower cycles of cyclic loading than that under plain fatigue condition. The fretting damage, for example, can be observed in fossil and nuclear power plant, aircraft, automobile and petroleum chemical plants etc. INCONEL alloy 690 is a high-chromium nickel alloy having excellent resistance to many corrosive aqueous media and high-temperature atmospheres. This alloy is used extensively in the industries of nuclear power, chemicals, heat-treatment and electronics. In this paper, the effect of fretting damage on fatigue behavior for INCONEL alloy 690 was studied. Also, various kinds of tests on mechanical properties such as hardness, tension and plain fatigue tests are performed. Fretting fatigue tests were carried out with flat-flat contact configuration using a bridge type contact pad and plate type specimen. Through these experiments, it is found that the fretting fatigue strength decreased about 43% compared to the plain fatigue strength. In fretting fatigue, the wear debris is observed on the contact surface, and the oblique micro-cracks are initiated at an earlier stage. These results can be used as the basic data in a structural integrity evaluation of heat and corrosion resistant alloy considering fretting damages.

  1. Studying the effect of Ruthenium on High Temperature Mechanical Properties of Nickel Based Superalloys and Determining the Universal Behavior of Ruthenium at Atomic Scale with respect to alloying elements, Stress and Temperature

    Directory of Open Access Journals (Sweden)

    Sriswaroop Dasari

    2016-10-01

    Full Text Available Any property of a material is a function of its microstructure and microstructure is a function of material composition. So, to maximize the desired properties of a material, one has to understand the evolution of microstructure which in turn is nothing but the reflection of the role of alloying elements. Research has not been done to understand the universal behavior of a certain base/alloying element. Let’s take the example of Cl- ion in HCl, we all know that in general, chloride ion can only be replaced by Fluoride or oxygen ion and that no other ion can replace it. But when you consider a metal like Ni, Co, Cr, Fe etc. there is no establishment that it behaves only in a certain way. Though I concord to the fact that discovery of universal behavior of Ni is lot complex than chloride ion, I think that future research should be focused in this direction also. Superalloys are the candidate materials required to improve thermal efficiency of a gas turbine by allowing higher turbine inlet gas temperatures. Gas turbines are the heart of local power systems, next generation jet engines and high performance space rockets. Recent research in superalloys showed that addition of some alloying elements in minor quantities can result in drastic change in properties. Such an alloying element is Ruthenium (Ru. Addition of Ruthenium to superalloys has shown improvement in mechanical properties by an order of magnitude. However reasons for such improvement are not known yet. Hence, there is a need to identify its role and discover the universal behavior of ruthenium to utilize it efficiently. In this proposal, we study materials with different compositions that are derived based on one ruthenium containing superalloy, and different thermomechanical history. Based on the evolution of microstructures and results of mechanical testing, we plan to determine the exact role of Ruthenium and prediction of its behavior with respect to other elements in the material

  2. High Temperature Degradation of Powder-processed Ni-based Superalloy

    Directory of Open Access Journals (Sweden)

    Natália Luptáková

    2015-05-01

    Full Text Available The aim of present work is to study the high temperature degradation of the powder-processed polycrystalline superalloy Ni-15Cr-18Co-4Al-3.5Ti-5Mo. This superalloy has been applied as material for grips of a creep machine. The material was exposed at 1100 °C for about 10 days at 10 MPa stress. During the creep test occurred unacceptable creep deformation of grips as well as severe surface oxidation with scales peeling off. Three types of the microstructure were observed in the studied alloy: (i unexposed state; (ii heat treated (annealing - 10 min/1200 °C and (iii after using as a part of the equipment of the creep machine during the creep test. It is shown that the microstructure degradation resulting from the revealed γ´ phase fcc Ni3(Al,Ti particles preferentially created at the grain boundaries of the samples after performing creep tests affects mechanical properties of the alloy and represents a significant contribution to all degradation processes affecting performance and service life of the creep machine grips. Based on investigation and obtained results, the given material is not recommended to be used for grips of creep machine at temperatures above 1000 °C.

  3. The influence of applied heat-treatment on in 718 fatigue life at three point flexural bending

    Directory of Open Access Journals (Sweden)

    J. Belan

    2017-01-01

    Full Text Available The Inconel alloy 718 is an iron-nickel based superalloy with a working temperature up to 650 °C. Presented phases such as γ'' (Ni3Nb, γ' (Ni3Al, and δ (delta – Ni3Nb are responsible for the alloy's unique properties. The δ – delta phase is profitable when situated at grain boundaries in small quantities due to increasing fatigue life. However, at temperatures close to 650 °C the γ'' transforms to δ – delta and causes a decrease in fatigue life. Heat-treatment (800°C/ for 72 hours and its influence on fatigue life are discussed in this paper. Fatigue tests were carried out at room temperature. After the tests we plotted the S-N curves for both stages. SEM (Scanning Electron Microscopy fractography was carried out as well.

