  1. Characterization of Mode 1 and Mode 2 delamination growth and thresholds in graphite/peek composites

    Science.gov (United States)

    Martin, Roderick H.; Murri, Gretchen B.

    1988-01-01

    Composite materials often fail by delamination. The onset and growth of delamination in AS4/PEEK, a tough thermoplastic matrix composite, was characterized for mode 1 and mode 2 loadings, using the Double Cantilever Beam (DCB) and the End Notched Flexure (ENF) test specimens. Delamination growth per fatigue cycle, da/dN, was related to strain energy release rate, G, by means of a power law. However, the exponents of these power laws were too large for them to be adequately used as a life prediction tool. A small error in the estimated applied loads could lead to large errors in the delamination growth rates. Hence strain energy release rate thresholds, G sub th, below which no delamination would occur were also measured. Mode 1 and 2 threshold G values for no delamination growth were found by monitoring the number of cycles to delamination onset in the DCB and ENF specimens. The maximum applied G for which no delamination growth had occurred until at least 1,000,000 cycles was considered the threshold strain energy release rate. Comments are given on how testing effects, facial interference or delamination front damage, may invalidate the experimental determination of the constants in the expression.

  2. Characterization of Mode I and Mode II delamination growth and thresholds in AS4/PEEK composites

    Science.gov (United States)

    Martin, Roderick H.; Murri, Gretchen Bostaph

    1990-01-01

    Composite materials often fail by delamination. The onset and growth of delamination in AS4/PEEK, a tough thermoplastic matrix composite, was characterized for mode 1 and mode 2 loadings, using the Double Cantilever Beam (DCB) and the End Notched Flexure (ENF) test specimens. Delamination growth per fatigue cycle, da/dN, was related to strain energy release rate, G, by means of a power law. However, the exponents of these power laws were too large for them to be adequately used as a life prediction tool. A small error in the estimated applied loads could lead to large errors in the delamination growth rates. Hence strain energy release rate thresholds, G sub th, below which no delamination would occur were also measured. Mode 1 and 2 threshold G values for no delamination growth were found by monitoring the number of cycles to delamination onset in the DCB and ENF specimens. The maximum applied G for which no delamination growth had occurred until at least 1,000,000 cycles was considered the threshold strain energy release rate. Comments are given on how testing effects, facial interference or delamination front damage, may invalidate the experimental determination of the constants in the expression.

  3. Understanding mixed-mode cyclic fatigue delamination growth in unidirectional composites : An experimental approach

    NARCIS (Netherlands)

    Amaral, L.; Alderliesten, R.C.; Benedictus, R.

    2017-01-01

    Due to the lack of fundamental knowledge of the physics behind delamination growth, certification authorities currently require that composite structures in aircraft are designed such that any delamination will not grow. This usually leads to an overdesign of the structure, hampering weight

  4. Influence of Mixed Mode I-Mode II Loading on Fatigue Delamination Growth Characteristics of a Graphite Epoxy Tape Laminate

    Science.gov (United States)

    Ratcliffe, James G.; Johnston, William M., Jr.

    2014-01-01

    Mixed mode I-mode II interlaminar tests were conducted on IM7/8552 tape laminates using the mixed-mode bending test. Three mixed mode ratios, G(sub II)/G(sub T) = 0.2, 0.5, and 0.8, were considered. Tests were performed at all three mixed-mode ratios under quasi-static and cyclic loading conditions, where the former static tests were used to determine initial loading levels for the latter fatigue tests. Fatigue tests at each mixed-mode ratio were performed at four loading levels, Gmax, equal to 0.5G(sub c), 0.4G(sub c), 0.3G(sub c), and 0.2G(sub c), where G(sub c) is the interlaminar fracture toughness of the corresponding mixed-mode ratio at which a test was performed. All fatigue tests were performed using constant-amplitude load control and delamination growth was automatically documented using compliance solutions obtained from the corresponding quasi-static tests. Static fracture toughness data yielded a mixed-mode delamination criterion that exhibited monotonic increase in Gc with mixed-mode ratio, G(sub II)/G(sub T). Fatigue delamination onset parameters varied monotonically with G(sub II)/G(sub T), which was expected based on the fracture toughness data. Analysis of non-normalized data yielded a monotonic change in Paris law exponent with mode ratio. This was not the case when normalized data were analyzed. Fatigue data normalized by the static R-curve were most affected in specimens tested at G(sub II)/G(sub T)=0.2 (this process has little influence on the other data). In this case, the normalized data yielded a higher delamination growth rate compared to the raw data for a given loading level. Overall, fiber bridging appeared to be the dominant mechanism, affecting delamination growth rates in specimens tested at different load levels and differing mixed-mode ratios.

  5. 3D finite element analysis of stress distributions and strain energy release rates for adhesive bonded flat composite lap shear joints having pre-existing delaminations

    Energy Technology Data Exchange (ETDEWEB)

    Parida, S. K.; Pradhan, A. K. [Indian Institute of Technology, Bhubaneswar (India)

    2014-02-15

    The rate of propagation of embedded delamination in the strap adherend of lap shear joint (LSJ) made of carbon/epoxy composites has been evaluated employing three-dimensional non-linear finite elements. The delamination has been presumed to pre-exist in the thin resin layer between the first and second plies of the strap adherend. The inter-laminar peel and shear stress distributions have been studied in details and are seen to be predominantly three-dimensional in nature. The components of strain energy release rate (SERR) corresponding to the opening, sliding and cross sliding modes of delamination are significantly different at the two fronts of the embedded delamination. The sequential release of multi-point constraint (MPC) finite elements in the vicinity of the delamination fronts enables to simulate the growth of the delamination at either ends. This simulation procedure can be utilized effectively for evaluation of the status of the structural integrity of the bonded joints.

  6. Reduction of cathodic delamination rates of anticorrosive coatings using free radical scavengers

    DEFF Research Database (Denmark)

    Sørensen, Per Aggerholm; Weinell, C. E.; Dam-Johansen, Kim

    2010-01-01

    Cathodic delamination is one of the major modes of failure for anticorrosive coatings subjected to a physical damage and immersed in seawater. The cause of cathodic delamination has been reported to be the result of a chemical attack at the coating-steel interface by free radicals and peroxides...... formed as intermediates in the cathodic reaction during the corrosion process. In this study, antioxidants (i.e., free radical scavengers and peroxide decomposers) have been incorporated into various generic types of coatings to investigate the effect of antioxidants on the rate of cathodic delamination...... of epoxy coatings on cold rolled steel. The addition of free radical scavengers to epoxy coatings improved the resistance toward cathodic delamination by up to 50% during seawater immersion, while peroxide decomposers had a limited effect. Testing using substrates prepared from stainless steel...

  7. The concept of fatigue fracture toughness in fatigue delamination growth behavior

    NARCIS (Netherlands)

    Yao, L.; Alderliesten, R.C.; Benedictus, R.

    2015-01-01

    This paper provides a study on mode I fatigue delamination growth in composite laminates using energy principles. Experimental data has been obtained from fatigue tests conducted on Double Cantilever Beam (DCB) specimens at various stress ratios. A concept of fatigue fracture toughness is proposed

  8. Cathodic delamination: Quantification of ionic transport rates along coating-steel interfaces

    DEFF Research Database (Denmark)

    Sørensen, P.A.; Dam-Johansen, Kim; Weinell, C.E.

    2010-01-01

    So-called cathodic delamination is one of the major modes of failure for organic coatings immersed in electrolyte solutions (e.g. seawater). Cathodic delamination occurs as a result of the electrochemical reactions, which takes place on a corroding steel surface. This means that reactants must...... continuously be transported from the bulk solution to the cathodic areas. The transport of sodium ions from a defect in the coating to the cathodic areas is generally considered the rate-determining step for cathodic delamination because the transport of oxygen and water through the coating is sufficient...... for the corrosion processes. In this work, a novel practical method, which allows direct estimation of the apparent diffusion coefficient of sodium ions in the ultrathin aqueous layer at the coating-steel interface, is described. The apparent diffusion coefficients estimated are of similar magnitude as previously...

  9. Energy based study of quasi-static delamination as a low cycle fatigue process

    NARCIS (Netherlands)

    Amaral, L.; Yao, L.; Alderliesten, R.C.; Benedictus, R.

    2015-01-01

    This work proposes to treat quasi-static mode I delamination growth of CFRP as a low-cycle fatigue process. To this end, mode I quasi-static and fatigue delamination tests were performed. An average physical Strain Energy Release Rate (SERR), derived from an energy balance, is used to characterize

  10. Fatigue Crack and Delamination Growth in Fibre Metal Laminates under Variable Amplitude Loading

    NARCIS (Netherlands)

    Khan, S.

    2013-01-01

    This thesis presents the investigation into the fatigue propagation and delamination growth of Fibre Metal Laminates under variable amplitude loading. As explained in the first chapter, the motivation of the research is twofold: first, to obtain a clear understanding and detailed characterization of

  11. Cyclic delamination behavior of plasma-sprayed hydroxyapatite coating on Ti-6Al-4V substrates in simulated body fluid.

    Science.gov (United States)

    Otsuka, Yuichi; Kawaguchi, Hayato; Mutoh, Yoshiharu

    2016-10-01

    This study aimed to clarify the effect of a simulated body fluid (SBF) on the cyclic delamination behavior of a plasma-sprayed hydroxapatite (HAp) coating. A HAp coating is deposited on the surfaces of surgical metallic materials in order to enhance the bond between human bone and such surfaces. However, the HAp coating is susceptible to delamination by cyclic loading from the patient's gait. Although hip joints are subjected to both positive and negative moments, only the effects of tensile bending stresses on vertical crack propagation behavior have been investigated. Thus, the cyclic delamination behavior of a HAp coating was observed at the stress ratio R=-1 in order to determine the effects of tensile/compressive loading on the delamination behavior. The delamination growth rate increased with SBF immersion, which decreased the delamination life. Raman spectroscopy analysis revealed that the selective phase dissolution in the HAp coating was promoted at interfaces. Finite element analysis revealed that the energy release rate Gmax showed a positive value even in cases with compressive loading, which is a driving force for the delamination of a HAp coating. A prediction model for the delamination growth life was developed that combines a fracture mechanics parameter with the assumed stress-dependent dissolution rate. The predicted delamination life matched the experimental data well in cases of lower stress amplitudes with SBF. Copyright © 2016 Elsevier B.V. All rights reserved.

  12. Combined effect of matrix cracking and stress-free edge on delamination

    Science.gov (United States)

    Salpekar, S. A.; Obrien, T. K.

    1990-01-01

    The effect of the stress-free edge on the growth of local delaminations initiating from a matrix crack in (0 sub 2/90 sub 4) sub s and (+ or - 45.90 sub 4) sub s glass epoxy laminates is investigated using 3-D finite element analysis. The presence of high interlaminar normal stresses at the intersection (corner) of the matrix crack with the stress-free edge, suggests that a mode I delamination may initiate at the corners. The strain energy release rates (G) were calculated by modeling a uniform through-width delamination and two inclined delaminations at 10.6 deg and 45 deg to the matrix crack. All components of G have high values near the free edges. The mode I component of G is high at small delamination length and becomes zero for a delamination length of one-ply thickness. The total G values near the free edge agreed well with previously derived closed form solution. The quasi-3D solutions agreed well with the 3-D interior solutions.

  13. Buckling-driven delamination growth in composite laminates: Guidelines for assessing the threat posed by interlaminar matrix delamination

    DEFF Research Database (Denmark)

    Bhushan, Karihaloo; Stang, Henrik

    2008-01-01

    This paper is concerned with development of a simple procedure to assess the threat posed by interlaminar matrix delaminations to the integrity of composite laminates when they are situated in a compressive stress field. Depending upon the size of the delamination, its location below the surface...

  14. Delamination tolerance studies in laminated composite panels

    Indian Academy of Sciences (India)

    Abstract. Determination of levels of tolerance in delaminated composite panels is an important issue in composite structures technology. The primary intention is to analyse delaminated composite panels and estimate Strain. Energy Release Rate (SERR) parameters at the delamination front to feed into acceptability criteria.

  15. Thermally induced delamination of multilayers

    DEFF Research Database (Denmark)

    Sørensen, Bent F.; Sarraute, S.; Jørgensen, O.

    1998-01-01

    Steady-state delamination of multilayered structures, caused by stresses arising during processing due to thermal expansion mismatch, is analyzed by a fracture mechanics model based on laminate theory. It is found that inserting just a few interlayers with intermediate thermal expansion coefficie...... coefficients may be an effective way of reducing the delamination energy release rate. Uneven layer thickness and increasing elastic mismatch are shown to raise the energy release rate. Experimental work confirms important trends of the model.......Steady-state delamination of multilayered structures, caused by stresses arising during processing due to thermal expansion mismatch, is analyzed by a fracture mechanics model based on laminate theory. It is found that inserting just a few interlayers with intermediate thermal expansion...

  16. In situ characterization of delamination and crack growth of a CGO–LSM multi-layer ceramic sample investigated by X-ray tomographic microscopy

    DEFF Research Database (Denmark)

    Bjørk, Rasmus; Esposito, Vincenzo; Lauridsen, Erik Mejdal

    2014-01-01

    The densification, delamination and crack growth behavior in a Ce0.9Gd0.1O1.95 (CGO) and (La0.85Sr0.15)0.9MnO3 (LSM) multi-layer ceramic sample was studied using in situ X-ray tomographic microscopy (microtomography) to investigate the critical dynamics of crack propagation and delamination...... in a multilayered sample. Naturally occurring defects, caused by the sample preparation process, are shown not to be critical in sample degradation. Instead defects are nucleated during the debinding step. Crack growth is significantly faster along the material layers than perpendicular to them, and crack growth...

  17. Cathodic delamination: Quantification of ionic transport rates along coating-steel interfaces

    DEFF Research Database (Denmark)

    Sørensen, Per Aggerholm; Dam-Johansen, Kim; Erik Weinell, Claus

    2010-01-01

    So-called cathodic delamination is one of the major modes of failure for organic coatings immersed in electrolyte solutions (e.g. seawater). Cathodic delamination occurs as a result of the electrochemical reactions. which takes place on a corroding steel surface. This means that reactants must co...

  18. THE INFLUENCE OF THE TOOL POINT ANGLE AND FEED RATE ON THE DELAMINATION AT DRILLING OF PRE-LAMINATED PARTICLEBOARD

    Directory of Open Access Journals (Sweden)

    Mihai ISPAS

    2015-12-01

    Full Text Available Pre-laminated particleboard is a wood based composite extensively used in the furniture industry. Drilling is the most common machining process which prepares the panels for joining using twist/helical drills in the absolute majority of cases. The point angle of the drill bit and the feed speed during drilling play a major role in gaining a good surface quality and minimizing the delamination tendency of the pre-laminated particleboard. The objective of this study was to measure and analyze the influence of the two above-mentioned factors on the processing quality, evaluated by de size of delaminations, both, at the entrance side and the exit side of the drill bit. To assess the defect, two parameters were used: the delamination factor and the effective area of delamination. The results showed that, in general, the combination of small point angle with low feed rate minimizes the delamination of pre-laminated particleboard panels at drilling.

  19. THE EFFECT OF SUPPORT PLATE ON DRILLING-INDUCED DELAMINATION

    Directory of Open Access Journals (Sweden)

    Navid Zarif Karimi

    2016-02-01

    Full Text Available Delamination is considered as a major problem in drilling of composite materials, which degrades the mechanical properties of these materials. The thrust force exerted by the drill is considered as the major cause of delamination; and one practical approach to reduce delamination is to use a back-up plate under the specimen. In this paper, the effect of exit support plate on delamination in twist drilling of glass fiber reinforced composites is studied. Firstly, two analytical models based on linear fracture mechanics and elastic bending theory of plates are described to find critical thrust forces at the beginning of crack growth for drilling with and without back-up plate. Secondly, two series of experiments are carried out on glass fiber reinforced composites to determine quantitatively the effect of drilling parameters on the amount of delamination. Experimental findings verify a large reduction in the amount of delaminated area when a back-up plate is placed under the specimen.

  20. Numerical investigation of the effect of delaminations on fracture characteristics of glare

    Science.gov (United States)

    Bhat, Sunil; Narayanan, S.

    2013-10-01

    A finite element examination of the effect of delaminations on fracture characteristics of fibre metal laminate (Glare), by comparing energy release rates of normal cracks in laminates with and without delaminations, is presented in the paper. Glare comprising thin cracked 2024-T3 aerospace aluminum alloy layers alternately bonded with E-glass fibre based composite prepregs is considered for the analysis. Delaminations are modeled with interface cohesive elements. Energy release rates of normal cracks in laminates with delaminations are found to be higher than those in the laminates without delaminations.

  1. Delaminated sodium nonatitanate and a method for producing delaminated sodium nonatitanate

    Science.gov (United States)

    Nyman, May D.

    2016-02-02

    A hydrothermal synthesis method of making a delaminated titanate is disclosed. The delaminated titanate has a unique structure or morphology. The delaminated titanate is first formed by forming at a low temperature a layered sodium nonatitanate (SNT), which may be referred to as layered sodium titanate. The layered SNT has a unique morphology. The layered SNT is then synthesized into a delaminated titanate having a unique morphology.

  2. Delaminated rotator cuff tear: extension of delamination and cuff integrity after arthroscopic rotator cuff repair.

    Science.gov (United States)

    Gwak, Heui-Chul; Kim, Chang-Wan; Kim, Jung-Han; Choo, Hye-Jeung; Sagong, Seung-Yeob; Shin, John

    2015-05-01

    The purpose of this study was to evaluate the extension of delamination and the cuff integrity after arthroscopic repair of delaminated rotator cuff tears. Sixty-five patients with delaminated rotator cuff tears were retrospectively reviewed. The delaminated tears were divided into full-thickness delaminated tears and partial-thickness delaminated tears. To evaluate the medial extension, we calculated the coronal size of the delaminated portion. To evaluate the posterior extension, we checked the tendon involved. Cuff integrity was evaluated by computed tomography arthrography. The mean medial extension in the full-thickness and partial-thickness delaminated tears was 18.1 ± 6.0 mm and 22.7 ± 6.3 mm, respectively (P = .0084). The posterior extension into the supraspinatus and the infraspinatus was 36.9% and 32.3%, respectively, in the full-thickness delaminated tears, and it was 27.7% and 3.1%, respectively, in the partial-thickness delaminated tears (P = .0043). With regard to cuff integrity, 35 cases of anatomic healing, 10 cases of partial healing defects, and 17 cases of retear were detected. Among the patients with retear and partial healing of the defect, all the partially healed defects showed delamination. Three retear patients showed delamination, and 14 retear patients did not show delamination; the difference was statistically significant (P = .0001). The full-thickness delaminated tears showed less medial extension and more posterior extension than the partial-thickness delaminated tears. Delamination did not develop in retear patients, but delamination was common in the patients with partially healed defects. Copyright © 2015 Journal of Shoulder and Elbow Surgery Board of Trustees. Published by Elsevier Inc. All rights reserved.

  3. The Effect of Substrate Topography on Coating Cathodic Delamination

    DEFF Research Database (Denmark)

    Erik Weinell, Claus; Sørensen, Per A.; Kiil, Søren

    2011-01-01

    This article describes the effect of steel substrate topography on coating cathodic delamination. The study showed that the surface preparation can be used to control and minimize the rate of cathodic delamination. The coating should have maximum wetting properties so that substrates with high...

  4. Delamination of Composite Cylinders

    Science.gov (United States)

    Davies, Peter; Carlsson, Leif A.

    The delamination resistance of filament wound glass/epoxy cylinders has been characterized for a range of winding angles and fracture mode ratios using beam fracture specimens. The results reveal that the delamination fracture resistance increases with increasing winding angle and mode II (shear) fraction (GΠ/G). It was also found that interlaced fiber bundles in the filament wound cylinder wall acted as effective crack arresters in mode I loading. To examine the sensitivity of delamina-tion damage on the strength of the cylinders, external pressure tests were performed on filament-wound glass/epoxy composite cylinders with artificial defects and impact damage. The results revealed that the cylinder strength was insensitive to the presence of single delaminations but impact damage caused reductions in failure pressure. The insensitivity of the failure pressure to a single delamination is attributed to the absence of buckling of the delaminated sublaminates before the cylinder wall collapsed. The impacted cylinders contained multiple delaminations, which caused local reduction in the compressive load capability and reduction in failure pressure. The response of glass/epoxy cylinders was compared to impacted carbon reinforced cylinders. Carbon/epoxy is more sensitive to damage but retains higher implosion resistance while carbon/PEEK shows the opposite trend.

  5. The coupled effects of thickness and delamination on cracking resistance of X70 pipeline steel

    International Nuclear Information System (INIS)

    Guo, W.; Dong, H.; Lu, M.; Zhao, X.

    2002-01-01

    The effects of thickness and delamination on the fracture toughness and stable crack growth behaviour of high-toughness pipeline steels were investigated experimentally by use of compact tension specimens with thicknesses of 3-15 mm cut from a 17 mm-thick wall pipe. Material resistance curves were generated based on the stress intensity factor (SIF) K and the J-integral. The critical SIF K c and the J-resistance curves are found to be independent of thickness as the delaminations near the crack tip within the material reduce the out-of-plane constraint in thicker specimens. Both fracture mechanism and mechanics analyses shown that the fracture behaviour of the steel is controlled by the strong-coupled effects of thickness and delaminations. With increasing thickness, the out-of-plane stress constraint increases and causes the inclusion separation, growth and coalescence to form delaminations of different sizes before the main crack initiates. The delaminations in turn, reduce the out-of-plane constraint and thus, the thickness effect upon fracture. The advantages and disadvantages of delaminations in a safety assessment of pipelines are also discussed based on three-dimensional fracture theory

  6. Influence of substrate topography on cathodic delamination of anticorrosive coatings

    DEFF Research Database (Denmark)

    Sørensen, Per Aggerholm; Kiil, Søren; Dam-Johansen, Kim

    2009-01-01

    and thereby the substrate topography, whereas the coating thickness had little influence. The presence of a significant potential gradient between the anode and the cathode and the dependency of the delamination rate on the tortuosity of the steel surface suggests that cathodic delamination is controlled...

  7. Optimization of Cutting Parameters on Delamination of Drilling Glass-Polyester Composites

    Directory of Open Access Journals (Sweden)

    Majid Habeeb Faidh-Allah

    2018-02-01

    Full Text Available This paper attempted to study the effect of cutting parameters (spindle speed and feed rate on delamination phenomena during the drilling glass-polyester composites. Drilling process was done by CNC machine with 10 mm diameter of high-speed steel (HSS drill bit. Taguchi technique with L16 orthogonal layout was used to analyze the effective parameters on delamination factor. The optimal experiment was no. 13 with spindle speed 1273 rpm and feed 0.05 mm/rev with minimum delamination factor 1.28.

  8. Mode I fatigue delamination growth in composite laminates with fibre bridging

    NARCIS (Netherlands)

    Yao, L.

    2015-01-01

    Advanced composite materials have been commonly used in aerospace engineering, because of their good mechanical properties and attractive potential for creating lightweight structures. Susceptibility to delamination is one of the most important issues in the applications of these materials. This

  9. Hygrothermal influence on delamination behavior of graphite/epoxy laminates

    Science.gov (United States)

    Garg, A.; Ishai, O.

    1985-01-01

    The hygrothermal effect on the fracture behavior of graphite-epoxy laminates was investigated to develop a methodology for damage tolerance predictions in advanced composite materials. Several T300/934 laminates were tested using a number of specimen configurations to evaluate the effects of temperature and humidity on delamination fracture toughness under mode 1 and mode 2 loading. It is indicated that moisture has a slightly beneficial influence on fracture toughness or critical strain energy release rate during mode 1 delamination, but has a slightly deleterious effect on mode 2 delamination, and mode 1 transverse cracking. The failed specimens are examined by SEM and topographical differences due to fracture modes are identified. It is concluded that the effect of moisture on fracture topography can not be distinguished.

  10. Microscopic mechanisms of graphene electrolytic delamination from metal substrates

    International Nuclear Information System (INIS)

    Fisichella, G.; Di Franco, S.; Roccaforte, F.; Giannazzo, F.; Ravesi, S.

    2014-01-01

    In this paper, hydrogen bubbling delamination of graphene (Gr) from copper using a strong electrolyte (KOH) water solution was performed, focusing on the effect of the KOH concentration (C KOH ) on the Gr delamination rate. A factor of ∼10 decrease in the time required for the complete Gr delamination from Cu cathodes with the same geometry was found increasing C KOH from ∼0.05 M to ∼0.60 M. After transfer of the separated Gr membranes to SiO 2 substrates by a highly reproducible thermo-compression printing method, an accurate atomic force microscopy investigation of the changes in Gr morphology as a function of C KOH was performed. Supported by these analyses, a microscopic model of the delamination process has been proposed, where a key role is played by graphene wrinkles acting as nucleation sites for H 2 bubbles at the cathode perimeter. With this approach, the H 2 supersaturation generated at the electrode for different electrolyte concentrations was estimated and the inverse dependence of t d on C KOH was quantitatively explained. Although developed in the case of Cu, this analysis is generally valid and can be applied to describe the electrolytic delamination of graphene from several metal substrates.

  11. Edge delamination of composite laminates subject to combined tension and torsional loading

    Science.gov (United States)

    Hooper, Steven J.

    1990-01-01

    Delamination is a common failure mode of laminated composite materials. Edge delamination is important since it results in reduced stiffness and strength of the laminate. The tension/torsion load condition is of particular significance to the structural integrity of composite helicopter rotor systems. Material coupons can easily be tested under this type of loading in servo-hydraulic tension/torsion test stands using techniques very similar to those used for the Edge Delamination Tensile Test (EDT) delamination specimen. Edge delamination of specimens loaded in tension was successfully analyzed by several investigators using both classical laminate theory and quasi-three dimensional (Q3D) finite element techniques. The former analysis technique can be used to predict the total strain energy release rate, while the latter technique enables the calculation of the mixed-mode strain energy release rates. The Q3D analysis is very efficient since it produces a three-dimensional solution to a two-dimensional domain. A computer program was developed which generates PATRAN commands to generate the finite element model. PATRAN is a pre- and post-processor which is commonly used with a variety of finite element programs such as MCS/NASTRAN. The program creates a sufficiently dense mesh at the delamination crack tips to support a mixed-mode fracture mechanics analysis. The program creates a coarse mesh in those regions where the gradients in the stress field are low (away from the delamination regions). A transition mesh is defined between these regions. This program is capable of generating a mesh for an arbitrarily oriented matrix crack. This program significantly reduces the modeling time required to generate these finite element meshes, thus providing a realistic tool with which to investigate the tension torsion problem.

  12. Delamination of Compressed Thin Layers at Corners

    DEFF Research Database (Denmark)

    Sørensen, Kim D.; Jensen, Henrik Myhre; Clausen, Johan

    2008-01-01

    An analysis of delamination for a thin elastic layer under compression, attached to a substrate at a corner is carried out. The analysis is performed by combining results from interface fracture mechanics and the theory of thin shells. In contrast with earlier results for delamination on a flat s...... layers, Fracture mechanics, Crack closure, Steady state crack propagation.......An analysis of delamination for a thin elastic layer under compression, attached to a substrate at a corner is carried out. The analysis is performed by combining results from interface fracture mechanics and the theory of thin shells. In contrast with earlier results for delamination on a flat...... results for the fracture mechanical properties have been obtained, and these are applied in a study of the effect of contacting crack faces. Special attention has been given to analyse conditions under which steady state propagation of buckling driven delamination takes place. Keywords: Delamination, Thin...

  13. Delamination detection using methods of computational intelligence

    Science.gov (United States)

    Ihesiulor, Obinna K.; Shankar, Krishna; Zhang, Zhifang; Ray, Tapabrata

    2012-11-01

    Abstract Reliable delamination prediction scheme is indispensable in order to prevent potential risks of catastrophic failures in composite structures. The existence of delaminations changes the vibration characteristics of composite laminates and hence such indicators can be used to quantify the health characteristics of laminates. An approach for online health monitoring of in-service composite laminates is presented in this paper that relies on methods based on computational intelligence. Typical changes in the observed vibration characteristics (i.e. change in natural frequencies) are considered as inputs to identify the existence, location and magnitude of delaminations. The performance of the proposed approach is demonstrated using numerical models of composite laminates. Since this identification problem essentially involves the solution of an optimization problem, the use of finite element (FE) methods as the underlying tool for analysis turns out to be computationally expensive. A surrogate assisted optimization approach is hence introduced to contain the computational time within affordable limits. An artificial neural network (ANN) model with Bayesian regularization is used as the underlying approximation scheme while an improved rate of convergence is achieved using a memetic algorithm. However, building of ANN surrogate models usually requires large training datasets. K-means clustering is effectively employed to reduce the size of datasets. ANN is also used via inverse modeling to determine the position, size and location of delaminations using changes in measured natural frequencies. The results clearly highlight the efficiency and the robustness of the approach.

  14. Synthesis of mullite nanometers microwave from bentonite delaminated

    International Nuclear Information System (INIS)

    Gomes, J.; Azevedo, N.A.; Vieira, D.A.; Neves, G.A.; Santana, L.N.L.; Menezes, R.R.

    2011-01-01

    The smectite clays present as lamellar structure is formed by two layers of silica tetrahedrons and one layer of aluminum octahedra, which can be individually delaminated, reaching a thickness of about 1mm. Mullite is the only thermodynamically stable crystalline phase of SiO 2 and Al2O 3 system and can be synthesized from minerals that exhibit these oxides in its composition. The microwave synthesis offers advantages over conventional methods, the heating is rapid and uniform, avoiding an undesirable grain growth. This study aims to obtain nanometric mullite from bentonites delamined subjected to microwave heating. The samples were initially treated, then rehydrated, frozen and deagglomeration in a ball mill for 4 and 8 hours. Subsequently subjected to centrifugation, drying and microwave heating. The results showed that nano-mullite was obtained for samples subjected to longer heating and dispersions. (author)

  15. In Search of a Time Efficient Approach to Crack and Delamination Growth Predictions in Composites

    Science.gov (United States)

    Krueger, Ronald; Carvalho, Nelson

    2016-01-01

    Analysis benchmarking was used to assess the accuracy and time efficiency of algorithms suitable for automated delamination growth analysis. First, the Floating Node Method (FNM) was introduced and its combination with a simple exponential growth law (Paris Law) and Virtual Crack Closure technique (VCCT) was discussed. Implementation of the method into a user element (UEL) in Abaqus/Standard(Registered TradeMark) was also presented. For the assessment of growth prediction capabilities, an existing benchmark case based on the Double Cantilever Beam (DCB) specimen was briefly summarized. Additionally, the development of new benchmark cases based on the Mixed-Mode Bending (MMB) specimen to assess the growth prediction capabilities under mixed-mode I/II conditions was discussed in detail. A comparison was presented, in which the benchmark cases were used to assess the existing low-cycle fatigue analysis tool in Abaqus/Standard(Registered TradeMark) in comparison to the FNM-VCCT fatigue growth analysis implementation. The low-cycle fatigue analysis tool in Abaqus/Standard(Registered TradeMark) was able to yield results that were in good agreement with the DCB benchmark example. Results for the MMB benchmark cases, however, only captured the trend correctly. The user element (FNM-VCCT) always yielded results that were in excellent agreement with all benchmark cases, at a fraction of the analysis time. The ability to assess the implementation of two methods in one finite element code illustrated the value of establishing benchmark solutions.

  16. Cathodic delamination of seawater-immersed anticorrosive coatings: Mapping of parameters affecting the rate

    DEFF Research Database (Denmark)

    Sørensen, Per Aggerholm; Dam-Johansen, Kim; Weinell, C. E.

    2010-01-01

    Abstract: Cathodic delamination is one of the major modes of failure for organic coatings immersed in seawater and refers to the weakening or loss of adhesion between the coating and the substrate. The diminished adhesion is the result of electrochemical reactions occurring at the coating...

  17. Effects of surface roughness, texture and polymer degradation on cathodic delamination of epoxy coated steel samples

    International Nuclear Information System (INIS)

    Khun, N.W.; Frankel, G.S.

    2013-01-01

    Highlights: ► Cathodic delamination of epoxy coated steel samples was studied using SKP. ► Delamination of the coating decreased with increased substrate surface roughness. ► Delamination of the coating was faster on the substrate with parallel surface scratches. ► Delamination of the coating exposed to weathering conditions increased with prolonged exposure. - Abstract: The Scanning Kelvin Probe (SKP) technique was used to investigate the effects of surface roughness, texture and polymer degradation on cathodic delamination of epoxy coated steel. The cathodic delamination rate of the epoxy coatings dramatically decreased with increased surface roughness of the underlying steel substrate. The surface texture of the steel substrates also had a significant effect in that samples with parallel abrasion lines exhibiting faster cathodic delamination in the direction of the lines compared to the direction perpendicular to the lines. The cathodic delamination kinetics of epoxy coatings previously exposed to weathering conditions increased with prolonged exposure due to pronounced polymer degradation. SEM observation confirmed that the cyclic exposure to UV radiation and water condensation caused severe deterioration in the polymer structures with surface cracking and erosion. The SKP results clearly showed that the cathodic delamination of the epoxy coatings was significantly influenced by the surface features of the underlying steel substrates and the degradation of the coatings.

  18. Experimental Characterization and Cohesive Laws for Delamination of Off-Axis GFRP Laminates

    DEFF Research Database (Denmark)

    Lindgaard, Esben; Bak, Brian Lau Verndal

    2015-01-01

    This work experimentally characterizes mixed mode delamination in glass fibre reinforced polymer laminates taking into account the influence of the off-axis angle between the lamina orientation and the crack growth direction on the fracture properties. Thus, providing a cohesive law that enables...... analysis of 3D models in which mixed mode crack growth within laminates having anisotropic fracture properties takes place....

  19. Analysis of a 'barb test' for measuring the mixed-mode delamination toughness of coatings

    International Nuclear Information System (INIS)

    Liu Yufu; Kagawa, Y.; Evans, A.G.

    2008-01-01

    The durability of thermal barrier coatings (TBCs) employed in most turbine engines is limited by delamination, both within the coating and at the coating-substrate interface. A test used for evaluating the mixed-mode toughness pertinent to such delaminations has been fully-analyzed by determining the steady-state energy release rate, the mode mixity and the critical length for buckling. An analytic solution based on beam theory establishes basic estimates and scaling relationships. Selected finite-element calculations have been used to affirm the fidelity of the results. The energy release rate attains steady-state, but the phase angle changes throughout because of a small (but significant) bending moment induced at the supports. The coating buckles at a critical delamination length, whereupon the energy release rate increases rapidly and violates steady state. The solutions are used to re-interpret measurements reported in the literature for an electron beam physically deposited TBC

  20. Quasistatic delamination models for Kirchhoff-Love plates

    Czech Academy of Sciences Publication Activity Database

    Freddi, L.; Paroni, R.; Roubíček, Tomáš; Zanini, Ch.

    2011-01-01

    Roč. 91, č. 11 (2011), s. 845-865 ISSN 0044-2267 R&D Projects: GA ČR(CZ) GAP201/10/0357 Institutional research plan: CEZ:AV0Z20760514 Keywords : brittle delamination * adhesive contact * rate-independent processes Subject RIV: BA - General Mathematics Impact factor: 0.863, year: 2011 http://onlinelibrary.wiley.com/doi/10.1002/zamm.201000171/abstract

  1. Delamination Detection of Reinforced Concrete Decks Using Modal Identification

    Directory of Open Access Journals (Sweden)

    Shutao Xing

    2012-01-01

    Full Text Available This study addressed delamination detection of concrete slabs by analyzing global dynamic responses of structures. Both numerical and experimental studies are presented. In the numerical examples, delaminations with different sizes and locations were introduced into a concrete slab; the effects of presence, sizes, and locations of delaminations on the modal frequencies and mode shapes of the concrete slab under various support conditions were studied. In the experimental study, four concrete deck specimens with different delamination sizes were constructed, and experimental tests were conducted. Traditional peak-picking, frequency domain decomposition, and stochastic subspace identification methods were applied to the modal identification from dynamic response measurements. The modal parameters identified by these three methods correlated well. The changes in modal frequencies, damping ratios, and mode shapes that were extracted from the dynamic measurements were investigated and correlated to the actual delaminations and can indicate presence and severity of delamination. Finite element (FE models of reinforced concrete decks with different delamination sizes and locations were established. The modal parameters computed from the FE models were compared to those obtained from the laboratory specimens, and the FE models were validated. The delamination detection approach was proved to be effective for concrete decks on beams.

  2. Numerical simulations of the mantle lithosphere delamination

    Science.gov (United States)

    Morency, C.; Doin, M.-P.

    2004-03-01

    Sudden uplift, extension, and increased igneous activity are often explained by rapid mechanical thinning of the lithospheric mantle. Two main thinning mechanisms have been proposed, convective removal of a thickened lithospheric root and delamination of the mantle lithosphere along the Moho. In the latter case, the whole mantle lithosphere peels away from the crust by the propagation of a localized shear zone and sinks into the mantle. To study this mechanism, we perform two-dimensional (2-D) numerical simulations of convection using a viscoplastic rheology with an effective viscosity depending strongly on temperature, depth, composition (crust/mantle), and stress. The simulations develop in four steps. (1) We first obtain "classical" sublithospheric convection for a long time period (˜300 Myr), yielding a slightly heterogeneous lithospheric temperature structure. (2) At some time, in some simulations, a strong thinning of the mantle occurs progressively in a small area (˜100 km wide). This process puts the asthenosphere in direct contact with the lower crust. (3) Large pieces of mantle lithosphere then quickly sink into the mantle by the horizontal propagation of a detachment level away from the "asthenospheric conduit" or by progressive erosion on the flanks of the delaminated area. (4) Delamination pauses or stops when the lithospheric mantle part detaches or when small-scale convection on the flanks of the delaminated area is counterbalanced by heat diffusion. We determine the parameters (crustal thicknesses, activation energies, and friction coefficients) leading to delamination initiation (step 2). We find that delamination initiates where the Moho temperature is the highest, as soon as the crust and mantle viscosities are sufficiently low. Delamination should occur on Earth when the Moho temperature exceeds ˜800°C. This condition can be reached by thermal relaxation in a thickened crust in orogenic setting or by corner flow lithospheric erosion in the

  3. Guided Wave Delamination Detection and Quantification With Wavefield Data Analysis

    Science.gov (United States)

    Tian, Zhenhua; Campbell Leckey, Cara A.; Seebo, Jeffrey P.; Yu, Lingyu

    2014-01-01

    Unexpected damage can occur in aerospace composites due to impact events or material stress during off-nominal loading events. In particular, laminated composites are susceptible to delamination damage due to weak transverse tensile and inter-laminar shear strengths. Developments of reliable and quantitative techniques to detect delamination damage in laminated composites are imperative for safe and functional optimally-designed next-generation composite structures. In this paper, we investigate guided wave interactions with delamination damage and develop quantification algorithms by using wavefield data analysis. The trapped guided waves in the delamination region are observed from the wavefield data and further quantitatively interpreted by using different wavenumber analysis methods. The frequency-wavenumber representation of the wavefield shows that new wavenumbers are present and correlate to trapped waves in the damage region. These new wavenumbers are used to detect and quantify the delamination damage through the wavenumber analysis, which can show how the wavenumber changes as a function of wave propagation distance. The location and spatial duration of the new wavenumbers can be identified, providing a useful means not only for detecting the presence of delamination damage but also allowing for estimation of the delamination size. Our method has been applied to detect and quantify real delamination damage with complex geometry (grown using a quasi-static indentation technique). The detection and quantification results show the location, size, and shape of the delamination damage.

  4. Finite elements modeling of delaminations in composite laminates

    DEFF Research Database (Denmark)

    Gaiotti, m.; Rizzo, C.M.; Branner, Kim

    2011-01-01

    of the buckling strength of composite laminates containing delaminations. Namely, non-linear buckling and post-buckling analyses are carried out to predict the critical buckling load of elementary composite laminates affected by rectangular delaminations of different sizes and locations, which are modelled......The application of composite materials in many structures poses to engineers the problem to create reliable and relatively simple methods, able to estimate the strength of multilayer composite structures. Multilayer composites, like other laminated materials, suffer from layer separation, i.......e., delaminations, which may affect the stiffness and stability of structural components. Especially deep delaminations in the mid surface of laminates are expected to reduce the effective flexural stiffness and lead to collapse, often due to buckling behaviour. This paper deals with the numerical modelling...

  5. Edge Delamination of Monolayer Transition Metal Dichalcogenides.

    Science.gov (United States)

    Ly, Thuc Hue; Yun, Seok Joon; Thi, Quoc Huy; Zhao, Jiong

    2017-07-25

    Delamination of thin films from the supportive substrates is a critical issue within the thin film industry. The emergent two-dimensional, atomic layered materials, including transition metal dichalcogenides, are highly flexible; thus buckles and wrinkles can be easily generated and play vital roles in the corresponding physical properties. Here we introduce one kind of patterned buckling behavior caused by the delamination from a substrate initiated at the edges of the chemical vapor deposition synthesized monolayer transition metal dichalcogenides, led by thermal expansion mismatch. The atomic force microscopy and optical characterizations clearly showed the puckered structures associated with the strain, whereas the transmission electron microscopy revealed the special sawtooth-shaped edges, which break the geometrical symmetry for the buckling behavior of hexagonal samples. The condition of the edge delamination is in accordance with the fracture behavior of thin film interfaces. This edge delamination and buckling process is universal for most ultrathin two-dimensional materials, which requires more attention in various future applications.

  6. Delamination of Compressed Thin Layers at Corners

    DEFF Research Database (Denmark)

    Sørensen, Kim D.; Jensen, Henrik Myhre; Clausen, Johan

    2008-01-01

    An analysis of delamination for a thin elastic layer under compression, attached to a substrate at a corner is carried out. The analysis is performed by combining results from interface fracture mechanics and the theory of thin shells. In contrast with earlier results for delamination on a flat...

  7. Experimental evaluation of coating delamination in vinyl coated metal forming

    International Nuclear Information System (INIS)

    Son, Young Ki; Lee, Chan Joo; Kim, Byung Min; Lee, Jung Min; Byoen, Sang Doek; Lee, Soen Bong

    2012-01-01

    In this paper, a new evaluation and prediction method for coating delamination during sheet metal forming is presented. On the basis of the forming limit diagram (FLD), the current study evaluates the delamination of PET coating by using a cross cut specimen, dome test, and rectangular cup drawing test. Dome test specimens were subjected to biaxial, plane strain, and uniaxial deformation modes. Rectangular cup drawing test specimens were subjected to the deep drawing deformation mode, and compression deformation mode. A vinyl coated metal (VCM) sheet consists of three layers of polymer on the sheet metals: a protective film, a PET layer and a PVC layer. The areas with coating delamination were identified, and the results of the evaluation were plotted according to major and minor strain values, depicting coating delamination. The constructed delamination limit diagram (DLD) can be used to determine the forming limit of VCM during the complex press forming process. ARGUS (GOM) was employed to identify the strain value and deformation mode of the delaminated surface after the press forming. After identifying the areas of delamination, the DLD of the PET coating can be constructed in a format similar to that of the FLD. The forming limit of the VCM sheet can be evaluated using the superimposition of the delamination limit strain of the coating onto the FLD of VCM sheet. The experimental results showed that the proposed test method will support the sheet metal forming process design for VCM sheets. The assessment method presented in this study can be used to determine the delamination limit strain under plastic deformation of other polymer coated metals. The experimental results suggested that the proposed testing method is effective in evaluating delamination for specific applications

  8. Experimental evaluation of coating delamination in vinyl coated metal forming

    Energy Technology Data Exchange (ETDEWEB)

    Son, Young Ki; Lee, Chan Joo; Kim, Byung Min [Pusan National Univ., Busan (Korea, Republic of); Lee, Jung Min [Korea Institute of Industrial Technology, Busan (Korea, Republic of); Byoen, Sang Doek [HA Digital Engineering Gr., Seongsan Gu (Korea, Republic of); Lee, Soen Bong [Keimyung Univ., Daegu (Korea, Republic of)

    2012-10-15

    In this paper, a new evaluation and prediction method for coating delamination during sheet metal forming is presented. On the basis of the forming limit diagram (FLD), the current study evaluates the delamination of PET coating by using a cross cut specimen, dome test, and rectangular cup drawing test. Dome test specimens were subjected to biaxial, plane strain, and uniaxial deformation modes. Rectangular cup drawing test specimens were subjected to the deep drawing deformation mode, and compression deformation mode. A vinyl coated metal (VCM) sheet consists of three layers of polymer on the sheet metals: a protective film, a PET layer and a PVC layer. The areas with coating delamination were identified, and the results of the evaluation were plotted according to major and minor strain values, depicting coating delamination. The constructed delamination limit diagram (DLD) can be used to determine the forming limit of VCM during the complex press forming process. ARGUS (GOM) was employed to identify the strain value and deformation mode of the delaminated surface after the press forming. After identifying the areas of delamination, the DLD of the PET coating can be constructed in a format similar to that of the FLD. The forming limit of the VCM sheet can be evaluated using the superimposition of the delamination limit strain of the coating onto the FLD of VCM sheet. The experimental results showed that the proposed test method will support the sheet metal forming process design for VCM sheets. The assessment method presented in this study can be used to determine the delamination limit strain under plastic deformation of other polymer coated metals. The experimental results suggested that the proposed testing method is effective in evaluating delamination for specific applications.

  9. Integrated global digital image correlation for interface delamination characterization

    KAUST Repository

    Hoefnagels, Johan P.M.

    2013-07-23

    Interfacial delamination is a key reliability challenge in composites and micro-electronic systems due to (high-density) integration of dissimilar materials. Predictive finite element models are used to minimize delamination failures during design, but require accurate interface models to capture (irreversible) crack initiation and propagation behavior observed in experiments. Therefore, an Integrated Global Digital Image Correlation (I-GDIC) strategy is developed for accurate determination of mechanical interface behavior from in-situ delamination experiments. Recently, a novel miniature delamination setup was presented that enables in-situ microscopic characterization of interface delamination while sensitively measuring global load-displacement curves for all mode mixities. Nevertheless, extraction of detailed mechanical interface behavior from measured images is challenging, because deformations are tiny and measurement noise large. Therefore, an advanced I-GDIC methodology is developed which correlates the image patterns by only deforming the images using kinematically-admissible \\'eigenmodes\\' that correspond to the few parameters controlling the interface tractions in an analytic description of the crack tip deformation field, thereby greatly enhancing accuracy and robustness. This method is validated on virtual delamination experiments, simulated using a recently developed self-adaptive cohesive zone (CZ) finite element framework. © The Society for Experimental Mechanics, Inc. 2014.

  10. Non-destructive delamination detection in solid oxide fuel cells

    Energy Technology Data Exchange (ETDEWEB)

    Gazzarri, J.I.; Kesler, O. [Department of Mechanical Engineering, University of British Columbia, 2054-6250 Applied Science Lane, Vancouver, BC V6T 1Z4 (Canada)

    2007-05-15

    A finite element model has been developed to simulate the steady state and impedance behaviour of a single operating solid oxide fuel cell (SOFC). The model results suggest that electrode delamination can be detected minimally-invasively by using electrochemical impedance spectroscopy. The presence of cathode delamination causes changes in the cell impedance spectrum that are characteristic of this type of degradation mechanism. These changes include the simultaneous increase in both the series and polarization resistances, in proportion to the delaminated area. Parametric studies show the dependence of these changes on the extent of delamination, on the operating point, and on the kinetic characteristics of the fuel cell under study. (author)

  11. Scattering of guided waves at delaminations in composite plates.

    Science.gov (United States)

    Murat, Bibi I S; Khalili, Pouyan; Fromme, Paul

    2016-06-01

    Carbon fiber laminate composites are increasingly employed for aerospace structures as they offer advantages, such as a good strength to weight ratio. However, impact during the operation and servicing of the aircraft can lead to barely visible and difficult to detect damage. Depending on the severity of the impact, fiber and matrix breakage or delaminations can occur, reducing the load carrying capacity of the structure. Efficient nondestructive testing and structural health monitoring of composite panels can be achieved using guided ultrasonic waves propagating along the structure. The scattering of the A0 Lamb wave mode at delaminations was investigated using a full three-dimensional (3D) finite element (FE) analysis. The influence of the delamination geometry (size and depth) was systematically evaluated. In addition to the depth dependency, a significant influence of the delamination width due to sideways reflection of the guided waves within the delamination area was found. Mixed-mode defects were simulated using a combined model of delamination with localized material degradation. The guided wave scattering at cross-ply composite plates with impact damage was measured experimentally using a non-contact laser interferometer. Good agreement between experiments and FE predictions using the mixed-mode model for an approximation of the impact damage was found.

  12. Simulation of delamination crack growth in composite laminates: application of local and non-local interface damage models

    International Nuclear Information System (INIS)

    Ijaz, H.; Asad, M.

    2015-01-01

    The use of composite laminates is increasing in these days due to higher strength and low density values in comparison of metals. Delamination is a major source of failure in composite laminates. Damage mechanics based theories are employed to simulate the delamination phenomena between composite laminates. These damage models are inherently local and can cause the concentration of stresses around the crack tip. In the present study integral type non-local damage formulation is proposed to avoid the localization problem associated to damage formulation. A comprehensive study is carried out for the models and classical local damage model are performed and results are compared with available experimental data for un IMS/924 Carbon/fiber epoxy composite laminate. (author)

  13. Failure analysis of multiple delaminated composite plates due

    Indian Academy of Sciences (India)

    The present work aims at the first ply failure analysis of laminated composite plates with arbitrarily located multiple delaminations subjected to transverse static load as well as impact. The theoretical formulation is based on a simple multiple delamination model. Conventional first order shear deformation is assumed using ...

  14. Floating Carpets and the Delamination of Elastic Sheets

    KAUST Repository

    Wagner, Till J. W.

    2011-07-22

    We investigate the deformation of a thin elastic sheet floating on a liquid surface and subject to a uniaxial compression. We show that at a critical compression the sheet delaminates from the liquid over a finite region forming a delamination "blister." This blistering regime adds to the wrinkling and localized folding regimes that have been studied previously. The transition from wrinkled to blistered states occurs when delamination becomes energetically favorable compared with wrinkling. We determine the initial blister size and the evolution of blister size with continuing compression before verifying our theoretical results with experiments at a macroscopic scale. © 2011 American Physical Society.

  15. Numerical Investigation of Delamination in Drilling of Carbon Fiber Reinforced Polymer Composites

    Science.gov (United States)

    Tang, Wenliang; Chen, Yan; Yang, Haojun; Wang, Hua; Yao, Qiwei

    2018-03-01

    Drilling of carbon fiber reinforced polymer (CFRP) is a challenging task in modern manufacturing sector and machining induced delamination is one of the major problems affecting assembly precision. In this work, a new three-dimensional (3D) finite element model is developed to study the chip formation and entrance delamination in drilling of CFRP composites on the microscopic level. Fiber phase, matrix phase and equivalent homogeneous phase in the multi-phase model have different constitutive behaviors, respectively. A comparative drilling test, in which the cement carbide drill and unidirectional CFRP laminate are employed, is conducted to validate the proposedmodel in terms of the delamination and the similar changing trend is obtained. Microscopic mechanism of entrance delamination together with the chip formation process at four special fiber cutting angles (0°, 45°, 90° and 135°) is investigated. Moreover, the peeling force is also predicted. The results show that the delamination occurrence and the chip formation are both strongly dependent on the fiber cutting angle. The length of entrance delamination rises with increasing fiber cutting angles. Negligible delamination at 0° is attributed to the compression by the minor flank face. For 45° and 90°, the delamination resulted from the mode III fracture. At 135°, serious delamination which is driven by the mode I and III fractures is more inclined to occur and the peeling force reaches its maximum. Such numerical models can help understand the mechanism of hole entrance delamination further and provide guidance for the damage-free drilling of CFRP.

  16. Study of multilayer packaging delamination mechanisms using different surface analysis techniques

    Energy Technology Data Exchange (ETDEWEB)

    Garrido-Lopez, Alvaro [Department of Chemistry, University of La Rioja, C/Madre de Dios 51, E-26006 Logrono, La Rioja (Spain); Tena, Maria Teresa, E-mail: maria-teresa.tena@unirioja.es [Department of Chemistry, University of La Rioja, C/Madre de Dios 51, E-26006 Logrono, La Rioja (Spain)

    2010-04-01

    Multilayer packaging, consisting of different layers joined by using an adhesive or an extrusion process, is widely used to promote different products, such as food, cosmetics, etc. The main disadvantage in using this form of packaging is the delamination process. In this work, different surface techniques (X-ray photoelectron spectroscopy, time-of-flight secondary ion mass spectroscopy and attenuated total reflection Fourier transform infrared spectroscopy) are used to analyse the delaminated surfaces in order to study the mechanisms that cause delamination of multilayer packaging. According to our results, the reaction of migrated molecules with adhesive-aluminium bonds is the main cause of the chemical delamination process. In contrast, the delamination of extruded materials would seem to be caused by the breaking of Van der Waals bonds.

  17. Study on drilling induced delamination of woven kenaf fiber reinforced epoxy composite using carbide drills

    Science.gov (United States)

    Suhaily, M.; Hassan, C. H. Che; Jaharah, A. G.; Azmi, H.; Afifah, M. A.; Khairusshima, M. K. Nor

    2018-04-01

    In this research study, it presents the influences of drilling parameters on the delamination factor during the drilling of woven kenaf fiber reinforced epoxy composite laminates when using the carbide drill bits. The purpose of this study is to investigate the influence of drilling parameters such as cutting speed, feed rate and drill sizes on the delamination produced when drilling woven kenaf reinforced epoxy composite using the non-coated carbide drill bits. The damage generated on the woven kenaf reinforced epoxy composite laminates were observed both at the entrance and exit surface during the drilling operation. The experiments were conducted according to the Box Behnken experimental designs. The results indicated that the drill diameter has a significant influence on the delamination when drilling the woven kenaf fiber reinforced epoxy composites.

  18. Characterization of Blistering and Delamination in Depleted Uranium Hohlraums

    Energy Technology Data Exchange (ETDEWEB)

    Biobaum, K. J. M.

    2013-03-01

    Blistering and delamination are the primary failure mechanisms during the processing of depleted uranium (DU) hohlraums. These hohlraums consist of a sputter-deposited DU layer sandwiched between two sputter-deposited layers of gold; a final thick gold layer is electrodeposited on the exterior. The hohlraum is deposited on a copper-coated aluminum mandrel; the Al and Cu are removed with chemical etching after the gold and DU layers are deposited. After the mandrel is removed, blistering and delamination are observed on the interiors of some hohlraums, particularly at the radius region. It is hypothesized that blisters are caused by pinholes in the copper and gold layers; etchant leaking through these holes reaches the DU layer and causes it to oxidize, resulting in a blister. Depending on the residual stress in the deposited layers, blistering can initiate larger-scale delamination at layer interfaces. Scanning electron microscopy indicates that inhomogeneities in the machined aluminum mandrel are replicated in the sputter-deposited copper layer. Furthermore, the Cu layer exhibits columnar growth with pinholes that likely allow etchant to come in contact with the gold layer. Any inhomogeneities or pinholes in this initial gold layer then become nucleation sites for blistering. Using a focused ion beam system to etch through the gold layer and extract a cross-sectional sample for transmission electron microscopy, amorphous, intermixed layers at the gold/DU interfaces are observed. Nanometer-sized bubbles in the sputtered and electrodeposited gold layers are also present. Characterization of the morphology and composition of the deposited layers is the first step in determining modifications to processing parameters, with the goal of attaining a significant improvement in hohlraum yield.

  19. Repair of prestressed concrete cylinder with localized delamination

    International Nuclear Information System (INIS)

    Wang, Shen; Munshi, Javeed A.

    2015-01-01

    For prestressed concrete cylindrical structures such as nuclear containments, tanks and silos, the curvature effect of the tendons introduces radial tensile stresses in the concrete shell which are generally neglected in the design of such structures. For example, many prestressed concrete nuclear containments in US, especially those which were not designed following radial reinforcement requirement of ACI-359, are reinforced only in the circumferential (hoop) and meridional (vertical) directions but not in the radial direction. This leaves these structures vulnerable to potential laminar cracking and delamination, especially during post-tensioning and/or detensioning process. Should delamination occur, the structure needs to be repaired by either replacing cracked concrete or by “pinning” the delaminated concrete layers together by post-installed anchors. The latter option of post-installed anchors is less invasive from construction stand point and generally suitable for repairing small or localized delamination only. A comprehensive study is undertaken to explore various aspects and design consideration of post-installed anchors for prestressed concrete cylinders. The radial tension demand is first established by combining a mechanical based model with a detailed finite element analysis. With such design demand for post-installed anchors established, the next step aims at developing the tightness requirement of existing delamination cracks for effective use of post-installed anchors. A comprehensive literature search and evaluation is carried out for shear transfer capacity across cracks of various widths. The findings are used to develop specific recommendations for acceptable crack widths to ensure adequate in-plane shear transfer capacity for various design load conditions. A design process for post-installed anchors is proposed for repairing a delaminated prestressed concrete cylindrical structure at the end of the paper, supplemented by an illustrative

  20. Repair of prestressed concrete cylinder with localized delamination

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Shen, E-mail: swang@bechtel.com; Munshi, Javeed A., E-mail: jamunshi@bechtel.com

    2015-12-15

    For prestressed concrete cylindrical structures such as nuclear containments, tanks and silos, the curvature effect of the tendons introduces radial tensile stresses in the concrete shell which are generally neglected in the design of such structures. For example, many prestressed concrete nuclear containments in US, especially those which were not designed following radial reinforcement requirement of ACI-359, are reinforced only in the circumferential (hoop) and meridional (vertical) directions but not in the radial direction. This leaves these structures vulnerable to potential laminar cracking and delamination, especially during post-tensioning and/or detensioning process. Should delamination occur, the structure needs to be repaired by either replacing cracked concrete or by “pinning” the delaminated concrete layers together by post-installed anchors. The latter option of post-installed anchors is less invasive from construction stand point and generally suitable for repairing small or localized delamination only. A comprehensive study is undertaken to explore various aspects and design consideration of post-installed anchors for prestressed concrete cylinders. The radial tension demand is first established by combining a mechanical based model with a detailed finite element analysis. With such design demand for post-installed anchors established, the next step aims at developing the tightness requirement of existing delamination cracks for effective use of post-installed anchors. A comprehensive literature search and evaluation is carried out for shear transfer capacity across cracks of various widths. The findings are used to develop specific recommendations for acceptable crack widths to ensure adequate in-plane shear transfer capacity for various design load conditions. A design process for post-installed anchors is proposed for repairing a delaminated prestressed concrete cylindrical structure at the end of the paper, supplemented by an illustrative

  1. Critical current survival in the YBCO superconducting layer of a delaminated coated conductor

    Science.gov (United States)

    Feng, Feng; Fu, Qishu; Qu, Timing; Mu, Hui; Gu, Chen; Yue, Yubin; Wang, Linli; Yang, Zhirong; Han, Zhenghe; Feng, Pingfa

    2018-04-01

    A high-temperature superconducting coated conductor can be practically applied in electric equipment due to its favorable mechanical properties and critical current (I c) performance. However, the coated conductor can easily delaminate because of its poor stress tolerance along the thickness direction. It would be interesting to investigate whether the I c of the delaminated YBa2Cu3O7-δ (YBCO) layer can be preserved. In this study, coated conductor samples manufactured through the metal organic deposition route were delaminated by liquid nitrogen immersion. Delaminated samples, including the YBCO layer and silver stabilizer, were obtained. Delamination occurred inside the YBCO layer and near the YBCO-CeO2 interface, as suggested by the results of scanning electron microscopy (SEM) and x-ray diffraction. A scanning Hall probe system was employed to measure the I c distribution of the original sample and the delaminated sample. It was found that approximately 50% of the I c can be preserved after delamination, which was verified by I c measurements using the four-probe method. Dense and crack-free morphologies of the delaminated surfaces were observed by SEM, which accounts for the I c survival of the delaminated YBCO layer. The potential application of the delaminated sample in superconducting joints was discussed based on the oxygen diffusion estimation.

  2. MR imaging of delamination tears of the rotator cuff tendons

    International Nuclear Information System (INIS)

    Walz, Daniel M.; Chen, Steven; Miller, Theodore T.; Hofman, Josh

    2007-01-01

    The objective was to describe the imaging appearances and location of delamination tears of the rotator cuff tendons on non-contrast conventional MR imaging. This study was reviewed and approved by our Institutional Review Board. The reports of 548 consecutive MR examinations of the shoulder were reviewed, looking for mention or description of delamination tears of the rotator cuff. The images of the identified cases were then reviewed by two radiologists to confirm the findings. Correlation with surgical and arthroscopic information was then performed. Delamination tears were defined as horizontal retraction of either the bursal or articular surface of the tendon, manifest as thickening of the torn retracted edge, and/or interstitial splitting of the tendon, manifest as fluid-like high signal intensity on fat-suppressed T2-weighted oblique coronal images. Fourteen cases of delamination tears were identified in 13 patients. Ten of the cases involved the supraspinatus tendon, all with articular surface involvement. Nine of these supraspinatus cases were isolated tears and one occurred as part of a full thickness tear. All 10 of these supraspinatus cases showed medial retraction of the articular surface of the tendon, with thickening of the retracted edge, and 5 of the 10 had a demonstrable horizontal cleft in the interstitium. Four cases involved the subscapularis tendon, with articular surface disruption in three and pure interstitial delamination in one. Medial subluxation of the tendon of the long head of the biceps was present in all four cases. No delamination tears occurred on the bursal surface. Only three of the 14 shoulders underwent surgical repair with one confirmation of supraspinatus delamination, one confirmation of a subscapularis tear that had become a full thickness tear 10 months after initial imaging and another interstitial subscapularis delamination that was not identified arthroscopically. Delamination tears occur most often in the

  3. MR imaging of delamination tears of the rotator cuff tendons

    Energy Technology Data Exchange (ETDEWEB)

    Walz, Daniel M.; Chen, Steven [North Shore University Hospital, Department of Radiology, Manhasset, NY (United States); Miller, Theodore T. [Hospital for Special Surgery, Department of Radiology and Imaging, New York, NY (United States); Hofman, Josh [Long Island Jewish Medical Center, New Hyde Park, NY (United States)

    2007-05-15

    The objective was to describe the imaging appearances and location of delamination tears of the rotator cuff tendons on non-contrast conventional MR imaging. This study was reviewed and approved by our Institutional Review Board. The reports of 548 consecutive MR examinations of the shoulder were reviewed, looking for mention or description of delamination tears of the rotator cuff. The images of the identified cases were then reviewed by two radiologists to confirm the findings. Correlation with surgical and arthroscopic information was then performed. Delamination tears were defined as horizontal retraction of either the bursal or articular surface of the tendon, manifest as thickening of the torn retracted edge, and/or interstitial splitting of the tendon, manifest as fluid-like high signal intensity on fat-suppressed T2-weighted oblique coronal images. Fourteen cases of delamination tears were identified in 13 patients. Ten of the cases involved the supraspinatus tendon, all with articular surface involvement. Nine of these supraspinatus cases were isolated tears and one occurred as part of a full thickness tear. All 10 of these supraspinatus cases showed medial retraction of the articular surface of the tendon, with thickening of the retracted edge, and 5 of the 10 had a demonstrable horizontal cleft in the interstitium. Four cases involved the subscapularis tendon, with articular surface disruption in three and pure interstitial delamination in one. Medial subluxation of the tendon of the long head of the biceps was present in all four cases. No delamination tears occurred on the bursal surface. Only three of the 14 shoulders underwent surgical repair with one confirmation of supraspinatus delamination, one confirmation of a subscapularis tear that had become a full thickness tear 10 months after initial imaging and another interstitial subscapularis delamination that was not identified arthroscopically. Delamination tears occur most often in the

  4. Failure analysis of multiple delaminated composite plates due to ...

    Indian Academy of Sciences (India)

    Unknown

    plates are assumed to contain both single and multiple delaminations. For the case of impact, ... delamination on the first ply failure of the laminate is scarce. ..... 1 in the bottom layer, it was of the opposite sign for the top layer. The plots for ...

  5. Delamination Resistance Of Laminate Made With VBO MTM46/HTS Prepreg

    Directory of Open Access Journals (Sweden)

    Czarnocki Piotr

    2015-09-01

    Full Text Available A laminate made with the Vacuum Bag Only (VBO prepregs can be cured out of autoclave. Because of low curing pressure such a process can result in deterioration of laminate mechanical properties. They can be significantly lower than those displayed by the autoclave cured ones. The resistance against delamination can be among the most affected. Since this property is a week point of all the laminates it was of particular interest. Delamination resistance of unidirectional laminate made from VBO MTM46/HTS(12K prepreg was in the scope of the presented research and the critical values of the Strain Energy Release Rates and the Paris-type equations corresponding to Mode I, Mode II and Mixed-Mode I/II static and cyclic loadings, respectively, were determined.

  6. Zr-doped TiO{sub 2} supported on delaminated clay materials for solar photocatalytic treatment of emerging pollutants

    Energy Technology Data Exchange (ETDEWEB)

    Belver, C., E-mail: carolina.belver@uam.es; Bedia, J.; Rodriguez, J.J.

    2017-01-15

    Highlights: • Novel Zr-doped TiO{sub 2} delaminated clay materials were prepared by a sol-gel process. • Zr is incorporated into the anatase lattice. • Zr-TiO{sub 2} nanoparticles are homogenously distributed over the delaminated clay. • Zr doping enhances the photoactivity by reducing the band gap. • Degradation rates were favored at low concentrations and high radiation intensities. - Abstract: Solar light-active Zr-doped TiO{sub 2} nanoparticles were successfully immobilized on delaminated clay materials by a one-step sol-gel route. Fixing the amount of TiO{sub 2} at 65 wt.%, this work studies the influence of Zr loading (up to 2%) on the photocatalytic activity of the resulting Zr-doped TiO{sub 2}/clay materials. The structural characterization demonstrates that all samples were formed by a delaminated clay with nanostructured anatase assembled on its surface. The Zr dopant was successfully incorporated into the anatase lattice, resulting in a slight deformation of the anatase crystal and the reduction of the band gap. These materials exhibit high surface area with a disordered mesoporous structure formed by TiO{sub 2} particles (15–20 nm) supported on a delaminated clay. They were tested in the solar photodegradation of antipyrine, usually used as an analgesic drug and selected as an example of emerging pollutant. High degradation rates have been obtained at low antipyrine concentrations and high solar irradiation intensities with the Zr-doped TiO{sub 2}/clay catalyst, more effective than the undoped one. This work demonstrates the potential application of the synthesis method for preparing novel and efficient solar-light photocatalysts based on metal-doped anatase and a delaminated clay.

  7. Cracking and delamination of vapor-deposited tantalum films

    International Nuclear Information System (INIS)

    Fisher, R.M.; Duan, J.Z.; Liu, J.B.

