WorldWideScience

Sample records for fluorocarbon rubber fkm

  1. Comprehensive testing to measure the response of fluorocarbon rubber (FKM) to Hanford tank waste simulant

    Energy Technology Data Exchange (ETDEWEB)

    NIGREY,PAUL J.; BOLTON,DENNIS L.

    2000-02-01

    This report presents the findings of the Chemical Compatibility Program developed to evaluate plastic packaging components that may be incorporated in packaging mixed-waste forms for transportation. Consistent with the methodology outlined in this report, the authors performed the second phase of this experimental program to determine the effects of simulant Hanford tank mixed wastes on packaging seal materials. That effort involved the comprehensive testing of five plastic liner materials in an aqueous mixed-waste simulant. The testing protocol involved exposing the materials to {approximately}143, 286, 571, and 3,670 Krad of gamma radiation and was followed by 7-, 14-, 28-, 180-day exposures to the waste simulant at 18, 50, and 60 C. Fluorocarbon (FKM) rubber samples subjected to the same protocol were then evaluated by measuring seven material properties: specific gravity, dimensional changes, mass changes, hardness, compression set, vapor transport rates, and tensile properties. From the analyses, they determined that FKM rubber is not a good seal material to withstand aqueous mixed wastes having similar composition to the one used in this study. They have determined that FKM rubber has limited chemical durability after exposure to gamma radiation followed by exposure to the Hanford tank simulant mixed waste at elevated temperatures above 18 C.

  2. Tribological behavior of W-DLC coated rubber seals

    NARCIS (Netherlands)

    Pei, Y.T.; Bui, X.L.; Zhou, X.B.; Hosson, J.Th.M. De

    2008-01-01

    Tungsten-containing diamond-like carbon (W-DLC) coatings have been deposited on FKM (fluorocarbon) and HNBR (hydrogenated nitrile butadiene) rubbers via unbalanced magnetron reactive sputtering from a WC target in a C2H2/Ar plasma. The surface morphology and fracture cross sections of uncoated and c

  3. Microstructure and tribological behavior of tungsten-containing diamondlike carbon coated rubbers

    NARCIS (Netherlands)

    Pei, Y.T.; Bui, X.L.; Zhou, Xiao; Hosson, J.Th.M. De

    2008-01-01

    Tungsten-containing diamondlike carbon (W-DLC) coatings have been deposited on FKM (fluorocarbon), ACM (acrylate), and HNBR (hydrogenated nitrile butadiene) rubbers via unbalanced magnetron reactive sputtering from a WC target in C2H2/Ar plasma. The surface morphology and, fracture cross sections of

  4. Structure and Properties of FKM/ACM Blend%FKM/ACM并用胶的结构及性能研究

    Institute of Scientific and Technical Information of China (English)

    刘岚; 陈娟娟; 王亚明; 贾德民; 罗远芳

    2011-01-01

    对采用双酚AF/促进剂BPP硫化体系的氟橡胶(FKM)/丙烯酸酯橡胶(AcM)并用胶的各项性能进行研究.结果表明:以双酚AF/促进剂BPP为硫化体系,FKM和ACM可以实现共硫化,制得的FKM/ACM并用胶物理性能优良,耐热氧、耐紫外光和耐臭氧老化性能以及热稳定性较好,压缩永久变形性能优异}扫描电子显微镜显示FKM和ACM具有较好的相容性.%The properties of FKM/ACM blends prepared by bisphenol AF/BPP vulcanization system were investigated. The results showed that, FKM and ACM could be covulcanized under the bisphenol AF/BPP vulcanization system, and the physical properties, thermal oxidative aging property, ultraviolet aging property,ozone aging property, thermal stability and compression set of FKM/ACM blends were good. The scanning electron microscope analysis showed that FKM and ACM had good compatibility.

  5. Investigating Low Temperature Properties of Rubber Seals - 13020

    Energy Technology Data Exchange (ETDEWEB)

    Jaunich, M.; Wolff, D.; Stark, W. [BAM Federal Institute for Materials Research and Testing, Unter den Eichen 87, 12203 Berlin (Germany)

    2013-07-01

    To achieve the required tightness levels of containers for low and intermediate level radioactive wastes rubbers are widely applied as main sealing materials. The save encapsulation of the radioactive container contents has to be guaranteed according to legislation and appropriate guidelines for long storage periods as well as down to temperatures of -40 deg. C during transportation. Therefore the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance. It is known that the material properties of rubbers are strongly influenced by temperature. At low temperatures this is caused by the rubber-glass transition (abbr. glass transition). During continuous cooling the material changes from rubber-like entropy-elastic to stiff energy-elastic behaviour, that allows nearly no strain or retraction. Therefore, rubbers are normally used above their glass transition but the minimum working temperature limit is not defined precisely, what can cause problems during application. The temperature range where full functionality is possible is strongly dependent on the application conditions and the material. For this investigation mainly ethylene propylene diene (EPDM) and fluorocarbon rubbers (FKM) were selected as they are often used for radioactive waste containers. Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are typically used for the determination of the temperature range of the glass transition process. The standardized compression set measurement according to ISO 815 is common for investigation of rubber sealing materials as the test simulates the seal behaviour after release. To reduce the test time of the standard tests a faster technique giving the same information was developed. Additionally, the breakdown temperature of the sealing function of complete O-ring seals is measured in a component test setup to compare it with the results of the other tests. The experimental setup is capable of

  6. Mass spectrometry of fluorocarbon-labeled glycosphingolipids

    DEFF Research Database (Denmark)

    Li, Yunsen; Arigi, Emma; Eichert, Heather;

    2010-01-01

    A method for generation of novel fluorocarbon derivatives of glycosphingolipids (GSLs) with high affinity for fluorocarbon phases has been developed, and their potential applications to mass spectrometry (MS)-based methodologies for glycosphingolipidomics have been investigated. Sphingolipid...

  7. Fluorocarbon Adsorption in Hierarchical Porous Frameworks

    Energy Technology Data Exchange (ETDEWEB)

    Motkuri, Radha K.; Annapureddy, Harsha V.; Vijayakumar, M.; Schaef, Herbert T.; Martin, P F.; McGrail, B. Peter; Dang, Liem X.; Krishna, Rajamani; Thallapally, Praveen K.

    2014-07-09

    The adsorption behavior of a series of fluorocarbon derivatives was examined on a set of microporous metal organic framework (MOF) sorbents and another set of hierarchical mesoporous MOFs. The microporous M-DOBDC (M = Ni, Co) showed a saturation uptake capacity for R12 of over 4 mmol/g at a very low relative saturation pressure (P/Po) of 0.02. In contrast, the mesoporous MOF MIL-101 showed an exceptionally high uptake capacity reaching over 14 mmol/g at P/Po of 0.4. Adsorption affinity in terms of mass loading and isosteric heats of adsorption were found to generally correlate with the polarizability of the refrigerant with R12 > R22 > R13 > R14 > methane. These results suggest the possibility of exploiting MOFs for separation of azeotropic mixtures of fluorocarbons and use in eco-friendly fluorocarbon-based adsorption cooling and refrigeration applications.

  8. Influence of lubricant additives on rubber properties in conditions similar to the field

    Energy Technology Data Exchange (ETDEWEB)

    Dinzburg, B.N. [CR Industries, Elgin, IL (United States)

    1995-10-01

    Using FTIR spectroscopy, an investigation was performed to establish the oil degradation in a car engine under field conditions. This investigation was used as a baseline to create the laboratory rubber immersion in oil test with aeration. Aeration is required to improve the correlation of the laboratory immersion test with field conditions. The effects of dispersants, corrosion inhibitors and oxidation inhibitors containing amine groups on rubber compounds were evaluated in oil with and without aeration. Two rubber base compounds were tested: highly saturated butadiene-nitrile (HNBR) and fluoroelastomer (FKM). The aggressiveness of the inhibitors containing amines was varied and was affected to differing degrees by aeration, water, and type of rubber. 35 refs., 13 figs., 3 tabs.

  9. Friction and wear characteristics of elastomers in lubricated contact with EALs

    OpenAIRE

    Mofidi, Mohammad; Simmons, Gregory; Prakash, Braham

    2008-01-01

    The friction and wear characteristics of several elastomers have been studied during reciprocating sliding conditions when lubricated with uncontaminated environmentally adapted lubricants and the same lubricants contaminated with moisture. The elastomers studied are Nitrile Butadiene Rubber (NBR), Hydrogenated Nitrile Butadiene Rubber (HNBR), and Fluorocarbon Rubber (FKM). The lubricants used are complex ester and polyol ester as well as both aged and non-aged polyol esters with 5% water con...

  10. Fluorocarbon adsorption in hierarchical porous frameworks

    Science.gov (United States)

    Motkuri, Radha Kishan; Annapureddy, Harsha V. R.; Vijaykumar, M.; Schaef, H. Todd; Martin, Paul F.; McGrail, B. Peter; Dang, Liem X.; Krishna, Rajamani; Thallapally, Praveen K.

    2014-07-01

    Metal-organic frameworks comprise an important class of solid-state materials and have potential for many emerging applications such as energy storage, separation, catalysis and bio-medical. Here we report the adsorption behaviour of a series of fluorocarbon derivatives on a set of microporous and hierarchical mesoporous frameworks. The microporous frameworks show a saturation uptake capacity for dichlorodifluoromethane of >4 mmol g-1 at a very low relative saturation pressure (P/Po) of 0.02. In contrast, the mesoporous framework shows an exceptionally high uptake capacity reaching >14 mmol g-1 at P/Po of 0.4. Adsorption affinity in terms of mass loading and isosteric heats of adsorption is found to generally correlate with the polarizability and boiling point of the refrigerant, with dichlorodifluoromethane >chlorodifluoromethane >chlorotrifluoromethane >tetrafluoromethane >methane. These results suggest the possibility of exploiting these sorbents for separation of azeotropic mixtures of fluorocarbons and use in eco-friendly fluorocarbon-based adsorption cooling.

  11. Rubber Reclamation

    Science.gov (United States)

    Williams, Kathryn R.

    2007-01-01

    The safety and health hazards related to recycling of used rubber, due to the scarcity and high price of virgin rubber are reported. Various threats like stagnant water pools trapped in tires leading to diseases and ignited tires, which become very difficult to extinguish and generating smoke that is extremely detrimental to the environment, have…

  12. Comparing Measured Fluorocarbon Leader Breaking Strength with Manufacturer Claims

    CERN Document Server

    Haight, Christine; McQueeney, Kathleen; Courtney, Ya'el

    2012-01-01

    The experiment reported in this article addresses manufacturer claims of fluorocarbon leader material strength versus experimental tests of leaders strength. Breaking strength of fishing line is the most common specification when marketing fishing line. In this study, eight leaders rated near 15 pounds by their manufacturers were tested. Each leader was tested with a knot in the line and without a knot in the line. The strongest leader tested without a knot was Cabela's Seaguar fluorocarbon and the weakest leader tested without a knot was Cabela's Premier leader. The highest strength of leaders with a knot was the Ande Monofilament Fluorocarbon and the lowest breaking strength of leaders with a knot was the Seaguar Grand Max Fluorocarbon. Few published studies actually test the breaking strength of a leader to determine the accuracy of manufacturers' claims. Tensile strengths are also reported.

  13. Fluorocarbon compounds in MRI diagnostics and medical therapy

    Science.gov (United States)

    Pirogov, Yu

    2016-02-01

    The lecture describes the application of fluorocarbon compounds as blood substitutes and contrasting preparations in MRI diagnostics. A blood substitute product fluorocarbon Perfluorane® has shown effectiveness in oxygen delivery to the tissues of living organisms, and cardioprotective effect which does not depend on the patient's blood group. Inclusion of paramagnetic atoms (gadolinium, iron, etc.) to the Perfluorane® chemical formula creates a new compound with high MRI contrast efficiencies at Larmor frequencies of protons so and fluorine-19 nuclei.

  14. Properties of in-situ polymerized ACM/FKM blend%原位聚合丙烯酸酯橡胶/氟橡胶并用胶性能研究

    Institute of Scientific and Technical Information of China (English)

    陈春明; 熊传溪; 董丽杰

    2006-01-01

    在氟橡胶(FKM)的丙酮溶液中,采用原位聚合法制备丙烯酸酯橡胶(ACM),研究原位聚合ACM/FKM并用胶的性能.结果表明,原位聚合ACM/FKM并用胶中,ACM与FKM相容性较好;与ACM相比,ACM/FKM并用胶的物理性能和热稳定性明显提高.

  15. Health effects among refrigeration repair workers exposed to fluorocarbons.

    OpenAIRE

    1986-01-01

    Refrigeration repair workers may be intermittently exposed to fluorocarbons and their thermal decomposition products. A case of peripheral neuropathy (distal axonopathy) in a commercial refrigeration repairman prompted an epidemiological investigation of the health of refrigeration repair workers. No additional cases of peripheral neuropathy were identified among the 27 refrigeration repair workers studied. A reference group of 14 non-refrigeration repair workers was also studied. No differen...

  16. Natural rubber: leather composites

    OpenAIRE

    K. Ravichandran; N. Natchimuthu

    2005-01-01

    Leather is a fibrous protein consisting of collagen in a three dimensionally crosslinked network. Chrome tanning of leather improves the appearance of leather but at the same time emits both solid and liquid chrome leather wastes. Scrap rubber recycling using untreated and neutralized leather fibrous particles in natural rubber has been studied. Vulcanization, mechanical, morphological and swelling properties of the natural rubber - scrap rubber composites containing neutralized leather have ...

  17. Developments in rubber technology 2 synthetic rubbers

    CERN Document Server

    Lee, K

    1981-01-01

    This book is intended for those people who have a knowledge or understanding of rubber materials and processes but who wish to update their knowledge. It should be read in conjunction with Developments in Rubber Technology-l as that volume discussed developments in natural rubber and selected special purpose synthetic rubbers as well as additives. The authors have been selected for their expertise in each particular field and we, as editors, would like to express our appreciation to the individual authors and also to their companies. Such a book would be impossible to produce without such active cooperation as we have received. Volumes 1 and 2 of Developments in Rubber Technology cover rubbers which are processed and vulcanised in the traditional manner. It is appreciated that the omission of non-vulcanised rubber materials (the so­ called thermoplastic elastomers) will be unwelcome to many readers but it is intended, because of the size of the subject, to cover these materials in a subsequent volume. A.W. K...

  18. Mechanochemical modification of natural rubber

    Science.gov (United States)

    Mikhaylov, I. A.; Sukhareva, K. V.; Andriasyan, Yu. O.; Popov, A. A.; Vorontsov, N. V.

    2016-11-01

    Thermomechanochemical changes of SVR 3L natural rubber after the treatment in the internal rubber mixer in the self-heating mode were studied. The effect of the molecular mass and content of the gel fraction of natural rubber is shown. Properties of rubber compounds and vulcanized rubber are presented. Taking into account modern requirements, a new alternative technology of obtaining halogenated elastomers based on the solid-phase (mechanochemical) halide modification is created. New halogen-containing natural rubber produced by this technology proves themselves in the conditions of rubber production. New fluorinated natural rubber produced by this technology proves themselves in the conditions of rubber production.

  19. Integration Process Development for Improved Compatibility with Organic Non-Porous Ultralow-k Dielectric Fluorocarbon on Advanced Cu Interconnects

    Science.gov (United States)

    Gu, Xun; Tomita, Yugo; Nemoto, Takenao; Miyatani, Kotaro; Saito, Akane; Kobayashi, Yasuo; Teramoto, Akinobu; Kuroda, Rihito; Kuroki, Shin-Ichiro; Kawase, Kazumasa; Nozawa, Toshihisa; Matsuoka, Takaaki; Sugawa, Shigetoshi; Ohmi, Tadahiro

    2012-05-01

    Integration of an organic non-porous ultralow-k dielectric, fluorocarbon (k= 2.2), into advanced Cu interconnects was demonstrated. The challenges of process-induced damage, such as delamination and variances of both the structure and electrical properties of the fluorocarbon during fabrication, were investigated on Cu/fluorocarbon damascene interconnects. A titanium-based barrier layer, instead of a tantalum-based barrier layer, was used to avoid delamination between Cu and fluorocarbon in Cu/fluorocarbon interconnects. A moisture-hermetic dielectric protective layer was also effective to avoid damage induced by wet chemical cleaning. On the other hand, a post-etching nitrogen plasma treatment to form a stable protective layer on the surface of the fluorocarbon was proposed for the practical minimization of damage introduction to fluorocarbon in the following damascene process, such as post-etching cleaning.

  20. Thermodynamics of Rubber Elasticity

    Science.gov (United States)

    Pellicer, J.; Manzanares, J. A.; Zúñiga, J.; Utrillas, P.; Fernández, J.

    2001-02-01

    A thermodynamic study of an isotropic rubber band under uniaxial stress is presented on the basis of its equation of state. The behavior of the rubber band is compared with both that of an ideal elastomer and that of an ideal gas, considering the generalized Joule's law as the ideality criterion. First, the thermal expansion of rubber at constant stress and the change in the stress with temperature at constant length are described. Thermoelastic inversion is then considered, and the experimental observations are easily rationalized. Finally, the temperature changes observed in the adiabatic stretching of a rubber band are evaluated from the decrease of entropy with length.

  1. Optimized plasma-deposited fluorocarbon coating for dry release and passivation of thin SU-8 cantilevers

    DEFF Research Database (Denmark)

    Keller, Stephan Urs; Häfliger, Daniel; Boisen, Anja

    2008-01-01

    Plasma-deposited fluorocarbon coatings are introduced as a convenient method for the dry release of polymer structures. In this method, the passivation process in a deep reactive ion etch reactor was used to deposit hydrophobic fluorocarbon films. Standard photolithography with the negative epoxy......-based photoresist SU-8 was used to fabricate polymer structures such as cantilevers and membranes on top of the nonadhesive release layer. The authors identify the plasma density as the main parameter determining the surface properties of the deposited fluorocarbon films. They show that by modifying the pressure...

  2. Influence of Rubber Size on Properties of Crumb Rubber Mortars

    Directory of Open Access Journals (Sweden)

    Yong Yu

    2016-06-01

    Full Text Available Studies on the properties and applications of rubber cement-based materials are well documented. The sizes of rubbers used in these materials varied. However, information about the effects of rubber size on the properties of rubber cement-based materials, especially pore structure, mechanical strengths, and drying shrinkage properties, remains limited. Three groups of rubber with major particle sizes of 2–4 mm, 1–3 mm, and 0–2 mm were selected in this study. This paper presents experimental studies on the effects of rubber size on the consistency, fresh density, pore structure, mechanical properties, and drying shrinkage properties of crumb rubber mortars (CRMs. Results demonstrated that the consistency and fresh density of CRMs decreased with the rubber size. As to the pore structure, the total pore volume increased with the decrease of the rubber size. By contrast, the influence of the rubber size on the mesopore (<50 nm volume is not as significant as that of the rubber content. The mechanical properties of CRMs decreased with the rubber size. Low rubber stiffness and large pore volumes, especially those of small sized rubbers, contribute to the reduction of CRMs strength. The drying shrinkage of CRM increases as the rubber size decreases. The influences of rubber size on capillary tension are not significant. Thus, the shrinkage increases with the decrease of rubber size mainly because of its function in the deformation modulus reduction of CRMs.

  3. Blue rubber bleb naevus

    Directory of Open Access Journals (Sweden)

    Mittal R

    1995-01-01

    Full Text Available A 35 year old female had multiple progressive painful, tender, soft, bluish compressible nodules with the feel of rubber nipples. There was no evidence of gastrointestinal haemangiomas or other systemic abnormalities. Histopathologically, cavernous haemangioma with prominent smooth muscle outline proved the clinical diagnosis of blue rubber bleb naevus. Only cutaneous lesions were seen in the patient.

  4. Biodiversity in rubber agroforests

    NARCIS (Netherlands)

    Beukema, Hendrien

    2013-01-01

    Jungle rubber tuinen zijn extensieve rubber agroforests die qua structuur op secundaire bossen lijken, en waarin wilde soorten door de boer worden getolereerd. Met het verdwijnen van het laaglandregenwoud rijst de vraag of de begroeiing die ervoor in de plaats komt een aantal kenmerken en functies v

  5. Natural rubber biosynthesis in plants: rubber transferase.

    Science.gov (United States)

    Cornish, Katrina; Xie, Wenshuang

    2012-01-01

    Rubber biosynthesis in plants is a fascinating biochemical system, which evolved at the dawn of the dicotyledoneae and is present in at least four of the dictolydonous superorders. Rubber biosynthesis is catalyzed by a membrane complex in a monolayer membrane envelope, requires two distinct substrates and a divalent cation cofactor, and produces a high-molecular-weight isoprenoid polymer. A solid understanding of this system underpins valuable papers in the literature. However, the published literature is rife with unreliable reports in which the investigators have fallen into traps created by the current incomplete understanding of the biochemistry of rubber synthesis. In this chapter, we attempt to guide both new and more established researchers around these pitfalls.

  6. Interaction of Fluorocarbon Containing Hydrophobically Modified Polyelectrolyte with Nonionic Surfactants

    Institute of Scientific and Technical Information of China (English)

    GUO,Jin-Feng(郭金峰); ZHUANG,Dong-Qing(庄东青); ZHOU,Hui(周晖); ZHANG,Yun-Xiang(章云祥)

    2002-01-01

    The interaction of fluorocarbon containing hydrophobically modified polyelectrolyte (FMPAANa) with two kinds of nonionic surfactants (hydrogenated and fluorinated) in a semidilute (0.5 wt% ) aqueous solution had been studied by rheological measurements. Association behavior was found in both systems. The hydrophobic interaction of FMPAANa with fluorinated surfactant (FC171) is much stronger than that with hydrogenated surfactant (NP7.5) at low surfactant concentrations. The interaction is strengthened by surfactants being added for the density of active junctions increased. Whereas distinct phenomena for FC171 and NP7. 5 start to be found as the surfactants added over their respective certain concentration. The interaction of polyelectrolyte with fluorinated surfactant increases dramatical ly while that with hydrogenated surfactant decreases.

  7. Multilayer graphene rubber nanocomposites

    Science.gov (United States)

    Schartel, Bernhard; Frasca, Daniele; Schulze, Dietmar; Wachtendorf, Volker; Krafft, Bernd; Morys, Michael; Böhning, Martin; Rybak, Thomas

    2016-05-01

    Multilayer Graphene (MLG), a nanoparticle with a specific surface of BET = 250 m2/g and thus made of only approximately 10 graphene sheets, is proposed as a nanofiller for rubbers. When homogenously dispersed, it works at low loadings enabling the replacement of carbon black (CB), increase in efficiency, or reduction in filler concentration. Actually the appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing and mechanical properties of different rubbers, as shown for Chlorine-Isobutylene-Isoprene Rubber (CIIR), Nitrile-Butadiene Rubber (NBR), Natural Rubber (NR), and Styrene-Butadiene Rubber (SBR). A mere 3 phr of MLG tripled the Young's modulus of CIIR, an effect equivalent to 20 phr of carbon black. Similar equivalents are observed for MLG/CB mixtures. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards fire behavior. The later shown by the reduction in heat release rate in the cone calorimeter. The higher the nanofiller concentration is (3 phr, 5 phr, and 10 phr was investigated), the greater the improvement in the properties of the nanocomposites. Moreover, the MLG nanocomposites improve stability of mechanical properties against weathering. An increase in UV-absorption as well as a pronounced radical scavenging are proposed and were proved experimentally. To sum up, MLG is interesting as a multifunctional nanofiller and seems to be quite ready for rubber development.

  8. Radiation vulcanization of rubbers

    Energy Technology Data Exchange (ETDEWEB)

    Makuuchi, Keizo [Japan Atomic Energy Research Inst., Takasaki, Gunma (Japan). Takasaki Radiation Chemistry Research Establishment

    2002-02-01

    An abstract of the radiation process of polymer materials and the polymer reaction by radiation is explained. Main radiation is 250 keV to 10 MeV of electron rays in the industry. Radiation cross-linked rubber has less the tensile strength than that by sulfur and organic peroxide crosslinking. The main origins of low tensile strength are caused by cut of backbone chain and ozone depend on radiation. Acceleration of crosslinking and short time of radiation are necessary to improve these defects. To accelerate crosslinking, we used crosslinking accelerators, for example, three poly-functional monomers (PFM). The maximum tensile strength of styrene-butadiene rubber (SBR) not added crosslinking accelerators showed 3 MPa at 110 kGy, but SBR added A-TMMT (tetramethylolmethane tetraacrylate) showed 5.5 MPa at 110 kGy. Radiation crosslinking of many kinds of rubber: isoprene (IR), SBR, CR, nitrile rubber (NBR), hydrogenated nitrile rubber (HNBR), butyl rubber (IIR), chlorinated butyl rubber (CIIR), EPM and TPE are explained. (S.Y.)

  9. Global Synethetic Rubber Industrial Outlook

    Institute of Scientific and Technical Information of China (English)

    Dr.Leon Loh

    2011-01-01

    @@ This paper is to compile and analyze the statistical data of synthetic rubber capacity and consumption to understand its impact of supply/demand on the global synthetic rubber market.Some forecasted consumption data were generated and published by the joint efforts of both IISRP(International Institute of Synthetic Rubber Producers)and IRSG(International Rubber Study group).The report also covers the observed industrial trends as well as some emerging issues in the synthetic rubber industry.

  10. Ericameria Nauseosa (rubber rabbitbrush): a complementary rubber feedstock to augment the guayule rubber production stream

    Science.gov (United States)

    Ericameria nauseosa (rubber rabbitbrush) is a highly prolific desert shrub that produces high quality natural rubber. Over the past several years we have investigated rabbitbrush’s potential as a commercial rubber feedstock. Like guayule, rabbitbrush produces natural rubber within its bark tissues a...

  11. Runaway Rubber Removal

    Science.gov (United States)

    1989-01-01

    High hysteresis Good tract;on characteristic Poor affinity for blending Polyisoprene PI Strong wear resistance Very similar to natural rubber Low...with a "base of cresylic acid and a blend of benzene, with a synthetic detergent for a wetting agent" are recommended [8]. For AC runways, alkaline...you expect the runway to change after rubber is removed? Response Maintenance Operations Pilots Improved Skid Resistance! Brak inq Act ion/Fr ictior 7

  12. Investigations of the environmental acceptability of fluorocarbon alternatives to chlorofluorocarbons.

    Science.gov (United States)

    McFarland, M

    1992-02-01

    Chlorofluorocarbons (CFCs) are currently used in systems for preservation of perishable foods and medical supplies, increasing worker productivity and consumer comfort, conserving energy and increasing product reliability. As use of CFCs is phased out due to concerns of ozone depletion, a variety of new chemicals and technologies will be needed to serve these needs. In choosing alternatives, industry must balance concerns over safety and environmental acceptability and still meet the preformance characteristics of the current technology, the only viable alternatives meeting the safety, performance, and environmental requirements for the remaining 40% of demand are fluorocarbons, hydrochlorofluorocarbons (HCFs), and hydrofluorocarbons (HFCs). HCFCs and HFCs possess many of the desirable properties of the CFCs, but because of the, hydrogen, they results in shorter atmospheric lifetimes compared to CFCs and reduces their potential to contribute to stratospheric ozone depletion or global warming; HFCs do not contain chlorine and have no potential to destroy ozone. This paper provides an overview of challenges faced by industry, regulators, and society in general in continuing to meet societal needs and consumer demands while reducing risk to the enviroment without compromising consumer or worker safety.

  13. Biodesulfurization of rubber materials

    Energy Technology Data Exchange (ETDEWEB)

    Torma, A.E. (EG and G Idaho, Inc., Idaho Falls, ID (USA)); Raghavan, D. (Illinois Univ., Urbana, IL (USA). Dept. of Materials Science and Engineering)

    1990-01-01

    One of the most challenging problems in municipal waste treatment is the recycling of polymeric waste materials. The present study has demonstrated the applicability of biotechnological principles in the desulfurization of rubber using shake flask and Warburg respirometric techniques. In terms of oxygen uptake and specific rate of oxygen uptake, it was found that the mixed culture of Thiobacillus ferrooxidans and Thiobacillus thiooxidans was more efficient in this process than the individual pure cultures of these bacteria. Furthermore, the mixed cultures resulted in ten times higher sulfur removals from rubber relative to those of sterile controls. Additional studies are needed to elucidate the mechanisms of biodesulfurization of rubber. It is expected that the development of this process may provide a solution to recycling of car tire materials. 32 refs., 4 figs., 3 tabs.

  14. Novel fluoro-carbon functional monomer for dental bonding.

    Science.gov (United States)

    Yoshihara, K; Yoshida, Y; Hayakawa, S; Nagaoka, N; Kamenoue, S; Okihara, T; Ogawa, T; Nakamura, M; Osaka, A; Van Meerbeek, B

    2014-02-01

    Among several functional monomers, 10-methacryloxydecyl dihydrogen phosphate (10-MDP) bonded most effectively to hydroxyapatite (HAp). However, more hydrolysis-resistant functional monomers are needed to improve bond durability. Here, we investigated the adhesive potential of the novel fluoro-carbon functional monomer 6-methacryloxy-2,2,3,3,4,4,5,5-octafluorohexyl dihydrogen phosphate (MF8P; Kuraray Noritake Dental Inc., Tokyo, Japan) by studying its molecular interaction with powder HAp using solid-state nuclear magnetic resonance ((1)H MAS NMR) and with dentin using x-ray diffraction (XRD) and by characterizing its interface ultrastructure at dentin using transmission electron microscopy (TEM). We further determined the dissolution rate of the MF8P_Ca salt, the hydrophobicity of MF8P, and the bond strength of an experimental MF8P-based adhesive to dentin. NMR confirmed chemical adsorption of MF8P onto HAp. XRD and TEM revealed MF8P_Ca salt formation and nano-layering at dentin. The MF8P_Ca salt was as stable as that of 10-MDP; MF8P was as hydrophobic as 10-MDP; a significantly higher bond strength was recorded for MF8P than for 10-MDP. In conclusion, MF8P chemically bonded to HAp. Despite its shorter size, MF8P possesses characteristics similar to those of 10-MDP, most likely to be associated with the strong chemical bond between fluorine and carbon. Since favorable bond strength to dentin was recorded, MF8P can be considered a good candidate functional monomer for bonding.

  15. Electron attachment and positive ion chemistry of monohydrogenated fluorocarbon radicals

    Energy Technology Data Exchange (ETDEWEB)

    Wiens, Justin P.; Shuman, Nicholas S.; Miller, Thomas M.; Viggiano, Albert A., E-mail: afrl.rvborgmailbox@kirtland.af.mil [Air Force Research Laboratory, Space Vehicles Directorate, Kirtland AFB, New Mexico 87117 (United States)

    2015-08-21

    Rate coefficients and product branching fractions for electron attachment and for reaction with Ar{sup +} are measured over the temperature range 300–585 K for three monohydrogenated fluorocarbon (HFC) radicals (CF{sub 3}CHF, CHF{sub 2}CF{sub 2}, and CF{sub 3}CHFCF{sub 2}), as well as their five closed-shell precursors (1-HC{sub 2}F{sub 4}I, 2-HC{sub 2}F{sub 4}I, 2-HC{sub 2}F{sub 4}Br, 1-HC{sub 3}F{sub 6}I, 2-HC{sub 3}F{sub 6}Br). Attachment to the HFC radicals is always fairly inefficient (between 0.1% and 10% of the Vogt–Wannier capture rate), but generally faster than attachment to analogous perfluorinated carbon radicals. The primary products in all cases are HF-loss to yield C{sub n}F{sub m−1}{sup −} anions, with only a minor branching to F{sup −} product. In all cases the temperature dependences are weak. Attachment to the precursor halocarbons is near the capture rate with a slight negative temperature dependence in all cases except for 2-HC{sub 2}F{sub 4}Br, which is ∼10% efficient at 300 K and becomes more efficient, approaching the capture rate at higher temperatures. All attachment kinetics are successfully reproduced using a kinetic modeling approach. Reaction of the HFC radicals with Ar{sup +} proceeds at or near the calculated collisional rate coefficient in all cases, yielding a wide variety of product ions.

  16. Properties of Low Surface Energy Fluorocarbon Polymers with Fluoro-acrylic Resins

    Institute of Scientific and Technical Information of China (English)

    LIU Xiusheng; WANG Can; LIU Lanxuan; LI Jian; GAO Wanzhen

    2008-01-01

    The low surface energy fluorocarbon polymer from the synthesized fluoro-acrylic resins was developed. Then the molecule orientation principle of nonpolar and polar functional groups in the polymers was analyzed. And the contact angles of pure water drops on the surfaces of various fluoro-monomer homopolymers and interpolymers were measured. So the relation of polymers' fluoro-content with the surface energy was determined. The distribution of fluoric functional groups in the polymers was investigated. And the test results show that though the total fluorine content of the fluorocarbon polymers is relative few, their surface energy is really low due to the enrichment of fluoro-chains on the polymers surface.

  17. Dry cleaning of fluorocarbon residues by low-power electron cyclotron resonance hydrogen plasma

    CERN Document Server

    Lim, S H; Yuh, H K; Yoon Eui Joon; Lee, S I

    1988-01-01

    A low-power ( 50 W) electron cyclotron resonance hydrogen plasma cleaning process was demonstrated for the removal of fluorocarbon residue layers formed by reactive ion etching of silicon dioxide. The absence of residue layers was confirmed by in-situ reflection high energy electron diffraction and cross-sectional high resolution transmission electron microscopy. The ECR hydrogen plasma cleaning was applied to contact cleaning of a contact string structure, resulting in comparable contact resistance arising during by a conventional contact cleaning procedure. Ion-assisted chemical reaction involving reactive atomic hydrogen species generated in the plasma is attributed for the removal of fluorocarbon residue layers.

  18. The Study of Low Surface Energy Fluorocarbon Coatings with Fluor Content Being Lower

    Institute of Scientific and Technical Information of China (English)

    GAO Wan-zhen; LIU Xiu-sheng; ZHONG Ping

    2004-01-01

    A kind of low surface energy fluorocarbon coatings from the synthesized fluoro-acrylic resin was developed.The molecule orientation principle of nonpolar and polar functional groups in the coatings was analyzed. The contact angles of pure water drops on the surfaces of various fluoro-monomer homopolymers and interpolymers were measured. The relation of coatings' fluoro-content with the surface energy was determined. The distribution of fluoric functional groups in the coatings was investigated. The test results show that though the total content of fluor of the fluorocarbon coatings is relative few, their surface energy is really low due to the enrichment of fluoro-chains on the surfaces.

  19. Effect of Rubber Particle Modification on Properties of Rubberized Concrete

    Institute of Scientific and Technical Information of China (English)

    ZHANG Haibo; GOU Mifeng; LIU Xiaoxing; GUAN Xuemao

    2014-01-01

    To improve the combination of cement matrix and waste tire rubber particles in concrete, the rubber particles were treated with acrylic acid (ACA) and polyethylene glycol (PEG) for grafting hydrophilic groups on their surfaces. The X-Ray photoelectron spectroscopy (XPS) and surface contact angle were used to characterize the hydrophilicity and surface functional group of rubber particles. The effect of rubber particle modification on fresh/hardened properties of rubberized concrete was studied. The experimental results show that the contact angle between rubber particle surface and water decreases when rubber particle is modified. Compared with the unmodified rubberized concrete(RC), the unit weight of modified rubberized concrete(MRC) changes slightly. However, the slump, air-entrainment, compressive strength, flexural strength, and impact performance of MRC are obviously improved. Under good condition of slump, the water-cement ratio of the MRC can be reduced from 0.4 to 0.38. And the compressive strength and flexural strength of the MRC(10%rubber particle content) can be increased by 25.9%and 26.4%, respectively.

  20. Fluorocarbon coatings deposited on micron-sized particles by atmospheric PECVD

    NARCIS (Netherlands)

    Abadjieva, E.; Heijden, A.E.D.M. van der; Creyghton, Y.L.M.; Ommen, J.R. van

    2012-01-01

    Fluorocarbon coatings have been deposited on micron-sized silica particles by means of atmospheric pressure plasma-enhanced chemical vapor deposition (PECVD). The silica particles have a diameter in the range between 40 and 70 ?m. They are fluidized at atmospheric pressure in a circulating fluidized

  1. EXPERIMENTAL CHARACTERIZATION OF FLUOROCARBON-MODIFIED POLYACRYLAMIDE/SURFACTANT AQUEOUS SOLUTIONS

    Institute of Scientific and Technical Information of China (English)

    Huai-tian Bu; Zhen-zhong Yang; Yun-xiang Zhang

    2003-01-01

    The interaction between surfactants and fluorocarbon-modified polyacrylamide (FC-PAM) in aqueous solutions was evaluated by theological means and fluorescence spectroscopy and was found to be strong regardless of the surfactant's nature. Two representative surfactants, anionic sodium dodecyl sulfate (SDS) and nonionic Triton X-100, were used. The origin of the interaction and its dependence on the surfactant concentration were discussed.

  2. Aspects of the use of saturated fluorocarbon fluids in high energy physics

    Energy Technology Data Exchange (ETDEWEB)

    Hallewell, G., E-mail: Gregory.Hallewell@cern.c [Centre de Physique des Particules de Marseille, 163 Avenue de Luminy, Case 907, 13288 Marseille Cedex 09 (France)

    2011-05-21

    The excellent dielectric properties of saturated fluorocarbons have allowed their use in direct immersion liquid cooling of electronics, including supercomputers and as heat transfer media in vapour phase soldering and burn-in testing of electronics. Their high density, UV transparency, non-flammability, non-toxicity and radiation tolerance have led to their use as liquid and gas radiator media for RICH detectors in numerous particle physics experiments. Systems to circulate and purify saturated fluorocarbon Cherenkov radiator vapours often rely on thermodynamic evaporation-condensation cycles similar to those used in refrigeration. Their use as evaporative refrigerants was pioneered for the ATLAS silicon tracker, and they are now also used as evaporative coolants in ALICE and TOTEM and as liquid coolants in ATLAS and CMS. Ultrasonic techniques for vapour phase analysis of fluorocarbon mixtures-developed for the SLAC SLD barrel CRID radiator during the 1980s as an alternative to UV refractometry are again under development for the ATLAS tracker evaporative cooling system. Examples of fluorocarbon circulation systems, together with purification and analysis techniques for these versatile fluids are mentioned.

  3. Residual stresses in rubber formed thermoplastic composites

    NARCIS (Netherlands)

    Wijskamp, Sebastiaan; Lamers, E.A.D.; Akkerman, Remko; Brucato, V.

    2003-01-01

    The rubber pressing process is applied for the rapid production of thermoplastic composite products. However, rubber pressed products show geometrical distortions, such as warpage, due to processinduced residual stresses. An experimental study is performed to measure the curvature after rubber

  4. Preparation of Hydrogenated Nitrile Rubber

    Institute of Scientific and Technical Information of China (English)

    2001-01-01

    @@ Hydrogenated nitrile rubber is an oil and solvent resistant rubber and particularly give more resistant to heat, ozone, light. It is generally prepared from nitrile rubber by selective hydrogenation using a suitable catalyst system. In the present work a prepared method was adapted for the hydrogenation reaction of nitrile rubber using homogeneous tris(tri-phenlphosphine)chlorhodium(I) catalyst (RhCl(PPh3)) system. The hydrogenation reaction was carriedout at different temperature, pressure, time and catalyst concentration, the concentration, the conditions of hydrogenation are stated in table 1.

  5. QENS investigation of filled rubbers

    Energy Technology Data Exchange (ETDEWEB)

    Triolo, A.; Lechner, R.E.; Desmedt, A.; Pieper, J. [CNR - Istituto per i Processi Chimico-Fisici, sez. Messina, Via La Farina 237, 98123 Messina (Italy); Lo Celso, F.; Triolo, R. [Dip. Chimica Fisica, V. le delle Scienze, Parco d' Orleans, Padiglione 17, Universita di Palermo, 90128 Palermo (Italy); Negroni, F. [Pirelli Pneumatici S.p.A, V. le Sarca 222, 20126 Milano (Italy); Arrighi, V.; Qian, H. [Chemistry School of Engineering and Physical Sciences, Heriot-Watt University, EH14 4AS Edinburgh (United Kingdom); Frick, B. [Institut Laue-Langevin, 6, rue Jules Horowitz, BP 156, 38042 Grenoble, Cedex 9 (France)

    2002-07-01

    The polymer segmental dynamics is investigated in a series of silica-filled rubbers. The presence of inert fillers in polymers greatly affects the mechanical and physical performance of the final materials. For example, silica has been proposed as a reinforcing agent of elastomers in tire production. Results from quasielastic neutron scattering and Dynamic Mechanical Thermal Analysis (DMTA) measurements are presented on styrene-ran-butadiene rubber filled with silica. A clear indication is obtained of the existence of a bimodal dynamics, which can be rationalized in terms of the relaxation of bulk rubber and the much slower relaxation of the rubber adsorbed on the filler surface. (orig.)

  6. QENS investigation of filled rubbers

    CERN Document Server

    Triolo, A; Desmedt, A; Pieper, J K; Lo Celso, F; Triolo, R; Negroni, F; Arrighi, V; Qian, H; Frick, B

    2002-01-01

    The polymer segmental dynamics is investigated in a series of silica-filled rubbers. The presence of inert fillers in polymers greatly affects the mechanical and physical performance of the final materials. For example, silica has been proposed as a reinforcing agent of elastomers in tire production. Results from quasielastic neutron scattering and Dynamic Mechanical Thermal Analysis (DMTA) measurements are presented on styrene-ran-butadiene rubber filled with silica. A clear indication is obtained of the existence of a bimodal dynamics, which can be rationalized in terms of the relaxation of bulk rubber and the much slower relaxation of the rubber adsorbed on the filler surface. (orig.)

  7. QENS investigation of filled rubbers

    Science.gov (United States)

    Triolo, A.; Lo Celso, F.; Negroni, F.; Arrighi, V.; Qian, H.; Lechner, R. E.; Desmedt, A.; Pieper, J.; Frick, B.; Triolo, R.

    The polymer segmental dynamics is investigated in a series of silica-filled rubbers. The presence of inert fillers in polymers greatly affects the mechanical and physical performance of the final materials. For example, silica has been proposed as a reinforcing agent of elastomers in tire production. Results from quasielastic neutron scattering and Dynamic Mechanical Thermal Analysis (DMTA) measurements are presented on styrene-ran-butadiene rubber filled with silica. A clear indication is obtained of the existence of a bimodal dynamics, which can be rationalized in terms of the relaxation of bulk rubber and the much slower relaxation of the rubber adsorbed on the filler surface.

  8. Preparation of Hydrogenated Nitrile Rubber

    Institute of Scientific and Technical Information of China (English)

    LIU; ZhiCai

    2001-01-01

    Hydrogenated nitrile rubber is an oil and solvent resistant rubber and particularly give more resistant to heat, ozone, light. It is generally prepared from nitrile rubber by selective hydrogenation using a suitable catalyst system. In the present work a prepared method was adapted for the hydrogenation reaction of nitrile rubber using homogeneous tris(tri-phenlphosphine)chlorhodium(I) catalyst (RhCl(PPh3)) system.  The hydrogenation reaction was carriedout at different temperature, pressure, time and catalyst concentration, the concentration, the conditions of hydrogenation are stated in table 1.  ……

  9. Laboratory performance of asphalt rubber mixtures

    OpenAIRE

    Fontes, Liseane; Trichês, Glicério; Pais, Jorge; Pereira, Paulo; Minhoto, Manuel

    2009-01-01

    Asphalt rubber mixtures are one of the most promising techniques to extend the service life of asphalt pavement overlays. Asphalt rubber binder is composed of crumb rubber from reclaimed tires and conventional asphalt. The asphalt rubber binder can be obtained through wet process in two different systems: tire rubber modified asphalt binder (produced at industrial plants) and continuous blending (produced in asphalt plants). This study presents a laboratory evaluation of asphalt rubber mixtur...

  10. CRIA Sians A areement with Rubber Valley

    Institute of Scientific and Technical Information of China (English)

    2011-01-01

    The signing ceremony of establishing strategic partnership between China Rubber Industry Association and Rubber Valley Co., Ltd. was held in Rubber Valley on September 13. Leaders such as Xu Wenying, Deputy Secretary-General of CRIA, repre-senting CRIA, and Zhang Yan, Deputy Director of Rubber Valley Management Committee and General Manager of Rubber Valley Co., Ltd., representing Rubber Valley, signed on the cooperation agreement. Fan Rende, President of CRIA, Cai Quanji,

  11. The environmental history and probable future of fluorocarbon-11

    Science.gov (United States)

    Khalil, M. A. K.; Rasmussen, R. A.

    1993-12-01

    The atmospheric concentration of fluorocarbon 11 (F-11) has increased steadily since it was first put into commercial use in the late 1930s and early 1940s. The observed trends, however, have two periods of dramatic declines. The first occurred around 1974, when trends started falling from their all time high of 13.8 pptv/yr down to around 7.8 pptv/yr (1 pptv = 10-12 parts by volume) in 1982. This decline occurred at first, probably, because of market conditions and later because of the ban in the United States on inessential uses of F-11, particularly in aerosol spray cans. In the meantime, other uses of F-11, such as blowing foams, increased, causing an increasing trend once again until around 1987, when the atmospheric trends reached 11 pptv/yr (measured 1986-1988, inclusive). After this time, however, the trends have fallen dramatically and are now only 4.6 pptv/yr (measured 1990-1992) and even lower in the middle northern latitudes (about 2 pptv/yr). The recent decline of trend is attributed to the effect of the Montreal Protocol and subsequent agreements that are designed to ban worldwide production before the turn of this century. The atmospheric trends reflect estimated emissions, which reached highest values in 1974 (340-355 Gg/yr; 1 Gg = 109g) and again in 1988 (314-380 Gg/yr). The observed concentrations and trends agree extremely well with those calculated from independent estimates of emissions from the various sources. Atmospheric concentrations of F-11 are calculated from a mass balance theory involving seven reservoirs and their interactions. Three of the reservoirs are at the Earth's surface arising from the uses of F-11 (quick-release applications such as open cell foams and aerosols, nonhermetically sealed refrigeration, and rigid polyurethane foams). We estimate that of the 9150 Gg of F-11 that have been produced throughout its history, at present about 1040 Gg are tied up in rigid foams (90 Gg and 24 Gg are tied up in refrigeration and quick

  12. Alternative sources of natural rubber

    NARCIS (Netherlands)

    Mooibroek, H.; Cornish, K.

    2000-01-01

    Rubber (cis-1,4-polyisoprene) is one of the most important polymers naturally produced by plants because it is a strategic raw material used in more than 40,000 products, including more than 400 medical devices. The sole commercial source, at present, is natural rubber harvested from the Brazilian r

  13. Warpage of rubber pressed composites

    NARCIS (Netherlands)

    Wijskamp, Sebastiaan; Lamers, E.A.D.; Akkerman, Remko; van de Ven, Erik

    2002-01-01

    The rubber pressing process is applied for the rapid production of thermoplastic composite products. However, rubber pressed products show geometrical distortions, such as warpage, due to process-induced residual stresses. It is believed that these stresses build up as a result of the large thermal

  14. Engineered Plastics Containing Recycled Rubber

    Institute of Scientific and Technical Information of China (English)

    Dong Yang Wu

    2000-01-01

    @@ 1. Introduction In Australia 10.5 million rubber tyres are discarded annually, representing 120,000 tonnes of wasted rubber resource. Growing local and global concern about the impact of this waste on the environment requires action for the management and recycling of this highly valuable resource through the development of recycling technologies and innovative recycled/recyclable products.

  15. Rubber compounding and processing

    CSIR Research Space (South Africa)

    John

    2014-06-01

    Full Text Available stream_source_info John_2014_ABSTRACT ONLY.pdf.txt stream_content_type text/plain stream_size 886 Content-Encoding ISO-8859-1 stream_name John_2014_ABSTRACT ONLY.pdf.txt Content-Type text/plain; charset=ISO-8859...-1 Handbook of Green Materials Processing Technologies, Properties and Applications Chapter 15 RUBBER COMPOUNDING AND PROCESSING MAYA JACOB JOHN1,2 1CSIR Materials Science and Manufacturing, Polymers and Composites Competence Area, P.O. Box 1124...

  16. Down-regulation of small rubber particle protein expression affects integrity of rubber particles and rubber content in Taraxacum brevicorniculatum.

    Directory of Open Access Journals (Sweden)

    Andrea Hillebrand

    Full Text Available The biosynthesis of rubber is thought to take place on the surface of rubber particles in laticifers, highly specialized cells that are present in more than 40 plant families. The small rubber particle protein (SRPP has been supposed to be involved in rubber biosynthesis, and recently five SRPPs (TbSRPP1-5 were identified in the rubber-producing dandelion species Taraxacum brevicorniculatum. Here, we demonstrate by immunogold labeling that TbSRPPs are localized to rubber particles, and that rubber particles mainly consist of TbSRPP3, 4 and 5 as shown by high-resolution two-dimensional gel electrophoresis and mass spectrometric analysis. We also carried out an RNA-interference approach in transgenic plants to address the function of TbSRPPs in rubber biosynthesis as well as rubber particle morphology and stability. TbSRPP-RNAi transgenic T. brevicorniculatum plants showed a 40-50% reduction in the dry rubber content, but neither the rubber weight average molecular mass nor the polydispersity of the rubber were affected. Although no phenotypical differences to wild-type particles could be observed in vivo, rubber particles from the TbSRPP-RNAi transgenic lines were less stable and tend to rapidly aggregate in expelling latex after wounding of laticifers. Our results prove that TbSRPPs are very crucial for rubber production in T. brevicorniculatum, probably by contributing to a most favourable and stable rubber particle architecture for efficient rubber biosynthesis and eventually storage.

  17. Down-regulation of small rubber particle protein expression affects integrity of rubber particles and rubber content in Taraxacum brevicorniculatum.

    Science.gov (United States)

    Hillebrand, Andrea; Post, Janina J; Wurbs, David; Wahler, Daniela; Lenders, Malte; Krzyzanek, Vladislav; Prüfer, Dirk; Gronover, Christian Schulze

    2012-01-01

    The biosynthesis of rubber is thought to take place on the surface of rubber particles in laticifers, highly specialized cells that are present in more than 40 plant families. The small rubber particle protein (SRPP) has been supposed to be involved in rubber biosynthesis, and recently five SRPPs (TbSRPP1-5) were identified in the rubber-producing dandelion species Taraxacum brevicorniculatum. Here, we demonstrate by immunogold labeling that TbSRPPs are localized to rubber particles, and that rubber particles mainly consist of TbSRPP3, 4 and 5 as shown by high-resolution two-dimensional gel electrophoresis and mass spectrometric analysis. We also carried out an RNA-interference approach in transgenic plants to address the function of TbSRPPs in rubber biosynthesis as well as rubber particle morphology and stability. TbSRPP-RNAi transgenic T. brevicorniculatum plants showed a 40-50% reduction in the dry rubber content, but neither the rubber weight average molecular mass nor the polydispersity of the rubber were affected. Although no phenotypical differences to wild-type particles could be observed in vivo, rubber particles from the TbSRPP-RNAi transgenic lines were less stable and tend to rapidly aggregate in expelling latex after wounding of laticifers. Our results prove that TbSRPPs are very crucial for rubber production in T. brevicorniculatum, probably by contributing to a most favourable and stable rubber particle architecture for efficient rubber biosynthesis and eventually storage.

  18. Synthesis and Characterization of Surfactant PEG Macromonomers with Fluorocarbon End-capped Groups and its Copolymers

    Institute of Scientific and Technical Information of China (English)

    LIU, Shou-Ping; ZHUANG, Dong-Qing; ZHANG, Yun-Xiang; CHEN, Jun-Yan; JIANG, Ming; WU, Shu-Guang; SWIFT, Graham

    2001-01-01

    Fluorocarbon (RF) or hydrocarbon (RH) end-capped PEG macromonomers were prepared by coupling method. Several factors that affect the synthesis were studied and optimum condition was obtained. The critical micelle concentrations (CMC) of these macromonomers were determined by fluorescence method. A new type of fluorocarbon-containing hydrophobically modified alkali swellable/soluble copolymers were obtained by copolymerization of RF or RH alkyl endcapped PEG macromonomers with acrylic acid in organic solvent. The preliminary researches on viscosity property of these copolymer solutions were conducted under different conditions, such as various macromonomer content in the copolymer, polymer concentration, shear rate, pH value and temperature. All the results proved that there existed a very strong hydrophobic association among hydrophobes in these copolymer solutions.

  19. Stability and Hydrocarbon/Fluorocarbon Sorption of a Metal-Organic Framework with Fluorinated Channels

    Directory of Open Access Journals (Sweden)

    Jijiang Xie

    2016-04-01

    Full Text Available The stabilities and hydrocarbon/fluorocarbon sorption properties of a zeolite-like metal-organic framework (MOF Zn(hfipbb with fluorinated channels has been studied. By the combination of thermogravimetric analysis (TGA and powder X-ray diffraction (PXRD measurements, we confirm that Zn(hfipbb has exceptionally high hydrothermal and thermal stabilities. The adsorption behaviors of water and methanol by Zn(hfipbb indicate that it is highly hydrophobic but with high adsorption of alcohols. Hexane and perfluorohexane adsorption measurements show that the fluorinated channels in Zn(hfipbb have high affinity with hydrocarbon and fluorocarbon. The high fluorophilic nature of the channels and the high stability of the compound suggest its potential utility in practical separation applications.

  20. Robotically enhanced rubber hand illusion.

    Science.gov (United States)

    Arata, Jumpei; Hattori, Masashi; Ichikawa, Shohei; Sakaguchi, Masamichi

    2014-01-01

    The rubber hand illusion is a well-known multisensory illusion. In brief, watching a rubber hand being stroked by a paintbrush while one's own unseen hand is synchronously stroked causes the rubber hand to be attributed to one's own body and to "feel like it's my hand." The rubber hand illusion is thought to be triggered by the synchronized tactile stimulation of both the subject's hand and the fake hand. To extend the conventional rubber hand illusion, we introduce robotic technology in the form of a master-slave telemanipulator. The developed one degree-of-freedom master-slave system consists of an exoskeleton master equipped with an optical encoder that is worn on the subject's index finger and a motor-actuated index finger on the rubber hand, which allows the subject to perform unilateral telemanipulation. The moving rubber hand illusion has been studied by several researchers in the past with mechanically connected rigs between the subject's body and the fake limb. The robotic instruments let us investigate the moving rubber hand illusion with less constraints, thus behaving closer to the classic rubber hand illusion. In addition, the temporal delay between the body and the fake limb can be precisely manipulated. The experimental results revealed that the robotic instruments significantly enhance the rubber hand illusion. The time delay is significantly correlated with the effect of the multisensory illusion, and the effect significantly decreased at time delays over 100 ms. These findings can potentially contribute to the investigations of neural mechanisms in the field of neuroscience and of master-slave systems in the field of robotics.

  1. Mechanical properties of isolated fetal miniature pig lungs after substitution with fluorocarbons.

    Science.gov (United States)

    Widjaja, B; Wuthe, J; Schmidt, A; Seitz, B; Rüfer, R

    1988-01-01

    In our present study we tried to inflate and stabilize isolated immature lungs of fetal minipigs in gestation age of 95 days (= 85% of total normal gestation period) with different fluorocarbons. Based on our previous experiences, the immature lungs at day 95 are almost non inflatable with air. For our experiments we used fluorocarbon 43 (FC-43) with a surface tension of 16 mN/m and fluorocarbon 72 (FC-72) with a surface tension of 12 mN/m. Eighteen fetal immature lungs were used. In group 1 the lungs were rinsed with FC-43; in group 2 the rinse solution was FC-72, and in group 3 the lungs were untreated. After removing the fluorocarbon, in the case of groups 1 and 2, the lungs were artificially ventilated. Pressure-volume (p-v) curves were registered in the beginning (immediately after FC lavage), after 10 and 20 min of artificial ventilation. Airway opening pressure (pi) and weight-specific end-inspiratory lung compliance (ci) were investigated. Statistically significant differences in weight-specific end-inspiratory compliance were found between FC groups and untreated group 3, but no stabilization could be seen during the investigation period of 20 min. No statistically significant improvement in weight-specific end-inspiratory compliance was observed between group 1 and 2, although the compliances of group 2 with FC-72 were better than those of group 1 with FC-43 in three p-v diagrams registered in the beginning and after 10 and 20 min of artificial ventilation.(ABSTRACT TRUNCATED AT 250 WORDS)

  2. The Effect of Fluorocarbon Surfactant Additives on the Effective Viscosity of Acetone Solutions of Cellulose Diacetate,

    Science.gov (United States)

    2014-09-26

    34 FOREIGN TECHNOLOGY DIVISION i00 Lfl .. THE EFFECT OF FLUOROCARBON SURFACTANT ADDITIVES ON THE EFFECTIVE VISCOSITY OF ACETONE SOLUTIONS OF CELLULOSE ...ADDITIVES ON TH~ .. t- ’_ ition EFFECTIVE VISCOSITY OF ACETONE SOLUTIONS OF CELLULOSE DIACETATE D~rbt~l By: L.A. Shits, N. Yu. Kal’nova Codesuton English...VISCOSITY OF ACETONE SOLUTIONS OF CELLULOSE DIACETATE L. A. Shits, N. Yu. Kal’nova (Institute of Physical Chemistry of the AS USSR, Moscow) ! - The

  3. Surface characterization and platelet adhesion studies on fluorocarbons prepared by plasma-induced graft polymerization.

    Science.gov (United States)

    Lin, J C; Tiong, S L; Chen, C Y

    2000-01-01

    It is believed that the interactions between the biological environment and biomaterial surface are the key factors influencing its biocompatibility. Therefore, plasma processing, which can vary the surface properties without altering the bulk properties, has been considered as one of the important techniques for improving a materials' biocompatibility. In this investigation, plasma-induced grafting polymerization of vinylidene fluoride (VDF) and chlorotrifluoroethylene (CTFE), instead of direct plasma polymerization, was attempted with an aim to improve the substrate blood compatibility. Contact angle measurement indicated both fluorocarbon-grafted Pdyethylenes (PEs) are hydrophobic. Due to the additional fluorine and chlorine atoms on the CTFE chain, the PCTFE-grafted PE exhibited a higher hydrophobicity than the PVDF-grafted one. ESCA analysis has revealed that these two plasma-induced fluorocarbon deposits contain almost no CFx (x > 2) binding on the surface layer, indicating the grafting polymerization mainly follows the free radical mechanism instead of the molecule-highly-fragmented reaction steps commonly seen in the direct plasma polymerization treatment. In addition, ATR-FTIR has shown the surface chemical configuration of these PVDF- and PCTFE-grafted PEs to be very similar to those of the bulk samples of PVDF and PCTFE. The surface roughness decreased after oxygen plasma treatment and was further reduced by VDF and CTFE grafting polymerization. In vitro platelet adhesion testing indicated these two fluorocarbon grafted PEs are less platelet-activating than the nontreated PE control and oxygen plasma activated one.