  4. Corrosion of nickel-base heat resistant alloys in simulated VHTR coolant helium at very high temperatures

    International Nuclear Information System (INIS)

    Shindo, Masami; Kondo, Tatsuo

    1976-01-01

    A comparative evaluation was made on three commercial nickel-base heat resistant alloys exposed to helium-base atmosphere at 1000 0 C, which contained several impurities in simulating the helium cooled very high temperature nuclear reactor (VHTR) environment. The choice of alloys was made so that the effect of elements commonly found in commercial alloys were typically examined. The corrosion in helium at 1000 0 C was characterized by the sharp selection of thermodynamically unstable elements in the oxidizing process and the resultant intergranular penetration and internal oxidation. Ni-Cr-Mo-W type solution hardened alloy such as Hastelloy-X showed comparatively good resistance. The alloy containing Al and Ti such as Inconel-617 suffered adverse effect in contrast to its good resistance to air oxidation. The alloy nominally composed only of noble elements, Ni, Fe and Mo, such as Hastelloy-B showed least apparent corrosion, while suffered internal oxidation due to small amount of active impurities commonly existing in commercial heats. The results were discussed in terms of selection and improvement of alloys for uses in VHTR and the similar systems. (auth.)

  5. Analysis of shot-peening and residual stress relaxation in the nickel-based superalloy RR1000

    International Nuclear Information System (INIS)

    Foss, B.J.; Gray, S.; Hardy, M.C.; Stekovic, S.; McPhail, D.S.; Shollock, B.A.

    2013-01-01

    This work assesses the residual stress relaxation of the nickel-based alloy RR1000 due to thermal exposure and dwell-fatigue loading. A number of different characterization methods, including X-ray residual stress analysis, electron back-scattered diffraction, microhardness testing and focused ion beam secondary electron imaging, contributed to a detailed study of the shot-peened region. Thermal exposure at 700 °C resulted in a large reduction in the residual stresses and work-hardening effects in the alloy, but the subsurface remained in a beneficial compressive state. Oxidizing environments caused recrystallization in the near surface, but did not affect the residual stress-relaxation behaviour. Dwell-fatigue loading caused the residual stresses to return to approximately zero at nearly all depths. This work forms part of an ongoing investigation to determine the effects of shot-peening in this alloy with the motivation to improve the fatigue and oxidation resistance at 700 °C

  6. The metallurgy of superalloys part 2

    International Nuclear Information System (INIS)

    Abdelazim, M.E.; Hammad, F.H.

    1990-01-01

    This is part II of the report titled 'the metallurgy of superalloys'. It deals with the effect of heat treatment and operating conditions (thermal exposure and environment) on the mechanical properties of superalloys. The heat treatment is important in the development of superalloys through that it controls type, amount, size shape and distribution of the precipitate and the grain size of the matrix. The thermal exposure leads to reduction in the amount of the primary carbides and to precipitation of secondary carbides. Also it leads to the agglomeration and coarsening of gamma or the transformation of gamma phase to phase. The environment may lead to the internal oxidation, carburization, decarburization or sulphidization of the superalloys which may result in the degradation of their mechanical properties. This part gives also an example of applications of superalloys in the field of nuclear reactors especially high temperature-gas cooled reactors. Joined with this part a table which contains the major superalloys including its chemical analysis, creep rupture strength and some of its applications. 1 tab

  7. Aleación superficial de superaleaciones base níquel mediante láser

    Directory of Open Access Journals (Sweden)

    Rodríguez, G. P.

    1998-04-01

    Full Text Available Ni based superalloys present a high oxidation resistance at high temperature as well as good mechanical properties. But new tecnhology developments forcé to research in this materials to improve their properties at high temperature. In this work, two Ni based superalloys (Nimonic 80A and Inconel 600 were surface alloyed with aluminium using a high power laser. SEM and EDX were used to study the microstructure of the obtained coatings. Alloyed specimens were tested at 1.273 K between 24 and 250 h. Results showed the generation of a protective and continuous coating of alumina on the laser treated specimens surface that can improve oxidation resistance.

    Las superaleaciones base níquel presentan una elevada resistencia a la oxidación a alta temperatura, así como excelentes propiedades mecánicas. Los nuevos desarrollos tecnológicos (condiciones cada vez más agresivas obligan a una casi continua modificación de dichas aleaciones. En el presente trabajo, dos superaleaciones base níquel (Nimonic 80A e Inconel 600 se alean superficialmente con aluminio utilizando un láser de alta potencia. Se estudia la microestructura de la capas obtenidas mediante SEM y EDX. Se realizan ensayos de oxidación a 1.273 K sobre las probetas aleadas y sobre el material base durante tiempos variables entre 24 y 250 h. Los resultados indican la formación de una capa protectora de alúmina sobre las probetas aleadas que puede incrementar la resistencia a la oxidación.