    1990-01-01

    This paper reports on tantalum films which begin to crack and spall during vapor deposition on glass at a thickness of 180 nm. Islands and ribbons, 10 - 30 μm in size, delaminate by crack growth along the Ta/glass interface for several μm after which the crack penetrates into the glass to a depth of 0.5 - 1 μm and complete spalling occurs. X-ray diffraction showed that about 50% of the original bct, β-tantalum, phase had transformed to the bcc α-Ta phase. When Ta was deposited on glass that was first covered with 52 nm of copper, spalling was observed to begin at a thickness of 105 nm. In this case, the film first cracks and then peels along the Cu/glass interface and curls into scrolls indicating the presence of a small stress gradient. X-ray diffraction of the as-deposited film, and electron diffraction of ion-milled flakes, showed that the Ta films deposited on Cu-coated glass almost completely transform to bcc α-Ta. The critical thickness for delamination along the Cu/glass interface is about 1/2 that for cracking in the glass substrate when an intermediate layer of Cu is not present. All of the above findings are in good agreement with previous observations on Cr films

  8. Characterization of exfoliated/delamination kaolinite

    International Nuclear Information System (INIS)

    Sun, Dewen; Li, Bin; Li, Yanfeng; Yu, Cui; Zhang, Bo; Fei, Huafeng

    2011-01-01

    A novel and facile approach for the preparation of exfoliated/delamination kaolinite was reported in this study. Kaolinite was mechanochemically activated by grinding with dimethylsulfoxide in a globe mill for different periods of time, and then the activated samples were treated for several hours at 120 o C to obtain the precursors of kaolinite. The resulting materials were characterized by X-ray powder diffraction, scanning electron microscopy, transmission electron microscopy, and X-ray photoelectron spectroscopy. The experimental data indicated that the clay layers were well exfoliated/delamination under mechanochemical effect in a significantly short intercalation time. The expansion of the basal spacing (d 001 ) of raw kaolinite by 0.40 nm pointed out that the hydrogen bonds between adjacent kaolinite layers were partially broken as a result of the intercalation with dimethylsulfoxide.

  9. Mechanistic Study of Delamination Fracture in Al-Li Alloy C458 (2099)

    Science.gov (United States)

    Tayon, W. A.; Crooks, R. E.; Domack, M. S.; Wagner, J. A.; Beaudoin, A. J.; McDonald, R. J.

    2009-01-01

    Delamination fracture has limited the use of lightweight Al-Li alloys. In the present study, electron backscattered diffraction (EBSD) methods were used to characterize crack paths in Al-Li alloy C458 (2099). Secondary delamination cracks in fracture toughness samples showed a pronounced tendency for fracture between grain variants of the same deformation texture component. These results were analyzed by EBSD mapping methods and simulated with finite element analyses. Simulation procedures include a description of material anisotropy, local grain orientations, and fracture utilizing crystal plasticity and cohesive zone elements. Taylor factors computed for each grain orientation subjected to normal and shear stresses indicated that grain pairs with the largest Taylor factor differences were adjacent to boundaries that failed by delamination. Examination of matching delamination fracture surface pairs revealed pronounced slip bands in only one of the grains bordering the delamination. These results, along with EBSD studies, plasticity simulations, and Auger electron spectroscopy observations support a hypothesis that delamination fracture occurs due to poor slip accommodation along boundaries between grains with greatly differing plastic response.

  10. An in-situ experimental-numerical approach for interface delamination characterization

    NARCIS (Netherlands)

    Murthy Kolluri, N.V.V.R.

    2011-01-01

    Interfacial delamination is a key reliability challenge in composites and microelectronic systems due to (high density) integration of dissimilar materials. Delamination occurs due to significant stresses generated at the interfaces, for instance, caused by thermal cycling due to the mismatch in

  11. Delamination behaviour of GdBCO coated conductor tapes under transverse tension

    International Nuclear Information System (INIS)

    Gorospe, A.; Nisay, A.; Dizon, J.R.; Shin, H.S.

    2013-01-01

    Highlights: •Installation of a test frame which gives precisely aligned transverse load. •Investigation of I c degradation behaviour depending on the type of sample delamination. •Inhomogeneity of the CC tapes caused large variation on delamination strength. •SEM and EDS analysis of delamination sites under transverse loading. -- Abstract: The electromechanical property behaviour of 2G coated conductor (CC) tapes fabricated by multi-layer deposition process both in the in-plane and transverse direction should be understood. The CC tapes are used in the fabrication of epoxy resin-impregnated coils. In such case, the Lorentz force due to the high magnetic field applied as well as the thermal stress due to the difference in coefficient of thermal expansion (CTE) among constituent layers during cooling to cryogenic temperature will induce transversely applied load to the surface of CC tapes in coils. Hence, the CC tape should have a good mechanical property in the transverse direction in order to maintain its superior performance under magnetic field. In this study, a test frame which gives precisely aligned transverse load was devised. Using the fixture, the delamination behaviours including the delamination strength of the GdBCO CC tapes under transverse tensile loading were investigated. Large variation on the delamination strength of the CC tapes was recorded and might have resulted from the slit edge effect and the inhomogeneity of the CC tapes. The I c degradation behaviour under transverse load was related to the location where delamination occurred in the sample

  12. Delamination propensity of pharmaceutical glass containers by accelerated testing with different extraction media.

    Science.gov (United States)

    Guadagnino, Emanuel; Zuccato, Daniele

    2012-01-01

    The delamination of pharmaceutical glass is a serious issue, as it can cause glass particles to appear in vials, a problem that has forced a number of drug product recalls in recent years. In Type I pharmaceutical glass vials, delamination occurs generally at the bottom and shoulder, where extensive flaming during the conversion process can favor a strong evaporation of alkali and borate species and the formation of heavily enriched silica layers. The contact with parenteral preparations dissolved in an alkaline medium increases the rate of glass corrosion, while the differential hydration of these layers can cause the detachment of flakes. The purpose of this study was to investigate the effect of the pH and the composition of the extraction solutions on the propensity of different glass types to delaminate. Repeated autoclave extractions at 121 °C were carried out on different glass types with different extraction media, including organic extractants like citric and glutaric acid. When vials were in contact with alkaline solutions and similarly aggressive media, an increase in silica extraction values indicated glass corrosion and an increasing risk for further delamination. Under such conditions expansion 33 glass is extensively corroded, showing high silica concentration and heavy flaking as compared to other glass types. Sulfur-treated glass also showed early flaking, even if SiO(2) concentration was very low. A similar ranking was observed with extractions carried out with glutaric and citric acids, but at far much higher SiO(2) concentration levels. Extractions with 0.9% KCl solution can be used as an accelerated test to highlight the propensity of a glass to delaminate, but in no case it can be taken as a guarantee that the glass will not delaminate when exposed to the pharmaceutical drug, whose extraction ability requires case-by-case study. How can injectable drug manufacturers prevent glass delamination? The issue of delamination is a serious one, as it

  13. Delamination in surface plies of graphite/epoxy caused by the edge trimming process

    Science.gov (United States)

    Colligan, K.; Ramulu, M.

    Delamination in surface plies of graphite/epoxy laminates caused by edge trimming using polycrystalline diamond (PCD) and carbide cutters is investigated. The effect of several machining variables on formation of delaminations in the surface plies of a graphite fiber reinforced composite material is presented. Machining tests were performed to assess the impact of cutter geometry, feedrate, rotation direction, and graphite fiber orientation. Three typical delamination modes were observed and documented. Feedrate was found to have a significant effect on surface ply delamination in graphite/epoxy composite materials.

  14. Delamination behaviour in differently copper laminated REBCO coated conductor tapes under transverse loading

    Energy Technology Data Exchange (ETDEWEB)

    Gorospe, Alking [Department of Mechanical Design Engineering, Andong National University, 1375 Kyungdong-Ro, Andong 760-749 (Korea, Republic of); Department of Engineering, Aurora State College of Technology, Baler Aurora 3200 (Philippines); Nisay, Arman [Department of Mechanical Design Engineering, Andong National University, 1375 Kyungdong-Ro, Andong 760-749 (Korea, Republic of); Shin, Hyung-Seop, E-mail: hsshin@andong.ac.kr [Department of Mechanical Design Engineering, Andong National University, 1375 Kyungdong-Ro, Andong 760-749 (Korea, Republic of)

    2014-09-15

    Highlights: • I{sub c} degradation behavior under transverse tension loading in different CC tape structure. • Weibull distribution analysis applied on delamination mechanism of CC tape. • Delamination mechanism on CC tapes depending on copper lamination type. • SEM and WDS mapping analysis of delamination sites under transverse loading. - Abstract: Laminated HTS coated conductor (CC) tapes having a unique multi-layer structure made them vulnerable when exposed to transverse loading. Electromechanical transport properties of these CC tapes can be affected by excessive transverse stresses. Due to the coefficient of thermal expansion (CTE) mismatch and incompatibility among constituent materials used in coil applications, delamination among layers occurs and causes critical current, I{sub c} degradation in the CC tapes. In this study, the delamination behaviors in copper (Cu) solder-laminated CC tapes by soldering and surround Cu-stabilized ones by electroplating under transverse tension loading were investigated. Similarly to the surround Cu-stabilized CC tapes in our previous reports, the Cu solder-laminated CC tapes also showed an abrupt and gradual I{sub c} degradation behavior. However, the Cu solder-laminated CC tapes showed different delamination morphologies as compared to the surround Cu-stabilized CC tapes; the superconducting side and the substrate side of the Cu solder laminated CC tapes were totally separated by delamination. On the other hand, the brass laminate did not show any significant effect on the delamination strength when it is added upon the surround Cu-stabilized CC tapes.

  15. Application of scanning laser Doppler vibrometry for delamination detection in composite structures

    Science.gov (United States)

    Kudela, Pawel; Wandowski, Tomasz; Malinowski, Pawel; Ostachowicz, Wieslaw

    2017-12-01

    In this paper application of scanning laser Doppler vibrometry for delamination detection in composite structures was presented. Delamination detection was based on a guided wave propagation method. In this papers results from numerical and experimental research were presented. In the case of numerical research, the Spectral Element Method (SEM) was utilized, in which a mesh was composed of 3D spectral elements. SEM model included also a piezoelectric transducer. In the experimental research guided waves were excited using the piezoelectric transducer whereas the sensing process was conducted using scanning laser Doppler vibrometer (SLDV). Analysis of guided wave propagation and its interaction with delamination was based on a full wavefield approach. Attention was focused on interactions of guided waves with delamination manifested by A0 mode reflection, A0 mode entrapment, and S0/A0 mode conversion. Delamination was simulated by a teflon insert located between plies of composite material. Results of interaction with symmetrically and nonsymmetrical placed delamination (in respect to the composite sample thickness) were presented. Moreover, the authors investigated different size of delaminations. Damage detection was based on a new signal processing algorithm proposed by the authors. In this approach the weighted RMS was utilized selectively. It means that the summation in RMS formula was performed only for a specially selected time instances. Results for simple composite panels, panel with honeycomb core, and real stiffened composite panel from the aircraft were presented.

  16. Role of Delamination in Zeolite-Catalyzed Aromatic Alkylation: UCB-3 versus 3-D Al-SSZ-70

    Energy Technology Data Exchange (ETDEWEB)

    Runnebaum, Ron C.; Ouyang, Xiaoying; Edsinga, Jeffrey A.; Rea, Thomas; Arslan, Ilke; Hwang, Son-Jong; Zones, Stacey I.; Katz, Alexander

    2014-07-03

    Delaminated zeolite UCB-3 exhibits 2.4-fold greater catalytic activity relative to its three-dimensional (3D) zeolite counterpart, Al-SSZ-70, and 2.0-fold greater activity (per catalyst mass) when compared with industrial catalyst MCM-22, for the alkylation of toluene with propylene at 523 K. The former increase is nearly equal to the observed relative increase in external surface area and acid sites upon delamination. However, at 423 K for the same reaction, UCB-3 exhibits a 3.5-fold greater catalytic activity relative to 3D Al-SSZ-70. The higher relative rate enhancement for the delaminated material at lower temperature can be elucidated on the basis of increased contributions from internal acid sites. Evidence of possible contributions from such acid sites is obtained by performing catalysis after silanation treatment, which demonstrates that although virtually all catalysis in MCM-22 occurs on the external surface, catalysis also occurs on internal sites for 3D Al-SSZ-70. The additional observed enhancement at low temperatures can therefore be rationalized by greater access to internal active sites as a result of sheet breakage during delamination. Such breakage leads to shorter characteristic internal diffusion paths and was visualized using TEM comparisons of UCB-3 and 3D Al-SSZ-70.

  17. Cartilage Delamination Flap Mimicking a Torn Medial Meniscus

    Directory of Open Access Journals (Sweden)

    Gan Zhi-Wei Jonathan

    2016-01-01

    Full Text Available We report a case of a chondral delamination lesion due to medial parapatellar plica friction syndrome involving the medial femoral condyle. This mimicked a torn medial meniscus in clinical and radiological presentation. Arthroscopy revealed a chondral delamination flap, which was debrided. Diagnosis of chondral lesions in the knee can be challenging. Clinical examination and MRI have good accuracy for diagnosis and should be used in tandem. Early diagnosis and treatment of chondral lesions are important to prevent progression to early osteoarthritis.

  18. Local Guided Wavefield Analysis for Characterization of Delaminations in Composites

    Science.gov (United States)

    Rogge, Matthew D.; Campbell Leckey, Cara A.

    2012-01-01

    Delaminations in composite laminates resulting from impact events may be accompanied by minimal indication of damage at the surface. As such, inspection techniques are required to ensure defects are within allowable limits. Conventional ultrasonic scanning techniques have been shown to effectively characterize the size and depth of delaminations but require physical contact with the structure. Alternatively, a noncontact scanning laser vibrometer may be used to measure guided wave propagation in the laminate structure. A local Fourier domain analysis method is presented for processing guided wavefield data to estimate spatially-dependent wavenumber values, which can be used to determine delamination depth. The technique is applied to simulated wavefields and results are analyzed to determine limitations of the technique with regards to determining defect size and depth. Finally, experimental wavefield data obtained in quasi-isotropic carbon fiber reinforced polymer (CFRP) laminates with impact damage is analyzed and wavenumber is measured to an accuracy of 8.5% in the region of shallow delaminations. Keywords: Ultrasonic wavefield imaging, Windowed Fourier transforms, Guided waves, Structural health monitoring, Nondestructive evaluation

  19. DELAMINATION PREDICTION IN DRILLING OF CFRP COMPOSITES USING ARTIFICIAL NEURAL NETWORK

    Directory of Open Access Journals (Sweden)

    K. PALANIKUMAR

    2011-04-01

    Full Text Available Carbon fibre reinforced plastic (CFRP materials play a major role in the applications of aeronautic, aerospace, sporting and transportation industries. Machining is indispensible and hence drilling of CFRP materials is considered in this present study with respect to spindle speed in rpm, drill size in mm and feed in mm/min. Delamination is one of the major defects to be dealt with. The experiments are carried out using computer numerical control machine and the results are applied to an artificial neural network (ANN for the prediction of delamination factor at the exit plane of the CFRP material. It is found that ANN model predicts the delamination for any given set of machining parameters with a maximum error of 0.81% and a minimum error of 0.03%. Thus an ANN model is highly suitable for the prediction of delamination in CFRP materials.

  20. Delamination evaluation of thermal barrier coating on turbine blade owing to isothermal degradation using ultrasonic C-scan image

    International Nuclear Information System (INIS)

    Lee, Ho Girl; Kim, Hak Joon; Song, Sung Jin; Seok, Chang Sung

    2016-01-01

    Thermal barrier coating (TBC) is an essential element consisting of a super-alloy base and ceramic coating designed to achieve long operational time under a high temperature and pressure environment. However, the top coat of TBC can be delaminated at certain temperatures with long operation time. As the delamination of TBC is directly related to the blade damage, the coupling status of the TBC should be assured for reliable operation. Conventional studies of nondestructive evaluation have been made for detecting generation of thermally grown oxide (TGO) or qualitatively evaluating delamination in TBC. In this study, the ultrasonic C-scan method was developed to obtain the damage map inside TBC by estimating the delamination in a quantitative way. All specimens were isothermally degraded at 1,100°C with different time, having different partial delamination area. To detect partial delamination in TBC, the C-scan was performed by a single transducer using pulse-echo method with normal incidence. Partial delamination coefficients of 1 mm to 6 mm were derived by the proportion of the surface reflection signal and flaw signal which were theoretical signals using Rogers-Van Buren and Kim's equations. Using the partial delamination coefficients, the partial delamination maps were obtained. Regardless of the partial delamination coefficient, partial delamination area was increased when degradation time was increased in TBC. In addition, a decrease in partial delamination area in each TBC specimen was observed when the partial delamination coefficient was increased. From the portion of the partial delamination maps, the criterion for delamination was derived

  1. Delamination evaluation of thermal barrier coating on turbine blade owing to isothermal degradation using ultrasonic C-scan image

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Ho Girl; Kim, Hak Joon; Song, Sung Jin; Seok, Chang Sung [Dept. of Mechanical Engineering, Sungkyunkwan University, Suwon (Korea, Republic of)

    2016-10-15

    Thermal barrier coating (TBC) is an essential element consisting of a super-alloy base and ceramic coating designed to achieve long operational time under a high temperature and pressure environment. However, the top coat of TBC can be delaminated at certain temperatures with long operation time. As the delamination of TBC is directly related to the blade damage, the coupling status of the TBC should be assured for reliable operation. Conventional studies of nondestructive evaluation have been made for detecting generation of thermally grown oxide (TGO) or qualitatively evaluating delamination in TBC. In this study, the ultrasonic C-scan method was developed to obtain the damage map inside TBC by estimating the delamination in a quantitative way. All specimens were isothermally degraded at 1,100°C with different time, having different partial delamination area. To detect partial delamination in TBC, the C-scan was performed by a single transducer using pulse-echo method with normal incidence. Partial delamination coefficients of 1 mm to 6 mm were derived by the proportion of the surface reflection signal and flaw signal which were theoretical signals using Rogers-Van Buren and Kim's equations. Using the partial delamination coefficients, the partial delamination maps were obtained. Regardless of the partial delamination coefficient, partial delamination area was increased when degradation time was increased in TBC. In addition, a decrease in partial delamination area in each TBC specimen was observed when the partial delamination coefficient was increased. From the portion of the partial delamination maps, the criterion for delamination was derived.

  2. Modeling Quasi-Static and Fatigue-Driven Delamination Migration

    Science.gov (United States)

    De Carvalho, N. V.; Ratcliffe, J. G.; Chen, B. Y.; Pinho, S. T.; Baiz, P. M.; Tay, T. E.

    2014-01-01

    An approach was proposed and assessed for the high-fidelity modeling of progressive damage and failure in composite materials. It combines the Floating Node Method (FNM) and the Virtual Crack Closure Technique (VCCT) to represent multiple interacting failure mechanisms in a mesh-independent fashion. Delamination, matrix cracking, and migration were captured failure and migration criteria based on fracture mechanics. Quasi-static and fatigue loading were modeled within the same overall framework. The methodology proposed was illustrated by simulating the delamination migration test, showing good agreement with the available experimental data.

  3. Numerical model of glulam beam delamination in dependence on cohesive strength

    Science.gov (United States)

    Kawecki, Bartosz; Podgórski, Jerzy

    2018-01-01

    This paper presents an attempt of using a finite element method for predicting delamination of a glue laminated timber beam through a cohesive layer. There were used cohesive finite elements, quadratic stress damage initiation criterion and mixed mode energy release rate failure model. Finite element damage was equal to its complete stiffness degradation. Timber material was considered to be an orthotropic with plastic behaviour after reaching bending limit.

  4. Correlating bilayer tablet delamination tendencies to micro-environmental thermodynamic conditions during pan coating.

    Science.gov (United States)

    Zacour, Brian M; Pandey, Preetanshu; Subramanian, Ganeshkumar; Gao, Julia Z; Nikfar, Faranak

    2014-06-01

    The objective of this study was to determine the impact that the micro-environment, as measured by PyroButton data loggers, experienced by tablets during the pan coating unit operation had on the layer adhesion of bilayer tablets in open storage conditions. A full factorial design of experiments (DOE) with three center points was conducted to study the impact of final tablet hardness, film coating spray rate and film coating exhaust temperature on the delamination tendencies of bilayer tablets. PyroButton data loggers were placed (fixed) at various locations in a pan coater and were also allowed to freely move with the tablet bed to measure the micro-environmental temperature and humidity conditions of the tablet bed. The variance in the measured micro-environment via PyroButton data loggers accounted for 75% of the variance in the delamination tendencies of bilayer tablets on storage (R(2 )= 0.75). A survival analysis suggested that tablet hardness and coating spray rate significantly impacted the delamination tendencies of the bilayer tablets under open storage conditions. The coating exhaust temperature did not show good correlation with the tablets' propensity to crack indicating that it was not representative of the coating micro-environment. Models created using data obtained from the PyroButton data loggers outperformed models created using primary DOE factors in the prediction of bilayer tablet strength, especially upon equipment or scale transfers. The coating micro-environment experienced by tablets during the pan coating unit operation significantly impacts the strength of the bilayer interface of tablets on storage.

  5. Aerogel to simulate delamination and porosity defects in carbon-fiber reinforced polymer composites

    Science.gov (United States)

    Juarez, Peter; Leckey, Cara A. C.

    2018-04-01

    Representative defect standards are essential for the validation and calibration of new and existing inspection techniques. However, commonly used methods of simulating delaminations in carbon-fiber reinforced polymer (CFRP) composites do not accurately represent the behavior of the real-world defects for several widely-used NDE techniques. For instance, it is common practice to create a delamination standard by inserting Polytetrafluoroethylene (PTFE) in between ply layers. However, PTFE can transmit more ultrasonic energy than actual delaminations, leading to an unrealistic representation of the defect inspection. PTFE can also deform/wrinkle during the curing process and has a thermal effusivity two orders of magnitude higher than air (almost equal to that of a CFRP). It is therefore not effective in simulating a delamination for thermography. Currently there is also no standard practice for producing or representing a known porosity in composites. This paper presents a novel method of creating delamination and porosity standards using aerogel. Insertion of thin sheets of solid aerogel between ply layers during layup is shown to produce air-gap-like delaminations creating realistic ultrasonic and thermographic inspection responses. Furthermore, it is shown that depositing controlled amounts of aerogel powder can represent porosity. Micrograph data verifies the structural integrity of the aerogel through the composite curing process. This paper presents data from multiple NDE methods, including X-ray computed tomography, immersion ultrasound, and flash thermography to the effectiveness of aerogel as a delamination and porosity simulant.

  6. Vibration of a Laminated Beam with a Delamination Including Contact Effects

    Directory of Open Access Journals (Sweden)

    W. Ostachowicz

    2004-01-01

    Full Text Available Certain results are presented in this paper on damped vibration of a laminated cantilever beam with a single closing delamination. In order to investigate this task the finite element method has been applied in the current study. For modelling the beam higher order shear deformation beam finite elements have been used. The vibration of the beam is investigated in the time domain using a dynamic contact algorithm developed by the authors. The algorithm is based on the Newmark method and also incorporates a Newton-Raphson based procedure for resolving the equation of motion. The time series obtained from solving the equation of motion have been subsequently analysed in the frequency domain by using FFT (Fast Fourier Transform. The vibration responses of the beam due to various harmonic and impulse excitations, at different delamination locations, and for different delamination lengths, as well as changes in the dissipation of damping energy due to the delamination, have all been considered in the paper.

  7. Delamination detection in reinforced concrete using thermal inertia

    International Nuclear Information System (INIS)

    Del Grande, N K; Durbin, P F.

    1998-01-01

    We investigated the feasibility of thermal inertia mapping for bridge deck inspections. Using pulsed thermal imaging, we heat-stimulated surrogate delaminations in reinforced concrete and asphalt-concrete slabs. Using a dual-band infrared camera system, we measured thermal inertia responses of Styrofoam implants under 5 cm of asphalt, 5 cm of concrete, and 10 cm of asphalt and concrete. We compared thermal maps from solar-heated concrete and asphalt-concrete slabs with thermal inertia maps from flash-heated concrete and asphalt-concrete slabs. Thermal inertia mapping is a tool for visualizing and quantifying subsurface defects. Physically, thermal inertia is a measure of the resistance of the bridge deck to temperature change. Experimentally, it is determined from the inverse slope of the surface temperature versus the inverse square root of time. Mathematically, thermal inertia is the square root of the product of thermal conductivity, density, and heat capacity. Thermal inertia mapping distinguishes delaminated decks which have below-average thermal inertias from normal or shaded decks. Key Words: Pulsed Thermal Imaging, Thermal Inertia, Detection Of Concrete Bridgedeck Delaminations

  8. The effect of delaminations on local buckling in wind turbine blades

    DEFF Research Database (Denmark)

    Haselbach, Philipp Ulrich; Bitsche, Robert; Branner, Kim

    2015-01-01

    In this article the effect of delaminations on the load carrying capacity of a large wind turbine blade is studied numerically. For this purpose an 8.65 m long blade section with different initial delaminations in the main spar was subjected to a flapwise dominated bending moment. The model...

  9. Quantitative Evaluation of Delamination in Composites Using Lamb Waves

    Science.gov (United States)

    Michalcová, L.; Hron, R.

    2018-03-01

    Ultrasonic guided wave monitoring has become very popular in the area of structural health monitoring (SHM) of aerospace structures. Any possible type of damage must be reliably assessed. The paper deals with delamination length determination in DCB specimens using Lamb waves. An analytical equation based on the velocity dependence on variable thickness is utilized. The group velocity of the fundamental antisymmetric A0 mode rapidly changes in a particular range of the frequency-thickness product. Using the same actuation frequency the propagation velocity is different for delaminated structure. Lamb wave based delamination lengths were compared to the visually determined lengths. The method of the wave velocity determination proved to be essential. More accurate results were achieved by tracking the maximum amplitude of A0 mode than the first signal arrival. These findings are considered as the basis for the damage evaluation of complex structures.

  10. Piecewise delamination of Moroccan lithosphere from beneath the Atlas Mountains

    Science.gov (United States)

    Bezada, M. J.; Humphreys, E. D.; Davila, J. M.; Carbonell, R.; Harnafi, M.; Palomeras, I.; Levander, A.

    2014-04-01

    The elevation of the intracontinental Atlas Mountains of Morocco and surrounding regions requires a mantle component of buoyancy, and there is consensus that this buoyancy results from an abnormally thin lithosphere. Lithospheric delamination under the Atlas Mountains and thermal erosion caused by upwelling mantle have each been suggested as thinning mechanisms. We use seismic tomography to image the upper mantle of Morocco. Our imaging resolves the location and shape of lithospheric cavities and of delaminated lithosphere ˜400 km beneath the Middle Atlas. We propose discontinuous delamination of an intrinsically unstable Atlas lithosphere, enabled by the presence of anomalously hot mantle, as a mechanism for producing the imaged structures. The Atlas lithosphere was made unstable by a combination of tectonic shortening and eclogite loading during Mesozoic rifting and Cenozoic magmatism. The presence of hot mantle sourced from regional upwellings in northern Africa or the Canary Islands enhanced the instability of this lithosphere. Flow around the retreating Alboran slab focused upwelling mantle under the Middle Atlas, which we infer to be the site of the most recent delamination. The Atlas Mountains of Morocco stand as an example of large-scale lithospheric loss in a mildly contractional orogen.

  11. Free vibration analysis of delaminated composite shells using different shell theories

    International Nuclear Information System (INIS)

    Nanda, Namita; Sahu, S.K.

    2012-01-01

    Free vibration response of laminated composite shells with delamination is presented using the finite element method based on first order shear deformation theory. The shell theory used is the extension of dynamic, shear deformable theory according to the Sanders' first approximation for doubly curved shells, which can be reduced to Love's and Donnell's theories by means of tracers. An eight-noded C 0 continuity, isoparametric quadrilateral element with five degrees of freedom per node is used in the formulation. For modeling the delamination, multipoint constraint algorithm is incorporated in the finite element code. The natural frequencies of the delaminated cylindrical (CYL), spherical (SPH) and hyperbolic paraboloid (HYP) shells are determined by using the above mentioned shell theories, namely Sanders', Love's, and Donnell's. The validity of the present approach is established by comparing the authors' results with those available in the literature. Additional studies on free vibration response of CYL, SPH and HYP shells are conducted to assess the effects of delamination size and number of layers considering all three shell theories. It is shown that shell theories according to Sanders and Love always predict practically identical frequencies. Donnell's theory gives reliable results only for shallow shells. Moreover, the natural frequency is found to be very sensitive to delamination size and number of layers in the shell.

  12. Using glass-graded zirconia to increase delamination growth resistance in porcelain/zirconia dental structures.

    Science.gov (United States)

    Chai, Herzl; Mieleszko, Adam J; Chu, Stephen J; Zhang, Yu

    2018-01-01

    Porcelain fused to zirconia (PFZ) restorations are widely used in prosthetic dentistry. However, their tendency to delaminate along the P/Z interface remains a practical problem so that assessing and improving the interfacial strength are important design aspects. This work examines the effect of modifying the zirconia veneering surface with an in-house felspathic glass on the interfacial fracture resistance of fused P/Z. Three material systems are studied: porcelain fused to zirconia (control) and porcelain fused to glass-graded zirconia with and without the presence of a glass interlayer. The specimens were loaded in a four-point-bend fixture with the porcelain veneer in tension. The evolution of damage is followed with the aid of a video camera. The interfacial fracture energy G C was determined with the aid of a FEA, taking into account the stress shielding effects due to the presence of adjacent channel cracks. Similarly to a previous study on PFZ specimens, the fracture sequence consisted of unstable growth of channel cracks in the veneer followed by stable cracking along the P/Z interface. However, the value of GC for the graded zirconia was approximately 3 times that of the control zirconia, which is due to the good adhesion between porcelain and the glass network structure on the zirconia surface. Combined with its improved bonding to resin-based cements, increased resistance to surface damage and good esthetic quality, graded zirconia emerges as a viable material concept for dental restorations. Copyright © 2017 The Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

  13. Buckling Analysis of Single and Multi Delamination In Composite Beam Using Finite Element Method

    Science.gov (United States)

    Simanjorang, Hans Charles; Syamsudin, Hendri; Giri Suada, Muhammad

    2018-04-01

    Delamination is one type of imperfection in structure which found usually in the composite structure. Delamination may exist due to some factors namely in-service condition where the foreign objects hit the composite structure and creates inner defect and poor manufacturing that causes the initial imperfections. Composite structure is susceptible to the compressive loading. Compressive loading leads the instability phenomenon in the composite structure called buckling. The existence of delamination inside of the structure will cause reduction in buckling strength. This paper will explain the effect of delamination location to the buckling strength. The analysis will use the one-dimensional modelling approach using two- dimensional finite element method.

  14. Delaminated Transfer of CVD Graphene

    Science.gov (United States)

    Clavijo, Alexis; Mao, Jinhai; Tilak, Nikhil; Altvater, Michael; Andrei, Eva

    Single layer graphene is commonly synthesized by dissociation of a carbonaceous gas at high temperatures in the presence of a metallic catalyst in a process known as Chemical Vapor Deposition or CVD. Although it is possible to achieve high quality graphene by CVD, the standard transfer technique of etching away the metallic catalyst is wasteful and jeopardizes the quality of the graphene film by contamination from etchants. Thus, development of a clean transfer technique and preservation of the parent substrate remain prominent hurdles to overcome. In this study, we employ a copper pretreatment technique and optimized parameters for growth of high quality single layer graphene at atmospheric pressure. We address the transfer challenge by utilizing the adhesive properties between a polymer film and graphene to achieve etchant-free transfer of graphene films from a copper substrate. Based on this concept we developed a technique for dry delamination and transferring of graphene to hexagonal boron nitride substrates, which produced high quality graphene films while at the same time preserving the integrity of the copper catalyst for reuse. DOE-FG02-99ER45742, Ronald E. McNair Postbaccalaureate Achievement Program.

  15. Cdc42/N-WASP signaling links actin dynamics to pancreatic β cell delamination and differentiation

    Science.gov (United States)

    Kesavan, Gokul; Lieven, Oliver; Mamidi, Anant; Öhlin, Zarah Löf; Johansson, Jenny Kristina; Li, Wan-Chun; Lommel, Silvia; Greiner, Thomas Uwe; Semb, Henrik

    2014-01-01

    Delamination plays a pivotal role during normal development and cancer. Previous work has demonstrated that delamination and epithelial cell movement within the plane of an epithelium are associated with a change in cellular phenotype. However, how this positional change is linked to differentiation remains unknown. Using the developing mouse pancreas as a model system, we show that β cell delamination and differentiation are two independent events, which are controlled by Cdc42/N-WASP signaling. Specifically, we show that expression of constitutively active Cdc42 in β cells inhibits β cell delamination and differentiation. These processes are normally associated with junctional actin and cell-cell junction disassembly and the expression of fate-determining transcription factors, such as Isl1 and MafA. Mechanistically, we demonstrate that genetic ablation of N-WASP in β cells expressing constitutively active Cdc42 partially restores both delamination and β cell differentiation. These findings elucidate how junctional actin dynamics via Cdc42/N-WASP signaling cell-autonomously control not only epithelial delamination but also cell differentiation during mammalian organogenesis. PMID:24449844

  16. Delamination wear mechanism in gray cast irons

    International Nuclear Information System (INIS)

    Salehi, M.

    2000-01-01

    An investigation of the friction and sliding wear of gray cast iron against chromium plated cast irons was carried out on a newly constructed reciprocating friction and wear tester. The tests were the first to be done on the test rig under dry conditions and at the speed of 170 cm/min, and variable loads of 20-260 N for a duration of 15 min. to 3 hours. The gray cast iron surfaces worn by a process of plastic deformation at the subsurface, crack nucleation, and crack growth leading to formation of plate like debris and therefore the delamination theory applies. No evidence of adhesion was observed. This could be due to formation of oxides on the wear surface which prevent adhesion. channel type chromium plating ''picked'' up cast iron from the counter-body surfaces by mechanically trapping cast iron debris on and within the cracks. The removal of the plated chromium left a pitted surface on the cast iron

  17. Utilizing the meso-scale grain boundary stress to estimate the onset of delamination in 2099-T861 aluminium–lithium

    International Nuclear Information System (INIS)

    McDonald, Russell J; Beaudoin, Armand J

    2010-01-01

    Aluminium–lithium alloys provide a lower density and higher stiffness alternative to other high strength aluminium alloys. However, many Al–Li alloys exhibit a non-traditional failure mechanism called delamination, which refers to the failure of the elongated grain boundary interface. In this investigation, delaminations were observed after cyclic deformation of both uniaxial and torsion experiments. A cyclically stable rate-independent crystal plasticity framework with kinematic hardening was developed to address many experimental trends of stabilized cyclic plasticity. Utilizing this framework, meso-scale grain boundary interface stresses were estimated with uniform deformation and bi-crystal models. These models are computationally amenable to investigate both orientation dependence and the statistical nature of the grain boundary stresses for a given bulk texture and nominal loading. A coupled shear-normal Findley-based damage parameter was formulated to quantitatively characterize the nucleation of delamination consistently with experimental trends

  18. Delamination Detection in Carbon Fibre Reinforced Composites Using Electrical Resistance Measurement

    International Nuclear Information System (INIS)

    Kovalovs, A; Rucevskis, S; Kulakov, V; Aniskevich, A

    2016-01-01

    In the present study 2-D numerical analysis of strip-type laminated composite specimens with and without damage is considered and numerical investigation is carried out by using a finite element method. The surface and oblique resistances are numerically calculated according to the two-probe and four-probe methods. The electrical conductivity of the composite laminate in the longitudinal direction is constant, while the electrical conductivity in the through-thickness direction is used as a variable in the parametric study. The resistance change due to delamination for each case is estimated by comparing the obtained resistance with the corresponding resistance of the specimen without delamination. Applicability and effectiveness of the proposed method are investigated by using various lengths of a delaminated crack in the specimen. (paper)

  19. To improve impact damage response of single and multi-delaminated FRP composites using natural Flax yarn

    International Nuclear Information System (INIS)

    Ghasemnejad, H.; Soroush, V.R.; Mason, P.J.; Weager, B.

    2012-01-01

    Highlights: ► To study the impact resistance of delaminated composite structures. ► To improve the impact resistance of delaminated composite structures using natural Flax yarn. ► To investigate the effect of z-pinning on the damage process of composite materials. ► To develop FE techniques to model the impact process of composite structures using LSDYNA. -- Abstract: The ply delamination which is known as a principle mode of failure of layered composites due to separation along the interfaces of the layers is one of the main concerns in designing of composite material structures. In this regard, the effect of hybrid laminate lay-up in multi-delaminated composite beam was investigated. The Charpy impact test was chosen to study the energy absorbing capability of delaminated composite beam. Hybrid composite beams were fabricated from combination of glass/epoxy and carbon/epoxy composites. To improve the impact behaviour of multi-delaminated composite beams the laminated hybrid composite beams were pinned using Flax yarns before curing process. It was shown that the multi-delaminated composite beams which are pinned in z-direction are able to arrest the crack propagation and consequently absorb more energy in comparison with simple ones in hybrid composite beams. The Charpy impact test of delaminated composite beams was also simulated by finite element software LS-DYNA and the results were verified with the relevant experimental results.

  20. Laser Doppler Vibrometer Based Examination of the Efficiency of Introducing Artificial Delaminations into Composite Shells

    Directory of Open Access Journals (Sweden)

    Kustroń Kamila

    2015-09-01

    Full Text Available During its operation, the laminate shell of the watercraft hull can be exposed to local stability losses caused by the appearance and development of delaminations. The sources of these delaminations are discontinuities, created both in the production process and as a result of bumps of foreign bodies into the hull in operation. In the environment of fatigue loads acting on the hull, the delaminations propagate and lead to the loss of load capacity of the hull structure. There is a need to improve diagnostic systems used in Structural Health Monitoring (SHM of laminate hull elements to detect and monitor the development of the delaminations. Effective diagnostic systems used for delamination assessment base on expert systems. Along with other tools, the expert diagnostic advisory systems make use of the non-destructive examination method which consists in generating elastic waves in the hull shell structure and observing their changes by comparing the recorded signal with damage patterns collected in the expert system database. This system requires introducing certain patterns to its knowledge base, based on the results of experimental examinations performed on specimens with implemented artificial delaminations. The article presents the results of the examination oriented on assessing the delaminations artificially generated in the structure of glass- and carbon-epoxy laminates by introducing local non-adhesive layers with the aid of thin polyethylene film, teflon insert, or thin layer of polyvinyl alcohol. The efficiency of each method was assessed using laser vibrometry. The effect of the depth of delamination position in the laminate on the efficiency of the applied method is documented as well.

  1. Controlled delamination of metal films by hydrogen loading

    Energy Technology Data Exchange (ETDEWEB)

    Nikitin, Eugen

    2008-11-18

    n this work we quantitatively determine the adhesion energy between metal films and their substrates. Therefore a new controlled buckling technique is established, applying the strong compressive in-plane stress that results in thin films clamped on rigid substrates during hydrogen loading. When the elastic energy stored in the H-loaded thin film exceeds the adhesion energy between film and substrate, delamination occurs. At the onset of delamination, a critical hydrogen concentration, a critical stress value and a critical bending of the substrate are present, which are quantitative measures for the adhesion energy and permit its calculation. As the critical values are determined at the onset of delamination, plastic deformation is negligible, which denies the quantitative determination of adhesion energies in conventional test setups. In multilayer-systems, adhesion energies between substrates and films that hardly absorb hydrogen can be measured by the controlled buckling technique, when the films of interest are coated with hydrogen absorbing films (active layer). The measurements are performed easily and can be repeated under the same test conditions, while variables such as the thickness of the coating materials or the boundary surface structure can be varied and optimized. In this work the adhesion energies of different materials on polycarbonate and niobium on sapphire are investigated. (orig.)

  2. Delamination R-curve as a material property of unidirectional glass/epoxy composites

    International Nuclear Information System (INIS)

    Shokrieh, M.M.; Heidari-Rarani, M.; Ayatollahi, M.R.

    2012-01-01

    Highlights: → The R-curve behavior of a unidirectional laminate as a material property is investigated. → Effect of initial crack length and thickness on R-curve is experimentally shown. → A mathematical relation is proposed to model the R-curve behavior of any unidirectional laminated composite. -- Abstract: It is still questionable to think of delamination resistance of a double cantilever beam (DCB) as a material property independent of the specimen size and geometry. In this research, the effects of initial crack length and DCB specimen thickness on the mode I delamination resistance curve (R-curve) behavior of different unidirectional glass/epoxy DCB specimens are experimentally investigated. It is observed that the magnitudes of initiation and propagation delamination toughness (G Ic-init and G Ic-prop ) as well as the fiber bridging length are constant in a specific range of the initial crack length to the DCB specimen thickness ratios of 8.5 0 /h < 19. Finally, a mathematical relationship is proposed for prediction of mode I delamination behavior (from the initiation to propagation) of E-glass/epoxy DCB specimens.

  3. Delamination of Pearlitic Steel Wires: The Defining Role of Prior-Drawing Microstructure

    Science.gov (United States)

    Durgaprasad, A.; Giri, S.; Lenka, S.; Sarkar, Sudip Kumar; Biswas, Aniruddha; Kundu, S.; Mishra, S.; Chandra, S.; Doherty, R. D.; Samajdar, I.

    2018-03-01

    This article reports the occasional (alignment of the pearlite: 22 ± 5 pct vs 34 ± 4 pct in the nondelaminated wires. Although all wires had similar through-thickness texture and stress gradients, delaminated wires had stronger gradients in composition and higher hardness across the ferrite-cementite interface. Carbide dissolution and formation of supersaturated ferrite were clearly correlated with delamination, which could be effectively mitigated by controlled laboratory annealing at 673 K. Direct observations on samples subjected to simple shear revealed significant differences in shear localizations. These were controlled by pearlite morphology and interlamellar spacing. Prior-drawing microstructure of coarse misaligned pearlite thus emerged as a critical factor in the wire drawing-induced delamination of the pearlitic wires.

  4. Ag-Coated Heterostructures of ZnO-TiO2/Delaminated Montmorillonite as Solar Photocatalysts

    Directory of Open Access Journals (Sweden)

    Carolina Belver

    2017-08-01

    Full Text Available Heterostructures based on ZnO-TiO2/delaminated montmorillonite coated with Ag have been prepared by sol–gel and photoreduction procedures, varying the Ag and ZnO contents. They have been thoroughly characterized by XRD, WDXRF, UV–Vis, and XPS spectroscopies, and N2 adsorption, SEM, and TEM. In all cases, the montmorillonite was effectively delaminated with the formation of TiO2 anatase particles anchored on the clay layer’s surface, yielding porous materials with high surface areas. The structural and textural properties of the heterostructures synthesized were unaffected by the ZnO incorporated. The photoreduction led to solids with Ag nanoparticles decorating the surface. These materials were tested as photocatalysts for the degradation of several emerging contaminants with different nitrogen-bearing chemical structures under solar light. The catalysts yielded high rates of disappearance of the starting pollutants and showed quite stable performance upon successive applications.

  5. Modeling delamination of FRP laminates under low velocity impact

    Science.gov (United States)

    Jiang, Z.; Wen, H. M.; Ren, S. L.

    2017-09-01

    Fiber reinforced plastic laminates (FRP) have been increasingly used in various engineering such as aeronautics, astronautics, transportation, naval architecture and their impact response and failure are a major concern in academic community. A new numerical model is suggested for fiber reinforced plastic composites. The model considers that FRP laminates has been constituted by unidirectional laminated plates with adhesive layers. A modified adhesive layer damage model that considering strain rate effects is incorporated into the ABAQUS / EXPLICIT finite element program by the user-defined material subroutine VUMAT. It transpires that the present model predicted delamination is in good agreement with the experimental results for low velocity impact.

  6. Delamination-Debond Behaviour of Composite T- Joints in Wind Turbine Blades

    International Nuclear Information System (INIS)

    Gulasik, H; Coker, D

    2014-01-01

    Wind turbine industry utilizes composite materials in turbine blade structural designs because of their high strength/stiffness to weight ratio. T-joint is one of the design configurations of composite wind turbine blades. T-joints consist of a skin panel and a stiffener co-bonded or co-cured together with a filler material between them. T-joints are prone to delaminations between skin/stiffener plies and debonds between skin-stiffener-filler interfaces. In this study, delamination/debond behavior of a co-bonded composite T-joint is investigated under 0° pull load condition by 2D finite element method. Using Abaqus® commercial FE software, zero-thickness cohesive elements are used to simulate delamination/debond in ply interfaces and bonding lines. Pulling load at 0° is applied and load-displacement behavior and failure scenario are observed. The failure sequence consists of debonding of filler/stringer interface during one load drop followed by a second drop in which the 2nd filler/stringer debonds, filler/skin debonding and skin delamination leading to total loss of load carrying capacity. This type of failure initiation has been observed widely in the literature. When the debond strength is increased 30%, failure pattern is found to change in addition to increasing the load capacity by 200% before total loss of loading carrying capacity occurs. Failure initiation and propagation behavior, initial and max failure loads and stress fields are affected by the property change. In all cases mixed-mode crack tip loading is observed in the failure initiation and propagation stages. In this paper, the detailed delamination/debonding history in T-joints is predicted with cohesive elements for the first time

  7. Hierarchical system for autonomous sensing-healing of delamination in large-scale composite structures

    International Nuclear Information System (INIS)

    Minakuchi, Shu; Sun, Denghao; Takeda, Nobuo

    2014-01-01

    This study combines our hierarchical fiber-optic-based delamination detection system with a microvascular self-healing material to develop the first autonomous sensing-healing system applicable to large-scale composite structures. In this combined system, embedded vascular modules are connected through check valves to a surface-mounted supply tube of a pressurized healing agent while fiber-optic-based sensors monitor the internal pressure of these vascular modules. When delamination occurs, the healing agent flows into the vascular modules breached by the delamination and infiltrates the damage for healing. At the same time, the pressure sensors identify the damaged modules by detecting internal pressure changes. This paper begins by describing the basic concept of the combined system and by discussing the advantages that arise from its hierarchical nature. The feasibility of the system is then confirmed through delamination infiltration tests. Finally, the hierarchical system is validated in a plate specimen by focusing on the detection and infiltration of the damage. Its self-diagnostic function is also demonstrated. (paper)

  8. Fiber Optic Thermal Detection of Composite Delaminations

    Science.gov (United States)

    Wu, Meng-Chou; Winfree, William P.

    2011-01-01

    A recently developed technique is presented for thermographic detection of delaminations in composites by performing temperature measurements with fiber optic Bragg gratings. A single optical fiber with multiple Bragg gratings employed as surface temperature sensors was bonded to the surface of a composite with subsurface defects. The investigated structure was a 10-ply composite specimen with prefabricated delaminations of various sizes and depths. Both during and following the application of a thermal heat flux to the surface, the individual Bragg grating sensors measured the temporal and spatial temperature variations. The data obtained from grating sensors were analyzed with thermal modeling techniques of conventional thermography to reveal particular characteristics of the interested areas. Results were compared and found to be consistent with the calculations using numerical simulation techniques. Also discussed are methods including various heating sources and patterns, and their limitations for performing in-situ structural health monitoring.

  9. Impulse response measurements as dependent on crack depth. Delamination

    International Nuclear Information System (INIS)

    Ulriksen, Peter

    2011-02-01

    The purpose of the project is to investigate the impulse-response method's ability to detect delamination at different depths. This method is of particular interest, since some of it's realizations strongly resembles established methods like 'bomknackning' . Since the personnel that will be responsible for future measurements with new technology, should feel confidence in new methods, it is an advantage if the new methods connect to older, accepted methods. The project consists of three parts and a fourth is planned. The first part of the investigation is made with a vibrator connected to an impedance head which in turn is connected to the surface of the concrete test specimen with internal delaminations at different depths. The vibrator is controlled by a dynamic signal analyze, which also measures the force- and acceleration signals from the impedance head and convert them to impedance. Since the impedance head must be glued to the surface of the concrete this method is only of laboratory interest. This method gives a complete description of the behavior of the concrete for the frequencies investigated. Thus in following investigations the frequencies of interest are known. From the experiment it follows that delamination down to a depth of 80-100 mm can be detected through a clear and solitary resonance peak. This resonance frequency is a function of concrete slab thickness and extension, so if the extension can be measured it may be possible to calculate depth. The second part of the investigation is about using an instrumented hammer to hit the different delamination specimens. The hammer is equipped with a force transducer giving an opportunity to measure the force exerted by the strike against the concrete surface. When a hammer is struck against a concrete surface a spectrum of vibrations is created, dependent on the weight of the hammer and the elasticity of the concrete. A light hammer generates higher frequencies than a heavy one. Three different hammer

  10. Calibration of a finite element composite delamination model by experiments

    DEFF Research Database (Denmark)

    Gaiotti, M.; Rizzo, C.M.; Branner, Kim

    2013-01-01

    This paper deals with the mechanical behavior under in plane compressive loading of thick and mostly unidirectional glass fiber composite plates made with an initial embedded delamination. The delamination is rectangular in shape, causing the separation of the central part of the plate into two...... distinct sub-laminates. The work focuses on experimental validation of a finite element model built using the 9-noded MITC9 shell elements, which prevent locking effects and aiming to capture the highly non linear buckling features involved in the problem. The geometry has been numerically defined...

  11. Acoustic Emission based on sentry function to monitor the initiation of delamination in composite materials

    International Nuclear Information System (INIS)

    Bakhtiary Davijani, A.A.; Hajikhani, M.; Ahmadi, M.

    2011-01-01

    Research highlights: → Constant load does not confirm constant damage in composite materials. → Different damages have different AE events. → Sentry function is a useful tool to monitor the initiation of damage in delamination. → The less sentry function number is the more damage the material has endured. -- Abstract: Delamination is the most common failure mode in composite materials, since it will result in the reduction of stiffness and can grow throughout other layers. Delamination is consisted of two main stages including initiation and propagation. Understanding the behavior of the material in these zones is very important, hence it has been thoroughly studied by different methods such as numerical methods, Acoustic Emission (AE), and modeling. Between these two regions initiation is a more vital stage in the delamination of the material. Once initiation occurs, which normally requires greater amount of force, cracks can easily propagate through the structure with little force and cause the failure of the structure. A better knowledge of initiation can lead to better design and production of stronger materials. Additionally, more knowledge about crack initiation and its internal microevents would help improve other parameters and result in higher strength against crack initiation. AE is a suitable method for in situ monitoring of damage in composite materials. In this study, AE was applied to test different glass/epoxy specimens which were loaded under mode I delamination. A function that combines AE and mechanical information is employed to investigate the initiation of delamination. Scanning electron microscope (SEM) was used to verify the results of this function. It is shown that this method is an appropriate technique to monitor the behavior of the initiation of delamination.

  12. Delamination of hexagonal boron nitride in a stirred media mill

    International Nuclear Information System (INIS)

    Damm, C.; Körner, J.; Peukert, W.

    2013-01-01

    A scalable process for delamination of hexagonal boron nitride in an aqueous solution of the non-ionic surfactant TWEEN85 using a stirred media mill is presented. The size of the ZrO 2 beads used as grinding media governs the dimensions of the ground boron nitride particles as atomic force microscopic investigations (AFM) reveal: the mean flakes thickness decreases from 3.5 to 1.5 nm and the ratio between mean flake area and mean flake thickness increases from 2,200 to 5,800 nm if the grinding media size is reduced from 0.8 to 0.1 mm. This result shows that a high number of stress events in combination with low stress energy (small grinding media) facilitate delamination of the layered material whereas at high stress energies in combination with a low number of stress events (large grinding media) breakage of the layers dominates over delamination. The results of particle height analyses by AFM show that few-layer structures have been formed by stirred media milling. This result is in agreement with the layer thickness dependence of the delamination energy for hexagonal boron nitride. The concentration of nanoparticles remaining dispersed after centrifugation of the ground suspension increases with grinding time and with decreasing grinding media size. After 5 h of grinding using 0.1 mm ZrO 2 grinding media the yield of nanoparticle formation is about 5 wt%. The nanoparticles exhibit the typical Raman peak for hexagonal boron nitride at 1,366 cm −1 showing that the in-plane order in the milled platelets is remained.

  13. Mechanism of Electrochemical Delamination of Two-Dimensional Materials from Their Native Substrates by Bubbling.

    Science.gov (United States)

    Sun, Jie; Fan, Xing; Guo, Weiling; Liu, Lihui; Liu, Xin; Deng, Jun; Xu, Chen

    2015-12-16

    A capacitor-based circuit model is proposed to explain the electrochemical delamination of two-dimensional materials from their native substrates where produced gas bubbles squeeze into the interface. The delamination is actually the electric breakdown of the capacitor formed between the solution and substrate. To facilitate the procedure, the backside of the ubstrate has to be shielded so that the capacitor breakdown voltage can be reached. The screening effect can be induced either by nonreactive ions around the electrode or, more effectively, by an undetachable insulator. This mechanism serves as a guideline for the surface science and applications involving the bubbling delamination.

  14. Quantitative Evaluation of Delamination Inside of Composite Materials by ESPI

    International Nuclear Information System (INIS)

    Kim, Koung Suk; Yang, Kwang Young; Kang, Ki Soo; Ji, Chang June

    2004-01-01

    Electronic speckle pattern interferometry (ESPI) for quantitative evaluation of delaminations inside of a composite material plate is described. Delaminations caused by the impact on composite materials are difficult to detect visual inspection and ultrasonic testing due to non-homeogenous structure. This paper proposes the quantitative evaluation technique of the defects made in the composite plates by impact load. Artificial defects are introduced inside of the composite plate for the development of a reliable ESPI inspection technique. Real defects produced by impact tester are inspected and compared with the results of visual inspection which shows a good agreement within 5% error

  15. Analysis and modeling of delamination factor in drilling of woven kenaf fiber reinforced epoxy using Box Behnken experimental design

    Science.gov (United States)

    Suhaily, M.; Che Hassan, C. H.; Jaharah, A. G.; Afifah, M. A.; Nor Khairusshima, M. K.

    2018-01-01

    In this research study, it presents a comprehensive mathematical model for correlating the influences of drilling parameters on the delamination factor during the drilling of woven kenaf fiber reinforced epoxy composite laminates using the Box Behnken experimental design. The purpose of this study is to investigate the influence of drilling parameters such as cutting speed, feed rate and drill sizes on the delamination produced when drilling woven kenaf reinforced epoxy composite using the non-coated HSS drill bits. The damage generated on the woven kenaf reinforced epoxy composite laminates were observed both at the entrance and exit surface during the drilling operation. The experiments were conducted according to the Box Behnken experimental designs.

  16. Peeling back the lithosphere: Controlling parameters, surface expressions and the future directions in delamination modeling

    Science.gov (United States)

    Göğüş, Oğuz H.; Ueda, Kosuke

    2018-06-01

    Geodynamical models investigate the rheological and physical properties of the lithosphere that peels back (delaminates) from the upper-middle crust. Meanwhile, model predictions are used to relate to a set of observations in the geological context to the test the validity of delamination. Here, we review numerical and analogue models of delamination from these perspectives and provide a number of first-order topics which future modeling studies may address. Models suggest that the presence of the weak lower crust that resides between the strong mantle lithosphere (at least 100 times more viscous/stronger) and the strong upper crust is necessary to develop delamination. Lower crustal weakening may be induced by melt infiltration, shear heating or it naturally occurs through the jelly sandwich type strength profile of the continental lithosphere. The negative buoyancy of the lithosphere required to facilitate the delamination is induced by the pre-existing ocean subduction and/or the lower crustal eclogitization. Surface expression of the peeling back lithosphere has a distinct transient and migratory imprint on the crust, resulting in rapid surface uplift/subsidence, magmatism, heating and shortening/extension. New generation of geodynamical experiments can explain how different types of melting (e.g hydrated, dry melting) occurs with delamination. Reformation of the lithosphere after removal, three dimensional aspects, and the termination of the process are key investigation areas for future research. The robust model predictions, as with other geodynamic modeling studies should be reconciled with observations.

  17. Numerical models of delamination behavior in 2G HTS tapes under transverse tension and peel

    Science.gov (United States)

    Duan, Yujie; Ta, Wurui; Gao, Yuanwen

    2018-02-01

    In extreme operating environments, delamination in 2G HTS tapes occurs within and/or near the superconductor layer from high transverse tensile stresses caused by fabrication, Lorentz forces and thermal mismatch, etc. Generally, transverse opening and peeling off are the main delamination modes, and are always studied in anvil and peel tests, respectively. Numerical models of these modes for 2G HTS tape are presented wherein the mixed-mode traction-separation law at the interface of the silver and superconductor layers is considered. Plastic deformations of copper, silver, and Hastelloy® in the HTS tape are taken into account. The results obtained from the transverse opening model show that the maximum average tensile stress is smaller than the delamination tensile strength because delamination is asynchronous in the tape. When a crack appears in the tape, only a small stress ( ≤ 1 MPa) is required to expand the crack to other stress free areas through peeling. Using the peeling model, the dependency of the peel strength on peeling angle is investigated under constant fracture toughness. Peel strength decreases with the peeling angle until the minimum value is reached at 150°, and thereafter increases slightly. Other results indicate that peel strength depends strongly on delamination strength, fracture toughness, and thickness of copper layer. The fracture toughness of the delamination interface, which is difficult to obtain by experiment, can be extracted using the present model.

  18. Numerical evaluation of delamination in CFRP laminates by stereo X-ray pictures

    International Nuclear Information System (INIS)

    Kunoo, Kazuo; Uda, Nobuhide; Ono, Kousei; Onohara, Kaoru; Takahashi, Toshiaki; Tanaka, Hisahiro.

    1989-01-01

    This paper presents a method for quantifying damage in composite laminates by stereo X-ray pictures. A three dimensional image of delamination, which is one of the characteristic types of damage in composite laminates can be reconstructed with this method. A digital image processing technique is used to analyze X-ray pictures. Experimental results of reconstructing delaminations in carbon/epoxy cross-ply laminates show that this method is accurate enough for practical usage. (author)

  19. Piecewise Delamination Drives Uplift in the Atlas Mountains Region of Morocco

    Science.gov (United States)

    Bezada, M. J.; Humphreys, E.; Martin Davila, J.; mimoun, H.; Josep, G.; Palomeras, I.

    2013-12-01

    The elevation of the intra-continental Atlas Mountains of Morocco and surrounding regions requires a mantle component of buoyancy, and there is consensus that this buoyancy results from an abnormally thin lithosphere. Lithospheric delamination under the Atlas Mountains and thermal erosion caused by upwelling mantle have each been suggested as thinning mechanisms. We use seismic tomography to image the upper mantle of Morocco by inverting teleseimic p-wave delay times, complemented with local delays, recorded on a dense array of stations in the Iberian peninsula and Morocco. A surface wave model provides constraint on the shallower layers. We determine the geometry of lithospheric cavities and mantle upwelling beneath the Middle Atlas and central High Atlas, and image delaminated lithosphere at ~400 km beneath the Middle Atlas. We propose discontinuous delamination of an intrinsically unstable Atlas lithosphere, enabled by the presence of anomalously hot mantle, as a mechanism for producing the imaged structures. The Atlas lithosphere was made unstable by a combination of tectonic shortening and eclogite loading during Mesozoic rifting and Cenozoic magmatism. The presence of hot mantle, sourced from regional upwellings in northern Africa or the Canary Islands, enabled the mobilization of this lithosphere. Flow around the retreating Alboran slab focused upwelling mantle under the Middle Atlas, where we image the most recent delamination. The Atlas Mountains of Morocco stand as an example of mantle-generated uplift and large-scale lithospheric loss in a mildly contractional orogen.

  20. Mechanism of Electrochemical Delamination of Two-Dimensional Materials from Their Native Substrates by Bubbling

    Directory of Open Access Journals (Sweden)

    Jie Sun

    2015-12-01

    Full Text Available A capacitor-based circuit model is proposed to explain the electrochemical delamination of two-dimensional materials from their native substrates where produced gas bubbles squeeze into the interface. The delamination is actually the electric breakdown of the capacitor formed between the solution and substrate. To facilitate the procedure, the backside of the ubstrate has to be shielded so that the capacitor breakdown voltage can be reached. The screening effect can be induced either by nonreactive ions around the electrode or, more effectively, by an undetachable insulator. This mechanism serves as a guideline for the surface science and applications involving the bubbling delamination.

  1. Progressive delamination in polymer matrix composite laminates: A new approach

    Science.gov (United States)

    Chamis, C. C.; Murthy, P. L. N.; Minnetyan, L.

    1992-01-01

    A new approach independent of stress intensity factors and fracture toughness parameters has been developed and is described for the computational simulation of progressive delamination in polymer matrix composite laminates. The damage stages are quantified based on physics via composite mechanics while the degradation of the laminate behavior is quantified via the finite element method. The approach accounts for all types of composite behavior, laminate configuration, load conditions, and delamination processes starting from damage initiation, to unstable propagation, and to laminate fracture. Results of laminate fracture in composite beams, panels, plates, and shells are presented to demonstrate the effectiveness and versatility of this new approach.

  2. Effect of Location of Delamination on Free Vibration of Cross-Ply Conical Shells

    Directory of Open Access Journals (Sweden)

    Sudip Dey

    2012-01-01

    Full Text Available Location of delamination is a triggering parameter for structural instability of laminated composites. In this paper, a finite element method is employed to determine the effects of location of delamination on free vibration characteristics of graphite-epoxy cross-ply composite pre-twisted shallow conical shells. The generalized dynamic equilibrium equation is derived from Lagrange's equation of motion neglecting Coriolis effect for moderate rotational speeds. The formulation is exercised by using an eight noded isoparametric plate bending element based on Mindlin's theory. Multi-point constraint algorithm is utilized to ensure the compatibility of deformation and equilibrium of resultant forces and moments at the delamination crack front. The standard eigen value problem is solved by applying the QR iteration algorithm. Finite element codes are developed to obtain the numerical results concerning the effects of location of delamination, twist angle and rotational speed on the natural frequencies of cross-ply composite shallow conical shells. The mode shapes are also depicted for a typical laminate configuration. Numerical results obtained from parametric studies of both symmetric and anti-symmetric cross-ply laminates are the first known non-dimensional natural frequencies for the type of analyses carried out here.

  3. Allometries of Maximum Growth Rate versus Body Mass at Maximum Growth Indicate That Non-Avian Dinosaurs Had Growth Rates Typical of Fast Growing Ectothermic Sauropsids

    Science.gov (United States)

    Werner, Jan; Griebeler, Eva Maria

    2014-01-01

    We tested if growth rates of recent taxa are unequivocally separated between endotherms and ectotherms, and compared these to dinosaurian growth rates. We therefore performed linear regression analyses on the log-transformed maximum growth rate against log-transformed body mass at maximum growth for extant altricial birds, precocial birds, eutherians, marsupials, reptiles, fishes and dinosaurs. Regression models of precocial birds (and fishes) strongly differed from Case’s study (1978), which is often used to compare dinosaurian growth rates to those of extant vertebrates. For all taxonomic groups, the slope of 0.75 expected from the Metabolic Theory of Ecology was statistically supported. To compare growth rates between taxonomic groups we therefore used regressions with this fixed slope and group-specific intercepts. On average, maximum growth rates of ectotherms were about 10 (reptiles) to 20 (fishes) times (in comparison to mammals) or even 45 (reptiles) to 100 (fishes) times (in comparison to birds) lower than in endotherms. While on average all taxa were clearly separated from each other, individual growth rates overlapped between several taxa and even between endotherms and ectotherms. Dinosaurs had growth rates intermediate between similar sized/scaled-up reptiles and mammals, but a much lower rate than scaled-up birds. All dinosaurian growth rates were within the range of extant reptiles and mammals, and were lower than those of birds. Under the assumption that growth rate and metabolic rate are indeed linked, our results suggest two alternative interpretations. Compared to other sauropsids, the growth rates of studied dinosaurs clearly indicate that they had an ectothermic rather than an endothermic metabolic rate. Compared to other vertebrate growth rates, the overall high variability in growth rates of extant groups and the high overlap between individual growth rates of endothermic and ectothermic extant species make it impossible to rule out either

  4. Allometries of maximum growth rate versus body mass at maximum growth indicate that non-avian dinosaurs had growth rates typical of fast growing ectothermic sauropsids.

    Science.gov (United States)

    Werner, Jan; Griebeler, Eva Maria

    2014-01-01

    We tested if growth rates of recent taxa are unequivocally separated between endotherms and ectotherms, and compared these to dinosaurian growth rates. We therefore performed linear regression analyses on the log-transformed maximum growth rate against log-transformed body mass at maximum growth for extant altricial birds, precocial birds, eutherians, marsupials, reptiles, fishes and dinosaurs. Regression models of precocial birds (and fishes) strongly differed from Case's study (1978), which is often used to compare dinosaurian growth rates to those of extant vertebrates. For all taxonomic groups, the slope of 0.75 expected from the Metabolic Theory of Ecology was statistically supported. To compare growth rates between taxonomic groups we therefore used regressions with this fixed slope and group-specific intercepts. On average, maximum growth rates of ectotherms were about 10 (reptiles) to 20 (fishes) times (in comparison to mammals) or even 45 (reptiles) to 100 (fishes) times (in comparison to birds) lower than in endotherms. While on average all taxa were clearly separated from each other, individual growth rates overlapped between several taxa and even between endotherms and ectotherms. Dinosaurs had growth rates intermediate between similar sized/scaled-up reptiles and mammals, but a much lower rate than scaled-up birds. All dinosaurian growth rates were within the range of extant reptiles and mammals, and were lower than those of birds. Under the assumption that growth rate and metabolic rate are indeed linked, our results suggest two alternative interpretations. Compared to other sauropsids, the growth rates of studied dinosaurs clearly indicate that they had an ectothermic rather than an endothermic metabolic rate. Compared to other vertebrate growth rates, the overall high variability in growth rates of extant groups and the high overlap between individual growth rates of endothermic and ectothermic extant species make it impossible to rule out either of

  5. Allometries of maximum growth rate versus body mass at maximum growth indicate that non-avian dinosaurs had growth rates typical of fast growing ectothermic sauropsids.

    Directory of Open Access Journals (Sweden)

    Jan Werner

    Full Text Available We tested if growth rates of recent taxa are unequivocally separated between endotherms and ectotherms, and compared these to dinosaurian growth rates. We therefore performed linear regression analyses on the log-transformed maximum growth rate against log-transformed body mass at maximum growth for extant altricial birds, precocial birds, eutherians, marsupials, reptiles, fishes and dinosaurs. Regression models of precocial birds (and fishes strongly differed from Case's study (1978, which is often used to compare dinosaurian growth rates to those of extant vertebrates. For all taxonomic groups, the slope of 0.75 expected from the Metabolic Theory of Ecology was statistically supported. To compare growth rates between taxonomic groups we therefore used regressions with this fixed slope and group-specific intercepts. On average, maximum growth rates of ectotherms were about 10 (reptiles to 20 (fishes times (in comparison to mammals or even 45 (reptiles to 100 (fishes times (in comparison to birds lower than in endotherms. While on average all taxa were clearly separated from each other, individual growth rates overlapped between several taxa and even between endotherms and ectotherms. Dinosaurs had growth rates intermediate between similar sized/scaled-up reptiles and mammals, but a much lower rate than scaled-up birds. All dinosaurian growth rates were within the range of extant reptiles and mammals, and were lower than those of birds. Under the assumption that growth rate and metabolic rate are indeed linked, our results suggest two alternative interpretations. Compared to other sauropsids, the growth rates of studied dinosaurs clearly indicate that they had an ectothermic rather than an endothermic metabolic rate. Compared to other vertebrate growth rates, the overall high variability in growth rates of extant groups and the high overlap between individual growth rates of endothermic and ectothermic extant species make it impossible to rule

  6. Nondestructive testing of delaminated interfaces between two materials using electromagnetic interrogation

    Science.gov (United States)

    Cakoni, Fioralba; de Teresa, Irene; Monk, Peter

    2018-06-01

    We consider the problem of detecting whether two materials that should be in contact have separated or delaminated using electromagnetic radiation. The interface damage is modeled as a thin opening between two materials of different electromagnetic properties. To derive a reconstruction algorithm that focuses on testing for the delamination at the interface between the two materials, we use the approximate asymptotic model for the forward problem derived in de Teresa (2017 PhD Thesis University of Delaware). In this model, the differential equations in the small opening are replaced by approximate transmission conditions for the electromagnetic fields across the interface. We also assume that the undamaged or background state is known and it is desired to find where the delamination has opened. We adapt the linear sampling method to this configuration in order to locate the damaged part of the interface from a knowledge of the scattered field and the undamaged configuration, but without needing to know the electromagnetic properties of the opening. Numerical examples are presented to validate our algorithm.

