WorldWideScience

Sample records for maximum time-averaged corrosion

  1. An implementation of the maximum-caliber principle by replica-averaged time-resolved restrained simulations.

    Science.gov (United States)

    Capelli, Riccardo; Tiana, Guido; Camilloni, Carlo

    2018-05-14

    Inferential methods can be used to integrate experimental informations and molecular simulations. The maximum entropy principle provides a framework for using equilibrium experimental data, and it has been shown that replica-averaged simulations, restrained using a static potential, are a practical and powerful implementation of such a principle. Here we show that replica-averaged simulations restrained using a time-dependent potential are equivalent to the principle of maximum caliber, the dynamic version of the principle of maximum entropy, and thus may allow us to integrate time-resolved data in molecular dynamics simulations. We provide an analytical proof of the equivalence as well as a computational validation making use of simple models and synthetic data. Some limitations and possible solutions are also discussed.

  2. Study on Corrosion-induced Crack Initiation and Propagation of Sustaining Loaded RCbeams

    Science.gov (United States)

    Zhong, X. P.; Li, Y.; Yuan, C. B.; Yang, Z.; Chen, Y.

    2018-05-01

    For 13 pieces of reinforced concrete beams with HRB500 steel bars under long-term sustained loads, at time of corrosion-induced initial crack of concrete, and corrosion-induced crack widths of 0.3mm and 1mm, corrosion of steel bars and time-varying behavior of corrosion-induced crack width were studied by the ECWD (Electro-osmosis - constant Current – Wet and Dry cycles) accelerated corrosion method. The results show that when cover thickness was between 30 and 50mm,corrosion rates of steel bars were between 0.8% and 1.7% at time of corrosion-induced crack, and decreased with increasing concrete cover thickness; when corrosion-induced crack width was 0.3mm, the corrosion rate decreased with increasing steel bar diameter, and increased with increasing cover thickness; its corrosion rate varied between 0.98% and 4.54%; when corrosion-induced crack width reached 1mm, corrosion rate of steel bars was between 4% and 4.5%; when corrosion rate of steel bars was within 5%, the maximum and average corrosion-induced crack and corrosion rate of steel bars had a good linear relationship. The calculation model predicting the maximum and average width of corrosion-induced crack is given in this paper.

  3. Prediction of reinforcement corrosion using corrosion induced cracks width in corroded reinforced concrete beams

    International Nuclear Information System (INIS)

    Khan, Inamullah; François, Raoul; Castel, Arnaud

    2014-01-01

    This paper studies the evolution of reinforcement corrosion in comparison to corrosion crack width in a highly corroded reinforced concrete beam. Cracking and corrosion maps of the beam were drawn and steel reinforcement was recovered from the beam to observe the corrosion pattern and to measure the loss of mass of steel reinforcement. Maximum steel cross-section loss of the main reinforcement and average steel cross-section loss between stirrups were plotted against the crack width. The experimental results were compared with existing models proposed by Rodriguez et al., Vidal et al. and Zhang et al. Time prediction models for a given opening threshold are also compared to experimental results. Steel cross-section loss for stirrups was also measured and was plotted against the crack width. It was observed that steel cross-section loss in the stirrups had no relationship with the crack width of longitudinal corrosion cracks. -- Highlights: •Relationship between crack and corrosion of reinforcement was investigated. •Corrosion results of natural process and then corresponds to in-situ conditions. •Comparison with time predicting model is provided. •Prediction of load-bearing capacity from crack pattern was studied

  4. The effects of disjunct sampling and averaging time on maximum mean wind speeds

    DEFF Research Database (Denmark)

    Larsén, Xiaoli Guo; Mann, J.

    2006-01-01

    Conventionally, the 50-year wind is calculated on basis of the annual maxima of consecutive 10-min averages. Very often, however, the averages are saved with a temporal spacing of several hours. We call it disjunct sampling. It may also happen that the wind speeds are averaged over a longer time...

  5. A generic statistical methodology to predict the maximum pit depth of a localized corrosion process

    International Nuclear Information System (INIS)

    Jarrah, A.; Bigerelle, M.; Guillemot, G.; Najjar, D.; Iost, A.; Nianga, J.-M.

    2011-01-01

    Highlights: → We propose a methodology to predict the maximum pit depth in a corrosion process. → Generalized Lambda Distribution and the Computer Based Bootstrap Method are combined. → GLD fit a large variety of distributions both in their central and tail regions. → Minimum thickness preventing perforation can be estimated with a safety margin. → Considering its applications, this new approach can help to size industrial pieces. - Abstract: This paper outlines a new methodology to predict accurately the maximum pit depth related to a localized corrosion process. It combines two statistical methods: the Generalized Lambda Distribution (GLD), to determine a model of distribution fitting with the experimental frequency distribution of depths, and the Computer Based Bootstrap Method (CBBM), to generate simulated distributions equivalent to the experimental one. In comparison with conventionally established statistical methods that are restricted to the use of inferred distributions constrained by specific mathematical assumptions, the major advantage of the methodology presented in this paper is that both the GLD and the CBBM enable a statistical treatment of the experimental data without making any preconceived choice neither on the unknown theoretical parent underlying distribution of pit depth which characterizes the global corrosion phenomenon nor on the unknown associated theoretical extreme value distribution which characterizes the deepest pits. Considering an experimental distribution of depths of pits produced on an aluminium sample, estimations of maximum pit depth using a GLD model are compared to similar estimations based on usual Gumbel and Generalized Extreme Value (GEV) methods proposed in the corrosion engineering literature. The GLD approach is shown having smaller bias and dispersion in the estimation of the maximum pit depth than the Gumbel approach both for its realization and mean. This leads to comparing the GLD approach to the GEV one

  6. Stochastic modelling of the monthly average maximum and minimum temperature patterns in India 1981-2015

    Science.gov (United States)

    Narasimha Murthy, K. V.; Saravana, R.; Vijaya Kumar, K.

    2018-04-01

    The paper investigates the stochastic modelling and forecasting of monthly average maximum and minimum temperature patterns through suitable seasonal auto regressive integrated moving average (SARIMA) model for the period 1981-2015 in India. The variations and distributions of monthly maximum and minimum temperatures are analyzed through Box plots and cumulative distribution functions. The time series plot indicates that the maximum temperature series contain sharp peaks in almost all the years, while it is not true for the minimum temperature series, so both the series are modelled separately. The possible SARIMA model has been chosen based on observing autocorrelation function (ACF), partial autocorrelation function (PACF), and inverse autocorrelation function (IACF) of the logarithmic transformed temperature series. The SARIMA (1, 0, 0) × (0, 1, 1)12 model is selected for monthly average maximum and minimum temperature series based on minimum Bayesian information criteria. The model parameters are obtained using maximum-likelihood method with the help of standard error of residuals. The adequacy of the selected model is determined using correlation diagnostic checking through ACF, PACF, IACF, and p values of Ljung-Box test statistic of residuals and using normal diagnostic checking through the kernel and normal density curves of histogram and Q-Q plot. Finally, the forecasting of monthly maximum and minimum temperature patterns of India for the next 3 years has been noticed with the help of selected model.

  7. Maximum time-dependent space-charge limited diode currents

    Energy Technology Data Exchange (ETDEWEB)

    Griswold, M. E. [Tri Alpha Energy, Inc., Rancho Santa Margarita, California 92688 (United States); Fisch, N. J. [Princeton Plasma Physics Laboratory, Princeton University, Princeton, New Jersey 08543 (United States)

    2016-01-15

    Recent papers claim that a one dimensional (1D) diode with a time-varying voltage drop can transmit current densities that exceed the Child-Langmuir (CL) limit on average, apparently contradicting a previous conjecture that there is a hard limit on the average current density across any 1D diode, as t → ∞, that is equal to the CL limit. However, these claims rest on a different definition of the CL limit, namely, a comparison between the time-averaged diode current and the adiabatic average of the expression for the stationary CL limit. If the current were considered as a function of the maximum applied voltage, rather than the average applied voltage, then the original conjecture would not have been refuted.

  8. Contribution of archaeological analogs to the estimation of average corrosion rates and long term corrosion mechanisms of low carbon steel in soil

    International Nuclear Information System (INIS)

    Neff, D.

    2003-11-01

    . This corrosion form, constituted among others by a siderite layer is due to a particular environment: waterlogged soil containing wood. In the whole, analyses conducted in the TM show that it is composed of goethite badly crystallized in comparison with those of the DPL. Moreover, in this zone, the average elemental iron amount decreases progressively from the metal to the soil in which it stabilizes. In order to know the behaviour of the identified phases in soil water, some thermodynamic data have been involved to calculate their solubility in function of pH, potential and various water composition. The first conclusion concerns the influence of the composition and the structure of the material which is not important for the corrosion behaviour. From the results, some hypothesis have been formulated on the long term corrosion mechanisms of hypo-eutectoids steels in the considered environment. The role of the cracks formed in the DPL during the burial was evidenced. Moreover, these corrosion products undertake a dissolution in the soil water and a reprecipitation, explaining the progressive decrease of the iron amount in the TM. Lastly, some average corrosion rates have been measured with the help of the analytical and thermodynamic results: they do not exceed 4 μm/year. (author)

  9. Accurate computations of monthly average daily extraterrestrial irradiation and the maximum possible sunshine duration

    International Nuclear Information System (INIS)

    Jain, P.C.

    1985-12-01

    The monthly average daily values of the extraterrestrial irradiation on a horizontal plane and the maximum possible sunshine duration are two important parameters that are frequently needed in various solar energy applications. These are generally calculated by solar scientists and engineers each time they are needed and often by using the approximate short-cut methods. Using the accurate analytical expressions developed by Spencer for the declination and the eccentricity correction factor, computations for these parameters have been made for all the latitude values from 90 deg. N to 90 deg. S at intervals of 1 deg. and are presented in a convenient tabular form. Monthly average daily values of the maximum possible sunshine duration as recorded on a Campbell Stoke's sunshine recorder are also computed and presented. These tables would avoid the need for repetitive and approximate calculations and serve as a useful ready reference for providing accurate values to the solar energy scientists and engineers

  10. Real-time monitoring of copper corrosion at the Aespoe HRL

    Energy Technology Data Exchange (ETDEWEB)

    Rosborg, Bo; Pan, Jinshan [Div. Corrosion Science, Royal Institute of Technology, Drottning Kristinas vaeg 51, SE - 100 44 Stockholm (Sweden); Eden, David [InterCorr International, Inc., 14503 Bammel-N Houston, Suite 300, Houston, TX 77014 (United States); Karnland, Ola [Clay Technology AB, Ideon Research Center, SE - 223 70 Lund (Sweden); Werme, Lars [Svensk Kaernbraenslehantering AB, P.O. Box 5864, SE - 102 40 Stockholm (Sweden)

    2004-07-01

    In Sweden the principal strategy for high-level radioactive waste disposal is to enclose the spent nuclear fuel in tightly sealed copper canisters that are embedded in bentonite clay about 500 m down in the Swedish bed-rock. Initially, a limited amount of air will be left in a repository after emplacement. The entrapped oxygen will be consumed through reactions with minerals in the rock and the bentonite and also through microbial activity. After the oxygen has been consumed in the repository, after a few hundred years at the very most, corrosion will be controlled completely by the supply of dissolved sulphide to the canister. The present work concerns the oxic period after emplacement. The main hypothesis is that the average corrosion rate of the canister under oxic conditions will be less than 7 {mu}m/year, and that pitting will only be possible under these conditions. The Aespoe Hard Rock Laboratory offers a realistic environment for different experiments and tests under the conditions that will prevail in a deep repository. Real-time monitoring of copper corrosion is presently performed with polarization resistance, harmonic distortion analysis and electrochemical noise techniques. The first two techniques are used to derive information regarding the general corrosion rate and the third to derive information regarding localized corrosion. In order to support these measurements at Aespoe, laboratory work is also performed at the Royal Institute of Technology in Stockholm using the very same corrosion monitoring equipment and also other equipment and techniques. Copper coupons are also exposed at Aespoe. Results from the work at Aespoe and in Stockholm are presented with an emphasis on the gained information concerning localized corrosion. The recorded corrosion rates at Aespoe are well below the value given above, and the recorded localization factors are interpreted as indicating only a slight tendency to local attack. (authors)

  11. Real-time monitoring of copper corrosion at the Aespoe HRL

    International Nuclear Information System (INIS)

    Rosborg, Bo; Pan, Jinshan; Eden, David; Karnland, Ola; Werme, Lars

    2004-01-01

    In Sweden the principal strategy for high-level radioactive waste disposal is to enclose the spent nuclear fuel in tightly sealed copper canisters that are embedded in bentonite clay about 500 m down in the Swedish bed-rock. Initially, a limited amount of air will be left in a repository after emplacement. The entrapped oxygen will be consumed through reactions with minerals in the rock and the bentonite and also through microbial activity. After the oxygen has been consumed in the repository, after a few hundred years at the very most, corrosion will be controlled completely by the supply of dissolved sulphide to the canister. The present work concerns the oxic period after emplacement. The main hypothesis is that the average corrosion rate of the canister under oxic conditions will be less than 7 μm/year, and that pitting will only be possible under these conditions. The Aespoe Hard Rock Laboratory offers a realistic environment for different experiments and tests under the conditions that will prevail in a deep repository. Real-time monitoring of copper corrosion is presently performed with polarization resistance, harmonic distortion analysis and electrochemical noise techniques. The first two techniques are used to derive information regarding the general corrosion rate and the third to derive information regarding localized corrosion. In order to support these measurements at Aespoe, laboratory work is also performed at the Royal Institute of Technology in Stockholm using the very same corrosion monitoring equipment and also other equipment and techniques. Copper coupons are also exposed at Aespoe. Results from the work at Aespoe and in Stockholm are presented with an emphasis on the gained information concerning localized corrosion. The recorded corrosion rates at Aespoe are well below the value given above, and the recorded localization factors are interpreted as indicating only a slight tendency to local attack. (authors)

  12. Real time corrosion monitoring in atmosphere using automated battery driven corrosion loggers

    DEFF Research Database (Denmark)

    Prosek, T.; Kouril, M.; Hilbert, Lisbeth Rischel

    2008-01-01

    diminishes due to corrosion. Zinc, iron, copper and nickel sensors at several thicknesses are available. Sensitivity of the corrosion measurement varies from 1 to 10 nm depending on the type and thickness of the sensor. Changes in the air corrosivity can be thus detected within hours or even tens of minutes......A logger enabling continuous measurement of corrosion rate of selected metals in indoor and outdoor atmospheres has been developed. Principle of the measurement method is based on the increasing electrical resistance of a measuring element made of the material concerned as its cross-sectional area....... The logger lifetime in medium corrosive environments is designed to be 2 years with full autonomy. Data on the sensor corrosion rate are available any time through GPRS connection or by a non-contact inductive reading without the need of retracting the logger from the exposure site....

  13. Corrosion of copper and copper alloys in a basaltic repository environment

    International Nuclear Information System (INIS)

    Brehm, W.F.

    1990-01-01

    Corrosion testing done on copper and copper alloys in support of the basalt repository program is discussed. Tests were performed under anoxic conditions at 50C, 100C, 150C and 200C in the presence of a saturated basalt-bentonite packing. Tests were also performed in an air/steam mixture at temperatures between 150C and 200C. Some tests, particularly those in air/steam mixtures, were done in the presence of radiation fields of 10 2 , 10 3 or 10 4 rad/h. Exposure periods were up to 28 months. A synthetic groundwater, Grande Ronde ≠4, was used. The materials studied were ASTM B402μm·a for copper and 17 μm·a for cupronickel, but the average rates were muμm·a was obtained. The rates at longer times were less than a third of this value. Corrosion increased monotonically with time and temperature. Chalcocite (Cu 2 S) was the corrosion product at 200C. There was no detectable radiation effect, and no pitting was observed. In air/steam corrosion was uniform with no pitting. Linear corrosion was observed for pure copper. The maximum corrosion penetration after 25 months was 0.13 mm at 300C; cupronickel corroded more slowly, with a maximum penetration of 0.045mm after 25 months. Cuprite (Cu 2 O) and tenorite (CuO) were identified on cupronickel, but only Cu 2 O on copper. A pronounced radiation effect was seen at 250C, but not at 150C; the surface film morphology was different under irradiation. In the short term the presence of packing increased the corrosion rate. 5 refs

  14. Corrosion of Nickel-Titanium Orthodontic Archwires in Saliva and Oral Probiotic Supplements

    Directory of Open Access Journals (Sweden)

    Gianluca Turco

    2017-01-01

    Full Text Available Objectives: The aim of the study was to examine how probiotic supplements affect the corrosion stability of orthodontic archwires made of nickel-titanium alloy (NiTi. Materials and Methods: Ni-Ti archwires (0.508x0.508 and having the length of 2.5 cm were tested. The archwires (composition Ni=50.4%, Ti=49.6% were uncoated, nitrified and rhodium coated. Surface microgeometry was observed by using scanning electron microscope and surface roughness was measured by profilometer through these variables: roughness average, maximum height and maximum roughness depth. Corrosion was examined by electrochemical method of cyclic polarisation. Results: Rhodium coated alloy in saliva has significantly higher general corrosion in saliva than nitrified alloy and uncoated alloy, with large effect size (p=0.027; η2=0.700. In the presence of probiotics, the result was even more pronounced (p<0.001; η2=0.936. Probiotic supplement increases general and localised corrosion of rhodium coated archwire and slightly decreases general corrosion and increases localised corrosion in uncoated archwire , while in the case of nitrified archwire the probability of corrosion is very low. The differences in surface roughness between NiTi wires before corrosion are not significant. Exposure to saliva decreases roughness average in rhodium coated wire (p=0.015; η2=0.501. Media do not significantly influence surface microgeometry in nitrified and uncoated wires. Conclusion: Probiotic supplement affects corrosion depending on the type of coating of the NiTi archwire. It increases general corrosion of rhodium coated wire and causes localised corrosion of uncoated and rhodium coated archwire. Probiotic supplement does not have greater influence on surface roughness compared to that of saliva.

  15. Analytical model for time to cover cracking in RC structures due to rebar corrosion

    International Nuclear Information System (INIS)

    Bhargava, Kapilesh; Ghosh, A.K.; Mori, Yasuhiro; Ramanujam, S.

    2006-01-01

    The structural degradation of concrete structures due to reinforcement corrosion is a major worldwide problem. Reinforcement corrosion causes a volume increase due to the oxidation of metallic iron, which is mainly responsible for exerting the expansive radial pressure at the steel-concrete interface and development of hoop tensile stresses in the surrounding concrete. Cracking occurs, once the maximum hoop tensile stress exceeds the tensile strength of the concrete. The cracking begins at the steel-concrete interface and propagates outwards and eventually results in the thorough cracking of the cover concrete and this would indicate the loss of service life for the corrosion affected structures. An analytical model is proposed to predict the time required for cover cracking and the weight loss of reinforcing bar in corrosion affected reinforced concrete structures. The modelling aspects of the residual strength of cracked concrete and the stiffness contribution from the combination of reinforcement and expansive corrosion products have also been incorporated in the model. The problem is modeled as a boundary value problem and the governing equations are expressed in terms of the radial displacement. The analytical solutions are presented considering a simple two-zone model for the cover concrete, viz. cracked or uncracked. Reasonable estimation of the various parameters in the model related to the composition and properties of expansive corrosion products based on the available published experimental data has also been discussed. The performance of the proposed corrosion cracking model is then investigated through its ability to reproduce available experimental trends. Reasonably good agreement between experimental results and the analytical predictions has been obtained. It has also been found that tensile strength and initial tangent modulus of cover concrete, annual mean corrosion rate and modulus of elasticity of reinforcement plus corrosion products combined

  16. Effect of Sonification Time on Synthesisi and Corrosion Resistance of Epoxy-Clay Nanocomposite

    Directory of Open Access Journals (Sweden)

    Niloufar Bahrami Panah

    2016-09-01

    Full Text Available In recent years many research works have been carried out on anti-corrosive nanocomposites coatings containing mineral reinforcements. The most important criteria in these attempts are polymerization method and the type of matrix and reinforcement of nanocomposites. In this regard, the physical and mechanical properties of the polymers in which a small amount of filler is used can be improved. In this research, an epoxy-clay nanocomposite was synthesized by in-situ polymerization method using a resin matrix based on bisphenol-A type epoxy and montmorillonite clay (Closite 15A. The treatment was used at different ultrasonic stirring times to disperse 1-4 weight percentages of clay particles into the matrix. The structure of synthesized epoxy-clay nanocomposite was studied by scanning electron microscopy and X-ray diffraction techniques. The average size of clay particles was determined by X-ray diffraction measurement. Then, anti-corrosion properties of epoxy-clay coatings, prepared under different ultrasonic durations and applied on carbon steel panels, were investigated by Tafel and electrochemical impedance spectroscopy techniques. For this purpose, the carbon steel panels coated with these coatings were immersed in 3.5% sodium chloride solution and tested at different immersion times. The results indicated that a nanocomposite containing 1% clay, synthesized, stirred 60 min ultrasonically, produced smaller particle size, lower corrosion current density and higher coating corrosion resistance than the other composite formulations. This nanocomposite provided superior protection against corrosion in sodium chloride solution.

  17. A non-destructive test method to monitor corrosion products and corrosion-induced cracking in reinforced cement based materials

    DEFF Research Database (Denmark)

    Michel, Alexander; Pease, Bradley Justin; Peterova, Adela

    2011-01-01

    ) was conducted to describe the impact of water-to-cement ratio and corrosion current density (i.e., corrosion rate) on the reinforcement corrosion process. Focus was placed, in particular on the determination of the corrosion accommodating region (CAR) and time to corrosion-induced cracking. Experimental results...... showed that x-ray attenuation measurements allow determination of the actual concentrations of corrosion products averaged through the specimen thickness. The total mass loss of steel measured by x-ray attenuation was found to be in very good agreement with the calculated mass loss obtained by Faraday......’s law. Furthermore, experimental results demonstrated that the depth of penetration of corrosion products as well as time to corrosion-induced cracking is varying for the different water-to-cement ratios and applied corrosion current densities....

  18. Maximum: Recent Implementation and Application to the Study of Corrosion-Induced Microstructures in Thin Films of Aluminum-Copper Metallization.

    Science.gov (United States)

    Liang, Shoudeng

    We describe the recent implementation of a synchrotron radiation based scanning soft X-ray photoemission microscope - MAXIMUM, and discuss its application to the investigation of corrosion-induced microstructures in Al-Cu-Si thin films. The microscope employs a Mo/Si multilayer-coated Schwarzschild objective to focus 95eV X-rays from an undulator beamline. The photoelectrons are energy-analyzed by a CMA, and the sample is rastered to produce an image. We have achieved 980A spatial and 250meV energy resolution. Recent addition of a sample preparation and transfer system to the microscope enables us to perform surface and materials studies under UHV conditions. Since the spatial resolution of the microscope is determined by the spot size of the focused X-rays, any electrostatic potential from surface charging will not affect the image quality. This allowed the study of highly insulating films with the use of an electron flood gun to compensate for spectral shifts. We have employed MAXIMUM to investigate corrosion -induced surface microstructures in the Al-Cu-Si thin films commonly utilized in VLSI metallization. Spectromicroscopy was performed to characterize the chemical species and their distribution on the film surface after corrosion under 85% relative humidity at 85^circ C. The experimental images demonstrated that Cu -rich precipitates were formed near the surface region beneath the oxide layer upon annealing. We also observed a correlation between the precipitates and the increased corrosion in the alloy film: the localized corrosion occurs only at those sites where precipitation has taken place. This implies that the surface oxide layer is modified by the underlying Cu-rich phase such that it loses protection against moisture. After pitting, the Cu-rich phase acts as a cathode to facilitate corrosion of the surrounding Cu-deficient Al matrix via galvanic action. The corrosion -induced microstructures show characteristic circular features in the micrographs of

  19. Corrosion behavior of carbon steel exposed for long time to an inoculation medium of sulfate-reducing bacteria; Ryusan`en kangenkin ga seisokusuru baichi ni chokikan shinshinshita tansoko no fushoku kyodo

    Energy Technology Data Exchange (ETDEWEB)

    Baba, F.; Suzuki, T. [Ajinomoto Co. Inc., Kawasaki (Japan). Technology and Engineering Lab.; Seo, M. [Hokkaido Univ., Sapporo (Japan). Graduate School of Engineering

    1996-10-15

    In this paper, carbon steel was exposed more than six weeks to an inoculation medium of the sulfate-reducing bacteria in which the Fe{sup 2+} concentration was adjusted to a fixed value, the corrosion behavior of carbon steel was investigated by measuring the weight change and surface analysis using EPMA. As a result, the conclusions were obtained as follows: in the case of the medium with high Fe{sup 2+} concentration, the corrosion rate reached a maximum. In this case, the corrosion rate was suppressed to be low during the exposure for up to three weeks, and was increased above four weeks. The corrosion rate became 0.06 mm year{sup -1} by extrapolating the weight loss during the exposure up to six weeks. This value was higher than the average corrosion rate of carbon steel in a neutral solution with deaeration. It was shown from the analysis results using the EPMA that the FeS scale area covered on the surface of carbon steel would act as a cathode, and the other area would act as an anode. The formation of a scale effectively acting as a cathode depended on the exposure time and the formation of FeS in the medium. 15 refs., 10 figs., 1 tab.

  20. Table for monthly average daily extraterrestrial irradiation on horizontal surface and the maximum possible sunshine duration

    International Nuclear Information System (INIS)

    Jain, P.C.

    1984-01-01

    The monthly average daily values of the extraterrestrial irradiation on a horizontal surface (H 0 ) and the maximum possible sunshine duration are two important parameters that are frequently needed in various solar energy applications. These are generally calculated by scientists each time they are needed and by using the approximate short-cut methods. Computations for these values have been made once and for all for latitude values of 60 deg. N to 60 deg. S at intervals of 1 deg. and are presented in a convenient tabular form. Values of the maximum possible sunshine duration as recorded on a Campbell Stoke's sunshine recorder are also computed and presented. These tables should avoid the need for repetition and approximate calculations and serve as a useful ready reference for solar energy scientists and engineers. (author)

  1. Maximum stress estimation model for multi-span waler beams with deflections at the supports using average strains.

    Science.gov (United States)

    Park, Sung Woo; Oh, Byung Kwan; Park, Hyo Seon

    2015-03-30

    The safety of a multi-span waler beam subjected simultaneously to a distributed load and deflections at its supports can be secured by limiting the maximum stress of the beam to a specific value to prevent the beam from reaching a limit state for failure or collapse. Despite the fact that the vast majority of accidents on construction sites occur at waler beams in retaining wall systems, no safety monitoring model that can consider deflections at the supports of the beam is available. In this paper, a maximum stress estimation model for a waler beam based on average strains measured from vibrating wire strain gauges (VWSGs), the most frequently used sensors in construction field, is presented. The model is derived by defining the relationship between the maximum stress and the average strains measured from VWSGs. In addition to the maximum stress, support reactions, deflections at supports, and the magnitudes of distributed loads for the beam structure can be identified by the estimation model using the average strains. Using simulation tests on two multi-span beams, the performance of the model is evaluated by estimating maximum stress, deflections at supports, support reactions, and the magnitudes of distributed loads.

  2. Stochastic modeling of pitting corrosion: A new model for initiation and growth of multiple corrosion pits

    International Nuclear Information System (INIS)

    Valor, A.; Caleyo, F.; Alfonso, L.; Rivas, D.; Hallen, J.M.

    2007-01-01

    In this work, a new stochastic model capable of simulating pitting corrosion is developed and validated. Pitting corrosion is modeled as the combination of two stochastic processes: pit initiation and pit growth. Pit generation is modeled as a nonhomogeneous Poisson process, in which induction time for pit initiation is simulated as the realization of a Weibull process. In this way, the exponential and Weibull distributions can be considered as the possible distributions for pit initiation time. Pit growth is simulated using a nonhomogeneous Markov process. Extreme value statistics is used to find the distribution of maximum pit depths resulting from the combination of the initiation and growth processes for multiple pits. The proposed model is validated using several published experiments on pitting corrosion. It is capable of reproducing the experimental observations with higher quality than the stochastic models available in the literature for pitting corrosion

  3. Stochastic modeling of pitting corrosion: A new model for initiation and growth of multiple corrosion pits

    Energy Technology Data Exchange (ETDEWEB)

    Valor, A. [Facultad de Fisica, Universidad de La Habana, San Lazaro y L, Vedado, 10400 Havana (Cuba); Caleyo, F. [Departamento de Ingenieria, Metalurgica, IPN-ESIQIE, UPALM Edif. 7, Zacatenco, Mexico DF 07738 (Mexico)]. E-mail: fcaleyo@gmail.com; Alfonso, L. [Departamento de Ingenieria, Metalurgica, IPN-ESIQIE, UPALM Edif. 7, Zacatenco, Mexico DF 07738 (Mexico); Rivas, D. [Departamento de Ingenieria, Metalurgica, IPN-ESIQIE, UPALM Edif. 7, Zacatenco, Mexico DF 07738 (Mexico); Hallen, J.M. [Departamento de Ingenieria, Metalurgica, IPN-ESIQIE, UPALM Edif. 7, Zacatenco, Mexico DF 07738 (Mexico)

    2007-02-15

    In this work, a new stochastic model capable of simulating pitting corrosion is developed and validated. Pitting corrosion is modeled as the combination of two stochastic processes: pit initiation and pit growth. Pit generation is modeled as a nonhomogeneous Poisson process, in which induction time for pit initiation is simulated as the realization of a Weibull process. In this way, the exponential and Weibull distributions can be considered as the possible distributions for pit initiation time. Pit growth is simulated using a nonhomogeneous Markov process. Extreme value statistics is used to find the distribution of maximum pit depths resulting from the combination of the initiation and growth processes for multiple pits. The proposed model is validated using several published experiments on pitting corrosion. It is capable of reproducing the experimental observations with higher quality than the stochastic models available in the literature for pitting corrosion.

  4. Probabilistic models for steel corrosion loss and pitting of marine infrastructure

    International Nuclear Information System (INIS)

    Melchers, R.E.; Jeffrey, R.J.

    2008-01-01

    With the increasing emphasis on attempting to retain in service ageing infrastructure models for the description and prediction of corrosion losses and for maximum pit depth are of increasing interest. In most cases assessment and prediction will be done in a probabilistic risk assessment framework and this then requires probabilistic corrosion models. Recently, novel models for corrosion loss and maximum pit depth under marine immersion conditions have been developed. The models show that both corrosion loss and pit depth progress in a non-linear fashion with increased exposure time and do so in a non-monotonic manner as a result of the controlling corrosion process changing from oxidation to being influenced by bacterial action. For engineers the importance of this lies in the fact that conventional 'corrosion rates' have no validity, particularly for the long-term corrosion effects as relevant to deteriorated infrastructure. The models are consistent with corrosion science principles as well as current understanding of the considerable influence of bacterial processes on corrosion loss and pitting. The considerable practical implications of this are described

  5. Maximum Stress Estimation Model for Multi-Span Waler Beams with Deflections at the Supports Using Average Strains

    Directory of Open Access Journals (Sweden)

    Sung Woo Park

    2015-03-01

    Full Text Available The safety of a multi-span waler beam subjected simultaneously to a distributed load and deflections at its supports can be secured by limiting the maximum stress of the beam to a specific value to prevent the beam from reaching a limit state for failure or collapse. Despite the fact that the vast majority of accidents on construction sites occur at waler beams in retaining wall systems, no safety monitoring model that can consider deflections at the supports of the beam is available. In this paper, a maximum stress estimation model for a waler beam based on average strains measured from vibrating wire strain gauges (VWSGs, the most frequently used sensors in construction field, is presented. The model is derived by defining the relationship between the maximum stress and the average strains measured from VWSGs. In addition to the maximum stress, support reactions, deflections at supports, and the magnitudes of distributed loads for the beam structure can be identified by the estimation model using the average strains. Using simulation tests on two multi-span beams, the performance of the model is evaluated by estimating maximum stress, deflections at supports, support reactions, and the magnitudes of distributed loads.

  6. Real Time Corrosion Monitoring in Lead and Lead-Bismuth Systems

    Energy Technology Data Exchange (ETDEWEB)

    James F. Stubbins; Alan Bolind; Ziang Chen

    2010-02-25

    The objective of this research program is to develop a real-time, in situ corrosion monitoring technique for flowing liquid Pb and eutectic PbBi (LBE) systems in a temperature range of 400 to 650 C. These conditions are relevant to future liquid metal cooled fast reactor operating parameters. THis program was aligned with the Gen IV Reactor initiative to develp technologies to support the design and opertion of a Pb or LBE-cooled fast reactor. The ability to monitor corrosion for protection of structural components is a high priority issue for the safe and prolonged operation of advanced liquid metal fast reactor systems. In those systems, protective oxide layers are intentionally formed and maintained to limit corrosion rates during operation. This program developed a real time, in situ corrosion monitoring tecnique using impedance spectroscopy (IS) technology.

  7. Monitoring corrosion and corrosion control of iron in HCl by non-ionic surfactants of the TRITON-X series - Part III. Immersion time effects and theoretical studies

    International Nuclear Information System (INIS)

    Amin, Mohammed A.; Ahmed, M.A.; Arida, H.A.; Kandemirli, Fatma; Saracoglu, Murat; Arslan, Taner; Basaran, Murat A.

    2011-01-01

    Graphical abstract: . Display Omitted Research highlights: → The inhibition effect of TX-100, TX-165 and TX-305 on iron corrosion in 1.0 M HCl was studied. → TX-305 inhibited iron corrosion more effectively than TX-100 and TX-165. → In most cases, inhibition efficiency increased with time during the first 60 min of immersion, then decreased. → Calculated quantum chemical parameters confirmed the experimental inhibition efficiencies of the tested surfactants. - Abstract: The inhibition performance of three selected non-ionic surfactants of the TRITON-X series, namely TRITONX-100 (TX-100), TRITON-X-165 (TX-165) and TRITON-X-305 (TX-305), on the corrosion of iron was studied in 1.0 M HCl solutions as a function of inhibitor concentration (0.01-0.20 g L -1 ) and immersion time (0.0-8 h) at 298 K. Measurements were conducted based on Tafel polarization, LPR and impedance studies. At high frequencies, the impedance spectrum showed a depressed capacitive loop in the complex impedance plane, whose diameter is a function of the immersion time and the type and concentration of the introduced surfactant. In all cases, an inductive loop was observed in the low frequency and this could be attributed to the adsorption behavior. The inhibition efficiency increased with immersion time, reached a maximum and then decreased. This was attributed to the orientation change of adsorbed surfactant molecules. TX-305 inhibited iron corrosion more effectively than TX-100 and TX-165. The frontier orbital energies, the energy gap between frontier orbitals, dipole moments (μ), charges on the C and O atoms, the polarizabilities, and the quantum chemical descriptors were calculated. The quantum chemical calculation results inferred that for the HOMO representing the condensed Fukui function for an electrophilic attack (f k + ), the contributions belong to the phenyl group and the oxygen atom attached to the phenyl group for each tested surfactant. Quantitative structure

  8. Corrosion and electrochemical properties of lanthanum

    International Nuclear Information System (INIS)

    Tomashov, N.D.; Matveeva, T.V.

    The kinetics of the corrosion rate of lanthanum at 25 0 in air of different relative humidities, distilled water, sulfuric acid, hydrochloric acid, nitric acid, phosphoric acid, hydrofluoric acid, potassium hydroxide of different concentrations and at 100 0 C in distilled water and potassium hydroxide have been studied. In air at 22--100% relative humidity, the corrosion rate of lanthanum increases with time and with increasing humidity. In distilled water and in potassium hydroxide solutions, the corrosion rate of lanthanum increases with time and decreasees when the concentration of alkali exceeds 20%. With increasing concentration of the acids, the corrosion rate of lanthanum increases in hydrochloric acid and nitric acid and passes through a maximum in sulfuric acid (20%) and phosphoric acid (60%). The values of the corrosion rates of lanthanum in 40% nitric acid, 35% hydrochloric acid, 20% sulfuric acid, 60% phosphoric acid, and 40% hydrofluoric acid are 8 x 10 5 ; 4.4 x 10 4 ; 1.3 x 10 3 ; 9 g/m 2 h respectively

  9. Experimental and Empirical Time to Corrosion of Reinforced Concrete Structures under Different Curing Conditions

    Directory of Open Access Journals (Sweden)

    Ahmed A. Abouhussien

    2014-01-01

    Full Text Available Reinforced concrete structures, especially those in marine environments, are commonly subjected to high concentrations of chlorides, which eventually leads to corrosion of the embedded reinforcing steel. The total time to corrosion of such structures may be divided into three stages: corrosion initiation, cracking, and damage periods. This paper evaluates, both empirically and experimentally, the expected time to corrosion of reinforced concrete structures. The tested reinforced concrete samples were subjected to ten alternative curing techniques, including hot, cold, and normal temperatures, prior to testing. The corrosion initiation, cracking, and damage periods in this investigation were experimentally monitored by an accelerated corrosion test performed on reinforced concrete samples. Alternatively, the corrosion initiation time for counterpart samples was empirically predicted using Fick’s second law of diffusion for comparison. The results showed that the corrosion initiation periods obtained experimentally were comparable to those obtained empirically. The corrosion initiation was found to occur at the first jump of the current measurement in the accelerated corrosion test which matched the half-cell potential reading of around −350 mV.

  10. The Effect of Impingement Velocity and Angle Variation on the Erosion Corrosion Performance of API 5L-X65 Carbon Steel in a Flow Loop

    Directory of Open Access Journals (Sweden)

    Ihsan UlHaq Toor

    2018-05-01

    Full Text Available Erosion corrosion performance of API 5L-X65 carbon steel was investigated at three different impingement velocities (3, 6 & 12 m/s, five different angles (15, 30, 45, 60, & 90°, and with/without solid particles (average particle size of 314 µm. The experiments were conducted in 0.2 M NaCl solution at room temperature for a duration of 24 h and the results showed that the maximum erosion corrosion rate was observed at 45° irrespective of the velocity. The highest erosion corrosion rate at 45° was due to the balance between the shear and normal impact stress at this angle. Ploughing, deep craters, and micro-forging/plastic deformation were found to be the main erosion corrosion mechanisms. The maximum wear scar depth measured using optical profilometery was found to be 51 µm (average at an impingement angle of 45°.

  11. Long Term Corrosion/Degradation Test Six Year Results

    Energy Technology Data Exchange (ETDEWEB)

    M. K. Adler Flitton; C. W. Bishop; M. E. Delwiche; T. S. Yoder

    2004-09-01

    The Subsurface Disposal Area (SDA) of the Radioactive Waste Management Complex (RWMC) located at the Idaho National Engineering and Environmental Laboratory (INEEL) contains neutron-activated metals from non-fuel, nuclear reactor core components. The Long-Term Corrosion/Degradation (LTCD) Test is designed to obtain site-specific corrosion rates to support efforts to more accurately estimate the transfer of activated elements to the environment. The test is using two proven, industry-standard methods—direct corrosion testing using metal coupons, and monitored corrosion testing using electrical/resistance probes—to determine corrosion rates for various metal alloys generally representing the metals of interest buried at the SDA, including Type 304L stainless steel, Type 316L stainless steel, Inconel 718, Beryllium S200F, Aluminum 6061, Zircaloy-4, low-carbon steel, and Ferralium 255. In the direct testing, metal coupons are retrieved for corrosion evaluation after having been buried in SDA backfill soil and exposed to natural SDA environmental conditions for times ranging from one year to as many as 32 years, depending on research needs and funding availability. In the monitored testing, electrical/resistance probes buried in SDA backfill soil will provide corrosion data for the duration of the test or until the probes fail. This report provides an update describing the current status of the test and documents results to date. Data from the one-year and three-year results are also included, for comparison and evaluation of trends. In the six-year results, most metals being tested showed extremely low measurable rates of general corrosion. For Type 304L stainless steel, Type 316L stainless steel, Inconel 718, and Ferralium 255, corrosion rates fell in the range of “no reportable” to 0.0002 mils per year (MPY). Corrosion rates for Zircaloy-4 ranged from no measurable corrosion to 0.0001 MPY. These rates are two orders of magnitude lower than those specified in

  12. Effect of ageing time and temperature on corrosion behaviour of aluminum alloy 2014

    Science.gov (United States)

    Gadpale, Vikas; Banjare, Pragya N.; Manoj, Manoranjan Kumar

    2018-03-01

    In this paper, the effect of corrosion behaviour of aluminium alloy 2014 were studied by potentiodynamic polarization in 1 mole of NaCl solution of aged sample. The experimental testing results concluded that, corrosion resistance of Aluminum alloy 2014 degraded with the increasing the temperature (150°C & 200°C) and time of ageing. Corroded surface of the aged specimens was tested under optical microscopes for microstructures for phase analysis. Optical micrographs of corroded surfaces showed general corrosion and pitting corrosion. The corrosion resistance of lower ageing temperature and lower ageing time is higher because of its fine distribution of precipitates in matrix phase.

  13. Corrosion resistance of biomimetic calcium phosphate coatings on magnesium due to varying pretreatment time

    Energy Technology Data Exchange (ETDEWEB)

    Waterman, J., E-mail: jay.waterman@pg.canterbury.ac.nz [Department of Mechanical Engineering, University of Canterbury, Christchurch (New Zealand); Pietak, A. [Department of Anatomy and Structural Biology, University of Otago, Dunedin (New Zealand); Birbilis, N. [Department of Materials Engineering, Monash University (Australia); Woodfield, T. [Department of Mechanical Engineering, University of Canterbury, Christchurch (New Zealand); Department of Orthopaedic Surgery, University of Otago, Christchurch (New Zealand); Dias, G. [Department of Anatomy and Structural Biology, University of Otago, Dunedin (New Zealand); Staiger, M.P., E-mail: mark.staiger@canterbury.ac.nz [Department of Mechanical Engineering, University of Canterbury, Christchurch (New Zealand)

    2011-12-15

    Calcium phosphate coatings were prepared on magnesium substrates via a biomimetic coating process. The effects of a magnesium hydroxide pretreatment on the formation and the ultimate corrosion protection of the coatings were studied. The pretreatment layer was found to affect the amount of defects present in the coatings. Corrosion resistance of the coatings was studied in vitro using two simulated body fluids, 0.8% NaCl and Hanks solution. In NaCl, the resistance to corrosion of all samples decreases with time as corrosion proceeded through cracks and other defects in the coatings. Samples with no pretreatment displayed the highest corrosion resistance as these samples had the fewest defects in the coating. However, in Hanks solution, corrosion resistance increased with time due to additional nucleation of calcium phosphate from the fluid on to the substrate. In this solution, additional pretreatment time was beneficial to the overall corrosion resistance.

  14. Determination of pollution for the effect of sea salt aerosols corrosion

    International Nuclear Information System (INIS)

    Nakayasu, Fumio; Umehara, Toshihiro; Mizutani, Masatoshi; Matsukawa, Kiyokazu

    2007-01-01

    All of 15 nuclear power plants in Fukui Prefecture are located in the Japan Sea Coast. Corrosion is strongly influenced by material and environmental factors. We installed the salt damage experimental yard at Awara sea coast in March, 2006. We are doing the open air test, sheltered test without filter and with filter. The corrosivity of carbon steel of winter was higher than it of summer at Awara facility. The measurement of chloride deposition rate was done by the dry gauze method. The correlation between chloride deposition rate and the average velocity of the wind was found. The correlation between chloride deposition rate and the average rainfall was a little complicate. It means the chloride deposition rate has maximum value at a certain rainfall amount. No other clear relation was found. (author)

  15. Flow-induced corrosion of absorbable magnesium alloy: In-situ and real-time electrochemical study

    International Nuclear Information System (INIS)

    Wang, Juan; Jang, Yongseok; Wan, Guojiang; Giridharan, Venkataraman; Song, Guang-Ling; Xu, Zhigang; Koo, Youngmi; Qi, Pengkai; Sankar, Jagannathan; Huang, Nan; Yun, Yeoheung

    2016-01-01

    Highlights: • An in-situ and real-time electrochemical monitoring of flow-induced corrosion of Mg alloy is designed in a vascular bioreactor. • Effect of hydrodynamics on corrosion kinetics, types, rates and products is analyzed. • Flow accelerates mass and electron transfer, leading to an increase in uniform and localized corrosions. • Flow increases not only the thickness of uniform corrosion product layer, but the removal rate of localized corrosion products. • Electrochemical impedance spectroscopy and linear polarization-measured polarization resistances provide a consistent correlation to corrosion rate calculated by computed tomography. - Abstract: An in-situ and real-time electrochemical study in a vascular bioreactor was designed to analyze corrosion mechanism of magnesium alloy (MgZnCa) under mimetic hydrodynamic conditions. Effect of hydrodynamics on corrosion kinetics, types, rates and products was analyzed. Flow-induced shear stress (FISS) accelerated mass and electron transfer, leading to an increase in uniform and localized corrosions. FISS increased the thickness of uniform corrosion layer, but filiform corrosion decreased this layer resistance at high FISS conditions. FISS also increased the removal rate of localized corrosion products. Impedance-estimated and linear polarization-measured polarization resistances provided a consistent correlation to corrosion rate calculated by computed tomography.

  16. Estimating the lifetimes of titanium containers for nuclear fuel waste: A damage function for the crevice corrosion of grade-2 titanium

    International Nuclear Information System (INIS)

    Shoesmith, D.W.; Ikeda, B.M.; Quinn, M.J.; Kolar, M.

    1995-06-01

    The assumptions upon which the lifetime failure model used in the postclosure assessment is based are reevaluated. In particular, the conservations involved in assuming that crevice initiation would occur, and that sufficient oxygen would be present to maintain crevice propagation to failure, are discussed. Unless the period required to saturate the environment around the container can be specified with some certainty, it remains necessary to assume corrosion would initiate rapidly on all containers. A modified version of the container lifetime model has been developed which avoids the need to use averaged temperature profiles. In this model, these profiles are converted to propagation rate profiles using an experimental activation energy and then numerically integrated to predict container failure times. A damage function is developed relating the maximum depth of penetration by crevice corrosion to either the time since emplacement in the vault or the total amount of oxygen consumed. This function is used to estimate the maximum penetration depth expected if all the oxygen available in a borehole is consumed in crevice corrosion and to determine the impact on container lifetimes of various repassivation criteria. The factors likely to cause repassivation are summarized, and a number of engineering approaches to extending container lifetimes suggested. (author). 22 refs., 1 tab., 17 figs

  17. Time averaging, ageing and delay analysis of financial time series

    Science.gov (United States)

    Cherstvy, Andrey G.; Vinod, Deepak; Aghion, Erez; Chechkin, Aleksei V.; Metzler, Ralf

    2017-06-01

    We introduce three strategies for the analysis of financial time series based on time averaged observables. These comprise the time averaged mean squared displacement (MSD) as well as the ageing and delay time methods for varying fractions of the financial time series. We explore these concepts via statistical analysis of historic time series for several Dow Jones Industrial indices for the period from the 1960s to 2015. Remarkably, we discover a simple universal law for the delay time averaged MSD. The observed features of the financial time series dynamics agree well with our analytical results for the time averaged measurables for geometric Brownian motion, underlying the famed Black-Scholes-Merton model. The concepts we promote here are shown to be useful for financial data analysis and enable one to unveil new universal features of stock market dynamics.

  18. A discussion for stabilization time of carbon steel in atmospheric corrosion

    Science.gov (United States)

    Zhang, Zong-kai; Ma, Xiao-bing; Cai, Yi-kun

    2017-09-01

    Stabilization time is an important parameter in long-term prediction of carbon steel corrosion in atmosphere. The range of the stabilization time of carbon steel in atmospheric corrosion has been published in many scientific literatures. However, the results may not precise because engineering experiences is dominant. This paper deals with the recalculation of stabilization time based on ISO CORRAG program, and analyzes the results and makes a comparison to the data mentioned above. In addition, a new thinking to obtain stabilization time will be proposed.

  19. Effect of aging on the general corrosion and stress corrosion cracking of uranium--6 wt % niobium alloy

    International Nuclear Information System (INIS)

    Koger, J.W.; Ammons, A.M.; Ferguson, J.E.

    1975-11-01

    Mechanical properties of the uranium-6 wt percent niobium alloy change with aging time and temperature. In general, the ultimate tensile strength and hardness reach a peak, while elongation becomes a minimum at aging temperatures between 400 and 500 0 C. The first optical evidence of a second phase was in the 400 0 C-aged alloy, while complete transformation to a two-phase structure was seen in the 600 0 C-aged alloy. The maximum-strength conditions correlate with the minimum stress corrosion cracking (SCC) resistance. The maximum SCC resistance is found in the as-quenched and 150, 200, and 600 0 C-aged specimens. The as-quenched and 300 0 C-aged specimens had the greatest resistance to general corrosion in aqueous chloride solutions; the 600 0 C-aged specimen had the least resistance

  20. Some observations on phosphate based corrosion inhibitors in preventing carbon steel corrosion

    International Nuclear Information System (INIS)

    Anupkumar, B.; Satpathy, K.K.

    2000-01-01

    Among the various types of phosphonic acid based inhibitors assayed, namely HEDP, ATMP and a commercial corrosion inhibitor (code named Betz), it was found that Betz has the maximum amount of organic phosphate followed by HEDP and ATMP. The corrosion rate studies show that Betz gives the highest inhibition efficiency followed by HEDP and ATMP. This shows that organic phosphate plays a significant role in corrosion protection. However, it was observed that due to synergestic effect, HEDP in the presence of Zn 2+ gave a better corrosion protection than Betz. The results are discussed in the light of available literature. (author)

  1. Statistical analysis of electrochemical noise records at aluminium corrosion; Analisis estadistico de los registros de ruido electroquimico obtenidos en la corrosion del aluminio

    Energy Technology Data Exchange (ETDEWEB)

    Sanchez, A.; Sanjurjo, M.; Bouzada, F.; Urrejola, S.

    2005-07-01

    Given that the experimental signals obtained in an electrochemical noise measurement, ENM, are recorded over a discrete time period, the most direct way of analysing them will be in the time domain resorting to starting to statistical methods. These can be classified into two groups according to use; those which attempt to quantify the degree of the corrosion process (standard deviations, statistical power); and those which attempt to provide information on the corrosion mechanism (based on the assumption that the shape of the time records is a reflection of itself). Among the later the use of the average, the skewness and the kurtosis of the signals or the pitting index can be pointed out as being able to reflect the changes in the corrosion mechanism. Noise resistance stands out above all these parameters. In this work has undertaken the statistical treatment of ENM data obtained by subjecting aluminium to three electrolytes that provoke several types of corrosion in it: passivity, pitting corrosion and generalized corrosion. (Author) 22 refs.

  2. Flow-induced corrosion of absorbable magnesium alloy: In-situ and real-time electrochemical study.

    Science.gov (United States)

    Wang, Juan; Jang, Yongseok; Wan, Guojiang; Giridharan, Venkataraman; Song, Guang-Ling; Xu, Zhigang; Koo, Youngmi; Qi, Pengkai; Sankar, Jagannathan; Huang, Nan; Yun, Yeoheung

    2016-03-01

    An in-situ and real-time electrochemical study in a vascular bioreactor was designed to analyze corrosion mechanism of magnesium alloy (MgZnCa) under mimetic hydrodynamic conditions. Effect of hydrodynamics on corrosion kinetics, types, rates and products was analyzed. Flow-induced shear stress (FISS) accelerated mass and electron transfer, leading to an increase in uniform and localized corrosions. FISS increased the thickness of uniform corrosion layer, but filiform corrosion decreased this layer resistance at high FISS conditions. FISS also increased the removal rate of localized corrosion products. Impedance-estimated and linear polarization-measured polarization resistances provided a consistent correlation to corrosion rate calculated by computed tomography.

  3. Flow-induced corrosion of absorbable magnesium alloy: In-situ and real-time electrochemical study

    Science.gov (United States)

    Wang, Juan; Jang, Yongseok; Wan, Guojiang; Giridharan, Venkataraman; Song, Guang-Ling; Xu, Zhigang; Koo, Youngmi; Qi, Pengkai; Sankar, Jagannathan; Huang, Nan; Yun, Yeoheung

    2016-01-01

    An in-situ and real-time electrochemical study in a vascular bioreactor was designed to analyze corrosion mechanism of magnesium alloy (MgZnCa) under mimetic hydrodynamic conditions. Effect of hydrodynamics on corrosion kinetics, types, rates and products was analyzed. Flow-induced shear stress (FISS) accelerated mass and electron transfer, leading to an increase in uniform and localized corrosions. FISS increased the thickness of uniform corrosion layer, but filiform corrosion decreased this layer resistance at high FISS conditions. FISS also increased the removal rate of localized corrosion products. Impedance-estimated and linear polarization-measured polarization resistances provided a consistent correlation to corrosion rate calculated by computed tomography. PMID:28626241

  4. Brillouin Corrosion Expansion Sensors for Steel Reinforced Concrete Structures Using a Fiber Optic Coil Winding Method

    Directory of Open Access Journals (Sweden)

    Xingjun Lv

    2011-11-01

    Full Text Available In this paper, a novel kind of method to monitor corrosion expansion of steel rebars in steel reinforced concrete structures named fiber optic coil winding method is proposed, discussed and tested. It is based on the fiber optical Brillouin sensing technique. Firstly, a strain calibration experiment is designed and conducted to obtain the strain coefficient of single mode fiber optics. Results have shown that there is a good linear relationship between Brillouin frequency and applied strain. Then, three kinds of novel fiber optical Brillouin corrosion expansion sensors with different fiber optic coil winding packaging schemes are designed. Sensors were embedded into concrete specimens to monitor expansion strain caused by steel rebar corrosion, and their performance was studied in a designed electrochemical corrosion acceleration experiment. Experimental results have shown that expansion strain along the fiber optic coil winding area can be detected and measured by the three kinds of sensors with different measurement range during development the corrosion. With the assumption of uniform corrosion, diameters of corrosion steel rebars were obtained using calculated average strains. A maximum expansion strain of 6,738 με was monitored. Furthermore, the uniform corrosion analysis model was established and the evaluation formula to evaluate mass loss rate of steel rebar under a given corrosion rust expansion rate was derived. The research has shown that three kinds of Brillouin sensors can be used to monitor the steel rebar corrosion expansion of reinforced concrete structures with good sensitivity, accuracy and monitoring range, and can be applied to monitor different levels of corrosion. By means of this kind of monitoring technique, quantitative corrosion expansion monitoring can be carried out, with the virtues of long durability, real-time monitoring and quasi-distribution monitoring.

  5. Brillouin corrosion expansion sensors for steel reinforced concrete structures using a fiber optic coil winding method.

    Science.gov (United States)

    Zhao, Xuefeng; Gong, Peng; Qiao, Guofu; Lu, Jie; Lv, Xingjun; Ou, Jinping

    2011-01-01

    In this paper, a novel kind of method to monitor corrosion expansion of steel rebars in steel reinforced concrete structures named fiber optic coil winding method is proposed, discussed and tested. It is based on the fiber optical Brillouin sensing technique. Firstly, a strain calibration experiment is designed and conducted to obtain the strain coefficient of single mode fiber optics. Results have shown that there is a good linear relationship between Brillouin frequency and applied strain. Then, three kinds of novel fiber optical Brillouin corrosion expansion sensors with different fiber optic coil winding packaging schemes are designed. Sensors were embedded into concrete specimens to monitor expansion strain caused by steel rebar corrosion, and their performance was studied in a designed electrochemical corrosion acceleration experiment. Experimental results have shown that expansion strain along the fiber optic coil winding area can be detected and measured by the three kinds of sensors with different measurement range during development the corrosion. With the assumption of uniform corrosion, diameters of corrosion steel rebars were obtained using calculated average strains. A maximum expansion strain of 6,738 με was monitored. Furthermore, the uniform corrosion analysis model was established and the evaluation formula to evaluate mass loss rate of steel rebar under a given corrosion rust expansion rate was derived. The research has shown that three kinds of Brillouin sensors can be used to monitor the steel rebar corrosion expansion of reinforced concrete structures with good sensitivity, accuracy and monitoring range, and can be applied to monitor different levels of corrosion. By means of this kind of monitoring technique, quantitative corrosion expansion monitoring can be carried out, with the virtues of long durability, real-time monitoring and quasi-distribution monitoring.

  6. Lateral dispersion coefficients as functions of averaging time

    International Nuclear Information System (INIS)

    Sheih, C.M.

    1980-01-01

    Plume dispersion coefficients are discussed in terms of single-particle and relative diffusion, and are investigated as functions of averaging time. To demonstrate the effects of averaging time on the relative importance of various dispersion processes, and observed lateral wind velocity spectrum is used to compute the lateral dispersion coefficients of total, single-particle and relative diffusion for various averaging times and plume travel times. The results indicate that for a 1 h averaging time the dispersion coefficient of a plume can be approximated by single-particle diffusion alone for travel times <250 s and by relative diffusion for longer travel times. Furthermore, it is shown that the power-law formula suggested by Turner for relating pollutant concentrations for other averaging times to the corresponding 15 min average is applicable to the present example only when the averaging time is less than 200 s and the tral time smaller than about 300 s. Since the turbulence spectrum used in the analysis is an observed one, it is hoped that the results could represent many conditions encountered in the atmosphere. However, as the results depend on the form of turbulence spectrum, the calculations are not for deriving a set of specific criteria but for demonstrating the need in discriminating various processes in studies of plume dispersion

  7. Results from transcranial Doppler examination on children and adolescents with sickle cell disease and correlation between the time-averaged maximum mean velocity and hematological characteristics: a cross-sectional analytical study

    Directory of Open Access Journals (Sweden)

    Mary Hokazono

    Full Text Available CONTEXT AND OBJECTIVE: Transcranial Doppler (TCD detects stroke risk among children with sickle cell anemia (SCA. Our aim was to evaluate TCD findings in patients with different sickle cell disease (SCD genotypes and correlate the time-averaged maximum mean (TAMM velocity with hematological characteristics. DESIGN AND SETTING: Cross-sectional analytical study in the Pediatric Hematology sector, Universidade Federal de São Paulo. METHODS: 85 SCD patients of both sexes, aged 2-18 years, were evaluated, divided into: group I (62 patients with SCA/Sß0 thalassemia; and group II (23 patients with SC hemoglobinopathy/Sß+ thalassemia. TCD was performed and reviewed by a single investigator using Doppler ultrasonography with a 2 MHz transducer, in accordance with the Stroke Prevention Trial in Sickle Cell Anemia (STOP protocol. The hematological parameters evaluated were: hematocrit, hemoglobin, reticulocytes, leukocytes, platelets and fetal hemoglobin. Univariate analysis was performed and Pearson's coefficient was calculated for hematological parameters and TAMM velocities (P < 0.05. RESULTS: TAMM velocities were 137 ± 28 and 103 ± 19 cm/s in groups I and II, respectively, and correlated negatively with hematocrit and hemoglobin in group I. There was one abnormal result (1.6% and five conditional results (8.1% in group I. All results were normal in group II. Middle cerebral arteries were the only vessels affected. CONCLUSION: There was a low prevalence of abnormal Doppler results in patients with sickle-cell disease. Time-average maximum mean velocity was significantly different between the genotypes and correlated with hematological characteristics.

  8. Exploratory shaft liner corrosion estimate

    International Nuclear Information System (INIS)

    Duncan, D.R.

    1985-10-01

    An estimate of expected corrosion degradation during the 100-year design life of the Exploratory Shaft (ES) is presented. The basis for the estimate is a brief literature survey of corrosion data, in addition to data taken by the Basalt Waste Isolation Project. The scope of the study is expected corrosion environment of the ES, the corrosion modes of general corrosion, pitting and crevice corrosion, dissimilar metal corrosion, and environmentally assisted cracking. The expected internal and external environment of the shaft liner is described in detail and estimated effects of each corrosion mode are given. The maximum amount of general corrosion degradation was estimated to be 70 mils at the exterior and 48 mils at the interior, at the shaft bottom. Corrosion at welds or mechanical joints could be significant, dependent on design. After a final determination of corrosion allowance has been established by the project it will be added to the design criteria. 10 refs., 6 figs., 5 tabs

  9. Bounds on Average Time Complexity of Decision Trees

    KAUST Repository

    Chikalov, Igor

    2011-01-01

    In this chapter, bounds on the average depth and the average weighted depth of decision trees are considered. Similar problems are studied in search theory [1], coding theory [77], design and analysis of algorithms (e.g., sorting) [38]. For any diagnostic problem, the minimum average depth of decision tree is bounded from below by the entropy of probability distribution (with a multiplier 1/log2 k for a problem over a k-valued information system). Among diagnostic problems, the problems with a complete set of attributes have the lowest minimum average depth of decision trees (e.g, the problem of building optimal prefix code [1] and a blood test study in assumption that exactly one patient is ill [23]). For such problems, the minimum average depth of decision tree exceeds the lower bound by at most one. The minimum average depth reaches the maximum on the problems in which each attribute is "indispensable" [44] (e.g., a diagnostic problem with n attributes and kn pairwise different rows in the decision table and the problem of implementing the modulo 2 summation function). These problems have the minimum average depth of decision tree equal to the number of attributes in the problem description. © Springer-Verlag Berlin Heidelberg 2011.

  10. Electrochemical noise measurements of steel corrosion in the molten NaCl-K2SO4 system

    DEFF Research Database (Denmark)

    Cappeln, Frederik Vilhelm; Bjerrum, Niels; Petrushina, Irina

    2005-01-01

    -called active corrosion (i.e., the corrosion proceeds with no passivation due to the influence of chlorine), characterized by the formation of volatile metal chlorides as a primary corrosion product. It was found possible to obtain an empirical separation of general and intergranular corrosion using kurtosis (a......Electrochemical noise measurements have been carried out on AISI347, 10CrMo910, 15Mo3, and X20CrMoV121 steels in molten NaCl-K2SO4 at 630 degrees C. Different types of current noise have been identified for pitting, intergranular and peeling corrosion. The corrosion mechanism was the so...... statistical parameter calculated from the electrochemical noise data). It was found that average kurtosis values above 6 indicated intergranular corrosion and average values below 6 indicated general corrosion. The response time for localized corrosion detection in in-plant monitoring was approximately 90 min...

  11. Hot corrosion of pack cementation aluminized carbon steel

    International Nuclear Information System (INIS)

    Waheed, A.F.; Mohamed, K.E.; Abd El-Azim, M.E.; Soliman, H.M.

    1998-01-01

    Low carbon steel was aluminized by the pack cementation technique at various aluminizing temperatures and times in or der to have different aluminide coatings. The aluminized specimens were sprayed at the beginning of the hot corrosion experiments with Na C 1+Na 2 SO 4 solution. The hot corrosion tests were carried out by thermal cycling at 850 degree C in air. The results were evaluated by, corrosion kinetics based on weight change measurements, scanning electron microscopy and energy dispersive X-ray analysis. It was found that the maximum corrosion resistance to this corrosive environment is achieved by aluminizing at 900 degree C for 19 h or 950 degree C for >4 h. These aliminizing conditions lead to formation of thick aluminide coatings with sufficient aluminium concentration (>15 wt%) at their outer surface necessary for continuous formation of protective Al 2 O 3 scale. The tested materials are used in protection of some components used in electric power stations (conventional or nuclear)

  12. An Invariance Property for the Maximum Likelihood Estimator of the Parameters of a Gaussian Moving Average Process

    OpenAIRE

    Godolphin, E. J.

    1980-01-01

    It is shown that the estimation procedure of Walker leads to estimates of the parameters of a Gaussian moving average process which are asymptotically equivalent to the maximum likelihood estimates proposed by Whittle and represented by Godolphin.

  13. Corrosion and stress corrosion cracking in supercritical water

    Science.gov (United States)

    Was, G. S.; Ampornrat, P.; Gupta, G.; Teysseyre, S.; West, E. A.; Allen, T. R.; Sridharan, K.; Tan, L.; Chen, Y.; Ren, X.; Pister, C.

    2007-09-01

    Supercritical water (SCW) has attracted increasing attention since SCW boiler power plants were implemented to increase the efficiency of fossil-based power plants. The SCW reactor (SCWR) design has been selected as one of the Generation IV reactor concepts because of its higher thermal efficiency and plant simplification as compared to current light water reactors (LWRs). Reactor operating conditions call for a core coolant temperature between 280 °C and 620 °C at a pressure of 25 MPa and maximum expected neutron damage levels to any replaceable or permanent core component of 15 dpa (thermal reactor design) and 100 dpa (fast reactor design). Irradiation-induced changes in microstructure (swelling, radiation-induced segregation (RIS), hardening, phase stability) and mechanical properties (strength, thermal and irradiation-induced creep, fatigue) are also major concerns. Throughout the core, corrosion, stress corrosion cracking, and the effect of irradiation on these degradation modes are critical issues. This paper reviews the current understanding of the response of candidate materials for SCWR systems, focusing on the corrosion and stress corrosion cracking response, and highlights the design trade-offs associated with certain alloy systems. Ferritic-martensitic steels generally have the best resistance to stress corrosion cracking, but suffer from the worst oxidation. Austenitic stainless steels and Ni-base alloys have better oxidation resistance but are more susceptible to stress corrosion cracking. The promise of grain boundary engineering and surface modification in addressing corrosion and stress corrosion cracking performance is discussed.

  14. A predictive approach to fitness-for-service assessment of pitting corrosion

    International Nuclear Information System (INIS)

    Shekari, Elahe; Khan, Faisal; Ahmed, Salim

    2016-01-01

    Pitting corrosion is a localized corrosion that often causes leak and failure of process components. The aim of this work is to present a new fitness-for-service (FFS) assessment methodology for process equipment to track and predict pitting corrosion. In this methodology, pit density is modeled using a non-homogenous Poisson process and induction time for pit initiation is simulated as the realization of a Weibull process. The non-homogenous Markov process is used to estimate maximum pit depth, considering that only the current state of the damage influences its future development. Subsequently, the distributions of the operating pressure and the estimated burst pressure of the defected component are integrated with Monte Carlo simulations and First Order Second Moment (FOSM) method to calculate the reliability index and probability of failure. This methodology provides a more realistic failure assessment and enables consideration of uncertainty associated with estimating pit characteristics. The practical application of the proposed model is demonstrated using a piping case study. - Highlights: • A new model to estimate maximum pit depth and pit density as two main pit characteristics. • Integrating maximum pit depth with failure analysis considering allowable pressure of defected component. • Time dependent failure analysis to determine the remaining life.

  15. A time-averaged cosmic ray propagation theory

    International Nuclear Information System (INIS)

    Klimas, A.J.

    1975-01-01

    An argument is presented, which casts doubt on our ability to choose an appropriate magnetic field ensemble for computing the average behavior of cosmic ray particles. An alternate procedure, using time-averages rather than ensemble-averages, is presented. (orig.) [de

  16. Markov Chain Models for the Stochastic Modeling of Pitting Corrosion

    Directory of Open Access Journals (Sweden)

    A. Valor

    2013-01-01

    Full Text Available The stochastic nature of pitting corrosion of metallic structures has been widely recognized. It is assumed that this kind of deterioration retains no memory of the past, so only the current state of the damage influences its future development. This characteristic allows pitting corrosion to be categorized as a Markov process. In this paper, two different models of pitting corrosion, developed using Markov chains, are presented. Firstly, a continuous-time, nonhomogeneous linear growth (pure birth Markov process is used to model external pitting corrosion in underground pipelines. A closed-form solution of the system of Kolmogorov's forward equations is used to describe the transition probability function in a discrete pit depth space. The transition probability function is identified by correlating the stochastic pit depth mean with the empirical deterministic mean. In the second model, the distribution of maximum pit depths in a pitting experiment is successfully modeled after the combination of two stochastic processes: pit initiation and pit growth. Pit generation is modeled as a nonhomogeneous Poisson process, in which induction time is simulated as the realization of a Weibull process. Pit growth is simulated using a nonhomogeneous Markov process. An analytical solution of Kolmogorov's system of equations is also found for the transition probabilities from the first Markov state. Extreme value statistics is employed to find the distribution of maximum pit depths.

  17. Online, real-time corrosion monitoring in district heating systems

    DEFF Research Database (Denmark)

    Hilbert, Lisbeth Rischel; Thorarinsdottir, R.I.

    2005-01-01

    The corrosion control in district heating systems is today performed primarily with control of the water quality. The corrosion rate is kept low by assuring low dissolved oxygen concentration, high pH and low conductivity. Corrosion failures can occur, e.g. as a result of unknown oxygen ingress, ......, precipitation of deposits or crevices. The authors describe methods used for on-line monitoring of corrosion, cover the complications and the main results of a Nordic project.......The corrosion control in district heating systems is today performed primarily with control of the water quality. The corrosion rate is kept low by assuring low dissolved oxygen concentration, high pH and low conductivity. Corrosion failures can occur, e.g. as a result of unknown oxygen ingress...

  18. Corrosion of Zircaloy-clad fuel rods in high-temperature PWRs: Measurement of waterside corrosion in North Anna Unit 1

    International Nuclear Information System (INIS)

    Balfour, M.G.; Kilp, G.R.; Comstock, R.J.; McAtee, K.R.; Thornburg, D.R.

    1992-03-01

    Twenty-four peripheral rods and two interior rods from North Anna Unit 1, End-of-Cycle 7, were measured at poolside for waterside corrosion on four-cycle Region 6 assemblies F35 and F66, with rod average burnups of 60 GWD/MTU. Similar measurements were obtained on 24 two-cycle fuel rods from Region 8A assemblies H02 and H10 with average burnups of about 40 GWD/MTU. The Region 6 peripheral rods had been corrosion measured previously after three cycles, at 45 GWD/MTU average burnup. The four-cycle Region 6 fuel rods showed high corrosion, compared to only intermediate corrosion level after three cycles. The accelerated corrosion rate in the fourth cycle was accompanied by extensive laminar cracking and spalling of the oxide film in the thickest regions. The peak corrosion of the two-cycle region 8A rods was 32 μm to 53 μm, with some isolated incipient oxide spalling. In conjunction with the in-reactor corrosion measurements, extensive characterization tests plus long-term autoclave corrosion tests were performed on archive samples of the three major tubing lots represented in the North Anna measurements. The autoclave tests generally showed the same ordering of corrosion by tubing lot as in the reactor; the chief difference between the archive tubing samples was a lower tin content (1.38 percent) for the lot with the lowest corrosion rate compared with a higher tin content (1.58) for the lot with the highest corrosion rate. There was no indication in the autoclave tests of an accelerated rate of corrosion as observed in the reactor

  19. Stochastic theory of fatigue corrosion

    Science.gov (United States)

    Hu, Haiyun

    1999-10-01

    A stochastic theory of corrosion has been constructed. The stochastic equations are described giving the transportation corrosion rate and fluctuation corrosion coefficient. In addition the pit diameter distribution function, the average pit diameter and the most probable pit diameter including other related empirical formula have been derived. In order to clarify the effect of stress range on the initiation and growth behaviour of pitting corrosion, round smooth specimen were tested under cyclic loading in 3.5% NaCl solution.