  8. 3D imaging using X-Ray tomography and SEM combined FIB to study non isothermal creep damage of (111) oriented samples of γ / γ ′ nickel base single crystal superalloy MC2

    KAUST Repository

    Jouiad, Mustapha

    2012-01-01

    An unprecedented investigation consisting of the association of X-Ray tomography and Scanning Electron Microscopy combined with Focus Ion Beam (SEM-FIB) is conducted to perform a 3D reconstruction imaging. These techniques are applied to study the non-isothermal creep behavior of close (111) oriented samples of MC2 nickel base superalloys single crystal. The issue here is to develop a strategy to come out with the 3D rafting of γ\\' particles and its interaction whether with dislocation structures or/and with the preexisting voids. This characterization is uncommonly performed away from the conventional studied orientation [001] in order to feed the viscoplastic modeling leading to its improvement by taking into account the crystal anisotropy. The creep tests were performed at two different conditions: classical isothermal tests at 1050°C under 140 MPa and a non isothermal creep test consisting of one overheating at 1200°C and 30 seconds dwell time during the isothermal creep life. The X-Ray tomography shows a great deformation heterogeneity that is pronounced for the non-isothermal tested samples. This deformation localization seems to be linked to the preexisting voids. Nevertheless, for both tested samples, the voids coalescence is the precursor of the observed damage leading to failure. SEM-FIB investigation by means of slice and view technique gives 3D views of the rafted γ\\' particles and shows that γ corridors evolution seems to be the main creep rate controlling parameter. © 2012 Trans Tech Publications, Switzerland.

  9. Design of high entropy alloys based on the experience from commercial superalloys

    Science.gov (United States)

    Wang, Z.; Huang, Y.; Wang, J.; Liu, C. T.

    2015-01-01

    High entropy alloys (HEAs) have been drawing increasing attention recently and gratifying results have been obtained. However, the existing metallurgic rules of HEAs could not provide specific information of selecting candidate alloys for structural applications. Our brief survey reveals that many commercial superalloys have medium and even to high configurational entropies. The experience of commercial superalloys provides a clue for helping us in the development of HEAs for structural applications.

  10. Creep Crack Initiation and Growth Behavior for Ni-Base Superalloys

    Science.gov (United States)

    Nagumo, Yoshiko; Yokobori, A. Toshimitsu, Jr.; Sugiura, Ryuji; Ozeki, Go; Matsuzaki, Takashi

    The structural components which are used in high temperature gas turbines have various shapes which may cause the notch effect. Moreover, the site of stress concentration might have the heterogeneous microstructural distribution. Therefore, it is necessary to clarify the creep fracture mechanism for these materials in order to predict the life of creep fracture with high degree of accuracy. In this study, the creep crack growth tests were performed using in-situ observational testing machine with microscope to observe the creep damage formation and creep crack growth behavior. The materials used are polycrystalline Ni-base superalloy IN100 and directionally solidified Ni-base superalloy CM247LC which were developed for jet engine turbine blades and gas turbine blades in electric power plants, respectively. The microstructural observation of the test specimens was also conducted using FE-SEM/EBSD. Additionally, the analyses of two-dimensional elastic-plastic creep finite element using designed methods were conducted to understand the effect of microstructural distribution on creep damage formation. The experimental and analytical results showed that it is important to determine the creep crack initiation and early crack growth to predict the life of creep fracture and it is indicated that the highly accurate prediction of creep fracture life could be realized by measuring notch opening displacement proposed as the RNOD characteristic.

  11. Microstructure and mechanical behavior of direct metal laser sintered Inconel alloy 718

    Energy Technology Data Exchange (ETDEWEB)

    Smith, Derek H. [Department of Mechanical Engineering, University of New Hampshire, Durham, NH 03824 (United States); Bicknell, Jonathan; Jorgensen, Luke [Turbocam Energy Solutions, Turbocam International, Dover, NH 03820 (United States); Patterson, Brian M.; Cordes, Nikolaus L. [Materials Science Division, Los Alamos National Laboratory, Los Alamos, NM 87545 (United States); Tsukrov, Igor [Department of Mechanical Engineering, University of New Hampshire, Durham, NH 03824 (United States); Knezevic, Marko, E-mail: marko.knezevic@unh.edu [Department of Mechanical Engineering, University of New Hampshire, Durham, NH 03824 (United States)

    2016-03-15

    In this paper, we investigate microstructure and quasi-static mechanical behavior of the direct metal laser sintered Inconel 718 superalloy as a function of build direction (BD). The printed material was further processed by annealing and double-aging, hot isostatic pressing (HIP), and machining. We characterize porosity fraction and distribution using micro X-ray computed tomography (μXCT), grain structure and crystallographic texture using electron backscattered diffraction (EBSD), and mechanical response in quasi-static tension and compression using standard mechanical testing at room temperature. Analysis of the μXCT imaging shows that majority of porosity develops in the outer layer of the printed material. However, porosity inside the material is also present. The EBSD measurements reveal formation of columnar grains, which favor < 001 > fiber texture components along the BD. These measurements also show evidence of coarse-grained microstructure present in the samples treated by HIP. Finally, analysis of grain boundaries reveal that HIP results in a large number of annealing twins compared to that in samples that underwent annealing and double-aging. The yield strength varies with the testing direction by approximately 7%, which is governed by a combination of grain morphology and crystallographic texture. In particular, we determine tension–compression asymmetry in the yield stress as well as anisotropy of the material flow during compression. We find that HIP lowers yield stress but improves ductility relative to the annealed and aged material. These results are discussed and critically compared with the data reported for wrought material in the same condition. - Highlights: • Microstructure and mechanical properties of DMLS Inconel 718 are studied in function of build direction. • Inhomogeneity of microstructure in the material in several conditions is quantified by μXCT and EBSD. • Anisotropy and asymmetry in the mechanical response are

  12. Microstructure and mechanical behavior of direct metal laser sintered Inconel alloy 718

    International Nuclear Information System (INIS)