  7. Transient Dynamic Response of Delaminated Composite Rotating Shallow Shells Subjected to Impact

    Directory of Open Access Journals (Sweden)

    Amit Karmakar

    2006-01-01

    Full Text Available In this paper a transient dynamic finite element analysis is presented to study the response of delaminated composite pretwisted rotating shallow shells subjected to low velocity normal impact. Lagrange's equation of motion is used to derive the dynamic equilibrium equation and moderate rotational speeds are considered wherein the Coriolis effect is negligible. An eight noded isoparametric plate bending element is employed in the finite element formulation incorporating rotary inertia and effects of transverse shear deformation based on Mindlin's theory. To satisfy the compatibility of deformation and equilibrium of resultant forces and moments at the delamination crack front a multipoint constraint algorithm is incorporated which leads to unsymmetric stiffness matrices. The modified Hertzian contact law which accounts for permanent indentation is utilized to compute the contact force, and the time dependent equations are solved by Newmark's time integration algorithm. Parametric studies are performed in respect of location of delamination, angle of twist and rotational speed for centrally impacted graphite-epoxy composite cylindrical shells.

  8. Quasistatic Delamination of Sandwich-Like Kirchhoff-Love Plates

    Czech Academy of Sciences Publication Activity Database

    Freddi, L.; Roubíček, Tomáš; Zanini, Ch.

    2013-01-01

    Roč. 113, č. 2 (2013), s. 219-250 ISSN 0374-3535 R&D Projects: GA ČR GAP201/10/0357 Institutional research plan: CEZ:AV0Z20760514 Keywords : adhesive contact * delamination * mixed modes Subject RIV: BA - General Mathematics Impact factor: 1.043, year: 2013

  9. Utilization of Large Cohesive Interface Elements for Delamination Simulation

    DEFF Research Database (Denmark)

    Bak, Brian Lau Verndal; Lund, Erik

    2012-01-01

    This paper describes the difficulties of utilizing large interface elements in delamination simulation. Solutions to increase the size of applicable interface elements are described and cover numerical integration of the element and modifications of the cohesive law....

  10. Modeling Delamination of Interfacial Corner Cracks in Multilayered Structures

    DEFF Research Database (Denmark)

    Veluri, Badrinath (Badri); Jensen, Henrik Myhre

    2013-01-01

    Multilayered electronic components, typically of heterogeneous materials, delaminate under thermal and mechanical loading. A phenomenological model focused on modeling the shape of such interface cracks close to corners in layered interconnect structures for calculating the critical stress...

  11. Distributed fiber optic sensor-enhanced detection and prediction of shrinkage-induced delamination of ultra-high-performance concrete overlay

    Science.gov (United States)

    Bao, Yi; Valipour, Mahdi; Meng, Weina; Khayat, Kamal H.; Chen, Genda

    2017-08-01

    This study develops a delamination detection system for smart ultra-high-performance concrete (UHPC) overlays using a fully distributed fiber optic sensor. Three 450 mm (length) × 200 mm (width) × 25 mm (thickness) UHPC overlays were cast over an existing 200 mm thick concrete substrate. The initiation and propagation of delamination due to early-age shrinkage of the UHPC overlay were detected as sudden increases and their extension in spatial distribution of shrinkage-induced strains measured from the sensor based on pulse pre-pump Brillouin optical time domain analysis. The distributed sensor is demonstrated effective in detecting delamination openings from microns to hundreds of microns. A three-dimensional finite element model with experimental material properties is proposed to understand the complete delamination process measured from the distributed sensor. The model is validated using the distributed sensor data. The finite element model with cohesive elements for the overlay-substrate interface can predict the complete delamination process.

  12. Delaminating and restacking MgAl-layered double hydroxide monitored and characterized by a range of instrumental methods

    Science.gov (United States)

    Muráth, Szabolcs; Somosi, Zoltán; Tóth, Ildikó Y.; Tombácz, Etelka; Sipos, Pál; Pálinkó, István

    2017-07-01

    The delamination-restacking properties of MgAl-layered double hydroxide (MgAl-LDH) were studied in various solvents. The LDH samples were successfully delaminated in polar amides (formamide, N-methylformamide, N-methylacetamide). Usually, delamination was finalized by ultrasonic treatment. As rehydrating solutions, numerous Na-salts with single-, double- and triple-charged anions were used. Reconstruction was accomplished with anions of one or two negative charges, but triple-charged ones generally disrupted the rebuilding process, likely, because their salts with the metals of the LDH are very stable, and the thin layers can more readily transform to salts than the ordered materials. Samples and delamination-restacking processes were characterized by X-ray diffractometry (XRD), infrared spectroscopy (IR), dynamic light scattering (DLS), scanning electron microscopy (SEM) and energy-dispersive X-ray analysis (EDX).

  13. The ‘Sticky Elastica’: delamination blisters beyond small deformations

    KAUST Repository

    Wagner, Till J. W.; Vella, Dominic

    2013-01-01

    We consider the form of an elastic loop adhered to a rigid substrate: the 'Sticky Elastica'. In contrast to previous studies of the shape of delamination 'blisters', the theory developed accounts for deflections with large slope (i.e. geometrically

  14. Structural health monitoring strategy for detection of interlaminar delamination in composite plates

    International Nuclear Information System (INIS)

    Quaegebeur, N; Micheau, P; Masson, P; Maslouhi, A

    2010-01-01

    In this paper, a structural health monitoring strategy for detecting interlaminar delamination in a carbon fiber reinforced polymer structure using Lamb waves is proposed. The delamination is simulated by inserting a Teflon tape between two transverse plies and the Lamb wave generation and measurement is enabled by using piezoceramic elements. The Lamb wave theoretical propagation and through thickness strain distribution are studied, in order to determine the optimal configuration of the final system in terms of mode and frequency selection, and piezoceramic sizing and spacing, for detection of cross-sectional delamination. Pitch and catch measurements are performed by comparing wave propagations for different frequencies and along damaged and undamaged paths of the structure, and the analysis of results is performed using the reassigned short time Fourier transform. It appears that in the low frequency range (below 300 kHz), the A0 mode is sensitive to the damage, while in the high frequency range, S1 and A1 modes are both very sensitive to the damage while the propagation of the S0 mode is not affected very much

  15. Identification of delamination interface in composite laminates using scattering characteristics of lamb wave: numerical and experimental studies

    Science.gov (United States)

    Singh, Rakesh Kumar; Ramadas, C.; Balachandra Shetty, P.; Satyanarayana, K. G.

    2017-04-01

    Considering the superior strength properties of polymer based composites over metallic materials, they are being used in primary structures of aircrafts. However, these polymeric materials are much more complex in behaviour due to their structural anisotropy along with existence of different materials unlike in metallic alloys. These pose challenge in flaw detection, residual strength determination and life of a structure with their high susceptibility to impact damage in the form of delaminations/disbonds or cracks. This reduces load-bearing capability and potentially leads to structural failure. With this background, this study presents a method to identify location of delamination interface along thickness of a laminate. Both numerical and experimental studies have been carried out with a view to identify the defect, on propagation, mode conversion and scattering characteristics of fundamental anti-symmetric Lamb mode (Ao) when it passed through a semi-infinite delamination. Further, the reflection and transmission scattering coefficients based on power and amplitude ratios of the scattered waves have been computed. The methodology was applied on numerically simulated delaminations to illustrate the efficacy of the method. Results showed that it could successfully identify delamination interface.

  16. Time dependent response of low velocity impact induced composite conical shells under multiple delamination

    Science.gov (United States)

    Dey, Sudip; Karmakar, Amit

    2014-02-01

    This paper presents the time dependent response of multiple delaminated angle-ply composite pretwisted conical shells subjected to low velocity normal impact. The finite element formulation is based on Mindlin's theory incorporating rotary inertia and effects of transverse shear deformation. An eight-noded isoparametric plate bending element is employed to satisfy the compatibility of deformation and equilibrium of resultant forces and moments at the delamination crack front. A multipoint constraint algorithm is incorporated which leads to asymmetric stiffness matrices. The modified Hertzian contact law which accounts for permanent indentation is utilized to compute the contact force, and the time dependent equations are solved by Newmark's time integration algorithm. Parametric studies are conducted with respect to triggering parameters like laminate configuration, location of delamination, angle of twist, velocity of impactor, and impactor's displacement for centrally impacted shells.

  17. Laser micromachining of indium tin oxide films on polymer substrates by laser-induced delamination

    International Nuclear Information System (INIS)

    Willis, David A; Dreier, Adam L

    2009-01-01

    A Q-switched neodymium : yttrium-aluminium-garnet (Nd : YAG) laser was used to ablate indium tin oxide (ITO) thin films from polyethylene terephthalate substrates. Film damage and partial removal with no evidence of a melt zone was observed above 1.7 J cm -2 . Above the film removal threshold (3.3 J cm -2 ) the entire film thickness was removed without substrate damage, suggesting that ablation was a result of delamination of the film in the solid phase. Measurements of ablated fragment velocities near the ablation threshold were consistent with calculations of velocities caused by stress-induced delamination of the ITO film, except for a high velocity component at higher fluences. Nanosecond time-resolved shadowgraph photography revealed that the high velocity component was a shock wave induced by the rapid compression of ambient air when the film delaminated.

  18. Enhancement of delamination strength in Cu-stabilized coated conductor tapes through additional treatments under transverse tension at room temperature

    Energy Technology Data Exchange (ETDEWEB)

    Shin, Hyung Seop; Bautista, Zhierwinjay [Andong National University, Andong (Korea, Republic of); Moon, Seung Hyun; Lee, Jae Hun; Mean, Byoung Jean [SuNAM Co Ltd., Anseong (Korea, Republic of)

    2017-06-15

    In superconducting coil applications particularly in wet wound coils, coated conductor (CC) tapes are subjected to different type of stresses that could affect its electromechanical transport property. These include hoop stress acting along the length of the CC tape and the Lorentz force acting perpendicular to the CC tape’s surface. Since the latter is commonly associated with the delamination problem of multi-layered REBCO CC tapes, more understanding and attention on the delamination phenomena induced in the case of coil applications are needed. Difference on the coefficient of thermal expansion (CTE) of each constituent layer of the CC tape, the bobbin, and the impregnating materials is the main causes of delamination in CC tapes when subjected to thermal and mechanical cycling. In the design of degradation-free superconducting coils, therefore, characterization of the delamination behaviors including mechanism and strength in the multi-layered REBCO CC tapes becomes a critical issue. Various trials to increase the delamination strength by improving interface characteristics at interlayers have been performed. In this study, in order to investigate the influences of laser cleaning and Ag annealing treated at the substrate side surface, transverse tensile tests were conducted under different sample configurations using 4.5mm x 8 mm upper anvil. The mechanical delamination strength of differently processed CC samples was examined at room temperature (RT). As a result, the Sample 1 with the additional laser cleaning and Ag annealing processes and the Sample 2 with additional Ag annealing process only showed higher mechanical delamination strength as compared to the Sample 3 without such additional treatments. Sample 3 showed quite different behavior when the loading direction is to the substrate side where the delamination strength much lower as compared to other cases.

  19. Dynamic behavior of a rotating delaminated composite beam including rotary inertia and shear deformation effects

    Directory of Open Access Journals (Sweden)

    Ramazan-Ali Jafari-Talookolaei

    2015-09-01

    Full Text Available A finite element (FE model is developed to study the free vibration of a rotating laminated composite beam with a single delamination. The rotary inertia and shear deformation effects, as well as the bending–extension, bending–twist and extension–twist coupling terms are taken into account in the FE model. Comparison between the numerical results of the present model and the results published in the literature verifies the validity of the present model. Furthermore, the effects of various parameters, such as delamination size and location, fiber orientation, hub radius, material anisotropy and rotating speed, on the vibration of the beam are studied in detail. These results provide useful information in the study of the free vibration of rotating delaminated composite beams.

  20. Delamination and debonding failure of laminated composite T-joints

    NARCIS (Netherlands)

    Cui, H.

    2014-01-01

    Composites are increasingly being used in aerospace, automotive and other industries. The T-joint (also named stringer stiffened skin) is a typical connection, broadly used in thin-walled structures, such as the wing and fuselage of aircraft. This thesis presents the analysis of the delamination and

  1. Elevated temperature crack growth in advanced powder metallurgy aluminum alloys

    Science.gov (United States)

    Porr, William C., Jr.; Gangloff, Richard P.

    1990-01-01

    Rapidly solidified Al-Fe-V-Si powder metallurgy alloy FVS0812 is among the most promising of the elevated temperature aluminum alloys developed in recent years. The ultra fine grain size and high volume fraction of thermally stable dispersoids enable the alloy to maintain tensile properties at elevated temperatures. In contrast, this alloy displays complex and potentially deleterious damage tolerant and time dependent fracture behavior that varies with temperature. J-Integral fracture mechanics were used to determine fracture toughness (K sub IC) and crack growth resistance (tearing modulus, T) of extruded FVS0812 as a function of temperature. The alloy exhibits high fracture properties at room temperature when tested in the LT orientation, due to extensive delamination of prior ribbon particle boundaries perpendicular to the crack front. Delamination results in a loss of through thickness constraint along the crack front, raising the critical stress intensity necessary for precrack initiation. The fracture toughness and tensile ductility of this alloy decrease with increasing temperature, with minima observed at 200 C. This behavior results from minima in the intrinsic toughness of the material, due to dynamic strain aging, and in the extent of prior particle boundary delaminations. At 200 C FVS0812 fails at K levels that are insufficient to cause through thickness delamination. As temperature increases beyond the minimum, strain aging is reduced and delamination returns. For the TL orientation, K (sub IC) decreased and T increased slightly with increasing temperature from 25 to 316 C. Fracture in the TL orientation is governed by prior particle boundary toughness; increased strain localization at these boundaries may result in lower toughness with increasing temperature. Preliminary results demonstrate a complex effect of loading rate on K (sub IC) and T at 175 C, and indicate that the combined effects of time dependent deformation, environment, and strain aging

  2. Testing linear growth rate formulas of non-scale endogenous growth models

    NARCIS (Netherlands)

    Ziesemer, Thomas

    2017-01-01

    Endogenous growth theory has produced formulas for steady-state growth rates of income per capita which are linear in the growth rate of the population. Depending on the details of the models, slopes and intercepts are positive, zero or negative. Empirical tests have taken over the assumption of

  3. Identification of Delamination in Concrete Slabs by SIBIE Procedure

    International Nuclear Information System (INIS)

    Yamada, M.; Yagi, Y.; Ohtsu, M.

    2017-01-01

    The Impact-Echo method is known as a non-destructive testing for concrete structures. The technique is based on the use of low-frequency elastic waves that propagate in concrete to determine the thickness and to detect internal flaws in concrete. The presence and locations of defects in concrete are estimated from identifying peak frequencies in the frequency spectra, which are responsible for the resonance due to time-of-flight from the defects. In practical applications, however, obtained spectra include so many peak frequencies that it is fairly difficult to identify the defects correctly. In order to improve the Impact-Echo method, Stack Imaging of spectral amplitudes Based on Impact-Echo (SIBIE) procedure is developed as an imaging technique applied to the Impact-Echo data, where defects in concrete are identified visually at the cross-section. In this study, the SIBIE procedure is applied to identify the delamination in a concrete slab. It is demonstrated that the delamination can be identified with reasonable accuracy. (paper)

  4. Larval developmental rate, metabolic rate and future growth performance in Atlantic salmon

    DEFF Research Database (Denmark)

    Serrano, Jonathan Vaz; Åberg, Madelene; Gjoen, Hans Magnus

    2009-01-01

    , quantified as time to first feeding, and growth in later stages was demonstrated in Atlantic salmon (Salmo salar L.). The observed relationship between future growth and larval developmental rate suggests that sorting larvae by time to first feeding can be a potential tool to optimize feeding strategies...... and growth in commercial rearing of Atlantic salmon. Furthermore, the link between larval standard metabolic rate and developmental rate and future growth is discussed in the present study....

  5. Connection between the growth rate distribution and the size dependent crystal growth

    Science.gov (United States)

    Mitrović, M. M.; Žekić, A. A.; IIić, Z. Z.

    2002-07-01

    The results of investigations of the connection between the growth rate dispersions and the size dependent crystal growth of potassium dihydrogen phosphate (KDP), Rochelle salt (RS) and sodium chlorate (SC) are presented. A possible way out of the existing confusion in the size dependent crystal growth investigations is suggested. It is shown that the size independent growth exists if the crystals belonging to one growth rate distribution maximum are considered separately. The investigations suggest possible reason for the observed distribution maxima widths, and the high data scattering on the growth rate versus the crystal size dependence.

  6. Delamination of neural crest cells requires transient and reversible Wnt inhibition mediated by Dact1/2.

    Science.gov (United States)

    Rabadán, M Angeles; Herrera, Antonio; Fanlo, Lucia; Usieto, Susana; Carmona-Fontaine, Carlos; Barriga, Elias H; Mayor, Roberto; Pons, Sebastián; Martí, Elisa

    2016-06-15

    Delamination of neural crest (NC) cells is a bona fide physiological model of epithelial-to-mesenchymal transition (EMT), a process that is influenced by Wnt/β-catenin signalling. Using two in vivo models, we show that Wnt/β-catenin signalling is transiently inhibited at the time of NC delamination. In attempting to define the mechanism underlying this inhibition, we found that the scaffold proteins Dact1 and Dact2, which are expressed in pre-migratory NC cells, are required for NC delamination in Xenopus and chick embryos, whereas they do not affect the motile properties of migratory NC cells. Dact1/2 inhibit Wnt/β-catenin signalling upstream of the transcriptional activity of T cell factor (TCF), which is required for EMT to proceed. Dact1/2 regulate the subcellular distribution of β-catenin, preventing β-catenin from acting as a transcriptional co-activator to TCF, yet without affecting its stability. Together, these data identify a novel yet important regulatory element that inhibits β-catenin signalling, which then affects NC delamination. © 2016. Published by The Company of Biologists Ltd.

  7. Metal-etching-free direct delamination and transfer of single-layer graphene with a high degree of freedom.

    Science.gov (United States)

    Yang, Sang Yoon; Oh, Joong Gun; Jung, Dae Yool; Choi, HongKyw; Yu, Chan Hak; Shin, Jongwoo; Choi, Choon-Gi; Cho, Byung Jin; Choi, Sung-Yool

    2015-01-14

    A method of graphene transfer without metal etching is developed to minimize the contamination of graphene in the transfer process and to endow the transfer process with a greater degree of freedom. The method involves direct delamination of single-layer graphene from a growth substrate, resulting in transferred graphene with nearly zero Dirac voltage due to the absence of residues that would originate from metal etching. Several demonstrations are also presented to show the high degree of freedom and the resulting versatility of this transfer method. © 2014 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

  8. Growth Rates of Microbes in the Oceans.

    Science.gov (United States)

    Kirchman, David L

    2016-01-01

    A microbe's growth rate helps to set its ecological success and its contribution to food web dynamics and biogeochemical processes. Growth rates at the community level are constrained by biomass and trophic interactions among bacteria, phytoplankton, and their grazers. Phytoplankton growth rates are approximately 1 d(-1), whereas most heterotrophic bacteria grow slowly, close to 0.1 d(-1); only a few taxa can grow ten times as fast. Data from 16S rRNA and other approaches are used to speculate about the growth rate and the life history strategy of SAR11, the most abundant clade of heterotrophic bacteria in the oceans. These strategies are also explored using genomic data. Although the methods and data are imperfect, the available data can be used to set limits on growth rates and thus on the timescale for changes in the composition and structure of microbial communities.

  9. Effect of massing on larval growth rate.

    Science.gov (United States)

    Johnson, Aidan P; Wallman, James F

    2014-08-01

    Estimation of minimum postmortem interval commonly relies on predicting the age of blowfly larvae based on their size and an estimate of the temperatures to which they have been exposed throughout their development. The majority of larval growth rate data have been developed using small larval masses in order to avoid excess heat generation. The current study collected growth rate data for larvae at different mass volumes, and assessed the temperature production of these masses, for two forensically important blow fly species, Chrysomya rufifacies and Calliphora vicina. The growth rate of larvae in a small mass, exposed to the higher temperatures equivalent to those experienced by large masses, was also assessed to determine if observed differences were due to the known temperature effects of maggot masses. The results showed that temperature production increased with increasing mass volume, with temperature increases of 11 °C observed in the large Ch. rufifacies masses and increases of 5 °C in the large C. vicina masses. Similarly, the growth rate of the larvae was affected by mass size. The larvae from small masses grown at the higher temperatures experienced by large masses displayed an initial delay in growth, but then grew at a similar rate to those larvae at a constant 23 °C. Since these larvae from masses of equivalent sizes displayed similar patterns of growth rate, despite differing temperatures, and these growth rates differed from larger masses exposed to the same temperatures, it can be concluded that larval growth rate within a mass may be affected by additional factors other than temperature. Overall, this study highlights the importance of understanding the role of massing in larval development and provides initial developmental data for mass sizes of two forensically important blowfly species commonly encountered in Australian forensic casework. Copyright © 2014 Elsevier Ireland Ltd. All rights reserved.

  10. Predictions and Experimental Microstructural Characterization of High Strain Rate Failure Modes in Layered Aluminum Composites

    Science.gov (United States)

    Khanikar, Prasenjit

    applications. The second major objective of this investigation was the use of recently developed dynamic fracture formulations to model and analyze the crack nucleation and propagation of aluminum layered composites subjected to high strain rate loading conditions and how microstructural effects, such as precipitates, dispersed particles, and GB orientations affect failure evolution. This dynamic fracture approach is used to investigate crack nucleation and crack growth as a function of the different microstructural characteristics of each alloy in layered composites with and without pre-existing cracks. The zigzag nature of the crack paths were mainly due to the microstructural features, such as precipitates and dispersed particles distributions and orientations ahead of the crack front, and it underscored the capabilities of the fracture methodology. The evolution of dislocation density and the formation of localized shear slip contributed to the blunting of the propagating crack. Extensive geometrical and thermal softening due to the localized plastic slip also affected crack path orientations and directions. These softening mechanisms resulted in the switching of cleavage planes, which affected crack path orientations. Interface delamination can also have an important role in the failure and toughening of the layered composites. Different scenarios of delamination were investigated, such as planar crack growth and crack penetration into the layers. The presence of brittle surface oxide platelets in the interface region also significantly influenced the interface delamination process. Transmission Electron Microscopy (TEM), Scanning Electron Microscopy (SEM) and Optical Microscopy (OM) characterization provided further physical insights and validation of the predictive capabilities. The inherent microstructural features of each alloy play a significant role in the dynamic fracture, shear strain localization, and interface delamination of the layered metallic composite

  11. An enriched cohesive zone model for delamination in brittle interfaces

    NARCIS (Netherlands)

    Samimi, M.; Dommelen, van J.A.W.; Geers, M.G.D.

    2009-01-01

    Application of standard cohesive zone models in a finite element framework to simulate delamination in brittle interfaces may trigger non-smooth load-displacement responses that lead to the failure of iterative solution procedures. This non-smoothness is an artifact of the discretization; and hence

  12. High acidity unilamellar zeolite MCM-56 and its pillared and delaminated derivatives.

    Science.gov (United States)

    Gil, Barbara; Makowski, Wacław; Marszalek, Bartosz; Roth, Wieslaw J; Kubu, Martin; Čejka, Jiři; Olejniczak, Zbigniew

    2014-07-21

    The unilamellar form of zeolite MWW, MCM-56, which is obtained by direct hydrothermal synthesis has been studied with regard to acidity and porosity in its original and post-synthesis modified pillared and delaminated forms. The acidity measured by FTIR was found to be only slightly lower than the highly active 3-D MWW forms, MCM-22 and MCM-49. Pivalonitrile adsorption, which is a measure of spatial openness, showed 50% accessibility vs. MCM-22/49. It highlights the potential of MCM-56 as a layered material with increased access to acid sites because it does not entail laborious post-synthesis modification. Swelling, pillaring and delamination of MCM-56 are facile but result in a reduction in the number of Brønsted acid sites (BAS) while increasing accessibility to pivalonitrile. The delamination procedure involving sonication and acidification of the highly basic mother liquor produces the most visible increase in surface area and access to all BAS. The accompanying doubling of the solid yield and the decrease in absolute number of BAS suggest significant precipitation of dissolved silica generated during swelling and sonication in high pH medium. The viability of separating surfactant covered layers upon sonication with the consequence of exposing hydrophobic hydrocarbon tails to aqueous environment is addressed.

  13. Floating Node Method and Virtual Crack Closure Technique for Modeling Matrix Cracking-Delamination Migration

    Science.gov (United States)

    DeCarvalho, Nelson V.; Chen, B. Y.; Pinho, Silvestre T.; Baiz, P. M.; Ratcliffe, James G.; Tay, T. E.

    2013-01-01

    A novel approach is proposed for high-fidelity modeling of progressive damage and failure in composite materials that combines the Floating Node Method (FNM) and the Virtual Crack Closure Technique (VCCT) to represent multiple interacting failure mechanisms in a mesh-independent fashion. In this study, the approach is applied to the modeling of delamination migration in cross-ply tape laminates. Delamination, matrix cracking, and migration are all modeled using fracture mechanics based failure and migration criteria. The methodology proposed shows very good qualitative and quantitative agreement with experiments.

  14. GROWTH RATE DISTRIBUTION OF BORAX SINGLE CRYSTALS ON THE (001 FACE UNDER VARIOUS FLOW RATES

    Directory of Open Access Journals (Sweden)

    Suharso Suharso

    2010-06-01

    Full Text Available The growth rates of borax single crystals from aqueous solutions at various flow rates in the (001 direction were measured using in situ cell method. From the growth rate data obtained, the growth rate distribution of borax crystals was investigated using Minitab Software and SPSS Software at relative supersaturation of 0807 and temperature of 25 °C. The result shows that normal, gamma, and log-normal distribution give a reasonably good fit to GRD. However, there is no correlation between growth rate distribution and flow rate of solution.   Keywords: growth rate dispersion (GRD, borax, flow rate

  15. Dinosaur Metabolism and the Allometry of Maximum Growth Rate.

    Science.gov (United States)

    Myhrvold, Nathan P

    2016-01-01

    The allometry of maximum somatic growth rate has been used in prior studies to classify the metabolic state of both extant vertebrates and dinosaurs. The most recent such studies are reviewed, and their data is reanalyzed. The results of allometric regressions on growth rate are shown to depend on the choice of independent variable; the typical choice used in prior studies introduces a geometric shear transformation that exaggerates the statistical power of the regressions. The maximum growth rates of extant groups are found to have a great deal of overlap, including between groups with endothermic and ectothermic metabolism. Dinosaur growth rates show similar overlap, matching the rates found for mammals, reptiles and fish. The allometric scaling of growth rate with mass is found to have curvature (on a log-log scale) for many groups, contradicting the prevailing view that growth rate allometry follows a simple power law. Reanalysis shows that no correlation between growth rate and basal metabolic rate (BMR) has been demonstrated. These findings drive a conclusion that growth rate allometry studies to date cannot be used to determine dinosaur metabolism as has been previously argued.

  16. Dinosaur Metabolism and the Allometry of Maximum Growth Rate

    Science.gov (United States)

    Myhrvold, Nathan P.

    2016-01-01

    The allometry of maximum somatic growth rate has been used in prior studies to classify the metabolic state of both extant vertebrates and dinosaurs. The most recent such studies are reviewed, and their data is reanalyzed. The results of allometric regressions on growth rate are shown to depend on the choice of independent variable; the typical choice used in prior studies introduces a geometric shear transformation that exaggerates the statistical power of the regressions. The maximum growth rates of extant groups are found to have a great deal of overlap, including between groups with endothermic and ectothermic metabolism. Dinosaur growth rates show similar overlap, matching the rates found for mammals, reptiles and fish. The allometric scaling of growth rate with mass is found to have curvature (on a log-log scale) for many groups, contradicting the prevailing view that growth rate allometry follows a simple power law. Reanalysis shows that no correlation between growth rate and basal metabolic rate (BMR) has been demonstrated. These findings drive a conclusion that growth rate allometry studies to date cannot be used to determine dinosaur metabolism as has been previously argued. PMID:27828977

  17. Fatigue crack propagation and delamination growth in Glare

    NARCIS (Netherlands)

    Alderliesten, R.C.

    2005-01-01

    Fibre Metal Laminate Glare consists of thin aluminium layers bonded together with pre-impregnated glass fibre layers and shows an excellent fatigue crack growth behaviour compared to monolithic aluminium. The fibres are insensitive to the occurring fatigue loads and remain intact while the fatigue

  18. Potential-Induced Degradation-Delamination Mode in Crystalline Silicon Modules: Preprint

    Energy Technology Data Exchange (ETDEWEB)

    Hacke, Peter L [National Renewable Energy Laboratory (NREL), Golden, CO (United States); Kempe, Michael D [National Renewable Energy Laboratory (NREL), Golden, CO (United States); Wohlgemuth, John [National Renewable Energy Laboratory (NREL), Golden, CO (United States); Li, Jichao [SunPower Corporation; Shen, Yu-Chen [SunPower Corporation

    2018-03-21

    A test sequence producing potential-induced degradation-delamination (PID-d) in crystalline silicon modules has been tested and found comparable under visual inspection to cell/encapsulant delamination seen in some fielded modules. Four commercial modules were put through this sequence, 85 degrees C, 85%, 1000 h damp heat, followed by an intensive PID stress sequence of 72 degrees C, 95% RH, and -1000 V, with the module face grounded using a metal foil. The 60 cell c-Si modules exhibiting the highest current transfer (4.4 center dot 10-4 A) exhibited PID-d at the first inspection after 156 h of PID stress. Effects promoting PID-d are reduced adhesion caused by damp heat, sodium migration further reducing adhesion to the cells, and gaseous products of electrochemical reactions driven by the applied system voltage. A new work item proposal for an IEC test standard to evaluate for PID-d is anticipated.

  19. Microtubules Growth Rate Alteration in Human Endothelial Cells

    Directory of Open Access Journals (Sweden)

    Irina B. Alieva

    2010-01-01

    Full Text Available To understand how microtubules contribute to the dynamic reorganization of the endothelial cell (EC cytoskeleton, we established an EC model expressing EB3-GFP, a protein that marks microtubule plus-ends. Using this model, we were able to measure microtubule growth rate at the centrosome region and near the cell periphery of a single human EC and in the EC monolayer. We demonstrate that the majority of microtubules in EC are dynamic, the growth rate of their plus-ends is highest in the internal cytoplasm, in the region of the centrosome. Growth rate of microtubule plus-ends decreases from the cell center toward the periphery. Our data suggest the existing mechanism(s of local regulation of microtubule plus-ends growth in EC. Microtubule growth rate in the internal cytoplasm of EC in the monolayer is lower than that of single EC suggesting the regulatory effect of cell-cell contacts. Centrosomal microtubule growth rate distribution in single EC indicated the presence of two subpopulations of microtubules with “normal” (similar to those in monolayer EC and “fast” (three times as much growth rates. Our results indicate functional interactions between cell-cell contacts and microtubules.

  20. Exchange-rate regimes and economic growth: An empirical evaluation

    OpenAIRE

    Simón Sosvilla-Rivero; María del Carmen Ramos-Herrera

    2014-01-01

    Based on a dataset of 123 economies, this paper empirically investigates the relation between exchange-rate regimes and economic growth. We find that growth performance is best under intermediate exchange rate regimes, while the smallest growth rates are associated with flexible exchange rates. Nevertheless, this conclusion is tempered when we analyze the countries by income level: even though countries that adopt intermediate exchange-rate regimes are characterized by higher economic growth,...

  1. The effect of nylon nanofibers on the dynamic behaviour and the delamination resistance of GFRP composites

    Directory of Open Access Journals (Sweden)

    Garcia Cristobal

    2018-01-01

    Full Text Available Vibrations are responsible for a considerable number of accidents in aircrafts, bridges and other civil engineering structures. Therefore, there is a need to reduce the vibrations on structures made of composite materials. Delamination is a particularly dangerous failure mode for composite materials because delaminated composites can lose up to 60% of their strength and stiffness and still remain unchanged. One of the methods to suppress vibrations and preventing delamination is to incorporate nanofibers into the composite laminates. The aim of the present work is to investigate how nylon nanofibers affect the dynamic behaviour and delamination resistance of glass fibre reinforced polymer (GFRP composites. Experiments and numerical simulations using finite element modelling (FEM analysis are used to estimate the natural frequencies, the damping ratio and inter-laminar strength in GFRP composites with and without nylon nanofibers. It is found that the natural frequencies of the nylon nano-modified composites do not change significantly as compared to the traditional composites. However, nano-modified composites demonstrated a considerable increase in damping ratio and inter-laminar shear strength due to the incorporation of nylon nanofibers. This work contributes to the knowledge about the mechanical and dynamic properties of glass fibre reinforced polymer (GFRP composites with nylon nanofibers.

  2. Laser Structuring of Thin Layers for Flexible Electronics by a Shock Wave-induced Delamination Process

    Science.gov (United States)

    Lorenz, Pierre; Ehrhardt, Martin; Zimmer, Klaus

    The defect-free laser-assisted structuring of thin films on flexible substrates is a challenge for laser methods. However, solving this problem exhibits an outstanding potential for a pioneering development of flexible electronics. Thereby, the laser-assisted delamination method has a great application potential. At the delamination process: the localized removal of the layer is induced by a shock wave which is produced by a laser ablation process on the rear side of the substrate. In this study, the thin-film patterning process is investigated for different polymer substrates dependent on the material and laser parameters using a KrF excimer laser. The resultant structures were studied by optical microscopy and white light interferometry (WLI). The delamination process was tested at different samples (indium tin oxide (ITO) on polyethylene terephthalate (PET), epoxy-based negative photoresist (SU8) on polyimide (PI) and indium tin oxide/copper indium gallium selenide/molybdenum (ITO/CIGS/Mo) on PI.

  3. Microwave detection of delaminations between fiber reinforced polymer (FRP) composite and hardened cement paste

    Science.gov (United States)

    Hughes, D.; Kazemi, M.; Marler, K.; Zoughi, R.; Myers, J.; Nanni, A.

    2002-05-01

    Fiber reinforced polymer (FRP) composites are increasingly being used for the rehabilitation of concrete structures. Detection and characterization of delaminations between an FRP composite and a concrete surface are of paramount importance. Consequently, the development of a one sided, non-contact, real time and rapid nondestructive testing (NDT) technique for this purpose is of great interest. Near-field microwave NDT techniques, using open-ended rectangular waveguide probes, have shown great potential for detecting delaminations in layered composite structures such as these. The results of some theoretical and experimental investigations on a specially prepared cement paste specimen are presented here.

  4. Growth and development rates have different thermal responses.

    Science.gov (United States)

    Forster, Jack; Hirst, Andrew G; Woodward, Guy

    2011-11-01

    Growth and development rates are fundamental to all living organisms. In a warming world, it is important to determine how these rates will respond to increasing temperatures. It is often assumed that the thermal responses of physiological rates are coupled to metabolic rate and thus have the same temperature dependence. However, the existence of the temperature-size rule suggests that intraspecific growth and development are decoupled. Decoupling of these rates would have important consequences for individual species and ecosystems, yet this has not been tested systematically across a range of species. We conducted an analysis on growth and development rate data compiled from the literature for a well-studied group, marine pelagic copepods, and use an information-theoretic approach to test which equations best describe these rates. Growth and development rates were best characterized by models with significantly different parameters: development has stronger temperature dependence than does growth across all life stages. As such, it is incorrect to assume that these rates have the same temperature dependence. We used the best-fit models for these rates to predict changes in organism mass in response to temperature. These predictions follow a concave relationship, which complicates attempts to model the impacts of increasing global temperatures on species body size.

  5. Division-Based, Growth Rate Diversity in Bacteria

    Directory of Open Access Journals (Sweden)

    Ghislain Y. Gangwe Nana

    2018-05-01

    Full Text Available To investigate the nature and origins of growth rate diversity in bacteria, we grew Escherichia coli and Bacillus subtilis in liquid minimal media and, after different periods of 15N-labeling, analyzed and imaged isotope distributions in individual cells with Secondary Ion Mass Spectrometry. We find a striking inter- and intra-cellular diversity, even in steady state growth. This is consistent with the strand-dependent, hyperstructure-based hypothesis that a major function of the cell cycle is to generate coherent, growth rate diversity via the semi-conservative pattern of inheritance of strands of DNA and associated macromolecular assemblies. We also propose quantitative, general, measures of growth rate diversity for studies of cell physiology that include antibiotic resistance.

  6. Measurements of Protein Crystal Face Growth Rates

    Science.gov (United States)

    Gorti, S.

    2014-01-01

    Protein crystal growth rates will be determined for several hyperthermophile proteins.; The growth rates will be assessed using available theoretical models, including kinetic roughening.; If/when kinetic roughening supersaturations are established, determinations of protein crystal quality over a range of supersaturations will also be assessed.; The results of our ground based effort may well address the existence of a correlation between fundamental growth mechanisms and protein crystal quality.

  7. Analytical prediction model for non-symmetric fatigue crack growth in Fibre Metal Laminates

    NARCIS (Netherlands)

    Wang, W.; Rans, C.D.; Benedictus, R.

    2017-01-01

    This paper proposes an analytical model for predicting the non-symmetric crack growth and accompanying delamination growth in FMLs. The general approach of this model applies Linear Elastic Fracture Mechanics, the principle of superposition, and displacement compatibility based on the

  8. Emittance growth rates for displaced beams

    International Nuclear Information System (INIS)

    Anderson, O.A.

    1993-05-01

    Emittance growth rates have been previously analyzed for nonuniform beams in linear channels and for initially uniform mismatched beams in nonlinear channels. These studies were for centered beams. Additional emittance growth can arise in cases where the beam is initially displaced. The purpose of this study is to obtain growth rates for displaced beams. This work differs from studies involving random displacement of electrodes. Our analysis assumes instead that the focusing system is perfectly aligned but that the beam is initially displaced with respect to the equilibrium axis. If the focusing force is slightly nonlinear, we find a gradual transfer of the potential energy of beam displacement into kinetic energy associated with emittance growth. We present explicit results for the emittance growth distance as a function of the nonlinearity of the channel. These results will have practical importance for designers of accelerators and transport systems when setting realistic tolerances for initial beam alignment. These tolerances will depend on the nonlinearity and the length of the system

  9. Growth rate of YBCO-Ag superconducting single grains

    Science.gov (United States)

    Congreve, J. V. J.; Shi, Y. H.; Dennis, A. R.; Durrell, J. H.; Cardwell, D. A.

    2017-12-01

    The large scale use of (RE)Ba2Cu3O7 bulk superconductors, where RE=Y, Gd, Sm, is, in part, limited by the relatively poor mechanical properties of these inherently brittle ceramic materials. It is reported that alloying of (RE)Ba2Cu3O7 with silver enables a significant improvement in the mechanical strength of bulk, single grain samples without any detrimental effect on their superconducting properties. However, due to the complexity and number of inter-related variables involved in the top seeded melt growth (TSMG) process, the growth of large single grains is difficult and the addition of silver makes it even more difficult to achieve successful growth reliably. The key processing variables in the TSMG process include the times and temperatures of the stages within the heating profile, which can be derived from the growth rate during the growth process. To date, the growth rate of the YBa2Cu3O7-Ag system has not been reported in detail and it is this lacuna that we have sought to address. In this work we measure the growth rate of the YBCO-Ag system using a method based on continuous cooling and isothermal holding (CCIH). We have determined the growth rate by measuring the side length of the crystallised region for a number of samples for specified isothermal hold temperatures and periods. This has enabled the growth rate to be modelled and from this an optimized heating profile for the successful growth of YBCO-Ag single grains to be derived.

  10. Feedback amplification loop drives malignant growth in epithelial tissues.

    Science.gov (United States)

    Muzzopappa, Mariana; Murcia, Lada; Milán, Marco

    2017-08-29

    Interactions between cells bearing oncogenic mutations and the surrounding microenvironment, and cooperation between clonally distinct cell populations, can contribute to the growth and malignancy of epithelial tumors. The genetic techniques available in Drosophila have contributed to identify important roles of the TNF-α ligand Eiger and mitogenic molecules in mediating these interactions during the early steps of tumor formation. Here we unravel the existence of a tumor-intrinsic-and microenvironment-independent-self-reinforcement mechanism that drives tumor initiation and growth in an Eiger-independent manner. This mechanism relies on cell interactions between two functionally distinct cell populations, and we present evidence that these cell populations are not necessarily genetically different. Tumor-specific and cell-autonomous activation of the tumorigenic JNK stress-activated pathway drives the expression of secreted signaling molecules and growth factors to delaminating cells, which nonautonomously promote proliferative growth of the partially transformed epithelial tissue. We present evidence that cross-feeding interactions between delaminating and nondelaminating cells increase each other's sizes and that these interactions can explain the unlimited growth potential of these tumors. Our results will open avenues toward our molecular understanding of those social cell interactions with a relevant function in tumor initiation in humans.

  11. Minimizing and predicting delamination of southern plywood in exterior exposure

    Science.gov (United States)

    Peter Koch

    1967-01-01

    Southern pine plywood is substantially all being manufactured with phenolic glue for exterior use. Because panels must not delaminate in service, a reliable predictor of glueline durability is required. Drawing on the experience of the Douglas-fir plywood industry, southern manufacutrers have adopted as a predictor the percentage of wood failure(% WF) observed in...

  12. Delamination Mechanisms of Thermal and Environmental Barrier Coatings on SiC/SiC Ceramic Matrix Composites

    Science.gov (United States)

    Zhu, Dongming; Choi, Sung R.; Lee, Kang N.; Miller, Robert A.

    2003-01-01

    Advanced ceramic thermal harrier coatings will play an increasingly important role In future gas turbine engines because of their ability to effectively protect the engine components and further raise engine temperatures. However, the coating durability issue remains a major concern with the ever-increasing temperature requirements. In this paper, thermal cyclic response and delamination failure modes of a ZrO2-8wt%Y2O3 and mullite/BSAS thermaVenvironmenta1 barrier coating system on SiC/SiC ceramic matrix composites were investigated using a laser high-heat-flux technique. The coating degradation and delamination processes were monitored in real time by measuring coating apparent conductivity changes during the cyclic tests under realistic engine temperature and stress gradients, utilizing the fact that delamination cracking causes an apparent decrease in the measured thermal conductivity. The ceramic coating crack initiation and propagation driving forces under the cyclic thermal loads, in conjunction with the mechanical testing results, will be discussed.

  13. Growth rate, population entropy, and perturbation theory.

    OpenAIRE

    Demetrius, L.

    1989-01-01

    This paper is concerned with the connection between two classes of population variables: measures of population growth rate—the Malthusian parameter, the net reproduction rate, the gross reproduction rate, and the mean life expectancy; and measures of demographic heterogeneity—population entropy. It is shown that the entropy functions predict the response of the growth rate parameters to perturbations in the age-specific fecundity and mortality schedule. These results are invoked to introduce...

  14. Delamination Assessment Tool for Spacecraft Composite Structures

    Science.gov (United States)

    Portela, Pedro; Preller, Fabian; Wittke, Henrik; Sinnema, Gerben; Camanho, Pedro; Turon, Albert

    2012-07-01

    Fortunately only few cases are known where failure of spacecraft structures due to undetected damage has resulted in a loss of spacecraft and launcher mission. However, several problems related to damage tolerance and in particular delamination of composite materials have been encountered during structure development of various ESA projects and qualification testing. To avoid such costly failures during development, launch or service of spacecraft, launcher and reusable launch vehicles structures a comprehensive damage tolerance verification approach is needed. In 2009, the European Space Agency (ESA) initiated an activity called “Delamination Assessment Tool” which is led by the Portuguese company HPS Lda and includes academic and industrial partners. The goal of this study is the development of a comprehensive damage tolerance verification approach for launcher and reusable launch vehicles (RLV) structures, addressing analytical and numerical methodologies, material-, subcomponent- and component testing, as well as non-destructive inspection. The study includes a comprehensive review of current industrial damage tolerance practice resulting from ECSS and NASA standards, the development of new Best Practice Guidelines for analysis, test and inspection methods and the validation of these with a real industrial case study. The paper describes the main findings of this activity so far and presents a first iteration of a Damage Tolerance Verification Approach, which includes the introduction of novel analytical and numerical tools at an industrial level. This new approach is being put to the test using real industrial case studies provided by the industrial partners, MT Aerospace, RUAG Space and INVENT GmbH

  15. Contribution to interplay between a delamination test and a sensory analysis of mid-range lipsticks.

    Science.gov (United States)

    Richard, C; Tillé-Salmon, B; Mofid, Y

    2016-02-01

    Lipstick is currently one of the most sold products of cosmetics industry, and the competition between the various manufacturers is significant. Customers mainly seek products with high spreadability, especially long-lasting or long wear on the lips. Evaluation tests of cosmetics are usually performed by sensory analysis. This can then represent a considerable cost. The object of this study was to develop a fast and simple test of delamination (objective method with calibrated instruments) and to interplay the obtained results with those of a discriminative sensory analysis (subjective method) in order to show the relevance of the instrumental test. Three mid-range lipsticks were randomly chosen and were tested. They were made of compositions as described by the International Nomenclature of Cosmetic Ingredients (INCI). Instrumental characterization was performed by texture profile analysis and by a special delamination test. The sensory analysis was voluntarily conducted with an untrained panel as blind test to confirm or reverse the possible interplay. The two approaches or methods gave the same type of classification. The high-fat lipstick had the worst behaviour with the delamination test and the worst notation of the intensity of descriptors with the sensory analysis. There is a high correlation between the sensory analysis and the instrumental measurements in this study. The delamination test carried out should permit to quickly determine the lasting (screening test) and in consequence optimize the basic formula of lipsticks. © 2015 Society of Cosmetic Scientists and the Société Française de Cosmétologie.

  16. Study on Fatigue Performance of Composite Bolted Joints with Bolt-Hole Delamination

    Science.gov (United States)

    Liu, M. J.; Yu, S.; Zhao, Q. Y.

    2018-03-01

    Fatigue performance of composite structure with imperfections is a challenging subject at present. Based on cohesive zone method and multi-continuum theory, delamination evolution response and fatigue life prediction of a 3D composite single-lap joint with a bolt-hole have been investigated through computer codes Abaqus and Fe-safe. Results from the comparison of a perfect composite bolted joint with another defect one indicates that a relatively small delamination damage around the bolt hole brings about significant degradation of local material performance. More notably, fatigue life of stress concentration region of composite bolted joints is highly sensitive to external loads, as an increase of 67% cyclic load amplitude leads to an decrease of 99.5% local fatigue life in this study. However, the numerical strategy for solving composite fatigue problems is meaningful to engineering works.

  17. DETECTION OF DELAMINATION IN A COMPOSITE PLATE BY SEM

    Institute of Scientific and Technical Information of China (English)

    2001-01-01

    A numerical method of integration of Green's functi ons of strip element method (SEM) is proposed. The response of ultrasonic sourc e generated by a transducer on the surface of a multi-ply composite plate conta ining a delamination is analyzed by the use of SEM. The numerical results show that the scanning features of the ultrasonic waves may be used to identify the d elamination inside the composite plate .

  18. EVIDENCE ON EMPLOYMENT RATE AND ECONOMIC GROWTH

    Directory of Open Access Journals (Sweden)

    Cornelia VĂCEANU

    2014-11-01

    Full Text Available This paper explores a causal relationship between employment rate and economic growth for European Union countries, in general, and produces a structural assessment of employment on the background of labour market dynamics. Economic growth is the key in economic theory and the main source of well-being and quality of life. Since the 2008 financial crisis, most European countries have experienced job shortage and unemployment problem, but today's European economic outlook is strengthening on the bases of a GDP growing momentum. Empirical data shows, regardless the GDP's moderate positive trend, the employment rate did not increase enough. Given this, the present analysis address the question: to what extent the employment rate is affected by economic growth?

  19. Shadowgraph studies of laser-assisted non-thermal structuring of thin layers on flexible substrates by shock-wave-induced delamination processes

    Energy Technology Data Exchange (ETDEWEB)

    Lorenz, Pierre, E-mail: pierre.lorenz@iom-leipzig.de [Leibniz-Institut für Oberflächenmodifizierung e. V., Permoserstraße 15, 04318 Leipzig (Germany); Smausz, Tomi [Department of Optics and Quantum Electronics, University of Szeged, H-6720 Szeged, Dóm tér 9 (Hungary); MTA-SZTE Research Group on Photoacoustic Spectroscopy, University of Szeged, H-6720 Szeged, Dóm tér 9 (Hungary); Csizmadia, Tamas [Department of Optics and Quantum Electronics, University of Szeged, H-6720 Szeged, Dóm tér 9 (Hungary); Ehrhardt, Martin; Zimmer, Klaus [Leibniz-Institut für Oberflächenmodifizierung e. V., Permoserstraße 15, 04318 Leipzig (Germany); Hopp, Bela [Department of Optics and Quantum Electronics, University of Szeged, H-6720 Szeged, Dóm tér 9 (Hungary)

    2015-05-01

    Highlights: • The shock-wave-induced film delamination (SWIFD) is a laser patterning process. • The SWIFD process of CIGS solar cells was studied by shadowgraph measurements. • The study presented that SWIFD allows the structuring of CIGS solar cells. • The dynamics of the delamination process was analyzed. - Abstract: The laser-assisted microstructuring of thin films especially for electronic applications without damaging the layers or the substrates is a challenge for the laser micromachining techniques. The laser-induced thin-film patterning by ablation of the polymer substrate at the rear side that is called ‘SWIFD’ – shock-wave-induced film delamination patterning has been demonstrated. This study focuses on the temporal sequence of processes that characterize the mechanism of this SWIFD process on a copper indium gallium selenide (CIGS) solar cell stacks on polyimide. For this purpose high-speed shadowgraph experiments were performed in a pump probe experimental set-up using a KrF excimer laser for ablating the rear side of the polyimide substrate and measuring the shock wave generation at laser ablation of the polymer substrate as well as the thin-film delamination. The morphology and size of the thin-film structures were studied by scanning electron microscopy (SEM). Furthermore, the composition after the laser treatment was analyzed by energy dispersive X-ray (EDX) spectroscopy. The shadowgraph experiments allow the time-dependent identification and evaluation of the shock wave formation, substrate bending, and delamination of the thin film in dependence on the laser parameters. These results will contribute to improve the physical understanding of the laser-induced delamination effect for thin-film patterning.

  20. Hatching rate and growth rate of Nothobranchius guentheri fertilized eggs after space flight

    International Nuclear Information System (INIS)

    Guo Mingzhong; Zheng Leyun; Lin Guangji; Zhong Jianxing; Yang Huosheng; Zheng Yangfu

    2012-01-01

    Hatching, abnormal, growth and survival rate of the fertilized eggs of Nothobranchius guentheri were carried by Shenzhou 7 spacecraft were studied. The results indicated that the hatching and abnormal rate were no significant difference between the spaceflight group (99.3% and 16.8%) and ground group (97.2% and 10.4%); but the growth rate of male fish from spaceflight group was significant higher (0.094 g/d) than that of ground group (0.059 g/d), leading to the significant bigger of the male fish from spaceflight group. The survival rate of spaceflight group (66.7%) was higher than the ground group (47.9%). It was concluded that there was a higher growth and survival rate of Nothobranchius guentheri fertilized eggs after space flight. (authors)

  1. The effect of size and competition on tree growth rate in old-growth coniferous forests

    Science.gov (United States)

    Das, Adrian

    2012-01-01

    Tree growth and competition play central roles in forest dynamics. Yet models of competition often neglect important variation in species-specific responses. Furthermore, functions used to model changes in growth rate with size do not always allow for potential complexity. Using a large data set from old-growth forests in California, models were parameterized relating growth rate to tree size and competition for four common species. Several functions relating growth rate to size were tested. Competition models included parameters for tree size, competitor size, and competitor distance. Competitive strength was allowed to vary by species. The best ranked models (using Akaike’s information criterion) explained between 18% and 40% of the variance in growth rate, with each species showing a strong response to competition. Models indicated that relationships between competition and growth varied substantially among species. The results also suggested that the relationship between growth rate and tree size can be complex and that how we model it can affect not only our ability to detect that complexity but also whether we obtain misleading results. In this case, for three of four species, the best model captured an apparent and unexpected decline in potential growth rate for the smallest trees in the data set.

  2. Delamination measurement of a laminates composite panel due to hole punching based on the focus variation technique

    Science.gov (United States)

    Abdullah, A. B.; Zain, M. S. M.; Abdullah, M. S.; Samad, Z.

    2017-07-01

    Structural materials, such as composite panels, must be assembled, and such panels are typically constructed via the insertion of a fastener through a drilled hole. The main problem encountered in drilling is delamination, which affects assembly strength. The cost of drilling is also high because of the severe wear on drill bits. The main goal of this research is to develop a new punching method as an alternative to drilling during hole preparation. In this study, the main objective is to investigate the effect of different puncher profiles on the quality of holes punched into carbon fiber reinforcement polymer (CFRP) composite panels. Six types of puncher profiles were fabricated with minimum die clearance (1%), and two quality aspects, namely, incomplete shearing and delamination factor, were measured. The conical puncher incurred the least defects in terms of delamination and yielded an acceptable amount of incomplete shearing in comparison with the other punchers.

  3. Surface modified MXene Ti_3C_2 multilayers by aryl diazonium salts leading to large-scale delamination

    International Nuclear Information System (INIS)

    Wang, Hongbing; Zhang, Jianfeng; Wu, Yuping; Huang, Huajie; Li, Gaiye; Zhang, Xin; Wang, Zhuyin

    2016-01-01

    Highlights: • A novel and simple method to delaminate MXene Ti_3C_2 multilayers. • Surface modification using aryl diazonium salts induced swelling that conversely weakened the bonds between MXene layers. • The grafting of phenylsulfonic acid groups on MXene surfaces resulted in excellent water dispersibility. - Abstract: Herein we report a simple and facile method to delaminate MXene Ti_3C_2 multilayers by the assistance of surface modification using aryl diazonium salts. The basic strategy involved the preparation of layered MAX Ti_3AlC_2 and the exfoliation of Ti_3AlC_2 into Ti_3C_2 multilayers, followed by Na"+ intercalation and surface modification using sulfanilic acid diazonium salts. The resulting chemically grafted Ti_3C_2 flakes were characterized by Fourier transform infrared (FT-IR) spectroscopy and X-ray photoelectron spectroscopy (XPS) to confirm the presence of the surface organic species. Ultraviolet-visible spectroscopy revealed that surface-modified MXene Ti_3C_2 sheets disperse well in water and the solutions obey Lambert–Beer’s law. Scanning electron microscopy (SEM), transmission electron microscopy (TEM) and X-ray diffraction (XRD) were used to demonstrate the morphology and structure of delaminating MXene Ti_3C_2 flakes. The results indicated that chemical modification for MXene multilayers by aryl diazonium salts induced swelling that conversely weakened the bonds between MX layers, hence leading to large-scale delamination of multilayered MXene Ti_3C_2via mild sonication. Advantages of the present approach rely not only on the simplicity and efficiency of the delamination procedure but also on the grafting of aryl groups to MXene surfaces, highly suitable for further applications of the newly discovered two-dimensional materials.

  4. A negative modulatory role for rho and rho-associated kinase signaling in delamination of neural crest cells

    Directory of Open Access Journals (Sweden)

    Kalcheim Chaya

    2008-10-01

    Full Text Available Abstract Background Neural crest progenitors arise as epithelial cells and then undergo a process of epithelial to mesenchymal transition that precedes the generation of cellular motility and subsequent migration. We aim at understanding the underlying molecular network. Along this line, possible roles of Rho GTPases that act as molecular switches to control a variety of signal transduction pathways remain virtually unexplored, as are putative interactions between Rho proteins and additional known components of this cascade. Results We investigated the role of Rho/Rock signaling in neural crest delamination. Active RhoA and RhoB are expressed in the membrane of epithelial progenitors and are downregulated upon delamination. In vivo loss-of-function of RhoA or RhoB or of overall Rho signaling by C3 transferase enhanced and/or triggered premature crest delamination yet had no effect on cell specification. Consistently, treatment of explanted neural primordia with membrane-permeable C3 or with the Rock inhibitor Y27632 both accelerated and enhanced crest emigration without affecting cell proliferation. These treatments altered neural crest morphology by reducing stress fibers, focal adhesions and downregulating membrane-bound N-cadherin. Reciprocally, activation of endogenous Rho by lysophosphatidic acid inhibited emigration while enhancing the above. Since delamination is triggered by BMP and requires G1/S transition, we examined their relationship with Rho. Blocking Rho/Rock function rescued crest emigration upon treatment with noggin or with the G1/S inhibitor mimosine. In the latter condition, cells emigrated while arrested at G1. Conversely, BMP4 was unable to rescue cell emigration when endogenous Rho activity was enhanced by lysophosphatidic acid. Conclusion Rho-GTPases, through Rock, act downstream of BMP and of G1/S transition to negatively regulate crest delamination by modifying cytoskeleton assembly and intercellular adhesion.

  5. Volume growth rate of acoustic neurinomas

    International Nuclear Information System (INIS)

    Laasonen, E.M.; Troupp, H.

    1986-01-01

    Of 79 acoustic neurinomas seen between June 1980 and June 1984, at least two CT scans were available for each of 23 tumours (21 patients); the scans were performed at intervals of at least 6 months. The volume growth rate of the tumours was either moderate, with a volume doubling time ranging from 205 to 545 days, or slow, with a doubling time ranging from 1090 days to no observable growth. No single clinical, radiological or histological feature correlated with any type of growth rate. However, some conclusions were drawn. If a primary CT scan is negative, at least 1 year should elapse before it is worthwhile taking another scan, even though audiological findings suggest growth; after an apparently radical removal, at least 3 years should elapse before a check CT scan is worthwhile; and if a small acoustic neurinoma is diagnosed, but for some reason not operated upon, a second CT scan should be carried out 1 year later in order to reassess the case. (orig.)

  6. Selective role of bainitic lath boundary in influencing slip systems and consequent deformation mechanisms and delamination in high-strength low-alloy steel

    Science.gov (United States)

    Liu, S.; Li, X.; Guo, H.; Yang, S.; Wang, X.; Shang, C.; Misra, R. D. K.

    2018-04-01

    We elucidate here the deformation behaviour and delamination phenomenon in a high-strength low-alloy bainitic steel, in terms of microstructure, texture and stress evolution during deformation via in situ electron back-scattered diffraction and electron microscopy. Furthermore, the selective role of bainitic lath boundary on slip systems was studied in terms of dislocation pile-up and grain boundary energy models. During tensile deformation, the texture evolution was concentrated at {1 1 0} and the laths were turn parallel to loading direction. The determining role of lath on the deformation behaviour is governed by length/thickness (l/t) ratio. When l/t > 28, the strain accommodates along the bainite lath rather than along the normal direction. The delamination crack initiated normal to (0 1 1) plane, and become inclined to (0 1 1) plane with continued strain along (0 1 1) plane and lath plane. This indicated that the delamination is not brittle process but plastic process. The lack of dimples at the delaminated surface is because of lack of strain normal to the direction of lath. The delaminated (0 1 1) planes were associated with cleavage along the (1 0 0) plane.

  7. Money Supply, Interest Rate, and Economic Growth in Cameroon: A ...

    African Journals Online (AJOL)

    Money Supply, Interest Rate, and Economic Growth in Cameroon: A Time Series ... the impacts of money and interest rate on economic growth and development. ... Money Supply, Interest Rates, Economic growth, Co-integration and Inflation.

  8. Predictions of Poisson's ratio in cross-ply laminates containing matrix cracks and delaminations

    Science.gov (United States)

    Harris, Charles E.; Allen, David H.; Nottorf, Eric W.

    1989-01-01

    A damage-dependent constitutive model for laminated composites has been developed for the combined damage modes of matrix cracks and delaminations. The model is based on the concept of continuum damage mechanics and uses second-order tensor valued internal state variables to represent each mode of damage. The internal state variables are defined as the local volume average of the relative crack face displacements. Since the local volume for delaminations is specified at the laminate level, the constitutive model takes the form of laminate analysis equations modified by the internal state variables. Model implementation is demonstrated for the laminate engineering modulus E(x) and Poisson's ratio nu(xy) of quasi-isotropic and cross-ply laminates. The model predictions are in close agreement to experimental results obtained for graphite/epoxy laminates.

  9. Response of Escherichia coli growth rate to osmotic shock.

    Science.gov (United States)

    Rojas, Enrique; Theriot, Julie A; Huang, Kerwyn Casey

    2014-05-27

    It has long been proposed that turgor pressure plays an essential role during bacterial growth by driving mechanical expansion of the cell wall. This hypothesis is based on analogy to plant cells, for which this mechanism has been established, and on experiments in which the growth rate of bacterial cultures was observed to decrease as the osmolarity of the growth medium was increased. To distinguish the effect of turgor pressure from pressure-independent effects that osmolarity might have on cell growth, we monitored the elongation of single Escherichia coli cells while rapidly changing the osmolarity of their media. By plasmolyzing cells, we found that cell-wall elastic strain did not scale with growth rate, suggesting that pressure does not drive cell-wall expansion. Furthermore, in response to hyper- and hypoosmotic shock, E. coli cells resumed their preshock growth rate and relaxed to their steady-state rate after several minutes, demonstrating that osmolarity modulates growth rate slowly, independently of pressure. Oscillatory hyperosmotic shock revealed that although plasmolysis slowed cell elongation, the cells nevertheless "stored" growth such that once turgor was reestablished the cells elongated to the length that they would have attained had they never been plasmolyzed. Finally, MreB dynamics were unaffected by osmotic shock. These results reveal the simple nature of E. coli cell-wall expansion: that the rate of expansion is determined by the rate of peptidoglycan insertion and insertion is not directly dependent on turgor pressure, but that pressure does play a basic role whereby it enables full extension of recently inserted peptidoglycan.

  10. Can we estimate bacterial growth rates from ribosomal RNA content?

    Energy Technology Data Exchange (ETDEWEB)

    Kemp, P.F.

    1995-12-31

    Several studies have demonstrated a strong relationship between the quantity of RNA in bacterial cells and their growth rate under laboratory conditions. It may be possible to use this relationship to provide information on the activity of natural bacterial communities, and in particular on growth rate. However, if this approach is to provide reliably interpretable information, the relationship between RNA content and growth rate must be well-understood. In particular, a requisite of such applications is that the relationship must be universal among bacteria, or alternately that the relationship can be determined and measured for specific bacterial taxa. The RNA-growth rate relationship has not been used to evaluate bacterial growth in field studies, although RNA content has been measured in single cells and in bulk extracts of field samples taken from coastal environments. These measurements have been treated as probable indicators of bacterial activity, but have not yet been interpreted as estimators of growth rate. The primary obstacle to such interpretations is a lack of information on biological and environmental factors that affect the RNA-growth rate relationship. In this paper, the available data on the RNA-growth rate relationship in bacteria will be reviewed, including hypotheses regarding the regulation of RNA synthesis and degradation as a function of growth rate and environmental factors; i.e. the basic mechanisms for maintaining RNA content in proportion to growth rate. An assessment of the published laboratory and field data, the current status of this research area, and some of the remaining questions will be presented.

  11. Resistive Wall Growth Rate Measurements in the Fermilab Recycler

    Energy Technology Data Exchange (ETDEWEB)

    Ainsworth, R. [Fermilab; Adamson, P. [Fermilab; Burov, A. [Fermilab; Kourbanis, I. [Fermilab

    2016-10-05

    Impedance could represent a limitation of running high intensity beams in the Fermilab recycler. With high intensity upgrades foreseen, it is important to quantify the impedance. To do this,studies have been performed measuring the growth rate of presumably the resistive wall instability. The growth rates at varying intensities and chromaticities are shown. The measured growth rates are compared to ones calculated with the resistive wall impedance.

  12. Effective Exchange Rate Classifications and Growth

    OpenAIRE

    Justin M. Dubas; Byung-Joo Lee; Nelson C. Mark

    2005-01-01

    We propose an econometric procedure for obtaining de facto exchange rate regime classifications which we apply to study the relationship between exchange rate regimes and economic growth. Our classification method models the de jure regimes as outcomes of a multinomial logit choice problem conditional on the volatility of a country's effective exchange rate, a bilateral exchange rate and international reserves. An `effective' de facto exchange rate regime classification is then obtained by as...

  13. A propagator matrix method for the Rayleigh-Taylor instability of multiple layers: a case study on crustal delamination in the early Earth

    Science.gov (United States)

    Mondal, Puskar; Korenaga, Jun

    2018-03-01

    The dispersion relation of the Rayleigh-Taylor instability, a gravitational instability associated with unstable density stratification, is of profound importance in various geophysical contexts. When more than two layers are involved, a semi-analytical technique based on the biharmonic formulation of Stokes flow has been extensively used to obtain such dispersion relation. However, this technique may become cumbersome when applied to lithospheric dynamics, where a number of layers are necessary to represent the continuous variation of viscosity over many orders of magnitude. Here, we present an alternative and more efficient method based on the propagator matrix formulation of Stokes flow. With this approach, the original instability problem is reduced to a compact eigenvalue equation whose size is solely determined by the number of primary density contrasts. We apply this new technique to the stability of the early crust, and combined with the Monte Carlo sensitivity analysis, we derive an empirical formula to compute the growth rate of the Rayleigh-Taylor instability for this particular geophysical setting. Our analysis indicates that the likelihood of crustal delamination hinges critically on the effective viscosity of eclogite.

  14. Failure Predictions of Out-of-Autoclave Sandwich Joints with Delaminations Under Flexure Loads

    Science.gov (United States)

    Nordendale, Nikolas A.; Goyal, Vinay K.; Lundgren, Eric C.; Patel, Dhruv N.; Farrokh, Babak; Jones, Justin; Fischetti, Grace; Segal, Kenneth N.

    2015-01-01

    An analysis and a test program was conducted to investigate the damage tolerance of composite sandwich joints. The joints contained a single circular delamination between the face-sheet and the doubler. The coupons were fabricated through out-of-autoclave (OOA) processes, a technology NASA is investigating for joining large composite sections. The four-point bend flexure test was used to induce compression loading into the side of the joint where the delamination was placed. The compression side was chosen since it tends to be one of the most critical loads in launch vehicles. Autoclave cure was used to manufacture the composite sandwich sections, while the doubler was co-bonded onto the sandwich face-sheet using an OOA process after sandwich panels were cured. A building block approach was adopted to characterize the mechanical properties of the joint material, including the fracture toughness between the doubler and face-sheet. Twelve four-point-bend samples were tested, six in the sandwich core ribbon orientation and six in sandwich core cross-ribbon direction. Analysis predicted failure initiation and propagation at the pre-delaminated location, consistent with experimental observations. A building block approach using fracture analyses methods predicted failure loads in close agreement with tests. This investigation demonstrated a small strength reduction due to a flaw of significant size compared to the width of the sample. Therefore, concerns of bonding an OOA material to an in-autoclave material was mitigated for the geometries, materials, and load configurations considered.

  15. Buckle initiation and delamination of patterned ITO layers on a polymer substrate

    NARCIS (Netherlands)

    Abdallah, Amir; Bouten, P.C.P.; Toonder, den J.M.J.; With, de G.