  4. Absorption and recovery of n-hexane in aqueous solutions of fluorocarbon surfactants.

    Science.gov (United States)

    Xiao, Xiao; Yan, Bo; Fu, Jiamo; Xiao, Xianming

    2015-11-01

    n-Hexane is widely used in industrial production as an organic solvent. As an industrial exhaust gas, the contribution of n-hexane to air pollution and damage to human health are attracting increasing attention. In the present study, aqueous solutions of two fluorocarbon surfactants (FSN100 and FSO100) were investigated for their properties of solubilization and dynamic absorption of n-hexane, as well as their capacity for regeneration and n-hexane recovery by thermal distillation. The results show that the two fluorocarbon surfactants enhance dissolution and absorption of n-hexane, and their effectiveness is closely related to their concentrations in solution. For low concentration solutions (0.01%-0.30%), the partition coefficient decreases dramatically and the saturation capacity increases significantly with increasing concentration, but the changes for both are more modest when the concentration is over 0.30%. The FSO100 solution presents a smaller partition coefficient and a greater saturation capacity than the FSN100 solution at the same concentration, indicating a stronger solubilization for n-hexane. Thermal distillation is a feasible method to recover n-hexane from these absorption solutions, and to regenerate them. With 90sec heating at 80-85°C, the recovery of n-hexane ranges between 81% and 85%, and the regenerated absorption solution maintains its original performance during reuse. This study provides basic information on two fluorocarbon surfactants for application in the treatment of industrial n-hexane waste gases.

  5. Effect of temperature on deposition layer formation in HBr/N2/fluorocarbon-based plasma

    Science.gov (United States)

    Iwase, Taku; Yokogawa, Kenetsu; Mori, Masahito

    2017-06-01

    The effects of wafer temperature on etching rate and surface composition were investigated to clarify the surface reaction mechanism under HBr/N2/fluorocarbon-based gas plasma for developing a process for three-dimensional NAND flash devices. The etching rates of both polycrystalline silicon (poly-Si) and SiO2 were found to increase at a wafer temperature of 20 °C as compared with those at 60 °C. Comparing the gas combination of fluorocarbon/N2 and HBr/N2 mixtures, the temperature dependence of SiO2 etching rates was considered to relevant to the sticking probability of fluorocarbon polymers. To determine the cause of the temperature dependence of the poly-Si etching rate, surface composition was evaluated by thermal-desorption-spectroscopy and laser-sputtered-neutral-mass-spectrometry analyses. Ammonium bromide was confirmed in the deposition film at a wafer temperature of 20 °C. The observed increase in poly-Si etching rate at lower temperatures was possibly caused by increased amounts of nitrogen, hydrogen, and bromine fixed to the surface with the formation of ammonium bromide.

  6. Synthesis and applications of vegetable oil-based fluorocarbon water repellent agents on cotton fabrics.

    Science.gov (United States)

    Zhao, Tao; Zheng, Junzhi; Sun, Gang

    2012-06-05

    Vegetable oil-based fluorocarbon water repellent agents were prepared by chemical modifications of different vegetable oils - soybean and linseed oils through several reactions, including saponification, acidification, acylation of vegetable oil and trans-esterification with 2,2,2-trifluoroethanol and 2,2,3,3-tetrafluoropropanol. The resulted fluorocarbon agents were then copolymerized with styrene. The structures of the vegetable oil based agents were characterized by FT-IR and NMR. By evaluating water contact angle and time of water disappearance on cotton fabrics, as well as whiteness and breaking strength of cotton fabrics that were treated by these agents, optimum fabric finishing conditions were explored. The cotton fabrics finished with the vegetable oil-based fluorocarbon agents showed excellent water repellency, while other properties of the cotton fabrics declined to certain level. The linseed oil-based tetrafluoropropanol water repellent agent displayed the highest water repellency among all modified oils. All the treated fabrics exhibited good durability of water repellency. The linseed oil-based tetrafluoropropanol water repellent agent demonstrated the best durability among all repellent agents. Copyright © 2012 Elsevier Ltd. All rights reserved.

  7. Nano-reinforcement of tire rubbers: silica-technology for natural rubber : exploring the infuence of non-rubber constituents on the natural rubber-silica system

    NARCIS (Netherlands)

    Sarkawi, S.S.

    2013-01-01

    Natural rubber is a renewable resource material with outstanding properties which offers significant advantages over its counterparts, the fossil-resource synthetic rubbers. In fact, a natural rubber tree is an efficient carbon dioxide sequester. Since natural rubber is a natural product, it is subj

  8. Hydrogenated nitrile rubber for improved durability of automotive rubber parts

    Energy Technology Data Exchange (ETDEWEB)

    Mirza, J.; Leibbrandt, F.; Thoermer, J.

    1987-01-01

    Rubber articles with improved heat resistance and better performance characteristics are becoming of increasing importance for the automotive industry. A new type of elastomer has therefore been developed based on saturated hydrocarbon backbone - for improved heat resistance - with nitrile side groups providing good resistance to swelling. Some of the typical characteristics of hydrogenated nitrile rubber (HNBR) vulcanizates such as good physical properties pattern at elevated low temperatures dynamic properties, ozone resistance and swelling in automotive fluids are discussed. Potential applications are suggested to improve the performance of various rubber parts used in automotive applications such as high performance seals.

  9. Rubber friction on (apparently) smooth lubricated surfaces

    Energy Technology Data Exchange (ETDEWEB)

    Mofidi, M; Prakash, B [Division of Machine Elements, Luleaa University of Technology, Luleaa SE-97187 (Sweden); Persson, B N J [IFF, FZ-Juelich, 52425 Juelich (Germany); Albohr, O [Pirelli Deutschland AG, 64733 Hoechst/Odenwald, Postfach 1120 (Germany)

    2008-02-27

    We study rubber sliding friction on hard lubricated surfaces. We show that even if the hard surface appears smooth to the naked eye, it may exhibit short-wavelength roughness, which may make the dominant contribution to rubber friction. That is, the observed sliding friction is mainly due to the viscoelastic deformations of the rubber by the counterface surface asperities. The results presented are of great importance for rubber sealing and other rubber applications involving (apparently) smooth surfaces.

  10. Rubber friction on (apparently) smooth lubricated surfaces

    Science.gov (United States)

    Mofidi, M.; Prakash, B.; Persson, B. N. J.; Albohr, O.

    2008-02-01

    We study rubber sliding friction on hard lubricated surfaces. We show that even if the hard surface appears smooth to the naked eye, it may exhibit short-wavelength roughness, which may make the dominant contribution to rubber friction. That is, the observed sliding friction is mainly due to the viscoelastic deformations of the rubber by the counterface surface asperities. The results presented are of great importance for rubber sealing and other rubber applications involving (apparently) smooth surfaces.

  11. Rubberized Concrete Durability Against Abrasion

    Directory of Open Access Journals (Sweden)

    Md Noor Nurazuwa

    2016-01-01

    Full Text Available Durability performance of rubberized concrete against abrasion is presented in this paper. Surface depth loss was measured when abrasion load was constantly applied on concrete surface at each 500 interval rotation. Specimen with water-to cement ratio of 0.50 and 0.35 was prepared and tested at 28 days of curing age. In addition, 10% silica fume, SF was added to provide denser concrete and to understand its effectiveness against wear when added with crumb rubber. Results showed that crumb rubber shows good potential in providing abrasion resistance to concrete mix. However, in the case of rubberized concrete with silica fume, abrasion resistance was found to be slightly decreased with compressive strength more than 50N/mm2 due to the lack of low elastic modulus of CR particles to accommodate with denser cement matrix.

  12. Silicone-Rubber Stitching Seal

    Science.gov (United States)

    Wang, D. S.

    1985-01-01

    Fabric products protected from raveling by coating threads and filling stitching holes with silicone rubber. Uncored silicone rubber applied to stitching lines with air-pressurized sealant gun. Next, plastic release film placed on coated side, and blanket flipped over so release film lies underneath. Blanket then bagged and adhesive cured under partial vacuum of about 3.5 psi or under pressure. Applications include balloons, parachutes, ultralight aircraft, sails, rescue harnesses, tents, or other fabric products highly stressed in use.

  13. Superheated rubber for cold storage

    Energy Technology Data Exchange (ETDEWEB)

    Katzenberg, Frank; Heuwers, Benjamin; Tiller, Joerg Christian [Biomaterials and Polymer Science, Department of Biochemical and Chemical Engineering, TU Dortmund, D-44221 Dortmund (Germany)

    2011-04-26

    Highly stretched rubber cools down upon relaxation. A natural rubber material that stores high elongations up to 1000% strain upon strain-induced crystallization at room temperature is reported. The strain recovered and, with this, the stored ''cold'' is released only by a thermal or athermal trigger. (Copyright copyright 2011 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  14. Rubber mixing process and its relationship with bound rubber and crosslink density

    Science.gov (United States)

    Hasan, A.; Rochmadi; Sulistyo, H.; Honggokusumo, S.

    2017-06-01

    This research studied the relationship between bound rubber and crosslink density based on rubber mixing process. Bound rubber was obtained after natural rubber was masticated and mixed with rubber chemicals and filler while crosslink density was collected after rubber compound was vulcanized. Four methods are used and each method refers to four ways of incorporating carbon black during mixing. The first method, after rubber was masticated for 5 minutes, the addition of rubber chemicals and filler was done simultaneously. Rubber was masticated for 1 minute and continued mixing of rubber chemicals and filler where mixing was different from first method. This was the second method. The third method was the same as the second method but the filler used N 660 while in the second method N 330. The last method is not the same as the first and second, the rubber is only masticated for 3 minutes and then mixed with filler and followed by rubber chemicals sequentially. The results showed that bound rubber and crosslink density were influenced by mixing and mastication process. Bound rubber dropped and crosslink density was relatively stable in the first three mixing methods for increasing carbon black at the beginning of the mixing process. Bound rubber and crosslink density stated opposite results in the fourth mixing method. The higher the bound rubber the lower the crosslink density. Without regard to mixing methods, there is a non-linear relationship between bound rubber formation and crosslink density determination

  15. THERMAL CONDUCTIVITY OF RUBBERIZED GYPSUM BOARD

    Directory of Open Access Journals (Sweden)

    Taher Abu-Lebdeh

    2014-01-01

    Full Text Available The disposal of scrap tires is a challenging task and hence an innovative solution to meet these challenges is needed. Extensive work has been done on the utilization of waste tires in a variety of applications in asphalt pavements and concrete. However, previous investigations focus only on the mechanical properties of the rubberized materials, but few on the thermal performance. This is especially true for rubberized gypsum. Limited or no experimental data on the thermal performance of rubberized gypsum board are available. In this study, an experimental program is established to investigate the effect of amount and size of crumb rubber on the thermal properties of gypsum materials. Gypsum is replaced by four different percentage of crumb rubber: 10, 20, 30 and 40% by weight of gypsum and two sizes of crumb rubber (#30, #10_20 to make eight rubberized gypsum specimens. The prepared specimens were tested for thermal conductivity using an apparatus specially designed and constructed for this purpose. The experimental program was concluded by proposing an empirical equation to predict the thermal conductivity of rubberized gypsum board. Results indicated better thermal performance of the gypsum board due to the addition of crumb rubber. Thermal conductivity of the rubberized gypsum was 18-38% lower than the ordinary gypsum. It is concluded that thermal conductivity of rubberized gypsum decreases with the increase of crumb rubber regardless the size of the rubber and that thermal conductivity of mixtures contained 40% of rubber was about 38% lower than conventional mixture when crumb rubber #10_20 was added, while the thermal conductivity reduced by 22% when crumb rubber #30 was added. The study suggested for future work to investigate the effect of air voids size and ratio on the thermal conductivity of rubberized gypsum.

  16. Hydrophobically Modified Polyelectrolytes: V. Interaction of Fluorocarbon Modified Poly (acrylic acid) with Various Added Surfactants

    Institute of Scientific and Technical Information of China (English)

    ZHOU,Hui(周晖); SONG,Guo-Qaiang(宋国强); GUO,Jin-Feng(郭金峰); ZHANG,Yun-xiang (章云祥); DIEING,Reinhold; MA,Lian(马莲); HAEUSSLING,Lukas

    2001-01-01

    The interactions between fiuorocarbon-medified pol(sodium acrylate) and various kinds of added surfactant have been studied by means of viscometric measurement. Association behavior was found in both hydrogenated and fluorinated anionic, nonionic and cationic surfactants. Among them, the interactions between fluorocarbon-modified poly ( sodium acrylate) and cationic surfactants are the strongest, owing to the cooperation of both electrostatic attractions and hydrophobic associations. The anionic surfactants have the weakest effects on the solution properties because of the existence of unfavorable electrostatic repulsion. The hydrophobic interactions between copolymers and fluorinated surfactants are much stronger than those between copolymers and hydrogenated surfactants.

  17. Mesoporous Fluorinated Metal-Organic Frameworks with Exceptional Adsorption of Fluorocarbons and CFCs

    Energy Technology Data Exchange (ETDEWEB)

    Chen, Teng-Hao; Popov, Ilya; Kaveevivitchai, Watchareeya; Chuang, Yu-Chun; Chen, Yu-Sheng; Jacobson, Allan J.; Miljani,; #263; Ognjen, Š. [NSRRC; (UC); (Houston)

    2016-02-08

    Two mesoporous fluorinated metal–organic frameworks (MOFs) were synthesized from extensively fluorinated tritopic carboxylate- and tetrazolate-based ligands. The tetrazolate-based framework MOFF-5 has an accessible surface area of 2445 m2g-1, the highest among fluorinated MOFs. Crystals of MOFF-5 adsorb hydrocarbons, fluorocarbons, and chlorofluorocarbons (CFCs)—the latter two being ozone-depleting substances and potent greenhouse species—with weight capacities of up to 225%. The material exhibits an apparent preference for the adsorption of non-spherical molecules, binding unusually low amounts of both tetrafluoromethane and sulfur hexafluoride.

  18. Properties of solid polymer electrolyte fluorocarbon film. [used in hydrogen/oxygen fuel cells

    Science.gov (United States)

    Alston, W. B.

    1973-01-01

    The ionic fluorocarbon film used as the solid polymer electrolyte in hydrogen/oxygen fuel cells was found to exhibit delamination failures. Polarized light microscopy of as-received film showed a lined region at the center of the film thickness. It is shown that these lines were not caused by incomplete saponification but probably resulted from the film extrusion process. The film lines could be removed by an annealing process. Chemical, physical, and tensile tests showed that annealing improved or sustained the water contents, spectral properties, thermo-oxidative stability, and tensile properties of the film. The resistivity of the film was significantly decreased by the annealing process.

  19. Natural rubber latex allergy

    Directory of Open Access Journals (Sweden)

    Deval Ravi

    2008-01-01

    Full Text Available Natural rubber latex (NRL is a ubiquitous allergen as it is a component of > 40,000 products in everyday life. Latex allergy might be attributed to skin contact or inhalation of latex particles. Latex allergy is an IgE-mediated hypersensitivity to NRL, presenting a wide range of clinical symptoms such as angioedema, swelling, cough, asthma, and anaphylactic reactions. Until 1979, latex allergy appeared only as type IV delayed hypersensitivity; subsequently, the proportion of different allergy types drifted towards type IV contact allergy reactions. Several risk factors for sensitization to NRL are already known and well documented. Some authors have established a positive correlation between a history of multiple surgical interventions, atopy, spina bifida malformation, and latex allergy incidence. We suspect an increase in latex allergy incidence in association with increased atopy and sensitivity to environmental allergens in the industrial population. It is often postulated in literature that the groups of workers at risk for this allergy are essentially workers in the latex industry and healthcare professionals. In this population, direct internal and mucosal contact with NRL medical devices may be the route of sensitization as factors such as the number of procedures and use of NRL materials (catheters and tubes were associated with increased risk of latex sensitization and allergy.

  20. Synthesis and optical activity of isosorbide chiral derivative containing fluorocarbon group as chiral dopant in liquid crystal materials

    Institute of Scientific and Technical Information of China (English)

    Kong Liang Xie; Yin He Su; Chun Xiang Zhang

    2011-01-01

    Novel isosorbide derivative containing perfluorocarbon group, bi(perfluorooctanesulfonyl)isosorbide ester as chiral dopant in liquid crystal, was synthesized. Chemical structure was characterized by elemental analysis, FT-IR, 1H NMR and 19F NMR. The optical texture of the mixture was observed by polarized optical microscopy (POM). Novel chiral dopant containing perfluorocarbon group had excellent optical activity. Its specific rotation and molar rotation were noticeable higher than those of bi(4-chloromethylbenzenecarbonic)isosorbide ester. The fluorocarbon group improved the molar rotation of chiral compound and did not affect optical rotation direction. The texture of the mixture added isosorbide derivative with fluorocarbon group showed the oily streak texture.

  1. Isoprene Rubber Has Broad Market Potential

    Institute of Scientific and Technical Information of China (English)

    Xu Qingsbeng

    2007-01-01

    @@ Isoprene Rubber (IR) is a macro molecular substance polymerized from isoprene monomer, with a structure and properties that are basically similar to those of natural rubber (NR). It features excellent elasticity, wear resistance,heat resistance, low temperature flexibility, etc.

  2. 75 FR 57980 - Polychloroprene Rubber From Japan

    Science.gov (United States)

    2010-09-23

    ... From the Federal Register Online via the Government Publishing Office INTERNATIONAL TRADE COMMISSION Polychloroprene Rubber From Japan AGENCY: United States International Trade Commission. ACTION... whether revocation of the antidumping duty finding on polychloroprene rubber from Japan would be likely to...

  3. Advances in rubber/halloysite nanotubes nanocomposites.

    Science.gov (United States)

    Jia, Zhixin; Guo, Baochun; Jia, Demin

    2014-02-01

    The research advances in rubber/halloysite nanotubes (rubber/HNTs) nanocomposites are reviewed. HNTs are environmentally-friendly natural nanomaterials, which could be used to prepare the rubber-based nanocomposites with high performance and low cost. Unmodified HNTs could be adopted to prepare the rubber/HNTs composites with improved mechanical properties, however, the rubber/HNTs nanocomposites with fine morphology and excellent properties were chiefly prepared with various modifiers by in situ mixing method. A series of rubber/HNTs nanocomposites containing several rubbers (SBR, NR, xSBR, NBR, PU) and different modifiers (ENR, RH, Si69, SA, MAA, ILs) have been investigated. The results showed that all the rubber/HNTs nanocomposites achieved strong interfacial interaction via interfacial covalent bonds, hydrogen bonds or multiple interactions, realized significantly improved dispersion of HNTs at nanoscale and exhibited excellent mechanical performances and other properties.

  4. Fundamental studies on dynamic wear behavior of SBR rubber compounds modified by SBR rubber powder

    OpenAIRE

    Euchler, Eric; Heinrich, Gert; Michael, Hannes; Gehde, Michael; Stocek, Radek; Kratina, Ondrej; Kipscholl, Reinhold; Bunzel, Jörg-Michael; Saal, Wolfgang

    2016-01-01

    The aim of this study is focused on the experimental investigation of dynamic wear behavior of carbon black filled rubber compounds comprising pristine styrene butadiene rubber (SBR) together with incorporated SBR ground rubber (rubber powder). We also analyzed and described quantitatively the service conditions of some dynamically loaded rubber products, which are liable to wear (e.g. conveyor belts, tires). Beside the well-known standard test method to characterize wear resistance at steady...

  5. 75 FR 38119 - Polychloroprene Rubber From Japan

    Science.gov (United States)

    2010-07-01

    ... COMMISSION Polychloroprene Rubber From Japan AGENCY: United States International Trade Commission. ACTION: Institution of a five-year review concerning the antidumping duty finding on polychloroprene rubber from Japan... antidumping duty finding on polychloroprene rubber from Japan would be likely to lead to continuation or...

  6. Morphology, Tensile Strength and Oil Resistance of Gum Rubber Sheets Prepared from Lignin Modified Natural Rubber

    Directory of Open Access Journals (Sweden)

    Asrul M.

    2014-07-01

    Full Text Available The paper describes the preparation of lignin filled natural rubber latex composite and its subsequent use to obtain lignin modified rubber. Two types of lignin i.e.: rubber wood and commercial alkali lignin were used as rubber filler. Gum rubber sheets were prepared from the lignin modified rubber and their properties were compared to Standard Malaysian Rubber (SMR 20 and a type of rubber obtained from the coagulation of high ammonia latex. Rubber morphology was investigated using Scanning Electron Microscope on the cross-sectional area of cryo-fractured samples. Oil resistance of the rubber sheets was determined by measuring the mass change before and after ASTM IRM 903 oil immersion, while the tensile strengths were determined according to ASTM D412 standard. Low values of tensile strength obtained for the commercial alkali lignin modified rubber sheet relative to the rest of the rubber samples was attributed to poor lignin dispersion. This occurrence was substantiated by the SEM analysis of cryo-fractured samples where crazes and inhomogeneity was observed. Nonetheless, both lignin modified rubbers exhibited higher level of oil resistance compared to SMR 20. This is due to the nature of lignin as a hydrophilic component and its presence in the rubber matrix complicates the oil diffusion process into rubber.

  7. Modeling the liquid-liquid equilibria of water plus fluorocarbons with the cubic-plus-association equation of state

    DEFF Research Database (Denmark)

    Oliveira, Mariana B.; Freire, Mara G.; Marrucho, Isabel M.

    2007-01-01

    Fluorocarbons (FCs) are a family of chemicals that are composed primarily of carbon and fluorine. They present weak intermolecular and strong intramolecular interactions, which confers them unusual thermophysical properties. They can also solubilize large amounts of gases such as oxygen and carbo...

  8. Blue rubber bleb naevus syndrome

    DEFF Research Database (Denmark)

    Lybecker, Martin Bell; Stawowy, Marek; Clausen, Niels

    2016-01-01

    Blue rubber bleb naevus syndrome (BRBNS) is a rare vascular disorder with malformed veins, or blebs, appearing in the skin or internal organs. Gastrointestinal tract involvement is the most common feature and often subject to bleeding, potentially resulting in chronic occult blood loss and iron...

  9. Application of fluorocarbon remover DEF%氟树脂去除剂DEF的应用

    Institute of Scientific and Technical Information of China (English)

    董玲

    2012-01-01

    The fluorochemical water- and oil- repeffent on textiles must be stripped firstly in color restoration of finished polyester dyeings. The stripping process is carried out by immersion method with fluorocarbon remover DEF. Influences of remover dosage, NaOH dosage, stripping temperature and time on the stripping effects are investigated according to the water- and oil- repellent effect of polyester fabric before and after washing. The optimum stripping process is as follows; fluorocarbon remover DEF 1.0~1.5 g/L,Na0H 1 g/L, material ratio 1:20, stripping at 90~100 ℃ for 20 min. The results show that fluorocarbon re-mover DEF features good stripping effect. The water repellent effect of refinished fabric reaches 100 and the oil-repellent effect is 5. The refinished fabric has a little change in K/S value and a little decrease in tear strength.%含氟拒水拒油整理涤纶染色布修色时,需先剥除拒水拒油整理剂.试验采用氟树脂去除剂DEF,以浸渍法剥除织物上的整理剂.根据水洗前后织物的拒水拒油性能,讨论了去除剂用量、烧碱用量、温度、时间对剥除效果的影响,优化的剥除工艺为:去除剂DEF1.0-1.5 g/L,烧碱1 g/L,浴比1:20,温度90-100℃,时间20 min.结果表明,去除剂DEF可有效地剥除含氟整理剂,重新整理后织物拒水等级达到100分,拒油级别达到5级,对色光影响较小,强力稍有下降.

  10. In-depth proteome analysis of the rubber particle of Hevea brasiliensis (para rubber tree).

    Science.gov (United States)

    Dai, Longjun; Kang, Guijuan; Li, Yu; Nie, Zhiyi; Duan, Cuifang; Zeng, Rizhong

    2013-05-01

    The rubber particle is a special organelle in which natural rubber is synthesised and stored in the laticifers of Hevea brasiliensis. To better understand the biological functions of rubber particles and to identify the candidate rubber biosynthesis-related proteins, a comprehensive proteome analysis was performed on H. brasiliensis rubber particles using shotgun tandem mass spectrometry profiling approaches-resulting in a thorough report on the rubber particle proteins. A total of 186 rubber particle proteins were identified, with a range in relative molecular mass of 3.9-194.2 kDa and in isoelectric point values of 4.0-11.2. The rubber particle proteins were analysed for gene ontology and could be categorised into eight major groups according to their functions: including rubber biosynthesis, stress- or defence-related responses, protein processing and folding, signal transduction and cellular transport. In addition to well-known rubber biosynthesis-related proteins such as rubber elongation factor (REF), small rubber particle protein (SRPP) and cis-prenyl transferase (CPT), many proteins were firstly identified to be on the rubber particles, including cyclophilin, phospholipase D, cytochrome P450, small GTP-binding protein, clathrin, eukaryotic translation initiation factor, annexin, ABC transporter, translationally controlled tumour protein, ubiquitin-conjugating enzymes, and several homologues of REF, SRPP and CPT. A procedure of multiple reaction monitoring was established for further protein validation. This comprehensive proteome data of rubber particles would facilitate investigation into molecular mechanisms of biogenesis, self-homeostasis and rubber biosynthesis of the rubber particle, and might serve as valuable biomarkers in molecular breeding studies of H. brasiliensis and other alternative rubber-producing species.

  11. Domain Structure in Calcium-Cerium Fluorocarbonate Minerals, Mianning County, Sichuan Province, China

    Institute of Scientific and Technical Information of China (English)

    2000-01-01

    The domain structures in calcium-cerium fluorocarbonate mineral series from a rare earth mineral deposit within an aegirine alkali granite massif in Mianning County, Sichuan Province, China, were studied by means of transmission electron microscopy. Many categories of domain structures in this mineral series were observed and investigated, including the microtwin domains of parisite-6R2 and B2S-6R, the antiphase domains of B2S-2H. The results show that the antiphase domains which are faults along crystal plane (0001) are formed by the displacement of crystal lattice in c* direction and the displacement is 0.471 nm. A new polytype (B4S2-3R) of regular mixed-layer structure with B4S2 type is found in the domain region of mixed-layer structure.

  12. Development of molecular based optical techniques for thermometry and velocimetry for fluorocarbon media

    Science.gov (United States)

    Pouya, Shahram; Blanchard, Gary; Koochesfahani, Manoochehr

    2016-11-01

    Fluorocarbon solvents are very stable inert fluids with unique physical properties that make them attractive compounds as refrigerant and several medical applications such as contrast enhanced ultrasound imaging. Since they do not mix with typical organic solvents or water, most luminescent (fluorescent or phosphorescent) probes cannot be used as tracers for optical diagnostic techniques. Perfluoropentane, a compound from this family, is used as a simulant fluid by NASA for two-phase heat transfer/mixing experiments under micro-gravity condition due to its low boiling temperature. Here we study the feasibility of employing non-intrusive optical methods for measurements of temperature and/or velocity within Perfluoropentane as the working fluid. Preliminary results of temperature and velocity measurement using Laser Induced Fluorescence and Molecular Tagging Velocimetry are presented. This work was supported by NASA Grant Number NNX16AD52A.

  13. Development of fluorocarbon evaporative cooling recirculators and controls for the ATLAS inner silicon tracker

    CERN Document Server

    Bayer, C; Bonneau, P; Bosteels, Michel; Burckhart, H J; Cragg, D; English, R; Hallewell, G D; Hallgren, Björn I; Ilie, S; Kersten, S; Kind, P; Langedrag, K; Lindsay, S; Merkel, M; Stapnes, Steinar; Thadome, J; Vacek, V

    2000-01-01

    We report on the development of evaporative fluorocarbon cooling recirculators and their control systems for the ATLAS inner silicon tracker. We have developed a prototype circulator using a dry, hermetic compressor with C/sub 3/F/sup 8/ refrigerant, and have prototyped the remote-control analog pneumatic links for the regulation of coolant mass flows and operating temperatures that will be necessary in the magnetic field and radiation environment around ATLAS. pressure and flow measurement and control use 150+ channels of standard ATLAS LMB ("Local Monitor Board") DAQ and DACs on a multi-drop CAN network administered through a BridgeVIEW user interface. A hardwired thermal interlock system has been developed to cut power to individual silicon modules should their temperatures exceed safe values. Highly satisfactory performance of the circulator under steady state, partial-load and transient conditions was seen, with proportional fluid flow tuned to varying circuit power. Future developments, including a 6 kW...

  14. Fluorocarbons and cardiac arrhythmia: does difluorodichloromethane (FC 12) inhibit cardiac metabolism

    Energy Technology Data Exchange (ETDEWEB)

    Lessard, Y.; Begue, J.M.; Paulet, G.

    1986-01-01

    Certain fluorocarbons, such as difluorodichloromethane (FC 12), depress the cardiovascular system by diminution of all the transmembrane ionic conductances in cardiac tissues. Does FC 12 also inhibit active transport and thus enzymatic activity and cellular energy. We measured phosphocreatine (PC), adenosine triphosphate (ATP) and cyclic adenosine monophosphate (AMPc) in rat hearts. Rats were randomly divided into 4 groups; 2 control groups: one breathing a mixture of oxygen (21%) and nitrogen (79%) (group C) and the other breathing the same mixture but simultaneously perfused with 1 microgram/kg/min. epinephrine (groupe E-C); 2 trial groups T and E-T where nitrogen was replaced by FC 12. The maximal FC 12 concentration of 720 micrograms/ml in arterial blood produced no significant difference in the concentrations of these three metabolites compared with controls.

  15. Growth of Fluorocarbon Films by Low-Pressure Dielectric Barrier Discharge

    Institute of Scientific and Technical Information of China (English)

    LI Wei; TAN Xiaodong; LIU Dongping; LIU Yanhong; FENG Zhiqing; CHEN Baoxiang

    2008-01-01

    Plasma polymerized fluorocarbon (FC) films have been deposited on silicon sub-strates from dielectric barrier discharge (DBD) plasma of C4Fs at room temperature under a pressure of 25~125 Pa. The effects of the discharge pressure and frequency of power supply on the films have been systematically investigated. FC films with a less cross linked structure may be formed at a relatively high pressure. Increase in the frequency of power supply leads to a signifi-cant increase in the deposition rate. Static contact angle measurements show that deposited FC films have a stable, hydrophobic surface property. All deposited films show smooth surfaces with an atomic surface roughness. The relationship between plasma parameters and the properties of the deposited FC films are discussed.

  16. Hydrophobically modified polyelectrolytes I. Dilute solution properties of fluorocarbon-containingpoly(acrylic acid)

    Institute of Scientific and Technical Information of China (English)

    ZHOU, Hui(周晖); SONG, Guo-Qiang(宋国强); ZHANG, Yun-Xiang(章云祥); DIEING, Reinhold; MA, Lian; HAEUSSLING, Lukas

    2000-01-01

    Dilute solution viscosity of fluorocarbon-containing hydrophobically modified poly(acrylic acid) was measured in aqueous solutions of various NaCl concentrations. The intrinsic viscosity ([η]) and Huggins coefficient (kH) were evaluated using Huggins equations. It is found that, at low NaCl concentration, the modified polymers exhibit values of intrinsic viscosity ( [η] ) and Huggins coefficient (kH) similar to those of unmodified polymers. For both of the modified and unmodified polymers, the intrinsic viscosity decreases with increase of NaCl concentration, while the Huggins coefficient increases upon addition of NaCl. But the variation of [η] and kH is more significant for the modified polymers, which reflects the enhanced intra- and intermolecular hydrophobic association at higher NaCl concentration.

  17. Assessment of effects on vegetation of degradation products from alternative fluorocarbons

    Science.gov (United States)

    Mccune, D. C.; Weinstein, L. H.

    1990-01-01

    Concern with the effects of fluorides on plants has been devoted to that resulting from dry deposition (mainly with reference to gaseous HF and secondarily with particulate forms). The occurrence of precipitation as rain or mist and the presence of dew or free water on the foliage has mainly been considered with respect to their effects on the accumulation of air-borne fluoride and not with fluoride in wet deposition. That is, precipitation has been viewed primarily with respect to its facilitation of the solution and subsequent absorption of deposits by the foliar tissues or its elution of deposited fluoride from foliage. Accordingly, our evaluation of inorganic fluoride from fluorocarbon degradation rests upon a comparison with what is known about the effects of industrial emissions and what could be considered the natural condition.

  18. Preparation of transparent fluorocarbon/TiO2-SiO2 composite coating with improved self-cleaning performance and anti-aging property

    Science.gov (United States)

    Zhou, Jianping; Tan, Zhongyuan; Liu, Zhilei; Jing, Mengmeng; Liu, Wenjie; Fu, Wanli

    2017-02-01

    This work reports a facile method to fabricate transparent self-cleaning fluorocarbon coatings filled by semicrystalline colloidal particles of TiO2-SiO2 composite oxide presenting a particle size ranging from 6 to 10 nm. Anatase-TiO2 crystallites were successfully obtained after microwave heating treatment of the TiO2-SiO2 colloidal particles as confirmed by XRD, TEM and FTIR measurements. The fluorocarbon/TiO2-SiO2 composite coatings exhibited a superior hydrophilicity and an improved photocatalytic activity in contrast to the TiO2-filled coatings. In particular, a water contact angle (WCA) value of 4.5° and a decolorization ratio relative to methyl orange as high as 96.0% were achieved for the composite coatings containing 1.5 wt% of TiO2-SiO2 colloidal particles. The results of the anti-soiling experiments indicated that the fluorocarbon/TiO2-SiO2 composite coatings exhibited a prominent self-cleaning performance, while the accelerated aging experiments revealed that the fluorocarbon/TiO2-SiO2 composite coatings were highly stable toward UV irradiation when compared to the TiO2-filled fluorocarbon coatings. These findings indicated that the fluorocarbon/TiO2-SiO2 composite coatings could be a very attractive solution for many practical areas, especially for outdoor applications.

  19. Thermomechanical characterisation of cellular rubber

    Science.gov (United States)

    Seibert, H.; Scheffer, T.; Diebels, S.

    2016-09-01

    This contribution discusses an experimental possibility to characterise a cellular rubber in terms of the influence of multiaxiality, rate dependency under environmental temperature and its behaviour under hydrostatic pressure. In this context, a mixed open and closed cell rubber based on an ethylene propylene diene monomer is investigated exemplarily. The present article intends to give a general idea of the characterisation method and the considerable effects of this special type of material. The main focus lies on the experimental procedure and the used testing devices in combination with the analysis methods such as true three-dimensional digital image correlation. The structural compressibility is taken into account by an approach for a material model using the Theory of Porous Media with additional temperature dependence.

  20. Constructing better roads with asphalt rubber

    Directory of Open Access Journals (Sweden)

    Pais Jorge C.

    2015-12-01

    Full Text Available Brazilians mixtures containing asphalt rubber were evaluated by mechanical laboratory tests. A conventional mixture with asphalt CAP-50/70 was produced as a mixture control. With the aim of compare the Brazilians mixtures performance, a Portuguese asphalt rubber mixture was tested as well. The testing set involved the determination of the mechanical properties, fatigue and permanent deformation, of asphalt rubber produced by wet process through two different systems: continuous blend and terminal blend. The asphalt rubber morphology was evaluated in order to determine the compatibility of the systems. The asphalt rubber mixtures exhibit good resistance to permanent deformation and prolonged fatigue life in relation to mixture control. Therefore it is concluded that the application of asphalt rubber alters the characteristics of asphalt mixture in a very beneficial way.

  1. Prehistoric polymers: rubber processing in ancient mesoamerica

    Science.gov (United States)

    Hosler; Burkett; Tarkanian

    1999-06-18

    Ancient Mesoamerican peoples harvested latex from Castilla elastica, processed it using liquid extracted from Ipomoea alba (a species of morning glory vine), and fashioned rubber balls, hollow rubber figurines, and other rubber artifacts from the resulting material. Chemical and mechanical analyses of the latex and of the processed rubber indicate that the enhanced elastic behavior of the rubber relative to the unprocessed latex is due to purification of the polymer component and to an increase in the strength and number of interchain interactions that are induced by organic compounds present in I. alba. These ancient peoples' control over the properties of latex and processed rubber gave rise to the Mesoamerican ball game, a central ritual element in all ancient Mesoamerican societies.

  2. Impregnation of Natural Rubber into Rubber Wood: A Green Wood Composite

    OpenAIRE

    Wassa Ruayruay; Sureurg Khongtong

    2014-01-01

    A green wood composite material was developed from the two environmentally friendly substrates natural rubber (cis-1,4-polyisoprene) and rubber wood (Hevea brasiliensis). Natural rubber (NR) was introduced into rubber wood by pressurization of NR latex, followed by the removal of the aqueous phase to allow only dry NR to remain inside the wood structure. Scanning electron microscopy images and the weight increase of the dry impregnated samples revealed the retention of dry NR within the rubbe...

  3. VULCANIZATION KINETICS OF SILICONE RUBBER

    Institute of Scientific and Technical Information of China (English)

    YUAN Qiang; LI Yufu; LI Guangliang

    1988-01-01

    Vulcanization rate of silicone rubber with the aid of organic peroxide or hydrosilylation agent was studied by using oscillation disk rheometer. It was found that the process of network formation would take place through one, two or three steps depending on the structure of the reactants. The effect of phenyl group, vinyl terminals on polysiloxane chain and the functionality of silylation agent was also studied.

  4. Chemistry of rubber processing and disposal.

    Science.gov (United States)

    Bebb, R L

    1976-10-01

    The major chemical changes during the processing of rubber occur with the breakdown in mastication and during vulcanization of the molded tire. There is little chemical change during the compounding, calendering, extrusion, and molding steps. Reclaiming is the process of converting scrap rubber into an unsaturated, processible product that can be vulcanized with sulfur. Pyrolysis of scrap rubber yields a complex mixture of liquids, gas, and residue in varying ratios dependent on the nature of the scrap and the conditions of pyrolysis.

  5. Rubber friction: comparison of theory with experiment.

    Science.gov (United States)

    Lorenz, B; Persson, B N J; Dieluweit, S; Tada, T

    2011-12-01

    We have measured the friction force acting on a rubber block slid on a concrete surface. We used both unfilled and filled (with carbon black) styrene butadiene (SB) rubber and have varied the temperature from -10 °C to 100 °C and the sliding velocity from 1 μm/s to 1000 μm/s. We find that the experimental data at different temperatures can be shifted into a smooth master-curve, using the temperature-frequency shifting factors obtained from measurements of the bulk viscoelastic modulus. The experimental data has been analyzed using a theory which takes into account the contributions to the friction from both the substrate asperity-induced viscoelastic deformations of the rubber, and from shearing the area of real contact. For filled SB rubber the frictional shear stress σ(f) in the area of real contact results mainly from the energy dissipation at the opening crack on the exit side of the rubber-asperity contact regions. For unfilled rubber we instead attribute σ(f) to shearing of a thin rubber smear film, which is deposited on the concrete surface during run in. We observe very different rubber wear processes for filled and unfilled SB rubber, which is consistent with the different frictional processes. Thus, the wear of filled SB rubber results in micrometer-sized rubber particles which accumulate as dry dust, which is easily removed by blowing air on the concrete surface. This wear process seams to occur at a steady rate. For unfilled rubber a smear film forms on the concrete surface, which cannot be removed even using a high-pressure air stream. In this case the wear rate appears to slow down after some run in time period.

  6. Chemical modifications of liquid natural rubber

    Science.gov (United States)

    Azhar, Nur Hanis Adila; Rasid, Hamizah Md; Yusoff, Siti Fairus M.

    2016-11-01

    Liquid natural rubber (LNR) was synthesized via photosentisized degradation of natural rubber (NR). LNR was modified into epoxidized liquid natural rubber (LENR) and hydroxylated liquid natural rubber (LNR-OH) using Na2WO4/CH3COOH/H2O2 catalytic system. Chemical structures of LNR and modified LNRs were characterized using Attenuated Total Reflectance Fourier Transform Infrared (ATR-FTIR) and 1H Nuclear Magnetic Resonance (NMR) spectroscopies. Integration of 1H NMR was used to calculate the epoxy content (%) of LENR. 1H NMR detected the formation of LNR-OH after prolonged heating and increased of catalyst in oxidation reaction.

  7. Malaria-associated rubber plantations in Thailand.

    Science.gov (United States)

    Bhumiratana, Adisak; Sorosjinda-Nunthawarasilp, Prapa; Kaewwaen, Wuthichai; Maneekan, Pannamas; Pimnon, Suntorn

    2013-01-01

    Rubber forestry is intentionally used as a land management strategy. The propagation of rubber plantations in tropic and subtropic regions appears to influence the economical, sociological and ecological aspects of sustainable development as well as human well-being and health. Thailand and other Southeast Asian countries are the world's largest producers of natural rubber products; interestingly, agricultural workers on rubber plantations are at risk for malaria and other vector-borne diseases. The idea of malaria-associated rubber plantations (MRPs) encompasses the complex epidemiological settings that result from interactions among human movements and activities, land cover/land use changes, agri-environmental and climatic conditions and vector population dynamics. This paper discusses apparent issues pertaining to the connections between rubber plantations and the populations at high risk for malaria. The following questions are addressed: (i) What are the current and future consequences of rubber plantations in Thailand and Southeast Asia relative to malaria epidemics or outbreaks of other vector-borne diseases? (ii) To what extent is malaria transmission in Thailand related to the forest versus rubber plantations? and (iii) What are the vulnerabilities of rubber agricultural workers to malaria, and how contagious is malaria in these areas?

  8. A nanoscale fluorocarbon coating on PET surfaces improves the adhesion and growth of cultured coronary endothelial cells

    Energy Technology Data Exchange (ETDEWEB)

    Pezzatini, S; Morbidelli, L; Ziche, M [Section of Pharmacology, Department of Molecular Biology, University of Siena, Via Aldo Moro 2, 53100 Siena (Italy); Gristina, R [IMIP, CNR, University of Bari, Via Orabona 4, 70126 Bari (Italy); Favia, P [Department of Chemistry, University of Bari, Via Orabona 4, 70126 Bari (Italy)], E-mail: ziche@unisi.it

    2008-07-09

    Plasma deposition was applied to deposit smooth and nanostructured fluorocarbon coatings on polyethylene terephthalate substrates, with the aim to obtain surfaces with identical chemical composition but different roughness to improve the endothelialization process on PET surfaces. We found that increased roughness was associated with enhanced endothelial cell response, as shown by the ability of cells to grow and adhere to nanostructures. We also observed specific interaction of filopodia protruding from the cell membrane with individual nanostructures, leading to increased cell attachment, spreading and cell viability. Among the modified surfaces, one termed PET-tfl90 emerged as the one capable of best sustaining the formation of a confluent monolayer of endothelial cells. In conclusion, PET modified by nanostructured fluorocarbon film represents an improved graft material, over conventional PET, for endothelial cell adhesion and growth.

  9. Influence of crumb rubber and digestion time on the asphalt rubber binders

    OpenAIRE

    Neto, Silvrano Adonias Dantas; De Farias, Márcio Muniz; Pais, Jorge C.; Pereira, Paulo A. A.; Sousa, Jorge B.

    2006-01-01

    This paper shows the results of a study about the mechanical behavior of dense graded asphalt-rubber hot mixes prepared with two different types of asphalt-rubber binders. These asphalt-rubber binders were obtained with penetration grade asphalt (AC 50/70) mixed with 21% and 25% of crumb rubber in weight. The rubber was recycled from unserviceable tires using the ambient grinding process. Hot mixes made with the conventional binder AC 50/70 were also studied for comparison. The...

  10. EPDM Rubber Reclaim from Devulcanized EPDM

    NARCIS (Netherlands)

    Sutanto, P.; Picchioni, F.; Janssen, L.P.B.M.; Dijkhuis, K.A.J.; Dierkes, Wilma K.; Noordermeer, Jacobus W.M.

    2006-01-01

    Two types of ethylene-propylene-diene monomer (EPDM) rubbers, namely an efficient vulcanized (EV) and a semiefficient vulcanized (SEV), have been used to produce devulcanizates in a continuous setup. The devulcanizates are re-cured using the same recipes as for the virgin rubber. The influence of

  11. EPDM rubber reclaim from devulcanized EPDM

    NARCIS (Netherlands)

    Sutanto, P.; Picchioni, F.; Janssen, L. P. B. M.; Dijkhuis, K. A. J.; Dierkes, W. K.; Noordermeer, J. W. M.

    2006-01-01

    Two types of ethylene-propylene-diene monomer (EPDM) rubbers, namely an efficient vulcanized (EV) and a serniefficient vulcanized (SEV), have been used to produce devulcanizates in a continuous setup. The devulcanizates are re-cured using the same recipes as for the virgin rubber. The influence of

  12. Unraveling the Mystery of Natural Rubber Biosynthesis

    Science.gov (United States)

    Natural rubber (NR) is primarily obtained from Hevea brasiliensis, commonly known as the Brazilian rubber tree. As this species contains little genetic variation, it is susceptible to pathogen-based eradication. Consequently, it is imperative that a biomimetic pathway for NR production be developed....

  13. EPDM rubber reclaim from devulcanized EPDM

    NARCIS (Netherlands)

    Sutanto, P.; Picchioni, F.; Janssen, L. P. B. M.; Dijkhuis, K. A. J.; Dierkes, W. K.; Noordermeer, J. W. M.

    2006-01-01

    Two types of ethylene-propylene-diene monomer (EPDM) rubbers, namely an efficient vulcanized (EV) and a serniefficient vulcanized (SEV), have been used to produce devulcanizates in a continuous setup. The devulcanizates are re-cured using the same recipes as for the virgin rubber. The influence of m

  14. Biorefinery of proteins from rubber plantation residues

    NARCIS (Netherlands)

    Widyarani, R.

    2016-01-01

    Biorefinery of rubber tree side streams could add economic value and income for farmers, who already grow the trees for latex production. The objective of this research was to design a process for the recovery of proteinaceous fractions from rubber tree. The aimed applications were expected to be su

  15. Rheological testing of crumb rubber modified bitumen

    CSIR Research Space (South Africa)

    Mturi, GAJ

    2011-08-01

    Full Text Available used to analyse crumb rubber modified (CRM) bitumen is that the specified gap setting in the configuration of the DSR between the upper and lower test platens is too small to accommodate crumb rubber particles. DSR testing of CRM bitumen therefore...

  16. Biorefinery of proteins from rubber plantation residues

    NARCIS (Netherlands)

    Widyarani, R.

    2016-01-01

    Biorefinery of rubber tree side streams could add economic value and income for farmers, who already grow the trees for latex production. The objective of this research was to design a process for the recovery of proteinaceous fractions from rubber tree. The aimed applications were expected to be su

  17. Better Tomorrow of China Rubber Chemicals Industry

    Institute of Scientific and Technical Information of China (English)

    2011-01-01

    I. Development of China Rubber Chemicals Industry During the "11th Five-Year Plan" period, China rubber Chemicals industry fully implemented the development guideline of "Adhering to science and technology development, developing green chemistry with environmental protection, safety and energy conservation as the core, and building enterprise and world brands". With the great support of the state,

  18. Zinc leaching from tire crumb rubber.

    Science.gov (United States)

    Rhodes, Emily P; Ren, Zhiyong; Mays, David C

    2012-12-04

    Because tires contain approximately 1-2% zinc by weight, zinc leaching is an environmental concern associated with civil engineering applications of tire crumb rubber. An assessment of zinc leaching data from 14 studies in the published literature indicates that increasing zinc leaching is associated with lower pH and longer leaching times, but the data display a wide range of zinc concentrations, and do not address the effect of crumb rubber size or the dynamics of zinc leaching during flow through porous crumb rubber. The present study was undertaken to investigate the effect of crumb rubber size using the synthetic precipitation leaching procedure (SPLP), the effect of exposure time using quiescent batch leaching tests, and the dynamics of zinc leaching using column tests. Results indicate that zinc leaching from tire crumb rubber increases with smaller crumb rubber and longer exposure time. Results from SPLP and quiescent batch leaching tests are interpreted with a single-parameter leaching model that predicts a constant rate of zinc leaching up to 96 h. Breakthrough curves from column tests displayed an initial pulse of elevated zinc concentration (~3 mg/L) before settling down to a steady-state value (~0.2 mg/L), and were modeled with the software package HYDRUS-1D. Washing crumb rubber reduces this initial pulse but does not change the steady-state value. No leaching experiment significantly reduced the reservoir of zinc in the crumb rubber.

  19. Amino acid modifiers in guayule rubber compounds

    Science.gov (United States)

    Tire producers are increasingly interested in biobased materials, including rubber but also as compounding chemicals. An alternative natural rubber for tire use is produced by guayule, a woody desert shrub native to North America. Alternative compounding chemicals include naturally-occurring amino a...

  20. Estimation of genetic parameters in rubber progenies

    Directory of Open Access Journals (Sweden)

    Cecília Khusala Verardi

    2012-09-01

    Full Text Available This study was designed to evaluate the genetic variability, the potential for rubber yield and secondary traits of rubber tree progenies at three locations in the state of Sao Paulo. The experiments were conducted in a randomized block design with 22 progenies and 6 replications. At the age of three years, the progenies were evaluated for rubber yield, girth growth and total number of latex vessel rings. The results showed the existence of genetic variability among progenies for each location separately as well as between locations, with differences in the progeny performance for the traits. The individual heritabilities calculated for rubber yield, girth growth and total number of latex vessel rings (0.30, 0.63 and 0.29, respectively, associated with high genetic gains with selection for the traits studied at each site, showed that the populations can be considered suitable for the rubber breeding program, provided that an appropriate selection procedure is used.

  1. Lignocellulosic fiber reinforced rubber composites

    CSIR Research Space (South Africa)

    Jacob John, Maya

    2009-04-01

    Full Text Available stream_source_info John_d1_2009.pdf.txt stream_content_type text/plain stream_size 43167 Content-Encoding UTF-8 stream_name John_d1_2009.pdf.txt Content-Type text/plain; charset=UTF-8 -252- CHAPTER 10: LIGNOCELLULOSIC... FIBER REINFORCED RUBBER COMPOSITES Maya JACOB JOHN1 Rajesh D. ANANDJIWALA2 (1)CSIR Materials Science and Manufacturing, Fibres and Textiles Competence Area, P.O. Box 1124, Port Elizabeth 6000, South Africa, E-mail: mjohn@csir.co.za (2) Department...

  2. Surface modification of silicon-containing fluorocarbon films prepared by plasma-enhanced chemical vapor deposition

    Science.gov (United States)

    Jin, Yoonyoung; Desta, Yohannes; Goettert, Jost; Lee, G. S.; Ajmera, P. K.

    2005-07-01

    Surface modification of silicon-containing fluorocarbon (SiCF) films achieved by wet chemical treatments and through x-ray irradiation is examined. The SiCF films were prepared by plasma-enhanced chemical vapor deposition, using gas precursors of tetrafluoromethane and disilane. As-deposited SiCF film composition was analyzed by x-ray photoelectron spectroscopy. Surface modification of SiCF films utilizing n-lithiodiaminoethane wet chemical treatment is discussed. Sessile water-drop contact angle changed from 95°+/-2° before treatment to 32°+/-2° after treatment, indicating a change in the film surface characteristics from hydrophobic to hydrophilic. For x-ray irradiation on the SiCF film with a dose of 27.4 kJ/cm3, the contact angle of the sessile water drop changed from 95°+/-2° before radiation to 39°+/-3° after x-ray exposure. The effect of x-ray exposure on chemical bond structure of SiCF films is studied using Fourier transform infrared measurements. Electroless Cu deposition was performed to test the applicability of the surface modified films. The x-ray irradiation method offers a unique advantage in making possible surface modification in a localized area of high-aspect-ratio microstructures. Fabrication of a Ti-membrane x-ray mask is introduced here for selective surface modification using x-ray irradiation.

  3. Modification of tin oxide nanoparticles by fluorocarbon solids via a mechanochemical route

    Energy Technology Data Exchange (ETDEWEB)

    Senna, Mamoru, E-mail: senna@applc.keio.ac.jp; Turianicová, Erika; Zorkovská, Anna [Slovak Academy of Sciences, Institute of Geotechnics (Slovakia); Makreski, Petre [SS Cyril and Methodius University, Institute of Chemistry, Faculty of Natural Sciences and Mathematics (Macedonia, The Former Yugoslav Republic of); Kaňuchová, Mária [Technical University of Košice, Institute of Montaneous Sciences and Environmental Protection (Slovakia); Scholz, Gudrun [Humboldt-Universität zu Berlin, Department of Chemistry (Germany); Baláž, Matej; Baláž, Peter; Šepelák, Vladimír [Slovak Academy of Sciences, Institute of Geotechnics (Slovakia); Hahn, Horst [Institute of Nanotechnology, Karlsruhe Institute of Technology (Germany)

    2015-09-15

    Interfacial reactions at the surface of SnO{sub 2} nanoparticles adjacent to the fluorocarbon solids (FCS) under mechanical stressing were compared in an attempt to their modification by introducing fluorine and carbon. Emphasis was laid on the comparison of the reactivity of 3 different species of FCS, i.e., polyvinylidene fluoride (PVdF), polytetrafluoroethylene (PTFE), and perfluorooctanoic acid (PFOA). PVdF exhibited the highest reactivity, followed by PTFE and PFOA, as confirmed by Raman, FT-IR, XPS, and {sup 19}F MAS NMR spectra. The preferential reactivity could be explained in terms of the electrophilicity of FCS toward the nucleophilic oxygen in SnO{sub 2}, since the decomposition of FCS is catalyzed by the coexisting SnO{sub 2}. PFOA behaved in a different manner, due to its carboxylic groups. At the same time, carbon nanospecies were introduced as a decomposed product of FCS. This results in the formation of SnO{sub 2}:F/C nanocomposite. Fluorine introduced to SnO{sub 2} survived even after heating up to 600 °C either in air or in Ar. This indicates the thermal stability of the present partially fluorinated SnO{sub 2} nanoparticles.

  4. Fluidization of a dipalmitoyl phosphatidylcholine monolayer by fluorocarbon gases: potential use in lung surfactant therapy.

    Science.gov (United States)

    Gerber, Frédéric; Krafft, Marie Pierre; Vandamme, Thierry F; Goldmann, Michel; Fontaine, Philippe

    2006-05-01

    Fluorocarbon gases (gFCs) were found to inhibit the liquid-expanded (LE)/liquid-condensed (LC) phase transition of dipalmitoyl phosphatidylcholine (DPPC) Langmuir monolayers. The formation of domains of an LC phase, which typically occurs in the LE/LC coexistence region upon compression of DPPC, is prevented when the atmosphere above the DPPC monolayer is saturated with a gFC. When contacted with gFC, the DPPC monolayer remains in the LE phase for surface pressures lower than 38 mN m(-1), as assessed by compression isotherms and fluorescence microscopy (FM). Moreover, gFCs can induce the dissolution of preexisting LC phase domains and facilitate the respreading of the DPPC molecules on the water surface, as shown by FM and grazing incidence x-ray diffraction. gFCs have thus a highly effective fluidizing effect on the DPPC monolayer. This gFC-induced fluidizing effect was compared with the fluidizing effect brought about by a mixture of unsaturated lipids and proteins, namely the two commercially available lung surfactant substitutes, Curosurf and Survanta, which are derived from porcine and bovine lung extracts, respectively. The candidate FCs were chosen among those already investigated for biomedical applications, and in particular for intravascular oxygen transport, i.e., perfluorooctyl bromide, perfluorooctylethane, bis(perfluorobutyl)ethene, perfluorodecalin, and perfluorooctane. The fluidizing effect is most effective with the linear FCs. This study suggests that FCs, whose biocompatibility is well documented, may be useful in lung surfactant substitute compositions.

  5. THE EFFECT OF FLUOROCARBON ARTIFICIAL BLOOD (FC-34 IN ACUTE VASOGENIC BRAIN EDEMA

    Directory of Open Access Journals (Sweden)

    M NEEMATBAKHSH

    2000-03-01

    Full Text Available Background. Oxygen transport to tissue after an acute ischemia is strongly important. Fluorocarbon liquids are able to facilitated the oxygen transport. An animal experiment was designed to study the effect of FC-34 in acute brain ischemia. Methods. The left common carotid arteries were ligated in three groups of anesthetized animals for 30 minutes to obtain acute brain edema. The animals were subjected to received 15 ml/kg saline (group 1, 10% monitol (group 2 or FC-43 (group 3. All animals were recovered, and they monitored for two weeks. The electrolytes, BUN, and creatinine were measured before (all animals and after two weeks (survived animals. Pathological investigation was obtained by light and electron microscope via pathological process. Findings. The group 1 animals were died during first five days, but one and four animals were survived by two weeks in groups 2 & 3 respectively (P < 0.05. The pathological determinations indicate less cellular damages in group 3. No significant differences were detected in potassium, calcium, BUN, and creatinine before and after the experiment. Conclusion. The particle size and oxygen solubility in FC-43 is the major factors for better oxygen transport in ischem

  6. Time resolved measurements of the CF{sub 2} rotational temperature in pulsed fluorocarbon rf plasmas

    Energy Technology Data Exchange (ETDEWEB)

    Gabriel, O; Stepanov, S; Pfafferott, M; Meichsner, J [Institute of Physics, University of Greifswald, Domstrasse 10a, D-17498, Greifswald (Germany)

    2006-11-01

    Knowledge of the absolute densities of small radicals like CF, CF{sub 2} and CF{sub 3} in fluorocarbon plasmas is essential for a fundamental understanding of plasma chemical processes and plasma surface interaction. Infrared absorption spectroscopy by means of tunable diode lasers (IR-TDLAS) was established and widely used for density measurements in the last decade. The often unknown parameter in the calculation of absolute radical densities from a measured absorption of a single line is the rotational temperature. In particular, a strong dependence of the line strength on rotational temperature has a significant influence on density calculation. In this paper we report on measurements of the CF{sub 2} rotational temperature in capacitively coupled CF{sub 4}/H{sub 2} plasmas (CCP) with rf (13.56 MHz) powers up to 200 W. Rotational temperatures in continuous and pulsed modes of the discharge were found to be between 300 and 450 K. Furthermore, first measurements of the time dependence of the rotational temperature in pulsed rf plasma are presented. The rotational temperature rises in the plasma phase within 0.1 s and goes down again to the temperature of the background gas in the plasma pause within 0.5 s. It is also shown that accurate density measurements of the radicals by means of single line absorption need correct information about the rotational temperature and careful selection of a suitable absorption line.