    Smith, Derek H.; Bicknell, Jonathan; Jorgensen, Luke; Patterson, Brian M.; Cordes, Nikolaus L.; Tsukrov, Igor; Knezevic, Marko

    2016-01-01

    In this paper, we investigate microstructure and quasi-static mechanical behavior of the direct metal laser sintered Inconel 718 superalloy as a function of build direction (BD). The printed material was further processed by annealing and double-aging, hot isostatic pressing (HIP), and machining. We characterize porosity fraction and distribution using micro X-ray computed tomography (μXCT), grain structure and crystallographic texture using electron backscattered diffraction (EBSD), and mechanical response in quasi-static tension and compression using standard mechanical testing at room temperature. Analysis of the μXCT imaging shows that majority of porosity develops in the outer layer of the printed material. However, porosity inside the material is also present. The EBSD measurements reveal formation of columnar grains, which favor fiber texture components along the BD. These measurements also show evidence of coarse-grained microstructure present in the samples treated by HIP. Finally, analysis of grain boundaries reveal that HIP results in a large number of annealing twins compared to that in samples that underwent annealing and double-aging. The yield strength varies with the testing direction by approximately 7%, which is governed by a combination of grain morphology and crystallographic texture. In particular, we determine tension–compression asymmetry in the yield stress as well as anisotropy of the material flow during compression. We find that HIP lowers yield stress but improves ductility relative to the annealed and aged material. These results are discussed and critically compared with the data reported for wrought material in the same condition. - Highlights: • Microstructure and mechanical properties of DMLS Inconel 718 are studied in function of build direction. • Inhomogeneity of microstructure in the material in several conditions is quantified by μXCT and EBSD. • Anisotropy and asymmetry in the mechanical response are determined by

  13. Magnetic susceptibility of Inconel alloys 718, 625, and 600 at cryogenic temperatures

    Science.gov (United States)

    Goldberg, Ira B.; Mitchell, Michael R.; Murphy, Allan R.; Goldfarb, Ronald B.; Loughran, Robert J.

    1990-01-01

    After a hydrogen fuel bleed valve problem on the Discovery Space Shuttle was traced to the strong magnetization of Inconel 718 in the armature of the linear variable differential transformer near liquid hydrogen temperatures, the ac magnetic susceptibility of three samples of Inconel 718 of slightly different compositions, one sample of Inconel 625, and on sample of Inconel 600 were measured as a function of temperature. Inconel 718 alloys are found to exhibit a spin glass state below 16 K. Inconel 600 exhibits three different magnetic phases, the lowest-temperature state (below 6 K) being somewhat similar to that of Inconel 718. The magnetic states of the Inconel alloys and their magnetic susceptibilities appear to be strongly dependent on the exact composition of the alloy.

  14. Noburnium: Systems design of niobium superalloys

    Science.gov (United States)

    Misra, Abhijeet

    2005-11-01

    A systems-based approach, integrating quantum mechanical calculations with efficient experimentation, was employed to design niobium-based superalloys. The microstructural concept of gamma-gamma' nickel-based superalloys was adopted, where, the coherent gamma ' aluminides act both as the strengthening phase and a source of aluminum for Al2O3 passivation. Building on previous research, the selected bcc-type ordered aluminide was L2 1 structured Pd2HfAl phase. Comprehensive phase relations were measured on Nb-Pd-Hf-Al prototype alloys, and key tie-tetrahedra were identified. Aluminide precipitation in a bcc matrix was demonstrated in designed Nb+Pd2HfAl alloys. Thermodynamic databases were developed by integrating first-principles calculations with measured phase relations. Atomic volume models were developed for the bcc matrix and the Pd2HfAl phase and matrix elements which would reduce lattice misfit were identified. An experimental 2-phase alloy demonstrated a misfit of 3%. A modified Wagner's model was used to predict the required transient properties to form external Al2O3. The principal oxidation design goal was to decrease the oxygen permeability ( NSOx DO ) divided by the aluminum diffusivity (DAl) by 5 orders of magnitude. A multicomponent mobility database was developed to predict the diffusivities. Guided by first-principles calculations the effect of alloying elements on the oxygen diffusivity in Nb was measured, and the mobility database was experimentally validated. Based on the mobility database, it was found that increasing Al solubility in the bcc matrix greatly increased Al diffusivity. Alloying elements were identified that would increase Al solubility in the bcc matrix. Prototype alloys were prepared and the best oxidation performance was exhibited by a bcc+Nb2Al Nb-Hf-Al alloy, which exhibited parabolic oxidation behavior at 1300°C. The alloy was shown to have achieved the required 5 orders of magnitude reduction in the design parameter. The

  15. Superalloy Lattice Block Developed for Use in Lightweight, High-Temperature Structures

    Science.gov (United States)

    Hebsur, Mohan G.; Whittenberger, J. Daniel; Krause, David L.