    2011-01-01

    Buckle initiation and delamination of patterned ITO layers on a polymer substrate were studied. Various buckle modes have been observed depending on the type of etch defects and the crack patterns. The buckle density was found to be dependent on the number of etch defects, imperfections, applied

  16. Surface modified MXene Ti3C2 multilayers by aryl diazonium salts leading to large-scale delamination

    Science.gov (United States)

    Wang, Hongbing; Zhang, Jianfeng; Wu, Yuping; Huang, Huajie; Li, Gaiye; Zhang, Xin; Wang, Zhuyin

    2016-10-01

    Herein we report a simple and facile method to delaminate MXene Ti3C2 multilayers by the assistance of surface modification using aryl diazonium salts. The basic strategy involved the preparation of layered MAX Ti3AlC2 and the exfoliation of Ti3AlC2 into Ti3C2 multilayers, followed by Na+ intercalation and surface modification using sulfanilic acid diazonium salts. The resulting chemically grafted Ti3C2 flakes were characterized by Fourier transform infrared (FT-IR) spectroscopy and X-ray photoelectron spectroscopy (XPS) to confirm the presence of the surface organic species. Ultraviolet-visible spectroscopy revealed that surface-modified MXene Ti3C2 sheets disperse well in water and the solutions obey Lambert-Beer's law. Scanning electron microscopy (SEM), transmission electron microscopy (TEM) and X-ray diffraction (XRD) were used to demonstrate the morphology and structure of delaminating MXene Ti3C2 flakes. The results indicated that chemical modification for MXene multilayers by aryl diazonium salts induced swelling that conversely weakened the bonds between MX layers, hence leading to large-scale delamination of multilayered MXene Ti3C2via mild sonication. Advantages of the present approach rely not only on the simplicity and efficiency of the delamination procedure but also on the grafting of aryl groups to MXene surfaces, highly suitable for further applications of the newly discovered two-dimensional materials.

  17. Re-assessing copepod growth using the Moult Rate method

    DEFF Research Database (Denmark)

    Hirst, Andrew G.; Keister, J. E.; Richardson, A. J.

    2014-01-01

    Estimating growth and production rates of mesozooplankton, and copepods in particular, is important in describing flows of material and energy though pelagic systems. Over the past 30 years, the Moult Rate (MR) method has been used to estimate juvenile copepod growth rates in ∼40 papers. Yet the MR......-moulting stage, e.g. copepodite stage 5 to adult. We performed experiments with Calanus pacificus to estimate growth of stage C5 using an alternative method. We found that the error size and sign varied between mass type (i.e. DW, C and N). Recommendations for practical future assessments of growth in copepods...

  18. Microfractographic analysis of delamination growth in fatigue loaded - carbon fibre/thermosetting matrix composites; Mikrofraktographische Analyse des Delaminationswachstums in zyklisch belasteten Kohlenstoffaser/Duroplastharz-Verbundwerkstoffen

    Energy Technology Data Exchange (ETDEWEB)

    Heutling, F.; Franz, H.E. [Daimler-Benz AG, Muenchen (Germany); Friedrich, K. [Kaiserslautern Univ. (Germany). Inst. for Composite Materials Ltd.

    1998-05-01

    Carbon-fibre-reinforced plastics (CFRP) are known to be considerably less sensitive to fatigue loading than aluminium (Al) alloys, for instance. However, even in the presence of small delaminations, the damage tolerance of structural components may be considerably reduced. The scope of the present contribution is to investigate fatigue phenomena in CFRP materials (with thermosetting matrix) by means of microfractography. The microfractographic features of the fracture surfaces mirror the processes of deformation and fracture at the delamination front. The fatigue fracture behaviour of a CFRP laminate subjected to cyclic mixed-mode loading is determined by matrix-controlled failure mechanisms. Under pure mode-II loading conditions, rollers in addition to fatigue striations appear in the fibre imprints whose formation mechanism was explained by means of high-resolution field-emission scanning electron microscopy (FE-SEM). The ratio between the local tensile and shear stress components influences the propagation direction of secondary cracks originating at the fibres. The local fracture propagations in these secondary cracks can be recognised through the fatigue striations appearing on the surface of the matrix. A comparison with static mixed-mode loading reveals that in both cases the crack propagation follows the path of the local maximum main stress. Applying mathematical relationships derived from the theory of elasticity permitted developing a mixed-mode loading model which makes it possible to predict the crack processes and hence to explain the formation of typical fracture-morphological features. (orig.) 26 refs.

  19. Divergent biparietal diameter growth rates in twin pregnancies.

    Science.gov (United States)

    Houlton, M C

    1977-05-01

    Twenty-eight twin pregnancies were monitored by serial ultrasonic cephalometry from 30 or 31 weeks' gestation. The rates of growth of the individual twins as determined by biparietal diameters were similar in 11 cases (39%) and divergent in 17 (61%). When the rates of growth were divergent, the lesser rate was always below the mean for singleton pregnancies, and the incidence of small-for-gestational-age babies was 18 of 34 (53%). It was apparent that the greater the difference in biparietal diameters within the 2 weeks preceding delivery, the higher the risk of a small-for-gestation-age baby being delivered. No comment could be made on the growth rate prior to 28 weeks except that at diagnosis there was little or no difference in biparietal diameters.

  20. Preliminary observation of genital secretions, growth rate and ...

    African Journals Online (AJOL)

    Cane rats are large terrestial rodents which have the potential to increase animal protein intake. There is paucity of information on the genital secretions and growth rate of caged cane rats. This study observed the genital secretions, growth rate, feeds, feeding and the behaviour of caged cane rats. When animals adjusted to ...

  1. Seasonal variations in ectotherm growth rates: Quantifying growth as an intermittent non steady state compensatory process

    Science.gov (United States)

    Guarini, J.-M.; Chauvaud, Laurent; Cloern, J.E.; Clavier, J.; Coston-Guarini, J.; Patry, Y.

    2011-01-01

    Generally, growth rates of living organisms are considered to be at steady state, varying only under environmental forcing factors. For example, these rates may be described as a function of light for plants or organic food resources for animals and these could be regulated (or not) by temperature or other conditions. But, what are the consequences for an individual's growth (and also for the population growth) if growth rate variations are themselves dynamic and not steady state? For organisms presenting phases of dormancy or long periods of stress, this is a crucial question. A dynamic perspective for quantifying short-term growth was explored using the daily growth record of the scallop Pecten maximus (L.). This species is a good biological model for ectotherm growth because the shell records growth striae daily. Independently, a generic mathematical function representing the dynamics of mean daily growth rate (MDGR) was implemented to simulate a diverse set of growth patterns. Once the function was calibrated with the striae patterns, the growth rate dynamics appeared as a forced damped oscillation during the growth period having a basic periodicity during two transitory phases (mean duration 43. days) and appearing at both growth start and growth end. This phase is most likely due to the internal dynamics of energy transfer within the organism rather than to external forcing factors. After growth restart, the transitory regime represents successive phases of over-growth and regulation. This pattern corresponds to a typical representation of compensatory growth, which from an evolutionary perspective can be interpreted as an adaptive strategy to coping with a fluctuating environment. ?? 2011 Elsevier B.V.

  2. Detecting closing delaminations in laminated composite plates using nonlinear structural intensity and time reversal mirrors

    International Nuclear Information System (INIS)

    Lamberti, Alfredo; Semperlotti, Fabio

    2013-01-01

    Closing delaminations in composite laminated structures exhibit a nonlinear dynamic response when excited by high frequency elastic waves. The contact acoustic nonlinear effects taking place at the damage interface act as a mechanism of energy redistribution from the driving frequency to the nonlinear harmonic frequencies. In this paper, we extend the concept of nonlinear structural intensity (NSI) to the analysis of closing delaminations in composite laminated plates. NSI is calculated using a method based on a combination of finite element and finite difference techniques, which is suitable for processing both numerical and experimental data. NSI is proven to be an effective metric to identify the presence and location of closing delaminations. The highly directional nature of orthotropic composites results in vibrational energy propagating in a different direction from that of the initial elastic wave. This aspect reduces the ability to effectively interrogate the damage and, therefore, the sensitivity to the damage. The time reversal mirror technique is explored as a possible approach to overcome the effect of the material directionality and increase the ability to interrogate the damage. Numerical simulations show that this technique is able to overcome the material directionality and to drastically enhance the ability to interrogate the damage. (paper)

  3. Analysis of Mode I and Mode II Crack Growth Arrest Mechanism with Z-Fibre Pins in Composite Laminated Joint

    Science.gov (United States)

    Jeevan Kumar, N.; Ramesh Babu, P.

    2018-04-01

    This paper presents the numerical study of the mode I and mode II interlaminar crack growth arrest in hybrid laminated curved composite stiffened joint with Z-fibre reinforcement. A FE model of hybrid laminated skin-stiffener joint reinforced with Z-pins is developed to investigate the effect of Z- fibre pins on mode I and mode II crack growth where the delamination is embedded inbetween the skin and stiffener interface. A finite element model was developed using S4R element of a 4-node doubly curved thick shell elements to model the composite laminates and non linear interface elements to simulate the reinforcements. The numerical analyses revealed that Z-fibre pinning were effective in suppressing the delamination growth when propagated due to applied loads. Therefore, the Z-fibre technique effectively improves the crack growth resistance and hence arrests or delays crack growth extension.

  4. Resolving nanoparticle growth mechanisms from size- and time-dependent growth rate analysis

    Science.gov (United States)

    Pichelstorfer, Lukas; Stolzenburg, Dominik; Ortega, John; Karl, Thomas; Kokkola, Harri; Laakso, Anton; Lehtinen, Kari E. J.; Smith, James N.; McMurry, Peter H.; Winkler, Paul M.

    2018-01-01

    Atmospheric new particle formation occurs frequently in the global atmosphere and may play a crucial role in climate by affecting cloud properties. The relevance of newly formed nanoparticles depends largely on the dynamics governing their initial formation and growth to sizes where they become important for cloud microphysics. One key to the proper understanding of nanoparticle effects on climate is therefore hidden in the growth mechanisms. In this study we have developed and successfully tested two independent methods based on the aerosol general dynamics equation, allowing detailed retrieval of time- and size-dependent nanoparticle growth rates. Both methods were used to analyze particle formation from two different biogenic precursor vapors in controlled chamber experiments. Our results suggest that growth rates below 10 nm show much more variation than is currently thought and pin down the decisive size range of growth at around 5 nm where in-depth studies of physical and chemical particle properties are needed.

  5. Estimation of the growth curve and heritability of the growth rate for giant panda (Ailuropoda melanoleuca) cubs.

    Science.gov (United States)

    Che, T D; Wang, C D; Jin, L; Wei, M; Wu, K; Zhang, Y H; Zhang, H M; Li, D S

    2015-03-27

    Giant panda cubs have a low survival rate during the newborn and early growth stages. However, the growth and developmental parameters of giant panda cubs during the early lactation stage (from birth to 6 months) are not well known. We examined the growth and development of giant panda cubs by the Chapman growth curve model and estimated the heritability of the maximum growth rate at the early lactation stage. We found that 83 giant panda cubs reached their maximum growth rate at approximately 75-120 days after birth. The body weight of cubs at 75 days was 4285.99 g. Furthermore, we estimated that the heritability of the maximum growth rate was moderate (h(2) = 0.38). Our study describes the growth and development of giant panda cubs at the early lactation stage and provides valuable growth benchmarks. We anticipate that our results will be a starting point for more detailed research on increasing the survival rate of giant panda cubs. Feeding programs for giant panda cubs need further improvement.

  6. Exchange Rate Fluctuation and the Nigeria Economic Growth

    Directory of Open Access Journals (Sweden)

    Lawal Adedoyin Isola

    2016-11-01

    Full Text Available The aim of this study is to investigate the impact of exchange rate fluctuation on economic growth in Nigeria within the context of four profound theories: purchasing power parity; monetary model of exchange rates; the portfolio balance approach; and the optimal currency area theory. Data was collected from the CBN statistical bulletin in Nigeria from 2003– 2013and the Autoregressive Distributed Lag (ARDL model was employed to estimate the model. In the model, real GDP (RGDP was used as the proxy for economic growth while Inflation rate (IF, Exchange rate (EXC, Interest rate (INT and Money Supply(M2 as proxies for other macroeconomic variables. The empirical results show that exchange rate fluctuation has no effect on economic growth in the long run though a short run relationship exist between the two. Based on these findings, this paper recommends that the Central bank for policy purposes should ensure that stern foreign exchange control policies are put in place in order to help in appropriate determination of the value of the exchange rate. This will in the long run help to strengthen the value of the Naira.

  7. Surface modified MXene Ti{sub 3}C{sub 2} multilayers by aryl diazonium salts leading to large-scale delamination

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Hongbing [College of Mechanics and Materials, Hohai University, Nanjing, Jiangsu Province 210098 (China); Department of Mathematics and Physics, Nanjing Institute of Technology, Nanjing, Jiangsu Province 211167 (China); Zhang, Jianfeng, E-mail: jfzhang_sic@163.com [College of Mechanics and Materials, Hohai University, Nanjing, Jiangsu Province 210098 (China); Wu, Yuping; Huang, Huajie; Li, Gaiye; Zhang, Xin; Wang, Zhuyin [College of Mechanics and Materials, Hohai University, Nanjing, Jiangsu Province 210098 (China)

    2016-10-30

    Highlights: • A novel and simple method to delaminate MXene Ti{sub 3}C{sub 2} multilayers. • Surface modification using aryl diazonium salts induced swelling that conversely weakened the bonds between MXene layers. • The grafting of phenylsulfonic acid groups on MXene surfaces resulted in excellent water dispersibility. - Abstract: Herein we report a simple and facile method to delaminate MXene Ti{sub 3}C{sub 2} multilayers by the assistance of surface modification using aryl diazonium salts. The basic strategy involved the preparation of layered MAX Ti{sub 3}AlC{sub 2} and the exfoliation of Ti{sub 3}AlC{sub 2} into Ti{sub 3}C{sub 2} multilayers, followed by Na{sup +} intercalation and surface modification using sulfanilic acid diazonium salts. The resulting chemically grafted Ti{sub 3}C{sub 2} flakes were characterized by Fourier transform infrared (FT-IR) spectroscopy and X-ray photoelectron spectroscopy (XPS) to confirm the presence of the surface organic species. Ultraviolet-visible spectroscopy revealed that surface-modified MXene Ti{sub 3}C{sub 2} sheets disperse well in water and the solutions obey Lambert–Beer’s law. Scanning electron microscopy (SEM), transmission electron microscopy (TEM) and X-ray diffraction (XRD) were used to demonstrate the morphology and structure of delaminating MXene Ti{sub 3}C{sub 2} flakes. The results indicated that chemical modification for MXene multilayers by aryl diazonium salts induced swelling that conversely weakened the bonds between MX layers, hence leading to large-scale delamination of multilayered MXene Ti{sub 3}C{sub 2}via mild sonication. Advantages of the present approach rely not only on the simplicity and efficiency of the delamination procedure but also on the grafting of aryl groups to MXene surfaces, highly suitable for further applications of the newly discovered two-dimensional materials.

  8. Criteria for initiation of delamination in quasi-static punch-shear tests of a carbon-fiber composite material.

    Energy Technology Data Exchange (ETDEWEB)

    Chin, Eric Brian [Sandia National Lab. (SNL-CA), Livermore, CA (United States); English, Shawn Allen [Sandia National Lab. (SNL-CA), Livermore, CA (United States); Briggs, Timothy [Sandia National Lab. (SNL-CA), Livermore, CA (United States)

    2015-09-01

    V arious phenomenological delamination initiation criteria are analyzed in quasi - static punch - shear tests conducted on six different geometries. These six geometries are modeled and analyzed using elastic, large - deformation finite element analysis. Analysis output is post - processed to assess different delamination initiation criteria, and their applicability to each of the geometries. These criteria are compared to test results to assess whether or not they are appropriate based on what occurred in testing. Further, examinations of CT scans and ultrasonic images o f test specimens are conducted in the appendix to determine the sequence of failure in each test geometry.

  9. EVALUATION OF STRENGTH TO SHEAR AND DELAMINATION IN GLUED LAMINATED WOOD

    Directory of Open Access Journals (Sweden)

    Carlito Calil Neto

    2014-12-01

    Full Text Available The Glued Laminated Wood has a large range of applications. In Brazil, its employment as cross-piece poles for overhead electrical power has attracted the attention of companies in the industry, motivated by the potential use of this material. Among the factors that influence the mechanical performance of Glulam solutions stand out efficiency and affinity of the adhesives to the species of wood used, the type of treatment and moisture content of wood veneer, motivating the development of new research on this topic. This research aimed to investigate, by Design of Experiments (DOE, the influence of wood (pinus, teca, eucalipto, adhesive (Purbond; Cascophen and treatment (CCA, CCB, CCBS in the variable responses shear strength and delamination, consisting in the same combination factors evaluated in ANEEL/EESC-PD220-07 project: Head Crosshead Glulam Series. The results of the statistical analysis showed that the species factor expressed significant effect for both response variables evaluated, did not occur with adhesive and treatment factors. Moisture content was significant in the wood evaluated when analyzed the shear strength, and the teca wood showed the highest shear strength and also relating to the delamination.

  10. Effect of selection for relative growth rate and bodyweight of mice on rate, composition and efficiency of growth

    NARCIS (Netherlands)

    Bakker, H.

    1974-01-01

    To evaluate the effect of selection for parameters of a growth curve, four selection lines and a control line were started from one base population. In the selection lines is selected for a large and a small relative growth rate between 21 and 29 days (RGH and RGL) and for a large and

  11. Growth-rate-dependent dynamics of a bacterial genetic oscillator

    Science.gov (United States)

    Osella, Matteo; Lagomarsino, Marco Cosentino

    2013-01-01

    Gene networks exhibiting oscillatory dynamics are widespread in biology. The minimal regulatory designs giving rise to oscillations have been implemented synthetically and studied by mathematical modeling. However, most of the available analyses generally neglect the coupling of regulatory circuits with the cellular “chassis” in which the circuits are embedded. For example, the intracellular macromolecular composition of fast-growing bacteria changes with growth rate. As a consequence, important parameters of gene expression, such as ribosome concentration or cell volume, are growth-rate dependent, ultimately coupling the dynamics of genetic circuits with cell physiology. This work addresses the effects of growth rate on the dynamics of a paradigmatic example of genetic oscillator, the repressilator. Making use of empirical growth-rate dependencies of parameters in bacteria, we show that the repressilator dynamics can switch between oscillations and convergence to a fixed point depending on the cellular state of growth, and thus on the nutrients it is fed. The physical support of the circuit (type of plasmid or gene positions on the chromosome) also plays an important role in determining the oscillation stability and the growth-rate dependence of period and amplitude. This analysis has potential application in the field of synthetic biology, and suggests that the coupling between endogenous genetic oscillators and cell physiology can have substantial consequences for their functionality.

  12. Variation in coral growth rates with depth at Discovery Bay, Jamaica

    Energy Technology Data Exchange (ETDEWEB)

    Huston, M

    1985-01-01

    Growth rates, determined by X-radiographic measurement of skeletal extension, decreased with depth for four of six species of coral examined at Discovery Bay, Jamaica. Growth of Porites astreoides, Montastrea annularis, Colpophyllia natans, and Siderastrea siderea decreased significantly with depth over a 1- to 30-m depth range. In Montastrea cavernosa, the highest growth rate occurred in the middle of the sampled depth range. Agaricia agaricites had no measurable change in growth rate with depth. A compilation of available growth data for Atlantic and Pacific corals shows a strong pattern of highest growth rates a short distance below the surface and a decrease with depth.

  13. Investigation of growth rate dispersion in lactose crystallisation by AFM

    Science.gov (United States)

    Dincer, T. D.; Ogden, M. I.; Parkinson, G. M.

    2014-09-01

    α-Lactose monohydrate crystals have been reported to exhibit growth rate dispersion (GRD). Variation in surface dislocations has been suggested as the cause of GRD, but this has not been further investigated to date. In this study, growth rate dispersion and the change in morphology were investigated in situ and via bottle roller experiments. The surfaces of the (0 1 0) faces of crystals were examined with Atomic Force Microscopy. Smaller, slow growing crystals tend to have smaller (0 1 0) faces with narrow bases and displayed a single double spiral in the centre of the crystal with 2 nm high steps. Additional double spirals in other crystals resulted in faster growth rates. Large, fast growing crystals were observed to have larger (0 1 0) faces with fast growth in both the a and b directions (giving a broader crystal base) with macro steps parallel to the (c direction). The number and location of spirals or existence of macro steps appears to influence the crystal morphology, growth rates and growth rate dispersion in lactose crystals.

  14. The effect of cerium-based conversion treatment on the cathodic delamination and corrosion protection performance of carbon steel-fusion-bonded epoxy coating systems

    Energy Technology Data Exchange (ETDEWEB)

    Ramezanzadeh, B., E-mail: ramezanzadeh@aut.ac.ir [Department of Surface Coatings and Corrosion, Institute for Color Science and Technology (ICST), 16765-654, Tehran (Iran, Islamic Republic of); Rostami, M. [Department of Nanomaterials and Nanocoatings, Institute for Color Science and Technology (ICST), 16765-654, Tehran (Iran, Islamic Republic of)

    2017-01-15

    Highlights: • Steel surface was treated by Ce and acid phosphoric solutions. • Ce treatment considerably enhanced the surface energy and produce nanoscale roughness. • Ce treated samples showed enhanced adhesion to FBE coating. • Ce treatment of steel significantly reduced the FBE cathodic delamination rate. • Ce treated sample showed enhanced corrosion resistance. - Abstract: The effect of surface pre-treatment of pipe surface by green cerium compound and phosphoric acid solution on the fusion-bonded epoxy (FBE) coating performance was studied. The composition and surface morphology of the steel samples treated by acid and Ce solutions were characterized by X-ray photoelectron spectroscopy (XPS) and scanning electron microscopy (SEM), equipped with energy dispersive spectroscopy (EDS). Also, the surface free energy was evaluated on these samples through contact angle measurements. In addition, the effect of Ce and acid washing procedures on the adhesion properties and corrosion protection performance of the FBE was examined by pull-off, salt spray and electrochemical impedance spectroscopy (EIS) tests. Results showed that compared to acid washing, the chemical treatment by Ce solution noticeably increased the surface free energy of steel, improved the adhesion properties of FBE, decreased the cathodic delamination rate of FBE, and enhanced the coating corrosion resistance compared to the acid washed samples.

  15. GROWTH-RATES OF SHRUBS ON DIFFERENT SOILS IN TANZANIA

    NARCIS (Netherlands)

    PRINS, HHT; VANDERJEUGD, HP

    1992-01-01

    Because little is known of growth rates of shrubs in East Africa, the growth rates of Acalypha fructicosa, Gardenia jovis-tonantis, Justicia cordata, Maerua triphylla, and Ocimum suave were measured in Lake Manyara National Park, northern Tanzania. Branch diameter increments and branch length

  16. Growth rates of shrubs on different soils in Tanzania.

    NARCIS (Netherlands)

    Prins, H.H.T.; Jeugd, van der H.P.

    1992-01-01

    Because little is known of growth rates of shrubs in East Africa, the growth rates of Acalypha fructicosa, Gardenia jovis-tonantis, Justicia cordata, Maerua triphylla, and Ocimum suave were measured in Lake Manyara National Park, northern Tanzania. Branch diameter increments and branch length

  17. A thick level set interface model for simulating fatigue-drive delamination in composites

    NARCIS (Netherlands)

    Latifi, M.; Van der Meer, F.P.; Sluys, L.J.

    2015-01-01

    This paper presents a new damage model for simulating fatigue-driven delamination in composite laminates. This model is developed based on the Thick Level Set approach (TLS) and provides a favorable link between damage mechanics and fracture mechanics through the non-local evaluation of the energy

  18. Ductile film delamination from compliant substrates using hard overlayers.

    Science.gov (United States)

    Cordill, M J; Marx, V M; Kirchlechner, C

    2014-11-28

    Flexible electronic devices call for copper and gold metal films to adhere well to polymer substrates. Measuring the interfacial adhesion of these material systems is often challenging, requiring the formulation of different techniques and models. Presented here is a strategy to induce well defined areas of delamination to measure the adhesion of copper films on polyimide substrates. The technique utilizes a stressed overlayer and tensile straining to cause buckle formation. The described method allows one to examine the effects of thin adhesion layers used to improve the adhesion of flexible systems.

  19. Postnatal Growth Rates of Hummingbirds : Review and New Records

    NARCIS (Netherlands)

    Freymann, Bernd P.; Schuchmann, Karl-Ludwig

    2008-01-01

    We review the published information on postnatal growth rates of hummingbirds (13 species), and report previously unpublished records for nine additional trochilid species. The allometric relationship based on the log(10)-transformed data of K (logistic growth rate constant) and body mass has a

  20. The Variance Composition of Firm Growth Rates

    Directory of Open Access Journals (Sweden)

    Luiz Artur Ledur Brito

    2009-04-01

    Full Text Available Firms exhibit a wide variability in growth rates. This can be seen as another manifestation of the fact that firms are different from one another in several respects. This study investigated this variability using the variance components technique previously used to decompose the variance of financial performance. The main source of variation in growth rates, responsible for more than 40% of total variance, corresponds to individual, idiosyncratic firm aspects and not to industry, country, or macroeconomic conditions prevailing in specific years. Firm growth, similar to financial performance, is mostly unique to specific firms and not an industry or country related phenomenon. This finding also justifies using growth as an alternative outcome of superior firm resources and as a complementary dimension of competitive advantage. This also links this research with the resource-based view of strategy. Country was the second source of variation with around 10% of total variance. The analysis was done using the Compustat Global database with 80,320 observations, comprising 13,221 companies in 47 countries, covering the years of 1994 to 2002. It also compared the variance structure of growth to the variance structure of financial performance in the same sample.

  1. Vertical instability in TCV: comparison of experimental and theoretical growth rates

    International Nuclear Information System (INIS)

    Hofmann, F.; Dutch, M.J.; Ward, D.J.; Anton, M.; Furno, I.; Lister, J.B.; Moret, J.M.

    1996-12-01

    Growth rates of the axisymmetric mode in vertically elongated plasmas in the TCV tokamak are measured and compared with numerically calculated growth rates for the reconstructed equilibria. This comparison is made over a range of discharge parameters including elongation, triangularity, and vertical position within the vacuum vessel. Growth rates increase with respect to increasing elongation, decreasing triangularity and increasing vertical distance from the top of the vacuum vessel, as expected. The agreement between the measured growth rates in the experiment and the numerically determined growth rates is excellent, in particular for the full linear MHD model which accounts for the non-rigid motion of strongly shaped plasma cross-sections. (author) 7 figs., 22 refs

  2. Nd isotopes and crustal growth rate

    International Nuclear Information System (INIS)

    Albarede, F.

    1988-01-01

    Sm/Nd isotopic constraints on crustal growth is discussed. In order to constrain Sm/Nd fractionation between continental crust and depleted mantle, an extensive data base of isotopic measurements (assumed to be adequately representative of continental crust) was compiled. The results imply that the evolution of depleted mantles was roughly linear, with no major discontinuities over the course of geologic time. This is different from other determinations of depleting mantle evolution, which show nonlinear behavior. The Sm/Nd evolution lines for continental crust and depleted mantle intersect between 3.8 to 4.0 Ga, which may indicate that the onset of continental growth was later than 4.5 Ga. A mathematical model is described, the results of which imply that time integrated crustal additions from the mantle are about 1.8 to 2.5 cu km/a, whereas crustal subtractions by sediment recycling are about 0.6 to 1.5 cu km/a. This results in a net time integrated crustal growth rate of about 1 cu km/a, which is similar to present day rates determined, for example, by Reymer and Schubert

  3. Comparing Basal Area Growth Rates in Repeated Inventories: Simpson's Paradox in Forestry

    Science.gov (United States)

    Charles E. Thomas; Bernard R. Parresol

    1989-01-01

    Recent analyses of radial growth rates in southern commercial forests have shown that current rates are lower than past rates when compared diameter class by diameter class. These results have been interpreted as an indication that the growth rate of the forest is declining. In this paper, growth rates of forest populations in Alabama are studied. Basal area growth (a...

  4. Protein thermodynamics can be predicted directly from biological growth rates.

    Directory of Open Access Journals (Sweden)

    Ross Corkrey

    Full Text Available Life on Earth is capable of growing from temperatures well below freezing to above the boiling point of water, with some organisms preferring cooler and others hotter conditions. The growth rate of each organism ultimately depends on its intracellular chemical reactions. Here we show that a thermodynamic model based on a single, rate-limiting, enzyme-catalysed reaction accurately describes population growth rates in 230 diverse strains of unicellular and multicellular organisms. Collectively these represent all three domains of life, ranging from psychrophilic to hyperthermophilic, and including the highest temperature so far observed for growth (122 °C. The results provide credible estimates of thermodynamic properties of proteins and obtain, purely from organism intrinsic growth rate data, relationships between parameters previously identified experimentally, thus bridging a gap between biochemistry and whole organism biology. We find that growth rates of both unicellular and multicellular life forms can be described by the same temperature dependence model. The model results provide strong support for a single highly-conserved reaction present in the last universal common ancestor (LUCA. This is remarkable in that it means that the growth rate dependence on temperature of unicellular and multicellular life forms that evolved over geological time spans can be explained by the same model.

  5. Influence of crystallographic texture in X70 pipeline steels on toughness anisotropy and delamination

    Science.gov (United States)

    Al-Jabr, Haytham M.

    The effects of microstructure and crystallographic texture in four commercially-produced API X70 pipeline steels and their relation to planar anisotropy of toughness and delamination were evaluated. The experimental steels were processed through either a hot strip mill, a Steckel mill, or a compact strip mill. Different processing routes were selected to obtain plates with potential variations in the microstructure and anisotropic characteristics. Tensile and Charpy impact testing were used to evaluate the mechanical properties in three orientations: longitudinal (L), transverse (T) and diagonal (D) with respect to the rolling direction to evaluate mechanical property anisotropy. The yield and tensile strengths were higher in the T orientation and toughness was lower in the D orientation for all plates. Delamination was observed in some of the ductile fracture surfaces of the impact samples. To further study the splitting behavior and effects on impact toughness, a modified impact test (MCVN) specimen with side grooves was designed to intensify induced stresses parallel to the notch root and thus facilitate evaluation of delamination. Scanning electron microscopy combined with electron backscattered diffraction (EBSD) were used to evaluate the grain size, microstructural constituents, and crystallographic texture to determine the factors leading to delamination and the anisotropy in toughness. The ferrite grain size is mainly responsible for the differences in DBTTs between the L and T orientations. The higher DBTT in the D orientation observed in pipeline steels is attributed to crystallographic texture. The higher DBTT in the D direction is due to the higher volume fraction of grains having their {100} planes parallel or close to the primary fracture plane for the D orientation. An equation based on a new "brittleness parameter," based on an assessment of grain orientations based on EBSD data, was developed to predict the changes in DBTTs with respect to sample

  6. Cohesive delamination and frictional contact on joining surface via XFEM

    Directory of Open Access Journals (Sweden)

    Francesco Parrinello

    2018-02-01

    Full Text Available In the present paper, the complex mechanical behaviour of the surfaces joining two differentbodies is analysed by a cohesive-frictional interface constitutive model. The kinematical behaviouris characterized by the presence of discontinuous displacement fields, that take place at the internalconnecting surfaces, both in the fully cohesive phase and in the delamination one. Generally, in order tocatch discontinuous displacement fields, internal connecting surfaces (adhesive layers are modelled bymeans of interface elements, which connect, node by node, the meshes of the joined bodies, requiringthe mesh to be conforming to the geometry of the single bodies and to the relevant connecting surface.In the present paper, the Extended Finite Element Method (XFEM is employed to model, both fromthe geometrical and from the kinematical point of view, the whole domain, including the connectedbodies and the joining surface. The joining surface is not discretized by specific finite elements, butit is defined as an internal discontinuity surface, whose spatial position inside the mesh is analyticallydefined. The proposed approach is developed for two-dimensional composite domains, formed by twoor more material portions joined together by means of a zero thickness adhesive layer. The numericalresults obtained with the proposed approach are compared with the results of the classical interfacefinite element approach. Some examples of delamination and frictional contact are proposed withlinear, circular and curvilinear adhesive layer.

  7. Automated detection of delamination and disbond from wavefield images obtained using a scanning laser vibrometer

    International Nuclear Information System (INIS)

    Sohn, H; Yang, J Y; Dutta, D; DeSimio, M; Olson, S; Swenson, E

    2011-01-01

    The paper presents signal and image processing algorithms to automatically detect delamination and disbond in composite plates from wavefield images obtained using a scanning laser Doppler vibrometer (LDV). Lamb waves are excited by a lead zirconate titanate transducer (PZT) mounted on the surface of a composite plate, and the out-of-plane velocity field is measured using an LDV. From the scanned time signals, wavefield images are constructed and processed to study the interaction of Lamb waves with hidden delaminations and disbonds. In particular, the frequency–wavenumber (f–k) domain filter and the Laplacian image filter are used to enhance the visibility of defects in the scanned images. Thereafter, a statistical cluster detection algorithm is used to identify the defect location and distinguish damaged specimens from undamaged ones

  8. Individual Growth Rates of Nikolsky’s Viper, Vipera berus nikolskii (Squamata, Viperidae

    Directory of Open Access Journals (Sweden)

    Bondarenko Z. S.

    2016-02-01

    Full Text Available Capture-mark-recapture data was used to infer growth rates of the Nikolsky’s viper, Vipera berus nikolskii (Vedmederja, Grubant et Rudaeva, 1986, in the Eastern Ukraine. We have found that growth rate is negatively correlated with age. The difference in growth rates before maturation is not significant between different sexes. Growth rates decrease rapidly after maturation in males and females, however adult males retain significantly higher average growth rates. There is large dispersion of growth rates in the group of adult females, which is caused, probably, by alteration of complete arrest of growth in the years with reproduction and more intensive growth in the years without it. Asymptotic snout-ventral length estimated after Von Bertalanffy model was 680 mm in females and 630 mm in males. Females mature after fifth and males mature after fourth hibernation. The larger females in vipers can not be the result of higher growth rates in females, but are the outcome of a combination of other factors including different maturation time and size (older and being larger, and, perhaps, longer life span due to lower mortality. Growth rates of the Nikolsky’s viper in the nature are higher than in other species in the group of small Eurasian vipers.

  9. Dinosaur Metabolism and the Allometry of Maximum Growth Rate

    OpenAIRE

    Myhrvold, Nathan P.

    2016-01-01

    The allometry of maximum somatic growth rate has been used in prior studies to classify the metabolic state of both extant vertebrates and dinosaurs. The most recent such studies are reviewed, and their data is reanalyzed. The results of allometric regressions on growth rate are shown to depend on the choice of independent variable; the typical choice used in prior studies introduces a geometric shear transformation that exaggerates the statistical power of the regressions. The maximum growth...

  10. Effect of feeding frequency and feeding rate on growth of ...

    African Journals Online (AJOL)

    Effect of feeding frequency and feeding rate on growth of Oreochromis mossambicus (Teleostei: Cichlidae) fry. ... Weight gain, specific growth rate and gross food conversion ratio were significantly affected by ... AJOL African Journals Online.

  11. An high order Mixed Interpolation Tensorial Components (MITC) shell element approach for modeling the buckling behavior of delaminated composites

    DEFF Research Database (Denmark)

    Gaiotti, Marco; Rizzo, Cesare M.; Branner, Kim

    2014-01-01

    This paper describes the experimental and numerical studies carried out on delaminated fiberglass epoxy resin laminates made-up by different fabrication methods, namely by vacuum infusion and prepreg. While the tested specimens were originally intended for the assessment of buckling behavior...... of composite laminates of wind turbine blades, results were found valuable for the marine industry as well, because similar laminates are used for the hull shell and stiffeners. Systematic calculations were carried out to assess the effects of an embedded delamination on the buckling load, varying the size...

  12. Growth rates of breeder reactor fuel. Final report

    International Nuclear Information System (INIS)

    Ott, K.O.

    1979-01-01

    During the contract period, a consistent formalism for the definition of the growth rates (and thus the doubling time) of breeder reactor fuel has been developed. This formalism was then extended to symbiotic operation of breeder and converter reactors. Further, an estimation prescription for the growth rate has been developed which is based upon the breeding worth factors. The characteristics of this definition have been investigated, which led to an additional integral concept, the breeding bonus

  13. Effects of lowered pH on marine phytoplankton growth rates

    DEFF Research Database (Denmark)

    Berge, Terje; Daugbjerg, Niels; Andersen, Betinna Balling

    2010-01-01

    concentration of seawater. Ocean acidification may potentially both stimulate and reduce primary production by marine phytoplankton. Data are scarce on the response of marine phytoplankton growth rates to lowered pH/increased CO2. Using the acid addition method to lower the seawater pH and manipulate...... the carbonate system, we determined in detail the lower pH limit for growth rates of 2 model species of common marine phytoplankton. We also tested whether growth and production rates of 6 other common species of phytoplankton were affected by ocean acidification (lowered to pH 7.0). The lower pH limits...... statistically similar in the pH range of ~7.0 to 8.5. Our results and literature reports on growth at lowered pH indicate that marine phytoplankton in general are resistant to climate change in terms of ocean acidification, and do not increase or decrease their growth rates according to ecological relevant...

  14. Modification of cell growth rate by irradiation

    International Nuclear Information System (INIS)

    Itoh, Hisao; Takemasa, Kazuhiko; Nishiguchi, Iku; Ka, Wei-Jei; Kutsuki, Shoji; Hashimoto, Shozo

    1993-01-01

    The effect of irradiation on the proliferation kinetics of the monolayer cells has been studied. Two human cell lines with different doubling times (HeLa-P and RMUG) and two clones that have the same radiosensitivity but different doubling times (HeLa-R and HeLa-S) were irradiated with a daily dose of 2 Gy for 6 days. The number of the clonogenic cells/dish was calculated by multiplying the number of total cell/dish by the survival fraction. In the rapidly growing cells (HeLa-P, HeLa-R), the number of the clonogenic cells was not decreased by the first two fractionated irradiations, but decreased thereafter at a similar rate as by single-dose fractionation, whereas the clonogenic cell number decreased from the first fractionated irradiation in the slowly growing cells (RMUG, HeLa-S). When the proliferation of clonogenic cell number increased along with a similar growth rates that was seen in all other types of cells. Further, no correlation was seen between the growth rates of cells without irradiation and cells that received irradiation. This latter result suggests that the slow growth rate of non-irradiated cells may not be the predictive factor of the tumor cure and the interruption of radiotherapy may reduce the beneficial effect of this treatment even in slow growing tumors. (author)

  15. Numerical simulations and experimental measurements of steel and ice impacts on concrete for acoustic interrogation of delaminations in bridge decks

    Energy Technology Data Exchange (ETDEWEB)

    Mazzeo, Brian A.; Patil, Anjali N.; Klis, Jeffrey M. [Brigham Young University, Department of Electrical and Computer Engineering, Provo, Utah, 84602 (United States); Hurd, Randy C.; Truscott, Tadd T. [Brigham Young University, Department of Mechanical Engineering, Provo, Utah, 84602 (United States); Guthrie, W. Spencer [Brigham Young University, Department of Civil and Environmental Engineering, Provo, Utah, 84602 (United States)

    2014-02-18

    Delaminations in bridge decks typically result from corrosion of the top mat of reinforcing steel, which leads to a localized separation of the concrete cover from the underlying concrete. Because delaminations cannot be detected using visual inspection, rapid, large-area interrogation methods are desired to characterize bridge decks without disruption to traffic, without the subjectivity inherent in existing methods, and with increased inspector safety. To this end, disposable impactors such as water droplets or ice chips can be dropped using automatic dispensers onto concrete surfaces to excite mechanical vibrations while acoustic responses can be recorded using air-coupled microphones. In this work, numerical simulations are used to characterize the flexural response of a model concrete bridge deck subject to both steel and ice impactors, and the results are compared with similar experiments performed in the laboratory on a partially delaminated concrete bridge deck slab. The simulations offer greater understanding of the kinetics of impacts and the responses of materials.

  16. Ballistic protection performance of curved armor systems with or without debondings/delaminations

    International Nuclear Information System (INIS)

    Tan, Ping

    2014-01-01

    Highlights: • Influence of pre-existing defect in an armor system on its ballistic performance. • Development of finite element models for the ballistic performance of armor systems. • Prediction of the ballistic limit and back face deformation of curved armor systems. - Abstract: In order to discern how pre-existing defects such as single or multiple debondings/delaminations in a curved armor system may affect its ballistic protection performance, two-dimensional axial finite element models were generated using the commercial software ANSYS/Autodyn. The armor systems considered in this investigation are composed of boron carbide front component and Kevlar/epoxy backing component. They are assumed to be perfectly bonded at the interface without defects. The parametric study shows that for the cases considered, the maximum back face deformation of a curved armor system with or without defects is more sensitive to its curvature, material properties of the ceramic front component, and pre-existing defect size and location than the ballistic limit velocity. Additionally, both the ballistic limit velocity and maximum back face deformation are significantly affected by the backing component thickness, front/backing component thickness ratio and the number of delaminations

  17. Measurement of adherence of residually stressed thin films by indentation. I. Mechanics of interface delamination

    International Nuclear Information System (INIS)

    Marshall, D.B.; Evans, A.G.

    1984-01-01

    A fracture analysis of indentation-induced delamination of thin films is presented. The analysis is based on a model system in which the section of film above the delaminating crack is treated as a rigidly clamped disc, and the crack extension force is derived from changes in strain energy of the system as the crack extends. Residual deposition stresses influence the cracking response by inducing buckling of the film above the crack and by providing an additional crack driving force once buckling occurs. A relation for the equilibrium crack length is derived in terms of the indenter load and geometry, the film thickness and mechanical properties, the residual stress level and the fracture toughness of the interface. The analysis provides a basis for using controlled indentation cracking as a quantitative measure of interface toughness and for evaluating contact-induced damage in thin films

  18. Analytic solutions for Rayleigh-Taylor growth rates in smooth density gradients

    International Nuclear Information System (INIS)

    Munro, D.H.

    1988-01-01

    The growth rate of perturbations on the shell of a laser fusion target can be estimated as √gk , where g is the shell acceleration and k is the transverse wave number of the perturbation. This formula overestimates the growth rate, and should be modified for the effects of density gradients and/or ablation of the unstable interface. The density-gradient effect is explored here analytically. With the use of variational calculus to explore all possible density profiles, the growth rate is shown to exceed √gk/(1+kL) , where L is a typical density-gradient scale length. Density profiles actually exhibiting this minimum growth rate are found

  19. Continental Delamination of the Romanian Eastern Carpathians: A Lower Crustal Origin of the Vrancea Seismogenic Zone?

    Science.gov (United States)

    Fillerup, M. A.; Knapp, J. H.; Knapp, C. C.

    2006-12-01

    Two lithosphere-scale, explosive-source seismic reflection profiles (DRACULA I and DACIA PLAN), inclusive of the hinterland and foreland of the Romanian Eastern Carpathians, provide new evidence for the geodynamic origin of the Vrancea Seismogenic Zone (VSZ) of Romania. These data, collected to evaluate existing subduction-related and delamination geodynamic models proposed to explain the intermediate depth seismicity associated with the Vrancea zone, show evidence of continental crust extending continuously above the VSZ from the Carpathian foreland well into the Transylvanian hinterland. Crustal thicknesses inferred from these data based on reflectivity show a 40-45 km crust below the Transylvanian basin abruptly shallowing to 32 km for ~120 km beneath the fold and thrust belt of the main Carpathian orogen and thickening again to 38-42 km crust in the foreland. This thinned crust outlines an apparent lower crustal sub-orogenic cavity that is overlain by a relatively subhorizontal reflective fabric absent of dipping reflectivity. The northwest dipping Vrancea seismogenic body, a 30x70x200 km volume of intermediate depth earthquakes, is located on the eastern flank of the apparently thin crust beneath the Carpathian orogen. Amplitude decay curves show penetration of seismic energy to a depth of ~60 km in the vicinity of the sub-orogenic cavity, implying this non- reflective zone is a geologic signature. Rotation of the VSZ about a hinge beneath the foreland basin at a depth of ~50 km restores to fill the lower-crustal cavity under the orogen, suggesting the VSZ represents a portion of brittle lower crust delaminated during continental lithospheric delamination which may have caused regional uplift of the Transylvanian basin. The lack of through-going, dipping crustal-scale boundaries along this composite lithospheric transect would appear to preclude subduction as an explanation for seismicity in the VSZ, consistent with abundant surface geologic data. These

  20. Modelling of tomato stem diameter growth rate based on physiological responses

    International Nuclear Information System (INIS)

    Li, L.; Tan, J.; Lv, T.

    2017-01-01

    The stem diameter is an important parameter describing the growth of tomato plant during vegetative growth stage. A stem diameter growth model was developed to predict the response of plant growth under different conditions. By analyzing the diurnal variations of stem diameter in tomato (Solanum lycopersicum L.), it was found that the stem diameter measured at 3:00 am was the representative value as the daily basis of tomato stem diameter. Based on the responses of growth rate in stem diameter to light and temperature, a linear regression relationship was applied to establish the stem diameter growth rate prediction model for the vegetative growth stage in tomato and which was further validated by experiment. The root mean square error (RMSE) and relative error (RE) were used to test the correlation between measured and modeled stem diameter variations. Results showed that the model can be used in prediction for stem diameter growth rate at vegetative growth stage in tomato. (author)

  1. COMPOSITIONAL AND THERMAL DIFFERENCES BETWEEN LITHOSPHERIC AND ASTHENOSPHERIC MANTLE AND THEIR INFLUENCE ON CONTINENTAL DELAMINATION

    Directory of Open Access Journals (Sweden)

    A. I. Kiselev

    2015-01-01

    Full Text Available The lower part of lithosphere in collisional orogens may delaminate due to density inversion between the asthenosphere and the cold thickened lithospheric mantle. Generally, standard delamination models have neglected density changes within the crust and the lithospheric mantle, which occur due to phase transitions and compositional variations upon changes of P-T parameters. Our attention is focused on effects of phase and density changes that may be very important and even dominant when compared with the effect of a simple change of the thermal mantle structure. The paper presents the results of numerical modeling for eclogitization of basalts of the lower crust as well as phase composition changes and density of underlying peridotite resulted from tectonic thickening of the lithosphere and its foundering into the asthenosphere. As the thickness of the lower crust increases, the mafic granulite (basalt passes into eclogite, and density inversion occurs at the accepted crust-mantle boundary (P=20 kbar because the newly formed eclogite is heavier than the underlying peridotite by 6 % (abyssal peridotite, according to [Boyd, 1989]. The density difference is a potential energy for delamination of the eclogitic portion of the crust. According to the model, P=70 kbar and T=1300 °C correspond to conditions at the lower boundary of the lithosphere. Assuming the temperature adiabatic distribution within the asthenosphere, its value at the given parameters ranges from 1350 °C to 1400 °C. Density inversion at dry conditions occurs with the identical lithospheric and asthenospheric compositions at the expense of the temperature difference at 100 °C with the density difference of only 0.0022 %. Differences of two other asthenospheric compositions (primitive mantle, and lherzolite KH as compared to the lithosphere (abyssal peridotite are not compensated for by a higher temperature. The asthenospheric density is higher than that of the lithospheric base

  2. Incorporation of plasma-functionalized carbon nanostructures in composite laminates for interlaminar reinforcement and delamination crack monitoring

    Science.gov (United States)

    Kravchenko, O. G.; Pedrazzoli, D.; Kovtun, D.; Qian, X.; Manas-Zloczower, I.

    2018-01-01

    A new approach employing carbon nanostructure (CNS) buckypapers (BP) was used to prepare glass fiber/epoxy composite materials with enhanced resistance to delamination along with damage monitoring capability. The CNS-BP was subjected to plasma treatment to improve its wettability by epoxy and to promote stronger interfacial bonding. An increase up to 20% in interlaminar fracture toughness in mode I and mode II was observed in composite laminates incorporating CNS BP. Morphological analysis of the fracture surfaces indicated that failure in the conductive CNS layer provided a more effective energy dissipation mechanism, resulting in interlaminar fracture toughness increase. Moreover, fracture of the conductive CNS layer enabled damage monitoring of the composite by electrical resistance measurements upon delamination. The proposed approach provides multifunctional ply interphases, allowing to couple damage monitoring with interlaminar reinforcement of composite laminates.

  3. Moisture-Induced Delamination Video of an Oxidized Thermal Barrier Coating

    Science.gov (United States)

    Smialek, James L.; Zhu, Dongming; Cuy, Michael D.

    2008-01-01

    PVD TBC coatings were thermally cycled to near-failure at 1150 C. Normal failure occurred after 200 to 300 1-hr cycles with only moderate weight gains (0.5 mg/sq cm). Delamination and buckling was often delayed until well after cooldown (desktop spallation), but could be instantly induced by the application of water drops, as shown in a video clip which can be viewed by clicking on figure 2 of this report. Moisture therefore plays a primary role in delayed desktop TBC failure. Hydrogen embrittlement is proposed as the underlying mechanism.

  4. Surface modification of carbon/epoxy prepreg using oxygen plasma and its effect on the delamination resistance behavior of carbon/epoxy composites

    International Nuclear Information System (INIS)

    Kim, M.H.; Rhee, K.Y.; Kim, H.J.; Jung, D.H.

    2007-01-01

    It was shown in previous study that the fracture toughness of carbon/epoxy laminated composites could be significantly improved by modifying the surface of the prepreg using Ar + irradiation in an oxygen environment. In this study, the surface of carbon/epoxy prepreg was modified using an oxygen plasma to improve the delamination resistance behavior of carbon/epoxy laminated composites. The variation of the contact angle on the prepreg surface was determined as a function of the modification time, in order to determine the optimal modification time. An XPS analysis was conducted to investigate the chemical changes on the surface of the prepreg caused by the plasma modification. Mode I delamination resistance curves of the composites with and without surface modification were plotted as a function of the delamination increment. The results showed that the contact angle varied from ∼64 o to ∼47 o depending on the modification time and reached a minimum for a modification time of 30 min. The XPS analysis showed that the hydrophilic carbonyl C=O group was formed by the oxygen plasma modification. The results also showed that the delamination resistance behavior was significantly improved by the plasma modification of the prepreg. This improvement was caused by the better layer-to-layer adhesion as well as increased interfacial strength between the fibers and matrix

  5. A quantitative theory of solid tumor growth, metabolic rate and vascularization.

    Directory of Open Access Journals (Sweden)

    Alexander B Herman

    Full Text Available The relationships between cellular, structural and dynamical properties of tumors have traditionally been studied separately. Here, we construct a quantitative, predictive theory of solid tumor growth, metabolic rate, vascularization and necrosis that integrates the relationships between these properties. To accomplish this, we develop a comprehensive theory that describes the interface and integration of the tumor vascular network and resource supply with the cardiovascular system of the host. Our theory enables a quantitative understanding of how cells, tissues, and vascular networks act together across multiple scales by building on recent theoretical advances in modeling both healthy vasculature and the detailed processes of angiogenesis and tumor growth. The theory explicitly relates tumor vascularization and growth to metabolic rate, and yields extensive predictions for tumor properties, including growth rates, metabolic rates, degree of necrosis, blood flow rates and vessel sizes. Besides these quantitative predictions, we explain how growth rates depend on capillary density and metabolic rate, and why similar tumors grow slower and occur less frequently in larger animals, shedding light on Peto's paradox. Various implications for potential therapeutic strategies and further research are discussed.

  6. Growth rate correlates negatively with protein turnover in Arabidopsis accessions.

    Science.gov (United States)

    Ishihara, Hirofumi; Moraes, Thiago Alexandre; Pyl, Eva-Theresa; Schulze, Waltraud X; Obata, Toshihiro; Scheffel, André; Fernie, Alisdair R; Sulpice, Ronan; Stitt, Mark

    2017-08-01

    Previous studies with Arabidopsis accessions revealed that biomass correlates negatively to dusk starch content and total protein, and positively to the maximum activities of enzymes in photosynthesis. We hypothesized that large accessions have lower ribosome abundance and lower rates of protein synthesis, and that this is compensated by lower rates of protein degradation. This would increase growth efficiency and allow more investment in photosynthetic machinery. We analysed ribosome abundance and polysome loading in 19 accessions, modelled the rates of protein synthesis and compared them with the observed rate of growth. Large accessions contained less ribosomes than small accessions, due mainly to cytosolic ribosome abundance falling at night in large accessions. The modelled rates of protein synthesis resembled those required for growth in large accessions, but were up to 30% in excess in small accessions. We then employed 13 CO 2 pulse-chase labelling to measure the rates of protein synthesis and degradation in 13 accessions. Small accessions had a slightly higher rate of protein synthesis and much higher rates of protein degradation than large accessions. Protein turnover was negligible in large accessions but equivalent to up to 30% of synthesised protein day -1 in small accessions. We discuss to what extent the decrease in growth in small accessions can be quantitatively explained by known costs of protein turnover and what factors may lead to the altered diurnal dynamics and increase of ribosome abundance in small accessions, and propose that there is a trade-off between protein turnover and maximisation of growth rate. © 2017 The Authors The Plant Journal © 2017 John Wiley & Sons Ltd.

  7. Investigating calcite growth rates using a quartz crystal microbalance with dissipation (QCM-D)

    Science.gov (United States)

    Cao, Bo; Stack, Andrew G.; Steefel, Carl I.; DePaolo, Donald J.; Lammers, Laura N.; Hu, Yandi

    2018-02-01

    Calcite precipitation plays a significant role in processes such as geological carbon sequestration and toxic metal sequestration and, yet, the rates and mechanisms of calcite growth under close to equilibrium conditions are far from well understood. In this study, a quartz crystal microbalance with dissipation (QCM-D) was used for the first time to measure macroscopic calcite growth rates. Calcite seed crystals were first nucleated and grown on sensors, then growth rates of calcite seed crystals were measured in real-time under close to equilibrium conditions (saturation index, SI = log ({Ca2+}/{CO32-}/Ksp) = 0.01-0.7, where {i} represent ion activities and Ksp = 10-8.48 is the calcite thermodynamic solubility constant). At the end of the experiments, total masses of calcite crystals on sensors measured by QCM-D and inductively coupled plasma mass spectrometry (ICP-MS) were consistent, validating the QCM-D measurements. Calcite growth rates measured by QCM-D were compared with reported macroscopic growth rates measured with auto-titration, ICP-MS, and microbalance. Calcite growth rates measured by QCM-D were also compared with microscopic growth rates measured by atomic force microscopy (AFM) and with rates predicted by two process-based crystal growth models. The discrepancies in growth rates among AFM measurements and model predictions appear to mainly arise from differences in step densities, and the step velocities were consistent among the AFM measurements as well as with both model predictions. Using the predicted steady-state step velocity and the measured step densities, both models predict well the growth rates measured using QCM-D and AFM. This study provides valuable insights into the effects of reactive site densities on calcite growth rate, which may help design future growth models to predict transient-state step densities.

  8. Growth rates of alien Oreochromis niloticus and indigenous ...

    African Journals Online (AJOL)

    Growth rates of indigenous Oreochromis mortimeri and alien Oreochromis niloticus from Lake Kariba were estimated from samples collected in 1997–2000, 2003–2005 and 2010–2011. Growth zones on scales and otoliths of O. niloticus and on the otoliths and opercula of O. mortimeri were deposited annually.

  9. Fatigue Crack Growth Rate and Stress-Intensity Factor Corrections for Out-of-Plane Crack Growth

    Science.gov (United States)

    Forth, Scott C.; Herman, Dave J.; James, Mark A.

    2003-01-01

    Fatigue crack growth rate testing is performed by automated data collection systems that assume straight crack growth in the plane of symmetry and use standard polynomial solutions to compute crack length and stress-intensity factors from compliance or potential drop measurements. Visual measurements used to correct the collected data typically include only the horizontal crack length, which for cracks that propagate out-of-plane, under-estimates the crack growth rates and over-estimates the stress-intensity factors. The authors have devised an approach for correcting both the crack growth rates and stress-intensity factors based on two-dimensional mixed mode-I/II finite element analysis (FEA). The approach is used to correct out-of-plane data for 7050-T7451 and 2025-T6 aluminum alloys. Results indicate the correction process works well for high DeltaK levels but fails to capture the mixed-mode effects at DeltaK levels approaching threshold (da/dN approximately 10(exp -10) meter/cycle).

  10. Growth rates, grazing, sinking, and iron limitation of equatorial Pacific phytoplankton

    International Nuclear Information System (INIS)

    Chavez, F.P.; Buck, K.R.; Coale, K.H.; Martin, J.H.; DiTullio, G.R.; Welschmeyer, N.A.; Barber, R.T.; Jacobson, A.C.

    1991-01-01

    Concentrations of phytoplankton and NO 3 are consistently low and high in surface waters of the oceanic eastern and central equatorial Pacific, and phytoplankton populations are dominated by small solitary phytoplankton. Growth rates of natural phytoplankton populations, needed to assess the relative importance of many of the processes considered in the equatorial Pacific, were estimated by several methods. The growth rates of natural phytoplankton populations were found to be ∼0.7 d -1 or 1 biomass doubling d -1 and were similar for all methods. To keep this system in its observed balance requires that loss rates approximate observed growth rates. Grazing rates, measured with a dilution grazing experiment, were high, accounting for a large fraction of the daily production. Additions of various forms of Fe to 5-7-d incubations utilizing ultraclean techniques resulted in significant shifts in autotrophic and heterotrophic assemblages between initial samples, controls, and Fe enrichments, which were presumably due to Fe, grazing by both protistan and metazoan components, and incubation artifacts. Estimated growth rates of small pennate diatoms showed increases in Fe enrichments with respect to controls. The growth rates of the pennate diatoms were similar to those estimated for the larger size fraction of the natural populations

  11. Sales Growth Rate Forecasting Using Improved PSO and SVM

    Directory of Open Access Journals (Sweden)

    Xibin Wang

    2014-01-01

    Full Text Available Accurate forecast of the sales growth rate plays a decisive role in determining the amount of advertising investment. In this study, we present a preclassification and later regression based method optimized by improved particle swarm optimization (IPSO for sales growth rate forecasting. We use support vector machine (SVM as a classification model. The nonlinear relationship in sales growth rate forecasting is efficiently represented by SVM, while IPSO is optimizing the training parameters of SVM. IPSO addresses issues of traditional PSO, such as relapsing into local optimum, slow convergence speed, and low convergence precision in the later evolution. We performed two experiments; firstly, three classic benchmark functions are used to verify the validity of the IPSO algorithm against PSO. Having shown IPSO outperform PSO in convergence speed, precision, and escaping local optima, in our second experiment, we apply IPSO to the proposed model. The sales growth rate forecasting cases are used to testify the forecasting performance of proposed model. According to the requirements and industry knowledge, the sample data was first classified to obtain types of the test samples. Next, the values of the test samples were forecast using the SVM regression algorithm. The experimental results demonstrate that the proposed model has good forecasting performance.

  12. Do fish growth rates correlate with PCB body burdens?

    Science.gov (United States)

    Andrew L. Rypel; David R.. Bayne

    2010-01-01

    We evaluated whether growth rates of six fish species correlated with PCB concentrations in a moderately-to-heavily polluted freshwater ecosystem. Using a large dataset (n ¼ 984 individuals), and after accounting for growth effects related to fish age, habitat, sex, and lipids, growth correlated significantly, but positively with lipid-corrected PCB concentrations for...

  13. On the growth rate of the foliicolous lichen Strigula elegans

    NARCIS (Netherlands)

    Wilde-Duyfjes, de B.E.E.

    1967-01-01

    The diametral growth rate of the foliicolous lichen Strigula elegans (Fée) Müll. Arg., measured under natural conditions in the African tropical rainforest, has been established to amount to (0.7-)3-3-6(-8) mm annually. As compared to the diametral growth rate of lichens from temperate regions,

  14. A comparative study on free vibration analysis of delaminated torsion stiff and bending stiff composite shells

    International Nuclear Information System (INIS)

    Dey, Sudip; Karmakar, Amit

    2013-01-01

    This paper presents a finite element method to compare the effects of delamination on free vibration of graphite-epoxy bending stiff and torsion stiff composite pretwisted shallow conical shells. The generalized dynamic equilibrium equation is derived from Lagrange's equation of motion neglecting the Coriolis effect for moderate rotational speeds. An eight noded isoparametric plate bending element is employed incorporating rotary inertia and effects of transverse shear deformation based on Mindlin's theory. The multipoint constraint; algorithm is utilized to ensure the compatibility of deformation and equilibrium of resultant forces and moments at the delamination crack front. The standard eigen value problem is solved by applying the QR iteration algorithm. Mode shapes for typical configurations are also depicted. Numerical results obtained are the first known non-dimensional frequencies which could serve as reference solutions for the future investigators.

  15. Enhancement of Impact Toughness by Delamination Fracture in a Low-Alloy High-Strength Steel with Al Alloying

    Science.gov (United States)

    Sun, Junjie; Jiang, Tao; Liu, Hongji; Guo, Shengwu; Liu, Yongning

    2016-12-01

    The effect of delamination toughening of martensitic steel was investigated both at room and low temperatures [253 K and 233 K (-20 °C and -40 °C)]. Two low-alloy martensitic steels with and without Al alloying were both prepared. Layered structure with white band and black matrix was observed in Al alloyed steel, while a homogeneous microstructure was displayed in the steel without Al. Both steels achieved high strength (tensile strength over 1600 MPa) and good ductility (elongation over 11 pct), but they displayed stark contrasts on impact fracture mode and Charpy impact energy. Delamination fracture occurred in Al alloyed steel and the impact energies were significantly increased both at room temperature (from 75 to 138 J, i.e., nearly improved up to 2 times) and low temperatures [from 47.9 to 71.3 J at 233 K (-40 °C)] compared with the one without Al. Alloying with Al promotes the segregation of Cr, Mn, Si and C elements to form a network structure, which is martensite with higher carbon content and higher hardness than that of the matrix. And this network structure evolved into a band structure during the hot rolling process. The difference of yield stress between the band structure and the matrix gives rise to a delamination fracture during the impact test, which increases the toughness greatly.

  16. Pretreatment Growth Rate Predicts Radiation Response in Vestibular Schwannomas

    International Nuclear Information System (INIS)

    Niu, Nina N.; Niemierko, Andrzej; Larvie, Mykol; Curtin, Hugh; Loeffler, Jay S.; McKenna, Michael J.; Shih, Helen A.

    2014-01-01

    Purpose: Vestibular schwannomas (VS) are often followed without initial therapeutic intervention because many tumors do not grow and radiation therapy is associated with potential adverse effects. In an effort to determine whether maximizing initial surveillance predicts for later treatment response, the predictive value of preirradiation growth rate of VS on response to radiation therapy was assessed. Methods and Materials: Sixty-four patients with 65 VS were treated with single-fraction stereotactic radiation surgery or fractionated stereotactic radiation therapy. Pre- and postirradiation linear expansion rates were estimated using volumetric measurements on sequential magnetic resonance images (MRIs). In addition, postirradiation tumor volume change was classified as demonstrating shrinkage (ratio of volume on last follow-up MRI to MRI immediately preceding irradiation <80%), stability (ratio 80%-120%), or expansion (ratio >120%). The median pre- and postirradiation follow-up was 20.0 and 27.5 months, respectively. Seven tumors from neurofibromatosis type 2 (NF2) patients were excluded from statistical analyses. Results: In the 58 non-NF2 patients, there was a trend of correlation between pre- and postirradiation volume change rates (slope on linear regression, 0.29; P=.06). Tumors demonstrating postirradiation expansion had a median preirradiation growth rate of 89%/year, and those without postirradiation expansion had a median preirradiation growth rate of 41%/year (P=.02). As the preirradiation growth rate increased, the probability of postirradiation expansion also increased. Overall, 24.1% of tumors were stable, 53.4% experienced shrinkage, and 22.5% experienced expansion. Predictors of no postirradiation tumor expansion included no prior surgery (P=.01) and slower tumor growth rate (P=.02). The control of tumors in NF2 patients was only 43%. Conclusions: Radiation therapy is an effective treatment for VS, but tumors that grow quickly preirradiation may be

  17. Pretreatment Growth Rate Predicts Radiation Response in Vestibular Schwannomas

    Energy Technology Data Exchange (ETDEWEB)

    Niu, Nina N. [Department of Radiation Oncology, Harvard Medical School, Massachusetts General Hospital, Boston, Massachusetts (United States); Harvard Medical School, Department of Medicine, Brigham and Women' s Hospital, Boston, Massachusetts (United States); Niemierko, Andrzej [Department of Radiation Oncology, Harvard Medical School, Massachusetts General Hospital, Boston, Massachusetts (United States); Larvie, Mykol [Harvard Medical School, Department of Radiology, Massachusetts General Hospital, Boston, Massachusetts (United States); Curtin, Hugh [Harvard Medical School, Department of Radiology, Massachusetts Eye and Ear Infirmary, Boston, Massachusetts (United States); Loeffler, Jay S. [Department of Radiation Oncology, Harvard Medical School, Massachusetts General Hospital, Boston, Massachusetts (United States); McKenna, Michael J. [Harvard Medical School, Department of Otolaryngology, Massachusetts Eye and Ear Infirmary, Boston, Massachusetts (United States); Shih, Helen A., E-mail: hshih@partners.org [Department of Radiation Oncology, Harvard Medical School, Massachusetts General Hospital, Boston, Massachusetts (United States)

    2014-05-01

    Purpose: Vestibular schwannomas (VS) are often followed without initial therapeutic intervention because many tumors do not grow and radiation therapy is associated with potential adverse effects. In an effort to determine whether maximizing initial surveillance predicts for later treatment response, the predictive value of preirradiation growth rate of VS on response to radiation therapy was assessed. Methods and Materials: Sixty-four patients with 65 VS were treated with single-fraction stereotactic radiation surgery or fractionated stereotactic radiation therapy. Pre- and postirradiation linear expansion rates were estimated using volumetric measurements on sequential magnetic resonance images (MRIs). In addition, postirradiation tumor volume change was classified as demonstrating shrinkage (ratio of volume on last follow-up MRI to MRI immediately preceding irradiation <80%), stability (ratio 80%-120%), or expansion (ratio >120%). The median pre- and postirradiation follow-up was 20.0 and 27.5 months, respectively. Seven tumors from neurofibromatosis type 2 (NF2) patients were excluded from statistical analyses. Results: In the 58 non-NF2 patients, there was a trend of correlation between pre- and postirradiation volume change rates (slope on linear regression, 0.29; P=.06). Tumors demonstrating postirradiation expansion had a median preirradiation growth rate of 89%/year, and those without postirradiation expansion had a median preirradiation growth rate of 41%/year (P=.02). As the preirradiation growth rate increased, the probability of postirradiation expansion also increased. Overall, 24.1% of tumors were stable, 53.4% experienced shrinkage, and 22.5% experienced expansion. Predictors of no postirradiation tumor expansion included no prior surgery (P=.01) and slower tumor growth rate (P=.02). The control of tumors in NF2 patients was only 43%. Conclusions: Radiation therapy is an effective treatment for VS, but tumors that grow quickly preirradiation may be

  18. Growth-Phase Sterigmatocystin Formation on Lactose Is Mediated via Low Specific Growth Rates in Aspergillus nidulans

    Directory of Open Access Journals (Sweden)

    Zoltán Németh

    2016-11-01

    Full Text Available Seed contamination with polyketide mycotoxins such as sterigmatocystin (ST produced by Aspergilli is a worldwide issue. The ST biosynthetic pathway is well-characterized in A. nidulans, but regulatory aspects related to the carbon source are still enigmatic. This is particularly true for lactose, inasmuch as some ST production mutant strains still synthesize ST on lactose but not on other carbon substrates. Here, kinetic data revealed that on d-glucose, ST forms only after the sugar is depleted from the medium, while on lactose, ST appears when most of the carbon source is still available. Biomass-specified ST production on lactose was significantly higher than on d-glucose, suggesting that ST formation may either be mediated by a carbon catabolite regulatory mechanism, or induced by low specific growth rates attainable on lactose. These hypotheses were tested by d-glucose limited chemostat-type continuous fermentations. No ST formed at a high growth rate, while a low growth rate led to the formation of 0.4 mg·L−1 ST. Similar results were obtained with a CreA mutant strain. We concluded that low specific growth rates may be the primary cause of mid-growth ST formation on lactose in A. nidulans, and that carbon utilization rates likely play a general regulatory role during biosynthesis.