  7. Absorption of gaseous toluene in aqueous solutions of some kinds of fluorocarbon surfactant.

    Science.gov (United States)

    Xiao, Xiao; Yan, Bo; Fu, Jiamo; Xiao, Xianming

    2015-01-01

    A self-designed device was applied to treat a simulated exhaust gas loaded with toluene by aqueous solutions of five kinds of fluorocarbon surfactant (FS-3100, FS-22, FSN-100, FSO-100 and FSG) under the controlled laboratory conditions. The simulated exhaust gas is generated by a mixture of clean air and toluene vapor, and its toluene concentration can be controlled by changing the volume ratio of the inlet air to the vapor. Two mass transfer methods: liquid-liquid transfer and gas-liquid transfer, were compared for their toluene saturation capacities of these absorbent solutions, and it was found that more toluene was dissolved by the liquid-liquid transfer than by the gas-liquid transfer. According to the saturation capacities of these absorbent solutions and their Henry's Constants, FSO-100 is the best absorbent to treat the simulated exhaust gas and was selected for further experiments. The FSO-100 absorbent solution with a concentration of 0.1 % shows an efficient absorption to the simulated exhaust gas, with a toluene saturation capacity of 4.2 mg/g. Heating distillation (90- 95 oC) is highly efficient to recover toluene from the FSO-100 absorbent solution as well as regenerate it. A toluene recovery of about 85 % was achieved. The regenerated absorption solution can keep its initial toluene absorption capacity during the reuse.

  8. Hierarchical ZnO particles grafting by fluorocarbon polymer derivative: Preparation and superhydrophobic behavior

    Energy Technology Data Exchange (ETDEWEB)

    Gao, Dahai; Jia, Mengqiu, E-mail: jiamq@mail.buct.edu.cn

    2015-07-15

    Graphical abstract: - Highlights: • The hierarchical particles were prepared by a simple, mild hydrothermal process. • The obtained “chestnut” ZnO particles show dual-scale morphology with high roughness. • FEVE derivative was creatively imported to graft onto hierarchical particles. • Superhydrophobic surfaces were obtained, on which the contact angles surpass 150°. • A special model was proposed to explain the wetting state in this work. - Abstract: Superhydrophobic surfaces on the basis of hierarchical ZnO particles grafted by fluoroethylene-vinylether (FEVE) polymer derivative were prepared using a facile, mild and low-cost method. X-ray diffraction (XRD) and scanning electron microscope (SEM) revealed that the resulting ZnO particles via hydrothermal process exhibit micro–nano dual-scale morphology with high purity under a suitable surfactant amount and alkali concentration. The grafting of FEVE derivative was confirmed by Fourier transform infrared spectroscopy (FTIR) and energy-dispersive X-ray spectrometer (EDS), suggesting that hierarchical surface of ZnO particles was an imported monomolecular layer of fluorocarbon polymer. The obtained surface fabricated by drop-casting shows considerably high contact angle and good resistance to water immersion. The wetting behavior in this work was furthermore analyzed by theoretical wetting model. This work demonstrates that the sufficient low-wettable surface and high roughness both take a vital role in the superhydrophobic behavior.

  9. Extraction and characterization of latex and natural rubber from rubber-bearing plants.

    Science.gov (United States)

    Buranov, Anvar U; Elmuradov, Burkhon J

    2010-01-27

    Consecutive extraction of latex and natural rubber from the roots of rubber-bearing plants such as Taraxacum kok-saghyz (TKS), Scorzonera tau-saghyz (STS), and Scorzonera Uzbekistanica (SU) were carried out. Latex extraction was carried via two methods: Blender method and Flow method. The results of latex extraction were compared. Cultivated rubber-bearing plants contained slightly higher latex contents compared to those from wild fields. Several creaming agents for latex extraction were compared. About 50% of total natural rubber was extracted as latex. The results of the comparative studies indicated that optimum latex extraction can be achieved with Flow method. The purity of latex extracted by Blender method ( approximately 75%) was significantly lower than that extracted by Flow method (99.5%). When the latex particles were stabilized with casein, the latex was concentrated significantly. Through concentrating latex by flotation, the latex concentration of 35% was obtained. Bagasse contained mostly solid natural rubber. The remaining natural rubber in the bagasse (left after the latex extraction) was extracted using sequential solvent extraction first with acetone and then with several nonpolar solvents. Solid natural rubber was analyzed for gel content and characterized by size exclusion chromatography (SEC) for molecular weight determinations. SEC of solid natural rubber has shown that the molecular weight is about 1.8E6 and they contain less gel compared to TSR20 (Grade 20 Technically Specified Rubber), a commercial natural rubber from Hevea brasiliensis.

  10. How to Develop Rubber Production in Xishuangbanna Dai Autonomous Prefecture?

    Institute of Scientific and Technical Information of China (English)

    Huide; HUANG; Haolun; HUANG; Wanzhen; ZHANG

    2015-01-01

    The natural rubber planting area in Xishuangbanna Dai Autonomous Prefecture accounts for about 30% of rubber planting area in China. At the end of 2013,the rubber planting area in Xishuangbanna Dai Autonomous Prefecture was 29. 4 ha,the tapped rubber plantation area was 17. 49 ha,and the dry rubber production was 317000 t. Currently,the production and management level of rubber plantation has declined in Xishuangbanna Dai Autonomous Prefecture,the tapping technique is outdated,and the tapping technology management system is difficult to implement. Therefore,some ways can be employed to promote the development of rubber industry such as enhancing the operation and management level of rubber industry,organizing the rubber production team,and developing the new rubber farmers’ cooperatives.

  11. Zinc Leaching from Tire Crumb Rubber

    Science.gov (United States)

    Rhodes, E. P.; Ren, J.; Mays, D. C.

    2010-12-01

    Recent estimates indicate that more than 2 billion scrap tires are currently stockpiled in the United States and approximately 280 million more tires are added annually. Various engineering applications utilize recycled tires in the form of shredded tire crumb rubber. However, the use of tire crumb rubber may have negative environmental impacts, especially when the rubber comes into contact with water. A review of the literature indicates that leaching of zinc from tire crumb rubber is the most significant water quality concern associated with using this material. Zinc is generally used in tire manufacturing, representing approximately 1.3% of the final product by mass. This study will report results from the U.S. Environmental Protection Agency’s (EPA’s) Synthetic Precipitation Leaching Procedure, batch leaching tests, and column leaching tests performed to quantify the process by which zinc leaches from tire crumb rubber into water. Results are interpreted with a first-order kinetic attachment/detachment model, implemented with the U.S. Agricultural Research Service software HYDRUS-1D, in order to determine the circumstances when zinc leaching from tire crumb rubber would be expected to comply with the applicable discharge limits. One potential application for recycled tires is replacing sand with tire crumb rubber in granular media filters used for stormwater pollution control. For this to be a viable application, the total zinc in the stormwater discharge must be below the EPA’s benchmark value of 0.117 mg/L.

  12. History of Rubber and Its Use

    Science.gov (United States)

    Müller, Ingo; Strehlow, Peter

    Despite its spectacular properties rubber was not much good for anything before the latter part of the 19th century. To be sure the Aztecs had used it to make balls for their ceremonial ball games - or so we are told. But those games died along with the Aztec culture in the 16th century and there is no record of other useful applications until the late 18th century. But then, after that, rubber took off in a small way. After the American inventor Samuel Peal had obtained a patent in 1791 for the production of rubber-coated watertight textiles, the Scottish chemist Charles Macintosh (1766-1843) used such textiles for making rain-coats, and Thomas Hancock (1786-1865) produced rubber boots. At that time it was not really appropriate to speak of a rubber industry. What little material the evil-smelling workshops in New York and London needed, could be satisfied with the import of 30 tons of Caoutchouc1 annually - extracted from the sap of the tree Hevea brasiliensis - and most of that went for making erasers. Indeed, it had been reported by the English minister and scientist Joseph Priestley (1733-1804) that pieces of rubber are well-suited to rub out (sic!) pencil marks. Even today there is nothing better for the purpose and rubber became the English word for Caoutchouc.

  13. Polypropylene–rubber blends: 2. The effect of the rubber content on the deformation and impact behaviour

    NARCIS (Netherlands)

    Wal, van der A.; Nijhof, R.; Gaymans, R.J.

    1999-01-01

    The effect of the rubber content on the deformation and impact behaviour of polypropylene–EPDM rubber blends is studied. The blends are made on a twin screw extruder. The rubber content ranged from 0 to 40 vol.%. The tensile modulus and the yield stress decrease linearly with increasing rubber conte

  14. Effect of Rubberized Bitumen Blending Methods on Permanent Deformation of SMA Rubberized Asphalt Mixtures

    Directory of Open Access Journals (Sweden)

    Herda Yati Katman

    2016-01-01

    Full Text Available This study aims at comparing the permanent deformation of Stone Mastic Asphalt (SMA rubberized asphalt mixtures produced by the wet process. In this study, rubberized binders were prepared using two different blending methods, namely, continuous blend and terminal blend. To study the creep behaviour of control and rubberized asphalt mixtures, the dynamic creep test was performed using Universal Materials Testing Apparatus (UMATTA at different temperatures and stress levels. Zhou three-stage creep model was utilized to evaluate the deformation characteristics of the mixtures. In all test conditions, the highest resistance to permanent deformation is showed by the rubberized mixtures produced with continuous blend binders. This study also reveals that the permanent deformation of rubberized mixtures cannot be predicted based on the characteristics of the rubberized binders.

  15. Structural characterization of rubber from jackfruit and euphorbia as a model of natural rubber.

    Science.gov (United States)

    Mekkriengkrai, Dararat; Ute, Koiichi; Swiezewska, Ewa; Chojnacki, Tadeusz; Tanaka, Yasuyuki; Sakdapipanich, Jitladda T

    2004-01-01

    A structural study of low molecular weight rubbers from Jackfruit (Artocarpus heterophyllus) and Painted spurge (Euphorbia heterophylla) was carried out as model compounds of natural rubber from Hevea brasiliensis. The rubber content of latex from Jackfruit was 0.4-0.7%, which is very low compared with that of 30-35% in the latex from Hevea tree. The rubber from Jackfruit latex was low molecular weight with narrow unimodal molecular weight distribution (MWD), whereas that obtained from E. heterophylla showed very broad MWD. The 1H and 13C NMR analyses showed that Jackfruit rubber consists of a dimethylallyl group and two trans-isoprene units connected to a long sequence of cis-isoprene units. The alpha-terminal group of Jackfruit rubber was presumed to be composed of a phosphate group based on the presence of 1H NMR signal at 4.08 ppm corresponding to the terminal =CH-CH2OP group.

  16. Thermal properties of hydrogenated liquid natural rubber

    Energy Technology Data Exchange (ETDEWEB)

    Jamaluddin, Naharullah; Abdullah, Ibrahim; Yusoff, Siti Fairus M. [School of Chemical Sciences and Food Technology, Faculty of Science and Technology, Universiti Kebangsaan Malaysia, 43600 Bangi, Selangor (Malaysia)

    2015-09-25

    Natural rubber (NR) was modified to form liquid natural rubber (LNR) via photooxidative degradation. Hydrogenated liquid natural rubber (HLNR) was synthesized by using diimide as source of hydrogen which the diimide is produced by thermolysis of p-toluenesulfonyl hydrazide (TSH). The structure of HLNR was characterized by determining the changes of main peaks in Fourier Transform infrared and nuclear magnetic resonance spectra after hydrogenation. Thermogravimetric analysis showed that the HLNR had higher decomposition temperature compared to LNR and the decomposition temperature is directly proportional to the percentage of conversion.

  17. Properties of Nanokaolin and Its Rubber Composites

    Institute of Scientific and Technical Information of China (English)

    ZHANG Yu-de; LIU Qin-fu; JI Lei-bo; LU Yin-ping

    2005-01-01

    A kind of nanokaolin powder with a thickness of 20-50nm and an average diameter of 300nm is produced through combined procedure of purification, delamination, surface modification and pulverization. The application experiments in butadiene rubber (BR), ethylene-propylene diene methylene (EPDM), and natural rubber (NR) indicates that this nano-kaolin powder material is much better than precipitated silica in reinforcement, while in styrene-butadiene rubber (SBR) it is close to precipitated silica. Nanokaolin is of superiority in elasticity, elongation at break, anti-flexure property.

  18. Life assessment of rubber articles in fuels

    OpenAIRE

    Selldén, Emmy

    2013-01-01

    The choice of rubber material for use in sealings and hoses in the fuel system is of great importance. If a wrong type of rubber is used, premature failure during service may occur. This impacts the environmental performance, the safety during driving, uptime and economy of the transport. In this diploma work, rubbers for use in sealing and hoses in the fuel system have been evaluated to assess which materials have the potential to be used under long-term use in contact with commercial fuels....

  19. Chemistry of rubber processing and disposal.

    Science.gov (United States)

    Bebb, R L

    1976-01-01

    The major chemical changes during the processing of rubber occur with the breakdown in mastication and during vulcanization of the molded tire. There is little chemical change during the compounding, calendering, extrusion, and molding steps. Reclaiming is the process of converting scrap rubber into an unsaturated, processible product that can be vulcanized with sulfur. Pyrolysis of scrap rubber yields a complex mixture of liquids, gas, and residue in varying ratios dependent on the nature of the scrap and the conditions of pyrolysis. PMID:799964

  20. Suitability of rubber concrete for railway sleepers

    Directory of Open Access Journals (Sweden)

    Afia S. Hameed

    2016-09-01

    Full Text Available An experimental investigation by replacing 15% by volume fraction of fine aggregate by crumb rubber was conducted to find the fatigue failure load and impact resistance. The design strength of 50 and 55 MPa was achieved. Test result indicated that there was reduction in compressive strength and modulus values. The fatigue failure and impact resistance were high for rubber concrete when compared with ordinary high strength concrete. The impact strength for railway sleeper with crumb rubber replacement showed increase of about 60% when compared to prestressed concrete sleeper.

  1. Material Model Research on Rubber Vibration Isolators

    Institute of Scientific and Technical Information of China (English)

    2007-01-01

    A viscohyperelastic constitutive model is proposed to describe the mechanical behaviour of vibration isolation rubber under broad-band vibration. This constitutive model comprises two parts: a component with three parameters to characterize the hyperelastic static properties of rubber materials,and the other component incorporating two relaxation time parameters, corresponding to high and low strain rates, respectively, to describe the dynamic response under vibration and impact loadings. Based on this proposed constitutive model, a series of experiments were performed on two types of rubber materials over a wide strain rate range. The results predicted from this model are in good agreement with the experimental data.

  2. An interactive web-based design system for rubber injection mold: Automotive rubber parts

    OpenAIRE

    Chamnarn Thongmark; Jariyaporn Onwong

    2016-01-01

    This research aims at integrating a knowledge-based system and web-based technology to facilitate the rubber and rubber composite injection mold design. The system integrates both of computer-aided design and web-based management by using the application programming interface. The research processes started with gathering data and knowledge concerning on rubber injection mold design and process, with the designed framework of the system included. An example part was demonstrated i...

  3. An interactive web-based design system for rubber injection mold: Automotive rubber parts

    OpenAIRE

    Chamnarn Thongmark; Jariyaporn Onwong

    2016-01-01

    This research aims at integrating a knowledge-based system and web-based technology to facilitate the rubber and rubber composite injection mold design. The system integrates both of computer-aided design and web-based management by using the application programming interface. The research processes started with gathering data and knowledge concerning on rubber injection mold design and process, with the designed framework of the system included. An example part was demonstrated i...

  4. 氟碳杂化表面活性剂的研究进展%Research Progress of Fluorocarbon-hydrocarbon Hybrid Surfactants

    Institute of Scientific and Technical Information of China (English)

    刘刚芝; 冯浦涌; 荣新明; 费晨洪; 王碧清; 王继宇; 冯玉军

    2013-01-01

    氟碳杂化表面活性剂是指分子结构中同时含有氟碳链和碳氢链的表面活性剂.从氟碳杂化表面活性剂的类型,合成路线,溶液性能及应用等方面系统地综述了其研究进展.参考文献46篇.%Fluorocarbon-hydrocarbon hybrid surfactants are amphiphilies in which fluorocarbon and hydrocarbon chains coexist.In this paper,the classification,synthesis,surface activities and application of fluorocarbon-hydrocarbon hybrid surfactants are reviewed with 46 references.

  5. Micromorphological characterization and label-free quantitation of small rubber particle protein in natural rubber latex.

    Science.gov (United States)

    Wang, Sai; Liu, Jiahui; Wu, Yanxia; You, Yawen; He, Jingyi; Zhang, Jichuan; Zhang, Liqun; Dong, Yiyang

    2016-04-15

    Commercial natural rubber is traditionally supplied by Hevea brasiliensis, but now there is a big energy problem because of the limited resource and increasing demand. Intensive study of key rubber-related substances is urgently needed for further research of in vitro biosynthesis of natural rubber. Natural rubber is biosynthesized on the surface of rubber particles. A membrane protein called small rubber particle protein (SRPP) is a key protein associated closely with rubber biosynthesis; however, SRPP in different plants has been only qualitatively studied, and there are no quantitative reports so far. In this work, H. brasiliensis was chosen as a model plant. The microscopic distribution of SRPP on the rubber particles during the washing process was investigated by transmission electron microscopy-immunogold labeling. A label-free surface plasmon resonance (SPR) immunosensor was developed to quantify SRPP in H. brasiliensis for the first time. The immunosensor was then used to rapidly detect and analyze SRPP in dandelions and prickly lettuce latex samples. The label-free SPR immunosensor can be a desirable tool for rapid quantitation of the membrane protein SRPP, with excellent assay efficiency, high sensitivity, and high specificity. The method lays the foundation for further study of the functional relationship between SRPP and natural rubber content.

  6. Characterization of rubber particles and rubber chain elongation in Taraxacum koksaghyz

    Directory of Open Access Journals (Sweden)

    Prüfer Dirk

    2010-02-01

    Full Text Available Abstract Background Natural rubber is a biopolymer with exceptional qualities that cannot be completely replaced using synthetic alternatives. Although several key enzymes in the rubber biosynthetic pathway have been isolated, mainly from plants such as Hevea brasiliensis, Ficus spec. and the desert shrub Parthenium argentatum, there have been no in planta functional studies, e.g. by RNA interference, due to the absence of efficient and reproducible protocols for genetic engineering. In contrast, the Russian dandelion Taraxacum koksaghyz, which has long been considered as a potential alternative source of low-cost natural rubber, has a rapid life cycle and can be genetically transformed using a simple and reliable procedure. However, there is very little molecular data available for either the rubber polymer itself or its biosynthesis in T. koksaghyz. Results We established a method for the purification of rubber particles - the active sites of rubber biosynthesis - from T. koksaghyz latex. Photon correlation spectroscopy and transmission electron microscopy revealed an average particle size of 320 nm, and 13C nuclear magnetic resonance (NMR spectroscopy confirmed that isolated rubber particles contain poly(cis-1,4-isoprene with a purity >95%. Size exclusion chromatography indicated that the weight average molecular mass (w of T. koksaghyz natural rubber is 4,000-5,000 kDa. Rubber particles showed rubber transferase activity of 0.2 pmol min-1 mg-1. Ex vivo rubber biosynthesis experiments resulted in a skewed unimodal distribution of [1-14C]isopentenyl pyrophosphate (IPP incorporation at a w of 2,500 kDa. Characterization of recently isolated cis-prenyltransferases (CPTs from T. koksaghyz revealed that these enzymes are associated with rubber particles and are able to produce long-chain polyprenols in yeast. Conclusions T. koksaghyz rubber particles are similar to those described for H. brasiliensis. They contain very pure, high molecular mass

  7. Feature Profile Evolution of SiO2 Trenches In Fluorocarbon Plasmas

    Science.gov (United States)

    Hwang, Helen; Govindan, T. R.; Meyyappan, M.; Arunachalam, Valli; Rauf, Shahid; Coronell, Dan; Carroll, Carol W. (Technical Monitor)

    1999-01-01

    Etching of silicon microstructures for semiconductor manufacturing in chlorine plasmas has been well characterized. The etching proceeds in a two-part process, where the chlorine neutrals passivate the Si surface and then the ions etch away SiClx. However, etching in more complicated gas mixtures and materials, such as etching of SiO2 in Ar/C4F8, requires knowledge of the ion and neutral distribution functions as a function of angle and velocity, in addition to modeling the gas surface reactions. In order to address these needs, we have developed and integrated a suite of models to simulate the etching process from the plasma reactor level to the feature profile evolution level. This arrangement allows for a better understanding, control, and prediction of the influence of equipment level process parameters on feature profile evolution. We are currently using the HPEM (Hybrid Plasma Equipment Model) and PCMCM (Plasma Chemistry Monte Carlo Model) to generate plasma properties and ion and neutral distribution functions for argon/fluorocarbon discharges in a GEC Reference Cell. These quantities are then input to the feature scale model, Simulation of Profile Evolution by Level Sets (SPELS). A surface chemistry model is used to determine the interaction of the incoming species with the substrate material and simulate the evolution of the trench profile. The impact of change of gas pressure and inductive power on the relative flux of CFx and F to the wafer, the etch and polymerization rates, and feature profiles will be examined. Comparisons to experimental profiles will also be presented.

  8. Novel antifoam for fermentation processes: fluorocarbon-hydrocarbon hybrid unsymmetrical bolaform surfactant.

    Science.gov (United States)

    Calik, Pinar; Ileri, Nazar; Erdinç, Burak I; Aydogan, Nihal; Argun, Muharrem

    2005-09-13

    As foaming appears as a problem in chemical and fermentation processes that inhibits reactor performance, the eminence of a novel fluorocarbon-hydrocarbon unsymmetrical bolaform (FHUB: OH(CH2)11N+(C2H4)2(CH2)2(CF2)5CF3 I-) surfactant as an antifoaming agent as well as a foam-reducing agent was investigated and compared with other surfactants and a commercial antifoaming agent. The surface elasticity of FHUB was determined as 4 mN/m, indicating its high potential on thinning of the foam film. The interactions between FHUB and the microoganism were investigated in a model fermentation process related with an enzyme production by recombinant Escherichia coli, in V = 3.0 dm3 bioreactor systems with V(R) = 1.65 dm3 working volume at air inlet rate of Q(o)/V(R) = 0.5 dm3 dm(-3) min(-1) and agitation rate of N = 500 min(-1) oxygen transfer conditions, at T = 37 degrees C, pH(o) = 7.2, and C(FHUB) = 0 and 0.1 mM, in a glucose-based defined medium. As FHUB did not influence the metabolism, specific enzyme activity values obtained with and without FHUB were close to each other; however, because of the slight decrease in oxygen transfer coefficient, slightly lower volumetric enzyme activity and cell concentrations were obtained. However, when FHUB is compared with widely used silicon oil based Antifoam A, with the use of the FHUB, higher physical oxygen transfer coefficient (K(L)a) values are obtained. Moreover, as the amount required for the foam control is very low, minute changes in the working volume of the bioreactor were obtained indicating the high potential of the use of FHUB as an antifoaming agent as well as a foam-reducing agent.

  9. STUDIES ON THE PERMEABILITY OF PVC /EBBA OVERLAPPED ULTRATHIN COMPOSITE MEMBRANES MODIFIED BY PLASMA- POLYMERIZATION WITH FLUOROCARBON MONOMERS

    Institute of Scientific and Technical Information of China (English)

    FU Xiucheng; JIN Xigao; Tisato KAJIYAMA

    1989-01-01

    The PVC/EBBA ultrathin composite membranes with thickness of about 100 nm were prepared by spreading the solution on water surface. The overlapped composite membrane showed a characteristic aggregation structure in which the polymer matrix exists as a three-dimensional spongy network and the liquid crystal domains were observedThe surface modification for the overlapped membranes was carried out by means of plasma-polymerization with the monomers of fluorocarbon compounds. Both Arrhenius plots of permeability coefficients for oxygen (-Po2) in the membrane samples before and after modification showed significant increase in the vicinity of the TKN of EBBA.

  10. Transmission properties of fluorocarbon polymer-coated silver hollow glass waveguide with tapered section for Er:YAG laser light

    Science.gov (United States)

    Wang, You; Hiraga, Hajime; Miura, Daisuke; Kato, Yuji; Miyagi, Mitsunobu

    1996-11-01

    We have succeeded in fabricating low-loss fluorocarbon polymer (FCP)-coated silver hollow glass waveguides by using a liquid-flow coating method. The thickness of a FCP film is strongly dependent on the flow speed and the concentration of FCP solution. It is shown that the optimum condition exists for depositing the polymer to reduce the roughness of layer. The transmission loss of the fabricated waveguide with inner diameter of 700 micrometers is about 0.2 dB/m for Er:YAG laser light. An efficient tapered coupler with a lens is also investigated to couple the laser beam with large diameter to small-bore waveguides.

  11. Pore-Engineered Metal–Organic Frameworks with Excellent Adsorption of Water and Fluorocarbon Refrigerant for Cooling Applications

    Energy Technology Data Exchange (ETDEWEB)

    Zheng, Jian [Physical; Vemuri, Rama S. [Energy; Estevez, Luis [Energy; Koech, Phillip K. [Energy; Varga, Tamas [Environmental; Camaioni, Donald M. [Physical; Blake, Thomas A. [Physical; McGrail, B. Peter [Energy; Motkuri, Radha Kishan [Energy

    2017-07-20

    Metal–organic frameworks (MOFs) are found to be promising sorbents for adsorption cooling applications. Using organic ligands with 1, 2, and 3 phenylene rings, we construct moisture-stable Ni-MOF-74 members with adjustable pore apertures. These pore-engineered materials exhibit excellent sorption capabilities towards water and fluorocarbons. The adsorption patterns for these materials differ significantly and are attributed to variances in the hydrophobic/hydrophilic pore character, associated with differences in pore size. Complementary ex situ characterizations and in situ FTIR spectra are deployed to understand the correlations between the mechanisms of gas loadings and the pore environment of the MOFs.

  12. Visual evoked potentials in rubber factory workers.

    Science.gov (United States)

    Tandon, O P; Kumar, V

    1997-01-01

    Pattern reversal visual evoked potentials (pVEP) were studied in 39 male rubber factory workers in the age range of 18-55 years and 20 control subjects (aged 18-46 years) not exposed to the rubber factory environment. Results revealed that 20 (51%) rubber factory workers had abnormal latencies of wave P1 (dominant component of pVEP) as per accepted criteria of 99% tolerance limit set for the control group (i.e. any value above mean +3 SD of control was considered abnormal). The section-wise per cent distribution of abnormalities was vulcanization (83%), tubing (75%), calendering (60%), loading (38%) and mixing (14%). This study provides electrophysiological evidence that rubber factory environments affect the conduction processes in optical pathways from their origin in the retina to striate cortex. However, this study has its limitations in not identifying the specific chemical(s) causing these changes in VEP.

  13. Oils and rubber from arid land plants

    Science.gov (United States)

    Johnson, J. D.; Hinman, C. W.

    1980-05-01

    In this article the economic development potentials of Cucurbita species (buffalo gourd and others), Simmondsia chinensis (jojoba), Euphorbia lathyris (gopher plant), and Parthenium argentatum (guayule) are discussed. All of these plants may become important sources of oils or rubber.

  14. The effect of polar end of long-chain fluorocarbon oligomers in promoting the superamphiphobic property over multi-scale rough Al alloy surfaces

    Science.gov (United States)

    Saifaldeen, Zubayda S.; Khedir, Khedir R.; Camci, Merve T.; Ucar, Ahmet; Suzer, Sefik; Karabacak, Tansel

    2016-08-01

    Rough structures with re-entrant property and their subsequent surface energy reduction with long-chain fluorocarbon oligomers are both critical in developing superamphiphobic (SAP, i.e. both super hydrophobic and superoleophobic) surfaces. However, morphology of the low-surface energy layer on a rough re-entrant substrate can strongly depend on the fluorocarbon oligomers used. In this study, the effect of polar end of different kinds of long-chain fluorocarbon oligomers in promoting a self-assembled monolayer with close packed molecules and robust adhesion on multi-scale rough Al alloy surfaces was investigated. Hierarchical Al alloy surfaces with microgrooves and nanograss structures were developed by a simple combination of one-directional mechanical sanding and post treatment in boiling de-ionized water (DIW). Three types of long-chain fluorocarbon oligomers of 1H, 1H, 2H, 2H-perfluorodecyltriethoxysilane (PFDTS), 1H, 1H, 2H, 2H-perfluorodecyltrichlorosilane (PFDCS), and perfluorooctanoic acid (PFOA) were chemically vaporized onto these rough Al alloy surfaces. The PFDCS exhibited the lowest surface free energy of less than 10 mN/m. The contact angle and sliding angle measurements for water, ethylene glycol, and peanut oil verified the SAP property of hierarchical rough Al alloy surfaces treated with alkylsilane oligomers (PFDTS, PFDCS). However, the hierarchical surfaces treated with fluorocarbon oligomer with polar acidic tail (PFOA) showed highly amphiphobic properties but could not reach the threshold for SAP. Chemical stability of the hierarchical Al alloy surfaces treated with the fluorocarbon oligomers was tested under the harsh conditions of ultra-sonication in acetone and annealing at high temperature after different treatment times. Contact angle measurements revealed the robustness of the alkylsilane oligomers and deterioration of the PFOA coating particularly for low surface tension liquids. The robust adhesion and close-packing of the alkylsilane

  15. Contact allergy to rubber accelerators remains prevalent

    DEFF Research Database (Denmark)

    Schwensen, J F; Menné, T; Johansen, J D

    2016-01-01

    INTRODUCTION: Chemicals used for the manufacturing of rubber are known causes of allergic contact dermatitis on the hands. Recent European studies have suggested a decrease in thiuram contact allergy. Moreover, while an association with hand dermatitis is well established, we have recently observ.......2% (19/54) and 35.4% (17/48) of the cases respectively. CONCLUSION: Contact allergy to rubber accelerators remains prevalent. Clinicians should be aware of the hitherto unexplored clinical association with facial dermatitis....

  16. THERMAL CONDUCTIVITY OF RUBBERIZED GYPSUM BOARD

    OpenAIRE

    Taher Abu-Lebdeh; Ellie Fini; Ashraf Fadiel

    2014-01-01

    The disposal of scrap tires is a challenging task and hence an innovative solution to meet these challenges is needed. Extensive work has been done on the utilization of waste tires in a variety of applications in asphalt pavements and concrete. However, previous investigations focus only on the mechanical properties of the rubberized materials, but few on the thermal performance. This is especially true for rubberized gypsum. Limited or no experimental data on the thermal performance of rubb...

  17. Rubber-Modified Epoxies: Transitions and Morphology.

    Science.gov (United States)

    1980-09-01

    temperatures used for cure (i.e. Tso > Tcure). A low molecular weight liquid diglycidyl ether of bisphenol A ( DGEBA ) epoxy resin, Epon 828, Shell Chemical Co...the rubber damping peak always occurs at or below the Tg of unreacted CTBN even though CTBN is capped with DGEBA (see Ref. 5 which also shows that the...depression of RTg decreases with increasing amounts of rubber modifier in the formulations). DGEBA and CTBN must be incorporated in the domains since

  18. [Detection of pentachlorophenol in natural rubber latex].

    Science.gov (United States)

    Jaworska, E

    1976-01-01

    The method of detection of pentachlorophenol in natural rubber latex is proposed. Pentachlorophenol is isolated from other nonrubber-like substances by thin-layer chromatography and identified by spectroscopic method in UV-light. Isolation of pentachlorophenol is carried out from water extracts obtained from the dry caoutchouc films, so the same method can be used for examination of the rubber articles designed for the medicinetoo.

  19. Establishment of new crops for the production of natural rubber.

    Science.gov (United States)

    van Beilen, Jan B; Poirier, Yves

    2007-11-01

    Natural rubber is a unique biopolymer of strategic importance that, in many of its most significant applications, cannot be replaced by synthetic alternatives. The rubber tree Hevea brasiliensis is the almost exclusive commercial source of natural rubber currently and alternative crops should be developed for several reasons, including: a disease risk to the rubber tree that could potentially decimate current production, a predicted shortage of natural rubber supply, increasing allergic reactions to rubber obtained from the Brazilian rubber tree and a general shift towards renewables. This review summarizes our knowledge of plants that can serve as alternative sources of natural rubber, of rubber biosynthesis and the scientific gaps that must be filled to bring the alternative crops into production.

  20. Microstructure and Properties of Desulfurized Crumb Rubber Modified Bitumen

    Institute of Scientific and Technical Information of China (English)

    2003-01-01

    The microstructures of general crumb rubber(CR), dynamic desulfurized crumb rubber(DDCR) and high speed agitation desulfurized crumb rubber(HSADCR) modified bitumens were investigated by a fluorescence microscope, and the physical properties of these three modified bitumens were studied.The results show that the dynamic desulfuration can improve the swelling capacity of crumb rubber in bitumen by destroying the sulfuratized bond of the crumb rubber,but the reunion of rubber particles during dynamic desulfuration also makes the swelling and the DDCR in bitumen difficult, so properties of the DDCR modified bitumen are not superior to the general crumb rubber modified bitumen.However,high speed agitation desulfuration can not only improve the swelling capacity of crumb rubber in bitumen,but also avoid the reunion of rubber particles,so some properties of bitumen can be improved by the modification of HSADCR.

  1. Use of waste rubber as concrete additive.

    Science.gov (United States)

    Chou, Liang Hsing; Lu, Chun-Ku; Chang, Jen-Ray; Lee, Maw Tien

    2007-02-01

    For resource reutilization, scrap tyres have long been investigated as an additive to concrete to form 'Rubcrete' for various applications and have shown promising results. However, the addition of rubber particles leads to the degradation of physical properties, particularly, the compressive strength of the concrete. In this study, a theoretical model was proposed to shed light on the mechanisms of decrease in compressive strength due to the addition of rubber particles as well as improvement in compressive strength through modification of particle surfaces. The literature suggests that the compressive strength can be improved by soaking the rubber particles in alkaline solution first to increase the inter-phase bonding between the rubber particles and cement. Instead, we discovered that the loss in compressive strength was due to local imperfections in the hydration of cement, induced by the addition of heterogeneous and hydrophobic rubber particles. Microscopic studies showed that the rubber particles disturbed the water transfer to create channels, which were prone to cracking and led to a loss in the compressive strength. Unexpectedly, no cracking was found along the surfaces of the rubber particles, indicating that the bonding strength between the rubber particles and cement phases was not the critical factor in determining the compressive strength. Therefore, a theoretical model was proposed to describe the water transfer in the Rubcrete specimens to explain the experimental data. In the model, the local water available for hydration (Q) is: Q = -A(slv)/6piv, where Q, A(slv), and v are mass flow rate (kg s(-1)), Hamaker constant (J), and dynamic viscosity (m2 s(-1)), respectively. By maximizing the quantity Q and, in turn, the Hamaker constant A(slv), the compressive strength could be improved. The Hamaker constant A(slv) for water film on rubber particle surfaces was smaller than that for the hydrated cement particles; the water transfer rate was lower in

  2. Influence of melt mixer on injection molding of thermoset elastomers

    Science.gov (United States)

    Rochman, Arif; Zahra, Keith

    2016-10-01

    One of the drawbacks in injection molding is that the plasticizing screw is short such that polymers having high concentrations of additives, such as thermoset elastomers, might not mix homogeneously within the short period of time during the plasticizing stage. In this study, various melt mixers inside the nozzle chamber, together forming a mixing nozzle, were developed. Three different materials were investigated, namely nitrile butadiene rubber (NBR), ethylene propylene-diene monomer (EPDM) and fluorocarbon (FKM). The use of these melt mixers resulted in better homogeneity and properties of the molded parts despite a curing time reduction of 10 s. This was due to the increase in mixing and shearing introduced a higher rate of crosslinking formation in the molded parts.

  3. Effect of non-rubber constituents on guayule and Hevea rubber intrinsic properties

    Science.gov (United States)

    To meet the increasing demand for natural rubber (NR), and address price volatility and steadily increasing labor costs, alternate rubber-producing species are in commercial development. One of these, guayule (Parthenium argentatum), has emerged on the market as a sustainable commercial source of h...

  4. Euphorbia characias latex: micromorphology of rubber particles and rubber transferase activity.

    Science.gov (United States)

    Spanò, Delia; Pintus, Francesca; Esposito, Francesca; Loche, Danilo; Floris, Giovanni; Medda, Rosaria

    2015-02-01

    We have recently characterized a natural rubber in the latex of Euphorbia characias. Following that study, we here investigated the rubber particles and rubber transferase in that Mediterranean shrub. Rubber particles, observed by scanning electron microscopy, are spherical in shape with diameter ranging from 0.02 to 1.2 μm. Washed rubber particles exhibit rubber transferase activity with a rate of radiolabeled [(14)C]IPP incorporation of 4.5 pmol min(-1)mg(-1). Denaturing electrophoresis profile of washed rubber particles reveals a single protein band of 37 kDa that is recognized in western blot analysis by antibodies raised against the synthetic peptide whose sequence, DVVIRTSGETRLSNF, is included in one of the five regions conserved among cis-prenyl chain elongation enzymes. The cDNA nucleotide sequence of E. characias rubber transferase (GenBank JX564541) and the deduced amino acid sequence appear to be highly homologous to the sequence of several plant cis-prenyltransferases.

  5. Elastomers for Tracked Vehicles: 1980-1997 Program to Improve Durability of Rubber Tank Pads for Army Tracked Vehicles

    Science.gov (United States)

    2015-06-01

    blends of the polymers styrene butadiene rubber , natural rubber , and... Natural -SBR-PBD rubber blends : formulations .........................................................50 Table 15b Natural -SBR-PBD rubber blends ...properties .............................................................53 Table 16a SBR blends with natural and polybutadiene rubber

  6. 21 CFR 801.437 - User labeling for devices that contain natural rubber.

    Science.gov (United States)

    2010-04-01

    ... User labeling for devices that contain natural rubber. (a) Data in the Medical Device Reporting System..., natural rubber that contacts humans. The term “natural rubber” includes natural rubber latex, dry natural rubber, and synthetic latex or synthetic rubber that contains natural rubber in its......

  7. Improvements in the technique of vascular perfusion-fixation employing a fluorocarbon-containing perfusate and a peristaltic pump controlled by pressure feedback

    DEFF Research Database (Denmark)

    Rostgaard, J; Qvortrup, K; Poulsen, Steen Seier

    1993-01-01

    oxygenated fluorocarbon to glutaraldehyde perfusate-fixatives, enough oxygen is made accessible for cellular respiration as well as for the oxygen-consuming chemical reactions of glutaraldehyde with the tissue. Data on anaesthesia, operative manoeuvres, mechanical components of the system, preparation...

  8. Effect of plasma dissociation on fluorocarbon layers formed under C4F8/Ar pulsed plasma for SiO2 etching

    Science.gov (United States)

    Matsui, Miyako; Usui, Tatehito; Ono, Tetsuo

    2017-06-01

    We investigated the effects of gas pressure on the dissociation of C4F8/Ar plasma and the formations of fluorocarbon layers on etched materials by SiO2 etching using pulsed-microwave electron-cyclotron-resonance plasma. Dissociated radicals and molecules of C x F y and CF x species generated from C4F8/Ar plasma were measured by ion attachment mass spectrometry, which is a fragment-free method. The thickness and chemical state of the fluorocarbon layers formed on the etched materials were analyzed by X-ray photoelectron spectroscopy. Higher selective etching of SiO2 relative to Si3N4 was possible at 2.0 Pa but not at 0.5 Pa. Thick fluorocarbon layers, which protect etched materials from ion bombardment, formed on both SiO2 and Si3N4 surfaces; thus, both the SiO2 and Si3N4 etching rates were reduced at a high pressure. However, the CF2 flux ratio increased while the flux ratio of C2F2 decreased as the pressure increased. The increased flux of CF2 enhanced SiO2 etching because CF2 is the main etchant of SiO2. This CF2-rich plasma formed CF2-rich fluorocarbon layers, enhancing the SiO2 etching reaction.

  9. Rubber Tree (Hevea brasiliensis Muell. Arg).

    Science.gov (United States)

    Venkatachalam, Perumal; Jayashree, Radha; Rekha, Karumamkandathil; Sushmakumari, Sreedharannair; Sobha, Sankaren; Kumari Jayasree, Parukkuttyamma; Kala, Radha Gopikkuttanunithan; Thulaseedharan, Arjunan

    2006-01-01

    Rubber tree (Hevea brasiliensis Muell. Arg.) is an important industrial crop for natural rubber production. At present, more than 9.5 million hectares in about 40 countries are devoted to rubber tree cultivation with a production about 6.5 million tons of dry rubber each year. The world supply of natural rubber is barely keeping up with a global demand for 12 million tons of natural rubber in 2020. Tapping panel dryness (TPD) is a complex physiological syndrome widely found in rubber tree plantations, which causes severe yield and crop losses in natural rubber producing countries. Currently, there is no effective prevention or treatment for this serious malady. As it is a perennial tree crop, the integration of specific desired traits through conventional breeding is both time-consuming and labour-intensive. Genetic transformation with conventional breeding is certainly a more promising tool for incorporation of agronomically important genes that could improve existing Hevea genotype. This chapter provides an Agrobacterium-mediated transformation protocol for rubber tree using immature anther-derived calli as initial explants. We have applied this protocol to generate genetically engineered plants from a high yielding Indian clone RRII 105 of Hevea brasiliensis (Hb). Calli were co-cultured with Agrobacterium tumefaciens harboring a plasmid vector containing the Hb superoxide dismutase (SOD) gene and the reporter gene used was beta-glucuronidase (GUS) gene (uidA). The selectable marker gene used was neomycin phosphotransferase (nptII) and kanamycin was used as selection agent. We found that a suitable transformation protocol for Hevea consists of a 3-d co-cultivation with Agrobacterium in the presence of 20 mM acetosyringone, 15 mM betaine HCl, and 11.55 mM proline followed by selection on medium containing 300 mg/L kanamycin. Transformed calli surviving on medium containing 300 mg/L kanamycin showed a strong GUS-positive reaction. Upon subsequent subculture into

  10. Comparative analysis of rubber seed methyl ester with other methyl ...

    African Journals Online (AJOL)

    Comparative analysis of rubber seed methyl ester with other methyl esters. ... In order to achieve a two-step transesterification process was developed to convert rubber seed oil to its methyl esters. The first step, acid catalyzed ... Article Metrics.

  11. A crumb rubber modified syntactic foam

    Energy Technology Data Exchange (ETDEWEB)

    Li Guoqiang [Department of Mechanical Engineering, Louisiana State University, Baton Rouge, LA 70803 (United States); Department of Mechanical Engineering, Southern University, Baton Rouge, LA 70813 (United States)], E-mail: guoli@me.lsu.edu; John, Manu [Department of Mechanical Engineering, Louisiana State University, Baton Rouge, LA 70803 (United States)

    2008-02-15

    In this study, the impact response and residual strength of a crumb rubber modified syntactic foam, which contained up to 20% by volume of crumb rubbers, were investigated. The foam had a hybrid microstructure bridging over several length scales. It was formed by dispersing hollow glass beads and crumb rubber particles into a microfiber and nanoclay filled epoxy matrix. Sandwich beam specimens were prepared using the hybrid foam as core and fiber reinforced epoxy as facings. A low velocity impact test using an instrumented drop tower impact machine was conducted on the sandwich beams and control beams made of the foam only. Four-point bending tests were conducted on the impact damaged specimens and control specimens without impact damage. The effect of the hybrid foam on the low velocity impact response and residual strength was evaluated based on the test results. The stress field interaction was evaluated using a finite element analysis. It was found that the rubberized syntactic foam possessed a higher capacity to dissipate impact energy and to retain bending strength. There was a positive composite action between the hollow glass bead particles and crumb rubber particles by means of stress field interaction and reduction in stress concentration.

  12. Removal Water Turbidity by Crumb Rubber Media

    Directory of Open Access Journals (Sweden)

    Abeer I. Alwared

    2014-06-01

    Full Text Available The removal of water turbidity by using crumb rubber filter was investigated .The present study was conducted to evaluate the effect of variation of influent water turbidity (10, 25 and 50 NTU, media size (0.6and 1.14mm, filtration rate (25, 45 and 65 l/hr and bed depth (30 and 60 cm on the performance of mono crumb rubber filter in response to the effluent filtered water turbidity and head loss development, and compare it with that of conventional sand filter. Results revealed that 25 l/hr flow rate and 25 NTU influent turbidity were the best operating conditions. smaller media size and higher bed depth gave the best removal efficiency while higher media size and small bed depth gave lower head loss. The optimum results show that 92.7% removal efficiency and 8.3 mm head loss. The comparison results show that at constant operating conditions, pressure drop for crumb rubber filter is lower than conventional sand filter; about 42% reduction in pressure drop than sand filter and the conventional sand filter has a little enhancement in removal efficiency than crumb rubber filter, 96.8% for sand while for crumb rubber 92.7%.

  13. Stimuli-responsive cement-reinforced rubber.

    Science.gov (United States)

    Musso, Simone; Robisson, Agathe; Maheshwar, Sudeep; Ulm, Franz-Josef

    2014-05-14

    In this work, we report the successful development of a cement-rubber reactive composite with reversible mechanical properties. Initially, the composite behaves like rubber containing inert filler, but when exposed to water, it increases in volume and reaches a stiffness that is intermediate between that of hydrogenated nitrile butadiene rubber (HNBR) and hydrated cement, while maintaining a relatively large ductility characteristic of rubber. After drying, the modulus increases even further up to 400 MPa. Wet/drying cycles prove that the elastic modulus can reversibly change between 150 and 400 MPa. Utilizing attenuated total reflection Fourier transform infrared spectroscopy), we demonstrate that the high pH produced by the hydration of cement triggers the hydrolysis of the rubber nitrile groups into carboxylate anions. Thus, the salt bridges, generated between the carboxylate anions of the elastomer and the cations of the filler, are responsible for the reversible variations in volume and elastic modulus of the composite as a consequence of environmental moisture exposure. These results reveal that cement nanoparticles can successfully be used to accomplish a twofold task: (a) achieve an original postpolymerization modification that allows one to work with carboxylate HNBR (HXNBR) not obtained by direct copolymerization of carboxylate monomers with butadiene, and (b) synthesize a stimuli-responsive polymeric composite. This new type of material, having an ideal behavior for sealing application, could be used as an alternative to cement for oil field zonal isolation applications.

  14. Super-hydrophobicity and oleophobicity of silicone rubber modified by CF 4 radio frequency plasma

    Science.gov (United States)

    Gao, Song-Hua; Gao, Li-Hua; Zhou, Ke-Sheng

    2011-03-01

    Owing to excellent electric properties, silicone rubber (SIR) has been widely employed in outdoor insulator. For further improving its hydrophobicity and service life, the SIR samples are treated by CF 4 radio frequency (RF) capacitively coupled plasma. The hydrophobic and oleophobic properties are characterized by static contact angle method. The surface morphology of modified SIR is observed by atom force microscope (AFM). X-ray photoelectron spectroscopy (XPS) is used to test the variation of the functional groups on the SIR surface due to the treatment by CF 4 plasma. The results indicate that the static contact angle of SIR surface is improved from 100.7° to 150.2° via the CF 4 plasma modification, and the super-hydrophobic surface of modified SIR, which the corresponding static contact angle is 150.2°, appears at RF power of 200 W for a 5 min treatment time. It is found that the super-hydrophobic surface ascribes to the coaction of the increase of roughness created by the ablation action and the formation of [-SiF x(CH 3) 2- x-O-] n ( x = 1, 2) structure produced by F atoms replacement methyl groups reaction, more importantly, the formation of [-SiF 2-O-] n structure is the major factor for super-hydrophobic surface, and it is different from the previous studies, which proposed the fluorocarbon species such as C-F, C-F 2, C-F 3, CF-CF n, and C-CF n, were largely introduced to the polymer surface and responsible for the formation of low surface energy.

  15. Preparation of Self-crosslinked Fluorocarbon Polymer Emulsion with Core-shell Structure by the Method of Soap-free Emulsion Polymerization

    Institute of Scientific and Technical Information of China (English)

    CHEN Lijun; SHI Hongxin; XIANG Juping; WU Hongke

    2009-01-01

    Using methyl methacrylate(MMA),butyl acrylate(BA)and hexafluorobutyl acry-late(HFBA)as main raw materials,we prepared self-crosslinked fluorocarbon polymer emulsion with core-shell structure via soap-free emulsion polymerization when the conception of particle design and polymer morphology was adopted.Moreover,the influence of mole ratio of BA to MAA,pH value on the oligomer was studied.And the effects of the added amount of oligomer,self-crosslinked monomer and HFBA,mass ratio of BA to MMA,reaction temperature and the initiator on the polymerization technology and the performance of the product,were investigated and optimized.The structure and performance of the fluorocarbon polymer emulsion were characterized and tested with FTIR,TEM, MFT and contact angle and water absorption of the latex film.The experimental results show that the optimal conditions for preparing fluorocarbon polymer emulsion are as follows:for preparing the oligomer,mol ratio of BA to MAA is equal to 1.0:1.60,and pH value is controlled within the range of 8.0 and 9.0;for preparing fluorocarbon polymer emulsion,the added amount of oligmer[P(BA/MANa)] is 6%;mass ratio of BA to MMA is 40:60;the added amount of self-crosslinked monomer is 2%,the added amount of HFBA is 15%;reaction temperature is 80℃;the mixture of potassium persulfate and sodium bisulfite is used as the initiator.The film-forming stability of the fluorocarbon polymer emul-sion and the performance of the latex film,which is prepared with the soap-free emulsion polymeri-zation,are better than that prepared with the conventional emulsion polymerization.

  16. Isolation of Microorganisms Able To Metabolize Purified Natural Rubber

    OpenAIRE

    Heisey, R. M.; Papadatos, S

    1995-01-01

    Bacteria able to grow on purified natural rubber in the absence of other organic carbon sources were isolated from soil. Ten isolates reduced the weight of vulcanized rubber from latex gloves by >10% in 6 weeks. Scanning electron microscopy clearly revealed the ability of the microorganisms to colonize, penetrate, and dramatically alter the physical structure of the rubber. The rubber-metabolizing bacteria were identified on the basis of fatty acid profiles and cell wall characteristics. Seve...

  17. Study on Production of Rubber Sealing Strips with Steel Bones

    Institute of Scientific and Technical Information of China (English)

    2002-01-01

    Rubber sealing strips with steel bones are used in car manufacturing that produced in large quantities. Cutting processes, such as milling and punching, are needed when the strips are produced. Accuracy, smoothness and flatness of the machined surface have to be guaranteed in the cutting process; moreover, deformation of the steel bone and peeling-off of the rubber must be avoided. Therefore cutting action of rubber/steel strips differs from that of rubber or metal workpiece separately. In this paper, milli...

  18. Lifetime Analysis of Rubber Gasket Composed of Methyl Vinyl Silicone Rubber with Low-Temperature Resistance

    Directory of Open Access Journals (Sweden)

    Young-Doo Kwon

    2015-01-01

    Full Text Available Most machines and instruments constantly require elastomeric materials like rubber for the purposes of shock absorption, noise attenuation, and sealing. The material properties and accurate lifetime prediction of rubber are closely related to the quality of machines, especially their durability and reliability. The properties of rubber-like elastomers are influenced by ambient conditions, such as temperature, environment, and mechanical load. Moreover, the initial properties of rubber gaskets must be sustained under working conditions to satisfy their required function. Because of its technical merits, as well as its low cost, the highly accelerated life test (HALT is used by many researchers to predict the long-term lifetime of rubber materials. Methyl vinyl silicone rubber (VMQ has recently been adopted to improve the lifetime of automobile radiator gaskets. A four-parameter method of determining the recovery ability of the gaskets was recently published, and two revised methods of obtaining the recovery were proposed for polyacrylate (ACM rubber. The recovery rate curves for VMQ were acquired using the successive zooming genetic algorithm (SZGA. The gasket lifetime for the target recovery (60% of a compressed gasket was computed somewhat differently depending on the selected regression model.

  19. Synergistic effect of plasma-modified halloysite nanotubes and carbon black in natural rubber-butadiene rubber blend

    NARCIS (Netherlands)

    Poikelispaa, Minna; Das, Amit; Dierkes, Wilma; Vuorinen, Jyrki

    2013-01-01

    Halloysite nanotubes (HNTs) were investigated concerning their suitability for rubber reinforcement. As they have geometrical similarity with carbon nanotubes, they were expected to impart a significant reinforcement effect on the rubber compounds but the dispersion of the nanofillers is difficult.

  20. Food Preferences of the Rubber Plantation Litter Beetle, Luprops tristis, a Nuisance Pest in Rubber Tree Plantations

    National Research Council Canada - National Science Library

    Thomas K. Sabu; K.V. Vinod

    2009-01-01

    .... Ready availability of the preferred, prematurely fallen, tender rubber tree leaves as a food resource is suggested as being responsible for the exceptionally high abundance of L. tristis in rubber tree plantation belts.

  1. Greenhouse Gas Emissions from Rubber Industry in Thailand

    NARCIS (Netherlands)

    Jawjit, W.; Kroeze, C.; Rattanapan, S.

    2010-01-01

    Rubber production has been taking place in Thailand for many decades. Thailand is currently the world's largest natural rubber producer. We present emissions of greenhouse gases associated with the production of fresh latex, and three primary rubber products, including concentrated latex, block rubb

  2. Guayule and Russian dandelion as alternative sources of natural rubber.

    Science.gov (United States)

    van Beilen, Jan B; Poirier, Yves

    2007-01-01

    Natural rubber, obtained almost exclusively from the Para rubber tree (Hevea brasiliensis), is a unique biopolymer of strategic importance that, in many of its most significant applications, cannot be replaced by synthetic rubber alternatives. Several pressing motives lead to the search for alternative sources of natural rubber. These include increased evidence of allergenic reactions to Hevea rubber, the danger that the fungal pathogen Microcyclus ulei, causative agent of South American Leaf Blight (SALB), might spread to Southeast Asia, which would severely disrupt rubber production, potential shortages of supply due to increasing demand and changes in land use, and a general trend towards the replacement of petroleum-derived chemicals with renewables. Two plant species have received considerable attention as potential alternative sources of natural rubber: the Mexican shrub Guayule (Parthenium argentatum Gray) and the Russian dandelion (Taraxacum koksaghyz). This review will summarize the current production methods and applications of natural rubber (dry rubber and latex), the threats to the production of natural rubber from the rubber tree, and describe the current knowledge of the production of natural rubber from guayule and Russian dandelion.

  3. Interface interactions of natural rubber and protein/fiber aggregates

    Science.gov (United States)

    Mechanical properties of natural rubber are improved with a renewable filler for rubber applications. Aggregates of protein and fiber that constitute soy protein concentrate were shear-reduced and used to enhance the tensile modulus of the natural rubber. The aqueous dispersion of the shear-reduced ...

  4. Greenhouse Gas Emissions from Rubber Industry in Thailand

    NARCIS (Netherlands)

    Jawjit, W.; Kroeze, C.; Rattanapan, S.

    2010-01-01

    Rubber production has been taking place in Thailand for many decades. Thailand is currently the world's largest natural rubber producer. We present emissions of greenhouse gases associated with the production of fresh latex, and three primary rubber products, including concentrated latex, block

  5. 21 CFR 872.6300 - Rubber dam and accessories.

    Science.gov (United States)

    2010-04-01

    ... 21 Food and Drugs 8 2010-04-01 2010-04-01 false Rubber dam and accessories. 872.6300 Section 872...) MEDICAL DEVICES DENTAL DEVICES Miscellaneous Devices § 872.6300 Rubber dam and accessories. (a) Identification. A rubber dam and accessories is a device composed of a thin sheet of latex with a hole in...

  6. 27 CFR 21.125 - Rubber hydrocarbon solvent.

    Science.gov (United States)

    2010-04-01

    ... 27 Alcohol, Tobacco Products and Firearms 1 2010-04-01 2010-04-01 false Rubber hydrocarbon solvent. 21.125 Section 21.125 Alcohol, Tobacco Products and Firearms ALCOHOL AND TOBACCO TAX AND TRADE BUREAU....125 Rubber hydrocarbon solvent. (a) Rubber hydrocarbon solvent is a petroleum derivative....

  7. 30 CFR 77.606-1 - Rubber gloves; minimum requirements.

    Science.gov (United States)

    2010-07-01

    ... 30 Mineral Resources 1 2010-07-01 2010-07-01 false Rubber gloves; minimum requirements. 77.606-1... COAL MINES Trailing Cables § 77.606-1 Rubber gloves; minimum requirements. (a) Rubber gloves (lineman's... be used and tested in accordance with the provisions of §§ 77.704-6 through 77.704-8. (b)...

  8. Treatment of wastewater from rubber industry in Malaysia ...

    African Journals Online (AJOL)

    Treatment of wastewater from rubber industry in Malaysia. ... Discharge of untreated rubber effluent to waterways resulted in water pollution that affected the human health. ... waste minimization, utilization of waste, resource recovery and recycling of ... Key words: Rubber industry, effluent, waste management, Malaysia.

  9. Investigations on cementitious composites based on rubber particle waste additions

    Directory of Open Access Journals (Sweden)

    Glaucio Laun Nacif

    2013-04-01

    Full Text Available The amount of waste rubber has gradually increased over recent years because of over-growing use of rubber products. The disposal of waste rubber has caused serious environmental problems. The incorporation of recycled materials into cementitious composites is a feasible alternative that has gained ground in civil construction. The performance of such materials is much affected not only by the rubber addition, but also the particle size which has been controversially reported in the literature. In order to investigate the single effect of rubber particles into cement based materials, rubber cementitious composites were prepared with no silica particle additions. A full factorial design has been conducted to assess the influence of the rubber particle size (0.84/0.58 mm and 0.28/0.18 mm; mass fraction used (5, 15 and 30%; and water/cement ratio (0.35 and 0.50 on the physic-mechanical properties of the composites. The materials were characterized through apparent density, porosity, compressive strength, flexural strength, modulus of elasticity and microstructural analysis. The interactions of rubber particle size, rubber fraction and water/cement ratio affected significantly the density and compressive strength of the composites. The apparent porosity was influenced mainly by the rubber particle size. The flexural strength was affected by the main factors and the modulus of elasticity was affected by the interaction factors rubber particle size and fraction, and rubber fraction and w/c ratio.

