WorldWideScience

Sample records for control rod cladding

  1. Fission reactor control rod

    International Nuclear Information System (INIS)

    Irie, Tomoo.

    1991-01-01

    The present invention concerns a control rod in a PWR type reactor. A control rod has an inner cladding tube and an outer cladding tube disposed coaxially, and a water draining hole is formed at the inside of the inner cladding tube. Neutron absorbers are filled in an annular gap between the outer cladding tube and the inner cladding tube. The water draining hole opens at the lower end thereof to the top end of the control rod and at the upper end thereof to the side of the upper end plug of the control rod. If the control rod is dropped to a control rod guide thimble for reactor scram, coolants from the control rod guide thimble are flown from the lower end of the water draining hole and discharged from the upper end passing through the water draining hole. In this way, water from the control rod guide thimble is removed easily when the control rod is dropped. Further, the discharging amount of water itself is reduced by the provision of the water draining hole. Accordingly, sufficient control rod dropping speed can be attained. (I.N.)

  2. Control rod drives

    International Nuclear Information System (INIS)

    Hayakawa, Hiroyasu; Kawamura, Atsuo.

    1979-01-01

    Purpose: To reduce pellet-clad mechanical interactions, as well as improve the fuel safety. Constitution: In the rod drive of a bwr type reactor, an electric motor operated upon intermittent input such as of pulse signals is connected to a control rod. A resolver for converting the rotational angle of the motor to electric signals is connected to the rotational shaft of the motor and the phase difference between the output signal from the resolver and a reference signal is adapted to detect by a comparator. Based on the detection result, the controller is actuated to control a motor for control rod drive so that fine control for the movement of the control rod is made possible. This can reduce the moving distance of the control rod, decrease the thermal stress applied to the control rod and decrease the pellet clad mechanical interaction failures due to thermal expansion between the cladding tube and the pellets caused by abrupt changes in the generated power. (Furukawa, Y.)

  3. Inspection system for Zircaloy clad fuel rods

    International Nuclear Information System (INIS)

    Yancey, M.E.; Porter, E.H.; Hansen, H.R.

    1975-10-01

    A description is presented of the design, development, and performance of a remote scanning system for nondestructive examination of fuel rods. Characteristics that are examined include microcracking of fuel rod cladding, fuel-cladding interaction, cladding thickness, fuel rod diameter variation, and fuel rod bowing. Microcracking of both the inner and outer fuel rod surfaces and variations in wall thickness are detected by using a pulsed eddy current technique developed by Argonne National Laboratory (ANL). Fuel rod diameter variation and fuel rod bowing are detected by using two linear variable differential transformers (LVDTs) and a signal conditioning system. The system's mechanical features include variable scanning speeds, a precision indexing system, and a servomechanism to maintain proper probe alignment. Initial results indicate that the system is a very useful mechanism for characterizing irradiated fuel rods

  4. Clad buffer rod sensors for liquid metals

    International Nuclear Information System (INIS)

    Jen, C.-K.; Ihara, I.

    1999-01-01

    Clad buffer rods, consisting of a core and a cladding, have been developed for ultrasonic monitoring of liquid metal processing. The cores of these rods are made of low ultrasonic-loss materials and the claddings are fabricated by thermal spray techniques. The clad geometry ensures proper ultrasonic guidance. The lengths of these rods ranges from tens of centimeters to 1m. On-line ultrasonic level measurements in liquid metals such as magnesium at 700 deg C and aluminum at 960 deg C are presented to demonstrate their operation at high temperature and their high ultrasonic performance. A spherical concave lens is machined at the rod end for improving the spatial resolution. High quality ultrasonic images have been obtained in the liquid zinc at 600 deg C. High spatial resolution is needed for the detection of inclusions in liquid metals during processing. We also show that the elastic properties such as density, longitudinal and shear wave velocities of liquid metals can be measured using a transducer which generates and receives both longitudinal and shear waves and is mounted at the end of a clad buffer rod. (author)

  5. Modelling of pellet-cladding interaction for PWRs reactors fuel rods

    International Nuclear Information System (INIS)

    Esteves, A.M.