  19. Bistable Bacterial Growth Rate in Response to Antibiotics with Low Membrane Permeability

    Science.gov (United States)

    Elf, Johan; Nilsson, Karin; Tenson, Tanel; Ehrenberg, Måns

    2006-12-01

    We demonstrate that growth rate bistability for bacterial cells growing exponentially at a fixed external antibiotic concentration can emerge when the cell wall permeability for the drug is low and the growth rate sensitivity to the intracellular drug concentration is high. Under such conditions, an initially high growth rate can remain high, due to dilution of the intracellular drug concentration by rapid cell volume increase, while an initially low growth rate can remain low, due to slow cell volume increase and insignificant drug dilution. Our findings have implications for the testing of novel antibiotics on growing bacterial strains.

  20. Fatigue Life Methodology for Tapered Hybrid Composite Flexbeams

    Science.gov (United States)

    urri, Gretchen B.; Schaff, Jeffery R.

    2006-01-01

    Nonlinear-tapered flexbeam specimens from a full-size composite helicopter rotor hub flexbeam were tested under combined constant axial tension and cyclic bending loads. Two different graphite/glass hybrid configurations tested under cyclic loading failed by delamination in the tapered region. A 2-D finite element model was developed which closely approximated the flexbeam geometry, boundary conditions, and loading. The analysis results from two geometrically nonlinear finite element codes, ANSYS and ABAQUS, are presented and compared. Strain energy release rates (G) associated with simulated delamination growth in the flexbeams are presented from both codes. These results compare well with each other and suggest that the initial delamination growth from the tip of the ply-drop toward the thick region of the flexbeam is strongly mode II. The peak calculated G values were used with material characterization data to calculate fatigue life curves for comparison with test data. A curve relating maximum surface strain to number of loading cycles at delamination onset compared well with the test results.

  1. Circadian cycles in growth and feeding rates of heterotrophic protist plankton

    DEFF Research Database (Denmark)

    Jakobsen, Hans Henrik; Strom, S.L.

    2004-01-01

    Growth and feeding rates of four species of planktonic marine heterotrophic protists showed pronounced diel cycles. In most cases, rates were higher during the day and lower at night. However, for the ciliate Strobilidium sp., growth was highest at night. In another ciliate species, Balanion...... comatum, no day-night difference in growth and feeding rates was found. Maintenance of day-night rate differences during 24-h exposures to continuous darkness demonstrated that most of these protists had circadian cycles. The heterotrophic dinoflagellate Oxyrrhis marina exhibited a clear irradiance...... to culturing in a day: night light cycle in O. marina and found that resetting the circadian cycle in this dinoflagellate temporarily arrested growth and feeding. We suggest that protists use a time-integrated light threshold rather than an instantaneous irradiance to maintain the circadian cell cycle...

  2. Evidence of A Bimodal US GDP Growth Rate Distribution: A Wavelet Approach

    Directory of Open Access Journals (Sweden)

    Sandro Claudio Lera

    2017-04-01

    Full Text Available We present a quantitative characterisation of the fluctuations of the annualized growth rate of the real US GDP per capita at many scales, using a wavelet transform analysis of two data sets, quarterly data from 1947 to 2015 and annual data from 1800 to 2010. The chosen mother wavelet (first derivative of the Gaussian function applied to the logarithm of the real US GDP per capita provides a robust estimation of the instantaneous growth rate at different scales. Our main finding is that business cycles appear at all scales and the distribution of GDP growth rates can be well approximated by a bimodal function associated to a series of switches between regimes of strong growth rate $\\rho_\\text{high}$ and regimes of low growth rate $\\rho_\\text{low}$. The succession of such two regimes compounds to produce a remarkably stable long term average real annualized growth rate of 1.6% from 1800 to 2010 and $\\approx 2.0\\%$ since 1950, which is the result of a subtle compensation between the high and low growth regimes that alternate continuously. Thus, the overall growth dynamics of the US economy is punctuated, with phases of strong growth that are intrinsically unsustainable, followed by corrections or consolidation until the next boom starts. We interpret these findings within the theory of "social bubbles" and argue as a consequence that estimations of the cost of the 2008 crisis may be misleading. We also interpret the absence of strong recovery since 2008 as a protracted low growth regime $\\rho_\\text{low}$ associated with the exceptional nature of the preceding large growth regime.

  3. Numerical Analysis of Inlet Gas-Mixture Flow Rate Effects on Carbon Nanotube Growth Rate

    Directory of Open Access Journals (Sweden)

    B. Zahed

    2013-01-01

    Full Text Available The growth rate and uniformity of Carbon Nano Tubes (CNTs based on Chemical Vapor Deposition (CVD technique is investigated by using a numerical model. In this reactor, inlet gas mixture, including xylene as carbon source and mixture of argon and hydrogen as  carrier gas enters into a horizontal CVD reactor at atmospheric pressure. Based on the gas phase and surface reactions, released carbon atoms are grown as CNTs on the iron catalysts at the reactor hot walls. The effect of inlet gas-mixture flow rate, on CNTs growth rate and its uniformity is discussed. In addition the velocity and temperature profile and also species concentrations throughout the reactor are presented.

  4. Radiocarbon Based Ages and Growth Rates: Hawaiian Deep Sea Corals

    Energy Technology Data Exchange (ETDEWEB)

    Roark, E B; Guilderson, T P; Dunbar, R B; Ingram, B L

    2006-01-13

    The radial growth rates and ages of three different groups of Hawaiian deep-sea 'corals' were determined using radiocarbon measurements. Specimens of Corallium secundum, Gerardia sp., and Leiopathes glaberrima, were collected from 450 {+-} 40 m at the Makapuu deep-sea coral bed using a submersible (PISCES V). Specimens of Antipathes dichotoma were collected at 50 m off Lahaina, Maui. The primary source of carbon to the calcitic C. secundum skeleton is in situ dissolved inorganic carbon (DIC). Using bomb {sup 14}C time markers we calculate radial growth rates of {approx} 170 {micro}m y{sup -1} and ages of 68-75 years on specimens as tall as 28 cm of C. secundum. Gerardia sp., A. dichotoma, and L. glaberrima have proteinaceous skeletons and labile particulate organic carbon (POC) is their primary source of architectural carbon. Using {sup 14}C we calculate a radial growth rate of 15 {micro}m y{sup -1} and an age of 807 {+-} 30 years for a live collected Gerardia sp., showing that these organisms are extremely long lived. Inner and outer {sup 14}C measurements on four sub-fossil Gerardia spp. samples produce similar growth rate estimates (range 14-45 {micro}m y{sup -1}) and ages (range 450-2742 years) as observed for the live collected sample. Similarly, with a growth rate of < 10 {micro}m y{sup -1} and an age of {approx}2377 years, L. glaberrima at the Makapuu coral bed, is also extremely long lived. In contrast, the shallow-collected A. dichotoma samples yield growth rates ranging from 130 to 1,140 {micro}m y{sup -1}. These results show that Hawaiian deep-sea corals grow more slowly and are older than previously thought.

  5. GROWTH RATE DISPERSION (GRD OF THE (010 FACE OF BORAX CRYSTALS IN FLOWING SOLUTION

    Directory of Open Access Journals (Sweden)

    Suharso Suharso

    2010-06-01

    Full Text Available The growth rates of borax crystals from aqueous solutions in the (010 direction at various flow rates were measured. The observed variations of the growth rate can be represented by a normal distribution.  It was found that there is no correlation between growth rate distribution and solution flow under these experimental conditions.   Keywords: Growth rate dispersion (GRD, borax, flow rate

  6. Bacterial growth on surfaces: Automated image analysis for quantification of growth rate-related parameters

    DEFF Research Database (Denmark)

    Møller, S.; Sternberg, Claus; Poulsen, L. K.

    1995-01-01

    species-specific hybridizations with fluorescence-labelled ribosomal probes to estimate the single-cell concentration of RNA. By automated analysis of digitized images of stained cells, we determined four independent growth rate-related parameters: cellular RNA and DNA contents, cell volume......, and the frequency of dividing cells in a cell population. These parameters were used to compare physiological states of liquid-suspended and surfacegrowing Pseudomonas putida KT2442 in chemostat cultures. The major finding is that the correlation between substrate availability and cellular growth rate found...

  7. Metabolic enzyme cost explains variable trade-offs between microbial growth rate and yield.

    Directory of Open Access Journals (Sweden)

    Meike T Wortel

    2018-02-01

    Full Text Available Microbes may maximize the number of daughter cells per time or per amount of nutrients consumed. These two strategies correspond, respectively, to the use of enzyme-efficient or substrate-efficient metabolic pathways. In reality, fast growth is often associated with wasteful, yield-inefficient metabolism, and a general thermodynamic trade-off between growth rate and biomass yield has been proposed to explain this. We studied growth rate/yield trade-offs by using a novel modeling framework, Enzyme-Flux Cost Minimization (EFCM and by assuming that the growth rate depends directly on the enzyme investment per rate of biomass production. In a comprehensive mathematical model of core metabolism in E. coli, we screened all elementary flux modes leading to cell synthesis, characterized them by the growth rates and yields they provide, and studied the shape of the resulting rate/yield Pareto front. By varying the model parameters, we found that the rate/yield trade-off is not universal, but depends on metabolic kinetics and environmental conditions. A prominent trade-off emerges under oxygen-limited growth, where yield-inefficient pathways support a 2-to-3 times higher growth rate than yield-efficient pathways. EFCM can be widely used to predict optimal metabolic states and growth rates under varying nutrient levels, perturbations of enzyme parameters, and single or multiple gene knockouts.

  8. [Clinical research of arthroscopic separate double-layer suture bridge technique for delaminated rotator cuff tear].

    Science.gov (United States)

    Ren, Jiangtao; Xu, Cong; Liu, Xianglin; Wang, Jiansong; Li, Zhihuai; Lü, Yongming

    2017-10-01

    To explore the effectiveness of the arthroscopic separate double-layer suture bridge technique in treatment of the delaminated rotator cuff tear. Between May 2013 and May 2015, 54 patients with the delaminated rotator cuff tears were recruited in the study. They were randomly allocated into 2 groups to receive repair either using arthroscopic separate double-layer suture bridge technique (trial group, n =28) or using arthroscopic whole-layer suture bridge technique (control group, n =26). There was no significant difference in gender, age, injured side, tear type, and preoperative visual analogue scale (VAS) score, Constants score, American Shoulder and Elbow Surgeons (ASES) score, University of California Los Angeles (UCLA) score, and the range of motion of shoulder joint between 2 groups ( P >0.05). Postoperative functional scores, range of motion, and recurrence rate of tear in 2 groups were observed and compared. The operation time was significant longer in trial group than in control group ( t =8.383, P =0.000). All incisions healed at stage Ⅰ without postoperative complication. All the patients were followed up 12 months. At 12 months postoperatively, the UCLA score, ASES score, VAS score, Constant score, and the range of motion were significantly improved when compared with the preoperative values in 2 groups ( P 0.05). Four cases (14.3%) of rotator cuff tear recurred in trial group while 5 cases (19.2%) in control group, showing no significant difference ( χ 2 =0.237, P =0.626). Compared with the arthroscopic whole-layer suture bridge technique, arthroscopic separate double-layer suture bridge technique presents no significant difference in the shoulder function score, the range of motion, and recurrence of rotator cuff tear, while having a longer operation time.

  9. Nationwide Macroeconomic Variables and the Growth Rate of Bariatric Surgeries in Brazil.

    Science.gov (United States)

    Cazzo, Everton; Ramos, Almino Cardoso; Pareja, José Carlos; Chaim, Elinton Adami

    2018-06-06

    The effect of nationwide economic issues on the necessary expansion in the number of bariatric procedures remains unclear. This study aims to determine whether there are correlations between the growth rate in the number of bariatric surgeries and the major macroeconomic variables over time in Brazil. It is a nationwide analysis regarding the number of bariatric surgeries in Brazil and the main national macroeconomic variables from 2003 through 2016: gross domestic product (GDP), inflation rate, and the unemployment rate, as well as the evolution in the number of registered bariatric surgeons. There were significant positive correlations of the growth rate of surgeries with the early variations of the GDP (R = 0.5558; p = 0.04863) and of the overall health expenditure per capita (R = 0.78322; p = 0.00259). The growth rate of the number of bariatric surgeries was not correlated with the unemployment and inflation rates, as well as with the growth rate of available bariatric surgeons. There were direct relationships between the growth rate of bariatric surgeries and the evolutions of the GDP and health care expenditure per capita. These variables appear to influence the nationwide offer of bariatric surgery.

  10. Age class, longevity and growth rate relationships: protracted growth increases in old trees in the eastern United States.

    Science.gov (United States)

    Johnson, Sarah E; Abrams, Marc D

    2009-11-01

    This study uses data from the International Tree-Ring Data Bank website and tree cores collected in the field to explore growth rate (basal area increment, BAI) relationships across age classes (from young to old) for eight tree species in the eastern US. These species represent a variety of ecological traits and include those in the genera Populus, Quercus, Pinus, Tsuga and Nyssa. We found that most trees in all age classes and species exhibit an increasing BAI throughout their lives. This is particularly unusual for trees in the older age classes that we expected to have declining growth in the later years, as predicted by physiological growth models. There exists an inverse relationship between growth rate and increasing age class. The oldest trees within each species have consistently slow growth throughout their lives, implying an inverse relationship between growth rate and longevity. Younger trees (trees when they are of the same age resulting from a higher proportion of fast-growing trees in these young age classes. Slow, but increasing, BAI in the oldest trees in recent decades is a continuation of their growth pattern established in previous centuries. The fact that they have not shown a decreasing growth rate in their old age contradicts physiological growth models and may be related to the stimulatory effects of global change phenomenon (climate and land-use history).

  11. Orbit width scaling of TAE instability growth rate

    International Nuclear Information System (INIS)

    Wong, H.V.; Berk, H.L.; Breizman, B.N.

    1995-07-01

    The growth rate of Toroidal Alfven Eigenmodes (TAE) driven unstable by resonant coupling of energetic charged particles is evaluated in the ballooning limit over a wide range of parameters. All damping effects are ignored. Variations in orbit width, aspect ratio, and the ratio of alfven velocity to energetic particle birth velocity, are explored. The relative contribution of passing and trapped particles, and finite Larmor radius effects, are also examined. The phase space location of resonant particles with interact strongly with the modes is described. The accuracy of the analytic results with respect to growth rate magnitude and parametric dependence is investigated by comparison with numerical results

  12. Orbit width scaling of TAE instability growth rate

    International Nuclear Information System (INIS)

    Wong, H.V.; Berk, H.L.; Breizman, B.N.

    1995-01-01

    The growth rate of toroidal Alfven eigenmodes (TAEs) driven unstable by resonant coupling of energetic charged particles is evaluated in the 'ballooning' limit over a wide range of parameters. All damping effects are ignored. Variations in orbit width, aspect ratio and the ratio of Alfven velocity to energetic particle 'birth' velocity are explored. The relative contribution of passing and trapped particles, and finite Larmor radius effects, are also examined. The phase space location of resonant particles that interact strongly with the modes is described. The accuracy of the analytic results with respect to growth rate magnitude and parametric dependence is investigated by comparison with numerical results. (author). 16 refs, 8 figs

  13. Growth rate regulated genes and their wide involvement in the Lactococcus lactis stress responses

    Directory of Open Access Journals (Sweden)

    Redon Emma

    2008-07-01

    Full Text Available Abstract Background The development of transcriptomic tools has allowed exhaustive description of stress responses. These responses always superimpose a general response associated to growth rate decrease and a specific one corresponding to the stress. The exclusive growth rate response can be achieved through chemostat cultivation, enabling all parameters to remain constant except the growth rate. Results We analysed metabolic and transcriptomic responses of Lactococcus lactis in continuous cultures at different growth rates ranging from 0.09 to 0.47 h-1. Growth rate was conditioned by isoleucine supply. Although carbon metabolism was constant and homolactic, a widespread transcriptomic response involving 30% of the genome was observed. The expression of genes encoding physiological functions associated with biogenesis increased with growth rate (transcription, translation, fatty acid and phospholipids metabolism. Many phages, prophages and transposon related genes were down regulated as growth rate increased. The growth rate response was compared to carbon and amino-acid starvation transcriptomic responses, revealing constant and significant involvement of growth rate regulations in these two stressful conditions (overlap 27%. Two regulators potentially involved in the growth rate regulations, llrE and yabB, have been identified. Moreover it was established that genes positively regulated by growth rate are preferentially located in the vicinity of replication origin while those negatively regulated are mainly encountered at the opposite, thus indicating the relationship between genes expression and their location on chromosome. Although stringent response mechanism is considered as the one governing growth deceleration in bacteria, the rigorous comparison of the two transcriptomic responses clearly indicated the mechanisms are distinct. Conclusion This work of integrative biology was performed at the global level using transcriptomic analysis

  14. Unusual growth rate during cystic echinococcosis.

    Science.gov (United States)

    Valour, Florent; Khenifer, Safia; Della-Schiava, Nellie; Cotte, Eddy; Guibert, Benoit; Wallon, Martine; Durupt, Stéphane; Durieu, Isabelle

    2014-04-01

    Cystic echinococcosis is a world wild zoonosis caused by Echinococcus granulosus, leading to hepatic and lung cysts with a usually slight growth rate. We report the case of an 82year-old Algerian woman with hepatic and lung cystic echinococcosis with a 10-fold size increase in 6months. Copyright © 2013. Published by Elsevier Ireland Ltd.

  15. A panel data investigation of real exchange rate misalignment and growth

    Directory of Open Access Journals (Sweden)

    Flávio Vilela Vieira

    2012-09-01

    Full Text Available The paper investigates the role of real exchange rate misalignment on long-run growth for a set of ninety countries using time series data from 1980 to 2004. We first estimate a panel data model (fixed and random effects for the real exchange rate in order to produce estimates of the equilibrium real exchange rate and this is then used to construct measures of real exchange rate misalignment. We provide an alternative set of estimates of RER misalignment using panel cointegration methods. The results for the two-step System GMM panel growth models indicate that the coefficients for real exchange rate misalignment are positive for different model specification and samples, which means that a more depreciated (appreciated real exchange rate helps (harms long-run growth. The estimated coefficients are higher for developing and emerging countries.

  16. The effect of rumen content transfer on rate of bacteria and protozoa growth

    International Nuclear Information System (INIS)

    Suharyono; M Winugroho; Y Widiati; S Marijati

    1998-01-01

    The aims the experiment wants to know the benefit of rate of microbial protein in rumen content and to complete the information that isolates is useful for ruminant animals feed. The result indicated that buffaloes from East Nusa Tenggara is the best when they are used as donor rumen transfer making isolate. When rumen of ongole cattle generation was mixed in rumen content of buffaloes from East Nusa Tenggara and incubated 48 h, the rate of bacteria cell growth is better than rate of protozoa cell growth comparing to the other animals. The values are 30.99 mg/h/100 ml and 24.92 mg.h/100 ml respectively. The results of isolate selection in 48 h incubation indicated that treatment F is the best. The results rates of bacteria cell growth and rate of protozoa's cell growth are 26.96 mg/h/100 ml and 2.53 mg/h/100 respectively. The result of in vitro study indicated that pH and ammonia concentration support the rate of bacteria cell growth and do not cause the toxicity of microbes and animal . The rate of bacteria cell growth on D treatment is significant to A,B, and C treatments. The values are 21.44 mg/h/100 ml. 7.99; 13.13; and 13.38 mg/h/100 ml respectively. The result rates of protozoa's cell growth tends lower than rates of bacteria cell. The overall conclusion is a lower or a higher rate of microorganism cell growth depends on the environment condition. (author)

  17. The frequency effect on the fatigue crack growth rate of 304 stainless steel

    International Nuclear Information System (INIS)

    Shih, Y.-S.; Chen, J.-J.

    1999-01-01

    Under cyclic loading condition, the fatigue crack growth (FCG) rate governed by stress intensity factor and stress ratio is well known; Walker's equation, Forman's equation and Elber's equation are typical formulae to describe the fatigue crack growth rate. However, the loading frequency effect on the fatigue crack growth rate has yet to be explored. Recently, studies have focused on the loading frequency effect on some visco-elastic materials, and have provided a clearer understanding of the frequency effect on the fatigue crack growth rate. In a physical sense, knowledge about the loading frequency effect on the fatigue crack growth rate for 304 stainless steel is still lacking. James conducted a lot of experiments, and through data analysis, he concluded an evaluation equation which is based upon the experimental illustration. In this study, the physical properties of the material are used to illustrate the modification of fatigue crack growth rate, and a new formula which is based upon the modified Forman's equation, is provided. (orig.)

  18. On the growth rate of gallstones in the human gallbladder

    Science.gov (United States)

    Nudelman, I.

    1993-05-01

    The growth rate of a single symmetrically oval shaped gallbladder stone weighing 10.8 g was recorded over a period of six years before surgery and removal. The length of the stone was measured by ultrasonography and the growth rate was found to be linear with time, with a value of 0.4 mm/year. A smaller stone growing in the wall of the gallbladder was detected only three years before removal and grew at a rate of ˜ 1.33 mm/year. The morphology and metallic ion chemical composition of the large stone and of a randomly selected small stone weighing about 1.1 g, extracted from another patient, were analyzed and compared. It was found that the large stone contained besides calcium also lead, whereas the small stone contained mainly calcium. It is possible that the lead causes a difference in mechanism between the growth of a single large and growth of multiple small gallstones.

  19. DKDP crystal growth controlled by cooling rate

    Science.gov (United States)

    Xie, Xiaoyi; Qi, Hongji; Shao, Jianda

    2017-08-01

    The performance of deuterated potassium dihydrogen phosphate (DKDP) crystal directly affects beam quality, energy and conversion efficiency in the Inertial Confinement Fusion(ICF)facility, which is related with the initial saturation temperature of solution and the real-time supersaturation during the crystal growth. However, traditional method to measure the saturation temperature is neither efficient nor accurate enough. Besides, the supersaturation is often controlled by experience, which yields the higher error and leads to the instability during the crystal growth. In this paper, DKDP solution with 78% deuteration concentration is crystallized in different temperatures. We study the relation between solubility and temperature of DKDP and fit a theoretical curve with a parabola model. With the model, the measurement of saturation temperature is simplified and the control precision of the cooling rate is improved during the crystal growth, which is beneficial for optimizing the crystal growth process.

  20. Restraining Na-Montmorillonite Delamination in Water by Adsorption of Sodium Dodecyl Sulfate or Octadecyl Trimethyl Ammonium Chloride on the Edges

    Directory of Open Access Journals (Sweden)

    Hongliang Li

    2016-08-01

    Full Text Available The delamination of montmorillonite in water leads to sliming in ore slurry, which is detrimental to mineral flotation and solid/water separation. In this work, the delamination of Na-montmorillonite (Na-MMT has been restrained by sodium dodecyl sulfate (SDS or octadecyl trimethyl ammonium chloride (1831 through the adsorption on the edge of the mineral. The experimental results have shown that the pretreatment by adding SDS and 1831 could greatly reduce the Stokes size percentage of −1.1 µm particles in the aqueous Na-MMT suspension. From the X-ray diffractometer (XRD results, the interlayer spacing of the MMT pre-treated by SDS and 1831 is smaller than that of original MMT particles. Adsorption position of SDS and 1831 on MMT surfaces was analyzed by the measurements of adsorption capacity of SDS and 1831, inductively-coupled plasma spectra, and zeta potential before and after the plane surface of MMT was covered with tetraethylenepentaminecopper ([Cu(tetren]2+. The results indicated that SDS and 1831 are adsorbed on the edge and the whole surface of Na-MMT, respectively. Delamination of MMT could be well restrained by the adsorption of SDS and 1831 on the edges of MMT.

  1. The influence of a delaminated layer on the impedance spectrum of an operating solid oxide fuel cell

    Energy Technology Data Exchange (ETDEWEB)

    Gazzarri, J.I. [British Columbia Univ., Vancouver, BC (Canada). Dept. of Mechanical Engineering; Kesler, O. [National Research Council of Canada, Vancouver, BC (Canada). Inst. for Fuel Cell Innovation

    2005-07-01

    The development of a 2-dimensional finite element model of Solid Oxide Fuel Oxide (SOFC) AC impedance behavior was discussed. The model was developed to simulate the frequency response of a single cell with and without mechanical damage. Impedance spectroscopy was used in the development of a diagnostic technique to identify a delamination failure within a working SOFC. Changes in the impedance spectrum of a working cell were observed on the appearance of a delamination between 2 adjacent layers. The intent was to identify distinctive patterns in the cracked cell spectra that provide enough information about the degradation process so that it can be recognized and distinguished from other electrochemical processes and degradation modes. It was anticipated that the method will provide a useful tool for both maintenance and research purposes, providing insight into the causes of inadequate functioning. Results indicate that the presence of mechanically induced damage within the components of an SOFC can be detected by comparing the frequency response of the undamaged cell with that of a cell in which in-plane cracking or delamination has occurred. The presence of such defects manifests itself as a new semicircle in the Nyquist impedance diagram of the full cell, with a relaxation frequency of approximately 35 kHz. It was concluded that the ability to distinguish the crack-induced semicircle from the semicircles induced by electrochemical reactions depended on the difference between the characteristic relaxation times and their relative sizes. 17 refs., 1 tab.,10 figs.

  2. Confinement - assisted shock-wave-induced thin-film delamination (SWIFD) of copper indium gallium diselenide (CIGS) on a flexible substrate

    Science.gov (United States)

    Lorenz, Pierre; Zagoranskiy, Igor; Ehrhardt, Martin; Han, Bing; Bayer, Lukas; Zimmer, Klaus

    2017-12-01

    The laser structuring of CIGS (copper indium gallium (di)selenide) solar cell material without influence and damaging the functionality of the active layer is a challenge for laser methods The shock-wave-induced thin-film delamination (SWIFD) process allows structuring without thermal modifications due to a spatial separation of the laser absorption from the functional layer removal process. In the present study, SWIFD structuring of CIGS solar cell stacks was investigated. The rear side of the polyimide was irradiated with a KrF-Excimer laser. The laser-induced ablation process generates a traverse shock wave, and the interaction of the shock wave with the layer-substrate interface results in a delamination process. The effect of a water confinement on the SWIFD process was studied where the rear side of the substrate was covered with a ∼2 mm thick water layer. The resultant surface morphology was analysed and discussed. At a sufficient number of laser pulses N and laser fluences Φ, the CIGS layer can be selectively removed from the Mo back contact. The water confinement, as well as the increasing laser beam size A0 and N, results in the reduction of the necessary minimal laser fluence Φth. Further, the delaminated CIGS area increased with increasing Φ, N, and A0.

  3. Skeletal muscle protein accretion rates and hindlimb growth are reduced in late gestation intrauterine growth-restricted fetal sheep.

    Science.gov (United States)

    Rozance, Paul J; Zastoupil, Laura; Wesolowski, Stephanie R; Goldstrohm, David A; Strahan, Brittany; Cree-Green, Melanie; Sheffield-Moore, Melinda; Meschia, Giacomo; Hay, William W; Wilkening, Randall B; Brown, Laura D

    2018-01-01

    Adults who were affected by intrauterine growth restriction (IUGR) suffer from reductions in muscle mass, which may contribute to insulin resistance and the development of diabetes. We demonstrate slower hindlimb linear growth and muscle protein synthesis rates that match the reduced hindlimb blood flow and oxygen consumption rates in IUGR fetal sheep. These adaptations resulted in hindlimb blood flow rates in IUGR that were similar to control fetuses on a weight-specific basis. Net hindlimb glucose uptake and lactate output rates were similar between groups, whereas amino acid uptake was significantly lower in IUGR fetal sheep. Among all fetuses, blood O 2 saturation and plasma glucose, insulin and insulin-like growth factor-1 were positively associated and norepinephrine was negatively associated with hindlimb weight. These results further our understanding of the metabolic and hormonal adaptations to reduced oxygen and nutrient supply with placental insufficiency that develop to slow hindlimb growth and muscle protein accretion. Reduced skeletal muscle mass in the fetus with intrauterine growth restriction (IUGR) persists into adulthood and may contribute to increased metabolic disease risk. To determine how placental insufficiency with reduced oxygen and nutrient supply to the fetus affects hindlimb blood flow, substrate uptake and protein accretion rates in skeletal muscle, late gestation control (CON) (n = 8) and IUGR (n = 13) fetal sheep were catheterized with aortic and femoral catheters and a flow transducer around the external iliac artery. Muscle protein kinetic rates were measured using isotopic tracers. Hindlimb weight, linear growth rate, muscle protein accretion rate and fractional synthetic rate were lower in IUGR compared to CON (P fetal norepinephrine and reduced IGF-1 and insulin. © 2017 The Authors. The Journal of Physiology © 2017 The Physiological Society.

  4. Study on the PWSCC Crack Growth Rate for Steam Generator Tubing

    International Nuclear Information System (INIS)

    Kang, Shin Hoo; Hwang, Il Soon; Lim, Jun; Lee, Seung Gi; Ryu, Kyung Ha

    2008-03-01

    Using in-situ Raman spectroscopy and crack growth rate lest system in simulated PWR primary water environment, the relationship between the oxide film chemistry and the PWSCC growth rate has been studied. We used I/2T compact tension specimen and disk specimen made of Alloy 182 and Alloy 600 for crack growth rate test and in-situ Raman spectroscopy measurement. Test was made in a refreshed autoclave with 30 cc STP / kg of dissolved hydrogen concentration. Conductivity, pH, dissolved hydrogen and oxygen concentration were continuously monitored at the outlet. The crack growth rate was measured by using switching DCPD technique under cyclinc triangular loading and at the same time oxide phase was determined by using in-situ Raman spectra at the elevation of the temperature. Additionally Raman spectroscopy was achieved for oxide phase transition of Alloy 600 according to the temperature and dissolved hydrogen concentration, 2 and 30cc STP / kg

  5. Effects of tensile and compressive in-plane stress fields on adhesion in laser induced delamination experiments

    NARCIS (Netherlands)

    Fedorov, A.; Vellinga, W. P.; De Hosson, J. Th. M.

    2008-01-01

    In this work, the adhesion of a polymer coating on steel substrate subjected to uniaxial tensile plastic deformations was studied with the laser induced delamination technique. A decrease in the practical work of adhesion has been measured as the deformation of the substrate progressed. Moreover, it

  6. Breast meat quality of chickens with divergent growth rates and its relation to growth curve parameters

    Directory of Open Access Journals (Sweden)

    P. C. Muth

    2017-11-01

    Full Text Available The effects of the increase of body weight of contemporary broilers during growth on functional meat quality and color characteristics of the chicken breast muscle are controversially debated. Therefore, male chickens (n = 264 of a fast-growing commercial broiler (Ross 308 and two slow-growing experimental meat-type chicken lines were compared at equal age and at similar body weight in order to investigate the effect of growth rate on selected functional breast meat traits and meat color. Additionally, the breast meat characteristics of birds with different growth profiles were compared within lines. When the body weight of commercial broilers reached about 40 to 60 % of their growth potential, they exhibited particularly high ultimate pH values compared with slow-growing lines. The ability of the meat of fast-growing broilers to retain water during cooking was impaired (5 to 16 percentage points increased cooking loss compared to slow-growing lines, which, in contrast to pH, was only marginally affected by body weight and/or age at slaughter. No unfavorable correlations of breast meat quality traits with the growth profile, represented by growth curve parameters derived from the Gompertz–Laird equation, were detected within any of the investigated chicken lines. It is noteworthy that the associations of ultimate pH and cooking loss with maximum growth speed indicate a non-linear relationship. Thus, some of the functional characteristics of breast meat of the fast-growing broiler resembled the white-striping defect described for poultry meat, but the hypothesis that selection on increased growth rates is detrimental for meat quality per se could not be confirmed. In fact, an elevated growth potential in particular, i.e., body weight at maturity, could have some beneficial effects for the water-holding capacity of breast meat, regardless of the genotypic growth rate.

  7. Long-term growth rates and effects of bleaching in Acropora hyacinthus

    Science.gov (United States)

    Gold, Zachary; Palumbi, Stephen R.

    2018-03-01

    Understanding the response of coral growth to natural variation in the environment, as well as to acute temperature stress under current and future climate change conditions, is critical to predicting the future health of coral reef ecosystems. As such, ecological surveys are beginning to focus on corals that live in high thermal stress environments to understand how future coral populations may adapt to climate change. We investigated the relationship between coral growth, thermal microhabitat, symbionts type, and thermal acclimatization of four species of the Acropora hyacinthus complex in back-reef lagoons in American Samoa. Coral growth was measured from August 2010 to April 2016 using horizontal planar area of coral colonies derived from photographs and in situ maximum width measurements. Despite marked intraspecific variation, we found that planar colony growth rates were significantly different among cryptic species. The highly heat tolerant A. hyacinthus variant "HE" increased in area an average of 2.9% month-1 (0.03 cm average mean radial extension month-1). By contrast, the three less tolerant species averaged 6.1% (0.07 cm average mean radial extension month-1). Planar growth rates were 40% higher on average in corals harboring Clade C versus Clade D symbiont types, although marked inter-colony variation in growth rendered this difference nonsignificant. Planar growth rates for all four species dropped to near zero following a 2015 bleaching event, independent of the visually estimated percent area of bleaching. Within 1 yr, growth rates recovered to previous levels, confirming previous studies that found sublethal effects of thermal stress on coral growth. Long-term studies of individual coral colonies provide an important tool to measure impacts of environmental change and allow integration of coral physiology, genetics, symbionts, and microclimate on reef growth patterns.

  8. Growth rate change driven by external perturbation in the azuki bean weevil

    CERN Document Server

    Fukano, T

    2003-01-01

    In laboratory experiments we obtain that the apparent growth rate of the population becomes larger than one under the normal condition, triggered by the external perturbation as the removal of individuals. The changed growth rate is stable for a while. We also propose a simple model of population dynamics allowing both matching and mis-matching the trend of the external perturbation, and show that the growth rate of the model population is changeable and stable to some extent.

  9. Growth rate change driven by external perturbation in the azuki bean weevil

    International Nuclear Information System (INIS)

    Fukano, Takao; Gunji, Yukio-Pegio

    2003-01-01

    In laboratory experiments we obtain that the apparent growth rate of the population becomes larger than one under the normal condition, triggered by the external perturbation as the removal of individuals. The changed growth rate is stable for a while. We also propose a simple model of population dynamics allowing both matching and mis-matching the trend of the external perturbation, and show that the growth rate of the model population is changeable and stable to some extent

  10. Cell Size and Growth Rate Are Modulated by TORC2-Dependent Signals.

    Science.gov (United States)

    Lucena, Rafael; Alcaide-Gavilán, Maria; Schubert, Katherine; He, Maybo; Domnauer, Matthew G; Marquer, Catherine; Klose, Christian; Surma, Michal A; Kellogg, Douglas R

    2018-01-22

    The size of all cells, from bacteria to vertebrates, is proportional to the growth rate set by nutrient availability, but the underlying mechanisms are unknown. Here, we show that nutrients modulate cell size and growth rate via the TORC2 signaling network in budding yeast. An important function of the TORC2 network is to modulate synthesis of ceramide lipids, which play roles in signaling. TORC2-dependent control of ceramide signaling strongly influences both cell size and growth rate. Thus, cells that cannot make ceramides fail to modulate their growth rate or size in response to changes in nutrients. PP2A associated with the Rts1 regulatory subunit (PP2A Rts1 ) is embedded in a feedback loop that controls TORC2 signaling and helps set the level of TORC2 signaling to match nutrient availability. Together, the data suggest a model in which growth rate and cell size are mechanistically linked by ceramide-dependent signals arising from the TORC2 network. Copyright © 2017 Elsevier Ltd. All rights reserved.

  11. Investigation Analysis of Crack Growth Arresting with Fasteners in Hybrid Laminated Skin-Stiffener Joint

    Science.gov (United States)

    Jeevan Kumar, N.; Ramesh Babu, P.

    2018-02-01

    In recent years carbon fibre-reinforced polymers (CFRP) emerged its increasing demand in aerospace engineering. Due to their high specific strength to weight ratio, these composites offer more characteristics and considerable advantages compared to metals. Metals, unlike composites, offer plasticity effects to evade high stress concentrations during postbuckling. Under compressive load, composite structures show a wide range of damage mechanisms where a set of damage modes combined together might lead to the eventual structural collapse. Crack is one of the most critical damages in fiber composites, which are being employed in primary aircraft structures. A parametric study is conducted to investigate the arrest mechanism of the delamination or crack growth with installation of multiple fasteners when the delamination is embedded in between the skin and stiffener interface.

  12. Influence of Crucible Support Rod on the Growth Rate and Temperature Gradient in a Bridgman Growth of Tin Crystal

    OpenAIRE

    IMASHIMIZU, Yuji; MIURA, Koji; KAMATA, Masaki; WATANABE, Jiro

    2003-01-01

    Bridgman growth of tincrystal was carried out in a graphite crucible that was fixed on a quartz support rod or a copper one. The growth rate and axial temperature distribution were examined by recording the temperature variation with time at each of four prescribed positions in the solid-liquidsystem during solidification, l) Actual growth rate of crystal increased with progress of solidification while the furnace elevated at a constant rate, but the tendency was different depending on the ty...

  13. [Specific growth rate and the rate of energy metabolism in the ontogenesis of axolotl, Ambystoma mexicanum (Amphibia: Ambystomatidae)].

    Science.gov (United States)

    Vladimirova, I G; Kleĭmenov, S Iu; Alekseeva, T A; Radzinskaia, L I

    2003-01-01

    Concordant changes in the rate of energy metabolism and specific growth rate of axolotls have been revealed. Several periods of ontogeny are distinguished, which differ in the ratio of energy metabolism to body weight and, therefore, are described by different allometric equations. It is suggested that the specific growth rate of an animal determines the type of dependence of energy metabolism on body weight.

  14. Postnatal growth rates covary weakly with embryonic development rates and do not explain adult mortality probability among songbirds on four continents.

    Science.gov (United States)

    Martin, Thomas E; Oteyza, Juan C; Mitchell, Adam E; Potticary, Ahva L; Lloyd, Penn

    2015-03-01

    Growth and development rates may result from genetic programming of intrinsic processes that yield correlated rates between life stages. These intrinsic rates are thought to affect adult mortality probability and longevity. However, if proximate extrinsic factors (e.g., temperature, food) influence development rates differently between stages and yield low covariance between stages, then development rates may not explain adult mortality probability. We examined these issues based on study of 90 songbird species on four continents to capture the diverse life-history strategies observed across geographic space. The length of the embryonic period explained little variation (ca. 13%) in nestling periods and growth rates among species. This low covariance suggests that the relative importance of intrinsic and extrinsic influences on growth and development rates differs between stages. Consequently, nestling period durations and nestling growth rates were not related to annual adult mortality probability among diverse songbird species within or among sites. The absence of a clear effect of faster growth on adult mortality when examined in an evolutionary framework across species may indicate that species that evolve faster growth also evolve physiological mechanisms for ameliorating costs on adult mortality. Instead, adult mortality rates of species in the wild may be determined more strongly by extrinsic environmental causes.

  15. Ergodicity, hidden bias and the growth rate gain

    Science.gov (United States)

    Rochman, Nash D.; Popescu, Dan M.; Sun, Sean X.

    2018-05-01

    Many single-cell observables are highly heterogeneous. A part of this heterogeneity stems from age-related phenomena: the fact that there is a nonuniform distribution of cells with different ages. This has led to a renewed interest in analytic methodologies including use of the ‘von Foerster equation’ for predicting population growth and cell age distributions. Here we discuss how some of the most popular implementations of this machinery assume a strong condition on the ergodicity of the cell cycle duration ensemble. We show that one common definition for the term ergodicity, ‘a single individual observed over many generations recapitulates the behavior of the entire ensemble’ is implied by the other, ‘the probability of observing any state is conserved across time and over all individuals’ in an ensemble with a fixed number of individuals but that this is not true when the ensemble is growing. We further explore the impact of generational correlations between cell cycle durations on the population growth rate. Finally, we explore the ‘growth rate gain’—the phenomenon that variations in the cell cycle duration leads to an improved population-level growth rate—in this context. We highlight that, fundamentally, this effect is due to asymmetric division.

  16. Effect of neutron irradiation on hatching rate of eggs and growth rate of chicken

    International Nuclear Information System (INIS)

    Liu Yubin; Zhao Jide; Liu Shengdian; Xy Xiuwei

    1995-01-01

    It was proved through 3 years of experiments and productions that after the eggs of AA meat chickens being irradiated by 14 MeV fast neutron, the hatching rate and the survival rate as well the weight of commercial chickens increased greatly. In addition it is found that the optimum neutron fluence for hatching and growth rate is 6.2 x 10 5 n·cm -2

  17. CHRONIC UNSTABILITY AND POTENTIAL GROWTH RATE: TURKISH EXPERIENCE, 1960-2006

    Directory of Open Access Journals (Sweden)

    MUSTAFA İSMİHAN

    2013-06-01

    Full Text Available This study investigates the role of macroeconomic instability on potential growth rate of output in Turkey over the period 1960-2006. In doing so, it also attempts to estimate the potential growth rate of Turkish economy over the sample period by using Hodrick-Prescott filter and model based on production function approach. Descriptive and empirical results suggest that Turkish economy suffered from a significant output loss during the chronic instability episodes, between the mid-1970s and 2001. A significant fall in macroeconomic instability has provided the main contribution to the achievement of the recent high growth episode (2002-2006 of Turkish economy. However, in order to continue the desired high growth performance in near future it is necessary to accelerate both human and physical capital formation while preserving stability.

  18. Growth, Mortality and Exploitation Rates of Sarotherodon ...

    African Journals Online (AJOL)

    Evans

    ABSTRACT. Sarotherodon melanotheron population of Dominli Lagoon in the Western Region of Ghana was studied for its growth and mortality parameters as well as exploitation rate. The study generally aimed at providing basic information necessary for the assessment and management of the fish stock in the lagoon.

  19. Testing and Life Prediction for Composite Rotor Hub Flexbeams

    Science.gov (United States)

    Murri, Gretchen B.

    2004-01-01

    A summary of several studies of delamination in tapered composite laminates with internal ply-drops is presented. Initial studies used 2D FE models to calculate interlaminar stresses at the ply-ending locations in linear tapered laminates under tension loading. Strain energy release rates for delamination in these laminates indicated that delamination would likely start at the juncture of the tapered and thin regions and grow unstably in both directions. Tests of glass/epoxy and graphite/epoxy linear tapered laminates under axial tension delaminated as predicted. Nonlinear tapered specimens were cut from a full-size helicopter rotor hub and were tested under combined constant axial tension and cyclic transverse bending loading to simulate the loading experienced by a rotorhub flexbeam in flight. For all the tested specimens, delamination began at the tip of the outermost dropped ply group and grew first toward the tapered region. A 2D FE model was created that duplicated the test flexbeam layup, geometry, and loading. Surface strains calculated by the model agreed very closely with the measured surface strains in the specimens. The delamination patterns observed in the tests were simulated in the model by releasing pairs of MPCs along those interfaces. Strain energy release rates associated with the delamination growth were calculated for several configurations and using two different FE analysis codes. Calculations from the codes agreed very closely. The strain energy release rate results were used with material characterization data to predict fatigue delamination onset lives for nonlinear tapered flexbeams with two different ply-dropping schemes. The predicted curves agreed well with the test data for each case studied.

  20. A review on pipeline corrosion, in-line inspection (ILI), and corrosion growth rate models

    International Nuclear Information System (INIS)

    Vanaei, H.R.; Eslami, A.; Egbewande, A.

    2017-01-01

    Pipelines are the very important energy transmission systems. Over time, pipelines can corrode. While corrosion could be detected by in-line inspection (ILI) tools, corrosion growth rate prediction in pipelines is usually done through corrosion rate models. For pipeline integrity management and planning selecting the proper corrosion ILI tool and also corrosion growth rate model is important and can lead to significant savings and safer pipe operation. In this paper common forms of pipeline corrosion, state of the art ILI tools, and also corrosion growth rate models are reviewed. The common forms of pipeline corrosion introduced in this paper are Uniform/General Corrosion, Pitting Corrosion, Cavitation and Erosion Corrosion, Stray Current Corrosion, Micro-Bacterial Influenced Corrosion (MIC). The ILI corrosion detection tools assessed in this study are Magnetic Flux Leakage (MFL), Circumferential MFL, Tri-axial MFL, and Ultrasonic Wall Measurement (UT). The corrosion growth rate models considered in this study are single-value corrosion rate model, linear corrosion growth rate model, non-linear corrosion growth rate model, Monte-Carlo method, Markov model, TD-GEVD, TI-GEVD model, Gamma Process, and BMWD model. Strengths and limitations of ILI detection tools, and also corrosion predictive models with some practical examples are discussed. This paper could be useful for those whom are supporting pipeline integrity management and planning. - Highlights: • Different forms of pipeline corrosion are explained. • Common In-Line Inspection (ILI) tools and corrosion growth rate models are introduced. • Strength and limitations of corrosion growth rate models/ILI tools are discussed. • For pipeline integrity management programs using more than one corrosion growth rate model/ILI tool is suggested.

  1. Stainless steels: general considerations and rates of crack growth

    International Nuclear Information System (INIS)

    Chator, T.

    1992-05-01

    This report describes the different types of stainless steels, and presents the laws governing the rates of crack growth for several stainless steels extensively used for the manufacture of structures in nuclear power plants. The laws are not discussed in detail in the report. After a brief review of the development of stainless steels, the main categories of stainless steels, their mechanical characteristics and corrosion resistance, are presented. Finally, the rates of crack growth are presented for various stainless steels, mainly austenitic. The study overall aim is an investigation of the cracking in the 900 MWe primary pump thermal barriers and shafts

  2. DETERMINATION OF THE SPECIFIC GROWTH RATE ON ...

    African Journals Online (AJOL)

    Sewage generation is one of the dense problems Nigerians encounter on daily bases, mostly at the urbanized area where factories and industries are located. This paper is aimed at determining the specific growth rate “K” of biological activities on cassava wastewater during degradation using Michaelis-Menten Equation.

  3. Size-dependent standard deviation for growth rates: empirical results and theoretical modeling.

    Science.gov (United States)

    Podobnik, Boris; Horvatic, Davor; Pammolli, Fabio; Wang, Fengzhong; Stanley, H Eugene; Grosse, I

    2008-05-01

    We study annual logarithmic growth rates R of various economic variables such as exports, imports, and foreign debt. For each of these variables we find that the distributions of R can be approximated by double exponential (Laplace) distributions in the central parts and power-law distributions in the tails. For each of these variables we further find a power-law dependence of the standard deviation sigma(R) on the average size of the economic variable with a scaling exponent surprisingly close to that found for the gross domestic product (GDP) [Phys. Rev. Lett. 81, 3275 (1998)]. By analyzing annual logarithmic growth rates R of wages of 161 different occupations, we find a power-law dependence of the standard deviation sigma(R) on the average value of the wages with a scaling exponent beta approximately 0.14 close to those found for the growth of exports, imports, debt, and the growth of the GDP. In contrast to these findings, we observe for payroll data collected from 50 states of the USA that the standard deviation sigma(R) of the annual logarithmic growth rate R increases monotonically with the average value of payroll. However, also in this case we observe a power-law dependence of sigma(R) on the average payroll with a scaling exponent beta approximately -0.08 . Based on these observations we propose a stochastic process for multiple cross-correlated variables where for each variable (i) the distribution of logarithmic growth rates decays exponentially in the central part, (ii) the distribution of the logarithmic growth rate decays algebraically in the far tails, and (iii) the standard deviation of the logarithmic growth rate depends algebraically on the average size of the stochastic variable.

  4. Size-dependent standard deviation for growth rates: Empirical results and theoretical modeling

    Science.gov (United States)

    Podobnik, Boris; Horvatic, Davor; Pammolli, Fabio; Wang, Fengzhong; Stanley, H. Eugene; Grosse, I.

    2008-05-01

    We study annual logarithmic growth rates R of various economic variables such as exports, imports, and foreign debt. For each of these variables we find that the distributions of R can be approximated by double exponential (Laplace) distributions in the central parts and power-law distributions in the tails. For each of these variables we further find a power-law dependence of the standard deviation σ(R) on the average size of the economic variable with a scaling exponent surprisingly close to that found for the gross domestic product (GDP) [Phys. Rev. Lett. 81, 3275 (1998)]. By analyzing annual logarithmic growth rates R of wages of 161 different occupations, we find a power-law dependence of the standard deviation σ(R) on the average value of the wages with a scaling exponent β≈0.14 close to those found for the growth of exports, imports, debt, and the growth of the GDP. In contrast to these findings, we observe for payroll data collected from 50 states of the USA that the standard deviation σ(R) of the annual logarithmic growth rate R increases monotonically with the average value of payroll. However, also in this case we observe a power-law dependence of σ(R) on the average payroll with a scaling exponent β≈-0.08 . Based on these observations we propose a stochastic process for multiple cross-correlated variables where for each variable (i) the distribution of logarithmic growth rates decays exponentially in the central part, (ii) the distribution of the logarithmic growth rate decays algebraically in the far tails, and (iii) the standard deviation of the logarithmic growth rate depends algebraically on the average size of the stochastic variable.

  5. Mathematical model for predicting molecular-beam epitaxy growth rates for wafer production

    International Nuclear Information System (INIS)

    Shi, B.Q.

    2003-01-01

    An analytical mathematical model for predicting molecular-beam epitaxy (MBE) growth rates is reported. The mathematical model solves the mass-conservation equation for liquid sources in conical crucibles and predicts the growth rate by taking into account the effect of growth source depletion on the growth rate. Assumptions made for deducing the analytical model are discussed. The model derived contains only one unknown parameter, the value of which can be determined by using data readily available to MBE growers. Procedures are outlined for implementing the model in MBE production of III-V compound semiconductor device wafers. Results from use of the model to obtain targeted layer compositions and thickness of InP-based heterojunction bipolar transistor wafers are presented

  6. Growth rate in the dynamical dark energy models

    International Nuclear Information System (INIS)

    Avsajanishvili, Olga; Arkhipova, Natalia A.; Samushia, Lado; Kahniashvili, Tina

    2014-01-01

    Dark energy models with a slowly rolling cosmological scalar field provide a popular alternative to the standard, time-independent cosmological constant model. We study the simultaneous evolution of background expansion and growth in the scalar field model with the Ratra-Peebles self-interaction potential. We use recent measurements of the linear growth rate and the baryon acoustic oscillation peak positions to constrain the model parameter α that describes the steepness of the scalar field potential. (orig.)

  7. Growth rate in the dynamical dark energy models.

    Science.gov (United States)

    Avsajanishvili, Olga; Arkhipova, Natalia A; Samushia, Lado; Kahniashvili, Tina

    Dark energy models with a slowly rolling cosmological scalar field provide a popular alternative to the standard, time-independent cosmological constant model. We study the simultaneous evolution of background expansion and growth in the scalar field model with the Ratra-Peebles self-interaction potential. We use recent measurements of the linear growth rate and the baryon acoustic oscillation peak positions to constrain the model parameter [Formula: see text] that describes the steepness of the scalar field potential.

  8. Calcite growth-rate inhibition by fulvic acid and magnesium ion—Possible influence on biogenic calcite formation

    Science.gov (United States)

    Reddy, Michael M.

    2012-01-01

    Increases in ocean surface water dissolved carbon dioxide (CO2) concentrations retard biocalcification by reducing calcite supersaturation (Ωc). Reduced calcification rates may influence growth-rate dependent magnesium ion (Mg) incorporation into biogenic calcite modifying the use of calcifying organisms as paleoclimate proxies. Fulvic acid (FA) at biocalcification sites may further reduce calcification rates. Calcite growth-rate inhibition by FA and Mg, two common constituents of seawater and soil water involved in the formation of biogenic calcite, was measured separately and in combination under identical, highly reproducible experimental conditions. Calcite growth rates (pH=8.5 and Ωc=4.5) are reduced by FA (0.5 mg/L) to 47% and by Mg (10−4 M) to 38%, compared to control experiments containing no added growth-rate inhibitor. Humic acid (HA) is twice as effective a calcite growth-rate inhibitor as FA. Calcite growth rate in the presence of both FA (0.5 mg/L) and Mg (10−4 M) is reduced to 5% of the control rate. Mg inhibits calcite growth rates by substitution for calcium ion at the growth site. In contrast, FA inhibits calcite growth rates by binding multiple carboxylate groups on the calcite surface. FA and Mg together have an increased affinity for the calcite growth sites reducing calcite growth rates.

  9. Coordinated Changes in Mutation and Growth Rates Induced by Genome Reduction

    Directory of Open Access Journals (Sweden)

    Issei Nishimura

    2017-07-01

    Full Text Available Genome size is determined during evolution, but it can also be altered by genetic engineering in laboratories. The systematic characterization of reduced genomes provides valuable insights into the cellular properties that are quantitatively described by the global parameters related to the dynamics of growth and mutation. In the present study, we analyzed a small collection of W3110 Escherichia coli derivatives containing either the wild-type genome or reduced genomes of various lengths to examine whether the mutation rate, a global parameter representing genomic plasticity, was affected by genome reduction. We found that the mutation rates of these cells increased with genome reduction. The correlation between genome length and mutation rate, which has been reported for the evolution of bacteria, was also identified, intriguingly, for genome reduction. Gene function enrichment analysis indicated that the deletion of many of the genes encoding membrane and transport proteins play a role in the mutation rate changes mediated by genome reduction. Furthermore, the increase in the mutation rate with genome reduction was highly associated with a decrease in the growth rate in a nutrition-dependent manner; thus, poorer media showed a larger change that was of higher significance. This negative correlation was strongly supported by experimental evidence that the serial transfer of the reduced genome improved the growth rate and reduced the mutation rate to a large extent. Taken together, the global parameters corresponding to the genome, growth, and mutation showed a coordinated relationship, which might be an essential working principle for balancing the cellular dynamics appropriate to the environment.

  10. Diagnostic Accuracy of Growth Rate in Differentiating Etiologies of Short Stature in Children

    Directory of Open Access Journals (Sweden)

    Mohammad Reza Alaei

    2016-08-01

    Full Text Available Background  Short stature is a manifestation of a wide variety of conditions that some of which may be amenable to timely treatment and a suboptimal growth rate may be an early marker pointing to the cause of growth retardation. This study was conducted to evaluate the diagnostic utility of growth rate in differential diagnosis of children with short stature. Materials and Methods All children between the ages of 2 and 18 years who visited in pediatric endocrinology clinic in a five years period were recruited in a prospective cohort study. Children with standing height Results One hundred forty three patients fulfilled the inclusion criteria. Mean follow up period was 14.4±10.9 months. Etiologies of short stature were: constitutional growth delay (CGD 46.9%, familial short stature (FSS 28.7%, hypothyroidism 4.2%, growth hormone deficiency (GHD 4.2% and miscellaneous causes in 16% of patients.  Mean Z- score for children with constitutional growth delay was -2.3±0.69, in familial short stature was -2.3±0.65 and for other condition was -2.7±1.49. There was a meaningful statistical correlation between growth rate and etiology of short stature (P0.05. Conclusion There was significant difference in growth rate between children with constitutional growth delay and familial short stature in comparing to short stature due to endocrine problem and other etiologies. Assessment of growth rate has some utility in diagnosing the etiology of short stature.

  11. Daily changes in temperature, not the circadian clock, regulate growth rate in Brachypodium distachyon.

    Directory of Open Access Journals (Sweden)

    Dominick A Matos

    Full Text Available Plant growth is commonly regulated by external cues such as light, temperature, water availability, and internal cues generated by the circadian clock. Changes in the rate of growth within the course of a day have been observed in the leaves, stems, and roots of numerous species. However, the relative impact of the circadian clock on the growth of grasses has not been thoroughly characterized. We examined the influence of diurnal temperature and light changes, and that of the circadian clock on leaf length growth patterns in Brachypodium distachyon using high-resolution time-lapse imaging. Pronounced changes in growth rate were observed under combined photocyles and thermocycles or with thermocycles alone. A considerably more rapid growth rate was observed at 28°C than 12°C, irrespective of the presence or absence of light. In spite of clear circadian clock regulated gene expression, plants exhibited no change in growth rate under conditions of constant light and temperature, and little or no effect under photocycles alone. Therefore, temperature appears to be the primary cue influencing observed oscillations in growth rate and not the circadian clock or photoreceptor activity. Furthermore, the size of the leaf meristem and final cell length did not change in response to changes in temperature. Therefore, the nearly five-fold difference in growth rate observed across thermocycles can be attributed to proportionate changes in the rate of cell division and expansion. A better understanding of the growth cues in B. distachyon will further our ability to model metabolism and biomass accumulation in grasses.

  12. Dispersion relation and growth rate in a Cherenkov free electron laser: Finite axial magnetic field

    International Nuclear Information System (INIS)

    Kheiri, Golshad; Esmaeilzadeh, Mahdi

    2013-01-01

    A theoretical analysis is presented for dispersion relation and growth rate in a Cherenkov free electron laser with finite axial magnetic field. It is shown that the growth rate and the resonance frequency of Cherenkov free electron laser increase with increasing axial magnetic field for low axial magnetic fields, while for high axial magnetic fields, they go to a saturation value. The growth rate and resonance frequency saturation values are exactly the same as those for infinite axial magnetic field approximation. The effects of electron beam self-fields on growth rate are investigated, and it is shown that the growth rate decreases in the presence of self-fields. It is found that there is an optimum value for electron beam density and Lorentz relativistic factor at which the maximum growth rate can take place. Also, the effects of velocity spread of electron beam are studied and it is found that the growth rate decreases due to the electron velocity spread

  13. Spatial distribution of soda straws growth rates of the Coufin Cave (Vercors, France

    Directory of Open Access Journals (Sweden)

    Perrette Yves

    2010-07-01

    Full Text Available The Choranche Cave system (Vercors, France is an excellent locality for measuring the growth rates of large numbers soda straws. This is especially the case for the Coufin Cave, as enlargement of the cave entrance in 1875 led to a change in stalactite color from brown to white, thus providing a reliable chronomarker. The date of this brown-to-white calcite transition has been confirmed by lamina counting. We measured and georeferenced the growth-lengths of 306 soda straws in a 1m2 area of the roof of the Coufin Cave entrance chamber. Because of the very slow and sometimes inexistent water feeding of those stalactites, hydrochemistry analysis were not achieved and drop rate effect on growth were neglected; this study is based on a geomorphological and geostatistical work. By measuring a large number of soda straws in a very small area for which most of the parameters affecting stalactite growth could be considered uniform, and because flow rates are very slow (frequencies are always superior to 1 drop per half hour, we could ascribe differences in growth rates to variations in the global increase of water flow through the unsaturated matrix. Statistical and geostatistical analyses of the measurements showed that this set of similarly shaped stalactites actually consisted of three Gaussian populations with different mean growth rates: fast growth rate (FGR- mean of 0.92 mm.y-1, medium growth rate (MGR- mean of 0.47 mm.y-1 and low growth rate (LGR- 0.09 mm.y-1. Plotting the lengths and spatial distribution of the 20 longest FGR soda straws revealed that there is a rough pattern to the water flow through the cave roof. Even if no direction is statisticaly different from others, the observed directional pattern is consistent with local and regional tectonic observations. Plots of the spatial distribution of the soda straws show that FGR soda straws follow lines of regional geological stress, whereas MGR and LGR soda straws are more dispersed.

  14. Variability in growth rates of larval haddock in the northern North Sea

    DEFF Research Database (Denmark)

    Gallego, A.; Heath, M.R.; Basford, D.J.

    1999-01-01

    of the spring plankton production bloom, and a likely explanation for the absence of environmental effects on larval growth was high food availability and larval feeding rates. Nevertheless, differences in growth were observed between cohorts, with larvae hatched later in the spring displaying higher growth...... at age than those hatched earlier. Particle-tracking modelling suggested that differences in temperature history between cohorts, on their own or compounded by a potential interaction between temperature and the development of plankton production, may explain the higher growth rate of the larvae hatched...

  15. Gross domestic product growth rates as confined Lévy flights: Towards a unifying theory of economic growth rate fluctuations

    Science.gov (United States)

    Lera, Sandro Claudio; Sornette, Didier

    2018-01-01

    A model that combines economic growth rate fluctuations at the microscopic and macroscopic levels is presented. At the microscopic level, firms are growing at different rates while also being exposed to idiosyncratic shocks at the firm and sector levels. We describe such fluctuations as independent Lévy-stable fluctuations, varying over multiple orders of magnitude. These fluctuations are aggregated and measured at the macroscopic level in averaged economic output quantities such as GDP. A fundamental question is thereby to what extent individual firm size fluctuations can have a noticeable impact on the overall economy. We argue that this question can be answered by considering the Lévy fluctuations as embedded in a steep confining potential well, ensuring nonlinear mean-reversal behavior, without having to rely on microscopic details of the system. The steepness of the potential well directly controls the extent to which idiosyncratic shocks to firms and sectors are damped at the level of the economy. Additionally, the theory naturally accounts for business cycles, represented in terms of a bimodal economic output distribution and thus connects two so far unrelated fields in economics. By analyzing 200 years of U.S. gross domestic product growth rates, we find that the model is in good agreement with the data.

  16. Influence of corruption on economic growth rate and foreign investment

    Science.gov (United States)

    Podobnik, Boris; Shao, Jia; Njavro, Djuro; Ivanov, Plamen Ch.; Stanley, H. E.

    2008-06-01

    We analyze the dependence of the Gross Domestic Product ( GDP) per capita growth rates on changes in the Corruption Perceptions Index ( CPI). For the period 1999 2004 for all countries in the world, we find on average that an increase of CPI by one unit leads to an increase of the annual GDP per capita growth rate by 1.7%. By regressing only the European countries with transition economies, we find that an increase of CPI by one unit generates an increase of the annual GDP per capita growth rate by 2.4%. We also analyze the relation between foreign direct investments received by different countries and CPI, and we find a statistically significant power-law functional dependence between foreign direct investment per capita and the country corruption level measured by the CPI. We introduce a new measure to quantify the relative corruption between countries based on their respective wealth as measured by GDP per capita.

  17. CK2 activity is modulated by growth rate in Saccharomyces cerevisiae

    International Nuclear Information System (INIS)

    Tripodi, Farida; Cirulli, Claudia; Reghellin, Veronica; Marin, Oriano; Brambilla, Luca; Schiappelli, Maria Patrizia; Porro, Danilo; Vanoni, Marco; Alberghina, Lilia; Coccetti, Paola

    2010-01-01

    Research highlights: → CK2 subunits are nuclear both in glucose and in ethanol growing yeast cells. → CK2 activity is modulated in S. cerevisiae. → CK2 activity is higher in conditions supporting higher growth rates. → V max is higher in faster growing cells, while K m is not affected. -- Abstract: CK2 is a highly conserved protein kinase controlling different cellular processes. It shows a higher activity in proliferating mammalian cells, in various types of cancer cell lines and tumors. The findings presented herein provide the first evidence of an in vivo modulation of CK2 activity, dependent on growth rate, in Saccharomyces cerevisiae. In fact, CK2 activity, assayed on nuclear extracts, is shown to increase in exponential growing batch cultures at faster growth rate, while localization of catalytic and regulatory subunits is not nutritionally modulated. Differences in intracellular CK2 activity of glucose- and ethanol-grown cells appear to depend on both increase in molecule number and k cat . Also in chemostat cultures nuclear CK2 activity is higher in faster growing cells providing the first unequivocal demonstration that growth rate itself can affect CK2 activity in a eukaryotic organism.

  18. Tax Rates, Tax Evasion, and Growth in a Multi-period Economy

    OpenAIRE

    Jordi Caballé; Judith Panadés

    2007-01-01

    We extend the basic tax evasion model to a multi-period economy exhibiting sustained growth. When individuals conceal part of their true income from the tax authority, they face the risk of being audited and hence of paying the corresponding fine. Both taxes and fines determine individual saving and the rate of capital accumulation. We show that, if the penalty imposed on tax evaders is proportional to the amount of evaded taxes, then the growth rate is decreasing in the tax rate. However, th...

  19. [Growth rate and bone maturation in celiac disease (author's transl)].

    Science.gov (United States)

    Martínez Sopena, M J; Calvo Romero, M C; Bedate Calderón, P; Alonso Franch, M; Sánchez Villares, E

    1978-05-01

    The growth and bone maturation of 43 celiac patients were analyzed. A significant correlation between gluten intake and growth rate was found. The authors suggest this is a good parameter to advise the best moment to make the control biopsie and the provocation test.

  20. Growth, exchange rates and trade in Brazil: a structuralist post-Keynesian approach

    Directory of Open Access Journals (Sweden)

    Nelson H. Barbosa Filho

    2004-01-01

    Full Text Available This paper presents a structuralist post-Keynesian analysis of trade adjustment in Brazil. Based on the concept of the balance-of-payments (BoP constraint on growth, the paper investigates the relationship between income growth and real-exchange-rate devaluation necessary to adjust trade to a foreign-exchange constraint. The main result is that, with price-inelastic and income-elastic imports and based on its trade structure in 2002, Brazil may have to compensate an additional 1% of income growth with approximately 7% of real-exchange-rate devaluation in order to keep its trade balance stable in relation to GDP in the near future. Moreover, the trade parameters of Brazil seem to be unfavorable to growth with stable trade, that is, even moderate rates of GDP expansion lead to a substantial increase of imports and, therefore, require an also substantial devaluation of the real exchange rate to avoid a deterioration of the trade balance.

  1. Growth, exchange rates and trade in Brazil: a structuralist post Keynesian approach

    Directory of Open Access Journals (Sweden)

    Nelson H. Barbosa Filho

    2009-06-01

    Full Text Available This paper presents a structuralist post-Keynesian analysis of trade adjustment in Brazil. Based on the concept of the balance-of-payments (BoP constraint on growth, the paper investigates the relationship between income growth and real-exchange-rate devaluation necessary to adjust trade to a foreign-exchange constraint. The main result is that, with price-inelastic and income-elastic imports and based on its trade structure in 2002, Brazil may have to compensate an additional 1% of income growth with approximately 7% of real-exchange-rate devaluation in order to keep its trade balance stable in relation to GDP in the near future. Moreover, the trade parameters of Brazil seem to be unfavorable to growth with stable trade, that is, even moderate rates of GDP expansion lead to a substantial increase of imports and, therefore, require an also substantial devaluation of the real exchange rate to avoid a deterioration of the trade balance.

  2. A Minimalistic Resource Allocation Model to Explain Ubiquitous Increase in Protein Expression with Growth Rate.

    Directory of Open Access Journals (Sweden)

    Uri Barenholz

    Full Text Available Most proteins show changes in level across growth conditions. Many of these changes seem to be coordinated with the specific growth rate rather than the growth environment or the protein function. Although cellular growth rates, gene expression levels and gene regulation have been at the center of biological research for decades, there are only a few models giving a base line prediction of the dependence of the proteome fraction occupied by a gene with the specific growth rate. We present a simple model that predicts a widely coordinated increase in the fraction of many proteins out of the proteome, proportionally with the growth rate. The model reveals how passive redistribution of resources, due to active regulation of only a few proteins, can have proteome wide effects that are quantitatively predictable. Our model provides a potential explanation for why and how such a coordinated response of a large fraction of the proteome to the specific growth rate arises under different environmental conditions. The simplicity of our model can also be useful by serving as a baseline null hypothesis in the search for active regulation. We exemplify the usage of the model by analyzing the relationship between growth rate and proteome composition for the model microorganism E.coli as reflected in recent proteomics data sets spanning various growth conditions. We find that the fraction out of the proteome of a large number of proteins, and from different cellular processes, increases proportionally with the growth rate. Notably, ribosomal proteins, which have been previously reported to increase in fraction with growth rate, are only a small part of this group of proteins. We suggest that, although the fractions of many proteins change with the growth rate, such changes may be partially driven by a global effect, not necessarily requiring specific cellular control mechanisms.