  20. Atmospheric corrosion Monitoring with Time-of-Wetness (TOW) sensor and Thin Film Electric Resistance (TFER) sensor

    International Nuclear Information System (INIS)

    Jung, Sung Won; Kim, Young Geun; Song, Hong Seok; Lee, Seung Min; Kho, Young Tai

    2002-01-01

    In this study, TOW sensor was fabricated with the same P. J. Serada's in NRC and was evaluated according to pollutant amount and wet/dry cycle. Laboratorily fabricated thin film electric resistance (TFER) probes were applied in same environment for the measurement of corrosion rate for feasibility. TOW sensor could not differentiate the wet and dry time especially at polluted environment like 3.5% NaCl solution. This implies that wet/dry time monitoring by means of TOW sensor need careful application on various environment. TFER sensor could produce instant atmospheric corrosion rate regardless of environment condition. And corrosion rate obtained by TFER sensor could be differentiated according to wet/dry cycle, wet/dry cycle time variation and solution chemistry. Corrosion behaviors of TFER sensor showed that corrosion could proceed even after wet cycle because of remained electrolyte at the surface

  1. Effect of aging time on intergranular corrosion behavior of a newly developed LDX 2404 lean duplex stainless steel

    Energy Technology Data Exchange (ETDEWEB)

    Zhao, Hui [School of Materials Engineering, Shanghai University of Engineering Science, Shanghai 201620 (China); Zhang, Ziying, E-mail: zzying@sues.edu.cn [School of Materials Engineering, Shanghai University of Engineering Science, Shanghai 201620 (China); Zhang, Huizhen [School of Management, University of Shanghai for Science and Technology, Shanghai 200093 (China); Hu, Jun [School of Materials Engineering, Shanghai University of Engineering Science, Shanghai 201620 (China); Li, Jin [Department of Materials Science, Fudan University, Shanghai 200433 (China)

    2016-07-05

    The effect of aging at 700 °C for various times on the intergranular corrosion behavior of LDX 2404 duplex stainless steel is investigated by morphological observation and electrochemical detection. Scanning electronic microscopy and transmission electronic microscopy analysis reveal that Cr{sub 2}N, M{sub 23}C{sub 6} and the sigma and chi phases nucleate simultaneously at the initial stages of aging. The granular particles of sigma phase grow larger but fewer with the increase of aging time. The electrochemical detection results show that intergranular corrosion become more severe and the corrosion type evolves from intergranular corrosion into general corrosion as the holding time extends to 48 h. - Highlights: • The IGC behavior of aged LDX 2404 is investigated. • Cr{sub 2}N, M{sub 23}C{sub 6} and the σ and χ phases nucleate simultaneously at the initial stages of aging. • IGC resistance decreases with the increase of aging time. • The corrosion type evolves from IGC into general corrosion for longer aging times.

  2. Assessing resistance of stabilized corrosion resistant steels to intergranular corrosion

    International Nuclear Information System (INIS)

    Karas, A.; Cihal, V. Jr.; Vanek, V.; Herzan, J.; Protiva, K.; Cihal, V.

    1987-01-01

    Resistance to intergranular corrosion was determined for four types of titanium-stabilized steels from the coefficients of stabilization efficiency according to the degree the chemical composition was known. The ATA SUPER steel showed the highest resistance parameter value. The resistance of this type of steel of a specific composition, showing a relatively low value of mean nitrogen content was compared with steel of an optimized chemical composition and with low-carbon niobium stabilized, molybdenum modified steels. The comparison showed guarantees of a sufficient resistance of the steel to intergranular corrosion. The method of assessing the resistance to intergranular corrosion using the calculation of the minimum content of Cr', i.e., the effective chromium content, and the maximum effective carbon content C' giving the resistance parameter k seems to be prospective for practical use in the production of corrosion resistant steels. (author). 1 tab., 5 figs., 15 refs

  3. Scale-invariant Green-Kubo relation for time-averaged diffusivity

    Science.gov (United States)

    Meyer, Philipp; Barkai, Eli; Kantz, Holger

    2017-12-01

    In recent years it was shown both theoretically and experimentally that in certain systems exhibiting anomalous diffusion the time- and ensemble-averaged mean-squared displacement are remarkably different. The ensemble-averaged diffusivity is obtained from a scaling Green-Kubo relation, which connects the scale-invariant nonstationary velocity correlation function with the transport coefficient. Here we obtain the relation between time-averaged diffusivity, usually recorded in single-particle tracking experiments, and the underlying scale-invariant velocity correlation function. The time-averaged mean-squared displacement is given by 〈δ2¯〉 ˜2 DνtβΔν -β , where t is the total measurement time and Δ is the lag time. Here ν is the anomalous diffusion exponent obtained from ensemble-averaged measurements 〈x2〉 ˜tν , while β ≥-1 marks the growth or decline of the kinetic energy 〈v2〉 ˜tβ . Thus, we establish a connection between exponents that can be read off the asymptotic properties of the velocity correlation function and similarly for the transport constant Dν. We demonstrate our results with nonstationary scale-invariant stochastic and deterministic models, thereby highlighting that systems with equivalent behavior in the ensemble average can differ strongly in their time average. If the averaged kinetic energy is finite, β =0 , the time scaling of 〈δ2¯〉 and 〈x2〉 are identical; however, the time-averaged transport coefficient Dν is not identical to the corresponding ensemble-averaged diffusion constant.

  4. An assessment of corrosion life of copper overpack

    International Nuclear Information System (INIS)

    Honda, A.; Taniguchi, N.

    1999-08-01

    Corrosion life of copper overpack is estimated on the basis of current understandings of copper corrosion processes. The assessment is based on the mass balance. Oxygen and sulfide were taken into account as corrosive species. The sulfate existing in bentonite is assumed to be reduced to sulfide by sulfate reducing bacteria and corrodes copper overpacks. Pitting is involved in the assesment using two methods. One method is use of pitting factor acquired from analysis of archeological artifacts. The other is use of extreme value statistical technique. The time evolution of parameters for cumulative probability distribution function, Gumbel distribution, was estimated using the data from copper specimens buried in various soil and archeological artifacts of the bronze age. The pitting depth for 1000 years is estimated using the parameters for probability distribution function. The result of estimation shows 39-mm is the maximum penetration for 1000 years. Natural analogue data suggest the corrosion rate of 3 mm/1000 years. Therefore the estimation is considered to be conservative. (author)

  5. Concrete cover cracking with reinforcement corrosion of RC beam during chloride-induced corrosion process

    International Nuclear Information System (INIS)

    Zhang Ruijin; Castel, Arnaud; Francois, Raoul

    2010-01-01

    This paper deals with the evolution of the corrosion pattern based on two beams corroded by 14 years (beam B1CL1) and 23 years (beam B2CL1) of conservation in a chloride environment. The experimental results indicate that, at the cracking initiation stage and the first stage of cracking propagation, localized corrosion due to chloride ingress is the predominant corrosion pattern and pitting corrosion is the main factor that influences the cracking process. As corrosion cracking increases, general corrosion develops rapidly and gradually becomes predominant in the second stage of cracking propagation. A comparison between existing models and experimental results illustrates that, although Vidal et al.'s model can better predict the reinforcement corrosion of beam B1CL1 under localized corrosion, it cannot predict the corrosion of beam B2CL1 under general corrosion. Also, Rodriguez's model, derived from the general corrosion due to electrically accelerated corrosion experiments, cannot match natural chloride corrosion irrespective of whether corrosion is localized or general. Thus, for natural general corrosion in the second stage of cracking propagation, a new model based on the parameter of average steel cross-section loss is put forward to predict steel corrosion from corrosion cracking.

  6. Penetration of corrosion products and corrosion-induced cracking in reinforced cementitious materials

    DEFF Research Database (Denmark)

    Michel, Alexander; Pease, Brad J.; Peterova, Adela

    2014-01-01

    This paper describes experimental investigations on corrosion-induced deterioration in reinforced cementitious materials and the subsequent development and implementation of a novel conceptual model. Rejnforced mortar specimens of varying water-to-cement ratios were subjected to current-induced c......This paper describes experimental investigations on corrosion-induced deterioration in reinforced cementitious materials and the subsequent development and implementation of a novel conceptual model. Rejnforced mortar specimens of varying water-to-cement ratios were subjected to current......-dependent concentrations of corrosion products averaged through the specimen thickness. Digital image correlation (DIC) was used to measure corrosion-induced deformations including deformations between steel and cementitious matrix as well as formation and propagation of corrosion-induced cracks. Based on experimental...... observations, a conceptual model was developed to describe the penetration of solid corrosion products into capillary pores of the cementitious matrix. Only capillary pores within a corrosion accommodating region (CAR), i.e. in close proximity of the steel reinforcement, were considered accessible...

  7. Electrochemical and corrosion properties of carbon steel in simulated geological disposal environments

    International Nuclear Information System (INIS)

    Sugimoto, Katsuhisa

    2011-01-01

    This paper reviews electrochemical and corrosion studies on the application of carbon steel to an overpack container, which is used for the geological disposal of radioactive wastes. Deaerated alkaline Na 2 SO 4 -NaHCO 3 - NaCl solutions and bentonite soaked with the solutions are used as simulated geological disposal environments. Electrochemical studies show the corrosion of the steel in an early stage is the activation control. Corrosion rates are controlled by the composition of the solutions, alloying elements, and the structure of the steel. The rates decrease with time due to the formation of FeCO 3 (siderite) film on the steel. Immersion corrosion tests show general corrosion morphology. Average corrosion rates of long duration have been evaluated. Clear proofs of the initiation of localized corrosion, such as pitting, crevice corrosion, hydrogen embrittlement and stress-corrosion cracking, have not been reported. (author)

  8. Influence of Applied Voltage and Film-Formation Time on Microstructure and Corrosion Resistance of Coatings Formed on Mg-Zn-Zr-Ca Bio-magnesium Alloy

    Science.gov (United States)

    Yandong, Yu; Shuzhen, Kuang; Jie, Li

    2015-09-01

    The influence of applied voltage and film-formation time on the microstructure and corrosion resistance of coatings formed on a Mg-Zn-Zr-Ca novel bio-magnesium alloy has been investigated by micro-arc oxidation (MAO) treatment. Phase composition and microstructure of as-coated samples were analyzed by the x-ray diffraction, energy dispersive x-ray spectroscopy and scanning electron microscopy. And the porosity and average of micro-pore aperture of the surface on ceramic coatings were analyzed by general image software. Corrosion microstructure of as-coated samples was caught by a microscope digital camera. The long-term corrosion resistance of as-coated samples was tested in simulated body fluid for 30 days. The results showed that the milky white smooth ceramic coating formed on the Mg-Zn-Zr-Ca novel bio-magnesium alloy was a compound of MgO, Mg2SiO4 and MgSiO3, and its corrosion resistance was significantly improved compared with that of the magnesium substrate. In addition, when the MAO applied voltage were 450 V and 500 V and film-formation time were 9 min and 11 min, the surface micro-morphology and the corrosion resistance of as-coated samples were relatively improved. The results provided a theoretical foundation for the application of the Mg-Zn-Zr-Ca novel bio-magnesium alloy in biomedicine.

  9. Modeling time-dependent corrosion fatigue crack propagation in 7000 series aluminum alloys

    Science.gov (United States)

    Mason, Mark E.; Gangloff, Richard P.

    1994-01-01

    Stress corrosion cracking and corrosion fatigue experiments were conducted with the susceptible S-L orientation of AA7075-T651, immersed in acidified and inhibited NaCl solution, to provide a basis for incorporating environmental effects into fatigue crack propagation life prediction codes such as NASA FLAGRO. This environment enhances da/dN by five to ten-fold compared to fatigue in moist air. Time-based crack growth rates from quasi-static load experiments are an order of magnitude too small for accurate linear superposition prediction of da/dN for loading frequencies above 0.001 Hz. Alternate methods of establishing da/dt, based on rising-load or ripple-load-enhanced crack tip strain rate, do not increase da/dt and do not improve linear superposition. Corrosion fatigue is characterized by two regimes of frequency dependence; da/dN is proportional to f(exp -1) below 0.001 Hz and to F(exp 0) to F(exp -0.1) for higher frequencies. Da/dN increases mildly both with increasing hold-time at K(sub max) and with increasing rise-time for a range of loading waveforms. The mild time-dependence is due to cycle-time-dependent corrosion fatigue growth. This behavior is identical for S-L nd L-T crack orientations. The frequency response of environmental fatigue in several 7000 series alloys is variable and depends on undefined compositional or microstructural variables. Speculative explanations are based on the effect of Mg on occluded crack chemistry and embritting hydrogen uptake, or on variable hydrogen diffusion in the crack tip process zone. Cracking in the 7075/NaCl system is adequately described for life prediction by linear superposition for prolonged load-cycle periods, and by a time-dependent upper bound relationship between da/dN and delta K for moderate loading times.

  10. Corrosion of ferrous materials in a basaltic environment

    International Nuclear Information System (INIS)

    Brehm, W.F.

    1990-01-01

    The results of corrosion tests on A27 cast low-carbon steel are discussed. The corrosion performance of these materials was tested in condensed systems at temperature ranging from 50 C to 200 C and in air-steam mixtures between 150 C and 300 C. The groundwater used was a deoxygenated mild sodium chloride solution. When used, the packing material was 75 percent crushed basalt and 25 percent Wyoming sodium bentonite. In synthetic groundwater corrosion rates for both cast carbon steel and A387 steel in saturated packing and air-steam mixtures were low; maximum rates of 9 μm/a for A27 steel and 1.8 μm/a for A387 steel were observed. These maximum rates were observed at intermediate temperatures because of the formation of non-protective corrosion films. In A27 steel magnetite was the principal corrosion product, with non-protective siderite observed at 100 C. Pits were difficult to produce in saturated packing in A27 steel and did not grow. In air-steam mixtures corrosion rates of both steels were again very low, less than 1 μm/a. Magnetite and small amounts of hematite were detected in corrosion product films

  11. Time average vibration fringe analysis using Hilbert transformation

    International Nuclear Information System (INIS)

    Kumar, Upputuri Paul; Mohan, Nandigana Krishna; Kothiyal, Mahendra Prasad

    2010-01-01

    Quantitative phase information from a single interferogram can be obtained using the Hilbert transform (HT). We have applied the HT method for quantitative evaluation of Bessel fringes obtained in time average TV holography. The method requires only one fringe pattern for the extraction of vibration amplitude and reduces the complexity in quantifying the data experienced in the time average reference bias modulation method, which uses multiple fringe frames. The technique is demonstrated for the measurement of out-of-plane vibration amplitude on a small scale specimen using a time average microscopic TV holography system.

  12. Galvanic corrosion of laser weldments of AA6061 aluminium alloy

    International Nuclear Information System (INIS)

    Rahman, A.B.M. Mujibur; Kumar, S.; Gerson, A.R.

    2007-01-01

    Galvanic corrosion of laser welded AA6061 aluminium alloy, arising from the varying rest potentials of the various weldment regions, was examined. The weld fusion zone is found to be the most cathodic region of the weldment while the base material is the most anodic region. The rate of galvanic corrosion, controlled by the cathodic process at the weld fusion zone, increases with time until a steady state maximum is reached. On galvanic corrosion the corrosion potential of the weld fusion zone shifts in the positive direction and the free corrosion current increases. It is proposed that the cathodic process at the weld fusion zone causes a local increase in pH that in turn causes dissolution of the surface film resulting in the loss of Al to solution and the increase of intermetallic phases. The increase in galvanic corrosion may result from either the build up of the intermetallic phases in the surface layer and/or significant increase in surface area of the weld fusion zone due to the porous nature of the surface layer

  13. Biotribocorrosion-an appraisal of the time dependence of wear and corrosion interactions: I. The role of corrosion

    International Nuclear Information System (INIS)

    Yan, Y; Neville, A; Dowson, D

    2006-01-01

    With the increasing interest in metal-on-metal (MoM) joint implants, studies have been focused on their wear and corrosion behaviour. Integrated electrochemical tests have been conducted and are reported in this paper. The corrosion, wear and wear-corrosion behaviour for three materials (high carbon CoCrMo, low carbon CoCrMo and UNS S31603) have been discussed. Corrosion effects on the overall performance for the three materials are analysed. Two distinct regimes have been found for the three materials: (a) the running-in regime and (b) the steady state regime, in line with other research. Even in the steady state regime, 20%-30% of the material degradation can be attributed to corrosion-related damage. High carbon CoCrMo showed excellent corrosion, wear and corrosion-wear resistance and therefore it delivered the best overall performance in terms of a lower wear rate, a lower friction coefficient and a higher resistance to corrosion

  14. Salecker-Wigner-Peres clock and average tunneling times

    International Nuclear Information System (INIS)

    Lunardi, Jose T.; Manzoni, Luiz A.; Nystrom, Andrew T.

    2011-01-01

    The quantum clock of Salecker-Wigner-Peres is used, by performing a post-selection of the final state, to obtain average transmission and reflection times associated to the scattering of localized wave packets by static potentials in one dimension. The behavior of these average times is studied for a Gaussian wave packet, centered around a tunneling wave number, incident on a rectangular barrier and, in particular, on a double delta barrier potential. The regime of opaque barriers is investigated and the results show that the average transmission time does not saturate, showing no evidence of the Hartman effect (or its generalized version).

  15. An Experimental Study for Quantitative Estimation of Rebar Corrosion in Concrete Using Ground Penetrating Radar

    Directory of Open Access Journals (Sweden)

    Md Istiaque Hasan

    2016-01-01

    Full Text Available Corrosion of steel rebar in reinforced concrete is one the most important durability issues in the service life of a structure. In this paper, an investigation is conducted to find out the relationship between the amount of reinforced concrete corrosion and GPR maximum positive amplitude. Accelerated corrosion was simulated in the lab by impressing direct current into steel rebar that was submerged in a 5% salt water solution. The amount of corrosion was varied in the rebars with different levels of mass loss ranging from 0% to 45%. The corroded rebars were then placed into three different oil emulsion tanks having different dielectric properties similar to concrete. The maximum amplitudes from the corroded bars were recorded. A linear relationship between the maximum positive amplitudes and the amount of corrosion in terms of percentage loss of area was observed. It was proposed that the relationship between the GPR maximum amplitude and the amount of corrosion can be used as a basis of a NDE technique of quantitative estimation of corrosion.

  16. Multistage parallel-serial time averaging filters

    International Nuclear Information System (INIS)

    Theodosiou, G.E.

    1980-01-01

    Here, a new time averaging circuit design, the 'parallel filter' is presented, which can reduce the time jitter, introduced in time measurements using counters of large dimensions. This parallel filter could be considered as a single stage unit circuit which can be repeated an arbitrary number of times in series, thus providing a parallel-serial filter type as a result. The main advantages of such a filter over a serial one are much less electronic gate jitter and time delay for the same amount of total time uncertainty reduction. (orig.)

  17. Corrosion measurements on apt prototypic materials in the Lansce high-power proton beam and applicability to other systems

    International Nuclear Information System (INIS)

    Lillard, R.S.; Gac, F.D.; James, M.R.; Maloy, S.A.; Paciotti, M.A.; Waters, L.S.; Willcutt, G.J.; Chandler, G.T.; Ferguson, P.D.

    2003-01-01

    The corrosion rates of several corrosion resistant materials behave in a similar manner even under the intense radiation of the LANSCE high-power beam. A second observation was made, showing that the corrosion rates saturated under high instantaneous radiation intensity in corrosion experiments conducted for the accelerator production of tritium (APT) programme. The LANSCE H + beam is not prototypic of the proposed APT production plant in several respects. The instantaneous proton flux in the APT production plant beam is about 10 times that of the LANSCE beam. The small transverse APT beam spot is rastered to spread the power density over the area of the target, and as the beam rasters, it creates a pulsed character to the beam at a specific location. In order to develop correlations that would enable extrapolation of the corrosion data to the proposed APT production plant, the experimental programme included measurements over a range of average beam currents, measurements at high and low instantaneous beam current, and measurements at various combinations of pulse width and repetition rate. The correlations that were developed are based on an approximately linear dependence of corrosion rate on average beam current (average radiation intensity) and the saturation effect observed at high instantaneous radiation intensity. For a given transverse beam profile and for the same average beam current, the correlations predict the highest corrosion rate in a do beam and the lowest corrosion rate in the lowest duty cycle beams. In the case of the APT extrapolation, the predicted corrosion rates were a factor of 5 lower than for a do beam depositing the same average power density. The measured corrosion rates and the formulated extrapolations are applicable to water-cooled targets and components in proton beams. (authors)

  18. Comparison of the long-time corrosion behavior of certain Zr alloys in PWR, BWR, and laboratory tests

    International Nuclear Information System (INIS)

    Garzarolli, F.; Broy, Y.; Busch, R.A.

    1996-01-01

    Laboratory corrosion tests have always been an important tool for Zr alloy development and optimization. However, it must be known whether a test is representative for the application in-reactor. To shed more light on this question, coupons of several Zr alloys were exposed under isothermal conditions in BWR and PWR type environments. For evaluation of the in-PWR tests and for comparison of out-of-pile and in-pile tests, the different temperatures and times were normalized to a temperature-independent normalized time by assuming an activation temperature (Q/R) of 14,200 K. Comparison of in-PWR and out-of-pile corrosion behavior of Zircaloy shows that corrosion deviates to higher values in PWR if a weight gain of about 50 mg/dm 2 is exceeded. In the case of the Zr2.5Nb alloy, a slight deviation of corrosion as compared to laboratory results starts in PWR only above a weight gain of 100 mg/dm 2 . In BWR, corrosion of Zircaloy is enhanced early in time if compared with out-of-pile. Zr2.5Nb exhibits higher corrosion results in BWR than Zircaloy-4. Alloying chemistry and material condition affect corrosion of Zr alloys. However, several of the material parameters have shown a different ranking in the different environments. Nevertheless, several material parameters influencing in-reactor corrosion like the second phase particle (SPP) size of in-PWR behavior as the Sn and Fe content can be optimized by out-of-pile corrosion tests

  19. Influence of Short-time Oxidation on Corrosion Properties of Directionally Solidified Superalloys with Different Orientations

    Directory of Open Access Journals (Sweden)

    MA Luo-ning

    2016-07-01

    Full Text Available In order to investigate the corrosion performance on intersecting and longitudinal surfaces of unoxidized and oxidized directionally solidified superalloys, Ni-base directionally solidified superalloy DZ125 and Co-base directionally solidified superalloy DZ40M were selected. Oxidation behavior on both alloys with different orientations was investigated at 1050℃ at different times, simulating the oxidation process of vanes or blades in service; subsequent electrochemical performance in 3.5%NaCl aqueous solution was studied on two orientations of unoxidized and oxidized alloys, simulating the corrosion process of superalloy during downtime. The results show that grain boundaries and sub-boundaries of directionally solidified superalloys are susceptible to corrosion and thus longitudinal surface with lower area fraction of grain boundaries has higher corrosion resistance. Compared to intersecting surface of alloys, the structure of grain boundaries of longitudinal surface is less conducive to diffusion and thus the oxidation rate on longitudinal surface is lower. Formation of oxide layers on alloys after short-time oxidation provides protective effect and enhances the corrosion resistance.

  20. Serpent-COREDAX analysis of CANDU-6 time-average model

    Energy Technology Data Exchange (ETDEWEB)

    Motalab, M.A.; Cho, B.; Kim, W.; Cho, N.Z.; Kim, Y., E-mail: yongheekim@kaist.ac.kr [Korea Advanced Inst. of Science and Technology (KAIST), Dept. of Nuclear and Quantum Engineering Daejeon (Korea, Republic of)

    2015-07-01

    COREDAX-2 is the nuclear core analysis nodal code that has adopted the Analytic Function Expansion Nodal (AFEN) methodology which has been developed in Korea. AFEN method outperforms in terms of accuracy compared to other conventional nodal methods. To evaluate the possibility of CANDU-type core analysis using the COREDAX-2, the time-average analysis code system was developed. The two-group homogenized cross-sections were calculated using Monte Carlo code, Serpent2. A stand-alone time-average module was developed to determine the time-average burnup distribution in the core for a given fuel management strategy. The coupled Serpent-COREDAX-2 calculation converges to an equilibrium time-average model for the CANDU-6 core. (author)

  1. Time-variant flexural reliability of RC beams with externally bonded CFRP under combined fatigue-corrosion actions

    International Nuclear Information System (INIS)

    Bigaud, David; Ali, Osama

    2014-01-01

    Time-variant reliability analysis of RC highway bridges strengthened with carbon fibre reinforced polymer CFRP laminates under four possible competing damage modes (concrete crushing, steel rupture after yielding, CFRP rupture and FRP plate debonding) and three degradation factors is analyzed in terms of reliability index β using FORM. The first degradation factor is chloride-attack corrosion which induces reduction in steel area and concrete cover cracking at characteristic key times (corrosion initiation, severe surface cover cracking). The second degradation factor considered is fatigue which leads to damage in concrete and steel rebar. Interaction between corrosion and fatigue crack growth in steel reinforcing bars is implemented. The third degradation phenomenon is the CFRP properties deterioration due to aging. Considering these three degradation factors, the time-dependent flexural reliability profile of a typical simple 15 m-span intermediate girder of a RC highway bridge is constructed under various traffic volumes and under different corrosion environments. The bridge design options follow AASHTO-LRFD specifications. Results of the study have shown that the reliability is very sensitive to factors governing the corrosion. Concrete damage due to fatigue slightly affects reliability profile of non-strengthened section, while service life after strengthening is strongly related to fatigue damage in concrete. - Highlights: • We propose a method to follow the time-variant reliability of strengthened RC beams. • We consider multiple competing failure modes of CFRP strengthened RC beams. • We consider combined degradation mechanisms (corrosion, fatigue, ageing of CFRP)

  2. Extremely high resolution corrosion monitoring of pipelines: retrofittable, non-invasive and real-time

    Energy Technology Data Exchange (ETDEWEB)

    Baltzersen, Oeystein; Tveit, Edd [Sensorlink AS, Trondheim (Norway); Verley, Richard [StatoilHydro ASA, Stockholm (Sweden)

    2009-07-01

    The Ultramonit unit is a clamp-on tool (removable) that uses an array of sensors to provide online, real-time, reliable and repeatable high accuracy ultrasonic wall thickness measurements and corrosion monitoring at selected locations along the pipeline. The unit can be installed on new or existing pipelines by diver or ROV. The system is based on the well-established ultrasonic pulse-echo method (A-scan). Special processing methods, and the fact that the unit is fixed to the pipeline, enable detection of changes in wall thickness in the micro-meter range. By utilizing this kind of resolution, it is possible to project corrosion rates in hours or days. The tool is used for calibration of corrosion inhibitor programs, verification and calibration of inspection pig data and general corrosion monitoring of new and existing pipelines. (author)

  3. Fretting Corrosion Behavior of Experimental Ti-20Cr Compared to Titanium.

    Science.gov (United States)

    Sawada, Tomofumi; Schille, Christine; Almadani, Atif; Geis-Gerstorfer, Jürgen

    2017-02-17

    Experimental cast titanium alloys containing 20 mass% chromium (Ti-20Cr) show preferable mechanical properties and a good corrosion resistance. This study evaluated the fretting corrosion behavior of Ti-20Cr. Ti-20Cr ( n = 4) and commercially pure titanium (CP-Ti, n = 6) disk specimens were used. The fretting corrosion test was performed by electrochemical corrosion at 0.3 V in 0.9% saline solution and mechanical damage using 10 scratching cycles with three different scratching speeds (10-40 mm/s) at 10 N. After testing, the activation peak, repassivation time and surface morphology of each specimen were analyzed. The differences between the results were tested by parametric tests (α = 0.05). The average activation peaks were significantly higher in CP-Ti than in Ti-20Cr ( p Ti. Slight differences in the repassivation time were observed between the materials at every scratching speed; faster scratching speeds showed shorter repassivation times in both materials ( p Ti showed severe damage and significantly higher wear depth than Ti-20Cr ( p < 0.05). In conclusion, adding chromium to titanium reduced surface damage and improved the fretting corrosion resistance.

  4. Maintained ship hull girder ultimate strength reliability considering corrosion and fatigue

    DEFF Research Database (Denmark)

    Hu, Yong; Cui, W.; Pedersen, Preben Terndrup

    2004-01-01

    The prupose of this paper is to propose a methodology to assess the time-variant ultimate strength of ship hull girder under the degradations of corrosion and fatigue. The effects of fatigue cracks on the tensile and compressive residual ultimate strength of stiffened panels and unstiffened plates......, webs and flanges, respectively. The effects of inspections and repair are taken into account. A minimum net thickness rule is used to determine repair policies. A procedure is proposed to determine the maximum allowable corrosion thickness of different parts of the hull cross section. The procedure...

  5. Increasing the maximum daily operation time of MNSR reactor by modifying its cooling system

    International Nuclear Information System (INIS)

    Khamis, I.; Hainoun, A.; Al Halbi, W.; Al Isa, S.

    2006-08-01

    thermal-hydraulic natural convection correlations have been formulated based on a thorough analysis and modeling of the MNSR reactor. The model considers detailed description of the thermal and hydraulic aspects of cooling in the core and vessel. In addition, determination of pressure drop was made through an elaborate balancing of the overall pressure drop in the core against the sum of all individual channel pressure drops employing an iterative scheme. Using this model, an accurate estimation of various timely core-averaged hydraulic parameters such as generated power, hydraulic diameters, flow cross area, ... etc. for each one of the ten-fuel circles in the core can be made. Furthermore, distribution of coolant and fuel temperatures, including maximum fuel temperature and its location in the core, can now be determined. Correlation among core-coolant average temperature, reactor power, and core-coolant inlet temperature, during both steady and transient cases, have been established and verified against experimental data. Simulating various operating condition of MNSR, good agreement is obtained for at different power levels. Various schemes of cooling have been investigated for the purpose of assessing potential benefits on the operational characteristics of the syrian MNSR reactor. A detailed thermal hydraulic model for the analysis of MNSR has been developed. The analysis shows that an auxiliary cooling system, for the reactor vessel or installed in the pool which surrounds the lower section of the reactor vessel, will significantly offset the consumption of excess reactivity due to the negative reactivity temperature coefficient. Hence, the maximum operating time of the reactor is extended. The model considers detailed description of the thermal and hydraulic aspects of cooling the core and its surrounding vessel. Natural convection correlations have been formulated based on a thorough analysis and modeling of the MNSR reactor. The suggested 'micro model

  6. Asymptotic Time Averages and Frequency Distributions

    Directory of Open Access Journals (Sweden)

    Muhammad El-Taha

    2016-01-01

    Full Text Available Consider an arbitrary nonnegative deterministic process (in a stochastic setting {X(t,  t≥0} is a fixed realization, i.e., sample-path of the underlying stochastic process with state space S=(-∞,∞. Using a sample-path approach, we give necessary and sufficient conditions for the long-run time average of a measurable function of process to be equal to the expectation taken with respect to the same measurable function of its long-run frequency distribution. The results are further extended to allow unrestricted parameter (time space. Examples are provided to show that our condition is not superfluous and that it is weaker than uniform integrability. The case of discrete-time processes is also considered. The relationship to previously known sufficient conditions, usually given in stochastic settings, will also be discussed. Our approach is applied to regenerative processes and an extension of a well-known result is given. For researchers interested in sample-path analysis, our results will give them the choice to work with the time average of a process or its frequency distribution function and go back and forth between the two under a mild condition.

  7. On-line electrochemical monitoring of microbially influenced corrosion

    International Nuclear Information System (INIS)

    Dowling, N.J.E.; Stansbury, E.E.; White, D.C.; Borenstein, S.W.; Danko, J.C.

    1989-01-01

    Newly emerging electrochemical measurement techniques can provide on-line, non-destructive monitoring of the average corrosion rate and indications of localized pitting corrosion together with insight into fundamental electrochemical mechanisms responsible for the corrosion process. This information is relevant to evaluating, monitoring, understanding and controlling microbially influenced corrosion (MIC). MIC of coupons exposed in sidestream devices on site or in laboratory-based experiments, where the corrosion response is accelerated by exposure to active consortia of microbes recovered from specific sites, can be utilized to evaluate mitigation strategies. The average corrosion rates can be determined by small amplitude cyclic voltametry (SACV), and AC impedance spectroscopy (EIS). EIS can also give insight into the mechanisms of the MIC and indications of localized corrosion. Pitting corrosion can be detected non-destructively with open circuit potential monitoring (OCP). OCP also responds to bacterial biofilm activities such as oxygen depletion and other electrochemical activities. Utilizing these methods, accelerated tests can be designed to direct the selection of materials, surface treatments of materials, and welding filler materials, as well as the optimization of chemical and mechanical countermeasures with the microbial consortia recovered and characterized from the specific sites of interest

  8. A Time-Variant Reliability Model for Copper Bending Pipe under Seawater-Active Corrosion Based on the Stochastic Degradation Process

    Directory of Open Access Journals (Sweden)

    Bo Sun

    2018-03-01

    Full Text Available In the degradation process, the randomness and multiplicity of variables are difficult to describe by mathematical models. However, they are common in engineering and cannot be neglected, so it is necessary to study this issue in depth. In this paper, the copper bending pipe in seawater piping systems is taken as the analysis object, and the time-variant reliability is calculated by solving the interference of limit strength and maximum stress. We did degradation experiments and tensile experiments on copper material, and obtained the limit strength at each time. In addition, degradation experiments on copper bending pipe were done and the thickness at each time has been obtained, then the response of maximum stress was calculated by simulation. Further, with the help of one kind of Monte Carlo method we propose, the time-variant reliability of copper bending pipe was calculated based on the stochastic degradation process and interference theory. Compared with traditional methods and verified by maintenance records, the results show that the time-variant reliability model based on the stochastic degradation process proposed in this paper has better applicability in the reliability analysis, and it can be more convenient and accurate to predict the replacement cycle of copper bending pipe under seawater-active corrosion.

  9. Intergranular corrosion of 13Cr and 17Cr martensitic stainless steels in accelerated corrosive solution and high-temperature, high-purity water

    International Nuclear Information System (INIS)

    Ozaki, Toshinori; Ishikawa, Yuichi

    1988-01-01

    Intergranular corrosion behavior of 13Cr and 17Cr martensitic stainless steels was studied by electrochemical and immersing corrosion tests. Effects of the mEtallurgical and environmental conditions on the intergranular corrosion of various tempered steels were examined by the following tests and discussed. (a) Anodic polarization measurement and electrolytical etching test in 0.5 kmol/m 3 H 2 SO 4 solution at 293 K. (b) Immersion corrosion test in 0.88 kmol/m 3 HNO 3 solution at 293 K. (c) Long-time immersion test for specimens with a crevice in a high purity water at 473 K∼561 K. It was found from the anodic polarization curves in 0.5 kmol/m 3 H 2 SO 4 solution-at 293 K that the steels tempered at 773∼873 K had susceptibility to intergranular corrosion in the potential region indicating a second current maximum (around-0.1 V. vs. SCE). But the steel became passive in the more noble potential region than the second current peak potential, while in the less noble potential region general corrosion occurred independent of its microstructure. The intergranular corrosion occurred due to the localized dissolution along the pre-austenitic grain boundary and the martensitic lath boundary. It could be explained by the same dissolution model of the chromium depleted zone as proposed for the intergranular corrosion of austenitic and ferritic stainless steels. The intergranular corrosion occurred entirely at the free surface in 0.88 kmol/m 3 HNO 3 solution, while in the high temperature and high purity water only the entrance of the crevice corroded. It was also suggested that this intergranular corrosion might serve as the initiation site for stress corrosion cracking of the martensitic stainless steel. (author)

  10. Contribution of archaeological analogs to the estimation of average corrosion rates and long term corrosion mechanisms of low carbon steel in soil; Apport des analogues archeologiques a l'estimation des vitesses moyennes et a l'etude des mecanismes de corrosion a tres long terme des aciers non allies dans les sols

    Energy Technology Data Exchange (ETDEWEB)

    Neff, D

    2003-11-15

    identified. This corrosion form, constituted among others by a siderite layer is due to a particular environment: waterlogged soil containing wood. In the whole, analyses conducted in the TM show that it is composed of goethite badly crystallized in comparison with those of the DPL. Moreover, in this zone, the average elemental iron amount decreases progressively from the metal to the soil in which it stabilizes. In order to know the behaviour of the identified phases in soil water, some thermodynamic data have been involved to calculate their solubility in function of pH, potential and various water composition. The first conclusion concerns the influence of the composition and the structure of the material which is not important for the corrosion behaviour. From the results, some hypothesis have been formulated on the long term corrosion mechanisms of hypo-eutectoids steels in the considered environment. The role of the cracks formed in the DPL during the burial was evidenced. Moreover, these corrosion products undertake a dissolution in the soil water and a reprecipitation, explaining the progressive decrease of the iron amount in the TM. Lastly, some average corrosion rates have been measured with the help of the analytical and thermodynamic results: they do not exceed 4 {mu}m/year. (author)

  11. Monitoring reinforcement corrosion and corrosion-induced cracking using non-destructive x-ray attenuation measurements

    DEFF Research Database (Denmark)

    Michel, Alexander; Pease, Bradley Justin; Geiker, Mette Rica

    2011-01-01

    To test the applicability of the x-ray attenuation method to monitor the movement of corrosion products as well as the formation and propagation of cracks in cementitious materials reinforced mortar samples were prepared and tested under accelerated corrosion conditions. It is evident from the ex...... of the corrosion products averaged through the specimen thickness. The total mass loss of steel, obtained by the x-ray attenuation method, was found to be in very good agreement with the mass loss obtained by gravimetric method as well as Faraday's law....

  12. Acoustic emission intensity analysis of corrosion in prestressed concrete piles

    Science.gov (United States)

    Vélez, William; Matta, Fabio; Ziehl, Paul

    2014-02-01

    Corrosion of steel strands in prestressed concrete (PC) bridges may lead to substantial damage or collapse well before the end of the design life. Acoustic Emission (AE) is a suitable nondestructive technique to detect and locate corrosion in reinforced and prestressed concrete, which is key to prioritize inspection and maintenance. An effective tool to analyze damage-related AE data is intensity analysis (IA), which is based on two data trends, namely Severity (average signal strength of high amplitude hits) and Historic Index (ratio of the average signal strength of the most recent hits to the average of all hits). IA criteria for corrosion assessment in PC were recently proposed based on empirical evidence from accelerated corrosion tests. In this paper, AE data from prestressed and non-prestressed concrete pile specimens exposed to salt water wet-dry cycling for over 600 days are used to analyze the relation between Severity and Historic Index and actual corrosion. Evidence of corrosion is gained from the inspection of decommissioned specimens. The selection of suitable J and K parameters for IA is discussed, and an IA chart with updated corrosion criteria for PC piles is presented.

  13. Development of Flow Accelerated Corrosion Reduction Technology

    Energy Technology Data Exchange (ETDEWEB)

    Heo, Min Bum; Choi, Won Yeol; Lee, Jong Chan; Lim, Dong Seok; Kwon, Byung Il; Ku, Hee Kwon; Kim, Jong Uk [FNC Tech, Yongin (Korea, Republic of)

    2015-10-15

    Development of flow accelerated corrosion reduction technology is necessary for prevent this kind of accidents. This study deals with development of flow accelerated corrosion reduction technology through platinum injection and developed of flow accelerated corrosion reduction technology by imitating water chemical condition in PWR secondary system in practice. In addition, in order to get reliability of water chemical simulator in PWR secondary system, analyzed and compared with test result through CFD analysis. This study composed test device that can simulate water chemical environment in PWR secondary system, in order to develop flow accelerated corrosion reduction , and evaluated the ratio of corrosion in water chemical environment in PWR secondary system. In conclusion, corrosion ratio of low alloy steel material that includes more Cr and Mo was lower. And the results were confirmed to be the maximum corrosion rate in the case that replicate the 90 elbow. Additionally, inserted Pt nano particle for developing flow accelerated corrosion rate reduction technology, the test results, it was confirmed for about 80% of the flow accelerated corrosion rate reduction than before input.

  14. Stress corrosion cracking for 316 stainless steel clips in a condensate stabilizer

    Energy Technology Data Exchange (ETDEWEB)

    Al-Awar, A.; Aldajah, S.; Harhara, A. [Department of Mechanical Engineering, United Arab Emirates University, P. O. Box 17555 Al-AIn 17555 (United Arab Emirates)

    2011-09-15

    In one of the gas processing facilities in Abu Dhabi, UAE; a case of 316L stainless steel material failure occurred in the fractionating column due to stress cracking corrosion twice in a cycle of less than 2 years. This paper studies the stress corrosion cracking behavior of the 316L stainless steel in an accelerated corrosion environment and compares it with a higher corrosion resistant nickel alloy (Inconel 625). The experimental work was designed according to ASTM G36 standard, the samples were immersed in a boiling magnesium chloride medium which provided the accelerated corrosion environment and the tested samples were shaped into U-bend specimens as they underwent both plastic and elastic stresses. The specimens were then tested to determine the time required for cracks to initiate. The results of the experimental work showed that the main mode of failure was stress corrosion cracking initiated by the proven presence of chlorides, hydrogen sulfide, and water at elevated temperatures. Inconel 625 samples placed in the controlled environment showed better corrosion resistance as it took them an average of 56 days to initiate cracks, whereas it took an average of 24 days to initiate cracks in the stainless steel 316L samples. The scanning electron microscopy (SEM) micrographs showed that the cracks in the stainless steel 316L samples were longer, wider, and deeper compared to the cracks of Inconel 625. (Copyright copyright 2011 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  15. Corrosion studies of carbon steel under impinging jets of simulated slurries of neutralized current acid waste (NCAW) and neutralized cladding removal waste (NCRW)

    International Nuclear Information System (INIS)

    Smith, H.D.; Elmore, M.R.

    1992-01-01

    Plans for the disposal of radioactive liquid and solid wastes presently stored in double-shell tanks at the Hanford Site call for retrieval and processing of the waste to create forms suitable for permanent disposal. Waste will be retrieved from a tank using a submerged slurry pump in conjunction with one or more rotating slurry jet mixer pumps. Pacific Northwest Laboratory (PNL) has conducted tests using simulated waste slurries to assess the effects of a impinging slurry jet on the corrosion rate of the tank wall and floor, an action that could potentially compromise the tank's structural integrity. Corrosion processes were investigated on a laboratory scale with a simulated neutralized cladding removal waste (NCRW) slurry and in a subsequent test with simulated neutralized current acid waste (NCAW) slurry. The test slurries simulated the actual NCRW and NCAW both chemically and physically. The tests simulated those conditions expected to exist in the respective double-shell tanks during waste retrieval operations. Results of both tests indicate that, because of the action of the mixer pump slurry jets, the waste retrieval operations proposed for NCAW and NCRW will moderately accelerate corrosion of the tank wall and floor. Based on the corrosion of initially unoxidized test specimens, and the removal of corrosion products from those specimens, the maximum time-averaged corrosion rates of carbon steel in both waste simulants for the length of the test was ∼4 mil/yr. The protective oxide layer that exists in each storage tank is expected to inhibit corrosion of the carbon steel

  16. In situ AFM study of pitting corrosion and corrosion under strain on a 304L stainless steel

    International Nuclear Information System (INIS)

    Martin, F.A.; Cousty, J.; Masson, J-L.; Bataillon, C.

    2004-01-01

    Our study is centred on surface localised corrosion under strain of a standard stainless steel (304L). The interest we take in these corrosion phenomena is led by the general misunderstanding of its primary initiation steps. The goal of this study is to determine precisely the relationships between local geometrical defects (grain boundaries, dislocation lines, etc) or chemical defects (inclusions) with the preferential sites of corrosion on the strained material. By combining three techniques at the same time: Atomic Force Microscopy, an electrochemical cell and a traction plate, we can observe in situ the effect of localised stress and deformation on the sample surface exposed to a corrosive solution. We managed to build an original set-up compatible with all the requirements of these three different techniques. Furthermore, we prepared the surface of our sample as flat as possible to decrease at maximum the topographical noise in order to observe the smallest defect on the surface. By using a colloidal suspension of SiO 2 , we obtained surfaces with a typical corrugation (RMS) of about 1 A for areas of at least 1 μm 2 . Our experimental study has been organised in two primary investigations: - In situ study of the morphology evolution of the surface under a corrosive chloride solution (borate buffer with NaCl salt). The influence of time, NaCl concentration, and potential was investigated; - In situ exploration of a 304L strained surface. It revealed the first stages of the surface plastic evolutions like activation of sliding dislocations, materialized by parallel steps of about 2 nm high in the same grain. The secondary sliding plane systems were also noticeable for higher deformation rates. Recent results concerning in situ AFM observation of corroded surfaces under strain in a chloride media will be presented. (authors)

  17. In situ AFM study of pitting corrosion and corrosion under strain on a 304L stainless steel

    Energy Technology Data Exchange (ETDEWEB)

    Martin, F.A. [CEA de Saclay, DRECAM/SPCSI, 91191 Gif-sur-Yvette cedex (France); Cousty, J.; Masson, J-L. [CEA de Saclay, DRECAM/SPCSI, 91191 Gif-sur-Yvette cedex (France); Bataillon, C. [CEA de Saclay, DEN/DPC/LECA, 91191 Gif-sur-Yvette cedex (France)

    2004-07-01

    Our study is centred on surface localised corrosion under strain of a standard stainless steel (304L). The interest we take in these corrosion phenomena is led by the general misunderstanding of its primary initiation steps. The goal of this study is to determine precisely the relationships between local geometrical defects (grain boundaries, dislocation lines, etc) or chemical defects (inclusions) with the preferential sites of corrosion on the strained material. By combining three techniques at the same time: Atomic Force Microscopy, an electrochemical cell and a traction plate, we can observe in situ the effect of localised stress and deformation on the sample surface exposed to a corrosive solution. We managed to build an original set-up compatible with all the requirements of these three different techniques. Furthermore, we prepared the surface of our sample as flat as possible to decrease at maximum the topographical noise in order to observe the smallest defect on the surface. By using a colloidal suspension of SiO{sub 2}, we obtained surfaces with a typical corrugation (RMS) of about 1 A for areas of at least 1 {mu}m{sup 2}. Our experimental study has been organised in two primary investigations: - In situ study of the morphology evolution of the surface under a corrosive chloride solution (borate buffer with NaCl salt). The influence of time, NaCl concentration, and potential was investigated; - In situ exploration of a 304L strained surface. It revealed the first stages of the surface plastic evolutions like activation of sliding dislocations, materialized by parallel steps of about 2 nm high in the same grain. The secondary sliding plane systems were also noticeable for higher deformation rates. Recent results concerning in situ AFM observation of corroded surfaces under strain in a chloride media will be presented. (authors)

  18. Mobile evaporator corrosion test results

    International Nuclear Information System (INIS)

    Rozeveld, A.; Chamberlain, D.B.

    1997-05-01

    Laboratory corrosion tests were conducted on eight candidates to select a durable and cost-effective alloy for use in mobile evaporators to process radioactive waste solutions. Based on an extensive literature survey of corrosion data, three stainless steel alloys (304L, 316L, AL-6XN), four nickel-based alloys (825, 625, 690, G-30), and titanium were selected for testing. The corrosion tests included vapor phase, liquid junction (interface), liquid immersion, and crevice corrosion tests on plain and welded samples of candidate materials. Tests were conducted at 80 degrees C for 45 days in two different test solutions: a nitric acid solution. to simulate evaporator conditions during the processing of the cesium ion-exchange eluant and a highly alkaline sodium hydroxide solution to simulate the composition of Tank 241-AW-101 during evaporation. All of the alloys exhibited excellent corrosion resistance in the alkaline test solution. Corrosion rates were very low and localized corrosion was not observed. Results from the nitric acid tests showed that only 316L stainless steel did not meet our performance criteria. The 316L welded interface and crevice specimens had rates of 22.2 mpy and 21.8 mpy, respectively, which exceeds the maximum corrosion rate of 20 mpy. The other welded samples had about the same corrosion resistance as the plain samples. None of the welded samples showed preferential weld or heat-affected zone (HAZ) attack. Vapor corrosion was negligible for all alloys. All of the alloys except 316L exhibited either open-quotes satisfactoryclose quotes (2-20 mpy) or open-quotes excellentclose quotes (<2 mpy) corrosion resistance as defined by National Association of Corrosion Engineers. However, many of the alloys experienced intergranular corrosion in the nitric acid test solution, which could indicate a susceptibility to stress corrosion cracking (SCC) in this environment

  19. Improving the Corrosion Inhibitive Strength of Sodium Sulphite in Hydrogen Cyanide Solution Using Sodium Benzoate

    Directory of Open Access Journals (Sweden)

    Muhammed Olawale Hakeem AMUDA

    2008-12-01

    Full Text Available The improvement in the inhibitive strength of sodium sulphite on corrosion of mild steel in hydrogen cyanide by adding sodium benzoate in regulated volume was investigated using the fundamental weight loss measurement.500 ppm concentration inhibitive mixtures of sodium benzoate and sodium sulphite in three different volume ratios (5/15, 10/10, 15/5 were formulated and studied for corrosion rate in 200ml hydrogen cyanide fluid. Result obtained indicates that the corrosion rate of mild steel in hydrogen cyanide in the presence of sodium benzoate/sodium sulphite inhibitive mixtures range 0.322mmpy to 1.1269mmpy across the three volumetric ratios considered. The 15ml5ml sodium benzoatesodium sulphite mixture had the best average corrosion rate of 0.5123mmpy.The corrosion rate followed reducing pattern after the first 200 hours of immersion. The average corrosion rate in the sodium benzoate / sodium sulphite mixture is less than the rate in sodium sulphite and the mixture is only effective after long time exposure.It is concluded that adding sodium benzoate to sodium sulphite in the volumetric ratio 155ml improves the inhibitive strength of sodium sulphite on the corrosion of mild steel in hydrogen cyanide environment.

  20. Study of pitting corrosion in line-pipe steel under the influence of remanent magnetization

    Energy Technology Data Exchange (ETDEWEB)

    Espina-Hernandez, J H; Caleyo, F; Hallen, J M [Instituto Politecnico Nacional (IPN), Zacatenco (Mexico)

    2009-07-01

    The influence of remanent magnetization on pitting corrosion in line-pipe steels is studied. Pitting corrosion experiments have been carried out on samples of an API 5L grade 52 steel under a magnetization level of the same order of magnitude of the remanent magnetization in the pipeline wall after in-line inspection based on magnetic flux leakage. The samples were magnetized using rings of the same grade as the investigated steel. Immediately after magnetization, the investigated samples were subjected to pitting by immersing them in a solution containing dissolved Cl{sup -} and SO{sup 2-}{sub 4} and ions. The pitting experiments were conducted during a seven days period. The pit depth distribution and the maximum pit depth in each sample were recorded and used to conduct extreme value analyses of the pitting process in magnetized and non-magnetized control samples. The statistical assessment of the pitting corrosion data collected during this study shows that the magnetic field reduces the average depth of the pit population and also the extreme pit depth values that can be predicted from the maximum values observed in the magnetized samples in comparison with to the non-magnetized control samples. Scanning electron microscopy observations show that the magnetic field alters the pit morphology by increasing the pit mouth opening. (author)

  1. Corrosion pit depth extreme value prediction from limited inspection data

    International Nuclear Information System (INIS)

    Najjar, D.; Bigerelle, M.; Iost, A.; Bourdeau, L.; Guillou, D.

    2004-01-01

    Passive alloys like stainless steels are prone to localized corrosion in chlorides containing environments. The greater the depth of the localized corrosion phenomenon, the more dramatic the related damage that can lead to a structure weakening by fast perforation. In practical situations, because measurements are time consuming and expensive, the challenge is usually to predict the maximum pit depth that could be found in a large scale installation from the processing of a limited inspection data. As far as the parent distribution of pit depths is assumed to be of exponential type, the most successful method was found in the application of the statistical extreme-value analysis developed by Gumbel. This study aims to present a new and alternative methodology to the Gumbel approach with a view towards accurately estimating the maximum pit depth observed on a ferritic stainless steel AISI 409 subjected to an accelerated corrosion test (ECC1) used in automotive industry. This methodology consists in characterising and modelling both the morphology of pits and the statistical distribution of their depths from a limited inspection dataset. The heart of the data processing is based on the combination of two recent statistical methods that avoid making any choice about the type of the theoretical underlying parent distribution of pit depths: the Generalized Lambda Distribution (GLD) is used to model the distribution of pit depths and the Bootstrap technique to determine a confidence interval on the maximum pit depth. (authors)

  2. Numerical Evaluation of Averaging BDFT(bidirectional flow tube) Flow Meter on Applicability in the Fouling Condition

    International Nuclear Information System (INIS)

    Park, J. P.; Jeong, J. H.; Yuna, B. J.; Jerng, D. W.

    2013-01-01

    The results show that the averaging BDFT is a promising flow meter for the accurate measurement of flow rates in the fouling condition of the NPPs. A new instrumentation, an averaging BDFT, was proposed to measure the accurate flow rate under corrosion environment. In this study, to validate the applicability of the averaging BDFT on the fouling conditions, flow analyses using the CFD code were performed. Analyses results show that this averaging BDFT does not lose the measuring performance even under the corrosion environment. Therefore, it is expected that the averaging BDFT can replace the type flow meters for the feedwater pipe of steam generator of NPPs. Most of the NPPs adopt pressure difference type flow meters such as venturi and orifice meters for the measurement of feedwater flow rates to calculate reactor thermal power. However, corrosion products in the feedwater deposits on the flow meter as operating time goes. These effects lead to severe errors in the flow indication and then determination of reactor thermal power. The averaging BDFT has a potentiality to minimize this problem. Therefore, it is expected that the averaging BDFT can replace the type venturi meters for the feedwater pipe of steam generator of NPPs. The present work compares the amplification factor, K, based on CFD calculation against the K obtained from experiments in order to confirm whether a CFD code can be applicable to the evaluation of characteristic for the averaging BDFT. In addition to this, the simulations to take into account of fouling effect are also carried out by rough wall option

  3. Stochastic behavior of a cold standby system with maximum repair time

    Directory of Open Access Journals (Sweden)

    Ashish Kumar

    2015-09-01

    Full Text Available The main aim of the present paper is to analyze the stochastic behavior of a cold standby system with concept of preventive maintenance, priority and maximum repair time. For this purpose, a stochastic model is developed in which initially one unit is operative and other is kept as cold standby. There is a single server who visits the system immediately as and when required. The server takes the unit under preventive maintenance after a maximum operation time at normal mode if one standby unit is available for operation. If the repair of the failed unit is not possible up to a maximum repair time, failed unit is replaced by new one. The failure time, maximum operation time and maximum repair time distributions of the unit are considered as exponentially distributed while repair and maintenance time distributions are considered as arbitrary. All random variables are statistically independent and repairs are perfect. Various measures of system effectiveness are obtained by using the technique of semi-Markov process and RPT. To highlight the importance of the study numerical results are also obtained for MTSF, availability and profit function.

  4. Average inactivity time model, associated orderings and reliability properties

    Science.gov (United States)

    Kayid, M.; Izadkhah, S.; Abouammoh, A. M.

    2018-02-01

    In this paper, we introduce and study a new model called 'average inactivity time model'. This new model is specifically applicable to handle the heterogeneity of the time of the failure of a system in which some inactive items exist. We provide some bounds for the mean average inactivity time of a lifespan unit. In addition, we discuss some dependence structures between the average variable and the mixing variable in the model when original random variable possesses some aging behaviors. Based on the conception of the new model, we introduce and study a new stochastic order. Finally, to illustrate the concept of the model, some interesting reliability problems are reserved.

  5. Study of sulphate-reducing bacteria corrosion in the weld joint for API X-70 steel

    Energy Technology Data Exchange (ETDEWEB)

    Flores, J. E.; Patino-Carachure, C.; Alfonso, I.; Rodriguez, J. A.; Rosas, G.

    2012-11-01

    The corrosion behavior originated by sulfate-reducing bacteria (SRB) was studied in two regions of welded API X-70 steel pipeline. The studies were focused on base material (BM) and heat affected zone (HAZ), from the internal region of the pipe. SRB were extracted from oil and grown in a Postgate medium. Corrosion was evaluated at 60 degree centigrade for times between 5 and 64 days. Potentiodynamic polarization curves, obtained by electrochemical techniques, indicated surface activation at short times. Structural and morphological characterizations were carried out by scanning electron microscopy (SEM) and optical microscopy (OM). H{sub 2}S concentration and pH were also measured. Results showed an important increase in the corrosion damage up to 20 days, influenced by the SRB activity, which lead to a maximum of H{sub 2}S (pH minimum). It was found a localized corrosion attack in the HAZ in a higher quantity compared to BM; and the formation of a thin film on the steel surface, originated by corrosion products and bacterial activity. (Author) 15 refs.

  6. [The effect of bacteria reaction time on corrosion properties of Ni-Cr alloys pretreated with different proteins].

    Science.gov (United States)

    Qi, Han-quan; Zhang, Song-mei; Qian, Chao; Yuan-Li, Zheng

    2015-12-01

    To evaluate the corrosion properties of absorbed protein on the surface of NiCr alloys, and provide experimental base for corrosion resistance of dental casting alloys. NiCr alloy specimens were divided into 3 groups: one group was exposed to the artificial saliva(control group), and the other 2 groups were exposed to the artificial saliva with 1% bovine serum albumin(BSA), or 0.22% lysozyme(LSZ). Group of BSA and group of LSZ were the experimental group. Specimens in 3 groups were cultured in solution of Streptococcus mutans for 12 h, 24 h, 36 h and 48h, and investigated with electrochemical impedance spectroscopy measurement(EIS) and potentiodynamic polarization measurement(POT) to determine the corrosion resistance of the alloys. The data was analyzed with SPSS 17.0 software package. The results indicated that the corrosion resistance of both BSA group and LSZ group were higher than that of the control group (Pcorrosion resistance of BSA group and LSZ group had no significant difference (P>0.05), but was still higher than that of the control group. After 36 h culture time, the control group and the BSA group had no statistical difference in corrosion resistance (P>0.05), while the LSZ group had the poorest corrosion resistance. When the culture time extended to 48 h, the control group had a better corrosion resistance compared with the BAS group and the LSZ group(Pcorrosion properties than LSZ group. The potentiodynamic polarization curve and electrochemical impedance spectroscopy had similar results. The adhesion of BSA and LSZ on the surface of the NiCr alloys in the early time could effectively inhibit the corrosive effect of Streptococcus mutans. The LSZ had better effect than BSA. With the continuing role of bacteria and the consumption of the absorb protein, the corrosion resistance of NiCr alloys toward Streptococcus mutans becomes lower than the alloys without absorb protein, which demonstrated that the adhesion of protein would change the surface

  7. Corrosion Cost and Corrosion Map of Korea - Based on the Data from 2005 to 2010

    International Nuclear Information System (INIS)

    Kim, Y. S.; Lim, H. K.; Kim, J. J.; Hwang, W. S.; Park, Y. S.

    2011-01-01

    Corrosion of metallic materials occurs by the reaction with corrosive environment such as atmosphere, marine, soil, urban, high temperature etc. In general, reduction of thickness and cracking and degradation are resulted from corrosion. Corrosion in all industrial facilities and infrastructure causes large economic losses as well as a large number of accidents. Economic loss by corrosion has been reported to be nearly 1-6% of GNP or GDP. In order to reduce corrosion damage of industrial facilities, corrosion map as well as a systematic investigation of the loss of corrosion in each industrial sector is needed. The Corrosion Science Society of Korea in collaboration with 15 universities and institutes has started to survey on the cost of corrosion and corrosion map of Korea since 2005. This work presents the results of the survey on cost of corrosion by Uhlig, Hoar, and input-output methods, and the evaluation of atmospheric corrosion rate of carbon steel, weathering steel, galvanized steel, copper, and aluminum in Korea. The total corrosion cost was estimated in terms of the percentage of the GDP of industry sectors and the total GDP of Korea. According to the result of Input/output method, corrosion cost of Korea was calculated as 2.9% to GDP (2005). Time of wetness was shown to be categories 3 to 4 in all exposure areas. A definite seasonal difference was observed in Korea. In summer and fall, time of wetness was higher than in other seasons. Because of short exposure period (12 months), significant corrosion trends depending upon materials and exposure corrosion environments were not revealed even though increased mass loss and decreased corrosion rate by exposure time

  8. Flexible time domain averaging technique

    Science.gov (United States)

    Zhao, Ming; Lin, Jing; Lei, Yaguo; Wang, Xiufeng

    2013-09-01

    Time domain averaging(TDA) is essentially a comb filter, it cannot extract the specified harmonics which may be caused by some faults, such as gear eccentric. Meanwhile, TDA always suffers from period cutting error(PCE) to different extent. Several improved TDA methods have been proposed, however they cannot completely eliminate the waveform reconstruction error caused by PCE. In order to overcome the shortcomings of conventional methods, a flexible time domain averaging(FTDA) technique is established, which adapts to the analyzed signal through adjusting each harmonic of the comb filter. In this technique, the explicit form of FTDA is first constructed by frequency domain sampling. Subsequently, chirp Z-transform(CZT) is employed in the algorithm of FTDA, which can improve the calculating efficiency significantly. Since the signal is reconstructed in the continuous time domain, there is no PCE in the FTDA. To validate the effectiveness of FTDA in the signal de-noising, interpolation and harmonic reconstruction, a simulated multi-components periodic signal that corrupted by noise is processed by FTDA. The simulation results show that the FTDA is capable of recovering the periodic components from the background noise effectively. Moreover, it can improve the signal-to-noise ratio by 7.9 dB compared with conventional ones. Experiments are also carried out on gearbox test rigs with chipped tooth and eccentricity gear, respectively. It is shown that the FTDA can identify the direction and severity of the eccentricity gear, and further enhances the amplitudes of impulses by 35%. The proposed technique not only solves the problem of PCE, but also provides a useful tool for the fault symptom extraction of rotating machinery.

  9. In situ corrosion tests on HLW glass as part of a larger approach

    International Nuclear Information System (INIS)

    Van Iseghem, P.

    1997-01-01

    In-situ corrosion tests were performed on various candidate high-level waste glasses in the underground laboratory in clay underneath SCK x CEN. The tests exposed the glass samples directly to the Boom clay rock, for maximum durations of 7.5 years. We succeeded to interpret the corrosion data at 90 deg C in terms of dissolution mechanisms, and we concluded that the glass composition has a determining effect on the corrosion stability. The data from our in-situ tests were of high relevance for estimating the long-term behaviour of the glasses. The long-term in-situ tests provide corrosion data which show different trends than other corrosion tests, e.g. shorter duration tests in Boom clay, or tests in deionized water. The initial dissolution rate using MCC1 test at 90 deg C is about the same for the three glasses discussed, but the longest duration in Boom clay at 90 deg C shows a difference in mass loss of about 25 times. We finally present some ideas on how the corrosion tests can meet the needs, such as the modelling of the glass corrosion or providing input in the performance assessment. (author)

  10. Design and operation of thermal-convection loops for corrosion measurements in LiF--LiCl--LiBr

    International Nuclear Information System (INIS)

    Keiser, J.R.; DeVan, J.H.

    1979-01-01

    Using a most sophisticated design of a thermal-convection loop to study the corrosion behavior of type 316 stainless steel and the salt mixture LiF--LiCl--LiBr is reported. The corrosion rate is being determined as a function of time and temperature through weight change measurements. The maximum corrosion rate measured is about 20 μm/year on removable corrosion specimens. Controlled potential voltammetry has been found to be satisfactory and is being used to monitor the oxidation potential of the salt. Measurements demonstrate the effect on the oxidation potential of impurities introduced during specimen insertion, and techniques should show the effect of a lithium addition on the oxidation potential

  11. Simple experiments studying the catastrophic corrosion of stainless steel caused by sodium leaks

    International Nuclear Information System (INIS)

    Mathison, J.; Trevalion, P.A.; Hamer, A.N.

    1971-01-01

    Under certain conditions, small quantities of soditum escaping through a small hole may cause extensive corrosion and cratering on the outside of the containment in the vicinity of the leak and there is a possibility that this might lead to a major rupture of the containment. It is difficult to estimate such a corrosion rate by conducting post mortems after an incident because of the lack of precise information about times and temperatures. Simple sodium burning experiments have therefore been carried out in an attempt to provide rough quantitative data on the size of these corrosion rates. These showed that the average rate of corrosion of specimens of 18.8.1 stainless steel beneath a burning pool of sodium was of the order of 0.05 cm/hr at 600 ° C and 0.005 cm/hr at 400 ° C. Enhanced corrosion occurs at the periphery of the burning sodium. The rate of penetration will depend on the shape of the corrosion profile which exists in the affected surface. The times needed to penetrate different wall thicknesses of stainless steel pipework have been calculated for various corrosion profiles similar to those which have been observed after incidents in REML. (author)

  12. Savannah River Site Tank Cleaning: Corrosion Rate For One Versus Eight Percent Oxalic Acid Solution

    International Nuclear Information System (INIS)

    Ketusky, E.; Subramanian, K.

    2011-01-01

    Until recently, the use of oxalic acid for chemically cleaning the Savannah River Site (SRS) radioactive waste tanks focused on using concentrated 4 and 8-wt% solutions. Recent testing and research on applicable dissolution mechanisms have concluded that under appropriate conditions, dilute solutions of oxalic acid (i.e., 1-wt%) may be more effective. Based on the need to maximize cleaning effectiveness, coupled with the need to minimize downstream impacts, SRS is now developing plans for using a 1-wt% oxalic acid solution. A technology gap associated with using a 1-wt% oxalic acid solution was a dearth of suitable corrosion data. Assuming oxalic acid's passivation of carbon steel was proportional to the free oxalate concentration, the general corrosion rate (CR) from a 1-wt% solution may not be bound by those from 8-wt%. Therefore, after developing the test strategy and plan, the corrosion testing was performed. Starting with the envisioned process specific baseline solvent, a 1-wt% oxalic acid solution, with sludge (limited to Purex type sludge-simulant for this initial effort) at 75 C and agitated, the corrosion rate (CR) was determined from the measured weight loss of the exposed coupon. Environmental variations tested were: (a) Inclusion of sludge in the test vessel or assuming a pure oxalic acid solution; (b) acid solution temperature maintained at 75 or 45 C; and (c) agitation of the acid solution or stagnant. Application of select electrochemical testing (EC) explored the impact of each variation on the passivation mechanisms and confirmed the CR. The 1-wt% results were then compared to those from the 8-wt%. The immersion coupons showed that the maximum time averaged CR for a 1-wt% solution with sludge was less than 25-mils/yr for all conditions. For an agitated 8-wt% solution with sludge, the maximum time averaged CR was about 30-mils/yr at 50 C, and 86-mils/yr at 75 C. Both the 1-wt% and the 8-wt% testing demonstrated that if the sludge was removed from

  13. Measuring the corrosion rate of steel in concrete – effect of measurement technique, polarisation time and current

    DEFF Research Database (Denmark)

    Nygaard, Peter Vagn; Geiker, Mette Rica

    2012-01-01

    , are in some studies considered the main reasons for the variations. This paper presents an experimental study on the quantitative effect of polarisation time and current on the measured polarisation resistance – and thus the corrosion current density – of passively and actively corroding steel. Two...... electrochemical techniques often used in instruments for on-site corrosion rate measurements are investigated. On passively corroding reinforcement the measured polarisation resistance was for both techniques found to be highly affected by the polarisation time and current and no plateaus at either short or long...... rate for actively corroding steel. For both techniques guidelines for polarisation times and currents are given for (on-site) non-destructive corrosion rate measurements on reinforcement steel in concrete....

  14. The corrosion rate of copper in a bentonite test package measured with electric resistance sensors

    Energy Technology Data Exchange (ETDEWEB)

    Rosborg, Bo [Division of Surface and Corrosion Science, KTH, Stockholm (Sweden); Kosec, Tadeja; Kranjc, Andrej; Kuhar, Viljem; Legat, Andraz [Slovenian National Building and Civil Engineering Institute, Ljubljana (Slovenia)

    2012-12-15

    LOT1 test parcel A2 was exposed for six years in the Aespoe Hard Rock Laboratory, which offers a realistic environment for the conditions that will prevail in a deep repository for high-level radioactive waste disposal in Sweden. The test parcel contained copper electrodes for real-time corrosion monitoring in bentonite ring 36, where the temperature was 24 deg C, and copper coupons in bentonite rings 22 and 30, where the temperature was higher. After retrieval of the test parcel in January 2006, a bentonite test package consisting of bentonite rings 35 - 37 was placed in a container and sealed with a thick layer of paraffin. Later the same year new copper electrodes were installed in the test package. In January 2007 electric resistance (ER) sensors of pure copper with a thickness of 35 {mu}m were also installed in the test package mainly to facilitate the interpretation of the results from the real-time corrosion monitoring with electrochemical techniques. The ER measurements have shown that the corrosion rate of pure copper exposed in an oxic bentonite/ saline groundwater environment at room temperate decreases slowly with time to low but measurable values. The corrosion rates estimated from the regularly performed EIS measurements replicate the ER data. Thus, for this oxic environment in which copper acquires corrosion potentials of the order of 200 mV (SHE) or higher, electrochemical measurements provide believable data. Comparing the recorded ER data with an estimate of the average corrosion rate based on comparing cross-sections from exposed and protected sensor elements, it is obvious that the former overestimates the actual corrosion rate, which is understandable. It seems as if electrochemical measurements can provide a better estimate of the corrosion rate; however, this is quite dependent on the use of proper measuring frequencies and evaluation methods. In this respect ER measurements are more reliable. It has been shown that real-time corrosion

  15. The corrosion rate of copper in a bentonite test package measured with electric resistance sensors

    International Nuclear Information System (INIS)

    Rosborg, Bo; Kosec, Tadeja; Kranjc, Andrej; Kuhar, Viljem; Legat, Andraz

    2012-12-01

    LOT1 test parcel A2 was exposed for six years in the Aespoe Hard Rock Laboratory, which offers a realistic environment for the conditions that will prevail in a deep repository for high-level radioactive waste disposal in Sweden. The test parcel contained copper electrodes for real-time corrosion monitoring in bentonite ring 36, where the temperature was 24 deg C, and copper coupons in bentonite rings 22 and 30, where the temperature was higher. After retrieval of the test parcel in January 2006, a bentonite test package consisting of bentonite rings 35 - 37 was placed in a container and sealed with a thick layer of paraffin. Later the same year new copper electrodes were installed in the test package. In January 2007 electric resistance (ER) sensors of pure copper with a thickness of 35 μm were also installed in the test package mainly to facilitate the interpretation of the results from the real-time corrosion monitoring with electrochemical techniques. The ER measurements have shown that the corrosion rate of pure copper exposed in an oxic bentonite/ saline groundwater environment at room temperate decreases slowly with time to low but measurable values. The corrosion rates estimated from the regularly performed EIS measurements replicate the ER data. Thus, for this oxic environment in which copper acquires corrosion potentials of the order of 200 mV (SHE) or higher, electrochemical measurements provide believable data. Comparing the recorded ER data with an estimate of the average corrosion rate based on comparing cross-sections from exposed and protected sensor elements, it is obvious that the former overestimates the actual corrosion rate, which is understandable. It seems as if electrochemical measurements can provide a better estimate of the corrosion rate; however, this is quite dependent on the use of proper measuring frequencies and evaluation methods. In this respect ER measurements are more reliable. It has been shown that real-time corrosion

  16. Comparison of power pulses from homogeneous and time-average-equivalent models

    International Nuclear Information System (INIS)

    De, T.K.; Rouben, B.