    1991-01-01

    The pellet-cladding interaction that can occur in a PWR fuel rod design is modelled with the computer codes FRAPCON-1 and ANSYS. The fuel performance code FRAPCON-1 analyzes the fuel rod irradiation behavior and generates the initial conditions for the localized fuel rod thermal and mechanical modelling in two and three-dimensional finite elements with ANSYS. In the mechanical modelling, a pellet fragment is placed in the fuel rod gap. Two types of fuel rod cladding materials are considered: Zircaloy and austenitic stainless steel. Linear and non-linear material behaviors are allowed. Elastic, plastic and creep behaviors are considered for the cladding materials. The modelling is applied to Angra-II fuel rod design. The results are analyzed and compared. (author)

  6. Reduction in degree of absorber-cladding mechanical interaction by shroud tube in control rods for the fast reactor

    International Nuclear Information System (INIS)

    Donomae, Takako; Katsuyama, Kozo; Tachi, Yoshiaki; Maeda, Koji; Yamamoto, Masaya; Soga, Tomonori

    2011-01-01

    Research and development of a long-life control rod for fast reactors is being conducted at Joyo. One of the challenges in developing a long-life control rod is the restraint of absorber-cladding mechanical interaction (ACMI). First, a helium-bonding rod was selected as a control rod for the experimental fast reactor Joyo, which is the first liquid metal fast reactor in Japan. Its lifetime was limited by ACMI, which is induced by the swelling and relocation of B 4 C pellets. To restrain ACMI, a shroud tube was inserted into the gap between the B 4 C pellets and the cladding tube. However, once B 4 C pellets cracked and broke into small fragments, relocation occurred. After this, the narrow gap closed immediately as the degree of B 4 C pellet swelling increased. To solve this problem, the gap was widened during design, and sodium was selected as the bonding material instead of helium to restrain the increase in pellet temperature. Irradiation testing of the modified sodium-bonding control rod confirmed that ACMI would be restrained by the shroud tube regardless of the occurrence of B 4 C pellet relocation. As a result of these improvements, the estimated lifetime of the control rod at Joyo was doubled. In this paper, the results of postirradiation examination are reported. (author)

  7. Embedded cladding surface thermocouples on Zircaloy-sheathed heater rods

    International Nuclear Information System (INIS)

    Wilkins, S.C.

    1977-06-01

    Titanium-sheathed Type K thermocouples embedded in the cladding wall of zircaloy-sheathed heater rods are described. These thermocouples constitute part of a program intended to characterize the uncertainty of measurements made by surface-mounted cladding thermocouples on nuclear fuel rods. Fabrication and installation detail, and laboratory testing of sample thermocouple installations are included

  8. Influence of pellet-clad-gap-size on LWR fuel rod performance

    International Nuclear Information System (INIS)

    Brzoska, B.; Fuchs, H.P.; Garzarolli, F.; Manzel, R.

    1979-01-01

    The as-fabricated pellet-clad-gap size varies due to fabricational tolerances of the cladding inner diameter and the pellet outer diameter. The consequences of these variations on the fuel rod behaviour are analyzed using the KWU fuel rod code CARO. The code predictions are compared with experimental results of special pathfinder test fuel rods irradiated in the OBRIGHEIM nuclear power plant. These test fuel rods include gap sizer in the range of 140 μm to 270 μm, prepressurization between 13 bar to 36 bar and Helium and Argon fill gases irradiated up to a local burnup of 35 MWd/kg(U). Post irradiation examination were performed at different burnups. CARC calculations have been performed with special emphasis in cladding creep down, fission gas release and pellet clad gap closure. (orig.)

  9. Study of pellet clad interaction defects in Dresden-3 fuel rods

    International Nuclear Information System (INIS)

    Pasupathi, V.; Perrin, J.S.

    1979-01-01

    During Cycle-3 operation of Dresden-3, fuel rod failures occurred following a transient power increase. Ten fuel rods from five of the leaking fuel assemblies were examined at Battelle's Columbus Laboratory and General Electric-Vallecitos Nuclear Center. Examinations consisted of nondestructive and destructive methods including metallography and scanning electron microscopy (SEM). Results showed the cause of fuel rod failure to be pellet clad interaction involving stress corrosion cracking. Results of SEM studies of the cladding crack surfaces and deposits on clad inner surfaces were in agreement with those reported by other investigators

  10. Duke Power Company's control rod wear program

    International Nuclear Information System (INIS)

    Culp, D.C.; Kitlan, M.S. Jr.