  3. Automatic delamination defect detection in radiographic sequence of rocket boosters

    International Nuclear Information System (INIS)

    Rebuffel, V.; Pires, S.; Caplier, A.; Lamarque, P.

    2003-01-01

    Solid rocket motors are routinely examined in real-time X-ray radioscopic mode. The large and cylindrical boosters are rotating between a high energy source and a two dimensional detector. The purpose of this control is to detect possible defects all through the sample. In the tangential configuration, the part of the object that intersects the X-rays beam is the peripheral one, allowing to detect the delamination defect between the propellant and the external metal envelope. But the defect detectability is very poor due to the strong attenuation of the X-rays through the motors. During the rotation of the booster, the system acquires a sequence of radiographs where the defects are visible over several successive instants. We have previously developed a real-time tomo-synthesis system, processing the radiographs on line, and based on a tomo-synthesis reconstruction algorithm in order to improve the signal-to-noise ratio. This system is installed at the industrial site of Kourou, and is currently used by the operators in charge of the visual inspection of the boosters. In this paper, we present a method that processes the digital images obtained by the system in the purpose of automatically extracting the delamination defects. Due to the size and the poor contrast of the defects, a single image is not sufficient to perform this detection. A spatio-temporal aspect is required for the algorithm to be robust and efficient. In a first step, the proposed method computes the apparent local displacement between the current radiograph and a reference one. This reference image is acquired at the beginning of the rotation, with few noise, and is supposed to be defect free. The apparent displacement is due to the non-perfect rotation positioning. It may be uniform or not, depending on the deformation of the insulation liner of the metallic wall. The images are then registered and compared. On the resulting difference image we apply a smoothed threshold to obtain an

  4. Characterization of the adhesion of thin film by Cross-Sectional Nanoindentation. Analysis of the substrate edge chipping and the film delamination

    Science.gov (United States)

    Felder, Eric; Roy, Sébastien; Darque-Ceretti, Evelyne

    2011-07-01

    Cross-Sectional Nanoindentation (CSN) is a recent method for adhesion measurement of nanoscale thin films in Ultra-Large Scale Integrated circuits. In the case of ductile thin films, the motion of the substrate chip implies significant plastic deformation of the film and complex geometry of delaminated areas. This article recalls first the experimental procedure and the two main features observed in this test performed on various plane copper films deposited on silicon: the critical force producing silicon edge chipping increases linearly with the distance of the indenter to the interface; on the section the delaminated length of the film ( a-b) is proportional to the residual silicon chip displacement u and the ratio S=u/(a-b) depends on the manufacturing process of the film, and is so related to its adhesion to the substrate. One proposes a simple analysis of the silicon edge chipping. Then a model of pull-off of an elastic-strain hardening plastic film is developed, which suggests an explanation for the delamination process. Application of the model to experimental results starting from films plastic properties deduced from nanoindentation measurements provides plausible results. Some improvements for performing the CSN test are proposed in order to make easier its interpretation.

  5. Evaluation of Mycelium Growth Rate and Yield of White Button Mushroom Isolates (Agaricus bisporus in Iran

    Directory of Open Access Journals (Sweden)

    Mohammad Javad Ahmadi Lahijani

    2017-10-01

    Full Text Available Introduction: Among edible mushrooms, white button mushroom is the most cultivated one around the world. Mono-spores diversity in terms of growth rate, colony type, yield and etc. is used for intra strain genetic improvement. High yielding isolates with filamentous mycelium type are screened and used for spawn production (Farsi and Gordan, 2002. Success in mushroom production largely depends on the quality of spawn produced in sterile conditions (Sanchez, 2010. Farsi and Gordan, (2004 reported that colony shape and mycelium growth type are very important factors in screening isolates in terms of mycelium growth rate and yield. To screen isolates based on their mycelium growth, solid media are among the most suitable ones (Griffin, 1994. In a study conducted to evaluate mycelium growth rate of six Morchella species on different media, PDA and MEA were known as the best ones (Kalmis and Kalyoncu, 2008. The present study was conducted in order to evaluate mycelium growth rate and yield of white button mushroom isolates in solid medium, spawn and compost media. Materials and methods: Eighteen isolates of white button mushroom were compared on PDA (Potato Dextrose Agar, CYM (Complete Yeast Medium, spawn and compost media based on mycelium growth rate, type and class growth and yield at the mushroom research center of Faculty of Agriculture, Ferdowsi University of Mashhad, in 2014. A piece of mycelium of each isolate was placed in the center of each petri dish and was kept in 23±1°C, and the radial growth rate of mycelium was measured as two perpendicular diameters in three consecutive weeks. Mycelium growth rate on spawn and compost media was measured based on the percentage of surface coverage during the 15 consecutive days. Yield of each isolate was measured by daily harvesting of mushrooms during 35 days of experiment. Analysis of variance and means comparison of the variables were carried out using SAS software. Means analysis was performed

  6. Comparison of histologic healing and biomechanical characteristics between repair techniques for a delaminated rotator cuff tear in rabbits.

    Science.gov (United States)

    Cheon, Sang-Jin; Kim, Jung-Han; Gwak, Heui-Chul; Kim, Chang-Wan; Kim, Jeon-Kyo; Park, Ji-Hwan

    2017-05-01

    The purpose of this study was to compare histologic healing and biomechanical characteristics between 2 repair techniques (layer by layer, repair of each layer to bone separately; and whole layer, repair of each layer to the bone en masse) for delaminated rotator cuff tear. Rabbits were used as subjects and classified into 2 groups: group A, right side, the layer-by-layer repair group; and group B, left side, the whole-layer repair group. Histologic evaluations were done at 3 weeks (n = 7) and 6 weeks (n = 4) after operation. Biomechanical tests to evaluate the tensile property were done at time 0 (n = 5) and 3 weeks (n = 5) after operation. Histologic healing improved in all groups. A smaller cleft was found between layers in group B compared with the cleft in group A at 3 weeks after operation. At time 0, group A showed a higher yield load and ultimate failure load (67 ± 10.5 N and 80 ± 7.8 N, respectively). However, at 3 weeks after operation, group B showed a higher yield load (48 ± 7.6 N). In the delaminated rotator cuff tear model in the rabbit, the whole-layer repair showed a narrow gap between layers and a higher yield load at 3 weeks after operation. Surgical techniques that unite the cleft in a delaminated tear could improve biomechanical strength after operation. Copyright © 2017 Journal of Shoulder and Elbow Surgery Board of Trustees. Published by Elsevier Inc. All rights reserved.

  7. Last Five Years Pakistan Economic Growth Rate GDP And Its Comparison With China India And Bangladesh

    Directory of Open Access Journals (Sweden)

    Abdul Rehman

    2015-01-01

    Full Text Available Abstract This paper formulates and reviews Pakistans last five years economic growth rate and its comparison with the growth rate of China India and Bangladesh. As growth rate the amount of increment of a specific variable has gained within a specific period of time and context. In fact economic growth rate provides general direction and magnitude of growth for overall economy.

  8. Capital accumulation, structural change and real exchange rate in a Keynesian-Structuralist growth model

    Directory of Open Access Journals (Sweden)

    Oreiro José Luis

    2015-01-01

    Full Text Available The aim of this paper is to show at theoretical level that maintaining a competitive real exchange rate positively affects the economic growth of developing countries by means of a Keynesian-Structuralist model that combines elements of Kaleckian growth models with the balance of payments constrained growth models pioneered developed by Thirlwall. In this setting, the level of real exchange rate is capable, due to its effect over capital accumulation, to induce a structural change in the economy, making endogenous income elasticities of exports and imports. For reasonable parameter values it is shown that in steady-state growth there is two long-run equilibrium values for real exchange rate, one that corresponds to an under-valued currency and another that corresponds to an over-valued currency. If monetary authorities run exchange rate policy in order to target a competitive level for real exchange rate, than under-valued equilibrium is stable and the economy will show a high growth rate in the long-run.

  9. Variation in relative growth rate and growth traits in wild and cultivated Capsicum accessions grown under different temperatures

    NARCIS (Netherlands)

    Swart, de E.A.M.; Marcelis, L.F.M.; Voorrips, R.E.

    2006-01-01

    Differences in environmental conditions are known to influence plant growth and growth-related traits. The aim of this study was to identify the variation in relative growth rate (RGR), and its underlying physiological and morphological traits, in a group of ten wild and cultivated Capsicum

  10. Coral growth rates revisited after 31 years: what is causing lower extension rates in Acropora palmata?

    NARCIS (Netherlands)

    Bak, R.P.M.; Nieuwland, G.; Meesters, H.W.G.

    2009-01-01

    Linear extension of branches in the same Acropora palmata (Lamarck, 1816) population in Curaçao was measured, employing exactly the same methods, in 1971-1973 and in 2002-2004, and the resulting coral growth rates are compared. Linear growth shows the same pattern over seasons in both periods with

  11. Optimal tax rate and economic growth. Evidence from Nigeria and South Africa

    Directory of Open Access Journals (Sweden)

    Olufemi Muibi SAIBU

    2015-05-01

    Full Text Available The recent economic crisis had made developing countries to look inward for financial resources to finance development. The readily alternative is the tax revenues however, the possible adverse direct and indirect effects of tax on productivity and work efforts as well as on aggregate consumption had make some African countries (especially Nigeria and South Africa reluctant in implementing far reaching tax policy reform. This paper examines optimal tax burden and real output growth Nigeria and South Africa, two of the top four economies in Africa. The paper empirically determined what should be the optimal tax rate for Nigeria and South Africa-the two leading economies in Africa. The paper found that nonlinearity hypothesis in the effects of tax in the case of South Africa is rejected while a significant nonlinear relationship is found in the case of Nigeria. The results suggest that the growth-maximizing tax rate is about 15% of per capita GDP for South Africa and 30% for Nigeria. At that tax rate, the economic growth rate would be around 6% and 8% instead of the actual mean growth rate of 2.84% and 4.51% for South Africa and Nigeria respectively. The paper concluded the current tax burden in the two countries may be sub-optimal and may hurt long term sustainable growth process in the two countries

  12. The evaluation system of city's smart growth success rates

    Science.gov (United States)

    Huang, Yifan

    2018-04-01

    "Smart growth" is to pursue the best integrated perform+-ance of the Economically prosperous, socially Equitable, and Environmentally Sustainable(3E). Firstly, we establish the smart growth evaluation system(SGI) and the sustainable development evaluation system(SDI). Based on the ten principles and the definition of three E's of sustainability. B y using the Z-score method and the principal component analysis method, we evaluate and quantify indexes synthetically. Then we define the success of smart growth as the ratio of the SDI to the SGI composite score growth rate (SSG). After that we select two cities — Canberra and Durres as the objects of our model in view of the model. Based on the development plans and key data of these two cities, we can figure out the success of smart growth. And according to our model, we adjust some of the growth indicators for both cities. Then observe the results before and after adjustment, and finally verify the accuracy of the model.

  13. Growth-rate regulated genes have profound impact on interpretation of transcriptome profiling in Saccharomyces cerevisiae

    DEFF Research Database (Denmark)

    Regenberg, Birgitte; Grotkjær, Thomas; Winther, Ole

    2006-01-01

    Growth rate is central to the development of cells in all organisms. However, little is known about the impact of changing growth rates. We used continuous cultures to control growth rate and studied the transcriptional program of the model eukaryote Saccharomyces cerevisiae, with generation time...

  14. Growth Rates and Mechanisms of Magmatic Orbicule Formation: Insights from Calcium Isotopes

    Science.gov (United States)

    Antonelli, M. A.; Watkins, J. M.; DePaolo, D. J.

    2017-12-01

    Orbicular diorites and granites are rare plutonic rock textures that remain enigmatic despite a century of study. Orbicules consist of a rounded core (xenolith, xenocryst, or autolith) surrounded by a variable number of concentric rings defined by different modal mineralogies and textures. Recent work suggests that the alternating layers of mineral growth are a consequence of either changes in external conditions of the magma (e.g. temperature, magma composition due to mixing, changes in volatile abundances), or rapid growth of one mineral phase (e.g plagioclase) creating a depleted boundary layer that then promotes precipitation of an alternative mineral phase (e.g. pyroxene). This process can be repeated to produce multiple layers. The rates at which orbicules grow is also of interest and relates to the mechanisms. Studies of orbicular diorites from the northern Sierra Nevada suggest exceptionally high growth rates (McCarthy et al., 2016). Ca isotopes can offer a unique perspective on orbicule formation, as diffusive isotope fractionation should be substantial when growth rates are high, and they are also sensitive to the nature of the growth medium (silicate liquid or supercritical fluid phase). We present δ44Ca measurements and chemistry for a transect of a dioritic orbicule collected from Emerald Lake, California (Sierra Nevada), where the growth layers are defined by variations in plagioclase/pyroxene ratio, grain size, and texture. Ca concentration varies from 5-13 wt%, and d44Ca values oscillate between -0.5 to 0.0‰ relative to BSE, correlating with changes in mineralogy and texture. Zones of plagioclase comb texture are associated with negative δ44Ca excursions of -0.2 to -0.4‰, consistent with diffusive isotope fractionation during rapid mineral growth. Assuming a 10‰ difference in diffusivity for 44Ca vs. 40Ca in dioritic liquids (Watson et al., 2016), and using the models of Watson and Muller (2009) as a guide, these small fractionations

  15. Growth rate distribution in the forming lateral root of arabidopsis.

    Science.gov (United States)

    Szymanowska-Pułka, Joanna; Lipowczan, Marcin

    2014-10-01

    Microscopic observations of lateral roots (LRs) in Arabidopsis thaliana reveal that the cross-sectional shape of the organ changes from its basal to its apical region. The founder cells for LRs are elongated along the parent root axis, and thus from the site of initiation the base of LRs resemble an ellipse. The circumference of the apical part of LRs is usually a circle. The objective of this study was to analyse the characteristics of changes in the growth field of LRs possessing various shapes in their basal regions. The LRs of the wild type (Col-0) and two transgenic arabidopsis lines were analysed. On the basis of measurements of the long and short diameters (DL and DS, respectively) of the ellipse-like figure representing the bases of particular LRs, their asymmetry ratios (DL/DS) were determined. Possible differences between accessions were analysed by applying statistical methods. No significant differences between accessions were detected. Comparisons were therefore made of the maximal, minimal and mean value of the ratio of all the LRs analysed. Taking into consideration the lack of circular symmetry of the basal part, rates of growth were determined at selected points on the surface of LRs by the application of the growth tensor method, a mathematical tool previously applied only to describe organs with rotational symmetry. Maps showing the distribution of growth rates were developed for surfaces of LRs of various asymmetry ratios. The maps of growth rates on the surfaces of LRs having various shapes of the basal part show differences in both the geometry and the manner of growth, thus indicating that the manner of growth of the LR primordium is correlated to its shape. This is the first report of a description of growth of an asymmetric plant organ using the growth tensor method. The mathematical modelling adopted in the study provides new insights into plant organ formation and shape. © The Author 2014. Published by Oxford University Press on

  16. Wavelength dependence of the linear growth rate of the Es layer instability

    Directory of Open Access Journals (Sweden)

    R. B. Cosgrove

    2007-06-01

    Full Text Available It has recently been shown, by computation of the linear growth rate, that midlatitude sporadic-E (Es layers are subject to a large scale electrodynamic instability. This instability is a logical candidate to explain certain frontal structuring events, and polarization electric fields, which have been observed in Es layers by ionosondes, by coherent scatter radars, and by rockets. However, the original growth rate derivation assumed an infinitely thin Es layer, and therefore did not address the short wavelength cutoff. Also, the same derivation ignored the effects of F region loading, which is a significant wavelength dependent effect. Herein is given a generalized derivation that remedies both these short comings, and thereby allows a computation of the wavelength dependence of the linear growth rate, as well as computations of various threshold conditions. The wavelength dependence of the linear growth rate is compared with observed periodicities, and the role of the zeroth order meridional wind is explored. A three-dimensional paper model is used to explain the instability geometry, which has been defined formally in previous works.

  17. Slow growth rates of Amazonian trees: Consequences for carbon cycling

    Science.gov (United States)

    Vieira, Simone; Trumbore, Susan; Camargo, Plinio B.; Selhorst, Diogo; Chambers, Jeffrey Q.; Higuchi, Niro; Martinelli, Luiz Antonio

    2005-01-01

    Quantifying age structure and tree growth rate of Amazonian forests is essential for understanding their role in the carbon cycle. Here, we use radiocarbon dating and direct measurement of diameter increment to document unexpectedly slow growth rates for trees from three locations spanning the Brazilian Amazon basin. Central Amazon trees, averaging only ≈1mm/year diameter increment, grow half as fast as those from areas with more seasonal rainfall to the east and west. Slow growth rates mean that trees can attain great ages; across our sites we estimate 17-50% of trees with diameter >10 cm have ages exceeding 300 years. Whereas a few emergent trees that make up a large portion of the biomass grow faster, small trees that are more abundant grow slowly and attain ages of hundreds of years. The mean age of carbon in living trees (60-110 years) is within the range of or slightly longer than the mean residence time calculated from C inventory divided by annual C allocation to wood growth (40-100 years). Faster C turnover is observed in stands with overall higher rates of diameter increment and a larger fraction of the biomass in large, fast-growing trees. As a consequence, forests can recover biomass relatively quickly after disturbance, whereas recovering species composition may take many centuries. Carbon cycle models that apply a single turnover time for carbon in forest biomass do not account for variations in life strategy and therefore may overestimate the carbon sequestration potential of Amazon forests. PMID:16339903

  18. Stress corrosion crack growth rate in dissimilar metal welds

    International Nuclear Information System (INIS)

    Fernandez, M. P.; Lapena, J.; Lancha, A. M.; Perosanz, F. J.; Navas, M.

    2000-01-01

    Dissimilar welds, used to join different sections in light water reactors, are potentially susceptible to stress corrosion cracking (SCC) in aqueous mediums characteristic of nuclear plants. However, the study of these The ma has been limited to evaluating the weld material susceptibility in these mediums. Little scarce data are available on crack growth rates due, fundamentally, to inadequate testing techniques. In order to address this lack of information the crack growth rate at the interface of ferritic SA 533 B-1 alloy and alloy I-82, in a dissimilar weld (SA533B-1/I-82/316L), was studied. Experiments were conducted in water at 288 degree centigrade, 8 ppm of O 2 and 1 μS/cm conductivity. (Author) 33 refs

  19. Growth rate effects on the formation of dislocation loops around deep helium bubbles in Tungsten

    International Nuclear Information System (INIS)

    Sandoval, Luis; Perez, Danny; Uberuaga, Blas P.; Voter, Arthur Ford

    2016-01-01

    Here, the growth process of spherical helium bubbles located 6 nm below a (100) surface is studied using molecular dynamics and parallel replica dynamics simulations, over growth rates from 10"6 to 10"1"2 helium atoms per second. Slower growth rates lead to a release of pressure and lower helium content as compared with fast growth cases. In addition, at slower growth rates, helium bubbles are not decorated by multiple dislocation loops, as these tend to merge or emit given sufficient time. At faster rates, dislocation loops nucleate faster than they can emit, leading to a more complicated dislocation structure around the bubble.

  20. Growth rates of important East African montane forest trees, with ...

    African Journals Online (AJOL)

    These trees showed growth rates at least twice as high as those of the primary species. Juniperus procera was found to be the fastest growing species in the cedar forest, underlining its success in forming dense stands after a fire. Only young Podocarpus latifolius showed a similar fast growth. Olea europaea ssp. cuspidata, ...

  1. SCC crack growth rate of cold worked 316L stainless steel in PWR environment

    Science.gov (United States)

    Du, Donghai; Chen, Kai; Yu, Lun; lu, Hui; Zhang, Lefu; Shi, Xiuqiang; Xu, Xuelian

    2015-01-01

    Many component failures in nuclear power plants were found to be caused by stress corrosion cracking (SCC) of cold worked austenitic steels. Some of the pressure boundary component materials are even cold worked up to 35% plastic deformation, leaving high residual stress and inducing high growth rate of corrosion crack. Controlling water chemistry is one of the best counter measure to mitigate this problem. In this work, the effects of temperature (200 up to 325 °C) and dissolved oxygen (0 up to 2000 μg/L) on SCC crack growth rates of cold worked austenitic stainless steel type 316L have been tested by using direct current potential drop (DCPD) method. The results showed that temperature affected SCC crack growth rates more significantly in oxygenated water than in deaerated water. In argon deaerated water, the crack growth rate exhibited a peak at about 250 °C, which needs further verification. At 325 °C, the SCC crack growth rate increased rapidly with the increase of dissolved oxygen concentration within the range from 0 up to 200 μg/L, while when dissolved oxygen was above 200 μg/L, the crack growth rate followed a shallower dependence on dissolved oxygen concentration.

  2. Sex-based differences in Adelie penguin (Pygoscelis adeliae) chick growth rates.

    Science.gov (United States)

    Jennings, Scott; Varsani, Arvind; Dugger, Catherine; Ballard, Grant; Ainley, David G.

    2016-01-01

    Sexually size-dimorphic species must show some difference between the sexes in growth rate and/or length of growing period. Such differences in growth parameters can cause the sexes to be impacted by environmental variability in different ways, and understanding these differences allows a better understanding of patterns in productivity between individuals and populations. We investigated differences in growth rate and diet between male and female Adélie Penguin (Pygoscelis adeliae) chicks during two breeding seasons at Cape Crozier, Ross Island, Antarctica. Adélie Penguins are a slightly dimorphic species, with adult males averaging larger than adult females in mass (~11%) as well as bill (~8%) and flipper length (~3%). We measured mass and length of flipper, bill, tibiotarsus, and foot at 5-day intervals for 45 male and 40 female individually-marked chicks. Chick sex was molecularly determined from feathers. We used linear mixed effects models to estimate daily growth rate as a function of chick sex, while controlling for hatching order, brood size, year, and potential variation in breeding quality between pairs of parents. Accounting for season and hatching order, male chicks gained mass an average of 15.6 g d-1 faster than females. Similarly, growth in bill length was faster for males, and the calculated bill size difference at fledging was similar to that observed in adults. There was no evidence for sex-based differences in growth of other morphological features. Adélie diet at Ross Island is composed almost entirely of two species—one krill (Euphausia crystallorophias) and one fish (Pleuragramma antarctica), with fish having a higher caloric value. Using isotopic analyses of feather samples, we also determined that male chicks were fed a higher proportion of fish than female chicks. The related differences in provisioning and growth rates of male and female offspring provides a greater understanding of the ways in which ecological factors may impact

  3. Age, growth rate, and otolith growth of polar cod (Boreogadus saida in two fjords of Svalbard, Kongsfjorden and Rijpfjorden

    Directory of Open Access Journals (Sweden)

    Dariusz P. Fey

    2017-10-01

    Full Text Available This work presents biological information for polar cod (Boreogadus saida collected with a Campelen 1800 shrimp bottom trawl in Kongsfjorden (two stations located in the inner part of the fjord adjacent to the glacier and Rijpfjorden (one station at the entrance to the fjord in September and October 2013. The otolith-based ages of polar cod collected in Kongsfjorden (6.1–24 cm total length TL; n = 813 ranged from 0 to 4 years. The growth rate was relatively constant at approximately 4.7 cm year−1 between years 1 and 4, which indicates that growth was fast in the glacier area. The ages of polar cod collected in Rijpfjorden (8.6–15.9 cm TL; n = 64 ranged from 2 to 3 years. The fish from Rijpfjorden were smaller at age than those from Kongsfjorden, and their growth rate between years 2 and 3 (no other age classes were available was approximately 3.3 cm year−1. In both fjords, males and females were of the same size-at-age and the same weight-at-TL. The small sampling area means that the results on growth rate are not representative of the entire fjords. Instead, the results can be discussed as presenting the possible growth rates of some populations. A strong relationship was identified between otolith size (length and weight and fish size (TL and TW, with no differences between males and females or the fjords. A significant, strong relationship was also noted between fish and otolith growth rates.

  4. The ‘Sticky Elastica’: delamination blisters beyond small deformations

    KAUST Repository

    Wagner, Till J. W.

    2013-01-01

    We consider the form of an elastic loop adhered to a rigid substrate: the \\'Sticky Elastica\\'. In contrast to previous studies of the shape of delamination \\'blisters\\', the theory developed accounts for deflections with large slope (i.e. geometrically nonlinear). Starting from the classical Euler Elastica we provide numerical results for the dimensions of such blisters for a variety of end-end confinements and develop asymptotic expressions that reproduce these results well, even up to the point of self-contact. Interestingly, we find that the width of such blisters does not grow monotonically with increased confinement. Our theoretical predictions are confirmed by simple desktop experiments and suggest a new method for the measurement of the elastocapillary length for deformations that cannot be considered small. We discuss the implications of our results for applications such as flexible electronics. © 2013 The Royal Society of Chemistry.

  5. Effect of diffusion from a lateral surface on the rate of GaN nanowire growth

    International Nuclear Information System (INIS)

    Sibirev, N. V.; Tchernycheva, M.; Cirlin, G. E.; Patriarche, G.; Harmand, J. C.; Dubrovskii, V. G.

    2012-01-01

    The kinetics of the growth of GaN crystalline nanowires on a Si (111) surface with no catalyst is studied experimentally and theoretically. Noncatalytic GaN nanowires were grown by molecular-beam epitaxy with AlN inserts, which makes it possible to determine the rate of the vertical growth of nanowires. A model for the formation of GaN nanowires is developed, and an expression for their rate of growth is derived. It is shown that, in the general case, the dependence of the rate of growth on the nanowire diameter has a minimum. The diameter corresponding to the experimentally observed minimum of the rate of growth steadily increases with increasing diffusion flux from the lateral surface.

  6. Mechanisms promoting higher growth rate in arctic than in temperate shorebirds

    NARCIS (Netherlands)

    Schekkerman, H.; Tulp, I.Y.M.; Piersma, T.; Visser, G.H.

    2003-01-01

    We compared prefledging growth, energy expenditure, and time budgets in the arctic-breeding red knot (Calidris canutus) to those in temperate shorebirds, to investigate how arctic chicks achieve a high growth rate despite energetic difficulties associated with precocial development in a cold

  7. Mechanisms promoting higher growth rate in arctic than in temperate shorebirds

    NARCIS (Netherlands)

    Schekkerman, H; Tulp, Ingrid; Piersma, T.; Visser, G.H.

    We compared prefledging growth, energy expenditure, and time budgets in the arctic-breeding red knot (Calidris canutus) to those in temperate shorebirds, to investigate how arctic chicks achieve a high growth rate despite energetic difficulties associated with precocial development in a cold

  8. Ecological regime shift drives declining growth rates of sea turtles throughout the West Atlantic

    Science.gov (United States)

    Bjorndal, Karen A.; Bolten, Alan B.; Chaloupka, Milani; Saba, Vincent S.; Bellini, Cláudio; Marcovaldi, Maria A.G.; Santos, Armando J.B.; Bortolon, Luis Felipe Wurdig; Meylan, Anne B.; Meylan, Peter A.; Gray, Jennifer; Hardy, Robert; Brost, Beth; Bresette, Michael; Gorham, Jonathan C.; Connett, Stephen; Crouchley, Barbara Van Sciver; Dawson, Mike; Hayes, Deborah; Diez, Carlos E.; van Dam, Robert P.; Willis, Sue; Nava, Mabel; Hart, Kristen M.; Cherkiss, Michael S.; Crowder, Andrew; Pollock, Clayton; Hillis-Starr, Zandy; Muñoz Tenería, Fernando A.; Herrera-Pavón, Roberto; Labrada-Martagón, Vanessa; Lorences, Armando; Negrete-Philippe, Ana; Lamont, Margaret M.; Foley, Allen M.; Bailey, Rhonda; Carthy, Raymond R.; Scarpino, Russell; McMichael, Erin; Provancha, Jane A.; Brooks, Annabelle; Jardim, Adriana; López-Mendilaharsu, Milagros; González-Paredes, Daniel; Estrades, Andrés; Fallabrino, Alejandro; Martínez-Souza, Gustavo; Vélez-Rubio, Gabriela M.; Boulon, Ralf H.; Collazo, Jaime; Wershoven, Robert; Hernández, Vicente Guzmán; Stringell, Thomas B.; Sanghera, Amdeep; Richardson, Peter B.; Broderick, Annette C.; Phillips, Quinton; Calosso, Marta C.; Claydon, John A.B.; Metz, Tasha L.; Gordon, Amanda L.; Landry, Andre M.; Shaver, Donna J.; Blumenthal, Janice; Collyer, Lucy; Godley, Brendan J.; McGowan, Andrew; Witt, Matthew J.; Campbell, Cathi L.; Lagueux, Cynthia J.; Bethel, Thomas L.; Kenyon, Lory

    2017-01-01

    Somatic growth is an integrated, individual-based response to environmental conditions, especially in ectotherms. Growth dynamics of large, mobile animals are particularly useful as bio-indicators of environmental change at regional scales. We assembled growth rate data from throughout the West Atlantic for green turtles, Chelonia mydas, which are long-lived, highly migratory, primarily herbivorous mega-consumers that may migrate over hundreds to thousands of kilometers. Our dataset, the largest ever compiled for sea turtles, has 9690 growth increments from 30 sites from Bermuda to Uruguay from 1973 to 2015. Using generalized additive mixed models, we evaluated covariates that could affect growth rates; body size, diet, and year have significant effects on growth. Growth increases in early years until 1999, then declines by 26% to 2015. The temporal (year) effect is of particular interest because two carnivorous species of sea turtles – hawksbills, Eretmochelys imbricata, and loggerheads, Caretta caretta – exhibited similar significant declines in growth rates starting in 1997 in the West Atlantic, based on previous studies. These synchronous declines in productivity among three sea turtle species across a trophic spectrum provide strong evidence that an ecological regime shift (ERS) in the Atlantic is driving growth dynamics. The ERS resulted from a synergy of the 1997/1998 El Niño Southern Oscillation (ENSO) – the strongest on record – combined with an unprecedented warming rate over the last two to three decades. Further support is provided by the strong correlations between annualized mean growth rates of green turtles and both sea surface temperatures (SST) in the West Atlantic for years of declining growth rates (r = -0.94) and the Multivariate ENSO Index (MEI) for all years (r = 0.74). Granger-causality analysis also supports the latter finding. We discuss multiple stressors that could reinforce and prolong the effect of the ERS. This study

  9. Ecological regime shift drives declining growth rates of sea turtles throughout the West Atlantic.

    Science.gov (United States)

    Bjorndal, Karen A; Bolten, Alan B; Chaloupka, Milani; Saba, Vincent S; Bellini, Cláudio; Marcovaldi, Maria A G; Santos, Armando J B; Bortolon, Luis Felipe Wurdig; Meylan, Anne B; Meylan, Peter A; Gray, Jennifer; Hardy, Robert; Brost, Beth; Bresette, Michael; Gorham, Jonathan C; Connett, Stephen; Crouchley, Barbara Van Sciver; Dawson, Mike; Hayes, Deborah; Diez, Carlos E; van Dam, Robert P; Willis, Sue; Nava, Mabel; Hart, Kristen M; Cherkiss, Michael S; Crowder, Andrew G; Pollock, Clayton; Hillis-Starr, Zandy; Muñoz Tenería, Fernando A; Herrera-Pavón, Roberto; Labrada-Martagón, Vanessa; Lorences, Armando; Negrete-Philippe, Ana; Lamont, Margaret M; Foley, Allen M; Bailey, Rhonda; Carthy, Raymond R; Scarpino, Russell; McMichael, Erin; Provancha, Jane A; Brooks, Annabelle; Jardim, Adriana; López-Mendilaharsu, Milagros; González-Paredes, Daniel; Estrades, Andrés; Fallabrino, Alejandro; Martínez-Souza, Gustavo; Vélez-Rubio, Gabriela M; Boulon, Ralf H; Collazo, Jaime A; Wershoven, Robert; Guzmán Hernández, Vicente; Stringell, Thomas B; Sanghera, Amdeep; Richardson, Peter B; Broderick, Annette C; Phillips, Quinton; Calosso, Marta; Claydon, John A B; Metz, Tasha L; Gordon, Amanda L; Landry, Andre M; Shaver, Donna J; Blumenthal, Janice; Collyer, Lucy; Godley, Brendan J; McGowan, Andrew; Witt, Matthew J; Campbell, Cathi L; Lagueux, Cynthia J; Bethel, Thomas L; Kenyon, Lory

    2017-11-01

    Somatic growth is an integrated, individual-based response to environmental conditions, especially in ectotherms. Growth dynamics of large, mobile animals are particularly useful as bio-indicators of environmental change at regional scales. We assembled growth rate data from throughout the West Atlantic for green turtles, Chelonia mydas, which are long-lived, highly migratory, primarily herbivorous mega-consumers that may migrate over hundreds to thousands of kilometers. Our dataset, the largest ever compiled for sea turtles, has 9690 growth increments from 30 sites from Bermuda to Uruguay from 1973 to 2015. Using generalized additive mixed models, we evaluated covariates that could affect growth rates; body size, diet, and year have significant effects on growth. Growth increases in early years until 1999, then declines by 26% to 2015. The temporal (year) effect is of particular interest because two carnivorous species of sea turtles-hawksbills, Eretmochelys imbricata, and loggerheads, Caretta caretta-exhibited similar significant declines in growth rates starting in 1997 in the West Atlantic, based on previous studies. These synchronous declines in productivity among three sea turtle species across a trophic spectrum provide strong evidence that an ecological regime shift (ERS) in the Atlantic is driving growth dynamics. The ERS resulted from a synergy of the 1997/1998 El Niño Southern Oscillation (ENSO)-the strongest on record-combined with an unprecedented warming rate over the last two to three decades. Further support is provided by the strong correlations between annualized mean growth rates of green turtles and both sea surface temperatures (SST) in the West Atlantic for years of declining growth rates (r = -.94) and the Multivariate ENSO Index (MEI) for all years (r = .74). Granger-causality analysis also supports the latter finding. We discuss multiple stressors that could reinforce and prolong the effect of the ERS. This study demonstrates the

  10. Linear Stability of Binary Alloy Solidification for Unsteady Growth Rates

    Science.gov (United States)

    Mazuruk, K.; Volz, M. P.

    2010-01-01

    An extension of the Mullins and Sekerka (MS) linear stability analysis to the unsteady growth rate case is considered for dilute binary alloys. In particular, the stability of the planar interface during the initial solidification transient is studied in detail numerically. The rapid solidification case, when the system is traversing through the unstable region defined by the MS criterion, has also been treated. It has been observed that the onset of instability is quite accurately defined by the "quasi-stationary MS criterion", when the growth rate and other process parameters are taken as constants at a particular time of the growth process. A singular behavior of the governing equations for the perturbed quantities at the constitutional supercooling demarcation line has been observed. However, when the solidification process, during its transient, crosses this demarcation line, a planar interface is stable according to the linear analysis performed.

  11. Extending the durability of cultivar resistance by limiting epidemic growth rates.

    Science.gov (United States)

    Carolan, Kevin; Helps, Joe; van den Berg, Femke; Bain, Ruairidh; Paveley, Neil; van den Bosch, Frank

    2017-09-27

    Cultivar resistance is an essential part of disease control programmes in many agricultural systems. The use of resistant cultivars applies a selection pressure on pathogen populations for the evolution of virulence, resulting in loss of disease control. Various techniques for the deployment of host resistance genes have been proposed to reduce the selection for virulence, but these are often difficult to apply in practice. We present a general technique to maintain the effectiveness of cultivar resistance. Derived from classical population genetics theory; any factor that reduces the population growth rates of both the virulent and avirulent strains will reduce selection. We model the specific example of fungicide application to reduce the growth rates of virulent and avirulent strains of a pathogen, demonstrating that appropriate use of fungicides reduces selection for virulence, prolonging cultivar resistance. This specific example of chemical control illustrates a general principle for the development of techniques to manage the evolution of virulence by slowing epidemic growth rates. © 2017 The Author(s).

  12. Causality Relationship Between Import, Export and Growth Rate in Developing Countries

    Directory of Open Access Journals (Sweden)

    Serhat YUKSEL

    2017-06-01

    Full Text Available In this paper, we tried to determine the relationship between imports, exports and growth rate in developing countries. Within this scope, 6 developing countries (Argentina, Brazil, China, Malaysia, Mexico and Turkey were analyzed in this study. In order to achieve this purpose, annual data for the periods between 1961 and 2014 was tested by using Engle Granger co-integration analysis, Vector Error Correction Model and Toda Yamamoto causality analysis. According to the result of the analysis, it was determined that there is not any relationship among three variables in Brazil and Mexico. On the other hand, we defined that increase in export causes higher growth rate in Argentina. Moreover, it was concluded that there is a causal relationship from import to export in China and Turkey. Furthermore, it was determined that export causes higher import in Malaysia. Therefore, it can be concluded that the relationship between import, export and growth rate is not same for all developing countries..

  13. Population growth, interest rate, and housing tax in the transitional China

    Science.gov (United States)

    He, Ling-Yun; Wen, Xing-Chun

    2017-03-01

    This paper combines and develops the models in Lastrapes (2002) and Mankiw and Weil (1989), which enables us to analyze the effects of interest rate and population growth shocks on housing price in one integrated framework. Based on this model, we carry out policy simulations to examine whether the housing (stock or flow) tax reduces the housing price fluctuations caused by interest rate or population growth shocks. Simulation results imply that the choice of housing tax tools depends on the kind of shock that housing market faces. In the situation where the housing price volatility is caused by the population growth shock, the flow tax can reduce the volatility of housing price while the stock tax makes no difference to it. If the shock is resulting from the interest rate, the policy maker should not impose any kind of the housing taxes. Furthermore, the effect of one kind of the housing tax can be strengthened by that of the other type of housing tax.

  14. Layered zinc hydroxide salts: Delamination, preferred orientation of hydroxide lamellae, and formation of ZnO nanodiscs

    Czech Academy of Sciences Publication Activity Database

    Demel, Jan; Pleštil, Josef; Bezdička, Petr; Janda, Pavel; Klementová, Mariana; Lang, Kamil

    2011-01-01

    Roč. 360, č. 2 (2011), s. 532-539 ISSN 0021-9797 R&D Projects: GA MŠk ME09058; GA ČR GAP207/10/1447 Institutional research plan: CEZ:AV0Z40320502; CEZ:AV0Z40500505; CEZ:AV0Z40400503 Keywords : layered zinc hydroxide * delamination * exfoliation * hydroxide layer * ZnO Subject RIV: CA - Inorganic Chemistry Impact factor: 3.070, year: 2011

  15. Regeneration and growth rates of allofragments in four common stream plants

    DEFF Research Database (Denmark)

    Riis, Tenna; Madsen, Tom Vindbæk; Sennels, R. S. H.

    2009-01-01

    perfoliatus L. and Ranunculus baudotii x pseudofluitans. The objectives of this study were to determine (1) if shoots with an apical tip have higher regeneration (growth of new shoots and rhizomes from allofragments) and colonisation (root attachment in sediment) abilities and higher relative growth rates...

  16. Growth rates of rhizosphere microorganisms depend on competitive abilities of plants for nitrogen

    Science.gov (United States)

    Blagodatskaya, Evgenia; Littschwager, Johanna; Lauerer, Marianna; Kuzyakov, Yakov

    2010-05-01

    Rhizosphere - one of the most important ‘hot spots' in soil - is characterized not only by accelerated turnover of microbial biomass and nutrients but also by strong intra- and inter-specific competition. Intra-specific competition occurs between individual plants of the same species, while inter-specific competition can occur both at population level (plant species-specific, microbial species-specific interactions) and at community level (plant - microbial interactions). Such plant - microbial interactions are mainly governed by competition for available N sources, since N is one of the main growth limiting nutrients in natural ecosystems. Functional structure and activity of microbial community in rhizosphere is not uniform and is dependent on quantity and quality of root exudates which are plant specific. It is still unclear how microbial growth and turnover in the rhizosphere are dependent on the features and competitive abilities of plants for N. Depending on C and N availability, acceleration and even retardation of microbial activity and carbon mineralization can be expected in the rhizosphere of plants with high competitive abilities for N. We hypothesized slower microbial growth rates in the rhizosphere of plants with smaller roots, as they usually produce less exudates compared to plants with small shoot-to-root ratio. As the first hypothesis is based solely on C availability, we also expected the greater effect of N availability on microbial growth in rhizosphere of plants with smaller root mass. These hypothesis were tested for two plant species of strawberry: Fragaria vesca L. (native species), and Duchesnea indica (Andrews) Focke (an invasive plant in central Europe) growing in intraspecific and interspecific competition. Microbial biomass and the kinetic parameters of microbial growth in the rhizosphere were estimated by dynamics of CO2 emission from the soil amended with glucose and nutrients. Specific growth rate (µ) of soil microorganisms was

  17. Influence of temperature on growth rate and lag phase of fungi isolated from Argentine corn.

    Science.gov (United States)

    González, H H; Resnik, S L; Vaamonde, G

    1988-03-01

    The influence of temperature on the growth of nine strains of fungi belonging to the genera Eurotium, Aspergillus, Penicillium and Fusarium has been investigated for the temperature range 15-35 degrees C. The lag phase and the growth rate were evaluated by using a laboratory medium. The maximum growth rate for E. repens, A. wentii and P. chrysogenum was observed at about 25 degrees C, for P. citrinum near 30 degrees C and for F. semitectum and F. moniliforme between 20 and 25 degrees C. The growth rate of A. niger, A. flavus and A. parasiticus increased with increasing temperatures in the range studied. For all strains studied it appeared that the higher the growth rate the lower the lag phase was.

  18. The Effect of Veneer Layers on the Bending Shear Strength and Delamination of Laminated Veneer Lumber (LVL) from Oil Palm Trunk (OPT)

    Science.gov (United States)

    Jamaludin, M. A.; Nordin, K.; Bahari, S. A.; Ahmad, M.

    2010-03-01

    The aim of this study was to evaluate the effects of the number of veneer layers on the bending shear strength and delamination of Laminated Veneer Lumber (LVL) from oil palm trunk (OPT). Five (5), Six (6) and Seven (7) veneer layers of OPT LVL were manufactured. The dimension of the boards was 45 cm by 45 cm by 1.9 cm. The boards were hot pressed for 13 minutes at a pressure of 31 kgf per m2. Urea formaldehyde (UF) supplied by a local adhesive manufacturer was used as the binder for the boards. The bending shear tests consisted of the edgewise and flatwise tests, whereas the delamination test consisted of the cold and hot water boil tests. The preparation of the test specimens and tests set-up was in accordance to the Japanese Standards, JAS-1991 [1]. Six replications were used for each test. The results were analyzed by Analysis of Variance (ANOVA) using the Duncan's Multiple Range Test to test for significant differences. The results indicated that as the number of layers increased the strength also increased. All the boards passed the standard. The difference in strength between the different types of samples was significant at 95 percent confidence level. Bending shear failures were primarily in the veneers. It is possible to use the boards as light weight interior building and furniture components. Over the years, the supply of quality timber resources from the natural forest has decrease as the wood-based industry experienced rapid growth. The supply of rubberwood for the furniture industry is also decreasing as a result of increase latex price. Accordingly, OPT LVL can be an alternative or supplementary raw material for the wood-based industry.

  19. The effect of salinity on growth rate and osmolyte concentration of ...

    African Journals Online (AJOL)

    Although at a slower rate, growth is maintained in seawater cultures supplemented with nutrients. Differences were found in carbohydrate content between cultures in different growth media. The highest carbohydrate content was observed in cultures growing in Zarrouk medium supplemented with 4 NaCl and in seawater ...

  20. Comparison of cyanobacterial and green algal growth rates at different temperatures

    NARCIS (Netherlands)

    Lurling, M.; Faassen, E.J.; Kosten, S.; Eshetu, Z.; Huszar, V.M.

    2013-01-01

    1.The hypothesis that cyanobacteria have higher optimum growth temperatures and higher growth rates at the optimum as compared to chlorophytes was tested by running a controlled experiment with eight cyanobacteria species and eight chlorophyte species at six different temperatures (20-35°C) and by

  1. Measurement of fatigue crack growth rate of reactor structural material in air based on DCPD method

    International Nuclear Information System (INIS)

    Du Donghai; Chen Kai; Yu Lun; Zhang Lefu; Shi Xiuqiang; Xu Xuelian

    2014-01-01

    The principles and details of direct current potential drop (DCPD) in monitoring the crack growth of reactor structural materials was introduced in this paper. Based on this method, the fatigue crack growth rate (CGR) of typical structural materials in nuclear power systems was measured. The effects of applied load, load ratio and loading frequency on the fatigue crack growth rate of reactor structural materials were discussed. The result shows that the fatigue crack growth rate of reactor structural materials depends on the hardness of materials, and the harder the material is, the higher the rate of crack growth is. (authors)

  2. Volume doubling time and growth rate of renal cell carcinoma determined by helical CT: a single-institution experience

    International Nuclear Information System (INIS)

    Lee, Ji Young; Kim, Chan Kyo; Choi, Dongil; Park, Byung Kwan

    2008-01-01

    The purpose of this study was to retrospectively evaluate the volume doubling time (VDT) and growth rate of renal cell carcinomas (RCC) on a serial computed tomography (CT) scan. Thirty pathologically proven RCCs were reviewed with helical CT. Each tumor underwent at least two CT scans. Tumor volume was determined using an area measuring tool and the summation-of-areas technique. Growth rate was evaluated in terms of diameter and volume changes. VDT and volume growth rate were compared in relation to several factors (initial diameter, initial volume, diameter growth rate, volume growth rate, tumor grade, tumor subtype, sex or age). Mean VDT of RCCs was 505 days. Mean diameter and volume growth rate were 0.59 cm/year and 19.1 cm 3 /year, respectively. For volume and diameter growth rate, tumors ≤4 cm showed lower rates than those >4 cm (P 0.05). Volume growth rate was moderately to strongly positively correlated with initial diameter, initial volume and diameter growth rate (P < 0.05). In conclusion, small RCCs grew at a slow rate both diametrically and volumetrically. More accurate assessment of tumor growth rate and VDT may be helpful to understand the natural history of RCC. (orig.)

  3. Exchange-Driven Growth with Birth Rate Less Than Death

    International Nuclear Information System (INIS)

    Lin Zhenquan; Ye Gaoxiang; Ke Jianhong

    2005-01-01

    We further study the kinetic behavior of the exchange-driven growth with birth and death for the case of birth rate kernel being less than that of death based on the mean-field theory. The symmetric exchange rate kernel is K(k,j) = K'(k,j) = Ikj υ , and the birth and death rates are proportional to the aggregate's size. The long time asymptotic behavior of the aggregate size distribution a k (t) is found to obey a much unusual scaling law with an exponentially growing scaling function Φ(x) = exp (x).

  4. The Effect of Growth Temperature and V/III Flux Ratio of MOCVD Antimony Based Semiconductors on Growth Rate and Surface Morphology

    Directory of Open Access Journals (Sweden)

    Ramelan Ari Handono

    2017-01-01

    Full Text Available Epitaxial Alx Ga1-x Sb layers on GaSb and GaAs substrates have been grown by atmospheric pressure metalorganic chemical vapor deposition using TMAl, TMGa and TMSb. Nomarski microscope and a profiler were employed to examine the surface morphology and growth rate of the samples. We report the effect of growth temperature and V/III flux ratio on growth rate and surface morphology. Growth temperatures in the range of 520°C and 680°C and V/III ratios from 1 to 5 have been investigated. A growth rate activation energy of 0.73 eV was found. At low growth temperatures between 520 and 540°C, the surface morphology is poor due to antimonide precipitates associated with incomplete decomposition of the TMSb. For layers grown on GaAs at 580°C and 600°C with a V/III ratio of 3 a high quality surface morphology is typical, with a mirror-like surface and good composition control. It was found that a suitable growth temperature and V/III flux ratio was beneficial for producing good AlGaSb layers. Undoped AlGaSb grown at 580°C with a V/III flux ratio of 3 at the rate of 3.5 μm/hour shows p-type conductivity with smooth surface morphology

  5. Influence of water relations and growth rate on plant element uptake and distribution

    International Nuclear Information System (INIS)

    Greger, Maria

    2006-02-01

    Plant uptake of Ni, Sr, Mo, Cs, La, Th, Se, Cl and I was examined to determine how plant water relations and growth rate influence the uptake and distribution of these elements in the studied plants. The specific questions were how water uptake and growth rate influenced the uptake of various nuclides and how transpiration influenced translocation to the shoot. The knowledge gained will be used in future modelling of radionuclide leakage from nuclear waste deposits entering the ecosystem via plants. The plant studied was willow, Salix viminalis, a common plant in the areas suggested for waste disposal; since there can be clone variation, two different clones having different uptake properties for several other heavy metals were used. The plants were grown in nutrient solution and the experiments on 3-month-old plants were run for 3 days. Polyethylene glycol was added to the medium to decrease the water uptake rate, a fan was used to increase the transpiration rate, and different light intensities were used to produce different growth rates. Element concentration was analysed in roots and shoots. The results show that both the uptake and distribution of various elements are influenced in different ways and to various extents by water flow and plant growth rate, and that it is not possible from the chemical properties of these elements to know how they will react. However, in most cases increased growth rate diluted the concentration of the element in the tissue, reduced water uptake reduced the element uptake, while transpiration had no effect on the translocation of elements to the shoot. The clones did not differ in terms of either the uptake or translocation of the elements, except that I was not taken up and translocated to the shoot in one of the clones when the plant water flow or growth rate was too low. Not all of the elements were found in the plant in the same proportions as they had been added to the nutrient solution

  6. Influence of water relations and growth rate on plant element uptake and distribution

    Energy Technology Data Exchange (ETDEWEB)

    Greger, Maria [Stockholm Univ. (Sweden). Dept. of Botany

    2006-02-15

    Plant uptake of Ni, Sr, Mo, Cs, La, Th, Se, Cl and I was examined to determine how plant water relations and growth rate influence the uptake and distribution of these elements in the studied plants. The specific questions were how water uptake and growth rate influenced the uptake of various nuclides and how transpiration influenced translocation to the shoot. The knowledge gained will be used in future modelling of radionuclide leakage from nuclear waste deposits entering the ecosystem via plants. The plant studied was willow, Salix viminalis, a common plant in the areas suggested for waste disposal; since there can be clone variation, two different clones having different uptake properties for several other heavy metals were used. The plants were grown in nutrient solution and the experiments on 3-month-old plants were run for 3 days. Polyethylene glycol was added to the medium to decrease the water uptake rate, a fan was used to increase the transpiration rate, and different light intensities were used to produce different growth rates. Element concentration was analysed in roots and shoots. The results show that both the uptake and distribution of various elements are influenced in different ways and to various extents by water flow and plant growth rate, and that it is not possible from the chemical properties of these elements to know how they will react. However, in most cases increased growth rate diluted the concentration of the element in the tissue, reduced water uptake reduced the element uptake, while transpiration had no effect on the translocation of elements to the shoot. The clones did not differ in terms of either the uptake or translocation of the elements, except that I was not taken up and translocated to the shoot in one of the clones when the plant water flow or growth rate was too low. Not all of the elements were found in the plant in the same proportions as they had been added to the nutrient solution.

  7. The use of Ampelisca abdita growth rate as an indicator of sediment quality

    International Nuclear Information System (INIS)

    Weston, D.P.; Thompson, B.

    1995-01-01

    Acute lethal bioassays with amphipod crustaceans are routinely used to assess toxicity of bulk sediments. A study within the San Francisco Bay Regional Monitoring Program (RMP) is in progress to develop a chronic bioassay with the amphipod Ampelisca abdita, measuring both survivorship and growth rates. This approach is attractive because depression of growth rate is likely to be a more sensitive indicator of toxic effects than acute lethality, and natural populations of A. abdita exist throughout the Bay. Spiked sediment bioassays, using cadmium and crude oil, were used to demonstrate the relative sensitivity of the standard 10-day lethal test vs. the 30-day growth test. Sediments were also collected from 9 sites throughout the Bay, ranging from areas adjacent to municipal wastewater discharges to areas distant from known point source inputs. These samples were then split, and used for side-by-side comparison of acute (lethal) and chronic (growth) toxicity tests. Survivorship exceeded 90% in all tests, including those sediments collected nearest the wastewater outfalls. Growth rates were contrasted among the various treatments to examine the utility of this end point in discriminating the outfall sites. Data on the spatial distribution, abundance, and size-frequency distribution of native populations was examined within the context of using growth rate as an indicator of toxic effects in natural populations as well

  8. Transcription factor control of growth rate dependent genes in Saccharomyces cerevisiae: A three factor design

    DEFF Research Database (Denmark)

    Fazio, Alessandro; Jewett, Michael Christopher; Daran-Lapujade, Pascale

    2008-01-01

    , such as Ace2 and Swi6, and stress response regulators, such as Yap1, were also shown to have significantly enriched target sets. Conclusion: Our work, which is the first genome-wide gene expression study to investigate specific growth rate and consider the impact of oxygen availability, provides a more......Background: Characterization of cellular growth is central to understanding living systems. Here, we applied a three-factor design to study the relationship between specific growth rate and genome-wide gene expression in 36 steady-state chemostat cultures of Saccharomyces cerevisiae. The three...... factors we considered were specific growth rate, nutrient limitation, and oxygen availability. Results: We identified 268 growth rate dependent genes, independent of nutrient limitation and oxygen availability. The transcriptional response was used to identify key areas in metabolism around which m...

  9. Airborne measurements of nucleation mode particles I: coastal nucleation and growth rates

    Directory of Open Access Journals (Sweden)

    C. D. O'Dowd

    2007-01-01

    Full Text Available A light aircraft was equipped with a bank of Condensation Particle Counters (CPCs (50% cut from 3–5.4–9.6 nm and a nano-Scanning Mobility Particle Sizer (nSMPS and deployed along the west coast of Ireland, in the vicinity of Mace Head. The objective of the exercise was to provide high resolution micro-physical measurements of the coastal nucleation mode in order to map the spatial extent of new particle production regions and to evaluate the evolution, and associated growth rates of the coastal nucleation-mode aerosol plume. Results indicate that coastal new particle production is occurring over most areas along the land-sea interface with peak concentrations at the coastal plume-head in excess of 106 cm−3. Pseudo-Lagrangian studies of the coastal plume evolution illustrated significant growth of new particles to sizes in excess of 8 nm approximately 10 km downwind of the source region. Close to the plume head (<1 km growth rates can be as high as 123–171 nm h−1, decreasing gradually to 53–72 nm h−1 at 3 km. Further along the plume, at distances up to 10 km, the growth rates are calculated to be 17–32 nm h−1. Growth rates of this magnitude suggest that after a couple of hours, coastal nucleation mode particles can reach significant sizes where they can contribution to the regional aerosol loading.

  10. Species Diversity Enhances Predator Growth Rates

    International Nuclear Information System (INIS)

    Olson, M.H.; Jacobs, R.P.; O'Donnell, E.B.

    2007-01-01

    Predators can be important top-down regulators of community structure and are known to have both positive and negative effects on species diversity. However, little is known about the reciprocal effects of species diversity on predators. Across a set of 80 lakes in Connecticut, USA, we found a strong positive correlation between prey species diversity (using the Shannon-Weiner Diversity Index) and growth rates of largemouth bass (Micropterus salmoides). This correlation was strongest for small predators and decreased with body size. Although the underlying mechanisms are not known, the correlation is not driven by total fish abundance, predator abundance, or productivity.

  11. Novel method of assessing delamination of the anterior lens capsule using spectral-domain optical coherence tomography

    OpenAIRE

    Tan, Deborah KL; Aung, Tin; Perera, Shamira A

    2012-01-01

    Deborah KL Tan,1 Tin Aung,1–3 Shamira A Perera1,21Singapore National Eye Centre, Singapore; 2Singapore Eye Research Institute, Singapore; 3National University of Singapore, Yong Loo Lin School of Medicine, SingaporeBackground: Delamination of the anterior lens capsule producing a double-ring sign during continuous curvilinear capsulorhexis is commonly associated with true exfoliation syndrome.Methods: Previous studies have concentrated on light- and transmission-electron microscopic...

  12. A Longitudinal Study and Color Rating System of Acquisition Cost Growth

    Science.gov (United States)

    2017-03-23

    cost growth analysis. Ways in which this research can be carried forward include: • Collect more SAR data to further populate our research database... Growth Cory N. D’Amico Follow this and additional works at: https://scholar.afit.edu/etd Part of the Finance and Financial Management Commons This...and Color Rating System of Acquisition Cost Growth " (2017). Theses and Dissertations. 781. https://scholar.afit.edu/etd/781 A Longitudinal

  13. Effect of extremely low frequency electromagnetic fields on growth rate and morphology of bacteria.

    Science.gov (United States)

    Inhan-Garip, Ayse; Aksu, Burak; Akan, Zafer; Akakin, Dilek; Ozaydin, A Nilufer; San, Tangul

    2011-12-01

    To determine the effect of extremely low frequency (bacteria and to determine any morphological changes that might have been caused by ELF-EMF. Six bacterial strains, three Gram-negative and three Gram-positive were subjected to 50 Hz, 0.5 mT ELF-EMF for 6 h. To determine growth rate after ELF-EMF application, bacteria exposed to ELF-EMF for 3 h were collected, transferred to fresh medium and cultured without field application for another 4 h. Growth-rate was determined by optical density (OD) measurements made every hour. Morphological changes were determined with Transmission electron microscopy (TEM) for two gram-negative and two gram-positive strains collected after 3 h of field application. A decrease in growth rate with respect to control samples was observed for all strains during ELF-EMF application. The decrease in growth-rate continued when exposed bacteria were cultured without field application. Significant ultrastructural changes were observed in all bacterial strains, which were seen to resemble the alterations caused by cationic peptides. This study shows that ELF-EMF induces a decrease in growth rate and morphological changes for both Gram-negative and Gram-positive bacteria.

  14. Inferring time derivatives including cell growth rates using Gaussian processes

    Science.gov (United States)

    Swain, Peter S.; Stevenson, Keiran; Leary, Allen; Montano-Gutierrez, Luis F.; Clark, Ivan B. N.; Vogel, Jackie; Pilizota, Teuta

    2016-12-01

    Often the time derivative of a measured variable is of as much interest as the variable itself. For a growing population of biological cells, for example, the population's growth rate is typically more important than its size. Here we introduce a non-parametric method to infer first and second time derivatives as a function of time from time-series data. Our approach is based on Gaussian processes and applies to a wide range of data. In tests, the method is at least as accurate as others, but has several advantages: it estimates errors both in the inference and in any summary statistics, such as lag times, and allows interpolation with the corresponding error estimation. As illustrations, we infer growth rates of microbial cells, the rate of assembly of an amyloid fibril and both the speed and acceleration of two separating spindle pole bodies. Our algorithm should thus be broadly applicable.

  15. Impact of Macroeconomic Policies on Poverty and Unemployment Rates in Nigeria, Implications for Attaining Inclusive Growth

    Directory of Open Access Journals (Sweden)

    Philip Nwosa

    2016-04-01

    Full Text Available This paper examined the effect of macroeconomic policies on unemployment and poverty rates in Nigeria from 1980 to 2013 with implication to achieving inclusive growth. The inability of macroeconomic policies in addressing the rising issues unemployment and poverty rates in Nigeria despite the impressive economic growth experience over the last decades has increasingly called for the need for the pursuance of inclusive growth to address the social issues of unemployment and poverty rate. Previous studies have not considered the extent to which macroeconomic policies affects unemployment and poverty rate in Nigeria, and the implication of this relationship to the attainment of inclusive growth in Nigeria. The study adopts the Ordinary Least Square (OLS technique. The study observed that among macroeconomic policy variables only exchange rate significantly influenced unemployment rate while only fiscal policy significantly influenced and poverty rate. This implies that present macroeconomic policies in Nigeria do not guarantee the attainment of inclusive growth in Nigeria. The contribution of the paper is that to achieve inclusive growth that guarantees high employment and reduced poverty rate, there is the need for a re-examination of macroeconomic policy management in Nigeria.

  16. Major Changes in Growth Rate and Growth Variability of Beech (Fagus sylvatica L. Related to Soil Alteration and Climate Change in Belgium

    Directory of Open Access Journals (Sweden)

    Nicolas Latte

    2016-08-01

    Full Text Available Global change—particularly climate change, forest management, and atmospheric deposition—has significantly altered forest growing conditions in Europe. The influences of these changes on beech growth (Fagus sylvatica L. were investigated for the past 80 years in Belgium, using non-linear mixed effects models on ring-width chronologies of 149 mature and dominant beech trees (87–186 years old. The effects of the developmental stage (i.e., increasing tree size were filtered out in order to focus on time-dependent growth changes. Beech radial growth was divided into a low-frequency signal (=growth rate, mainly influenced by forest management and atmospheric deposition, and into a high-frequency variability (≈mean sensitivity, mainly influenced by climate change. Between 1930 and 2008, major long-term and time-dependent changes were highlighted. The beech growth rate has decreased by about 38% since the 1950–1960s, and growth variability has increased by about 45% since the 1970–1980s. Our results indicate that (1 before the 1980s, beech growth rate was not predominantly impacted by climate change but rather by soil alteration (i.e., soil compaction and/or nitrogen deposition; and (2 since the 1980s, climate change induced more frequent and intense yearly growth reductions that amplified the growth rate decrease. The highlighted changes were similar in the two ecoregions of Belgium, although more pronounced in the lowlands than in the uplands.

  17. Exchange Rate Volatility and Employment Growth in Developing Countries: Evidence from Turkey

    OpenAIRE

    Demir, Firat

    2010-01-01

    Employing a unique panel of 691 private firms that accounted for 26% of total value-added in manufacturing in Turkey, the paper explores the impacts of exchange rate volatility on employment growth during the period of 1983 - 2005. The empirical analysis using a variety of specifications, estimation techniques, and robustness tests suggests that exchange rate volatility has a statistically and economically significant employment growth reducing effect on manufacturing firms. Using point estim...

  18. Nitrogen deficiency inhibits leaf blade growth in Lolium perenne by increasing cell cycle duration and decreasing mitotic and post-mitotic growth rates.

    Science.gov (United States)

    Kavanová, Monika; Lattanzi, Fernando Alfredo; Schnyder, Hans

    2008-06-01

    Nitrogen deficiency severely inhibits leaf growth. This response was analysed at the cellular level by growing Lolium perenne L. under 7.5 mM (high) or 1 mM (low) nitrate supply, and performing a kinematic analysis to assess the effect of nitrogen status on cell proliferation and cell growth in the leaf blade epidermis. Low nitrogen supply reduced leaf elongation rate (LER) by 43% through a similar decrease in the cell production rate and final cell length. The former was entirely because of a decreased average cell division rate (0.023 versus 0.032 h(-1)) and thus longer cell cycle duration (30 versus 22 h). Nitrogen status did not affect the number of division cycles of the initial cell's progeny (5.7), and accordingly the meristematic cell number (53). Meristematic cell length was unaffected by nitrogen deficiency, implying that the division and mitotic growth rates were equally impaired. The shorter mature cell length arose from a considerably reduced post-mitotic growth rate (0.033 versus 0.049 h(-1)). But, nitrogen stress did not affect the position where elongation stopped, and increased cell elongation duration. In conclusion, nitrogen deficiency limited leaf growth by increasing the cell cycle duration and decreasing mitotic and post-mitotic elongation rates, delaying cell maturation.

  19. Colorimetry provides a rapid objective measurement of de novo hair growth rate in mice.

    Science.gov (United States)

    Tzung, Tien-Yi; Yang, Chia-Yi; Huang, Yung-Chang; Kao, Fu-Jen

    2009-11-01

    Depilated mice have been used as a test platform for hair growth-regulating agents. However, currently available assessment tools for hair growth in mice are less than ideal. Tristimulus colorimetry of the fur color of depilated agouti, albino, and black mice with L*, a*, and b* values were performed daily until the full growth of pelage. Using light-emitting diode (LED) irradiation (650 and 890 nm) with a daily dose of 3.5 J/cm(2) as hair growth regulators, the hair growth rates observed by the global assessment were compared with those derived from colorimetry. In contrast to a* and b* values, L* values changed more drastically over time in the anagen phase regardless of fur color. Unlike the inhibitory effect of 650 nm irradiation, LED of 890 nm promoted de novo hair regrowth in mice. The difference in hair growth rates detected by colorimetry paralleled the observation made by the global assessment. The L* value of fur color obtained by tristimulus colorimetry was a sensitive yet quantitative indicator of de novo hair growth, and could be used to project the hair growth rate in mice.

  20. Effect of different saccharides on growth, sporulation rate and d ...

    African Journals Online (AJOL)

    MFCS

    2012-05-17

    May 17, 2012 ... general, high sporulation rate was related with high growth rate and high viable cell count (>1.5 x 1012 cfu/ml). .... The sterile culture medium (180 ml) in a 1000 ml Erlenmeyer flask was ... The column temperature was set at 85°C. A series of ..... inactivation of certain sugar-metabolizing operons, such as lac ...

  1. Population Growth Rate, Life Expectancy and Pension Program Improvement in China

    OpenAIRE

    Yang, Zaigui

    2008-01-01

    Applying an overlapping-generations model with lifetime uncertainty, we examine in this paper China’s partially funded public pension system. The findings show that the individual contribution rate does not affect the capital-labor ratio but the firm contribution rate does. The optimal firm contribution rate depends on the capital share of income, social discount factor, survival probability, and population growth rate. The simulation results indicate that the optimal firm contribution rate r...

  2. Translation elicits a growth rate-dependent, genome-wide, differential protein production in Bacillus subtilis.

    Science.gov (United States)

    Borkowski, Olivier; Goelzer, Anne; Schaffer, Marc; Calabre, Magali; Mäder, Ulrike; Aymerich, Stéphane; Jules, Matthieu; Fromion, Vincent

    2016-05-17

    Complex regulatory programs control cell adaptation to environmental changes by setting condition-specific proteomes. In balanced growth, bacterial protein abundances depend on the dilution rate, transcript abundances and transcript-specific translation efficiencies. We revisited the current theory claiming the invariance of bacterial translation efficiency. By integrating genome-wide transcriptome datasets and datasets from a library of synthetic gfp-reporter fusions, we demonstrated that translation efficiencies in Bacillus subtilis decreased up to fourfold from slow to fast growth. The translation initiation regions elicited a growth rate-dependent, differential production of proteins without regulators, hence revealing a unique, hard-coded, growth rate-dependent mode of regulation. We combined model-based data analyses of transcript and protein abundances genome-wide and revealed that this global regulation is extensively used in B. subtilis We eventually developed a knowledge-based, three-step translation initiation model, experimentally challenged the model predictions and proposed that a growth rate-dependent drop in free ribosome abundance accounted for the differential protein production. © 2016 The Authors. Published under the terms of the CC BY 4.0 license.