    1995-01-01

    The time-average-equivalent model is an 'instantaneous' core model designed to reproduce the same three dimensional power distribution as that generated by a time-average model. However it has been found that the time-average-equivalent model gives a full-core static void reactivity about 8% smaller than the time-average or homogeneous models. To investigate the consequences of this difference in static void reactivity in time dependent calculations, simulations of the power pulse following a hypothetical large-loss-of-coolant accident were performed with a homogeneous model and compared with the power pulse from the time-average-equivalent model. The results show that there is a much smaller difference in peak dynamic reactivity than in static void reactivity between the two models. This is attributed to the fact that voiding is not complete, but also to the retardation effect of the delayed-neutron precursors on the dynamic flux shape. The difference in peak reactivity between the models is 0.06 milli-k. The power pulses are essentially the same in the two models, because the delayed-neutron fraction in the time-average-equivalent model is lower than in the homogeneous model, which compensates for the lower void reactivity in the time-average-equivalent model. (author). 1 ref., 5 tabs., 9 figs

  17. Asymptotic behaviour of time averages for non-ergodic Gaussian processes

    Science.gov (United States)

    Ślęzak, Jakub

    2017-08-01

    In this work, we study the behaviour of time-averages for stationary (non-ageing), but ergodicity-breaking Gaussian processes using their representation in Fourier space. We provide explicit formulae for various time-averaged quantities, such as mean square displacement, density, and analyse the behaviour of time-averaged characteristic function, which gives insight into rich memory structure of the studied processes. Moreover, we show applications of the ergodic criteria in Fourier space, determining the ergodicity of the generalised Langevin equation's solutions.

  18. A high speed digital signal averager for pulsed NMR

    International Nuclear Information System (INIS)

    Srinivasan, R.; Ramakrishna, J.; Ra agopalan, S.R.

    1978-01-01

    A 256-channel digital signal averager suitable for pulsed nuclear magnetic resonance spectroscopy is described. It implements 'stable averaging' algorithm and hence provides a calibrated display of the average signal at all times during the averaging process on a CRT. It has a maximum sampling rate of 2.5 μ sec and a memory capacity of 256 x 12 bit words. Number of sweeps is selectable through a front panel control in binary steps from 2 3 to 2 12 . The enhanced signal can be displayed either on a CRT or by a 3.5-digit LED display. The maximum S/N improvement that can be achieved with this instrument is 36 dB. (auth.)

  19. Corrosion inhibition of magnesium heated in wet air, by surface fluoridation

    International Nuclear Information System (INIS)

    Caillat, R.; Darras, R.; Leclercq, D.

    1960-01-01

    The maximum temperature (350 deg. C) of magnesium corrosion resistance in wet air may be raised to 490-500 deg. C by the formation of a superficial fluoride film. This can be obtained by two different ways: either by addition of hydrofluoric acid to the corroding medium in a very small proportion such as 0,003 mg/litre; at atmospheric pressure, or by dipping the magnesium in a dilute aqueous solution of nitric and hydrofluoric acids at room temperature before exposing it to the corroding atmosphere. In both cases the corrosion inhibition is effective over a very long time, even several thousand hours. (author) [fr

  20. Stochastic process corrosion growth models for pipeline reliability

    International Nuclear Information System (INIS)

    Bazán, Felipe Alexander Vargas; Beck, André Teófilo

    2013-01-01

    Highlights: •Novel non-linear stochastic process corrosion growth model is proposed. •Corrosion rate modeled as random Poisson pulses. •Time to corrosion initiation and inherent time-variability properly represented. •Continuous corrosion growth histories obtained. •Model is shown to precisely fit actual corrosion data at two time points. -- Abstract: Linear random variable corrosion models are extensively employed in reliability analysis of pipelines. However, linear models grossly neglect well-known characteristics of the corrosion process. Herein, a non-linear model is proposed, where corrosion rate is represented as a Poisson square wave process. The resulting model represents inherent time-variability of corrosion growth, produces continuous growth and leads to mean growth at less-than-one power of time. Different corrosion models are adjusted to the same set of actual corrosion data for two inspections. The proposed non-linear random process corrosion growth model leads to the best fit to the data, while better representing problem physics

  1. Corrosion of well casings in compressed air energy storage environments

    Energy Technology Data Exchange (ETDEWEB)

    Elmore, R.P.; Stottlemyre, J.A.

    1980-10-01

    The goal of this study was to determine corrosive effects of compressed air energy storage (CAES) environments on several well casing materials to aid in material selections. A literature search on corrosion behavior of well casing material in similar environments revealed that corrosion rates of 0.20 to 0.25 mm/y might be expected. This information was employed in designing the laboratory study. Unstressed electrically isolate samples of various carbon steels were autoclaved at varying humidities, temperatures, and exposure durations to simulate anticipated environments in the well bore during CAES operation. All compressed air tests were run at 12.1 MPa. Temperatures varied from 323/sup 0/K to 573/sup 0/K, and humidity varied from 100% to completely dry air. The effects of salts in the humidified air were also studied. Results indicated that typical well casings of carbon steel as used in oil, gas, and water production wells adequately withstand the anticipated CAES reservoir environment. An acceptable corrosion rate arrived at by these laboratory simulations was between 0.0015 and 0.15 mm/y. Corrosion was caused by metal oxidation that formed a protective scale of iron oxide. Higher temperatures, humidity rates, or salinity content of the humid air increased corrosion. Corrosion also increased on a metal coupon in contact with a sandstone sample, possibly due to crevice corrosion. For each of these factors either singularly or collectively, the increased corrosion rates were still acceptable with the maximum measured at 0.15 mm/y. When coupons were reused in an identical test, the corrosion rates increased beyond the anticipated values that had been determined by extrapolation from one-time runs. Fine cracking of the protective scale probably occurred due to thermal variations, resulting in increased corrosion rates and a greater potential for particulates, which could plug the reservoir.

  2. Is average daily travel time expenditure constant? In search of explanations for an increase in average travel time.

    NARCIS (Netherlands)

    van Wee, B.; Rietveld, P.; Meurs, H.

    2006-01-01

    Recent research suggests that the average time spent travelling by the Dutch population has increased over the past decades. However, different data sources show different levels of increase. This paper explores possible causes for this increase. They include a rise in incomes, which has probably

  3. Multiperiod Maximum Loss is time unit invariant.

    Science.gov (United States)

    Kovacevic, Raimund M; Breuer, Thomas

    2016-01-01

    Time unit invariance is introduced as an additional requirement for multiperiod risk measures: for a constant portfolio under an i.i.d. risk factor process, the multiperiod risk should equal the one period risk of the aggregated loss, for an appropriate choice of parameters and independent of the portfolio and its distribution. Multiperiod Maximum Loss over a sequence of Kullback-Leibler balls is time unit invariant. This is also the case for the entropic risk measure. On the other hand, multiperiod Value at Risk and multiperiod Expected Shortfall are not time unit invariant.

  4. 75 FR 18153 - Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2010-04-09

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Extension of Time Limit for Preliminary Results of... countervailing duty order on corrosion-resistant carbon steel flat products (CORE) from Korea. See Countervailing...

  5. 77 FR 16810 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2012-03-22

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limit for Preliminary Results of... Register the countervailing duty order on corrosion-resistant carbon steel flat products (CORE) from Korea...

  6. 76 FR 20954 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2011-04-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limit for Preliminary Results of... Register the countervailing duty order on corrosion-resistant carbon steel flat products (CORE) from Korea...

  7. Space-Time Chip Equalization for Maximum Diversity Space-Time Block Coded DS-CDMA Downlink Transmission

    Directory of Open Access Journals (Sweden)

    Petré Frederik

    2004-01-01

    Full Text Available In the downlink of DS-CDMA, frequency-selectivity destroys the orthogonality of the user signals and introduces multiuser interference (MUI. Space-time chip equalization is an efficient tool to restore the orthogonality of the user signals and suppress the MUI. Furthermore, multiple-input multiple-output (MIMO communication techniques can result in a significant increase in capacity. This paper focuses on space-time block coding (STBC techniques, and aims at combining STBC techniques with the original single-antenna DS-CDMA downlink scheme. This results into the so-called space-time block coded DS-CDMA downlink schemes, many of which have been presented in the past. We focus on a new scheme that enables both the maximum multiantenna diversity and the maximum multipath diversity. Although this maximum diversity can only be collected by maximum likelihood (ML detection, we pursue suboptimal detection by means of space-time chip equalization, which lowers the computational complexity significantly. To design the space-time chip equalizers, we also propose efficient pilot-based methods. Simulation results show improved performance over the space-time RAKE receiver for the space-time block coded DS-CDMA downlink schemes that have been proposed for the UMTS and IS-2000 W-CDMA standards.

  8. Dictionary corrosion and corrosion control

    International Nuclear Information System (INIS)

    1985-01-01

    This dictionary has 13000 entries in both languages. Keywords and extensive accompanying information simplify the choice of word for the user. The following topics are covered: Theoretical principles of corrosion; Corrosion of the metals and alloys most frequently used in engineering. Types of corrosion - (chemical-, electro-chemical, biological corrosion); forms of corrosion (superficial, pitting, selective, intercrystalline and stress corrosion; vibrational corrosion cracking); erosion and cavitation. Methods of corrosion control (material selection, temporary corrosion protection media, paint and plastics coatings, electro-chemical coatings, corrosion prevention by treatment of the corrosive media); Corrosion testing methods. (orig./HP) [de

  9. Parameterization of Time-Averaged Suspended Sediment Concentration in the Nearshore

    Directory of Open Access Journals (Sweden)

    Hyun-Doug Yoon

    2015-11-01

    Full Text Available To quantify the effect of wave breaking turbulence on sediment transport in the nearshore, the vertical distribution of time-averaged suspended sediment concentration (SSC in the surf zone was parameterized in terms of the turbulent kinetic energy (TKE at different cross-shore locations, including the bar crest, bar trough, and inner surf zone. Using data from a large-scale laboratory experiment, a simple relationship was developed between the time-averaged SSC and the time-averaged TKE. The vertical variation of the time-averaged SSC was fitted to an equation analogous to the turbulent dissipation rate term. At the bar crest, the proposed equation was slightly modified to incorporate the effect of near-bed sediment processes and yielded reasonable agreement. This parameterization yielded the best agreement at the bar trough, with a coefficient of determination R2 ≥ 0.72 above the bottom boundary layer. The time-averaged SSC in the inner surf zone showed good agreement near the bed but poor agreement near the water surface, suggesting that there is a different sedimentation mechanism that controls the SSC in the inner surf zone.

  10. Effects of chitosan inhibitor on the electrochemical corrosion behavior of 2205 duplex stainless steel

    Science.gov (United States)

    Yang, Se-fei; Wen, Ying; Yi, Pan; Xiao, Kui; Dong, Chao-fang

    2017-11-01

    The effects of chitosan inhibitor on the corrosion behavior of 2205 duplex stainless steel were studied by electrochemical measurements, immersion tests, and stereology microscopy. The influences of immersion time, temperature, and chitosan concentration on the corrosion inhibition performance of chitosan were investigated. The optimum parameters of water-soluble chitosan on the corrosion inhibition performance of 2205 duplex stainless steel were also determined. The water-soluble chitosan showed excellent corrosion inhibition performance on the 2205 duplex stainless steel. Polarization curves demonstrated that chitosan acted as a mixed-type inhibitor. When the stainless steel specimen was immersed in the 0.2 g/L chitosan solution for 4 h, a dense and uniform adsorption film covered the sample surface and the inhibition efficiency (IE) reached its maximum value. Moreover, temperature was found to strongly influence the corrosion inhibition of chitosan; the inhibition efficiency gradually decreased with increasing temperature. The 2205 duplex stainless steel specimen immersed in 0.4 g/L water-soluble chitosan at 30°C displayed the best corrosion inhibition among the investigated specimens. Moreover, chitosan decreased the corrosion rate of the 2205 duplex stainless steel in an FeCl3 solution.

  11. 77 FR 25405 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2012-04-30

    ... antidumping duty order on corrosion-resistant carbon steel flat products from the Republic of Korea, covering... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limit for the Preliminary Results of...

  12. 76 FR 21332 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2011-04-15

    ... antidumping duty order on corrosion-resistant carbon steel flat products from the Republic of Korea, covering... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limits for the Preliminary Results of...

  13. 75 FR 25841 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Science.gov (United States)

    2010-05-10

    ... antidumping duty order on corrosion-resistant carbon steel flat products from the Republic of Korea, covering... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limits for the Preliminary Results of...

  14. An Influence Study of Hydrogen Evolution Characteristics on the Negative Strap Corrosion of Lead Acid Battery

    Directory of Open Access Journals (Sweden)

    Zhong Guobin

    2015-01-01

    Full Text Available Negative strap corrosion is an important reason for the failure of valve regulated lead acid battery. This paper selected the Pb-Sb alloy material and Pb-Sn alloy material, made an investigation on the negative corrosion resistance and hydrogen evolution of these two alloy materials by scanning electron microscope analysis, metallographic analysis, chemical study and linear sweep voltammetry, and discussed the influence of lead alloy hydrogen evolution on the negative strap corrosion. The results showed that the hydrogen evolution reaction rates of the alloys had an impact on the corrosion areas with the maximum thickness of the alloys and the depth of corrosion layers. Greater hydrogen evolution reaction rate can lead to shorter distance between the corrosion area with the maximum thickness and the liquid level; whereas the greater corrosion layer thickness can bring aggravated risk of negative strap corrosion failure.

  15. Assessment of multi-phase movements in a gas-gathering pipeline and the relevance to on-line, real-time corrosion monitoring and inhibitor injection

    Energy Technology Data Exchange (ETDEWEB)

    Baker, M.A.; Asperger, R.G.

    1988-01-01

    A study was conducted to determine the time required for aqueous fluid to travel 100 miles (160 km) from an offshore platform in the Gulf of Mexico to landfill. If this time is short, the corrosivity of the water at landfall may be used as the basis for setting the offshore corrosion inhibitor injection rates. But, for this particular system, the traveling time was found to be long, greater than 65 days. Therefore, the corrosivity as measured on-shore can not be used for online, real-time adjustments of the offshore, corrosion inhibitor chemical pumps.

  16. Performance evaluation of corrosion probes in simulated WVNS tank 8D-2 waste: WVNS tank farm process support

    International Nuclear Information System (INIS)

    Elmore, M.R.

    1994-07-01

    Five corrosion probes were received from West Valley Nuclear Services for evaluation in simulated tank 8D-2 3rd-stage sludge wash slurry. The same waste slurry simulated was also used in a series of ongoing corrosion studies assessing the effects of in-tank sludge washing on the integrity of tank 8D-2. Two of the corrosion probes were installed in the coupon corrosion test vessels operating at ∼150 degrees F to compare performance of the probes with that observed by coupon tests conducted in the same vessels. Corrosion rate data calculated from electrical resistance measurements of the corrosion probes were evaluated for this study using two slightly different approaches. One approach uses the total length of exposure of the probe to give a ''time-averaged'' value of the corrosion rate. The other approach uses a shorter period of time (relative to the length of the test) in the calculation of corrosion rate, and is referred to as the ''instantaneous'' rate. The interpretation of the probe data and the implications of corrosion rates calculated with either of these methods are discussed in this report

  17. Chitosan coatings crosslinked with genipin for corrosion protection of AZ31 magnesium alloy sheets.

    Science.gov (United States)

    de Y Pozzo, Ludmila; da Conceição, Thiago F; Spinelli, Almir; Scharnagl, Nico; Pires, Alfredo T N

    2018-02-01

    In this study, coatings of chitosan crosslinked with genipin were prepared on sheets of AZ31 magnesium alloy and their corrosion protection properties were characterized by means of potentiodynamic polarization and electrochemical impedance spectroscopy (EIS). The coatings were also characterized by means of FTIR and XPS. It was observed that the crosslinking process decreases the corrosion current and shifts the corrosion potential of the alloy to less negative values. The EIS analysis demonstrated that the crosslinking process increases the maximum impedance after short and long exposure times. The superior performance of the crosslinked coatings is related to a lower degree of swelling, as observed in the swelling tests carried out on free-standing films. Copyright © 2017 Elsevier Ltd. All rights reserved.

  18. Corrosion Resistant FBG-Based Quasi-Distributed Sensor for Crude Oil Tank Dynamic Temperature Profile Monitoring

    Science.gov (United States)

    da Silva Marques, Rogério; Prado, Adilson Ribeiro; da Costa Antunes, Paulo Fernando; de Brito André, Paulo Sérgio; Ribeiro, Moisés R. N.; Frizera-Neto, Anselmo; Pontes, Maria José

    2015-01-01

    This article presents a corrosion resistant, maneuverable, and intrinsically safe fiber Bragg grating (FBG)-based temperature optical sensor. Temperature monitoring is a critical activity for the oil and gas industry. It typically involves acquiring the desired parameters in a hazardous and corrosive environment. The use of polytetrafluoroethylene (PTFE) was proposed as a means of simultaneously isolating the optical fiber from the corrosive environment and avoiding undesirable mechanical tensions on the FBGs. The presented sensor head is based on multiple FBGs inscribed in a lengthy single mode fiber. The sensor presents an average thermal sensitivity of 8.82 ± 0.09 pm/°C, resulting in a typical temperature resolution of ~0.1 °C and an average time constant value of 6.25 ± 0.08 s. Corrosion and degradation resistance were verified by infrared spectroscopy and scanning electron microscopy during 90 days exposure to high salinity crude oil samples. The developed sensor was tested in a field pilot test, mimicking the operation of an inland crude tank, demonstrating its abilities to dynamically monitor temperature profile. PMID:26690166

  19. Corrosion management in nuclear industry

    International Nuclear Information System (INIS)

    Kamachi Mudali, U.

    2012-01-01

    Corrosion is a major degradation mechanism of metals and alloys which significantly affects the global economy with an average loss of 3.5% of GDP of several countries in many important industrial sectors including chemical, petrochemical, power, oil, refinery, fertilizer etc. The demand for higher efficiency and achieving name plate capacity, in addition to ever increasing temperatures, pressures and complexities in equipment geometry of industrial processes, necessitate utmost care in adopting appropriate corrosion management strategies in selecting, designing, fabricating and utilising various materials and coatings for engineering applications in industries. Corrosion control and prevention is an important focus area as the savings achieved from practicing corrosion control and prevention would bring significant benefits to the industry. Towards this, advanced corrosion management strategies starting from design, manufacturing, operation, maintenance, in-service inspection and online monitoring are essential. At the Indira Gandhi Centre for Atomic Research (IGCAR) strategic corrosion management efforts have been pursued in order to provide solutions to practical problems emerging in the plants, in addition to innovative efforts to provide insight into mechanism and understanding of corrosion of various engineering materials and coatings. In this presentation the author highlights how the nuclear industry benefited from the practical approach to successful corrosion management, particularly with respect to fast breeder reactor programme involving both reactor and associated reprocessing plants. (author)

  20. Biocide-mediated corrosion of coiled tubing.

    Science.gov (United States)

    Sharma, Mohita; An, Dongshan; Liu, Tao; Pinnock, Tijan; Cheng, Frank; Voordouw, Gerrit

    2017-01-01

    Coiled tubing corrosion was investigated for 16 field water samples (S5 to S20) from a Canadian shale gas field. Weight loss corrosion rates of carbon steel beads incubated with these field water samples averaged 0.2 mm/yr, but injection water sample S19 had 1.25±0.07 mm/yr. S19 had a most probable number of zero acid-producing bacteria and incubation of S19 with carbon steel beads or coupons did not lead to big changes in microbial community composition. In contrast other field water samples had most probable numbers of APB of 102/mL to 107/mL and incubation of these field water samples with carbon steel beads or coupons often gave large changes in microbial community composition. HPLC analysis indicated that all field water samples had elevated concentrations of bromide (average 1.6 mM), which may be derived from bronopol, which was used as a biocide. S19 had the highest bromide concentration (4.2 mM) and was the only water sample with a high concentration of active bronopol (13.8 mM, 2760 ppm). Corrosion rates increased linearly with bronopol concentration, as determined by weight loss of carbon steel beads, for experiments with S19, with filtered S19 and with bronopol dissolved in defined medium. This indicated that the high corrosion rate found for S19 was due to its high bronopol concentration. The corrosion rate of coiled tubing coupons also increased linearly with bronopol concentration as determined by electrochemical methods. Profilometry measurements also showed formation of multiple pits on the surface of coiled tubing coupon with an average pit depth of 60 μm after 1 week of incubation with 1 mM bronopol. At the recommended dosage of 100 ppm the corrosiveness of bronopol towards carbon steel beads was modest (0.011 mm/yr). Higher concentrations, resulting if biocide is added repeatedly as commonly done in shale gas operations, are more corrosive and should be avoided. Overdosing may be avoided by assaying the presence of residual biocide by HPLC

  1. Recorded corrosion rates on copper electrodes in the Prototype Repository at the Aespoe HRL

    Energy Technology Data Exchange (ETDEWEB)

    Rosborg, Bo [Rosborg Consulting, Nykoeping (Sweden)

    2013-04-15

    Real-time corrosion monitoring by means of electrochemical methods has been applied in an effort to measure corrosion rates of pure copper in the Prototype Repository at the Aspo Hard Rock Laboratory. Copper electrodes were installed in bentonite blocks on top of the electrically heated copper canisters in two deposition holes (dh). Three nominally identical cylindrical copper electrodes were installed in dh 1 and another three in dh 5 a few days before the heat was turned on to the canisters in September 2001 and in May 2003 respectively. The temperature of the copper electrodes has been around 30 deg C in dh 1 and somewhat below 35 deg C in dh 5. Real-time corrosion monitoring for both electrode setups was first applied in January 2004, and then periodically in 2005, 2006, 2008, and most recently in the end of 2010 just before work to open the outer section of the Prototype Repository was started. The recorded corrosion rates fall below 1.3 {mu}m/year (using a default value of n=2 in the software to convert the corrosion current density to a penetration rate by means of Faraday's law, and with no correction applied for the used measuring frequency of 0.01 Hz; also disregarding highly scattered data obtained for the copper electrodes in dh 1 during 2010). While the recorded rates on the electrodes in dh 5 first increased from about 0.2 {mu}m/year in 2004 up to a maximum of 1.3 {mu}m/year a year later (the drainage of the inner and outer sections was temporary closed in the end of 2004), and then gradually decreased to 0.7 {mu}m/year in the end of 2010, the recorded rates on the electrodes in dh 1 show a quite different picture. The recorded rates fall in the range 0.4-0.7 {mu}m/year and do not reflect any obvious decrease. However, it is anticipated that a similar time dependence as observed for the electrodes in dh 5 could have been present early on in the exposure; the electrodes were installed in 2001 but the first measurements were performed in 2004. Also

  2. Recorded corrosion rates on copper electrodes in the Prototype Repository at the Aespoe HRL

    International Nuclear Information System (INIS)

    Rosborg, Bo

    2013-04-01

    Real-time corrosion monitoring by means of electrochemical methods has been applied in an effort to measure corrosion rates of pure copper in the Prototype Repository at the Aspo Hard Rock Laboratory. Copper electrodes were installed in bentonite blocks on top of the electrically heated copper canisters in two deposition holes (dh). Three nominally identical cylindrical copper electrodes were installed in dh 1 and another three in dh 5 a few days before the heat was turned on to the canisters in September 2001 and in May 2003 respectively. The temperature of the copper electrodes has been around 30 deg C in dh 1 and somewhat below 35 deg C in dh 5. Real-time corrosion monitoring for both electrode setups was first applied in January 2004, and then periodically in 2005, 2006, 2008, and most recently in the end of 2010 just before work to open the outer section of the Prototype Repository was started. The recorded corrosion rates fall below 1.3 μm/year (using a default value of n=2 in the software to convert the corrosion current density to a penetration rate by means of Faraday's law, and with no correction applied for the used measuring frequency of 0.01 Hz; also disregarding highly scattered data obtained for the copper electrodes in dh 1 during 2010). While the recorded rates on the electrodes in dh 5 first increased from about 0.2 μm/year in 2004 up to a maximum of 1.3 μm/year a year later (the drainage of the inner and outer sections was temporary closed in the end of 2004), and then gradually decreased to 0.7 μm/year in the end of 2010, the recorded rates on the electrodes in dh 1 show a quite different picture. The recorded rates fall in the range 0.4-0.7 μm/year and do not reflect any obvious decrease. However, it is anticipated that a similar time dependence as observed for the electrodes in dh 5 could have been present early on in the exposure; the electrodes were installed in 2001 but the first measurements were performed in 2004. Also, saturation of

  3. Response of reinforced concrete structures to macrocell corrosion of reinforcements. Part I: Before propagation of microcracks via an analytical approach

    International Nuclear Information System (INIS)

    Kiani, Keivan; Shodja, Hossein M.

    2011-01-01

    Highlights: ► Response of RC structures to macrocell corrosion of a rebar is studied analytically. ► The problem is solved prior to the onset of microcrack propagation. ► Suitable Love's potential functions are used to study the steel-rust-concrete media. ► The role of crucial factors on the time of onset of concrete cracking is examined. ► The effect of vital factors on the maximum radial stress of concrete is explored. - Abstract: Assessment of the macrocell corrosion which deteriorates reinforced concrete (RC) structures have attracted the attention of many researchers during recent years. In this type of rebar corrosion, the reduction in cross-section of the rebar is significantly accelerated due to the large ratio of the cathode's area to the anode's area. In order to examine the problem, an analytical solution is proposed for prediction of the response of the RC structure from the time of steel depassivation to the stage just prior to the onset of microcrack propagation. To this end, a circular cylindrical RC member under axisymmetric macrocell corrosion of the reinforcement is considered. Both cases of the symmetric and asymmetric rebar corrosion along the length of the anode zone are studied. According to the experimentally observed data, corrosion products are modeled as a thin layer with a nonlinear stress–strain relation. The exact expressions of the elastic fields associated with the steel, and concrete media are obtained using Love's potential function. By imposing the boundary conditions, the resulting set of nonlinear equations are solved in each time step by Newton's method. The effects of the key parameters which have dominating role in the time of the onset of concrete cracking and maximum radial stress field of the concrete have been examined.

  4. Extending the maximum operation time of the MNSR reactor.

    Science.gov (United States)

    Dawahra, S; Khattab, K; Saba, G

    2016-09-01

    An effective modification to extend the maximum operation time of the Miniature Neutron Source Reactor (MNSR) to enhance the utilization of the reactor has been tested using the MCNP4C code. This modification consisted of inserting manually in each of the reactor inner irradiation tube a chain of three polyethylene-connected containers filled of water. The total height of the chain was 11.5cm. The replacement of the actual cadmium absorber with B(10) absorber was needed as well. The rest of the core structure materials and dimensions remained unchanged. A 3-D neutronic model with the new modifications was developed to compare the neutronic parameters of the old and modified cores. The results of the old and modified core excess reactivities (ρex) were: 3.954, 6.241 mk respectively. The maximum reactor operation times were: 428, 1025min and the safety reactivity factors were: 1.654 and 1.595 respectively. Therefore, a 139% increase in the maximum reactor operation time was noticed for the modified core. This increase enhanced the utilization of the MNSR reactor to conduct a long time irradiation of the unknown samples using the NAA technique and increase the amount of radioisotope production in the reactor. Copyright © 2016 Elsevier Ltd. All rights reserved.

  5. Computing the Maximum Detour of a Plane Graph in Subquadratic Time

    DEFF Research Database (Denmark)

    Wulff-Nilsen, Christian

    Let G be a plane graph where each edge is a line segment. We consider the problem of computing the maximum detour of G, defined as the maximum over all pairs of distinct points p and q of G of the ratio between the distance between p and q in G and the distance |pq|. The fastest known algorithm f...... for this problem has O(n^2) running time. We show how to obtain O(n^{3/2}*(log n)^3) expected running time. We also show that if G has bounded treewidth, its maximum detour can be computed in O(n*(log n)^3) expected time....

  6. Improving pitting corrosion resistance of aluminum by anodizing process

    International Nuclear Information System (INIS)

    John, P.; Khan, I.U.

    2013-01-01

    Summary: Anodizing of aluminum was studied in sulphuric/citric/boric acid electrolyte system to improve pitting corrosion resistance. Maximum oxide film thickness was obtained using 5% sulphuric acid, 3% citric acid and 0.5% boric acid electrolyte composition. The corrosion resistance of aluminum sample was determined to find the effectiveness of oxide coating by potentiodynamic polarization test. The surface morphology of aluminum samples was investigated using scanning electron microscope (SEM) before and after corrosion test. It was found that the coated aluminum sample obtained by anodizing in sulphuric/citric/boric acid electrolyte system exhibited better pitting corrosion resistance with no significant difference in surface morphology. (author)

  7. Time-dependent angularly averaged inverse transport

    International Nuclear Information System (INIS)

    Bal, Guillaume; Jollivet, Alexandre

    2009-01-01

    This paper concerns the reconstruction of the absorption and scattering parameters in a time-dependent linear transport equation from knowledge of angularly averaged measurements performed at the boundary of a domain of interest. Such measurement settings find applications in medical and geophysical imaging. We show that the absorption coefficient and the spatial component of the scattering coefficient are uniquely determined by such measurements. We obtain stability results on the reconstruction of the absorption and scattering parameters with respect to the measured albedo operator. The stability results are obtained by a precise decomposition of the measurements into components with different singular behavior in the time domain

  8. A maximum principle for time dependent transport in systems with voids

    International Nuclear Information System (INIS)

    Schofield, S.L.; Ackroyd, R.T.

    1996-01-01

    A maximum principle is developed for the first-order time dependent Boltzmann equation. The maximum principle is a generalization of Schofield's κ(θ) principle for the first-order steady state Boltzmann equation, and provides a treatment of time dependent transport in systems with void regions. The formulation comprises a direct least-squares minimization allied with a suitable choice of bilinear functional, and gives rise to a maximum principle whose functional is free of terms that have previously led to difficulties in treating void regions. (Author)

  9. An overview of erosion corrosion models and reliability assessment for corrosion defects in piping system

    International Nuclear Information System (INIS)

    Srividya, A.; Suresh, H.N.; Verma, A.K.; Gopika, V.; Santosh

    2006-01-01

    Piping systems are part of passive structural elements in power plants. The analysis of the piping systems and their quantification in terms of failure probability is of utmost importance. The piping systems may fail due to various degradation mechanisms like thermal fatigue, erosion-corrosion, stress corrosion cracking and vibration fatigue. On examination of previous results, erosion corrosion was more prevalent and wall thinning is a time dependent phenomenon. The paper is intended to consolidate the work done by various investigators on erosion corrosion in estimating the erosion corrosion rate and reliability predictions. A comparison of various erosion corrosion models is made. The reliability predictions based on remaining strength of corroded pipelines by wall thinning is also attempted. Variables in the limit state functions are modelled using normal distributions and Reliability assessment is carried out using some of the existing failure pressure models. A steady state corrosion rate is assumed to estimate the corrosion defect and First Order Reliability Method (FORM) is used to find the probability of failure associated with corrosion defects over time using the software for Component Reliability evaluation (COMREL). (author)

  10. Maximum Likelihood Blind Channel Estimation for Space-Time Coding Systems

    Directory of Open Access Journals (Sweden)

    Hakan A. Çırpan

    2002-05-01

    Full Text Available Sophisticated signal processing techniques have to be developed for capacity enhancement of future wireless communication systems. In recent years, space-time coding is proposed to provide significant capacity gains over the traditional communication systems in fading wireless channels. Space-time codes are obtained by combining channel coding, modulation, transmit diversity, and optional receive diversity in order to provide diversity at the receiver and coding gain without sacrificing the bandwidth. In this paper, we consider the problem of blind estimation of space-time coded signals along with the channel parameters. Both conditional and unconditional maximum likelihood approaches are developed and iterative solutions are proposed. The conditional maximum likelihood algorithm is based on iterative least squares with projection whereas the unconditional maximum likelihood approach is developed by means of finite state Markov process modelling. The performance analysis issues of the proposed methods are studied. Finally, some simulation results are presented.

  11. Furniture Rack Corrosion Coupon Surveillance - 2012 Update

    International Nuclear Information System (INIS)

    Mickalonis, J. I.; Murphy, T. R.; Berry, C. J.

    2012-01-01

    Under the L Basin corrosion surveillance program furniture rack coupons immersed for 14 years (FY2009 coupons) and 16 years (FY2011 coupons) were analyzed and the results trended with coupons exposed for shorter times. In addition, a section harvested from an actual furniture rack that was immersed for 14 years was analyzed for pitting in the weld and heat-affected-zone (HAZ) regions. The L Basin operations maintained very good water quality over the entire immersion period for these samples. These results for FY2009 and FY2011 coupons showed that the average pit depths for the 6061 and 6063 base metal are 1 and 2 mils, respectively, while those for the weld and HAZ are 3 and 4 mils, respectively. The results for the weld and HAZ regions are similar to coupons removed during the period of FY2003 to FY2007. These similarities indicate that the pit development occurred quickly followed by slow kinetics of increase in pit depth. For the actual furniture rack sample average pits of 5 and 2 mils were measured for the HAZ and weld, respectively. These results demonstrate that pitting corrosion of the aluminum furniture racks used to support the spent fuel occurs in waters of good quality. The corrosion kinetics or pit depth growth rate is much less that 1 mil/year, and would not impact long-term use of this material system for fuel storage racks in L Basin if good water quality is maintained

  12. Time-averaged MSD of Brownian motion

    OpenAIRE

    Andreanov, Alexei; Grebenkov, Denis

    2012-01-01

    We study the statistical properties of the time-averaged mean-square displacements (TAMSD). This is a standard non-local quadratic functional for inferring the diffusion coefficient from an individual random trajectory of a diffusing tracer in single-particle tracking experiments. For Brownian motion, we derive an exact formula for the Laplace transform of the probability density of the TAMSD by mapping the original problem onto chains of coupled harmonic oscillators. From this formula, we de...

  13. Evaluation of local corrosion life by statistical method

    International Nuclear Information System (INIS)

    Kato, Shunji; Kurosawa, Tatsuo; Takaku, Hiroshi; Kusanagi, Hideo; Hirano, Hideo; Kimura, Hideo; Hide, Koichiro; Kawasaki, Masayuki

    1987-01-01

    In this paper, for the purpose of achievement of life extension of light water reactor, we examined the evaluation of local corrosion by satistical method and its application of nuclear power plant components. There are many evaluation examples of maximum cracking depth of local corrosion by dowbly exponential distribution. This evaluation method has been established. But, it has not been established that we evaluate service lifes of construction materials by satistical method. In order to establish of service life evaluation by satistical method, we must strive to collect local corrosion dates and its analytical researchs. (author)

  14. Archaeological analogs and corrosion; Analogues archeologiques et corrosion

    Energy Technology Data Exchange (ETDEWEB)

    David, D

    2008-07-01

    In the framework of the high level and long life radioactive wastes disposal deep underground, the ANDRA built a research program on the material corrosion. In particular they aim to design containers for a very long time storage. Laboratory experiments are in progress and can be completed by the analysis of metallic archaeological objects and their corrosion after hundred years. (A.L.B.)

  15. Fitting a function to time-dependent ensemble averaged data

    DEFF Research Database (Denmark)

    Fogelmark, Karl; Lomholt, Michael A.; Irbäck, Anders

    2018-01-01

    Time-dependent ensemble averages, i.e., trajectory-based averages of some observable, are of importance in many fields of science. A crucial objective when interpreting such data is to fit these averages (for instance, squared displacements) with a function and extract parameters (such as diffusion...... method, weighted least squares including correlation in error estimation (WLS-ICE), to particle tracking data. The WLS-ICE method is applicable to arbitrary fit functions, and we provide a publically available WLS-ICE software....

  16. Evaluation of the flow-accelerated corrosion downstream of an orifice. 2. Measurement of corrosion rate and evaluation on the effects of the flow field

    International Nuclear Information System (INIS)

    Nagaya, Yukinori; Utanohara, Yoichi; Nakamura, Akira; Murase, Michio

    2008-01-01

    In this study, in order to evaluate the effects of flow field on corrosion rate due to flow accelerated corrosion (FAC), a corrosion rate downstream of an orifice was measured using the electric resistance method. The diameter of the pipe is 50 mm and that of the orifice is 24.3 mm, and flow velocity of the experimental loop was set at 5m/s, and the temperature of water was controlled within ±1 at 150deg-C. There were no significant circumferential difference in measured corrosion rate, and the maximum corrosion rate was observed at 1D or 2D downstream from the orifice. The ratios of the measured corrosion rate and the calculated wall shear stress at the 1D downstream from the orifice to the value at upstream under well developed flow agreed well. (author)

  17. Determining average path length and average trapping time on generalized dual dendrimer

    Science.gov (United States)

    Li, Ling; Guan, Jihong

    2015-03-01

    Dendrimer has wide number of important applications in various fields. In some cases during transport or diffusion process, it transforms into its dual structure named Husimi cactus. In this paper, we study the structure properties and trapping problem on a family of generalized dual dendrimer with arbitrary coordination numbers. We first calculate exactly the average path length (APL) of the networks. The APL increases logarithmically with the network size, indicating that the networks exhibit a small-world effect. Then we determine the average trapping time (ATT) of the trapping process in two cases, i.e., the trap placed on a central node and the trap is uniformly distributed in all the nodes of the network. In both case, we obtain explicit solutions of ATT and show how they vary with the networks size. Besides, we also discuss the influence of the coordination number on trapping efficiency.

  18. Corrosion of iron-base alloys by lithium

    International Nuclear Information System (INIS)

    Selle, J.E.

    1976-01-01

    A review of corrosion mechanisms operating in lithium-iron-base alloy systems is presented along with data obtained with thermal-convection loops of niobium-stabilized 2 1 / 4 percent Cr-1 percent Mo steel and types 304L and 321 stainless steels. A corrosion rate of 2.3 μm/year (0.09 mil/year) was obtained on the 2 1 / 4 percent Cr-1 percent Mo steel at 600 0 C. Considerably more mass transport of alloying constituents and a maximum corrosion rate of about 14 μm/year (0.55 mil/year) was obtained with the austenitic stainless steels. Results of metallography, x-ray fluorescence analysis, scanning electron microscopy, and weight-change data are presented and discussed

  19. Development of Copper Corrosion Products and Relation between Surface Appearance and Corrosion Rate

    International Nuclear Information System (INIS)

    Lan, Tran Thi Ngoc; Binh, Nguyen Thi Thanh; Tru, Nguyen Nhi; Yoshino, Tsujino; Yasuki, Maeda

    2008-01-01

    Copper was exposed unsheltered and sheltered in four humid tropical sites, representing urban, urban-industrial, urban-marine and rural environments. The corrosion rates and the sequence of corrosion product formation are presented and discussed in relation with climatic and atmospheric pollution parameters. Chemical compositions of corrosion products were found to depend on environments and duration of exposure. In all environments, cuprite was the predominating corrosion product that formed first and continuously increased during the exposure. Among the sulphur-containing corrosion products, posnjakite and brochantite were more frequently found and the first formed earlier. Nantokite was the most common chlorine-containing products for most cases, except the high-chloride environment, where atacamite was detected instead. The corrosion rate of copper was well indicated by the colour of patina. The red-purple colour corresponded to the high corrosion rate and the greenish grey colour corresponded to the low corrosion rate. Corrosion rate of sheltered copper in urban-marine environment increased with the exposure time

  20. The Development of Corrosion Resistant Zirconium Alloy

    International Nuclear Information System (INIS)

    Abdul-Latief; Noor-Yudhi; Isfandi; Djoko-Kisworo; Pranjono

    2000-01-01

    Corrosion test of Zr alloy consisting of quenching and tempering Zry-2,Zry-4 cast, Zr-1% Nb cast, has been. conducted. In corrosion test, thechanges during β-quenching, tempering and corrosion test at varioustemperature and time in autoclave water medium, can be seen. The treatmentconsisted of heating at 1050 o C for 30 minutes, quenching in water andtempering at 200 o C, 300 o C, 400 o C, 500 o C, 600 o C as well as corrosiontests at 225 o C, 275 o C, 325 o C at 4, 8, 12 hours. Sample preparation forcorrosion test was based on ASTM G-2 procedure, which consisted of washing,rinsing, pickling (3.5 cc HF 50%; 2.9 cc HNO 3 65% and 57 cc AMB),neutralizing in 0.1 M Al(NO 3 ) 3 , 9 H 2 O and ultrasonic rinsing/washing.Measurement performed are weight gain during corrosion, hardness test andmicrostructure observation using microscope optic. The results show thatβ-quenching of Zr alloy which was followed by tempering can turn αmartensite into tempered α 1 martensit. The increase of temperingtemperature decreases the Zr alloy hardness and the lowest hardness ispossessed by Zr-1% Nb alloy. The corrosion test at 275 o C and 325 o C showsthat the weight gain depends on the tempering temperature, the temperingtemperature of 400 o C and 200 o C gives the maximum weight gain for Zry-2,Zry-4 cast, Zr-1% Nb. The largest number of hydride formed during corrosionis found in Zry-2, while the small one is in Zr-1% Nb. (author)

  1. Corrosion of carbon steel under waste disposal conditions

    International Nuclear Information System (INIS)

    Marsh, G.

    1990-01-01

    The corrosion of carbon steel has been studied in the United Kingdom under granitic groundwater conditions, with pH between 5 and 10 and possibly substantial amounts of Cl - , SO 4 2- and HCO 3 - /CO 3 2- . Corrosion modes considered include uniform corrosion under both aerobic and anaerobic conditions; passive corrosion; localized attack in the form of pitting or crevice corrosion; and environmentally assisted cracking - hydrogen embrittlement or stress corrosion cracking. Studies of these processes are being carried out in order to predict the metal thicknesses required to give container lifetimes of 500 to 1000 years. A simple uniform corrosion model predicts a corrosion rate of around 13.4 μm/a at 20C, rising to 69 μm/a at 50C and 208 μm/a at 90C. A radiation dose of 10 5 rad/h and a G-value of 2.8 for the production of oxidizing species would account for an increase in corrosion rate of 7 μm/a. This model overestimates slightly the results actually achieved for experimental samples exposed for two years, the difference being due to a protective film formed on the samples. These corrosion rates predict that the container must be 227 mm thick to withstand uniform corrosion; however, they predict very high levels of hydrogen production. Conditions will be favourable for localized or pitting corrosion for about 125 years, leading to a maximum penetration of 160 mm. Since the exposure environment cannot be predicted precisely, one cannot state that stress corrosion cracking is impossible. Thus the container must be stress relieved. Other corrosion mechanisms such as microbial corrosion and hydrogen embrittlement are not considered significant

  2. Real time nanogravimetric monitoring of corrosion in radioactive environments

    OpenAIRE

    Tzagkaroulakis, Ioannis; Boxall, Colin

    2017-01-01

    Monitoring and understanding the mechanism of metal corrosion throughout the nuclear fuel cycle play a key role in the safe asset management of facilities. They also provide information essential for making an informed choice regarding the selection of decontamination methods for steel plant and equipment scheduled for decommissioning. Recent advances in Quartz Crystal Nanobalance (QCN) technology offer the means of monitoring corrosion in-situ, in radiologically harsh environments, in real t...

  3. Full-signature real-time corrosion detection of underground casing pipes

    NARCIS (Netherlands)

    Yin, Jiming; Lu, Mi; Pineda de Gyvez, J.

    2000-01-01

    Corrosion monitoring and early detection of pits and wall thinning for casing pipes are considerably important to gas and petroleum industries since the frequently occurring corrosion at the internal or external parts of those steel casing pipes used in underground gas storage or oil fields causes

  4. How to average logarithmic retrievals?

    Directory of Open Access Journals (Sweden)

    B. Funke

    2012-04-01

    Full Text Available Calculation of mean trace gas contributions from profiles obtained by retrievals of the logarithm of the abundance rather than retrievals of the abundance itself are prone to biases. By means of a system simulator, biases of linear versus logarithmic averaging were evaluated for both maximum likelihood and maximum a priori retrievals, for various signal to noise ratios and atmospheric variabilities. These biases can easily reach ten percent or more. As a rule of thumb we found for maximum likelihood retrievals that linear averaging better represents the true mean value in cases of large local natural variability and high signal to noise ratios, while for small local natural variability logarithmic averaging often is superior. In the case of maximum a posteriori retrievals, the mean is dominated by the a priori information used in the retrievals and the method of averaging is of minor concern. For larger natural variabilities, the appropriateness of the one or the other method of averaging depends on the particular case because the various biasing mechanisms partly compensate in an unpredictable manner. This complication arises mainly because of the fact that in logarithmic retrievals the weight of the prior information depends on abundance of the gas itself. No simple rule was found on which kind of averaging is superior, and instead of suggesting simple recipes we cannot do much more than to create awareness of the traps related with averaging of mixing ratios obtained from logarithmic retrievals.

  5. Corrosion of carbon steel in neutral water

    International Nuclear Information System (INIS)

    Kawai, Noboru; Iwahori, Toru; Kurosawa, Tatsuo

    1983-01-01

    The initial corrosion behavior of materials used in the construction of heat exchanger and piping system of BWR nuclear power plants and thermal power plants have been examined in neutral water at 30, 50, 100, 160, 200, and 285 deg C with two concentrations of dissolved oxygen in the water. In air-saturated water, the corrosion rate of carbon steel was so higher than those in deaerated conditions and the maximum corrosion rate was observed at 200 deg C. The corrosion rate in deaerated water gradually increased with increasing the water temperature. Low alloy steel (2.25 Cr, 1Mo) exhibited good corrosion resistance compared with the corrosion of carbon steel under similar testing conditions. Oxide films grown on carbon steel in deaerated water at 50, 100, 160, 200, and 285 deg C for 48 and 240 hrs were attacked by dissolved oxygen in room temperature water respectively. However the oxide films formed higher than about 160 deg C showed more protective. The electrochemical behavior of carbon steel with oxide films was also similar to the effect of temperature on the stability of oxide films. (author)

  6. Corrosion fatigue of bladed disk attachments of low-pressure turbine

    International Nuclear Information System (INIS)

    Asai, K.; Sakurai, S.; Nomura, K.; Saito, E.; Namura, K.

    2004-01-01

    The mechanism of a disk cracking in a low-pressure steam turbine was investigated by finite-element and fracture mechanics analysis and, based on the results of the investigation, a life assessment method was derived. The disk cracking was found to be caused by growth of corrosion pits, superposition of multiple vibration modes, and an increase in the standard deviation of the natural frequency of grouped blades after long-term operation. Taking these findings into consideration, the authors then developed a life-assessment method for disk cracking composed of evaluations (1) maximum corrosion pit size at the current situation, (2) corrosion pit growth after a certain term, and (3) failure-occurrence ratio for the estimated corrosion pit depth. Maximum corrosion-pit size is evaluated by extreme value statistical analysis using the data obtained by replica inspection. The failure-occurrence ratio is evaluated by Monte Carlo simulation considering two uncertainties, namely, the standard deviation of the natural frequency of grouped blades and the stimulus ratio. The values of both uncertainties were determined by the inverse problem analysis of the disk cracking. In light of these results, the authors found that replacing conventional tenon-shroud grouped blades with continuous-cover blades is effective from the view point of vibratory behavior. (orig.)

  7. Corrosion and corrosion control

    International Nuclear Information System (INIS)

    Khanna, A.S.; Totlani, M.K.

    1995-01-01

    Corrosion has always been associated with structures, plants, installations and equipment exposed to aggressive environments. It effects economy, safety and product reliability. Monitoring of component corrosion has thus become an essential requirement for the plant health and safety. Protection methods such as appropriate coatings, cathodic protection and use of inhibitors have become essential design parameters. High temperature corrosion, especially hot corrosion, is still a difficult concept to accommodate in corrosion allowance; there is a lack of harmonized system of performance testing of materials at high temperatures. In order to discuss and deliberate on these aspects, National Association for Corrosion Engineers International organised a National Conference on Corrosion and its Control in Bombay during November 28-30, 1995. This volume contains papers presented at the symposium. Paper relevant to INIS is indexed separately. refs., figs., tabs

  8. Long-time corrosion and high-temperature oxidation of zirconium alloys applied on NPP like fuel elements cover

    International Nuclear Information System (INIS)

    Vrtilkova, V.; Novotny, L.; Lingart, S.; Doukha, R.; Yarosh, Ya.; Kolenchik, Ya.

    2007-01-01

    Zirconium is applying in nuclear energy since 50-th of last century in capacity of material for cover production for fuel elements, reactor fuel and structural parts, and mainly due to both corrosion stability and low effective cross section for thermal neutrons capture. Impurities in doping elements form and alloy production technology has influence on mechanical and corrosion properties of finite alloy. Long-time corrosion tests for several zirconium alloys in forcing autoclave under different reaction conditions were carried out. After that process kinetics was studied, mass increase, hydrogen formation, zirconium hydride forming morphology, zirconium oxide layer thickness have been determined as well

  9. Corrosion behavior of the aluminum under the simulated environmental condition of low-level waste. Part 1. Effect of dry storage on the corrosion behavior of pre-filmed specimen

    International Nuclear Information System (INIS)

    Fujiwara, Kazutoshi; Tani, Junichi; Tanaka, Yukihisa

    2016-01-01

    Aluminum alloy remains in the Low-level Radioactive Waste (LLW) generated at nuclear facilities. It is well known that aluminum reactors to the alkaline component of cement, or water, generating hydrogen gas. For the saft management of radioactive waste disposal facilities, it is necessary to evaluate the corrosion behavior of aluminum and the hydrogen generation behavior in consideration with transition of the burial environment. In the present study, the corrosion behaviors of aluminum in the alkaline solutions at 15degC were evaluated. Pure aluminium was used as specimen. The test solutions used in this study were water in equilibrium with the cement paste grain produced from ordinary portland cement (OPC). The temperature and pH of solutions were 15degC and 11.5-12.5, respectively. In order to make a corrosion product on the surface, the specimens were immersed in the solution for about 3000 hours as pretreatment. The corrosion behaviors of pre-filmed specimen were evaluated after drying. The test results shows that the maximum in a corrosion rate appeared in early stages and it decrease to less than 1x10 -3 mm/y. The maximum did not appear when the corrosion products were formed in the OPC grain as conditions similar to actual environment. (author)

  10. Effect of Precipitate State on Mechanical Properties, Corrosion Behavior, and Microstructures of Al-Zn-Mg-Cu Alloy

    Science.gov (United States)

    Peng, Xiaoyan; Li, Yao; Xu, Guofu; Huang, Jiwu; Yin, Zhimin

    2018-03-01

    The mechanical properties, corrosion behavior and microstructures of the Al-Zn-Mg-Cu alloy under various ageing treatments were investigated comparatively. The results show that the tensile strength and corrosion resistance are strongly affected by the precipitate state. Massive fine intragranular precipitates contribute to high strength. Discontinuous coarse grain boundary precipitates containing high Cu content, as well as the narrow precipitate free zone, result in low corrosion susceptibility. After the non-isothermal ageing (NIA) treatment, the tensile strength of 577 MPa is equivalent to that of 579 MPa for the T6 temper. Meanwhile, the stress corrosion susceptibility r tf and the maximum corrosion depth are 97.8% and 23.5 μm, which are comparable to those of 92.8% and 26.7 μm for the T73 temper. Moreover, the total ageing time of the NIA treatment is only 7.25 h, which is much less than that of 48.67 h for the retrogression and re-ageing condition.

  11. Risk based service life prediction of underground cast iron pipes subjected to corrosion

    International Nuclear Information System (INIS)

    Li, C.Q.; Mahmoodian, M.

    2013-01-01

    Aging and deterioration of underground cast iron pipes is inevitable after their long time in service, with corrosion being the most predominant mechanism for pipe failures. Although considerable research has been undertaken in the past few decades, more is on the effects of corrosion on structural capacity of pipes than that on the prediction of their service life. This paper presents a methodology to quantitatively assess the risk of pipe collapse and predict its remaining service life using a time-dependent reliability theory. The concept of stress intensity in fracture mechanics is employed to establish the failure criterion of pipe collapse. An empirical model is derived for maximum pit growth of corrosion from the available data based on mathematical regressions. An example is provided to illustrate the application of the proposed method. It is found in the paper that the risk of pipe collapse increases with an increase in the diameter of the pipe for both external and internal corrosion. It is also found that the tougher the pipe is, the smaller the risk of its collapse. The paper concludes that a time-dependent reliability method is a very useful tool to predict the risk of pipe collapse and its remaining service life. The proposed method can help the water industry develop rehabilitation or replacement strategy for existing pipe networks with a view for better management of the pipe asset

  12. A review on pipeline corrosion, in-line inspection (ILI), and corrosion growth rate models

    International Nuclear Information System (INIS)

    Vanaei, H.R.; Eslami, A.; Egbewande, A.

    2017-01-01

    Pipelines are the very important energy transmission systems. Over time, pipelines can corrode. While corrosion could be detected by in-line inspection (ILI) tools, corrosion growth rate prediction in pipelines is usually done through corrosion rate models. For pipeline integrity management and planning selecting the proper corrosion ILI tool and also corrosion growth rate model is important and can lead to significant savings and safer pipe operation. In this paper common forms of pipeline corrosion, state of the art ILI tools, and also corrosion growth rate models are reviewed. The common forms of pipeline corrosion introduced in this paper are Uniform/General Corrosion, Pitting Corrosion, Cavitation and Erosion Corrosion, Stray Current Corrosion, Micro-Bacterial Influenced Corrosion (MIC). The ILI corrosion detection tools assessed in this study are Magnetic Flux Leakage (MFL), Circumferential MFL, Tri-axial MFL, and Ultrasonic Wall Measurement (UT). The corrosion growth rate models considered in this study are single-value corrosion rate model, linear corrosion growth rate model, non-linear corrosion growth rate model, Monte-Carlo method, Markov model, TD-GEVD, TI-GEVD model, Gamma Process, and BMWD model. Strengths and limitations of ILI detection tools, and also corrosion predictive models with some practical examples are discussed. This paper could be useful for those whom are supporting pipeline integrity management and planning. - Highlights: • Different forms of pipeline corrosion are explained. • Common In-Line Inspection (ILI) tools and corrosion growth rate models are introduced. • Strength and limitations of corrosion growth rate models/ILI tools are discussed. • For pipeline integrity management programs using more than one corrosion growth rate model/ILI tool is suggested.

  13. NASA's Beachside Corrosion Test Site and Current Environmentally Friendly Corrosion Control Initiatives

    Science.gov (United States)

    Russell, Richard W.; Calle, Luz Marina; Johnston, Frederick; Montgomery, Eliza L.; Curran, Jerome P.; Kolody, Mark R.

    2013-01-01

    NASA began corrosion studies at the Kennedy Space Center (KSC) in 1966 during the Gemini/Apollo Programs with the evaluation of long-term corrosion protective coatings for carbon steel. KSC's Beachside Corrosion Test Site (BCTS), which has been documented by the American Society of Materials (ASM) as one of the most corrosive, naturally occurring, environments in the world, was established at that time. With the introduction of the Space Shuttle in 1981, the already highly corrosive conditions at the launch pad were rendered even more severe by the acid ic exhaust from the solid rocket boosters. In the years that followed, numerous studies have identified materials, coatings, and maintenance procedures for launch hardware and equipment exposed to the highly corrosive environment at the launch pad. This paper presents a historical overview of over 45 years of corrosion and coating evaluation studies and a description of the BCTS's current capabilities. Additionally, current research and testing programs involving chromium free coatings, environmentally friendly corrosion preventative compounds, and alternates to nitric acid passivation will be discussed.

  14. Real-time traffic signal optimization model based on average delay time per person

    Directory of Open Access Journals (Sweden)

    Pengpeng Jiao

    2015-10-01

    Full Text Available Real-time traffic signal control is very important for relieving urban traffic congestion. Many existing traffic control models were formulated using optimization approach, with the objective functions of minimizing vehicle delay time. To improve people’s trip efficiency, this article aims to minimize delay time per person. Based on the time-varying traffic flow data at intersections, the article first fits curves of accumulative arrival and departure vehicles, as well as the corresponding functions. Moreover, this article transfers vehicle delay time to personal delay time using average passenger load of cars and buses, employs such time as the objective function, and proposes a signal timing optimization model for intersections to achieve real-time signal parameters, including cycle length and green time. This research further implements a case study based on practical data collected at an intersection in Beijing, China. The average delay time per person and queue length are employed as evaluation indices to show the performances of the model. The results show that the proposed methodology is capable of improving traffic efficiency and is very effective for real-world applications.

  15. The effects of time, temperature and rotation of water on the corrosion rate of different types of steels

    International Nuclear Information System (INIS)

    Muhamad Daud; Jamaliah Shariff.

    1984-01-01

    By using hot plate/magnetic stirrer and immersion technique, the steel corroded uniformly and their corrosion rates vary due to type of steel, time of immersion, temperature and rotation of water. Therefore the rate of general corrosion, or sealing, of steel alloys is influenced by a number of factors, those best established being the composition of the metal, time, temperature, velocity, cleanliness or roughness of the metal surface and direct contact with solutions of the other materials. (author)

  16. Graphene: corrosion-inhibiting coating.

    Science.gov (United States)

    Prasai, Dhiraj; Tuberquia, Juan Carlos; Harl, Robert R; Jennings, G Kane; Rogers, Bridget R; Bolotin, Kirill I

    2012-02-28

    We report the use of atomically thin layers of graphene as a protective coating that inhibits corrosion of underlying metals. Here, we employ electrochemical methods to study the corrosion inhibition of copper and nickel by either growing graphene on these metals, or by mechanically transferring multilayer graphene onto them. Cyclic voltammetry measurements reveal that the graphene coating effectively suppresses metal oxidation and oxygen reduction. Electrochemical impedance spectroscopy measurements suggest that while graphene itself is not damaged, the metal under it is corroded at cracks in the graphene film. Finally, we use Tafel analysis to quantify the corrosion rates of samples with and without graphene coatings. These results indicate that copper films coated with graphene grown via chemical vapor deposition are corroded 7 times slower in an aerated Na(2)SO(4) solution as compared to the corrosion rate of bare copper. Tafel analysis reveals that nickel with a multilayer graphene film grown on it corrodes 20 times slower while nickel surfaces coated with four layers of mechanically transferred graphene corrode 4 times slower than bare nickel. These findings establish graphene as the thinnest known corrosion-protecting coating.

  17. Latitudinal Change of Tropical Cyclone Maximum Intensity in the Western North Pacific

    OpenAIRE

    Choi, Jae-Won; Cha, Yumi; Kim, Hae-Dong; Kang, Sung-Dae

    2016-01-01

    This study obtained the latitude where tropical cyclones (TCs) show maximum intensity and applied statistical change-point analysis on the time series data of the average annual values. The analysis results found that the latitude of the TC maximum intensity increased from 1999. To investigate the reason behind this phenomenon, the difference of the average latitude between 1999 and 2013 and the average between 1977 and 1998 was analyzed. In a difference of 500 hPa streamline between the two ...

  18. Concentration fluctuations and averaging time in vapor clouds

    CERN Document Server

    Wilson, David J

    2010-01-01

    This book contributes to more reliable and realistic predictions by focusing on sampling times from a few seconds to a few hours. Its objectives include developing clear definitions of statistical terms, such as plume sampling time, concentration averaging time, receptor exposure time, and other terms often confused with each other or incorrectly specified in hazard assessments; identifying and quantifying situations for which there is no adequate knowledge to predict concentration fluctuations in the near-field, close to sources, and far downwind where dispersion is dominated by atmospheric t

  19. A liquid aluminum corrosion resistance surface on steel substrate

    International Nuclear Information System (INIS)

    Wang Deqing; Shi Ziyuan; Zou Longjiang

    2003-01-01

    The process of hot dipping pure aluminum on a steel substrate followed by oxidation was studied to form a surface layer of aluminum oxide resistant to the corrosion of aluminum melt. The thickness of the pure aluminum layer on the steel substrate is reduced with the increase in temperature and time in initial aluminizing, and the thickness of the aluminum layer does not increase with time at given temperature when identical temperature and complete wetting occur between liquid aluminum and the substrate surface. The thickness of the Fe-Al intermetallic layer on the steel base is increased with increasing bath temperature and time. Based on the experimental data and the mathematics model developed by the study, a maximum exists in the thickness of the Fe-Al intermetallic at certain dipping temperature. X-ray diffraction (XRD) and energy dispersive X-ray (EDX) analysis reveals that the top portion of the steel substrate is composed of a thin layer of α-Al 2 O 3 , followed by a thinner layer of FeAl 3 , and then a much thicker one of Fe 2 Al 5 on the steel base side. In addition, there is a carbon enrichment zone in diffusion front. The aluminum oxide surface formed on the steel substrate is in perfect condition after corrosion test in liquid aluminum at 750 deg. C for 240 h, showing extremely good resistance to aluminum melt corrosion

  20. Corrosion inhibition of magnesium heated in wet air, by surface fluoridation; Inhibition de la corrosion du magnesium chauffe dans l'air humide, par fluoruration superficielle

    Energy Technology Data Exchange (ETDEWEB)

    Caillat, R; Darras, R; Leclercq, D [Commissariat a l' Energie Atomique, Saclay (France).Centre d' Etudes Nucleaires

    1960-07-01

    The maximum temperature (350 deg. C) of magnesium corrosion resistance in wet air may be raised to 490-500 deg. C by the formation of a superficial fluoride film. This can be obtained by two different ways: either by addition of hydrofluoric acid to the corroding medium in a very small proportion such as 0,003 mg/litre; at atmospheric pressure, or by dipping the magnesium in a dilute aqueous solution of nitric and hydrofluoric acids at room temperature before exposing it to the corroding atmosphere. In both cases the corrosion inhibition is effective over a very long time, even several thousand hours. (author) [French] La temperature limite (350 deg. C) de resistance du magnesium a la corrosion par l'air humide, peut etre elevee jusque 490-500 deg. C par la formation d'une couche fluoruree superficielle. Deux procedes permettent d'obtenir ce resultat: l'atmosphere corrodante peut etre additionnee d'acide fluorhydrique a une concentration aussi faible que 0,003 mg/litre, a la pression atmospherique, ou bien le magnesium peut etre traite a froid, avant exposition a la corrosion, dans une solution aqueuse diluee d'acides nitrique et fluorhydrique. Dans les deux cas, la protection est assuree, meme pour de tres longues durees d'exposition: plusieurs milliers d'heures. (auteur)

  1. Anaerobic Corrosion of 304 Stainless Steel Caused by the Pseudomonas aeruginosa Biofilm

    Directory of Open Access Journals (Sweden)

    Ru Jia

    2017-11-01

    Full Text Available Pseudomonas aeruginosa is a ubiquitous bacterium capable of forming problematic biofilms in many environments. They cause biocorrosion of medical implants and industrial equipment and infrastructure. Aerobic corrosion of P. aeruginosa against stainless steels has been reported by some researchers while there is a lack of reports on anaerobic P. aeruginosa corrosion in the literature. In this work, the corrosion by a wild-type P. aeruginosa (strain PAO1 biofilm against 304 stainless steel (304 SS was investigated under strictly anaerobic condition for up to 14 days. The anaerobic corrosion of 304 SS by P. aeruginosa was reported for the first time. Results showed that the average sessile cell counts on 304 SS coupons after 7- and 14-day incubations were 4.8 × 107 and 6.2 × 107 cells/cm2, respectively. Scanning electron microscopy and confocal laser scanning microscopy corroborated the sessile cell counts. The X-ray diffraction analysis identified the corrosion product as iron nitride, confirming that the corrosion was caused by the nitrate reducing biofilm. The largest pit depths on 304 SS surfaces after the 7- and 14-day incubations with P. aeruginosa were 3.9 and 7.4 μm, respectively. Electrochemical tests corroborated the pitting data.

  2. Corrosion of metallic materials. Dry corrosion, aqueous corrosion and corrosion by liquid metal, methods of protection

    International Nuclear Information System (INIS)

    Helie, Max

    2015-01-01

    This book is based on a course on materials given in an engineering school. The author first gives an overview of metallurgy issues: metallic materials (pure metals, metallic alloys), defects of crystal lattices (point defects, linear defects or dislocations), equilibrium diagrams, steels and cast, thermal processing of steels, stainless steels, aluminium and its alloys, copper and its alloys. The second part addresses the properties and characterization of surfaces and interfaces: singularity of a metal surface, surface energy of a metal, energy of grain boundaries, adsorption at a material surface, metal-electrolyte interface, surface oxide-electrolyte interface, techniques of surface analysis. The third chapter addresses the electrochemical aspects of corrosion: description of the corrosion phenomenon, free enthalpy of a compound and free enthalpy of a reaction, case of dry corrosion (thermodynamic aspect, Ellingham diagram, oxidation mechanisms, experimental study, macroscopic modelling), case of aqueous corrosion (electrochemical thermodynamics and kinetics, experimental determination of corrosion rate). The fourth part addresses the different forms of aqueous corrosion: generalized corrosion (atmospheric corrosion, mechanisms and tests), localized corrosion (galvanic, pitting, cracking, intergranular, erosion and cavitation), particular cases of stress cracking (stress corrosion, fatigue-corrosion, embrittlement by hydrogen), and bi-corrosion (of non alloyed steels, of stainless steels, and of aluminium and copper alloys). The sixth chapter addresses the struggle and the protection against aqueous corrosion: methods of prevention, scope of use of main alloys, geometry-based protection of pieces, use of corrosion inhibitors, use of organic or metallic coatings, electrochemical protection. The last chapter proposes an overview of corrosion types in industrial practices: in the automotive industry, in the oil industry, in the aircraft industry, and in the

  3. A constant travel time budget? In search for explanations for an increase in average travel time

    NARCIS (Netherlands)

    Rietveld, P.; Wee, van B.

    2002-01-01

    Recent research suggests that during the past decades the average travel time of the Dutch population has probably increased. However, different datasources show different levels of increase. Possible causes of the increase in average travel time are presented here. Increased incomes have

  4. Effect of Dissolved Oxygen and Immersion Time on the Corrosion Behaviour of Mild Steel in Bicarbonate/Chloride Solution

    Directory of Open Access Journals (Sweden)

    Gaius Debi Eyu

    2016-09-01

    Full Text Available The electrochemical behavior of mild steel in bicarbonate solution at different dissolved oxygen (DO concentrations and immersion times has been studied under dynamic conditions using electrochemical techniques. The results show that both DO and immersion times influence the morphology of the corrosion products. In comparative tests, the corrosion rate was systematically found to be lower in solutions with lower DO, lower HCO3− concentrations and longer immersion time. The SEM analyses reveal that the iron dissolution rate was more severe in solutions containing higher DO. The decrease in corrosion rate can be attributed to the formation of a passive layer containing mainly α -FeO (OH and ( γ -Fe2O3/Fe3O4 as confirmed by the X-ray diffractometry (XRD and X-ray photoelectron spectroscopy (XPS. Passivation of mild steel is evident in electrochemical test at ≈ −600 mVSCE at pH ≥ 8 in dearated ( ≤ 0.8 ppm DO chloride bicarbonate solution under dynamic conditions.

  5. Corrosion of beryllium

    International Nuclear Information System (INIS)

    Mueller, J.J.; Adolphson, D.R.

    1987-01-01

    The corrosion behavior of beryllium in aqueous and elevated-temperature oxidizing environments has been extensively studied for early-intended use of beryllium in nuclear reactors and in jet and rocket propulsion systems. Since that time, beryllium has been used as a structural material in les corrosive environments. Its primary applications include gyro systems, mirror and reentry vehicle structures, and aircraft brakes. Only a small amount of information has been published that is directly related to the evaluation of beryllium for service in the less severe or normal atmospheric environments associated with these applications. Despite the lack of published data on the corrosion of beryllium in atmospheric environments, much can be deduced about its corrosion behavior from studies of aqueous corrosion and the experiences of fabricators and users in applying, handling, processing, storing, and shipping beryllium components. The methods of corrosion protection implemented to resist water and high-temperature gaseous environments provide useful information on methods that can be applied to protect beryllium for service in future long-term structural applications

  6. Effect of assembled time on the corrosion behaviors of SAMs film on the AM60B alloy and its assembled mechanism

    Energy Technology Data Exchange (ETDEWEB)

    Liu, Xianbin, E-mail: xbliu@imr.ac.cn; Shan, Dayong; Song, Yingwei; Han, En-hou

    2015-01-15

    The influence of assembled time on the corrosion behaviors of SAMs film on the AM60B alloy and its assembled mechanism have been investigated by electrochemical measurements, scanning electron microscopy (SEM) observation and X-ray photoelectron spectroscopy (XPS) analysis. The self-assembled experiment on the AM60B magnesium alloy indicates that the corrosion susceptibility decreases with increasing assembled time until 24 h on cast AM60B alloy and then increases with increase of the assembled time proved by EIS measurement and potentiodynamic curves. The self-assembled experiments on pure magnesium and various heat treated cast AM60B magnesium alloy illuminate that the dissolved aluminum in magnesium solid solution is the key factor for assembled efficiency and is hard to self-assemble on the pure magnesium without aluminum. The corrosion resistance of self-assembled film on AM60B magnesium alloy is monotonically increasing with the dissolved aluminum. The results of XPS analysis reveal the assembled mechanism on AM60B and corroborate the function of Al element. - Highlights: • It is hard to self-assemble on the pure magnesium. • 24 h assembled film has the low corrosion susceptibility by EIS and polarization. • The corrosion susceptibility of SAMs film lie on the Al atom state in AM60B. • The corrosion susceptibility of SAMs film is decreasing with the dissolved Al.