  10. Development of rubber gloves by radiation vulcanization

    Science.gov (United States)

    Makuuchi, K.; Yoshii, F.; Ishigaki, I.; Tsushima, K.; Mogi, M.; Saito, T.

    The processes of radiation vulcanization and production of protective rubber gloves for radioactive contamination are described. A newly developed sensitizing system consisting of 5 phr 2-ethylhexyl acrylate and 1 phr carbon tetrachloride was used to vulcanize natural rubber latex at 12 kGy. Transparent and soft gloves were obtained from the radiation vulcanized latex by a coagulant dipping process. The mechanical properties of the gloves meet Japanese Industrial Standard specification for protective gloves. Combustion analysis of the gloves revealed that the amount of evolved sulfur dioxide and remaining ashes are less than those from commercially available rubber gloves. A trial usage of the gloves at a nuclear power plant showed that the gloves were easy to use for delicate work without undergoing fatigue.

  11. The Properties of Sulfur Rubber Concrete (SRC)

    Institute of Scientific and Technical Information of China (English)

    2006-01-01

    The mix designs and specimen preparation for the dry process and wet process of sulfur rubber concrete (SRC) were investigated.The compressive strength, corrosion-resistance and toughness were studied and discussed.The results show that SRC is corrosion-resistanct.Although the compressive strength of SRC decreases with increasing rubber content, the toughness increases instead.Adding micro-filler will improve the compressive strength of SRC. There is a threshold value for the sulfur content, at which the compressive strength and the work ability of SRC reach an optimum balanc e.The bond between rubber particles and surrounding sulfur is strong due to the vulcanization process that generates cross-links through S-C bonds.

  12. Supply of Rubber Wood Log in Malaysia

    Directory of Open Access Journals (Sweden)

    A. W. Noraida

    2014-06-01

    Full Text Available Issue on shortage of raw material for wood processing solved by discovery of rubber wood log as one of the substitutes the natural log. This paper examines the supply of rubber wood log in Malaysia. We employ ARDL Bound Approach Test and time series data from 1980 to 2010 which represented the whole Malaysia are used to achieve the established objectives. The result shown, in the long run harvested area and wages have 1% and 10% significant level respectively. While in the short run, there was only harvested area having an impact with 1% significant level. This result indicates that, the harvested area become the most impact towards supply of rubber wood log either in short run or in the long run. While wages as input cost gave less impact in another word it become unburden to the producers.

  13. Effect of crumb rubber gradation on a rubberized cold recycled mixture for road pavements

    DEFF Research Database (Denmark)

    Pettinari, Matteo; Simone, Andrea

    2015-01-01

    asphalt design. The mix design represents a key phase of the cold mix production. The study of workability and compactability properties combined with a deep laboratory investigation is required. The idea of introducing crumb rubber in the cold mixtures was developed based on the concept of maximizing...... and cement. The spring-back effects of the rubber particles, which occur after compaction, together with the Indirect Tensile Strength and the Indirect Tensile Stiffness Modulus have been studied. The results show that the gradation of the adopted crumb rubber sensibly affects the compaction and mechanical...

  14. Anisotropic fluorocarbon plasma etching of silicon/silicon germanide heterostructures and plasma etching-induced sidewall damage

    Science.gov (United States)

    Ding, Ruhang

    Plasma etching is a critical tool in the fabrication of Si/SiGe heterostructure quantum devices, but with challenges addressed herein, including (1) control of etch profiles and (2) damage to etched feature sidewalls that affects device performance. (1) Fluorocarbon-based plasma etching often results in device profiles with undercuts due to preferential etching of SiGe over silicon. A C4F8/N2/Ar etch plasma gas mixture introduced here has been successfully used to achieve straight sidewalls through heterostructure layers by formation of a fluorocarbon inhibitor film on feature sidewalls to prevent undercutting. (2) Chemical and structural changes in the semiconductor at feature sidewalls associated with plasma-surface interactions are considered damage, as they affect band structure and electrical conduction in the active region of the device, known as the 2-dimensional electron gas (2DEG). In experiments designed to better understand the mechanisms of plasma-induced sidewall damage, damage to straight wires was characterized both by the width of a non-conductive "sidewall depletion" region at the device sidewall, and by the noise level factor, gamma H/N, determined from spectra of low frequency noise. Observed increases in sidewall depletion width with increasing etch depth are tentatively attributed to the increase in total number of defects with increased plasma exposure time. Excess negative charge incorporated into the fluorocarbon inhibitor film could be another contributing factor. Other factors considered, including defects at the bottom of etched features as well as leakage current bypassing the wire, are ruled out as their contribution is expected to diminish as the distance between the 2DEG and feature bottom increases. The noise level factor, gammaH /N, shows a maximum with increasing etch depth, possibly the result of two competing effects: increasing ion dose and decreasing leakage current. The noise level shows a minimum at an ion bombardment energy

  15. Oxygen exchange in silicone rubber capillaries.

    Science.gov (United States)

    Heineken, F G; Predecki, P K; Filley, G F

    1978-06-01

    Capillaries of 7 and 12.5 mu diameter have been fabricated in silicone rubber. Whole blood treated with heparin has been perfused through these capillaries. Under flowing conditions, no clotting or other clumping effects have been observed and red cells appear to maintain a constant velocity. Oxygen transfer data to and from saline perfusing the 12.5 mu diameter capillaries have been obtained in order to determine how rapidly O2 will permeate the silicone rubber film. The data indicate that the capillaries simulate lung tissue oxygen exchange and will allow for the first time the experimental determination of oxygen exchange kinetics in flowing whole blood.

  16. Phase behavior, rheological property, and transmutation of vesicles in fluorocarbon and hydrocarbon surfactant mixtures.

    Science.gov (United States)

    Yuan, Zaiwu; Qin, Menghua; Chen, Xiushan; Liu, Changcheng; Li, Hongguang; Hao, Jingcheng

    2012-06-26

    We present a detailed study of a salt-free cationic/anionic (catanionic) surfactant system where a strongly alkaline cationic surfactant (tetradecyltrimethylammonium hydroxide, TTAOH) was mixed with a single-chain fluorocarbon acid (nonadecafluorodecanoic acid, NFDA) and a hyperbranched hydrocarbon acid [di-(2-ethylhexyl)phosphoric acid, DEHPA] in water. Typically the concentration of TTAOH is fixed while the total concentration and mixing molar ratio of NFDA and DEHPA is varied. In the absence of DEHPA and at a TTAOH concentration of 80 mmol·L(-1), an isotropic L(1) phase, an L(1)/L(α) two-phase region, and a single L(α) phase were observed successively with increasing mixing molar ratio of NFDA to TTAOH (n(NFDA)/n(TTAOH)). In the NFDA-rich region (n(NFDA)/n(TTAOH) > 1), a small amount of excess NFDA can be solubilized into the L(α) phase while a large excess of NFDA eventually leads to phase separation. When NFDA is replaced gradually by DEHPA, the mixed system of TTAOH/NFDA/DEHPA/H(2)O follows the same phase sequence as that of the TTAOH/NFDA/H(2)O system and the phase boundaries remain almost unchanged. However, the viscoelasticity of the samples in the single L(α) phase region becomes higher at the same total surfactant concentration as characterized by rheological measurements. Cryo-transmission electron microscopic (cryo-TEM) observations revealed a microstructural evolution from unilamellar vesicles to multilamellar ones and finally to gaint onions. The size of the vesicle and number of lamella can be controlled by adjusting the molar ratio of NFDA to DEHPA. The dynamic properties of the vesicular solutions have also been investigated. It is found that the yield stress and the storage modulus are time-dependent after a static mixing process between the two different types of vesicle solutions, indicating the occurrence of a dynamic fusion between the two types of vesicles. The microenvironmental changes induced by aggregate transitions were probed by

  17. Rheological Properties of the Aqueous Solution for Fluorocarbon-containing Hydrophobically Modified Sodium PolyacrylicAcid with Various Surfactants

    Institute of Scientific and Technical Information of China (English)

    GUO,Jin-Feng(郭金峰); ZHUANG,Dong-Qing(庄东青); ZHOU,Hui(周晖); ZHANG,Yun-Xiang(章云祥)

    2001-01-01

    The interaction of fluorocarbon-containing hydrophobicallymodified sodiun polyacryiic acid (FMPAANa) (0.5 wt% )with various surfactants (anionic,nonionic and cationic) hasbeen investigated by theological measurements.Different rhe-ological behaviors are displayed for ionic surfactants and non-ionic surfactants.Fluorinated surfactants have stronger affini-ty with polyelectrolyte hydrophobes comparing with hydro-genated surfactants.The hydrophobic association of FM-PAANa with a cationic surfactant (CTAB) and a fluorinatednonionic surfactant (FC171) is much stronger than with anonionic surfactant (NP7.5 ) and an anionic surfactant(FC143).Further investigation of the effects of temperatureon solution properties shows that the dissociation energy Em iscorrelated to the strength of the aggregated junctions.``

  18. Simulation Process Analysis of Rubber Shock Absorber for Machine Tool

    Directory of Open Access Journals (Sweden)

    Chai Rong Xia

    2016-01-01

    Full Text Available The simulation on rubber shock absorber of machine tool was studied. The simple material model of rubber was obtained by through the finite element analysis software ABAQUS. The compression speed and the hardness of rubber material were considered to obtain the deformation law of rubber shock absorber. The location of fatigue were confirmed from the simulation results. The results shown that the fatigue position is distributed in the corner of shock absorber. The degree of deformation is increased with increasing of compress speed, and the hardness of rubber material is proportional to deformation.

  19. An interactive web-based design system for rubber injection mold: Automotive rubber parts

    Directory of Open Access Journals (Sweden)

    Chamnarn Thongmark

    2016-10-01

    Full Text Available This research aims at integrating a knowledge-based system and web-based technology to facilitate the rubber and rubber composite injection mold design. The system integrates both of computer-aided design and web-based management by using the application programming interface. The research processes started with gathering data and knowledge concerning on rubber injection mold design and process, with the designed framework of the system included. An example part was demonstrated in order to validate the developed system. Based on standardized procedures, the system provides counseling that is able to resolve relevant issues at the early stage of the mold design. The system can be used for both designing and training in rubber mold fabrication.

  20. Surface films of short fluorocarbon-hydrocarbon diblocks studied by molecular dynamics simulations: Spontaneous formation of elongated hemimicelles.

    Science.gov (United States)

    Piñeiro, Angel; Prieto, Gerardo; Ruso, Juan M; Verdes, Pedro V; Sarmiento, Félix

    2009-01-15

    Using grazing incidence small-angle X-ray scattering (GISAXS), and atomic force microscopy (AFM) it has been recently demonstrated that linear fluorocarbon-hydrocarbon diblocks (FnHm) self-assemble in water/air interfaces forming elongated and circular hemimicelles. Those structures have been observed for diblocks with at least eight fluorinated carbons. Based on the lack of a collapse pressure for F6H16, and due to the fact that no stable surface pressure values are reached under compression, it has been concluded that these molecules do not form stable monolayers. It has been also suggested that F6H16 and shorter diblocks desorb from the water surface under compression. It is not easy to accept that a significant concentration of so hydrophobic molecules can be stable in aqueous solution even when the employed experimental techniques were not able to clearly detect a well defined structure on the interface. In the present work the adsorption and arrangement of F6H16 and F6H10 at the water surface are studied by molecular dynamics (MD) simulations as a function of the available area per molecule. Starting from a random mixture, the spontaneous formation of elongated hemimicelles is observed for both systems when the area per molecule is higher than approximately 50 A(2). For intermediate areas two pseudo-phases, one rich in hydrocarbons and the other with higher fluorocarbon concentration, are formed. For the systems with less than approximately 30 A(2) available per molecule the formation of multilayers is observed. This is the first time that the dynamics and structure of perfluoroalkane (PFA) films, and in particular of hemimicelles on a liquid surface, are observed and characterized at atomic level.

  1. Effect of gamma irradiation on the properties of natural rubber/styrene butadiene rubber blends

    OpenAIRE

    A.B. Moustafa; Rania Mounir; A.A. El Miligy; Maysa A. Mohamed

    2016-01-01

    Blends of natural rubber (NR) with styrene butadiene rubber (SBR) with varying ratios have been prepared. Vulcanization of the prepared blends has been induced by irradiation of gamma rays with varying doses up to 250 kGy. Mechanical properties, namely tensile strength, tensile modulus at 100% elongation, elongation at break have been followed up as a function of irradiation dose as well as blend composition. Physical properties, namely gel fraction and swelling number have been followed up u...

  2. Behaviour of asphalt rubber mixtures with different crumb rubber and asphalt binder sources

    OpenAIRE

    Fontes, Liseane P. T. L.; Pereira, Paulo A. A.; Pais, Jorge C.; Trichês, Glicério

    2006-01-01

    This study evaluates the performance in laboratory of gap graded mixture prepared with different crumb rubber types and different conventional grade asphalt binders. The asphalt rubbers were prepared via wet process (continuous blend) and their properties were measured through the current tests: (i) penetration;(ii) softening point: (iii) resilience; (iv) apparent viscosity using a Brookfield viscometer. The rheological properties for conventional asphalts were measured too, in order to evalu...

  3. Natural rubber (NR) biosynthesis: perspectives from polymer chemistry

    Energy Technology Data Exchange (ETDEWEB)

    Barkakaty, Balaka [ORNL

    2014-01-01

    Natural rubber is an important strategic raw material for manufacturing a wide variety of industrial products. There are at least 2,500 different latex-producing plant species; however, only Hevea brasiliensis (the Brazilian rubber tree) is a commercial source. The chemical structure of natural rubber is cis-1,4-polyisoprene, but the exact structure of the head and end groups remains unknown. Since synthetic cis-1,4-polyisoprenes cannot match the superior properties of natural rubber, understanding the chemistry behind the biosynthetic process is key to finding a possible replacement. T his chapter summarizes our current understandings from the perspective of a polymer scientist by comparing synthetic polyisoprenes to natural rubber. The chapter also highlights biomimetic polymerization, research towards a synthetic match of natural rubber and the role of natural rubber in health care.

  4. Rubber recovery from centrifuged natural rubber latex residue using sulfuric acid

    Directory of Open Access Journals (Sweden)

    Wirach Taweepreda

    2013-04-01

    Full Text Available Waste latex sludge from centrifuged residue, which is a null by-product of concentrated latex manufacturing, wasdigested to retrieve the rubber by using sulfuric acid. It was found that the acid concentration and digestion time have aneffect on the amount and purity of the retrieved rubber. Sulfuric acid at concentrations of more than 10% by weight with adigestion time of 48 hours completely digested waste latex sludge and gave rubber 10% by weight. The quality of the retrievedrubber was examined for Mooney viscosity (MV, plasticity retention index, nitrogen content, and ash content. The averagemolecular weight of the retrieved rubber, using gel permeation chromatography, was lower than that of normal natural rubber(NR which corresponds with the MV and initial plasticity (Po. The molecular structure from Fourier transform infraredspectroscopy (FT-IR indicated that the retrieved rubber surface is wet composed with hydroxyl functional ended group.The residue solution was evaporated and crystallized. The structure of crystals was determined using power X-ray diffractometer.

  5. Hardness and compression resistance of natural rubber and synthetic rubber mixtures

    Science.gov (United States)

    Arguello, J. M.; Santos, A.

    2016-02-01

    This project aims to mechanically characterize through compression resistance and shore hardness tests, the mixture of hevea brasiliensis natural rubber with butadiene synthetic rubber (BR), styrene-butadiene rubber (SBR) and ethylene-propylene-diene monomer rubber (EPDM). For each of the studied mixtures were performed 10 tests, each of which increased by 10% the content of synthetic rubber in the mixture; each test consisted of carrying out five tests of compression resistance and five tests of shore hardness. The specimens were vulcanized on a temperature of 160°C, during an approximate time of 15 minutes, and the equipment used in the performance of the mechanical tests were a Shimadzu universal machine and a digital durometer. The results show that the A shore hardness increases directly proportional, with a linear trend, with the content of synthetic BR, SBR or EPDM rubber present in the mixture, being the EPDM the most influential. With respect to the compression resistance is observed that the content of BR or SBR increase this property directly proportional through a linear trend; while the EPDM content also increases but with a polynomial trend.

  6. Preparation of sulfonic acid-containing rubbers from natural rubber vulcanizates

    Science.gov (United States)

    Poonsawat, Worapong; Poompradub, Sirilux; Ngamcharussrivichai, Chawalit

    2014-06-01

    In this work, a series of sulfonic acid-containing rubbers were prepared by aqueous phase oxidation of natural rubber vulcanizates in the presence of hydrogen peroxide (H2O2) and formic acid (HCOOH). The starting vulcanizates were neatly prepared via an efficient vulcanization (EV) system by varying mass ratio of N-cyclohexyl-2-benzothiazole sulfonamide (CBS), as an accelerator, to sulfur. The oxidation conditions were controlled at the molar ratio of H2O2: HCOOH = 1:1, the concentration of H2O2 = 15 wt.%, the temperature = 50 °C, and the reaction time = 3 h. The rubber materials before and after the oxidation were characterized for their physicochemical properties by using Fourier transform infrared spectroscopy, bomb calorimetry, acid-base titration and swelling measurements. The results indicated the presence of sulfonic acid group in the oxidized rubbers, generated by the oxidative cleaves of sulfide crosslinks in the rubber vulcanizates. The oxidation decreased the sulfur content of the rubber in which the level of sulfur loss was determined by the CBS/sulfur ratio. Moreover, the acidity of the oxidized products was correlated with the amount of sulfur remaining.

  7. Reinforcement of graphene in natural rubber nanocomposite

    Science.gov (United States)

    Azira, A. A.; Kamal, M. M.; Rusop, M.

    2016-07-01

    In the present work, we report the use of graphene as multi-functional nanofiller for natural rubber (NR). Dispersion of reduced graphene into natural rubber (NR) was found to enhance the mechanical and electrical properties of NR. Through a facile approach rubber molecules are successfully grafted onto the surface of graphene. Stable graphene suspension with NR afforded a weblike morphology consisting of platelet networks between the rubber particles, while internal mixer processing broke down this structure, yielding a homogeneous and improved dispersion. The resulting graphene can be dispersed in NR via dry mixing. It is found that graphene is prominent in improving the mechanical properties of NR at low filler loading. The percolation point of graphene in the nanocomposites takes place at a content of less than 0.1 wt%. With incorporation of as low as 0.1 wt% of graphene, an increase in the tensile strength and improvement in the tensile modulus achieved. The improvement in the mechanical properties of NR nanocomposites at such low filler loading is attributed to the strong interfacial interaction and the molecular-level dispersion of graphene in the NR matrix. .

  8. Valorisation of Proteins from Rubber Tree

    NARCIS (Netherlands)

    Widyarani,; Coulen, Stef C.W.; Sanders, Johan P.M.; Bruins, Marieke E.

    2016-01-01

    Purpose: The objective of this study was to identify the availability, possible applications, and economic potential of proteins that are present in different parts of the rubber tree. Proteins from non-food sources can be used in e.g. animal feed or biochemicals production with no or little competi

  9. Rubber Recycling: Chemistry, Processing, and Applications

    NARCIS (Netherlands)

    Myhre, M.; Saiwari, S.; Dierkes, W.K.; Noordermeer, J.W.M.

    2012-01-01

    For both environmental and economic reasons, there is broad interest in recycling rubber and in the continued development of recycling technologies. The use of postindustrial materials is a fairly well-established and documented business. Much effort over the past decade has been put into dealing wi

  10. NUTRITIVE VALUE OF RUBBER SEED (Hevea brasiliensis

    Directory of Open Access Journals (Sweden)

    Md. Emran HOSSAIN

    2016-01-01

    Full Text Available The study was undertaken to find out the chemical composition of rubber seeds (Hevea brasiliensis available in Bangladesh. Hevea brasiliensis seeds were collected directly from 200 rubber trees of the rubber garden in the Bandarban area under standard random sampling technique. Seeds were decorticated, ground and dried in hot air oven. Chemical analyses of the samples were carried out in triplicate for moisture, dry matter (DM, crude protein (CP, crude fiber (CF, nitrogen free extract (NFE, ether extract (EE and ash in the animal nutrition laboratory, Chittagong Veterinary and Animal Sciences University, Chittagong, Bangladesh. Metabolizable energy (ME was calculated mathematically by using standard mathematical formula. Results indicated that, decorticated Hevea brasiliensis seeds contained 85.7% DM, 26.1% CP, 43.0% CF, 13.8% NFE, 11.0% EE and 1.8% ash. ME contents in in the seeds was 2101.1 kcal/kg DM. Since, decorticated rubber seeds contained substantial amount of metabolizable energy and proximate components, therefore it could be assumed that, like other unconventional feeds, it might be a promising feed resource for livestock.

  11. Numerical modelling of rubber vibration isolators

    NARCIS (Netherlands)

    Beijers, Clemens A.J.; Boer, de André; Nilsson, A.; Boden, H.

    2003-01-01

    An important cause for interior noise in vehicles is structure-borne sound from the engine. The vibrations of the source (engine) are transmitted to the receiver structure (the vehicle) causing interior noise in the vehicle. For this reason the engine is supported by rubber isolators for passive iso

  12. Rubber Impact on 3D Textile Composites

    Science.gov (United States)

    Heimbs, Sebastian; Van Den Broucke, Björn; Duplessis Kergomard, Yann; Dau, Frederic; Malherbe, Benoit

    2012-06-01

    A low velocity impact study of aircraft tire rubber on 3D textile-reinforced composite plates was performed experimentally and numerically. In contrast to regular unidirectional composite laminates, no delaminations occur in such a 3D textile composite. Yarn decohesions, matrix cracks and yarn ruptures have been identified as the major damage mechanisms under impact load. An increase in the number of 3D warp yarns is proposed to improve the impact damage resistance. The characteristic of a rubber impact is the high amount of elastic energy stored in the impactor during impact, which was more than 90% of the initial kinetic energy. This large geometrical deformation of the rubber during impact leads to a less localised loading of the target structure and poses great challenges for the numerical modelling. A hyperelastic Mooney-Rivlin constitutive law was used in Abaqus/Explicit based on a step-by-step validation with static rubber compression tests and low velocity impact tests on aluminium plates. Simulation models of the textile weave were developed on the meso- and macro-scale. The final correlation between impact simulation results on 3D textile-reinforced composite plates and impact test data was promising, highlighting the potential of such numerical simulation tools.

  13. Filled liquid silicone rubbers: Possibilities and challenges

    DEFF Research Database (Denmark)

    Yu, Liyun; Vudayagiri, Sindhu; Zakaria, Shamsul Bin

    2014-01-01

    Liquid silicone rubbers (LSRs) have been shown to possess very favorable properties as dielectric electroactive polymers due to their very high breakdown strengths (up to 170 V/μm) combined with their fast response, relatively high tear strength, acceptable Young’s modulus as well as they can...

  14. Identification and Waste Reduction on Rubber Industry

    Science.gov (United States)

    Syahputri, K.; Sari, R. M.; Rizkya, I.; Siregar, I.

    2017-03-01

    Lots of activities in production process can be lead to waste activities. The waste may cause a degree of efficiency of an industry to be low. This research was conducted in the rubber industry. In the rubber industry has been a decline in the level of efficiency. Decreased levels of efficiency occurs because many inefficient activities that take place during the production process. Activities that were not contributed to the value of the product lead to waste during the production process. Identification by the activity is a way to minimize the waste that occurs so that the efficiency of the production process can be improved. Process activity mapping in the rubber industry used to identify the activities that take place on the floor of production in order to reduce waste and propose improvements that can be done to improve efficiency. The total waste that occurs in crumb rubber industry amounted to 94 minutes or 1.56 hours. For the proposed improvements in order to reduce waste are based on two activities, such as transport and unnecessary motion. Transport activities proposed use of material handling in their daily activities and to unnecessary motion by doing a variety of work on the operator.

  15. Cancer mortality and morbidity among rubber workers.

    Science.gov (United States)

    Monson, R R; Fine, L J

    1978-10-01

    Mortality and morbidity from cancer among a cohort of 13,570 white male rubber workers were examined. Each man worked for at least 5 years at the Akron, Ohio, plant of the B. F. Goodrich Company. The potential period of follow-up was from January 1, 1940 to June 30, 1976. Departmental work histories were based primarily on records maintained by Local no. 5, United Rubber Workers. The occurrence of cancer was measured by death certificates and by a survey of Akron-area hospital tumor registries from 1964 to 1974. Two types of analyses were made: 1) an external comparison of mortality rates of rubber workers versus rates of U.S. white males, and 2) an internal comparison of cancer morbidity rates among persons who were employed in various work areas of the plant. Excess cases of specific cancers (observed/expected numbers) among workers in specific work areas included: stomach and intestine: rubber making (30/14.4); lung: tire curing (31/14.1), fuel cells and/or deicers (46/29.1); bladder: chemical plant (6/2.4), and tire building (16/10.7); skin cancer: tire assembly (12/1.9); brain cancer: tire assembly (8/2.0); lymphatic cancer: tire building (8/3.2); and leukemia: calendering (8/2.2), tire curing (8/2.6), tire building (12/7.5), elevators (4/1.4), tubes (4/1.6), and rubber fabrics (4/1.1). Agents that may be responsible for these excesses were considered.

  16. Silencing the lettuce homologs of small rubber particle protein does not influence natural rubber biosynthesis in lettuce (Lactuca sativa).

    Science.gov (United States)

    Chakrabarty, Romit; Qu, Yang; Ro, Dae-Kyun

    2015-05-01

    Natural rubber, cis-1,4-polyisoprene, is an important raw material in chemical industries, but its biosynthetic mechanism remains elusive. Natural rubber is known to be synthesized in rubber particles suspended in laticifer cells in the Brazilian rubber tree (Hevea brasiliensis). In the rubber tree, rubber elongation factor (REF) and its homolog, small rubber particle protein (SRPP), were found to be the most abundant proteins in rubber particles, and they have been implicated in natural rubber biosynthesis. As lettuce (Lactuca sativa) can synthesize natural rubber, we utilized this annual, transformable plant to examine in planta roles of the lettuce REF/SRPP homologs by RNA interference. Among eight lettuce REF/SRPP homologs identified, transcripts of two genes (LsSRPP4 and LsSRPP8) accounted for more than 90% of total transcripts of REF/SRPP homologs in lettuce latex. LsSRPP4 displays a typical primary protein sequence as other REF/SRPP, while LsSRPP8 is twice as long as LsSRPP4. These two major LsSRPP transcripts were individually and simultaneously silenced by RNA interference, and relative abundance, polymer molecular weight, and polydispersity of natural rubber were analyzed from the LsSRPP4- and LsSRPP8-silenced transgenic lettuce. Despite previous data suggesting the implications of REF/SRPP in natural rubber biosynthesis, qualitative and quantitative alterations of natural rubber could not be observed in transgenic lettuce lines. It is concluded that lettuce REF/SRPP homologs are not critically important proteins in natural rubber biosynthesis in lettuce. Copyright © 2014 Elsevier Ltd. All rights reserved.

  17. Carbon and Oxygen Isotopic Characteristics of REE—Fluorocarbonate Minerals and Their Genetic Implications,Bayan Obo Deposit,Inner Mongloia,China

    Institute of Scientific and Technical Information of China (English)

    方涛; 裘愉卓; 等

    1996-01-01

    REE-fluorocarbonates as major REE minerals in the Bayan Obo deposit,the largest REE deposit in the world,were analyzed for their stable isotopic compositions,The δ13 C and δ18 O values of huanghoite,cebaite and bastnaesite from late-stage veins vary in the ranges of 7.8--4.0‰ and 6.7-9.4‰,respectively,These data are relatively similar to those of bastnaesites from banded ores:δ13C-5.6--5.2‰ andδ18O3.6-5.5‰.The REE fluorocarbonates from both late-staege veins and banded ores are characterized by lower δ13 C and δ18O values,especially the δ18O values of bastnaesites from banded ores.Compared with them,the disseminated bastnaesits the dolomite-type ores possess rather highδ13 C and δ18O values,i.e.,-2.1-0.4‰ and 8.6-12.9‰ respectively.The high values are typical of the sedimentary host dolomite rocks as well as of the dolomite-type-ores.The carbon and oxygen isotopic characteristics of REE fluorocarbonate minerals provide new evidence for the hypothesis on the origin of Bayan Obo deposit-epigenetic hydrothermal metasomatism.

  18. Surface etching mechanism of carbon-doped Ge{sub 2}Sb{sub 2}Te{sub 5} phase change material in fluorocarbon plasma

    Energy Technology Data Exchange (ETDEWEB)

    Shen, Lanlan [Chinese Academy of Sciences, State Key Laboratory of Functional Materials for Informatics, Shanghai Institute of Micro-system and Information Technology, Shanghai (China); Graduate School of the Chinese Academy of Sciences, Beijing (China); Song, Sannian; Song, Zhitang; Li, Le; Guo, Tianqi; Cheng, Yan; Lv, Shilong; Wu, Liangcai; Liu, Bo; Feng, Songlin [Chinese Academy of Sciences, State Key Laboratory of Functional Materials for Informatics, Shanghai Institute of Micro-system and Information Technology, Shanghai (China)

    2016-09-15

    Recently, carbon-doped Ge2Sb2Te5 (CGST) phase change material has been widely researched for being highly promising material for future phase change memory application. In this paper, the reactive-ion etching of CGST film in CF{sub 4}/Ar plasma is studied. Compared with GST, the etch rate of CGST is relatively lower due to the existence of carbon which reduce the concentration of F or CF{sub x} reactive radicals. It was found that Argon plays an important role in defining the sidewall edge acuity. Compared with GST, more physical bombardment is required to obtain vertical sidewall of CGST. The effect of fluorocarbon gas on the damage of the etched CGST film was also investigated. A Ge- and Sb-deficient layer with tens of nanometers was observed by TEM combining with XPS analysis. The reaction between fluorocarbon plasma and CGST is mainly dominated by the diffusion and consumption of reactive fluorine radicals through the fluorocarbon layer into the CGST substrate material. The formation of damage layer is mainly caused by strong chemical reactivity, low volatility of reaction compounds and weak ion bombardment. (orig.)

  19. Shape memory rubber bands & supramolecular ionic copolymers

    Science.gov (United States)

    Brostowitz, Nicole

    The primary focus of this dissertation is to understand the thermo-mechanical properties that govern shape memory in rubber blends. An ideal shape memory polymer (SMP) has a large entropic component that drives shape recovery with a distinct transition mechanism to control the recovery conditions. Polyisoprene rubber is highly elastic and shows shape memory behavior through strain induced crystallization above its glass transition temperature. However, this transition temperature is below 0°C and not suitable for most applications. Shape memory blends can tailor the transition temperature through selection of the switching phase. Most SMP blends require complicated synthesis routes or intensive compounding which would be inhibitive for production. A facile method was developed for fabrication of a robust shape memory polymer by swelling cross-linked natural rubber with stearic acid. Thermal, microscopic studies showed that stearic acid formed a percolated network of crystalline platelets within the natural rubber. Further investigation of the material interactions was carried out with a low molecular weight polyisoprene analog, squalene, and stearic acid gel. Tensile tests on the rubber band demonstrated the thermo-mechanical effect of swelling with stearic acid. Low hysteresis was observed under cyclic loading which indicated viability for the stearic acid swollen rubber band as an SMP. The microscopic crystals and the cross-linked rubber produce a temporary network and a permanent network, respectively. These two networks allow thermal shape memory cycling with deformation and recovery above the melting point of stearic acidand fixation below that point. Under manual, strain-controlled tensile deformation, the shape memory rubber bands exhibited fixity and recovery of 100% +/- 10%. The recovery properties of the SMP were studied under various loading conditions and a model was fit to describe the potential recovery with relation to the fixation. An additional

  20. Occupational disease in the rubber industry.

    Science.gov (United States)

    Peters, J M; Monson, R R; Burgess, W A; Fine, L J

    1976-10-01

    We have studied mortality patterns in a large cohort of rubber workers. We have examined workers exposed to curing fumes, processing dusts, and industrial talc and have begun to evaluate exposures of these workers in detail. Gastrointestinal (especially stomach) cancer appears in excess in processing workers. Lung cancer is excessive in curing workers. Leukemia is increased generally. All three groups studied for respiratory disease have an increase in disease prevalence which is related to intensity and duration of exposure. Since both an increase in stomach cancer and respiratory disease is seen in processing workers, exposures in this area must be controlled. Since both lung cancer and chronic respiratory disease is excessive in curing rooms, this exposure must be controlled. The leukemia risk is probably related to solvents. Whether this is all explainable by past benzene exposure is unknown. Further studies are planned to refine our knowledge concerning these risks so that occupational disease in the rubber industry can be prevented.

  1. Synthetic rubbers prepared by lanthanide coordination catalysts

    Institute of Scientific and Technical Information of China (English)

    2009-01-01

    China is rich in rare earth resources. Rare earth elements, also named lanthanides, are number 58 to number 81 elements in the elemental periodic table. They have unique electronic structures and may form various coordination compounds. In the early 1960s, researchers at the Changchun Institute of Applied Chemistry, Chinese Academy of Sciences (CIAC) found the catalytic activities of lanthanide compounds in stereospecific polymerization of conjugated dienes, and published the first paper on this topic in 1964. On the basis of this finding, CIAC launched extensive research activities on lanthanide compounds as diene polymerization catalysts, from a series of fundamental research to the efforts of industrializing the rare earth catalyzed cis-1,4-polybutatine rubber and cis-1,4-polyisoprene rubber. This review aims to summarize the progress in this field in the past half century.

  2. Synthetic rubbers prepared by lanthanide coordination catalysts

    Institute of Scientific and Technical Information of China (English)

    CHEN WenQi; WANG FoSong

    2009-01-01

    China is rich in rare earth resources. Rare earth elements, also named Ianthanides, are number 58 to number 81 elements in the elemental periodic table. They have unique electronic structures and may form various coordination compounds. In the early 1960s, researchers at the Changchun Institute of Applied Chemistry, Chinese Academy of Sciences (CIAC) found the catalytic activities of lanthanide compounds in stereospecific polymerization of conjugated dienes, and published the first paper on this topic in 1964. On the basis of this finding, CIAC launched extensive research activities on lanthanide compounds as diene polymerization catalysts, from a series of fundamental research to the efforts of industrializing the rare earth catalyzed cis~(-1),4-polybutatine rubber and cis~(-1),4-polyisoprene rubber. This review aims to summarize the progress in this field in the past half century.

  3. On the response of rubbers at high strain rates.

    Energy Technology Data Exchange (ETDEWEB)

    Niemczura, Johnathan Greenberg (University of Texas-Austin)

    2010-02-01

    In this report, we examine the propagation of tensile waves of finite deformation in rubbers through experiments and analysis. Attention is focused on the propagation of one-dimensional dispersive and shock waves in strips of latex and nitrile rubber. Tensile wave propagation experiments were conducted at high strain-rates by holding one end fixed and displacing the other end at a constant velocity. A high-speed video camera was used to monitor the motion and to determine the evolution of strain and particle velocity in the rubber strips. Analysis of the response through the theory of finite waves and quantitative matching between the experimental observations and analytical predictions was used to determine an appropriate instantaneous elastic response for the rubbers. This analysis also yields the tensile shock adiabat for rubber. Dispersive waves as well as shock waves are also observed in free-retraction experiments; these are used to quantify hysteretic effects in rubber.

  4. Biodiesel Production from Rubber Seed Oil via Esterification Process

    Directory of Open Access Journals (Sweden)

    W Widayat

    2012-07-01

    Full Text Available One promise source of alternative energy is biodiesel from rubber seed oil, because the raw materials available in plentiful quantities and can be renewed. In addition, the rubber seed is still lack of utilization, and Indonesia is one of the largest rubbers producing country in the world. The objective of this research is to studied on biodiesel production by esterification process. Parameters used in this study are the ratio of catalyst and temperature and its influence on the characteristics of the resulting biodiesel product. Characterization of rubber seed include acid content number analysis, saponification numbers, density, viscosity, iodine number, type of free fatty acids and triglyceride oils. The results of analysis showed that rubber seed oil content obtained is 50.5%. The results of the GCMS analysis showed that a free fatty acid level in rubber seed is very high. Conversion into bio-diesel oil is obtained by at most 59.91% and lowest 48.24%.

  5. MODIFYING V-14 RUBBER WITH CARBON FIBERS

    Directory of Open Access Journals (Sweden)

    Shadrinov N. V.

    2016-01-01

    Full Text Available The influence of carbon fibers and modified carbon fibers on properties of industrially produced V-14 rubber is examined. The dependences of physical and mechanical properties, hardness, abrasion resistance and resistance in aggressive environment on few amount of filled fiber are established. Structural properties of reinforced elastomeric composites are studied by scanning electron microscopy. Elastomeric layer on the surface of modified carbon fiber, confirmed with high adhesion is identified

  6. Magnesium affects rubber biosynthesis and particle stability in Ficus elastica, Hevea brasiliensis and Parthenium argentatum

    Science.gov (United States)

    Natural rubber biosynthesis occurs in laticifers of Ficus elastica and Hevea brasiliensis, and in parenchyma cells of Parthenium argentatum. Natural rubber is synthesized by rubber transferase using allylic pyrophosphates as initiators, isopentenyl pyrophosphate as monomeric substrate and magnesium ...

  7. 75 FR 36472 - Goodyear Tire and Rubber Company, Receipt of Petition for Decision of Inconsequential Noncompliance

    Science.gov (United States)

    2010-06-25

    ... National Highway Traffic Safety Administration Goodyear Tire and Rubber Company, Receipt of Petition for Decision of Inconsequential Noncompliance Goodyear Tire and Rubber Company, (Goodyear),\\1\\ has determined... 573, Defect and Noncompliance Responsibility and Reports. \\1\\ Goodyear Tire and Rubber...

  8. 78 FR 9775 - Cooper Tire & Rubber Company, Receipt of Petition for Decision of Inconsequential Noncompliance

    Science.gov (United States)

    2013-02-11

    ... National Highway Traffic Safety Administration Cooper Tire & Rubber Company, Receipt of Petition for.... ACTION: Receipt of Petition. SUMMARY: Cooper Tire & Rubber Company (Cooper),\\1\\ has determined that..., Defect and Noncompliance Responsibility and Reports. \\1\\ Cooper Tire & Rubber Company, is a...

  9. 76 FR 28502 - Cooper Tire & Rubber Tire Company, Receipt of Petition for Decision of Inconsequential Noncompliance

    Science.gov (United States)

    2011-05-17

    ... National Highway Traffic Safety Administration Cooper Tire & Rubber Tire Company, Receipt of Petition for Decision of Inconsequential Noncompliance Cooper Tire & Rubber Tire Company, (Cooper),\\1\\ has determined...\\ Cooper Tire & Rubber Tire Company (Cooper) is a replacement equipment manufacturer incorporated in...

  10. Use of rubber crumb for preparation of asphalt-concrete mixtures

    Directory of Open Access Journals (Sweden)

    Yerbol Tileuberdi

    2012-03-01

    Full Text Available In this article use of rubber crumb from spent tire for preparation of rubber-bitumen compounds is investigated. Then the rubber-bitumen compositions are used in composition of asphalt concrete mixes .

  11. Use of rubber crumb for preparation of asphalt-concrete mixtures

    OpenAIRE

    Yerbol Tileuberdi; S. Kozbakarova; Yerdos Ongarbayev; B. Tuleutaev; Zulkhair Mansurov

    2012-01-01

    In this article use of rubber crumb from spent tire for preparation of rubber-bitumen compounds is investigated. Then the rubber-bitumen compositions are used in composition of asphalt concrete mixes .

  12. Tensile Strength of PHBV/Natural Rubber Latex Mixtures

    OpenAIRE

    Promkotra Sarunya; Kangsadan Tawiwan

    2015-01-01

    A polyhydroxybutyrate-co-hydroxyvalerate (PHBV) is mingled with natural rubber latex (R) to develop its mechanical property of the blend. Normally, substantial effects of the PHBV are hard, fragile, and inelastic, whereas the natural rubber is represented itself as very high elastic matter. The mixtures between the PHBV and natural rubber latex (R) are considered in different proportions. The PHBV solutions (w/v) are defined suitability at 1% (P1), 2% (P2), and 3% (P3). Their liquid mixtures ...

  13. Impact resistance of concrete – using slit rubber from tyres

    OpenAIRE

    Coventry, Kathryn; Richardson, Alan; Diaz, Eli

    2015-01-01

    This paper examines recycled tyre rubber, which was machine cut into slits and these were added to Portland cement concrete mixes in different percentages, based on specimen volume. They were then tested to determine the impact performance of each mix in comparison to a plain non-rubberised mix. \\ud The results indicated that concrete samples containing recycled rubber, exhibited a loss in compressive strength when compared to the plain concrete mix, however, the rubber modified samples were ...

  14. The improvement of pavement performance using asphalt rubber hot mixes

    OpenAIRE

    Pais, Jorge C.; Pereira, Paulo A. A.

    2007-01-01

    The need of a better pavement performance has led researchers to develop new road materials, mainly for the asphalt layers, where the modification of the asphalt is the main example. This modification usually forces the use of polymers and fibers and, more recently, the use of crumb rubber from ground tires, where the modified asphalt is known as asphalt rubber. This asphalt rubber used in asphalt mixtures produces a superior performance if compared to the asphalt mixtures with...

  15. Effect of base bitumen composition on asphalt rubber binder properties

    OpenAIRE

    Partl, M.N.; Ould-Henia, M.; Dumont, A.-G.

    2008-01-01

    The asphalt rubber blend properties are strongly related to its base components properties. The base bitumen composition is considered as a key factor influencing the final rheological properties of asphalt rubber binder. This paper describes results from a laboratory investigation of the interaction between crumb rubber and different composition bitumen according to the wet process. The bitumen composition is determined according to the SARA decomposition approac...

  16. Design, manufacturing and testing of Controllable Rubber Trailing Edge Flaps

    DEFF Research Database (Denmark)

    Løgstrup Andersen, Tom; Aagaard Madsen, Helge; Barlas, Thanasis K

    The overall goal for the INDUFLAP project was realization of a test facility for development and test of Controllable Rubber Trailing Edge Flaps (CRTEF) for wind turbines. This report covers experimental work at DTU Wind Energy including design, manufacture and test of different configurations...... of flaps with voids in chord- or spanwise direction. Development of rubber flaps has involved further design improvements. Non-metallic spring elements and solutions for sealing of continuous extruded rubber profiles have been investigated....

  17. Impact resistance of concrete – using slit rubber from tyres

    OpenAIRE

    Coventry, Kathryn; Richardson, Alan; Diaz, Eli

    2015-01-01

    This paper examines recycled tyre rubber, which was machine cut into slits and these were added to Portland cement concrete mixes in different percentages, based on specimen volume. They were then tested to determine the impact performance of each mix in comparison to a plain non-rubberised mix. \\ud The results indicated that concrete samples containing recycled rubber, exhibited a loss in compressive strength when compared to the plain concrete mix, however, the rubber modified samples were ...

  18. Mortality among rubber workers: V. processing workers.

    Science.gov (United States)

    Delzell, E; Monson, R R

    1982-07-01

    Cause-specific mortality was evaluated among 2,666 men employed in the processing division of a rubber manufacturing plant. The division was divided into two sections: front processing (compounding, mixing and milling operations) and back processing (extrusion, calendering, cement mixing and rubberized fabrics operations). Mortality rates for all processing workers combined and for men in each section were compared with rates for U.S. White males or for workers employed in other divisions of the same plant. Compared with either referent group, men in the processing division had increased mortality from leukemia, emphysema, and cancers of the stomach, large intestine, and biliary passages and liver. An excess number of deaths from stomach and larger intestine cancer was found predominantly among men in the front processing section (33 observed vs. 17.7 expected deaths, based on rates in nonprocessing workers). Increased mortality from leukemia (14 observed vs. 7.3 expected) and from emphysema (22 observed vs. 11.0 expected) was present among men employed in the back processing section. Examination of mortality from these causes according to age and the year starting work, duration of employment, and years since starting work in the relevant sections of the processing division suggested that observed excesses of stomach cancer, large intestine cancer, leukemia, and emphysema among processing workers are related to occupational exposures. These results are consistent with the findings of studies of other groups of rubber workers.

  19. Boron-Loaded Silicone Rubber Scintillators

    CERN Document Server

    Bell, Z W; Maya, L; Sloop, F V J

    2003-01-01

    Silicone rubber received attention as an alternative to polyvinyltoluene in applications in which the scintillator is exposed to high doses because of the increased resistance of the rubber to the formation of blue-absorbing color centers. Work by Bowen, et al., and Harmon, et al., demonstrated their properties under gamma/x-ray irradiation, and Bell, et al. have shown their response to thermal neutrons. This last work, however, provided an example of a silicone in which both the boron and the scintillator were contained in the rubber as solutes, a formulation which led to the precipitation of solids and sublimation of the boron component. In the present work we describe a scintillator in which the boron is chemically bonded to the siloxane and so avoids the problem of precipitation and loss of boron to sublimation. Material containing up to 18% boron, by weight, was prepared, mounted on photomultipliers, and exposed to both neutron and gamma fluxes. Pulse height spectra showing the neutron and photon respons...

  20. Elucidation of filler-to-filler and filler-to-rubber interactions in silica-reinforced natural rubber by TEM Network Visualization

    NARCIS (Netherlands)

    Sarkawi, S.S.; Dierkes, W.K.; Noordermeer, J.W.M.

    2014-01-01

    Filler-to-rubber interaction is a key parameter in the reinforcement of rubber. This paper presents an investigation into filler-to-filler and filler-to-rubber interactions in silica-reinforced natural rubber (NR) in the presence and absence of a silane coupling agent. Using a special network visual

  1. Barrierity of hydrogenated butadiene-acrylonitrile rubber and butyl rubber after exposure to organic solvents.

    Science.gov (United States)

    Krzemińska, Sylwia; Rzymski, Władysław M

    2011-01-01

    Resistance of antichemical clothing primarily depends on the type of material it is made from, in particular on the type of polymer used for coating the fabric carrier. This paper reports on systematic investigations on the influence of the cross-linking density of an elastomer and the composition of a cross-linked elastomer on its resistance to permeation of selected organic solvents. Tests of barrier material samples made from nonpolar butyl rubber (IIR) and polar hydrogenated butadiene-acrylonitrile rubber (HNBR) showed that (a) in rubber-solvent systems with medium thermodynamic affinity, cross-linking density influenced resistance to permeation and (b) the polarity of the system had a significant influence on barrierity.

  2. Geotechnical Properties of Rubber Tires and Sediments Mixtures

    Directory of Open Access Journals (Sweden)

    H. Sellaf

    2014-04-01

    Full Text Available An experimental work was undertaken to study the effect of rubber tires on the geotechnical properties of a dredged sediment, using a mixing ratio of large size. For comparison, two types of soil were studied (dredged sediment from Fergoug dam and Tizi Tuff from the north west of Algeria. Taking into account the high compressibility and the low water absorption of the rubber tires, grain size analysis, density, Atterberg limits analysis, chemical composition, direct shear tests, loading-unloading tests, modified Proctor and CBR tests are performed on the two soils and their mixtures with different scrap tire rubber (10, 20, 25 and 50%. The results show that liquid limits and plastic indexes decrease with the scrap tire rubber content and that the decrease is more significant for soil with high plasticity. Cohesion also decreases with scrap tire rubber content when the internal friction angle is vacillating. Compression and recompression indexes increase gradually with the scrap tire rubber content and the variation for compression index is more significant for the two soils. Compaction characteristics and CBR values decrease with scrap tire rubber content. The CBR values for W=3% are important compared to those with W=5% excepted for mixture with (75% tuff and 25% scrap tire rubber. The results show that the scrap tire rubber can be used as a reinforcement material for dredged soil, but with a content that should not highly affect the compressibility.

  3. [Contamination of solid-cast rubber tires by microscopic fungi].

    Science.gov (United States)

    Chuienko, A I; Subbota, A H; Olishevs'ka, S V; Zaslavs'kyĭ, V A; Zhdanova, N M

    2010-01-01

    The main peculiarities of fungal resistance of two types of unit cast rubber tires of domestic manufacture have been investigated. Rubber tires which contained synthetic plasticizer were non-resistant to fungal contamination in contrast to ones with natural plasticizer. Using the method of confocal laser-scanning microscopy, it was shown that inner layers of two types of rubber tires were contaminated with fungal mycelium. Our findings indicate that the investigation of microscopic fungi resistance of new materials is necessary for general mechanical rubber goods, especially exported to tropical climate countries.

  4. Amphiphilic semi-interpenetrating polymer networks using pulverized rubber

    Science.gov (United States)

    Shahidi, Nima

    Scrap rubber materials provide a significant challenge to either reuse or safe disposal. Every year, millions of tires are discarded to landfills in the United States, consuming a staggering amount of land space, creating a high risk for large fires, breeding mosquitoes that spread diseases, and wasting the planet's natural resources. This situation cannot be sustained. The challenge of reusing scrap rubber materials is mainly due to the crosslinked structure of vulcanized rubber that prevent them from melting and further processing for reuse. The most feasible recycling approach is believed to be a process in which the vulcanized rubber is first pulverized into a fine powder and then incorporated into new products. The production of fine rubber particles is generally accomplished through the use of a cryogenic process that is costly. Therefore, development of a cost effective technology that utilizes a large quantity of the scrap rubber materials to produce high value added materials is an essential element in maintaining a sustainable solution to rubber recycling. In this research, a cost effective pulverization process, solid state shear extrusion (SSSE), was modified and used for continuous pulverization of the rubber into fine particles. In the modified SSSE process, pulverization takes place at high compressive shear forces and a controlled temperature. Furthermore, an innovative particle modification process was developed to enhance the chemical structure and surface properties of the rubber particles for manufacturing of high value added products. Modification of rubber particles was accomplished through the polymerization of a hydrophilic monomer mixture within the intermolecular structure of the hydrophobic rubber particles. The resulting composite particles are considered as amphiphilic particulate phase semi-interpenetrating polymer networks (PPSIPNs). The modified rubber particles are water dispersible and suitable for use in a variety of aqueous media

  5. Research on the sound absorption performance of metal rubber material

    Institute of Scientific and Technical Information of China (English)

    XIA Yuhong; JIANG Hongyuan; WU Guoqi; E.A. Izzheurov

    2009-01-01

    The sound absorption performance of Metal Rubber material was studied theoreti-cally and experimentally. The acoustic impedance rate and the sound absorption coefficient were derived based on the acoustic parameters of metal rubber material. The relation of structure constant, compressibility modulus and structural parameters was investigated experimentally. The results showed that the specimen of metal rubber with the same mean porosity diame-ter had the same structure constant. For the same structural parameters, the compressibility modulus of metal rubber material was approximately constant in certain frequency range. The calculated acoustic parameters are in good agreement with the experimental results, demon-strating the effectiveness of theoretical models.

  6. Effect of Chipped Rubber Aggregates on Performance of Concrete

    Directory of Open Access Journals (Sweden)

    Sunil N. Shah

    2014-12-01

    Full Text Available Due to rapid growth in automobile industry, use of tyre increases day to day and there is no reuse of the same to decrease the environmental pollution. The decomposition and disposing of waste tyre rubber is harmful to environment. This research reflects the reuse of waste tyre rubber into concrete after observing their properties. In that experimental work chipped rubber aggregates replaced to the natural coarse aggregates by varying percentage of 3, 6, 9 and 12 with comparison of 0% replacement. Silica fume is replaced in 10% with cement for improving the bond properties between cement paste and rubber. In evaluation, test has been carried out to determine the properties of concrete such as workability, unit weight, flexural strength and split tensile strength. The workability of fresh concrete is observed with the help of compaction factor test. From the test of compaction factor, workability is decrease with increasing percentage of chipped rubber. The specific gravity of chipped rubber aggregates is lower as compared to natural aggregates therefore decrease the unit weight of rubber mix concrete. Increasing chipped rubber aggregates as partial replacement into concrete reduces compressive strength. So these can use in non-primary structural applications of medium to low strength requirements. The overall results of study show that it is possible to use recycled rubber tyre aggregates in concrete construction as partial replacement to natural coarse aggregates.

  7. Influence of temperature changes on torsional rigidity and damping coefficient of rubber torsional vibration damper

    OpenAIRE

    Wojciech HOMIK

    2011-01-01

    The short explanation of usefulness of rubber torsional dampers in crankshaft in multi-cylinder engines is presented. The description of the construction and operation of rubber torsional damper is also included. In the rubber torsional damper, the damping is achieved as the effect of internal friction resulting from the deformation of the rubber material. This deformation appears while the internal rubber elasticity is overloaded. Both the physical and mechanical rubber properties depend on ...

  8. A Review on the Effect of Crumb Rubber Addition to the Rheology of Crumb Rubber Modified Bitumen

    Directory of Open Access Journals (Sweden)

    Mohd Rasdan Ibrahim

    2013-01-01

    Full Text Available Crumb rubber modification has been proven to enhance the properties of pure bitumen. This paper looks at some of the international standards for producing crumb rubber modified bitumen (CRMB and reviews the effect of crumb rubber to the rheology of crumb rubber modified bitumen. The review shows that the rheology of CRMB depends on internal factors such as crumb rubber quantity, particle size, and pure bitumen composition, and external factors such as the mixing time, temperature, and also the modification technique. These factors govern the swelling process of crumb rubber particles that lead to the increase of viscosity of the modified bitumen. However, the mixing temperature and duration can cause rubber particles to depolymerize and subsequently cause loss of viscosity. Crumb rubber modification also improves the properties of bitumen by increasing the storage and loss modulus and enhancing the high and low temperature susceptibility. The effect of crumb rubber to aging properties of CRMB is also discussed. Finally several techniques of chemical modification to terminal blends of CRMB and the subsequent improvement to the settling property of CRMB are explained.

  9. Mesoporous fluorocarbon-modified silica aerogel membranes enabling long-term continuous CO2 capture with large absorption flux enhancements.

    Science.gov (United States)

    Lin, Yi-Feng; Chen, Chien-Hua; Tung, Kuo-Lun; Wei, Te-Yu; Lu, Shih-Yuan; Chang, Kai-Shiun

    2013-03-01

    The use of a membrane contactor combined with a hydrophobic porous membrane and an amine absorbent has attracted considerable attention for the capture of CO2 because of its extensive use, low operational costs, and low energy consumption. The hydrophobic porous membrane interface prevents the passage of the amine absorbent but allows the penetration of CO2 molecules that are captured by the amine absorbent. Herein, highly porous SiO2 aerogels modified with hydrophobic fluorocarbon functional groups (CF3 ) were successfully coated onto a macroporous Al2 O3 membrane; their performance in a membrane contactor for CO2 absorption is discussed. The SiO2 aerogel membrane modified with CF3 functional groups exhibits the highest CO2 absorption flux and can be continuously operated for CO2 absorption for extended periods of time. This study suggests that a SiO2 aerogel membrane modified with CF3 functional groups could potentially be used in a membrane contactor for CO2 absorption. Also, the resulting hydrophobic SiO2 aerogel membrane contactor is a promising technology for large-scale CO2 absorption during the post-combustion process in power plants.

  10. Nanoscale mechanical and tribological properties of fluorocarbon films grafted onto plasma-treated low-density polyethylene surfaces

    Science.gov (United States)

    Cheng, Q.; Komvopoulos, K.

    2012-03-01

    Fluorocarbon (FC) films were grafted onto Ar plasma-treated low-density polyethylene (LDPE) surfaces by plasma polymerization and deposition. The evolution of the surface morphology of the grafted FC films was investigated at different scales with an atomic force microscope. Nanoscale sliding experiments performed with a surface force microscope provided insight into the nanotribological properties of Ar plasma-treated LDPE, with and without grafted FC films, in terms of applied normal load and number of sliding cycles. The observed trends are explained in the context of microstructure models accounting for morphological and structure changes at the LDPE surface due to the effects of plasma treatment (e.g., selective etching of amorphous phase, chain crosslinking and FC film grafting) and surface sliding (e.g., crystalline lamellae alignment along the sliding direction). Nanoindentation experiments elucidated the effect of plasma treatment on surface viscoelasticity and global contact stiffness. The results of this study demonstrate that plasma-assisted grafting of FC films is an effective surface modification method for tuning the nanomechanical/tribological properties of polymers.

  11. Plasma-deposited fluorocarbon polymer films on titanium for preventing cell adhesion: a surface finishing for temporarily used orthopaedic implants

    Science.gov (United States)

    Finke, B.; Testrich, H.; Rebl, H.; Walschus, U.; Schlosser, M.; Zietz, C.; Staehlke, S.; Nebe, J. B.; Weltmann, K. D.; Meichsner, J.; Polak, M.

    2016-06-01

    The design of a titanium implant surface should ideally support its later application in clinical use. Temporarily used implants have to fulfil requirements different from permanent implants: they should ensure the mechanical stabilization of the bone stock but in trauma surgery they should not be integrated into the bone because they will be removed after fracture healing. Finishing of the implant surface by a plasma-fluorocarbon-polymer (PFP) coating is a possible approach for preventing cell adhesion of osteoblasts. Two different low pressure gas-discharge plasma processes, microwave (MW 2.45 GHz) and capacitively coupled radio frequency (RF 13.56 MHz) plasma, were applied for the deposition of the PFP film using a mixture of the precursor octafluoropropane (C3F8) and hydrogen (H2). The thin films were characterized by x-ray photoelectron spectroscopy, Fourier transform infrared reflection absorption spectroscopy, and water contact angle measurements. Cell culture experiments show that cell adhesion and spreading of MG-63 osteoblasts were clearly reduced or nonexistent on these surfaces, also after 24 h of storage in the cell culture medium. In vivo data demonstrated that the local inflammatory tissue response for the PFP films deposited in MW and RF plasma were comparable to uncoated controls.