  3. Growth rates and energy intake of hand-reared cheetah cubs (Acinonyx jubatus) in South Africa.

    Science.gov (United States)

    Bell, K M; Rutherfurd, S M; Morton, R H

    2012-04-01

    Growth rate is an important factor in neonatal survival. The aim of this study was to determine growth rates in hand-reared cheetah cubs in South Africa fed a prescribed energy intake, calculated for growth in the domestic cat. Growth was then compared with previously published data from hand-reared cubs in North America and the relationship between growth and energy intake explored. Daily body weight (BW) gain, feed and energy intake data was collected from 18 hand-reared cheetah cubs up to 120 days of age. The average pre-weaning growth rate was 32 g/day, which is lower than reported in mother-reared cubs and hand-reared cubs in North American facilities. However, post-weaning growth increased to an average of 55 g/day. Growth was approximately linear prior to weaning, but over the entire age range it exhibited a sigmoidal shape with an asymptotic plateau averaging 57 kg. Energy intake associated with pre-weaning growth was 481 kJ ME/kg BW(0.75). Regression analysis described the relationship between metabolic BW, metabolisable energy (ME) intake, and hence daily weight gain. This relationship may be useful in predicting energy intake required to achieve growth rates in hand-reared cheetah cubs similar to those observed for their mother-reared counterparts. © 2011 Blackwell Verlag GmbH.

  4. Adhesion-delamination phenomena at the surfaces and interfaces in microelectronics and MEMS structures and packaged devices

    International Nuclear Information System (INIS)

    Khanna, V K

    2011-01-01

    Physico-chemical mechanisms of adhesion and debonding at the various surfaces and interfaces of semiconductor devices, integrated circuits and microelectromechanical systems are systematically examined, starting from chip manufacturing and traversing the process stages to the ultimate finished product. Sources of intrinsic and thermal stresses in these devices are pointed out. Thin film ohmic contacts to the devices call for careful attention. The role of an adhesion layer in multilayer metallization schemes is highlighted. In packaged devices, sites facing potential risks of delamination are indicated. As MEMS devices incorporate moving parts, there are additional issues due to adhesion of suspended structures to surfaces in the vicinity, both during chip fabrication and their subsequent operation. Proper surface treatments for preventing adhesion together with design considerations for overcoming stiction pave the way to reliable functioning of these devices. Adhesion-delamination issues in microelectronics and MEMS continue to pose significant challenges to both design and process engineers. This paper is an attempt to survey the adhesion characteristics of materials, their compatibilities and limitations and look at future research trends. In addition, it addresses some of the techniques for improved or reduced adhesion, as demanded by the situation. The paper encompasses fundamental aspects to contemporary applications.

  5. MODELLING THE DELAMINATION FAILURE ALONG THE CFRP-CFST BEAM INTERACTION SURFACE USING DIFFERENT FINITE ELEMENT TECHNIQUES

    Directory of Open Access Journals (Sweden)

    AHMED W. AL-ZAND

    2017-01-01

    Full Text Available Nonlinear finite element (FE models are prepared to investigate the behaviour of concrete-filled steel tube (CFST beams strengthened by carbon fibre reinforced polymer (CFRP sheets. The beams are strengthened from the bottom side only by varied sheet lengths (full and partial beam lengths and then subjected to ultimate flexural loads. Three surface interaction techniques are used to implement the bonding behaviour between the steel tube and the CFRP sheet, namely, full tie interaction (TI, cohesive element (CE and cohesive behaviour (CB techniques using ABAQUS software. Results of the comparison between the FE analysis and existing experimental study confirm that the FE models with the TI technique could be applicable for beams strengthened by CFRP sheets with a full wrapping length; the technique could not accurately implement the CFRP delamination failure, which occurred for beams with a partial wrapping length. Meanwhile, the FE models with the CE and CB techniques are applicable in the implementation of both CFRP failures (rapture and delamination for both full and partial wrapping lengths, respectively. Where, the ultimate loads' ratios achieved by the FE models using TI, CE and CB techniques about 1.122, 1.047 and 1.045, respectively, comparing to the results of existing experimental tests.

  6. Detection of Delamination in Laminate Wind Turbine Blades Using One-Dimensional Wavelet Analysis of Modal Responses

    Directory of Open Access Journals (Sweden)

    Łukasz Doliński

    2018-01-01

    Full Text Available This paper demonstrates the effectiveness of a nondestructive diagnostic technique used to determine the location and size of delamination in laminated coatings of wind turbine blades. This is realized based on results of numerical and experimental investigations obtained by the use of the finite element method (FEM and laser scanning vibrometry (LSV. The proposed method is based on the one-dimensional continuous wavelet transform of vibration parameters of a wind turbine blade. The investigations were conducted for a 1 : 10 scaled-down blade of a 36 m rotor wind turbine. Glass fibres and epoxy resin were used as laminate components. For numerical studies, a simple delamination model was proposed. The results obtained by the authors were used to determine the optimal set of parameters of the continuous wavelet transform. The application of high-quality LSV for experimental measurements allowed determining the optimal conditions of measuring procedures. At the same time the capabilities and limitations, resulting from the nature of the measurement method, were identified. In order to maximize the effectiveness of the detection method, preliminary signal processing was performed. Beside base wavelets also different waveform families were tested. The results obtained by the authors showed that it is possible to identify and localize even relatively small damage.

  7. The dependence of the growth rate and meat content of young boars on semen parameters and conception rate.

    Science.gov (United States)

    Knecht, D; Jankowska-Mąkosa, A; Duziński, K

    2017-05-01

    Boars have a decisive impact on the progress in pig production, however, there is no recent information about the optimal growth parameters during the rearing period for modern breed later used in artificial insemination (AI) stations. Therefore, the objective of the research was to conduct semen parameter and conception rate analyses on the basis of growth rate and meat content assessments made during the rearing of AI boars of different genotypes. The study was carried out between 2010 and 2014 and included 184 boars in five breed combinations: 46 Polish Large White, 50 Polish Landrace, 27 Pietrain, 36 Duroc×Pietrain and 25 Hampshire×Pietrain. Boars were qualified by daily gains and meat content assessment (between 170 and 210 days of life). A total number of 38 272 ejaculates were examined (semen volume (ml), spermatozoa concentration (×106 ml-1), total number of spermatozoa (×109) and number of insemination doses from one ejaculate (n)). The fertility was determined by the conception rate (%). Semen volume, spermatozoa concentration and conception rate (PMeat content affected semen volume, number of insemination doses and conception rate (Pmeat content helps AI stations to increase the efficiency and economic profitability, and the number of insemination doses to increase by up to 300 doses/boar within a year. The analyses of growth parameters may help increase the efficiency and economic viability of AI stations.

  8. Periodic matrix population models: growth rate, basic reproduction number, and entropy.

    Science.gov (United States)

    Bacaër, Nicolas

    2009-10-01

    This article considers three different aspects of periodic matrix population models. First, a formula for the sensitivity analysis of the growth rate lambda is obtained that is simpler than the one obtained by Caswell and Trevisan. Secondly, the formula for the basic reproduction number R0 in a constant environment is generalized to the case of a periodic environment. Some inequalities between lambda and R0 proved by Cushing and Zhou are also generalized to the periodic case. Finally, we add some remarks on Demetrius' notion of evolutionary entropy H and its relationship to the growth rate lambda in the periodic case.

  9. Physiological levels of nitrate support anoxic growth by denitrification of Pseudomonas aeruginosa at growth rates reported in cystic fibrosis lungs and sputum

    DEFF Research Database (Denmark)

    Line, Laura; Alhede, Morten; Kolpen, Mette

    2014-01-01

    denitrification. The growth rate of P. aeruginosa achieved by denitrification at physiological levels (~400 μM) of nitrate (NO(-) 3) is however, not known. Therefore, we have measured growth rates of anoxic cultures of PAO1 and clinical isolates (n = 12) in LB media supplemented with NO(-) 3 and found...... a significant increase of growth when supplementing PAO1 and clinical isolates with ≥150 μM NO(-) 3 and 100 μM NO(-) 3, respectively. An essential contribution to growth by denitrification was demonstrated by the inability to establish a significantly increased growth rate by a denitrification deficient Δnir...... of the four N-oxide reductases in PAO1 (Nar, Nir, Nor, Nos) further verified the engagement of denitrification, showing a transient increase in activation and expression and rapid consumption of NO(-) 3 followed by a transient increase of NO(-) 2. Growth rates obtained by denitrification in this study were...

  10. Densification rate and interfacial adhesion of bilayer cemented tungsten carbide and steel

    Energy Technology Data Exchange (ETDEWEB)

    Ojo-kupoluyi, Oluwatosin Job; Tahir, Suraya Mohd; Ariff, Azmah Hanim Mohamed; Baharudin, B.T. Hang Tuah [Univ. Putra Malaysia, Selangor (Malaysia). Dept. of Mechanical and Manufacturing Engineering; Matori, Khamirul Amin [Univ. Putra Malaysia, Selangor (Malaysia). Dept. of Physics; Univ. Putra Malaysia, Selangor (Malaysia). Inst. of Advanced Technology (ITMA); Shamsul Anuar, Mohd [Univ. Putra Malaysia, Selangor (Malaysia). Dept. of Process and Food Engineering

    2017-12-15

    Manufacturing tailored materials is commonly faced with the challenge of shrinkage mismatch between layers resulting in delamination. The effects of sintering temperature and carbon variation on the densification and interfacial bond strength of bilayer cemented tungsten carbide and steel processed through powder metallurgy are analyzed. It is revealed through field-emission scanning electron microscopy images that inter-layer diffusion induced by liquid-phase sintering plays a major role in the densification and bonding of layers. Through dimensional analysis of sintered bilayer specimens, the strain rate of cemented tungsten carbide is observed to surpass that of steel. An enhanced densification rate of 6.1 % and M{sub 6}C (eta carbide) reduction with increased carbon level results in strong interfacial bonding in specimens sintered at 1 280 C. At 1 295 C, diffusion accelerates and the axial and radial shrinkage increase by 14.05 % and 13.35 %, respectively, in 93.8 wt.% WC - 6 wt.% Fe - 0.2 wt.% C and 93.2 wt.% Fe - 6 wt.% WC - 0.8 wt.% C, thereby increasing the tendency for complete delamination.

  11. Densification rate and interfacial adhesion of bilayer cemented tungsten carbide and steel

    International Nuclear Information System (INIS)

    Ojo-kupoluyi, Oluwatosin Job; Tahir, Suraya Mohd; Ariff, Azmah Hanim Mohamed; Baharudin, B.T. Hang Tuah; Shamsul Anuar, Mohd

    2017-01-01

    Manufacturing tailored materials is commonly faced with the challenge of shrinkage mismatch between layers resulting in delamination. The effects of sintering temperature and carbon variation on the densification and interfacial bond strength of bilayer cemented tungsten carbide and steel processed through powder metallurgy are analyzed. It is revealed through field-emission scanning electron microscopy images that inter-layer diffusion induced by liquid-phase sintering plays a major role in the densification and bonding of layers. Through dimensional analysis of sintered bilayer specimens, the strain rate of cemented tungsten carbide is observed to surpass that of steel. An enhanced densification rate of 6.1 % and M 6 C (eta carbide) reduction with increased carbon level results in strong interfacial bonding in specimens sintered at 1 280 C. At 1 295 C, diffusion accelerates and the axial and radial shrinkage increase by 14.05 % and 13.35 %, respectively, in 93.8 wt.% WC - 6 wt.% Fe - 0.2 wt.% C and 93.2 wt.% Fe - 6 wt.% WC - 0.8 wt.% C, thereby increasing the tendency for complete delamination.

  12. Microscopic Rate Constants of Crystal Growth from Molecular Dynamic Simulations Combined with Metadynamics

    Directory of Open Access Journals (Sweden)

    Dániel Kozma

    2012-01-01

    Full Text Available Atomistic simulation of crystal growth can be decomposed into two steps: the determination of the microscopic rate constants and a mesoscopic kinetic Monte Carlo simulation. We proposed a method to determine kinetic rate constants of crystal growth. We performed classical molecular dynamics on the equilibrium liquid/crystal interface of argon. Metadynamics was used to explore the free energy surface of crystal growth. A crystalline atom was selected at the interface, and it was displaced to the liquid phase by adding repulsive Gaussian potentials. The activation free energy of this process was calculated as the maximal potential energy density of the Gaussian potentials. We calculated the rate constants at different interfacial structures using the transition state theory. In order to mimic real crystallization, we applied a temperature difference in the calculations of the two opposite rate constants, and they were applied in kinetic Monte Carlo simulation. The novelty of our technique is that it can be used for slow crystallization processes, while the simple following of trajectories can be applied only for fast reactions. Our method is a possibility for determination of elementary rate constants of crystal growth that seems to be necessary for the long-time goal of computer-aided crystal design.

  13. Concurrent growth rate and transcript analyses reveal essential gene stringency in Escherichia coli.

    Directory of Open Access Journals (Sweden)

    Shan Goh

    Full Text Available BACKGROUND: Genes essential for bacterial growth are of particular scientific interest. Many putative essential genes have been identified or predicted in several species, however, little is known about gene expression requirement stringency, which may be an important aspect of bacterial physiology and likely a determining factor in drug target development. METHODOLOGY/PRINCIPAL FINDINGS: Working from the premise that essential genes differ in absolute requirement for growth, we describe silencing of putative essential genes in E. coli to obtain a titration of declining growth rates and transcript levels by using antisense peptide nucleic acids (PNA and expressed antisense RNA. The relationship between mRNA decline and growth rate decline reflects the degree of essentiality, or stringency, of an essential gene, which is here defined by the minimum transcript level for a 50% reduction in growth rate (MTL(50. When applied to four growth essential genes, both RNA silencing methods resulted in MTL(50 values that reveal acpP as the most stringently required of the four genes examined, with ftsZ the next most stringently required. The established antibacterial targets murA and fabI were less stringently required. CONCLUSIONS: RNA silencing can reveal stringent requirements for gene expression with respect to growth. This method may be used to validate existing essential genes and to quantify drug target requirement.

  14. Facilitating control of fed-batch fermentation processes by monitoring the growth rates of saccharomyces cerevisiae

    NARCIS (Netherlands)

    Keulers, M.L.B.; Ariaans, L.J.J.M.; Soeterboek, R.; Giuseppin, M.

    1994-01-01

    In this paper we present a growth rate controller for a fed-batch bioprocess. An observer estimates the growth rate. The observer is based on knowledge about the stoichiometric relations of the process. Furthermore, the observer needs online measurements of the oxygen uptake rate and the

  15. EFFECT OF SODIUM DODECYLBENZENESULFONIC ACID (SDBS ON THE GROWTH RATE AND MORPHOLOGY OF BORAX CRYSTAL

    Directory of Open Access Journals (Sweden)

    Suharso Suharso

    2010-06-01

    Full Text Available An investigation of the effect of sodium dodecylbenzenesulfonic acid (SDBS on both growth rate and morphology of borax crystal has been carried out.  This experiment was carried out at temperature of 25 °C and relative supersaturation of 0.21 and 0.74 under in situ cell optical microscopy method.  The result shows that SDBS inhibits the growth rate and changes the morphology of borax crystal.   Keywords: Borax; growth rate; crystallization, SDBS

  16. Evaluation of interfacial mechanical properties under shear loading in EB-PVD TBCs by the pushout method

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Sang-Seok [Research Center for Advanced Science and Technology, University of Tokyo, Tokyo 153-8904 (Japan); Liu Yufu [Research Center for Advanced Science and Technology, University of Tokyo, Tokyo 153-8904 (Japan); Kagawa, Yutaka [Research Center for Advanced Science and Technology, University of Tokyo, Tokyo 153-8904 (Japan)]. E-mail: kagawa@iis.u-tokyo.ac.jp

    2007-06-15

    A new simple pushout technique for evaluation of interfacial shear mechanical properties in thermal barrier coatings has been developed. The technique is similar to the pushout test of fiber-reinforced ceramics, except for the specimen shape and support method. The technique has been applied to evaluation of interfacial delamination toughness, {gamma} {sub i}, of the electron beam physical vapor deposition (EB-PVD) ZrO{sub 2} thermal barrier coating (TBC) system. The change of {gamma} {sub i} in the EB-PVD system with thermal exposure is measured and discussed in terms of microstructural change and delamination crack path. The measured delamination toughness varied from {gamma} {sub i} = 10 to 115 J/m{sup 2}. The delamination path and TGO growth were found to be closely related. The delamination toughness significantly decreases due to the formation and growth of a spinel phase in the TGO layer. The relation between delamination toughness and delamination behavior is discussed.

  17. Generation and growth rates of nonlinear distortions in a traveling wave tube

    International Nuclear Information System (INIS)

    Woehlbier, John G.; Dobson, Ian; Booske, John H.

    2002-01-01

    The structure of a steady state multifrequency model of a traveling wave tube amplifier is exploited to describe the generation of intermodulation frequencies and calculate their growth rates. The model describes the evolution of Fourier coefficients of circuit and electron beam quantities and has the form of differential equations with quadratic nonlinearities. Intermodulation frequencies are sequentially generated by the quadratic nonlinearities in a series solution of the differential equations. A formula for maximum intermodulation growth rates is derived and compared to simulation results

  18. On Decidable Growth-Rate Properties of Imperative Programs

    Directory of Open Access Journals (Sweden)

    Amir M. Ben-Amram

    2010-05-01

    Full Text Available In 2008, Ben-Amram, Jones and Kristiansen showed that for a simple "core" programming language - an imperative language with bounded loops, and arithmetics limited to addition and multiplication - it was possible to decide precisely whether a program had certain growth-rate properties, namely polynomial (or linear bounds on computed values, or on the running time. This work emphasized the role of the core language in mitigating the notorious undecidability of program properties, so that one deals with decidable problems. A natural and intriguing problem was whether more elements can be added to the core language, improving its utility, while keeping the growth-rate properties decidable. In particular, the method presented could not handle a command that resets a variable to zero. This paper shows how to handle resets. The analysis is given in a logical style (proof rules, and its complexity is shown to be PSPACE-complete (in contrast, without resets, the problem was PTIME. The analysis algorithm evolved from the previous solution in an interesting way: focus was shifted from proving a bound to disproving it, and the algorithm works top-down rather than bottom-up.

  19. A fiber bridging model for fatigue delamination in composite materials

    International Nuclear Information System (INIS)

    Gregory, Jeremy R.; Spearing, S. Mark

    2004-01-01

    A fiber bridging model has been created to examine the effects of bridging on Mode I delamination fatigue fracture in a carbon fiber polymer-matrix composite. The model uses a cohesive zone law that is derived from quasi-static R-curves to determine the bridging energy applied in the bridged region. Timoshenko beam theory and an iterative self-consistent scheme are used to calculate the bridging tractions and displacements. After applying the bridging model to crack propagation data the scatter in the data was significantly reduced and clear trends were observed as a function of temperature that were not apparent previously. This indicated that the model appropriately accounted for the bridging in the experiments. Scanning electron microscopy crack opening displacement measurements were performed to validate the model's predictions. The measurements showed that the predictions were close to the actual bridging levels in the specimen

  20. Stiff mutant genes of Phycomyces target turgor pressure and wall mechanical properties to regulate elongation growth rate

    Directory of Open Access Journals (Sweden)

    Joseph K. E. Ortega

    2012-05-01

    Full Text Available Regulation of cell growth is paramount to all living organisms. In plants, algae and fungi, regulation of expansive growth of cells is required for development and morphogenesis. Also, many sensory responses of stage IVb sporangiophores of Phycomyces blakesleeanus are produced by regulating elongation growth rate (growth responses and differential elongation growth rate (tropic responses. Stiff mutant sporangiophores exhibit diminished tropic responses and are found to be defective in at least four genes; madD, madE, madF and madG. Prior experimental research suggests that the defective genes affect growth regulation, but this was not verified. All the growth of the single-celled stalk of the stage IVb sporangiophore occurs in a short region termed the growth zone. Prior experimental and theoretical research indicates that elongation growth rate of the stage IVb sporangiophore can be regulated by controlling the cell wall mechanical properties within the growth zone and the magnitude of the turgor pressure. A quantitative biophysical model for elongation growth rate is required to elucidate the relationship between wall mechanical properties and turgor pressure during growth regulation. In this study, it is hypothesized that the mechanical properties of the wall within the growth zone of stiff mutant sporangiophores are different compared to wild type. A biophysical equation for elongation growth rate is derived for fungal and plant cells with a growth zone. Two strains of stiff mutants are studied, C149 madD120 (- and C216 geo- (-. Experimental results demonstrate that turgor pressure is larger but irreversible deformation rates of the wall within the growth zone and growth zone length are smaller for stiff mutant sporangiophores compared to wild type. These findings explain the diminished tropic responses of the stiff mutant sporangiophores and suggest that the defective genes affect the amount of wall-building material delivered to the inner

  1. Synthesis, anion exchange, and delamination of Co-Al layered double hydroxide: assembly of the exfoliated nanosheet/polyanion composite films and magneto-optical studies.

    Science.gov (United States)

    Liu, Zhaoping; Ma, Renzhi; Osada, Minoru; Iyi, Nobuo; Ebina, Yasuo; Takada, Kazunori; Sasaki, Takayoshi

    2006-04-12

    This paper describes a systematic study on the synthesis, anion exchange, and delamination of Co-Al layered double hydroxide (LDH), with the aim of achieving fabrication and clarifying the properties of LDH nanosheet/polyanion composite films. Co-Al-CO3 LDH hexagonal platelets of 4 mum in lateral size were synthesized by the urea method under optimized reaction conditions. The as-prepared CO3(2-)-LDH was converted to Cl- -LDH by treating with a NaCl-HCl mixed solution, retaining its high crystallinity and hexagonal platelike morphology. LDHs intercalated with a variety of anions (such as NO3-, ClO4-, acetate, lactate, dodecyl sulfate, and oleate) were further prepared from Cl- -LDH via an anion-exchange process employing corresponding salts. Exchanged products in various anion forms were found to show different delamination behaviors in formamide. Among them, best results were observed for NO3- -LDH in terms of the exfoliating degree and the quality of the exfoliated nanosheets. The delamination gave a pink transparent suspension containing well-defined nanosheets with lateral sizes of up to 2 microm. The resulting nanosheets were assembled layer-by-layer with an anionic polymer, poly(sodium styrene 4-sulfonate) (PSS), onto quartz glass substrates to produce composite films. Magnetic circular dichroism (MCD) measurements revealed that the assembled multilayer films exhibited an interesting magneto-optical response.

  2. Hoof Growth Rates of the European Roe Deer (Capreolus capreolus for Dating the Hoof’s Isotopic Archive

    Directory of Open Access Journals (Sweden)

    Benjamin D. Hafner

    2017-11-01

    Full Text Available Hooves preserve the isotopic information laid down during their growth and may be used for reconstruction of animal feeding history. To assign certain positions along hooves to corresponding times, growth rates are required. Hoof growth rates are known for domestic animals; however, they cannot be obtained easily in wild animals. We estimated the hoof growth rate of the European roe deer (Capreolus capreolus L. by using the immediate drop in δ13C along the hoof as a tag that is assigned to the date of maize (Zea mays L. harvest. Keratin samples were taken each mm along 17 hooves and analyzed for their δ13C. A linear regression between (1 time differences of expected maize harvest to animal death and (2 distances between the points of the δ13C drop to the periople yielded the growth rate. Mean hoof growth rate was 0.122 mm/day (95% CI 0.014 mm/day and 0.365%/day (±0.026%/day of the hoof length and within the range of domestic animals. The method may be applied to determine growth rates of other incrementally growing tissues. Our estimated growth rate fosters dating isotopic information in hooves, facilitating research on feed resources and space use of roe deer.

  3. Growth-Rate Dependent Regulation of tRNA Level and Charging in Bacillus licheniformis.

    Science.gov (United States)

    Ferro, Iolanda; Liebeton, Klaus; Ignatova, Zoya

    2017-10-13

    Cellular growth crucially depends on protein synthesis and the abundance of translational components. Among them, aminoacyl-tRNAs play a central role in biosynthesis and shape the kinetics of mRNA translation, thus influencing protein production. Here, we used microarray-based approaches to determine the charging levels and tRNA abundance of Bacillus licheniformis. We observed an interesting cross-talk among tRNA expression, charging pattern, and growth rate. For a large subset of tRNAs, we found a co-regulated and augmented expression at high growth rate. Their tRNA aminoacylation level is kept relatively constant through riboswitch-regulated expression of the cognate aminoacyl-tRNA-synthetase (AARS). We show that AARSs with putative riboswitch-controlled expression are those charging tRNAs with amino acids which disfavor cell growth when individually added to the nutrient medium. Our results suggest that the riboswitch-regulated AARS expression in B. licheniformis is a powerful mechanism not only to maintain a constant ratio of aminoacyl-tRNA independent of the growth rate but concomitantly to control the intracellular level of free amino acids. Copyright © 2017 Elsevier Ltd. All rights reserved.

  4. Data compilation of respiration, feeding, and growth rates of marine pelagic organisms

    DEFF Research Database (Denmark)

    2013-01-01

    's adaptation to the environment, with consequently less universal mass scaling properties. Data on body mass, maximum ingestion and clearance rates, respiration rates and maximum growth rates of animals living in the ocean epipelagic were compiled from the literature, mainly from original papers but also from...

  5. Implementing statistical analysis in multi-channel acoustic impact-echo testing of concrete bridge decks: Determining thresholds for delamination detection

    Science.gov (United States)

    Hendricks, Lorin; Spencer Guthrie, W.; Mazzeo, Brian

    2018-04-01

    An automated acoustic impact-echo testing device with seven channels has been developed for faster surveying of bridge decks. Due to potential variations in bridge deck overlay thickness, varying conditions between testing passes, and occasional imprecise equipment calibrations, a method that can account for variations in deck properties and testing conditions was necessary to correctly interpret the acoustic data. A new methodology involving statistical analyses was therefore developed. After acoustic impact-echo data are collected and analyzed, the results are normalized by the median for each channel, a Gaussian distribution is fit to the histogram of the data, and the Kullback-Leibler divergence test or Otsu's method is then used to determine the optimum threshold for differentiating between intact and delaminated concrete. The new methodology was successfully applied to individual channels of previously unusable acoustic impact-echo data obtained from a three-lane interstate bridge deck surfaced with a polymer overlay, and the resulting delamination map compared very favorably with the results of a manual deck sounding survey.

  6. Thermal effects on growth and respiration rates of the mayfly, Dolania americana (ephemeroptera)

    International Nuclear Information System (INIS)

    Harvey, R.S.

    1975-01-01

    The mayfly Dolania Americana, common in the sand of Upper Three Runs Creek, Savannah River Plant, was studied to determine the effects of seasonal changes in temperature on population growth rates and to determine the effects of slight elevations in water temperature on respiration rates of this benthic species. Growth of the population increased with stream temperature until peak emergence of adults in June and July. There was a strong inverse correlation between body weight and respiration rates of immature nymphs. Respiration rates at 2.5, 5, and 10 0 C above ambient creekwater temperatures were not significantly higher than those measured at ambient creekwater temperatures. (auth)

  7. Investigating the asymmetric relationship between inflation-output growth exchange rate changes

    Science.gov (United States)

    Chu, Jenq Fei; Sek, Siok Kun

    2017-08-01

    The relationship between inflation-output growth or output variation has long been studied. In this study, we extend the investigation under two exchange rate flexibility/regime in four Asian countries (Indonesia, Korea, Philippines and Thailand) that have experienced drastic exchange rate regime changes aftermath the financial crisis of 1997. These countries have switched from fixed/rigid exchange rate regime to flexible exchange rate and inflation targeting (IT) regime after the crisis. Our main objective is to compare the inflation-output trade-off relationship in the pre-IT and post-IT periods as a tool to evaluate the efficiency of monetary policy. A nonlinear autoregressive distributed lags (NARDL) model is applied to capture the asymmetric effects of exchange rate changes (increases and decreases). The data ranging from 1981M1 onwards till 2016M3. Our results show that exchange rate has asymmetric effect on inflation both short-run and long-run with larger impact in the post-IT period under flexible regime. Depreciation of exchange rate has leads to higher inflation. Furthermore, we find evidences on the relationship between inflation and growth in both short-run and long-run, but the trade-off only detected in the short run both in the pre- and post-IT periods.

  8. A combined experimental and theoretical approach to establish the relationship between shear force and clay platelet delamination in melt-processed polypropylene nanocomposites

    CSIR Research Space (South Africa)

    Bandyopadhyay, J

    2014-04-01

    Full Text Available In this article, a combined experimental and theoretical approach has been proposed to establish a relationship between the required shear force and the degree of delamination of clay tactoids during the melt-processing of polymer nanocomposites...

  9. Rising CO2 interacts with growth light and growth rate to alter photosystem II photoinactivation of the coastal diatom Thalassiosira pseudonana.

    Directory of Open Access Journals (Sweden)

    Gang Li

    Full Text Available We studied the interactive effects of pCO(2 and growth light on the coastal marine diatom Thalassiosira pseudonana CCMP 1335 growing under ambient and expected end-of-the-century pCO(2 (750 ppmv, and a range of growth light from 30 to 380 µmol photons·m(-2·s(-1. Elevated pCO(2 significantly stimulated the growth of T. pseudonana under sub-saturating growth light, but not under saturating to super-saturating growth light. Under ambient pCO(2 susceptibility to photoinactivation of photosystem II (σ(i increased with increasing growth rate, but cells growing under elevated pCO(2 showed no dependence between growth rate and σ(i, so under high growth light cells under elevated pCO(2 were less susceptible to photoinactivation of photosystem II, and thus incurred a lower running cost to maintain photosystem II function. Growth light altered the contents of RbcL (RUBISCO and PsaC (PSI protein subunits, and the ratios among the subunits, but there were only limited effects on these and other protein pools between cells grown under ambient and elevated pCO(2.

  10. Using wavelength-normalized optical spectroscopy to improve the accuracy of bacteria growth rate quantification

    Science.gov (United States)

    McBirney, Samantha E.; Trinh, Kristy; Wong-Beringer, Annie; Armani, Andrea M.

    2017-02-01

    One of the fundamental analytical measurements performed in microbiology is monitoring and characterizing cell concentration in culture media. Measurement error will give rise to reproducibility problems in a wide range of applications, from biomanufacturing to basic research. Therefore, it is critical that the generated results are consistent. Single wavelength optical density (OD) measurements have become the preferred approach. Here, we compare the conventional OD600 technique with a multi-wavelength normalized scattering optical spectroscopy method to measure the growth rates of Pseudomonas aeruginosa and Staphylococcus aureus, two of the leading nosocomial pathogens with proven abilities to develop resistance. The multi-wavelength normalization process minimizes the impact of bacteria byproducts and environmental noise on the signal, thereby accurately quantifying growth rates with high fidelity at low concentrations. In contrast, due to poor absorbance and scattering at 600 nm, the classic OD600 measurement method is able to detect bacteria but cannot quantify the growth rate reliably. Our wavelength-normalization protocol to detect bacteria growth rates can be readily and easily adopted by research labs, given that it only requires the use of a standard spectrophotometer and implementation of straightforward data analysis. Measuring and monitoring bacteria growth rates play a critical role in a wide range of settings, spanning from therapeutic design and development to diagnostics and disease prevention. Having a full understanding of the growth cycles of bacteria known to cause severe infections and diseases will lead to a better understanding of the pathogenesis of these illnesses, leading to better treatment and, ultimately, the development of a cure.

  11. Radiosensitivity of the swiss-rap mouse as a function of its growth rate

    International Nuclear Information System (INIS)

    Legeay, G.; Glas, J.F.

    1969-01-01

    The results of an exhaustive study of the age dependence of the radiosensitivity of female Swiss-Rap mice are given. A close relationship of radiosensitivity versus age could not be brought out, whereas the weekly growth rate could be accurately related to radiosensitivity. Thus, the latter should be studied when a strain is to be used for biological experiments, as the rates of growth are different with the strains. (author) [fr

  12. Conifers in cold environments synchronize maximum growth rate of tree-ring formation with day length.

    Science.gov (United States)

    Rossi, Sergio; Deslauriers, Annie; Anfodillo, Tommaso; Morin, Hubert; Saracino, Antonio; Motta, Renzo; Borghetti, Marco

    2006-01-01

    Intra-annual radial growth rates and durations in trees are reported to differ greatly in relation to species, site and environmental conditions. However, very similar dynamics of cambial activity and wood formation are observed in temperate and boreal zones. Here, we compared weekly xylem cell production and variation in stem circumference in the main northern hemisphere conifer species (genera Picea, Pinus, Abies and Larix) from 1996 to 2003. Dynamics of radial growth were modeled with a Gompertz function, defining the upper asymptote (A), x-axis placement (beta) and rate of change (kappa). A strong linear relationship was found between the constants beta and kappa for both types of analysis. The slope of the linear regression, which corresponds to the time at which maximum growth rate occurred, appeared to converge towards the summer solstice. The maximum growth rate occurred around the time of maximum day length, and not during the warmest period of the year as previously suggested. The achievements of photoperiod could act as a growth constraint or a limit after which the rate of tree-ring formation tends to decrease, thus allowing plants to safely complete secondary cell wall lignification before winter.

  13. Effect of temperature on sulphate reduction, growth rate and growth yield in five psychrophilic sulphate-reducing bacteria from Arctic sediments

    DEFF Research Database (Denmark)

    Knoblauch, C.; Jørgensen, BB

    1999-01-01

    and T(opt). For strains LSv21 and LSv514, however, growth yields were highest at the lowest temperatures, around 0 degrees C. The results indicate that psychrophilic sulphate-reducing bacteria are specially adapted to permanently low temperatures by high relative growth rates and high growth yields......Five psychrophilic sulphate-reducing bacteria (strains ASv26, LSv21, PSv29, LSv54 and LSv514) isolated from Arctic sediments were examined for their adaptation to permanently low temperatures, All strains grew at -1.8 degrees C, the freezing point of sea water, but their optimum temperature...... for growth (T(opt)) were 7 degrees C (PSv29), 10 degrees C (ASv26, LSv54) and 18 degrees C (LSv21, LSv514), Although T(opt) was considerably above the in situ temperatures of their habitats (-1.7 degrees C and 2.6 degrees C), relative growth rates were still high at 0 degrees C, accounting for 25...

  14. Partial delamination of continental mantle lithosphere, uplift-related crust mantle decoupling, volcanism and basin formation: a new model for the Pliocene Quaternary evolution of the southern East-Carpathians, Romania

    Science.gov (United States)

    Chalot-Prat, F.; Girbacea, R.

    2000-11-01

    A geodynamic model is proposed for the Mid-Miocene to Quaternary evolution of the southern East-Carpathians in order to explain the relationships between shallow and deep geological phenomena that occurred synchronously during late-collision tectonics. In this area, an active volcanic zone cross-cuts since 2 My the suture between the overriding Tisza-Dacia and subducting European continental plates. Mafic calc-alkaline and alkaline magmas (south Harghita and Persani volcanoes) erupted contemporaneously. These magmas were supplied by partial melting of the mantle lithosphere of the subducting, and not of the overriding, plate. In an effort to decipher this geodynamically a-typical setting of magma generation, the spatial and temporal distribution of shallow and deep phenomena was successively examined in order to establish the degree of their interdependence. Our model indicates that intra-mantle delamination of the subducting European plate is the principal cause of a succession of events. It caused upwelling of the hot asthenosphere below a thinned continental lithosphere of the Carpathians, inducing the uplift of the lithosphere and its internal decoupling at the Moho level by isostatic and mostly thermal effects. During this uplift, the crust deformed flexurally whilst the mantle deformed in a ductile way. This triggered decompressional partial melting of the uppermost mantle lithosphere. Flexural deformation of the crust induced its fracturing, allowing for the rapid ascent of magmas to the surface, as well as reactivation of an older detachment horizon at the base of the Carpathian nappe stack above which the Brasov, Ciuc and Gheorghieni hinterland basins formed by extension and gravity spreading. The rapid subsidence of the Focsani foreland basin is controlled by the load exerted on the lithosphere by the delaminated mantle slab that is still attached to it. In this model, crust-mantle decoupling, magma genesis and volcanism, local near-surface hinterland

  15. Temperature Effects on the Growth Rates and Photosynthetic Activities of Symbiodinium Cells

    Directory of Open Access Journals (Sweden)

    Widiastuti Karim

    2015-06-01

    Full Text Available Coral bleaching is caused by environmental stress and susceptibility to bleaching stress varies among types of coral. The physiological properties of the algal symbionts (Symbiodinium spp., especially extent of damage to PSII and its repair capacity, contribute importantly to this variability in stress susceptibility. The objective of the present study was to investigate the relationship between the growth rates and photosynthetic activities of six cultured strains of Symbiodinium spp. (clades A, B, C, D, and F at elevated temperature (33 °C. We also observed the recovery of photodamaged-PSII in the presence or absence of a chloroplast protein synthesis inhibitor (lincomycin. The growth rates and photochemical efficiencies of PSII (Fv/Fm decreased in parallel at high temperature in thermally sensitive strains, B-K100 (clade B followed by culture name and A-Y106, but not in thermally tolerant strains, F-K102 and D-K111. In strains A-KB8 and C-Y103, growth declined markedly at high temperature, but Fv/Fm decreased only slightly. These strains may reallocate energy from growth to the repair of damaged photosynthetic machineries or protection pathways. Alternatively, since recoveries of photo-damaged PSII at 33 °C were modest in strains A-KB8 and C-Y103, thermal stressing of other metabolic pathways may have reduced growth rates in these two strains. This possibility should be explored in future research efforts.

  16. Constant savings rates and quasi-arithmetic population growth under exhaustible resource constraints

    NARCIS (Netherlands)

    Asheim, G.B.; Buchholz, W.; Hartwick, J.M.; Mitra, T.; Withagen, C.A.A.M.

    2007-01-01

    In the Dasgupta–Heal–Solow–Stiglitz (DHSS) model of capital accumulation and resource depletion we show the following equivalence: if an efficient path has constant (gross and net of population growth) savings rates, then population growth must be quasi-arithmetic and the path is a maximin or a

  17. Ant Larval Demand Reduces Aphid Colony Growth Rates in an Ant-Aphid Interaction

    Directory of Open Access Journals (Sweden)

    James M. Cook

    2012-02-01

    Full Text Available Ants often form mutualistic interactions with aphids, soliciting honeydew in return for protective services. Under certain circumstances, however, ants will prey upon aphids. In addition, in the presence of ants aphids may increase the quantity or quality of honeydew produced, which is costly. Through these mechanisms, ant attendance can reduce aphid colony growth rates. However, it is unknown whether demand from within the ant colony can affect the ant-aphid interaction. In a factorial experiment, we tested whether the presence of larvae in Lasius niger ant colonies affected the growth rate of Aphis fabae colonies. Other explanatory variables tested were the origin of ant colonies (two separate colonies were used and previous diet (sugar only or sugar and protein. We found that the presence of larvae in the ant colony significantly reduced the growth rate of aphid colonies. Previous diet and colony origin did not affect aphid colony growth rates. Our results suggest that ant colonies balance the flow of two separate resources from aphid colonies- renewable sugars or a protein-rich meal, depending on demand from ant larvae within the nest. Aphid payoffs from the ant-aphid interaction may change on a seasonal basis, as the demand from larvae within the ant colony waxes and wanes.

  18. Re-alimentation in harbor seal pups: effects on the somatotropic axis and growth rate.

    Science.gov (United States)

    Richmond, Julie P; Norris, Tenaya; Zinn, Steven A

    2010-01-15

    The metabolic hormones, growth hormone (GH) and insulin-like growth factor (IGF)-I, together with IGF binding proteins (IGFBP), have been well studied in domestic species and are the primary components of the somatotropic axis. This hormone axis is responsive to nutrient intake, associated with growth rate, and accretion of protein and adipose. However, this relationship has not been evaluated in species that rely heavily on adipose stores for survival, such as pinnipeds. The primary objectives of this research were to investigate the response of the somatotropic axis to reduced nutrient intake and re-alimentation in rehabilitated harbor seal pups, and to assess if these hormones are related to nutritional status and growth rate in harbor seals. Stranded harbor seal pups (n=24) arrived at the rehabilitation facility very thin after fasting for several days (nutritional nadir). Throughout rehabilitation nutrient intake increased and pups gained mass and body condition. Concentrations of GH and IGFBP-2 decreased with re-alimentation, while IGF-I and IGFBP-3 concentrations increased. Overall, GH and IGFBP-2 were negatively associated and IGF-I and IGFBP-3 were positively associated with growth rate and increased body condition of harbor sea pups. Further, the magnitude of the growth response was related to the magnitude in response of the somatotropic axis to varied levels of intake. These data suggest that multiple components of the somatotropic axis may be used to assess the energy status of individuals and may also provide information on the level of feed intake that is predictive of growth rate.

  19. Plant allometry, leaf nitrogen and phosphorus stoichiometry, and interspecific trends in annual growth rates.

    Science.gov (United States)

    Niklas, Karl J

    2006-02-01

    Life forms as diverse as unicellular algae, zooplankton, vascular plants, and mammals appear to obey quarter-power scaling rules. Among the most famous of these rules is Kleiber's (i.e. basal metabolic rates scale as the three-quarters power of body mass), which has a botanical analogue (i.e. annual plant growth rates scale as the three-quarters power of total body mass). Numerous theories have tried to explain why these rules exist, but each has been heavily criticized either on conceptual or empirical grounds. N,P-STOICHIOMETRY: Recent models predicting growth rates on the basis of how total cell, tissue, or organism nitrogen and phosphorus are allocated, respectively, to protein and rRNA contents may provide the answer, particularly in light of the observation that annual plant growth rates scale linearly with respect to standing leaf mass and that total leaf mass scales isometrically with respect to nitrogen but as the three-quarters power of leaf phosphorus. For example, when these relationships are juxtaposed with other allometric trends, a simple N,P-stoichiometric model successfully predicts the relative growth rates of 131 diverse C3 and C4 species. The melding of allometric and N,P-stoichiometric theoretical insights provides a robust modelling approach that conceptually links the subcellular 'machinery' of protein/ribosomal metabolism to observed growth rates of uni- and multicellular organisms. Because the operation of this 'machinery' is basic to the biology of all life forms, its allometry may provide a mechanistic explanation for the apparent ubiquity of quarter-power scaling rules.

  20. The daily weight gain, growth rate and length-weight relationships of ...

    African Journals Online (AJOL)

    The daily weight gain, growth rate and length-weight relationships of Clarias gariepinus, Heterobranchus longifilis and their reciprocal hybrids (Pisces: Clariidae) reared under ambient environmental conditions.

  1. Rate-dependent mode I interlaminar crack growth mechanisms in graphite/epoxy and graphite/PEEK

    Science.gov (United States)

    Gillespie, J. W., Jr.; Carlsson, L. A.; Smiley, A. J.

    1987-01-01

    In this paper the mode I fracture behavior of graphite/epoxy and graphite/PEEK composites is examined over four decades of crosshead rates (0.25-250 mm/min). Straight-sided double-cantilever-beam specimens consisting of unidirectional laminates were tested at room temperature. For graphite/epoxy the load-deflection response was linear to fracture, and stable slow crack growth initiating at the highest load level was observed for all rates tested. In contrast, mode I crack growth in the graphite/PEEK material was often unstable and showed stick-slip behavior. Subcritical crack growth occurring prior to the onset of fracture was observed at intermediate displacement rates. A mechanism for the fracture behavior of the graphite/PEEK material (based on viscoelastic, plastic, and microcrack coalescence in the process zone) is proposed and related to the observed rate-dependent phenomena.

  2. On the relationship between tumour growth rate and survival in non-small cell lung cancer

    Directory of Open Access Journals (Sweden)

    Hitesh B. Mistry

    2017-11-01

    Full Text Available A recurrent question within oncology drug development is predicting phase III outcome for a new treatment using early clinical data. One approach to tackle this problem has been to derive metrics from mathematical models that describe tumour size dynamics termed re-growth rate and time to tumour re-growth. They have shown to be strong predictors of overall survival in numerous studies but there is debate about how these metrics are derived and if they are more predictive than empirical end-points. This work explores the issues raised in using model-derived metric as predictors for survival analyses. Re-growth rate and time to tumour re-growth were calculated for three large clinical studies by forward and reverse alignment. The latter involves re-aligning patients to their time of progression. Hence, it accounts for the time taken to estimate re-growth rate and time to tumour re-growth but also assesses if these predictors correlate to survival from the time of progression. I found that neither re-growth rate nor time to tumour re-growth correlated to survival using reverse alignment. This suggests that the dynamics of tumours up until disease progression has no relationship to survival post progression. For prediction of a phase III trial I found the metrics performed no better than empirical end-points. These results highlight that care must be taken when relating dynamics of tumour imaging to survival and that bench-marking new approaches to existing ones is essential.

  3. Effects of void anisotropy on the ignition and growth rates of energetic materials

    Science.gov (United States)

    Rai, Nirmal Kumar; Sen, Oishik; Udaykumar, H. S.

    2017-06-01

    Initiation of heterogeneous energetic materials is thought to occur at hot spots; reaction fronts propagate from sites of such hot spots into the surrounding material resulting in complete consumption of the material. Heterogeneous materials, such as plastic bonded explosives (PBXs) and pressed materials contain numerous voids, defects and interfaces at which hot spots can occur. Amongst the various mechanisms of hot spot formation, void collapse is considered to be the predominant one in the high strain rate loading conditions. It is established in the past the shape of the voids has a significant effect on the initiation behavior of energetic materials. In particular, void aspect ratio and orientations play an important role in this regard. This work aims to quantify the effects of void aspect ratio and orientation on the ignition and growth rates of chemical reaction from the hot spot. A wide range of aspect ratio and orientations is considered to establish a correlation between the ignition and growth rates and the void morphology. The ignition and growth rates are obtained from high fidelity reactive meso-scale simulations. The energetic material considered in this work is HMX and Tarver McGuire HMX decomposition model is considered to capture the reaction mechanism of HMX. The meso-scale simulations are performed using a Cartesian grid based Eulerian solver SCIMITAR3D. The void morphology is shown to have a significant effect on the ignition and growth rates of HMX.

  4. Constant Growth Rate Can Be Supported by Decreasing Energy Flux and Increasing Aerobic Glycolysis

    Directory of Open Access Journals (Sweden)

    Nikolai Slavov

    2014-05-01

    Full Text Available Fermenting glucose in the presence of enough oxygen to support respiration, known as aerobic glycolysis, is believed to maximize growth rate. We observed increasing aerobic glycolysis during exponential growth, suggesting additional physiological roles for aerobic glycolysis. We investigated such roles in yeast batch cultures by quantifying O2 consumption, CO2 production, amino acids, mRNAs, proteins, posttranslational modifications, and stress sensitivity in the course of nine doublings at constant rate. During this course, the cells support a constant biomass-production rate with decreasing rates of respiration and ATP production but also decrease their stress resistance. As the respiration rate decreases, so do the levels of enzymes catalyzing rate-determining reactions of the tricarboxylic-acid cycle (providing NADH for respiration and of mitochondrial folate-mediated NADPH production (required for oxidative defense. The findings demonstrate that exponential growth can represent not a single metabolic/physiological state but a continuum of changing states and that aerobic glycolysis can reduce the energy demands associated with respiratory metabolism and stress survival.

  5. Human disturbance influences reproductive success and growth rate in California sea lions (Zalophus californianus.

    Directory of Open Access Journals (Sweden)

    Susannah S French

    Full Text Available The environment is currently undergoing changes at both global (e.g., climate change and local (e.g., tourism, pollution, habitat modification scales that have the capacity to affect the viability of animal and plant populations. Many of these changes, such as human disturbance, have an anthropogenic origin and therefore may be mitigated by management action. To do so requires an understanding of the impact of human activities and changing environmental conditions on population dynamics. We investigated the influence of human activity on important life history parameters (reproductive rate, and body condition, and growth rate of neonate pups for California sea lions (Zalophus californianus in the Gulf of California, Mexico. Increased human presence was associated with lower reproductive rates, which translated into reduced long-term population growth rates and suggested that human activities are a disturbance that could lead to population declines. We also observed higher body growth rates in pups with increased exposure to humans. Increased growth rates in pups may reflect a density dependent response to declining reproductive rates (e.g., decreased competition for resources. Our results highlight the potentially complex changes in life history parameters that may result from human disturbance, and their implication for population dynamics. We recommend careful monitoring of human activities in the Gulf of California and emphasize the importance of management strategies that explicitly consider the potential impact of human activities such as ecotourism on vertebrate populations.

  6. Higher Growth Rate of Branch Duct Intraductal Papillary Mucinous Neoplasms Associates With Worrisome Features.

    Science.gov (United States)

    Kolb, Jennifer M; Argiriadi, Pamela; Lee, Karen; Liu, Xiaoyu; Bagiella, Emilia; Lucas, Aimee L; Kim, Michelle Kang; Kumta, Nikhil A; Nagula, Satish; Sarpel, Umut; DiMaio, Christopher J

    2018-03-11

    For patients with branch duct intraductal papillary mucinous neoplasms (BD-IPMNs, cysts), it is a challenge to identify those at high risk for malignant lesions. We sought to identify factors associated with development of pancreatic cancer, focusing on neoplasm growth rate. We performed a retrospective study of 189 patients with BD-IPMNs who underwent at least 2 contrast-enhanced cross-sectional imaging studies, 1 year or more apart, at a tertiary referral center from January 2003 through 2013. Patients with cysts that had Fukuoka worrisome or high-risk features were excluded. Two radiologists reviewed all images. Cyst size was recorded at the initial and final imaging studies and growth rate was calculated. We collected patient demographic data, cyst characteristics, and clinical outcomes; univariate logistic regression models were used to determine the odds of developing worrisome features. The primary outcomes were to determine growth rate of low-risk BD-IPMNs and to assess whether cyst growth rate correlates high-risk features of IPMNs. Based on image analyses, cysts were initially a median 11 mm (range, 3-31 mm) and their final size was 12.5 mm (range, 3-42 mm). After a median follow-up time of 56 months (range, 12-163 months), the median cyst growth rate was 0.29 mm/year. Twelve patients developed worrisome features, no patients developed high-risk features, 4 patients had surgical resection, and no cancers developed. The rate of BD-IPMN growth was greater in patients who developed worrisome features than those who did not (2.84 mm/year vs 0.23 mm/year; P < .001). The odds of developing worrisome features increased for each unit (mm) increase in cyst size (odds ratio, 1.149; 95% CI, 1.035-1.276, P = .009). In a retrospective analysis of images from patients with BD-IPMN, we found low-risk BD-IPMNs to grow at an extremely low rate (less than 0.3 mm/year). BD-IPMNs in only about 6% of patients developed worrisome features, and none developed high-risk features

  7. Determination of a cohesive law for delamination modelling - Accounting for variation in crack opening and stress state across the test specimen width

    DEFF Research Database (Denmark)

    Joki, R. K.; Grytten, F.; Hayman, Brian

    2016-01-01

    by differentiating the fracture resistance with respect to opening displacement at the initial location of the crack tip, measured at the specimen edge. 2) Extend the bridging law to a cohesive law by accounting for crack tip fracture energy. 3) Fine-tune the cohesive law through an iterative modelling approach so......The cohesive law for Mode I delamination in glass fibre Non-Crimped Fabric reinforced vinylester is determined for use in finite element models. The cohesive law is derived from a delamination test based on DCB specimens loaded with pure bending moments taking into account the presence of large...... that the changing state of stress and deformation across the width of the test specimen is taken into account. The changing state of stress and deformation across the specimen width is shown to be significant for small openings (small fracture process zone size). This will also be important for the initial part...

  8. Growth rates in modern speleothems from Santana Cave, Brazil, by the 210Pb-method

    International Nuclear Information System (INIS)

    Bonotto, D.M.; Karmann, I.; Baskaran, M.M.

    2012-01-01

    The Santana Cave is located at the Upper Ribeira Touristic State Park (PETAR-Parque Estadual Turístico do Alto Ribeira) in southern São Paulo State, Brazil. This paper describes 210 Pb activity concentration data in soda straw stalactites samples collected at Salão das Flores in Santana Cave that is a fossil tributary of the cave river. Non-expensive alpha counting following some analytical steps for extracting and depositing 210 Po were used for providing the 210 Pb data. In the analyzed samples, 210 Pb values of increasingly older samples fitted an exponential curve, thus suggesting that the production of 210 Pb has been constant with time. Also, the near-ideal fit indicated that the growth was uniform and there was no break in the continuous growth. The soda straw growth rates were determined from the best fit to the exponential curve through the 210 Pb activity concentration. The results of the measurements allowed estimate a longitudinal rate corresponding to 1.3 mm/yr and a lateral rate of 0.01 mm/yr, which permitted calculate times of 70 years and 317–498 years for their formation, respectively. The lateral growth rate is compatible with values from studies of chemical weathering rates held under laboratory and natural conditions.

  9. An inverse modeling procedure to determine particle growth and nucleation rates from measured aerosol size distributions

    Directory of Open Access Journals (Sweden)

    B. Verheggen

    2006-01-01

    Full Text Available Classical nucleation theory is unable to explain the ubiquity of nucleation events observed in the atmosphere. This shows a need for an empirical determination of the nucleation rate. Here we present a novel inverse modeling procedure to determine particle nucleation and growth rates based on consecutive measurements of the aerosol size distribution. The particle growth rate is determined by regression analysis of the measured change in the aerosol size distribution over time, taking into account the effects of processes such as coagulation, deposition and/or dilution. This allows the growth rate to be determined with a higher time-resolution than can be deduced from inspecting contour plots ('banana-plots''. Knowing the growth rate as a function of time enables the evaluation of the time of nucleation of measured particles of a certain size. The nucleation rate is then obtained by integrating the particle losses from time of measurement to time of nucleation. The regression analysis can also be used to determine or verify the optimum value of other parameters of interest, such as the wall loss or coagulation rate constants. As an example, the method is applied to smog chamber measurements. This program offers a powerful interpretive tool to study empirical aerosol population dynamics in general, and nucleation and growth in particular.

  10. Effect of repeated oral therapeutic doses of methylphenidate on food intake and growth rate in rats.

    Science.gov (United States)

    Alam, Nausheen; Najam, Rahila

    2015-01-01

    Central nervous system stimulants are known to produce anorexia. Previous data suggest that methylphenidate can have variable effects on caloric intake and growth rate. A dose-response study was performed to monitor caloric intake, liquid intake and growth rate in rats following repeated administration of human oral therapeutic doses 2 mg/kg/day, 5mg/kg/day and 8mg/kg/day of methylphenidate. We found that food intake and water intake, increased in all weeks and at all doses used in the study. Growth rate increased more at higher dose (8mg/kg/day) and at low dose (2mg/kg/day) of methylphenidate in 1(st) and 2(nd) week whereas more decreased by the above doses in 3(rd) week, suggesting that food stimulation leads to initial increase in growth rate but long term administration of methylphenidate attenuate growth rate that is not due to modulation of appetite but may be due to anxiety and increased activity produce by stimulants. A possible role of DA, 5HT receptors in modulation of appetite and anxiety is discussed.

  11. Growth rate variation of the stalked barnacle Pollicipes pollicipes (Crustacea: Cirripedia using calcein as a chemical marker

    Directory of Open Access Journals (Sweden)

    David Jacinto

    2015-03-01

    Full Text Available This study describes the use of calcein as a chemical tagging methodology to estimate growth rate variation of the stalked barnacle Pollicipes pollicipes, an ecologically important intertidal species and economic resource, in SW Portugal. Calcein tagging had a high success rate (94% in marking both juvenile and adult barnacles for a period of 2.5 months, providing a valuable method for obtaining reliable data in growth studies of P. pollicipes. Growth rate decreased with barnacle size and was highly variable amongst individuals, particularly in smaller barnacles. No effect of shore level on barnacle growth was detected. Growth rates were higher in smaller juvenile barnacles, peaking at a 1.1-mm monthly increment in rostro-carinal length (RC for individuals with RC=5 mm, and decreased with barnacle size (monthly growth rates of 0.5 mm for adult barnacles with RC~12.5 mm. Growth rates observed in adults with commercial interest (RC ≥ 18 mm was < 0.25 mm per month. The advantages of tagging P. pollicipes with calcein were the possibility of mass marking individual barnacles of different size cohorts within a short period (less than 1 day of manipulation; and reduced time of fieldwork, which is very important because this species inhabits very exposed rocky shores.

  12. Determining the nucleation rate from the dimer growth probability

    NARCIS (Netherlands)

    Ter Horst, J.H.; Kashchiev, D.

    2005-01-01

    A new method is proposed for the determination of the stationary one-component nucleation rate J with the help of data for the growth probability P2 of a dimer which is the smallest cluster of the nucleating phase. The method is based on an exact formula relating J and P2, and is readily applicable

  13. Morphology and mycelial growth rate of Pleurotus spp. strains from the Mexican mixtec region

    Science.gov (United States)

    Guadarrama-Mendoza, P.C.; del Toro, G. Valencia; Ramírez-Carrillo, R.; Robles-Martínez, F.; Yáñez-Fernández, J.; Garín-Aguilar, M.E.; Hernández, C.G.; Bravo-Villa, G.

    2014-01-01

    Two native Pleurotus spp. strains (white LB-050 and pale pink LB-051) were isolated from rotten tree trunks of cazahuate (Ipomoea murucoides) from the Mexican Mixtec Region. Both strains were chemically dedikaryotized to obtain their symmetrical monokaryotic components (neohaplonts). This was achieved employing homogenization time periods from 60 to 65 s, and 3 day incubation at 28 °C in a peptone-glucose solution (PGS). Pairing of compatible neohaplonts resulted in 56 hybrid strains which were classified into the four following hybrid types: (R1-nxB1-n, R1-nxB2-1, R2-nxB1-n and R2-nxB2-1). The mycelial growth of Pleurotus spp. monokaryotic and dikaryotic strains showed differences in texture (cottony or floccose), growth (scarce, regular or abundant), density (high, regular or low), and pigmentation (off-white, white or pale pink). To determine the rate and the amount of mycelium growth in malt extract agar at 28 °C, the diameter of the colony was measured every 24 h until the Petri dish was completely colonized. A linear model had the best fit to the mycelial growth kinetics. A direct relationship between mycelial morphology and growth rate was observed. Cottony mycelium presented significantly higher growth rates (p < 0.01) in comparison with floccose mycelium. Thus, mycelial morphology can be used as criterion to select which pairs must be used for optimizing compatible-mating studies. Hybrids resulting from cottony neohaplonts maintained the characteristically high growth rates of their parental strains with the hybrid R1-nxB1-n being faster than the latter. PMID:25477920

  14. Growth rate enhancement of free-electron laser by two consecutive ...

    Indian Academy of Sciences (India)

    2014-06-03

    Jun 3, 2014 ... been the subject of many papers published by different groups all around the world. The radiation is generated by relativistic electron beam passing through a wiggler. ..... Shown in figure 2 are plots of growth rate, Im ¯k, vs.

  15. Sex-Based Differences in Adelie Penguin (Pygoscelis adeliae Chick Growth Rates and Diet.

    Directory of Open Access Journals (Sweden)

    Scott Jennings

    Full Text Available Sexually size-dimorphic species must show some difference between the sexes in growth rate and/or length of growing period. Such differences in growth parameters can cause the sexes to be impacted by environmental variability in different ways, and understanding these differences allows a better understanding of patterns in productivity between individuals and populations. We investigated differences in growth rate and diet between male and female Adélie Penguin (Pygoscelis adeliae chicks during two breeding seasons at Cape Crozier, Ross Island, Antarctica. Adélie Penguins are a slightly dimorphic species, with adult males averaging larger than adult females in mass (~11% as well as bill (~8% and flipper length (~3%. We measured mass and length of flipper, bill, tibiotarsus, and foot at 5-day intervals for 45 male and 40 female individually-marked chicks. Chick sex was molecularly determined from feathers. We used linear mixed effects models to estimate daily growth rate as a function of chick sex, while controlling for hatching order, brood size, year, and potential variation in breeding quality between pairs of parents. Accounting for season and hatching order, male chicks gained mass an average of 15.6 g d(-1 faster than females. Similarly, growth in bill length was faster for males, and the calculated bill size difference at fledging was similar to that observed in adults. There was no evidence for sex-based differences in growth of other morphological features. Adélie diet at Ross Island is composed almost entirely of two species--one krill (Euphausia crystallorophias and one fish (Pleuragramma antarctica, with fish having a higher caloric value. Using isotopic analyses of feather samples, we also determined that male chicks were fed a higher proportion of fish than female chicks. The related differences in provisioning and growth rates of male and female offspring provides a greater understanding of the ways in which ecological factors

  16. Maternal body size and condition determine calf growth rates in southern right whales

    DEFF Research Database (Denmark)

    Christiansen, Fredrik; Vivier, Fabien; Charlton, Claire

    2018-01-01

    The cost of reproduction is a key parameter determining a species' life history strategy. Despite exhibiting some of the fastest offspring growth rates among mammals, the cost of reproduction in baleen whales is largely unknown since standard field metabolic techniques cannot be applied. We...... quantified the cost of reproduction for southern right whales Eubalaena australis over a 3 mo breeding season. We did this by determining the relationship between calf growth rate and maternal rate of loss in energy reserves, using repeated measurements of body volume obtained from unmanned aerial vehicle...... period, and highlights the importance of sufficient maternal energy reserves for reproduction in this capital breeding species....

  17. Population Growth Rate: Teaching Guide. Measures of Progress Poster Kit Number 2.

    Science.gov (United States)

    World Bank, Washington, DC.

    This teaching guide accompanies the Population Growth Rate poster kit which is designed to teach students about population growth differences between rich and poor nations and about what people in developing countries are doing to help improve their quality of life. The guide is designed for use with: (1) a poster map of the world providing social…

  18. Role of temperature on growth and metabolic rate in the tenebrionid beetles Alphitobius diaperinus and Tenebrio molitor.

    Science.gov (United States)

    Bjørge, Julie Dahl; Overgaard, Johannes; Malte, Hans; Gianotten, Natasja; Heckmann, Lars-Henrik

    2018-03-10

    Insects are increasingly used as a dietary source for food and feed and it is therefore important to understand how rearing conditions affect growth and development of these agricultural animals. Temperature is arguably the most important factor affecting metabolism and growth rate in insects. Here, we investigated how rearing temperature affected growth rate, growth efficiency and macronutrient composition in two species of edible beetle larvae: Alphitobius diaperinus and Tenebrio molitor. Growth rates of both species were quantified at temperatures ranging from 15.2 to 38.0 °C after which we measured protein and lipid content of the different treatment groups. Metabolic rate was measured in a similar temperature range by measuring the rate of O 2 consumption (V·O 2 ) and CO 2 production (V·CO 2 ) using repeated measures closed respirometry. Using these measurements, we calculated the growth efficiency of mealworms by relating the energy assimilation rate to the metabolic rate. Maximum daily growth rates were 18.3% and 16.6% at 31 °C, for A. diaperinus and T. molitor respectively, and we found that A. diaperinus was better at maintaining growth at high temperatures while T. molitor had superior growth at lower temperatures. Both species had highest efficiencies of energy assimilation in the temperature range of 23.3-31.0 °C, with values close to 2 J assimilated/J metabolised in A. diaperinus and around 4 J assimilated/J metabolised in T. molitor. Compared to "conventional" terrestrial livestock, both species of insects were characterised by high growth rates and very high energy conversion efficiency at most experimental temperatures. For A. diaperinus, lipid content was approximately 30% of dry mass and protein content approximately 50% of dry mass across most temperatures. Temperature had a greater influence on the body composition of T. molitor. At 31.0 °C the lipid and protein content was measured to 47.4% and 37.9%, respectively but lipid

  19. Comparison of human dermal fibroblasts (HDFs) growth rate in culture media supplemented with or without basic fibroblast growth factor (bFGF).

    Science.gov (United States)

    Abdian, Narges; Ghasemi-Dehkordi, Payam; Hashemzadeh-Chaleshtori, Morteza; Ganji-Arjenaki, Mahbobe; Doosti, Abbas; Amiri, Beheshteh

    2015-12-01

    Basic fibroblast growth factor (bFGF or FGF-2) is a member of the FGF family secreted by different kinds of cells like HDFs and it is an important nutritional factor for cell growth and differentiation. The HDFs release bFGF in culture media at very low. The present study aims to investigate the HDFs growth rate in culture media supplemented either with or without bFGF. In brief, HDFs were isolated from human foreskin sample and were cultured in vitro in media containing bFGF and lack of this factor. The cells growth rate was calculated by trypan blue. The karyotyping was performed using G-banding to investigate the chromosomal abnormality of HDFs in both groups. Total RNA of each groups were extracted and cDNA samples were synthesized then, real-time Q-PCR was used to measure the expression level of p27kip1 and cyclin D1 genes normalized to internal control gene (GAPDH). The karyotype analysis showed that HDFs cultured in media or without bFGF had normal karyotype (46 chromosomes, XY) and chromosomal abnormalities were not observed. The cell growth rates in both groups were normal with proliferated exponentially but the slope of growth curve in HDFs cultured in media containing bFGF was increased. Karyotyp test showed that bFGF does not affect on cytogenetic stability of cells. The survey of p27kip1 and cyclin D1 genes by real-time Q-PCR showed that the expression level of these genes were up-regulated when adding bFGF in culture media (p culture media with growth factor like bFGF could enhance the proliferation and differentiation capacity of cells and improve cells growth rate. Similarly, fibroblast growth factors did not induce any chromosomal abnormality in cells. Furthermore, in HDFs cultured in bFGF supplemented media, the p27kip1 and cyclin D1 genes were up-regulated and suggesting an important role for bFGF in cell-cycle regulation and progression and fibroblast division stimulation. It also suggests that the effects of bFGF on different cell types with

  20. Influence of Cell-Cell Interactions on the Population Growth Rate in a Tumor

    Science.gov (United States)

    Chen, Yong

    2017-12-01

    The understanding of the macroscopic phenomenological models of the population growth at a microscopic level is important to predict the population behaviors emerged from the interactions between the individuals. In this work, we consider the influence of the population growth rate R on the cell-cell interaction in a tumor system and show that, in most cases especially small proliferative probabilities, the regulative role of the interaction will be strengthened with the decline of the intrinsic proliferative probabilities. For the high replication rates of an individual and the cooperative interactions, the proliferative probability almost has no effect. We compute the dependences of R on the interactions between the cells under the approximation of the nearest neighbor in the rim of an avascular tumor. Our results are helpful to qualitatively understand the influence of the interactions between the individuals on the growth rate in population systems. Supported by the National Natural Science Foundation of China under Grant Nos. 11675008 and 21434001

  1. Parameter estimations in predictive microbiology: Statistically sound modelling of the microbial growth rate.

    Science.gov (United States)

    Akkermans, Simen; Logist, Filip; Van Impe, Jan F

    2018-04-01

    When building models to describe the effect of environmental conditions on the microbial growth rate, parameter estimations can be performed either with a one-step method, i.e., directly on the cell density measurements, or in a two-step method, i.e., via the estimated growth rates. The two-step method is often preferred due to its simplicity. The current research demonstrates that the two-step method is, however, only valid if the correct data transformation is applied and a strict experimental protocol is followed for all experiments. Based on a simulation study and a mathematical derivation, it was demonstrated that the logarithm of the growth rate should be used as a variance stabilizing transformation. Moreover, the one-step method leads to a more accurate estimation of the model parameters and a better approximation of the confidence intervals on the estimated parameters. Therefore, the one-step method is preferred and the two-step method should be avoided. Copyright © 2017. Published by Elsevier Ltd.

  2. Climate is a stronger driver of tree and forest growth rates than soil and disturbance

    NARCIS (Netherlands)

    Toledo, M.; Poorter, L.; Peña-Claros, M.; Alarcón, A.; Balcázar, J.; Leaño, C.; Licona, J.C.; Llanque, O.; Vroomans, V.; Zuidema, P.; Bongers, F.