    1990-01-01

    Recent examinations performed at several foreign and domestic pressurized water reactors have identified significant control rod cladding wear, leading to the conclusion that previously believed control rod lifetimes are not attainable. To monitor control rod performance and reduce safety concerns associated with wear, Duke Power Company has developed a comprehensive control rod wear program for Ag-In-Cd and boron carbide (B 4 C) rods at the McGuire and Catawba nuclear stations. Duke Power currently uses the Westinghouse 17 x 17 Ag-In-Cd control rod design at McGuire Unit 1 and the Westinghouse 17 x 17 hybrid B 4 C control rod design with a Ag-In-Cd tip at McGuire Unit 2 and Catawba Units 1 and 2. The designs are similar, with the exception of the absorber material and clad thickness. There are 53 control rods per unit

  11. Gap conductance in Zircaloy-clad LWR fuel rods

    International Nuclear Information System (INIS)

    Ainscough, J.B.

    1982-04-01

    This report describes the procedures currently used to calculate fuel-cladding gap conductance in light water reactor fuel rods containing pelleted UO 2 in Zircaloy cladding, under both steady-state and transient conditions. The relevant theory is discussed together with some of the approximations usually made in performance modelling codes. The state of the physical property data which are needed for heat transfer calculations is examined and some of the relevant in- and out-of-reactor experimental work on fuel rod conductance is reviewed

  12. Secondary hydriding of defected zircaloy-clad fuel rods

    International Nuclear Information System (INIS)

    Olander, D.R.; Vaknin, S.

    1993-01-01

    The phenomenon of secondary hydriding in LWR fuel rods is critically reviewed. The current understanding of the process is summarized with emphasis on the sources of hydrogen in the rod provided by chemical reaction of water (steam) introduced via a primary defect in the cladding. As often noted in the literature, the role of hydrogen peroxide produced by steam radiolysis is to provide sources of hydrogen by cladding and fuel oxidation that are absent without fission-fragment irradiation of the gas. Quantitative description of the evolution of the chemical state inside the fuel rod is achieved by combining the chemical kinetics of the reactions between the gas and the fuel and cladding with the transport by diffusion of components of the gas in the gap. The chemistry-gas transport model provides the framework into which therate constants of the reactions between the gases in the gap and the fuel and cladding are incorporated. The output of the model calculation is the H 2 0/H 2 ratio in the gas and the degree of claddingand fuel oxidation as functions of distance from the primary defect. This output, when combined with a criterion for the onset of massive hydriding of the cladding, can provide a prediction of the time and location of a potential secondary hydriding failure. The chemistry-gas transport model is the starting point for mechanical and H-in-Zr migration analyses intended to determine the nature of the cladding failure caused by the development of the massive hydride on the inner wall

  13. The improvement of control rod in experimental fast reactor JOYO. The development of a sodium bonded type control rod

    Energy Technology Data Exchange (ETDEWEB)

    Soga, T.; Miyakawa, S.; Mitsugi, T. [Japan Nuclear Cycle Development Inst., Oarai Engineering Center, Irradiation Center, Irradiation and Administration Section, Oarai, Ibaraki (Japan)