  7. Effect of assembled time on the corrosion behaviors of SAMs film on the AM60B alloy and its assembled mechanism

    International Nuclear Information System (INIS)

    Liu, Xianbin; Shan, Dayong; Song, Yingwei; Han, En-hou

    2015-01-01

    The influence of assembled time on the corrosion behaviors of SAMs film on the AM60B alloy and its assembled mechanism have been investigated by electrochemical measurements, scanning electron microscopy (SEM) observation and X-ray photoelectron spectroscopy (XPS) analysis. The self-assembled experiment on the AM60B magnesium alloy indicates that the corrosion susceptibility decreases with increasing assembled time until 24 h on cast AM60B alloy and then increases with increase of the assembled time proved by EIS measurement and potentiodynamic curves. The self-assembled experiments on pure magnesium and various heat treated cast AM60B magnesium alloy illuminate that the dissolved aluminum in magnesium solid solution is the key factor for assembled efficiency and is hard to self-assemble on the pure magnesium without aluminum. The corrosion resistance of self-assembled film on AM60B magnesium alloy is monotonically increasing with the dissolved aluminum. The results of XPS analysis reveal the assembled mechanism on AM60B and corroborate the function of Al element. - Highlights: • It is hard to self-assemble on the pure magnesium. • 24 h assembled film has the low corrosion susceptibility by EIS and polarization. • The corrosion susceptibility of SAMs film lie on the Al atom state in AM60B. • The corrosion susceptibility of SAMs film is decreasing with the dissolved Al

  8. Temperature dependency of external stress corrosion crack propagation of 304 stainless steel

    International Nuclear Information System (INIS)

    Hayashibara, Hitoshi; Mizutani, Yoshihiro; Mayuzumi, Masami; Tani, Jun-ichi

    2010-01-01

    Temperature dependency of external stress corrosion cracking (ESCC) of 304 stainless steel was examined with CT specimens. Maximum ESCC propagation rates appeared in the early phase of ESCC propagation. ESCC propagation rates generally became smaller as testing time advance. Temperature dependency of maximum ESCC propagation rate was analyzed with Arrhenius plot, and apparent activation energy was similar to that of SCC in chloride solutions. Temperature dependency of macroscopic ESCC incubation time was different from that of ESCC propagation rate. Anodic current density of 304 stainless steel was also examined by anodic polarization measurement. Temperature dependency of critical current density of active state in artificial sea water solution of pH=1.3 was similar to that of ESCC propagation rate. (author)

  9. Time-averaged MSD of Brownian motion

    International Nuclear Information System (INIS)

    Andreanov, Alexei; Grebenkov, Denis S

    2012-01-01

    We study the statistical properties of the time-averaged mean-square displacements (TAMSD). This is a standard non-local quadratic functional for inferring the diffusion coefficient from an individual random trajectory of a diffusing tracer in single-particle tracking experiments. For Brownian motion, we derive an exact formula for the Laplace transform of the probability density of the TAMSD by mapping the original problem onto chains of coupled harmonic oscillators. From this formula, we deduce the first four cumulant moments of the TAMSD, the asymptotic behavior of the probability density and its accurate approximation by a generalized Gamma distribution

  10. Time-averaged MSD of Brownian motion

    Science.gov (United States)

    Andreanov, Alexei; Grebenkov, Denis S.

    2012-07-01

    We study the statistical properties of the time-averaged mean-square displacements (TAMSD). This is a standard non-local quadratic functional for inferring the diffusion coefficient from an individual random trajectory of a diffusing tracer in single-particle tracking experiments. For Brownian motion, we derive an exact formula for the Laplace transform of the probability density of the TAMSD by mapping the original problem onto chains of coupled harmonic oscillators. From this formula, we deduce the first four cumulant moments of the TAMSD, the asymptotic behavior of the probability density and its accurate approximation by a generalized Gamma distribution.

  11. Spatially and time-resolved element-specific in situ corrosion investigations with an online hyphenated microcapillary flow injection inductively coupled plasma mass spectrometry set-up

    International Nuclear Information System (INIS)

    Homazava, N.; Ulrich, A.; Kraehenbuehl, U.

    2008-01-01

    A novel technique for in situ spatial, time-resolved element-specific investigations of corrosion processes is developed. The technique is based on an online hyphenation of a specially designed microflow-capillary set-up to inductively coupled plasma mass spectrometry (ICP-MS) using flow injection sample introduction. Detailed aspects of the method development, optimization of the sample microflow introduction and flow injection characteristics for the localized corrosion analysis are described. Moreover, specific challenges of the ICP-MS analysis as applied to the analysis of corrosion sample probes, e.g. high matrix load and limited sample volume, are discussed. The efficiency of the developed technique is proved by corrosion susceptibility analysis of a commercial Al alloy. Results of the corrosion experiments of the aluminum alloy AA 6111 are presented to demonstrate the influence of various factors such as exposure time and pH value of the corrosive medium on the element-specific dissolution rates of the alloy. This novel technique provides new aspects in corrosion science and sheds new light on corrosion mechanisms

  12. Determination of the speed of corrosion of aluminum brass in drinking water

    International Nuclear Information System (INIS)

    Valcarce, M.B; Vasquez, M; Sanchez, S.R de

    2004-01-01

    Copper alloys are widely used for water conduits. This work defines the speed of corrosion of aluminum brass (Cu76Zn22Al2) in potable water by comparing the results from electrochemical tests and from weight loss tests. The chosen medium is synthetic drinking water (pH 7.6) whose composition is the average for the drinking water in Mar del Plata city. Coupons were prepared for the weight loss test, which were kept in artificial potable water for 90 days. The flow of corrosion was determined based on the resulting weight loss. After the period of immersion, the coupons showed pitting. The resistance to polarization (Rp) was also determined at different immersion times with potential jumps, potentiodynamic sweeps and electrochemical impedance spectroscopy (EIS). The Rp values obtained with the different electrochemical methods are in agreement, and they increase over time. This increase can be attributed to the growth of a layer of oxide over the metallic surface. Based on the record of polarization curves the Tafel slopes were obtained and the corrosion current was estimated after 2 hrs and 192 hrs of immersion. The corrosion current values obtained for the different electrochemical methods match the results obtained from the weight loss test (CW)

  13. Method for Evaluating the Corrosion Resistance of Aluminum Metallization of Integrated Circuits under Multifactorial Influence

    Science.gov (United States)

    Kolomiets, V. I.

    2018-03-01

    The influence of complex influence of climatic factors (temperature, humidity) and electric mode (supply voltage) on the corrosion resistance of metallization of integrated circuits has been considered. The regression dependence of the average time of trouble-free operation t on the mentioned factors has been established in the form of a modified Arrhenius equation that is adequate in a wide range of factor values and is suitable for selecting accelerated test modes. A technique for evaluating the corrosion resistance of aluminum metallization of depressurized CMOS integrated circuits has been proposed.

  14. An evaluation of corrosion resistant alloys by field corrosion test in Japanese refuse incineration plants

    International Nuclear Information System (INIS)

    Kawahara, Yuuzou; Nakamura, Masanori; Shibuya, Eiichi; Yukawa, Kenichi

    1995-01-01

    As the first step for development of the corrosion resistant superheater tube materials of 500 C, 100 ata used in high efficient waste-to-energy plants, field corrosion tests of six conventional alloys were carried out at metal temperatures of 450 C and 550 C for 700 and 3,000 hours in four typical Japanese waste incineration plants. The test results indicate that austenitic alloys containing approximately 80 wt% [Cr+Ni] show excellent corrosion resistance. When the corrosive environment is severe, intergranular corrosion of 40∼200 microm depth occurs in stainless steel and high alloyed materials. It is confirmed quantitatively that corrosion behavior is influenced by environmental corrosion factors such as Cl concentration and thickness of deposits on tube surface, metal temperature, and flue gas temperature. The excellent corrosion resistance of high [Cr+Ni+Mo] alloys such as Alloy 625 is explained by the stability of its protective oxide, such that the time dependence of corrosion nearly obeys the parabolic rate law

  15. SU-E-T-174: Evaluation of the Optimal Intensity Modulated Radiation Therapy Plans Done On the Maximum and Average Intensity Projection CTs

    Energy Technology Data Exchange (ETDEWEB)

    Jurkovic, I [University of Texas Health Science Center at San Antonio, San Antonio, TX (United States); Stathakis, S; Li, Y; Patel, A; Vincent, J; Papanikolaou, N; Mavroidis, P [Cancer Therapy and Research Center University of Texas Health Sciences Center at San Antonio, San Antonio, TX (United States)

    2014-06-01

    Purpose: To determine the difference in coverage between plans done on average intensity projection and maximum intensity projection CT data sets for lung patients and to establish correlations between different factors influencing the coverage. Methods: For six lung cancer patients, 10 phases of equal duration through the respiratory cycle, the maximum and average intensity projections (MIP and AIP) from their 4DCT datasets were obtained. MIP and AIP datasets had three GTVs delineated (GTVaip — delineated on AIP, GTVmip — delineated on MIP and GTVfus — delineated on each of the 10 phases and summed up). From the each GTV, planning target volumes (PTV) were then created by adding additional margins. For each of the PTVs an IMRT plan was developed on the AIP dataset. The plans were then copied to the MIP data set and were recalculated. Results: The effective depths in AIP cases were significantly smaller than in MIP (p < 0.001). The Pearson correlation coefficient of r = 0.839 indicates strong degree of positive linear relationship between the average percentage difference in effective depths and average PTV coverage on the MIP data set. The V2 0 Gy of involved lung depends on the PTV coverage. The relationship between PTVaip mean CT number difference and PTVaip coverage on MIP data set gives r = 0.830. When the plans are produced on MIP and copied to AIP, r equals −0.756. Conclusion: The correlation between the AIP and MIP data sets indicates that the selection of the data set for developing the treatment plan affects the final outcome (cases with high average percentage difference in effective depths between AIP and MIP should be calculated on AIP). The percentage of the lung volume receiving higher dose depends on how well PTV is covered, regardless of on which set plan is done.

  16. Screening of soil corrosivity by field testing: Results and design of an electrochemical soil corrosion probe

    DEFF Research Database (Denmark)

    Nielsen, Lars vendelbo; Bruun, Niels Kåre

    1996-01-01

    The corrosivity of different types of soil have been assessed by exposing carbon-steel plates at 50 different locations in Denmark for an extended period of time. The investigations included weight loss measurements and analysis of the chemical compositions of the corrosion products formed...... on the plates during exposure. An electrochemical soil corrosion probe has been designed and manufactured allowing for simultaneous measurements of several qauntities to predict corrosion. The probe consists of individual sections capable of measuring redox-potential, corrosion potential, soil resistivity...

  17. Impact of connected vehicle guidance information on network-wide average travel time

    Directory of Open Access Journals (Sweden)

    Jiangfeng Wang

    2016-12-01

    Full Text Available With the emergence of connected vehicle technologies, the potential positive impact of connected vehicle guidance on mobility has become a research hotspot by data exchange among vehicles, infrastructure, and mobile devices. This study is focused on micro-modeling and quantitatively evaluating the impact of connected vehicle guidance on network-wide travel time by introducing various affecting factors. To evaluate the benefits of connected vehicle guidance, a simulation architecture based on one engine is proposed representing the connected vehicle–enabled virtual world, and connected vehicle route guidance scenario is established through the development of communication agent and intelligent transportation systems agents using connected vehicle application programming interface considering the communication properties, such as path loss and transmission power. The impact of connected vehicle guidance on network-wide travel time is analyzed by comparing with non-connected vehicle guidance in response to different market penetration rate, following rate, and congestion level. The simulation results explore that average network-wide travel time in connected vehicle guidance shows a significant reduction versus that in non–connected vehicle guidance. Average network-wide travel time in connected vehicle guidance have an increase of 42.23% comparing to that in non-connected vehicle guidance, and average travel time variability (represented by the coefficient of variance increases as the travel time increases. Other vital findings include that higher penetration rate and following rate generate bigger savings of average network-wide travel time. The savings of average network-wide travel time increase from 17% to 38% according to different congestion levels, and savings of average travel time in more serious congestion have a more obvious improvement for the same penetration rate or following rate.

  18. Reliability-based management of buried pipelines considering external corrosion defects

    Science.gov (United States)

    Miran, Seyedeh Azadeh

    Corrosion is one of the main deteriorating mechanisms that degrade the energy pipeline integrity, due to transferring corrosive fluid or gas and interacting with corrosive environment. Corrosion defects are usually detected by periodical inspections using in-line inspection (ILI) methods. In order to ensure pipeline safety, this study develops a cost-effective maintenance strategy that consists of three aspects: corrosion growth model development using ILI data, time-dependent performance evaluation, and optimal inspection interval determination. In particular, the proposed study is applied to a cathodic protected buried steel pipeline located in Mexico. First, time-dependent power-law formulation is adopted to probabilistically characterize growth of the maximum depth and length of the external corrosion defects. Dependency between defect depth and length are considered in the model development and generation of the corrosion defects over time is characterized by the homogenous Poisson process. The growth models unknown parameters are evaluated based on the ILI data through the Bayesian updating method with Markov Chain Monte Carlo (MCMC) simulation technique. The proposed corrosion growth models can be used when either matched or non-matched defects are available, and have ability to consider newly generated defects since last inspection. Results of this part of study show that both depth and length growth models can predict damage quantities reasonably well and a strong correlation between defect depth and length is found. Next, time-dependent system failure probabilities are evaluated using developed corrosion growth models considering prevailing uncertainties where three failure modes, namely small leak, large leak and rupture are considered. Performance of the pipeline is evaluated through failure probability per km (or called a sub-system) where each subsystem is considered as a series system of detected and newly generated defects within that sub

  19. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C

    Energy Technology Data Exchange (ETDEWEB)

    Lambrinou, Konstantina, E-mail: klambrin@sckcen.be [SCK-CEN, Boeretang 200, 2400 Mol (Belgium); Charalampopoulou, Evangelia [SCK-CEN, Boeretang 200, 2400 Mol (Belgium); University of Antwerp, Electron Microscopy for Materials Science (EMAT), Groenenborgerlaan 171, 2020 Antwerpen (Belgium); Van der Donck, Tom [KU Leuven, Department of Materials Engineering, Kasteelpark Arenberg 44, 3001 Leuven (Belgium); Delville, Rémi [SCK-CEN, Boeretang 200, 2400 Mol (Belgium); Schryvers, Dominique [University of Antwerp, Electron Microscopy for Materials Science (EMAT), Groenenborgerlaan 171, 2020 Antwerpen (Belgium)

    2017-07-15

    This work addresses the dissolution corrosion behaviour of 316L austenitic stainless steels. For this purpose, solution-annealed and cold-deformed 316L steels were simultaneously exposed to oxygen-poor (<10{sup −8} mass%) static liquid lead-bismuth eutectic (LBE) for 253–3282 h at 500 °C. Corrosion was consistently more severe for the cold-drawn steels than the solution-annealed steel, indicating the importance of the steel thermomechanical state. The thickness of the dissolution-affected zone was non-uniform, and sites of locally-enhanced dissolution were occasionally observed. The progress of LBE dissolution attack was promoted by the interplay of certain steel microstructural features (grain boundaries, deformation twin laths, precipitates) with the dissolution corrosion process. The identified dissolution mechanisms were selective leaching leading to steel ferritization, and non-selective leaching; the latter was mainly observed in the solution-annealed steel. The maximum corrosion rate decreased with exposure time and was found to be inversely proportional to the depth of dissolution attack. - Highlights: •Dissolution corrosion was more severe in cold-deformed than solution-annealed 316L steels. •LBE penetration occurred along preferential paths in the steel microstructure. •The maximum dissolution rate was inversely proportionate to the depth of dissolution.

  20. A time averaged background compensator for Geiger-Mueller counters

    International Nuclear Information System (INIS)

    Bhattacharya, R.C.; Ghosh, P.K.

    1983-01-01

    The GM tube compensator described stores background counts to cancel an equal number of pulses from the measuring channel providing time averaged compensation. The method suits portable instruments. (orig.)

  1. Chemical vapour deposition at atmospheric pressure of graphene on molybdenum foil: Effect of annealing time on characteristics and corrosion stability of graphene coatings

    International Nuclear Information System (INIS)

    Naghdi, Samira; Jevremović, Ivana; Mišković-Stanković, Vesna; Rhee, Kyong Yop

    2016-01-01

    Highlights: • Atmospheric pressure chemical vapor deposition of graphene on molybdenum foils. • Quality and domain size of graphene layers increased with longer annealing times. • The number of graphene layers decreased with longer annealing times. • Graphene coatings on molybdenum foils exhibited corrosion inhibitive properties. - Abstract: In this work, the effect of pre-annealing of Mo substrate on the quality of graphene layers grown by chemical vapour deposition was investigated by X-ray diffraction, X-ray photoelectron spectroscopy, and Raman spectroscopy. Moreover, different electrochemical techniques were employed to investigate the corrosion stability of the graphene coated Mo in 0.1 M NaCl. Longer annealing time resulted in less defective graphene coatings with fewer layers. Graphene coating on the annealed Mo provided better protection against corrosion during the initial exposure times, while after prolonged exposure times, both graphene coatings on annealed and non-annealed Mo exhibited nearly the same corrosion inhibitive properties.

  2. Maximum likelihood window for time delay estimation

    International Nuclear Information System (INIS)

    Lee, Young Sup; Yoon, Dong Jin; Kim, Chi Yup

    2004-01-01

    Time delay estimation for the detection of leak location in underground pipelines is critically important. Because the exact leak location depends upon the precision of the time delay between sensor signals due to leak noise and the speed of elastic waves, the research on the estimation of time delay has been one of the key issues in leak lovating with the time arrival difference method. In this study, an optimal Maximum Likelihood window is considered to obtain a better estimation of the time delay. This method has been proved in experiments, which can provide much clearer and more precise peaks in cross-correlation functions of leak signals. The leak location error has been less than 1 % of the distance between sensors, for example the error was not greater than 3 m for 300 m long underground pipelines. Apart from the experiment, an intensive theoretical analysis in terms of signal processing has been described. The improved leak locating with the suggested method is due to the windowing effect in frequency domain, which offers a weighting in significant frequencies.

  3. A RED modified weighted moving average for soft real-time application

    Directory of Open Access Journals (Sweden)

    Domanśka Joanna

    2014-09-01

    Full Text Available The popularity of TCP/IP has resulted in an increase in usage of best-effort networks for real-time communication. Much effort has been spent to ensure quality of service for soft real-time traffic over IP networks. The Internet Engineering Task Force has proposed some architecture components, such as Active Queue Management (AQM. The paper investigates the influence of the weighted moving average on packet waiting time reduction for an AQM mechanism: the RED algorithm. The proposed method for computing the average queue length is based on a difference equation (a recursive equation. Depending on a particular optimality criterion, proper parameters of the modified weighted moving average function can be chosen. This change will allow reducing the number of violations of timing constraints and better use of this mechanism for soft real-time transmissions. The optimization problem is solved through simulations performed in OMNeT++ and later verified experimentally on a Linux implementation

  4. The consequences of time averaging for measuring temporal species turnover in the fossil record

    Science.gov (United States)

    Tomašových, Adam; Kidwell, Susan

    2010-05-01

    Modeling time averaging effects with simple simulations allows us to evaluate the magnitude of change in temporal species turnover that is expected to occur in long (paleoecological) time series with fossil assemblages. Distinguishing different modes of metacommunity dynamics (such as neutral, density-dependent, or trade-off dynamics) with time-averaged fossil assemblages requires scaling-up time-averaging effects because the decrease in temporal resolution and the decrease in temporal inter-sample separation (i.e., the two main effects of time averaging) substantially increase community stability relative to assemblages without or with weak time averaging. Large changes in temporal scale that cover centuries to millennia can lead to unprecedented effects on temporal rate of change in species composition. Temporal variation in species composition monotonically decreases with increasing duration of time-averaging in simulated fossil assemblages. Time averaging is also associated with the reduction of species dominance owing to the temporal switching in the identity of dominant species. High degrees of time averaging can cause that community parameters of local fossil assemblages converge to parameters of metacommunity rather that to parameters of individual local non-averaged communities. We find that the low variation in species composition observed among mollusk and ostracod subfossil assemblages can be explained by time averaging alone, and low temporal resolution and reduced temporal separation among assemblages in time series can thus explain a substantial part of the reduced variation in species composition relative to unscaled predictions of neutral model (i.e., species do not differ in birth, death, and immigration rates on per capita basis). The structure of time-averaged assemblages can thus provide important insights into processes that act over larger temporal scales, such as evolution of niches and dispersal, range-limit dynamics, taxon cycles, and

  5. 49 CFR 192.477 - Internal corrosion control: Monitoring.

    Science.gov (United States)

    2010-10-01

    ... 49 Transportation 3 2010-10-01 2010-10-01 false Internal corrosion control: Monitoring. 192.477... Control § 192.477 Internal corrosion control: Monitoring. If corrosive gas is being transported, coupons... internal corrosion. Each coupon or other means of monitoring internal corrosion must be checked two times...

  6. Extension of the time-average model to Candu refueling schemes involving reshuffling

    International Nuclear Information System (INIS)

    Rouben, Benjamin; Nichita, Eleodor

    2008-01-01

    Candu reactors consist of a horizontal non-pressurized heavy-water-filled vessel penetrated axially by fuel channels, each containing twelve 50-cm-long fuel bundles cooled by pressurized heavy water. Candu reactors are refueled on-line and, as a consequence, the core flux and power distributions change continuously. For design purposes, a 'time-average' model was developed in the 1970's to calculate the average over time of the flux and power distribution and to study the effects of different refueling schemes. The original time-average model only allows treatment of simple push-through refueling schemes whereby fresh fuel is inserted at one end of the channel and irradiated fuel is removed from the other end. With the advent of advanced fuel cycles and new Candu designs, novel refueling schemes may be considered, such as reshuffling discharged fuel from some channels into other channels, to achieve better overall discharge burnup. Such reshuffling schemes cannot be handled by the original time-average model. This paper presents an extension of the time-average model to allow for the treatment of refueling schemes with reshuffling. Equations for the extended model are presented, together with sample results for a simple demonstration case. (authors)

  7. Corrosion control when using secondary treated municipal wastewater as alternative makeup water for cooling tower systems.

    Science.gov (United States)

    Hsieh, Ming-Kai; Li, Heng; Chien, Shih-Hsiang; Monnell, Jason D; Chowdhury, Indranil; Dzombak, David A; Vidic, Radisav D

    2010-12-01

    Secondary treated municipal wastewater is a promising alternative to fresh water as power plant cooling water system makeup water, especially in arid regions. Laboratory and field testing was conducted in this study to evaluate the corrosiveness of secondary treated municipal wastewater for various metals and metal alloys in cooling systems. Different corrosion control strategies were evaluated based on varied chemical treatment. Orthophosphate, which is abundant in secondary treated municipal wastewater, contributed to more than 80% precipitative removal of phosphorous-based corrosion inhibitors. Tolyltriazole worked effectively to reduce corrosion of copper (greater than 95% inhibition effectiveness). The corrosion rate of mild steel in the presence of free chlorine 1 mg/L (as Cl2) was approximately 50% higher than in the presence of monochloramine 1 mg/L (as Cl2), indicating that monochloramine is a less corrosive biocide than free chlorine. The scaling layers observed on the metal alloys contributed to corrosion inhibition, which could be seen by comparing the mild steel 21-day average corrosion rate with the last 5-day average corrosion rate, the latter being approximately 50% lower than the former.

  8. Real Time Implementation of Incremental Fuzzy Logic Controller for Gas Pipeline Corrosion Control

    Directory of Open Access Journals (Sweden)

    Gopalakrishnan Jayapalan

    2014-01-01

    Full Text Available A robust virtual instrumentation based fuzzy incremental corrosion controller is presented to protect metallic gas pipelines. Controller output depends on error and change in error of the controlled variable. For corrosion control purpose pipe to soil potential is considered as process variable. The proposed fuzzy incremental controller is designed using a very simple control rule base and the most natural and unbiased membership functions. The proposed scheme is tested for a wide range of pipe to soil potential control. Performance comparison between the conventional proportional integral type and proposed fuzzy incremental controller is made in terms of several performance criteria such as peak overshoot, settling time, and rise time. Result shows that the proposed controller outperforms its conventional counterpart in each case. Designed controller can be taken in automode without waiting for initial polarization to stabilize. Initial startup curve of proportional integral controller and fuzzy incremental controller is reported. This controller can be used to protect any metallic structures such as pipelines, tanks, concrete structures, ship, and offshore structures.

  9. Accelerated Stress-Corrosion Testing

    Science.gov (United States)

    1986-01-01

    Test procedures for accelerated stress-corrosion testing of high-strength aluminum alloys faster and provide more quantitative information than traditional pass/fail tests. Method uses data from tests on specimen sets exposed to corrosive environment at several levels of applied static tensile stress for selected exposure times then subsequently tensile tested to failure. Method potentially applicable to other degrading phenomena (such as fatigue, corrosion fatigue, fretting, wear, and creep) that promote development and growth of cracklike flaws within material.

  10. Historical Data for Average Processing Time Until Hearing Held

    Data.gov (United States)

    Social Security Administration — This dataset provides historical data for average wait time (in days) from the hearing request date until a hearing was held. This dataset includes data from fiscal...

  11. Numerical method for time-dependent localized corrosion analysis with moving boundaries by combining the finite volume method and voxel method

    International Nuclear Information System (INIS)

    Onishi, Yuki; Takiyasu, Jumpei; Amaya, Kenji; Yakuwa, Hiroshi; Hayabusa, Keisuke

    2012-01-01

    Highlights: ► A novel numerical method to analyze time dependent localized corrosion is developed. ► It takes electromigration, mass diffusion, chemical reactions, and moving boundaries. ► Our method perfectly satisfies the conservation of mass and electroneutrality. ► The behavior of typical crevice corrosion is successfully simulated. ► Both verification and validation of our method are carried out. - Abstract: A novel numerical method for time-dependent localized corrosion analysis is presented. Electromigration, mass diffusion, chemical reactions, and moving boundaries are considered in the numerical simulation of localized corrosion of engineering alloys in an underwater environment. Our method combines the finite volume method (FVM) and the voxel method. The FVM is adopted in the corrosion rate calculation so that the conservation of mass is satisfied. A newly developed decoupled algorithm with a projection method is introduced in the FVM to decouple the multiphysics problem into the electrostatic, mass transport, and chemical reaction analyses with electroneutrality maintained. The polarization curves for the corroding metal are used as boundary conditions for the metal surfaces to calculate the corrosion rates. The voxel method is adopted in updating the moving boundaries of cavities without remeshing and mesh-to-mesh solution mapping. Some modifications of the standard voxel method, which represents the boundaries as zigzag-shaped surfaces, are introduced to generate smooth surfaces. Our method successfully reproduces the numerical and experimental results of a capillary electrophoresis problem. Furthermore, the numerical results are qualitatively consistent with the experimental results for several examples of crevice corrosion.

  12. Preparation and corrosion resistance of pulse electrodeposited Zn and Zn–SiC nanocomposite coatings

    International Nuclear Information System (INIS)

    Sajjadnejad, M.; Mozafari, A.; Omidvar, H.; Javanbakht, M.

    2014-01-01

    Highlights: • Zn and Zn–SiC coatings were obtained under different electrodeposition pulse conditions. • Effects of duty cycle, pulse frequency and applied current on SiC incorporation were investigated. • Potentiodynamic polarization tests were conducted to investigate corrosion behavior of coatings. • SiC incorporation enhances coatings corrosion behavior by filling gaps and defects. • Increasing pulse frequency and decreasing applied current favors SiC incorporation. - Abstract: Pure Zn and Zn matrix composite coatings containing nano-sized SiC particles with an average size of 50 nm were prepared from the zinc sulfate bath. The effects of the pulse frequency, maximum current density and duty cycle on the amount of particles embedded were examined. Electron microscopic studies revealed that the coating morphology was modified by the presence of SiC nanoparticles. In the presence of SiC nanoparticles deposit grows in outgrowth mode resulting in a very rough and porous microstructure. However, at very low and very high duty cycles a smooth and pore free microstructure was obtained. Corrosion resistance properties of the coatings were studied using potentiodynamic polarization technique in 1 M NaCl solution. It was established that presence of well-dispersed nanoparticles significantly improves corrosion resistance of the zinc by filling gaps and defects between zinc flakes and leading to a smoother surface. However, presence of the SiC nanoparticles led to a mixed microstructure with fine and coarse zinc flakes in some coatings, which presented a weak corrosion behavior. Incorporation of SiC nanoparticles enhanced hardness of the Zn coatings by fining deposit structure and through the dispersion hardening effect

  13. Improvements in zirconium alloy corrosion resistance

    International Nuclear Information System (INIS)

    Kilp, G.R.; Thornburg, D.R.; Comstock, R.J.

    1990-01-01

    The corrosion rates of a series of Zircaloy 4 and Zr-Nb alloys were evaluated in long-term (exceeding 500 days in some cases) autoclave tests. The testing was done at various conditions including 633 K (680 F) water, 633 K (650 F) water, 633 k (680 F) lithiated water (70 PPM/0.01 molal lithium), and 673 K (750 F) steam. Materials evaluated are from the following three groups: (1) standard Zircaloy 4; (2) Zircaloy 4 with tightened controls on chemistry limits and heat-treatment history; and (3) Zr-Nb alloys. To optimize the corrosion resistance of the Zircaloy 4 material, the effects of specific chemistry controls (tighter limits on nitrogen, oxygen, silicon, carbon and tin) were evaluated. Also the effects of the thermal history, as measured by integrated annealing of ''A'' time were determined. The ''A'' times ranged from 0.1x10 -18 (h) to 46x10 -18 (h). A material referred to as ''Improved Zircaloy 4'', having optimized chemistry and ''A'' time levels for reduced corrosion, has been developed and tested. This material has a reduced and more uniform corrosion rate compared to the prior Zircaloy 4 material. Alternative alloys were also evaluated for potential improvement in cladding corrosion resistance. ZIRLO TM material was chosen for development and has been included in the long-term corrosion testing. Demonstration fuel assemblies using ZIRLO cladding are now operating in a commercial reactor. The results for the various test conditions and compositions are reported and the relative corrosion characteristics summarized. Based on the BR-3 data, there is a ranking correspondence between in-reactor corrosion and autoclave testing in lithiated water. In particular, the ZIRLO material has significantly improved relative corrosion resistance in the lithiated water tests. Reduced Zircaloy-4 corrosion rates are also obtained from the tighter controls on the chemistry (specifically lower tin, nitrogen, and carbon; higher silicon; and reduced oxygen variability) and ''A

  14. Flow-induced corrosion behavior of absorbable magnesium-based stents.

    Science.gov (United States)

    Wang, Juan; Giridharan, Venkataraman; Shanov, Vesselin; Xu, Zhigang; Collins, Boyce; White, Leon; Jang, Yongseok; Sankar, Jagannathan; Huang, Nan; Yun, Yeoheung

    2014-12-01

    The aim of this work was to study corrosion behavior of magnesium (Mg) alloys (MgZnCa plates and AZ31 stents) under varied fluid flow conditions representative of the vascular environment. Experiments revealed that fluid hydrodynamics, fluid flow velocity and shear stress play essential roles in the corrosion behavior of absorbable magnesium-based stent devices. Flow-induced shear stress (FISS) accelerates the overall corrosion (including localized, uniform, pitting and erosion corrosions) due to the increased mass transfer and mechanical force. FISS increased the average uniform corrosion rate, the localized corrosion coverage ratios and depths and the removal rate of corrosion products inside the corrosion pits. For MgZnCa plates, an increase of FISS results in an increased pitting factor but saturates at an FISS of ∼0.15Pa. For AZ31 stents, the volume loss ratio (31%) at 0.056Pa was nearly twice that (17%) at 0Pa before and after corrosion. Flow direction has a significant impact on corrosion behavior as more severe pitting and erosion corrosion was observed on the back ends of the MgZnCa plates, and the corrosion product layer facing the flow direction peeled off from the AZ31 stent struts. This study demonstrates that flow-induced corrosion needs be understood so that Mg-based stents in vascular environments can be effectively designed. Copyright © 2014 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

  15. Corrosion mechanism applicable to biodegradable magnesium implants

    Energy Technology Data Exchange (ETDEWEB)

    Atrens, Andrej, E-mail: Andrejs.Atrens@uq.edu.au [University of Queensland, Division of Materials, Brisbane, Qld 4072 (Australia); Liu Ming; Zainal Abidin, Nor Ishida [University of Queensland, Division of Materials, Brisbane, Qld 4072 (Australia)

    2011-12-15

    Much of our understanding of the Mg corrosion mechanism is based on research using aggressive chloride based solutions like 3% NaCl, which are appropriate for understand the corrosion for applications such as auto construction. The chloride ions tend to cause break down of the partly protective surface film on the Mg alloy surface. The corrosion rate increases with exposure time until steady state is reached, which may take several weeks. An overview is provided of the aspects which determine the corrosion of Mg alloys: (i) measurement details; (ii) impurity elements Fe, Ni, Cu and Co; (iii) second phases; (iv) surface films and surface condition and (v) stress corrosion cracking (SCC). This understanding is used to help understand Mg corrosion for Mg as a biodegradable implant for medical applications. Solutions that elucidate these applications tend to form surface films and the corrosion rate tends to decrease with immersion time.

  16. Microstructural and corrosivity changes induced by nitrogen ion implantation on chromium films

    International Nuclear Information System (INIS)

    Shokouhy, A.; Larijani, M.M.; Ghoranneviss, M.; Hosseini G, S.H. Haji; Yari, M.; Sari, A.H.; Shahraki, M. Gholipur

    2006-01-01

    The chromium thin films were prepared using ion beam deposition on stainless steel 304. The chromium films were implanted by nitrogen ions after deposition at doses in the range of 4.5 x 10 17 to 2.7 x 10 18 N + /cm 2 and energy of 30 keV. The formation of nitride phases and corrosion behavior after nitrogen implantation were characterized by XRD and corrosion test, respectively. The results show that corrosion resistance rise, reach to a maximum at dose of 1.8 x 10 18 , and then fall down at higher doses. In addition, the effect of corrosion tests was analyzed using scanning electron microscopy (SEM)

  17. Corrosion Resistance of Laser Clads of Inconel 625 and Metco 41C

    Science.gov (United States)

    Němeček, Stanislav; Fidler, Lukáš; Fišerová, Pavla

    The present paper explores the impact of laser cladding parameters on the corrosion behaviour of the resulting surface. Powders of Inconel 625 and austenitic Metco 41C steel were deposited on steel substrate. It was confirmed that the level of dilution has profound impact on the corrosion resistance and that dilution has to be minimized. However, the chemical composition of the cladding is altered even in the course of the cladding process, a fact which is related to the increase in the substrate temperature. The cladding process was optimized to achieve maximum corrosion resistance. The results were verified and validated using microscopic observation, chemical analysis and corrosion testing.

  18. Electrochemical characterisation speeds up prediction of corrosion behaviour

    Energy Technology Data Exchange (ETDEWEB)

    Schuring, E.W.; Hooijmans, J.W. [ECN Environment and Energy Engineering, Petten (Netherlands)

    2013-04-15

    The contents of this presentation show the following elements: Introduction; Corrosion in real life; Why Electrochemical characterisation of corrosion; Applications (corrosion resistance coatings, corrosion behaviour (brazed) joints); Available electrochemical corrosion techniques; Standards; Conclusions. In the Conclusions the corrosion screening method is summarized: ECN method fast; within 1h -1 week results depending on test method; Fast pre-selection of promising materials/combinations (cost savings); Determining of corrosion initiation; Determination of corrosion mechanisms and propagation; Life time predictions possible; Strong combination with metallographic post-investigation; Ranking materials / constructions for corrosion performance.

  19. Effect of a high heat flux on the corrosion of 2 1/4 Cr-1 Mo steel in superheated steam

    International Nuclear Information System (INIS)

    Griess, J.C.; DeVan, J.H.; Maxwell, W.A.

    1977-01-01

    A series of corrosion tests was conducted to determine the effect of heat flux on the corrosion of 2 1 / 4 Cr-1 Mo steel in superheated steam. The tests were conducted with a constant heat flux of (126 kW/m 2 ) 40,000 Btu hr -1 ft -2 and surface temperatures varying from 950 to 1000 0 F (510 to 541 0 C) on each specimen. Specimens were exposed for varying lengths of time, ranging from 500 to 6000 hr. Essentially all the corrosion product oxide remained on the steel during the first 2000 hr, but after that time, exfoliation of the oxide began. The percentage of corrosion product oxide lost from the specimen increased with exposure time; about 33 percent was missing after 6000 hr. After an initial period of rapid corrosion, the average corrosion rate was constant at 1.8 mils/year (45 μm/year). In contrast, isothermal specimens exposed to superheated steam at 930 0 F (499 0 C) in the same test facility corroded at a decreasing rate throughout the test. Metallographic sections showed that, with heat transfer across the specimen-steam interface, both cracks and porosity developed in the oxide, even on short exposure, a face that was undoubtedly responsible for the early exfoliation of the oxide and the constant corrosion rate

  20. Depassivation and repassivation of austenitic stainless steels. Consequences on stress corrosion cracking

    International Nuclear Information System (INIS)

    Helie, M.; Desjardins, D.; Puiggali, M.; Petit, M.C.

    1983-06-01

    The influence of strain rate and solution temperature on depassivation and repassivation processes, and the consequences on stress corrosion cracking phenomenon are presented. The tests are performed in concentrated magnesium chloride solutions at various boiling temperatures (160 0 C, 153 0 C, 140 0 C, 130 0 C, 125 0 C, 110 0 C, 102 0 C) to which potassium dichromate is added in some cases. The depassivation and repassivation of the tested wires are analysed in term of current-time curves at fixed potential. The wire is placed into a ''corrosion cell'' with the boiling chloride solution on a tensile testing machine. Tests at 153 0 C on 304L and 309L stainless steels show that competition between passivation and depassivation depends on applied strain rate: at low strain rates rupture is mainly due to mechanical stress, at high strain rates the wire shows track of corrosion and the rupture is ductile. Between the two, stress corrosion cracking presents a maximum and in this case the rupture is mainly brittle. Influence of temperature shows the existence of a transitional temperature 130 0 C for a 304L. The cracking velocity is 100 times higher above 130 0 C than below and the cracking mode is transgranular and mainly intergranular below 130 0 C. Addition of potassium dichromate modifies both electrochemical and mechanical properties; it is more difficult to obtain a frank depassivation and the repassivation rate is higher

  1. Maximum vehicle cabin temperatures under different meteorological conditions

    Science.gov (United States)

    Grundstein, Andrew; Meentemeyer, Vernon; Dowd, John

    2009-05-01

    A variety of studies have documented the dangerously high temperatures that may occur within the passenger compartment (cabin) of cars under clear sky conditions, even at relatively low ambient air temperatures. Our study, however, is the first to examine cabin temperatures under variable weather conditions. It uses a unique maximum vehicle cabin temperature dataset in conjunction with directly comparable ambient air temperature, solar radiation, and cloud cover data collected from April through August 2007 in Athens, GA. Maximum cabin temperatures, ranging from 41-76°C, varied considerably depending on the weather conditions and the time of year. Clear days had the highest cabin temperatures, with average values of 68°C in the summer and 61°C in the spring. Cloudy days in both the spring and summer were on average approximately 10°C cooler. Our findings indicate that even on cloudy days with lower ambient air temperatures, vehicle cabin temperatures may reach deadly levels. Additionally, two predictive models of maximum daily vehicle cabin temperatures were developed using commonly available meteorological data. One model uses maximum ambient air temperature and average daily solar radiation while the other uses cloud cover percentage as a surrogate for solar radiation. From these models, two maximum vehicle cabin temperature indices were developed to assess the level of danger. The models and indices may be useful for forecasting hazardous conditions, promoting public awareness, and to estimate past cabin temperatures for use in forensic analyses.

  2. Corrosion behavior of low-alloy steel in the presence of Desulfotomaculum sp

    International Nuclear Information System (INIS)

    Cetin, Demet; Aksu, Mehmet Levent

    2009-01-01

    The objective of this study was to determine the effect of sulfate-reducing Desulfotomaculum sp. bacteria isolated from a crude oil field on the corrosion of low-alloy steel. The corrosion rate and mechanism were determined with the use of Tafel slopes, mass loss method and electrochemical impedance spectroscopy (EIS). The formation of the biofilm and the corrosion products on the steel surface was determined with scanning electron microscopy (SEM) micrographs and energy dispersive X-ray spectra (EDS) analysis. It was observed from the Tafel plots that the corrosion potential exhibited a cathodic shift that verifies an increase in the corrosion rates. The semicircles tended to open at lower frequencies in the Nyquist plots which indicates the rupture of the protective film. The corrosion current density reached its maximum value at the 14th hour after the inoculation and decreased afterwards. This was attributed to the accumulation of corrosion products on the surface.

  3. Corrosion measurement using flux gate magnetometer

    International Nuclear Information System (INIS)

    Rashdi Shah Ahmad; Chong Cheong Wei

    2001-01-01

    The ability of fluxgate magnetometer to detect and measure quantitatively the magnetic field generated by electrochemical corrosion is presented. In this study, each sample (iron plate) was exposed to a range of increasingly corrosive environment. During the exposure, we measured the magnetic field above the sample for specific duration of time. The result shows that there is a clear relationship between corrosivity of the environment and the change in magnitude of magnetic field that was generated by the corrosion reaction. Therefore, the measurement of magnetic field might be used to determine the corrosion rates. (Author)

  4. Measurement of weak magnetic field of corrosion current of isolated corrosion center

    Directory of Open Access Journals (Sweden)

    I. V. Bardin

    2015-01-01

    Full Text Available A very small magnetic field of corrosion current, of the order of 10−4 Oe, generated by isolated zinc inclusion in a copper platelet placed in electrolyte has been measured for the first time with a highly sensitive giant magneto-impedance magnetometer. The total corrosion current of the inclusion is estimated comparing the measured magnetic field distribution with corresponding theoretical calculation. The estimated value of the total corrosion current turns out to be in reasonable agreement with that one obtained in the standard gravimetric measurement.

  5. The Impact of Road Maintenance Substances on Metals Surface Corrosion

    Directory of Open Access Journals (Sweden)

    Jolita Petkuvienė

    2011-04-01

    Full Text Available The purpose of research is to assess changes in the visual metal surface due to the exposure of road maintenance salts and molasses (‘Safecote’. Chlorides of deicing salts (NaCl, CaCl2 are the main agents affecting soil and water resources as well as causing the corrosion of roadside metallic elements. Molasses (‘Safecote’ is offered as an alternative to deice road pavement by minimizing the corrosion of metal elements near the road. A laboratory experiment was carried out to immerse and spray metals with NaCl, CaCl2, NaCl:CaCl2 and NaCl:Safecote solutions. The obtained results showed that NaCl:Safecote solution had the lowest coating with corrosion products (the average 17±4 % of the surface. The solutions of NaCl, CaCl2 and NaCl:CaCl2 had the highest percentage rate of the corrosion product on the metal surface reaching an average of 33±5 %. Article in English

  6. Studies of corrosion resistance of Japanese steels in liquid lead-bismuth

    International Nuclear Information System (INIS)

    Kamata, Kin-ya; Ono, Hiroshi; Kitano, Teruaki; Ono, Mikinori

    2003-01-01

    Liquid lead-bismuth has attractive characteristics as a coolant in future fast reactors and Accelerator Driven Sub-critical Systems (ADS) applications. The corrosion behavior of structural materials in lead-bismuth eutectic is one of key problems in developing nuclear power plants and installations using lead-bismuth coolant. Our experiences with heat exchangers using liquid lead-bismuth and the results of corrosion tests of Japanese steels are reported in this paper. A series of corrosion tests was carried out in collaboration with the Institute of Physics and Power Engineering (IPPE). Test specimens of various Japanese steels were exposed in a non-isothermal forced circulation loop. The influence of maximum temperature and oxygen content in lead bismuth were chosen for study as the primary causes of corrosion in Japanese steels. After the corrosion tests, corrosion behavior was analyzed by visual inspection, measurement of weight loss and metallurgical examination of the microstructure of the corroded zone. The corrosion mechanism in liquid lead bismuth is discussed on the basis of the metallurgical examination of the corroded zone. (author)

  7. Nontoxic corrosion inhibitors for N80 steel in hydrochloric acid

    Directory of Open Access Journals (Sweden)

    M. Yadav

    2016-11-01

    Full Text Available The purpose of this paper is to evaluate the protective ability of 1-(2-aminoethyl-2-oleylimidazoline (AEOI and 1-(2-oleylamidoethyl-2-oleylimidazoline (OAEOI as corrosion inhibitors for N80 steel in 15% hydrochloric acid, which may find application as eco-friendly corrosion inhibitors in acidizing processes in petroleum industry. Different concentrations of synthesized inhibitors AEOI and OAEOI were added to the test solution (15% HCl and the corrosion inhibition of N80 steel in hydrochloric acid medium containing inhibitors was tested by weight loss, potentiodynamic polarization and AC impedance measurements. Influence of temperature (298–323 K on the inhibition behavior was studied. Surface studies were performed by using FTIR spectra and SEM. Both the inhibitors, AEOI and OAEOI at 150 ppm concentration show maximum efficiency 90.26% and 96.23%, respectively at 298 K in 15% HCl solution. Both the inhibitors act as mixed corrosion inhibitors. The adsorption of the corrosion inhibitors at the surface of N80 steel is the root cause of corrosion inhibition.

  8. Correlation between electrochemical impedance measurements and corrosion rate of magnesium investigated by real-time hydrogen measurement and optical imaging

    OpenAIRE

    Curioni, M.; Scenini, F.; Monetta, T.; Bellucci, F.

    2015-01-01

    The corrosion behaviour of magnesium in chloride-containing aqueous environment was investigated by potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) performed simultaneously with real-time hydrogen evolution measurements and optical imaging of the corroding surface. The potentiodynamic investigation revealed substantial deviations from linearity in close proximity of the corrosion potential. In particular, differences in the slope of the current/potential curves w...

  9. Maximum-likelihood methods for array processing based on time-frequency distributions

    Science.gov (United States)

    Zhang, Yimin; Mu, Weifeng; Amin, Moeness G.

    1999-11-01

    This paper proposes a novel time-frequency maximum likelihood (t-f ML) method for direction-of-arrival (DOA) estimation for non- stationary signals, and compares this method with conventional maximum likelihood DOA estimation techniques. Time-frequency distributions localize the signal power in the time-frequency domain, and as such enhance the effective SNR, leading to improved DOA estimation. The localization of signals with different t-f signatures permits the division of the time-frequency domain into smaller regions, each contains fewer signals than those incident on the array. The reduction of the number of signals within different time-frequency regions not only reduces the required number of sensors, but also decreases the computational load in multi- dimensional optimizations. Compared to the recently proposed time- frequency MUSIC (t-f MUSIC), the proposed t-f ML method can be applied in coherent environments, without the need to perform any type of preprocessing that is subject to both array geometry and array aperture.

  10. Application of a statistical methodology for the comprehension of corrosion phenomena on Phenix spent fuel pins

    International Nuclear Information System (INIS)

    Pantera, L.

    1992-11-01

    The maximum burnup of Phenix fuel elements is strongly conditioned by the internal corrosion of the steel cladding. This thesis is a part of a new study program on the corrosion phenomena. Based on the results of an experimental program during the years 1980-1990 its objective is the use of a statistical methodology for a better comprehension of the corrosion phenomena

  11. Influence of dispatching rules on average production lead time for multi-stage production systems.

    Science.gov (United States)

    Hübl, Alexander; Jodlbauer, Herbert; Altendorfer, Klaus

    2013-08-01

    In this paper the influence of different dispatching rules on the average production lead time is investigated. Two theorems based on covariance between processing time and production lead time are formulated and proved theoretically. Theorem 1 links the average production lead time to the "processing time weighted production lead time" for the multi-stage production systems analytically. The influence of different dispatching rules on average lead time, which is well known from simulation and empirical studies, can be proved theoretically in Theorem 2 for a single stage production system. A simulation study is conducted to gain more insight into the influence of dispatching rules on average production lead time in a multi-stage production system. We find that the "processing time weighted average production lead time" for a multi-stage production system is not invariant of the applied dispatching rule and can be used as a dispatching rule independent indicator for single-stage production systems.

  12. Thermal motion in proteins: Large effects on the time-averaged interaction energies

    International Nuclear Information System (INIS)

    Goethe, Martin; Rubi, J. Miguel; Fita, Ignacio

    2016-01-01

    As a consequence of thermal motion, inter-atomic distances in proteins fluctuate strongly around their average values, and hence, also interaction energies (i.e. the pair-potentials evaluated at the fluctuating distances) are not constant in time but exhibit pronounced fluctuations. These fluctuations cause that time-averaged interaction energies do generally not coincide with the energy values obtained by evaluating the pair-potentials at the average distances. More precisely, time-averaged interaction energies behave typically smoother in terms of the average distance than the corresponding pair-potentials. This averaging effect is referred to as the thermal smoothing effect. Here, we estimate the strength of the thermal smoothing effect on the Lennard-Jones pair-potential for globular proteins at ambient conditions using x-ray diffraction and simulation data of a representative set of proteins. For specific atom species, we find a significant smoothing effect where the time-averaged interaction energy of a single atom pair can differ by various tens of cal/mol from the Lennard-Jones potential at the average distance. Importantly, we observe a dependency of the effect on the local environment of the involved atoms. The effect is typically weaker for bulky backbone atoms in beta sheets than for side-chain atoms belonging to other secondary structure on the surface of the protein. The results of this work have important practical implications for protein software relying on free energy expressions. We show that the accuracy of free energy expressions can largely be increased by introducing environment specific Lennard-Jones parameters accounting for the fact that the typical thermal motion of protein atoms depends strongly on their local environment.

  13. Thermal motion in proteins: Large effects on the time-averaged interaction energies

    Energy Technology Data Exchange (ETDEWEB)

    Goethe, Martin, E-mail: martingoethe@ub.edu; Rubi, J. Miguel [Departament de Física Fonamental, Universitat de Barcelona, Martí i Franquès 1, 08028 Barcelona (Spain); Fita, Ignacio [Institut de Biologia Molecular de Barcelona, Baldiri Reixac 10, 08028 Barcelona (Spain)

    2016-03-15

    As a consequence of thermal motion, inter-atomic distances in proteins fluctuate strongly around their average values, and hence, also interaction energies (i.e. the pair-potentials evaluated at the fluctuating distances) are not constant in time but exhibit pronounced fluctuations. These fluctuations cause that time-averaged interaction energies do generally not coincide with the energy values obtained by evaluating the pair-potentials at the average distances. More precisely, time-averaged interaction energies behave typically smoother in terms of the average distance than the corresponding pair-potentials. This averaging effect is referred to as the thermal smoothing effect. Here, we estimate the strength of the thermal smoothing effect on the Lennard-Jones pair-potential for globular proteins at ambient conditions using x-ray diffraction and simulation data of a representative set of proteins. For specific atom species, we find a significant smoothing effect where the time-averaged interaction energy of a single atom pair can differ by various tens of cal/mol from the Lennard-Jones potential at the average distance. Importantly, we observe a dependency of the effect on the local environment of the involved atoms. The effect is typically weaker for bulky backbone atoms in beta sheets than for side-chain atoms belonging to other secondary structure on the surface of the protein. The results of this work have important practical implications for protein software relying on free energy expressions. We show that the accuracy of free energy expressions can largely be increased by introducing environment specific Lennard-Jones parameters accounting for the fact that the typical thermal motion of protein atoms depends strongly on their local environment.

  14. Corrosion inhibition of magnesium heated in wet air, by surface fluoridation; Inhibition de la corrosion du magnesium chauffe dans l'air humide, par fluoruration superficielle

    Energy Technology Data Exchange (ETDEWEB)

    Caillat, R.; Darras, R.; Leclercq, D. [Commissariat a l' Energie Atomique, Saclay (France).Centre d' Etudes Nucleaires

    1960-07-01

    The maximum temperature (350 deg. C) of magnesium corrosion resistance in wet air may be raised to 490-500 deg. C by the formation of a superficial fluoride film. This can be obtained by two different ways: either by addition of hydrofluoric acid to the corroding medium in a very small proportion such as 0,003 mg/litre; at atmospheric pressure, or by dipping the magnesium in a dilute aqueous solution of nitric and hydrofluoric acids at room temperature before exposing it to the corroding atmosphere. In both cases the corrosion inhibition is effective over a very long time, even several thousand hours. (author) [French] La temperature limite (350 deg. C) de resistance du magnesium a la corrosion par l'air humide, peut etre elevee jusque 490-500 deg. C par la formation d'une couche fluoruree superficielle. Deux procedes permettent d'obtenir ce resultat: l'atmosphere corrodante peut etre additionnee d'acide fluorhydrique a une concentration aussi faible que 0,003 mg/litre, a la pression atmospherique, ou bien le magnesium peut etre traite a froid, avant exposition a la corrosion, dans une solution aqueuse diluee d'acides nitrique et fluorhydrique. Dans les deux cas, la protection est assuree, meme pour de tres longues durees d'exposition: plusieurs milliers d'heures. (auteur)

  15. Pitting corrosion and structural reliability of corroding RC structures: Experimental data and probabilistic analysis

    International Nuclear Information System (INIS)

    Stewart, Mark G.; Al-Harthy, Ali

    2008-01-01

    A stochastic analysis is developed to assess the temporal and spatial variability of pitting corrosion on the reliability of corroding reinforced concrete (RC) structures. The structure considered herein is a singly reinforced RC beam with Y16 or Y27 reinforcing bars. Experimental data obtained from corrosion tests are used to characterise the probability distribution of pit depth. The RC beam is discretised into a series of small elements and maximum pit depths are generated for each reinforcing steel bar in each element. The loss of cross-sectional area, reduction in yield strength and reduction in flexural resistance are then inferred. The analysis considers various member spans, loading ratios, bar diameters and numbers of bars in a given cross-section, and moment diagrams. It was found that the maximum corrosion loss in a reinforcing bar conditional on beam collapse was no more than 16%. The probabilities of failure considering spatial variability of pitting corrosion were up to 200% higher than probabilities of failure obtained from a non-spatial analysis after 50 years of corrosion. This shows the importance of considering spatial variability in a structural reliability analysis for deteriorating structures, particularly for corroding RC beams in flexure

  16. Ageing temperature effect on inclination of martensite high strength steels EhP699, EhP678, EhP679 to corrosion cracking

    International Nuclear Information System (INIS)

    Rozenfel'd, I.L.; Spiridonov, V.B.; Konradi, M.V.; Krasnorutskaya, I.B.; Fridman, V.S.

    1979-01-01

    Stated are the data permitting to judge of the role of ageing temperature in the total number of factors, determining the inclination to corrosion cracking of high strength maraging steels, which contain chromium as a main alloying element. The inclination of the EhP699, EhP678, EhP679 steels to corrosion cracking was estimated on smooth stressed specimens in 3 % NaCl solution with the use of electrochemical polarization. The tensile stress resulted from deflection; anode and cathode current density was 10 mA/cm 2 . It is shown, that resistance to corrosion cracking depends on the ageing temperature: maximum sensitivity to corrosion cracking the steels manifest at the ageing temperatures, providing for maximum strength (470-500 deg). At the ageing temperatures by 20-30 deg over the temperature of this maximum the sensitivity to corrosion cracking disappears, which may result from the loss of coherence of strengthening phase in a matrix, from particle coagulation and stress relaxation in the crack peak

  17. Polyaspartic acid as a corrosion inhibitor for WE43 magnesium alloy

    OpenAIRE

    Lihui Yang; Yantao Li; Bei Qian; Baorong Hou

    2015-01-01

    The inhibition behavior of polyaspartic acid (PASP) as an environment-friendly corrosion inhibitor for WE43 magnesium alloy was investigated in 3.5 wt.% NaCl solution by means for EIS measurement, potentiodynamic polarization curve, and scanning electron microscopy. The results show that PASP can inhibit the corrosion of WE43 magnesium alloy. The maximum inhibition efficiency is achieved when PASP concentration is 400 ppm in this study.

  18. Synergy of corrosion activity and defects in weld bonds

    Directory of Open Access Journals (Sweden)

    Michal Černý

    2004-01-01

    Full Text Available Presented work evaluates synergism of atmosphere corrosive action and material defects. These defects appear not only during particular technological process of connecting of structural material but also during cooling and up to hundreds hours afterwards. The multiplication of degradation impact of defects in joint welds and heat-affected zone caused by activity of atmosphere acidic medium is simulated in condensation chambers. The verification is realized by use of mechanical uniaxial tension loading and following fractographic and metalgraphic analysis.The metal plasticity is sufficient factor to eliminate thermal stress in tough metal (11 373. This is reflected in more homogenous weld root area (with no cracks. The corrosion influence of environment is in case of such specimens limited to very slight decrease of weld maximum load. The ultimate strength value decreases approximately for 20MPa only in contrast to dramatic strength decrease in case of 11 503 material. Before metalographic examination was observed surprisingly great value of load capacity of spot welds. These welds were not ruptured nor in a single case even during maximum length of corrosion exploitation. The consequent material analysis discovered high qualitative material and strength properties of this kind of joint.

  19. Removal of corrosion products of construction materials in heat carrier

    International Nuclear Information System (INIS)

    1975-01-01

    A review of reported data has been made on the removal of structural material corrosion products into the heat-carrying agent of power reactors. The corrosion rate, and at the same time, removal of corrosion products into the heat-carrying agent (water) decreases with time. Thus, for example, the corrosion rate of carbon steel in boiling water at 250 deg C and O 2 concentration of 0.1 mg/1 after 3000 hr is 0.083 g/m 2 . day; after 9000 hr the corrosion rate has been reduced 2.5 times. Under static conditions the transfer rate of corrosion products into water has been smaller than in the stream and also depends on time. The corrosion rate of carbon steel under nuclear plant operating conditions is almost an order higher over that of steel Kh18N10T

  20. On the use of triazines as inhibitors of steel corrosion

    International Nuclear Information System (INIS)

    Sizaya, O.I.; Andrushko, A.P.

    2004-01-01

    A possibility of using substandard pesticides as a raw materials for synthesis of a set of triazines and also using them as a inhibitors of acidic corrosion of steel 20, as well as additions to epoxy powder coatings is considered. It is shown that triazines studied are inhibitors of acidic corrosion of steel 20. 2,4-di(ethylamino)-6-phenylhydrazono-1,3,5-triazine (In 4) has a maximum inhibiting effect among the studied compounds [ru

  1. Corrosion fatigue cracking behavior of Inconel 690 (TT) in secondary water of pressurized water reactors

    International Nuclear Information System (INIS)

    Xiao Jun; Chen Luyao; Qiu Shaoyu; Chen Yong; Lin Zhenxia; Fu Zhenghong

    2015-01-01

    Inconel 690 (TT) is one of the key materials for tubes of steam generators for pressurized water reactors, where it is susceptible to corrosion fatigue cracking. In this paper, the corrosion fatigue cracking behavior of Inconel 690 (TT) was investigated under small scale yielding conditions, in the simulated secondary water of pressurized water reactor. It was observed that the fatigue crack growth rate was accelerated by a maximum factor up to 3 in the simulated secondary water, comparing to that in room temperature air. In addition, it was found that the accelerating effect was influenced by out-of-plane cracking of corrosion fatigue cracks and also correlated with stress intensity factor range, maximum stress intensity factor and stress ratio. (authors)

  2. One-step fabrication of biomimetic superhydrophobic surface by electrodeposition on magnesium alloy and its corrosion inhibition.

    Science.gov (United States)

    Liu, Yan; Xue, Jingze; Luo, Dan; Wang, Huiyuan; Gong, Xu; Han, Zhiwu; Ren, Luquan

    2017-04-01

    A facile, rapid and one-step electrodeposition process has been employed to construct a superhydrophobic surface with micro/nano scale structure on a Mg-Sn-Zn (TZ51) alloy, which is expected to be applied as a biodegradable biomedical implant materials. By changing the electrodeposition time, the maximum contact angle of the droplet was observed as high as 160.4°±0.7°. The characteristics of the as-prepared surface were conducted by field emission scanning electron microscopy (FE-SEM), X-ray photoelectron spectroscopy (XPS) and Fourier-transform infrared spectroscopy (FT-IR). Besides, the anti-corrosion performance of the coatings in stimulated body fluid (SBF) solution were investigated by electrochemical measurement. The results demonstrated that the anti-corrosion property of superhydrophobic surface was greatly improved. This method show beneficial effects on the wettability and corrosion behavior, and therefore provides a efficient route to mitigate the undesirable rapid corrosion of magnesium alloy in favor of application for clinical field. Copyright © 2016 Elsevier Inc. All rights reserved.

  3. Generating pipeline networks for corrosion assessment

    Energy Technology Data Exchange (ETDEWEB)

    Ferguson, J. [Cimarron Engineering Ltd., Calgary, AB (Canada)

    2008-07-01

    Production characteristics and gas-fluid compositions of fluids must be known in order to assess pipelines for internal corrosion risk. In this study, a gathering system pipeline network was built in order to determine corrosion risk for gathering system pipelines. Connections were established between feeder and collector lines in order measure upstream production and the weighted average of the upstream composition of each pipeline in the system. A Norsok M-506 carbon dioxide (CO{sub 2}) corrosion rate model was used to calculate corrosion rates. A spreadsheet was then used to tabulate the obtained data. The analysis used straight lines drawn between the 'from' and 'to' legal sub-division (LSD) endpoints in order to represent pipelines on an Alberta township system (ATS) and identify connections between pipelines. Well connections were established based on matching surface hole location and 'from' LSDs. Well production, composition, pressure, and temperature data were sourced and recorded as well attributes. XSL hierarchical computations were used to determine the production and composition properties of the commingled inflows. It was concluded that the corrosion assessment process can identify locations within the pipeline network where potential deadlegs branched off from flowing pipelines. 4 refs., 2 tabs., 2 figs.

  4. Effect of chloride concentration and pH on pitting corrosion of waste package container materials

    International Nuclear Information System (INIS)

    Roy, A.K.; Fleming, D.L.; Gordon, S.R.

    1996-12-01

    Electrochemical cyclic potentiodynamic polarization experiments were performed on several candidate waste package container materials to evaluate their susceptibility to pitting corrosion at 90 degrees C in aqueous environments relevant to the potential underground high-level nuclear waste repository. Results indicate that of all the materials tested, Alloy C-22 and Ti Grade-12 exhibited the maximum corrosion resistance, showing no pitting or observable corrosion in any environment tested. Efforts were also made to study the effect of chloride ion concentration and pH on the measured corrosion potential (Ecorr), critical pitting and protection potential values

  5. Electrochemical and Corrosion Properties of Aluminum Brass in Seawater Desalination Environments

    Directory of Open Access Journals (Sweden)

    Hong JU

    2017-11-01

    Full Text Available The corrosion behavior and mechanism of aluminum brass (HAl77-2 in seawater desalination plant were investigated using electrochemical measurement, Scanning Electronic Microscope (SEM and Energy Dispersive X-ray spectroscopy (EDX analysis. The electrochemical results revealed that the corrosion of HAl77-2 in the desalination artificial seawater depended on chloride ion concentrations, displaying a maximum with a chloride ion concentration of 2.3 wt.%. Corrosion rate of HAl77-2 initial increased and subsequently decreased with the increasing of chloride ion concentration. Moreover, corrosion of HAl77-2 becomes more severe when temperature rises. The above results obtained by electrochemical impedance spectroscopy and potentiodynamic polarization tests were in a good agreement. The results of SEM and EDX methods showed selective localized corrosion appeared remarkably on the surface of HAl77-2.DOI: http://dx.doi.org/10.5755/j01.ms.23.4.17170

  6. Fitting a function to time-dependent ensemble averaged data.

    Science.gov (United States)

    Fogelmark, Karl; Lomholt, Michael A; Irbäck, Anders; Ambjörnsson, Tobias

    2018-05-03

    Time-dependent ensemble averages, i.e., trajectory-based averages of some observable, are of importance in many fields of science. A crucial objective when interpreting such data is to fit these averages (for instance, squared displacements) with a function and extract parameters (such as diffusion constants). A commonly overlooked challenge in such function fitting procedures is that fluctuations around mean values, by construction, exhibit temporal correlations. We show that the only available general purpose function fitting methods, correlated chi-square method and the weighted least squares method (which neglects correlation), fail at either robust parameter estimation or accurate error estimation. We remedy this by deriving a new closed-form error estimation formula for weighted least square fitting. The new formula uses the full covariance matrix, i.e., rigorously includes temporal correlations, but is free of the robustness issues, inherent to the correlated chi-square method. We demonstrate its accuracy in four examples of importance in many fields: Brownian motion, damped harmonic oscillation, fractional Brownian motion and continuous time random walks. We also successfully apply our method, weighted least squares including correlation in error estimation (WLS-ICE), to particle tracking data. The WLS-ICE method is applicable to arbitrary fit functions, and we provide a publically available WLS-ICE software.

  7. The corrosion protection of 6061-T6 aluminum by a polyurethane-sealed anodized coat

    Science.gov (United States)

    Danford, M. D.

    1990-01-01

    The corrosion protection of 6061-T6 anodized aluminum afforded by a newly patented polyurethane seal was studied using the ac impedance technique. Values of the average corrosion rates over a 27-day exposure period in 3.5 percent NaCl solutions at pH 5.2 and pH 9.5 compared very favorably for Lockheed-prepared polyurethane-sealed and dichromate-sealed coats of the same thickness. Average corrosion rates for both specimens over the first 7 days of exposure compared well with those for a hard anodized, dichromate-sealed coat, but rose well above those for the hard anodized coat over the entire 27-day period. This is attributed both to the greater thickness of the hard anodized coat, and possibly to its inherently better corrosion protective capability.

  8. Polyaspartic acid as a green corrosion inhibitor for carbon steel

    Energy Technology Data Exchange (ETDEWEB)

    Cui, R. [Department of Chemistry, Hebei Normal University, Shijiazhuang 050016 (China); Department of Chemistry and Materials Engineering, Changshu Institute of Technology, Changshu 215500 (China); Gu, N.; Li, C. [Department of Chemistry, Hebei Normal University, Shijiazhuang 050016 (China)

    2011-04-15

    The inhibitor effect of the environmentally friendly corrosion inhibitor polyaspartic acid (PASP) on the corrosion of carbon steel in 0.5 M H{sub 2}SO{sub 4} was investigated by weight loss, potentiodynamic polarization, electrochemical impedance spectroscopy (EIS), and scanning electron microscopy (SEM). Polarization curve results clearly reveal the fact that PASP is a good anode-type inhibitor. EIS results confirm its corrosion inhibition ability. The inhibition efficiency increases with increasing PASP concentration, and the maximum inhibition efficiency was 80.33% at 10 C. SEM reveals that a protective film forms on the surface of the inhibited sample. The adsorption of this inhibitor is found to follow the Freundlich adsorption isotherm. A mechanism is proposed to explain the inhibitory action of the corrosion inhibitor. (Copyright copyright 2011 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  9. Effect of tank geometry on its average performance

    Science.gov (United States)

    Orlov, Aleksey A.; Tsimbalyuk, Alexandr F.; Malyugin, Roman V.; Leontieva, Daria A.; Kotelnikova, Alexandra A.

    2018-03-01

    The mathematical model of non-stationary filling of vertical submerged tanks with gaseous uranium hexafluoride is presented in the paper. There are calculations of the average productivity, heat exchange area, and filling time of various volumes tanks with smooth inner walls depending on their "height : radius" ratio as well as the average productivity, degree, and filling time of horizontal ribbing tank with volume 6.10-2 m3 with change central hole diameter of the ribs. It has been shown that the growth of "height / radius" ratio in tanks with smooth inner walls up to the limiting values allows significantly increasing tank average productivity and reducing its filling time. Growth of H/R ratio of tank with volume 1.0 m3 to the limiting values (in comparison with the standard tank having H/R equal 3.49) augments tank productivity by 23.5 % and the heat exchange area by 20%. Besides, we have demonstrated that maximum average productivity and a minimum filling time are reached for the tank with volume 6.10-2 m3 having central hole diameter of horizontal ribs 6.4.10-2 m.

  10. Corrosion Inhibitor of Carbon Steel from Onion Peel Extract

    Directory of Open Access Journals (Sweden)

    Muhammad Samsudin Asep

    2018-01-01

    Full Text Available Carbon steels composed by two main elements, they are iron (Fe and carbon (C elements which widely used in industrial because of its resistance and more affordable than stainless steel, but their weakness is they have low corrosion resistance. One way to modify carbon steel is by coating them with antioxidant compounds that can delay, slow down, and prevent lipid oxidation process, which obtained from onion peel extract. Several studies on corrosion inhibitors have been performed. However, the efficiency was not reach the optimum. This study aims to examine the effect of onion peel extract concentration on the efficiency of corrosion inhibitor and characterization of the green corrosion inhibitor from onion peel extract. This research method begins by extracting onion peel to 200 ml solvent which we use aquadest and methanol and mixed with 5 grams of crushed onion peel, then let them be extracted for 60 minutes with room temperature. Once it was filtered and the solution obtained, followed by evaporating process with rotary evaporator to decrease the content of solvent. The product is ready to be used as a green corrosion inhibitor of carbon steel in 1 mol/L HCl. While the analysis used is HPLC qualitative analysis, and electroplatting process. The impedance is measured at a frequency of 100 kHz to 4 mHz with an AC current of 10mV. Inhibitor concentrations are vary between 2 ml and 4 ml of onion peel extract. Electroplatting is done within 30 minutes with 10 minutes each checking time. Furthermore, quantitative analysis was done for the analysis of corrosion rate and weight loss. Based on HPLC analysis, it is known that the extract of onion peel contains 1mg/L of quercetin, which is belong to flavonoid group as green inhibitor. While electroplatting process, aquadest solvent having average efficiency of 99,57% for 2 ml of extract, and 99,60% for 4 ml of extract. Methanol solvent having average efficiency of 99,52% for 2 ml of extract and 99

  11. Atmospheric corrosion of low carbon steel in a polar marine environment. Study of the effect of wind regime; Corrosion atmosferica del acero bajo en carbono en un ambiente marino polar. Estudio del efecto del regimen de vientos

    Energy Technology Data Exchange (ETDEWEB)

    Rivero, S.; Chico, B.; Fuente, D. de la; Morcillo, M.

    2007-07-01

    The present work studies the atmospheric corrosion of carbon steel (UNE-EN 10130) in a sub-polar marine environment (Artigas Antarctic Scientific Base (BCAA), Uruguay) as a function of site atmospheric salinity and exposure time. A linear relationship is established between corrosion rate and airborne salinity deposition rate, valid in the deposition range encountered (125-225 mg Cl-l/m{sup 2}.d) and a bi logarithmic relationship established between corrosion and exposure time (1-4 years). Atmospheric salinity is related with the monthly wind speed average, based on the concept of the wind run. chloride ion deposition rates of less than 300 mg Cl-l/m{sup 2}.d are related with remote (oceanic) winds and coastal winds basically of speeds between 1-40 km/h, while higher deposition rates (300-700 mg Cl-/m{sup 2}.d) correspond to coastal marine winds of a certain persistence with speeds of between 41-80 km/h. (Author) 39 refs.