    2003-01-01

    Successful development of advanced gas turbine engines for aircraft will require lightweight, high-temperature components. Currently titanium-aluminum- (TiAl) based alloys are envisioned for such applications because of their lower density (4 g/cm3) in comparison to superalloys (8.5 g/cm3), which have been utilized for hot turbine engine parts for over 50 years. However, a recently developed concept (lattice block) by JAMCORP, Inc., of Willmington, Massachusetts, would allow lightweight, high-temperature structures to be directly fabricated from superalloys and, thus, take advantage of their well-known, characterized properties. In its simplest state, lattice block is composed of thin ligaments arranged in a three dimensional triangulated trusslike configuration that forms a structurally rigid panel. Because lattice block can be fabricated by casting, correctly sized hardware is produced with little or no machining; thus very low cost manufacturing is possible. Together, the NASA Glenn Research Center and JAMCORP have extended their lattice block methodology for lower melting materials, such as Al alloys, to demonstrate that investment casting of superalloy lattice block is possible. This effort required advances in lattice block pattern design and assembly, higher temperature mold materials and mold fabrication technology, and foundry practice suitable for superalloys (ref. 1). Lattice block panels have been cast from two different Ni-base superalloys: IN 718, which is the most commonly utilized superalloy and retains its strength up to 650 C; and MAR M247, which possesses excellent mechanical properties to at least 1100 C. In addition to the open-cell lattice block geometry, same-sized lattice block panels containing a thin (1-mm-thick) solid face on one side have also been cast from both superalloys. The elevated-temperature mechanical properties of the open cell and face-sheeted superalloy lattice block panels are currently being examined, and the

  16. The role of particle ripening on the creep acceleration of Nimonic 263 superalloy

    Directory of Open Access Journals (Sweden)

    Angella Giuliano

    2014-01-01

    Full Text Available Physically based constitutive equations need to incorporate the most relevant microstructural features of materials to adequately describe their mechanical behaviour. To accurately model the creep behaviour of precipitation hardened alloys, the value and the evolution of strengthening particle size are important parameters to be taken into account. In the present work, creep tests have been run on virgin and overaged (up to 3500 h at 800 ∘C Nimonic 263, a polycrystalline nickel base superalloy used for combustion chambers of gas turbines. The experimental results suggest that the reinforcing particle evolution is not the main reason for the creep acceleration that seems to be better described by a strain correlated damage, such as the accumulation of mobile dislocations or the grain boundary cavitation. The coarsened microstructure, obtained by overageing the alloy at high temperature before creep testing, mainly influences the initial stage of the creep, resulting in a higher minimum creep rate and a corresponding reduction of the creep resistance.

  17. Compatibility of aluminide-coated Hastelloy x and Inconel 617 in a simulated gas-cooled reactor environment

    International Nuclear Information System (INIS)

    Chin, J.; Johnson, W.R.; Chen, K.

    1982-03-01

    Commercially prepared aluminide coatings on Hastelloy X and Inconel 617 substrates were exposed to controlled-impurity helium at 850 0 and 950 0 C for 3000 h. Optical and scanning electron (SEM) microscopy, electron microprobe profiles, and SEM X-ray mapping were used to evaluate and compare exposed and unexposed control samples. Four coatings were evaluated: aluminide, aluminide with platinum, aluminide with chromium, and aluminide with rhodium. With extended time at elevated temperature, nickel diffused into the aluminide coatings to form epsilon-phase (Ni 3 Al). This diffusion was the primary cause of porosity formation at the aluminide/alloy interface

  18. Barrier Coatings for Refractory Metals and Superalloys

    Energy Technology Data Exchange (ETDEWEB)

    SM Sabol; BT Randall; JD Edington; CJ Larkin; BJ Close

    2006-02-23

    In the closed working fluid loop of the proposed Prometheus space nuclear power plant (SNPP), there is the potential for reaction of core and plant structural materials with gas phase impurities and gas phase transport of interstitial elements between superalloy and refractory metal alloy components during service. Primary concerns are surface oxidation, interstitial embrittlement of refractory metals and decarburization of superalloys. In parallel with kinetic investigations, this letter evaluates the ability of potential coatings to prevent or impede communication between reactor and plant components. Key coating requirements are identified and current technology coating materials are reviewed relative to these requirements. Candidate coatings are identified for future evaluation based on current knowledge of design parameters and anticipated environment. Coatings were identified for superalloys and refractory metals to provide diffusion barriers to interstitial transport and act as reactive barriers to potential oxidation. Due to their high stability at low oxygen potential, alumina formers are most promising for oxidation protection given the anticipated coolant gas chemistry. A sublayer of iridium is recommended to provide inherent diffusion resistance to interstitials. Based on specific base metal selection, a thin film substrate--coating interdiffusion barrier layer may be necessary to meet mission life.

  19. Barrier Coatings for Refractory Metals and Superalloys

    International Nuclear Information System (INIS)

    SM Sabol; BT Randall; JD Edington; CJ Larkin; BJ Close

    2006-01-01

    In the closed working fluid loop of the proposed Prometheus space nuclear power plant (SNPP), there is the potential for reaction of core and plant structural materials with gas phase impurities and gas phase transport of interstitial elements between superalloy and refractory metal alloy components during service. Primary concerns are surface oxidation, interstitial embrittlement of refractory metals and decarburization of superalloys. In parallel with kinetic investigations, this letter evaluates the ability of potential coatings to prevent or impede communication between reactor and plant components. Key coating requirements are identified and current technology coating materials are reviewed relative to these requirements. Candidate coatings are identified for future evaluation based on current knowledge of design parameters and anticipated environment. Coatings were identified for superalloys and refractory metals to provide diffusion barriers to interstitial transport and act as reactive barriers to potential oxidation. Due to their high stability at low oxygen potential, alumina formers are most promising for oxidation protection given the anticipated coolant gas chemistry. A sublayer of iridium is recommended to provide inherent diffusion resistance to interstitials. Based on specific base metal selection, a thin film substrate--coating interdiffusion barrier layer may be necessary to meet mission life