    1999-06-01

    Currently, the lifetime of control rods in JOYO is limited by Absorber-Cladding Mechanical Interaction (ACMI) due to swelling of B{sub 4}C(boron carbide) pellets accelerated by relocation of pellet fragments. A sodium bonded type control rod was developed which improves the thermal conductivity by means of charging sodium into the gap between B{sub 4}C and cladding and by utilizing a shroud which wraps the pellet fragments in a thin tube. This new design will be able to enlarge the gap between B{sub 4}C and cladding, without heating B{sub 4}C or fragment relocation, thus extending the life of the control rod. The sodium bonded type will be fabricated as the ninth reload control rods in JOYO. (1) The specification of a sodium bonded type control rod was determined with the wide gap between B{sub 4}C and cladding. In the design simulation, main component temperature were below the maximum limit. And the local heating by helium bubble generated from B{sub 4}C in the sodium gap, was not a serious problem in the analysis which was considered. (2) A structural design for the sodium entrance into the pin was determined. A formula was developed which the limit for sodium charging given physical dimension of the structure and sodium property. Result from sodium out-pile experiments validated the theoretical formula. (3) The analysis of ACMI indicated a lifetime extension of the sodium bonded type by 4.6% in comparison with lifetime of the helium bonded type of 1.6%. This is due to the boron10 burn-up rate being three times higher in the sodium bonded type than in the helium bonded type. To achieve a target burn-up 10% in the future, it will be necessary to modify design based on irradiation data which will be obtained by practical use of the sodium bonded control rods in JOYO. (4) The effects due to Absorber-Cladding Chemical Interaction (ACCI) were reduced by controlling the cladding temperature and chromium coating to the cladding's inner surface. It was confirmed

  14. Cladding temperature measurement by thermocouples at preirradiated LWR fuel rod samples

    International Nuclear Information System (INIS)

    Leiling, W.

    1981-12-01

    This report describes the technique to measure cladding temperatures of test fuel rod samples, applied during the in-pile tests on fuel rod failure in the steam loop of the FR2 reactor. NiCr/Ni thermocouples with stainless steel and Inconel sheaths, respectively,of 1 mm diameter were resistance spot weld to the outside of the fuel rod cladding. For the pre-irradiated test specimens, welding had to be done under hot-cell conditions, i.e. under remote handling. In order to prevent the formation of eutectics between zirconium and the chemical elements of the thermocouple sheath at elevated temperatures, the thermocouples were covered with a platinum jacket of 1.4 mm outside diameter swaged onto the sheath in the area of the measuring junction. This thermocouple design has worked satisfactorily in the in-pile experiments performed in a steam atmosphere. Even in the heatup phase, in which cladding temperatures up to 1050 0 C were reached, only very few failures occured. This good performance is to a great part due to a careful control and a thorough inspection of the thermocouples. (orig.) [de

  15. Corrosion behaviour of zircaloy 4 fuel rod cladding in EDF power plants

    Energy Technology Data Exchange (ETDEWEB)

    Romary, H; Deydier, D [EDF, Direction de l` Equipment SEPTEN, Villeurbanne (France)

    1997-02-01

    Since the beginning of the French nuclear program, a surveillance of fuel has been carried out in order to evaluate the fuel behaviour under irradiation. Until now, nuclear fuels provided by suppliers have met EDF requirements concerning fuel behaviour and reliability. But, the need to minimize the costs and to increase the flexibility of the power plants led EDF to the definition of new targets: optimization of the core management and fuel cycle economy. The fuel behaviour experience shows that some of these new requirements cannot be fully fulfilled by the present standard fuel due to some technological limits. Particularly, burnup enhancement is limited by the oxidation and the hydriding of the Zircaloy 4 fuel rod cladding. Also, fuel suppliers and EDF need to have a better knowledge of the Zy-4 cladding behaviour in order to define the existing margins and the limiting factors. For this reason, in-reactor fuel characterization programs have been set up by fuel suppliers and EDF for a few years. This paper presents the main results and conclusions of EDF experience on Zy-4 in-reactor corrosion behaviour. Data obtained from oxide layer or zirconia thickness measurements show that corrosion performance of Zy-4 fuel rod cladding, as irradiated until now in EDF reactors, is satisfactory but not sufficient to meet the future needs. The fuel suppliers propose in order to improve the corrosion resistance of fuel rod cladding, low tin Zy-4 cladding and then optimized Zy-4 cladding. Irradiation of these claddings are ongoing. The available corrosion data show the better in-reactor corrosion resistance of optimized Zy-4 fuel rod cladding compared to the standard Zy-4 cladding. The scheduled fuel surveillance program will confirm if the optimized Zy-4 fuel rod cladding will meet the requirements for the future high burnup and high flexibility fuel. (author). 10 refs, 19 figs, 4 tabs.