  12. Bacillus sp. Acting as Dual Role for Corrosion Induction and Corrosion Inhibition with Carbon Steel (CS

    Directory of Open Access Journals (Sweden)

    Santosh K. Karn

    2017-10-01

    Full Text Available Present work investigated the role of five different bacteria species as a corrosion inducer as well as corrosion inhibitor with carbon steel (CS. We observed the ability of different bacteria species on the metal surface attachment, biofilm formation, and determined Peroxidase, Catalase enzyme activity in the detached biofilm from the CS surface. We found that each strain has diverse conduct for surface attachment like DS1 3.3, DS2 2.5, DS3 4.3, DS4 4.0, and DS5 4.71 log cfu/cm2 and for biofilm 8.3 log cfu/cm2. The enzyme Peroxidase, Catalase was found in huge concentration inside the biofilm Peroxidase was maximum for DS4 36.0 U/ml and least for DS3 19.54 U/ml. Whereas, Catalase was highest for DS4, DS5 70.14 U/ml and least 57.2 U/ml for DS2. Scanning electron microscopy (SEM was conducted to examine the biofilm and electrochemical impedance spectroscopy (EIS were utilized to observe corrosion in the presence of bacteria. The electrochemical results confirmed that DS1, DS3, DS4, and DS5 strains have statistically significant MIC-factors (Microbially Influenced Corrosion of 5.46, 8.51, 2.36, and 1.04, while DS2 protective effect factor of 0.89. Weight reduction results with carbon steel likewise supports that corrosion was initiated by DS1 and DS3, while DS2 and DS5 have no any impact though with DS4 we watched less weight reduction however assumed no role in the corrosion. We established the relation of Peroxidase enzyme activity of the isolates. DS1, DS3 and having Peroxidase in the range 22.18, 19.54 U/ml which induce the corrosion whereas DS2 and DS5 having 28.57 and 27.0 U/ml has no any effect and DS4 36 U/ml has inhibitory effect, increasing concentration inhibiting the corrosion. For Catalase DS1, DS3 have 67.28, 61.57 U/ml which induce corrosion while DS2 and DS5 57.71 and 59.14 U/ml also has no effect whereas DS4 70.14 U/ml can inhibit corrosion. Results clearly express that in a specific range both enzymes can induce the corrosion

  13. Local Times of Galactic Cosmic Ray Intensity Maximum and Minimum in the Diurnal Variation

    Directory of Open Access Journals (Sweden)

    Su Yeon Oh

    2006-06-01

    Full Text Available The Diurnal variation of galactic cosmic ray (GCR flux intensity observed by the ground Neutron Monitor (NM shows a sinusoidal pattern with the amplitude of 1sim 2 % of daily mean. We carried out a statistical study on tendencies of the local times of GCR intensity daily maximum and minimum. To test the influences of the solar activity and the location (cut-off rigidity on the distribution in the local times of maximum and minimum GCR intensity, we have examined the data of 1996 (solar minimum and 2000 (solar maximum at the low-latitude Haleakala (latitude: 20.72 N, cut-off rigidity: 12.91 GeV and the high-latitude Oulu (latitude: 65.05 N, cut-off rigidity: 0.81 GeV NM stations. The most frequent local times of the GCR intensity daily maximum and minimum come later about 2sim3 hours in the solar activity maximum year 2000 than in the solar activity minimum year 1996. Oulu NM station whose cut-off rigidity is smaller has the most frequent local times of the GCR intensity maximum and minimum later by 2sim3 hours from those of Haleakala station. This feature is more evident at the solar maximum. The phase of the daily variation in GCR is dependent upon the interplanetary magnetic field varying with the solar activity and the cut-off rigidity varying with the geographic latitude.

  14. Corrosion behaviour of laser surface melted magnesium alloy AZ91D

    International Nuclear Information System (INIS)

    Taltavull, C.; Torres, B.; Lopez, A.J.; Rodrigo, P.; Otero, E.; Atrens, A.; Rams, J.

    2014-01-01

    A high power diode laser (HPDL) was used to produce laser surface melting (LSM) treatments on the surface of the Mg alloy AZ91D. Different treatments with different microstructures were produced by varying the laser-beam power and laser-scanning speed. Corrosion evaluation, using hydrogen evolution and electrochemical measurements, led to a relationship between microstructure and corrosion. Most corrosion rates for LSM treated specimens were within the scatter of the as-received AZ91D, whereas some treatments gave higher corrosion rates and some of the samples had corrosion rates lower than the average of the corrosion rate for AZ91D. There were differences in corroded surface morphology. Nevertheless laser treatments introduced surface discontinuities, which masked the effect of the microstructure. Removing these surface defects decreased the corrosion rate for the laser-treated samples. - Highlights: • Corrosion behavior of AZ91D Mg alloys is intimately related with its microstructure. • Laser surface melting treatments allows surface modification of the microstructure. • Different laser parameters can achieve different microstructures. • Controlling laser parameters can produce different corrosion rates and morphologies. • Increase of surface roughness due to laser treatment is relevant to the corrosion rate

  15. Corrosion Monitoring System

    Energy Technology Data Exchange (ETDEWEB)

    Dr. Russ Braunling

    2004-10-31

    The Corrosion Monitoring System (CMS) program developed and demonstrated a continuously on-line system that provides real-time corrosion information. The program focused on detecting pitting corrosion in its early stages. A new invention called the Intelligent Ultrasonic Probe (IUP) was patented on the program. The IUP uses ultrasonic guided waves to detect small defects and a Synthetic Aperture Focusing Technique (SAFT) algorithm to provide an image of the pits. Testing of the CMS demonstrated the capability to detect pits with dimensionality in the sub-millimeter range. The CMS was tested in both the laboratory and in a pulp and paper industrial plant. The system is capable of monitoring the plant from a remote location using the internet.

  16. Electrochemical noise based corrosion monitoring: FY 2001 final report

    International Nuclear Information System (INIS)

    EDGAR, C.

    2001-01-01

    Underground storage tanks made of mild steel are used to contain radioactive waste generated by plutonium production at the Hanford Site. Corrosion of the walls of these tanks is a major issue. Corrosion monitoring and control are currently provided at the Hanford Site through a waste chemistry sampling and analysis program. In this process, tank waste is sampled, analyzed and compared to a selection of laboratory exposures of coupons in simulated waste. Tank wall corrosion is inferred by matching measured tank chemistries to the results of the laboratory simulant testing. This method is expensive, time consuming, and does not yield real-time data. Corrosion can be monitored through coupon exposure studies and a variety of electrochemical techniques. A small number of these techniques have been tried at Hanford and elsewhere within the DOE complex to determine the corrosivity of nuclear waste stored in underground tanks [1]. Coupon exposure programs, linear polarization resistance (LPR), and electrical resistance techniques have all been tried with limited degrees of success. These techniques are most effective for monitoring uniform corrosion, but are not well suited for early detection of localized forms of corrosion such as pitting and stress corrosion cracking (SCC). Pitting and SCC have been identified as the most likely modes of corrosion failure for Hanford Double Shell Tanks (DST'S) [2-3]. Over the last 20 years, a new corrosion monitoring system has shown promise in detecting localized corrosion and measuring uniform corrosion rates in process industries [4-20]. The system measures electrochemical noise (EN) generated by corrosion. The term EN is used to describe low frequency fluctuations in current and voltage associated with corrosion. In their most basic form, EN-based corrosion monitoring systems monitor and record fluctuations in current and voltage over time from electrodes immersed in an environment of interest. Laboratory studies and field

  17. The corrosion of depleted uranium in terrestrial and marine environments

    International Nuclear Information System (INIS)

    Toque, C.; Milodowski, A.E.; Baker, A.C.

    2014-01-01

    Depleted Uranium alloyed with titanium is used in armour penetrating munitions that have been fired in a number of conflict zones and testing ranges including the UK ranges at Kirkcudbright and Eskmeals. The study presented here evaluates the corrosion of DU alloy cylinders in soil on these two UK ranges and in the adjacent marine environment of the Solway Firth. The estimated mean initial corrosion rates and times for complete corrosion range from 0.13 to 1.9 g cm −2 y −1 and 2.5–48 years respectively depending on the particular physical and geochemical environment. The marine environment at the experimental site was very turbulent. This may have caused the scouring of corrosion products and given rise to a different geochemical environment from that which could be easily duplicated in laboratory experiments. The rate of mass loss was found to vary through time in one soil environment and this is hypothesised to be due to pitting increasing the surface area, followed by a build up of corrosion products inhibiting further corrosion. This indicates that early time measurements of mass loss or corrosion rate may be poor indicators of late time corrosion behaviour, potentially giving rise to incorrect estimates of time to complete corrosion. The DU alloy placed in apparently the same geochemical environment, for the same period of time, can experience very different amounts of corrosion and mass loss, indicating that even small variations in the corrosion environment can have a significant effect. These effects are more significant than other experimental errors and variations in initial surface area. -- Highlights: ► In-situ experiments were conducted to evaluate corrosion rates of depleted uranium. ► Samples were corroded in marine sediments, open sea water and two terrestrial soils. ► The depleted uranium titanium alloy corroded fastest in the marine environments. ► Rates of mass loss can vary through time if corrosion products are not removed.

  18. Experimental and theoretical studies of benzoxazines corrosion inhibitors

    Directory of Open Access Journals (Sweden)

    Abdulhadi Kadhim

    Full Text Available 2-Methyl-4H-benzo[d][1,3]oxazin-4-one (BZ1 and 3-amino-2-methylquinazolin-4(3H-one (BZ2 were evaluated for their corrosion inhibition properties on mild steel (MS in hydrochloric acid solution by weight loss technique and scanning electron microscopy. Results show the inhibition efficiency values depend on the amount of nitrogen in the inhibitor, the inhibitor concentration and the inhibitor molecular weight with maximum inhibition efficiency of 89% and 65% for BZ2 and BZ1 at highest concentration of the compounds. Keywords: Methylquinazoline, Benzoxazines, Corrosion, Inhibitors

  19. Modeling of Corrosion-induced Concrete Damage

    DEFF Research Database (Denmark)

    Thybo, Anna Emilie A.; Michel, Alexander; Stang, Henrik

    2013-01-01

    In the present paper a finite element model is introduced to simulate corrosion-induced damage in concrete. The model takes into account the penetration of corrosion products into the concrete as well as non-uniform formation of corrosion products around the reinforcement. To ac-count for the non...... of corrosion products affects both the time-to cover cracking and the crack width at the concrete surface.......In the present paper a finite element model is introduced to simulate corrosion-induced damage in concrete. The model takes into account the penetration of corrosion products into the concrete as well as non-uniform formation of corrosion products around the reinforcement. To ac-count for the non......-uniform formation of corrosion products at the concrete/reinforcement interface, a deterministic approach is used. The model gives good estimates of both deformations in the con-crete/reinforcement interface and crack width when compared to experimental data. Further, it is shown that non-uniform deposition...

  20. A multiscale constitutive model for intergranular stress corrosion cracking in type 304 austenitic stainless steel

    International Nuclear Information System (INIS)

    Siddiq, A; Rahimi, S

    2013-01-01

    Intergranular stress corrosion cracking (IGSCC) is a fracture mechanism in sensitised austenitic stainless steels exposed to critical environments where the intergranular cracks extends along the network of connected susceptible grain boundaries. A constitutive model is presented to estimate the maximum intergranular crack growth by taking into consideration the materials mechanical properties and microstructure characters distribution. This constitutive model is constructed based on the assumption that each grain is a two phase material comprising of grain interior and grain boundary zone. The inherent micro-mechanisms active in the grain interior during IGSCC is based on crystal plasticity theory, while the grain boundary zone has been modelled by proposing a phenomenological constitutive model motivated from cohesive zone modelling approach. Overall, response of the representative volume is calculated by volume averaging of individual grain behaviour. Model is assessed by performing rigorous parametric studies, followed by validation and verification of the proposed constitutive model using representative volume element based FE simulations reported in the literature. In the last section, model application is demonstrated using intergranular stress corrosion cracking experiments which shows a good agreement

  1. Corrosion Inhibition of Carbon Steel in HCl Solution by Some Plant Extracts

    Directory of Open Access Journals (Sweden)

    Ambrish Singh

    2012-01-01

    Full Text Available The strict environmental legislations and increasing ecological awareness among scientists have led to the development of “green” alternatives to mitigate corrosion. In the present work, literature on green corrosion inhibitors has been reviewed, and the salient features of our work on green corrosion inhibitors have been highlighted. Among the studied leaves, extract Andrographis paniculata showed better inhibition performance (98% than the other leaves extract. Strychnos nuxvomica showed better inhibition (98% than the other seed extracts. Moringa oleifera is reflected as a good corrosion inhibitor of mild steel in 1 M HCl with 98% inhibition efficiency among the studied fruits extract. Bacopa monnieri showed its maximum inhibition performance to be 95% at 600 ppm among the investigated stem extracts. All the reported plant extracts were found to inhibit the corrosion of mild steel in acid media.

  2. Failure prediction for Crack-in-Corrosion defects in natural gas transmission pipelines

    International Nuclear Information System (INIS)

    Bedairi, B.; Cronin, D.; Hosseini, A.; Plumtree, A.

    2012-01-01

    Cracks occurring coincidentally with corrosion (Crack-in-Corrosion or CIC), represent a new hybrid defect in pipelines that are not directly addressed in the current codes or assessment methods. To understand the failure response of these defects, the finite element method using an elastic–plastic fracture mechanics approach was applied to predict the failure pressures of comparable crack, corrosion and CIC defects in 508 mm diameter pipe with 5.7 mm wall thickness. Failure pressure predictions were made based on measured tensile, Charpy impact and J testing data, and validated using experimental rupture tests. Plastic collapse was predicted for corrosion and crack defects using the critical strength based on the material tensile strength, whereas fracture was predicted using the measured J 0.2 value. The model predictions were found to be conservative for the CIC defects (17.4% on average), 12.4% conservative for crack-only defects, and 3.2% conservative for corrosion defects compared to the experimental tests, demonstrating the applicability of the material-based failure criteria. For the defects considered in this study, all were predicted to fail by plastic collapse. The finite element method provided less conservative predictions than existing corrosion or crack-based analytical methods. Highlights: ► Cracks occurring coincidentally with corrosion represent a new hybrid defect in pipelines. ► Existing methods for prediction corrosion and crack defect failure pressures are conservative. ► The FE method can provide improved prediction of rupture pressure using actual material properties. ► Failure was predicted using FE with a critical stress for plastic collapse and J value for fracture. ► FE failure pressure predictions for crack in corrosion defects were 17% conservative on average.

  3. Polyaspartic acid as a corrosion inhibitor for WE43 magnesium alloy

    Directory of Open Access Journals (Sweden)

    Lihui Yang

    2015-03-01

    Full Text Available The inhibition behavior of polyaspartic acid (PASP as an environment-friendly corrosion inhibitor for WE43 magnesium alloy was investigated in 3.5 wt.% NaCl solution by means for EIS measurement, potentiodynamic polarization curve, and scanning electron microscopy. The results show that PASP can inhibit the corrosion of WE43 magnesium alloy. The maximum inhibition efficiency is achieved when PASP concentration is 400 ppm in this study.

  4. Comparison of Interpolation Methods as Applied to Time Synchronous Averaging

    National Research Council Canada - National Science Library

    Decker, Harry

    1999-01-01

    Several interpolation techniques were investigated to determine their effect on time synchronous averaging of gear vibration signals and also the effects on standard health monitoring diagnostic parameters...

  5. The corrosion of depleted uranium in terrestrial and marine environments.

    Science.gov (United States)

    Toque, C; Milodowski, A E; Baker, A C

    2014-02-01

    Depleted Uranium alloyed with titanium is used in armour penetrating munitions that have been fired in a number of conflict zones and testing ranges including the UK ranges at Kirkcudbright and Eskmeals. The study presented here evaluates the corrosion of DU alloy cylinders in soil on these two UK ranges and in the adjacent marine environment of the Solway Firth. The estimated mean initial corrosion rates and times for complete corrosion range from 0.13 to 1.9 g cm(-2) y(-1) and 2.5-48 years respectively depending on the particular physical and geochemical environment. The marine environment at the experimental site was very turbulent. This may have caused the scouring of corrosion products and given rise to a different geochemical environment from that which could be easily duplicated in laboratory experiments. The rate of mass loss was found to vary through time in one soil environment and this is hypothesised to be due to pitting increasing the surface area, followed by a build up of corrosion products inhibiting further corrosion. This indicates that early time measurements of mass loss or corrosion rate may be poor indicators of late time corrosion behaviour, potentially giving rise to incorrect estimates of time to complete corrosion. The DU alloy placed in apparently the same geochemical environment, for the same period of time, can experience very different amounts of corrosion and mass loss, indicating that even small variations in the corrosion environment can have a significant effect. These effects are more significant than other experimental errors and variations in initial surface area. Copyright © 2013. Published by Elsevier Ltd.

  6. Comparative analysis of adsorption and corrosion inhibitive properties of ethanol extract of Dialium Guineense leaves for mild steel in 0.5 M HCl

    OpenAIRE

    Shola Elijah Adeniji; Bamigbola Abiola Akindehinde

    2018-01-01

    Adsorption and corrosion inhibitive properties of ethanol extract of Dialium guineense leaves for mild steel in 0.5M HCl was studied using the gravimetric method. The results showed that the ethanol extract of Dialium guineense leaves is a good corrosion inhibitor for mild steel in 0.5 M HCl. The inhibition efficiency was found to increase with increase in the concentration of ethanol extract of Dialium guineense leaves up to the maximum of 92 %, but at the same time it decreased as the tempe...

  7. Optimal bounds and extremal trajectories for time averages in nonlinear dynamical systems

    Science.gov (United States)

    Tobasco, Ian; Goluskin, David; Doering, Charles R.

    2018-02-01

    For any quantity of interest in a system governed by ordinary differential equations, it is natural to seek the largest (or smallest) long-time average among solution trajectories, as well as the extremal trajectories themselves. Upper bounds on time averages can be proved a priori using auxiliary functions, the optimal choice of which is a convex optimization problem. We prove that the problems of finding maximal trajectories and minimal auxiliary functions are strongly dual. Thus, auxiliary functions provide arbitrarily sharp upper bounds on time averages. Moreover, any nearly minimal auxiliary function provides phase space volumes in which all nearly maximal trajectories are guaranteed to lie. For polynomial equations, auxiliary functions can be constructed by semidefinite programming, which we illustrate using the Lorenz system.

  8. Pitting corrosion of copper. An equilibrium - mass transport study

    International Nuclear Information System (INIS)

    Taxen, C.

    2002-08-01

    A mathematical model for the propagation of corrosion pits is described and used to calculate the potentials below which copper is immune to pitting. The model uses equilibrium data and diffusion coefficients and calculates the stationary concentration profiles of 26 aqueous species from the bulk water outside a corrosion pit to the site of the metal dissolution. Precipitation of oxides and salts of copper is considered. Studied conditions include water compositions from tap waters to seawater at the temperatures 25 deg C and 75 deg C. Carbonate and sulphate are aggressive towards copper because of complex formation with divalent copper. Carbonate is less aggressive in a corrosion pit than outside at the pH of the bulk. Carbonate carries acidity out from the pit, favours oxide formation and may prevent the initiation of acidic corrosion pits. The concentration profiles are used to estimate the maximum propagation rates for a corrosion pit. A high potential is found to be the most important factor for the rate of propagation. The levels of potential copper can sustain, as corrosion potentials are discussed in terms of the stability of cuprous oxide as a cathode material for oxygen reduction relative to non-conducting cupric phases

  9. Pitting corrosion of copper. An equilibrium - mass transport study

    Energy Technology Data Exchange (ETDEWEB)

    Taxen, C. [Swedish Corrosion Inst., Stockholm (Sweden)

    2002-08-01

    A mathematical model for the propagation of corrosion pits is described and used to calculate the potentials below which copper is immune to pitting. The model uses equilibrium data and diffusion coefficients and calculates the stationary concentration profiles of 26 aqueous species from the bulk water outside a corrosion pit to the site of the metal dissolution. Precipitation of oxides and salts of copper is considered. Studied conditions include water compositions from tap waters to seawater at the temperatures 25 deg C and 75 deg C. Carbonate and sulphate are aggressive towards copper because of complex formation with divalent copper. Carbonate is less aggressive in a corrosion pit than outside at the pH of the bulk. Carbonate carries acidity out from the pit, favours oxide formation and may prevent the initiation of acidic corrosion pits. The concentration profiles are used to estimate the maximum propagation rates for a corrosion pit. A high potential is found to be the most important factor for the rate of propagation. The levels of potential copper can sustain, as corrosion potentials are discussed in terms of the stability of cuprous oxide as a cathode material for oxygen reduction relative to non-conducting cupric phases.

  10. Effects of the Maximum Luminance in a Medical-grade Liquid-crystal Display on the Recognition Time of a Test Pattern: Observer Performance Using Landolt Rings.

    Science.gov (United States)

    Doi, Yasuhiro; Matsuyama, Michinobu; Ikeda, Ryuji; Hashida, Masahiro

    2016-07-01

    This study was conducted to measure the recognition time of the test pattern and to investigate the effects of the maximum luminance in a medical-grade liquid-crystal display (LCD) on the recognition time. Landolt rings as signals of the test pattern were used with four random orientations, one on each of the eight gray-scale steps. Ten observers input the orientation of the gap on the Landolt rings using cursor keys on the keyboard. The recognition times were automatically measured from the display of the test pattern on the medical-grade LCD to the input of the orientation of the gap in the Landolt rings. The maximum luminance in this study was set to one of four values (100, 170, 250, and 400 cd/m(2)), for which the corresponding recognition times were measured. As a result, the average recognition times for each observer with maximum luminances of 100, 170, 250, and 400 cd/m(2) were found to be 3.96 to 7.12 s, 3.72 to 6.35 s, 3.53 to 5.97 s, and 3.37 to 5.98 s, respectively. The results indicate that the observer's recognition time is directly proportional to the luminance of the medical-grade LCD. Therefore, it is evident that the maximum luminance of the medical-grade LCD affects the test pattern recognition time.

  11. Corrosion protection performance of waterborne epoxy coatings containing self-doped polyaniline nanofiber

    Energy Technology Data Exchange (ETDEWEB)

    Qiu, Shihui [Key Laboratory of Marine Materials and Related Technologies, Zhejiang Key Laboratory of Marine Materials and Protective Technologies, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo, 315201 (China); Faculty of Materials Science and Chemical Engineering, Ningbo University, Ningbo, 315211 (China); Chen, Cheng; Cui, Mingjun [Key Laboratory of Marine Materials and Related Technologies, Zhejiang Key Laboratory of Marine Materials and Protective Technologies, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo, 315201 (China); Li, Wei [Faculty of Materials Science and Chemical Engineering, Ningbo University, Ningbo, 315211 (China); Zhao, Haichao, E-mail: zhaohaichao@nimte.ac.cn [Key Laboratory of Marine Materials and Related Technologies, Zhejiang Key Laboratory of Marine Materials and Protective Technologies, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo, 315201 (China); Wang, Liping, E-mail: wangliping@nimte.ac.cn [Key Laboratory of Marine Materials and Related Technologies, Zhejiang Key Laboratory of Marine Materials and Protective Technologies, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo, 315201 (China)

    2017-06-15

    Highlights: • Self-dopedpolyaniline (SPANi) with good conductivity and dispersibility in water was copolymerized by aniline and its derivative. • Environmental friendly SPANi/epoxy composite coating with remarkable anti-corrosion performance was prepared. • The corrosion product of pure epoxy or composite coating was characterized by X-ray diffraction pattern and scanning electron microscope (SEM). - Abstract: Self-doped sulfonated polyaniline (SPANi) nanofiber was synthesized by the copolymerization of 2-aminobenzenesulfonic acid (ASA) and aniline via a rapid mixing polymerization approach. The chemical structure of SPANi was investigated by the Fourier-transform infrared (FT-IR), Raman, X-ray photoelectron spectroscopy (XPS), UV–vis spectra and X-ray diffraction (XRD) pattern. The as-prepared SPANi nanofibers had 45 nm average diameter and length up to 750 nm as measured by scanning electron microscope (SEM) and transmission electron microscope (TEM). The self-doped SPANi nanofiber possessed excellent aqueous solubility, good conductivity (0.11 S/cm) and reversible redox activity, making it suitable as a corrosion inhibitor for waterborne coatings. The prepared SPANi/waterborne epoxy composite coatings exhibited remarkably improved corrosion protection compared with pure waterborne epoxy coating as proved by the polarization curves and electrochemical impedance spectroscopy (EIS). The passivation effect of SPANi nanofiber and the corrosion products beneath the epoxy coatings immersed in 3.5% NaCl solution as a function of time were also investigated in this study.

  12. Corrosion protection performance of waterborne epoxy coatings containing self-doped polyaniline nanofiber

    International Nuclear Information System (INIS)

    Qiu, Shihui; Chen, Cheng; Cui, Mingjun; Li, Wei; Zhao, Haichao; Wang, Liping

    2017-01-01

    Highlights: • Self-dopedpolyaniline (SPANi) with good conductivity and dispersibility in water was copolymerized by aniline and its derivative. • Environmental friendly SPANi/epoxy composite coating with remarkable anti-corrosion performance was prepared. • The corrosion product of pure epoxy or composite coating was characterized by X-ray diffraction pattern and scanning electron microscope (SEM). - Abstract: Self-doped sulfonated polyaniline (SPANi) nanofiber was synthesized by the copolymerization of 2-aminobenzenesulfonic acid (ASA) and aniline via a rapid mixing polymerization approach. The chemical structure of SPANi was investigated by the Fourier-transform infrared (FT-IR), Raman, X-ray photoelectron spectroscopy (XPS), UV–vis spectra and X-ray diffraction (XRD) pattern. The as-prepared SPANi nanofibers had 45 nm average diameter and length up to 750 nm as measured by scanning electron microscope (SEM) and transmission electron microscope (TEM). The self-doped SPANi nanofiber possessed excellent aqueous solubility, good conductivity (0.11 S/cm) and reversible redox activity, making it suitable as a corrosion inhibitor for waterborne coatings. The prepared SPANi/waterborne epoxy composite coatings exhibited remarkably improved corrosion protection compared with pure waterborne epoxy coating as proved by the polarization curves and electrochemical impedance spectroscopy (EIS). The passivation effect of SPANi nanofiber and the corrosion products beneath the epoxy coatings immersed in 3.5% NaCl solution as a function of time were also investigated in this study.

  13. Mechanistic investigation of internal corrosion in nuclear waste containers over extended time periods

    International Nuclear Information System (INIS)

    Onumonu, E.; Stevens, D. N. P. C.

    2008-01-01

    Storage of the UK's Intermediate Level Wastes (ILW), which comprises Magnox fuel cladding, uranium and small items of equipment exposed to radiation, is currently achieved via encapsulation within cementitious grout housed in 500 litre 316L stainless steel drums. The cements used display a high pH; in such an environment many metals form surface hydroxides or oxides. Magnox reacts with free water at high pH with the liberation of hydrogen whilst undergoing corrosion to form hydroxide species. Corrosion of Magnox cladding has previously been monitored by measuring the rate of hydrogen evolution and/or weight loss. Recent work by our group has shown impedance techniques may also be useful in monitoring early corrosion behaviour. In this project electrochemical polarisation techniques will be employed to examine the corrosion behaviour of Magnox fuel in situations where it is in electrical contact with other metals, including uranium, and hence determine how galvanic effects influence corrosion behaviour. In this paper we describe the background to such experiments along with some preliminary results. (authors)

  14. Time-dependent Enhanced Corrosion of Ti6Al4V in the Presence of H2O2 and Albumin.

    Science.gov (United States)

    Zhang, Yue; Addison, Owen; Yu, Fei; Troconis, Brendy C Rincon; Scully, John R; Davenport, Alison J

    2018-02-16

    There is increasing concern regarding the biological consequences of metal release from implants. However, the mechanisms underpinning implant surface degradation, especially in the absence of wear, are often poorly understood. Here the synergistic effect of albumin and H 2 O 2 on corrosion of Ti6Al4V in physiological saline is studied with electrochemical methods. It is found that albumin induces a time-dependent dissolution of Ti6Al4V in the presence of H 2 O 2 in physiology saline. Potentiostatic polarisation measurements show that albumin supresses dissolution in the presence of H 2 O 2 at short times (<24 h) but over longer time periods (120 h) it significantly accelerates corrosion, which is attributed to albumin-catalysed dissolution of the corrosion product layer resulting in formation of a thinner oxide film. Dissolution of Ti6Al4V in the presence of albumin and H 2 O 2 in physiological saline is also found to be dependent on potential: the titanium ion release rate is found to be higher (0.57 µg/cm 2 ) at a lower potential (90 mV), where the oxide capacitance and resistance inferred from Electrochemical Impedance Spectroscopy also suggests a less resistant oxide film. The study highlights the importance of using more realistic solutions, and considering behaviour over longer time periods when testing corrosion resistance of metallic biomaterials.

  15. Corrosion effects on friction factors

    International Nuclear Information System (INIS)

    Magleby, H.L.; Shaffer, S.J.

    1996-01-01

    This paper presents the results of NRC-sponsored material specimen tests that were performed to determine if corrosion increases the friction factors of sliding surfaces of motor-operated gate valves, which could require higher forces to close and open safety-related valves when subjected to their design basis differential pressures. Friction tests were performed with uncorroded specimens and specimens subjected to accelerated corrosion. Preliminary tests at ambient conditions showed that corrosion increased the friction factors, indicating the need for additional tests duplicating valve operating parameters at hot conditions. The additional tests showed friction factors of corroded specimens were 0.1 to 0.2 higher than for uncorroded specimens, and that the friction factors of the corroded specimens were not very dependent on contact stress or corrosion film thickness. The measured values of friction factors for the three corrosion films tested (simulating three operating times) were in the range of 0.3 to 0.4. The friction factor for even the shortest simulated operating time was essentially the same as the others, indicating that the friction factors appear to reach a plateau and that the plateau is reached quickly

  16. A new corrosion monitoring technique

    International Nuclear Information System (INIS)

    Brown, Gerald K.

    2000-01-01

    Internal Corrosion Monitoring has relied upon 5 basic techniques. Little improvement in performance has been achieved in any of these. Many newer internal corrosion monitoring techniques have proved of little value in the field although some have instances of success in the laboratory. Industry has many high value hydrocarbon applications requiring corrosion rate monitoring for real-time problem solving and control. The high value of assets and the cost of asset replacement makes it necessary to practice cost effective process and corrosion control with sensitivity beyond the 5 basic techniques. This new metal loss technology offers this sensitivity. Traditional metal loss technology today provides either high sensitivity with short life, or conversely, long life but with substantially reduced sensitivity. The new metal loss technology offers an improved working life of sensors without significantly compromising performance. The paper discusses the limitations of existing on-line technologies and describes the performance of a new technology. This new metal loss technology was introduced at NACE Corrosion 99'. Since that time several field projects have been completed or are ongoing. This paper will discuss the new metal loss technology and report on some of the data that has been obtained.(author)

  17. Inspection about the corrosion of metallic archaeological artifacts in ground. 3

    International Nuclear Information System (INIS)

    Honda, Takashi; Yamaguchi, Shingo

    2003-01-01

    The corrosion behaviors of iron-based archaeological remains, which were dug out in six relics in Aomori-ken and Izumotaisya-keidai-iseki, were analyzed mainly with using X-ray CT. Several samples were cut and investigated on the details of metals and oxide films. The soils were also analyzed on redox-potential, resistance, chemical contents, and others. The results indicate that metal remains in 7/14 samples. The corrosion amounts of objects of Aomori-ken were estimated to be from 1 to 4 mm during 400-1000 years. The environments were supposed to be oxidizing. On the other hands, it is supposed that two objects in Izumotaisya-keidai-iseki were in a reducing condition. The corrosion amounts were 0.5-2 mm. Furthermore, the corrosion behavior of the cast gas-pipe, which had been buried for about 130 years, were evaluated. By analyzing analysis data of soil, the environment is estimated to be weak oxidizing, and the maximum graphitic corrosion depth was about 7 mm. (author)

  18. Seacoast stress corrosion cracking of aluminum alloys

    Science.gov (United States)

    Humphries, T. S.; Nelson, E. E.

    1981-01-01

    The stress corrosion cracking resistance of high strength, wrought aluminum alloys in a seacoast atmosphere was investigated and the results were compared with those obtained in laboratory tests. Round tensile specimens taken from the short transverse grain direction of aluminum plate and stressed up to 100 percent of their yield strengths were exposed to the seacoast and to alternate immersion in salt water and synthetic seawater. Maximum exposure periods of one year at the seacoast, 0.3 or 0.7 of a month for alternate immersion in salt water, and three months for synthetic seawater were indicated for aluminum alloys to avoid false indications of stress corrosion cracking failure resulting from pitting. Correlation of the results was very good among the three test media using the selected exposure periods. It is concluded that either of the laboratory test media is suitable for evaluating the stress corrosion cracking performance of aluminum alloys in seacoast atmosphere.

  19. Active Waste Materials Corrosion and Decontamination Tests

    International Nuclear Information System (INIS)

    Danielson, M.J.; Elmore, M.R.; Pitman, S.G.

    2000-01-01

    Stainless steel alloys, 304L and 316L, were corrosion tested in representative radioactive samples of three actual Hanford tank waste solutions (Tanks AW-101, C-104, AN-107). Both the 304L and 316L exhibited good corrosion performance when immersed in boiling waste solutions. The maximum general corrosion rate was 0.015 mm/y (0.60 mils per year). Generally, the 304L had a slightly higher rate than the 316L. No localized attack was observed after 122 days of testing in the liquid phase, liquid/vapor phase, or vapor phase. Radioactive plate-out decontamination tests indicated that a 24-hour exposure to 1 und M HNO 3 could remove about 99% of the radioactive components in the metal film when exposed to the C-104 and AN-107 solutions. The decontamination results are less certain for the AW-101 solution, since the initial contamination readings exceeded the capacity of the meter used for this test

  20. Applicability of Time-Averaged Holography for Micro-Electro-Mechanical System Performing Non-Linear Oscillations

    Directory of Open Access Journals (Sweden)

    Paulius Palevicius

    2014-01-01

    Full Text Available Optical investigation of movable microsystem components using time-averaged holography is investigated in this paper. It is shown that even a harmonic excitation of a non-linear microsystem may result in an unpredictable chaotic motion. Analytical results between parameters of the chaotic oscillations and the formation of time-averaged fringes provide a deeper insight into computational and experimental interpretation of time-averaged MEMS holograms.

  1. Applicability of Time-Averaged Holography for Micro-Electro-Mechanical System Performing Non-Linear Oscillations

    Science.gov (United States)

    Palevicius, Paulius; Ragulskis, Minvydas; Palevicius, Arvydas; Ostasevicius, Vytautas

    2014-01-01

    Optical investigation of movable microsystem components using time-averaged holography is investigated in this paper. It is shown that even a harmonic excitation of a non-linear microsystem may result in an unpredictable chaotic motion. Analytical results between parameters of the chaotic oscillations and the formation of time-averaged fringes provide a deeper insight into computational and experimental interpretation of time-averaged MEMS holograms. PMID:24451467

  2. Applicability of time-averaged holography for micro-electro-mechanical system performing non-linear oscillations.

    Science.gov (United States)

    Palevicius, Paulius; Ragulskis, Minvydas; Palevicius, Arvydas; Ostasevicius, Vytautas

    2014-01-21

    Optical investigation of movable microsystem components using time-averaged holography is investigated in this paper. It is shown that even a harmonic excitation of a non-linear microsystem may result in an unpredictable chaotic motion. Analytical results between parameters of the chaotic oscillations and the formation of time-averaged fringes provide a deeper insight into computational and experimental interpretation of time-averaged MEMS holograms.

  3. Kinetics of steel corrosion in water

    International Nuclear Information System (INIS)

    Vettegren', V.I.; Bashkarev, A.Ya.; Danchukov, K.G.; Morozov, G.I.

    2003-01-01

    Kinetics of corrosion damage accumulation in steels of different composition (Cr-Ni-Mo-Ti, Cr-Ni-Mn-N-V, Cr-Ni-N-Mn-Mo, Cr-Ni-Nb, Cr-Ni-Ti, Cr-Mn-Ni, Mn-Al-Nb-Si, Mn-Cr-Al-Si and Mn-Al-Si) in NaCl solution and in sea water was studied. It is shown that degree of corrosion damage relates to time according to the first order reaction expression. The values of corrosion activation energy and of parameter characterizing protection properties of corrosion film are determined [ru

  4. Electrochemical analysis of the corrosion inhibition effect of trypsin complex on the pitting corrosion of 420 martensitic stainless steel in 2M H2SO4 solution.

    Science.gov (United States)

    Loto, Roland Tolulope

    2018-01-01

    Inhibition effect of trypsin complex (TC) on the pitting corrosion of martensitic stainless steel (type 420) in 1M H2SO4 solution was studied with potentiodynamic polarization, open circuit potential measurement and optical microscopy. TC reduced the corrosion rate of the steel with maximum inhibition efficiency of 80.75%. Corrosion potential shifted anodically due to the electrochemical action of TC. The pitting potential increased from 1.088VAg/AgCl (3M) at 0% TC to 1.365VAg/AgCl(3M) at 4% TC. TC shifts the open circuit corrosion potential from -0.270s at 0% TC concentration to -0.255V at 5% TC. The compound completely adsorbed onto the steel according to Langmuir, Frumkin and Temkin isotherms. ATF-FTIR spectroscopy confirmed the inhibition mode to be through surface coverage. Thermodynamic calculations showed physisorption molecular interaction. Corrosion pits are present on the uninhibited 420 morphology in comparison to TC inhibited surface which slightly deteriorated.

  5. Corrosion surveillance of the chemical decontamination process in Kuosheng nuclear power plant

    International Nuclear Information System (INIS)

    Wang, L.H.

    2002-01-01

    The Piping Recirculation System (RRS) and reactor water clean-up system (RWCU) of Kuosheng Nuclear Power Plant of Taiwan Power Company were decontaminated by CORD process of Framatome ANP GmbH during the outage at October 2001. This is the first time that CORD process was adopted and applied in Taiwan Nuclear Power Plant. To verify minor corrosion damage and correct process control, the material corrosion condition was monitored during all the stages of the chemical decontamination work. Three kinds of specimen were adopted in this corrosion monitoring, including corrosion coupons for weight loss measurements, electrochemical specimens for on-line corrosion monitoring, and WOL specimens (wedge opening loaded) for stress corrosion evaluation. The measured metal losses from nine coupon materials did not reveal any unexpected or intolerable high corrosion damage from the CORD UV or CORD CS processes. The coupon materials included type 304 stainless steel (SS) with sensitized and as-received thermal history, type 308 weld filler, type CF8 cast SS, nickel base alloy 182 weld filler, Inconel 600, Stellite 6 hard facing alloy, NOREM low cobalt hard facing alloy, and A106B carbon steel (CS). The electrochemical noise (ECN) measurements from three-electrode electrochemical probe precisely depicted the metal corrosion variation with the decontamination process change. Most interestingly, the estimated trend of accumulated metal loss is perfectly corresponding to the total removed activities. The ECN measurements were also used for examining the effect of different SS oxide films pre-formed in NWC and HWC on the decontamination efficiency, and for evaluating the galvanic effect of CS with SS. The existing cracks did not propagate further during the decontamination. The average decontamination factors achieved were 50.8 and 4.2 respectively for RRS and RWCU. (authors)

  6. Archaeological analogs and corrosion

    International Nuclear Information System (INIS)

    David, D.

    2008-01-01

    In the framework of the high level and long life radioactive wastes disposal deep underground, the ANDRA built a research program on the material corrosion. In particular they aim to design containers for a very long time storage. Laboratory experiments are in progress and can be completed by the analysis of metallic archaeological objects and their corrosion after hundred years. (A.L.B.)

  7. Atmospheric corrosion: statistical validation of models

    International Nuclear Information System (INIS)

    Diaz, V.; Martinez-Luaces, V.; Guineo-Cobs, G.

    2003-01-01

    In this paper we discuss two different methods for validation of regression models, applied to corrosion data. One of them is based on the correlation coefficient and the other one is the statistical test of lack of fit. Both methods are used here to analyse fitting of bi logarithmic model in order to predict corrosion for very low carbon steel substrates in rural and urban-industrial atmospheres in Uruguay. Results for parameters A and n of the bi logarithmic model are reported here. For this purpose, all repeated values were used instead of using average values as usual. Modelling is carried out using experimental data corresponding to steel substrates under the same initial meteorological conditions ( in fact, they are put in the rack at the same time). Results of correlation coefficient are compared with the lack of it tested at two different signification levels (α=0.01 and α=0.05). Unexpected differences between them are explained and finally, it is possible to conclude, at least in the studied atmospheres, that the bi logarithmic model does not fit properly the experimental data. (Author) 18 refs

  8. An electrochemical study of the corrosion behavior of primer coated 2219-T87 aluminum

    Science.gov (United States)

    Danford, M. D.; Higgins, R. H.

    1985-01-01

    The corrosion behavior for 2219-T87 aluminum coated with various primers, including those used for the external tank and solid rocket boosters of the Space Shuttle Transportation System, were investigated using electrochemical techniques. Corrosion potential time, polarization resistance time, electrical resistance time, and corrosion rate time measurements were all investigated. It was found that electrical resistance time and corrosion rate time measurement were most useful for studying the corrosion behavior of painted aluminum. Electrical resistance time determination give useful information concerning the porosity of paint films, while corrosion rate time curves give important information concerning overall corrosion rates and corrosion mechanisms. In general, the corrosion rate time curves all exhibited at least one peak during the 30 day test period, which was attributed, according to the proposed mechanisms, to the onset of the hydrogen evolution reaction and the beginning of destruction of the protective properties of the paint film.

  9. Maximum-likelihood model averaging to profile clustering of site types across discrete linear sequences.

    Directory of Open Access Journals (Sweden)

    Zhang Zhang

    2009-06-01

    Full Text Available A major analytical challenge in computational biology is the detection and description of clusters of specified site types, such as polymorphic or substituted sites within DNA or protein sequences. Progress has been stymied by a lack of suitable methods to detect clusters and to estimate the extent of clustering in discrete linear sequences, particularly when there is no a priori specification of cluster size or cluster count. Here we derive and demonstrate a maximum likelihood method of hierarchical clustering. Our method incorporates a tripartite divide-and-conquer strategy that models sequence heterogeneity, delineates clusters, and yields a profile of the level of clustering associated with each site. The clustering model may be evaluated via model selection using the Akaike Information Criterion, the corrected Akaike Information Criterion, and the Bayesian Information Criterion. Furthermore, model averaging using weighted model likelihoods may be applied to incorporate model uncertainty into the profile of heterogeneity across sites. We evaluated our method by examining its performance on a number of simulated datasets as well as on empirical polymorphism data from diverse natural alleles of the Drosophila alcohol dehydrogenase gene. Our method yielded greater power for the detection of clustered sites across a breadth of parameter ranges, and achieved better accuracy and precision of estimation of clusters, than did the existing empirical cumulative distribution function statistics.

  10. A note on computing average state occupation times

    Directory of Open Access Journals (Sweden)

    Jan Beyersmann

    2014-05-01

    Full Text Available Objective: This review discusses how biometricians would probably compute or estimate expected waiting times, if they had the data. Methods: Our framework is a time-inhomogeneous Markov multistate model, where all transition hazards are allowed to be time-varying. We assume that the cumulative transition hazards are given. That is, they are either known, as in a simulation, determined by expert guesses, or obtained via some method of statistical estimation. Our basic tool is product integration, which transforms the transition hazards into the matrix of transition probabilities. Product integration enjoys a rich mathematical theory, which has successfully been used to study probabilistic and statistical aspects of multistate models. Our emphasis will be on practical implementation of product integration, which allows us to numerically approximate the transition probabilities. Average state occupation times and other quantities of interest may then be derived from the transition probabilities.

  11. Synthesis and characterization of a novel organic corrosion inhibitor for mild steel in 1 M hydrochloric acid

    Directory of Open Access Journals (Sweden)

    Mohammed H. Othman Ahmed

    2018-03-01

    Full Text Available The synthesis and characterization of a novel organic corrosion inhibitor (4-(3-mercapto-5,6,7,8-tetrahydro-[1,2,4]triazolo[4,3-b][1,2,4,5]tetrazin-6-ylphenol, for mild steel in 1 M hydrochloric acid (HCl has been successfully reported for the first time. The inhibitor evaluated as corrosion inhibitor for mild steel in 1 M of Hydrochloric acid solution using electrochemical impedance spectroscopy (EIS, and electrochemical frequency modulation (EFM measurement techniques. Changes in the impedance parameters suggested an adsorption of the inhibitor onto the mild steel surface, leading to the formation of protective films. The results show that the inhibition efficiencies increased with increasing the concentrations of the inhibitors and decreased with increasing temperature. The maximum inhibition efficiency up to 67% at the maximum concentration 0.5 mM. This shows that those inhibitors are effective in helping to reduce and slowing down the corrosion process that occurs to mild steel with a hydrochloric acid solution by providing an organic inhibitor for the mild steel that can be weakened by increasing the temperature. The adsorption process of the synthesized organic inhibitor depends on its electronic characteristics in addition to steric effects and the nature of metal surface, temperature degree and the varying degrees of surface-site activity. The synthesized inhibitor molecules were absorbed by metal surface and follow Langmuir isotherms. Keywords: Corrosion, Inhibitor, Mild steel, EIS spectroscopy

  12. Taphonomic trade-offs in tropical marine death assemblages: Differential time averaging, shell loss, and probable bias in siliciclastic vs. carbonate facies

    Science.gov (United States)

    Kidwell, Susan M.; Best, Mairi M. R.; Kaufman, Darrell S.

    2005-09-01

    Radiocarbon-calibrated amino-acid racemization ages of individually dated bivalve mollusk shells from Caribbean reef, nonreefal carbonate, and siliciclastic sediments in Panama indicate that siliciclastic sands and muds contain significantly older shells (median 375 yr, range up to ˜5400 yr) than nearby carbonate seafloors (median 72 yr, range up to ˜2900 yr; maximum shell ages differ significantly at p < 0.02 using extreme-value statistics). The implied difference in shell loss rates is contrary to physicochemical expectations but is consistent with observed differences in shell condition (greater bioerosion and dissolution in carbonates). Higher rates of shell loss in carbonate sediments should lead to greater compositional bias in surviving skeletal material, resulting in taphonomic trade-offs: less time averaging but probably higher taxonomic bias in pure carbonate sediments, and lower bias but greater time averaging in siliciclastic sediments from humid-weathered accretionary arc terrains, which are a widespread setting of tropical sedimentation.

  13. Radiation corrosion in aluminum alloy bellows

    International Nuclear Information System (INIS)

    Konno, Osamu

    1987-01-01

    Testing was carried out in which materials for vacuum devices (Al, Ti, Cu, SUS) are exposed to electron beams (50 MeV, average current 80 μA) to determine the changes in the quantity, partial pressure and composition of the gases released from the materials. The test appratus used are made of Al alloys alone. During the test, vacuum leak is found in the Al alloy bellows used in the drive device. The leak is found to result from corrosion caused by water. The surface structure is analyzed by SEM, EPMA, ESCA and IMA. It is confirmed that the Al alloy used as material for the bellows if highly resistant to corrosion. It is concluded that it is necessary to use high purity cooling water to prevent the cooling water from causing corrosion. It has been reported that high purity aluminum is very high in resistance to corrosion. Based on these measurements and considerations, it is suggested that when aluminum is to be used as material for vacuum devices in an accelerator, it is required to provide protection film on its surface to prevent corrosion or to use cooling water pipes cladded with pure aluminum and an aluminum alloy. In addition, the temperature of the cooling water should be set after adequately considering the environmental conditions in the room. (Nogami, K.)

  14. Corrosion behaviour of martensitic and austenitic steels in flowing lead-bismuth eutectic

    International Nuclear Information System (INIS)

    Martin-Munoz, F.J.; Soler-Crespo, L.; Gomez-Briceno, D.

    2011-01-01

    The LINCE loop is a forced convection loop designed for long-term corrosion tests in lead-bismuth eutectic (LBE) at CIEMAT. The LBE volume of in the loop is 250 l and the maximum flow velocity in the region of specimens is approximately 1 m s -1 . An oxygen control system has been implemented in the loop. The corrosion behaviour of AISI 316L and T91 steels was investigated in flowing LBE at temperatures of 575 and 725 K for exposure times of 2000, 5000 and 10,000 h. At 575 K, the results showed a good response, with no weight loss detected in any of the materials after exposure to the flowing LBE up to 10,000 h. A similar behaviour was observed for the specimens tested at 725 K during 2000 and 10,000 h. Specimens extracted at intermediate time (5000 h) showed an anomalous behaviour with important weight loss. These specimens were placed at the bottom of the hot test section, and this position probably made them to suffer an accused process of cavitation-erosion.

  15. Analysis of electrochemical noise (ECN) data in time and frequency domain for comparison corrosion inhibition of some azole compounds on Cu in 1.0 M H2SO4 solution

    Science.gov (United States)

    Ramezanzadeh, B.; Arman, S. Y.; Mehdipour, M.; Markhali, B. P.

    2014-01-01

    In this study, the corrosion inhibition properties of two similar heterocyclic compounds namely benzotriazole (BTA) and benzothiazole (BNS) inhibitors on copper in 1.0 M H2SO4 solution were studied by electrochemical techniques as well as surface analysis. The results showed that corrosion inhibition of copper largely depends on the molecular structure and concentration of the inhibitors. The effect of DC trend on the interpretation of electrochemical noise (ECN) results in time domain was evaluated by moving average removal (MAR) method. Accordingly, the impact of square and Hanning window functions as drift removal methods in frequency domain was studied. After DC trend removal, a good trend was observed between electrochemical noise (ECN) data and the results obtained from EIS and potentiodynamic polarization. Furthermore, the shot noise theory in frequency domain was applied to approach the charge of each electrochemical event (q) from the potential and current noise signals.

  16. Study on influence of native oxide and corrosion products on atmospheric corrosion of pure Al

    International Nuclear Information System (INIS)

    Liu, Yanjie; Wang, Zhenyao; Ke, Wei

    2014-01-01

    Highlights: •Corrosion products layer is only formed in coastal atmosphere. •In coastal atmosphere, rate controlling step is diffusion process. •In rural atmosphere, rate controlling step is charge transfer process. •Pitting area increases greatly in coastal site, but slightly in rural site. -- Abstract: Effects of native oxide and corrosion products on atmospheric corrosion of aluminium in rural and coastal sites were studied by electrochemical impedance spectroscopy (EIS), open-circuit potential (OCP) and scanning electron microscope (SEM) techniques after outdoor exposure. In the rural atmosphere, only the compact, adhesive native oxide layer exists, and the rate controlling step is diffusion process, while in the coastal atmosphere, another loose, inadhesive corrosion products layer exists, and a charge transfer process controls the corrosion process. The pitting area in the coastal atmosphere increases over time more obviously than that in the rural atmosphere

  17. Corrosion Rate Monitoring in District Heating Systems

    DEFF Research Database (Denmark)

    Hilbert, Lisbeth Rischel; Nielsen, Lars Vendelbo; Andersen, A.

    2005-01-01

    be applicable, and if on-line monitoring could improve the quality control. Water quality monitoring was applied as well as corrosion rate monitoring with linear polarization resistance (LPR), electrochemical impedance spectroscopy (EIS), electrical resistance (ER) technique, mass loss and a crevice corrosion......Quality control in district heating systems to keep uniform corrosion rates low and localized corrosion minimal is based on water quality control. Side-stream units equipped with carbon steel probes for online monitoring were mounted in district heating plants to investigate which techniques would...... cell for localized corrosion risk estimation. Important variations in corrosion rate due to changes in make-up water quality were detected with the continuous monitoring provided by ER and crevice cell, while LPR gave unreliable corrosion rates. The acquisition time of two-three days for EIS...

  18. Fatigue strength degradation of metals in corrosive environments

    OpenAIRE

    Adasooriya, Mudiyan Nirosha Damayanthi; Hemmingsen, Tor; Pavlou, Dimitrios

    2017-01-01

    Structures exposed to aggressive environmental conditions are often subjected to time-dependent loss of coating and loss of material due to corrosion; this causes reduction in the cross-sectional properties of the members, increased surface roughness, surface irregularities and corrosion pits, and degradation of material strengths. These effects have been identified and simulated in different research studies. However, time and corrosive media dependent fatigue strength curves for materials h...

  19. Lake Basin Fetch and Maximum Length/Width

    Data.gov (United States)

    Minnesota Department of Natural Resources — Linear features representing the Fetch, Maximum Length and Maximum Width of a lake basin. Fetch, maximum length and average width are calcuated from the lake polygon...

  20. Predicting Effects of Corrosion Erosion of High Strength Steel Pipelines Elbow on CO2-Acetic Acid (HAc) Solution

    International Nuclear Information System (INIS)

    Asmara, Y. P.; Ismail, M. F.; Chui, L. Giok; Halimi, Jamiludin

    2016-01-01

    Simultaneously effect of erosion combined with corrosion becomes the most concern in oil and gas industries. It is due to the fast deterioration of metal as effects of solid particles mixed with corrosive environment. There are many corrosion software to investigate possible degradation mechanisms developed by researchers. They are using many combination factors of chemical reactions and physical process. However effects of CO 2 and acid on pipelines orientations are still remain uncovered in their simulation. This research will investigate combination effects of CO 2 and HAc on corrosion and erosion artificial environmental containing sands particles in 45°, 90° and 180° elbow pipelines. The research used theoretical calculations combined with experiments for verification. The main concerns are to investigate the maximum erosion corrosion rate and maximum shear stress at the surface. Methodology used to calculate corrosion rate are Linear Polarization Resistance (LPR) and weight loss. The results showed that at 45°, erosion rate is the more significant effects in contributing degradation of the metal. The effects of CO 2 and HAc gave significant effects when flow rate of the solution are high which reflect synergism effects of solid particles and those chemical compositions. (paper)

  1. Corrosion

    Science.gov (United States)

    Slabaugh, W. H.

    1974-01-01

    Presents some materials for use in demonstration and experimentation of corrosion processes, including corrosion stimulation and inhibition. Indicates that basic concepts of electrochemistry, crystal structure, and kinetics can be extended to practical chemistry through corrosion explanation. (CC)

  2. The Maximum Entropy Method for Optical Spectrum Analysis of Real-Time TDDFT

    International Nuclear Information System (INIS)

    Toogoshi, M; Kano, S S; Zempo, Y

    2015-01-01

    The maximum entropy method (MEM) is one of the key techniques for spectral analysis. The major feature is that spectra in the low frequency part can be described by the short time-series data. Thus, we applied MEM to analyse the spectrum from the time dependent dipole moment obtained from the time-dependent density functional theory (TDDFT) calculation in real time. It is intensively studied for computing optical properties. In the MEM analysis, however, the maximum lag of the autocorrelation is restricted by the total number of time-series data. We proposed that, as an improved MEM analysis, we use the concatenated data set made from the several-times repeated raw data. We have applied this technique to the spectral analysis of the TDDFT dipole moment of ethylene and oligo-fluorene with n = 8. As a result, the higher resolution can be obtained, which is closer to that of FT with practically time-evoluted data as the same total number of time steps. The efficiency and the characteristic feature of this technique are presented in this paper. (paper)

  3. Measurement of reinforcement corrosion in concrete structures. Betonirakenteiden raudoituksen korroosion tutkiminen

    Energy Technology Data Exchange (ETDEWEB)

    Meuronen, A

    1992-03-01

    Ageing and aggressive enviromental conditions of concrete structures will result in deterioration of concrete and corrosion of steel in concrete. Corrosion of steel will in time result in the end of the service life or expensive renovations, unless corrosion of steel is noticed and renovated in time. Corrosion of steel in concrete can be found out by the present corrosion measurement methods, so that renovation can be started in right time. The report presents mainly on the basis of the literature references the following corrosion measurement methods: polarisation resistance, AC-impedance, electrical resistance probe, electrochemical noice and half-cell potential mapping. The half-cell potential mapping will be presented more precisely than the other corrosion measurement methods, for the potential mapping is the most used method. Concrete and Soils Laboratory of Imatran Voima Oy uses in the measurement of reinforcement corrosion the English, eight channel potential measuring equipment.

  4. Measurement of reinforcement corrosion in concrete structures; Betonirakenteiden raudoituksen korroosion tutkiminen

    Energy Technology Data Exchange (ETDEWEB)

    Meuronen, A

    1992-03-01

    Ageing and aggressive enviromental conditions of concrete structures will result in deterioration of concrete and corrosion of steel in concrete. Corrosion of steel will in time result in the end of the service life or expensive renovations, unless corrosion of steel is noticed and renovated in time. Corrosion of steel in concrete can be found out by the present corrosion measurement methods, so that renovation can be started in right time. The report presents mainly on the basis of the literature references the following corrosion measurement methods: polarisation resistance, AC-impedance, electrical resistance probe, electrochemical noice and half-cell potential mapping. The half-cell potential mapping will be presented more precisely than the other corrosion measurement methods, for the potential mapping is the most used method. Concrete and Soils Laboratory of Imatran Voima Oy uses in the measurement of reinforcement corrosion the English, eight channel potential measuring equipment.

  5. Effect of cold working on the corrosion resistance of JPCA stainless steel in flowing Pb–Bi at 450 °C

    International Nuclear Information System (INIS)

    Rivai, Abu Khalid; Saito, Shigeru; Tezuka, Masao; Kato, Chiaki; Kikuchi, Kenji

    2012-01-01

    Development of a high performance proton beam window material is one of the critical issues for the deployment of the accelerator-driven transmutation system (ADS) with liquid Pb–Bi eutectic as a spallation target and coolant. In the present study, we applied 20% cold work treatment to JPCA austenitic stainless steel and investigated it from the corrosion behavior viewpoint. The corrosion test of 20% cold-worked JPCA SS has been carried in the JLBL-1 (JAEA Lead–Bismuth Loop-1) apparatus. The maximum temperature, the temperature difference, the flow velocity and the exposure time of the liquid Pb–Bi were 450 °C, 100 °C, 1 m/s, and 1000 h, respectively. For comparison analysis, JPCA SS without cold working was also tested in the same time and conditions with the 20% cold-worked JPCA SS. The results showed a different corrosion behavior between the JPCA SS without and with cold working. As for the JPCA SS without cold working, Pb–Bi penetrated into the matrix through a ferrite layer which was formed because of constituent metals dissolution from the matrix into Pb–Bi. As for the 20% cold-worked JPCA SS, dissolution attack occurred only partially and formed localized superficial pitting corrosion. It was found that the different corrosion behavior occurred because the cold working induced a structure transformation from γ-austenite to α′-martensite and affected the corrosion resistance of the JPCA SS in flowing Pb–Bi at 450 °C.

  6. Inverse methods for estimating primary input signals from time-averaged isotope profiles

    Science.gov (United States)

    Passey, Benjamin H.; Cerling, Thure E.; Schuster, Gerard T.; Robinson, Todd F.; Roeder, Beverly L.; Krueger, Stephen K.

    2005-08-01

    Mammalian teeth are invaluable archives of ancient seasonality because they record along their growth axes an isotopic record of temporal change in environment, plant diet, and animal behavior. A major problem with the intra-tooth method is that intra-tooth isotope profiles can be extremely time-averaged compared to the actual pattern of isotopic variation experienced by the animal during tooth formation. This time-averaging is a result of the temporal and spatial characteristics of amelogenesis (tooth enamel formation), and also results from laboratory sampling. This paper develops and evaluates an inverse method for reconstructing original input signals from time-averaged intra-tooth isotope profiles. The method requires that the temporal and spatial patterns of amelogenesis are known for the specific tooth and uses a minimum length solution of the linear system Am = d, where d is the measured isotopic profile, A is a matrix describing temporal and spatial averaging during amelogenesis and sampling, and m is the input vector that is sought. Accuracy is dependent on several factors, including the total measurement error and the isotopic structure of the measured profile. The method is shown to accurately reconstruct known input signals for synthetic tooth enamel profiles and the known input signal for a rabbit that underwent controlled dietary changes. Application to carbon isotope profiles of modern hippopotamus canines reveals detailed dietary histories that are not apparent from the measured data alone. Inverse methods show promise as an effective means of dealing with the time-averaging problem in studies of intra-tooth isotopic variation.

  7. Evaluation of MELTGUARD{sup TM} - a measuring system for control of fireside corrosion in boilers; Utvaerdering av MELTGUARD{sup TM} - ett maetsystem foer kontroll av roekgassidig korrosion i pannor

    Energy Technology Data Exchange (ETDEWEB)

    Henderson, Pamela [Vattenfall Utveckling AB, Stockholm (Sweden)

    2001-10-01

    Studsvik AB has developed and now owns the patent for a product called MELTGUARD. According to information from Studsvik, Meltguard is a measuring probe that shows in real-time how much corrosion is occurring and that can reduce costs and increase the lifetime of power boilers burning biomass. The product consists of a tubular air-cooled probe which is exposed in the flue gas through an existing inspection port. The electrodes in the probe react with the flue gas and ash deposit and corrosion is registered as the short-circuited corrosion current (using the zero resistance method) between rings made of the investigated material. The aim of the project was to independently evaluate Meltguard, compare it with a conventional corrosion probe and to publish the results for the Swedish thermal power industry. Two steels have been compared on the probes (a Meltguard-probe can accommodate a maximum of two test pieces), with about the same temperature. Measurements have been carried out with the steels SS2218 (T22) and Esshete 1250 on a Meltguard probe in the biomass fired boiler at Naessjoe combined heat and power plant during the period November 2000 to March 2001. For a 48 hour period sulphur was added to the fuel supply to change the fuel chemistry and influence the corrosion rate. The corrosion current for SS2218 was unstable, fluctuating considerably throughout the measuring period, and was greatly affected by soot-blowing. Usually, soot-blowing resulted in a marked decrease in the corrosion current. No simple or clear relationship between the boiler load and the average corrosion current could be determined. The corrosion current for Esshete 1250 was mostly stable, about 20{mu}A. The current for SS2218 was a little higher than that for E1250, but the relationship between current and corrosion rate was unclear. It was obviously not a linear function as the corrosion measured in 2218, when the testing was completed, was approximately four times greater than that in E

  8. Modelling the waterside corrosion of PWR fuel rods

    International Nuclear Information System (INIS)

    Abram, T.J.

    1997-01-01

    The mechanism of zirconium alloy cladding corrosion in PWRs is briefly reviewed, and an engineering corrosion model is proposed. The basic model is intended to produce a best-estimate fit to circumferentially-average oxide thickness measurements obtained from inter-span positions, way from the effects of structural or flow mixing grids. The model comprises an initial pre-transition weight gain expression which follows cubic rate kinetics. On reaching a critical oxide thickness, a transition to linear rate kinetics occurs. The post-transition corrosion rate includes a term which is dependent on fast neutron flux, and an Arrhenius thermal corrosion rate which has been fitted to isothermal ex-reactor data. This thermal corrosion rate is enhanced by the presence of lithium in the coolant, and by the concentration of hydrogen in the cladding. Different cladding materials are accounted for in the selection of the model constants, and results for standard Zircaloy-4, low tin (or ''optimized'') Zircaloy-4, and the Westinghouse advanced alloy ZIRLO TM are presented. A method of accounting for the effects of grids is described, and the application of the model within the ENIGMA-B and ZROX codes is discussed. (author). 35 refs, 6 figs, 3 tabs

  9. Joint Maximum Likelihood Time Delay Estimation of Unknown Event-Related Potential Signals for EEG Sensor Signal Quality Enhancement

    Science.gov (United States)

    Kim, Kyungsoo; Lim, Sung-Ho; Lee, Jaeseok; Kang, Won-Seok; Moon, Cheil; Choi, Ji-Woong

    2016-01-01

    Electroencephalograms (EEGs) measure a brain signal that contains abundant information about the human brain function and health. For this reason, recent clinical brain research and brain computer interface (BCI) studies use EEG signals in many applications. Due to the significant noise in EEG traces, signal processing to enhance the signal to noise power ratio (SNR) is necessary for EEG analysis, especially for non-invasive EEG. A typical method to improve the SNR is averaging many trials of event related potential (ERP) signal that represents a brain’s response to a particular stimulus or a task. The averaging, however, is very sensitive to variable delays. In this study, we propose two time delay estimation (TDE) schemes based on a joint maximum likelihood (ML) criterion to compensate the uncertain delays which may be different in each trial. We evaluate the performance for different types of signals such as random, deterministic, and real EEG signals. The results show that the proposed schemes provide better performance than other conventional schemes employing averaged signal as a reference, e.g., up to 4 dB gain at the expected delay error of 10°. PMID:27322267

  10. Joint Maximum Likelihood Time Delay Estimation of Unknown Event-Related Potential Signals for EEG Sensor Signal Quality Enhancement

    Directory of Open Access Journals (Sweden)

    Kyungsoo Kim

    2016-06-01

    Full Text Available Electroencephalograms (EEGs measure a brain signal that contains abundant information about the human brain function and health. For this reason, recent clinical brain research and brain computer interface (BCI studies use EEG signals in many applications. Due to the significant noise in EEG traces, signal processing to enhance the signal to noise power ratio (SNR is necessary for EEG analysis, especially for non-invasive EEG. A typical method to improve the SNR is averaging many trials of event related potential (ERP signal that represents a brain’s response to a particular stimulus or a task. The averaging, however, is very sensitive to variable delays. In this study, we propose two time delay estimation (TDE schemes based on a joint maximum likelihood (ML criterion to compensate the uncertain delays which may be different in each trial. We evaluate the performance for different types of signals such as random, deterministic, and real EEG signals. The results show that the proposed schemes provide better performance than other conventional schemes employing averaged signal as a reference, e.g., up to 4 dB gain at the expected delay error of 10°.

  11. Corrosion calculations report for the safety assessment SR-Site

    International Nuclear Information System (INIS)

    2010-12-01

    This report is a compilation of the quantitative assessments of corrosion of the copper canisters in a KBS-3 repository. The calculations are part of the safety assessment SR-Site that is the long-term safety assessment to support the license application for building a final repository for spent nuclear fuel at Forsmark, Sweden. The safety assessment methodology gives the frame for the structured and documented approach to assess all conceivable corrosion processes. The quantitative assessments are done in different ways depending on the nature of the process and on the implications for the long-term safety. The starting point for the handling of the corrosion processes is the description of all known corrosion processes for copper with the current knowledge base and applied to the specific system and geology. Already at this stage some processes are excluded for further analysis, for example if the repository environment is not a sufficient prerequisite for the process to occur. The next step is to identify processes where the extent of corrosion could be bounded, e.g. by a mass balance approach. For processes where a mass balance is not limiting, the mass transport of corrodants (or corrosion products) is taken into account. A simple approach would be just to calculate the diffusive transport of corrodants through the bentonite, but generally the transport resistance for the interface between groundwater in a rock fracture intersecting the deposition hole and the bentonite buffer is more important. In SR-Site, the concept of equivalent flowrate, Q eq , is used. This assessment is done integrated with the evaluation of the geochemical and hydrogeological evolution of the repository. For most of the corrosion processes analysed, the corrosion depth is much smaller than the copper shell thickness, even for the assessment time of 10 6 years. Several processes give corrosion depths less than 100 μm, but no process give corrosion depths larger than a few millimetres

  12. Corrosion calculations report for the safety assessment SR-Site

    Energy Technology Data Exchange (ETDEWEB)

    2010-12-15

    This report is a compilation of the quantitative assessments of corrosion of the copper canisters in a KBS-3 repository. The calculations are part of the safety assessment SR-Site that is the long-term safety assessment to support the license application for building a final repository for spent nuclear fuel at Forsmark, Sweden. The safety assessment methodology gives the frame for the structured and documented approach to assess all conceivable corrosion processes. The quantitative assessments are done in different ways depending on the nature of the process and on the implications for the long-term safety. The starting point for the handling of the corrosion processes is the description of all known corrosion processes for copper with the current knowledge base and applied to the specific system and geology. Already at this stage some processes are excluded for further analysis, for example if the repository environment is not a sufficient prerequisite for the process to occur. The next step is to identify processes where the extent of corrosion could be bounded, e.g. by a mass balance approach. For processes where a mass balance is not limiting, the mass transport of corrodants (or corrosion products) is taken into account. A simple approach would be just to calculate the diffusive transport of corrodants through the bentonite, but generally the transport resistance for the interface between groundwater in a rock fracture intersecting the deposition hole and the bentonite buffer is more important. In SR-Site, the concept of equivalent flowrate, Q{sub eq}, is used. This assessment is done integrated with the evaluation of the geochemical and hydrogeological evolution of the repository. For most of the corrosion processes analysed, the corrosion depth is much smaller than the copper shell thickness, even for the assessment time of 106 years. Several processes give corrosion depths less than 100 mum, but no process give corrosion depths larger than a few

  13. The influence of Fe2+ concentration and deposition time on the corrosion resistance of the electrodeposited zinc–nickel–iron alloys

    Directory of Open Access Journals (Sweden)

    M.M. Abou-Krisha

    2016-11-01

    Full Text Available Electrodeposition operating conditions for Zn–Ni–Fe alloys from sulfate baths and the corrosion resistance of the electrodeposited alloys were studied. The comparison between Zn–Ni and Zn–Ni–Fe alloys co-deposition revealed that the remarkable inhibition of Ni and Fe deposition takes place due to the presence of Zn2+ in the plating bath. The electrodeposition was performed on the steel substrate, under galvanostatic conditions, for varying Fe2+ bath concentrations and at different times. X-ray diffraction studies of the deposit showed the presence of Fe3Ni2 phase and γ-phase with a composition of Ni2Zn11. The obtained data also exposed that the corrosion resistance increases as a result of increasing Fe2+ concentration and deposition time. Investigation was carried out using cyclic voltammetry and galvastatic techniques for electrodeposition, while linear polarization resistance and anodic linear sweeping voltammetry techniques were used for corrosion study.

  14. Corrosion in airframes

    OpenAIRE

    PETROVIC ZORAN C.

    2016-01-01

    The introductory chapter provides a brief reference to the issue of corrosion and corrosion damage to aircraft structures. Depending on the nature and dimensions of this non uniformity, three different categories of corrosion are defined: uniform, selective and localized corrosion. The following chapters present the forms of corrosion that can occur in three defined categories of corrosion. Conditions that cause certain types of corrosion in various corrosive environments are discussed. Examp...