  12. Development of a high speed cutting and pressure rolling technology for recycling of refrigerators with recovery of the fluorocarbon gas

    Energy Technology Data Exchange (ETDEWEB)

    Yotsumoto, M; Matsuda, Y. [Panasonic AVC Networks Co., (Japan)]|[Matsushita Electric Industrial Co. Ltd. (Japan)

    2004-07-01

    Refrigerators having reached end-of-life are a prime target for recycling because of their bulk and the relatively pristine condition of their components. This article reports on an innovative method of recycling these appliances. Conventional recycling relies on bulk crushing and then separation by magnetic, eddy current and possibly gravity methods. Separation of plastics by type is poor and the steel is often contaminated by copper. This innovative method replaces bulk crushing by high speed impact cutting, which cuts the metal-polymer-matrix composite material of the body into smaller parts (e.g. the walls, the door) of rectangular form. This is done by robots suitably controlled by sophisticated software which uses camera images as input, so that suitable pieces are precisely cut. High pressure rolling then liberates the cut plates of composite material into its constituent materials. The rolling process ruptures the polyurethane foam releasing the gas inside its unit cells. The gases traditionally used were fluorocarbons, but now flammable butane and cyclopentane is often used. The rolling system includes a gas recovery system to prevent escape of these environmentally sensitive substances. 5 refs., 2 tabs., 9 figs.

  13. New application of crystalline cellulose in rubber composites

    Science.gov (United States)

    Bai, Wen

    Rubber without reinforcement has limited applications. The strength of reinforced rubber composites can be ten times stronger than that of unreinforced rubbers. Therefore, rubber composites are widely used in various applications ranging from automobile tires to seals, valves, and gaskets because of their excellent mechanical elastic properties. Silica and carbon black are the two most commonly used reinforcing materials in rubber tires. They are derived from non-renewable materials and are expensive. Silica also contributes to a large amount of ash when used tires are disposed of by incineration. There is a need for a new reinforcing filler that is inexpensive, renewable and easily disposable. Cellulose is the most abundant natural polymer. Native cellulose includes crystalline regions and amorphous regions. Crystalline cellulose can be obtained by removing the amorphous regions with the acid hydrolysis of cellulose because the amorphous cellulose can be hydrolyzed faster than crystalline cellulose. We recently discovered that the partial replacement of silica with microcrystalline cellulose (MCC) provided numerous benefits: (1) low energy consumption for compounding, (2) good processability, (3) strong tensile properties, (4) good heat resistance, and (5) potential for good fuel efficiency in the application of rubber tires. Strong bonding between fillers and a rubber matrix is essential for imparting rubber composites with the desired properties for many specific applications. The bonding between hydrophilic MCC and the hydrophobic rubber matrix is weak and can be improved by addition of a coupling agent or surface modifications of MCC. In this study, MCC was surface-modified with acryloyl chloride or alkenyl ketene dimer (AnKD) to form acrylated MCC (A-MCC) and AnKD-modified MCC (AnKD-MCC). The surface modifications of MCC did not change the integrity and mechanical properties of MCC, but provided functional groups that were able to form covalent linkages with

  14. Super-hydrophobicity and oleophobicity of silicone rubber modified by CF{sub 4} radio frequency plasma

    Energy Technology Data Exchange (ETDEWEB)

    Gao Songhua, E-mail: gaosonghua2005@126.com [Functional Materials Laboratory, Department of Physics, Mechanical and Electrical Engineering, Sanming University, Sanming 365004 (China); Gao Lihua [Functional Materials Laboratory, Department of Physics, Mechanical and Electrical Engineering, Sanming University, Sanming 365004 (China); Zhou Kesheng [School of Physics Science and Technology, Central South University, Changsha 410083 (China)

    2011-03-15

    Owing to excellent electric properties, silicone rubber (SIR) has been widely employed in outdoor insulator. For further improving its hydrophobicity and service life, the SIR samples are treated by CF{sub 4} radio frequency (RF) capacitively coupled plasma. The hydrophobic and oleophobic properties are characterized by static contact angle method. The surface morphology of modified SIR is observed by atom force microscope (AFM). X-ray photoelectron spectroscopy (XPS) is used to test the variation of the functional groups on the SIR surface due to the treatment by CF{sub 4} plasma. The results indicate that the static contact angle of SIR surface is improved from 100.7 deg. to 150.2 deg. via the CF{sub 4} plasma modification, and the super-hydrophobic surface of modified SIR, which the corresponding static contact angle is 150.2 deg., appears at RF power of 200 W for a 5 min treatment time. It is found that the super-hydrophobic surface ascribes to the coaction of the increase of roughness created by the ablation action and the formation of [-SiF{sub x}(CH{sub 3}){sub 2-x}-O-]{sub n} (x = 1, 2) structure produced by F atoms replacement methyl groups reaction, more importantly, the formation of [-SiF{sub 2}-O-]{sub n} structure is the major factor for super-hydrophobic surface, and it is different from the previous studies, which proposed the fluorocarbon species such as C-F, C-F{sub 2}, C-F{sub 3}, CF-CF{sub n}, and C-CF{sub n}, were largely introduced to the polymer surface and responsible for the formation of low surface energy.

  15. Experimental study of temperature distribution in rubber material during microwave heating and vulcanization process

    Science.gov (United States)

    Chen, Hai-Long; Li, Tao; Liang, Yun; Sun, Bin; Li, Qing-Ling

    2017-03-01

    Microwave technology has been employed to heat sheet rubber, the optical fiber temperature online monitor and optical fiber temperature sensor have been employed to measure the temperature in sheet rubber. The temperature of sheet rubber increased with increase of heating time during microwave heating process in which the maximum of temperature was rubber was higher than the rate of temperature rising in marginal zone of sheet rubber, and the final temperature in central zone of sheet rubber was also higher than the final temperature in marginal zone of sheet rubber. In the microwave heating and vulcanization process of sheet rubber, the maximum of rate of temperature rising and the maximum of temperature belong to the central zone of sheet rubber, so the distribution of electric field was uneven in heating chamber, which led to the uneven temperature distribution of sheet rubber. The higher electric field intensity value converges on the central zone of sheet rubber.

  16. Natural rubber/nitrile butadiene rubber/hindered phenol composites with high-damping properties

    Directory of Open Access Journals (Sweden)

    Xiuying Zhao

    2015-10-01

    Full Text Available New natural rubber (NR/nitrile butadiene rubber (NBR/hindered phenol (AO-80 composites with high-damping properties were prepared in this study. The morphological, structural, and mechanical properties were characterized by atomic force microscopy (AFM, polarized Fourier transform infrared spectrometer (FTIR, dynamic mechanical thermal analyzer (DMTA, and a tensile tester. Each composite consisted of two phases: the NR phase and the NBR/AO-80 phase. There was partial compatibility between the NR phase and the NBR/AO-80 phase, and the NR/NBR/AO-80 (50/50/20 composite exhibited a co-continuous morphology. Strain-induced crystallization occurred in the NR phase at strains higher than 200%, and strain-induced orientation appeared in the NBR/AO-80 phase with the increase of strain from 100% to 500%. The composites had a special stress–strain behavior and mechanical properties because of the simultaneous strain-induced orientation and strain-induced crystallization. In the working temperature range of a seismic isolation bearing, the composites (especially the NR/NBR/AO-80 (50/50/20 composite presented a high loss factor, high area of loss peak (TA, and high hysteresis energy. Therefore, the NR/NBR/AO-80 rubber composites are expected to have important application as a high-performance damping material for rubber bearing.

  17. Penelitian penggunaan campuran karet alam RSS dengan stiren butadien rubber (SBR dalam pembuatan soft rubber lining

    Directory of Open Access Journals (Sweden)

    Penny Setyowati

    1995-06-01

    Full Text Available The objective of this research is to obtain optimum composition of RSS and SBR compound for making soft rubber lining compound. Based on seven combination of trials in compound formulation proved that formulation with composition of RSS 50 parts and SBR 50 parts give the best physical properties and highly cemented on steel by using “Desmodur R” adhesive solution.

  18. Creep Characteristics of Crumb Rubber Modified Asphalt Binder

    Institute of Scientific and Technical Information of China (English)

    WANG Lan; CHANG Chunqing; XING Yongming

    2011-01-01

    Crumb rubber modified asphalt containing 20 percent crumb rubber particles of 30mesh has been examined by Scanning Electron Microscope (SEM) to observe the microcosmic appearance and the characteristic distribution of crumb rubber particles in asphalt. The SEM pictures reveal that the crumb rubber particles distribute evenly in the asphalt and they are compatible well with asphalt. The shear creep test of crumb rubber modified asphalt was carried out at - 10 ℃ and 40 ℃ by Dynamic Shear Rheology (DSR). The shearing deformation at different temperature and creep stiffness modulus curve at loading stage of crumb rubber modified asphalt have been measured. The stiffness modulus of crumb rubber modified asphalt is much temperature sensitive and it decays much quick at the early stage of loading than normal asphalt. The rate of decay of stiffness modulus is slow at the subsequent stage and stiffness modulus approaches to a stable value at the final stage at a higher temperature. In addition, Burgers model is suitable to describe and simulate experimental results of viscoelastic properties of the crumb rubber modified asphalt.

  19. PHA-rubber blends: synthesis, characterization and biodegradation.

    Science.gov (United States)

    Bhatt, Rachana; Shah, Dishma; Patel, K C; Trivedi, Ujjval

    2008-07-01

    Medium chain length polyhydroxyalkanoates (mcl-PHA) and different rubbers; namely natural rubber, nitrile rubber and butadiene rubber were blended at room temperature using solution blending technique. Blends constituted 5%, 10% and 15% of mcl-PHA in different rubbers. Thermogravimetric analysis of mcl-PHA showed the melting temperature of the polymer around 50 degrees C. Thermal properties of the synthesized blend were studied by Differential Scanning Calorimetry which confirmed effective blending between the polymers. Blending of mcl-PHA with natural rubber led to the synthesis of a different polymer having the melting point of 90 degrees C. Degradation studies of the blends were carried out using a soil isolate, Pseudomonas sp. 202 for 30 days. Extracellular protein concentration as well as OD660 due to the growth of Pseudomonas sp. 202 was studied. The degradation of blended plastic material, as evidenced by % weight loss after degradation and increase in the growth of organism correlated with the amount of mcl-PHA present in the sample. Growth of Pseudomonas sp. 202 resulted in 14.63%, 16.12% and 3.84% weight loss of PHA:rubber blends (natural, nitrile and butadiene rubber). Scanning electron microscopic studies after 30 days of incubation further confirmed biodegradation of the films.

  20. Blends of guayule natural rubber latex with commercial latex polymers

    Science.gov (United States)

    Guayule (Parthenium argentatum) is a woody desert shrub that produces natural rubber, cis-1,4 polyisoprene, by biosynthesis. It is currently cultivated in the southwestern United States as a source of latex and rubber for commercial development. Guayule latex is similar to Hevea latex in polymer mo...

  1. A study of amino acid modifiers in guayule natural rubber

    Science.gov (United States)

    Natural rubber from the Hevea tree is a critical agricultural material vital to United States industry, medicine, and defense, yet the country is dependent on imports to meet domestic needs. Guayule, a desert shrub indigenous to the US, is under development as an alternative source of natural rubber...

  2. Flexible diamond-like carbon film coated on rubber

    NARCIS (Netherlands)

    Pei, Y.T.; Bui, X.L.; Pal, J.P. van der; Martinez-Martinez, D.; Hosson, J.Th.M. De

    2013-01-01

    Dynamic rubber seals are major sources of friction of lubrication systems and bearings, which may take up to 70% of the total friction. The solution we present is to coat rubbers with diamond-like carbon (DLC) thin films by which the coefficient of friction is reduced to less than one tenth. Coating

  3. Flexible protective diamond-like carbon film on rubber

    NARCIS (Netherlands)

    Pei, Y.T.; Bui, X.L.; Hosson, J.Th.M. De

    2010-01-01

    In this paper we report an experimental approach to deposit flexible diamond-like carbon (DLC) films on rubber via self-segmentation. By making use of the substantial thermal mismatch between the DLC film and rubber substrate a dense network of cracks forms in the DLC film, contributing to its flexi

  4. Research and Application Progress of Silicone Rubber Materials in Aviation

    Directory of Open Access Journals (Sweden)

    HUANG Yanhua

    2016-06-01

    Full Text Available The research progress of heat resistance, cold resistance, electrical conductivity and damping properties of aviation silicone rubber were reviewed in this article. The heat resistance properties of silicone rubber can be enhanced by changing the molecular structure (main chain, end-group, side chain and molecular weight of the gum and adding special heat-resistance filler. The cold resistance of aviation silicone rubber can be enhanced by adjusting the side chain molecular structure of the gum and the content of different gum chain. The electrical conductivity of silicone rubber can be improved by optimizing, blending and dispersing of conductive particles. The damping property of silicone rubber can be improved by designing and synthesizing of high-molecular polysiloxane damping agent. Furthermore, the application of aviation silicone rubber used in high-low temperature seal, electrical conduction and vibration damping technology are also summarized, and the high performance (for example long-term high temperature resistance, ultralow temperature resistance, high electromagnetic shelding, long-term fatigue resistance vibration damping, quasi constant modulus and so on of special silicone rubber is the future direction of aviation silicone rubber.

  5. Top 10 News of China Rubber Industry in 2011

    Institute of Scientific and Technical Information of China (English)

    2012-01-01

    1 Price of Rubber Raw Materials Greatly Fluctuated, Cost of Enterprises Hard to Be Controlled In 2011, the price of raw materials such as rubber fluctuated greatly. In the first quarter, NR hit the highest historical record of 43,500 yuan/ton.

  6. Influence of Plasma Treatments on the Frictional Performance of Rubbers

    NARCIS (Netherlands)

    Wolthuizen, D.J.; Martinez-Martinez, D.; Pei, Y.T.; Hosson, J.Th.M. De

    2012-01-01

    The frictional performance of several rubbers after pulsed-DC plasma treatments has been examined. In all cases, the treated rubbers showed better performance than the corresponding untreated ones. Stronger treatments, in terms of longer process time and/or higher substrate bias voltage, led to larg

  7. Viscoelastic properties of short aramid fibres-reinforced rubbers

    NARCIS (Netherlands)

    Sadatshirazi, S.; Talma, Auke; Noordermeer, Jacobus W.M.

    2013-01-01

    Among short fiber-reinforced composites, those with rubber matrices have gained great importance due to the advantages they have in processing and low cost, coupled with high strength. These composites combine the elastic behavior of rubbers with strength and stiffness of fibers. Reinforcement with

  8. Reinforcement of latex rubber by the incorporation of amphiphilic nanoparticles

    Science.gov (United States)

    Latex rubbers are fabricated from latex suspensions. During the fabrication process, latex particles are bound together while water is removed from the suspension. This report shows the mechanical properties of latex rubbers can be improved by incorporating a small amount of amphiphilic nanoparticle...

  9. An overview of the potentials of natural rubber (Hevea brasiliensis ...

    African Journals Online (AJOL)

    STORAGESEVER

    2009-12-29

    Dec 29, 2009 ... Rubber grows well in deciduous rain-forest regions of lowland tropics with temperature ranges of between 21. - 35°C and a well distributed .... In the bark of the rubber tree is a complex network of laticifers, or latex vessels, ... develop into embryo-like structures that go on to form plantlets. MULTIPLYING ...

  10. Guayule resin detection and influence on guayule rubber

    Science.gov (United States)

    Guayule (Parthenium argentatum) is a natural rubber (cis-1,4-polyisoprene) producing crop, native to North America. Guayule also produces organic resins, complex mixtures of terpenes, triglycerides, guayulins, triterpenoids and other components. During natural rubber extraction, guayule resins can b...

  11. Lifetime of metal rubber isolator with different vibration amplitudes

    Institute of Scientific and Technical Information of China (English)

    JIANG Hong-yuan; XIA Yu-hong; AO Hong-rui; DONG Chun-fang; A.M.Ulanov

    2005-01-01

    The lifetime of metal rubber isolator and its characteristics during lifetime experiment were studied. The stepped-up test principle was adopted to study the lifetime of resonant frequency, the breakage form of metal rubber isolator was obtained, and the relation between the energy dissipation, resonant frequency and stiffness was obtained in available lifetime of the isolator. Furthermore, the reason for the changes of properties of metal rubber isolator was analyzed with contact model of metal rubber material. The results show that if the resonant amplitude is large, the stiffness of metal rubber isolator will be kept steadily for a long time, its resonant frequency will be stable and the effective working time in the protecting area will be long. The lifetime of metal rubber isolator is more than 1 376 h in the experiment. The main failure forms of metal rubber isolator are accumulative wear and breaking of metal wires and spirals. In protecting area the metal rubber isolator can work effectively for a long time, and the effective working time depends on the concrete working condition.

  12. Viscoelastic properties of short aramid fibres-reinforced rubbers

    NARCIS (Netherlands)

    Shirazi, S.; Talma, A.G.; Noordermeer, J.W.M.

    2013-01-01

    Among short fiber-reinforced composites, those with rubber matrices have gained great importance due to the advantages they have in processing and low cost, coupled with high strength. These composites combine the elastic behavior of rubbers with strength and stiffness of fibers. Reinforcement with

  13. Cohesion in crumb rubber modified bitumen

    Directory of Open Access Journals (Sweden)

    Páez Dueñas, A.

    2006-12-01

    Full Text Available This article reports on a study of crumb rubber-mediated improvement in bitumen cohesion, analyzed with the UCL method. UCL, a procedure developed to characterize bituminous binders, evaluates the cohesion obtained by adding a certain amount of bitumen or bituminous mastic to a standard mix aggregate. This method was chosen because it can be used to assess bitumen containing crumb rubber added by either the wet or the dry mix process. In the dry mix process crumb rubber is combined with the mix as if it were a fine aggregate; i.e., crumb rubber and binder are blended during mix manufacture, laying and compaction. In the wet mix process, the binder is blended with the crumb rubber prior to mixing with the aggregate; i.e., when added to the mix, it has already been modified. The effect of digesting this dry mixed material prior to use was also analyzed in the present study. A comparison of the dry (with and without digestion and wet mix processes showed the latter to be more effective, particularly when the crumb rubber was blended with the binder via microscopic dispersion.El objetivo de este artículo es estudiar la influencia del polvo de neumático en la mejora de la cohesión proporcionada por la adición del polvo de neumático al betún mediante el método UCL. El método UCL es un procedimiento desarrollado para caracterizar ligantes bituminosos, basado en la evaluación de la cohesión dada por una cantidad determinada de un betún o un mástico bituminoso a unos áridos de granulometría establecida (mezcla patrón. Se ha empleado este método porque permite valorar al mismo tiempo los dos procedimientos de incorporación del polvo de neumático al betún: vía seca y vía húmeda.El procedimiento seco se lleva a cabo añadiendo el polvo de neumático a la mezcla como si fuera un filler, de modo que el polvo de neumático y el ligante se mezclan durante la fabricación, extendido y compactación de la mezcla. En el procedimiento h

  14. COMPRESSIVE AND SHEAR ANALYSIS OF RUBBER BLOCK UNDER LARGE STRAIN

    Directory of Open Access Journals (Sweden)

    K. Sridharan

    2013-01-01

    Full Text Available The Elastomeric materials have found use in a wide range of applications, including hoses, tires, gaskets, seals, vibration isolators, bearings and dock fenders. The analysis of rubber blocks for its compression and shear behavior has been carried out using the imaging techniques. The dynamic stressing and its associated change in shape of the rubber blocks during large compression are very limited as their measurements were difficult. A newly developed Machine Vision based image processing test has been effectively used to study the deformation characteristics of the rubber blocks under large strains. An extended analysis on the rubber blocks has been carried out to understand the compression and deformation behavior in static and dynamic condition and the nonlinear behavior were also characterized. The rubber blocks of distinguished geometries have shown diverse change in shape and nonlinear deformation behavior under compression/shear loading.

  15. Dynamic simulation on rubber spring supporting equipment of vibrating screen

    Institute of Scientific and Technical Information of China (English)

    SU Rong-hua; PENG Chen-yu

    2011-01-01

    By ANSYS, dynamic simulation analysis of rubber spring supporting equipment used in vibrating screen was made. The modal frequency, mode, and harmonic displacement under working frequency were obtained. Variation of rubber spring supporting equipment's dynamic performance was discussed first, which is under the condition of existing spring stiffness difference and exciting force bias. Also, the quantitative calculation formulas were given. The results indicate that the performance of vibrating screen is closely related with rubber spring supporting equipment's dynamic performance. Differences of springs' stiffness coefficients reduce the modal frequency reduced, decrease the dynamic stiffness, and increase vibration displacement. Exciting force bias induces a larger lateral displacement. When rubber springs' stiffness coefficients exist, differences and lateral force accounts for 5% in total exciting force; rubber spring supporting equipment's side swing is larger than 1 mm, exceeding the side swing limit.

  16. Analysis of impact of suspension rubber mounts on ride comfort

    Science.gov (United States)

    Chen, Bao; Chen, Zheming; Lei, Gang

    2017-01-01

    Two multi-body car models with rubber mounts and without rubber mounts have been built up to research how the suspension rubber mounts impact ride comfort. The comfort mount was used to simulate the impact process. Two scenarios have been set up, and time integrations have been performed to get the acceleration-time histories of seat surface in the x-, y-, and z-direction. A MATLAB program was compiled to calculate the weighted RMS acceleration. For the first scenario, the relative difference of weighted RMS acceleration between the car models with rubber mounts and without rubber mounts gradually decreases as the road roughness increases. For the second scenario, the relative difference increases as the driving speed increases. The conclusion shows that the change of driving speed or road roughness impacts ride comfort. Especially for high driving speed this impact is quite obvious.

  17. 3D silicone rubber interfaces for individually tailored implants.

    Science.gov (United States)

    Stieghorst, Jan; Bondarenkova, Alexandra; Burblies, Niklas; Behrens, Peter; Doll, Theodor

    2015-01-01

    For the fabrication of customized silicone rubber based implants, e.g. cochlear implants or electrocortical grid arrays, it is required to develop high speed curing systems, which vulcanize the silicone rubber before it runs due to a heating related viscosity drop. Therefore, we present an infrared radiation based cross-linking approach for the 3D-printing of silicone rubber bulk and carbon nanotube based silicone rubber electrode materials. Composite materials were cured in less than 120 s and material interfaces were evaluated with scanning electron microscopy. Furthermore, curing related changes in the mechanical and cell-biological behaviour were investigated with tensile and WST-1 cell biocompatibility tests. The infrared absorption properties of the silicone rubber materials were analysed with fourier transform infrared spectroscopy in transmission and attenuated total reflection mode. The heat flux was calculated by using the FTIR data, emissivity data from the infrared source manufacturer and the geometrical view factor of the system.

  18. New type of liquid rubber and compositions based on it.

    Science.gov (United States)

    Semikolenov, S V; Nartova, A V; Voronchikhin, V D; Dubkov, K A

    2014-11-01

    The new method for producing the functionalized polymers and oligomers containing carbonyl C=O groups is developed. The method is based on the noncatalytic oxidation of unsaturated rubbers by nitrous oxide (N2O) at 180-230 °С. The proposed method allows obtaining the new type of functionalized rubbers-liquid unsaturated polyketones with regulated molecular weight and concentration of C=O groups. The influence of the liquid polyketone addition on properties of rubber-based composites is investigated. The study indicates good prospects of using the liquid polyketones for the improvement of properties and operating characteristics of the various types of rubbers and the rubber-cord systems.

  19. Performance of the Cement Matrix Composite Material With Rubber Powder

    Institute of Scientific and Technical Information of China (English)

    SONG Shao-min; LIU Juan-hong; ZHANG Xi-qing

    2004-01-01

    The effect of the deferent rubber content substituted for fine aggregate on the mortar performancewas studied. The effects of the rubber coated with the coating materials on the mortar compressive strength, bendingstrength and impact work were discussed. The optimum rubber powder content and the suitable coating materialwere found. Through the electrical probe test- BEI, SEI and calcium ion distribution, and the slight crack and theinterface between the rubber and cement matrix are analyzed. The results show that the rubber powder coated withthe surface treatment materials A, B and C bas the capability of absorbing a large amount of energy under thecompressive and flexural load and the slight cracks of R- C were controlled and restrained.

  20. Reinforcement of rubber by fractal aggregates

    Science.gov (United States)

    Witten, T. A.; Rubinstein, M.; Colby, R. H.

    1993-03-01

    Rubber is commonly reinforced with colloidal aggregates of carbon or silica, whose structure has the scale invariance of a fractal object. Reinforced rubbers support large stresses, which often grow faster than linearly with the strain. We argue that under strong elongation the stress arises through lateral compression of the aggregates, driven by the large bulk modulus of the rubber. We derive a power-law relationship between stress and elongation λ when λgg 1. The predicted power p depends on the fractal dimension D and a second structural scaling exponent C. For diffusion-controlled aggregates this power p should lie beween 0.9 and 1.1 ; for reaction-controlled aggregates p should lie between 1.8 and 2.4. For uniaxial compression the analogous powers lie near 4. Practical rubbers filled with fractal aggregates should approach the conditions of validity for these scaling laws. On renforce souvent le caoutchouc avec des agrégats de carbone ou de silice dont la structure a l'invariance par dilatation d'un objet fractal. Les caoutchoucs ainsi renforcés supportent de grandes contraintes qui croissent souvent plus vite que l'élongation. Nous prétendons que, sous élongation forte, cette contrainte apparaît à cause d'une compression latérale des agrégats induite par le module volumique important du caoutchouc. Nous établissons une loi de puissance reliant la contrainte et l'élongation λ quand λgg 1. Cet exposant p dépend de la dimension fractale D et d'un deuxième exposant structural C. Pour des agrégats dont la cinétique de formation est limitée par diffusion, p vaut entre 0,9 et 1,1. Si la cinétique est limitée par le soudage local des particules, p vaut entre 1,8 et 2,4. Sous compression uniaxiale, les puissances homologues valent environ 4. Des caoutchoucs pratiques chargés de tels agrégats devraient approcher des conditions où ces lois d'échelle sont valables.

  1. On the inflation of a rubber balloon

    Science.gov (United States)

    Vandermarlière, Julien

    2016-12-01

    It is a well-known fact that it is difficult to start a balloon inflating. But after a pressure peak that occurs initially, it becomes far easier to do it! The purpose of this article is to establish the experimental pressure-radius chart for a rubber balloon and to compare it to the theoretical one. We will demonstrate that the barometer of a smartphone is a very suitable tool to reach this goal. We hope that this phenomenon will help students realize that sometimes very simple questions can lead to very interesting and counterintuitive science.

  2. Demotivating factors influencing rubber production workers

    Directory of Open Access Journals (Sweden)

    Mohammad Reza Iravani

    2012-01-01

    Full Text Available Motivation is one of the most important factors influencing workers' productivity. An increase in workers' motivation could add more value to organizations' structure and influence the profitability, significantly. In this paper, we study different factors on demotivating workers using questionnaire consist of various questions. The questionnaire is distributed among some employees who work for rubber production units located in Esfahan, Iran. The results of this survey indicate that discrimination on annual job compensation, entrusting responsibilities and unpleasant relationship with family partner are some of the most important factors influencing employees' motivation. While financial factors play important role on increasing employees' motivation, non-financial factors are considered more important.

  3. Characterization of Hexsyn, a polyolefin rubber.

    Science.gov (United States)

    McMillin, C R

    1987-07-01

    Hexsyn is the Goodyear Tire and Rubber Company tradename for a polyolefin rubber synthesized from 1-hexene with 3-5% methylhexadiene as the source of residual double bonds for vulcanization. Under license from Goodyear, this same polymer has been manufactured by Lord Corporation for the hinge portion of finger joint prostheses using the tradename Bion. This rubber is currently licensed to the University of Akron and to the Cleveland Clinic Foundation for use in biomedical applications, and is being used primarily for biocompatible and highly fatigue resistant rubber components in ventricular assist and artificial heart systems. Results are presented from the physical, mechanical, and biological characterization of Hexsyn. Procedures are described for the synthesis, compounding, and post-molding extraction for Hexsyn. The physical testing of Hexsyn reported includes determinations of its density at 23 and 37 degrees C, initial hardness and hardness after aging in oxygen, blood, pseudoextracellular fluid and polyethylene glycol 600, typical molecular weights determined by gel permeation chromatography/low angle laser light scattering and intrinsic viscosity, thermal analyses by differential scanning calorimetry of Hexsyn gum, and vulcanized Hexsyn after exposure to blood and blood/fatigue conditions. Also reported are results of differential thermal analyses, thermomechanical analyses of virgin and annealed samples, and thermogravimetric analyses conducted in helium and in air. Dynamic mechanical analyses of Hexsyn include Clash-Berg and Rheovibron tests. Swelling was conducted to determine lot-to-lot and sheet-to-sheet variation for quality control and also a number of solvents were used so that the polymer-solvent interaction parameters could be determined. The permeability of Hexsyn to water, water vapor, and a variety of gases is reported. The permeability by contact angle measurements, refractive index, residual solvent analyses, migration of blood components

  4. Properties of Concrete Containing Scrap-Tire Rubber

    Directory of Open Access Journals (Sweden)

    Mazyad Al-Fadhli

    2017-03-01

    Full Text Available Solid waste management is one of the major environmental concerns all over the world and in Kuwait. Over 5 billion tons of non-hazardous solid waste materials are generated in Kuwait each year. Of these, more than 2 million scrap-tires (approximately 2 million tons are generated each year. In addition to this, about seven million scrap-tires have been stockpiled. Due to the increasingly serious environmental problems presented by waste tires, the feasibility of using elastic and flexible tire–rubber particles as aggregate in concrete is investigated in this study. Tire–rubber particles composed of tire chips, crumb rubber, and a combination of tire chips and crumb rubber, were used to replace mineral aggregates in concrete. These particles were used to replace 10%, 15%, 20%, and 25% of the total mineral aggregate’s volume in concrete. Cylindrical shape concrete specimens 15 cm in diameter and 30 cm in height were fabricated and cured. The fresh rubberized concrete exhibited lower unit weight and acceptable workability compared to plain concrete. The results of a uniaxial compressive strain control test conducted on hardened concrete specimens indicate large reductions in the strength and tangential modulus of elasticity. A significant decrease in the brittle behavior of concrete with increasing rubber content is also demonstrated using nonlinearity indices. The maximum toughness index, indicating the post failure strength of concrete, occurs in concretes with 25% rubber content. Unlike plain concrete, the failure state in rubberized concrete occurs gently and uniformly, and does not cause any separation in the specimen. Crack width and its propagation velocity in rubberized concrete are lower than those of plain concrete. Ultrasonic analysis reveals large reductions in the ultrasonic modulus and high sound absorption for tire–rubber concrete.

  5. Statistical Discrimination of Latex between Healthy and White Root Infected Rubber Tree based on Dry Rubber Content

    Science.gov (United States)

    Suhaimi Sulaiman, Mohd; Hashim, Hadzli; Faiz Mohd Sampian, Ahmad; Korlina Madzhi, Nina; Faris Mohd Azmi, Azrie; Aishah Khairuzzaman, Noor; Aima Ismail, Faridatul

    2015-11-01

    Dry rubber content (DRC) is one of main material existing inside latex. It is usually in ranged of 25% - 45% of rubber latex. Statistical analysis are done to determine the discrimination of dry rubber content of latex between healthy and white root infected rubber tree. Based on 150 rubber trees and 10 clones tested, parametric test which include normality test, error-bar plot, and paired samples test are done. The result outcomes have shown that both data of dry rubber content of latex for healthy and white root infected rubber tree are normally distributed. Error-bar plot test is clearly indicated that there is visible discrimination between both cases. Paired samples test are done to reinforce this findings in terms of numerical p- value which is found to be less than 0.05. Thus, this indicate overwhelming evidence that healthy group can be discriminated from white root. Conclusively, changes in DRC content in latex can be correlated with white root disease infections of rubber tree.

  6. Reinforcing effect of plasma modified halloysite nanotubes in a carbon black filled natural rubber-butadien rubber matrix

    NARCIS (Netherlands)

    Poikelispaa, Minna; Das, Amit; Dierkes, Wilma; Vuorinen, Jyrki

    2011-01-01

    Rubber composites are generally produced by the direct incorporation of fillers like carbon black and/or silica into the rubber matrix. The incorporation of different types of nanofillers is the subject of recent research with the aim of preparing composites with special compositions and properties.

  7. Flexible diamond-like carbon films on rubber : Friction and the effect of viscoelastic deformation of rubber substrates

    NARCIS (Netherlands)

    Pei, Y. T.; Martinez-Martinez, D.; van der Pal, J. P.; Bui, X. L.; Zhou, X. B.; De Hosson, J. Th. M.

    2012-01-01

    This paper focuses on the frictional behavior of flexible diamond-like carbon (DLC) film-coated hydrogenated nitrile butadiene rubber. By making use of the substantial thermal mismatch between DLC film and rubber substrate, a dense network of cracks forms in the DLC films and contributes to flexibil

  8. Phase behavior of fluorocarbon and hydrocarbon double-chain hydroxylated and galactosylated amphiphiles and bolaamphiphiles. Long-term shelf-stability of their liposomes.

    Science.gov (United States)

    Clary, L; Gadras, C; Greiner, J; Rolland, J P; Santaella, C; Vierling, P; Gulik, A

    1999-06-01

    This paper describes the morphological characterization, by freeze-fracture electron microscopy, and the thermotropic phase behavior, by differential scanning calorimetry and/or X-ray scattering, of aqueous dispersions of various hydroxylated and galactosylated double-chain amphiphiles and bolaamphiphiles, several of them containing one or two hydrophobic fluorocarbon chains. Colloidal systems are observed in water with the hydroxylated hydrocarbon or fluorocarbon bolaamphiphiles only when they are dispersed with a co-amphiphile such as rac-1,2-dimyristoylphosphatidylcholine (DMPC) or rac-1,2-distearoylphosphatidylcholine (DSPC). Liposomes are formed providing the relative content of bolaamphiphiles does not exceed 20% mol. Most of these liposomes can be thermally sterilized and stored at room temperature for several months without any significant modification of their size and size distribution. The hydrocarbon galactosylated bolaamphiphile HO[C24][C12]Gal forms in water a lamellar phase (the gel to liquid-crystal phase transition is complete at 45 degrees C) and a Im3m cubic phase above 47 degrees C. The fluorocarbon HO[C24][F6C5]Gal analog displays a more complex and metastable phase behavior. The fluorinated non-bolaform galactosylated [F8C7][C16]AEGal and SerGal amphiphiles form lamellar phases in water. Low amounts (10% molar ratio) of the HO[C24][F6C5]Gal or HO[C24][C12]Gal bolaamphiphiles or of the single-headed [F8C7][C16]AEGal improve substantially the shelf-stability of reference phospholipon/cholesterol 2/1 liposomes. These liposomes when co-formulated with a single-headed amphiphile from the SerGal series are by far less stable.

  9. Rubber hand illusion affects joint angle perception.

    Directory of Open Access Journals (Sweden)

    Martin V Butz

    Full Text Available The Rubber Hand Illusion (RHI is a well-established experimental paradigm. It has been shown that the RHI can affect hand location estimates, arm and hand motion towards goals, the subjective visual appearance of the own hand, and the feeling of body ownership. Several studies also indicate that the peri-hand space is partially remapped around the rubber hand. Nonetheless, the question remains if and to what extent the RHI can affect the perception of other body parts. In this study we ask if the RHI can alter the perception of the elbow joint. Participants had to adjust an angular representation on a screen according to their proprioceptive perception of their own elbow joint angle. The results show that the RHI does indeed alter the elbow joint estimation, increasing the agreement with the position and orientation of the artificial hand. Thus, the results show that the brain does not only adjust the perception of the hand in body-relative space, but it also modifies the perception of other body parts. In conclusion, we propose that the brain continuously strives to maintain a consistent internal body image and that this image can be influenced by the available sensory information sources, which are mediated and mapped onto each other by means of a postural, kinematic body model.

  10. INDUSTRIAL SAFETY IN THE PRODUCTION OF RUBBER

    Directory of Open Access Journals (Sweden)

    S. V. Danilova

    2015-01-01

    Full Text Available Russian industry of synthetic rubber, is one of the most competitive and occupies a prominent place in the global petrochemical industry. However, the company production of synthetic rubber are among the most hazardous industrial facilities. The main operational risks are to fire and explosion hazards of raw materials used. Accidents in such establishments can damage not only the equipment, materials or buildings, but also cause serious environmental and economic consequences for the region. For the prevention of accidents, mitigation and elimination of losses, it is necessary to apply a set of measures aimed at the management and control of industrial safety. The legal basis of industrial safety in the Russian Federation is the Federal Law № 116-FZ dated 21.07.97 "On industrial safety of hazardous production facilities." Industrial Safety at work an important part of its normal functioning. The most important condition of industrial safety of hazardous production facilities is the examination of industrial safety. Federal rules and regulations in the field of industrial safety "rules of examination of industrial safety", approved by Order of RTN on November 14, 2013 N 538 established: the procedure of examination of industrial safety requirements for the design of expert opinions and requirements for experts.

  11. Pyrolysis of Rubber in a Screw Reactor

    Science.gov (United States)

    Lozhechnik, A. V.; Savchin, V. V.

    2016-11-01

    On the basis of an analysis of thermal methods described in the literature and from the results of experimental investigations of steam conversion, the authors have developed and created a facility for thermal processing of rubber waste. Rubber crumb was used as the raw material; the temperature in the reactor was 500°C; nitrogen, steam, and a mixture of light hydrocarbons (noncondensable part of pyrolysis products) represented the working medium. The pyrolysis yielded 36-38% of a solid fraction, 54-56% of a liquid hydrocarbon fraction, and 6-9% of noncondensable gases. Changes in the composition of the gas mixture have been determined at different stages of processing. Gas chromatography of pyrolysis gases has shown that the basic gases produced by pyrolysis are H2 and hydrocarbons C2H4, C3H6, C3H8, C4H8, C2H6, C3H6O2, and C4H10, and a small amount of H2S, CO, and CO2. Noncondensable gases will be used as a fuel to heat the reactor and to implement the process.

  12. Plant and bird diversity in rubber agroforests in the lowlands of Sumatra, Indonesia

    NARCIS (Netherlands)

    Beukema, Hendrien; Danielsen, Finn; Vincent, Gregoire; Hardiwinoto, Suryo; van Andel, Jelte

    Plant and bird diversity in the Indonesian jungle rubber agroforestry system was compared to that in primary forest and rubber plantations by integrating new and existing data from a lowland rain forest area in Sumatra. Jungle rubber gardens are low-input rubber (Hevea brasiliensis) agroforests that

  13. Plant and bird diversity in rubber agroforests in the lowlands of Sumatra, Indonesia

    NARCIS (Netherlands)

    Beukema, Hendrien; Danielsen, Finn; Vincent, Gregoire; Hardiwinoto, Suryo; van Andel, Jelte

    2007-01-01

    Plant and bird diversity in the Indonesian jungle rubber agroforestry system was compared to that in primary forest and rubber plantations by integrating new and existing data from a lowland rain forest area in Sumatra. Jungle rubber gardens are low-input rubber (Hevea brasiliensis) agroforests that

  14. 40 CFR 428.30 - Applicability; description of the solution crumb rubber subcategory.

    Science.gov (United States)

    2010-07-01

    ... solution crumb rubber subcategory. 428.30 Section 428.30 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY (CONTINUED) EFFLUENT GUIDELINES AND STANDARDS RUBBER MANUFACTURING POINT SOURCE CATEGORY Solution Crumb Rubber Subcategory § 428.30 Applicability; description of the solution crumb rubber...

  15. 75 FR 51981 - Polychloroprene Rubber from Japan: Final Results of Sunset Review and Revocation of Finding

    Science.gov (United States)

    2010-08-24

    ... International Trade Administration Polychloroprene Rubber from Japan: Final Results of Sunset Review and... review of the antidumping finding on polychloroprene rubber from Japan. Because the domestic interested... polychloroprene rubber from Japan. See Polychloroprene Rubber from Japan, 38 FR 33593 (December 6, 1973)....

  16. 40 CFR 428.40 - Applicability; description of the latex rubber subcategory.

    Science.gov (United States)

    2010-07-01

    ... latex rubber subcategory. 428.40 Section 428.40 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY (CONTINUED) EFFLUENT GUIDELINES AND STANDARDS RUBBER MANUFACTURING POINT SOURCE CATEGORY Latex Rubber Subcategory § 428.40 Applicability; description of the latex rubber subcategory. The provisions...

  17. 40 CFR 428.20 - Applicability; description of the emulsion crumb rubber subcategory.

    Science.gov (United States)

    2010-07-01

    ... emulsion crumb rubber subcategory. 428.20 Section 428.20 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY (CONTINUED) EFFLUENT GUIDELINES AND STANDARDS RUBBER MANUFACTURING POINT SOURCE CATEGORY Emulsion Crumb Rubber Subcategory § 428.20 Applicability; description of the emulsion crumb rubber...

  18. Fluorine-doped SiO{sub 2} and fluorocarbon low-k dielectrics investigated by SIMS

    Energy Technology Data Exchange (ETDEWEB)

    Cwil, M. [Tele and Radio Research Institute, Ratuszowa 11, 03-450 Warsaw (Poland)], E-mail: cwil@if.pw.edu.pl; Kalisz, M. [Faculty of Electronics and Information Technologies, Warsaw University of Technology, Koszykowa 75, 00-662 Warsaw (Poland); Konarski, P. [Tele and Radio Research Institute, Ratuszowa 11, 03-450 Warsaw (Poland)

    2008-12-15

    In this work, we present secondary ion mass spectrometry (SIMS) investigations of the incorporation of fluorine into thin SiO{sub 2} films adapted as low-k dielectrics in the metal-oxide-semiconductor (MOS) devices. The insulating SiOF oxides with the thickness ranging from 1 up to 15 nm have been prepared by plasma-enhanced chemical vapor deposition (PECVD) and/or by reactive ion etching (RIE) methods on <1 0 0> oriented p-Si substrates with the use of either CF{sub 4} or CHF{sub 3} source of the plasma. SIMS experiments were performed using ultra-low energy (1 keV) argon ion beam and quadrupole mass analyzer. Depth profiles of the resulting dielectric films illustrate: (i) the incorporation of F into the SiO{sub 2} matrix is accomplished by either the CHF{sub 3} or CF{sub 4} plasmas; (ii) no etching of SiO{sub 2} matrix is observed by using of CHF{sub 3}; (iii) CHF{sub 3} is a source of fluorocarbon film deposition on top of the SiO{sub 2} that prevents the SiO{sub 2} etching; and (iv) fluorine quantifications done based on implantation criteria give the maximum concentrations within the films from 6.0 x 10{sup 18} to 2.4 x 10{sup 20} atoms/cm{sup 3} depending on the different fluoridation conditions. The F concentration in SiO{sub 2} increases with the r.f. power of CF{sub 4} or with decreasing a gas pressure of CHF{sub 3} plasma.

  19. 氟碳表面活性剂环境风险控制措施初探%Environment risks control of fluorocarbon surfactants in foam extinguishing agents

    Institute of Scientific and Technical Information of China (English)

    朱江

    2012-01-01

    统计分析了山西省大中型石油化工企业数量以及2007-2011年全省油类火灾发生的时间、地点,由此估算出泡沫灭火剂储备量及含氟碳表面活性剂(主要是C8类氟碳表面活性剂)的用量.从中分析氟碳表面活性剂排入大气中、直接进入土壤、直接流入河流和通过下水道进入污水处理厂对环境造成的污染风险.介绍国际发达国家相关处理措施,提出我国消防领域解决控制氟碳表面活性剂的建议:一是大力开发和选用环境友好型泡沫灭火剂,把对环境的影响降至最低;二是积极应对,加强管理,妥善回收处理消防灭火剂使用后的残液;三是鼓励污水处理厂开发能降解氟碳表面活性剂的处理工艺,最终达到降低此类风险对人类的危害;四是提出研制新型泡沫灭火剂的思路.%In order to investigate the reserves of foam extinguishing agents and usage of fluorocarbon surfactants in fire fighting field of Shanxi Province, we made a statistics of the number of large and medium petrochemistry industries and the occurring time and sites of oil (ire during 2007 - 2011. And there existed environment risks for the fluorocarbon surfactants (especially C8). The control measures of fluorocarbon surfactants' pollution include utilize the green foam extinguishing agents without or with as few as C8 fluorocarbon surfactants such as perfluo-rooctane sulfonate (PFOS)and perfluorooctanoic acid (PFOA). collection of the used foam extinguishing agents, and development of the degradation techniques for them and new foam extinguishing agent.

  20. Influence of temperature changes on torsional rigidity and damping coefficient of rubber torsional vibration damper

    Directory of Open Access Journals (Sweden)

    Wojciech HOMIK

    2011-01-01

    Full Text Available The short explanation of usefulness of rubber torsional dampers in crankshaft in multi-cylinder engines is presented. The description of the construction and operation of rubber torsional damper is also included. In the rubber torsional damper, the damping is achieved as the effect of internal friction resulting from the deformation of the rubber material. This deformation appears while the internal rubber elasticity is overloaded. Both the physical and mechanical rubber properties depend on temperature change. In cooperation with rubber dampers manufacturer the experimental investigations are made in order to establish the influence of temperature change on torsional stiffness and damping.

  1. Enhancement of Adhesion between EPDM and Polyester Fabric by Using Natural Rubber Modified by Maleic Anhydride

    Directory of Open Access Journals (Sweden)

    A. A. El-Wakil

    2011-01-01

    Full Text Available This study presents a new method for improving adhesion between ethylene propylene diene monomer (EPDM rubber and polyester fabric. In this work, natural rubber was modified by maleic anhydride in order to improve the adhesion force between ethylene propylene diene monomer rubber and polyester fabric. The effect of thermal aging and ionizing radiation on the stability of the rubber mix as well as on the peel strength of the rubber-coated fabric was investigated. It was observed that the natural rubber modified by maleic anhydride improved the peel strength of the EPDM rubber-coated polyester fabric.

  2. Comparative studies on crosslinked and uncrosslinked natural rubber biodegradation by Pseudomonas sp.

    Science.gov (United States)

    Roy, Ram Vinod; Das, Mithu; Banerjee, Rintu; Bhowmick, Anil K

    2006-12-01

    A comparative study on biodegradation of di-cumyl peroxide (DCP) crosslinked and uncrosslinked natural rubber by Pseudomonas sp. was carried out. Decrease in organic carbon content along with the changes in tensile strength of the treated rubber, both DCP crosslinked and uncrosslinked natural rubber, indicated rubber hydrocarbon utilization by the Pseudomonas sp. A decrease in 60.88% MPa and 41.66% MPa was observed after five month's old treated uncrosslinked natural rubber and DCP crosslinked rubber, respectively. Biodegradation was more pronounced in natural uncrosslinked rubber, which was further confirmed by the formation of aldehydic compounds with decrease in CH2 stretching frequencies.

  3. Material and Flexural Properties of Fiber-reinforced Rubber Concrete

    Science.gov (United States)

    Helminger, Nicholas P.

    The purpose of this research is to determine the material properties of rubber concrete with the addition of fibers, and to determine optimal mixture dosages of rubber and fiber in concrete for structural applications. Fiber-reinforced concrete and rubberized concrete have been researched separately extensively, but this research intends to combine both rubber and fiber in a concrete matrix in order to create a composite material, fiber-reinforced rubber concrete (FRRC). Sustainability has long been important in engineering design, but much of the previous research performed on sustainable concrete does not result in a material that can be used for practical purposes. While still achieving a material that can be used for structural applications, economical considerations were given when choosing the proportions and types of constituents in the concrete mix. Concrete mixtures were designed, placed, and tested in accordance with common procedures and standards, with an emphasis on practicality. Properties that were investigated include compressive strength, tensile strength, modulus of elasticity, toughness, and ductility. The basis for determining the optimal concrete mixture is one that is economical, practical, and exhibits ductile properties with a significant strength. Results show that increasing percentages of rubber tend to decrease workability, unit weight, compressive strength, split tensile strength, and modulus of elasticity while the toughness is increased. The addition of steel needle fibers to rubber concrete increases unit weight, compressive strength, split tensile strength, modulus of elasticity, toughness, and ductility of the composite material.

  4. Mechanical properties and durability of crumb rubber concrete

    Science.gov (United States)

    Chylík, Roman; Trtík, Tomáš; Fládr, Josef; Bílý, Petr

    2017-09-01

    This paper is focused on concrete with admixture of rubber powder, generally called crumb rubber concrete (CRC). The inspiration was found in Arizona, where one of the first CRCs has been created. However, Arizona has completely different climates than Central Europe. Could we use the crumb rubber concrete on construction applications in the Central European climate too? The paper evaluates the influence of the rubber powder on material characteristics and durability of CRC. CRCs with various contents of fine and coarse crumb powder were compared. The tested parameters were slump, air content, permeability, resistance of concrete to water with deicing chemicals, compressive and splitting tensile strength. The tests showed that workability, compressive strength and permeability decreased as the amount of rubber increased, but the air content increased as the rubber content increased. Photos of air voids in cement matrix from electron microscope were captured. The results of laboratory tests showed that admixture of rubber powder in concrete could have a positive impact on durability of concrete and concurrently contribute to sustainable development. Considering the lower compressive strength, CRC is recommended for use in applications where the high strength of concrete is not required.

  5. Characterization of associated proteins and phospholipids in natural rubber latex.

    Science.gov (United States)

    Sansatsadeekul, Jitlada; Sakdapipanich, Jitladda; Rojruthai, Porntip

    2011-06-01

    Non-rubber components present in natural rubber (NR) latex, such as proteins and phospholipids, are presumed to be distributed in the serum fraction as well as surrounding the rubber particle surface. The phospholipid-protein layers covering the rubber particle surface are especially interesting due to their ability to enhance the colloidal stability of NR latex. In this study, we have characterized the components surrounding the NR particle surface and investigated their role in the colloidal stability of NR particles. Proteins from the cream fraction were proteolytically removed from the NR latex and compare to those from the serum fractions using SDS-polyacrylamide gel electrophoresis revealing that both fractions contained similar proteins in certain molecular weights such as 14.5, 25 and 27 kDa. Phospholipids removed from latex by treatment with NaOH were analyzed using (1)H-NMR spectroscopy and several major signals were assignable to -(CH(2))(n)-, -CH(2)OP, -CH(2)OC═O and -OCH(2)CH(2)NH-. These signals are important evidence that indicates phospholipids associate with the rubber chain. The colloidal behavior of rubber lattices before and after removal of protein-lipid membrane was evaluated by zeta potential analysis and scanning electron microscope (SEM). The lowest zeta potential value of NR particles was observed at pH 10, consequently leading to the highest stability of rubber particles. Additionally, SEM micrographs clearly displayed a gray ring near the particle surface corresponding to the protein-lipid membrane layer.

  6. Microcellular foaming of silicone rubber with supercritical carbon dioxide

    Energy Technology Data Exchange (ETDEWEB)

    Hong, In-Kwon; Lee, Sangmook [Dankook University, Youngin (Korea, Republic of)

    2014-01-15

    In spite of great concern on the industrial application of microcellular silicone rubber foams, such as in electric and medical devices, only a few works can be found about the foaming of silicone rubber. In this study, microcellular silicone rubber foams with a cell size of 12 µm were successfully prepared with curing by heat and foaming by supercritical CO{sub 2} as a green blowing agent. The microcellular silicone rubber foams exhibited a well-defined cell structure and a uniform cell size distribution. The crosslinking and foaming of silicone rubber was carried out separately. After foaming, the silicone rubber foam was cross-linked again to stabilize the foam structure and further improve its mechanical properties. Foaming process of cross-linked silicone rubber should be designed carefully based on the viscoelastic properties because of its elastic volume recovery in the atmosphere. The basic crosslinking condition for small cell size and high cell density was obtained after investigating the rheological behavior during crosslinking.

  7. Volume Changes in Filled Rubber Under Uniaxial Cyclic Loading

    Directory of Open Access Journals (Sweden)

    Elina KAZINA

    2011-09-01

    Full Text Available Styrene-butadiene rubber, neat and filled with different silica content was investigated under uniaxial cyclic loading under a constant crosshead speed, with increasing deformation amplitude in subsequent loading cycles. Rubber was investigated in order to evaluate the reversibility of structure rearrangements, occurring in rubber when subjected to cyclic loading. Volume uniformly increases with growing strain and shows hysteresis at unloading. After complete unloading, no residual strain changes are observed. These data are in good conformity with the data of density measurements, which were made on specimens before and after the tests. By correlating data, obtained from volume changes and kinetics of hysteresis losses there were made assumptions on deformation mechanisms at different elongations. Deformational mechanisms, responsible for volume changes in rubber are reversible. Volume changes in specimen occur due to voids formation caused by filler microstructure breakage, rubber chains disentanglement, spaces between rubber macromolecular chains shrinkage, and chain slippage under higher elongations. Voids formation and deformation of rubber macromolecular chain reaches equilibrium state after certain elongation.http://dx.doi.org/10.5755/j01.ms.17.3.592

  8. The Abrasion-resistance Investigation of Rubberized Concrete

    Institute of Scientific and Technical Information of China (English)

    KANG Jingfu; ZHANG Bo; LI Guangyu

    2012-01-01

    The abrasion resistance properties of rubberized concrete were comparatively studied by taking silica fume and crumb tire rubber as the additives.The abrasion tests were conducted in accordance with the Chinese standard test method DL/T 5150-2001,two recommended test methods:under water method and ring method,were used.The crumb tire rubbers with the sieve size of 8-mesh and 16-mesh were incorporated into the concrete by replacing same volume of sand and as an additive.The abrasion resistance of concrete was evaluated according to the abrasion resistance strength and the mass loss.Test results show that the addition of silica fume enhanced both compressive strength and abrasion resistance of concrete,and the addition of crumb rubber reduced the compressive strength but increased notably the abrasion resistance of the concrete.Silica fume concrete performed a better abrasion resistance than control concrete,and the rubberized concrete performed a much better abrasion resistance than silica fume concrete.The abrasion resistance of rubberized concrete increased with the increase of rubber content.

  9. Circuit racing, track texture, temperature and rubber friction

    Science.gov (United States)

    Sharp, R. S.; Gruber, P.; Fina, E.

    2016-04-01

    Some general observations relating to tyre shear forces and road surfaces are followed by more specific considerations from circuit racing. The discussion then focuses on the mechanics of rubber friction. The classical experiments of Grosch are outlined and the interpretations that can be put on them are discussed. The interpretations involve rubber viscoelasticity, so that the vibration properties of rubber need to be considered. Adhesion and deformation mechanisms for energy dissipation at the interface between rubber and road and in the rubber itself are highlighted. The enquiry is concentrated on energy loss by deformation or hysteresis subsequently. Persson's deformation theory is outlined and the material properties necessary to apply the theory to Grosch's experiments are discussed. Predictions of the friction coefficient relating to one particular rubber compound and a rough surface are made using the theory and these are compared with the appropriate results from Grosch. Predictions from Persson's theory of the influence of nominal contact pressure on the friction coefficient are also examined. The extent of the agreement between theory and experiment is discussed. It is concluded that there is value in the theory but that it is far from complete. There is considerable scope for further research on the mechanics of rubber friction.

  10. Improving rubber concrete by waste organic sulfur compounds.

    Science.gov (United States)

    Chou, Liang-Hisng; Lin, Chun-Nan; Lu, Chun-Ku; Lee, Cheng-Haw; Lee, Maw-Tien

    2010-01-01

    In this study, the use of crumb tyres as additives to concrete was investigated. For some time, researchers have been studying the physical properties of concrete to determine why the inclusion of rubber particles causes the concrete to degrade. Several methods have been developed to improve the bonding between rubber particles and cement hydration products (C-S-H) with the hope of creating a product with an improvement in mechanical strength. In this study, the crumb tyres were treated with waste organic sulfur compounds from a petroleum refining factory in order to modify their surface properties. Organic sulfur compounds with amphiphilic properties can enhance the hydrophilic properties of the rubber and increase the intermolecular interaction forces between rubber and C-S-H. In the present study, a colloid probe of C-S-H was prepared to measure these intermolecular interaction forces by utilizing an atomic force microscope. Experimental results showed that rubber particles treated with waste organic sulfur compounds became more hydrophilic. In addition, the intermolecular interaction forces increased with the adsorption of waste organic sulfur compounds on the surface of the rubber particles. The compressive, tensile and flexural strengths of concrete samples that included rubber particles treated with organic sulfur compound also increased significantly.

  11. Experimental Investigation of the Mechanical and Durability Properties of Crumb Rubber Concrete

    OpenAIRE

    Hanbing Liu; Xianqiang Wang; Yubo Jiao; Tao Sha

    2016-01-01

    Recycling waste tire rubber by incorporating it into concrete has become the preferred solution to dispose of waste tires. In this study, the effect of the volume content of crumb rubber and pretreatment methods on the performances of concrete was evaluated. Firstly, the fine aggregate and mixture were partly replaced by crumb rubber to produce crumb rubber concrete. Secondly, the mechanical and durability properties of crumb rubber concrete with different replacement forms and volume content...

  12. Experimental Investigation into Mechanical Properties of Nanomaterial-reinforced Table Tennis Rubber

    Directory of Open Access Journals (Sweden)

    Yu-Fen Chen

    2016-10-01

    Full Text Available A new table tennis rubber is prepared consisting of carbon nanotubes, zinc oxide and titanium oxide added to a mixture of natural and synthesized rubber. The Nano-reinforced rubber is attached to wooden table tennis blades and patterned with four different surface structures, namely flat, long pimples, short pimples and medium pimples. The results show that of the five rubbers, the Nano-reinforced rubber with a flat surface offers a significantly improved elastic and mechanical performance

  13. Interplanting banana at high densities with immature rubber crop for improved water use

    OpenAIRE

    Harischandra Lakshman Rodrigo, Vitharanage; Maeve Stirling, Clare; Teklehaimanot, Zewge; Kusum Samarasekera, Renuka; Dharmasiri Pathirana, Pathiranage

    2005-01-01

    International audience; Consumptive water use of the rubber/banana intercropping systems was assessed. Five systems were tested; sole rubber (R) and banana (B) crops and three intercrops comprising additive series of one (BR), two (BBR) and three (BBBR) rows banana to one row of rubber. Planting density of rubber remained constant across the treatments, hence the rate of transpiration associated closely with the planting density of banana with ca. 140% increase from banana-rubber to banana-ba...

  14. Experimental Investigation of the Mechanical and Durability Properties of Crumb Rubber Concrete

    OpenAIRE

    Hanbing Liu; Xianqiang Wang; Yubo Jiao; Tao Sha

    2016-01-01

    Recycling waste tire rubber by incorporating it into concrete has become the preferred solution to dispose of waste tires. In this study, the effect of the volume content of crumb rubber and pretreatment methods on the performances of concrete was evaluated. Firstly, the fine aggregate and mixture were partly replaced by crumb rubber to produce crumb rubber concrete. Secondly, the mechanical and durability properties of crumb rubber concrete with different replacement forms and volume content...