  16. Elastic plastic analysis of fuel element assemblies - hexagonal claddings and fuel rods

    International Nuclear Information System (INIS)

    Mamoun, M.M.; Wu, T.S.; Chopra, P.S.; Rardin, D.C.

    1979-01-01

    Analytical studies have been conducted to investigate the structural, thermal, and mechanical behavior of fuel rods, claddings and fuel element assemblies of several designs for a conceptual Safety Test Facility (STF). One of the design objectives was to seek a geometrical configuration for a clad by maximizing the volume fraction of fuel and minimizing the resultant stresses set-up in the clad. The results of studies conducted on various geometrical configurations showed that the latter design objective can be achieved by selecting a clad of an hexagonal geometry. The analytical studies necessitated developing solutions for determining the stresses, strains, and displacements experienced by fuel rods and an hexagonal cladding subjected to thermal fuel-bowing loads acting on its internal surface, the external pressure of the coolant, and elevated temperatures. This paper presents some of the initially formulated analytical methods and results. It should be emphasized that the geometrical configuration considered in this paper may not necessarily be similar to that of the final design. Several variables have been taken into consideration including cladding thickness, the dimensions of the fuel rod, the temperature of the fuel and cladding, the external pressure of the cooling fluid, and the mechanical strength properties of fuel and cladding. A finite-element computer program, STRAW Code, has also been employed to generate several numerical results which have been compared with those predicted by employing the initially formulated solutions. The theoretically predicted results are in good agreement with those of the STRAW Code. (orig.)

  17. Fuel-clad heat transfer coefficient of a defected fuel rod

    International Nuclear Information System (INIS)

    Bruet, M.; Stora, J.P.

    1976-01-01

    A special rod has been built with a stack of UO 2 pellets inside a thick zircaloy clad. The atmosphere inside the fuel rod can be changed and particularly the introduction of water is possible. The capsule was inserted in the Siloe pool reactor in a special device equipped with a neutron flux monitor. The fuel centerline temperature and the temperature at a certain radius of the clad were recorded by two thermocouples. The temperature profiles in the fuel and in the cladding have been calculated and then the heat transfer coefficient. In order to check the proper functioning of the device, two runs were successively achieved with a helium atmosphere. Then the helium atmosphere inside the fuel rod was removed and replaced by water. The heat transfer coefficients derived from the measurements at low power level are in agreement with the values given by the model based on thermal conductivity. However, for higher power levels, the heat transfer coefficients become higher than those based on the calculated gap

  18. Out-pile Test of Double Cladding Fuel Rod Mockups for a Nuclear Fuel Irradiation Test

    Energy Technology Data Exchange (ETDEWEB)

    Sohn, Jaemin; Park, Sungjae; Kang, Younghwan; Kim, Harkrho; Kim, Bonggoo; Kim, Youngki [Korea Atomic Energy Research Institute, Daejeon (Korea, Republic of)

    2008-05-15

    An instrumented capsule for a nuclear fuel irradiation test has been developed to measure fuel characteristics, such as a fuel temperature, internal pressure of a fuel rod, a fuel pellet elongation and a neutron flux during an irradiation test at HANARO. In the future, nuclear fuel irradiation tests under a high temperature condition are expected from users. To prepare for this request, we have continued developing the technology for a high temperature nuclear fuel irradiation test at HANARO. The purpose of this paper is to verify the possibility that the temperature of a nuclear fuel can be controlled at a high temperature during an irradiation test. Therefore we designed and fabricated double cladding fuel rod mockups. And we performed out-pile tests using these mockups. The purposes of a out-pile test is to analyze an effect of a gap size, which is between an outer cladding and an inner cladding, on the temperature and the effect of a mixture ratio of helium gas and neon gas on the temperature. This paper presents the design and fabrication of double cladding fuel rod mockups and the results of the out-pile test.

  19. Computer analysis of elongation of the WWER fuel rod claddings

    International Nuclear Information System (INIS)

    Scheglov, A.; Proselkov, V.