  20. Microstructural evolution during transient liquid phase bonding of Inconel 617 using Ni-Si-B filler metal

    Energy Technology Data Exchange (ETDEWEB)

    Jalilian, F. [McGill University, Department of Mining, Metals and Materials Engineering, 3610 University St., M.H. Wong Building, Montreal Que., H3A 2B2 (Canada); Jahazi, M. [Aerospace Manufacturing Technology Center, National Research Council of Canada (Canada); Drew, R.A.L. [McGill University, Department of Mining, Metals and Materials Engineering, 3610 University St., M.H. Wong Building, Montreal Que., H3A 2B2 (Canada)]. E-mail: robin.drew@mcgill.ca

    2006-05-15

    The influence of process parameters on microstructural characteristics of transient liquid phase (TLP) bonded Inconel 617 alloy was investigated. Experiments were carried out at 1065 deg. C using nickel based filler metal (Ni-4.5% Si-3% B) with B as the melting point depressant (MPD) element. Two different thickness of interlayer and various holding times were employed. The influence of these processing parameters on the characteristics of the joint area particularly size, morphology and composition of precipitates was investigated. The presence of MoB, Mo{sub 2}B, M{sub 23}C{sub 6}, TiC, M{sub 23}(B, C){sub 6} and Ni{sub 3}B precipitates in the diffusion layer and Ni{sub 3}B, Ni{sub 3}Si and Ni{sub 5}Si{sub 2} precipitates in the interlayer at the interface between the base metal and interlayer were demonstrated using electron back scattered diffraction (EBSD), energy dispersive spectrometry (EDS) and TEM.

  1. Influence of γ' precipitates on Portevin–Le Chatelier effect of Ni-based superalloys

    Energy Technology Data Exchange (ETDEWEB)

    Cai, Yulong [Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China); CAS Key Laboratory of Mechanical Behavior and Design of Materials, University of Science and Technology of China, Hefei 230027 (China); Tian, Chenggang [Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China); Fu, Shihua, E-mail: fushihua@ustc.edu.cn [CAS Key Laboratory of Mechanical Behavior and Design of Materials, University of Science and Technology of China, Hefei 230027 (China); Han, Guoming [Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China); Cui, Chuanyong, E-mail: chycui@imr.ac.cn [Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 (China); Zhang, Qingchuan, E-mail: zhangqc@ustc.edu.cn [CAS Key Laboratory of Mechanical Behavior and Design of Materials, University of Science and Technology of China, Hefei 230027 (China)

    2015-06-25

    The γ′ precipitate plays a critical role in improving the mechanical properties of Ni-based superalloys. An undesirable phenomenon referred to as the Portevin–Le Chatelier (PLC) effect always appears in Ni-based superalloys deformed within specific ranges of strain rate and temperature. In order to systematically investigate the influence of the γ′ precipitates on the PLC effect, four Ni-based superalloys with various γ′ contents were designed and fabricated. Microscopic observations from transmission electron microscopy (TEM) indicated that the volume fraction of the γ′ phase was consistent with the designed value. Furthermore, analysis of energy dispersive spectroscopy (EDS) results revealed that the γ matrix of all the alloys consisted of the same components. Uniaxial tensile tests were performed at strain rates and temperatures ranging from 1×10{sup −4} to 3×10{sup −3} s{sup −1} and 300–500 °C, respectively. We found that the ultimate strength increased while the elongation decreased with increasing γ′ content. In addition, the serration changed from type A to type B and to type C with increasing temperature, decreasing strain rate or increasing γ′ content; the amplitude of type B serrations was described by unimodal or bimodal distributions. Increasing volume fraction of γ′ precipitates shifted the region in which the PLC effect occurred, to the range of low temperatures and high strain rates. Moreover, the serration amplitude increased with increasing γ′ content at a given temperature, which indicated that the γ′ precipitate increases the dynamic strain ageing (DSA) effect.

  2. Mechanical Behaviour of Inconel 718 Thin-Walled Laser Welded Components for Aircraft Engines

    Directory of Open Access Journals (Sweden)

    Enrico Lertora

    2014-01-01

    Full Text Available Nickel alloys are very important in many aerospace applications, especially to manufacture gas turbines and aero engine components, where high strength and temperature resistance are necessary. These kinds of alloys have to be welded with high energy density processes, in order to preserve their high mechanical properties. In this work, CO2 laser overlap joints between Inconel 718 sheets of limited thickness in the absence of postweld heat treatment were made. The main application of this kind of joint is the manufacturing of a helicopter engine component. In particular the aim was to obtain a specific cross section geometry, necessary to overcome the mechanical stresses found in these working conditions without failure. Static and dynamic tests were performed to assess the welds and the parent material fatigue life behaviour. Furthermore, the life trend was identified. This research pointed out that a full joint shape control is possible by choosing proper welding parameters and that the laser beam process allows the maintenance of high tensile strength and ductility of Inconel 718 but caused many liquation microcracks in the heat affected zone (HAZ. In spite of these microcracks, the fatigue behaviour of the overlap welds complies with the technical specifications required by the application.