  15. Downhole corrosion mechanisms and mitigation strategies

    Energy Technology Data Exchange (ETDEWEB)

    McDougall, D. [Baker Hughes Canada, Calgary, AB (Canada)

    2010-07-01

    Pipeline corrosion refers to its deterioration because of a reaction with its environment. Although the physical condition of the metal at the anode initiates the corrosion process, it is the chemistry and composition of the electrolyte that controls the rate of the corrosion reaction and the severity of the corrosion. This presentation described the role of corrosion rate accelerators, with particular reference to dissolved gases such as oxygen, hydrogen sulfides and carbon dioxide, as well as pH levels, salinity, flow rate, temperature and presence of solids such as iron sulfides and sulfur. The effects of these accelerators were shown to be additive. Mitigation strategies include using materials such as resistant metal alloys or fiberglass, and applying coatings and chemical inhibitors. The importance of corrosion monitoring was also emphasized, with particular reference to the value of examining the number of corrosion related failures that have occurred over a fixed period of time. It was concluded that the ability to analyze samples of failed materials results in a better understanding of the cause of the failure, and is an integral part of designing any successful corrosion control program. tabs., figs.

  16. Corrosion engineering

    Energy Technology Data Exchange (ETDEWEB)

    Fontana, M.G.

    1986-01-01

    This book emphasizes the engineering approach to handling corrosion. It presents corrosion data by corrosives or environments rather than by materials. It discusses the corrosion engineering of noble metals, ''exotic'' metals, non-metallics, coatings, mechanical properties, and corrosion testing, as well as modern concepts. New sections have been added on fracture mechanics, laser alloying, nuclear waste isolation, solar energy, geothermal energy, and the Statue of Liberty. Special isocorrosion charts, developed by the author, are introduced as a quick way to look at candidates for a particular corrosive.

  17. Modeling an Application's Theoretical Minimum and Average Transactional Response Times

    Energy Technology Data Exchange (ETDEWEB)

    Paiz, Mary Rose [Sandia National Lab. (SNL-NM), Albuquerque, NM (United States)

    2015-04-01

    The theoretical minimum transactional response time of an application serves as a ba- sis for the expected response time. The lower threshold for the minimum response time represents the minimum amount of time that the application should take to complete a transaction. Knowing the lower threshold is beneficial in detecting anomalies that are re- sults of unsuccessful transactions. On the converse, when an application's response time falls above an upper threshold, there is likely an anomaly in the application that is causing unusual performance issues in the transaction. This report explains how the non-stationary Generalized Extreme Value distribution is used to estimate the lower threshold of an ap- plication's daily minimum transactional response time. It also explains how the seasonal Autoregressive Integrated Moving Average time series model is used to estimate the upper threshold for an application's average transactional response time.

  18. Experimental and quantum chemical simulations on the corrosion inhibition of mild steel by 3-((5-(3,5-dinitrophenyl)-1,3,4-thiadiazol-2-yl)imino)indolin-2-one

    Science.gov (United States)

    Al-Azawi, Khalida F.; Mohammed, Iman Mahdi; Al-Baghdadi, Shaimaa B.; Salman, Taghried A.; Issa, Hamsa A.; Al-Amiery, Ahmed A.; Gaaz, Tayser Sumer; Kadhum, Abdul Amir H.

    2018-06-01

    Iraq has been one of the most extensive oil and natural gas industries in the world. The corrosion of mild steel is costly and insufficiency process. It is responsible for great loss in manufacture and environment. Natural and organic inhibitors have been utilized for a long time to inhibit the corrosion. Selected thiadiazol derivative, namely 3-((5-(3,5-dinitrophenyl)-1,3,4-thiadiazol-2-yl)imino)indolin-2-one (TDIO) was investigated for it inhibitive impacts in 1 M HCl medium on corrosion of mild steel using weight loss and scanning electron microscope techniques. The maximum inhibition efficiency up to 90.7% at the maximum inhibitor concentration 0.5 mM. Surface morphology of results demonstrated that TDIO formed adsorbed film on surface of mild steel in hydrochloric acid solution. Give molecular based clarifications to the inhibitive impacts of the studied. The interactions between mild steel surface and the inhibitor molecules have been undertaken to further corroborate the methodological results.

  19. Influence of corrosion layers on quantitative analysis

    International Nuclear Information System (INIS)

    Denker, A.; Bohne, W.; Opitz-Coutureau, J.; Rauschenberg, J.; Roehrich, J.; Strub, E.

    2005-01-01

    Art historians and restorers in charge of ancient metal objects are often reluctant to remove the corrosion layer evolved over time, as this would change the appearance of the artefact dramatically. Therefore, when an elemental analysis of the objects is required, this has to be done by penetrating the corrosion layer. In this work the influence of corrosion was studied on Chinese and Roman coins, where removal of oxidized material was possible. Measurements on spots with and without corrosion are presented and the results discussed

  20. Corrosion in the nuclear power industry

    International Nuclear Information System (INIS)

    Danko, J.C.

    1987-01-01

    This article reviews the major corrosion problems in light water reactors, the research on the corrosion mechanism(s), and the development of engineering solutions and their implementation. To understand the occurrence of corrosion problems, a brief historical perspective of the corrosion design basis of commercial light water reactors, boiling water, and pressurized water reactors is necessary. Although corrosion was considered in the plant designs, it was not viewed as a serious problem. This was based on the results of laboratory experiments and in-reactor tests that did not indicate any major corrosion problems with the materials selected for the plant construction. However, the laboratory tests did not necessarily reproduce the reactor operating conditions and the early in-reactor test did not fully represent the commercial reactor conditions in all cases, and, finally, the test times were indeed of short duration relative to the plant design lifetime of 40 years. Thus, the design basis for the materials selection was determined on the favorable but limited test data that were available, and corrosion limitations on component integrity were therefore not anticipated

  1. Achievments of corrosion science and corrosion protection technology

    International Nuclear Information System (INIS)

    Fontana, M.; Stehjl, R.

    1985-01-01

    Problems of corrosion-mechanical strength of metals, effect of corrosive media on creep characteristics are presented. New concepts of the mechanism of corrosion cracking and its relation to hydrogen embrittlement are described. Kinetics and mechanism of hydrogen embrittlement effect on the process of corrosion cracking of different steels and alloys are considered. The dependence of such types of failure on various structural factors is shown. Data on corrosion cracking of high-strength aluminium and titanium alloys, mechanism of the processes and protective methods are given

  2. Corrosion of Continuous Fiber Reinforced Aluminum Metal Matrix Composites (CF-AMCs)

    Science.gov (United States)

    Tiwari, Shruti

    The first objective of this research is to study the atmospheric corrosion behavior of continuous reinforced aluminum matrix composites (CF-AMCs). The materials used for this research were alumina (Al2O3) and nickel (Ni) coated carbon (C) fibers reinforced AMCs. The major focus is to identify the correlation between atmospheric parameters and the corrosion rates of CF-AMCs in the multitude of microclimates and environments in Hawai'i. The micro-structures of CF-AMCs were obtained to correlate the microstructures with their corrosion performances. Also electrochemical polarization experiments were conducted in the laboratory to explain the corrosion mechanism of CF-AMCs. In addition, CF-AMCs were exposed to seven different test sites for three exposure periods. The various climatic conditions like temperature (T), relative humidity (RH), rainfall (RF), time of wetness (TOW), chloride (Cl- ) and sulfate (SO42-) deposition rate, and pH were monitored for three exposure period. Likewise, mass losses of CF-AMCs at each test site for three exposure periods were determined. The microstructure of the CF-AMCS showed that Al/C/50f MMCs contained a Ni-rich phase in the matrix, indicating that the Ni coating on the C fiber dissolved in the matrix. The intermetallic phases obtained in Al-2wt% Cu/Al 2O3/50f-T6 MMC and Al-2wt%-T6 monolith were rich in Cu and Fe. The intermetallic phases obtained in Al 7075/Al2O3/50f-T6 MMC and Al 7075-T6 monolith also contained traces of Mg, Zn, Ni, and Si. Electrochemical polarization experiment indicated that the Al/Al 2O3/50f Al-2wt% Cu/Al2O3/50f-T6 and Al 7075/Al2O3/50f-T6 MMC showed similar corrosion trends as their respective monoliths pure Al, Al-2wt%-T6 and Al 7075-T6 in both aerated and deaerated condition. Al2O3 fiber, being an insulator, did not have a great effect on the polarization behavior of the composites. Al/C/50f MMCs corroded at a much faster rate as compared to pure Al monolith due to the galvanic effect between C and Al

  3. CORROSION RATE OF STEELS DX51D AND S220GD IN DIFFERENT CORROSION ENVIRONMENT

    Directory of Open Access Journals (Sweden)

    Alina Crina CIUBOTARIU

    2016-06-01

    stability of the steel decrease in time and corrosion stability coefficient increase at 6. For steel S220GD it was found a corrosion stability coefficient equal with 6 after 21 days of immersion and 5 after 28 days of immersion in 5% NaOH solution. In 0.5M NaCl solution the corrosion stability coefficient at steel S220GD was 6 for all period tested.

  4. Corrosion life-time assessment of carbon steel and stainless alloys for geological disposal facility

    International Nuclear Information System (INIS)

    Kosaki, Akio; Komada, Hiroya

    1993-01-01

    The disposal facility for radioactive wastes requires long-term integrity. Metal is being considered for use as the engineered barrier which constructs the outer walls in such a facility, in order to prevent groundwater percolation. Thus, the most important problem for the integrity of the engineered barrier is corrosion by groundwater. There are two ways for using metal as an engineered barrier; one is as a structural material; and the other is as the inner-lining material of a concrete wall. This report discusses the corrosion lifetime assessment of carbon steel used as a structural and lining material, and stainless alloys, Type 304 steel and Titanium alloys used as lining materials. Corrosion potential and crevice corrosion are measured in the environment of neutral and alkalized water

  5. Erosion–corrosion and corrosion properties of DLC coated low temperature Erosion–corrosion and corrosion properties of DLC coated low temperature

    DEFF Research Database (Denmark)

    Jellesen, Morten Stendahl; Christiansen, Thomas; Hilbert, Lisbeth Rischel

    2009-01-01

    of AISI 316 as substrate for DLC coatings are investigated. Corrosion and erosion–corrosion measurements were carried out on low temperature nitrided stainless steel AISI 316 and on low temperature nitrided stainless steel AISI 316 with a top layer of DLC. The combination of DLC and low temperature...... nitriding dramatically reduces the amount of erosion–corrosion of stainless steel under impingement of particles in a corrosive medium....

  6. Passive Corrosion Behavior of Alloy 22

    International Nuclear Information System (INIS)

    R.B. Rebak; J.H. Payer

    2006-01-01

    Alloy 22 (NO6022) was designed to stand the most aggressive industrial applications, including both reducing and oxidizing acids. Even in the most aggressive environments, if the temperature is lower than 150 F (66 C) Alloy 22 would remain in the passive state having particularly low corrosion rates. In multi-ionic solutions that may simulate the behavior of concentrated ground water, even at near boiling temperatures, the corrosion rate of Alloy 22 is only a few nano-meters per year because the alloy is in the complete passive state. The corrosion rate of passive Alloy 22 decreases as the time increases. Immersion corrosion testing also show that the newer generation of Ni-Cr-Mo alloys may offer a better corrosion resistance than Alloy 22 only in some highly aggressive conditions such as in hot acids

  7. Corrosion of metal iron in contact with anoxic clay at 90 °C: Characterization of the corrosion products after two years of interaction

    International Nuclear Information System (INIS)

    Schlegel, Michel L.; Bataillon, Christian; Brucker, Florence; Blanc, Cécile; Prêt, Dimitri; Foy, Eddy; Chorro, Matthieu

    2014-01-01

    surface, and intermixed with clay minerals towards the bulk matrix. The average thickness of oxidized iron, as measured by the average of distances from the original to the final metal surface, was 13 ± 1 and 15 ± 1 μm for the massive rod and the micro-overpack, respectively. The corresponding Fe amount is about twice the amount of Fe present in the corrosion products. Thus a significant Fe fraction migrated in the nearby clay, likely as Fe (II) , and could act as a significant buffer of the electrochemical potential

  8. Predicting concrete corrosion of sewers using artificial neural network.

    Science.gov (United States)

    Jiang, Guangming; Keller, Jurg; Bond, Philip L; Yuan, Zhiguo

    2016-04-01

    Corrosion is often a major failure mechanism for concrete sewers and under such circumstances the sewer service life is largely determined by the progression of microbially induced concrete corrosion. The modelling of sewer processes has become possible due to the improved understanding of in-sewer transformation. Recent systematic studies about the correlation between the corrosion processes and sewer environment factors should be utilized to improve the prediction capability of service life by sewer models. This paper presents an artificial neural network (ANN)-based approach for modelling the concrete corrosion processes in sewers. The approach included predicting the time for the corrosion to initiate and then predicting the corrosion rate after the initiation period. The ANN model was trained and validated with long-term (4.5 years) corrosion data obtained in laboratory corrosion chambers, and further verified with field measurements in real sewers across Australia. The trained model estimated the corrosion initiation time and corrosion rates very close to those measured in Australian sewers. The ANN model performed better than a multiple regression model also developed on the same dataset. Additionally, the ANN model can serve as a prediction framework for sewer service life, which can be progressively improved and expanded by including corrosion rates measured in different sewer conditions. Furthermore, the proposed methodology holds promise to facilitate the construction of analytical models associated with corrosion processes of concrete sewers. Copyright © 2016 Elsevier Ltd. All rights reserved.

  9. The Tension and Puncture Properties of HDPE Geomembrane under the Corrosion of Leachate.

    Science.gov (United States)

    Xue, Qiang; Zhang, Qian; Li, Zhen-Ze; Xiao, Kai

    2013-09-17

    To investigate the gradual failure of high-density polyethylene (HDPE) geomembrane as a result of long-term corrosion, four dynamic corrosion tests were conducted at different temperatures and durations. By combining tension and puncture tests, we systematically studied the variation law of tension and puncture properties of the HDPE geomembrane under different corrosion conditions. Results showed that tension and puncture failure of the HDPE geomembrane was progressive, and tensile strength in the longitudinal grain direction was evidently better than that in the transverse direction. Punctures appeared shortly after puncture force reached the puncture strength. The tensile strength of geomembrane was in inversely proportional to the corrosion time, and the impact of corrosion was more obvious in the longitudinal direction than transverse direction. As corrosion time increased, puncture strength decreased and corresponding deformation increased. As with corrosion time, the increase of corrosion temperature induced the decrease of geomembrane tensile strength. Tensile and puncture strength were extremely sensitive to temperature. Overall, residual strength had a negative correlation with corrosion time or temperature. Elongation variation increased initially and then decreased with the increase in temperature. However, it did not show significant law with corrosion time. The reduction in puncture strength and the increase in puncture deformation had positive correlations with corrosion time or temperature. The geomembrane softened under corrosion condition. The conclusion may be applicable to the proper designing of the HDPE geomembrane in landfill barrier system.

  10. Standard practice for calculation of corrosion rates and related information from electrochemical measurements

    CERN Document Server

    American Society for Testing and Materials. Philadelphia

    1989-01-01

    1.1 This practice covers the providing of guidance in converting the results of electrochemical measurements to rates of uniform corrosion. Calculation methods for converting corrosion current density values to either mass loss rates or average penetration rates are given for most engineering alloys. In addition, some guidelines for converting polarization resistance values to corrosion rates are provided. 1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

  11. Corrosion behavior of Cu during graphene growth by CVD

    International Nuclear Information System (INIS)

    Dong, Yuhua; Liu, Qingqing; Zhou, Qiong

    2014-01-01

    Highlights: • Graphene films were deposited on the Cu by chemical vapor deposition method. • Annealing affects the corrosion property of Cu. • Graphene films improve corrosion performance of Cu for a short period of time. - Abstract: The corrosion performance of Cu samples may be affected by annealing at high temperatures during graphene growth via the chemical vapor deposition method. In this study, multiple graphene films were deposited on Cu and characterized by Raman spectroscopy and transmission electron microscopy. The corrosion behavior of Cu immersed in 3.5 wt.% NaCl solution was investigated using electrochemical impedance spectroscopy. The Cu morphology was observed by optical microscopy and scanning electron microscopy. Results indicated that annealing affects the corrosion process of Cu. The presence of graphene films on the Cu substrate improved the corrosion performance of the material for a short period of time

  12. Synthesis and characterization of a novel organic corrosion inhibitor for mild steel in 1 M hydrochloric acid

    Science.gov (United States)

    Ahmed, Mohammed H. Othman; Al-Amiery, Ahmed A.; Al-Majedy, Yasmin K.; Kadhum, Abdul Amir H.; Mohamad, Abu Bakar; Gaaz, Tayser Sumer

    2018-03-01

    The synthesis and characterization of a novel organic corrosion inhibitor (4-(3-mercapto-5,6,7,8-tetrahydro-[1,2,4]triazolo[4,3-b][1,2,4,5]tetrazin-6-yl)phenol), for mild steel in 1 M hydrochloric acid (HCl) has been successfully reported for the first time. The inhibitor evaluated as corrosion inhibitor for mild steel in 1 M of Hydrochloric acid solution using electrochemical impedance spectroscopy (EIS), and electrochemical frequency modulation (EFM) measurement techniques. Changes in the impedance parameters suggested an adsorption of the inhibitor onto the mild steel surface, leading to the formation of protective films. The results show that the inhibition efficiencies increased with increasing the concentrations of the inhibitors and decreased with increasing temperature. The maximum inhibition efficiency up to 67% at the maximum concentration 0.5 mM. This shows that those inhibitors are effective in helping to reduce and slowing down the corrosion process that occurs to mild steel with a hydrochloric acid solution by providing an organic inhibitor for the mild steel that can be weakened by increasing the temperature. The adsorption process of the synthesized organic inhibitor depends on its electronic characteristics in addition to steric effects and the nature of metal surface, temperature degree and the varying degrees of surface-site activity. The synthesized inhibitor molecules were absorbed by metal surface and follow Langmuir isotherms.

  13. Pullulan as a potent green inhibitor for corrosion mitigation of aluminum composite: Electrochemical and surface studies.

    Science.gov (United States)

    B P, Charitha; Rao, Padmalatha

    2018-06-01

    This work emphasizes the corrosion inhibition ability of pullulan, an environmentally benign fungal polysaccharide on acid corrosion of 6061Aluminum-15% (v) SiC (P) composite material (Al-CM). The electrochemical measurements such as potentiodynamic polarization (PDP) and electrochemical impedance spectroscopy (EIS) studies were carried out for the corrosion inhibition studies. Conditions were optimized to obtain maximum inhibition efficiency, by performing the experiment at varying concentrations of inhibitor, in the temperature range of 308K- 323K. Surface morphology studies were done to reaffirm the adsorption of inhibitor on the surface of composite material. Pullulan acted as mixed type of inhibitor with a maximum efficiency of 89% at 303K for the addition of 1.0 gL -1 of inhibitor. Evaluation of kinetic and thermodynamic parameters revealed that inhibitor underwent physical adsorption onto the surface of Al-CM and obeyed Freundlich adsorption isotherm. The surface characterization like SEM-EDX, AFM confirmed the adsorption of pullulan molecule. Pullulan can be considered as effective, eco friendly green inhibitor for the corrosion control of Al-CM. Copyright © 2018 Elsevier B.V. All rights reserved.

  14. Some in-reactor loop experiments on corrosion product transport and water chemistry

    International Nuclear Information System (INIS)

    Balakrishnan, P.V.; Allison, G.M.

    1978-01-01

    A study of the transport of activated corrosion products in the heat transport circuit of pressurized water-cooled nuclear reactors using an in-reactor loop showed that the concentration of particulate and dissolved corrosion products in the high-temperature water depends on such chemical parameters as pH and dissolved hydrogen concentration. Transients in these parameters, as well as in temperature, generally increase the concentration of suspended corrosion products. The maximum concentration of particles observed is much reduced when high-flow, high-temperature filtration is used. Filtration also reduces the steady-state concentration of particles. Dissolved corrosion products are mainly responsible for activity accumulation on surfaces. The data obtained from this study were used to estimate the rate constants for some of the transfer processes involved in the contamination of the primary heat transport circuit in water-cooled nuclear power reactors

  15. Corrosion Evaluation and Corrosion Control of Steam Generators

    International Nuclear Information System (INIS)

    Maeng, W. Y.; Kim, U. C.; Sung, K. W.; Na, J. W.; Lee, Y. H.; Lee, D. H.; Kim, K. M.

    2008-06-01

    Corrosion damage significantly influences the integrity and efficiency of steam generator. Corrosion problems of steam generator are unsolved issues until now even though much effort is made around world. Especially the stress corrosion cracking of heat exchange materials is the first issue to be solved. The corrosion protection method of steam generator is important and urgent for the guarantee of nuclear plant's integrity. The objectives of this study are 1) to evaluate the corrosion properties of steam generator materials, 2) to optimize the water chemistry of steam generator and 3) to develop the corrosion protection method of primary and secondary sides of steam generator. The results will be reflected to the water chemistry guideline for improving the integrity and efficiency of steam generator in domestic power plants

  16. Life time forecasting method upon occurrence of stress corrosion cracking of structure and test device therefor

    International Nuclear Information System (INIS)

    Anzai, Hideya; Kida, Toshitaka; Urayama, Yoshinao; Kikuchi, Eiji; Shimanuki, Sei; Kuniya, Jiro; Nakata, Kiyotomo; Izumitani, Masakiyo; Hattori, Shigeo.

    1993-01-01

    A load stress is applied to a metal piece made of a material identical with the constituent material of a structure and having the sensitivity enhanced to a predetermined level, and plurality of such pieces are immersed in a corrosive circumstance in this state. Then, the time from the immersion till the rupture thereof and the number of ruptured pieces of the metal pieces are detected while observing them. The relation with the probability of rupture is plotted on a paper to determine the life time for the occurrence of minimum stress corrosion creacks (SSC) of the metal pieces. Based on the relationship between the previously determined stress and the life time for the occurrence of minimum SSC, the ratio between the life time for the occurrence of minimum SSC relative to estimated stress applied to the structure and the life time for the occurrence of minimum SSC relative to the stress applied to the metal pieces is determined as a first SSC acceleration rate. The ratio between the time of occurrence for minimum SSC and the sensitivity is determined as a second SSC acceleration rate. The first and the second SSC acceleration rates are multiplied to estimate the time for the occurrence of SSC of the structure. Then, the life time for the occurrence of SSC for the equipments and structures can be recognized quantitatively, to prevent ruptures of actual equipments and extend the life time. (N.H.)

  17. A polynomial time algorithm for solving the maximum flow problem in directed networks

    International Nuclear Information System (INIS)

    Tlas, M.

    2015-01-01

    An efficient polynomial time algorithm for solving maximum flow problems has been proposed in this paper. The algorithm is basically based on the binary representation of capacities; it solves the maximum flow problem as a sequence of O(m) shortest path problems on residual networks with nodes and m arcs. It runs in O(m"2r) time, where is the smallest integer greater than or equal to log B , and B is the largest arc capacity of the network. A numerical example has been illustrated using this proposed algorithm.(author)

  18. Corrosion-Activated Micro-Containers for Environmentally Friendly Corrosion Protective Coatings

    Science.gov (United States)

    Li, Wenyan; Buhrow, J. W.; Zhang, X.; Johnsey, M. N.; Pearman, B. P.; Jolley, S. T.; Calle, L. M.

    2016-01-01

    This work concerns the development of environmentally friendly encapsulation technology, specifically designed to incorporate corrosion indicators, inhibitors, and self-healing agents into a coating, in such a way that the delivery of the indicators and inhibitors is triggered by the corrosion process, and the delivery of self-healing agents is triggered by mechanical damage to the coating. Encapsulation of the active corrosion control ingredients allows the incorporation of desired autonomous corrosion control functions such as: early corrosion detection, hidden corrosion detection, corrosion inhibition, and self-healing of mechanical damage into a coating. The technology offers the versatility needed to include one or several corrosion control functions into the same coating.The development of the encapsulation technology has progressed from the initial proof-of-concept work, in which a corrosion indicator was encapsulated into an oil-core (hydrophobic) microcapsule and shown to be delivered autonomously, under simulated corrosion conditions, to a sophisticated portfolio of micro carriers (organic, inorganic, and hybrid) that can be used to deliver a wide range of active corrosion ingredients at a rate that can be adjusted to offer immediate as well as long-term corrosion control. The micro carriers have been incorporated into different coating formulas to test and optimize the autonomous corrosion detection, inhibition, and self-healing functions of the coatings. This paper provides an overview of progress made to date and highlights recent technical developments, such as improved corrosion detection sensitivity, inhibitor test results in various types of coatings, and highly effective self-healing coatings based on green chemistry. The NASA Kennedy Space Centers Corrosion Technology Lab at the Kennedy Space Center in Florida, U.S.A. has been developing multifunctional smart coatings based on the microencapsulation of environmentally friendly corrosion

  19. Experiments and models of general corrosion and flow-assisted corrosion of materials in nuclear reactor environments

    Science.gov (United States)

    Cook, William Gordon

    Corrosion and material degradation issues are of concern to all industries. However, the nuclear power industry must conform to more stringent construction, fabrication and operational guidelines due to the perceived additional risk of operating with radioactive components. Thus corrosion and material integrity are of considerable concern for the operators of nuclear power plants and the bodies that govern their operations. In order to keep corrosion low and maintain adequate material integrity, knowledge of the processes that govern the material's breakdown and failure in a given environment are essential. The work presented here details the current understanding of the general corrosion of stainless steel and carbon steel in nuclear reactor primary heat transport systems (PHTS) and examines the mechanisms and possible mitigation techniques for flow-assisted corrosion (FAC) in CANDU outlet feeder pipes. Mechanistic models have been developed based on first principles and a 'solution-pores' mechanism of metal corrosion. The models predict corrosion rates and material transport in the PHTS of a pressurized water reactor (PWR) and the influence of electrochemistry on the corrosion and flow-assisted corrosion of carbon steel in the CANDU outlet feeders. In-situ probes, based on an electrical resistance technique, were developed to measure the real-time corrosion rate of reactor materials in high-temperature water. The probes were used to evaluate the effects of coolant pH and flow on FAC of carbon steel as well as demonstrate of the use of titanium dioxide as a coolant additive to mitigated FAC in CANDU outlet feeder pipes.

  20. Review on stress corrosion and corrosion fatigue failure of centrifugal compressor impeller

    Science.gov (United States)

    Sun, Jiao; Chen, Songying; Qu, Yanpeng; Li, Jianfeng

    2015-03-01

    Corrosion failure, especially stress corrosion cracking and corrosion fatigue, is the main cause of centrifugal compressor impeller failure. And it is concealed and destructive. This paper summarizes the main theories of stress corrosion cracking and corrosion fatigue and its latest developments, and it also points out that existing stress corrosion cracking theories can be reduced to the anodic dissolution (AD), the hydrogen-induced cracking (HIC), and the combined AD and HIC mechanisms. The corrosion behavior and the mechanism of corrosion fatigue in the crack propagation stage are similar to stress corrosion cracking. The effects of stress ratio, loading frequency, and corrosive medium on the corrosion fatigue crack propagation rate are analyzed and summarized. The corrosion behavior and the mechanism of stress corrosion cracking and corrosion fatigue in corrosive environments, which contain sulfide, chlorides, and carbonate, are analyzed. The working environments of the centrifugal compressor impeller show the behavior and the mechanism of stress corrosion cracking and corrosion fatigue in different corrosive environments. The current research methods for centrifugal compressor impeller corrosion failure are analyzed. Physical analysis, numerical simulation, and the fluid-structure interaction method play an increasingly important role in the research on impeller deformation and stress distribution caused by the joint action of aerodynamic load and centrifugal load.

  1. Scale dependence of the average potential around the maximum in Φ4 theories

    International Nuclear Information System (INIS)

    Tetradis, N.; Wetterich, C.

    1992-04-01

    The average potential describes the physics at a length scale k - 1 by averaging out the degrees of freedom with characteristic moments larger than k. The dependence on k can be described by differential evolution equations. We solve these equations for the nonconvex part of the potential around the origin in φ 4 theories, in the phase with spontaneous symmetry breaking. The average potential is real and approaches the convex effective potential in the limit k → 0. Our calculation is relevant for processes for which the shape of the potential at a given scale is important, such as tunneling phenomena or inflation. (orig.)

  2. Corrosion of copper under Canadian nuclear fuel waste disposal conditions

    International Nuclear Information System (INIS)

    King, F.; Litke, C.D.

    1990-01-01

    The corrosion of copper was studied under Canadian nuclear fuel waste disposal conditions. The groundwater in a Canadian waste vault is expected to be saline, with chloride concentrations from 0.1 to 1.0 mol/l. The container would be packed in a sand/clay buffer, and the maximum temperature on the copper surface would be 100C; tests were performed up to 150C. Radiation fields will initially be around 500 rad/h, and conditions will be oxidizing. Sulfides may be present. The minimum design lifetime for the container is 500 years. Most work has been done on uniform corrosion, although pitting has been considered. It was found that the rate of uniform corrosion in aerated NaCl at room temperature is limited by the rate of the anodic reaction, which is controlled mainly by the rate of transport of dissolved metal species away from the copper surface. The rate of corrosion should become controlled by the transport of oxygen to the copper surface only at very low oxygen concentrations. In the presence of gamma radiation the corrosion rate may never become cathodically transport limited. In compacted buffer material, the corrosion rate appears to be limited by the rate of transport of copper species away from the corroding surface. The authors recommend that long-term predictions of container lifetime should be based on the known rate-determining step for the overall corrosion process. 8 refs

  3. Intergranular corrosion testing of austenitic stainless steels in nitric acid solutions

    Energy Technology Data Exchange (ETDEWEB)

    Whillock, G.O.H.; Dunnett, B. F. [British Nuclear Fuels plc, BNFL, B170, Sellafield, Seascale, Cumbria CA20 1PG (United Kingdom)

    2004-07-01

    In hot strong nitric acid solutions, stainless steels exhibit intergranular corrosion. Corrosion rates are often measured from immersion testing of specimens manufactured from the relevant material (e.g. plate or pipe). The corrosion rates, measured from weight loss, are found to increase with time prior to reaching steady state, which can take thousands of hours to achieve. The apparent increase in corrosion rate as a function of time was found to be an artefact due to the surface area of the specimen's being used in the corrosion rate calculations, rather than that of the true area undergoing active corrosion i.e. the grain boundaries. The steady state corrosion rate coincided with the onset of stable grain dropping, where the use of the surface area of the specimen to convert the weight loss measurements to corrosion rates was found to be appropriate. This was confirmed by sectioning of the specimens and measuring the penetration depths. The rate of penetration was found to be independent of time and no induction period was observed. A method was developed to shorten considerably the testing time to reach the steady state corrosion rate by use of a pre-treatment that induces grain dropping. The long-term corrosion rates from specimens which were pre-treated was similar to that achieved after prolonged testing of untreated (i.e. initially ground) specimens. The presence of cut surfaces is generally unavoidable in the simple immersion testing of specimens in test solutions. However, inaccuracy in the results may occur as the measured corrosion rate is often influenced by the orientation of the microstructure, the highest rates typically being observed on the cut surfaces. Two methods are presented which allow deconvolution of the corrosion rates from immersion testing of specimens containing cut surfaces, thus allowing reliable prediction of the long-term corrosion rate of plate surfaces. (authors)

  4. Effect of zinc injection on BWR fuel cladding corrosion. Pt. 1. Study on an accelerated corrosion condition to evaluate corrosion resistance of zircaloy-2 fuel cladding

    International Nuclear Information System (INIS)

    Kawamura, Hirotaka; Kanbe, Hiromu; Furuya, Masahiro

    2002-01-01

    Japanese BWR utilities have a plan to apply zinc injection to the primary coolant in order to reduce radioactivity accumulation on the structure. Prior to applying the zinc injection to BWR plants, it is necessary to evaluate the effect of zinc injection on corrosion resistance of fuel cladding. The objective of this report was to examine the accelerated corrosion condition for evaluation of BWR fuel cladding corrosion resistance under non-irradiated conditions, as the first step of a zinc injection evaluation study. A heat transfer corrosion test facility, in which a two phase flow condition could be achieved, was designed and constructed. The effects of heat flux, void fraction and solution temperature on BWR fuel cladding corrosion resistance were quantitatively investigated. The main findings were as follows. (1) In situ measurements using high speed camera and a void sensor together with one dimensional two phase flow analysis results showed that a two phase flow simulated BWR core condition can be obtained in the corrosion test facility. (2) The heat transfer corrosion test results showed that the thickness of the zirconium oxide layer increased with increasing solution temperature and was independent of heat flux and void fraction. The corrosion accelerating factor was about 2.5 times in the case of a temperature increase from 288degC to 350degC. (author)

  5. Corrosion studies on selected metallic materials for application in nuclear waste disposal containers

    International Nuclear Information System (INIS)

    Smailos, E.; Fiehn, B.; Gago, J.A.; Azkarate, I.

    1994-03-01

    In previous corrosion studies, carbon steels and the alloy Ti 99.8-Pd were identified as promising materials for heat-generating nuclear waste containers acting as a radionuclide barrier in a rock-salt repository. To characterize the long-term corrosion behaviour of these materials in more detail, a research programme including laboratory-scale and in-situ corrosion studies has been undertaken jointly by KfK and ENRESA/INASMET. In the period under review, gamma irradiation corrosion studies of up to about 6 months at 10 Gy/h and stress corrosion cracking studies at slow strain rates (10 -4 -10 -7 s -1 ) were performed on three preselected carbon steels in disposal relevant brines (NaCl-rich, MgCl 2 -rich) at 90 C and 150 C (TStE 355, TStE 460, 15 MnNi 6.3). Moreover, results were obtained from long-term in-situ corrosion studies (maximum test duration 9 years) conducted on carbon steel, Ti 99.8-Pd, Hastelloy C4, Ni-resist D4, and Si-cast iron in boreholes in the Asse salt mine. (orig./MM) [de

  6. Corrosion mechanism of copper in palm biodiesel

    International Nuclear Information System (INIS)

    Fazal, M.A.; Haseeb, A.S.M.A.; Masjuki, H.H.

    2013-01-01

    Highlights: ► Corrosion of copper in biodiesel increases with the increase of immersion time. ► The corrosion patina is found to be composed of CuO, Cu 2 O, CuCO 3 and Cu(OH) 2 . ► Green CuCO 3 was found as the major corrosion product. ► The mechanisms governing corrosion of copper in palm biodiesel are discussed. - Abstract: Biodiesel is a promising alternative fuel. However, it causes enhanced corrosion of automotive materials, especially of copper based components. In the present study, corrosion mechanism of copper was investigated by scanning electron microscope (SEM), energy dispersive spectroscopy (EDS), X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS). Compositional change of biodiesel due to the exposure of copper was also investigated. Corrosion patina on copper is found to be composed of Cu 2 O, CuO, Cu(OH) 2 and CuCO 3. Dissolved O 2 , H 2 O, CO 2 and RCOO − radical in biodiesel seem to be the leading factors in enhancing the corrosiveness of biodiesel.

  7. A simulation study of Linsley's approach to infer elongation rate and fluctuations of the EAS maximum depth from muon arrival time distributions

    International Nuclear Information System (INIS)

    Badea, A.F.; Brancus, I.M.; Rebel, H.; Haungs, A.; Oehlschlaeger, J.; Zazyan, M.

    1999-01-01

    The average depth of the maximum X m of the EAS (Extensive Air Shower) development depends on the energy E 0 and the mass of the primary particle, and its dependence from the energy is traditionally expressed by the so-called elongation rate D e defined as change in the average depth of the maximum per decade of E 0 i.e. D e = dX m /dlog 10 E 0 . Invoking the superposition model approximation i.e. assuming that a heavy primary (A) has the same shower elongation rate like a proton, but scaled with energies E 0 /A, one can write X m = X init + D e log 10 (E 0 /A). In 1977 an indirect approach studying D e has been suggested by Linsley. This approach can be applied to shower parameters which do not depend explicitly on the energy of the primary particle, but do depend on the depth of observation X and on the depth X m of shower maximum. The distribution of the EAS muon arrival times, measured at a certain observation level relatively to the arrival time of the shower core reflect the pathlength distribution of the muon travel from locus of production (near the axis) to the observation locus. The basic a priori assumption is that we can associate the mean value or median T of the time distribution to the height of the EAS maximum X m , and that we can express T = f(X,X m ). In order to derive from the energy variation of the arrival time quantities information about elongation rate, some knowledge is required about F i.e. F = - ∂ T/∂X m ) X /∂(T/∂X) X m , in addition to the variations with the depth of observation and the zenith-angle (θ) dependence, respectively. Thus ∂T/∂log 10 E 0 | X = - F·D e ·1/X v ·∂T/∂secθ| E 0 . In a similar way the fluctuations σ(X m ) of X m may be related to the fluctuations σ(T) of T i.e. σ(T) = - σ(X m )· F σ ·1/X v ·∂T/∂secθ| E 0 , with F σ being the corresponding scaling factor for the fluctuation of F. By simulations of the EAS development using the Monte Carlo code CORSIKA the energy and angle

  8. Corrosion Evaluation and Corrosion Control of Steam Generators

    Energy Technology Data Exchange (ETDEWEB)

    Maeng, W. Y.; Kim, U. C.; Sung, K. W.; Na, J. W.; Lee, Y. H.; Lee, D. H.; Kim, K. M

    2008-06-15

    Corrosion damage significantly influences the integrity and efficiency of steam generator. Corrosion problems of steam generator are unsolved issues until now even though much effort is made around world. Especially the stress corrosion cracking of heat exchange materials is the first issue to be solved. The corrosion protection method of steam generator is important and urgent for the guarantee of nuclear plant's integrity. The objectives of this study are 1) to evaluate the corrosion properties of steam generator materials, 2) to optimize the water chemistry of steam generator and 3) to develop the corrosion protection method of primary and secondary sides of steam generator. The results will be reflected to the water chemistry guideline for improving the integrity and efficiency of steam generator in domestic power plants.

  9. Corrosion cracking

    International Nuclear Information System (INIS)

    Goel, V.S.

    1985-01-01

    This book presents the papers given at a conference on alloy corrosion cracking. Topics considered at the conference included the effect of niobium addition on intergranular stress corrosion cracking, corrosion-fatigue cracking in fossil-fueled-boilers, fracture toughness, fracture modes, hydrogen-induced thresholds, electrochemical and hydrogen permeation studies, the effect of seawater on fatigue crack propagation of wells for offshore structures, the corrosion fatigue of carbon steels in seawater, and stress corrosion cracking and the mechanical strength of alloy 600

  10. Statistical characterization of pitting corrosion process and life prediction

    International Nuclear Information System (INIS)

    Sheikh, A.K.; Younas, M.

    1995-01-01

    In order to prevent corrosion failures of machines and structures, it is desirable to know in advance when the corrosion damage will take place, and appropriate measures are needed to mitigate the damage. The corrosion predictions are needed both at development as well as operational stage of machines and structures. There are several forms of corrosion process through which varying degrees of damage can occur. Under certain conditions these corrosion processes at alone and in other set of conditions, several of these processes may occur simultaneously. For a certain type of machine elements and structures, such as gears, bearing, tubes, pipelines, containers, storage tanks etc., are particularly prone to pitting corrosion which is an insidious form of corrosion. The corrosion predictions are usually based on experimental results obtained from test coupons and/or field experiences of similar machines or parts of a structure. Considerable scatter is observed in corrosion processes. The probabilities nature and kinetics of pitting process makes in necessary to use statistical method to forecast the residual life of machine of structures. The focus of this paper is to characterization pitting as a time-dependent random process, and using this characterization the prediction of life to reach a critical level of pitting damage can be made. Using several data sets from literature on pitting corrosion, the extreme value modeling of pitting corrosion process, the evolution of the extreme value distribution in time, and their relationship to the reliability of machines and structure are explained. (author)

  11. Effect of friction stir processing on erosion–corrosion behavior of nickel–aluminum bronze

    International Nuclear Information System (INIS)

    Lotfollahi, M.; Shamanian, M.; Saatchi, A.

    2014-01-01

    Highlights: • The average hardness value of the FSP samples was higher than cast sample. • Erosion–corrosion rate of the FSP samples was higher than cast sample. • The gravimetric analysis showed a negative synergy. - Abstract: In the present investigation, effects of Friction Stir Processing (FSP) on Erosion–Corrosion (E–C) behavior of Nickel–Aluminum Bronze (NAB) were studied by weight-loss measurements and surface characterization using an impingement jet test system. After FSP, the initial coarse microstructure of the cast NAB was transformed to a fine structure, and the porosity defects were eliminated. In addition, different FSP structures were produced by each rotation rate. Microhardness measurements showed a marked increase in FSP samples depending upon the FSP parameters. E–C tests were carried out by erodent at kinetic energies about 0.45 μJ and in 30°, 60° and 90° impact angles to simulate actual service conditions. The maximum weight-loss was observed in FSP samples and Scanning Electron Microscopy (SEM) results showed signs of brittle fracture mechanism in FSP samples. By gravimetric analysis, the degree of synergy was evaluated at 0.45 μJ kinetic energy at normal impact angle and negative synergy result implies the presence of a protective film on all sample surfaces

  12. Corrosion of carbon steel in clay environments relevant to radioactive waste geological disposals, Mont Terri rock laboratory (Switzerland)

    Energy Technology Data Exchange (ETDEWEB)

    Necib, S. [Agence Nationale pour la Gestion des Déchets Radioactifs ANDRA, Meuse Haute-Marne, Center RD 960, Bure (France); Diomidis, N. [National Cooperative for the Disposal of Radioactive Waste (NAGRA), Wettingen (Switzerland); Keech, P. [Nuclear Waste Management Organisation NWMO, Toronto (Canada); Nakayama, M. [Japan Atomic Energy Agency JAEA, Horonobe-Cho (Japan)

    2017-04-15

    Carbon steel is widely considered as a candidate material for the construction of spent fuel and high-level waste disposal canisters. In order to investigate corrosion processes representative of the long term evolution of deep geological repositories, two in situ experiments are being conducted in the Mont Terri rock laboratory. The iron corrosion (IC) experiment, aims to measure the evolution of the instantaneous corrosion rate of carbon steel in contact with Opalinus Clay as a function of time, by using electrochemical impedance spectroscopy measurements. The Iron Corrosion in Bentonite (IC-A) experiment intends to determine the evolution of the average corrosion rate of carbon steel in contact with bentonite of different densities, by using gravimetric and surface analysis measurements, post exposure. Both experiments investigate the effect of microbial activity on corrosion. In the IC experiment, carbon steel showed a gradual decrease of the corrosion rate over a period of 7 years, which is consistent with the ongoing formation of protective corrosion products. Corrosion product layers composed of magnetite, mackinawite, hydroxychloride and siderite with some traces of oxidising species such as goethite were identified on the steel surface. Microbial investigations revealed thermophilic bacteria (sulphate and thiosulphate reducing bacteria) at the metal surface in low concentrations. In the IC-A experiment, carbon steel samples in direct contact with bentonite exhibited corrosion rates in the range of 2 µm/year after 20 months of exposure, in agreement with measurements in absence of microbes. Microstructural and chemical characterisation of the samples identified a complex corrosion product consisting mainly of magnetite. Microbial investigations confirmed the limited viability of microbes in highly compacted bentonite. (authors)

  13. Investigation of the pitting corrosion of low carbon steel containers

    International Nuclear Information System (INIS)

    Mughabghab, S.F.; Sullivan, T.M.

    1988-01-01

    The present study was undertaken because the prediction of the degradation rate of low carbon steel contains over long time frames is one of the crucial elements in the development of a source term model for low-level shallow land burial. The principal data base considered is that of the NBS corrosion measurements of ferrous materials buried in the ground for periods of up to 18 years. In this investigation, the maximum penetration in mils, hm, due to pitting corrosion was found to conform closely to the relation h m = kt n where it is the exposure time of the sample in years, κ is the pitting parameter in mil/(years) n , and n > O is a parameter related to the aeration property of the soil. The central objective of the present investigation is the determination of the dependence of the pitting parameters κ and n on the soil properties. The result of a detailed linear correlation analysis of κ on one hand, the pH value and the resistivity of the soil on the other hand revealed that κ is principally influenced by the pH value of the soil. The resistivity of the soil is found to play a minor role

  14. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C

    Science.gov (United States)

    Lambrinou, Konstantina; Charalampopoulou, Evangelia; Van der Donck, Tom; Delville, Rémi; Schryvers, Dominique

    2017-07-01

    This work addresses the dissolution corrosion behaviour of 316L austenitic stainless steels. For this purpose, solution-annealed and cold-deformed 316L steels were simultaneously exposed to oxygen-poor (steels than the solution-annealed steel, indicating the importance of the steel thermomechanical state. The thickness of the dissolution-affected zone was non-uniform, and sites of locally-enhanced dissolution were occasionally observed. The progress of LBE dissolution attack was promoted by the interplay of certain steel microstructural features (grain boundaries, deformation twin laths, precipitates) with the dissolution corrosion process. The identified dissolution mechanisms were selective leaching leading to steel ferritization, and non-selective leaching; the latter was mainly observed in the solution-annealed steel. The maximum corrosion rate decreased with exposure time and was found to be inversely proportional to the depth of dissolution attack.

  15. Engineering Task Plan for Fourth Generation Hanford Corrosion Monitoring System

    International Nuclear Information System (INIS)

    NORMAN, E.C.

    2000-01-01

    This Engineering Task Plan (ETP) describes the activities associated with the installation of cabinets containing corrosion monitoring equipment on tanks 241-AN-102 and 241-AN-107. The new cabinets (one per tank) will be installed adjacent to existing corrosion probes already installed in riser WST-RISER-016 on both tanks. The corrosion monitoring equipment to be installed utilizes the technique of electrochemical noise (EN) for monitoring waste tank corrosion. Typically, EN consists of low frequency (4 Hz) and small amplitude signals that are spontaneously generated by electrochemical reactions occurring at corroding or other surfaces. EN analysis is well suited for monitoring and identifying the onset of localized corrosion, and for measuring uniform corrosion rates. A typical EN based corrosion-monitoring system measures instantaneous fluctuations in corrosion current and potential between three nominally identical electrodes of the material of interest immersed in the environment of interest. Time-dependent fluctuations in corrosion current are described by electrochemical current noise, and time-dependent fluctuations of corrosion potential are described by electrochemical noise. The corrosion monitoring systems are designed to detect the onset of localized corrosion phenomena if tank conditions should change to allow these phenomena to occur. In addition to the EN technique, the systems also facilitate the use of the Linear Polarization Resistance (LPR) technique to collect uniform corrosion rate information. LPR measures the linearity at the origin of the polarization curve for overvoltages up to a few millivolts away from the rest potential or natural corrosion potential. The slope of the current vs. voltage plot gives information on uniform corrosion rates

  16. Effect of Anodizing Time and Annealing Temperature on Photoelectrochemical Properties of Anodized TiO2 Nanotube for Corrosion Prevention Application

    Directory of Open Access Journals (Sweden)

    Misriyani Misriyani

    2017-07-01

    Full Text Available A study on the influence of anodizing time, annealing temperature and photoelectrochemical properties of TiO2 nanotube (TiO2 NT has been investigated. The crystallinity was investigated using X-Ray Diffraction and the anti-corrosion performance of stainless steel 304 (SS 304 coupled with TiO2 NT was evaluated using electrochemical techniques under ultraviolet exposure. The optimum anodizing condition occurs at a voltage of 20 V for 3 h. After anodizing, the TiO2 NT amorf was calcined at 500 °C to obtain anatase crystalline phase. For the photoelectrochemical property, the effects of pH and NaCl concentration on corrosion prevention have been examined. The result showed that the corrosion rate of stainless steel 304 coupled with TiO2 NT can be reduced up to 1.7 times compared to the uncoupled stainless steel 304 (3.05×10-6 to 1.78×10-6 mpy under ultraviolet exposure by shifted the photopotential to the more negative value (-0.302 V to -0.354 V at a pH of 8 and 3% NaCl concentration (-0.264 V to -0.291 V. In conclusion, the TiO2 NT films, which was prepared by anodization and followed by annealing can prevent the corrosion of stainless steel 304.

  17. Pipeline corrosion prevention by pH stabilization or corrosion inhibitors

    Energy Technology Data Exchange (ETDEWEB)

    Nyborg, Rolf [Institute for Energy Technology, Oslo (Norway)

    2009-07-01

    In many offshore oil and gas projects the pipeline costs are a considerable part of the investment and can become prohibitively high if the corrosivity of the fluid necessitates the use of corrosion resistant alloys instead of carbon steel. Development of more robust and reliable methods for internal corrosion control can increase the application range of carbon steel and therefore have a large economic impact. Corrosion control of carbon steel pipelines has traditionally often been managed by the use of corrosion inhibitors. The pH stabilization technique has been successfully used for corrosion control of several large wet gas pipelines in the last years. This method has advantages over film forming corrosion inhibitors when no or little formation water is produced. The use of corrosion inhibitors in multiphase pipelines implies several challenges which are not fully accounted for in traditional corrosion inhibitor testing procedures. Specialized test procedures have been developed to take account for the presence of emulsions dispersions and sand and clay particles in corrosion inhibitor testing. (author)

  18. Aqueous corrosion study on U-Zr alloy

    International Nuclear Information System (INIS)

    Pal, Titas; Venkatesan, V.; Kumar, Pradeep; Khan, K.B.; Kumar, Arun

    2009-01-01

    In low power or research reactor, U-Zr alloy is a potential candidate for dispersion fuel. Moreover, Zirconium has a low thermal-neutron cross section and uranium alloyed with Zr has excellent corrosion resistance and dimensional stability during thermal cycling. In the present study aqueous corrosion behavior of U-Zr alloy samples was studied in autoclave at 200 deg C temperature. Corrosion rate was determined from weight loss with time. (author)

  19. Corrosion of tungsten microelectrodes used in neural recording applications.

    Science.gov (United States)

    Patrick, Erin; Orazem, Mark E; Sanchez, Justin C; Nishida, Toshikazu

    2011-06-15

    In neuroprosthetic applications, long-term electrode viability is necessary for robust recording of the activity of neural populations used for generating communication and control signals. The corrosion of tungsten microwire electrodes used for intracortical recording applications was analyzed in a controlled bench-top study and compared to the corrosion of tungsten microwires used in an in vivo study. Two electrolytes were investigated for the bench-top electrochemical analysis: 0.9% phosphate buffered saline (PBS) and 0.9% PBS containing 30 mM of hydrogen peroxide. The oxidation and reduction reactions responsible for corrosion were found by measurement of the open circuit potential and analysis of Pourbaix diagrams. Dissolution of tungsten to form the tungstic ion was found to be the corrosion mechanism. The corrosion rate was estimated from the polarization resistance, which was extrapolated from the electrochemical impedance spectroscopy data. The results show that tungsten microwires in an electrolyte of PBS have a corrosion rate of 300-700 μm/yr. The corrosion rate for tungsten microwires in an electrolyte containing PBS and 30 mM H₂O₂ is accelerated to 10,000-20,000 μm/yr. The corrosion rate was found to be controlled by the concentration of the reacting species in the cathodic reaction (e.g. O₂ and H₂O₂). The in vivo corrosion rate, averaged over the duration of implantation, was estimated to be 100 μm/yr. The reduced in vivo corrosion rate as compared to the bench-top rate is attributed to decreased rate of oxygen diffusion caused by the presence of a biological film and a reduced concentration of available oxygen in the brain. Copyright © 2011 Elsevier B.V. All rights reserved.

  20. 77 FR 25141 - Corrosion-Resistant Carbon Steel Flat Products From Germany and South Korea: Extension of Time...

    Science.gov (United States)

    2012-04-27

    ...-Resistant Carbon Steel Flat Products From Germany and South Korea: Extension of Time Limits for Preliminary...) orders on corrosion-resistant carbon steel flat products (CORE) from Germany and South Korea (Korea... from Germany and South Korea: Adequacy Redetermination Memorandum,'' (April 20, 2012). The preliminary...

  1. Underground pipeline corrosion

    CERN Document Server

    Orazem, Mark

    2014-01-01

    Underground pipelines transporting liquid petroleum products and natural gas are critical components of civil infrastructure, making corrosion prevention an essential part of asset-protection strategy. Underground Pipeline Corrosion provides a basic understanding of the problems associated with corrosion detection and mitigation, and of the state of the art in corrosion prevention. The topics covered in part one include: basic principles for corrosion in underground pipelines, AC-induced corrosion of underground pipelines, significance of corrosion in onshore oil and gas pipelines, n

  2. Modelling the waterside corrosion of PWR fuel rods

    Energy Technology Data Exchange (ETDEWEB)

    Abram, T J [Fuel Engineering Dept., British Nuclear Fuels plc, Salwick, Preston (United Kingdom)

    1997-08-01

    The mechanism of zirconium alloy cladding corrosion in PWRs is briefly reviewed, and an engineering corrosion model is proposed. The basic model is intended to produce a best-estimate fit to circumferentially-average oxide thickness measurements obtained from inter-span positions, way from the effects of structural or flow mixing grids. The model comprises an initial pre-transition weight gain expression which follows cubic rate kinetics. On reaching a critical oxide thickness, a transition to linear rate kinetics occurs. The post-transition corrosion rate includes a term which is dependent on fast neutron flux, and an Arrhenius thermal corrosion rate which has been fitted to isothermal ex-reactor data. This thermal corrosion rate is enhanced by the presence of lithium in the coolant, and by the concentration of hydrogen in the cladding. Different cladding materials are accounted for in the selection of the model constants, and results for standard Zircaloy-4, low tin (or ``optimized``) Zircaloy-4, and the Westinghouse advanced alloy ZIRLO{sup TM} are presented. A method of accounting for the effects of grids is described, and the application of the model within the ENIGMA-B and ZROX codes is discussed. (author). 35 refs, 6 figs, 3 tabs.

  3. Marine corrosion of mild steel at Lumut, Perak

    Science.gov (United States)

    Ting, Ong Shiou; Potty, Narayanan Sambu; Liew, Mohd. Shahir

    2012-09-01

    The corrosion rate of structural steels in the adverse marine and offshore environments affects the economic interest of offshore structures since the loss of steel may have significant impact on structural safety and performance. With more emphasis to maintain existing structures in service for longer time and hence to defer replacement costs, there is increasing interest in predicting corrosion rate at a given location for a given period of exposure once the protection coating or cathodic protection is lost. The immersion depth, salinity, steel composition and water pollution will be taken into account. Various corrosion allowances are prescribed for structural members by different standards. There are no studies to determine the appropriate corrosion allowance for steel structures in marine environment in Malaysia. The objectives of the research are to determine the nature and rate of corrosion in mm/year for steel structures in marine environment. It also tries to identify whether the corrosion rate is affected by differences in the chemical composition of the steels, and microalgae. Two sets of corrosion coupons of Type 3 Steel consisting of mild steel were fabricated and immersed in seawater using steel frames. The corrosion rate of the coupon in mm/ per year is estimated based on the material weight loss with time in service. The results are compared with recommendations of the code.

  4. Statistical analysis of failure time in stress corrosion cracking of fuel tube in light water reactor

    International Nuclear Information System (INIS)

    Hirao, Keiichi; Yamane, Toshimi; Minamino, Yoritoshi

    1991-01-01

    This report is to show how the life due to stress corrosion cracking breakdown of fuel cladding tubes is evaluated by applying the statistical techniques to that examined by a few testing methods. The statistical distribution of the limiting values of constant load stress corrosion cracking life, the statistical analysis by making the probabilistic interpretation of constant load stress corrosion cracking life, and the statistical analysis of stress corrosion cracking life by the slow strain rate test (SSRT) method are described. (K.I.)

  5. The influence of time-variable cathodic corrosion protection on a.c. corrosion; Einfluss von zeitlich variierendem kathodischem Korrosionsschutz auf die Wechselstromkorrosion

    Energy Technology Data Exchange (ETDEWEB)

    Buechler, Markus; Voute, Carl-Heinz; Joos, David [SGK Schweizerische Gesellschaft fuer Korrosionsschutz, Zuerich (Switzerland)

    2011-07-01

    The current limiting values for corrosion of pipelines under a.c. current stress may be difficult to apply to pipelines, owing to the very heterogeneous bedding of the pipeline, poor jacket quality, or high short-term a.c. voltages. In principle, periodic alternation between very high and very low protective currents may optimize cathodic corrosion protection. This pulsed current strategy was found to be effective in laboratory tests if the operating parameters are set accurately.

  6. Research and development on is process components for hydrogen production. (2) Corrosion resistance of glass lining in high temperature sulfuric acid

    International Nuclear Information System (INIS)

    Tanaka, Nobuyuki; Iwatsuki, Jin; Kubo, Shinji; Terada, Atsuhiko; Onuki, Kaoru

    2009-01-01

    Japan Atomic Energy Agency has been conducting a research and development on hydrogen production system using High Temperature Gas-Cooled Reactor. As a part of this effort, thermochemical water-splitting cycle featuring iodine- and sulfur-compounds (IS process) is under development considering its potential of large-scale economical hydrogen production. The IS process constitutes very severe environments on the materials of construction because of the corrosive nature of process chemicals, especially of the high temperature acidic solution of sulfuric acid and hydriodic acid dissolving iodine. Therefore, selection of the corrosion-resistant materials and development of the components has been studied as a crucial subject of the process development. This paper discusses corrosion resistance of commercially available glass-lining material in high temperature sulfuric acid. Corrosion resistance of a soda glass used for glass-lining was examined by immersion tests. The experiments were performed in 47-90wt% sulfuric acids at temperatures of up to 400degC and for the maximum immersion time of 100 hours using an autoclave designed for the concerned tests. In every condition tested, no indication of localized corrosion such as defect formation or pitting corrosion was observed. Also, the corrosion rates decreased with the progress of immersion, and were low enough (≅0.1 mm/year) after 60-90 hours of immersion probably due to formation of a silica rich surface. (author)

  7. Galvanic Corrosion of Lead by Iron (Oxyhydr)Oxides: Potential Impacts on Drinking Water Quality.

    Science.gov (United States)

    Trueman, Benjamin F; Sweet, Gregory A; Harding, Matthew D; Estabrook, Hayden; Bishop, D Paul; Gagnon, Graham A

    2017-06-20

    Lead exposure via drinking water remains a significant public health risk; this study explored the potential effects of upstream iron corrosion on lead mobility in water distribution systems. Specifically, galvanic corrosion of lead by iron (oxyhydr)oxides was investigated. Coupling an iron mineral cathode with metallic lead in a galvanic cell increased lead release by 531 μg L -1 on average-a 9-fold increase over uniform corrosion in the absence of iron. Cathodes were composed of spark plasma sintered Fe 3 O 4 or α-Fe 2 O 3 or field-extracted Fe 3 O 4 and α-FeOOH. Orthophosphate immobilized oxidized lead as insoluble hydroxypyromorphite, while humic acid enhanced lead mobility. Addition of a humic isolate increased lead release due to uniform corrosion by 81 μg L -1 and-upon coupling lead to a mineral cathode-release due to galvanic corrosion by 990 μg L -1 . Elevated lead in the presence of humic acid appeared to be driven by complexation, with 208 Pb and UV 254 size-exclusion chromatograms exhibiting strong correlation under these conditions (R 2 average = 0.87). A significant iron corrosion effect was consistent with field data: lead levels after lead service line replacement were greater by factors of 2.3-4.7 at sites supplied by unlined cast iron distribution mains compared with the alternative, lined ductile iron.

  8. Simulation of Corrosion Process for Structure with the Cellular Automata Method

    Science.gov (United States)

    Chen, M. C.; Wen, Q. Q.

    2017-06-01

    In this paper, from the mesoscopic point of view, under the assumption of metal corrosion damage evolution being a diffusive process, the cellular automata (CA) method was proposed to simulate numerically the uniform corrosion damage evolution of outer steel tube of concrete filled steel tubular columns subjected to corrosive environment, and the effects of corrosive agent concentration, dissolution probability and elapsed etching time on the corrosion damage evolution were also investigated. It was shown that corrosion damage increases nonlinearly with increasing elapsed etching time, and the longer the etching time, the more serious the corrosion damage; different concentration of corrosive agents had different impacts on the corrosion damage degree of the outer steel tube, but the difference between the impacts was very small; the heavier the concentration, the more serious the influence. The greater the dissolution probability, the more serious the corrosion damage of the outer steel tube, but with the increase of dissolution probability, the difference between its impacts on the corrosion damage became smaller and smaller. To validate present method, corrosion damage measurements for concrete filled square steel tubular columns (CFSSTCs) sealed at both their ends and immersed fully in a simulating acid rain solution were conducted, and Faraday’s law was used to predict their theoretical values. Meanwhile, the proposed CA mode was applied for the simulation of corrosion damage evolution of the CFSSTCs. It was shown by the comparisons of results from the three methods aforementioned that they were in good agreement, implying that the proposed method used for the simulation of corrosion damage evolution of concrete filled steel tubular columns is feasible and effective. It will open a new approach to study and evaluate further the corrosion damage, loading capacity and lifetime prediction of concrete filled steel tubular structures.

  9. Corrosion analysis in mooring chain links; Analise de corrosao em elos de amarras

    Energy Technology Data Exchange (ETDEWEB)

    Leal, Silvia N.; Pereira, Marcos V. [Pontificia Univ. Catolica do Rio de Janeiro, RJ (Brazil). Dept. de Ciencia dos Materiais e Metalurgia; Costa, Luis C. [PETROBRAS S.A., Rio de Janeiro, RJ (Brazil). Centro de Pesquisas; Motta, Sergio H. [Brasilamarras - Companhia Brasileira de Amarras, Niteroi, RJ (Brazil)

    2004-07-01

    The purpose of this work was to characterize the localized corrosion phenomenon in the weld region of offshore mooring chain links type ORQ. In this sense, a number of chain links were selected after finishing their projected life time without corrosion signs (chains without corrosion) as well as chain links which showed a reduced life time caused by localized corrosion (chains with corrosion). In the sequence, electrochemistry tests evaluated the corrosion susceptibility of the different regions of the weld joint. The results showed that the heat affected zone concerning the chains with corrosion was the anodic region, with high corrosion rate, while the same region on the not corroded chains was the cathodic one, with low corrosion rate. (author)

  10. Corrosion assessment of dry fuel storage containers

    Energy Technology Data Exchange (ETDEWEB)

    Graves, C.E.

    1994-09-01

    The structural stability as a function of expected corrosion degradation of 75 dry fuel storage containers located in the 200 Area Low-Level Waste Burial Grounds was evaluated. These containers include 22 concrete burial containers, 13 55-gal (208-l) drums, and 40 Experimental Breeder Reactor II (EBR-II) transport/storage casks. All containers are buried beneath at least 48 in. of soil and a heavy plastic tarp with the exception of 35 of the EBR-II casks which are exposed to atmosphere. A literature review revealed that little general corrosion is expected and pitting corrosion of the carbon steel used as the exterior shell for all containers (with the exception of the concrete containers) will occur at a maximum rate of 3.5 mil/yr. Penetration from pitting of the exterior shell of the 208-l drums and EBR-II casks is calculated to occur after 18 and 71 years of burial, respectively. The internal construction beneath the shell would be expected to preclude containment breach, however, for the drums and casks. The estimates for structural failure of the external shells, large-scale shell deterioration due to corrosion, are considerably longer, 39 and 150 years respectively for the drums and casks. The concrete burial containers are expected to withstand a service life of 50 years.

  11. Injection of nano-particles in mitigating flow accelerated corrosion (FAC) damage in the secondary system of nuclear power plants (NPPs)

    International Nuclear Information System (INIS)

    Lim, Dong Seok; Ku, Hee Kwon; Cho, Jae Seon

    2015-01-01

    NPPs produces electric energy through phase transition of water. According to this, a piping, which is flow path, integrity is essential for safety functions. Erosion, FAC and fittings are corrosion failure mechanism by increasing service life. Especially, there are 10-kilometers of piping in secondary systems. It needs to estimate FAC and apply periodic management. Iron oxides produced by FAC cause power reduction and Loss Of Coolant Accident (LOCA) will be occurred through the continued piping wall thinning. In this study, corrosion rate of pipe materials with carbon steel(SA106.Gr.B) and low-alloy steel (SA335.P22) was evaluated for pipe configuration and dissolved oxygen concentration on 150 °C, pH 9.5∼10.0 and flow velocity of 5m/s. Temperature of 150°C is well known that causes high FAC rate and pH consider a NPPs in-service condition. Further corrosion rate test was performed to develop FAC reduction technology through Pt-nanoparticle injection. In this study, corrosion rate is evaluated by weight depletion method. The results of material impact assessment show that corrosion rate of carbon steel is more higher than that of low-alloy steel because of Cr content. And also, the results of pipe configuration test show that case with 90° elbow had maximum wall thinning than with 180° horizontal pipe. The dissolved oxygen concentration test shows that low oxygen condition, ≤5 ppb, had high corrosion rate compared to normal condition and the corrosion rate decreased 50% at Pt-nanoparticle injection test on maximum corrosion rate condition compared to maximum wall thinning condition without Pt-nanoparticle injection. In this study, samples provided by each test case had analyzed through SEM-EDX (Scanning Electron Microscopy-Energy Dispersive X-ray Spectroscopy). Behavior evaluation for oxide film was performed and Electrochemical corrosion potential (ECP) was measured for electrochemistry evaluation. To apply Pt-nanoparticle injection technology on nuclear

  12. Monitoring corrosion rates and localised corrosion in low conductivity water

    DEFF Research Database (Denmark)

    Hilbert, Lisbeth Rischel

    2006-01-01

    Monitoring of low corrosion rates and localised corrosion in a media with low conductivity is a challenge. In municipal district heating, quality control may be improved by implementing on-line corrosion monitoring if a suitable technique can be identified to measure both uniform and localised...... corrosion. Electrochemical techniques (LPR, EIS, crevice corrosion current) as well as direct measurement techniques (high-sensitive electrical resistance, weight loss) have been applied in operating plants. Changes in the corrosion processes are best monitored in non-aggressive, low conductivity media...

  13. Modeling pore corrosion in normally open gold- plated copper connectors.

    Energy Technology Data Exchange (ETDEWEB)

    Battaile, Corbett Chandler; Moffat, Harry K.; Sun, Amy Cha-Tien; Enos, David George; Serna, Lysle M.; Sorensen, Neil Robert

    2008-09-01

    The goal of this study is to model the electrical response of gold plated copper electrical contacts exposed to a mixed flowing gas stream consisting of air containing 10 ppb H{sub 2}S at 30 C and a relative humidity of 70%. This environment accelerates the attack normally observed in a light industrial environment (essentially a simplified version of the Battelle Class 2 environment). Corrosion rates were quantified by measuring the corrosion site density, size distribution, and the macroscopic electrical resistance of the aged surface as a function of exposure time. A pore corrosion numerical model was used to predict both the growth of copper sulfide corrosion product which blooms through defects in the gold layer and the resulting electrical contact resistance of the aged surface. Assumptions about the distribution of defects in the noble metal plating and the mechanism for how corrosion blooms affect electrical contact resistance were needed to complete the numerical model. Comparisons are made to the experimentally observed number density of corrosion sites, the size distribution of corrosion product blooms, and the cumulative probability distribution of the electrical contact resistance. Experimentally, the bloom site density increases as a function of time, whereas the bloom size distribution remains relatively independent of time. These two effects are included in the numerical model by adding a corrosion initiation probability proportional to the surface area along with a probability for bloom-growth extinction proportional to the corrosion product bloom volume. The cumulative probability distribution of electrical resistance becomes skewed as exposure time increases. While the electrical contact resistance increases as a function of time for a fraction of the bloom population, the median value remains relatively unchanged. In order to model this behavior, the resistance calculated for large blooms has been weighted more heavily.

  14. Corrosion chemistry closing comments: opportunities in corrosion science facilitated by operando experimental characterization combined with multi-scale computational modelling.

    Science.gov (United States)

    Scully, John R

    2015-01-01

    Recent advances in characterization tools, computational capabilities, and theories have created opportunities for advancement in understanding of solid-fluid interfaces at the nanoscale in corroding metallic systems. The Faraday Discussion on Corrosion Chemistry in 2015 highlighted some of the current needs, gaps and opportunities in corrosion science. Themes were organized into several hierarchical categories that provide an organizational framework for corrosion. Opportunities to develop fundamental physical and chemical data which will enable further progress in thermodynamic and kinetic modelling of corrosion were discussed. These will enable new and better understanding of unit processes that govern corrosion at the nanoscale. Additional topics discussed included scales, films and oxides, fluid-surface and molecular-surface interactions, selected topics in corrosion science and engineering as well as corrosion control. Corrosion science and engineering topics included complex alloy dissolution, local corrosion, and modelling of specific corrosion processes that are made up of collections of temporally and spatially varying unit processes such as oxidation, ion transport, and competitive adsorption. Corrosion control and mitigation topics covered some new insights on coatings and inhibitors. Further advances in operando or in situ experimental characterization strategies at the nanoscale combined with computational modelling will enhance progress in the field, especially if coupling across length and time scales can be achieved incorporating the various phenomena encountered in corrosion. Readers are encouraged to not only to use this ad hoc organizational scheme to guide their immersion into the current opportunities in corrosion chemistry, but also to find value in the information presented in their own ways.

  15. On the detection of corrosion pit interactions using two-dimensional spectral analysis

    International Nuclear Information System (INIS)

    Jarrah, Adil; Nianga, Jean-Marie; Iost, Alain; Guillemot, Gildas; Najjar, Denis

    2010-01-01

    A statistical methodology for detecting pits interactions based on a two-dimensional spectral analysis is presented. This method can be used as a tool for the exploratory analysis of spatial point patterns and can be advanced as an alternative of classical methods based on distance. One of the major advantages of the spectral analysis approach over the use of classical methods is its ability to reveal more details about the spatial structure like the scale for which pits corrosion can be considered as independent. Furthermore, directional components of pattern can be investigated. The method is validated in a first time using numerical simulations on random, regular and aggregated structures. The density of pits, used in the numerical simulations, corresponds to that assessed from a corroded aluminium sheet. In a second time, this method is applied to verify the independence of the corrosion pits observed on the aforementioned aluminium sheet before applying the Gumbel theory to determine the maximum pit depth. Indeed, the property of independence is a prerequisite of the Gumbel theory which is one of the most frequently used in the field of safety and reliability.