  15. Model fire tests on polyphosphazene rubber and polyvinyl chloride (PVC)/nitrile rubber foams

    Science.gov (United States)

    Widenor, W. M.

    1978-01-01

    A video tape record of model room fire tests was shown, comparing polyphosphazene (P-N) rubber and polyvinyl chloride (PVC)/nitrile rubber closed-cell foams as interior finish thermal insulation under conditions directly translatable to an actual fire situation. Flashover did not occur with the P-N foam and only moderate amounts of low density smoke were formed, whereas with the PVC/nitrile foam, flashover occurred quickly and large volumes of high density smoke were emitted. The P-N foam was produced in a pilot plant under carefully controlled conditions. The PVC/nitrile foam was a commercial product. A major phase of the overall program involved fire tests on P-N open-cell foam cushioning.

  16. Effect of gamma irradiation on the properties of natural rubber/styrene butadiene rubber blends

    Directory of Open Access Journals (Sweden)

    A.B. Moustafa

    2016-09-01

    Full Text Available Blends of natural rubber (NR with styrene butadiene rubber (SBR with varying ratios have been prepared. Vulcanization of the prepared blends has been induced by irradiation of gamma rays with varying doses up to 250 kGy. Mechanical properties, namely tensile strength, tensile modulus at 100% elongation, elongation at break have been followed up as a function of irradiation dose as well as blend composition. Physical properties, namely gel fraction and swelling number have been followed up using benzene as a solvent. Thermal measurements namely thermogravimetric analysis were carried out. The results indicated that the addition of NR has improved the properties of NR / SBR blends. Also NR/SBR blend is thermally stable than NR alone.

  17. Functionalization of Liquid Natural Rubber via Oxidative Degradation of Natural Rubber

    Directory of Open Access Journals (Sweden)

    Suhawati Ibrahim

    2014-12-01

    Full Text Available Natural rubber (NR is a high molecular weight natural polymer and can be degraded to liquid natural rubber (LNR leaving certain functional groups at the end of chains. In this study, LNR samples prepared via oxidative degradation using H2O2 and NaNO2 as reagents were found to have different end groups depending on the pH of the reaction medium. In an acidic medium, LNR with hydroxyl terminal groups was formed as the degradation reaction was initiated by hydroxyl radicals produced from decomposition of peroxynitrite acid. In contrast, a redox reaction took place in an alkaline medium to yield LNR with carbonyl terminal groups. The mechanisms of reaction are discussed and proposed to explain the formation of different end groups when reaction carried out in acidic and alkaline media. Chain degradation in an acidic medium seems to be more effective than in an alkaline medium, and thus yields LNR with lower Mn.

  18. Radiation crosslinking of styrene-butadiene rubber containing waste tire rubber and polyfunctional monomers

    Science.gov (United States)

    Yasin, Tariq; Khan, Sara; Shafiq, Muhammad; Gill, Rohama

    2015-01-01

    The objective of this study was to investigate the influence of polyfunctional monomers (PFMs) and absorbed dose on the final characteristics of styrene-butadiene rubber (SBR) mixed with waste tire rubber (WTR). A series of SBR/WTR blends were prepared by varying the ratios of WTR in the presence of PFMs, namely trimethylolpropane trimethacrylate (TMPTMA) and trimethylolpropane triacrylate (TMPTA) and crosslinked using gamma rays. The physicochemical characteristics of the prepared blends were investigated. It was observed that tensile strength, hardness and gel content of the blends increased with absorbed dose while the blends containing TMPTA showed higher tensile strength, gel content and thermal stability as compared to the blends containing TMPTMA. Higher thermal stability was observed in the blends which were crosslinked by radiation as compared to the blends crosslinked by sulfur. These blends exhibited higher rate of swelling in organic solvents, whereas negligible swelling was observed in acidic and basic environment.

  19. The cross linking of EPDM and NBR rubber

    Directory of Open Access Journals (Sweden)

    Samardžija-Jovanović Suzana

    2005-01-01

    Full Text Available In the process of macromolecule cross linking, the choice of type and quantity of the components and the experimental conditions are important to obtain the new cross linked materials with better mechanical and chemical characteristics. The cross linking method depends on the rubber type and structure. Intermolecular cross linking results in the formation elastomer network. The basis of the cross linking process, between ethylene propylene diene rubber (EPDM and acrylonitrile butadiene rubber (NBR, is a chemical reaction. Fillers and other additives are present in different mass ratios in the material. The exploitation properties of the cross linked materials depend on the quantity of additive in the cross linked systems.

  20. Development of a Method to Fingerprint Rubber Fuel Hose Materials

    Science.gov (United States)

    1990-10-01

    ASTM Method D297 . The EPA method was chosen because it is commonly performed in 89293.01F:RWT Page 1-7 these laboratories and is of a larger scale...5746, March, 1987. 3 Method for Rubber Products - Chemical Analysis, Annual Book of ASTM Standards, ASTM D297 -81, v. 09.01, 1984. 4 Method for Rubber...composition and materials of construction. 2. Applicable Documents 2.1 ASTM Standards D297 - Rubber Products - Chemical Analysis, Sec 16-18 D3421

  1. Short Fibre and Particulate-reinforced Rubber Composites

    Directory of Open Access Journals (Sweden)

    Kavita Agarwal

    2002-07-01

    Full Text Available Particulate fillers (carbon black and silica and short fibre (aromatic polyamide, Kevlar have been utilised to produce rubber composites based on acrylonitrile-co-butadiene rubber (NBR. Mechanical properties of these composites have been determined and compared with unfilled rubber vulcanisate. The effect of surface treatment on the improvement of strength, in case of Kevlar, has also been considered. The influence of elevated temperature on tear strength, an important failure criterion, has been evaluated. Scanning electron microscopy has been used as a tool to correlate the topographical features associated with changes in the tear strength of the composites.

  2. Shear Flow Induced Alignment of Carbon Nanotubes in Natural Rubber

    Directory of Open Access Journals (Sweden)

    Yan He

    2015-01-01

    Full Text Available A new procedure for the fabrication of natural rubber composite with aligned carbon nanotubes is provided in this study. The two-step approach is based on (i the preparation of mixture latex of natural rubber, multiwalled carbon nanotubes, and other components and (ii the orientation of carbon nanotubes by a flow field. Rubber composite sheets filled with variable volume fraction of aligned carbon nanotubes were fabricated and then confirmed by transmission electron microscopy and Raman spectroscopy studies. An obvious increase in thermal conductivity has been obtained after the alignment of carbon nanotubes. The dynamic mechanical analysis was carried out in a tear mode for the composite.

  3. SUPPLY-CHAIN OF NATURAL RUBBER IN INDONESIA

    Directory of Open Access Journals (Sweden)

    Bustanul Arifin

    2011-08-01

    Full Text Available Normal 0 false false false MicrosoftInternetExplorer4 st1\\:*{behavior:url(#ieooui } /* Style Definitions */ table.MsoNormalTable {mso-style-name:"Table Normal"; mso-tstyle-rowband-size:0; mso-tstyle-colband-size:0; mso-style-noshow:yes; mso-style-parent:""; mso-padding-alt:0cm 5.4pt 0cm 5.4pt; mso-para-margin:0cm; mso-para-margin-bottom:.0001pt; mso-pagination:widow-orphan; font-size:10.0pt; font-family:"Times New Roman"; mso-ansi-language:#0400; mso-fareast-language:#0400; mso-bidi-language:#0400;} The study examines the supply chain of natural rubber production in Indonesia and assessing the transmission of prices to rubber growers and provides recommendations for a suitable scheme that would help to ensure high production standards and a sustainable return for natural rubber production.  The frameworks to examine the performance of supply chain of rubber marketing rely mostly on the efficiency level of marketing system of natural rubbers, including the value chain principles in marketing margin, and revealed price transmission from consumers to growers. The results show that the roles of subdistrict middlemen are extremely crucial in moving up the slabs from the village level to urban areas, where trader-brokers are expecting the slabs to be forwarded directly to crumb-rubber factories.  Changes in world price, hence the profits being accumulated by traders and rubber factories, are not transmitted properly to rubber farmers and/or sharetappers. Information asymmetry, the access over price information, and immediate response of rubber growers to the change in world price could explain this non-cointegration in price data between growers and exporters.  In the near future, the policy reforms in supply chain of natural rubber marketing in Indonesia should carefully address these issues in a more comprehensive manner.  Finally, in order to contribute to the positive environmental and social benefits, the major challenge for natural rubber

  4. Thermal and mechanical behavior of rubber systems

    Science.gov (United States)

    Macon, David James

    The study of the physical behavior of rubbery materials is motivated by the desire to use these materials in a variety of environments, different mechanical conditions, and at different temperatures. For this to be possible, accurate testing conditions and modeling schemes need to be devised. These tests can be difficult to perform and existing mathematical models often neglect several basic physical requirements. One model is the statistical thermodynamic approach for calculating the thermoelastic behavior of an ideal rubber network, which assumes affine deformation of crosslinked junctions and no internal energy change with isothermal deformation. Yet, when the same relations have been manipulated according to the laws of thermodynamics, an internal energy contribution is revealed. This result is an artifact of improperly referencing strain measures and elasticity coefficients with regard to temperature. When a proper strain reference state is selected, thermoelastic stress-strain-temperature relations result that are totally entropic yet reduce to the usual isothermal conditions. This work proposes a phenomenological model that accurately models existing thermoelastic data. Experimental methods to determine the entropic and energetic contributions to rubber elasticity usually focus on the force-temperature behavior of a uniaxial sample held at constant length. Ideally, these thermoelastic measurements would be made at constant volume. Measurements are made at constant pressure and require complex corrections. It is demonstrated that two dimensionally constrained membrane samples can overcome these difficulties. By using time-average vibrational holographic interferometry, the two principal stresses of a membrane in anisotropic biaxial extension can be directly determined as a function of temperature. This two dimensionally constrained stress-temperature response greatly simplifies the resulting mathematical relations and yields no difference between constant

  5. The role of pressure in rubber elasticity

    Science.gov (United States)

    Bower, A. F.; Weiner, J. H.

    2004-06-01

    We describe a series of molecular dynamics computations that reveal an intimate connection at the atomic scale between difference stress (which resists stretches) and pressure (which resists volume changes) in an idealized elastomer, in contrast to the classical theory of rubber elasticity. Our simulations idealize the elastomer as a "pearl necklace," in which the covalent bonds are stiff linear springs, while nonbonded atoms interact through a Lennard-Jones potential with energy εLJ and radius σLJ. We calculate the difference stress t11-(t22+t33)/2 and mean stress (t11+t22+t33)/3 induced by a constant volume extension in the x1 direction, as a function of temperature T and reduced density ρ*=NσIJ3/ν. Here, N is the number of atoms in the simulation cell and ν is the cell volume. Results show that for ρ*rubber elasticity, which neglects nonbonded interactions. However, data presented by van Krevelen [Properties of Polymers, 3rd ed. (Elsevier, Amsterdam, 1990), p. 79] indicate that rubber at standard conditions corresponds to ρ*=1.2. For ρ*>1, the system is entropic for kT/εLJ>2, but at lower temperatures the difference stress contains an additional energy component, which increases as ρ* increases and temperature decreases. Finally, the model exhibits a glass transition for ρ*=1.2 and kT/εLJ≈2. The atomic-scale processes responsible for generating stress are explored in detail. Simulations demonstrate that the repulsive portion of the Lennard-Jones potential provides a contribution σnbr>0 to the difference stress, the attractive portion provides σnba≈0, while the covalent bonds provide σb0, and Πb, σb=BΠb, where is a measure of the anisotropy of the orientation of the covalent bonds, and A and B are coefficients that depend weakly on ρ* and temperature. For high values of ρ*, we find that |σnbr|≫|σb|, and in this regime our model predicts behavior that is in good agreement with experimental data of D.L. Quested et al. [J. Appl. Phys. 52

  6. Self-healing properties of carbon nanotube filled natural rubber/bromobutyl rubber blends

    Directory of Open Access Journals (Sweden)

    H. H. Le

    2017-03-01

    Full Text Available In the present work, the development and characterization of an intrinsically self-healable material based on butyl imidazole modified bromobutyl rubber (BIIR/natural rubber (NR blends, which are filled with carbon nanotubes (CNTs are reported. It was found that the addition of CNTs and the blending with NR significantly enhance the tensile strength of the BIIR composites. The use of butyl imidazole as physical cross-linker for the BIIR phase provides the blend composites the non-covalent bondings, which are responsible for their self-healing properties. Owing to the increase of the viscosity of the BIIR phase upon its physical crosslinking the island-matrix morphology of the blend changes over to a co-continuous structure. The preferential wetting of the CNT surface by the low-loading NR phase in the NR/BIIR blends can be explained by the good rubber-filler interaction between the linked phospholipids of the NR molecules and the π-electrons of the CNT surface. As a result, the favored localization of the CNTs in the NR phase strongly improves the electrical properties of the blends according to the double percolation theory. On the other hand it does not deteriorate the self-healing of the BIIR phase. The high electrical conductivity provides us a possibility to heat the blend by application of an electrical voltage in order to accelerate the self-healing process.

  7. Interfacial interaction between the epoxidized natural rubber and silica in natural rubber/silica composites

    Energy Technology Data Exchange (ETDEWEB)

    Xu, Tiwen [College of Materials Science and Engineering, South China University of Technology, Guangzhou 510640 (China); Jia, Zhixin, E-mail: zxjia@scut.edu.cn [College of Materials Science and Engineering, South China University of Technology, Guangzhou 510640 (China); Luo, Yuanfang; Jia, Demin [College of Materials Science and Engineering, South China University of Technology, Guangzhou 510640 (China); Peng, Zheng [Agricultural Product Processing Research Institute, Chinese Academy of Tropical Agriculture Sciences, Zhanjiang 524001 (China)

    2015-02-15

    Highlights: • Substantiate the ring open reaction between Si-OH of silica and epoxy groups of ENR. • ENR can act as a bridge between NR and silica to enhance the interfacial interaction. • As a modifier, ENR gets the potential to be used in the tread of green tire for improving the wet skid resistance apparently. - Abstract: The epoxidized natural rubber (ENR) as an interfacial modifier was used to improve the mechanical and dynamical mechanical properties of NR/silica composites. In order to reveal the interaction mechanism between ENR and silica, the ENR/Silica model compound was prepared by using an open mill and the interfacial interaction of ENR with silica was investigated by Fourier transform infrared spectroscopy (FTIR), X-ray photoelectron spectroscopy (XPS), transmission electron microscopy (TEM), X-ray diffraction (XRD) and stress–strain testing. The results indicated that the ring-opening reaction occurs between the epoxy groups of ENR chains and Si-OH groups on the silica surfaces and the covalent bonds are formed between two phases, which can improve the dispersion of silica in the rubber matrix and enhance the interfacial combination between rubber and silica. The ring-opening reaction occurs not only in vulcanization process but also in mixing process, meanwhile, the latter seems to be more important due to the simultaneous effects of mechanical force and temperature.

  8. Unraveling the mystery of natural rubber biosythesis part I: investigation of the composition and growth of in vitro natural rubber using high resolution size exclusion chromatography

    Science.gov (United States)

    Monitoring the growth of in vitro natural rubberwas accomplished by high resolution size exclusion chromatography, SEC.Washed rubber particles isolated from H. brasiliensis latex, containing the rubber transferase enzyme, were used to catalyze the polymerization of synthetic isopentenyl pyrophosphat...

  9. Allergenic proteins of natural rubber latex.

    Science.gov (United States)

    Yeang, H Y; Arif, Siti Arija M; Yusof, Faridah; Sunderasan, E

    2002-05-01

    As the living cytoplasm of laticiferous cells, Hevea brasiliensis latex is a rich blend of organic substances that include a mélange of proteins. A small number of these proteins have given rise to the problem of latex allergy. The salient characteristics of H. brasiliensis latex allergens that are recognized by the International Union of Immunological Societies (IUIS) are reviewed. These are the proteins associated with the rubber particles, the cytosolic C-serum proteins and the B-serum proteins that originate mainly from the lutoids. Procedures for the isolation and purification of latex allergens are discussed, from latex collection in the field to various preparative approaches adopted in the laboratory. As interest in recombinant latex allergens increases, there is a need to validate recombinant proteins to ascertain equivalence with their native counterparts when used in immunological studies, diagnostics, and immunotherapy.

  10. Cellulose nanocrystal reinforced oxidized natural rubber nanocomposites.

    Science.gov (United States)

    Mariano, Marcos; El Kissi, Nadia; Dufresne, Alain

    2016-02-10

    Natural rubber (NR) latex particles were oxidized using KMnO4 as oxidant to promote the insertion of hydroxyl groups in the surface polyisoprene chains. Different degrees of oxidation were investigated. Both unoxidized and oxidized NR (ONR) latex were used to prepare nanocomposite films reinforced with cellulose nanocrystals (CNCs) by casting/evaporation. The oxidation of NR was carried out to promote chemical interactions between the hydroxyl groups of ONR with those of CNCs through hydrogen bonding. The effect of the degree of oxidation of the NR latex on the rheological behavior of CNC/NR and CNC/ONR suspensions, as well as on the mechanical, swelling and thermal properties of ensuing nanocomposites was investigated. Improved properties were observed for intermediate degrees of oxidation but they were found to degrade for higher oxidation levels.

  11. Silicone-Rubber Microvalves Actuated by Paraffin

    Science.gov (United States)

    Svelha, Danielle; Feldman, Sabrina; Barsic, David

    2004-01-01

    Microvalves containing silicone-rubber seals actuated by heating and cooling of paraffin have been proposed for development as integral components of microfluidic systems. In comparison with other microvalves actuated by various means (electrostatic, electromagnetic, piezoelectric, pneumatic, and others), the proposed valves (1) would contain simpler structures that could be fabricated at lower cost and (2) could be actuated by simpler (and thus less expensive) control systems. Each valve according to the proposal would include a flow channel bounded on one side by a flat surface and on the other side by a curved surface defined by an arched-cross-section, elastic seal made of silicone rubber [polydimethylsilane (PDMS)]. The seal would be sized and shaped so that the elasticity of the PDMS would hold the channel open except when the seal was pressed down onto the flat surface to close the channel. The principle of actuation would exploit the fact that upon melting or freezing, the volume of a typical paraffin increases or decreases, respectively, by about 15 percent. In a valve according to the proposal, the seal face opposite that of the channel would be in contact with a piston-like plug of paraffin. In the case of a valve designed to be normally open at ambient temperature, one would use a paraffin having a melting temperature above ambient. The seal would be pushed against the flat surface to close the channel by heating the paraffin above its melting temperature. In the case of a valve designed to be normally closed at ambient temperature, one would use a paraffin having a melting temperature below ambient. The seal would be allowed to spring away from the flat surface to open the channel by cooling the paraffin below its melting temperature. The availability of paraffins that have melting temperatures from 70 to +80 C should make it possible to develop a variety of normally closed and normally open valves. The figure depicts examples of prototype normally

  12. Polybenzoxazole-filled nitrile butadiene rubber compositions

    Science.gov (United States)

    Gajiwala, Himansu M. (Inventor); Guillot, David G. (Inventor)

    2008-01-01

    An insulation composition that comprises at least one nitrile butadiene rubber (NBR) having an acrylonitrile content that ranges from approximately 26% by weight to approximately 35% by weight and polybenzoxazole (PBO) fibers. The NBR may be a copolymer of acrylonitrile and butadiene and may be present in the insulation composition in a range of from approximately 45% by weight to approximately 56% by weight of a total weight of the insulation composition. The PBO fibers may be present in a range of from approximately 3% by weight to approximately 10% by weight of a total weight of the insulation composition. A rocket motor including the insulation composition and a method of insulating a rocket motor are also disclosed.

  13. Cellulose nanocrystals reinforced foamed nitrile rubber nanocomposites.

    Science.gov (United States)

    Chen, Yukun; Zhang, Yuanbing; Xu, Chuanhui; Cao, Xiaodong

    2015-10-05

    Research on foamed nitrile rubber (NBR)/cellulose nanocrystals (CNs) nanocomposites is rarely found in the literatures. In this paper, CNs suspension and NBR latex was mixed to prepared the foamed NBR/CNs nanocomposites. We found that the CNs mainly located in the cell walls, effectively reinforcing the foamed NBR. The strong interaction between the CNs and NBR matrix restricted the mobility of NBR chains surrounding the CNs, hence increasing the crosslink density of the NBR matrix. CNs exhibited excellent reinforcement on the foamed NBR: a remarkable increase nearly 76% in the tensile strength of the foamed nanocomposites was achieved with a load of only 15 phr CNs. Enhanced mechanical properties make the foamed NBR/CNs nanocomposites a promising damping material for industrial applications with a potential to reduce the petroleum consumption.

  14. HYDROPHOBICITY OF CONTAMINATED SILICONE RUBBER SURFACES

    Institute of Scientific and Technical Information of China (English)

    Zhi-min Zheng; Cai-hong Xu; Jian Jiang; Chang-yu Ren; Wei Gao; Ze-min Xie

    2002-01-01

    Silicone rubber (SIR) shows superior performance when used outdoors, but its surface can be transformed frominherently hydrophobic to hydrophilic by the adsorption of contaminants. Al(OH)3, Al2O3, quartz powder and active carbonwere selected as authentic contaminants. Hydrophobicity of the surface was determined using contact angle measurement.The results indicate that the adsorbability of the contaminants can strongly affect the hydrophobicity of contaminated SIRsurface. The increasing rate of contact angle of specimens contaminated by Al(OH)3 was much faster than that by Al2O3 andquartz due to the adsorption of migrated low molecular weight (LMW) polydimethylsiloxanes. Specimens contaminated byactive carbon could achieve surface hydrophobicity within 15 min because active carbon has high adsorbability. Surfaces ofcontaminated ultrapure SIR, polytetrafluoroethylene (PTFE) and glass remain hydrophilic because they contain no mobileLMW components. The addition of oligomeric polydimethylsiloxanes has little effect on the hydrophobicity of contaminantscovered on SIR surface.

  15. minimum variance estimation of yield parameters of rubber tree with ...

    African Journals Online (AJOL)

    2013-03-01

    Mar 1, 2013 ... STAMP, an OxMetric modular software system for time series analysis, was used to estimate the yield ... derlying regression techniques. .... Kalman Filter Minimum Variance Estimation of Rubber Tree Yield Parameters. 83.

  16. Thermo-Mechanical Analyses of Dynamically Loaded Rubber Cylinders

    Science.gov (United States)

    Johnson, Arthur R.; Chen, Tzi-Kang

    2002-01-01

    Thick rubber components are employed by the Army to carry large loads. In tanks, rubber covers road wheels and track systems to protect roadways. It is difficult for design engineers to simulate the details of the hysteretic heating for large strain viscoelastic deformations. In this study, an approximation to the viscoelastic energy dissipated per unit time is investigated for use in estimating mechanically induced viscoelastic heating. Coupled thermo-mechanical simulations of large cyclic deformations of rubber cylinders are presented. The cylinders are first compressed axially and then cyclically loaded about the compressed state. Details of the algorithm and some computational issues are discussed. The coupled analyses are conducted for tall and short rubber cylinders both with and without imbedded metal disks.

  17. Metal Rubber Sensor Appliquis for Rotor Blade Air Project

    Data.gov (United States)

    National Aeronautics and Space Administration — Thin film Metal RubberTM sensor appliqus have the potential to reduce the time, complexity and cost of measuring air flow-induced skin friction during the...

  18. Prevention of Fungal Growth on Rubber Earpads of Telecommunication Equipments

    Directory of Open Access Journals (Sweden)

    B. P. Uniyal

    1971-01-01

    Full Text Available This paper recommends an addition of 100% zinc oxide to the rubber composition during its manufacture to effectively prevent fungal growth on the earpads without producing any adverse on its materials/performance or the user.

  19. Super Lightweight, Metal Rubber Fabric for Extreme Space Environments Project

    Data.gov (United States)

    National Aeronautics and Space Administration — NanoSonic has fabricated revolutionary nanostructured, yet macroscale, multifunctional Metal RubberTM films via layer-by-layer, molecular self-assembly, which...

  20. Radiation Resistant, Reconfigurable, Shape Memory Metal Rubber Space Arrays Project

    Data.gov (United States)

    National Aeronautics and Space Administration — NanoSonic has demonstrated that Shape Memory Metal RubberTM (SM-MR) adaptive skins exhibit reconfigurable and durable RF properties. It is hypothesized that such...

  1. Sand - rubber mixtures submitted to isotropic loading: a minimal model

    Science.gov (United States)

    Platzer, Auriane; Rouhanifar, Salman; Richard, Patrick; Cazacliu, Bogdan; Ibraim, Erdin

    2017-06-01

    The volume of scrap tyres, an undesired urban waste, is increasing rapidly in every country. Mixing sand and rubber particles as a lightweight backfill is one of the possible alternatives to avoid stockpiling them in the environment. This paper presents a minimal model aiming to capture the evolution of the void ratio of sand-rubber mixtures undergoing an isotropic compression loading. It is based on the idea that, submitted to a pressure, the rubber chips deform and partially fill the porous space of the system, leading to a decrease of the void ratio with increasing pressure. Our simple approach is capable of reproducing experimental data for two types of sand (a rounded one and a sub-angular one) and up to mixtures composed of 50% of rubber.

  2. Ciprofloxacin Release Using Natural Rubber Latex Membranes as Carrier

    National Research Council Canada - National Science Library

    Dias Murbach, Heitor; Jaques Ogawa, Guilherme; Azevedo Borges, Felipe; Romeiro Miranda, Matheus Carlos; Lopes, Rute; Roberto de Barros, Natan; Guedes Mazalli, Alexandre Vinicius; Gonçalves da Silva, Rosângela; Ferreira Cinman, José Luiz; de Camargo Drago, Bruno; Donizetti Herculano, Rondinelli

    2014-01-01

      Natural rubber latex (NRL) from Hevea brasiliensis is easily manipulated, low cost, is of can stimulate natural angiogenesis and cellular adhesion, is a biocompatible, material and presents high mechanical resistance. Ciprofloxacin (CIP...

  3. Radiation Vulcanised Natural Rubber Latex: safer than conventionally processed latex?

    NARCIS (Netherlands)

    Geertsma RE; Orzechowski TJH; Jonker M; Dorpema JW; Asten JAAM van; LGM

    1996-01-01

    Door middel van cytotoxiciteitstesten is aangetoond dat RVNRL (straling-gevulcaniseerde natuurlijke latex rubber) materialen aanzienlijk minder cytotoxisch zijn dan zwavel-gevulcaniseerde materialen. Dit is een sterke aanwijzing dat een deel van de allergieproblemen, namelijk de zogeheten Type

  4. Utilization of surface-treated rubber particles from waste tires

    Energy Technology Data Exchange (ETDEWEB)

    Smith, F.G. [Argonne National Lab., IL (United States). Energy Systems Div.]|[Environmental Technologies Alternatives, Inc., Lima, OH (United States)

    1994-12-01

    During a 12-month program, the author successfully demonstrated commercial applications for surface-treated rubber particles in two major markets: footwear (shoe soles and components) and urethane-foam carpet underlay (padding). In these markets, he has clearly demonstrated the ease of using R-4080 and R-4030 surface-treated rubber particles in existing manufacturing plants and processes and have shown that the material meets or exceeds existing standards for performance, quality, and cost-effectiveness. To produce R-4080 and R-4030, vulcanized rubber, whole-tire material is finely ground to particles of nominal 80 and mesh size respectively. Surface treatment is achieved by reacting these rubber particles with chlorine gas. In this report, the author describes the actual test and evaluations of the participant companies, and identifies other potential end uses.

  5. Multifunctional, Nanostructured Metal Rubber Protective Films for Space Exploration Project

    Data.gov (United States)

    National Aeronautics and Space Administration — NanoSonic has developed revolutionary nanostructured, yet macroscale, multifunctional Metal RubberTM films. In support of NASA's Vision for Space Exploration, low...

  6. Lightweight Metal RubberTM Sensors and Interconnects Project

    Data.gov (United States)

    National Aeronautics and Space Administration — The objective of this NASA Phase II program is to develop and increase the Technology Readiness Level of multifunctional Metal RubberTM (MRTM) materials that can be...

  7. Advanced Metal Rubber Sensors for Hypersonic Decelerator Entry Systems Project

    Data.gov (United States)

    National Aeronautics and Space Administration — NanoSonic proposes to design and develop light-weight, low-modulus, and durable Metal Rubber™ sensors for aeroelastic analysis of Hypersonic Decelerator Entry...

  8. Strength of Concrete Containing Rubber Particle as Partial Cement Replacement

    Directory of Open Access Journals (Sweden)

    Abdullah Siti Radziah

    2016-01-01

    Full Text Available Uncontrolled issues of disposal waste tire rubber create huge environmental impact and health hazards. An alternative viable solution to minimize these problems is by utilizing the waste rubber tires in construction materials, which in turn can reduce the use of natural resources and eventually lessen the cost of construction. This paper mainly focuses on the use of waste rubber tires particles in concrete with different set of composition ranging from 3 to 12% of cement replacement. Concrete cubes size of 150mm x 150mm x 150mm were prepared for compressive strength test, and concrete cylinders size of 150m x 300mm were prepared for splitting tensile test. The result shows that the compressive and split tensile strength of concrete with rubber as cement replacements is 6-21% lower than the normal concrete.

  9. Tribological Aspect of Rubber Based Parts used in Engineering

    Directory of Open Access Journals (Sweden)

    D. Stamenković

    2014-03-01

    Full Text Available In most of the cases, the friction is considered as a negative side-effect concerning energy loss following every process of the power transmission. However, the friction has significant positive side effects, because it is an indispensable prerequisite for the movement of people, machines, transportation means and others. Efficiency of these movements mostly depends on the friction between rubber and different materials such as metals, concrete, earth, wood, plastic, etc. Certain standards relating to measurement and determination of the friction characteristics of rubber were established. However considering that tribology of the rubber is very complex problem, numerous studies around the world are conducted. This paper gives an overview of some of the existing standards and conducted researches in this area. The paper also provides an overview of theoretical and experimental studies of friction the rubber and the other materials, which are done at Faculty of Mechanical Engineering in Niš.

  10. Thermochemical Properties Enthalpy, Entropy, and Heat Capacity of C1-C4 Fluorinated Hydrocarbons: Fluorocarbon Group Additivity.

    Science.gov (United States)

    Wang, Heng; Castillo, Álvaro; Bozzelli, Joseph W

    2015-07-23

    Enthalpies of formation for 14 C2–C4 fluorinated hydrocarbons were calculated with nine popular ab initio and density functional theory methods: B3LYP, CBS-QB3, CBS-APNO, M06, M06-2X, ωB97X, G4, G4(MP2)-6X, and W1U via several series of isodesmic reactions. The recommended ideal gas phase ΔHf298° (kcal mol(–1)) values calculated in this study are the following: −65.4 for CH3CH2F; −70.2 for CH3CH2CH2F; −75.3 for CH3CHFCH3; −75.2 for CH3CH2CH2CH2F; −80.3 for CH3CHFCH2CH3; −108.1 for CH2F2; −120.9 for CH3CHF2; −125.8 for CH3CH2CHF2; −133.3 for CH3CF2CH3; −166.7 for CHF3; −180.5 for CH3CF3; −185.5 for CH3CH2CF3; −223.2 for CF4; and −85.8 for (CH3)3CF. Entropies (S298° in cal mol(–1) K(–1)) were estimated using B3LYP/6-31+G(d,p) computed frequencies and geometries. Rotational barriers were determined and hindered internal rotational contributions for S298°, and Cp(T) were calculated using the rigid rotor harmonic oscillator approximation, with direct integration over energy levels of the intramolecular rotation potential energy curve. Thermochemical properties for the fluorinated carbon groups C/C/F/H2, C/C2/F/H, C/C/F2/H, C/C2/F2, and C/C/F3 were derived from the above target fluorocarbons. Previously published enthalpies and groups for 1,2-difluoroethane, 1,1,2-trifluoroethane, 1,1,2,2-tetrafluoroethane, 1,1,1,2-tetrafluoroethane, 1,1,1,2,2-pentafluoroethane, 2-fluoro-2-methylpropane that were previously determined via work reaction schemes are revised using updated reference species values. Standard deviations are compared for the calculation methods.

  11. Altered levels of the Taraxacum kok-saghyz (Russian dandelion) small rubber particle protein, TkSRPP3, result in qualitative and quantitative changes in rubber metabolism.

    Science.gov (United States)

    Collins-Silva, Jillian; Nural, Aise Taban; Skaggs, Amanda; Scott, Deborah; Hathwaik, Upul; Woolsey, Rebekah; Schegg, Kathleen; McMahan, Colleen; Whalen, Maureen; Cornish, Katrina; Shintani, David

    2012-07-01

    Several proteins have been identified and implicated in natural rubber biosynthesis, one of which, the small rubber particle protein (SRPP), was originally identified in Hevea brasiliensis as an abundant protein associated with cytosolic vesicles known as rubber particles. While previous in vitro studies suggest that SRPP plays a role in rubber biosynthesis, in vivo evidence is lacking to support this hypothesis. To address this issue, a transgene approach was taken in Taraxacum kok-saghyz (Russian dandelion or Tk) to determine if altered SRPP levels would influence rubber biosynthesis. Three dandelion SRPPs were found to be highly abundant on dandelion rubber particles. The most abundant particle associated SRPP, TkSRPP3, showed temporal and spatial patterns of expression consistent with patterns of natural rubber accumulation in dandelion. To confirm its role in rubber biosynthesis, TkSRPP3 expression was altered in Russian dandelion using over-expression and RNAi methods. While TkSRPP3 over-expressing lines had slightly higher levels of rubber in their roots, relative to the control, TkSRPP3 RNAi lines showed significant decreases in root rubber content and produced dramatically lower molecular weight rubber than the control line. Not only do results here provide in vivo evidence of TkSRPP proteins affecting the amount of rubber in dandelion root, but they also suggest a function in regulating the molecular weight of the cis-1, 4-polyisoprene polymer.

  12. Time series analysis of the behavior of brazilian natural rubber

    Directory of Open Access Journals (Sweden)

    Antônio Donizette de Oliveira

    2009-03-01

    Full Text Available The natural rubber is a non-wood product obtained of the coagulation of some lattices of forest species, being Hevea brasiliensis the main one. Native from the Amazon Region, this species was already known by the Indians before the discovery of America. The natural rubber became a product globally valued due to its multiple applications in the economy, being its almost perfect substitute the synthetic rubber derived from the petroleum. Similarly to what happens with other countless products the forecast of future prices of the natural rubber has been object of many studies. The use of models of forecast of univariate timeseries stands out as the more accurate and useful to reduce the uncertainty in the economic decision making process. This studyanalyzed the historical series of prices of the Brazilian natural rubber (R$/kg, in the Jan/99 - Jun/2006 period, in order tocharacterize the rubber price behavior in the domestic market; estimated a model for the time series of monthly natural rubberprices; and foresaw the domestic prices of the natural rubber, in the Jul/2006 - Jun/2007 period, based on the estimated models.The studied models were the ones belonging to the ARIMA family. The main results were: the domestic market of the natural rubberis expanding due to the growth of the world economy; among the adjusted models, the ARIMA (1,1,1 model provided the bestadjustment of the time series of prices of the natural rubber (R$/kg; the prognosis accomplished for the series supplied statistically adequate fittings.

  13. Thermomechanical analysis of Natural Rubber behaviour stressed at room temperature.

    OpenAIRE

    Chrysochoos A.; Wattrisse B.; Muracciole J.M.; Caborgan R.

    2010-01-01

    Owing to their high molecular mobility, stressed rubber chains can easily change their conformations and get orientated. This phenomena leads to so high reversible draw ratio that this behaviour is called rubber elasticity [1-3]. The analogy with ideal gases leads to an internal energy independent of elongation, the stress being attributed to a so-called configuration entropy. However, this analysis cannot take thermal expansion into account and moreover prohibits predicting standard th...

  14. Dalian Rubber & Plastics Hong Kong Company Acquired a Rubber Machinery Enterprise of the Czech Republic%Dalian Rubber & Plastics Hong Kong Company Acquired a Rubber Machinery Enterprise of the Czech Republic

    Institute of Scientific and Technical Information of China (English)

    FengPei

    2011-01-01

    To further widen the international market, improve the technical content of products and boost the profitability of the enterprise, Dalian Rubber & Plastics Hong Kong Company, jointly invested and established by Dalian State-owned Assets Investment and Management Group Co., Ltd. and Dalian Rubber & Plastics Machinery Co., Ltd., plans to invest about EUR 12.50 million to acquire 90% stock fight of Buzuluk Company of the Czech Republic.

  15. Serbia: A new process for waste rubber and plastic recycling

    Directory of Open Access Journals (Sweden)

    Ozren Ocic

    2010-02-01

    Full Text Available This paper intends to describe a new technological process for waste rubber and plastic recycling up to the commercial components in safe environmental friendly way. Researches and all relevant technical-technological data related to this process are checked at constructed pilot plant. The future construction of these units for waste rubber and plastic recycling will allow interested parties to achieve the environmental effectiveness and economic efficiency.

  16. Studies on Hydrogenation of Liquid Natural Rubber Using Diimide

    Directory of Open Access Journals (Sweden)

    Nur Hanis Adila Azhar

    2015-01-01

    Full Text Available Liquid natural rubber (LNR is a depolymerized natural rubber (NR which consists of shorter polymeric chains and lower molecular weight (Mw90% was achieved by manipulating the reaction parameters such as sources of diimide, TSH concentration, solvent, and reaction time. The optimum condition was 3 : 1 weight ratio of TSH/LNR in o-xylene at 130°C in 4-hour reaction period.

  17. The toughening mechanism of rubber particles in polypropylene composite

    Science.gov (United States)

    Shi, L.; Xiao, J. M.

    2017-01-01

    Filling polypropylene materials with rubber particles can effectively increase the toughness of PP material and improve its cushioning properties. In this paper, we used the two kinds of method of the finite element analysis and experiment to study the rubber particles toughening mechanism, got the deformation process of particles when polypropylene material compressed and the yield stress of polypropylene after compression with particles filled or not.

  18. Characterization of Rubbers from Spherical Punch - Plate Indentation Tests

    Directory of Open Access Journals (Sweden)

    Florina Carmen Ciornei

    2016-12-01

    Full Text Available Rubber plates with different compositions and hardness were tested by continuous indentation, using a spherical punch and hysteretic phenomenon was evidenced. The experimental data interpolation with polynomial functions is accurate and permits estimation of the lost work during loading cycles. The interpolation by power law functions is more convenient by using less parameters and having a form accepted in literature. From the rubbers tested, two were considered to present good damping properties.

  19. Criteria for asphalt-rubber concrete in civil airport pavements: Mixture design

    Science.gov (United States)

    Roberts, F. L.; Lytton, R. L.; Hoyt, D.

    1986-07-01

    A mixture design procedure is developed to allow the use of asphalt-rubber binders in concrete for flexible airport pavement. The asphalt-rubber is produced by reacting asphalt with ground, scrap tire rubber to produce the binder for the asphalt-rubber concrete. Procedures for laboratory preparation of alsphalt-rubber binders using an equipment setup that was found by researchers to produce laboratory binders with similar properties to field processes are included. The rubber-asphalt concrete mixture design procedure includes adjustments to the aggregate gradation to permit space for the rubber particles in the asphalt-rubber binder as well as suggested mixing and compaction temperatures, and compaction efforts. While the procedure was used in the laboratory to successfully produce asphalt-rubber concrete mixtures, it should be evaluated in the field to ensure that consistent results can be achieved in a production environment.

  20. Waste tyre rubberized concrete: properties at fresh and hardened state.

    Science.gov (United States)

    Aiello, M A; Leuzzi, F

    2010-01-01

    The main objective of this paper is to investigate the properties of various concrete mixtures at fresh and hardened state, obtained by a partial substitution of coarse and fine aggregate with different volume percentages of waste tyres rubber particles, having the same dimensions of the replaced aggregate. Workability, unit weight, compressive and flexural strength and post-cracking behaviour were evaluated and a comparison of the results for the different rubcrete mixtures were proposed in order to define the better mix proportions in terms of mechanical properties of the rubberized concrete. Results showed in this paper were also compared to data reported in literature. Moreover, a preliminary geometrical, physical and mechanical characterization on scrap tyre rubber shreds was made. The rubberized concrete mixtures showed lower unit weight compared to plain concrete and good workability. The results of compressive and flexural tests indicated a larger reduction of mechanical properties of rubcrete when replacing coarse aggregate rather than fine aggregate. On the other hand, the post-cracking behaviour of rubberized concrete was positively affected by the substitution of coarse aggregate with rubber shreds, showing a good energy absorption and ductility indexes in the range observed for fibrous concrete, as suggested by standard (ASTM C1018-97, 1997).

  1. Dielectric Properties of Compatibilised EPDM/Silicone rubber Nanocomposites

    Directory of Open Access Journals (Sweden)

    Vijayalekshmi Vijayakumar

    2017-06-01

    Full Text Available EPDM/Silicone rubber nanocomposites are prepared by incorporating various phr of organically modified montmorillonite (OMMT nanoclay onto compatibilised and uncompatibilised EPDM/Silicone rubber blends using two roll mill. Compatibilisation of EPDM and Silicone rubber blend is achieved through insitu grafting of silane onto EPDM during mixing of rubbers. Effect of OMMT content and compatibilisation of blend system on electrical, mechanical and thermal properties of the nanocomposites are investigated. The results obtained for various properties indicate that the compatibilised EPDM/Silicone rubber nanocomposites have improved dielectric, mechanical and thermal properties compared to that of uncompatibilised blend nanocomposites. It is observed that, the addition of OMMT upto 5 phr onto both compatibilised and uncompatibilised blends of EPDM/Silicone offers significant improvement in the above mentioned properties. Increasing content of OMMT onto the blends cause marked enhancement in thermal stability of the nanocomposties. Transmission electron micrographs shows the compatibility between EPDM and silicone rubbers in the blend and the exfoliation of OMMT layers in the matrix phase. The present work reveals that the compatibilised EPDM/ Silicone/ OMMT nanocomposite can be a better candidate for high voltage electrical insulation due to its enhanced dielectric, mechanical and themal characteristics.

  2. Effects of rubberized flooring on Asian elephant behavior in captivity.

    Science.gov (United States)

    Meller, Camie L; Croney, Candace C; Shepherdson, David

    2007-01-01

    Six Asian elephants at the Oregon Zoo were observed to determine the effects of a poured rubber flooring substrate on captive Asian elephant behavior. Room utilization also was evaluated in seven rooms used for indoor housing, including Front and Back observation areas. Data were collected in three phases. Phase I (Baseline Phase) examined elephant behavior on old concrete floors. In Phase II (Choice Phase), elephant behavior was observed in the Back observation area where room sizes were comparable and when a choice of flooring substrates was available. Phase III (Final Phase) examined elephant behavior when all rooms in both observation areas, Front and Back, were converted to rubberized flooring. Room use in both observation areas remained stable throughout the study, suggesting that flooring substrate did not affect room use choice. However, there was a clear pattern of decreased discomfort behaviors on the new rubber flooring. Normal locomotion as well as stereotypic locomotion increased on the new rubber flooring. In addition, resting behavior changed to more closely reflect the resting behavior of wild elephants, which typically sleep standing up, and spend very little time in lateral recumbence. Overall, these findings suggest that the rubber flooring may have provided a more comfortable surface for locomotion as well as standing resting behavior. It is suggested that poured rubber flooring may be a beneficial addition to similar animal facilities. Zoo Biol 0:1-11, 2007. (c) 2007 Wiley-Liss, Inc.

  3. [Allergic contact dermatitis to synthetic rubber, neoprene in compression stockings].

    Science.gov (United States)

    Mizuno, Ju; In-Nami, Hiroshi

    2011-01-01

    Compression stockings are used for patients under general anesthesia to prevent occurrence of deep venous thrombosis. We report a case of allergic contact dermatitis to synthetic rubber, neoprene in compression stockings. A 53-year-old house wife had a history of sensitivity like skin eruption and disstasis to rubber products such as rubber band. Left nephrectomy for rupture of renal angiomyolipoma was scheduled under general and epidural anesthesia. Further examination for gum allergy was not performed before the operation, although latex allergy was suspected. The operation was performed uneventfully under latex-safe environment in the operating room under guideline for latex allergy. Postoperatively, ringed edematous erythema and wheal occurred in her bilateral thighs compressed with the upper part of compression stockings. The skin symptoms continued for more than four days. After disappearance of the skin symptoms, she was discharged from the hospital on the ninth day after the operation. Synthetic rubber, neoprene, in the upper part of compression stockings to prevent slipping down might cause allergic contact dermatitis. We should take care of occurrence of allergic contact dermatitis to synthetic rubber, neoprene in compression stockings in patients with rubber allergy.

  4. COORDINATION CROSSLINKING OF NITRILE RUBBER FILLED WITH COPPER SULFATE PARTICLES

    Institute of Scientific and Technical Information of China (English)

    2007-01-01

    By incorporating copper sulfate (CuSO4) particles into acrylonitrile butadiene rubber (NBR) followed by heat pressing.a novel vulcanization method is developed in rubber through the formation of coordination crosslinking.This method totally differs from traditional covalent or non-covalent vulcanization approaches of rubber.No other vulcanizing agent or additional additive is involved in this process.By analyzing the results of DMA,XPS and FT-IR,it is found that the crosslinking of CuSO4 particles filled NBR was induced by in situ coordination between nitrogen atoms of nitrile groups (-CN) and copper ions (Cu2+) from CuSO4.SEM and EDX results revealed the generation of a core (CuSO4 solid particle) shell (adherent NBR) structure,which leads to a result that the crosslinked rubber has excellent mechanical properties.Moreover,poly (vinyl chloride)(PVC) and liquid acrylonitrile-butadiene rubber (LNBR) were used as mobilizer to improve the coordination crosslinking of CuSO4/NBR.The addition of PVC or LNBR could lead to higher crosslink density and better mechanical properties of coordination vulcanization.In addition,crystal water in CuSO4 played a positive role to coordination crosslinking of rubber because it decreased the metal point of CuSO4 and promoted the metal ionization.

  5. Effect of rubber dam on mercury exposure during amalgam removal.

    Science.gov (United States)

    Kremers, L; Halbach, S; Willruth, H; Mehl, A; Welzl, G; Wack, F X; Hickel, R; Greim, H

    1999-06-01

    It was the aim of this investigation to treat 20 volunteers with maximally 5 amalgam fillings by the same comprehensive protocol in which all removals with (n = 8) and without (n = 12) rubber dam had been performed within a few months. Nine amalgam-related parameters indicated a close matching of both groups before removal. In the group without rubber dam, mercury (Hg) levels in plasma increased significantly above preremoval values at days 1 and 3 after removal; they decreased significantly below preremoval values at day 30 in the rubber-dam group and at day 100 in both groups. Excretion rates did not increase significantly in either group, but decreased significantly at day 100 in the protected group. Peak plasma-Hg was 0.6 ng/mL on average at day one and decreased with halftimes of 3 and 43 d in subjects protected by rubber dam. The results indicated that concentrations of total mercury in plasma responded rapidly to changes in the amalgam status and reflected the actual absorption most reliably. Notably, plasma-Hg levels were sensitive enough to detect a transient attenuation of the additional exposure by using rubber dam during the removal of only a few fillings. However, being small in magnitude and lasting 100 d at best, the rubber-dam effect had minor toxicological relevance.

  6. Genotoxic risk in rubber manufacturing industry: a systematic review.

    Science.gov (United States)

    Bolognesi, Claudia; Moretto, Angelo

    2014-10-15

    A large body of evidence from epidemiological studies among workers employed in the rubber manufacturing industry has indicated a significant excess cancer risk in a variety of sites. The International Agency for Research on Cancer has recently classified the "Occupational exposures in the rubber-manufacturing industry" as carcinogenic to humans (Group 1). A genotoxic mechanism for the increased cancer risk was suggested on the basis of the evidence from the scientific literature. Exposure assessment studies have shown that workers in the rubber manufacturing industry may be exposed to different airborne carcinogenic and/or genotoxic chemicals, such as certain aromatic amines, polycyclic aromatic hydrocarbons, N-nitrosamines, although the available information does not allow to establish a causal association of cancer or genotoxic risk with particular substances/classes of chemicals or specific jobs. The aim of this paper is to critically evaluate, by conducting a systematic review, the available biomonitoring studies using genotoxicity biomarkers in rubber manufacturing industry. This systematic review suggests that a genotoxic hazard may still be present in certain rubber manufacturing industries. A quantitative risk assessment needs further studies addressing the different, processes and chemicals in the rubber manufacturing industries.

  7. DAMAGE OF SILICONE RUBBER INDUCED BY PROTON IRRADIATION

    Institute of Scientific and Technical Information of China (English)

    Li-xin Zhang; Shi-qin Yang; Shi-yu He

    2003-01-01

    In this paper, the damage to methyl silicone rubber induced by irradiation with protons of 150 keV energy was studied. The surface morphology, tensile strength, Shore hardness, cross-linking density and glass transition temperature were examined. Positron annihilation lifetime spectrum analysis (PALS) was perfomed to reveal the damage mechanisms of the rubber. The results showed that tensile strength and Shore hardness of the rubber increased first and then decreased with increasing irradiation fluence. The PALS characteristics τ3 and I3, as well as the free volume Vf, decreased with increasing irradiation fluence up to 1015 cm-2, and then increased slowly. It indicates that proton irradiation causes a decrease of free volume in the methyl silicone rubber when the fluence is less than l015 cm-2, while the free volume increases when the fluence is greater than 1015 cm-2. The results on cross-linking density indicate that the cross-linking induced by proton irradiation is dominant at smaller proton fluences, increasing the tensile strength and Shore hardness of the rubber, while the degradation of rubber dominates at greater fluence, leading to a decrease of tensile strength and Shore hardness.

  8. Effect of filler water absorption on water swelling properties of natural rubber

    Science.gov (United States)

    Trakuldee, J.; Boonkerd, K.

    2017-07-01

    The efficient water swelling rubber can be obtained by using high hydrophilic rubber such as chloroprene rubber. However, chloroprene rubber is synthetic rubber developed from the petroleum. Recently, many researches try to replace the usage of synthetic rubber with natural rubber. This is not only due to the concerning of environment but the cost reduction as well. However, natural rubber is hydrophobic, thus not absorbing water. To develop the water swelling rubber from natural rubber, the addition of water absorption filler is needed. The study was aimed to formulate water swelling rubber from natural rubber filled with sodium polyacrylate (SA)/sodium bentonite clay (SBC) hybrid filler used to water absorbent. The filler loading was kept constantly at 150 phr. The effect of SA/SBC ratio varied from 1:0, 1:1, 1:2 and 1:3 on the water absorption of the hybrid filled natural rubber was determined. The obtained result showed that the water adsorption proportionally increased with increasing SA loading but decreased with increasing SBC loading. The effect of glycidyl methacrylate (GM) and poly ethylene glycol (PEG) on the water absorption was studied later. The result from a scanning electron microscope depicted that the presence of GM can depress the falling out of SA from the rubber matrix while the presence of PEG increased water absorption.

  9. STUDY ON THE PROPERTIES OF BLEND OF NATURAL RUBBER LATEX/METHYL METHACRYLATE GRAFTED RUBBER LATEX BY GAMMA RADIATION

    Institute of Scientific and Technical Information of China (English)

    2007-01-01

    Natural rubber latex (NRL) and methyl methacrylate (MMA) grafted rubber latex were blended in different ratios and irradiated at various absorbed doses by gamma rays from Co-60 source at room temperature.The tensile properties,swelling ratio and permanent set were measured.The maximum tensile strength and modulus at 500% elongation were obtained at an absorbed dose of 8 kGy.Modulus increases from 6.99 Mpa to 9.87 Mpa for an increase in proportion of MMA grafted rubber from 40% to 60% in the blend at similar absorbed dose.Elongation at break and swelling ratio decrease with increasing absorbed dose as well as the MMA grafted rubber content in the blends.The decreasing trend of permanent set is high up to 5 kGy absorbed dose, and beyond that dose,it becomes almost flat.

  10. Rubber and rubber-like materials, finite-element analyses and simulations, an addendum: a bibliography (1997 2003)

    Science.gov (United States)

    Mackerle, Jaroslav

    2004-09-01

    This paper gives a bibliographical review of the finite-element methods (FEMs) applied to the analysis and simulation of rubber and rubber-like materials. It is a continuation of the author's paper 'Rubber and Rubber-Like Materials, Finite-Element Analyses and Simulations: a Bibliography (1976-1997)' published in 1998 Modelling Simul. Mater. Sci. Eng. 6 171-98. The added bibliography at the end of this article contains 510 references to papers and conference proceedings on the subject that were published in 1997-2003. The following topics are included: incompressible elasticity problems in general, mechanical and material properties, a finite-element library for incompressible materials, contact problems, fracture mechanics, machine elements/structures, material processing and other topics.

  11. Biodegradation of a blended starch/natural rubber foam biopolymer and rubber gloves by Streptomyces coelicolor CH13

    OpenAIRE

    2012-01-01

    Background: The growing problem of environmental pollution caused by synthetic plastics has led to the search for alternative materials such as biodegradable plastics. Of the biopolymers presently under development, starch/natural rubber is one promising alternative. Several species of bacteria and fungi are capable of degrading natural rubber and many can degrade starch. Results: Streptomyces coelicolor CH13 was isolated from soil according to its ability to produce translucent halos on a mi...

  12. Reinforcing effect of plasma modified halloysite nanotubes in a carbon black filled natural rubber-butadien rubber matrix

    OpenAIRE

    Poikelispaa, Minna; Das, Amit; Dierkes, Wilma; Vuorinen, Jyrki

    2011-01-01

    Rubber composites are generally produced by the direct incorporation of fillers like carbon black and/or silica into the rubber matrix. The incorporation of different types of nanofillers is the subject of recent research with the aim of preparing composites with special compositions and properties. A successful application of such composites depends mainly on the degree of dispersion of the nano-sized fillers. Recently, a naturally occurring clay mineral, halloysite nanotubes (HNTs), is inve...

  13. 40 CFR 428.90 - Applicability; description of the pan, dry digestion, and mechanical reclaimed rubber subcategory.

    Science.gov (United States)

    2010-07-01

    ..., dry digestion, and mechanical reclaimed rubber subcategory. 428.90 Section 428.90 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY (CONTINUED) EFFLUENT GUIDELINES AND STANDARDS RUBBER MANUFACTURING POINT SOURCE CATEGORY Pan, Dry Digestion, and Mechanical Reclaimed Rubber Subcategory §...

  14. Predicting the glass transition temperature as function of crosslink density and polymer interactions in rubber compounds

    Science.gov (United States)

    D'Escamard, Gabriella; De Rosa, Claudio; Auriemma, Finizia

    2016-05-01

    Crosslink sulfur density in rubber compounds and interactions in polymer blends are two of the composition elements that affect the rubber compound properties and glass transition temperature (Tg), which is a marker of polymer properties related to its applications. Natural rubber (NR), butadiene rubber (BR) and styrene-butadiene rubber (SBR) compounds were investigated using calorimetry (DSC) and dynamic mechanical analysis (DMA). The results indicate that the Di Marzio's and Schneider's Models predict with accuracy the dependence of Tg on crosslink density and composition in miscible blends, respectively, and that the two model may represent the base to study the relevant "in service" properties of real rubber compounds.

  15. Dynamically vulcanized biobased polylactide/natural rubber blend material with continuous cross-linked rubber phase.

    Science.gov (United States)

    Chen, Yukun; Yuan, Daosheng; Xu, Chuanhui

    2014-03-26

    We prepared a biobased material, dynamically vulcanized polylactide (PLA)/natural rubber (NR) blend in which the cross-linked NR phase owned a continuous network-like dispersion. This finding breaks the traditional concept of a sea-island morphology formed after dynamic vulcanization of the blends. The scan electron microscopy and dissolution/swell experiments provided the direct proof of the continuous cross-linked NR phase. This new biobased PLA/NR blend material with the novel structure is reported for the first time in the field of dynamic vulcanization and shows promise for development for various functional applications.

  16. The unique processing of rubber-insulated wires by radiation

    Science.gov (United States)

    Ishitani, Hayao; Saito, Eisuke; Sasaki, Yasushi

    Ethylene-propylene rubbers are able to be crosslinked (vulcanized) by high energy radiation. The radiation-induced crosslinking of ethylene-propylene copolymer or ethylene-propylene-diene terpolymer depends upon the ethylene/propylene ratio, the molecular weight of the polymer, the unsaturating degree of terpolymer and kinds of tercomponents. The mechanical properties of the crosslinked rubber were affected mainly by the E/P ratio and the molecular weight, and improved by blending of low density polyethylene or ethylene-vinylacetate copolymer. Aging of the rubber, due to kinds and contents of tercomponents, was mostly determined by addition of antioxidants to the compound. We developed EP rubber compounds for wire insulation crosslinked by electron beam radiation and applied to the insulation cores of the ship's cables, in the place of the wire vulcanized conventionally by the pressurized steam in the continuous vulcanizer. The rubber compounds are consisted of ethylene-propylene-diene terpolymer with high ethylene contents, ethylene-vinylacetate copolymer and antioxidants. The high-ethylene polymers are supplied in the shape of pellets, and antioxidants were added to the compounds by means of dry blending of concentrates in which antioxidants are mixed into pellets of ethylene copolymer. The EP rubbers were covered on the copper wire by the extruder, used to plastic material, and irradiated with the electron beam from an accelerator. These insulated cores manufactured on radiation processing had the excellent properties, particularly aging and electrical properties. Further, they are more simply colored. Therefore, they will be considered to be used to other applications. This method of manufacturing of the rubber-insulated wires made it possible to reduce both the material costs by simple compounding and the operating costs by radiation-induced crosslinking, to compare with the conventional compounding and vulcanizing process, in which the materials are

  17. Interaction of Chloroprene and Nitrile- Butadiene Rubber with Lubricating Greases and Base Oils

    Institute of Scientific and Technical Information of China (English)

    2006-01-01

    The present communication addresses compatibility of two synthetic rubber types, chloroprene and nitrilebutadiene ones, with a number of base oils of petroleum origin and lubricating greases produced thereof. Four base oils,including three naphthenic products with varying degrees of refining and one paraffinic product,were compared with each other in terms of their effect on the rubbers. Degenerative changes occurring in the rubbers on contact with the oils and greases were studied using accelerated ageing tests. Alterations in rubber parameters, such as hardness, weight and glass transition temperature, caused by interaction with oil were monitored. The main physicochemical mechanisms standing behind the changes observed in the rubber properties were found to be (i) migration of plasticizer from rubber into the oil phase, (ii) absorption of oil by rubber,and (iii) oxidation of rubber. An increase in glass transition temperature (Tg) of rubber aged in a base oil or grease was considered as an indirect indication that the plasticizer had migrated out of rubber;the plasticizer accumulation in the oil phase being directly confirmed by gas chromatography. In order to suppress the plasticizer migration, oil additivation with dioctyl adipate (DOA), a common plasticizer used in rubber formulations, was attempted. However, the BOA-additivated oils, while reducing plasticizer migration, were found to cause more swelling than the original oils in the case of chloroprene rubber. As an alternative, replacement of BOA by an alkylated aryl phosphate in nitrile- butadiene rubber formulations was considered, but it did not solve the problem either.The results of this study suggest conclusively that the type of rubber, the plasticizer, and the base oil are all the crucial parameters that should be considered when matching rubber with oil in real- life applications. Interaction of rubber with base oils and with greases produced thereof is largely controlled by (i) solvency of the

  18. Random parking, Euclidean functionals, and rubber elasticity

    CERN Document Server

    Gloria, Antoine

    2012-01-01

    We study subadditive functions of the random parking model previously analyzed by the second author. In particular, we consider local functions $S$ of subsets of $\\mathbb{R}^d$ and of point sets that are (almost) subadditive in their first variable. Denoting by $\\xi$ the random parking measure in $\\mathbb{R}^d$, and by $\\xi^R$ the random parking measure in the cube $Q_R=(-R,R)^d$, we show, under some natural assumptions on $S$, that there exists a constant $\\bar{S}\\in \\mathbb{R}$ such that % $$ \\lim_{R\\to +\\infty} \\frac{S(Q_R,\\xi)}{|Q_R|}\\,=\\,\\lim_{R\\to +\\infty}\\frac{S(Q_R,\\xi^R)}{|Q_R|}\\,=\\,\\bar{S} $$ % almost surely. If $\\zeta \\mapsto S(Q_R,\\zeta)$ is the counting measure of $\\zeta$ in $Q_R$, then we retrieve the result by the second author on the existence of the jamming limit. The present work generalizes this result to a wide class of (almost) subadditive functions. In particular, classical Euclidean optimization problems as well as the discrete model for rubber previously studied by Alicandro, Cicalese,...