    2011-01-01

    1. Essential resources such as water, nutrients and light vary over space and time and plant growth rates are expected to vary accordingly. We examined the effects of climate, soil and logging disturbances on diameter growth rates at the tree and stand level, using 165 1-ha permanent sample plots

  3. Effects of Phlomis umbrosa Root on Longitudinal Bone Growth Rate in Adolescent Female Rats

    Directory of Open Access Journals (Sweden)

    Donghun Lee

    2016-04-01

    Full Text Available This study aimed to investigate the effects of Phlomis umbrosa root on bone growth and growth mediators in rats. Female adolescent rats were administered P. umbrosa extract, recombinant human growth hormone or vehicle for 10 days. Tetracycline was injected intraperitoneally to produce a glowing fluorescence band on the newly formed bone on day 8, and 5-bromo-2′-deoxyuridine was injected to label proliferating chondrocytes on days 8–10. To assess possible endocrine or autocrine/paracrine mechanisms, we evaluated insulin-like growth factor-1 (IGF-1, insulin-like growth factor binding protein-3 (IGFBP-3 or bone morphogenetic protein-2 (BMP-2 in response to P. umbrosa administration in either growth plate or serum. Oral administration of P. umbrosa significantly increased longitudinal bone growth rate, height of hypertrophic zone and chondrocyte proliferation of the proximal tibial growth plate. P. umbrosa also increased serum IGFBP-3 levels and upregulated the expressions of IGF-1 and BMP-2 in growth plate. In conclusion, P. umbrosa increases longitudinal bone growth rate by stimulating proliferation and hypertrophy of chondrocyte with the increment of circulating IGFBP-3. Regarding the immunohistochemical study, the effect of P. umbrosa may also be attributable to upregulation of local IGF-1 and BMP-2 expressions in the growth plate, which can be considered as a GH dependent autocrine/paracrine pathway.

  4. Estimating blue whale skin isotopic incorporation rates and baleen growth rates: Implications for assessing diet and movement patterns in mysticetes

    Science.gov (United States)

    Busquets-Vass, Geraldine; Newsome, Seth D.; Calambokidis, John; Serra-Valente, Gabriela; Jacobsen, Jeff K.; Aguíñiga-García, Sergio; Gendron, Diane

    2017-01-01

    Stable isotope analysis in mysticete skin and baleen plates has been repeatedly used to assess diet and movement patterns. Accurate interpretation of isotope data depends on understanding isotopic incorporation rates for metabolically active tissues and growth rates for metabolically inert tissues. The aim of this research was to estimate isotopic incorporation rates in blue whale skin and baleen growth rates by using natural gradients in baseline isotope values between oceanic regions. Nitrogen (δ15N) and carbon (δ13C) isotope values of blue whale skin and potential prey were analyzed from three foraging zones (Gulf of California, California Current System, and Costa Rica Dome) in the northeast Pacific from 1996–2015. We also measured δ15N and δ13C values along the lengths of baleen plates collected from six blue whales stranded in the 1980s and 2000s. Skin was separated into three strata: basale, externum, and sloughed skin. A mean (±SD) skin isotopic incorporation rate of 163±91 days was estimated by fitting a generalized additive model of the seasonal trend in δ15N values of skin strata collected in the Gulf of California and the California Current System. A mean (±SD) baleen growth rate of 15.5±2.2 cm y-1 was estimated by using seasonal oscillations in δ15N values from three whales. These oscillations also showed that individual whales have a high fidelity to distinct foraging zones in the northeast Pacific across years. The absence of oscillations in δ15N values of baleen sub-samples from three male whales suggests these individuals remained within a specific zone for several years prior to death. δ13C values of both whale tissues (skin and baleen) and potential prey were not distinct among foraging zones. Our results highlight the importance of considering tissue isotopic incorporation and growth rates when studying migratory mysticetes and provide new insights into the individual movement strategies of blue whales. PMID:28562625

  5. Insights into crystal growth rates from a study of orbicular granitoids from western Australia

    Science.gov (United States)

    Zhang, J.; Lee, C. T.

    2017-12-01

    The purpose of this study is to develop new tools for constraining crystal growth rate in geologic systems. Of interest is the growth of crystals in magmatic systems because crystallization changes the rheology of a magma as well as provides surfaces on which bubbles can nucleate. To explore crystal growth in more detail, we conducted a case study of orbicular granitoids from western Australia. The orbicules occur as spheroids dispersed in a granitic matrix. Most orbicules have at least two to three concentric bands, composed of elongate and radially oriented hornblende surrounded by interstitial plagioclase. We show that mineral modes and hence bulk composition at the scale of the band is homogeneous from rim to core. Crystal number density decreases and crystal size increases from rim to core. These observations suggest that the orbicules crystallized rapidly from rim to core. We hypothesize that the orbicules are blobs of hot dioritic liquid injected into a cold granitic magma and subsequently cooled and solidified. Crystals stop growing when the mass transport rate tends to zero due to the low temperature. We estimated cooling timescales based on conductive cooling models, constraining crystal growth rates to be 10-6 to 10-5 m/s. We also show that the oscillatory banding is controlled by disequilibrium crystallization, wherein hornblende preferentially crystallizes, resulting in the diffusive growth of a chemical boundary layer enriched in plagioclase component, which in turns results in crystallization of plagioclase. We show that the correlation between the width of each crystallization couplet (band) with distance from orbicule rim is linear, with the slope corresponding to the square root of the ratio between chemical diffusivity in the growth medium and thermal diffusivity. We estimate chemical diffusivity of 2*10-7 m2/s, which is remarkably fast for silicate liquids but reasonable for diffusion in hot aqueous fluids, suggesting that crystallization

  6. Systems Level Regulation of Rhythmic Growth Rate and Biomass Accumulation in Grasses

    Energy Technology Data Exchange (ETDEWEB)

    Kay, Steve A. [Univ. of Southern California, Los Angeles, CA (United States)

    2017-10-20

    Objectives: Several breakthroughs have been recently made in our understanding of plant growth and biomass accumulation. It was found that plant growth is rhythmically controlled throughout the day by the circadian clock through a complex interplay of light and phytohormone signaling pathways. While plants such as the C4 energy crop sorghum (Sorghum bicolor (L.) Moench) and possibly the C3 grass Brachypodium distachyon also exhibit daily rhythms in growth rate, the molecular details of its regulation remain to be explored. A better understanding of diurnally regulated growth behavior in grasses may lead to species-specific mechanisms highly relevant to future strategies to optimize energy crop biomass yield. Here we propose to devise a systems approach to identify, in parallel, regulatory hubs associated with rhythmic growth in C3 and C4 plants. We propose to use rhythmicity in daily growth patterns to drive the discovery of regulatory network modules controlling biomass accumulation. Description: The project is divided in three main parts: 1) Performing time-lapse imaging and growth measurement in B. distachyon and S. bicolor to determine growth rate dynamic during the day/night cycle. Identifying growth-associated genes whose expression patterns follow the observed growth dynamics using deep sequencing technology, 2) identifying regulators of these genes by screening for DNA-binding proteins interacting with the growth-associated gene promoters identified in Aim 1. Screens will be performed using a validated yeast-one hybrid strategy paired with a specifically designed B. distachyon and S. bicolor transcription factor libraries (1000 clones each), and 3) Selecting 50 potential growth regulators from the screen for downstream characterization. The selection will be made by using a sytems biology approach by calculating the connectivity between growth rate, rhythmic gene expression profiles and TF expression profile and determine which TF is likely part of a hub

  7. Value of volume measurements in evaluating abdominal aortic aneurysms growth rate and need for surgical treatment

    Energy Technology Data Exchange (ETDEWEB)

    Kontopodis, Nikolaos, E-mail: kontopodisn@yahoo.gr [Department of Vascular Surgery, University of Crete Medical School, Heraklion (Greece); Metaxa, Eleni, E-mail: emmetaxa@gmail.com [Institute of Applied and Computational Mathematics, Foundation for Research and Technology-Hellas, Heraklion, Crete (Greece); Papaharilaou, Yannis, E-mail: yannisp@iacm.forth.gr [Institute of Applied and Computational Mathematics, Foundation for Research and Technology-Hellas, Heraklion, Crete (Greece); Georgakarakos, Efstratios, E-mail: efstratiosgeorg@gmail.com [Vascular Surgery Department, “Demokritus” University of Thrace Medical School, Alexandroupolis (Greece); Tsetis, Dimitris, E-mail: tsetis@med.uoc.gr [Interventional Radiology Unit, Department of Radiology, University of Crete Medical School, Heraklion, Crete (Greece); Ioannou, Christos V., E-mail: ioannou@med.uoc.gr [Department of Vascular Surgery, University of Crete Medical School, Heraklion (Greece)

    2014-07-15

    Purpose: To examine whether indices other than the traditionally used abdominal aortic aneurysm (AAA) maximum diameter, such as AAA volume, intraluminal thrombus (ILT) thickness and ILT volume, may be superior to evaluate aneurismal enlargement. Materials and methods: Thirty-four small AAAs (initially presenting a maximum diameter <5.5 cm which is the threshold for surgical repair) with an initial and a follow-up CT were examined. Median increase and percentile annual change of these variables was calculated. Correlation between growth rates as determined by the new indices under evaluation and those of maximum diameter were assessed. AAAs were divided according to outcome (surveillance vs. elective repair after follow-up which is based on the maximum diameter criterion) and according to growth rate (high vs. low) based on four indices. Contingency between groups of high/low growth rate regarding each of the four indices on one hand and those regarding need for surgical repair on the other was assessed. Results: A strong correlation between growth rates of maximum diameter and those of AAA and ILT volumes could be established. Evaluation of contingency between groups of outcome and those of growth rate revealed significant associations only for AAA and ILT volumes. Subsequently AAAs with a rapid volumetric increase over time had a likelihood ratio of 10 to be operated compared to those with a slower enlargement. Regarding increase of maximum diameter, likelihood ratio between AAAs with rapid and those with slow expansion was only 3. Conclusion: Growth rate of aneurysms regarding 3Dimensional indices of AAA and ILT volumes is significantly associated with the need for surgical intervention while the same does not hold for growth rates determined by 2Dimensional indices of maximum diameter and ILT thickness.

  8. Value of volume measurements in evaluating abdominal aortic aneurysms growth rate and need for surgical treatment

    International Nuclear Information System (INIS)

    Kontopodis, Nikolaos; Metaxa, Eleni; Papaharilaou, Yannis; Georgakarakos, Efstratios; Tsetis, Dimitris; Ioannou, Christos V.

    2014-01-01

    Purpose: To examine whether indices other than the traditionally used abdominal aortic aneurysm (AAA) maximum diameter, such as AAA volume, intraluminal thrombus (ILT) thickness and ILT volume, may be superior to evaluate aneurismal enlargement. Materials and methods: Thirty-four small AAAs (initially presenting a maximum diameter <5.5 cm which is the threshold for surgical repair) with an initial and a follow-up CT were examined. Median increase and percentile annual change of these variables was calculated. Correlation between growth rates as determined by the new indices under evaluation and those of maximum diameter were assessed. AAAs were divided according to outcome (surveillance vs. elective repair after follow-up which is based on the maximum diameter criterion) and according to growth rate (high vs. low) based on four indices. Contingency between groups of high/low growth rate regarding each of the four indices on one hand and those regarding need for surgical repair on the other was assessed. Results: A strong correlation between growth rates of maximum diameter and those of AAA and ILT volumes could be established. Evaluation of contingency between groups of outcome and those of growth rate revealed significant associations only for AAA and ILT volumes. Subsequently AAAs with a rapid volumetric increase over time had a likelihood ratio of 10 to be operated compared to those with a slower enlargement. Regarding increase of maximum diameter, likelihood ratio between AAAs with rapid and those with slow expansion was only 3. Conclusion: Growth rate of aneurysms regarding 3Dimensional indices of AAA and ILT volumes is significantly associated with the need for surgical intervention while the same does not hold for growth rates determined by 2Dimensional indices of maximum diameter and ILT thickness

  9. The Effect of CO2 Injection on Macroalgae Gelidium latifolium Biomass Growth Rate and Carbohydrate Content

    Directory of Open Access Journals (Sweden)

    Mujizat Kawaroe

    2016-06-01

    Full Text Available There are many species of macroalga grow in marine ecosystem and potentially as raw material for bioethanol resource. Bioethanol is a conversion result of carbohydrate, one of macroalgae biomass content. The exploration of macroalgae require information about  growth rate ability to determine availability in the nature. This research analyze growth rate and carbohydrate content of marine macroalga Gelidium latifolium on cultivation using varied injection of carbon dioxide and aeration. The treatments were control (K, 2000 cc CO2 injection and aeration (P1, 3000 cc CO2 injection and aeration (P2, 2000 cc CO2 injection without aeration (P3, and 3000 cc CO2 injection without aeration (P4. Samples weight were 3 gram in early cultivation on laboratorium scale for 42 days observation. The results showed that the daily growth rate Gelidium latifolium during the study ranged from 0.02-1.06%. The highest daily growth rate was 1.06±0.14% (P2. Carbohydrate yield was 18.23% in early cultivation then 19.40% (K and P2, 20.40% (P1, 16.87% (K3, and 16.40% (P4 after cultivation. The high of carbohydrates value may not guarantee the sustainable Gelidium latifolium biomass utilization as raw material for bioethanol production because of the low growth rate, thus it is necessary to modified and encourage cultivation method effectively. Keywords: CO2 injection, growth rate, carbohydrate, macroalgae, Gelidium latifolium

  10. Interstate Differences on Economic Growth Rates in Australia, 1953-54 to 1990-91

    OpenAIRE

    Harris, P; Harris, D

    1992-01-01

    This paper examines interstate differences in economic growth rates in Australia over the period 1953-54 to 1990-91 using a six State classification (with ACT included in New South Wales and the Northern Territory in South Australia). The economic growth rate is measured by the increase in constant price gross state product at factor cost (GSP) per head of population over time, using three year moving averages of GSP and population to remove some of the annual fluctuations in the data. The an...

  11. In situ growth rates and biofilm development of Pseudomonas aeruginosa populations in chronic lung infections

    DEFF Research Database (Denmark)

    Yang, L.; Haagensen, J.A.; Jelsbak, L.

    2008-01-01

    matrix, whereas nonmucoid variants were present mainly as dispersed cells. To obtain estimates of the growth rates of P. aeruginosa in CF lungs, we used quantitative FISH to indirectly measure growth rates of bacteria in sputum samples (reflecting the in vivo lung conditions). The concentration of r......The growth dynamics of bacterial pathogens within infected hosts are a fundamental but poorly understood feature of most infections. We have focused on the in situ distribution and growth characteristics of two prevailing and transmissible Pseudomonas aeruginosa clones that have caused chronic lung......RNA in bacteria isolated from sputa was measured and correlated with the rRNA contents of the same bacteria growing in vitro at defined rates. The results showed that most cells were actively growing with doubling times of between 100 and 200 min, with some growing even faster. Only a small stationary...

  12. Flexibility in metabolic rate confers a growth advantage under changing food availability.

    Science.gov (United States)

    Auer, Sonya K; Salin, Karine; Rudolf, Agata M; Anderson, Graeme J; Metcalfe, Neil B

    2015-09-01

    1. Phenotypic flexibility in physiological, morphological and behavioural traits can allow organisms to cope with environmental challenges. Given recent climate change and the degree of habitat modification currently experienced by many organisms, it is therefore critical to quantify the degree of phenotypic variation present within populations, individual capacities to change and what their consequences are for fitness. 2. Flexibility in standard metabolic rate (SMR) may be particularly important since SMR reflects the minimal energetic cost of living and is one of the primary traits underlying organismal performance. SMR can increase or decrease in response to food availability, but the consequences of these changes for growth rates and other fitness components are not well known. 3. We examined individual variation in metabolic flexibility in response to changing food levels and its consequences for somatic growth in juvenile brown trout (Salmo trutta). 4. SMR increased when individuals were switched to a high food ration and decreased when they were switched to a low food regime. These shifts in SMR, in turn, were linked with individual differences in somatic growth; those individuals that increased their SMR more in response to elevated food levels grew fastest, while growth at the low food level was fastest in those individuals that depressed their SMR most. 5. Flexibility in energy metabolism is therefore a key mechanism to maximize growth rates under the challenges imposed by variability in food availability and is likely to be an important determinant of species' resilience in the face of global change. © 2015 The Authors. Journal of Animal Ecology published by John Wiley & Sons Ltd on behalf of British Ecological Society.

  13. Effect of Alfvén waves on the growth rate of the electron-cyclotron maser emission

    Energy Technology Data Exchange (ETDEWEB)

    Wu, D. J., E-mail: djwu@pmo.ac.cn [Purple Mountain Observatory, CAS, Nanjing 210008 (China)

    2014-06-15

    By using the non-relativistic approximation for the calculation of growth rates, but taking account of the weakly relativistic modification for the electron-cyclotron resonance condition, it is shown that the effect of Alfvén waves (AWs) on the electron-cyclotron maser emission leads to the significant increase of the O-mode growth rate, but has little effect on the X-mode growth rate. We propose that this is because the O-mode wave has the field-aligned polarization sense in the same as the field-aligned oscillatory current, which is created by the field-aligned oscillatory motion of the energetic electrons caused via the presence of AWs. It is this field-aligned oscillatory current that contributes a novel growth rate to the O-mode wave but has little effect on the X-mode wave.

  14. How to determine control of growth rate in a chemostat. Using metabolic control analysis to resolve the paradox

    DEFF Research Database (Denmark)

    Snoep, Jacky L.; Jensen, Peter Ruhdal; Groeneveld, Philip

    1994-01-01

    how, paradoxically, one can determine control of growth rate, of growth yield and of other fluxes in a chemostat. We develop metabolic control analysis for the chemostat. this analysis does not depend on the particular way in which specific growth rate varies with the concentration of the growth...

  15. TEST OF THE CATCH-UP HYPOTHESIS IN AFRICAN AGRICULTURAL GROWTH RATES

    Directory of Open Access Journals (Sweden)

    Kalu Ukpai IFEGWU

    2015-11-01

    Full Text Available The paper tested the catch-up hypothesis in agricultural growth rates of twenty-six African countries. Panel data used was drawn from the Food and Agricultural Organization Statistics (FAOSTAT of the United Nations. The Data Envelopment Analysis Method for measuring productivity was used to estimate productivity growth rates. The cross-section framework consisting of sigma-convergence and beta-convergence was employed to test the catching up process. Catching up is said to exist if the value of beta is negative and significant. Since catching up does not necessarily imply narrowing of national productivity inequalities, sigma-convergence which measures inequality, was estimated for the same variables. The results showed evidence of the catch-up process, but failed to find a narrowing of productivity inequalities among countries.

  16. Effect of feeding frequency and feeding rate on growth performance ...

    African Journals Online (AJOL)

    Fish fed at higher feeding rates accumulated significantly more lipid within the body and had associated decreases in moisture, protein, and ash content, but carcass composition was unaffected by feeding frequency. Juvenile pompano show better growth performance when fed 10% BW/day 3 and 6 times a day.

  17. A comparison of growth rate of late Holocene stalagmites with atmospheric precipitation and temperature, and its implications for paleoclimatology

    Science.gov (United States)

    Railsback, L. Bruce

    2018-05-01

    Growth rate of stalagmites can vary with many factors of physical environment, ecology, and karst hydrogeology, to the extent that growth rates calculated from a carefully selected set of data from 80 stalagmites from around the world vary by a factor of 400 from smallest to largest. Growth rates of those 80 stalagmites nonetheless collectively show correlations to atmospheric precipitation and temperature that are non-trivial (r2 = 0.12 and 0.20, respectively) and unlikely to have arisen randomly (p = 0.002 and 0.00002). Those global relationships are also supported by previously published studies of individual drip sites. The general trend of growth rates is not a monotonic increase with precipitation; instead, it reaches a maximum at annual precipitation rates between 700 and 2300 mm/year, which both counters many model predictions that growth rates should increase monotonically with drip rate and complicates use of growth rate as a proxy for past precipitation. The general trend of growth rates among the 80 stalagmites is a monotonic increase with temperature. However, the low values of r2 in both of these general trends indicate that growth rate can be at best a qualitative rather than quantitative proxy of past conditions. Growth rate shows no statistically significant relationship to effective precipitation, seemingly because of the confounding effect of temperature. Growth rates of aragonite-bearing stalagmites are commonly greater than rates in stalagmites in which calcite is the only carbonate mineral, suggesting both the need for careful identification of mineralogy and the special applicability of aragonitic stalagmites in high-resolution studies. Aragonite has exceptionally great frequency in settings with low effective atmospheric precipitation, supporting previous linkages of that mineral to warm dry environments. Closely-spaced sampling used in recent paleoclimatological studies suggests that unexploited long-term low-resolution records of past

  18. Linear growth rates of resistive tearing modes with sub-Alfvénic streaming flow

    International Nuclear Information System (INIS)

    Wu, L. N.; Ma, Z. W.

    2014-01-01

    The tearing instability with sub-Alfvénic streaming flow along the external magnetic field is investigated using resistive MHD simulation. It is found that the growth rate of the tearing mode instability is larger than that without the streaming flow. With the streaming flow, there exist two Alfvén resonance layers near the central current sheet. The larger perturbation of the magnetic field in two closer Alfvén resonance layers could lead to formation of the observed cone structure and can largely enhance the development of the tearing mode for a narrower streaming flow. For a broader streaming flow, a larger separation of Alfvén resonance layers reduces the magnetic reconnection. The linear growth rate decreases with increase of the streaming flow thickness. The growth rate of the tearing instability also depends on the plasma beta (β). When the streaming flow is embedded in the current sheet, the growth rate increases with β if β  s , but decreases if β > β s . The existence of the specific value β s can be attributed to competition between the suppressing effect of β and the enhancing effect of the streaming flow on the magnetic reconnection. The critical value β s increases with increase of the streaming flow strength

  19. Methods of forecasting crack growth rate under creep conditions

    International Nuclear Information System (INIS)

    Ol'kin, S.I.

    1979-01-01

    Using construction aluminium alloy application possibility of linear mechanics of the destruction for quantitative description of crack development process under creepage conditions is investigated. It is shown, that the grade dependence between the stress intensity coefficient and the crack growth rate takes place only at certain combination of the sample geometry and creepage parameters, and consequently, its applicability in every given case must necessarily be tested experimentally

  20. Quorum sensing influences Vibrio harveyi growth rates in a manner not fully accounted for by the marker effect of bioluminescence.

    Science.gov (United States)

    Nackerdien, Zeena E; Keynan, Alexander; Bassler, Bonnie L; Lederberg, Joshua; Thaler, David S

    2008-02-27

    The light-emitting Vibrios provide excellent material for studying the interaction of cellular communication with growth rate because bioluminescence is a convenient marker for quorum sensing. However, the use of bioluminescence as a marker is complicated because bioluminescence itself may affect growth rate, e.g. by diverting energy. The marker effect was explored via growth rate studies in isogenic Vibrio harveyi (Vh) strains altered in quorum sensing on the one hand, and bioluminescence on the other. By hypothesis, growth rate is energy limited: mutants deficient in quorum sensing grow faster because wild type quorum sensing unleashes bioluminescence and bioluminescence diverts energy. Findings reported here confirm a role for bioluminescence in limiting Vh growth rate, at least under the conditions tested. However, the results argue that the bioluminescence is insufficient to explain the relationship of growth rate and quorum sensing in Vh. A Vh mutant null for all genes encoding the bioluminescence pathway grew faster than wild type but not as fast as null mutants in quorum sensing. Vh quorum sensing mutants showed altered growth rates that do not always rank with their relative increase or decrease in bioluminescence. In addition, the cell-free culture fluids of a rapidly growing Vibrio parahaemolyticus (Vp) strain increased the growth rate of wild type Vh without significantly altering Vh's bioluminescence. The same cell-free culture fluid increased the bioluminescence of Vh quorum mutants. The effect of quorum sensing on Vh growth rate can be either positive or negative and includes both bioluminescence-dependent and independent components. Bioluminescence tends to slow growth rate but not enough to account for the effects of quorum sensing on growth rate.

  1. Quorum sensing influences Vibrio harveyi growth rates in a manner not fully accounted for by the marker effect of bioluminescence.

    Directory of Open Access Journals (Sweden)

    Zeena E Nackerdien

    2008-02-01

    Full Text Available The light-emitting Vibrios provide excellent material for studying the interaction of cellular communication with growth rate because bioluminescence is a convenient marker for quorum sensing. However, the use of bioluminescence as a marker is complicated because bioluminescence itself may affect growth rate, e.g. by diverting energy.The marker effect was explored via growth rate studies in isogenic Vibrio harveyi (Vh strains altered in quorum sensing on the one hand, and bioluminescence on the other. By hypothesis, growth rate is energy limited: mutants deficient in quorum sensing grow faster because wild type quorum sensing unleashes bioluminescence and bioluminescence diverts energy. Findings reported here confirm a role for bioluminescence in limiting Vh growth rate, at least under the conditions tested. However, the results argue that the bioluminescence is insufficient to explain the relationship of growth rate and quorum sensing in Vh. A Vh mutant null for all genes encoding the bioluminescence pathway grew faster than wild type but not as fast as null mutants in quorum sensing. Vh quorum sensing mutants showed altered growth rates that do not always rank with their relative increase or decrease in bioluminescence. In addition, the cell-free culture fluids of a rapidly growing Vibrio parahaemolyticus (Vp strain increased the growth rate of wild type Vh without significantly altering Vh's bioluminescence. The same cell-free culture fluid increased the bioluminescence of Vh quorum mutants.The effect of quorum sensing on Vh growth rate can be either positive or negative and includes both bioluminescence-dependent and independent components. Bioluminescence tends to slow growth rate but not enough to account for the effects of quorum sensing on growth rate.

  2. Interest Rate Deregulation, Bank Development And Economic Growth In South Africa: An Empirical Investigation

    OpenAIRE

    Nicholas M Odhiambo

    2010-01-01

    In this paper the dynamic relationship between interest rate reforms, bank-based financial development and economic growth is examined – using two models in a stepwise fashion. In the first model, the impact of interest rate reforms on financial development is examined using a financial deepening model. In the second model, the dynamic causal relationship between financial development and economic growth is examined, by including investment as an intermittent variable in the bi-variate settin...

  3. Growth rate of matter perturbations as a probe of large-scale magnetism

    CERN Document Server

    Giovannini, Massimo

    2011-01-01

    The growth rate of matter perturbations is computed in a magnetized environment for the LambdaCDM and wCDM paradigms. It is argued that the baryons do not necessarily follow into the dark matter potential wells after they are released from the drag of the photons. The baryonic evolution equations inherit a forcing term whose explicit form depends on the plasma description and can be deduced, for instance, in the resistive magnetohydrodynamical approximation. After deriving an analytical expression for the growth rate applicable when dark energy does not cluster, the effects of relativistic corrections and of the inhomogeneities associated with the other species of the plasma are taken into account numerically. The spectral amplitudes and slopes of the stochastic magnetic background are selected to avoid appreciable distortions in the measured temperature and polarization anisotropies of the Cosmic Microwave Background. The growth of structures in the current paradigms of structure formation represents a compl...

  4. Matrix resin effects in composite delamination - Mode I fracture aspects

    Science.gov (United States)

    Hunston, Donald L.; Moulton, Richard J.; Johnston, Norman J.; Bascom, Willard D.

    1987-01-01

    A number of thermoset, toughened thermoset, and thermoplastic resin matrix systems were characterized for Mode I critical strain energy release rates, and their composites were tested for interlaminar critical strain energy release rates using the double cantilever beam method. A clear correlation is found between the two sets of data. With brittle resins, the interlaminar critical strain energy release rates are somewhat larger than the neat resin values due to a full transfer of the neat resin toughness to the composite and toughening mechanisms associated with crack growth. With tougher matrices, the higher critical strain energy release rates are only partially transferred to the composites, presumably because the fibers restrict the crack-tip deformation zones.

  5. The impact of risk management on internal and sustainable growth rate: Evidence from Tehran Stock Exchange

    Directory of Open Access Journals (Sweden)

    Hamid Reza Vakili Fard

    2014-09-01

    Full Text Available Measuring the relative risk of firms has been an open discussion among researchers. There are many studies on learning how leverage may influence on growth of the firms. This article reviews the relationship between risk management, internal and sustainable growth of accepted companies in Tehran stock exchange. The survey considers three types of risks including operating, financial and compound and investigates their relationships with internal growth rate as well as sustainable growth rate. Using some regression techniques, the study has determined negative and meaningful relationships between different types of leverage on side and internal as well as sustainable growth on the other side.

  6. Survey: Did the TFP Growth Rate in Japan Decline in the 1990s?(in Japanese)

    OpenAIRE

    INUI Tomohiko; KWON Hyeog Ug

    2004-01-01

    This paper surveys the body of research grounded on a basic question "Did the total factor productivity (TFP) growth rate in Japan decline in the 1990s?" In addition, using industry-level data of the Japan Industrial Productivity Database (JIP database) we estimate the mark-ups and the degree of returns to scale and then re-estimate TFP growth rates. Most of studies reviewed in this paper show a decline in TFP growth in the 1990s at the macro-level and the industry-level. There are some studi...

  7. Decreased growth rate of P. falciparum blood stage parasitemia with age in a holoendemic population.

    Science.gov (United States)

    Pinkevych, Mykola; Petravic, Janka; Chelimo, Kiprotich; Vulule, John; Kazura, James W; Moormann, Ann M; Davenport, Miles P

    2014-04-01

    In malaria holoendemic settings, decreased parasitemia and clinical disease is associated with age and cumulative exposure. The relative contribution of acquired immunity against various stages of the parasite life cycle is not well understood. In particular, it is not known whether changes in infection dynamics can be best explained by decreasing rates of infection, or by decreased growth rates of parasites in blood. Here, we analyze the dynamics of Plasmodium falciparum infection after treatment in a cohort of 197 healthy study participants of different ages. We use both polymerase chain reaction (PCR) and microscopy detection of parasitemia in order to understand parasite growth rates and infection rates over time. The more sensitive PCR assay detects parasites earlier than microscopy, and demonstrates a higher overall prevalence of infection than microscopy alone. The delay between PCR and microscopy detection is significantly longer in adults compared with children, consistent with slower parasite growth with age. We estimated the parasite multiplication rate from delay to PCR and microscopy detections of parasitemia. We find that both the delay between PCR and microscopy infection as well as the differing reinfection dynamics in different age groups are best explained by a slowing of parasite growth with age.

  8. Multi-omics approach to study the growth efficiency and amino acid metabolism in Lactococcus lactis at various specific growth rates

    Directory of Open Access Journals (Sweden)

    Arike Liisa

    2011-02-01

    Full Text Available Abstract Background Lactococcus lactis is recognised as a safe (GRAS microorganism and has hence gained interest in numerous biotechnological approaches. As it is fastidious for several amino acids, optimization of processes which involve this organism requires a thorough understanding of its metabolic regulations during multisubstrate growth. Results Using glucose limited continuous cultivations, specific growth rate dependent metabolism of L. lactis including utilization of amino acids was studied based on extracellular metabolome, global transcriptome and proteome analysis. A new growth medium was designed with reduced amino acid concentrations to increase precision of measurements of consumption of amino acids. Consumption patterns were calculated for all 20 amino acids and measured carbon balance showed good fit of the data at all growth rates studied. It was observed that metabolism of L. lactis became more efficient with rising specific growth rate in the range 0.10 - 0.60 h-1, indicated by 30% increase in biomass yield based on glucose consumption, 50% increase in efficiency of nitrogen use for biomass synthesis, and 40% reduction in energy spilling. The latter was realized by decrease in the overall product formation and higher efficiency of incorporation of amino acids into biomass. L. lactis global transcriptome and proteome profiles showed good correlation supporting the general idea of transcription level control of bacterial metabolism, but the data indicated that substrate transport systems together with lower part of glycolysis in L. lactis were presumably under allosteric control. Conclusions The current study demonstrates advantages of the usage of strictly controlled continuous cultivation methods combined with multi-omics approach for quantitative understanding of amino acid and energy metabolism of L. lactis which is a valuable new knowledge for development of balanced growth media, gene manipulations for desired product

  9. Growth rate characteristics of acidophilic heterotrophic organisms from mine waste rock piles

    Science.gov (United States)

    Yacob, T. W.; Silverstein, J.; Jenkins, J.; Andre, B. J.; Rajaram, H.

    2010-12-01

    Autotrophic iron oxidizing bacteria play a key role in pyrite oxidation and generation of acid mine drainage AMD. Scarcity of organic substrates in many disturbed sites insures that IOB have sufficient oxygen and other nutrients for growth. It is proposed that addition of organic carbon substrate to waste rock piles will result in enrichment of heterotrophic microorganisms limiting the role of IOB in AMD generation. Previous researchers have used the acidophilic heterotroph Acidiphilium cryptum as a model to study the effects of organic substrate addition on the pyrite oxidation/AMD cycle. In order to develop a quantitative model of effects such as competition for oxygen, it is necessary to use growth and substrate consumption rate expressions, and one approach is to choose a model strain such as A. cryptum for kinetic studies. However we have found that the growth rate characteristics of A. cryptum may not provide an accurate model of the remediation effects of organic addition to subsurface mined sites. Fluorescent in-situ hybridization (FISH) assays of extracts of mine waste rock enriched with glucose and yeast extract did not produce countable numbers of cells in the Acidiphilium genus, with a detection limit of3 x 104 cells/gram rock, despite evidence of the presence of well established heterotrophic organisms. However, an MPN enrichment produced heterotrophic population estimates of 1x107 and 1x109 cells/gram rock. Growth rate studies of A. cryptum showed that cultures took 120 hours to degrade 50% of an initial glucose concentration of 2,000 mg/L. However a mixed culture enriched from mine waste rock consumed 100% of the same amount of glucose in 24 hours. Substrate consumption data for the mixed culture were fit to a Monod growth model: {dS}/{dt} = μ_{max}S {( {X_0}/{Y} + S_0 -S )}/{(K_s +S)} Kinetic parameters were estimated utilizing a non linear regression method coupled with an ODE solver. The maximum specific growth rate of the mixed population with

  10. Effect of deposition conditions on the growth rate and electrical properties of ZnO thin films grown by MOCVD

    Energy Technology Data Exchange (ETDEWEB)

    Roro, K.T.; Botha, J.R.; Leitch, A.W.R. [Department of Physics, Nelson Mandela Metropolitan University, P.O. Box 77000, Port Elizabeth 6031 (South Africa)

    2008-07-01

    ZnO thin films have been grown on glass substrates by MOCVD. The effect of deposition conditions such as VI/II molar ratio, DEZn flow rate and total reactor pressure on the growth rate and electrical properties of the films was studied. It is found that the growth rate decreases with an increase in the VI/II molar ratio. This behaviour is ascribed to the competitive adsorption of reactant species on the growth surface. The growth rate increases with an increase in DEZn flow rate, as expected. It is shown that the carrier concentration is independent of the DEZn flow rate. An increase in the total reactor pressure yields a decrease in growth rate. This phenomenon is attributed to the depletion of the gas phase due to parasitic prereactions between zinc and oxygen species at high pressure. (copyright 2008 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim) (orig.)

  11. Investigation of the growth rate for joint fast breeder reactor and light water reactor operation

    International Nuclear Information System (INIS)

    Hanan, N.A.; Borg, C.R.; Ott, K.O.

    1977-07-01

    An investigation of fuel consumption and breeding characteristics of FBR-LWR joint operation is presented. The FBR operates in a closed cycle with joint-reprocessing of core and blanket material. The LWR-portion that runs on FBR plutonium operates in an open cycle. The growth rate of the system is defined based upon the fact that the discharge from the system will make up a fraction of an identical system; the system growth rate is found to have an almost linear dependence on the fraction of the LWR fed by plutonium from the FBR. The LWR growth rate, which is negative, is a constant and represents the fraction of the fuel burnt in the LWR-fraction that runs on FBR plutonium per year

  12. EFFECTS OF INTEREST RATE DEREGULATION ON AGRICULTURAL FINANCE AND GROWTH IN NIGERIA

    Directory of Open Access Journals (Sweden)

    Louis O. ONYISHI

    2015-03-01

    Full Text Available The study examined the effects of interest rate deregulation on agricultural finance and growth in Nigeria. The study specifically ascertained the factors that determine the aggregate credit volume to agriculture within the periods of regulation and deregulation in the Nigerian economy, determined the effects of government finance interventions on agricultural sector performance in the Nigerian economy, determined the periodic effects of macroeconomic financial indicators on Agriculture’s gross domestic product (GDP contribution to Nigerian economy and estimated the level of real credit growth of agricultural finance in Nigeria. Descriptive statistics, Ordinary Least Squares (OLS regression technique and chow test were used for data analysis. The chow test showed that there was a significant differential effect on the aggregate credit volume to agricultural sector between the regulated and deregulated regimes. Interest rate was an important determinant of aggregate credit volume to the agricultural sector in Nigeria, especially during the deregulated period but monetary authorities should ensure appropriate determination of interest rate level that will break the double-edge effect of interest rates on savers and investors.

  13. Influence of nutrition on ovulation rate and testicular growth of Merino sheep

    International Nuclear Information System (INIS)

    Rowe, J.B.

    1988-01-01

    The effect of nutrition on reproductive performance was studied in a series of experiments using two models. Increased supply of nutrients was based on feeding lupin grain as a supplement and measurements of testicular growth or ovulation rates were used to measure reproductive characteristics. Purified sources of protein and energy were provided to determine the macronutrient(s), supplied with lupin feeding, responsible for initiating increases in testicular growth and ovulation rate. Increases in both of these parameters were closely related to the supply of additional energy but not protein. The production of acetate and glucose resulting from supplementary feeding with 750 g lupins/d was measured using infusions of 14 C tracers. Subsequently, infusions of glucose and acetate (individually and in combination) were found to produce similar increases in ovulation rate to those measured in ewes receiving lupins. It was concluded that effects of nutrition on ovulation rate are associated with increased energy intake and may be mediated through pathways linked with the synthesis and/or utilization of glucose. (author). 18 refs, 2 figs, 3 tabs

  14. Impact of delays in plutonium use on the stationary growth rate of fast breeder reactor fuel

    International Nuclear Information System (INIS)

    Borg, R.C.; Ott, K.O.

    1977-07-01

    The hierarchy of the four growth rate expressions originally derived from an instantaneous reuse scheme is expanded to account for finite burnup in the core and blanket, β-decay of 241 Pu, core and blanket loading schemes, reuse delays due to reprocessing and fabricating fuel and external fuel cycle losses. The most general growth rate expression, obtained from the asymptotic slope of the accumulating fuel material in an expanding park of breeder reactors, is formally the same in both cases. Formulation of the growth rate based on the condensation of the detailed information of the equilibrium fuel cycle for a single reactor, is more complicated than without delays due to the composition difference between the average residing and excess discharge material. The third growth rate expression results from a slightly more complicated fuel-cycle eigenvalue problem than without delays. The last definition employs isotopic breeding worth factors obtained from the adjoint fuel cycle eigenvalue problem

  15. Effect of a hard coat layer on buckle delamination of thin ITO layers on a compliant elasto-plastic substrate: an experimental–numerical approach

    NARCIS (Netherlands)

    Sluis, van der O.; Abdallah, Amir; Bouten, P.C.P.; Timmermans, P.H.M.; Toonder, den J.M.J.; With, de G.

    2011-01-01

    Layer buckling and delamination is a common interfacial failure phenomenon in thin film multi-layer structures that are used in flexible display applications. Typically, the substrate is coated on both sides with a hybrid coating, calleda hard coat (HC), which acts as a gas barrier and also

  16. Constant growth rate can be supported by decreasing energy flux and increasing aerobic glycolysis

    NARCIS (Netherlands)

    Slavov, Nikolai; Budnik, Bogdan A; Schwab, David; Airoldi, Edoardo M; van Oudenaarden, Alexander

    2014-01-01

    Fermenting glucose in the presence of enough oxygen to support respiration, known as aerobic glycolysis, is believed to maximize growth rate. We observed increasing aerobic glycolysis during exponential growth, suggesting additional physiological roles for aerobic glycolysis. We investigated such

  17. Productivity dynamics of Livestock in southern peninsular India: A Compound growth rate analysis

    Directory of Open Access Journals (Sweden)

    G. Kathiravan 1 and S. Selvam 2

    2011-04-01

    Full Text Available Although India possesses the large volume of livestock, their productivity is abysmally low at global level. India, with its wide variation in geo-ecological parameters, elucidates a high variation in the productivity of its livestock, among regions. The compound growth rate of livestock productivity was worked out for the Southern Peninsular state of India, Tamil Nadu. The average productivity of milk in cross bred cows and buffaloes in Tamil Nadu was less than the national average, while the productivity desi cows was a bit a more. The annual compound growth rate of milk productivity among crossbred cows of Tamil Nadu was at meager 0.54 per cent during the period between 1998-1999 and 2006- 2007, whereas the productivity of milk in desi cows had improved from at an annual compound growth rate of 1.29 per cent. Notably, the milk productivity in buffaloes had declined at a rate of 0.29 per cent during the period under study. The annual compound growth of egg productivity in improved hens of Tamil Nadu was 20.87 per cent. The average annual productivity was 109.531 eggs, which improved from 70.623 in 1998-1999 to 197.084 in 2004-2005. Correspondingly, the productivity of desi hens also had a positive swing from the year 2003-2004 onwards. The results implied that the simulation of increased productivity, better farm financing and improved milk marketing could result in enhanced livestock production that would meet the future demands. [Veterinary World 2011; 4(2.000: 68-74

  18. Influence of growth rate and onset of boar contact on puberty attainment of replacement gilts raised in Thailand.

    Science.gov (United States)

    Roongsitthichai, Atthaporn; Olanratmanee, Em-On; Tummaruk, Padet

    2014-10-01

    This study aimed to investigate the influence of growth rate and onset of boar contact on age at first observed estrus of the replacement gilts raised in Thailand. In total, 766 gilts were measured for body weight and backfat thickness prior to insemination. Body weight was further calculated for growth rate. Estrus detection was performed twice a day by back pressure test with an existence of mature boars with high libido. The first date of boar exposure and that of first observed estrus were individually recorded. Due to growth rate, they were classified into three groups: high (>700 g/day), moderate (600-700 g/day), and low (<600 g/day). According to onset of boar contact, the gilts were grouped into two categories: early (<150 days) and late (≥150 days). The results revealed that the gilts expressed first observed estrus, averagely, at age 205.1 ± 34.1 days, had a growth rate of 615.5 ± 57.6 g/day, and first contact with boars at 160.7 ± 19.9 days of age. The gilts with low growth rate expressed first estrus later than those with moderate (208.6 ± 2.0 vs 198.0 ± 3.2 days, P = 0.033) and high growth rate (208.6 ± 2.0 vs 193.9 ± 6.7 days, P = 0.005) groups. Together with the influence of boar exposure, the gilts contacted boar earlier with high growth rate showed first estrus at age 180.3 ± 10.1 days, whereas those with later boar contact with low growth rate showed first estrus at age 197.9 ± 3.2 days. In summary, the replacement gilts should have high growth rate and contact boar early to attain puberty faster and possess decent subsequent reproductive performance.

  19. Dual substrate feedback control of specific growth-rate in vaccine production

    NARCIS (Netherlands)

    Neeleman, R.; Beuvery, E.C.; Vries, D.; Straten, van G.; Boxtel, van A.J.B.

    2004-01-01

    Abstract: Unexpectedly, primary concern of bio-pharmaceutical industry is not optimisation of product yield or cost reduction, but consistency in production and product quality. This paper describes the methodology and experimental results of specific growth-rate control for vaccine production. The

  20. Calculating second derivatives of population growth rates for ecology and evolution

    NARCIS (Netherlands)

    Shyu, E.; Caswell, H.

    2014-01-01

    Second derivatives of the population growth rate measure the curvature of its response to demographic, physiological or environmental parameters. The second derivatives quantify the response of sensitivity results to perturbations, provide a classification of types of selection and provide one way

  1. Experimental design and estimation of growth rate distributions in size-structured shrimp populations

    International Nuclear Information System (INIS)

    Banks, H T; Davis, Jimena L; Ernstberger, Stacey L; Hu, Shuhua; Artimovich, Elena; Dhar, Arun K

    2009-01-01

    We discuss inverse problem results for problems involving the estimation of probability distributions using aggregate data for growth in populations. We begin with a mathematical model describing variability in the early growth process of size-structured shrimp populations and discuss a computational methodology for the design of experiments to validate the model and estimate the growth-rate distributions in shrimp populations. Parameter-estimation findings using experimental data from experiments so designed for shrimp populations cultivated at Advanced BioNutrition Corporation are presented, illustrating the usefulness of mathematical and statistical modeling in understanding the uncertainty in the growth dynamics of such populations

  2. Standard test method for measurement of fatigue crack growth rates

    CERN Document Server

    American Society for Testing and Materials. Philadelphia

    2015-01-01

    1.1 This test method covers the determination of fatigue crack growth rates from near-threshold to Kmax controlled instability. Results are expressed in terms of the crack-tip stress-intensity factor range (ΔK), defined by the theory of linear elasticity. 1.2 Several different test procedures are provided, the optimum test procedure being primarily dependent on the magnitude of the fatigue crack growth rate to be measured. 1.3 Materials that can be tested by this test method are not limited by thickness or by strength so long as specimens are of sufficient thickness to preclude buckling and of sufficient planar size to remain predominantly elastic during testing. 1.4 A range of specimen sizes with proportional planar dimensions is provided, but size is variable to be adjusted for yield strength and applied force. Specimen thickness may be varied independent of planar size. 1.5 The details of the various specimens and test configurations are shown in Annex A1-Annex A3. Specimen configurations other than t...

  3. Assessing a relationship between bone microstructure and growth rate: a fluorescent labelling study in the king penguin chick (Aptenodytes patagonicus).

    Science.gov (United States)

    de Margerie, E; Robin, J-P; Verrier, D; Cubo, J; Groscolas, R; Castanet, J

    2004-02-01

    Microstructure-function relationships remain poorly understood in primary bone tissues. The relationship between bone growth rate and bone tissue type, although documented in some species by previous works, remains somewhat unclear and controversial. We assessed this relationship in a species with extreme adaptations, the king penguin (Aptenodytes patagonicus). These birds have a peculiar growth, interrupted 3 months after hatching by the austral winter. Before this interruption, chicks undergo extremely rapid statural and ponderal growth. We recorded experimentally (by means of fluorescent labelling) the growth rate of bone tissue in four long bones (humerus, radius, femur and tibiotarsus) of four king penguin chicks during their fastest phase of growth (3-5 weeks after hatching) and identified the associated bone tissue types ('laminar', 'longitudinal', 'reticular' or 'radial' fibro-lamellar bone tissue). We found the highest bone tissue growth rate known to date, up to 171 microm day(-1) (mean 55 microm day(-1)). There was a highly significant relationship between bone tissue type and growth rate (P<10(-6)). Highest rates were obtained with the radial microarchitecture of fibro-lamellar bone, where cavities in the woven network are aligned radially. This result supports the heuristic value of a relationship between growth rate and bone primary microstructure. However, we also found that growth rates of bone tissue types vary according to the long bone considered (P<10(-5)) (e.g. growth rates were 38% lower in the radius than in the other long bones), a result that puts some restriction on the applicability of absolute growth rate values (e.g. to fossil species). The biomechanical disadvantages of accelerated bone growth are discussed in relation to the locomotor behaviour of the chicks during their first month of life.

  4. Astragalus Extract Mixture HT042 Increases Longitudinal Bone Growth Rate by Upregulating Circulatory IGF-1 in Rats

    Directory of Open Access Journals (Sweden)

    Donghun Lee

    2017-01-01

    Full Text Available Astragalus extract mixture HT042 is a standardized ingredient of health functional food approved by Korean FDA with a claim of “height growth of children.” HT042 stimulates bone growth rate and increases local IGF-1 expression in growth plate of rats which can be considered as direct stimulation of GH and its paracrine/autocrine actions. However, it remains unclear whether HT042 stimulates circulatory IGF-1 which also plays a major role to stimulate bone growth. To determine the effects on circulatory IGF-1, IGF-1 and IGFBP-3 expressions and phosphorylation of JAK2/STAT5 were evaluated in the liver after 10 days of HT042 administration. HT042 upregulated liver IGF-1 and IGFBP-3 mRNA expression, IGF-1 protein expression, and phosphorylation of JAK2/STAT5. HT042 also increased bone growth rate and proliferative zonal height in growth plate. In conclusion, HT042 stimulates bone growth rate via increment of proliferative rate by upregulation of liver IGF-1 and IGFBP-3 mRNA followed by IGF-1 protein expression through phosphorylation of JAK2/STAT5, which can be regarded as normal functioning of GH-dependent endocrine pathway.

  5. The Balance of Payments Constraint as an Explanation of International Growth Rate Differences

    Directory of Open Access Journals (Sweden)

    Anthony P. Thirlwall

    2011-12-01

    Full Text Available The paper shows that if long-run balance of payments equilibrium on current account is a requirement then a country's long run growth rate can be approximated by the ratio of the growth of exports to the income elasticity of demand for imports. The model fits well the experience of eighteen OECD countries. It is output, not relative prices, that adjusts the balance of payments, contrary to the neoclassical orthodoxy. Growth can be demand constained by the balance of payments.

  6. Growth rate of dislocation loop in Fe-Ni-Cr alloy under Kr+ ion and electron irradiation

    International Nuclear Information System (INIS)

    Kimoto, T.; Allen, C.W.; Rehn, L.E.

    1991-10-01

    In order to examine the effect of irradiating particle species on the growth rate of radiation-induced dislocation loops, a solution-annealed Fe-25Ni-15Cr-0.02C alloy was irradiated at 723 K first by 1.5 MeV Kr + ions for 2520 sec, then by 1.5 MeV Kr + ions and 1.0 MeV electrons simultaneously for 780 sec, and finally by 1.0 MeV electrons for 780 sec with the HVEM-Tandem Facility in Argonne National Laboratory. The calculated damage rate by 1.5 MeV Kr + ions was 5.8 x 10 -4 dpa/s, and that by 1.0 MeV electrons was 1 x 10 -4 dpa/s. The growth rate of a dislocation loop located at the center of the specimen was 7 x 10 -3 nm/s for the Kr + ion irradiation, 4 x 10 -2 nm/s for the simultaneous Kr + and electron irradiation, and (2--3) x 10 -2 nm/s for the electron irradiation. This implies that the electron irradiation is about 19 times more effective in the growth of radiation-induced dislocation loops than the Kr + ion irradiation. The dislocation loop growth rate under the simultaneous Kr + and electron irradiation is higher than the sum of the growth rates under the individual Kr + and electron irradiations. 5 refs., 4 figs

  7. Selection for growth rate and body size have altered the expression profiles of somatotropic axis genes in chickens

    Science.gov (United States)

    Liu, Yong; Xu, Zhiqiang; Duan, Xiaohua; Li, Qihua; Dou, Tengfei; Gu, Dahai; Rong, Hua; Wang, Kun; Li, Zhengtian; Talpur, Mir Zulqarnain; Huang, Ying; Wang, Shanrong; Yan, Shixiong; Tong, Huiquan; Zhao, Sumei; Zhao, Guiping; Su, Zhengchang; Ge, Changrong

    2018-01-01

    The growth hormone / insulin-like growth factor-1 (GH/IGF-1) pathway of the somatotropic axis is the major controller for growth rate and body size in vertebrates, but the effect of selection on the expression of GH/IGF-1 somatotropic axis genes and their association with body size and growth performance in farm animals is not fully understood. We analyzed a time series of expression profiles of GH/IGF-1 somatotropic axis genes in two chicken breeds, the Daweishan mini chickens and Wuding chickens, and the commercial Avian broilers hybrid exhibiting markedly different body sizes and growth rates. We found that growth rate and feed conversion efficiency in Daweishan mini chickens were significantly lower than those in Wuding chickens and Avian broilers. The Wuding and Daweishan mini chickens showed higher levels of plasma GH, pituitary GH mRNA but lower levels of hepatic growth hormone receptor (GHR) mRNA than in Avian broilers. Daweishan mini chickens showed significantly lower levels of plasma IGF-1, thigh muscle and hepatic IGF-1 mRNA than did Avian broilers and Wuding chickens. These results suggest that the GH part of the somatotropic axis is the main regulator of growth rate, while IGF-1 may regulate both growth rate and body weight. Selection for growth performance and body size have altered the expression profiles of somatotropic axis genes in a breed-, age-, and tissue-specific manner, and manner, and alteration of regulatory mechanisms of these genes might play an important role in the developmental characteristics of chickens. PMID:29630644

  8. Proposal of fatigue crack growth rate curve in air for nickel-base alloys used in BWR

    International Nuclear Information System (INIS)

    Ogawa, Takuya; Itatani, Masao; Nagase, Hiroshi; Aoike, Satoru; Yoneda, Hideki

    2013-01-01

    When the defects are detected in the nuclear components in Japan, structural integrity assessment should be performed for the technical judgment on continuous service based on the Rules on Fitness-for-Service for Nuclear Power Plants of the Japan Society of Mechanical Engineers Code (JSME FFS Code). Fatigue crack growth analysis is required when the cyclic loading would be applied for the components. Recently, fatigue crack growth rate curve in air environment for Nickel-base alloys weld metal used in BWR was proposed by the authors and it was adopted as a code case of JSME FFS Code to evaluate the embedded flaw. In this study, fatigue crack growth behavior for heat-affected zone (HAZ) of Nickel-base alloys in air was investigated. And a unified fatigue crack growth rate curve in air for HAZ and weld metal of Nickel-base alloys used in BWR was evaluated. As a result, it was found that the curve for weld metal could be applied as a curve for both HAZ and weld metal since moderately conservative assessment of fatigue crack growth rate of HAZ is possible by the curve for weld metal in the Paris region. And the threshold value of stress intensity far range (ΔK th ) is determined to 3.0 MPa√m based on the fatigue crack growth rate of HAZ. (author)

  9. Does raking basal duff affect tree growth rates or mortality?

    Science.gov (United States)

    Erin Noonan-Wright; Sharon M. Hood; Danny R. Cluck

    2010-01-01

    Mortality and reduced growth rates due to raking accumulated basal duff were evaluated for old, large-diameter ponderosa and Jeffrey pine trees on the Lassen National Forest, California. No fire treatments were included to isolate the effect of raking from fire. Trees were monitored annually for 5 years after the raking treatment for mortality and then cored to measure...

  10. Growth Rate and Health Status of Weaned Rabbits Fed Ensiled ...

    African Journals Online (AJOL)

    In a 6 week feeding experiment, twenty five New Zealand white breed of weaned rabbits, with an average age of 8-10 weeks were used to assess the effect of ensiled water hyacinth (WH) with different additives on growth rate and blood parameters of the animals. The animals were randomly allotted to five dietary groups, ...

  11. Short-term lower-leg growth rate and urine cortisol excretion in children treated with ciclesonide

    DEFF Research Database (Denmark)

    Agertoft, Lone; Pedersen, Søren

    2005-01-01

    BACKGROUND: Measurement of short-term lower-leg growth rate in children by means of knemometry has become established as an integral part of the available measures of systemic activity of topical steroids in children. OBJECTIVE: We sought to determine the effects of clinically effective doses....... There was no statistically significant dose-response effect. Likewise, no statistically significant differences or dose-response effects were found for urinary cortisol adjusted for creatinine. CONCLUSION: Short-term lower-leg growth rate and hypothalamic-pituitary-adrenal axis function are not affected by treatment...... of the novel inhaled corticosteroid ciclesonide on lower-leg growth rate and hypothalamic-pituitary-adrenal axis function in children with asthma. METHODS: In a double-blind, placebo-controlled, 4-period crossover study, 24 children aged 6 to 12 years sequentially received ciclesonide (40, 80, and 160 microg...

  12. EFFECT OF POST-LOGGING SILVICULTURAL TREATMENT ON GROWTH RATES OF RESIDUAL STAND IN A TROPICAL FOREST

    Directory of Open Access Journals (Sweden)

    Haruni Krisnawati

    2010-12-01

    Full Text Available Post-logging silvicultural treatments are generally performed to improve yields of the remaining tree species by increasing their growth rate. In this study the effects of silvicultural treatment on the growth rates of commercial (dipterocarps and non-dipterocarps as well as non- commercial tree species in a tropical forest in West Kalimantan were examined and were compared to a control treatment. Silvicultural treatment applied was liberation of future crop trees from lianas and neighbouring competing trees. Treatments were applied to six plots of 80 m x 80 m each. The plots comprised 64 quadrats of 10 m x 10 m to allow better control of measurements. The treatment and control plots were established 6 years after logging. Effects were measured 2,4 and 7 years after treatment application. In all obser vation periods, the growth rates increased with silvicultural treatment. Overall, commercial dipterocarps, commercial non-dipterocarps and non-commercial tree species groups differed in response to silvicultural treatment. The growth rates of commercial tree species in plots that received silvicultural treatment were 62–97% higher than in the control plots. For non-commercial tree species, the increase of growth rates was 20–58%, compared to the control plots. These results indicate that the application of silvicultural treatments after logging could help improve the growth of the residual stands. These provide quantitative information that silvicultural treatments in logged-over forest should be considered as a viable management option and may guide the choice of cutting cycle.

  13. Enhancement of low temperature toughness of nanoprecipitates strengthened ferritic steel by delamination structure

    Energy Technology Data Exchange (ETDEWEB)

    Zhao, Yu; Xu, Songsong; Li, Junpeng; Zhang, Jian [Key Laboratory of Superlight Materials and Surface Technology, Ministry of Education, College of Materials Science and Chemical Engineering, Harbin Engineering University, Harbin 150001, P R China (China); Sun, Liangwei; Chen, Liang; Sun, Guangai; Peng, Shuming [Key Laboratory of Neutron Physics and Institute of Nuclear Physics and Chemistry, China Academy of Engineering Physics (CAEP), Mianyang 621999 (China); Zhang, Zhongwu, E-mail: zwzhang@hrbeu.edu.cn [Key Laboratory of Superlight Materials and Surface Technology, Ministry of Education, College of Materials Science and Chemical Engineering, Harbin Engineering University, Harbin 150001, P R China (China)

    2017-04-13

    This study investigated the effects of aging and thermomechanical treatments on the microstructure evolution and mechanical properties of a nanoprecipitates strengthened ferritic steel. The toughness of steel at various temperatures was measured carefully and correlated with microstructural features. Tensile tests show that aging can improve the mechanical strength without scarifying the ductility. With high yield strength of ~1000 MPa, excellent low temperature Charpy impact energy more than 300 J at −80 °C can be obtained. The ductile brittle transition temperature (DBTT) is lower than −80 °C. The high strength can be contributed by the nanocluster precipitation as determined by small angle neutron scattering and transmission electron microscopy. The excellent low temperature toughness is attributed to the delamination structure of the steel, which blunts the cracks and restrains the crack propagation.

  14. Measurement of the volume growth rate of single budding yeast with the MOSFET-based microfluidic Coulter counter.

    Science.gov (United States)

    Sun, Jiashu; Stowers, Chris C; Boczko, Erik M; Li, Deyu

    2010-11-07

    We report on measurements of the volume growth rate of ten individual budding yeast cells using a recently developed MOSFET-based microfluidic Coulter counter. The MOSFET-based microfluidic Coulter counter is very sensitive, provides signals that are immune from the baseline drift, and can work with cell culture media of complex composition. These desirable features allow us to directly measure the volume growth rate of single cells of Saccharomyces cerevisiae LYH3865 strain budding yeast in YNB culture media over a whole cell cycle. Results indicate that all budding yeast follow a sigmoid volume growth profile with reduced growth rates at the initial stage before the bud emerges and the final stage after the daughter gets mature. Analysis of the data indicates that even though all piecewise linear, Gomperitz, and Hill's function models can fit the global growth profile equally well, the data strongly support local exponential growth phenomenon. Accurate volume growth measurements are important for applications in systems biology where quantitative parameters are required for modeling and simulation.

  15. Theoretical growth rates, periods, and pulsation constants for long-period variables

    International Nuclear Information System (INIS)

    Fox, M.W.; Wood, P.R.

    1982-01-01

    Theoretical values of the growth rate, period, and pulsation constant for the first three radial pulsation modes in red giants (Population II and galactic disk) and supergiants have been derived in the linear, nonadiabatic approximation. The effects of altering the surface boundary conditions, the effective temperature (or mixing length), and the opacity in the outer layers have been explored. In the standard models, the Q-value for the first overtone can be much larger (Q 1 1 roughly-equal0.04); in addition, the Q-value for the fundamental mode is reduced from previous values, as is the period ratio P 0 /P 1 . The growth rate for the fundamental mode is found to increase with luminosity on the giant branch while the growth rate for the first overtone decreases. Dynamical instabilities found in previous adiabatic models of extreme red giants do not occur when nonadiabatic effects are included in the models. In some massive, luminous models, period ratios P 0 /P 1 approx.7 occur when P 0 approx.2000--5000 days; it is suggested that the massive galactic supergiants and carbon stars which have secondary periods Papprox.2000--7000 days and primary periods Papprox.300--700 days are first-overtone pulsators in which the long secondary periods are due to excitation of the fundamental mode. Some other consequences of the present results are briefly discussed, with particular emphasis on the mode of pulsation of the Mira variables. Subject headings: stars: long-period variables: stars: pulsation: stars: supergiants

  16. Towards establishing a combined rate law of nucleation and crystal growth - The case study of gypsum precipitation

    Science.gov (United States)

    Rendel, Pedro M.; Gavrieli, Ittai; Wolff-Boenisch, Domenik; Ganor, Jiwchar

    2018-03-01

    The main obstacle in the formulation of a quantitative rate-model for mineral precipitation is the absence of a rigorous method for coupling nucleation and growth processes. In order to link both processes, we conducted a series of batch experiments in which gypsum nucleation was followed by crystal growth. Experiments were carried out using various stirring methods in several batch vessels made of different materials. In the experiments, the initial degree of supersaturation of the solution with respect to gypsum (Ωgyp) was set between 1.58 and 1.82. Under these conditions, heterogeneous nucleation is the dominant nucleation mode. Based on changes in SO42- concentration with time, the induction time of gypsum nucleation and the following rate of crystal growth were calculated for each experiment. The induction time (6-104 h) was found to be a function of the vessel material, while the rates of crystal growth, which varied over three orders of magnitude, were strongly affected by the stirring speed and its mode (i.e. rocking, shaking, magnetic stirrer, and magnetic impeller). The SO42- concentration data were then used to formulate a forward model that couples the simple rate laws for nucleation and crystal growth of gypsum into a single kinetic model. Accordingly, the obtained rate law is based on classical nucleation theory and heterogeneous crystal growth.

  17. Prediction of PWSCC in nickel base alloys using crack growth rate models

    International Nuclear Information System (INIS)

    Thompson, C.D.

    1995-01-01

    The Ford/Andresen slip dissolution SCC model, originally developed for stainless steel components in BWR environments, has been applied to Alloy 600 and Alloy X-750 tested in deaerated pure water chemistry. A method is described whereby the crack growth rates measured in compact tension specimens can be used to estimate crack growth in a component. Good agreement was found between model prediction and measured SCC in X-750 threaded fasteners over a wide range of temperatures, stresses, and material condition. Most data support the basic assumption of this model that cracks initiate early in life. The evidence supporting a particular SCC mechanism is mixed. Electrochemical repassivation data and estimates of oxide fracture strain indicate that the slip dissolution model can account for the observed crack growth rates, provided primary rather than secondary creep rates are used. However, approximately 100 cross-sectional TEM foils of SCC cracks including crack tips reveal no evidence of enhanced plasticity or unique dislocation patterns at the crack tip or along the crack to support a classic slip dissolution mechanism. No voids, hydrides,, or microcracks are found in the vicinity of the crack tips creating doubt about classic hydrogen related mechanisms. The bulk oxide films exhibit a surface oxide which is often different than the oxide found within a crack. Although bulk chromium concentration affects the rate of SCC, analytical data indicates the mechanism does not result from chromium depletion at the grain boundaries. The overall findings support a corrosion/dissolution mechanism but not one necessarily related to slip at the crack tip. (author). 12 refs, 27 figs

  18. Numerical Study of Operating Pressure Effect on Carbon Nanotube Growth Rate and Length Uniformity

    Directory of Open Access Journals (Sweden)

    B. Zahed

    2014-01-01

    Full Text Available Chemical Vapor Deposition (CVD is one of the most popular methods for producing Carbon Nanotubes (CNTs. The growth rate of CNTs based on CVD technique is investigated by using a numerical model based on finite volume method. Inlet gas mixture, including xylene as carbon source and mixture of argon and hydrogen as carrier gas enters into a horizontal CVD reactor at atmospheric pressure. In this article the operating pressure variations are studied as the effective parameter on CNT growth rate and length uniformity.

  19. Effects of growth rate, cell size, motion, and elemental stoichiometry on nutrient transport kinetics.

    Science.gov (United States)

    Flynn, Kevin J; Skibinski, David O F; Lindemann, Christian

    2018-04-01

    Nutrient acquisition is a critical determinant for the competitive advantage for auto- and osmohetero- trophs alike. Nutrient limited growth is commonly described on a whole cell basis through reference to a maximum growth rate (Gmax) and a half-saturation constant (KG). This empirical application of a Michaelis-Menten like description ignores the multiple underlying feedbacks between physiology contributing to growth, cell size, elemental stoichiometry and cell motion. Here we explore these relationships with reference to the kinetics of the nutrient transporter protein, the transporter rate density at the cell surface (TRD; potential transport rate per unit plasma-membrane area), and diffusion gradients. While the half saturation value for the limiting nutrient increases rapidly with cell size, significant mitigation is afforded by cell motion (swimming or sedimentation), and by decreasing the cellular carbon density. There is thus potential for high vacuolation and high sedimentation rates in diatoms to significantly decrease KG and increase species competitive advantage. Our results also suggest that Gmax for larger non-diatom protists may be constrained by rates of nutrient transport. For a given carbon density, cell size and TRD, the value of Gmax/KG remains constant. This implies that species or strains with a lower Gmax might coincidentally have a competitive advantage under nutrient limited conditions as they also express lower values of KG. The ability of cells to modulate the TRD according to their nutritional status, and hence change the instantaneous maximum transport rate, has a very marked effect upon transport and growth kinetics. Analyses and dynamic models that do not consider such modulation will inevitably fail to properly reflect competitive advantage in nutrient acquisition. This has important implications for the accurate representation and predictive capabilities of model applications, in particular in a changing environment.

  20. Temporal, spatial, and body size effects on growth rates of loggerhead sea turtles (Caretta caretta) in the Northwest Atlantic

    Science.gov (United States)

    Bjorndal, Karen A.; Schroeder, Barbara A.; Foley, Allen M.; Witherington, Blair E.; Bresette, Michael; Clark, David; Herren, Richard M.; Arendt, Michael D.; Schmid, Jeffrey R.; Meylan, Anne B.; Meylan, Peter A.; Provancha, Jane A.; Hart, Kristen M.; Lamont, Margaret M.; Carthy, Raymond R.; Bolten, Alan B.

    2013-01-01

    In response to a call from the US National Research Council for research programs to combine their data to improve sea turtle population assessments, we analyzed somatic growth data for Northwest Atlantic (NWA) loggerhead sea turtles (Caretta caretta) from 10 research programs. We assessed growth dynamics over wide ranges of geography (9–33°N latitude), time (1978–2012), and body size (35.4–103.3 cm carapace length). Generalized additive models revealed significant spatial and temporal variation in growth rates and a significant decline in growth rates with increasing body size. Growth was more rapid in waters south of the USA (productivity to a common environmental change should be explored to determine whether somatic growth rates can help interpret population trends based on annual counts of nests or nesting females. Because of the significant spatial and temporal variation in growth rates, population models of NWA loggerheads should avoid employing growth data from restricted spatial or temporal coverage to calculate demographic metrics such as age at sexual maturity.