  16. Comparative study on structure, corrosion and hardness of Zn-Ni alloy deposition on AISI 347 steel aircraft material

    Energy Technology Data Exchange (ETDEWEB)

    Gnanamuthu, RM. [Department of Chemical Engineering, College of Engineering, Kyung Hee University, 1732 Deogyeong-daero, Gihung, Yongin, Gyeonggi 446-701 (Korea, Republic of); Mohan, S., E-mail: sanjnamohan@yahoo.com [Central Electrochemical Research Institute, (CSIR), Karaikudi 630 006, Tamilnadu (India); Saravanan, G. [Central Electrochemical Research Institute, (CSIR), Karaikudi 630 006, Tamilnadu (India); Lee, Chang Woo, E-mail: cwlee@khu.ac.kr [Department of Chemical Engineering, College of Engineering, Kyung Hee University, 1732 Deogyeong-daero, Gihung, Yongin, Gyeonggi 446-701 (Korea, Republic of)

    2012-02-05

    Highlights: Black-Right-Pointing-Pointer Electrodeposition of Zn-Ni alloy on AISI 347 steel as an aircraft material has been carried out from various baths. Black-Right-Pointing-Pointer The effect of pulse duty cycle on thickness, current efficiency and hardness reached maximum values at 40% duty cycle and for 50 Hz frequencies average current density of 4 A dm{sup -2}. Black-Right-Pointing-Pointer The XRF characterizations of 88:12% Zn-Ni alloy provided excellent corrosion resistance. Black-Right-Pointing-Pointer It is found that Zn-Ni alloy on AISI 347 aircraft material has better structure and corrosion resistance by pulse electrodeposits from electrolyte-4. - Abstract: Zn-Ni alloys were electrodeposited on AISI 347 steel aircraft materials from various electrolytes under direct current (DCD) and pulsed electrodepositing (PED) techniques. The effects of pulse duty cycle on thickness, current efficiency and hardness of electrodeposits were studied. Alloy phases of the Zn-Ni were indexed by X-ray diffraction (XRD) techniques. Microstructural morphology, topography and elemental compositions were characterized using scanning electron microscopy (SEM), atomic force microscopy (AFM) and X-ray fluorescence spectroscopy (XRF). The corrosion resistance properties of electrodeposited Zn-Ni alloy in 3.5% NaCl aqueous solution obtained by DCD and PED were compared using potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) technique. Elemental analysis showed that 88% of Zn and 12% of Ni obtained from electrolyte-4 by PED technique at 40% duty cycle for 50 Hz frequencies having better corrosion resistance than that of deposits obtained from other electrolytes.

  17. Status of Database for Electrochemical Noise Based Corrosion Monitoring

    International Nuclear Information System (INIS)

    EDGEMON, G.L.

    1999-01-01

    Underground storage tanks made of mild steel are used to contain radioactive waste generated by plutonium production at the Hanford Site. Corrosion of the walls of these tanks is a major issue. Corrosion-related failure of waste tank walls could lead to the leakage of radioactive contaminants to the soil and groundwater. It is essential to monitor corrosion conditions of the tank walls to determine tank integrity and ensure safe waste storage until retrieval and final waste disposal can be accomplished. Corrosion monitoring/control is currently provided at the Hanford Site through a waste chemistry sampling and analysis program. In this process, tank waste is sampled, analyzed and compared to a selection of laboratory exposures of coupons in simulated waste. Tank wall corrosion is inferred by matching measured tank chemistries to the results of the laboratory simulant testing. This method is expensive, time consuming, and does not yield real-time data. A project to improve the Hanford Site's corrosion monitoring strategy was started in 1995

  18. Cracking and corrosion recovery boiler

    Energy Technology Data Exchange (ETDEWEB)

    Suik, H [Tallinn Technical University, Horizon Pulp and Paper, Tallinn (Estonia)

    1999-12-31

    The corrosion of heat surfaces and the cracking the drums are the main problems of the recovery boiler. These phenomena have been appeared during long-term operation of boiler `Mitsubishi - 315` erected at 1964. Depth of the crack is depending on the number of shutdowns and on operation time. Corrosion intensity of different heat surfaces is varying depend on the metal temperature and the conditions at place of positioning of tube. The lowest intensity of corrosion is on the bank tubes and the greatest is on the tubes of the second stage superheater and on the tubes at the openings of air ports. (orig.) 5 refs.

  19. Cracking and corrosion recovery boiler

    Energy Technology Data Exchange (ETDEWEB)

    Suik, H. [Tallinn Technical University, Horizon Pulp and Paper, Tallinn (Estonia)

    1998-12-31

    The corrosion of heat surfaces and the cracking the drums are the main problems of the recovery boiler. These phenomena have been appeared during long-term operation of boiler `Mitsubishi - 315` erected at 1964. Depth of the crack is depending on the number of shutdowns and on operation time. Corrosion intensity of different heat surfaces is varying depend on the metal temperature and the conditions at place of positioning of tube. The lowest intensity of corrosion is on the bank tubes and the greatest is on the tubes of the second stage superheater and on the tubes at the openings of air ports. (orig.) 5 refs.

  20. Corrosion of steel tanks in liquid nuclear wastes

    International Nuclear Information System (INIS)

    Carranza, Ricardo M.; Giordano, Celia M.; Saenz, Eduardo

    2005-01-01

    The objective of this work is to understand how solution chemistry would impact on the corrosion of waste storage steel tanks at the Hanford Site. Future tank waste operations are expected to process wastes that are more dilute with respect to some current corrosion inhibiting waste constituents. Assessment of corrosion damage and of the influence of exposure time and electrolyte composition, using simulated (non-radioactive) wastes, of the double-shell tank wall carbon steel alloys is being conducted in a statistically designed long-term immersion experiment. Corrosion rates at different times of immersion were determined using both weight-loss determinations and electrochemical impedance spectroscopy measurements. Localized corrosion susceptibility was assessed using short-term cyclic potentiodynamic polarization curves. The results presented in this paper correspond to electrochemical and weight-loss measurements of the immersed coupons during the first year of immersion from a two year immersion plan. A good correlation was obtained between electrochemical measurements, weight-loss determinations and visual observations. Very low general corrosion rates ( -1 ) were estimated using EIS measurements, indicating that general corrosion rate of the steel in contact with liquid wastes would no be a cause of tank failure even for these out-of-chemistry limit wastes. (author) [es

  1. The effect of discontinuities on the corrosion behaviour of copper canisters

    International Nuclear Information System (INIS)

    King, F.

    2004-03-01

    Discontinuities may remain in the weld region of copper canisters following the final closure welding and inspection procedures. Although the shell of the copper canister is expected to exhibit excellent corrosion properties in the repository environment, the question remains what impact these discontinuities might have on the long-term performance and service life of the canister. A review of the relevant corrosion literature has been carried out and an expert opinion of the impact of these discontinuities on the canister lifetime has been developed. Since the amount of oxidant in the repository is limited and the maximum wall penetration is expected to be 2 O/Cu(OH) 2 film at a critical electrochemical potential determines where and when pits initiate, not the presence of pit-shaped surface discontinuities. The factors controlling pit growth and death are well understood. There is evidence for a maximum pit radius for copper in chloride solutions, above which the small anodic: cathodic surface area ratio required for the formation of deep pits cannot be sustained. This maximum pit radius is of the order of 0.1-0.5 mm. Surface discontinuities larger than this size are unlikely to propagate as pits, and pits generated from smaller discontinuities will die once they reach this maximum size. Death of propagating pits will be compounded by the decrease in oxygen flux to the canister as the repository environment becomes anoxic. Surface discontinuities could impact the SCC behaviour either through their effect on the local environment or via stress concentration or intensification. There is no evidence that surface discontinuities will affect the initiation of SCC by ennoblement of the corrosion potential or the formation of locally aggressive conditions. Stress concentration at pits could lead to crack initiation under some circumstances, but the stress intensity factor for the resultant cracks, or for pre-existing crack-like discontinuities, will be smaller than the

  2. Pitting corrosion of copper. An equilibrium - mass transport study

    Energy Technology Data Exchange (ETDEWEB)

    Taxen, C

    1996-11-01

    A mathematical model for the propagation of corrosion pits on copper is described. The model is used to predict the potentials below which copper is immune to pitting. The criteria used for immunity against pitting is that the volume of the cuprous oxide formed at the site of the metal oxidation at the bottom of a corrosion pit must be smaller than the volume of the oxidised metal. Equal volumes would give a complete coverage of the metal in a pit by adherent cuprous oxide and propagation would not be possible. For potentials where copper is not immune to pitting an estimate of the maximum growth rate is given. The model uses equilibrium data and diffusion coefficients and calculates the stationary concentration profiles from the bulk water outside a corrosion pit to the site of the metal dissolution at the bottom a corrosion pit. Precipitation of oxides as well as of basic salts of copper is considered. A total of 26 aqueous species are considered in waters with compositions ranging from those of tap waters to that of sea water. Calculations are made for the temperatures 25 deg C and 75 deg C. 38 refs, 60 figs, 17 tabs

  3. Radionuclide decay effects on waste glass corrosion and weathering

    International Nuclear Information System (INIS)

    Wronkiewicz, D.J.

    1993-01-01

    The release of glass components into solution, including radionuclides, may be influenced by the presence of radiolytically produced nitric acid, carboxylic acid, and transient water dissociation products such as ·OH and O 2 - . Under batch test conditions, glass corrosion has been shown to increase up to a maximum of three-to five-fold in irradiated tests relative to nonirradiated tests, while in other studies the presence of radiolytic products has actually decreased glass corrosion rates. Bicarbonate groundwaters will buffer against pH decreases and changes in corrosion rates. Under high surface area-to-solution volume (S/V) conditions, the bicarbonate buffering reservoir may be quickly overwhelmed by radiolytic acids that are concentrated in the thin films of water contacting the samples. Glass reaction rates have been shown to increase up to 10-to-15-fold due to radiation exposure under high S/V conditions. Radiation damage to solid glass materials results in bond damage and atomic displacements. This type of damage has been shown to increase the release rates of glass components up to four-fold during subsequent corrosion tests, although under actual disposal conditions, glass annealing processes may negate the solid radiation damage effects

  4. Effect of pulse current parameters on the mechanical and corrosion properties of anodized nanoporous aluminum coatings

    Energy Technology Data Exchange (ETDEWEB)

    Mohammadi, Iman, E-mail: imanmohammadi68@gmail.com; Ahmadi, Shahab; Afshar, Abdollah

    2016-11-01

    In this study, the effects of pulse current parameters on corrosion resistance and mechanical properties of anodized coatings were evaluated. Hardness measurements, polarization and electrochemical impedance spectroscopy tests were employed to investigate the mechanical properties and corrosion behavior of these coatings. Also, field emission scanning electron microscopy (FE-SEM) was used to analyze the surface morphology and microstructure of the coatings. It was found that the properties of anodized coatings were dependent on various parameters, among which, time, temperature and pulse current parameters (current density limit, frequency and duty cycle) were optimized. Analysis of Variance (ANOVA) was conducted in order to optimize the results of designed experiments for predicting the hardness of anodic Al{sub 2}O{sub 3} coatings. Experimental results showed that the temperature and the interaction of quadratic behavior of minimum current density with frequency and duty cycle were the most important factors influencing the hardness of these coatings. It was indicated that the highest hardness value of 642 HV was attained at the maximum and minimum current densities of 4.4, 1.27 A/dm{sup 2}, respectively, a frequency of 82 Hz, procedure time of 27.2 min, duty cycle of 80.2% and the bath temperature of 13.5 °C. In addition, the FE-SEM micrographs showed that the highest density is obtained through the mentioned optimum conditions. Moreover, the electrochemical tests revealed that the highest polarization resistance obtained at optimum conditions was more than 20 times greater than the other samples. - Highlights: • Electrolyte temperature undesirably influences the hardness of anodized coatings. • Maximum hardness of coatings was evaluated by optimization of effective parameters. • The diameter of alumina nanotube considerably affects hardness of anodized coating. • R{sub P} of the sample formed at optimum condition was at least 20 times more than others

  5. Effect of pulse current parameters on the mechanical and corrosion properties of anodized nanoporous aluminum coatings

    International Nuclear Information System (INIS)

    Mohammadi, Iman; Ahmadi, Shahab; Afshar, Abdollah

    2016-01-01

    In this study, the effects of pulse current parameters on corrosion resistance and mechanical properties of anodized coatings were evaluated. Hardness measurements, polarization and electrochemical impedance spectroscopy tests were employed to investigate the mechanical properties and corrosion behavior of these coatings. Also, field emission scanning electron microscopy (FE-SEM) was used to analyze the surface morphology and microstructure of the coatings. It was found that the properties of anodized coatings were dependent on various parameters, among which, time, temperature and pulse current parameters (current density limit, frequency and duty cycle) were optimized. Analysis of Variance (ANOVA) was conducted in order to optimize the results of designed experiments for predicting the hardness of anodic Al_2O_3 coatings. Experimental results showed that the temperature and the interaction of quadratic behavior of minimum current density with frequency and duty cycle were the most important factors influencing the hardness of these coatings. It was indicated that the highest hardness value of 642 HV was attained at the maximum and minimum current densities of 4.4, 1.27 A/dm"2, respectively, a frequency of 82 Hz, procedure time of 27.2 min, duty cycle of 80.2% and the bath temperature of 13.5 °C. In addition, the FE-SEM micrographs showed that the highest density is obtained through the mentioned optimum conditions. Moreover, the electrochemical tests revealed that the highest polarization resistance obtained at optimum conditions was more than 20 times greater than the other samples. - Highlights: • Electrolyte temperature undesirably influences the hardness of anodized coatings. • Maximum hardness of coatings was evaluated by optimization of effective parameters. • The diameter of alumina nanotube considerably affects hardness of anodized coating. • R_P of the sample formed at optimum condition was at least 20 times more than others. • Porosity is the

  6. FY2005 AND FY2006 CORROSION SURVEILLANCE RESULTS FOR L BASIN

    International Nuclear Information System (INIS)

    Vormelker, P.; Cynthia Foreman, C.

    2008-01-01

    This report documents the results of the L-Basin Corrosion Surveillance Program for the fiscal years 2005 and 2006. The water quality and basin conditions for the coupon immersion period are compared to the corrosion evaluation results from detailed metallurgical analysis of the coupons. Test coupons were removed from the basin on two occasions, March 29, 2005 and May 23, 2006, examined and photographed. Selected coupons were metallurgically characterized to evaluate the extent of general corrosion and pitting. Crystallographic and energy dispersive spectroscopy analysis were performed on a typical specimen, as-removed from the basin, to characterize the surface debris. Marked changes were noted in both the 2005 and 2006 specimens compared to previous years corrosion results. A new pitting incidence has occurred on the faces of the aluminum coupons compared to localized pitting at crevice regions only on specimens withdrawn in 2003 and 2004. The pitting incidence is attributed to sand filter fines that entered the basin on July 27, 2004 from an inadvertent backflush of the new sand filter. Pitting rate results show a trend of slowing down over time which is consistent with aluminum pit kinetics. Average pit growth rates were equal to or lower in all 2006 aluminum coupons than those removed in 2005. A trend line shows that pitting corrosion rates on Al1100, 6061, and 6063 coupons are slowing down since pit depth measurements were initiated in 2003. No impact to stored spent fuel is expected from the debris. The storage configuration of the majority of L-Basin spent fuel, in bundles, should provide a measure of isolation from debris settling in the basin

  7. A strain-mediated corrosion model for bioabsorbable metallic stents.

    Science.gov (United States)

    Galvin, E; O'Brien, D; Cummins, C; Mac Donald, B J; Lally, C

    2017-06-01

    This paper presents a strain-mediated phenomenological corrosion model, based on the discrete finite element modelling method which was developed for use with the ANSYS Implicit finite element code. The corrosion model was calibrated from experimental data and used to simulate the corrosion performance of a WE43 magnesium alloy stent. The model was found to be capable of predicting the experimentally observed plastic strain-mediated mass loss profile. The non-linear plastic strain model, extrapolated from the experimental data, was also found to adequately capture the corrosion-induced reduction in the radial stiffness of the stent over time. The model developed will help direct future design efforts towards the minimisation of plastic strain during device manufacture, deployment and in-service, in order to reduce corrosion rates and prolong the mechanical integrity of magnesium devices. The need for corrosion models that explore the interaction of strain with corrosion damage has been recognised as one of the current challenges in degradable material modelling (Gastaldi et al., 2011). A finite element based plastic strain-mediated phenomenological corrosion model was developed in this work and was calibrated based on the results of the corrosion experiments. It was found to be capable of predicting the experimentally observed plastic strain-mediated mass loss profile and the corrosion-induced reduction in the radial stiffness of the stent over time. To the author's knowledge, the results presented here represent the first experimental calibration of a plastic strain-mediated corrosion model of a corroding magnesium stent. Copyright © 2017 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

  8. Average chewing pattern improvements following Disclusion Time reduction.

    Science.gov (United States)

    Kerstein, Robert B; Radke, John

    2017-05-01

    Studies involving electrognathographic (EGN) recordings of chewing improvements obtained following occlusal adjustment therapy are rare, as most studies lack 'chewing' within the research. The objectives of this study were to determine if reducing long Disclusion Time to short Disclusion Time with the immediate complete anterior guidance development (ICAGD) coronoplasty in symptomatic subjects altered their average chewing pattern (ACP) and their muscle function. Twenty-nine muscularly symptomatic subjects underwent simultaneous EMG and EGN recordings of right and left gum chewing, before and after the ICAGD coronoplasty. Statistical differences in the mean Disclusion Time, the mean muscle contraction cycle, and the mean ACP resultant from ICAGD underwent the Student's paired t-test (α = 0.05). Disclusion Time reductions from ICAGD were significant (2.11-0.45 s. p = 0.0000). Post-ICAGD muscle changes were significant in the mean area (p = 0.000001), the peak amplitude (p = 0.00005), the time to peak contraction (p chewing position became closer to centric occlusion (p chewing velocities increased (p chewing pattern (ACP) shape, speed, consistency, muscular coordination, and vertical opening improvements can be significantly improved in muscularly dysfunctional TMD patients within one week's time of undergoing the ICAGD enameloplasty. Computer-measured and guided occlusal adjustments quickly and physiologically improved chewing, without requiring the patients to wear pre- or post-treatment appliances.

  9. Review of corrosion causes and corrosion control in a technical facility

    International Nuclear Information System (INIS)

    Charng, T.; Lansing, F.

    1982-06-01

    Causes of corrosion of metals and their alloys are reviewed. The corrosion mechanism is explained by electrochemical reaction theory. The causes and methods of controlling of both physiochemical corrosion and biological corrosion are presented. Factors which influence the rate of corrosion are also discussed

  10. Degradation of normal portland and slag cement concrete under load, due to reinforcement corrosion

    International Nuclear Information System (INIS)

    Philipose, K.E.; Beaudoin, J.J.; Feldman, R.F.

    1992-08-01

    The corrosion of reinforcement is one of the major degradation mechanisms of reinforced concrete elements. The majority of studies published on concrete-steel corrosion have been conducted on unstressed specimens. Structural concrete, however, is subjected to substantial strain near the steel reinforcing bars that resist tensile loads, which results in a system of microcracks. This report presents the initial results of an investigation to determine the effect of applied load and microcracking on the rate of ingress of chloride ion and corrosion of steel in concrete. Simply-supported concrete beam specimens were loaded to give a maximum strain of about 600 με on the tension face. Chloride ion ingress on cores taken from loaded specimens was monitored using energy-dispersive X-ray analysis techniques. Corrosion current and rate measurements using linear polarization electrochemical techniques were also obtained on the same loaded specimens. Variables investigated included two concrete types, two steel cover-depths, three applied load levels, bonded and unbonded rebars and the exposure of tension and compression beam faces to chloride solution. One concrete mixture was made with type 10 Portland cement, the other with 75% blast furnace slag, 22% type 50 cement and 3% silica fume. The rate of chloride ion ingress into reinforced concrete, and hence the time for chloride ion to reach the reinforcing steel, is shown to be dependent on applied load and the concrete quality. The dependence of corrosion process descriptors - passive layer formation, initiation period and propagation period - on the level of applied load is discussed. (Author) (6 refs., 3 tabs., 10 figs.)

  11. Accelerated Test Method for Corrosion Protective Coatings Project

    Science.gov (United States)

    Falker, John; Zeitlin, Nancy; Calle, Luz

    2015-01-01

    This project seeks to develop a new accelerated corrosion test method that predicts the long-term corrosion protection performance of spaceport structure coatings as accurately and reliably as current long-term atmospheric exposure tests. This new accelerated test method will shorten the time needed to evaluate the corrosion protection performance of coatings for NASA's critical ground support structures. Lifetime prediction for spaceport structure coatings has a 5-year qualification cycle using atmospheric exposure. Current accelerated corrosion tests often provide false positives and negatives for coating performance, do not correlate to atmospheric corrosion exposure results, and do not correlate with atmospheric exposure timescales for lifetime prediction.

  12. A Study on the Effect of Electrolyte Thickness on Atmospheric Corrosion of Carbon Steel

    International Nuclear Information System (INIS)

    Chung, Kyeong Woo; Kim, Kwang Bum

    1998-01-01

    Effect of electrolyte layer thickness and increase in concentration of electrolyte during electrolyte thining on the atmospheric corrosion of carbon steel were investigated using EIS and cathodic polarization technique. The electrolyte layer thickness was controlled via two methods : one is mechanical method with microsyringe applying a different amount of electrolyte onto the metal surface to give different electrolyte thickness with the same electrolyte concentration. The other is drying method in which water layer thickness decreases through drying, causing increase in concentration of electrolyte during electrolyte thinning. In the region whose corrosion rate is controlled by cathodic reaction, corrosion rate for mechanical method is larger than that for drying method. However, for the electrolyte layers thinner than 20 ∼ 30 m, increase in concentration of electrolyte cause a higher corrosion rate for the case of the mechanical method compared with that of drying method. For a carbon steel covered with 0.1M Na 2 SO 4 , maximum corrosion rate is found at an electrolyte thickness of 45 ∼ 55 μm for mechanical method. However, maximum corrosion rate is found at an electrolyte thickness of 20 ∼ 35 μm for drying method. The limiting current is inversely proportional to electrolyte thickness for electrolyte thicker than 20 ∼ 30 μm. However, further decrease of the electrolyte thickness leads to an electrolyte thickness-independent limiting current reagion, where the oxygen rate is controlled by the solvation of oxygen at the electrolyte/gas interface. Diffusion limiting current for drying method is smaller compared with that for mechanica control. This can be attributed to decreasing in O 2 solubility caused by increase in concentration of electrolyte during electrolyte thining

  13. Microbiologically influenced corrosion in ship ballast tanks

    NARCIS (Netherlands)

    Heyer, A.

    2013-01-01

    Microbiologically influenced corrosion (MIC) is known to be a dangerous process in ship tanks due to its rapid and yet unpredictable occurrence, leading to extremely fast local corrosion, possibly jeopardizing the structural integrity, in a relatively short time. This project focuses on a

  14. Corrosion of porous silicon in tetramethylammonium hydroxide solution

    International Nuclear Information System (INIS)

    Lai, Chuan; Li, Xue-Ming; Zou, Li-Ke; Chen, Qiang; Xie, Bin; Li, Yu-Lian; Li, Xiao-Lin; Tao, Zhi

    2014-01-01

    Highlights: • The corrosion of porous silicon in (CH 3 ) 4 NOH solution was studied. • The residue of corrosion products was a mixture of [(CH 3 ) 4 N] 2 SiO 3 and SiO 2 . • The effect factors for porous silicon corrosion were elaborately investigated. • The additive of ethanol in (CH 3 ) 4 NOH solution could reduce the corrosion rate. • The 1.0 M (CH 3 ) 4 NOH could act as an applicable and novel corrosion solution. - Abstract: Corrosion of porous silicon in tetramethylammonium hydroxide (TMAH) solution was studied using weight loss measurements and scanning electron microscope. The effects of temperature, concentration of TMAH and volume ratio of ethanol in 1.0 M TMAH on corrosion rate and corrosion time were elaborately investigated. The residue of corrosion products were characterized as a mixture of [(CH 3 ) 4 N] 2 SiO 3 and SiO 2 . A comparative test among TMAH, KOH and NaOH illustrated that the 1.0 M TMAH could act as an applicable and novel corrosion solution to remove porous silicon layer for determining the porosity of porous silicon

  15. Linear Time Local Approximation Algorithm for Maximum Stable Marriage

    Directory of Open Access Journals (Sweden)

    Zoltán Király

    2013-08-01

    Full Text Available We consider a two-sided market under incomplete preference lists with ties, where the goal is to find a maximum size stable matching. The problem is APX-hard, and a 3/2-approximation was given by McDermid [1]. This algorithm has a non-linear running time, and, more importantly needs global knowledge of all preference lists. We present a very natural, economically reasonable, local, linear time algorithm with the same ratio, using some ideas of Paluch [2]. In this algorithm every person make decisions using only their own list, and some information asked from members of these lists (as in the case of the famous algorithm of Gale and Shapley. Some consequences to the Hospitals/Residents problem are also discussed.

  16. Anticorrosion potential of hydralazine for corrosion of mild steel in ...

    African Journals Online (AJOL)

    Anticorrosion potential of mild steel by Hydralazine as corrosion inhibitor for mild steel in 1M hydrochloric acid was investigated by chemical and electrochemical measurements at 303-333 K temperature. The maximum inhibition efficiency of inhibitor by Weight loss method is around 90%, Tafel polarization method is ...

  17. Online Self-Organizing Network Control with Time Averaged Weighted Throughput Objective

    Directory of Open Access Journals (Sweden)

    Zhicong Zhang

    2018-01-01

    Full Text Available We study an online multisource multisink queueing network control problem characterized with self-organizing network structure and self-organizing job routing. We decompose the self-organizing queueing network control problem into a series of interrelated Markov Decision Processes and construct a control decision model for them based on the coupled reinforcement learning (RL architecture. To maximize the mean time averaged weighted throughput of the jobs through the network, we propose a reinforcement learning algorithm with time averaged reward to deal with the control decision model and obtain a control policy integrating the jobs routing selection strategy and the jobs sequencing strategy. Computational experiments verify the learning ability and the effectiveness of the proposed reinforcement learning algorithm applied in the investigated self-organizing network control problem.

  18. The Proposed Yucca Mountain Repository From A Corrosion Perspective

    International Nuclear Information System (INIS)

    J.H. Payer

    2005-01-01

    Corrosion is a primary determinant of waste package performance at the proposed Yucca Mountain Repository and will control the delay time for radionuclide transport from the waste package. Corrosion is the most probable and most likely degradation process that will determine when packages will be penetrated and the shape size and distribution of those penetrations. The general issues in corrosion science, materials science and electrochemistry are well defined, and the knowledge base is substantial for understanding corrosion processes. In this paper, the Yucca Mountain Repository is viewed from a corrosion perspective

  19. Corrosion/95 conference papers

    International Nuclear Information System (INIS)

    Anon.

    1995-01-01

    The papers in this conference represent the latest technological advances in corrosion control and prevention. The following subject areas are covered: cathodic protection in natural waters; materials for fossil fuel combustion and conversion systems; modern problems in atmospheric corrosion; innovative ideas for controlling the decaying infrastructure; deposits and their effects on corrosion in industry; volatile high temperature and non aqueous corrosion inhibitors; corrosion of light-weight and precoated metals for automotive application; refining industry corrosion; corrosion in pulp and paper industry; arctic/cold weather corrosion; materials selection for waste incinerators and associated equipment; corrosion measurement technology; environmental cracking of materials; advancing technology in the coating industry; corrosion in gas treating; green inhibition; recent advances in corrosion control of rail equipment; velocity effects and erosion corrosion in oil and gas production; marine corrosion; corrosion of materials in nuclear systems; underground corrosion control; corrosion in potable and industrial water systems in buildings and its impact on environmental compliance; deposit related boiler tube failures; boiler systems monitoring and control; recent developments and experiences in reactive metals; microbiologically influenced corrosion; corrosion and corrosion control for steel reinforced concrete; international symposium on the use of 12 and 13 Cr stainless steels in oil and gas production environments; subsea corrosion /erosion monitoring in production facilities; fiberglass reinforced pipe and tubulars in oilfield service; corrosion control technology in power transmission and distribution; mechanisms and methods of scale and deposit control; closing the loop -- results oriented cooling system monitoring and control; and minimization of aqueous discharge

  20. Kumaraswamy autoregressive moving average models for double bounded environmental data

    Science.gov (United States)

    Bayer, Fábio Mariano; Bayer, Débora Missio; Pumi, Guilherme

    2017-12-01

    In this paper we introduce the Kumaraswamy autoregressive moving average models (KARMA), which is a dynamic class of models for time series taking values in the double bounded interval (a,b) following the Kumaraswamy distribution. The Kumaraswamy family of distribution is widely applied in many areas, especially hydrology and related fields. Classical examples are time series representing rates and proportions observed over time. In the proposed KARMA model, the median is modeled by a dynamic structure containing autoregressive and moving average terms, time-varying regressors, unknown parameters and a link function. We introduce the new class of models and discuss conditional maximum likelihood estimation, hypothesis testing inference, diagnostic analysis and forecasting. In particular, we provide closed-form expressions for the conditional score vector and conditional Fisher information matrix. An application to environmental real data is presented and discussed.

  1. Cyclic Oxidation and Hot Corrosion of NiCrY-Coated Disk Superalloys

    Science.gov (United States)

    Gabb, Timothy P.; Miller, Robert A.; Sudbrack, Chantal K.; Draper, Susan L.; Nesbitt, James A.; Rogers, Richard B.; Telesman, Ignacy; Ngo, Vanda; Healy, Jonathan

    2016-01-01

    Powder metallurgy disk superalloys have been designed for higher engine operating temperatures through improvement of their strength and creep resistance. Yet, increasing disk application temperatures to 704 degrees Centigrade and higher could enhance oxidation and activate hot corrosion in harmful environments. Protective coatings could be necessary to mitigate such attack. Cylindrical coated specimens of disk superalloys LSHR and ME3 were subjected to thermal cycling to produce cyclic oxidation in air at a maximum temperature of 760 degrees Centigrade. The effects of substrate roughness and coating thickness on coating integrity after cyclic oxidation were considered. Selected coated samples that had cyclic oxidation were then subjected to accelerated hot corrosion tests. This cyclic oxidation did not impair the coating's resistance to subsequent hot corrosion pitting attack.

  2. Cyclic Oxidation and Hot Corrosion of NiCrY-Coated Disk Superalloy

    Science.gov (United States)

    Gabb, Tim; Miller, R. A.; Sudbrack, C. K.; Draper, S. L.; Nesbitt, J.; Telesman, J.; Ngo, V.; Healy, J.

    2015-01-01

    Powder metallurgy disk superalloys have been designed for higher engine operating temperatures through improvement of their strength and creep resistance. Yet, increasing disk application temperatures to 704 C and higher could enhance oxidation and activate hot corrosion in harmful environments. Protective coatings could be necessary to mitigate such attack. Cylindrical coated specimens of disk superalloys LSHR and ME3 were subjected to thermal cycling to produce cyclic oxidation in air at a maximum temperature of 760 C. The effects of substrate roughness and coating thickness on coating integrity after cyclic oxidation were considered. Selected coated samples that had cyclic oxidation were then subjected to accelerated hot corrosion tests. The effects of this cyclic oxidation on resistance to subsequent hot corrosion attack were examined.

  3. Effects of ion implantation on corrosion of zirconium and zirconium base alloys

    International Nuclear Information System (INIS)

    Zelenskij, V.F.; Petel'guzov, I.A.; Rekova, L.P.; Rodak, A.G.

    1989-01-01

    The influence of He and Ar ion bombardment on the corrosion of Zr and Zr-1%Nb and Zr-2.5%Nb alloys is investigated with the aims of finding the irradiation influence laws, obtaining the dependences of the effect of increasing the corrosiuon resistance on the type and dose of bombarding ions and of finding the conditions for the maximum effect. The prolonged corrosion test of specimens (3500 hours) have shown that the strongest effect is obtained for the irradiation with Ar ions up to the dose 1x10 16 ion/cm 2 . The kinetics of ion thermosorption after corrosion of irradiated materials is studied, the temperature threshold of implanted ion stability in zirconium and its alloys is found to be 400 deg C

  4. Long term corrosion of iron and non alloy or low alloy steels in clay soils. Physico-chemical characterisation and electrochemical study of archaeological analogues

    International Nuclear Information System (INIS)

    Pons, Emmanuelle

    2002-01-01

    Archaeological objects of Gallo-Roman and Merovingian time, and from a battlefield of World War 1, were studied to better understand long term corrosion phenomena of iron in clay soils. This study is part of the French national program about nuclear waste deep repository, conducted by the ANDRA (French national Agency for Radioactive Waste Management). Iron archaeological analogues make a valuable contribution to the specifying of containers for long lived and high level wastes (HLWs), because they provide access to the considered time scale. The experimental issue is divided into two major parts: - a physico-chemical characterisation of corrosion products, by Raman spectroscopy; - an electrochemical study of the behaviour of the different corrosion layers. Although the metallic material is different between ancient artefacts (ferrite) and 1914-1918 remains (hypo-eutectoid steels), the same stable phases are identified in their corrosion products: mainly iron oxides and oxi-hydroxides. From a macroscopic point of view, these products are staggered into two layers: an internal one, and an external one, which contains soil markers. Under the microscope, a complex composite structure appears. Goethite a-FeOOH, which was identified on each object, is frequently in contact with the metal core. The average corrosion rate in the burial environment, deduced from the layers thickness, highlights a significant slowdown of corrosion after the first burial time, about one century. The electrochemical study showed the predominant role of transport phenomena in the pores of corrosion layers. The behaviour of the metal - internal layer system is well explained by a model of porous electrode (De Levie theory). Despite its porosity, the internal layer is protective, as it leads to a significant decrease of the corrosion rate (about ten time). (author) [fr

  5. The Proposed Yucca Mountain Repository From A Corrosion Perspective

    International Nuclear Information System (INIS)

    J.H. Payer

    2005-01-01

    Corrosion is a primary determinant of waste package performance at the proposed Yucca Mountain Repository and will control the delay time for radionuclide transport from the waste package. Corrosion is the most probable and most likely degradation process that will determine when packages will be penetrated and the shape, size, and distribution of those penetrations. The general issues in corrosion science, materials science and electrochemistry are well defined, and the knowledge base is substantial for understanding corrosion processes. In this paper, the Yucca Mountain Repository is viewed from a corrosion perspective. A major component of the long-term strategy for safe disposal of nuclear waste at the Yucca Mountain Repository is first to completely isolate the radionuclides in the waste packages for long times and to greatly retard the egress and transport of radionuclides from penetrated packages. Therefore, long-lived waste packages are important. The corrosion resistance of the waste package outer canister is reviewed, and a framework for the analysis of localized corrosion processes is presented. An overview is presented of the Materials Performance targeted thrust of the U.S. Department of Energy/Office of Civilian Radioactive Waste Management's Office of Science and Technology and International. The thrust program strives for increased scientific understanding, enhanced process models and advanced technologies for corrosion control

  6. Microbially influenced corrosion of stainless steel by marine bacterium Vibrio natriegens: (I) Corrosion behavior

    Energy Technology Data Exchange (ETDEWEB)

    Cheng Sha; Tian Jintao [Institute of Materials Science and Engineering, Ocean University of China, Qingdao 266100 (China); Chen Shougang, E-mail: sgchen@ouc.edu.cn [Institute of Materials Science and Engineering, Ocean University of China, Qingdao 266100 (China); Lei Yanhua; Chang Xueting; Liu Tao [Institute of Materials Science and Engineering, Ocean University of China, Qingdao 266100 (China); Yin Yansheng, E-mail: yys2006@ouc.edu.cn [Institute of Materials Science and Engineering, Ocean University of China, Qingdao 266100 (China)

    2009-04-30

    The microbially influenced corrosion of stainless steel (SS) by marine bacterium Vibrio natriegens (V. natriegens) was investigated using surface analysis (atomic force microscopy (AFM), scanning electron microscopy (SEM), and energy dispersive X-ray analysis (EDXA)) and electrochemical techniques (the open circuit potential, electrochemical impedance spectroscopy (EIS), and potentiodynamic polarization curves ). AFM images corroborated the results from the EIS models which show biofilm attachment and subsequent detachment over time. The SEM images revealed the occurrence of micro-pitting corrosion underneath the biofilms on the metal surface after the biofilm removal. The presence of carbon, oxygen, phosphor and sulfur obtained from EDXA proved the formation of biofilm. The electrochemical results showed that the corrosion of SS was accelerated in the presence of V. natriegens based on the decrease in the resistance of the charge transfer resistance (R{sub ct}) obtained from EIS and the increase in corrosion current densities obtained from potentiodynamic polarization curves.

  7. EUROCORR 2007 - The European corrosion congress - Progress by corrosion control. Book of Abstracts

    International Nuclear Information System (INIS)

    2007-01-01

    This book of abstracts contains lectures, workshops and posters which were held on the European Corrosion Congress 2007 in Freiburg (Germany). The main topics of the sessions and posters are: 1. Corrosion and scale inhibition; 2. Corrosion by hot gases and combustion products; 3. Nuclear corrosion; 4. Environment sensitive fracture; 5. Surface Science; 6. Physico-chemical methods of corrosion testing; 7. Marine corrosion; 8. Microbial corrosion; 9. Corrosion of steel in concrete; 10. Corrosion in oil and gas production; 11. Coatings; 12. Corrosion in the refinery industry; 13. Cathodic protection; 14. Automotive Corrosion; 15. Corrosion of polymer materials. The main topics of the workshops are: 1. High temperature corrosion in the chemical, refinery and petrochemical industries; 2. Bio-Tribocorrosion; 3. Stress corrosion cracking in nuclear power plants; 4. Corrosion monitoring in nuclear systems; 5. Cathodic protection for marine and offshore environments; 6. Self-healing properties of new surface treatments; 7. Bio-Tribocorrosion - Cost 533/Eureka-ENIWEP-Meeting; 8. Drinking water systems; 9. Heat exchangers for seawater cooling

  8. Fatigue strength degradation of metals in corrosive environments

    Science.gov (United States)

    Adasooriya, N. D.; Hemmingsen, T.; Pavlou, D.

    2017-12-01

    Structures exposed to aggressive environmental conditions are often subjected to time-dependent loss of coating and loss of material due to corrosion; this causes reduction in the cross-sectional properties of the members, increased surface roughness, surface irregularities and corrosion pits, and degradation of material strengths. These effects have been identified and simulated in different research studies. However, time and corrosive media dependent fatigue strength curves for materials have not been discussed in the design or assessment guidelines for structures. This paper attempts to review the corrosion degradation process and available approaches/models used to determine the fatigue strength of corroded materials and to interpolate corrosion deterioration data. High cycle fatigue and full range fatigue life formulae for fatigue strength of corroded materials are proposed. The above formulae depend on the endurance limit of corroded material, in addition to the stress-life fatigue curve parameters of the uncorroded material. The endurance limit of corroded material can either be determined by a limited number of tests in the very high-cycle fatigue region or predicted by an analytical approach. Comparison with experimentally measured corrosion fatigue behavior of several materials is provided and discussed.

  9. Corrosion of aluminium in soft drinks.

    Science.gov (United States)

    Seruga, M; Hasenay, D

    1996-04-01

    The corrosion of aluminium (Al) in several brands of soft drinks (cola- and citrate-based drinks) has been studied, using an electrochemical method, namely potentiodynamic polarization. The results show that the corrosion of Al in soft drinks is a very slow, time-dependent and complex process, strongly influenced by the passivation, complexation and adsorption processes. The corrosion of Al in these drinks occurs principally due to the presence of acids: citric acid in citrate-based drinks and orthophosphoric acid in cola-based drinks. The corrosion rate of Al rose with an increase in the acidity of soft drinks, i.e. with increase of the content of total acids. The corrosion rates are much higher in the cola-based drinks than those in citrate-based drinks, due to the facts that: (1) orthophosphoric acid is more corrosive to Al than is citric acid, (2) a quite different passive oxide layer (with different properties) is formed on Al, depending on whether the drink is cola or citrate based. The method of potentiodynamic polarization was shown as being very suitable for the study of corrosion of Al in soft drinks, especially if it is combined with some non-electrochemical method, e.g. graphite furnace atomic absorption spectrometry (GFAAS).

  10. Ultrasonic guided wave for monitoring corrosion of steel bar

    Science.gov (United States)

    Liu, Xi; Qin, Lei; Huang, Bosheng

    2018-01-01

    Steel corrosion of reinforced concrete structures has become a serious problem all over the word. In this paper, the work aims at monitoring steel corrosion using ultrasonic guided wave (UGW). Ultrasonic guided wave monitoring is a dynamic and non-destructive testing technology. The advantages of ultrasonic guided wave monitoring for reinforcement corrosion are real-time, online and continuous. In addition, it can judge the different stages of steel bar corrosion, which achieved non-destructive detection.

  11. Evaluation of intergranular corrosion rate and microstructure of forged 316L round bar

    International Nuclear Information System (INIS)

    Lim, H. K.; Kim, Y. S.

    2009-01-01

    When austenitic stainless steels are heat treated in the range of 500∼850 .deg. C, the alloys are sensitized due to the formation of chromium carbide at grain boundaries and then intergranular corrosion occurs. This paper aims to evaluate the intergranular corrosion rate and microstructural change of forged 316L stainless steel. To analyze the microstructure by forging conditions, ferrite phase, sigma phase, intergranular precipitation were observed. In order to evaluate the intergranular corrosion rate. Huey test was performed by ASTM A262. On the base of microstructural observation, ferrite and sigma phases were not detected, and also intergranular precipitation was not revealed in optical microscopic observation. By ASTM A262 Practice A, step structure was shown in all forging conditions. Intergranular corrosion rate gradually increased by Huey test periods but average corrosion rate was under 0.03 mm/month

  12. Evaluation of intergranular corrosion rate and microstructure of forged 316L round bar

    Energy Technology Data Exchange (ETDEWEB)

    Lim, H. K.; Kim, Y. S. [Andong National University, Andong (Korea, Republic of)

    2009-12-15

    When austenitic stainless steels are heat treated in the range of 500{approx}850 .deg. C, the alloys are sensitized due to the formation of chromium carbide at grain boundaries and then intergranular corrosion occurs. This paper aims to evaluate the intergranular corrosion rate and microstructural change of forged 316L stainless steel. To analyze the microstructure by forging conditions, ferrite phase, sigma phase, intergranular precipitation were observed. In order to evaluate the intergranular corrosion rate. Huey test was performed by ASTM A262. On the base of microstructural observation, ferrite and sigma phases were not detected, and also intergranular precipitation was not revealed in optical microscopic observation. By ASTM A262 Practice A, step structure was shown in all forging conditions. Intergranular corrosion rate gradually increased by Huey test periods but average corrosion rate was under 0.03 mm/month.

  13. The effect of corrosion on the structural reliability of steel offshore structures

    International Nuclear Information System (INIS)

    Melchers, Robert E.

    2005-01-01

    This paper considers essential theoretical concepts and data requirements for engineering structural reliability assessment suitable for the estimation of the safety and reliability of corroding ships, offshore structures and pipelines. Such infrastructure operates in a harsh environment. Allowance must be made for structural deterioration since protective measures such as paint coatings, galvanizing or cathodic protection may be ineffective. Reliability analysis requires accurate engineering models for the description and prediction of material corrosion loss and for the maximum depth of pitting. New probability-based models for both these forms of corrosion have been proposed recently and calibrated against a wide range of data. The effects of water velocity and of water pollution are reviewed and compared with recently reported field data for a corrosion at an offshore oil platform. The data interpreted according to the model show good correlation when allowance is made for the season of first immersion and the adverse effects of seawater velocity and of water pollution. An example is given to illustrate the application of reliability analysis to a pipeline subject to pitting corrosion. An important outcome is that good quality estimation of the longer-term probability of loss of structural integrity requires good modelling of the longer-term corrosion behaviour. This is usually associated with anaerobic corrosion. As a result, it cannot be extrapolated from data for short-term corrosion as this is associated with aerobic corrosion conditions

  14. The effect of corrosion on the structural reliability of steel offshore structures

    Energy Technology Data Exchange (ETDEWEB)

    Melchers, Robert E. [Centre for Infrastructure Performance and Reliability, Department of Civil, Surveying and Environmental Engineering, School of Engineering, University of Newcastle, University Drive, Callaghan NSW 2300 (Australia)]. E-mail: rob.melchers@newcastle.edu.au

    2005-10-01

    This paper considers essential theoretical concepts and data requirements for engineering structural reliability assessment suitable for the estimation of the safety and reliability of corroding ships, offshore structures and pipelines. Such infrastructure operates in a harsh environment. Allowance must be made for structural deterioration since protective measures such as paint coatings, galvanizing or cathodic protection may be ineffective. Reliability analysis requires accurate engineering models for the description and prediction of material corrosion loss and for the maximum depth of pitting. New probability-based models for both these forms of corrosion have been proposed recently and calibrated against a wide range of data. The effects of water velocity and of water pollution are reviewed and compared with recently reported field data for a corrosion at an offshore oil platform. The data interpreted according to the model show good correlation when allowance is made for the season of first immersion and the adverse effects of seawater velocity and of water pollution. An example is given to illustrate the application of reliability analysis to a pipeline subject to pitting corrosion. An important outcome is that good quality estimation of the longer-term probability of loss of structural integrity requires good modelling of the longer-term corrosion behaviour. This is usually associated with anaerobic corrosion. As a result, it cannot be extrapolated from data for short-term corrosion as this is associated with aerobic corrosion conditions.

  15. Evaluations of corrosion resistance of Ni-Cr plated and Zn-plated Fe Substrates Using an Electrolytic Corrosion Test

    International Nuclear Information System (INIS)

    Lee, Jaebong; Kim, Kyungwook; Park, Minwoo; Song, Taejun; Lee, Chaeseung; Lee, Euijong; Kim, Sangyeol

    2013-01-01

    An Eectrolytic Corrosion(EC) test method was evaluated by the comparison with Copper Accelerated Acetic Salt Spray(CASS) and Neutral Salt Spray(SS) tests. Those methods were applied in order to evaluate corrosion resistance of Ni-Cr plated and Zn-plated Fe substrates. The correlations between results obtained by different test methods were investigated. Results showed that the electrochemical method such as the EC test method was superior to the conventional methods such as CASS and SS, in terms of the quantitative accuracy and the test-time span. Furthermore, the EC test method provided the useful means to estimate the initiation of corrosion of each layer by monitoring the rest potentials of the coated layers such as Ni, Cr, and Zn on Fe substrate. With regard to test time spans, the EC test provided the 78 times and 182 times faster results than the CASS test in cases of Fe + 5μm Ni + 0.5 μm Cr and Fe + 20 μm Ni + 0.5 μm Cr respectively, while the EC test was 85 times faster results than the Salt Spray test in the case of Fe + 20 g/m 2 Zn. Therefore, the EC test can be the better method to evaluate the resistance to corrosion of coated layers than the conventional methods such as the SS test and the CASS

  16. Corrosion allowances for sodium heated steam generators: evaluation of effects and extrapolation to component life time

    Energy Technology Data Exchange (ETDEWEB)

    Grosser, E E; Menken, G

    1975-07-01

    Steam generator tubes are subjected to two categories of corrosion; metal/sodium reactions and metal/water-steam interactions. Referring to these environmental conditions the relevant parameters are discussed. The influences of these parameters on the sodium corrosion and water/steam-reactions are evaluated. Extrapolations of corrosion values to steam generator design conditions are performed and discussed in detail. (author)

  17. Corrosion allowances for sodium heated steam generators: evaluation of effects and extrapolation to component life time

    International Nuclear Information System (INIS)

    Grosser, E.E.; Menken, G.

    1975-01-01

    Steam generator tubes are subjected to two categories of corrosion; metal/sodium reactions and metal/water-steam interactions. Referring to these environmental conditions the relevant parameters are discussed. The influences of these parameters on the sodium corrosion and water/steam-reactions are evaluated. Extrapolations of corrosion values to steam generator design conditions are performed and discussed in detail. (author)

  18. A new steel with good low-temperature sulfuric acid dew point corrosion resistance

    Energy Technology Data Exchange (ETDEWEB)

    Cheng, X.Q.; Li, X.G. [Corrosion and Protection Center, University of Science and Technology Beijing (China); Key Laboratory of Corrosion and Protection (Ministry of Education), Beijing (China); Sun, F.L. [Corrosion and Protection Center, University of Science and Technology Beijing (China); Lv, S.J. [Corrosion and Protection Center, University of Science and Technology Beijing (China); Equipment and Power Department, Shijiazhuang Refine and Chemical Company Limited, SINOPEC, Shijiazhuang (China)

    2012-07-15

    In this work, new steels (1, 2, and 3) were developed for low-temperature sulfuric acid dew point corrosion. The mass loss rate, macro- and micro-morphologies and compositions of corrosion products of new steels in 10, 30, and 50% H{sub 2}SO{sub 4} solutions at its corresponding dew points were investigated by immersion test, scanning electron microscopy (SEM) and energy-dispersive spectrometry (EDS). The results indicated that mass loss rate of all the tested steels first strongly increased and then decreased as H{sub 2}SO{sub 4} concentration increased, which reached maximum at 30%. Corrosion resistance of 2 steel is the best among all specimens due to its fine and homogeneous morphologies of corrosion products. The electrochemical corrosion properties of new steels in 10 and 30% H{sub 2}SO{sub 4} solutions at its corresponding dew points were studied by potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) techniques. The results demonstrated that corrosion resistance of 2 steel is the best among all the experimental samples due to its lowest corrosion current density and highest charge transfer resistance, which is consistent with the results obtained from immersion tests. (Copyright copyright 2012 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  19. Numerical Study of Corrosion Crack Opening

    DEFF Research Database (Denmark)

    Thoft-Christensen, Palle; Frandsen, Henrik Lund; Svensson, Staffan

    2008-01-01

    is proportional. More recently, the constant of proportionality, the so-called crack-corrosion index, has been studied further with respect to its dependence on the diameter of the reinforcement and the concrete cover. In the present paper the above-mentioned work is presented and extended with more realistic 3D......-models of the cracked concrete beam. The crack-corrosion index is evaluated for a variation of different parameters, i.e. bar diameter, concrete cover, crack length and type of corrosion product. This paper is an extended version of a paper by Thoft-Christensen et al. (2005) presented at the IFIP WG 7.5 Conference...... for the corrosion crack opening. Experiments and theoretical analysis by a numerical method, FEM, support that the relation between the reduction of the reinforcement bar diameter due to corrosion and the corresponding increase in crack width for a given time interval, measured on the surface of a concrete specimen...

  20. Corrosion-fatigue studies of the Zr-based Vitreloy 105 bulk metallic glass

    International Nuclear Information System (INIS)

    Horton Jr, Joe A.; Morrison, M.L.; Buchanan, R.A.; Liaw, Peter K.; Green, B.A.; Wang, G.Y.

    2007-01-01

    The purpose of this study was to characterize the stress-life behavior of the Vitreloy 105 BMG alloy in the four-point bending configuration in a 0.6 M. NaCl electrolyte. At high stress amplitudes, the corrosion-fatigue life was similar to the fatigue lives observed in air. The environment became increasingly detrimental with decreases in stress, and the corrosion-fatigue endurance limit decreased to about 50 MPa, an 88% decrease relative to testing in air. Similar to the tests conducted in air, oxide particles were found on the fracture surfaces but did not appear to significantly affect the corrosion-fatigue lives. However, wear and the resultant corrosion at the outer loading pins resulted in crack initiation in most of the samples. Thus, these results are considered conservative estimates of the corrosion-fatigue behavior of this BMG alloy. Monitoring of the samples and the open-circuit potentials revealed that the onset of significant crack growth occurred at an average of 92% of the total fatigue life. The mechanism of corrosion-fatigue degradation was found to be anodic dissolution

  1. Surface monitoring for pitting evolution into uniform corrosion on Cu-Ni-Zn ternary alloy in alkaline chloride solution: ex-situ LCM and in-situ SECM

    Science.gov (United States)

    Kong, Decheng; Dong, Chaofang; Zheng, Zhaoran; Mao, Feixiong; Xu, Aoni; Ni, Xiaoqing; Man, Cheng; Yao, Jizheng; Xiao, Kui; Li, Xiaogang

    2018-05-01

    The evolution of the corrosion process on Cu-Ni-Zn alloy in alkaline chloride solution was investigated by in-situ scanning electrochemical microscopy, X-ray photoelectron spectroscopy, and ex-situ laser confocal microscopy, and the effects of ambient temperature and polarization time were also discussed. The results demonstrated a higher pitting nucleation rate and lower pit growth rate at low temperature. The ratio of pit depth to mouth diameter decreased with increasing pit volume and temperature, indicating that pits preferentially propagate in the horizontal direction rather than the vertical direction owing to the presence of corrosion products and deposited copper. The surface current was uniform and stabilized at approximately 2.2 nA during the passive stage, whereas the current increased after the pits were formed with the maximum approaching 3 nA. Increasing the temperature led to an increase in porous corrosion products (CuO, Zn(OH)2, and Ni(OH)2) and significantly increased the rate of transition from pitting to uniform corrosion. Dezincification corrosion was detected by energy dispersive spectrometry, and a mechanism for pitting transition into uniform corrosion induced by dezincification at the grain boundaries is proposed.

  2. Effect of Host Media on Microbial Influenced Corrosion due to Desulfotomaculum nigrificans

    Science.gov (United States)

    Lata, Suman; Sharma, Chhaya; Singh, Ajay K.

    2013-04-01

    This article reports about the tests carried to investigate microbial-induced corrosion on stainless steels due to sulfate-reducing bacteria sp. Desulfotomaculum nigrificans in different host media. Stainless steel 304L, 316L, and 2205 were selected for the test. Modified Baar's media (BM), sodium chloride solution, and artificial sea water (SW) were used as test solutions in anaerobic conditions. Electrochemical polarization and immersion test were performed to estimate the extent of corrosion rate and pitting on stainless steels. SEM/EDS were used to study the details inside/outside pits formed on the corroded samples. Biofilm formed on corroded coupons was analyzed for its components by UV/Visible spectroscopy. Corrosion attack on the test samples was observed maximum in case of exposure to SW followed by NaCl solution, both having sulfide and chloride whereas stainless steel exposed to BM, having sulfide, showed minimum attack. Tendency of extracellular polymeric substances to bind metal ions is observed to be responsible for governing the extent of corrosion attack.

  3. Analysis of stress corrosion data by means of the statistic of extreme values

    International Nuclear Information System (INIS)

    Imarisio, G.; Lanza, F.

    1978-01-01

    The possibility of examining stress corosion by means of extreme statistic was proposed. A series of test in boiling MgCl 2 of samples made on AISI 304 have been performed. Evolution of cracks dimension and time of life of samples was followed. It has been shown that the dimensions of the maximum cracks on the sample corroded for different times can be organized following the extreme values statistic. Also the life time of sample can be treated in the same way. A confirmation has been obtained using data taken from literature. Possible uses of predictions obtained with this type of analysis have been underlined. An extension of the toward less corrosive media and samples of several volumes is suggested to check the validity of the method

  4. Corrosion/96 conference papers

    International Nuclear Information System (INIS)

    Anon.

    1996-01-01

    Topics covered by this conference include: cathodic protection in natural waters; cleaning and repassivation of building HVAC systems; worldwide opportunities in flue gas desulfurization; advancements in materials technology for use in oil and gas service; fossil fuel combustion and conversion; technology of corrosion inhibitors; computers in corrosion control--modeling and information processing; recent experiences and advances of austenitic alloys; managing corrosion with plastics; corrosion measurement technology; corrosion inhibitors for concrete; refining industry; advances in corrosion control for rail and tank trailer equipment; CO 2 corrosion--mechanisms and control; microbiologically influenced corrosion; corrosion in nuclear systems; role of corrosion in boiler failures; effects of water reuse on monitoring and control technology in cooling water applications; methods and mechanisms of scale and deposit control; corrosion detection in petroleum production lines; underground corrosion control; environmental cracking--relating laboratory results and field behavior; corrosion control in reinforced concrete structures; corrosion and its control in aerospace and military hardware; injection and process addition facilities; progress reports on the results of reinspection of deaerators inspected or repaired per RP0590 criteria; near 100% volume solids coating technology and application methods; materials performance in high temperature environments containing halides; impact of toxicity studies on use of corrosion/scale inhibitors; mineral scale deposit control in oilfield related operations; corrosion in gas treating; marine corrosion; cold climate corrosion; corrosion in the pulp and paper industry; gaseous chlorine alternatives in cooling water systems; practical applications of ozone in recirculating cooling water systems; and water reuse in industry. Over 400 papers from this conference have been processed separately for inclusion on the data base

  5. Corrosion/94 conference papers

    International Nuclear Information System (INIS)

    Anon.

    1994-01-01

    The approximately 500 papers from this conference are divided into the following sections: Rail transit systems--stray current corrosion problems and control; Total quality in the coatings industry; Deterioration mechanisms of alloys at high temperatures--prevention and remediation; Research needs and new developments in oxygen scavengers; Computers in corrosion control--knowledge based system; Corrosion and corrosivity sensors; Corrosion and corrosion control of steel reinforced concrete structures; Microbiologically influenced corrosion; Practical applications in mitigating CO 2 corrosion; Mineral scale deposit control in oilfield-related operations; Corrosion of materials in nuclear systems; Testing nonmetallics for life prediction; Refinery industry corrosion; Underground corrosion control; Mechanisms and applications of deposit and scale control additives; Corrosion in power transmission and distribution systems; Corrosion inhibitor testing and field application in oil and gas systems; Decontamination technology; Ozone in cooling water applications, testing, and mechanisms; Corrosion of water and sewage treatment, collection, and distribution systems; Environmental cracking of materials; Metallurgy of oil and gas field equipment; Corrosion measurement technology; Duplex stainless steels in the chemical process industries; Corrosion in the pulp and paper industry; Advances in cooling water treatment; Marine corrosion; Performance of materials in environments applicable to fossil energy systems; Environmental degradation of and methods of protection for military and aerospace materials; Rail equipment corrosion; Cathodic protection in natural waters; Characterization of air pollution control system environments; and Deposit-related problems in industrial boilers. Papers have been processed separately for inclusion on the data base

  6. Evaluation of aluminum-clad spent fuel corrosion in Argentine basins

    International Nuclear Information System (INIS)

    Haddad, R.; Loberse, A.N.; Semino, C.J.; Guasp, R.

    2001-01-01

    An IAEA sponsored Coordinated Research Program was extended to study corrosion effects in several sites. Racks containing Aluminum samples were placed in different positions of each basin and periodic sampling of all the waters was performed to conduct chemical analysis. Different forms of corrosion have been encountered during the programme. In general, the degree of degradation is inversely proportional to the purity of the water. Maximum pit depths after 2 years of exposure are in the range of 100-200 μm. However, sediments deposited on the coupon surfaces seem to be responsible for the developing of large pits (1-2 mm in diameter). In many cases, what appears to be iron oxide particles were found originated by the corrosion of carbon steel components present elsewhere in the basin. These results correlate with observations made on the fuel itself, during exhaustive visual inspection. (author)

  7. THE CORROSION BEHAVIOR AND WEAR RESISTANCE OF GRAY CAST IRON

    Directory of Open Access Journals (Sweden)

    Lina F. Kadhim

    2018-01-01

    Full Text Available Gray cast iron has many applications as pipes , pumps and valve bodies where it has influenced by heat and contact with other solutions . This research has studied the corrosion behavior and Vickers hardness of gray cast iron by immersion in four strong alkaline solutions (NaOH, KOH, Ca(OH2, LiOHwith three concentrations (1%,2%,3% of each solution. Dry sliding wear has carried out before and after the heat treatments (stress relief ,normalizing, hardening and tempering. In this work ,maximum wear strength has obtained at tempered gray cast iron and minimum corrosion rate has obtained in LiOH solution by forming protective white visible oxide layer.

  8. Seismic load resistance of reinforcing steels in the as delivered condition and after corrosion - relevant material characteristics for performance evaluation

    Energy Technology Data Exchange (ETDEWEB)

    Moersch, Ing. Joerg [Max Aicher Engineering GmbH, Freilassing (Germany)

    2016-10-15

    This type of accelerated corrosion test was used to study the high number of test samples in due time. The corrosion phenomena obtained in salt spray testing deviate significantly from corrosion phenomena (pitting factor) obtained in practical conditions. Salt spray testing represents practical conditions for the more uniform corrosion as a result of a severe carbonation of the concrete and/or for higher chloride contents at the surface of the rebar. At low corrosion current densities the effect of pit depth on residual mechanical performance might be underestimated. Reinforced concrete (r.c.) buildings in seismic areas shall be designed to guarantee enough ductile resources as for example a sufficient rotational capacity to allow for load re-distribution. The rotational capacity is directly dependent on the ductility of the reinforcing steel which is generally expressed as elongation at maximum load (A+g{sub t}) and the hardening ratio (R{sub m}/R{sub e}). A direct testing of the seismic load resistance of reinforcing steels is not part of the construction product standards. Therefore it was decided by European Commission to introduce this performance requirement in the mandate for the revision of EN 10080:2005. In parallel to the standardization process a research project was carried out to deliver the scientific background.

  9. Detection and characterization of corrosion of bridge cables by time domain reflectometry

    Science.gov (United States)

    Liu, Wei; Hunsperger, Robert G.; Folliard, Kevin; Chajes, Michael J.; Barot, Jignesh; Jhaveri, Darshan; Kunz, Eric

    1999-02-01

    In this paper, we develop and demonstrate a nondestructive evaluation technique for corrosion detection of embedded or encased steel cables. This technique utilizes time domain reflectometry (TDR), which has been traditionally used to detect electrical discontinuities in transmission lines. By applying a sensor wire along with the bridge cable, we can model the cable as an asymmetric, twin-conductor transmission line. Physical defects of the bridge cable will change the electromagnetic properties of the line and can be detected by TDR. Furthermore, different types of defects can be modeled analytically, and identified using TDR. TDR measurement results from several fabricated bridge cable sections with built-in defects are reported.

  10. Aluminum corrosion product release kinetics

    Energy Technology Data Exchange (ETDEWEB)

    Edwards, Matt, E-mail: Matthew.Edwards@cnl.ca; Semmler, Jaleh; Guzonas, Dave; Chen, Hui Qun; Toor, Arshad; Hoendermis, Seanna

    2015-07-15

    Highlights: • Release of Al corrosion product was measured in simulated post-LOCA sump solutions. • Increased boron was found to enhance Al release kinetics at similar pH. • Models of Al release as functions of time, temperature, and pH were developed. - Abstract: The kinetics of aluminum corrosion product release was examined in solutions representative of post-LOCA sump water for both pressurized water and pressurized heavy-water reactors. Coupons of AA 6061 T6 were exposed to solutions in the pH 7–11 range at 40, 60, 90 and 130 °C. Solution samples were analyzed by inductively coupled plasma atomic emission spectroscopy, and coupon samples were analyzed by secondary ion mass spectrometry. The results show a distinct “boron effect” on the release kinetics, expected to be caused by an increase in the solubility of the aluminum corrosion products. New models were developed to describe both sets of data as functions of temperature, time, and pH (where applicable)

  11. Corrosion effect of fast reactor fuel claddings on their mechanical properties

    International Nuclear Information System (INIS)

    Davydov, E.F.; Krykov, F.N.; Shamardin, V.K.

    1985-01-01

    Fast reactor fuel cladding corrosion effect on its mechanical properties was investigated. UO 2 fuel elements were irradiated in the BOP-60 reactor at the linear heat rate of 42 kw/m. Fuel cladding is made of stainless steel OKh16N15M3BR. Calculated maximum cladding temperature is 920 K. Neutron fluence in the central part of fuel elements is 6.3x10 26 m+H- 2 . To investigate the strength changes temperature dependence of corrossion depth, cladding strength reduction factors was determined. Samples plasticity reduction with corrosion layer increase is considered to be a characteristic feature

  12. 49 CFR 398.6 - Hours of service of drivers; maximum driving time.

    Science.gov (United States)

    2010-10-01

    ... REGULATIONS TRANSPORTATION OF MIGRANT WORKERS § 398.6 Hours of service of drivers; maximum driving time. No person shall drive nor shall any motor carrier permit or require a driver employed or used by it to drive...

  13. Time-temperature influence on the corrosion resistance of Ni-Cr-Nb superalloys in contact with Na2SO4-V2O5 molten mixtures

    International Nuclear Information System (INIS)

    Otero, E.; Pardo, A.; Hernaez, J.; Hierro, P.

    1990-01-01

    Corrosion rate data obtained by the polarization resistance method in nickel-base superalloys in contact with Na 2 SO 4 -V 2 O 5 molten mixtures are presented. The instrumental technique is also described. Time-temperature influence on the corrosion kinetics in the described conditions is discussed (Author)

  14. Corrosion evaluation of uranyl nitrate solution evaporator and denitrator in Tokai reprocessing plant

    International Nuclear Information System (INIS)

    Yamanaka, Atsushi; Hashimoto, Kowa; Uchida, Toyomi; Shirato, Yoji; Isozaki, Toshihiko; Nakamura, Yoshinobu

    2011-01-01

    The Tokai reprocessing plant (TRP) adopted the PUREX method in 1977 and has reprocessed spent nuclear fuel of 1140 tHM (tons of heavy metals) since then. The reprocessing equipment suffers from various corrosion phenomena because of high nitric acidity, solution ion concentrations, such as uranium, plutonium, and fission products, and temperature. Therefore, considering corrosion performance in such a severe environment, stainless steels, titanium steel, and so forth were employed as corrosion resistant materials. The severity of the corrosive environment depends on the nitric acid concentration and the temperature of the solution, and uranium in the solution reportedly does not significantly affect the corrosion of stainless steels and controls the corrosion rates of titanium steel. The TRP equipment that handles uranyl nitrate solution operates at a low nitric acid concentration and has not experienced corrosion problems until now. However, there is a report that corrosion rates of some stainless steels increase in proportion to rising uranium concentrations. The equipment that handles the uranyl nitrate solution in the TRP includes the evaporators, which concentrate uranyl nitrate to a maximum concentration of about 1000 gU/L (grams of uranium per liter), and the denitrator, where uranyl nitrate is converted to UO 3 powder at about 320degC. These equipments are therefore required to grasp the degree of the progress of corrosion to handle high-temperature and high-concentration uranyl nitrate. The evaluation of this equipment on the basis of thickness measurement confirmed only minor corrosion and indicated that the equipment would be fully adequate for future operation. (author)

  15. Corrosion testing of uranium silicide fuel specimens

    International Nuclear Information System (INIS)

    Bourns, W.T.

    1968-09-01

    U 3 Si is the most promising high density natural uranium fuel for water-cooled power reactors. Power reactors fuelled with this material are expected to produce cheaper electricity than those fuelled with uranium dioxide. Corrosion tests in 300 o C water preceded extensive in-reactor performance tests of fuel elements and bundles. Proper heat-treatment of U-3.9 wt% Si gives a U 3 5i specimen which corrodes at less than 2 mg/cm 2 h in 300 o C water. This is an order of magnitude lower than the maximum corrosion rate tolerable in a water-cooled reactor. U 3 Si in a defected unbonded Zircaloy-2 sheath showed only a slow uniform sheath expansion in 300 o C water. All tests were done under isothermal conditions in an out-reactor loop. (author)

  16. The corrosion behavior of hafnium in high-temperature-water environments

    Energy Technology Data Exchange (ETDEWEB)

    Rishel, D.M.; Smee, J.D.; Kammenzind, B.F.

    1999-10-01

    The high-temperature-water corrosion performance of hafnium is evaluated. Corrosion kinetic data are used to develop correlations that are a function of time and temperature. The evaluation is based on corrosion tests conducted in out-of-pile autoclaves and in out-of-flux locations of the Advanced Test Reactor (ATR) at temperatures ranging from 288 to 360 C. Similar to the corrosion behavior of unalloyed zirconium, the high-temperature-water corrosion response of hafnium exhibits three corrosion regimes: pretransition, posttransition, and spalling. In the pretransition regime, cubic corrosion kinetics are exhibited, whereas in the posttransition regime, linear corrosion kinetics are exhibited. Because of the scatter in the spalling regime data, it is not reasonable to use a best fit of the data to describe spalling regime corrosion. Data also show that neutron irradiation does not alter the corrosion performance of hafnium. Finally, the data illustrate that the corrosion rate of hafnium is significantly less than that of Zircaloy-2 and Zircaloy-4.

  17. Inhibitory effect of konjac glucomanan on pitting corrosion of AA5052 aluminium alloy in NaCl solution.

    Science.gov (United States)

    Zhang, Kegui; Yang, Wenzhong; Xu, Bin; Chen, Yun; Yin, Xiaoshuang; Liu, Ying; Zuo, Huanzhen

    2018-05-01

    A natural carbohydrate polymer, konjac glucomanan, has been extracted from commercial product and studied as a green corrosion inhibitor for AA5052 aluminium alloy in 3.5 wt% NaCl solution by high-performance gel permeation chromatography (GPC), thermo gravimetric analysis (TGA), Fourier-transform infrared (FT-IR) spectra, electrochemical measurement and surface characterization techniques. The results of GPC measurements suggest the weight-average molecular weight and the number-average molecular weight of KGM with 98.2% purity are 1.61 × 10 5  g/mol and 1.54 × 10 5  g/mol, respectively. Potentiodynamic polarization curves show konjac glucomanan behaves as a mixed-type inhibitor with dominant anodic effect and that its maximum efficiency at 200 ppm is 94%. Electrochemical impedance spectroscopy (EIS) studies reveal the resistance of oxide film is approximately two orders of magnitude greater than the resistance of adsorbed inhibitor layer and that they both increase with KGM concentration. Moreover, in-situ electrochemical noise (EN) detection demonstrates that the growth and propagation stages of the pitting corrosion germinating on metal surface are blocked by polysaccharide additive, which is confirmed by the surface analysis of aluminium alloy using scanning electron microscope (SEM), energy dispersive spectroscopy (EDS) and Raman spectroscopy. At last, it is found that the addition of KGM makes it harder for water droplet containing NaCl to wet the metallic substrate. Copyright © 2018 Elsevier Inc. All rights reserved.

  18. Assessing corrosion in oil refining and petrochemical processing

    Directory of Open Access Journals (Sweden)

    Randy C. John

    2004-03-01

    Full Text Available This paper summarizes the development of an information system used to manage corrosion of metals and alloys by high temperature gases found in many different oil refining, petrochemical, power generation, and chemical processes. The database currently represents about 7.9 million h of exposure time for about 5,500 tests with 89 commercial alloys for a temperature range of 200 - 1,200°C. The system manages corrosion data from well-defined exposures and determines corrosion product stabilities. New models used in the analysis of thermochemical data for the Fe-Ni-Cr-Co-C-O-S-N-H system are being compiled. All known phases based upon combinations of the elements have been analyzed to allow complete assessments of corrosion product stabilities. Use of these data allows prediction of stable corrosion products and hence identification of the possible dominant corrosion mechanisms. The system has the potential to be used in corrosion research, alloy development, failure analysis, lifetime prediction, and process operations evaluations. The corrosion mechanisms emphasized are oxidation, sulfidation, sulfidation/oxidation, and carburization.