  3. Precipitation and clustering in the early stages of ageing in Inconel 718

    Energy Technology Data Exchange (ETDEWEB)

    Alam, Talukder, E-mail: talukder.alam@sydney.edu.au [Australian Centre for Microscopy and Microanalysis, University of Sydney, NSW 2006 (Australia); Chaturvedi, Mahesh [Department of Mechanical and Industrial Engineering, University of Manitoba, Winnipeg, MB R3T 5V6 (Canada); Ringer, Simon P.; Cairney, Julie M. [Australian Centre for Microscopy and Microanalysis, University of Sydney, NSW 2006 (Australia)

    2010-11-15

    Research highlights: {yields} IN718 could be age hardened rapidly by secondary phase formation. {yields} Co-located phases were observed in the earliest stage of detection. {yields} Clustering of Ti/Al and Nb atoms was observed prior to precipitation. - Abstract: In this report we investigate the onset and evolution of precipitation in the early stages of ageing in the alloy WE 91, a variant of the Ni-Fe-Cr superalloy Inconel 718 (IN718). Transmission electron microscopy and atom probe tomography were used to study the size and volume fraction of {gamma}' and {gamma}'' precipitates and the extent of pre-precipitate clustering of Al/Ti and Nb. Co-located {gamma}' and {gamma}'' precipitates were observed from the shortest ageing times that precipitates could be visualised using atom probe. At shorter times, prior to the observation of precipitates, clustering of Al/Ti and Nb was shown to occur. The respective volume fraction of the {gamma}' and {gamma}'' precipitates and the clustering of Al/Ti and Nb suggest that {gamma}'' nucleates prior to {gamma}' during ageing at 706 deg. C for this alloy.

  4. Microstructural evolutions and mechanical behaviour of the nickel based alloys 617 and 230 at high temperature

    International Nuclear Information System (INIS)

    Chomette, S.

    2009-11-01

    High Temperature Reactors (HTR), is one of the innovative nuclear reactor designed to be inherently safer than previous generation and to produce minimal waste. The most critical metallic component in that type of reactor is the Intermediate Heat exchanger (IHX). The constraints imposed by the conception and the severe operational conditions (high temperature of 850 C to 950 C, lifetime of 20,000 h) have guided the IHX material selection toward two solid solution nickel base alloys, the Inconel 617 and the Haynes 230. Inconel 617 is the primary candidate alloy thanks to its good high temperature mechanical and corrosion properties and the large data base developed in previous programs. However, its high cobalt content has to be considered as an issue (nuclear activation). The more recent alloy Haynes 230, in which most of the cobalt has been replaced by tungsten, present characteristics similar to the 617 alloy. The objective of this thesis is to study the high temperature mechanical behaviour of both alloys in relation with their microstructural evolutions. The as received microstructural observations have revealed primary carbides (M 6 C). Most of this precipitates are evenly distributed in the materials. Few M 23 C 6 secondary carbides are observed in both alloys in the as received state. Thermal ageing treatments at 850 C lead to an important M 23 C 6 precipitation on slip lines and at grain boundaries. The size of this carbides increases and their number decreases with increasing ageing duration. The intragranular precipitation of secondary carbides at 950 C is more limited and the intergranular evolution more important than at 850 C. The microstructural observations and the hardness evolution of both alloys show that the main microstructural evolutions occur before 1,000 h at both studied temperatures. The mechanical properties of the Inconel 617 and the Haynes 230 have been studied using tensile, creep, fatigue and relaxation-fatigue tests. Particularly, the

  5. LCF- and LCF/HCF-behaviour of the superalloy MAR-M247LC

    Energy Technology Data Exchange (ETDEWEB)

    Gelmedin, Domnin; Lang, Karl-Heinz [Karlsruhe Institute of Technology (KIT), Karlsruhe (Germany). Inst. fuer Werkstoffkunde I

    2010-07-01

    The fatigue behaviour of the Nickel-base superalloy Mar-M247LC was investigated at 650 C in air environment under total strain control. Pure low cycle fatigue (LCF) loading, pure high cycle fatigue (HCF) loading and superimposed LCF/HCF loading were realised. In LCF tests with a strain ratio of zero and a hold time of 60 seconds the cyclic deformation and the lifetime behaviour was investigated. The dependence of the fatigue limit on the mean strain was estimated in HCF tests at a frequency of 60 Hz using an ultimate number of cycles of ten million. Finally the influence of superimposed HCF and LCF loadings was examined. At high total strain ranges of the HCF loading the lifetime of the superalloy as reduced about more than one magnitude compared to the lifetime under pure LCF loading. With decreasing HCF loadings the reduction of the lifetime decreases. This life time reduction can be explained by the interaction of the LCF and the superimposed HCF loading. Crack initiation and first crack propagation is predominantly induced by the LCF loading. After reaching an adequate long fatigue crack length the superimposed HCF loading contributes considerably to the crack growth. This contribution can be determined evaluating the distance between the LCF marking lines which form on the fracture surface. The higher the superimposed HCF loading was the longer the distance between the LCF marking lines and the lower the crack length were when first LCF marking lines could be recognized. On the basis of this cognition the life time under superimposed LCF/HCF loading was modelled using a model basing on fracture mechanics. (orig.)