  19. Oil Gels Based on Styrene Butadiene Rubber

    Institute of Scientific and Technical Information of China (English)

    ZHOU Mei-hua (周美华); XU Jing-bo(徐静波); Won-jei CHO

    2004-01-01

    Four oil absorbents based on styrene butadiene (SBR),i. e., pure SBR (PS), 4- tert-butylstyrene-SBR (PBS),EPDM-SBR network (PES) and 4-tert-butylstyrene-EPDMSBR ( PBES ), were produced from crosslinking polymerization of uncured styrene butadiene rubber (SBR),4- tert-butylstyrene ( tBS ) and ethylene-propylene-diene terpolymer (EPDM). The reaction took place in toluene using benzoyl peroxide (BPO) as an initiator. Uncured SBR was used as both a pre-polymer and a crosslink agent in this work, and the crosslinked polymer was identified by IR spectroscopy. The oil absorbency of the crosslinked polymer was evaluated with the method ASTM (F726 - 81). The order of maximum oil absorbency was PBES > PBS >PES > PS. The maximum values of oil absorbency of PBES and PBS were 74.0g/g and 69.5g/g, respectively. Gel fractions and swelling kinetic constants, however, had the opposite sequences. The swelling kinetic constant of PS evaluated by an experimental equation was 49. 97 ×10-2h-1.

  20. About the cure kinetics in natural rubber/styrene Butadiene rubber blends at 433 K

    Science.gov (United States)

    Mansilla, M. A.; Marzocca, A. J.

    2012-08-01

    Vulcanized blends of elastomers are employed in several goods mainly to improve physical properties and reduce costs. One of the most used blends of this kind is that composed by natural rubber (NR) and styrene butadiene rubber (SBR). The cure kinetic of these blends depends mainly on the compound formulation and the cure temperature and time. The preparation method of the blends can influence the mechanical properties of the vulcanized compounds. In this work the cure kinetic at 433 K of NR/SBR blends vulcanized with the system sulfur/TBBS (N-t-butyl-2-benzothiazole sulfenamide) is analyzed in samples prepared by mechanical mixing and solution blending. The two methods produce elastomer domains of NR and SBR, which present different microstructure due to the cure level attained during vulcanization. The cure kinetics is studied by means of rheometer tests and the model proposed by Kamal and Sourour. The analysis of the cure rate is presented and is related to the structure obtained during the vulcanization process.

  1. About the cure kinetics in natural rubber/styrene Butadiene rubber blends at 433 K

    Energy Technology Data Exchange (ETDEWEB)

    Mansilla, M.A., E-mail: mmansilla@df.uba.ar [Laboratorio de Polimeros y Materiales Compuestos, Departamento de Fisica, Facultad de Ciencias Exactas y Naturales, Universidad de Buenos Aires, Ciudad Universitaria, Pabellon 1, C1428EGA Buenos Aires (Argentina); Marzocca, A.J. [Laboratorio de Polimeros y Materiales Compuestos, Departamento de Fisica, Facultad de Ciencias Exactas y Naturales, Universidad de Buenos Aires, Ciudad Universitaria, Pabellon 1, C1428EGA Buenos Aires (Argentina)

    2012-08-15

    Vulcanized blends of elastomers are employed in several goods mainly to improve physical properties and reduce costs. One of the most used blends of this kind is that composed by natural rubber (NR) and styrene butadiene rubber (SBR). The cure kinetic of these blends depends mainly on the compound formulation and the cure temperature and time. The preparation method of the blends can influence the mechanical properties of the vulcanized compounds. In this work the cure kinetic at 433 K of NR/SBR blends vulcanized with the system sulfur/TBBS (N-t-butyl-2-benzothiazole sulfenamide) is analyzed in samples prepared by mechanical mixing and solution blending. The two methods produce elastomer domains of NR and SBR, which present different microstructure due to the cure level attained during vulcanization. The cure kinetics is studied by means of rheometer tests and the model proposed by Kamal and Sourour. The analysis of the cure rate is presented and is related to the structure obtained during the vulcanization process.

  2. DEPENDENCE OF DAMPING CHARACTERISTICS OF A BEAM WITH DAMPING RUBBER MAGNETIC POWDER ON RUBBER PROPERTY

    Institute of Scientific and Technical Information of China (English)

    Ming Li; Zeng He; Huiming Zheng; Ning Zhang

    2008-01-01

    A cantilever beam with Damping Material Applying Rubber Magnetic Powder (DRM)has been investigated.Two methods are selected to hold DRM to a vibrating steel beam,one is to attach DRM by the magnetic attractive force (called DRM beam) and the other by adhesive bonding (called AB-DRM beam).Different from the damping property of AB-DRM beam caused by shear deformation of damping material,the damping property of DRM beam is characterized by the sliding frictional loss together with the internal loss of damping material.The authors established a formulation to predict the damping characteristics of DRM beam,which was validated experimentally.It is found that rubber material loss factor/β has a decisive influence on damping improvement of DRM beam versus AB-DRM beam.If/β is smaller than the critical value around 0.8255,a valid range of vibratory amplitude always exists in which DRM beam can achieve better damping than AB-DRM beam;conversely,if/β is bigger than the critical value,the valid range does not exist when slide occurs.Such results are used to determine the merits and limitations of DRM and develop design guidelines.

  3. Some Tribological Characterization of “EPDM” Rubber

    Directory of Open Access Journals (Sweden)

    A. Mukhopadhyay

    2014-06-01

    Full Text Available Ethylene Propylene Diene Monomer (EPDM rubber emerges as a dominant elastomer for major engineering applications. The major properties of EPDM are its outstanding heat, ozone and weather resistance ability. It has a good resistance to polar substances and steam condition too. In automobiles EPDM rubber has a common use as seals. This includes door seals, window seals, trunk seals and sometimes hood seals. Frequently these seals are the source of noise due to the movement of the door versus the car body. This is due to friction between the EPDM rubber parts and the mating surfaces. Thus, the contact iteration between the rubber sealing and the indenting object must be known to optimize the performance of rubber sealing. However, it is need less to mention that the behaviour of any viscoelastic material is very difficult to be predicted. In the present work various tribo-characteristics of EPDM rubber of different hardness have been evaluated utilizing the available laboratory test facilities in the Jadavpur University, Kolkata, India. Compression tests have been carried out using ‘Instron’ to determine the flow behaviour of EPDM rubber of different hardness both in dry as well as under different conditions of lubrication. The flow behaviour like load -vs.- elongation curves, true stress -vs.- elongation curves and true stress -vs.- true strain curves have been drawn from the experimental data. Abrasive wear behaviour has been evaluated using a two-body abrasion tester and the pattern abrasion has been appraised through SEM/EDAX study. Experimental results reveal that the hardness of EPDM rubber has significant effect on the flow behaviour and wear characteristics. The hardness, again, depends on the proportion of carbon black (CB content. Thus it can be stated that the flow behaviour can be governed by controlling the CB concentration in the EPDM rubber. Based on the experimental results conclusion has been drawn accordingly. Some of the

  4. VARIATION OF PHYSICO-CHEMICAL PROPERTIES OF RADIATION CROSSLINKED RUBBER WITH STORAGE TIME

    Institute of Scientific and Technical Information of China (English)

    N.C. Dafader; M.E. Haque; F. Akhtar

    2005-01-01

    The effect of storage on physico-chemical properties of non-irradiated natural rubber and radiation vulcanized natural rubber (RVNR) were evaluated. The rubber films were stored under two different conditions, namely in open air and sealed polyethylene bags. The antioxidant, tris(nonylated phenyl) phosphite (TNPP) was used for preventing degradation of RVNR films. Gel content, cross-link density, tensile strength at break and 500% elongation of rubber films were measured.The results show that the retention (%) of tensile properties of rubber films with TNPP is higher than that of rubber films without antioxidants. The rubber films stored in polyethylene bags also show better retention of tensile properties than those of rubber films stored in open air.

  5. Influence of Ultrasonic Vibrations on the Static Friction Characteristics of a Rubber/Aluminum Couple

    Institute of Scientific and Technical Information of China (English)

    程廷海; 高焓; 包钢

    2011-01-01

    A novel ultrasonic vibration approach is introduced into a chloroprene rubber/aluminum friction couple for improving the static friction properties betwesn rubber and metal.Compared to the test results without vibrations,the static friction force of a chloroprene rubber/aluminum couple decreases observably,leading to the ultimate displacement of rubber.The values of the static friction force and ultimate displacement can be ultimately reduced to 23.1% and 50% of those without ultrasonic vibrations,respectively.%A novel ultrasonic vibration approach is introduced into a chioroprene rubber/aluminum friction couple for improving the static friction properties between rubber and metal. Compared to the test results without vibrations, the static friction force of a chioroprene rubber/aluminum couple decreases observably, leading to the ultimate displacement of rubber. The values of the static friction force and ultimate displacement can be ultimately reduced to 23.1% and 50% of those without ultrasonic vibrations, respectively.

  6. Caltrans use of scrap tires in asphalt rubber products: a comprehensive review

    National Research Council Canada - National Science Library

    Zhou, Haiping; Holikatti, Sri; Vacura, Peter

    2014-01-01

    ...) and dry processes were used in early trials. Caltrans has also used rubber modified binders containing both crumb rubber modifier and polymer modifier that could be manufactured at a refinery facility, a terminal blend wet process...

  7. Nanolipoprotein particles comprising a natural rubber biosynthetic enzyme complex and related products, methods and systems

    Energy Technology Data Exchange (ETDEWEB)

    Hoeprich, Paul D.; Whalen, Maureen

    2016-04-05

    Provided herein are nanolipoprotein particles that comprise a biosynthetic enzyme more particularly an enzyme capable of catalyzing rubber or other rubbers polymerization, and related assemblies, devices, methods and systems.

  8. Microclimate, development and productivity of robusta coffee shaded by rubber trees and at full sun

    National Research Council Canada - National Science Library

    André Vasconcellos Araújo; Fábio Luiz Partelli; Gleison Oliosi; José Ricardo Macedo Pezzopane

    2016-01-01

      There are few studies about the shading of Robusta coffee with rubber trees. The aim of this study was evaluate the microclimate, development and yield of Coffea canephora grown at full sun and shaded by rubber trees...

  9. Patch testing with rubber series in Europe : a critical review and recommendation

    NARCIS (Netherlands)

    Warburton, Katharine L; Uter, Wolfgang; Geier, Johannes; Spiewak, Radoslaw; Mahler, Vera; Crépy, Marie-Noëlle; Schuttelaar, Marie-Louise; Bauer, Andrea; Wilkinson, Mark

    2016-01-01

    BACKGROUND: Rubber additives constitute an important group of contact allergens, particularly in certain occupations. OBJECTIVES: To collect information regarding the current practice of using a 'rubber series' in Europe, and discuss this against the background of evidence concerning the prevalence

  10. Three dimensional base isolation system on laminated thick rubber bearings

    Energy Technology Data Exchange (ETDEWEB)

    Kanazawa, Kenji; Matsuda, Akihiro; Hirata, Kazuta [Central Research Inst. of Electric Power Industry, Abiko, Chiba (Japan). Abiko Research Lab.

    1997-08-01

    In order to reduce horizontal and vertical earthquake response of internal equipments in the nuclear power plants, we evaluated the performance of three dimensional base isolation system using laminated thick rubber bearings. From the loading test of scaled model of laminated thick rubber bearing, it was found that the natural rubber bearing was able to be extended to thick rubber bearings, and the difference of mechanical characteristics was only the dependency of the vertical stiffness on the horizontal displacement. Second, we carried out shaking table test for scaled model of base isolated structure. The results showed that horizontal characteristics of thick rubber bearing was almost the same as the thin one, and the vertical stiffness was able to be determined according to the resonance period of internal equipments. After the test, we carried out the numerical analysis on the shaking table test. Numerical results showed that the response of the model for earthquake input motion and its response spectra were in good agreement with the experiment, and the resonance peak of the floor response spectra can be reduced when the damping coefficient of the vertical damper increases. (author)

  11. Taxonomic revision and phylogenetic analyses of rubber powdery mildew fungi.

    Science.gov (United States)

    Liyanage, K K; Khan, Sehroon; Brooks, Siraprapa; Mortimer, Peter E; Karunarathna, Samantha C; Xu, Jianchu; Hyde, Kevin D

    2017-02-09

    Powdery mildew is a fungal disease that infects a wide range of plants, including rubber trees, which results in a reduction of latex yields of up to 45%. The causal agent of powdery mildew of rubber was first described as Oidium heveae, but later morpho-molecular research suggested that in the past, O. heveae has been confused with Erysiphe quercicola. However, it is still under debate whether the causal agent should be classified as a species of the genus Erysiphe emend. or Golovinomyces and Podosphaera, respectively. Therefore, the aim of this study was to undertake the morpho-molecular characterization of powdery mildew species associated with rubber trees, thus resolving these taxonomic issues. Morphological observation under light and scanning electron microscopes (SEM) clearly identified two morphotypes of the rubber powdery mildew. With the support of morphological and phylogenetic data, one of the two morphotypes was identified as the asexual morph of E. quercicola, while the second morphotype is still insufficiently known and according to the morphological results obtained we assume that it might belong to the genus Golovinomyces. More collections and additional molecular data are required for final conclusions regarding the exact taxonomic position of the second morphotype of rubber powdery mildew and its relation to the name O. heveae. The haplotype analysis identified eight haplotype groups of E. quercicola indicating the high genetic diversity of the species.

  12. Tensile Strength of PHBV/Natural Rubber Latex Mixtures

    Directory of Open Access Journals (Sweden)

    Promkotra Sarunya

    2015-01-01

    Full Text Available A polyhydroxybutyrate-co-hydroxyvalerate (PHBV is mingled with natural rubber latex (R to develop its mechanical property of the blend. Normally, substantial effects of the PHBV are hard, fragile, and inelastic, whereas the natural rubber is represented itself as very high elastic matter. The mixtures between the PHBV and natural rubber latex (R are considered in different proportions. The PHBV solutions (w/v are defined suitability at 1% (P1, 2% (P2, and 3% (P3. Their liquid mixtures of the PHBV to natural rubber latex (P:R are fabricated the blended films in three different ratios of 2:3, 1:1 and 3:2, respectively. The PHBV blended films are characterized the crystallinity form by x-ray diffractometry (XRD, which are appeared their identity crystals at 13.30 and 16.68 degree (2θ. Mechanical characterizations of the blends are examined by a universal testing machine (UTM. The average elastic moduli of P1, P2, and P3 mixtures are indicated as 773, 955, and 1,007 kPa, respectively. Their tensile strengths, similarly to elastic moduli, enhance with the PHBV concentrations. The effects of mechanical behaviors and crystallinity reveal that the PHBV blends can be improved their properties by more flexible with natural rubber latex.

  13. Relaxation phenomena in rubber/layered silicate nanocomposites

    Directory of Open Access Journals (Sweden)

    2007-12-01

    Full Text Available Broadband Dielectric Spectroscopy (BDS is employed in order to investigate relaxation phenomena occurring in natural rubber (NR, polyurethane rubber (PUR and PUR/NR blend based nanocomposites, reinforced by 10 parts per hundred (phr Layered Silicates (LS. Nanocomposites and matrices were examined under identical conditions in a wide frequency (10–1 to 106 Hz and temperature (–100 to 50°C range. Experimental data are analyzed in terms of electric modulus formalism. The recorded relaxation phenomena include contributions from both the polymer matrices and the nanofiller. Natural rubber is a non-polar material and its performance is only slightly affected by the presence of layered silicates. Polyurethane rubber exhibits four distinct relaxation processes attributed, with ascending relaxation rate, to Interfacial Polarization (IP, glass/rubber transition (α-mode, local motions of polar side groups and small segments of the polymer chain (β, γ-mode. The same processes have been detected in all systems containing PUR. IP is present in all nanocomposites being the slowest recorded process. Finally, pronounced interfacial relaxation phenomena, occurring in the PUR+10 phr LS spectra, are attributed to nanoscale effects of intercalation and exfoliation.

  14. Mechanochromism of a luminescent natural rubber under tensile deformation

    Science.gov (United States)

    Ha, Jimin; Park, Minwook; Jeong, Kwang-Un; Nah, Changwoon

    2016-09-01

    Various examples are reported of chromogenic materials composed of a functional dye covalently linked to the polymer chains or physically dispersed in the continuous macromolecular matrix, the latter appears to be a more sustainable route for the industrial scale-up of these materials. In this study, a mechanochromic elastomer was prepared by physically dispersing dye materials into a rubber matrix by solution mixing technique. The employed rubber is natural rubber (NR). The NR was chosen because of its ability of strain-induced crystallization. Perylene diimide I is selected after considering its aggregachromic nature and affinity with rubber matrix. The optimum composition of dye in rubber composites was determined based on the mechanochromic performance characterized with ultraviolet/visible (UV/Vis) spectrometer, x-ray diffraction (XRD) and spectrofluorometer (FL). The UV/Vis spectrometer and FL monitor the optical responses, such as absorbance and emission property, under tensile deformation due to the breakage of dye aggregates. Spectroscopic analysis with polarization monitors the breakage of dye aggregates and anisotropic property of the sample. The XRD monitors the change in size of dye aggregates. With polarization filtering, the breakage of dye aggregates are clearly observed and anisotropic property of the sample is also confirmed. The XRD results indicate that dye aggregates were broken during stretching because the shear force is applied to dye aggregates.

  15. No pain relief with the rubber hand illusion.

    Directory of Open Access Journals (Sweden)

    Rahul Mohan

    Full Text Available The sense of body ownership can be easily disrupted during illusions and the most common illusion is the rubber hand illusion. An idea that is rapidly gaining popularity in clinical pain medicine is that body ownership illusions can be used to modify pathological pain sensations and induce analgesia. However, this idea has not been empirically evaluated. Two separate research laboratories undertook independent randomized repeated measures experiments, both designed to detect an effect of the rubber hand illusion on experimentally induced hand pain. In Experiment 1, 16 healthy volunteers rated the pain evoked by noxious heat stimuli (5 s duration; interstimulus interval 25 s of set temperatures (47°, 48° and 49°C during the rubber hand illusion or during a control condition. There was a main effect of stimulus temperature on pain ratings, but no main effect of condition (p = 0.32, nor a condition x temperature interaction (p = 0.31. In Experiment 2, 20 healthy volunteers underwent quantitative sensory testing to determine heat and cold pain thresholds during the rubber hand illusion or during a control condition. Secondary analyses involved heat and cold detection thresholds and paradoxical heat sensations. Again, there was no main effect of condition on heat pain threshold (p = 0.17, nor on cold pain threshold (p = 0.65, nor on any of the secondary measures (p<0.56 for all. We conclude that the rubber hand illusion does not induce analgesia.

  16. Natural Rubber Nanocomposite with Human-Tissue-Like Mechanical Characteristic

    Science.gov (United States)

    Murniati, Riri; Novita, Nanda; Sutisna; Wibowo, Edy; Iskandar, Ferry; Abdullah, Mikrajuddin

    2017-07-01

    The blends of synthetic rubber and natural rubber with nanosilica were prepared using a blending technique in presence of different filler volume fraction. The effect of filler on morphological and mechanical characteristics was studied. Utilization of human cadaver in means of medical study has been commonly used primarily as tools of medical teaching and training such as surgery. Nonetheless, human cadaver brought inevitable problems. So it is necessary to find a substitute material that can be used to replace cadavers. In orthopaedics, the materials that resemble in mechanical properties to biological tissues are elastomers such as natural rubber (latex) and synthetic rubber (polyurethanes, silicones). This substitution material needs to consider the potential of Indonesia to help the development of the nation. Indonesia is the second largest country producer of natural rubber in the world. This paper aims to contribute to adjusting the mechanical properties of tissue-mimicking materials (TMMs) to the recommended range of biological tissue value and thus allow the development of phantoms with greater stability and similarity to human tissues. Repeatability for the phantom fabrication process was also explored. Characteristics were then compared to the control and mechanical characteristics of different human body part tissue. Nanosilica is the best filler to produce the best nanocomposite similarities with human tissue. We produced composites that approaching the properties of human internal tissues.

  17. EVALUATION OF TIRE RUBBER DISPOSAL IN CONCRETE FOR PAVEMENTS

    Directory of Open Access Journals (Sweden)

    Rosa Cristina Cecche Lintz

    2009-12-01

    Full Text Available The production of waste by the tire industry has been a growing problem, indicating the need for its reuse. More than thirty million tires are discharged per year in Brazil, where regulation for the environment states that for each four new tires, five unusable ones must be adequately disposed by manufacturers and importers. Paving consumes an extremely large quantity of materials, which can be the source of rational application of waste and rejected materials. Research shows that tire rubber can be added to asphalt, which increases its durability and improves pavement quality and safety conditions by absorbing the rubber elastic properties, and also be used for architectural applications, among others. This study deals with the addition of rubber fibers from tire crushing in concrete for roadway pavements in order to provide proper indication about the alternative material disposal through an evaluation of the mechanical behavior of the modified concrete. Different concrete mixes were produced, within which, part of fine aggregates were substituted by tire rubber and mechanical experiment tests were performed, which show that, due to great resistance losses, the disposal of this alternative material in concrete should be considered for light traffic pavements, with the addition of rubber ranging up to 10% in mass.

  18. EVALUATION OF TIRE RUBBER DISPOSAL IN CONCRETE FOR PAVEMENTS

    Directory of Open Access Journals (Sweden)

    Rosa Cristina Cecche Lintz

    2009-01-01

    Full Text Available The production of waste by the tire industry has been a growing problem, indicating the need for its reuse. More than thirty million tires are discharged per year in Brazil, where regulation for the environment states that for each four new tires, five unusable ones must be adequately disposed by manufacturers and importers. Paving consumes an extremely large quantity of materials, which can be the source of rational application of waste and rejected materials. Research shows that tire rubber can be added to asphalt, which increases its durability and improves pavement quality and safety conditions by absorbing the rubber elastic properties, and also be used for architectural applications, among others. This study deals with the addition of rubber fibers from tire crushing in concrete for roadway pavements in order to provide proper indication about the alternative material disposal through an evaluation of the mechanical behavior of the modified concrete. Different concrete mixes were produced, within which, part of fine aggregates were substituted by tire rubber and mechanical experiment tests were performed, which show that, due to great resistance losses, the disposal of this alternative material in concrete should be considered for light traffic pavements, with the addition of rubber ranging up to 10% in mass.

  19. China Rubber Chemicals Production and Market Situation Analysis

    Institute of Scientific and Technical Information of China (English)

    Liang Cheng

    2011-01-01

    Because the stimulus driven impact of the rapid growth of tire and other rubber products' output,in recent years,the production and marketing of domestic rubber chemicals appear to increase,and the specific production and marketing conditions are as follows: 1.Rapid Growth of Chemicals Output From 2009 to 2010,in China an upsurge of expanding or building new rubber chemicals equipment was raised.These equipment were planned to be put into production in 2010 with newly increased production capacity of about 120,000 tons,among which there were 40,000 tons antioxidant 4020,50,000tons accelerator M,and about 40,000 tons other Chemicals.In 2010,the total output was 701,000 tons,with year-on-year growth of 17.8% or so.In 2010,the total sales volume of domestic rubber chemicals were 13 billion yuan,and the export volume was about 180,000 tons,basically the same with that in 2009.See the statistics of domestic rubber chemicals output from 2009 to 2010 in Table 1.

  20. Flashover Characteristics of Silicone Rubber Sheets under Various Environmental Conditions

    Directory of Open Access Journals (Sweden)

    Arshad

    2016-08-01

    Full Text Available Silicone rubber insulators are replacing the conventional ceramic and porcelain insulators rapidly in power transmission and distribution industry. Very limited field knowledge is available about the performance of silicone rubber insulators in polluted and contaminated environments and therefore need further investigation. A comprehensive analysis of silicone rubber sheets (intended for coating outdoor insulators was carried out in this paper based on experimental results. The main performance parameters analyzed were arc inception voltage and flashover voltage. Dependence of these parameters on equivalent salt deposit density (ESDD, non-soluble salt deposit density (NSDD, relative humidity, ambient temperature, fog rate, dry band formation, dry band location and number of dry bands were investigated extensively. Insulator orientation and its effect on performance were also studied. The authors believe that this paper will provide a comprehensive knowledge about the flashover characteristics of silicone rubber insulators under humid, contaminated and dry band conditions. These results could be used in the selection and design of silicone rubber insulators for polluted environments.

  1. Devulcanization of ground tire rubber: Physical and chemical changes after different microwave exposure times

    OpenAIRE

    P. S. Garcia; F. D. B. de Sousa; J.A. Lima; S. A. Cruz; C. H. Scuracchio

    2015-01-01

    Microwave devulcanization is known to be a promising and an efficient rubber recycling method which makes possible for the rubber to regain its fluidity, and makes it capable of being remolded and revulcanized. The focus of this work is to understand the physical and chemical changes that occur in the ground tire rubber after different microwave exposure periods. For this purpose chemical, thermal, rheological and morphological analyses were performed on the tire rubber, which contains natura...

  2. Optimisation of rubberised concrete with high rubber content: an experimental investigation

    OpenAIRE

    Raffoul, S.; Garcia, R; Pilakoutas, K.; Guadagnini, M.; Flores Medina, N.

    2016-01-01

    This article investigates experimentally the behaviour of rubberised concrete (RuC) with high rubber content so as to fully utilise the mechanical properties of vulcanised rubber. The fresh properties and short-term uniaxial compressive strength of 40 rubberised concrete mixes were assessed. The parameters examined included the volume (0–100%) and type of mineral aggregate replacement (fine or coarse), water or admixture contents, type of binder, rubber particle properties, and rubber surface...

  3. Strength and deformability of waste tyre rubber-filled reinforced concrete columns

    OpenAIRE

    Son, K.S.; Hajirasouliha, I.; Pilakoutas, K.

    2011-01-01

    This study aims to investigate the efficiency of waste tyre rubber-filled concrete to improve the deformability and energy absorption capacity of RC columns by considering different concrete compressive strength, size of waste tyre rubber particles and rubber content. Twelve column specimens were tested using concrete of compressive strength 24 and 28 MPa mixed with 0.6 and 1 mm tyre rubber particles. For each concrete batch, 27 control specimens were prepared to examine the concrete properti...

  4. A study on nonlinear finite element analysis of laminated rubber bearings. Pt.1. Development of evaluation method for mechanical properties of laminated rubber bearings for horizontal base isolation system considering volumetric deformation of rubber material

    Energy Technology Data Exchange (ETDEWEB)

    Matsuda, Akihiro; Ohtori, Yasuki; Yabana, Shuichi; Hirata, Kazuta [Central Research Inst. of Electric Power Industry, Abiko, Chiba (Japan). Abiko Research Lab

    1999-04-01

    The purpose of this research is to develop the evaluation method for mechanical properties of laminated rubber bearings by nonlinear finite element method (FEM) considering the volumetric deformation of natural rubber material. Relationship between pressure and volumetric strain of the natural rubber is obtained from the volumetric tests and is introduced into user-subroutine of the FEM code (ABAQUS). Finite element analyses of natural rubber bearings (NRB) and the natural rubber bearing with lead plug (LRB) are carried out. The results may be summarized as follows; 1) Horizontal, vertical stiffness and effect of shear deformation on vertical stiffness of natural rubber bearings that have various shape are simulated with enough accuracy. 2) Horizontal and vertical stiffness of LRB are also simulated well. (author)

  5. Influence of Rubber Concentration on Angular deformation in Injection Molded Parts of Talc and Rubber Filled Polypropylene

    Science.gov (United States)

    Takahara, Tadayoshi; Koyama, Kiyohito

    The most popular resin material for automotive plastic parts is polypropylene, which includes talc for stiffness and heat-resistance and rubber for impact-resistance. The anisotropic thermal expansion coefficient is well documented for talc reinforced polypropylene, but there are very few technical papers for warpage. Therefore, using this kind of material and molding with an L-shaped cross section, the influence of rubber concentration on corner deformation was discussed in this study. The results of this study are as follows 1) L-shaped cross section specimens show that the corner deformation increases linearly in proportion to the increase of rubber concentration. 2) Plane shape specimens show that the shrinkage rates in the planar direction decrease linearly and the shrinkage rates in the thickness direction increase linearly. 3) The strains in each rubber concentration are calculated using Hooke's Law. This force that induces corner deformation is assumed as the shrinkage difference between the planar and thickness directions. The tendencies of calculated strains are qualitatively consistent with measured corner deformations. 4) The reason why corner deformation decreases linearly to rubber concentration is due to the fact that the shrinkage difference between the planar and thickness directions increases and the fact that the flexural modulus decreases linearly.

  6. Biorefinery methods for separation of protein and oil fractions from rubber seed kernel

    NARCIS (Netherlands)

    Widyarani, R.; Ratnaningsih, E.; Sanders, J.P.M.; Bruins, M.E.

    2014-01-01

    Biorefinery of rubber seeds can generate additional income for farmers, who already grow rubber trees for latex production. The aim of this study was to find the best method for protein and oil production from rubber seed kernel, with focus on protein recovery. Different pre-treatments and oil separ

  7. Studies on ethylene-propylene-diene rubber modification by N-chlorothio-N-butyl-benzenesulfonamide

    NARCIS (Netherlands)

    Zhang, Hongmei; Datta, Rabin; Talma, Auke; Noordermeer, Jacobus W.M.

    2009-01-01

    N-Chlorothiosulfonamides have been used to modify ethylene-propylene-diene rubber (EPDM) to enhance the compatibility of EPDM in, e.g., natural rubber (NR)/butadiene rubber (BR)/EPDM blends for ozone resistance. N-Chlorothio-N-butyl-benzenesulfonamide (CTBBS) was selected as a representative for

  8. Impact behaviour of nylon-rubber blends: 6. Influence of structure on voiding processes; toughening mechanism

    NARCIS (Netherlands)

    Borggreve, R.J.M.; Gaymans, R.J.; Eichenwald, H.M.

    1989-01-01

    Dilatometry tests were performed on nylon-rubber blends with various rubber concentrations, particle sizes and types of impact modifier. Whereas rubber concentration and particle size do not affect the onset of voiding in the blends during a tensile test, the type of elastomer used has a considerabl

  9. Impact behaviour of nylon-rubber blends: 6. Influence of structure on voiding processes; toughening mechanism

    NARCIS (Netherlands)

    Borggreve, R.J.M.; Gaymans, R.J.; Eichenwald, H.M.

    1989-01-01

    Dilatometry tests were performed on nylon-rubber blends with various rubber concentrations, particle sizes and types of impact modifier. Whereas rubber concentration and particle size do not affect the onset of voiding in the blends during a tensile test, the type of elastomer used has a

  10. Modulus enhancement of natural rubber through the dispersion size reduction of protein/fiber aggregates

    Science.gov (United States)

    Improved mechanical properties of natural rubber are required for various rubber applications. Aggregates of protein and fiber that constitute soy protein concentrate were shear-reduced and used to enhance the tensile modulus of natural rubber. The aqueous dispersion of the shear-reduced aggregates ...

  11. 75 FR 7586 - Baled Natural Rubber in Tires; TSCA Section 21 Petition; Agency Response

    Science.gov (United States)

    2010-02-22

    ... AGENCY Baled Natural Rubber in Tires; TSCA Section 21 Petition; Agency Response AGENCY: Environmental... prohibiting the use and distribution in commerce of Hevea brasiliensis baled natural-rubber for the... tire ] manufacturers to use Hevea brasiliensis baled natural-rubber that satisfies ASTM...

  12. Toughness of natural rubber composites reinforced with hydrolyzed and modified wheat gluten aggregates

    Science.gov (United States)

    The toughness of natural rubber can be improved by using fillers for various rubber applications. Dry wheat gluten is a protein from wheat flour and is sufficiently rigid for rubber reinforcement. The wheat gluten was hydrolyzed to reduce its particle size and microfluidized to reduce and homogenize...

  13. Morphology of Silica-Reinforced Natural Rubber: Effect of Silane Coupling Agent

    NARCIS (Netherlands)

    Sarkawi, S.S.; Dierkes, W.K.; Noordermeer, J.W.M.

    2015-01-01

    A good dispersion of silica in a rubber vulcanizate is important as it influences the filler-to-rubber interaction and consequently the final properties. This article presents an investigation into the morphology of silica-reinforced natural rubber (NR) in the presence and absence of a silane coupli

  14. 21 CFR 177.1480 - Nitrile rubber modified acrylonitrile-methyl acrylate copolymers.

    Science.gov (United States)

    2010-04-01

    ... 21 Food and Drugs 3 2010-04-01 2009-04-01 true Nitrile rubber modified acrylonitrile-methyl... Nitrile rubber modified acrylonitrile-methyl acrylate copolymers. Nitrile rubber modified acrylonitrile... this chapter, subject to the provisions of this section. (a) For the purpose of this section, nitrile...

  15. 78 FR 58520 - Extruded Rubber Thread From Malaysia; Notice of Amended Final Results of Antidumping Duty...

    Science.gov (United States)

    2013-09-24

    ... unliquidated entries of certain extruded rubber thread from Malaysia produced and/or exported by Heveafil, and... International Trade Administration Extruded Rubber Thread From Malaysia; Notice of Amended Final Results of... review of the antidumping duty order on extruded rubber thread from Malaysia.\\1\\ The period of review...

  16. Experimental Investigation of the Mechanical and Durability Properties of Crumb Rubber Concrete

    Science.gov (United States)

    Liu, Hanbing; Wang, Xianqiang; Jiao, Yubo; Sha, Tao

    2016-01-01

    Recycling waste tire rubber by incorporating it into concrete has become the preferred solution to dispose of waste tires. In this study, the effect of the volume content of crumb rubber and pretreatment methods on the performances of concrete was evaluated. Firstly, the fine aggregate and mixture were partly replaced by crumb rubber to produce crumb rubber concrete. Secondly, the mechanical and durability properties of crumb rubber concrete with different replacement forms and volume contents had been investigated. Finally, the crumb rubber after pretreatment by six modifiers was introduced into the concrete mixture. Corresponding tests were conducted to verify the effectiveness of pretreatment methods as compared to the concrete containing untreated crumb rubber. It was observed that the mechanical strength of crumb rubber concrete was reduced, while durability was improved with the increasing of crumb rubber content. 20% replacement of fine aggregate and 5% replacement of the total mixture exhibited acceptable properties for practical applications. In addition, the results indicated that the modifiers had a positive impact on the mechanical and durability properties of crumb rubber concrete. It avoided the disadvantage of crumb rubber concrete having lower strength and provides a reference for the production of modified crumb rubber concrete. PMID:28773298

  17. 26 CFR 48.4073-3 - Exemption of tread rubber used for recapping nonhighway tires.

    Science.gov (United States)

    2010-04-01

    ... nonhighway tires. 48.4073-3 Section 48.4073-3 Internal Revenue INTERNAL REVENUE SERVICE, DEPARTMENT OF THE..., Tires, Tubes, Tread Rubber, and Taxable Fuel Tires, Tubes, and Tread Rubber § 48.4073-3 Exemption of tread rubber used for recapping nonhighway tires. (a) Sold direct by manufacturer for nontaxable...

  18. Experimental Investigation of the Mechanical and Durability Properties of Crumb Rubber Concrete

    Directory of Open Access Journals (Sweden)

    Hanbing Liu

    2016-03-01

    Full Text Available Recycling waste tire rubber by incorporating it into concrete has become the preferred solution to dispose of waste tires. In this study, the effect of the volume content of crumb rubber and pretreatment methods on the performances of concrete was evaluated. Firstly, the fine aggregate and mixture were partly replaced by crumb rubber to produce crumb rubber concrete. Secondly, the mechanical and durability properties of crumb rubber concrete with different replacement forms and volume contents had been investigated. Finally, the crumb rubber after pretreatment by six modifiers was introduced into the concrete mixture. Corresponding tests were conducted to verify the effectiveness of pretreatment methods as compared to the concrete containing untreated crumb rubber. It was observed that the mechanical strength of crumb rubber concrete was reduced, while durability was improved with the increasing of crumb rubber content. 20% replacement of fine aggregate and 5% replacement of the total mixture exhibited acceptable properties for practical applications. In addition, the results indicated that the modifiers had a positive impact on the mechanical and durability properties of crumb rubber concrete. It avoided the disadvantage of crumb rubber concrete having lower strength and provides a reference for the production of modified crumb rubber concrete.

  19. Experimental Investigation of the Mechanical and Durability Properties of Crumb Rubber Concrete.

    Science.gov (United States)

    Liu, Hanbing; Wang, Xianqiang; Jiao, Yubo; Sha, Tao

    2016-03-07

    Recycling waste tire rubber by incorporating it into concrete has become the preferred solution to dispose of waste tires. In this study, the effect of the volume content of crumb rubber and pretreatment methods on the performances of concrete was evaluated. Firstly, the fine aggregate and mixture were partly replaced by crumb rubber to produce crumb rubber concrete. Secondly, the mechanical and durability properties of crumb rubber concrete with different replacement forms and volume contents had been investigated. Finally, the crumb rubber after pretreatment by six modifiers was introduced into the concrete mixture. Corresponding tests were conducted to verify the effectiveness of pretreatment methods as compared to the concrete containing untreated crumb rubber. It was observed that the mechanical strength of crumb rubber concrete was reduced, while durability was improved with the increasing of crumb rubber content. 20% replacement of fine aggregate and 5% replacement of the total mixture exhibited acceptable properties for practical applications. In addition, the results indicated that the modifiers had a positive impact on the mechanical and durability properties of crumb rubber concrete. It avoided the disadvantage of crumb rubber concrete having lower strength and provides a reference for the production of modified crumb rubber concrete.

  20. Breakthroughs of Low-temperature Direct Rubber Mixing in Low-carbon Technology

    Institute of Scientific and Technical Information of China (English)

    2011-01-01

    Rubber mixing is the most energy-consuming procedure in tire production, covering about 40% energy of the whole tire producing workflow. The process of low temperature direct rubber mixing, developed by Triangle Group Co., Ltd., MESNAC Co., Ltd., Yiyang Rubber and Plastics Co., Ltd., TTA (Qingdao) Tire Technology Co., Ltd., Guangzhou SCUT Bestry Technology Co., Ltd., etc.

  1. Occupational vitiligo due to unsuspected presence of phenolic antioxidant byproducts in commercial bulk rubber

    Energy Technology Data Exchange (ETDEWEB)

    O' Malley, M.A.; Mathias, C.G.; Priddy, M.; Molina, D.; Grote, A.A.; Halperin, W.E.

    1988-06-01

    We investigated the occurrence of cutaneous depigmentation (vitiligo) among employees of a company that manufactured hydraulic pumps. The interiors of these pumps were injection-molded with rubber. We identified a small but significant cluster of vitiligo cases among a group of employees who frequently handled the rubber used in this injection molding process. Although none of the additives specified in the rubber formulations was a phenolic or catecholic derivative, known to be potential causes of chemically induced vitiligo, gas chromatographic analysis identified a para-substituted phenol (2,4-di-tert-butylphenol, DTBP) in solid samples of the most frequently used rubber. Surface wipe analysis confirmed that workers could be exposed to DTBP from simple handling of the rubber. We subsequently established that the solid bulk rubber used as the base in these stock rubber formulations contained both DTBP and smaller quantities of p-tert-butylphenol. Both had formed as unsuspected byproducts during chemical synthesis of two antioxidants added to the solid bulk rubber by a major rubber supplier. We conclude that the unsuspected presence of potential chemical depigmenting agents in solid bulk rubber, from which industrial rubber products are formulated, may contribute to the occurrence of occupational vitiligo, and that a simple review of ingredients in rubber formulations is inadequate to detect their presence.

  2. 77 FR 2775 - Goodyear Tire and Rubber Company, Grant of Petition for Decision of Inconsequential Noncompliance

    Science.gov (United States)

    2012-01-19

    ... National Highway Traffic Safety Administration Goodyear Tire and Rubber Company, Grant of Petition for.... ACTION: Notice of Petition Grant. SUMMARY: Goodyear Tire and Rubber Company,(Goodyear),\\1\\ has determined... Responsibility and Reports (dated December 16, 2010). \\1\\ Goodyear Tire and Rubber Company (Goodyear) is...

  3. 76 FR 15045 - Goodyear Tire and Rubber Company, Receipt of Petition for Decision of Inconsequential Noncompliance

    Science.gov (United States)

    2011-03-18

    ... TRANSPORTATION National Highway Traffic Safety Administration Goodyear Tire and Rubber Company, Receipt of Petition for Decision of Inconsequential Noncompliance Goodyear Tire and Rubber Company, (Goodyear),\\1\\ has... Responsibility and Reports, dated December 16, 2010. \\1\\ Goodyear Tire and Rubber Company (Goodyear) is...

  4. 40 CFR 428.80 - Applicability; description of the wet digestion reclaimed rubber subcategory.

    Science.gov (United States)

    2010-07-01

    ... digestion reclaimed rubber subcategory. 428.80 Section 428.80 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY (CONTINUED) EFFLUENT GUIDELINES AND STANDARDS RUBBER MANUFACTURING POINT SOURCE CATEGORY Wet Digestion Reclaimed Rubber Subcategory § 428.80 Applicability; description of the wet...

  5. Modelling conditional correlations in the volatility of Asian rubber spot and futures returns

    NARCIS (Netherlands)

    T. Khamkaew (Tanchanok); R. Tansuchat (Roengchai); C-L. Chang (Chia-Lin); M.J. McAleer (Michael)

    2009-01-01

    textabstractAsia is presently the most important market for the production and consumption of natural rubber. World prices of rubber are not only subject to changes in demand, but also to speculation regarding future markets. Japan and Singapore are the major futures markets for rubber, while Thaila

  6. 77 FR 38083 - Certain Rubber Resins and Processes for Manufacturing Same Institution of Investigation Pursuant...

    Science.gov (United States)

    2012-06-26

    ... COMMISSION Certain Rubber Resins and Processes for Manufacturing Same Institution of Investigation Pursuant... rubber resins and processes for manufacturing same by reason of misappropriation of trade secrets, the... importation, and the sale within the United States after importation of certain rubber resins and processes...

  7. Direct molding of pavement tiles made of ground tire rubber

    Science.gov (United States)

    Quadrini, Fabrizio; Gagliardi, Donatella; Tedde, Giovanni Matteo; Santo, Loredana; Musacchi, Ettore

    2016-10-01

    Large rubber products can be molded by using only ground tire rubber (GTR) without any additive or binder due to a new technology called "direct molding". Rubber granules and powders from tire recycling are compression molded at elevated temperatures and pressures. The feasibility of this process was clearly shown in laboratory but the step to the industrial scale was missing. Thanks to an European Project (SMART "Sustainable Molding of Articles from Recycled Tires") this step has been made and some results are reported in this study. The press used for compression molding is described. Some tests were made to measure the energy consumption so as to evaluate costs for production in comparison with conventional technologies for GTR molding (by using binders). Results show that 1 m2 tiles can be easily molded with several thicknesses in a reasonable low time. Energy consumption is higher than conventional technologies but it is lower than the cost for binders.

  8. On the Damping Properties of Modified Ground Rubber Tires

    Institute of Scientific and Technical Information of China (English)

    2002-01-01

    Large amounts of used rubber tires are discarded annually. A long time is neededfor them to degrade naturally. This poses two major problems: environmental pollutionand wastage of valuable rubber. On the other hand, with the harm of vibration and noisewidely recognized, desires to control them intensify. As an important means of vibrationcontrol, viscoelastic damping technology has advanced greatly. The need for cheap andhigh quality viscoelastic damping materials increases rapidly. This paper made a trial touse ground rubber tire (GRT) recovered from old tires to make damping materials. TheGRT is treated specially first. Then it was pressed into slabs and vulcanized. Finally, theproduct was cut into test samples. An Oberst beam was used to determine the loss factor βand storage modulus E. Results show that the damping materials exhibit good damping ability.

  9. Draft genome sequence of the rubber tree Hevea brasiliensis

    Directory of Open Access Journals (Sweden)

    Rahman Ahmad Yamin Abdul

    2013-02-01

    Full Text Available Abstract Background Hevea brasiliensis, a member of the Euphorbiaceae family, is the major commercial source of natural rubber (NR. NR is a latex polymer with high elasticity, flexibility, and resilience that has played a critical role in the world economy since 1876. Results Here, we report the draft genome sequence of H. brasiliensis. The assembly spans ~1.1 Gb of the estimated 2.15 Gb haploid genome. Overall, ~78% of the genome was identified as repetitive DNA. Gene prediction shows 68,955 gene models, of which 12.7% are unique to Hevea. Most of the key genes associated with rubber biosynthesis, rubberwood formation, disease resistance, and allergenicity have been identified. Conclusions The knowledge gained from this genome sequence will aid in the future development of high-yielding clones to keep up with the ever increasing need for natural rubber.

  10. HARD RUBBER COMPOSITES BERPENGUAT SERAT KENAF UNTUK PANEL

    Directory of Open Access Journals (Sweden)

    Agus Hariyanto

    2016-08-01

    Full Text Available Tujuan penelitian ini adalah menyelidiki pengaruh variasi sulfur 25 dan 30 phr (per hundred rubber komposit berpenguat serat kenaf dan peningkatan kekuatan tarik, bermatrix hard natural rubber (Ebonite.               Bahan utama penelitian adalah compount natural rubber/ebonite, serta kenaf acak. Komposit dibuat dengan metode cetak tekan panas (Hot Press Mold. Komposit tersusun terdiri dari serat kenaf dengan ebonite. Fraksi berat serat kenaf 8%. Spesimen dan prosedur pengujian tarik mengacu pada standar ASTM D 638-02.               Hasil penelitian ini menunjukkan pengaruh variasi sulfur 25 dan 30 phr terhadap kekuatan tarik pada komposit berpenguat serat kenaf meningkat. Kekuatan tarik komposit berpenguat serat kenaf sebesar 12 dan 29 Mpa. Kekuatan tarik memiliki harga yang paling optimum pada komposit berpenguat serat kenaf dengan variasi sulfur 30 phr.

  11. ASSESSMENT OF THE DYNAMIC PROPERTIES OF PLAIN AND RUBBERIZED CONCRETE

    Directory of Open Access Journals (Sweden)

    Ionuţ Ovidiu TOMA

    2015-11-01

    Full Text Available The use of rubber from discarded car tires as an alternative to natural aggregates in concrete may help preventing the complete depletion of natural resources and work towards a sustainable future. Moreover it can significantly reduce the environmental footprint of the construction industry. The assessment of the dynamic properties of a material are very important from the point of view of the energy dissipation capability of the investigated material. This can be determined from the dynamic modulus of elasticity, damping and the loss coefficients of the material. The paper presents the results obtained during an experimental program aimed at assessing the dynamic characteristics of plain and rubberized concrete containing rubber crumbs from discarded car tires. The theoretical background and the investigation methodology are presented with particular application to cylindrical concrete specimens.

  12. CHARACTERIZATION OF POLAR COMPONENTS IN HYTROTREATED NAPHTHENIC RUBBER PROCESS OIL

    Institute of Scientific and Technical Information of China (English)

    2005-01-01

    Polar components play a very important role toward light stability of hydrotreated naphthenic rubber process oil. Polar components in hydrotreated naphthenic rubber process oil are analyzed in detail. Polar components are firstly isolated from rubber process oil by column chromatography of silica gel, and then characterized by a series of instrument technology including elemental analysis, infrared spectroscopy, APCI/MS and XPS. The results show that the polar components comprise some hetero atoms compounds of sulfur, nitrogen and oxygen. Oxygen- containing compounds such as hydroxyl, carbonyl, and carboxyl groups constitute the main body of polar components. Nitrogen - containing compounds (NH2, NH, or NO2 and - N = N - ) and sulfur - containing compounds (SO42- and PHSSPH) only account for minor percent of polar components. The molecular weight distribution of polar components mainly concentrates between 300 and 500 and a minor portion distributes from 180 to 300.

  13. A Review of Constitutive Models for Rubber-Like Materials

    Directory of Open Access Journals (Sweden)

    Aidy Ali

    2010-01-01

    Full Text Available Problem statement: This study reviewed the needs of different constitutive models for rubber like material undergone large elastic deformation. The constitutive models are widely used in Finite Element Analysis (FEA packages for rubber components. Most of the starting point for modeling of various kinds of elastomer is a strain energy function. In order to define the hyperelastic material behavior, stress-strain response is required to determine material parameters in the strain energy potential and also proper selection of rubber elastic material model is the first attention. Conclusion: This review provided a sound basis decision to engineers and manufactures to choose the right model from several constitutive models based on strain energy potential for incompressible and isotropic materials.

  14. Rheological behavior of raw natural rubber coagulated by microorganisms

    Directory of Open Access Journals (Sweden)

    Zhifen Wang

    2014-01-01

    Full Text Available Tests of the strain sweep, frequency sweep and stress relaxation for raw natural rubber coagulated by microorganisms (NR-m and raw natural rubber coagulated by acid (NR-a were carried out with the use of a rubber process analyzer (RPA. The results showed that the storage torque, complex viscosity of NR-m were higher than those of NR-a while the loss factor was lower. The effect of temperature on viscosity of raw NR was studied following the Arrhenious-Frenkel-Eyring model. The viscous flow behavior of NR-m was poorer than those of NR-a. Furthermore, stress relaxation measurements of raw NR showed a longer period of relaxation for NR-m.

  15. Rubber oxygenase and latex clearing protein cleave rubber to different products and use different cleavage mechanisms.

    Science.gov (United States)

    Birke, Jakob; Jendrossek, Dieter

    2014-08-01

    Two types of enzyme for oxidative cleavage of poly(cis-1,4-isoprene) are known. One is rubber oxygenase (RoxA) that is secreted by Xanthomonas sp. strain 35Y and a few other Gram-negative rubber-degrading bacteria during growth on polyisoprene. RoxA was studied in the past, and the recently solved structure showed a structural relationship to bacterial cytochrome c peroxidases (J. Seidel et al., Proc. Natl. Acad. Sci. U. S. A. 110:13833-13838, 2013, http://dx.doi.org/10.1073/pnas.1305560110). The other enzyme is latex-clearing protein (Lcp) that is secreted by rubber-degrading actinomycetes, but Lcp has not yet been purified. Here, we expressed Lcp of Streptomyces sp. strain K30 in a ΔroxA background of Xanthomonas sp. strain 35Y and purified native (untagged) Lcp. The specific activities of Lcp and RoxA were 0.70 and 0.48 U/mg, respectively. Lcp differed from RoxA in the absence of heme groups and other characteristics. Notably, Lcp degraded polyisoprene via endo-type cleavage to tetra-C20 and higher oligo-isoprenoids with aldehyde and keto end groups, whereas RoxA used an exo-type cleavage mechanism to give the main end product 12-oxo-4,8-dimethyltrideca-4,8-diene-1-al (ODTD). RoxA was able to cleave isolated Lcp-derived oligo-isoprenoid molecules to ODTD. Inhibitor studies, spectroscopic investigations and metal analysis gave no indication for the presence of iron, other metals, or cofactors in Lcp. Our results suggest that Lcp could be a member of the growing group of cofactor-independent oxygenases and differs in the cleavage mechanism from heme-dependent RoxA. In conclusion, RoxA and Lcp represent two different answers to the same biochemical problem, the cleavage of polyisoprene, a polymer that has carbon-carbon double bonds as the only functional groups for enzymatic attack.

  16. Study on heat under dynamic loading of rubber

    Directory of Open Access Journals (Sweden)

    T. I. Igumenova

    2016-01-01

    Full Text Available A number of studies on heat buildup in tire rubber surface scan method samples using a thermal imaging camera. Investigated the exothermic chemical reaction mechanical destruction rubber when loading designs permanent cyclic stretching with deformation of the working zone 50%. Percentage of deformation of the working zone was chosen on the basis of the actual data on the stretch-compression zone "Rusk" tires, which is the maximum level difference of deformation during run-in. Experiment plan provided for periodic relaxation samples of at least 72 hours for more accurate simulation of operation process of structural products. Created and processed data on temperature changes in samples for bar and line profile for rubber compounds with the introduction of nanomodificator (fullerene-containing technical carbon in comparison with the control sample without him. The data obtained reflect the nature of heat depending on the composition of the compound. Identified common patterns of thermal nature of physicochemical process mechanical destruction rubbers. For rubber with nanomodifikatorom there has been an increase in the temperature interval reaction from a minimum to a maximum 2 degrees that is also linked to the rise in the average temperature of the reaction on the histogram also at 2-3 degrees of deformation under the same conditions and the level of cyclic loading. However, the temperature in the control sample that is associated with the beginning of the formation of hardened rubber structures, economies of Mallinza-Petrikeeva, occurs with delay twice compared with modified Fullerenes. Measurement of physic-mechanical indicators selected in the course of testing of samples showed the beginning of formation of structure with increased strength of samples in the sample temperature zone that corresponds to the thermal effect of èndotermičeskomu recombination reactions of macromolecules.

  17. Quantitative characterization of toughening mechanisms of rubber modified polymers

    Institute of Scientific and Technical Information of China (English)

    朱晓光; 漆宗能; 徐虎; 李刚; 蔡忠龙; C.L.Choy

    1997-01-01

    The volume changes of rubber modified polymers under creep at room temperature were successfully used to characterize the toughening mechanisms of blends with brittle polymer matrices such as high impact polystyrene.This approach cannot be applied to pseudo-ductile polymers such as polypropylene and polyamide,because they are ductile when stretched at low speed at room temperature.Based on the time-temperature equivalence princi ple,the volume change at low temperature is proposed to characterize quantitatively the toughening mechanisms of polymer blends with ductile matrices,which is illustrated by applying this approach to rubber modified polypropylene

  18. Exposure to mutagenic airborne particulate in a rubber manufacturing plant.

    Science.gov (United States)

    Fracasso, M E; Franceschetti, P; Mossini, E; Tieghi, S; Perbellini, L; Romeo, L

    1999-04-26

    Epidemiological studies conducted in the 1980s revealed that people working in the rubber manufacturing industry had an increased risk of cancer. Even now, workers employed in rubber processing are still at risk despite the measures adopted to improve their working conditions. The aim of the study was to evaluate the presence of a genotoxic risk in a rubber industry and to verify whether or not it was possible to locate the most dangerous position among the different rubber-working processes. The mutagenic activity of airborne particulate was evaluated in samples collected in the mixing department of a rubber manufacturing plant. Ambient air samples were taken over 3-h period in two stable positions near the mixing (Banbury mixer) and calendering areas. Personal air samples were taken over 2-h period during a normal workday from five workers employed in different rubber processing operations (mixing, weighing, calendering, compounding and extruding). The mutagenic activity of the air samples was determined by plate incorporation assay using Salmonella typhimurium strains (TA 98, TA 98NR, TA 100, YG 1021) with and without metabolic activation. Polycyclic aromatic hydrocarbon (PAH) concentrations were determined by high-performance liquid chromatography (HPLC); the presence of other presumable contaminants were carried out by gas chromatography-mass spectrometry (GC-MS). The results showed substantial direct and indirect frameshift mutagenicity in both ambient and personal samples. No mutagenic activity was present in S. typhimurium TA 100, except in the personal sample from a worker employed on the Banbury mixer. HPLC analysis revealed very low concentrations of PAHs. GC-MS analysis showed the presence of compounds such as azulene derivative, 1,2-dihydro-2,2,4-trimethylquinoline, N-methyl N-phenylbenzenamine, diphenylamine, bis(2-ethylhexyl)phthalate and bis(methyl-propyl)phthalate. We conclude that the high levels of mutagenic activity in ambiental and personal

  19. Curing characteristics of chlorosulphonated polyethylene and natural rubber blends

    OpenAIRE

    M. MARINOVIC-CINCOVIC; J. BUDINSKI SIMENDIC; Markovic, G.; Radovanovic, B.

    2005-01-01

    The dependence of the Mooney scorch time and cure index on the blend ratio of chlorosulphonated polyethylene/natural rubber (CSM/SMR 20 CV) and chlorosulphonated polyethylene/chlorinated natural rubber (CSM/Pergut S 40) blends were determined in the temperature range from 120 oC to 160 oC using a Monsanto Mooney viscometer. Semi-efficient vulcanization systems were used for the study. The morphology of the fracture surface of the crosslinked systems was determined by Scanning Electron Microsc...