  19. Real-time corrosion monitoring of steel influenced by microbial activity (SRB) under controlled seawater injection conditions

    Energy Technology Data Exchange (ETDEWEB)

    Kane, Russell D. [InterCorr International, Inc., 14503 Bammel N. Houston Road, Suite 300, Houston, TX 77019 (United States); Campbell, Scott [Commercial Microbiology Inc., 10400 Westoffice Drive Suite 107, Houston, TX 77042 (United States)

    2004-07-01

    An experimental study of microbiologically influenced corrosion (MIC) was conducted involving online, real-time monitoring of a bio-film loop under controlled conditions simulating oil field water handling and injection. Bio-film growth, MIC and biocide efficacy were monitored using an automated, multi-technique monitoring system including linear polarization resistance, electrochemical noise and harmonic distortion analysis. This data was correlated with conventional off-line methods to differentiate conditions of varying MIC activity in real-time to facilitate quick assessment and operator intervention. (authors)

  20. The Effect of Corrosion on the Seismic Behavior of Buried Pipelines and a Remedy for Their Seismic Retrofit

    International Nuclear Information System (INIS)

    Hosseini, Mahmood; Salek, Shamila; Moradi, Masoud

    2008-01-01

    The effect of corrosion phenomenon has been investigated by performing some sets of 3-Dimensional Nonlinear Time History Analysis (3-D NLTHA) in which soil structure interaction as well as wave propagation effects have been taken into consideration. The 3-D NLTHA has been performed by using a finite element computer program, and both states of overall and local corrosions have been considered for the study. The corrosion has been modeled in the computer program by introducing decreased values of either pipe wall thickness or modulus of elasticity and Poisson ratio. Three sets of 3-component accelerograms have been used in analyses, and some appropriate numbers of zeros have been added at the beginning of records to take into account the wave propagation in soil and its multi-support excitation effect. The soil has been modeled by nonlinear springs in longitudinal, lateral, and vertical directions. A relatively long segment of the pipeline has been considered for the study and the effect of end conditions has been investigated by assuming different kinds end supports for the segment. After studying the corroded pipeline, a remedy has been considered for the seismic retrofit of corroded pipe by using a kind of Fiber Reinforced Polymers (FRP) cover. The analyses have been repeated for the retrofitted pipeline to realize the adequacy of FRP cover. Numerical results show that if the length of the pipeline segment is large enough, comparing to the wave length of shear wave in the soil, the end conditions do not have any major effect on the maximum stress and strain values in the pipe. Results also show that corrosion can lead to the increase in plastic strain values in the pipe up to 4 times in the case of overall corrosion and up to 20 times in the case of local corrosion. The satisfactory effect of using FRP cover is also shown by the analyses results, which confirm the decrease of strain values to 1/3

  1. The Effect of Corrosion on the Seismic Behavior of Buried Pipelines and a Remedy for Their Seismic Retrofit

    Science.gov (United States)

    Hosseini, Mahmood; Salek, Shamila; Moradi, Masoud

    2008-07-01

    The effect of corrosion phenomenon has been investigated by performing some sets of 3-Dimensional Nonlinear Time History Analysis (3-D NLTHA) in which soil structure interaction as well as wave propagation effects have been taken into consideration. The 3-D NLTHA has been performed by using a finite element computer program, and both states of overall and local corrosions have been considered for the study. The corrosion has been modeled in the computer program by introducing decreased values of either pipe wall thickness or modulus of elasticity and Poisson ratio. Three sets of 3-component accelerograms have been used in analyses, and some appropriate numbers of zeros have been added at the beginning of records to take into account the wave propagation in soil and its multi-support excitation effect. The soil has been modeled by nonlinear springs in longitudinal, lateral, and vertical directions. A relatively long segment of the pipeline has been considered for the study and the effect of end conditions has been investigated by assuming different kinds end supports for the segment. After studying the corroded pipeline, a remedy has been considered for the seismic retrofit of corroded pipe by using a kind of Fiber Reinforced Polymers (FRP) cover. The analyses have been repeated for the retrofitted pipeline to realize the adequacy of FRP cover. Numerical results show that if the length of the pipeline segment is large enough, comparing to the wave length of shear wave in the soil, the end conditions do not have any major effect on the maximum stress and strain values in the pipe. Results also show that corrosion can lead to the increase in plastic strain values in the pipe up to 4 times in the case of overall corrosion and up to 20 times in the case of local corrosion. The satisfactory effect of using FRP cover is also shown by the analyses results, which confirm the decrease of strain values to 1/3.

  2. In situ synchrotron X-ray diffraction study of the effect of microstructure and boundary layer conditions on CO2 corrosion of pipeline steels

    International Nuclear Information System (INIS)

    Ko, M.; Ingham, B.; Laycock, N.; Williams, D.E.

    2015-01-01

    Highlights: • We studied the effects of steel microstructures and local conditions on CO 2 corrosion. • Microstructure influences the development of surface roughness during corrosion. • The effects of Cr alloying, on average, dominate over the effects of microstructure. • Spatial segregation of Cr between the phases in the steel may result in localised corrosion. - Abstract: This study demonstrates that the nucleation of crystalline scales of siderite and chukanovite onto the surface of low-alloy steels under CO 2 corrosion at elevated temperature is critically dependent on initial surface roughness, on microstructure-related surface roughness developed during corrosion, and on stirring in the solution. This study confirms that effects due to chromium micro-alloying in the steel are extremely important for siderite nucleation. On average, these effects dominate over the effects of microstructure. However, spatial variation of the corrosion deposit thickness indicates an interdependence between microstructure and chromium-enhanced siderite nucleation with the possibility of localised corrosion developing as a result

  3. Corrosion technology. V. 1

    International Nuclear Information System (INIS)

    Khan, I.H.

    1989-01-01

    This book has been produced for dissemination of information on corrosion technology, corrosion hazards and its control. Chapter one of this book presents an overall view of the subject and chapter 2-5 deals with electrochemical basics, types of corrosion, pourbaix diagrams and form of corrosion. The author explains polarization/kinetics of corrosion, passivity, aqueous corrosion and corrosion testing and monitoring in 6-11 chapters. The author hopes it will provide incentive to all those interested in the corrosion technology. (A.B.)

  4. Corrosion behaviour and biocorrosion of galvanized steel water distribution systems.

    Science.gov (United States)

    Delaunois, F; Tosar, F; Vitry, V

    2014-06-01

    Galvanized steel tubes are a popular mean for water distribution systems but suffer from corrosion despite their zinc or zinc alloy coatings. First, the quality of hot-dip galvanized (HDG) coatings was studied. Their microstructure, defects, and common types of corrosion were observed. It was shown that many manufactured tubes do not reach European standard (NBN EN 10240), which is the cause of several corrosion problems. The average thickness of zinc layer was found at 41μm against 55μm prescribed by the European standard. However, lack of quality, together with the usual corrosion types known for HDG steel tubes was not sufficient to explain the high corrosion rate (reaching 20μm per year versus 10μm/y for common corrosion types). Electrochemical tests were also performed to understand the corrosion behaviours occurring in galvanized steel tubes. Results have shown that the limiting step was oxygen diffusion, favouring the growth of anaerobic bacteria in steel tubes. EDS analysis was carried out on corroded coatings and has shown the presence of sulphur inside deposits, suggesting the likely bacterial activity. Therefore biocorrosion effects have been investigated. Actually sulphate reducing bacteria (SRB) can reduce sulphate contained in water to hydrogen sulphide (H2S), causing the formation of metal sulphides. Although microbial corrosion is well-known in sea water, it is less investigated in supply water. Thus, an experimental water main was kept in operation for 6months. SRB were detected by BART tests in the test water main. Copyright © 2014 Elsevier B.V. All rights reserved.

  5. The application of neutron reflectometry and atomic force microscopy in the study of corrosion inhibitor films

    International Nuclear Information System (INIS)

    John, Douglas; Blom, Annabelle; Bailey, Stuart; Nelson, Andrew; Schulz, Jamie; De Marco, Roland; Kinsella, Brian

    2006-01-01

    Corrosion inhibitor molecules function by adsorbing to a steel surface and thus prevent oxidation of the metal. The interfacial structures formed by a range of corrosion inhibitor molecules have been investigated by in situ measurements based on atomic force microscopy and neutron reflectometry. Inhibitors investigated include molecules cetyl pyridinium chloride (CPC), dodecyl pyridinium chloride (DPC), 1-hydroxyethyl-2-oleic imidazoline (OHEI) and cetyl dimethyl benzyl ammonium chloride (CDMBAC). This has shown that the inhibitor molecules adsorb onto a surface in micellar structures. Corrosion measurements confirmed that maximum inhibition efficiency coincides with the solution critical micelle concentration

  6. Corrosion monitoring along infrastructures using distributed fiber optic sensing

    Science.gov (United States)

    Alhandawi, Khalil B.; Vahdati, Nader; Shiryayev, Oleg; Lawand, Lydia

    2016-04-01

    Pipeline Inspection Gauges (PIGs) are used for internal corrosion inspection of oil pipelines every 3-5 years. However, between inspection intervals, rapid corrosion may occur, potentially resulting in major accidents. The motivation behind this research project was to develop a safe distributed corrosion sensor placed inside oil pipelines continuously monitoring corrosion. The intrinsically safe nature of light provided motivation for researching fiber optic sensors as a solution. The sensing fiber's cladding features polymer plastic that is chemically sensitive to hydrocarbons within crude oil mixtures. A layer of metal, used in the oil pipeline's construction, is deposited on the polymer cladding, which upon corrosion, exposes the cladding to surrounding hydrocarbons. The hydrocarbon's interaction with the cladding locally increases the cladding's refractive index in the radial direction. Light intensity of a traveling pulse is reduced due to local reduction in the modal capacity which is interrogated by Optical Time Domain Reflectometery. Backscattered light is captured in real-time while using time delay to resolve location, allowing real-time spatial monitoring of environmental internal corrosion within pipelines spanning large distances. Step index theoretical solutions were used to calculate the power loss due changes in the intensity profile. The power loss is translated into an attenuation coefficient characterizing the expected OTDR trace which was verified against similar experimental results from the literature. A laboratory scale experiment is being developed to assess the validity of the model and the practicality of the solution.

  7. Steel corrosion in radioactive waste storage tanks

    International Nuclear Information System (INIS)

    Carranza, Ricardo M.; Giordano, Celia M.; Saenz, E.; Weier, Dennis R.

    2004-01-01

    A collaborative study is being conducted by CNEA and USDOE (Department of Energy of the United States of America) to investigate the effects of tank waste chemistry on radioactive waste storage tank corrosion. Radioactive waste is stored in underground storage tanks that contain a combination of salts, consisting primarily of sodium nitrate, sodium nitrite and sodium hydroxide. The USDOE, Office of River Protection at the Hanford Site, has identified a need to conduct a laboratory study to better understand the effects of radioactive waste chemistry on the corrosion of waste storage tanks at the Hanford Site. The USDOE science need (RL-WT079-S Double-Shell Tanks Corrosion Chemistry) called for a multi year effort to identify waste chemistries and temperatures within the double-shell tank (DST) operating limits for corrosion control and operating temperature range that may not provide the expected corrosion protection and to evaluate future operations for the conditions outside the existing corrosion database. Assessment of corrosion damage using simulated (non-radioactive) waste is being made of the double-shell tank wall carbon steel alloy. Evaluation of the influence of exposure time, and electrolyte composition and/or concentration is being also conducted. (author) [es

  8. Mechanical Properties and Corrosion Characteristics of Thermally Aged Alloy 22

    International Nuclear Information System (INIS)

    Rebak, R B; Crook, P

    2002-01-01

    Alloy 22 (UNS N06022) is a candidate material for the external wall of the high level nuclear waste containers for the potential repository site at Yucca Mountain. In the mill-annealed (MA) condition, Alloy 22 is a single face centered cubic phase. When exposed to temperatures on the order of 600 C and above for times higher than 1 h, this alloy may develop secondary phases that reduce its mechanical toughness and corrosion resistance. The objective of this work was to age Alloy 22 at temperatures between 482 C and 760 C for times between 0.25 h and 6,000 h and to study the mechanical and corrosion performance of the resulting material. Aging was carried out using wrought specimens as well as gas tungsten arc welded (GTAW) specimens. Mechanical and corrosion testing was carried out using ASTM standards. Results show-that the higher the aging temperature and the longer the aging time, the lower the impact toughness of the aged material and the lower its corrosion resistance. However, extrapolating both mechanical and corrosion laboratory data predicts that Alloy 22 will remain corrosion resistant and mechanically robust for the projected lifetime of the waste container

  9. Erosion and erosion-corrosion

    International Nuclear Information System (INIS)

    Isomoto, Yoshinori

    2008-01-01

    It is very difficult to interpret the technical term of erosion-corrosion' which is sometimes encountered in piping systems of power plants, because of complicated mechanisms and several confusing definitions of erosion-corrosion phenomena. 'FAC (flow accelerated corrosion)' is recently introduced as wall thinning of materials in power plant systems, as a representative of 'erosion-corrosion'. FAC is, however, not necessarily well understood and compared with erosion-corrosion. This paper describes firstly the origin, definition and fundamental understandings of erosion and erosion-corrosion, in order to reconsider and reconfirm the phenomena of erosion, erosion-corrosion and FAC. Next, typical mapping of erosion, corrosion, erosion-corrosion and FAC are introduced in flow velocity and environmental corrosiveness axes. The concept of damage rate in erosion-corrosion is finally discussed, connecting dissolution rate, mass transfer of metal ions in a metal oxide film and film growth. (author)

  10. The Research of Car-Following Model Based on Real-Time Maximum Deceleration

    Directory of Open Access Journals (Sweden)

    Longhai Yang

    2015-01-01

    Full Text Available This paper is concerned with the effect of real-time maximum deceleration in car-following. The real-time maximum acceleration is estimated with vehicle dynamics. It is known that an intelligent driver model (IDM can control adaptive cruise control (ACC well. The disadvantages of IDM at high and constant speed are analyzed. A new car-following model which is applied to ACC is established accordingly to modify the desired minimum gap and structure of the IDM. We simulated the new car-following model and IDM under two different kinds of road conditions. In the first, the vehicles drive on a single road, taking dry asphalt road as the example in this paper. In the second, vehicles drive onto a different road, and this paper analyzed the situation in which vehicles drive from a dry asphalt road onto an icy road. From the simulation, we found that the new car-following model can not only ensure driving security and comfort but also control the steady driving of the vehicle with a smaller time headway than IDM.

  11. The effect of heat treatments on the corrosion behavior of Zircaloy-4

    International Nuclear Information System (INIS)

    Zhou Bangxin; Zhao Wenjin; Miao Zhi; Pan Shufang; Li Cong; Jiang Yourong

    1996-06-01

    The effect of penultimate annealing temperature and cooling rate on the corrosion behavior of Zircaloy-4 cladding tube has been investigated. Both nodular corrosion and uniform corrosion resistance can be improved obviously after changing the heat treatment from the original annealing at 650 degree C to quenching from 830 degree C (upper temperature of alpha phase region or lower temperature of beta phase region). Although the nodular corrosion resistance can be improved obviously after quenching from beta phase, there was a second transition in the variation between weight gain and exposure time, which shows a poor uniform corrosion resistance after a long exposure time during the autoclave tests. The main factor of affecting corrosion behavior is the solid solution contents of Fe and Cr in alpha zirconium rather than the size of second phase particles. About 200 μg/g Fe and Cr super saturated solid solution in alpha zirconium could get good uniform and nodular corrosion resistance, but much more solid solution contents of Fe and Cr in alpha zirconium could bring about a trend toward poor uniform corrosion resistance for long-term exposure time. (14 refs., 10 figs., 1 tab.)

  12. Study of biofilm influenced corrosion on cast iron pipes in reclaimed water

    International Nuclear Information System (INIS)

    Zhang, Haiya; Tian, Yimei; Wan, Jianmei; Zhao, Peng

    2015-01-01

    Highlights: • Compared to sterile water, biofilm in reclaimed water promoted corrosion process significantly. • Corrosion rate was accelerated by the biofilm in the first 7 days but was inhibited afterwards. • There was an inverse correlation between the biofilm thickness and general corrosion rate. • Corrosion process was influenced by bacteria, EPS and corrosion products comprehensively. • The corrosion process can be divided into three different stages in our study. - Abstract: Biofilm influenced corrosion on cast iron pipes in reclaimed water was systemically studied using the weight loss method and electrochemical impedance spectroscopy (EIS). The results demonstrated that compared to sterile water, the existence of the biofilm in reclaimed water promoted the corrosion process significantly. The characteristics of biofilm on cast iron coupons were examined by the surface profiler, scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS). The bacterial counts in the biofilm were determined using the standard plate count method and the most probable number (MPN). The results demonstrated that the corrosion process was influenced by the settled bacteria, EPS, and corrosion products in the biofilm comprehensively. But, the corrosion mechanisms were different with respect to time and could be divided into three stages in our study. Furthermore, several corresponding corrosion mechanisms were proposed for different immersion times.

  13. Study of biofilm influenced corrosion on cast iron pipes in reclaimed water

    Energy Technology Data Exchange (ETDEWEB)

    Zhang, Haiya, E-mail: flying850612@126.com; Tian, Yimei, E-mail: ymtian_2000@126.com; Wan, Jianmei, E-mail: 563926510@qq.com; Zhao, Peng, E-mail: zhpeng@tju.edu.cn

    2015-12-01

    Highlights: • Compared to sterile water, biofilm in reclaimed water promoted corrosion process significantly. • Corrosion rate was accelerated by the biofilm in the first 7 days but was inhibited afterwards. • There was an inverse correlation between the biofilm thickness and general corrosion rate. • Corrosion process was influenced by bacteria, EPS and corrosion products comprehensively. • The corrosion process can be divided into three different stages in our study. - Abstract: Biofilm influenced corrosion on cast iron pipes in reclaimed water was systemically studied using the weight loss method and electrochemical impedance spectroscopy (EIS). The results demonstrated that compared to sterile water, the existence of the biofilm in reclaimed water promoted the corrosion process significantly. The characteristics of biofilm on cast iron coupons were examined by the surface profiler, scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS). The bacterial counts in the biofilm were determined using the standard plate count method and the most probable number (MPN). The results demonstrated that the corrosion process was influenced by the settled bacteria, EPS, and corrosion products in the biofilm comprehensively. But, the corrosion mechanisms were different with respect to time and could be divided into three stages in our study. Furthermore, several corresponding corrosion mechanisms were proposed for different immersion times.

  14. Electromagnetic modeling of stress corrosion cracks in Inconel welds

    International Nuclear Information System (INIS)

    Huang, Haoyu; Miya, Kenzo; Yusa, Noritaka; Hashizume, Hidetoshi; Sera, Takehiko; Hirano, Shinro

    2011-01-01

    This study evaluates suitable numerical modeling of stress corrosion cracks appearing in Inconel welds from the viewpoint of electromagnetic nondestructive evaluations. The stress corrosion cracks analyzed in this study are five artificial ones introduced into welded flat plate, and three natural ones found in a pressurized nuclear power plant. Numerical simulations model a crack as a planar region having a uniform conductivity inside and a constant width, and evaluate the width and conductivity that reproduce the maximum eddy current signals obtained by experiments. The results obtained validate the existence of the minimum value of the equivalent resistance, which is defined by the width divided by conductivity. In contrast, the values of the width and conductivity themselves vary across a wide range. The results also lead to a discussion about (1) the effect of probe utilized on the numerical model, (2) the difference between artificial and natural stress corrosion cracks, and (3) the difference between stress corrosion cracks in base metals and those in Inconel welds in their models. Electromagnetic characteristics of four different Inconel weld alloys are additionally evaluated using a resistance tester and a vibrating sample magnetometer to support the validity of the numerical modeling and the generality of results obtained. (author)

  15. Corrosion behavior of stainless steel and zirconium in nitric acid containing highly oxidizing species

    International Nuclear Information System (INIS)

    Mayuzumi, Masami; Fujita, Tomonari

    1994-01-01

    Corrosion behavior of 304ELC, 310Nb stainless steels and Zirconium was investigated in the simulated dissolver solution of a reprocessing plant to obtain fundamental data for life prediction. Corrosion of heat transfer surface was also investigated in nitric acid solutions containing Ce ion. The results obtained are as follows: (1) Stainless steels showed intergranular corrosion in the simulated dissolver solution. The corrosion rate increased with time and reached to a constant value after several hundred hours of immersing time. The constant corrosion rate changed depending on potential suggesting that corrosion potential dominates the corrosion process. 310Nb showed superior corrosion resistance to 304ELC. (2) Corrosion rate of stainless steels increased in the heat transfer condition. The causes of corrosion enhancement are estimated to be higher corrosion potential and higher temperature of heat transfer surface. (3) Zirconium showed perfect passivity in all the test conditions employed. (author)

  16. Modeling flow-accelerated corrosion in CANDU

    International Nuclear Information System (INIS)

    Burrill, K.A.

    1995-11-01

    Flow-accelerated corrosion (FAC) of large areas of carbon steel in various circuits of CANDU plants generates significant quantities of corrosion products. As well, the relatively rapid corrosion rate can lead to operating difficulties with some components. Three areas in the plant are identified and a simple model of mass-transfer controlled corrosion of the carbon steel is derived and applied to these areas. The areas and the significant finding for each are given below: A number of lines in the feedwater system generate sludge by FAC, which causes steam generator fouling. Prediction of the steady-state iron concentration at the feedtrain outlet compares well with measured values. Carbon steel outlet feeders connect the reactor core with the steam generators. The feeder surface provides the dissolved iron through FAC, which fouls the primary side of the steam generator tubes, and can lead to derating of the plant and difficulty in tube inspection. Segmented carbon steel divider plates in the steam generator primary head leak at an increasing rate with time. The leakage rate is strongly dependent on the tightness of the overlapping joints. which undergo FAC at an increasing rate with time. (author) 7 refs., 5 tabs., 6 figs

  17. Oxide induced corrosion on the welded stainless steels SS 2352 and 2353

    International Nuclear Information System (INIS)

    Stroem, S.; Li Huiqin.

    1991-01-01

    The pitting corrosion properties have been investigated in welded and unwelded condition by polarization tests in sodium chloride solutions. The two steels were TIG welded without adding welding material and as shielding on the bottom side argon gas containing 2, 26 or 99 ppm oxygen was used. In some tests low breakthrough potentials were received, without discovering any pitting corrosion in the specimen surfaces. The unwelded SS 2352 steel had a critical (lowest) pitting temperature (CPT) of 5 degrees C in the more concentrated solution. For the same steel with weld pitting corrosion was obtained at 5 degrees C, which was the lowest temperature for the tests. Thus the CPT value was lower than 5 degrees C, but by looking at the pitting corrosion potentials the following conclusion could be drawn: Welding with higher oxygen content in the shielding gas implied lower pitting corrosion resistance. For the SS 2353 steel the CPT values were 25 and 27.5 degrees C for material without weld, in contact with the more concentrated and the more dilute solution respectively. Welded material was all through more sensitive to pitting corrosion, and the CPT values were 15-17.5, 15 and 5-10 degrees C for welded areas which had been gas shielded with argon containing 2, 26 and 99 ppm oxygen respectively. The result thus showed that welding with shielding gas containing maximum about 30 ppm oxygen does not substantially affect the pitting corrosion properties. Post treatment of the welding areas increased the pitting corrosion resistance. Acid pickling implied the highest pitting corrosion resistance with 15 degrees C as CPT value for the 2353 steel in the more concentrated solution. Steel brushing implied an obvious increase to the pitting corrosion resistance compared to untreated weld areas and the same statement could be done for sand blasted surfaces. (10 refs., 16 tabs., 11 figs.)

  18. Accelerated Corrosion Testing

    Science.gov (United States)

    1982-12-01

    Treaty Organization, Brussels, 1971), p. 449. 14. D. 0. Sprowls, T. J. Summerson, G. M. Ugianski, S. G. Epstein, and H. L. Craig , Jr., in Stress...National Association of Corrosion Engineers Houston, TX, 1972). 22. H. L. Craig , Jr. (ed.), Stress Corrosion-New Approaches, ASTM-STP- 610 (American...62. M. Hishida and H. Nakada, Corrosion 33 (11) 403 (1977). b3. D. C. Deegan and B. E. Wilde, Corrosion 34 (6), 19 (1978). 64. S. Orman, Corrosion Sci

  19. Time averaging procedure for calculating the mass and energy transfer rates in adiabatic two phase flow

    International Nuclear Information System (INIS)

    Boccaccini, L.V.

    1986-07-01

    To take advantages of the semi-implicit computer models - to solve the two phase flow differential system - a proper averaging procedure is also needed for the source terms. In fact, in some cases, the correlations normally used for the source terms - not time averaged - fail using the theoretical time step that arises from the linear stability analysis used on the right handside. Such a time averaging procedure is developed with reference to the bubbly flow regime. Moreover, the concept of mass that must be exchanged to reach equilibrium from a non-equilibrium state is introduced to limit the mass transfer during a time step. Finally some practical calculations are performed to compare the different correlations for the average mass transfer rate developed in this work. (orig.) [de

  20. Statistical evaluation of unobserved nonuniform corrosion in A216 steel

    International Nuclear Information System (INIS)

    Pulsipher, B.A.

    1988-07-01

    Tests designed to promote nonuniform corrosion have been conducted at PNL on A216 steel. In all of the tests performed to date, there have been no manifestations of significant nonuniform corrosion. Although this may suggest that nonuniform corrosion in A216 steel may not be a significant problem in the nuclear waste repository, a question arises as to whether enough tests have been conducted for a sufficient length of time to rule out nonuniform corrosion of A216 steel. In this report, a method for determining the required number of tests is examined for two of the mechanisms of nonuniform corrosion: pitting and crevice corrosion

  1. MATHEMATICAL MODELING AND NUMERICAL SOLUTION OF IRON CORROSION PROBLEM BASED ON CONDENSATION CHEMICAL PROPERTIES

    Directory of Open Access Journals (Sweden)

    Basuki Widodo

    2012-02-01

    Full Text Available Corrosion process is a natural case that happened at the various metals, where the corrosion process in electrochemical can be explained by using galvanic cell. The iron corrosion process is based on the acidity degree (pH of a condensation, iron concentration and condensation temperature of electrolyte. Those are applied at electrochemistry cell. The iron corrosion process at this electrochemical cell also able to generate electrical potential and electric current during the process takes place. This paper considers how to build a mathematical model of iron corrosion, electrical potential and electric current. The mathematical model further is solved using the finite element method. This iron corrosion model is built based on the iron concentration, condensation temperature, and iteration time applied. In the electric current density model, the current based on electric current that is happened at cathode and anode pole and the iteration time applied. Whereas on the potential  electric model, it is based on the beginning of electric potential and the iteration time applied. The numerical results show that the part of iron metal, that is gristle caused by corrosion, is the part of metal that has function as anode and it has some influences, such as time depth difference, iron concentration and condensation temperature on the iron corrosion process and the sum of reduced mass during corrosion process. Moreover, difference influence of time and beginning electric potential has an effect on the electric potential, which emerges during corrosion process at the electrochemical cell. Whereas, at the electrical current is also influenced by difference of depth time and condensation temperature applied.Keywords: Iron Corrosion, Concentration of iron, Electrochemical Cell and Finite Element Method

  2. Latitudinal Change of Tropical Cyclone Maximum Intensity in the Western North Pacific

    Directory of Open Access Journals (Sweden)

    Jae-Won Choi

    2016-01-01

    Full Text Available This study obtained the latitude where tropical cyclones (TCs show maximum intensity and applied statistical change-point analysis on the time series data of the average annual values. The analysis results found that the latitude of the TC maximum intensity increased from 1999. To investigate the reason behind this phenomenon, the difference of the average latitude between 1999 and 2013 and the average between 1977 and 1998 was analyzed. In a difference of 500 hPa streamline between the two periods, anomalous anticyclonic circulations were strong in 30°–50°N, while anomalous monsoon trough was located in the north of South China Sea. This anomalous monsoon trough was extended eastward to 145°E. Middle-latitude region in East Asia is affected by the anomalous southeasterlies due to these anomalous anticyclonic circulations and anomalous monsoon trough. These anomalous southeasterlies play a role of anomalous steering flows that make the TCs heading toward region in East Asia middle latitude. As a result, TCs during 1999–2013 had higher latitude of the maximum intensity compared to the TCs during 1977–1998.

  3. Comparative analysis of adsorption and corrosion inhibitive properties of ethanol extract of Dialium Guineense leaves for mild steel in 0.5 M HCl

    Directory of Open Access Journals (Sweden)

    Shola Elijah Adeniji

    2018-05-01

    Full Text Available Adsorption and corrosion inhibitive properties of ethanol extract of Dialium guineense leaves for mild steel in 0.5M HCl was studied using the gravimetric method. The results showed that the ethanol extract of Dialium guineense leaves is a good corrosion inhibitor for mild steel in 0.5 M HCl. The inhibition efficiency was found to increase with increase in the concentration of ethanol extract of Dialium guineense leaves up to the maximum of 92 %, but at the same time it decreased as the temperature was increased. Corrosion inhibition by the extract of Dialium guineense leaves is carried out by adsorption mechanism with the kinetics of corrosion following the pseudo first order reaction with high correlation. Thermodynamic consideration revealed that adsorption of the ethanol extract of Dialium guineense leaves on mild steel surface is an exothermic and spontaneous process that fitted the Langmuir adsorption isotherm. The values of activation energy and Gibb’s free energy were found within the range of limits expected for the mechanism of physical adsorption.

  4. Scoping calculation of nuclides migration in engineering barrier system for effect of volume expansion due to overpack corrosion and intrusion of the buffer material

    International Nuclear Information System (INIS)

    Yoshita, Takashi; Ishihara, Yoshinao; Ishiguro, Katsuhiko; Ohi, Takao; Nakajima, Kunihiko

    1999-11-01

    Corrosion of the carbon steel overpack leads to a volume expansion since the specific gravity of corrosion products is smaller than carbon steel. The buffer material is compressed due to the corrosive swelling, reducing its thickness and porosity. On the other hand, buffer material may be extruded into fractures of the surrounding rock and this may lead to a deterioration of the planned functions of the buffer, including retardation of nuclides migration and colloid filtration. In this study, the sensitivity analyses for the effect of volume expansion and intrusion of the buffer material on nuclide migration in the engineering barrier system are carried out. The sensitivity analyses were performed on the decrease in the thickness of the buffer material in the radial direction caused by the corrosive swelling, and the change in the porosity and dry density of the buffer caused by both compacting due to corrosive swelling and intrusion of buffer material. As results, it was found the maximum release rates of relatively shorter half-life nuclides from the outside of the buffer material decreased for taking into account of a volume expansion due to overpack corrosion. On the other hand, the maximum release rates increased when the intrusion of buffer material was also taking into account. It was, however, the maximum release rates of longer half-life nuclides, such as Cs-137 and Np-237, were insensitive to the change of buffer material thickness, and porosity and dry density of buffer. (author)

  5. Characterisation of corrosion products on pipeline steel under cathodic protection

    Energy Technology Data Exchange (ETDEWEB)

    Lanarde, Lise [Gaz de France Research and Development Division, 361 avenue du President Wilson, BP33, 93211 Saint Denis La Plaine (France)]|[UPR15 du CNRS, Laboratoire des Interfaces et Systemes Electrochimiques, Universite Pierre et Marie Curie, C.P. 133, 4 Place Jussieu, 75252 Paris Cedex 05 (France); Campaignolle, Xavier; Karcher, Sebastien; Meyer, Michel [Gaz de France Research and Development Division, 361 avenue du President Wilson, BP33, 93211 Saint Denis La Plaine (France); Joiret, Suzanne [UPR15 du CNRS, Laboratoire des Interfaces et Systemes Electrochimiques, Universite Pierre et Marie Curie, C.P. 133, 4 Place Jussieu 75252 Paris Cedex 05 (France)

    2004-07-01

    Onshore gas transmission lines are conjointly protected against external corrosion by cathodic protection (CP) and organic coatings. If both protection systems are simultaneously faulty, the pipe may be subjected to local loss of protection criteria. Consequently, the development of a corrosion due to the ground intrinsic corrosiveness may occur. To guarantee an optimal and safe use of its 31000 km buried gas transmission network, Gaz de France regularly inspects its pipelines. When indications of metal damage are suspected, excavations are realized to carry out a finer diagnosis and, if necessary, to repair. Whenever, corrosions are encountered, although it occurs very scarcely, it is necessary to evaluate its degree of gravity: activity, mechanism, and kinetics. Among corrosion defects, it is indeed essential to differentiate those active, from those older inactive at the time of excavation, since those last ones may possibly have been annihilated, by a PC reinforcement for instance. Eventually, the identification of the corrosion mechanism and its associated rate will provide an assessment of the risks encountered by other sections of the pipeline similar to that excavated. This study investigates to what extent the degree of gravity (activity, kinetics) of a corrosion can be determined by the characterization and identification of its associated corrosion products. Moreover, it will attempt to relate it to the close environment features as well as to the operating conditions of the pipe. The preliminary results presented in this paper consist in a laboratory study of the time evolution of corrosion products formed on the surface of ordinary low carbon steel samples. The specimens have been previously subjected to various polarization conditions in various aqueous media. The selected solutions are characteristic of ground waters. The main parameters considered for the definition of the media were its initial chemical composition, pH and dissolved gas composition

  6. [Travel time and distances to Norwegian out-of-hours casualty clinics].

    Science.gov (United States)

    Raknes, Guttorm; Morken, Tone; Hunskår, Steinar

    2014-11-01

    Geographical factors have an impact on the utilisation of out-of-hours services. In this study we have investigated the travel distance to out-of-hours casualty clinics in Norwegian municipalities in 2011 and the number of municipalities covered by the proposed recommendations for secondary on-call arrangements due to long distances. We estimated the average maximum travel times and distances in Norwegian municipalities using a postcode-based method. Separate analyses were performed for municipalities with a single, permanently located casualty clinic. Altogether 417 out of 430 municipalities were included. We present the median value of the maximum travel times and distances for the included municipalities. The median maximum average travel distance for the municipalities was 19 km. The median maximum average travel time was 22 minutes. In 40 of the municipalities (10 %) the median maximum average travel time exceeded 60 minutes, and in 97 municipalities (23 %) the median maximum average travel time exceeded 40 minutes. The population of these groups comprised 2 % and 5 % of the country's total population respectively. For municipalities with permanent emergency facilities(N = 316), the median average flight time 16 minutes and median average distance 13 km.. In many municipalities, the inhabitants have a long average journey to out-of-hours emergency health services, but seen as a whole, the inhabitants of these municipalities account for a very small proportion of the Norwegian population. The results indicate that the proposed recommendations for secondary on-call duty based on long distances apply to only a small number of inhabitants. The recommendations should therefore be adjusted and reformulated to become more relevant.

  7. A theory of timing in scintillation counters based on maximum likelihood estimation

    International Nuclear Information System (INIS)

    Tomitani, Takehiro

    1982-01-01

    A theory of timing in scintillation counters based on the maximum likelihood estimation is presented. An optimum filter that minimizes the variance of timing is described. A simple formula to estimate the variance of timing is presented as a function of photoelectron number, scintillation decay constant and the single electron transit time spread in the photomultiplier. The present method was compared with the theory by E. Gatti and V. Svelto. The proposed method was applied to two simple models and rough estimations of potential time resolution of several scintillators are given. The proposed method is applicable to the timing in Cerenkov counters and semiconductor detectors as well. (author)

  8. Humid-air and aqueous corrosion models for corrosion-allowance barrier material

    International Nuclear Information System (INIS)

    Lee, J.H.; Atkins, J.E.; Andrews, R.W.

    1995-01-01

    Humid-air and aqueous general and pitting corrosion models (including their uncertainties) for the carbon steel outer containment barrier were developed using the corrosion data from literature for a suite of cast irons and carbon steels which have similar corrosion behaviors to the outer barrier material. The corrosion data include the potential effects of various chemical species present in the testing environments. The atmospheric corrosion data also embed any effects of cyclic wetting and drying and salts that may form on the corroding specimen surface. The humid-air and aqueous general corrosion models are consistent in that the predicted humid-air general corrosion rates at relative humidities between 85 and 100% RH are close to the predicted aqueous general corrosion rates. Using the expected values of the model parameters, the model predicts that aqueous pitting corrosion is the most likely failure mode for the carbon steel outer barrier, and an earliest failure (or initial pit penetration) of the 100-mm thick barrier may occur as early as about 500 years if it is exposed continuously to an aqueous condition at between 60 and 70 degrees C

  9. Reactive-transport model for the prediction of the uniform corrosion behaviour of copper used fuel containers

    International Nuclear Information System (INIS)

    King, F.; Kolar, M.; Maak, P.

    2008-01-01

    Used fuel containers in a deep geological repository will be subject to various forms of corrosion. For containers made from oxygen-free, phosphorus-doped copper, the most likely corrosion processes are uniform corrosion, underdeposit corrosion, stress corrosion cracking, and microbiologically influenced corrosion. The environmental conditions within the repository are expected to evolve with time, changing from warm and oxidizing initially to cool and anoxic in the long-term. In response, the corrosion behaviour of the containers will also change with time as the repository environment evolve. A reactive-transport model has been developed to predict the time-dependent uniform corrosion behaviour of the container. The model is based on an experimentally-based reaction scheme that accounts for the various chemical, microbiological, electrochemical, precipitation/dissolution, adsorption/desorption, redox, and mass-transport processes at the container surface and in the compacted bentonite-based sealing materials within the repository. Coupling of the electrochemical interfacial reactions with processes in the bentonite buffer material allows the effect of the evolution of the repository environment on the corrosion behaviour of the container to be taken into account. The Copper Corrosion Model for Uniform Corrosion predicts the time-dependent corrosion rate and corrosion potential of the container, as well as the evolution of the near-field environment

  10. Averaged multivalued solutions and time discretization for conservation laws

    International Nuclear Information System (INIS)

    Brenier, Y.

    1985-01-01

    It is noted that the correct shock solutions can be approximated by averaging in some sense the multivalued solution given by the method of characteristics for the nonlinear scalar conservation law (NSCL). A time discretization for the NSCL equation based on this principle is considered. An equivalent analytical formulation is shown to lead quite easily to a convergence result, and a third formulation is introduced which can be generalized for the systems of conservation laws. Various numerical schemes are constructed from the proposed time discretization. The first family of schemes is obtained by using a spatial grid and projecting the results of the time discretization. Many known schemes are then recognized (mainly schemes by Osher, Roe, and LeVeque). A second way to discretize leads to a particle scheme without space grid, which is very efficient (at least in the scalar case). Finally, a close relationship between the proposed method and the Boltzmann type schemes is established. 14 references

  11. Effect of surface treatment on the corrosion properties of magnesium-based fibre metal laminate

    Science.gov (United States)

    Zhang, X.; Zhang, Y.; Ma, Q. Y.; Dai, Y.; Hu, F. P.; Wei, G. B.; Xu, T. C.; Zeng, Q. W.; Wang, S. Z.; Xie, W. D.

    2017-02-01

    The surface roughness, weight of phosphating film and wettability of magnesium alloy substrates after abrasion and phosphating treatment were investigated in this work. The interfacial bonding and corrosion properties of a magnesium-based fibre metal laminate (MgFML) were analysed. The results showed that the wettability of the magnesium alloy was greatly influenced by the surface roughness, and the rough surface possessed a larger surface energy and better wettability. The surface energy and wettability of the magnesium alloy were significantly improved by the phosphating treatment. After phosphating for 5 min, a phosphating film with a double-layer structure was formed on the magnesium substrate, and the weight of the phosphating film and the surface energy reached their maximum values. The surface energies of the phosphated substrate after abrasion with #120 and #3000 grit abrasive papers were 84.31 mJ/m2 and 83.65 mJ/m2, respectively. The wettability of the phosphated magnesium was significantly better than the abraded magnesium. The phosphated AZ31B sheet had a better corrosion resistance than the abraded AZ31B sheet within short times. The corrosion resistance of the magnesium alloy was greatly increased by being composited with glass fibre/epoxy prepregs.

  12. Corrosion of thin, magnetron sputtered Nb_2O_5 films

    International Nuclear Information System (INIS)

    Pillis, Marina Fuser; Geribola, Guilherme Altomari; Scheidt, Guilherme; Gonçalves de Araújo, Edval; Lopes de Oliveira, Mara Cristina; Antunes, Renato Altobelli

    2016-01-01

    Highlights: • Niobium oxide based films were obtained by DC magnetron sputtering. • Different deposition times were tested. • The best corrosion resistance was obtained for the Nb_2O_5 film produced at 15′. • Film porosity determines the corrosion resistance. - Abstract: Niobium oxide based thin films were deposited on AISI 316 stainless steel substrates using reactive DC magnetron sputtering. Structure, composition and corrosion resistance of the niobium oxide films were studied. The corrosion behavior of the specimens was evaluated by electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization. The concentration of niobium and oxygen in the films was obtained by Rutherford backscattering spectroscopy (RBS). The film structure was analyzed by X-ray diffractometry. The corrosion resistance of the substrate was improved by the Nb_2O_5 layers. The best protective performance was achieved for the deposition time of 15 min.

  13. Microstructure and mechanical properties of friction welded AISI 1040/AISI 304L steels before and after electrochemical corrosion

    Energy Technology Data Exchange (ETDEWEB)

    Sarsilmaz, Furkan [Firat Univ., Elazig (Turkey). Dept. of Mechatronics Engineering; Kirik, Ihsan [Batman Univ. (Turkey); Ozdemir, Niyazi [Firat Univ., Elazig (Turkey)

    2018-03-01

    The aim of the present study is to investigate the effect of welding parameters both on the electrochemical corrosion behavior and tensile strength of pre- and post-electrochemical corrosion of friction welded dissimilar steels. The microstructural changes of AISI 1040/AISI 304L friction welded couples and also parent materials were analyzed by using scanning electron microscopy. The electrochemical behaviors of AISI1040/AISI304L joints were comparatively investigated by potentiodynamic polarization curve test and by electrochemical impedance spectra. Moreover, tensile strength experiments were carried out determining the behavior of friction welded joints of pre- and post-electrochemical corrosion and results indicated that the maximum tensile test value of the dissimilar welded pre-electrochemical corrosion was higher than those of post-electrochemical corrosion and was also very close to AISI 1040 parent material value.

  14. Vehicle accelerated corrosion test procedures for automotive in Malaysia

    Directory of Open Access Journals (Sweden)

    Anuar Liza

    2017-01-01

    Full Text Available An accelerated corrosion test, known as proving ground accelerated test, is commonly performed by automotive manufacturers to evaluate the corrosion performance of a vehicle. The test combines corrosion and durability inputs to detect potential failures that may occur during in-service conditions. Currently, the test is conducted at an external test center overseas. Such test is aimed to simulate the effects of one year accelerated corrosion in severe corrosive environment of the north-east and south east of America. However, the test results obtained do not correlate with the actual corrosion conditions observed in the Malaysian market, which is likely attributed to the different test environment of the tropical climate of vehicles in service. Therefore, a vehicle accelerated corrosion test procedure that suits the Malaysian market is proposed and benchmarked with other global car manufacturers that have their own dedicated corrosion test procedure. In the present work, a test track is used as the corrosion test ground and consists of various types of roads for structural durability exposures. Corrosion related facilities like salt trough, mud trough and gravel road are constructed as addition to the existing facilities. The establishment of accelerated corrosion test facilities has contributed to the development of initial accelerated corrosion test procedure for the national car manufacturer. The corrosion exposure is monitored by fitting test coupons at the underbody of test vehicle using mass loss technique so that the desired corrosion rate capable of simulating the real time corrosion effects for its target market.

  15. Corrosion testing of uranium silicide fuel specimens

    Energy Technology Data Exchange (ETDEWEB)

    Bourns, W T

    1968-09-15

    U{sub 3}Si is the most promising high density natural uranium fuel for water-cooled power reactors. Power reactors fuelled with this material are expected to produce cheaper electricity than those fuelled with uranium dioxide. Corrosion tests in 300{sup o}C water preceded extensive in-reactor performance tests of fuel elements and bundles. Proper heat-treatment of U-3.9 wt% Si gives a U{sub 3}5i specimen which corrodes at less than 2 mg/cm{sup 2} h in 300{sup o}C water. This is an order of magnitude lower than the maximum corrosion rate tolerable in a water-cooled reactor. U{sub 3}Si in a defected unbonded Zircaloy-2 sheath showed only a slow uniform sheath expansion in 300{sup o}C water. All tests were done under isothermal conditions in an out-reactor loop. (author)

  16. Quantitative measures of corrosion and prevention: application to corrosion in agriculture

    NARCIS (Netherlands)

    Schouten, J.C.; Gellings, P.J.

    1987-01-01

    The corrosion protection factor (c.p.f.) and the corrosion condition (c.c.) are simple instruments for the study and evaluation of the contribution and efficiency of several methods of corrosion prevention and control. The application of c.p.f. and c.c. to corrosion and prevention in agriculture in

  17. Evaluation of corrosive behavior of SAE 5155 by corrosion environment

    International Nuclear Information System (INIS)

    An, Jae Pil; Park, Keyung Dong

    2005-01-01

    In this study, the influence of shot peening and corrosive condition for corrosion property was investigated on immersed in 3.5% NaCl, 10% HNO 3 + 3% HF, 6% FeCl 3 . The immersion test was performed on two kinds of specimen. The immersion periods was performed 30days. Corrosion potential, weight loss were investigated from experimental results. From test results, the effect of shot peening on the corrosion was evaluated

  18. Synergy effect of naphthenic acid corrosion and sulfur corrosion in crude oil distillation unit

    Science.gov (United States)

    Huang, B. S.; Yin, W. F.; Sang, D. H.; Jiang, Z. Y.

    2012-10-01

    The synergy effect of naphthenic acid corrosion and sulfur corrosion at high temperature in crude oil distillation unit was studied using Q235 carbon-manganese steel and 316 stainless steel. The corrosion of Q235 and 316 in corrosion media containing sulfur and/or naphthenic acid at 280 °C was investigated by weight loss, scanning electron microscope (SEM), EDS and X-ray diffractometer (XRD) analysis. The results showed that in corrosion media containing only sulfur, the corrosion rate of Q235 and 316 first increased and then decreased with the increase of sulfur content. In corrosion media containing naphthenic acid and sulfur, with the variations of acid value or sulfur content, the synergy effect of naphthenic acid corrosion and sulfur corrosion has a great influence on the corrosion rate of Q235 and 316. It was indicated that the sulfur accelerated naphthenic acid corrosion below a certain sulfur content but prevented naphthenic acid corrosion above that. The corrosion products on two steels after exposure to corrosion media were investigated. The stable Cr5S8 phases detected in the corrosion products film of 316 were considered as the reason why 316 has greater corrosion resistance to that of Q235.

  19. Effect of mixed alloy combinations on fretting corrosion performance of spinal screw and rod implants.

    Science.gov (United States)

    Mali, Sachin A; Singh, Vaneet; Gilbert, Jeremy L

    2017-07-01

    Spinal implants are made from a variety of materials to meet the unique mechanical demands of each application. However, the medical device community has raised concern about mixing dissimilar metals in an implant because of fear of inducing corrosion. There is a lack of systematic studies on the effects of mixing metals on performance of spinal implants, especially in fretting corrosion conditions. Hence, the goal was to determine whether mixing stainless steel (SS316L), titanium alloy (Ti6Al4V) and cobalt chromium (CoCrMo) alloy components in a spinal implant leads to any increased risk of corrosion degradation. Spinal constructs consisting of single assembly screw-connector-rod components were tested using a novel short-term cyclic fretting corrosion test method. A total of 17 alloy component combinations (comprised of SS316L, Ti6Al4V-anodized and CoCrMo alloy for rod, screws and connectors) were tested under three anatomic orientations. Spinal constructs having all SS316L were most susceptible to fretting-initiated crevice corrosion attack and showed higher average fretting currents (∼25 - 30 µA), whereas constructs containing all Ti6Al4V components were less susceptible to fretting corrosion with average fretting currents in the range of 1 - 6 µA. Mixed groups showed evidence of fretting corrosion but they were not as severe as all SS316L group. SEM results showed evidence of severe corrosion attack in constructs having SS316L components. There also did not appear to be any galvanic effects of combining alloys together. © 2016 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 105B: 1169-1177, 2017. © 2016 Wiley Periodicals, Inc.

  20. Degradation of aged plants by corrosion: 'Long cell action' in unresolved corrosion issues

    International Nuclear Information System (INIS)

    Saji, Genn

    2009-01-01

    In a series of previously published papers the author has identified that 'long cell action' corrosion plays a pivotal role in practically all unresolved corrosion issues for all types of nuclear power plants (e.g. PWR/VVER, BWR/RBMK and CANDU). Some of these unresolved issues are IGSCC, PWSCC, AOA and FAC (erosion-corrosion). In conventional corrosion science it is well established that 'long cell action' can seriously accelerate or suppress the local cell corrosion activities. Although long cell action is another fundamental mechanism of corrosion, especially in a 'soil corrosion' arena, potential involvement of this corrosion process has never been studied in nuclear and fossil power plants as far as the author has been able to establish. The author believes that the omission of this basic corrosion mechanism is the root cause of practically all un-resolved corrosion issues. In this paper, the author further elaborated on his assessment to other key corrosion issues, e.g. steam generator and turbine corrosion issues, while briefly summarizing previous discussions for completeness purposes, as well as introducing additional experimental and theoretical evidence of this basic corrosion mechanism. Due to the importance of this potential mechanism the author is calling for institutional review activities and further verification experiments in the form of a joint international project.

  1. Evaluation of Electrochemical Behavior of Nopal Extract (Opuntia Ficus- Indica as Possible Corrosion Inhibitor

    Directory of Open Access Journals (Sweden)

    Araceli Mandujano-Ruíz

    2017-11-01

    Full Text Available Corrosion is one of the main problems of degradation in components, tooling, equipment and even in structural applications, examples of this are the carbon steels. In the present work, the capacity of corrosion inhibition of a biodegradable organic extract from the Nopal plant (Opuntia ficus-indica, for the protection of carbon steel type AISI 1018 was studied adding 50% v/v of the Nopal extract (EN in a solution of H2SO4 (0.6 mol.l-1. Polarization Resistance (LPR and Electrochemical Impedance Spectroscopy (EIS techniques were used for the electrochemical evaluation at room temperature for 24 h in order to obtain corrosion rates (Vcorr and inhibition efficiency (IE. Metallographic examination was also carried out to register the surface damage by corrosion. The results showed a reduction of the Vcorr with a maximum IE value of about 84% by adding the organic- liquid extracted from Nopal.

  2. On the maximum-entropy/autoregressive modeling of time series

    Science.gov (United States)

    Chao, B. F.

    1984-01-01

    The autoregressive (AR) model of a random process is interpreted in the light of the Prony's relation which relates a complex conjugate pair of poles of the AR process in the z-plane (or the z domain) on the one hand, to the complex frequency of one complex harmonic function in the time domain on the other. Thus the AR model of a time series is one that models the time series as a linear combination of complex harmonic functions, which include pure sinusoids and real exponentials as special cases. An AR model is completely determined by its z-domain pole configuration. The maximum-entropy/autogressive (ME/AR) spectrum, defined on the unit circle of the z-plane (or the frequency domain), is nothing but a convenient, but ambiguous visual representation. It is asserted that the position and shape of a spectral peak is determined by the corresponding complex frequency, and the height of the spectral peak contains little information about the complex amplitude of the complex harmonic functions.

  3. The aluminum chemistry and corrosion in alkaline solutions

    International Nuclear Information System (INIS)

    Zhang Jinsuo; Klasky, Marc; Letellier, Bruce C.

    2009-01-01

    Aluminum-alkaline solution systems are very common in engineering applications including nuclear engineering. Consequently, a thorough knowledge of the chemistry of aluminum and susceptibility to corrosion in alkaline solutions is reviewed. The aluminum corrosion mechanism and corrosion rate are examined based on current experimental data. A review of the phase transitions with aging time and change of environment is also performed. Particular attention is given to effect of organic and inorganic ions. As an example, the effect of boron is examined in detail because of the application in nuclear reactor power systems. Methods on how to reduce the corrosion rate of aluminum in alkaline solutions are also highlighted

  4. Accelerated cyclic corrosion tests

    Directory of Open Access Journals (Sweden)

    Prošek T.

    2016-06-01

    Full Text Available Accelerated corrosion testing is indispensable for material selection, quality control and both initial and residual life time prediction for bare and painted metallic, polymeric, adhesive and other materials in atmospheric exposure conditions. The best known Neutral Salt Spray (NSS test provides unrealistic conditions and poor correlation to exposures in atmosphere. Modern cyclic accelerated corrosion tests include intermittent salt spray, wet and dry phases and eventually other technical phases. They are able to predict the material performance in service more correctly as documented on several examples. The use of NSS should thus be restricted for quality control.

  5. Corrosion rate of parent and weld materials of F82H and JPCA steels under LBE flow with active oxygen control at 450 and 500 deg. C

    International Nuclear Information System (INIS)

    Kikuchi, Kenji; Kamata, Kinya; Ono, Mikinori; Kitano, Teruaki; Hayashi, Kenichi; Oigawa, Hiroyuki

    2008-01-01

    Corrosion behavior of parent and weld materials of F82H and JPCA was studied in the circulating LBE loop under impinging flow. These are candidate materials for Japanese Accelerator Driven System (ADS) beam windows. Maximum temperatures were kept to 450 and 500 deg. C with 100 deg. C constant temperature difference. Main flow velocity was 0.4-0.6 m/s in every case. Oxygen concentration was controlled to 2-4 x 10 -5 mass% although there was one exception. Testing time durations were 500-3000 h. Round bar type specimens were put in the circular tube of the loop. An electron beam weld in the middle of specimens was also studied. Optical microscopy, electron microscopy, X-ray element analyses and X-ray diffraction were used to investigate corrosion in these materials. Consequently corrosion depth and stability of those oxide layers were characterized based on the analyses. For a long-term behavior a linear law is recommended to predict corrosion in the ADS target design

  6. ARMA-Based SEM When the Number of Time Points T Exceeds the Number of Cases N: Raw Data Maximum Likelihood.

    Science.gov (United States)

    Hamaker, Ellen L.; Dolan, Conor V.; Molenaar, Peter C. M.

    2003-01-01

    Demonstrated, through simulation, that stationary autoregressive moving average (ARMA) models may be fitted readily when T>N, using normal theory raw maximum likelihood structural equation modeling. Also provides some illustrations based on real data. (SLD)

  7. Source of non-arrhenius average relaxation time in glass-forming liquids

    DEFF Research Database (Denmark)

    Dyre, Jeppe

    1998-01-01

    then discuss a recently proposed model according to which the activation energy of the average relaxation time is determined by the work done in shoving aside the surrounding liquid to create space needed for a "flow event". In this model, which is based on the fact that intermolecular interactions...

  8. Corrosion Testing Facility

    Data.gov (United States)

    Federal Laboratory Consortium — The Corrosion Testing Facility is part of the Army Corrosion Office (ACO). It is a fully functional atmospheric exposure site, called the Corrosion Instrumented Test...

  9. On the time-averaging of ultrafine particle number size spectra in vehicular plumes

    Directory of Open Access Journals (Sweden)

    X. H. Yao

    2006-01-01

    Full Text Available Ultrafine vehicular particle (<100 nm number size distributions presented in the literature are mostly averages of long scan-time (~30 s or more spectra mainly due to the non-availability of commercial instruments that can measure particle distributions in the <10 nm to 100 nm range faster than 30 s even though individual researchers have built faster (1–2.5 s scanning instruments. With the introduction of the Engine Exhaust Particle Sizer (EEPS in 2004, high time-resolution (1 full 32-channel spectrum per second particle size distribution data become possible and allow atmospheric researchers to study the characteristics of ultrafine vehicular particles in rapidly and perhaps randomly varying high concentration environments such as roadside, on-road and tunnel. In this study, particle size distributions in these environments were found to vary as rapidly as one second frequently. This poses the question on the generality of using averages of long scan-time spectra for dynamic and/or mechanistic studies in rapidly and perhaps randomly varying high concentration environments. One-second EEPS data taken at roadside, on roads and in tunnels by a mobile platform are time-averaged to yield 5, 10, 30 and 120 s distributions to answer this question.

  10. Synergy effect of naphthenic acid corrosion and sulfur corrosion in crude oil distillation unit

    Energy Technology Data Exchange (ETDEWEB)

    Huang, B.S., E-mail: yinwenfeng2010@163.com [College of Materials Science and Engineering, Southwest Petroleum University, Sichuan, Chengdu, 610500 (China); Yin, W.F. [College of Mechatronic Engineering, Southwest Petroleum University, Sichuan, Chengdu, 610500 (China); Sang, D.H. [Sheng Li Construction Group International Engineering Department, Shandong, Dongying, 257000 (China); Jiang, Z.Y. [College of Materials Science and Engineering, Southwest Petroleum University, Sichuan, Chengdu, 610500 (China)

    2012-10-15

    Highlights: Black-Right-Pointing-Pointer The corrosion of a carbon-manganese steel and a stainless steel in sulfur and/or naphthenic acid media was investigated. Black-Right-Pointing-Pointer The corrosion rate of the carbon-manganese steel increased with the increase of the acid value and sulfur content. Black-Right-Pointing-Pointer The critical values of the concentration of sulfur and acid for corrosion rate of the stainless steel were ascertained respectively. Black-Right-Pointing-Pointer The stainless steel is superior to the carbon-manganese steel in corrosion resistance because of the presence of stable Cr{sub 5}S{sub 8} phases. - Abstract: The synergy effect of naphthenic acid corrosion and sulfur corrosion at high temperature in crude oil distillation unit was studied using Q235 carbon-manganese steel and 316 stainless steel. The corrosion of Q235 and 316 in corrosion media containing sulfur and/or naphthenic acid at 280 Degree-Sign C was investigated by weight loss, scanning electron microscope (SEM), EDS and X-ray diffractometer (XRD) analysis. The results showed that in corrosion media containing only sulfur, the corrosion rate of Q235 and 316 first increased and then decreased with the increase of sulfur content. In corrosion media containing naphthenic acid and sulfur, with the variations of acid value or sulfur content, the synergy effect of naphthenic acid corrosion and sulfur corrosion has a great influence on the corrosion rate of Q235 and 316. It was indicated that the sulfur accelerated naphthenic acid corrosion below a certain sulfur content but prevented naphthenic acid corrosion above that. The corrosion products on two steels after exposure to corrosion media were investigated. The stable Cr{sub 5}S{sub 8} phases detected in the corrosion products film of 316 were considered as the reason why 316 has greater corrosion resistance to that of Q235.

  11. PWR fuel rod corrosion in Japan

    International Nuclear Information System (INIS)

    Inoue, S.; Mori, K.; Murata, K.; Kobasyashi, S.

    1997-01-01

    Many particular appearance were observed on the fuel rod surfaces during fuel inspection at reactor outage in 1991. The appearances looked like small black circular nodules. The size was approximately 1 mm. This kind of appearances were found on fuel rods of which burnup exceeded approximately 30 GWd/t and at the second or third spans of the fuel assembly from the top. In order to clarify the cause, PIE was performed. The black nodules were confirmed to be oxide film spalling by visual inspection. Maximum oxide film thickness was 70 μm and spalling was observed where oxide thickness exceeded 40 t0 50 μm. Oxide film thickness was greater than expected. Many small pores were found in the oxide film when the oxide film had become thicker. Many circumferential cracks were also found in the film. It was speculated that these cracks caused the spalling of the oxide film. Hydride precipitates were mainly oriented circumferentially. Dense hydrides were observed near the outer rim of the cladding. No concentrated hydrides were observed near the spalling area. Maximum hydrogen content was 315 ppm. It was confirmed that the results of tensile test showed no significant effects by corrosion. The mechanism of accelerated corrosion was studied in detail. Water chemistry during irradiation was examined. Lithium content was maintained below 2.2 ppm. pH value was kept between 6.9 and 7.2. There was no anomalies in water chemistry during reactor operation. Cladding fabrication record clarified that heat treatment parameter was smaller than the optimum value. In Japan, heat treatment of the cladding was already optimized by improved fabrication process. Also chemical composition optimization of the cladding, such as low Tin and high Silicon content, was adopted for high burnup fuel. These remedies has already reduced fuel cladding corrosion and we believe we have solved this problem. (author). 6 figs, 1 tab

  12. PWR fuel rod corrosion in Japan

    Energy Technology Data Exchange (ETDEWEB)

    Inoue, S [Kansai Electric Power Co., Inc., Osaka (Japan); Mori, K; Murata, K; Kobasyashi, S [Nuclear Fuel Industries, Ltd, Osaka (Japan)

    1997-02-01

    Many particular appearance were observed on the fuel rod surfaces during fuel inspection at reactor outage in 1991. The appearances looked like small black circular nodules. The size was approximately 1 mm. This kind of appearances were found on fuel rods of which burnup exceeded approximately 30 GWd/t and at the second or third spans of the fuel assembly from the top. In order to clarify the cause, PIE was performed. The black nodules were confirmed to be oxide film spalling by visual inspection. Maximum oxide film thickness was 70 {mu}m and spalling was observed where oxide thickness exceeded 40 t0 50 {mu}m. Oxide film thickness was greater than expected. Many small pores were found in the oxide film when the oxide film had become thicker. Many circumferential cracks were also found in the film. It was speculated that these cracks caused the spalling of the oxide film. Hydride precipitates were mainly oriented circumferentially. Dense hydrides were observed near the outer rim of the cladding. No concentrated hydrides were observed near the spalling area. Maximum hydrogen content was 315 ppm. It was confirmed that the results of tensile test showed no significant effects by corrosion. The mechanism of accelerated corrosion was studied in detail. Water chemistry during irradiation was examined. Lithium content was maintained below 2.2 ppm. pH value was kept between 6.9 and 7.2. There was no anomalies in water chemistry during reactor operation. Cladding fabrication record clarified that heat treatment parameter was smaller than the optimum value. In Japan, heat treatment of the cladding was already optimized by improved fabrication process. Also chemical composition optimization of the cladding, such as low Tin and high Silicon content, was adopted for high burnup fuel. These remedies has already reduced fuel cladding corrosion and we believe we have solved this problem. (author). 6 figs, 1 tab.

  13. A review of fiber-optic corrosion sensor in civil engineering

    Science.gov (United States)

    Luo, Dong; Li, Junnan; Li, Yuanyuan

    2018-05-01

    Fiber-optical corrosion sensor (FOCS) is the research hotspot of corrosion monitoring sensor in recent years. It has the advantages of lightness, simplicity, anti-electromagnetic interference and distributed measurement, so it has an attractive application prospect. In this paper, the mechanism of metal corrosion is introduced. Several common methods for detecting optical fiber corrosion sensors are presented, and the latest progress of optical fiber corrosion sensors in recent years is described. We need to design a set of sensor devices that can directly monitor the corrosion of reinforcing steel bars directly, and propose a method of time dependent reliability assessment based on monitoring data, so as to form a complete research path.

  14. Synthesis and corrosion protection properties of poly(o-phenylenediamine nanofibers

    Directory of Open Access Journals (Sweden)

    P. Muthirulan

    2013-07-01

    Full Text Available The present study shows a novel method for the synthesis of uniformly-shaped poly(othophenylediamine (PoPD nanofibers by chemical oxidative polymerization method for application towards smart corrosion resistance coatings. Transmission Electron Microscopy (TEM and Scanning Electron Microscopy (SEM studies confirm morphology of PoPD with three dimensional (3D networked dendritic superstructures having average diameter of 50–70 nm and several hundred meters of length. UV–vis and FTIR spectral results shows the formation of PoPD nanofibers containing phenazine ring ladder-structure with benzenoid and quinoid imine units. Thermogravimetric analyses (TGA of PoPD nanofibers possess good thermal stability. The anti-corrosion behavior of PoPD nanofibers on 316L SS was investigated in 3.5% NaCl solution using potentiodynamic polarization and electrochemical impedance spectroscopic (EIS measurements. The PoPD coated 316L SS exhibits higher corrosion potential when compared to uncoated specimen. EIS studies, clearly ascertain that PoPD nanofiber coatings exhibits excellent potential barrier to protect the 316L SS against corrosion in 3.5% NaCl.

  15. Analysis of corrosion products of carbon steel in wet bentonite

    International Nuclear Information System (INIS)

    Osada, K.; Nagano, T.; Kozai, N.; Nakashima, S.; Nakayama, S.; Muraoka, S.

    1991-01-01

    The following conclusions were obtained; (1) At 40degC, the average corrosion rate of SS41 carbon steel in wet bentonite was 0.025 mm/y. This is smaller than the value of 0.042 mm/y obtained in pure water at 40degC. However, at 95degC, the corrosion rate of SS41 carbon steel in wet bentonite was 0.27 mm/y, which is much larger than that in pure water at 95degC. (2) At 95degC, γ-FeO(OH) (lepidocrocite) was formed only in wet bentonite, and it was absent in pure water. Evaporation of moisture resulted in the formation of partial covering of bentonite, which promoted local corrosion. Consequently, γ-FeO(OH) was considered to be formed. (3) In wet bentonite at 95degC, α-Fe 2 O 3 (hematite) can be identified by means of colorimetry. The color of corrosion products is orangish, indicating the contribution of α-Fe 2 O 3 in iron hydroxides. (author)

  16. Corrosion and tribological properties of basalt fiber reinforced composite materials

    Science.gov (United States)

    Ha, Jin Cheol; Kim, Yun-Hae; Lee, Myeong-Hoon; Moon, Kyung-Man; Park, Se-Ho

    2015-03-01

    This experiment has examined the corrosion and tribological properties of basalt fiber reinforced composite materials. There were slight changes of weight after the occurring of corrosion based on time and H2SO4 concentration, but in general, the weight increased. It is assumed that this happens due to the basalt fiber precipitate. Prior to the corrosion, friction-wear behavior showed irregular patterns compared to metallic materials, and when it was compared with the behavior after the corrosion, the coefficient of friction was 2 to 3 times greater. The coefficient of friction of all test specimen ranged from 0.1 to 0.2. Such a result has proven that the basalt fiber, similar to the resin rubber, shows regular patterns regardless of time and H2SO4 concentration because of the space made between resins and reinforced materials.

  17. General corrosion, irradiation-corrosion, and environmental-mechanical evaluation of nuclear-waste-package structural-barrier materials. Progress report

    International Nuclear Information System (INIS)

    Westerman, R.E.; Pitman, S.G.; Nelson, J.L.

    1982-09-01

    Pacific Northwest Laboratory is studying the general corrosion, irradiation-corrosion, and environmentally enhanced crack propagation of five candidate materials in high-temperature aqueous environments simulating those expected in basalt and tuff repositories. The materials include three cast ferrous materials (ductile cast iron and two low-alloy Cr-Mo cast steels) and two titanium alloys, titanium Grade 2 (commercial purity) and Grade 12 (a Ti-Ni-Mo alloy). The general corrosion results are being obtained by autoclave exposure of specimens to slowly replenished simulated ground water flowing upward through a bed of the appropriate crushed rock (basalt or tuff), which is maintained at the desired test temperature (usually 250 0 C). In addition, tests are being performed in deionized water. Metal penetration rates of iron-base alloys are being derived by stripping off the corrosion product film and weighing the specimen after the appropriate exposure time. The corrosion of titanium alloy specimens is being determined by weight gain methods. The irradiation-corrosion studies are similar to the general corrosion tests, except that the specimen-bearing autoclaves are held in a 60 Co gamma radiation field at dose rates up to 2 x 10 6 rad/h. For evaluating the resistance of the candidate materials to environmentally enhanced crack propagation, three methods are being used: U-bend and fracture toughness specimens exposed in autoclaves; slow strain rate studies in repository-relevant environments to 300 0 C; and fatigue crack growth rate studies at ambient pressure and 90 0 C. The preliminary data suggest a 1-in. corrosion allowance for iron-base barrier elements intended for 1000-yr service in basalt or tuff repositories. No evidence has yet been found that titanium Grade 2 or Grade 12 is susceptible to environmentally induced crack propagation or, by extension, to stress corrosion cracking

  18. Atmospheric corrosion tests along the Norwegian-Russian border. Part II

    Energy Technology Data Exchange (ETDEWEB)

    Henriksen, J.F.; Mikhailov, A.A.

    1997-12-31

    A bilateral exposure programme was carried out along the Norwegian-Russian border in 1990-1991, 1992-1993 and 1993-1994 to evaluate quantitatively the effect of sulphur pollutants on the atmospheric corrosion of important materials in sub-arctic climate. The first part of the programme demonstrated that also in subarctic climate do metals corrode depending on the atmospheric corrosivity, and dose-response functions were derived which combined the effects of SO{sub 2} and time of wetness. The second part of the programme, which is described in this report, involved exposures of carbon steel, zinc and copper at two sites in Norway and three sites in Russia. It is concluded that the accelerated atmospheric corrosion of metals in regions along the border is mainly due to dry deposition of sulphur. At some sites, dry deposition of Cl contributes because of sea-salt aerosols. The corrosivity of acid precipitation is certain but could not be represented as a function because of the small differences observed in the pH values at the different sites. At all test sites the kinetics of corrosion of steel, zinc and copper are characterized by a reduced corrosion rate after one year of exposure. Time of wetness is an important parameter in predicting atmospheric corrosion of metals even on a regional scale. Hence, for monitoring and for trend-effect analysis, it is very important to determine the corrosivity of SO{sub 2} with time of wetness. In accordance with dose-response functions obtained, the yearly corrosion rate for steel and zinc are higher for the areas with higher amounts of dry deposition of Cl than for areas with analogous but only SO{sub 2}-containing atmosphere. 6 refs., 8 figs., 15 tabs.

  19. A finite element modeling method for predicting long term corrosion rates

    International Nuclear Information System (INIS)

    Fu, J.W.; Chan, S.

    1984-01-01

    For the analyses of galvanic corrosion, pitting and crevice corrosion, which have been identified as possible corrosion processes for nuclear waste isolation, a finite element method has been developed for the prediction of corrosion rates. The method uses a finite element mesh to model the corrosive environment and the polarization curves of metals are assigned as the boundary conditions to calculate the corrosion cell current distribution. A subroutine is used to calculate the chemical change with time in the crevice or the pit environments. In this paper, the finite element method is described along with experimental confirmation

  20. Glove corrosive liquid immersion and permeability study

    International Nuclear Information System (INIS)

    Middleton, H.W.

    1977-01-01

    The Occupational Safety and Health Administration's requirement for protective equipment for personnel working with chemical hazards resulted in a study of gloves used in work with corrosive liquids. Gloves of different materials and weights were tested using ASTM methods, in various corrosive liquids. Results show the best material for gloves used for different lengths of time in the liquids