  6. Effect of Build Angle on Surface Properties of Nickel Superalloys Processed by Selective Laser Melting

    Science.gov (United States)

    Covarrubias, Ernesto E.; Eshraghi, Mohsen

    2018-03-01

    Aerospace, automotive, and medical industries use selective laser melting (SLM) to produce complex parts through solidifying successive layers of powder. This additive manufacturing technique has many advantages, but one of the biggest challenges facing this process is the resulting surface quality of the as-built parts. The purpose of this research was to study the surface properties of Inconel 718 alloys fabricated by SLM. The effect of build angle on the surface properties of as-built parts was investigated. Two sets of sample geometries including cube and rectangular artifacts were considered in the study. It was found that, for angles between 15° and 75°, theoretical calculations based on the "stair-step" effect were consistent with the experimental results. Downskin surfaces showed higher average roughness values compared to the upskin surfaces. No significant difference was found between the average roughness values measured from cube and rectangular test artifacts.

  7. Evaluation of powder metallurgy superalloy disk materials

    Science.gov (United States)

    Evans, D. J.

    1975-01-01

    A program was conducted to develop nickel-base superalloy disk material using prealloyed powder metallurgy techniques. The program included fabrication of test specimens and subscale turbine disks from four different prealloyed powders (NASA-TRW-VIA, AF2-1DA, Mar-M-432 and MERL 80). Based on evaluation of these specimens and disks, two alloys (AF2-1DA and Mar-M-432) were selected for scale-up evaluation. Using fabricating experience gained in the subscale turbine disk effort, test specimens and full scale turbine disks were formed from the selected alloys. These specimens and disks were then subjected to a rigorous test program to evaluate their physical properties and determine their suitability for use in advanced performance turbine engines. A major objective of the program was to develop processes which would yield alloy properties that would be repeatable in producing jet engine disks from the same powder metallurgy alloys. The feasibility of manufacturing full scale gas turbine engine disks by thermomechanical processing of pre-alloyed metal powders was demonstrated. AF2-1DA was shown to possess tensile and creep-rupture properties in excess of those of Astroloy, one of the highest temperature capability disk alloys now in production. It was determined that metallographic evaluation after post-HIP elevated temperature exposure should be used to verify the effectiveness of consolidation of hot isostatically pressed billets.

  8. Cutting Zone Temperature Identification During Machining of Nickel Alloy Inconel 718

    Science.gov (United States)

    Czán, Andrej; Daniš, Igor; Holubják, Jozef; Zaušková, Lucia; Czánová, Tatiana; Mikloš, Matej; Martikáň, Pavol

    2017-12-01

    Quality of machined surface is affected by quality of cutting process. There are many parameters, which influence on the quality of the cutting process. The cutting temperature is one of most important parameters that influence the tool life and the quality of machined surfaces. Its identification and determination is key objective in specialized machining processes such as dry machining of hard-to-machine materials. It is well known that maximum temperature is obtained in the tool rake face at the vicinity of the cutting edge. A moderate level of cutting edge temperature and a low thermal shock reduce the tool wear phenomena, and a low temperature gradient in the machined sublayer reduces the risk of high tensile residual stresses. The thermocouple method was used to measure the temperature directly in the cutting zone. An original thermocouple was specially developed for measuring of temperature in the cutting zone, surface and subsurface layers of machined surface. This paper deals with identification of temperature and temperature gradient during dry peripheral milling of Inconel 718. The measurements were used to identification the temperature gradients and to reconstruct the thermal distribution in cutting zone with various cutting conditions.

  9. Effect of Process Variables on the Inertia Friction Welding of Superalloys LSHR and Mar-M247

    Science.gov (United States)

    Mahaffey, D. W.; Senkov, O. N.; Shivpuri, R.; Semiatin, S. L.

    2016-08-01

    The effect of inertia friction welding process parameters on microstructure evolution, weld plane quality, and the tensile behavior of welds between dissimilar nickel-base superalloys was established. For this purpose, the fine-grain, powder metallurgy alloy LSHR was joined to coarse-grain cast Mar-M247 using a fixed level of initial kinetic energy, but different combinations of the flywheel moment of inertia and initial rotation speed. It was found that welds made with the largest moment of inertia resulted in a sound bond with the best microstructure and room-temperature tensile strength equal to or greater than that of the parent materials. A relationship between the moment of inertia and weld process efficiency was established. The post-weld tensile behavior was interpreted in the context of observed microstructure gradients and weld-line defects.

  10. Investigations of the microstructural stability of wrought Ni-(Fe)-based syperalloys for steam turbine rotor application beyond 700 C; Untersuchungen der Strukturstabilitaet von Ni-(Fe)-Basislegierungen fuer Rotorwellen in Dampfturbinen mit Arbeitstemperaturen ueber 700 C

    Energy Technology Data Exchange (ETDEWEB)

    Seliga, T.

    2005-07-01

    There is a continuous trend to improve the efficiency of modern power plants with steam turbine require operating steam temperature from 700 to 720 C. For substantial parts like turbine rotors and discs this means incr