  20. Complex processing of rubber waste through energy recovery

    Directory of Open Access Journals (Sweden)

    Roman Smelík

    2015-12-01

    Full Text Available This article deals with the applied energy recovery solutions for complex processing of rubber waste for energy recovery. It deals specifically with the solution that could maximize possible use of all rubber waste and does not create no additional waste that disposal would be expensive and dangerous for the environment. The project is economically viable and energy self-sufficient. The outputs of the process could replace natural gas and crude oil products. The other part of the process is also the separation of metals, which can be returned to the metallurgical secondary production.

  1. Surface coatings with soft rubber on large projects

    Energy Technology Data Exchange (ETDEWEB)

    Boehnert, J.

    1987-03-01

    The paper first provides a review of polymers in use and distinguishes between factory and construction site quality. By means of a sample presentation, the effects of various components of mixtures and also the production of mixtures and of plates are briefly considered. Reference is made to the construction site specifically for the application of work to be carried out on the structure up to the acceptance tests on the completed rubber coatings. The second section deals with the kinds of stresses imposed on rubber coatings in general. A distinction is made between wear, corrosion and chemical attack. Examples describe these types of stresses under mechanical and thermal conditions.

  2. Maillard Reaction in Natural Rubber Latex: Characterization and Physical Properties of Solid Natural Rubber

    Directory of Open Access Journals (Sweden)

    S. Montha

    2016-01-01

    Full Text Available Maillard reaction in Natural Rubber (NR latex was investigated by treating fresh NR latex with glutaraldehyde (C5H8O2 in amounts of 0, 50, 100, and 200 mmol/kg of latex. Protein cross-linking in fresh NR latex and solid NR was confirmed by using sodium dodecylsulfate polyacrylamide gel electrophoresis (SDS-PAGE and attenuated total reflection infrared (ATR-IR spectroscopy, respectively. It was found that degree of protein cross-linking in NR increased with increasing C5H8O2 concentration. Physical properties of untreated and treated NR substances in terms of gel content, initial Wallace plasticity (P0, plasticity retention index (PRI, Mooney viscosity, and tensile strength were carefully explored. Results clearly showed that the Maillard cross-linking of proteins had remarkable effect on bulk NR properties, that is, solvent resistance, hardness, resistance to oxidation, rheological behavior, and resistance to stretching out.

  3. Innovative neutron shielding materials composed of natural rubber-styrene butadiene rubber blends, boron oxide and iron(III) oxide

    Science.gov (United States)

    Jumpee, C.; Wongsawaeng, D.

    2015-05-01

    Optimized flexible and lightweight neutron shielding materials were designed using the Monte Carlo N-Particle (MCNP) code. Thicknesses of 10 mm and 100 mm were tested for neutron shielding performances. Simulation results indicated that the 10 mm shielding material of natural rubber (NR) and styrene butadiene rubber (SBR) blend (1:1) with 60 part per hundred rubber (phr) boron oxide (B2O3) and 100 mm shielding material with four alternating layers of NR with 100 phr iron (III) oxide (Fe2O3) and of NR and SBR blend (1:1) with 10 phr B2O3 were most suitable for thermal neutron shielding and all-energy neutron shielding, respectively. Experimental results verified the shielding efficiency of these optimal designs and ease of fabrication.

  4. Temperature dependence on free volume in cured natural rubber and styrene-butadiene rubber blends

    Science.gov (United States)

    Salgueiro, W.; Somoza, A.; Silva, L.; Consolati, G.; Quasso, F.; Mansilla, M. A.; Marzocca, A. J.

    2011-05-01

    A systematic study on the evolution of free volume as a function of the temperature in vulcanized at 433 K natural rubber (NR) and styrene butadiene rubber (SBR) in 25-75, 50-50, 75-25 NR-SBR (percent content of pure NR and SBR, respectively) blends was studied by positron annihilation lifetime spectroscopy. All samples were prepared with sulfur and TBBS (n-t-butyl-2-benzothiazole sulfenamide) as accelerator. The glass transition temperatures of the samples studied were determined by differential scanning calorimetry (DSC) and from lifetime data. In general, a sigmoidal-like complex behavior of the long-lived lifetime component, linked to the nanohole free volume, as a function of the temperature was found. For SBR, the slope of the ortho-positronium lifetime against temperature curves could be well-fitted using a linear function. For blends and also for NR, two different linear functions were necessary. This last behavior is explained in terms of the supercooled process involving a reconfiguration of the elastomeric chains. In the case of blends, the state of cure of NR and SBR in each NR-SBR sample was also taken into account in the discussion of the results obtained. Besides, thermal expansion coefficients of the free volumes in the transition and glassy region of all compounds were estimated. The differences observed in the values of this parameter are discussed by taking into account the morphology and formulation of each blend, the crosslink densities, and the role of the interphases formed between both NR and SBR elastomers.

  5. Recycling of waste gasket rubber granules by bulk CuCl2 and nano CuCl2: removal of Hg(II) ions by recycled rubber granules

    Science.gov (United States)

    Deivasigamani, Kalpana; Nanjan, Jayakumar; Mani, Hari Prasad

    2017-01-01

    Environmental problems arise due to the millions of tons of waste rubber that are thrown away in the natural environment. Management of this waste rubber is a big environmental challenge. So, a new, simple and cost-effective recycling method for obtaining recycled waste rubber should be developed. In this study, we found that waste gasket rubber can be desulfurized by means of bulk and nano-sized transition metal halides in the presence of solvents. The recycled product of desulfurized waste gasket rubber granules that is obtained can be used as the cheapest adsorbent in the removal of mercury(II) ions from aqueous solution. Comparative batch studies have been conducted to elucidate the adsorption efficiency of desulfurized rubber using bulk copper chloride and also using nano-sized copper chloride under optimum conditions with commercial activated carbon.

  6. Oxygen Plasma Treatment of Rubber Surface by the Atmospheric Pressure Cold Plasma Torch

    DEFF Research Database (Denmark)

    Lee, Bong-ju; Kusano, Yukihiro; Kato, Nobuko

    1997-01-01

    A new application of the atmospheric cold plasma torch has been investigated. Namely, the surface treatment of an air-exposed vulcanized rubber compound. The effect of plasma treatment was evaluated by the bondability of the treated rubber compound with another rubber compound using a polyurethane...... adhesive. The adhesion property was improved by treatment of the rubber compound with plasma containing oxygen radicals. Physical and chemical changes of the rubber surface as a result of the plasma treatment were analyzed by field emission scanning electron microscopy (FE-SEM) and fourier transform...

  7. Effect of rubber polarity on selective wetting of carbon nanotubes in ternary blends

    OpenAIRE

    Le, H.H.; M. Parsaker; M. N. Sriharish; S. Henning; Menzel, M.; S. Wiessner; Das, A; Q. K. Do; Heinrich, G.; H-J. Radusch

    2015-01-01

    Based on atomic force microscopy (AFM) and Fourier transform infrared spectroscopy (FTIR) analysis of the rubber-filler gel (wetting concept) the kinetics of selective wetting of carbon nanotubes (CNTs) in ternary styrene butadiene rubber (SBR)/butadiene rubber (BR)/natural rubber (NR) blends was qualitatively and quantitatively characterized. Almost all CNTs are found to be wetted by the non-polar NR but not by the other non-polar rubber like BR or weakly polar SBR. It was proposed that phos...

  8. Biolubricant induced phase inversion and superhydrophobicity in rubber-toughened biopolymer/organoclay nanocomposites

    Science.gov (United States)

    Bayer, Ilker S.; Steele, Adam; Martorana, Philip; Loth, Eric; Robinson, Scott J.; Stevenson, Darren

    2009-08-01

    We present a simple technique to fabricate rubber-toughened biopolymer/organoclay nanocomposite coatings with highly water repellent surface wetting characteristics and strong adhesion to metal surfaces. The technique combines the principles of phase inversion and atomization of multicomponent polymer/organoclay suspensions containing a biolubricant as the nonsolvent. The biolubricant was a blend of cyclomethicone/dimethiconol oil with fruit kernel oils. The ternary system of cellulose nitrate/solvent/biolubricant was blended with rubber dispersed organoclay nanofluids. Natural, synthetic, and fluoroacrylic latex rubbers were used for the purpose. Self-cleaning superhydrophobic coatings were obtained from synthetic and fluoroacrylic rubbers whereas natural rubber containing formulations resulted in sticky superhydrophobic coatings.

  9. 40 CFR 428.70 - Applicability; description of the large-sized general molded, extruded, and fabricated rubber...

    Science.gov (United States)

    2010-07-01

    ... large-sized general molded, extruded, and fabricated rubber plants subcategory. 428.70 Section 428.70... RUBBER MANUFACTURING POINT SOURCE CATEGORY Large-Sized General Molded, Extruded, and Fabricated Rubber... fabricated rubber plants subcategory. The following provisions of this subpart are applicable to...

  10. 40 CFR 428.50 - Applicability; description of the small-sized general molded, extruded, and fabricated rubber...

    Science.gov (United States)

    2010-07-01

    ... small-sized general molded, extruded, and fabricated rubber plants subcategory. 428.50 Section 428.50... RUBBER MANUFACTURING POINT SOURCE CATEGORY Small-Sized General Molded, Extruded, and Fabricated Rubber... fabricated rubber plants subcategory. The following provisions of this subpart are applicable to...

  11. Caltrans use of scrap tires in asphalt rubber products: a comprehensive review

    Directory of Open Access Journals (Sweden)

    Haiping Zhou

    2014-02-01

    Full Text Available The California Department of Transportation (Caltrans has been using scrap tire rubber in asphalt pavements since the 1970s in chip seals and the 1980s in rubberized hot mix asphalt(RHMA. Both the wet (field blend and dry processes were used in early trials. Caltrans has also used rubber modified binders containing both crumb rubber modifier and polymer modifier that could be manufactured at a refinery facility, a terminal blend wet process. Since the beginning of this century, Caltrans increased the use of scrap tire rubber in paving projects and invested considerable resources in developing technically sound, cost effective, and environmentally friendly strategies for using scrap tire rubber in roadway applications. By the end of year 2010, approximately 31%of all hot mix asphalt (HMA placed by Caltrans was rubberized HMA, roughly 1.2 million tons. Caltrans efforts in using asphalt rubber products were also demonstrated in its research and technology development. These included the construction of two full-scale field experiments, five warranty projects, and an accelerated pavement study using a heavy vehicle simulator. Additionally, terminal blend asphalt rubber and rubberized warm mix asphalts began to be experimented on trial basis. This paper provides a comprehensive review of Caltrans experience over four decades with asphalt rubber products. Current practices and future outlook are also discussed.

  12. Experimental study of temperature distribution in rubber material during microwave heating and vulcanization process

    Science.gov (United States)

    Chen, Hai-Long; Li, Tao; Liang, Yun; Sun, Bin; Li, Qing-Ling

    2016-07-01

    Microwave technology has been employed to heat sheet rubber, the optical fiber temperature online monitor and optical fiber temperature sensor have been employed to measure the temperature in sheet rubber. The temperature of sheet rubber increased with increase of heating time during microwave heating process in which the maximum of temperature was curves of temperature-time presented nonlinearity. The rate of temperature rising in central zone of sheet rubber was higher than the rate of temperature rising in marginal zone of sheet rubber, and the final temperature in central zone of sheet rubber was also higher than the final temperature in marginal zone of sheet rubber. In the microwave heating and vulcanization process of sheet rubber, the maximum of rate of temperature rising and the maximum of temperature belong to the central zone of sheet rubber, so the distribution of electric field was uneven in heating chamber, which led to the uneven temperature distribution of sheet rubber. The higher electric field intensity value converges on the central zone of sheet rubber.

  13. Surface Modification of Fillers and Curatives by Plasma Polymerization for Enhanced Performance of Single Rubbers and Dissimilar Rubber/Rubber Blends

    Science.gov (United States)

    Noordermeer, J. W. M.; Datta, R. N.; Dierkes, W. K.; Guo, R.; Mathew, T.; Talma, A. G.; Tiwari, M.; van Ooij, W.

    Plasma polymerization is a technique for modifying the surface characteristics of fillers and curatives for rubber from essentially polar to nonpolar. Acetylene, thiophene, and pyrrole are employed to modify silica and carbon black reinforcing fillers. Silica is easy to modify because its surface contains siloxane and silanol species. On carbon black, only a limited amount of plasma deposition takes place, due to its nonreactive nature. Oxidized gas blacks, with larger oxygen functionality, and particularly carbon black left over from fullerene production, show substantial plasma deposition. Also, carbon/silica dual-phase fillers react well because the silica content is reactive. Elemental sulfur, the well-known vulcanization agent for rubbers, can also be modified reasonably well.

  14. Cumulative Effect of Crumb Rubber and Steel Fiber on the Flexural Toughness of Concrete

    Directory of Open Access Journals (Sweden)

    B. H. Abu Bakar

    2017-02-01

    Full Text Available Concrete properties, such as toughness and ductility, are enhanced to resist different impacts or blast loads. Rubberized concrete, which could be considered a green material, is produced from recycled waste tires grinded into different crumb rubber particle sizes and mixed with concrete. In this study, the behavior of rubberized steel fiber-reinforced concrete is investigated. Flexural performance of concrete beams (400×100×100 mm manufactured from plain, steel fiber, crumb rubber and combination crumb rubber and steel fiber are also evaluated. Similarly, concrete slabs (500×500×50 mm are also tested under flexural loading. Flexural performance of the SFRRC mixtures was significantly enhanced. The toughness and maximum deflection of specimens with rubber were considerably improved. Steel fiber/crumb rubber-reinforced concrete can be used for practical application, which requires further studies.

  15. Performance of carbon fiber reinforced rubber composite armour against shaped charge jet penetration

    Directory of Open Access Journals (Sweden)

    Yue Lian-yong

    2016-01-01

    Full Text Available Natural rubber is reinforced with carbon fiber; the protective performances of the carbonfiber reinforced rubber composite armour to shaped charge jet have been studied based on the depth of penetration experiments. The craters on the witness blocks, the nature rubber based composite plates’ deformation and the Scanning Electron Microscopy for the hybrid fiber reinforced rubber plate also is analyzed. The results showed that the composite armour can affect the stability of the jet and made part of the jet fracture. The carbon fiber reinforced rubber composite armour has good defence ablity especially when the nature rubber plate hybrid 15% volume percentage carbonfiber and the obliquity angle is 68°. The hybrid fiber reinforced rubber composite armour can be used as a new kind of light protective armour.

  16. Genetic and biochemical evaluation of natural rubber from Eastern Washington prickly lettuce (Lactuca serriola L.).

    Science.gov (United States)

    Bell, Jared L; Burke, Ian C; Neff, Michael M

    2015-01-21

    Alternative sources of natural rubber are of importance due to economic, biological, and political threats that could diminish supplies of this resource. Prickly lettuce (Lactuca serriola L.) synthesizes long-chain natural rubber and was studied to determine underlying genetic and phenotypic characteristics of rubber biosynthesis. Genotypic and phenotypic analysis of an F2 segregating population using EST-SSR markers led to the discovery of genetic regions linked to natural rubber production. Interval mapping (IM) and multiple QTL mapping (MQM) identified several QTL in the mapping population that had significance based on LOD score thresholds. The discovered QTL and the corresponding local markers are genetic resources for understanding rubber biosynthesis in prickly lettuce and could be used in marker-assisted selection (MAS) breeding. Prickly lettuce is an excellent candidate for elucidating the rubber synthesis mechanism and has potential as a crop plant for rubber production.

  17. Influence of the Diene Monomer on Devulcanization of EPDM Rubber

    NARCIS (Netherlands)

    Verbruggen, M.A.L.; van der Does, L.; Noordermeer, Jacobus W.M.; van Duin, M.

    2008-01-01

    Ethylene–propylene–diene rubbers (EPDM) with 2-ethylidene-5-norbornene (ENB), dicyclopentadiene (DCPD), and 1,4-hexadiene (HD) as third monomers have been vulcanized with peroxide and with a conventional sulfur vulcanization recipe, and their devulcanization was subsequently investigated for

  18. Hazardous organic chemicals in rubber recycled tire playgrounds and pavers.

    Science.gov (United States)

    Llompart, Maria; Sanchez-Prado, Lucia; Pablo Lamas, J; Garcia-Jares, Carmen; Roca, Enrique; Dagnac, Thierry

    2013-01-01

    In this study, the presence of hazardous organic chemicals in surfaces containing recycled rubber tires is investigated. Direct material analyses using solvent extraction, as well as SPME analysis of the vapour phase above the sample, were carried out. Twenty-one rubber mulch samples were collected from nine different playgrounds. In addition, seven commercial samples of recycled rubber pavers were acquired in a local store of a multinational company. All samples were extracted by ultrasound energy, followed by analysis of the extract by GC-MS. The analysis confirmed the presence of a large number of hazardous substances including PAHs, phthalates, antioxidants (e.g. BHT, phenols), benzothiazole and derivatives, among other chemicals. The study evidences the high content of toxic chemicals in these recycled materials. The concentration of PAHs in the commercial pavers was extremely high, reaching values up to 1%. In addition, SPME studies of the vapour phase above the samples confirm the volatilisation of many of those organic compounds. Uses of recycled rubber tires, especially those targeting play areas and other facilities for children, should be a matter of regulatory concern.

  19. Cutting height effects on guayule latex, rubber and resin yields

    Science.gov (United States)

    Guayule (Parthenium argentatum Gray) is a perennial shrub native to the Chihuahuan Desert. While guayule traditionally has been cultivated for rubber, more recently it is being cultivated for its hypoallergenic latex. Other uses including termite resistant wood products and as an energy source have ...

  20. Nanocomposites of natural rubber and polyaniline-modified cellulose nanofibrils

    Science.gov (United States)

    Cellulose nanofibrils (CNF) were isolated from cotton microfibrils (CM) by acid hydrolysis and coated with polyaniline (PANI) by in situ polymerization of aniline onto CNF in the presence of hydrochloride acid and ammonium peroxydisulfate to produce CNF/PANI. Nanocomposites of natural rubber (NR) re...

  1. The challenges of silica-silane reinforcement of natural rubber

    NARCIS (Netherlands)

    Dierkes, W.K.; Sarkawi, S.S.; Noordermeer, J.W.M.

    2012-01-01

    In recent years, highly-dispersible silica has become the preferred alternative to carbon-black as reinforcing filler for low rolling-resistance tires. However, the application of this filler system is so far limited to passenger car tires, as their treads contain styrene butadiene rubber (SBR). In

  2. Properties of Cement Mortar Containing Rubber Ash as Sand Replacement

    Science.gov (United States)

    Syamir Senin, Mohamad; Shahidan, Shahiron; Syazani Leman, Alif; Izzati Raihan Ramzi Hannan, Nurul

    2016-11-01

    Discarded scrap tyres have become one of the major environmental problems nowadays. There has been increasing public worry about the mining of natural resources in recent years. In order to minimize the consumption of natural resources, rubber ash has been postulated as a potential material for partial replacement of sand in concrete materials especially for applications which are subjected to impact and vibration such as road and bridge construction. Thus, it contributes to the development of the construction industry in a sustainable way. This paper mainly emphasizes on the use of rubber ash from waste tyres in cement mortar. 100mm cubic specimens were produced by adding rubber ash volume ratios of 0%, 3%, 5% and 7% as sand replacement in M30 quality cement mortar. A compressive stress test and a density test were conducted at the end of 7, 14, and 28 days. The result shows that 5% is the optimum value for sand replacement in the cement mortar. Therefore, rubber ash is acceptable to be used as sand replacement.

  3. Hyperelastic Modelling and Finite Element Analysing of Rubber Bushing

    Directory of Open Access Journals (Sweden)

    Merve Yavuz ERKEK

    2015-03-01

    Full Text Available The objective of this paper is to obtain stiffness curves of rubber bushings which are used in automotive industry with hyperelastic finite element model. Hyperelastic material models were obtained with different material tests. Stress and strain values and static stiffness curves were determined. It is shown that, static stiffness curves are nonlinear. The level of stiffness affects the vehicle dynamics behaviour.

  4. Simple EOS for the silicone rubber Sylgard 184

    Energy Technology Data Exchange (ETDEWEB)

    Dowell, F.

    1984-08-01

    A simple equation of state (EOS) for the silicone rubber Sylgard 184 (initial state density rho/sub 0/ = 1.05 g/cm/sup 3/) was generated and added to the T-4 Sesame EOS Library as material number 7930. This EOS reproduces the experimental shock Hugoniot data for Sylgard. 17 references.

  5. Screening with rubber screen surfaces with variously shaped apertures

    Energy Technology Data Exchange (ETDEWEB)

    Bock, B.; Kraemer, T.

    1984-07-01

    Rubber screen surfaces are advantageous for bulk materials screening because of their low rate of wear and low noise emission and because they tend to prevent clogging. Screens with four different aperture shapes and sizes were available for experimental research. The cut sizes were determined in relation to the above-mentioned parameters with round and with crushed feed materials.

  6. [Allergic contact eczema because of diethylthiourea in neoprene rubber].

    Science.gov (United States)

    Buus, Sanne Krogsbøll; Andersen, Klaus Ejner

    2002-03-11

    Three cases are reported of acute allergic contact dermatitis caused by diethylthiourea in the neoprene rubber used in a diving suit and orthopedic braces. Patch testing should be done with the specific thiourea compounds, because testing with material from the suspected products may be negative. Cross-reactivity between thiourea compounds is uncommon.

  7. Tissue-Culture Method of Cloning Rubber Plants

    Science.gov (United States)

    Ball, E. A.

    1983-01-01

    Guayule plant, a high-yield rubber plant cloned by tissue-culture method to produce multiple new plants that mature quickly. By adjusting culture medium, excised shoot tip produces up to 50 identical guayule plants. Varying concentration of cytokinin, single excised tip produces either 1 or several (up to 50) new plants.

  8. Development and Capacity Forecast of China Rubber Raw Materials

    Institute of Scientific and Technical Information of China (English)

    2011-01-01

    The "1 lth Five-Year Plan" period is the most glorious period in the history of China raw materials such as NR and SR. During the "12th Five-Year Plan" period, the rubber raw materials will enter an important period of great development in technology, product and output.

  9. Linear motion feed through with thin wall rubber sealing element

    Science.gov (United States)

    Mikhailov, V. P.; Deulin, E. A.

    2017-07-01

    The patented linear motion feedthrough is based on elastic thin rubber walls usage being reinforced with analeptic string fixed in the middle part of the walls. The pneumatic or hydro actuators create linear movement of stock. The length of this movement is two times more the rubber wall length. This flexible wall is a sealing element of feedthrough. The main advantage of device is negligible resistance force that is less then mentioned one in sealing bellows that leads to positioning error decreasing. Nevertheless, the thin wall rubber sealing element (TRE) of the feedthrough is the main unreliable element that was the reason of this element longevity research. The theory and experimental results help to create equation for TRE longevity calculation under vacuum or extra high pressure difference action. The equation was used for TRE longevity determination for hydraulic or vacuum equipment realization also as it helps for gas flow being leaking through the cracks in thin walls of rubber sealing element of linear motion feedthrough calculation.

  10. No pain relief with the rubber hand illusion.

    Science.gov (United States)

    Mohan, Rahul; Jensen, Karin B; Petkova, Valeria I; Dey, Abishikta; Barnsley, Nadia; Ingvar, Martin; McAuley, James H; Moseley, G Lorimer; Ehrsson, Henrik H

    2012-01-01

    The sense of body ownership can be easily disrupted during illusions and the most common illusion is the rubber hand illusion. An idea that is rapidly gaining popularity in clinical pain medicine is that body ownership illusions can be used to modify pathological pain sensations and induce analgesia. However, this idea has not been empirically evaluated. Two separate research laboratories undertook independent randomized repeated measures experiments, both designed to detect an effect of the rubber hand illusion on experimentally induced hand pain. In Experiment 1, 16 healthy volunteers rated the pain evoked by noxious heat stimuli (5 s duration; interstimulus interval 25 s) of set temperatures (47°, 48° and 49°C) during the rubber hand illusion or during a control condition. There was a main effect of stimulus temperature on pain ratings, but no main effect of condition (p = 0.32), nor a condition x temperature interaction (p = 0.31). In Experiment 2, 20 healthy volunteers underwent quantitative sensory testing to determine heat and cold pain thresholds during the rubber hand illusion or during a control condition. Secondary analyses involved heat and cold detection thresholds and paradoxical heat sensations. Again, there was no main effect of condition on heat pain threshold (p = 0.17), nor on cold pain threshold (p = 0.65), nor on any of the secondary measures (pillusion does not induce analgesia.

  11. The computer-aided design of rubber-metal products

    Directory of Open Access Journals (Sweden)

    Pavlo S. Shvets

    2015-12-01

    Full Text Available The important problem in design of rubber-metal products is the optimization of their mass without sacrificing of proportionality factor is in the limits of standard. Aim: The aim of this work is to improve the computer-aided systems by development and implementation of improved optimization method in rubber-metal CAD systems for designers based on the reverse optimization. Materials and Methods: The paper studies the matters of computer-aided structural design of technical composite products composed of anisotropic materials that are essentially different in properties. Results: The structure of CAD systems for designers solving the problems of such design is offered and the work principles of its subsystems are described. It is shown that complicated systems optimization in CAD systems must consider as restrictions the entitative connection between separate elements of these systems within the area of the optimizing arguments. Conclusions: The problem of the “reverse” optimization when objective functions are the connectivity area parameters is considered. In many cases, this allows receiving solutions that are more effective during the computer-aided design process. The developed CAD system for designers was used during the production of rubber-metal shock absorbers at the Odessa Rubber Technical Articles Plant. The positive technical and economic effect was obtained.

  12. [Biological monitoring in the molding of plastics and rubbers].

    Science.gov (United States)

    Fustinoni, S; Campo, L; Cirla, A M; Cirla, P E; Cutugno, V; Lionetti, C; Martinotti, I; Mossini, E; Foà, V

    2007-01-01

    This survey was carried out in the molding of plastics and rubbers, in the "Professional Cancer Prevention Project" sponsored by the Lombardy region with the objective of developing and implementing protocols for evaluating exposure to carcinogens through the biological monitoring. The realities of molding the thermoplastic polymer ABS, rubber, and thermosetting plastics containing formaldehyde were examined. The carcinogenic substances identified in these processes were: 1,3-butadiene, acrylonitrile and styrene in molding ABS, polycyclic aromatic hydrocarbons (PAH) in molding rubber, and formaldehyde in molding the thermosetting plastics. Only for some of these substances biological indicators are available. The limited exposure to airborne chemicals in molding ABS and the intrinsic characteristics of biological indicators available for 1-3 butadiene have determined the non applicability of biological monitoring to this situation. The absence of a biological indicator of exposure to formaldehyde has made this situation not investigable. Exposure in the rubber molding was studied in 19 subjects applying the determination not metabolized PAH in urine. The levels of these indicators were similar to those measured in other groups of subjects without occupational exposure to PAH, confirming a low airborne contamination in this workplace.

  13. Temperature dependence of the dielectric properties of rubber wood

    Science.gov (United States)

    Mohammed Firoz Kabir; Wan M. Daud; Kaida B. Khalid; Haji A.A. Sidek

    2001-01-01

    The effect of temperature on the dielectric properties of rubber wood was investigated in three anisotropic directions—longitudinal, radial, and tangential, and at different measurement frequencies. Low frequency measurements were conducted with a dielectric spectrometer, and high frequencies used microwave applied with open-ended coaxial probe sensors. Dielectric...

  14. On the radiation induced degradation of NBR-EPDM rubbers

    Energy Technology Data Exchange (ETDEWEB)

    Chipara, M.D.; Grecu, V.V.; Chipara, M.I. E-mail: chipara@alpha1.infim.ro; Ponta, C.; Reyes Romero, J

    1999-05-02

    The modification of the elongation at break for NBR-EPDM rubbers subjected to gamma irradiation at various integral doses ranging from 10 to 200 kGy, at different dose rates (0.14, 0.47, 1, 3, 4.7 kGy/h) are reported. The presence of the dose rate effect is noticed.

  15. CURING AND MECHANICAL PROPERTIES OF CHLOROSULPHONATED POLYETHYLENE RUBBER BLEND

    Directory of Open Access Journals (Sweden)

    Jaroslava Budinski-Simendić

    2011-09-01

    Full Text Available In this paper, the curing and mechanical properties of two series of prepared blends, i.e., chlorosulphonated polyethylene (CSM/isobutylene-co-isoprene (IIR rubber blends and chlorosulphonated polyethylene (CSM/chlorinated isobutylene-co-isoprene (CIIR rubber blends were carried out. Blends were prepared using a two-roll mill at a temperature of 40-50 °C. The curing was assessed using a Monsanto oscillating disc rheometer R-100. The process of vulcanization accelerated sulfur of pure rubbers and their blends was carried out in an electrically heated laboratory hydraulic press under a pressure of about 4 MPa and 160 °C. The stress-strain experiments were performed using a tensile tester machine (Zwick 1425. Results indicate that the scorch time, ts2, and optimum cure time, tc90, increase with increasing CSM content in both blends. The value of modulus at 100 and 300% elongation and tensile strength increases with increasing CSM content, whereas elongation at break shows a decreasing trend. The enhancement in mechanical properties was supported by data of crosslink density in these samples obtained from swelling measurement and scanning electron microscopy studies of the rubber blends fractured surfaces

  16. Behavior of Rubber Materials under Exposure to High Electric Fields

    DEFF Research Database (Denmark)

    Candela Garolera, Anna; Holbøll, Joachim; Henriksen, M,

    2013-01-01

    The effect of high electrical stress on rubber materials is investigated by performing breakdown tests and tracking resistance tests on selected samples. The study is focused on the relationship between the dielectric strength and the thickness of the samples, as well as the influence of the inte...

  17. Influence of the diene monomer on devulcanization of EPDM rubber

    NARCIS (Netherlands)

    Verbruggen, M.; Does, van der L.; Noordermeer, J.W.M.; Duin, van M.

    2008-01-01

    Ethylene–propylene–diene rubbers (EPDM) with 2-ethylidene-5-norbornene (ENB), dicyclopentadiene (DCPD), and 1,4-hexadiene (HD) as third monomers have been vulcanized with peroxide and with a conventional sulfur vulcanization recipe, and their devulcanization was subsequently investigated for recycli

  18. Modification of Asphalt by the Use of Crumb Rubber

    Directory of Open Access Journals (Sweden)

    Shah Room

    2014-01-01

    Full Text Available Health aspects enforced to ponder a study on asphalt which incorporate rubber crumbs to increase strength and flexibility of asphalt. Disposal of waste tires is a menace and it’s a serious problem globally because it is not easily biodegradable as these tires consume large spaces, open burning cause serious problems. By the use of rubber tires, this scrap is utilized efficiently and reduces the cost of asphalt to produce economical system. The asphalt is absorbed by the rubber particles which swells at high temperature allowing greater concentration of liquid asphalt. The partial replacement of crumb rubber in asphalt is 5%, 10%, 15%, and 20% (D05, D10, D15, and D20. The analysis of incorporated asphalt was done in hot mix asphalt. The generated results showed that the value for resilient modulus and creep stiffness is more as compared to the conventional asphalt and in the accumulated strain the values are much lesser which is positive approach.

  19. Another Demo of the Unusual Thermal Properties of Rubber

    Science.gov (United States)

    Liff, Mark I.

    2010-01-01

    The unusual thermal behavior of rubbers, though discovered a long time ago, can still be mind-boggling for students and teachers who encounter this class of polymeric systems. Unlike other solids, stretched elastic polymers shrink upon heating. This is a manifestation of the Gough-Joule (G-J) effect. Joule in the 1850s studied the thermal behavior…

  20. Rubber Bands as Model Polymers in Couette Flow

    Science.gov (United States)

    Dunstan, Dave E.

    2008-01-01

    We present a simple device for demonstrating the essential aspects of polymers in flow in the classroom. Rubber bands are used as a macroscopic model of polymers to allow direct visual observation of the flow-induced changes in orientation and conformation. A transparent Perspex Couette cell, constructed from two sections of a tube, is used to…

  1. Polypropylene–rubber blends: 5. Deformation mechanism during fracture

    NARCIS (Netherlands)

    Wal, van der A.; Gaymans, R.J.

    1999-01-01

    The deformation mechanism of polypropylene–EPDM rubber blends during fracture was studied by post-mortem SEM fractography. The deformation mechanism was determined for various blend morphologies and test conditions. Brittle fracture merely gives rise to voids, which are caused by voiding of the rubb

  2. Positron Annihilation in a Rubber Modified Epoxy Resin

    DEFF Research Database (Denmark)

    Mogensen, O. E.; Jacobsen, F. M.; Pethrick, R. A.

    1979-01-01

    Positron annihilation data is reported on a rubber-modified epoxy resin. Studies of the temperature dependence of the o-positronium lifetime indicated the existence of three distinct regions; the associated transition temperatures by comparison with dilatometric data can be ascribed respectively...... to be glass transition of the epoxy phase and to that of a mixed acrylonitrile—epoxy—butadiene interfacial region....

  3. Impact Resistance of Rubberized Self-Compacting Concrete

    Directory of Open Access Journals (Sweden)

    Eehab Khalil

    2015-04-01

    Full Text Available Impact loads due to ship collision on irrigation structures is significantly decreasing their durability. Loss of material and degradation are quite common problems facing lock walls and piers. In the current research, rubberized self-compacting concrete (SCC was used to investigate problems associated with impact. SCC with cement kiln dust cement replacement was used for that purpose. Concrete specimens were prepared with different crumb rubber ratios of 10% (RSCC-10, 20% (RSCC-20, 30% (RSCC-30, and 40% (RSCC-40 sand replacement by volume. Standard compressive, flexure, and splitting strength tests were conducted to monitor the effect of the added rubber on concrete behavior. Moreover, impact testing program was applied to specific specimens, cylinder of diameter 200 mm and thickness 50 mm, according to ACI committee 544 procedures. The number of blows to first and ultimate cracks was determined. The relationship between the mechanical properties and impact resilience is also presented. With the increase in rubber percentage the resistance to impact increased, but there was a decrease in specimen strength and modulus of elasticity. The variation in results was discussed and mix RSCC-30 exhibited the best impact resistance, 3 times over control mix with 40% reduction of compressive strength.

  4. Sistem Informasi Akuntansi Penjualan Tunai PT. Madjin Crumb Rubber Factory

    OpenAIRE

    Dian Permata Sayang

    2009-01-01

    PT. Madjin Crumb Rubber Factory adalah perusahaan yang bergerak dalam bidang export karet menjadi SIR-20. Dalam penelitian ini penulis menggunakan metode deskriptif. Jenis data yang digunakan adalah data primer dan data sekunder. Adapun teknik pengumpulan data yang digunakan adalah wawancara dan observasi. Metode penganalisaan data adalah metode deskriptif, dimana data dikumpulkan, disusun, diikhtisarkan, dianalisis, dan interpretasikan sehingga menghasilkan keterangan dan jawaban yang jelas ...

  5. Feasibility study of a soil-based rubberized CLSM.

    Science.gov (United States)

    Wu, Jason Y; Tsai, Mufan

    2009-02-01

    The development of beneficial uses of recycled scrap tires is always in great demand around the world. The disposal of on-site surplus excavated soil and the production of standard engineering aggregates have also been facing increasing environmental and ecological challenges in congested islands, such as Taiwan. This paper presents an experimental study using recycled crumb rubber and native silty sand to produce a lightweight, soil-based, rubberized controlled low strength material (CLSM) for a bridge approach repair. To assess the technical feasibility of this material, the effects of weight ratios of cement-to-water (C/W) and water-to-solid (W/S), and of rubber content on the engineering properties for different mixtures were investigated. The presented test results include flowability, unit weight, strength, settlement potential, and bearing capacity. Based on the findings, we conclude that a soil-based rubberized CLSM with 40% sand by weight and an optimal design ratio of 0.7 for C/W and 0.35 for W/S can be used for the proposed bridge approach repair. Such a mixture has demonstrated acceptable flowability, strength, and bearing capacity. Its lower unit weight, negligible compressibility, and hydrocollapse potential also help ensure that detrimental settlement is unlikely to occur. The results illustrate a novel scheme of CLSM production, and suggest a beneficial alternative for the reduction of scrap tires as well as conservation of resources and environment.

  6. Biobased products from rubber, jatropha and sunflower oil

    NARCIS (Netherlands)

    Bin Abu Ghazali, Yusuf

    2015-01-01

    In dit proefschrift wordt onderzoek beschreven naar het identificeren van interessante producten uit de zaden van de rubber boom (Hevea brasiliensis). Deze zaden worden momenteel niet gebruikt en in vele rubberplantages gezien als afval. De zaden bestaan uit een harde schil (39 wt%) en een kern (61

  7. Rubber dam may increase the survival time of dental restorations.

    Science.gov (United States)

    Keys, William; Carson, Susan J

    2017-03-01

    Data sourcesCochrane Oral Health's Trials Register, Cochrane Central Register of Controlled Trials (CENTRAL), Medline, Embase, LILACS, SciELO, Chinese BioMedical Literature Database, VIP, China National Knowledge Infrastructure, ClinicalTrials.gov, World Health Organization International Clinical Trials Registry Platform, OpenGrey and Sciencepaper Online databases. Handsearches in a number of journals.Study selectionRandomised controlled trials, including split-mouth studies assessing the effects of rubber dam isolation for restorative treatments in dental patients.Data extraction and synthesisTwo review authors independently screened the results of the electronic searches, extracted data and assessed the risk of bias of the included studies.ResultsFour studies involving a total of 1,270 patients were included. The studies were at high risk of bias. One trial was excluded from the analysis due to inconsistencies in the presented data. Restorations had a significantly higher survival rate in the rubber dam isolation group compared to the cotton roll isolation group at six months in participants receiving composite restorative treatment of non-carious cervical lesions (risk ratio (RR) 1.19, 95% confidence interval (CI) 1.04 to 1.37, very low-quality evidence). The rubber dam group had a lower risk of failure at two years in children undergoing proximal atraumatic restorative treatment in primary molars (hazard ratio (HR) 0.80, 95% CI 0.66 to 0.97, very low-quality evidence). One trial reported limited data showing that rubber dam usage during fissure sealing might shorten the treatment time. None of the included studies mentioned adverse effects or reported the direct cost of the treatment, or the level of patient acceptance/satisfaction. There was also no evidence evaluating the effects of rubber dam usage on the quality of the restorations.ConclusionsWe found some very low-quality evidence, from single studies, suggesting that rubber dam usage in dental direct

  8. EFFECT of blend ratio and compatibilizer on solution casted treated waste natural rubber latex/polystyrene blends

    OpenAIRE

    Orathai Boondamnoen; A. Rashid Azura; Masahiro Ohshima; Saowaroj Chuayjuljit; Azlan Ariffin

    2013-01-01

    Natural rubber latex waste (WL) was treated with natural rubber latex (NRL) prior to blend with polystyrene. Differentblend compositions of treated waste natural rubber latex (TWL) and PS were carried out through solution blending. Tensileand tear properties were investigated. The compatibility improvement of the 70/30 TWL/PS blends was further investigatedusing styrene butadiene rubber (SBR) and styrene graft natural rubber (SNR) as compatibilizer. The mechanical properties forTWL/PS blends ...

  9. Fluorocarbon-bonded magnetic mesoporous microspheres for the analysis of perfluorinated compounds in human serum by high-performance liquid chromatography coupled to tandem mass spectrometry

    Energy Technology Data Exchange (ETDEWEB)

    Liu, Xiaodan; Yu, Yingjia [Department of Pharmaceutical Analysis, School of Pharmacy, Fudan University, No. 826 Zhangheng Road, Shanghai 201203 (China); Li, Yan, E-mail: yanli@fudan.edu.cn [Department of Pharmaceutical Analysis, School of Pharmacy, Fudan University, No. 826 Zhangheng Road, Shanghai 201203 (China); Zhang, Haiying [Department of Biology, Dezhou University, Shandong 253023 (China); Ling, Jin; Sun, Xueni; Feng, Jianan; Duan, Gengli [Department of Pharmaceutical Analysis, School of Pharmacy, Fudan University, No. 826 Zhangheng Road, Shanghai 201203 (China)

    2014-09-24

    Highlights: • New SPE method was developed for analysis of PFCs in human serum. • Fluorocarbon-bonded magnetic mesoporous microspheres were used as SPE absorbents. • PFCs in serum were directly extracted without any other pretreatment procedure. • The PFCs-adsorbed microspheres were simply and rapidly isolated by using a magnet. - Abstract: We report herein an extraction method for the analysis of perfluorinated compounds in human serum based on magnetic core–mesoporous shell microspheres with decyl-perfluorinated interior pore-walls (Fe{sub 3}O{sub 4}@mSiO{sub 2}-F{sub 17}). Thanks to the unique properties of the Fe{sub 3}O{sub 4}@mSiO{sub 2}-F{sub 17} microspheres, macromolecules like proteins could be easily excluded from the mesoporous channels due to size exclusion effect, and perfluorinated compounds (PFCs) in protein-rich biosamples such as serum could thus be directly extracted with the fluorocarbon modified on the channel wall without any other pretreatment procedure. The PFCs adsorbed Fe{sub 3}O{sub 4}@mSiO{sub 2}-F{sub 17} microspheres could then be simply and rapidly isolated by using a magnet, followed by being identified and quantified by LC–MS/MS (high-performance liquid chromatography coupled to tandem mass spectrometry). Five perfluorinatedcarboxylic acids (C6, C8–C11) and perfluorooctane sulfonate (PFOS) were selected as model analytes. In order to achieve the best extraction efficiency, some important factors including the amount of Fe{sub 3}O{sub 4}@mSiO{sub 2}-F{sub 17} microspheres added, adsorption time, type of elution solvent, eluting solvent volume and elution time were investigated. The ranges of the LOD were 0.02–0.05 ng mL{sup −1} for the six PFCs. The recovery of the optimized method varies from 83.13% to 92.42% for human serum samples.

  10. Hydrophobicity attainment and wear resistance enhancement on glass substrates by atmospheric plasma-polymerization of mixtures of an aminosilane and a fluorocarbon

    Science.gov (United States)

    Múgica-Vidal, Rodolfo; Alba-Elías, Fernando; Sainz-García, Elisa; Pantoja-Ruiz, Mariola

    2015-08-01

    Mixtures of different proportions of two liquid precursors were subjected to plasma-polymerization by a non-thermal atmospheric jet plasma system in a search for a coating that achieves a hydrophobic character on a glass substrate and enhances its wear resistance. 1-Perfluorohexene (PFH) was chosen as a low-surface-energy precursor to promote a hydrophobic character. Aminopropyltriethoxysilane (APTES) was chosen for its contribution to the improvement of wear resistance by the formation of siloxane bonds. The objective of this work was to determine which of the precursors' mixtures that were tested provides the coating with the most balanced enhancement of both hydrophobicity and wear resistance, given that coatings deposited with fluorocarbon-based precursors such as PFH are usually low in resistance to wear and coatings deposited with APTES are generally hydrophilic. The coatings obtained were analyzed by Scanning Electron Microscopy (SEM), Atomic Force Microscopy (AFM), Fourier Transform Infra-Red (FTIR) spectroscopy, X-ray Photoelectron Spectroscopy (XPS), static Water Contact Angle (WCA) measurements, tribological ball-on-disc tests and contact profilometry. A relationship between the achievement of a hydrophobic character and the modifications to roughness and surface morphology and the incorporation of fluorocarbon groups in the surface chemistry was observed. Also, it was seen that the wear resistance was influenced by the SiOSi content of the coatings. In turn, the SiOSi content appears to be directly related to the percentage of APTES used in the mixture of precursors. The best conjunction of hydrophobicity and wear resistance in this work was found in the sample that was coated using a mixture of APTES and PFH in proportions of 75 and 25%, respectively. Its WCA (100.2 ± 7.5°) was the highest of all samples that were measured and more than three times that of the uncoated glass (31 ± 0.7°). This sample underwent a change from a hydrophilic to a

  11. Dependence of Adhesion Properties on Blend Ratio of Ethylene-Propylene-Diene Rubber/Standard Malaysian Rubber Blend Adhesive

    Directory of Open Access Journals (Sweden)

    B. T. Poh

    2013-01-01

    Full Text Available Viscosity, tack and, peel and shear strengths of ethylene-propylene-diene rubber (EPDM/standard Malaysian rubber (SMR L blend adhesive were studied using various blend ratios of the two rubbers, ranging from 0 to 100% EPDM. Coumarone-indene resin, toluene, and poly(ethylene terephthalate (PET were used as the tackifier, solvent, and coating substrate, respectively. The tackifier content was fixed at 40 parts per hundred parts of rubber (phr. A SHEEN hand coater was used to coat the adhesive on PET film at four coating thicknesses, that is, 30, 60, 90, and 120 µm. The viscosity and adhesion properties were determined by a Brookfield viscometer and a Lloyd Adhesion Tester, respectively. Results show that the viscosity, loop tacks and peel strength of blend adhesives decrease gradually with increasing % EPDM. This observation is attributed to dilution effect and lowering in wettability and compatibility. Shear strength, however, passes through a maximum at 20–40% EPDM blend ratio, an observation which is ascribed to culmination of cohesive strength at the optimum EPDM blend ratio. Increasing coating thickness increases the adhesion properties in all blend ratios in this study.

  12. Compatibilization efficiency of carboxylated nitrile rubber and epoxy pre-polymer in nitrile/acrylic rubber blends

    Directory of Open Access Journals (Sweden)

    Micheli L. Celestin

    2013-01-01

    Full Text Available An investigation has been made of the effects from a compatibilizer, viz. carboxylated nitrile rubber (XNBR, on several properties of nitrile rubber (NBR and acrylic rubber (ACM blends, including curing characteristics, mechanical, dynamic mechanical and dielectric properties. The presence of XNBR until 10 phr resulted in an improvement of the ultimate tensile properties, especially elongation at break. The mechanical properties associated to the volume fraction of rubber in the network (Vr and torque values suggest the co-vulcanization phenomenon imparted by the compatibilization. The oil resistance of NBR/ACM (50:50 wt. (% blends (compatibilized and non compatibilized was similar to that observed for pure ACM and significantly higher than NBR. The addition of small amounts of epoxy pre-polymer in combination with XNBR resulted in an additional improvement of the tensile properties. The dynamic mechanical and dielectric properties of the blends were also investigated. The loss modulus values of the compatibilized blends were significantly lower indicating an increase of the elastic characteristics. All blends presented two dielectric relaxation peaks confirming the heterogeneity of the compatibilized blends

  13. 氟碳化合物等离子体处理丝绸织物的表面分析%The surface properties of silk fabrics treated by fluorocarbon compound plasma

    Institute of Scientific and Technical Information of China (English)

    沈丽; 朱泉; 曹淑华

    2013-01-01

    Silk fabrics were treated by low temperature plasma with fluorocarbons such as hexafluoropro-pene, perfluoroheptane, perfluorocyclobutane, perfluorooctyl ethylene, 1,1,1,3,3,3-hexafluoro-2-propanol, 2,2, 2-trifluoroethanol. The water and oil repellency of silk treated by fluorocarbon plasma was investigated. The changes of element composition and functional groups before and after treatment were characterized by X-ray photoelectron spectroscopy (XPS). Certain amounts of fluorine atoms were introduced to the surface of fluorocarbon plasma treated silk fabrics, which increased the water repellency of silk fabrics. C1s spectra showed that -CF, -CF2 and -CF3 groups were introduced to the silk surface. The fluoro containing groups on the silk fabrics surface varied with the kinds of fluorocarbon compounds, which indicated that the binding modes with silk fabric surface changed with the structures of fluorocarbon compounds.%以六氟丙烯、全氟庚烷、八氟环丁烷、全氟辛基乙烯、1,1,1,3,3,3-六氟-2-丙醇和2,2,2-三氟乙醇等氟碳化合物为气氛对丝绸织物进行等离子体处理,考察处理后丝绸织物的拒水拒油性能,利用X射线光电子能谱(XPS)分析等离子体处理前后元素组成及官能团的变化.不同氟碳化合物等离子体处理后在织物表面引入了一定量的氟元素,织物的拒水性能增加.Cls谱图表明在织物表面引入了—CF、—CF2和—CF3基团,不同氟碳化合物引入到织物表面的含氟基团有所不同,说明化合物结构不同使在丝绸织物表面的结合方式有所区别.

  14. De novo assembly and transcriptome analysis of the rubber tree (Hevea brasiliensis and SNP markers development for rubber biosynthesis pathways.

    Directory of Open Access Journals (Sweden)

    Camila Campos Mantello

    Full Text Available Hevea brasiliensis (Willd. Ex Adr. Juss. Muell.-Arg. is the primary source of natural rubber that is native to the Amazon rainforest. The singular properties of natural rubber make it superior to and competitive with synthetic rubber for use in several applications. Here, we performed RNA sequencing (RNA-seq of H. brasiliensis bark on the Illumina GAIIx platform, which generated 179,326,804 raw reads on the Illumina GAIIx platform. A total of 50,384 contigs that were over 400 bp in size were obtained and subjected to further analyses. A similarity search against the non-redundant (nr protein database returned 32,018 (63% positive BLASTx hits. The transcriptome analysis was annotated using the clusters of orthologous groups (COG, gene ontology (GO, Kyoto Encyclopedia of Genes and Genomes (KEGG, and Pfam databases. A search for putative molecular marker was performed to identify simple sequence repeats (SSRs and single nucleotide polymorphisms (SNPs. In total, 17,927 SSRs and 404,114 SNPs were detected. Finally, we selected sequences that were identified as belonging to the mevalonate (MVA and 2-C-methyl-D-erythritol 4-phosphate (MEP pathways, which are involved in rubber biosynthesis, to validate the SNP markers. A total of 78 SNPs were validated in 36 genotypes of H. brasiliensis. This new dataset represents a powerful information source for rubber tree bark genes and will be an important tool for the development of microsatellites and SNP markers for use in future genetic analyses such as genetic linkage mapping, quantitative trait loci identification, investigations of linkage disequilibrium and marker-assisted selection.

  15. De novo assembly and transcriptome analysis of the rubber tree (Hevea brasiliensis) and SNP markers development for rubber biosynthesis pathways.

    Science.gov (United States)

    Mantello, Camila Campos; Cardoso-Silva, Claudio Benicio; da Silva, Carla Cristina; de Souza, Livia Moura; Scaloppi Junior, Erivaldo José; de Souza Gonçalves, Paulo; Vicentini, Renato; de Souza, Anete Pereira

    2014-01-01

    Hevea brasiliensis (Willd. Ex Adr. Juss.) Muell.-Arg. is the primary source of natural rubber that is native to the Amazon rainforest. The singular properties of natural rubber make it superior to and competitive with synthetic rubber for use in several applications. Here, we performed RNA sequencing (RNA-seq) of H. brasiliensis bark on the Illumina GAIIx platform, which generated 179,326,804 raw reads on the Illumina GAIIx platform. A total of 50,384 contigs that were over 400 bp in size were obtained and subjected to further analyses. A similarity search against the non-redundant (nr) protein database returned 32,018 (63%) positive BLASTx hits. The transcriptome analysis was annotated using the clusters of orthologous groups (COG), gene ontology (GO), Kyoto Encyclopedia of Genes and Genomes (KEGG), and Pfam databases. A search for putative molecular marker was performed to identify simple sequence repeats (SSRs) and single nucleotide polymorphisms (SNPs). In total, 17,927 SSRs and 404,114 SNPs were detected. Finally, we selected sequences that were identified as belonging to the mevalonate (MVA) and 2-C-methyl-D-erythritol 4-phosphate (MEP) pathways, which are involved in rubber biosynthesis, to validate the SNP markers. A total of 78 SNPs were validated in 36 genotypes of H. brasiliensis. This new dataset represents a powerful information source for rubber tree bark genes and will be an important tool for the development of microsatellites and SNP markers for use in future genetic analyses such as genetic linkage mapping, quantitative trait loci identification, investigations of linkage disequilibrium and marker-assisted selection.

  16. Taking Advantage of Capital to Promote the Application of Advanced Technolo- gies and Rubber Industry Transform--Rubber Industry I & M High-end Forum and 2012 CHINA RUBBER Magazine Annual Conference closed%Taking Advantage of Capital to Promote the Application of Advanced Technolo- gies and Rubber Industry Transform--Rubber Industry I & M High-end Forum and 2012 CHINA RUBBER Magazine Annual Conference closed

    Institute of Scientific and Technical Information of China (English)

    2012-01-01

    From September 4 to 6, "Rubber Industry I & M High-end Forum and 2012 CHINA RUBBER Magazine Annual Conference" was held in Cheng- du, Sichuan Province. Fan Rende, President of CRIA, attended the conference and accepted the interview. He said that Chinese rubber industry be- gan to step into the competitive stage, and enter- prises in the industry should change their conc, epts, make lull use of the advanced technologies and capitals to achieve further development. Deng Yali, Executive Vice President and Secretary-General of CRIA, also attended the conference. He analyzed the current situation of Chinese rubber industry and prospected its development in the future. The rd 3 Council Conference held by China Rubber Magazine Agency was held at the same time.%.

  17. Investigation of Swelling and Dissolution Process of Natural Rubber in Aromatic Oil

    Institute of Scientific and Technical Information of China (English)

    Wang Feng; Kuang Minming; Li Guanlong; Zhou Xiaolong; Li Chenglie

    2015-01-01

    Aromatic oil has been used to promote the properties of crumb rubber modiifed asphalt which is an ideal method to deal with the resource utilization of waste rubber tires and by-product of reifnery. Furfural extract oil (FEO) was sepa-rated into the light fraction and the heavy fraction. Swelling and dissolution process of natural rubber sheet in these three oil samples was investigated to shed light on the interaction mechanism. Crumb rubber also interacted on FEO and asphalt respectively. Energy dispersive spectrometer (EDS), thermo-gravimetric analysis (TGA) and scanning electron microscope (SEM) were used to characterize the chemical and structural properties of processed rubber. The chemical composition of processed oils and asphalt was investigated by using the hydrocarbon group analysis (SARA) and gel permeation chroma-tography. The results revealed that the swelling rate and mass loss of rubber in oils were much higher than those in asphalt and rose with an increasing processing temperature. The heavy fraction of FEO had more diffusion and dissolving capabil-ity than the light fraction, whilst compatibility was observed between the heavy fraction and the light fraction. Selective ab-sorption was not observed in the study and detachment of dissolved rubber was disseminated from the outside to the inside. The cross-linking degree of the residue rubber was unchanged with the processing time, and sulfur predominantly remained in the undissolved rubber. Dissolution of crumbed rubber in oils was attributed to devulcanization, while that in the asphalt was mainly attributed to depolymerization.

  18. Preparation of magnetic rubber with high mechanical properties by latex compounding method

    Science.gov (United States)

    Hou, Chunlin; Gao, Li; Yu, Hailing; Sun, Youyi; Yao, Junru; Zhao, Guizhe; Liu, Yaqing

    2016-06-01

    the magnetic rubber based on Fe3O4 nanoparticles and nature rubber were prepared by latex compounding method, in which stable Fe3O4 aqueous solutions were mixed with natural rubber latex and additives. This process was fast, versatile, reliable, safe, environmentally friendly and inexpensive. What's more, it was found that the magnetic and mechanical properties of magnetic rubber increased together with increase in doping content of Fe3O4 nanoparticles. Especially, it was demonstrated that the tensile strength (25.0 Mpa) of magnetic rubber was improved to be 478.0% comparing to neat natural rubber (5.2 Mpa), which was 5 times higher than maximal value reported in previous work. At the same time, the magnetic rubber revealed better thermal stability and solvent resistance comparing to the neat natural rubber, too. The work dose not only provides a new way to environmentally friendly preparation of magnetic rubber at low temperature, but also improve the mechanical and magnetic properties of magnetic rubber applied in industry.

  19. Mapping Deciduous Rubber Plantation Areas and Stand Ages with PALSAR and Landsat Images

    Directory of Open Access Journals (Sweden)

    Weili Kou

    2015-01-01

    Full Text Available Accurate and updated finer resolution maps of rubber plantations and stand ages are needed to understand and assess the impacts of rubber plantations on regional ecosystem processes. This study presented a simple method for mapping rubber plantation areas and their stand ages by integration of PALSAR 50-m mosaic images and multi-temporal Landsat TM/ETM+ images. The L-band PALSAR 50-m mosaic images were used to map forests (including both natural forests and rubber trees and non-forests. For those PALSAR-based forest pixels, we analyzed the multi-temporal Landsat TM/ETM+ images from 2000 to 2009. We first studied phenological signatures of deciduous rubber plantations (defoliation and foliation and natural forests through analysis of surface reflectance, Normal Difference Vegetation Index (NDVI, Enhanced Vegetation Index (EVI, and Land Surface Water Index (LSWI and generated a map of rubber plantations in 2009. We then analyzed phenological signatures of rubber plantations with different stand ages and generated a map, in 2009, of rubber plantation stand ages (≤5, 6–10, >10 years-old based on multi-temporal Landsat images. The resultant maps clearly illustrated how rubber plantations have expanded into the mountains in the study area over the years. The results in this study demonstrate the potential of integrating microwave (e.g., PALSAR and optical remote sensing in the characterization of rubber plantations and their expansion over time.

  20. Effects of forests, roads and mistletoe on bird diversity in monoculture rubber plantations

    Science.gov (United States)

    Sreekar, Rachakonda; Huang, Guohualing; Yasuda, Mika; Quan, Rui-Chang; Goodale, Eben; Corlett, Richard T.; Tomlinson, Kyle W.

    2016-02-01

    Rising global demand for natural rubber is expanding monoculture rubber (Hevea brasilensis) at the expense of natural forests in the Old World tropics. Conversion of forests into rubber plantations has a devastating impact on biodiversity and we have yet to identify management strategies that can mitigate this. We determined the life-history traits that best predict bird species occurrence in rubber plantations in SW China and investigated the effects of surrounding forest cover and distance to roads on bird diversity. Mistletoes provide nectar and fruit resources in rubber so we examined mistletoe densities and the relationship with forest cover and rubber tree diameter. In rubber plantations, we recorded less than half of all bird species extant in the surrounding area. Birds with wider habitat breadths and low conservation value had a higher probability of occurrence. Species richness and diversity increased logarithmically with surrounding forest cover, but roads had little effect. Mistletoe density increased exponentially with rubber tree diameters, but was unrelated to forest cover. To maximize bird diversity in rubber-dominated landscapes it is therefore necessary to preserve as much forest as possible, construct roads through plantations and not forest, and retain some large rubber trees with mistletoes during crop rotations.