    2008-01-01

    In this paper description of mechanisms influencing changes of the WWER fuel cladding length and axial forces influencing fuel and cladding are presented. It is shown that shortening of the fuel claddings in case of high burnup can be explained by the change of the fuel and cladding reference state caused by reduction of the fuel rod power level - during reactor outages. It is noted that the presented calculated data are to be reviewed and interpreted as the preliminary results; further work is needed for their confirmation. (authors)

  20. Cladding tube of fuel rod for a BWR type reactor

    International Nuclear Information System (INIS)

    Nakayama, Hitoshi; Fujie, Kunio; Kuwahara, Heikichi; Hirai, Tadamasa; Kakizaki, Kimio.

    1976-01-01

    Object: To form a cladding tube wall with tunnels in communication with the exterior through a number of small-diameter openings to rapidly disperse a large quantity of heat thereby providing high density of the fuel rod. Structure: Tunnels adjacent to each other are provided under the skin in contact with cooling liquid of a cladding tube, and a number of openings through which said tunnels and the periphery of the cladding tube are placed in communication are formed, said openings each having its section smaller than that of said tunnel. With this arrangement, the cooling water entered the tunnel through some of small diameter openings absorbs heat of the fuel rod to be vaporized, which is flown out into the cooling water through the other small diameter openings and formed into vapor bubbles which move up for release of heat. (Taniai, N.)

  1. Deformation and collapse of zircaloy fuel rod cladding into plenum axial gaps

    International Nuclear Information System (INIS)

    Pfennigwerth, P.L.; Gorscak, D.A.; Selsley, I.A.

    1983-01-01

    To minimize support structure, blanket and reflector fuel rods of the thoria urania-fueled Light Water Breeder Reactor (LWBR) were designed with non-freestanding Zircaloy-4 cladding. An analytical model was developed to predict deformation of unirradiated cladding into axial gaps of fuel rod plenum regions where it is unsupported. This model uses the ACCEPT finite element computer program to calculate elastic-plastic deformation of cladding due to external pressure. The finite element is 20-node, triquadratic, isoparametric, and 3-dimensional. Its curved surface permits accurate modeling of the tube geometry, including geometric nonuniformities such as circumferential wall thickness variation and initial tube out-of-roundness. Progressive increases in axial gap length due to cladding elongation and fuel stack shrinkage are modeled, as are deformations of fuel pellets and stainless steel support sleeves which bound plenum axial gaps in LWBR type blanket fuel rods. Zircaloy-4 primary and secondary thermal creep representations were developed from uniaxial creep testing of fuel rod tubing. Creep response to multi-axial loading is modeled with a variation of Hill's formulation for anisotropic materials. Coefficients accounting for anisotropic thermal creep in Zircaloy-4 tubes were developed from creep testing of externally pressurized tubes having fixed axial gaps in the range 2.5 cm to 5.7 cm and radial clearances over simulated fuel pellets ranging from zero to 0.089 mm. (orig./RW)

  2. Modelling of pellet cladding interaction during power ramps in PWR rods by means of Transuranus fuel rod analysis code

    International Nuclear Information System (INIS)

    Di Marcello, V.; Luzzi, L.

    2008-01-01

    Pellet-cladding interaction (PCI) in PWR type rods subjected to power ramps was analysed by means of TRANSURANUS (TU) fuel rod performance code. PCI phenomena depend on the fuel power history - i.e. by several irradiation and thermal induced phenomena occurring in the fuel rod and mutually interacting during its life in reactor - and may become critical for cladding integrity under accidental conditions. Ten test fuel rods, whose power histories and post irradiation experiment (PIE) data were available from the OECD/NEA-IAEA International Fuel Performance Experiment (UTE) database through the Studsvik SUPER-RAMP Project, were simulated by TRANSURANUS. During a power ramp pellet gaseous swelling can be inhibited by cladding pressure and can be over-predicted by a normal operation swelling model. This phenomenon was simulated by a new formulation of a fuel swelling model already available in the code, in order to consider hot pressing of inter-granular -fuel porosity due to the high hydrostatic stress resulting from PCI: it was found that TRANSURANUS, as a result of the proposed swelling formulation as well as of the accurate modelling of the other phenomena occurring during irradiation, gives correct predictions on PCI induced fuel rod failures. In addition, PCI failure threshold identified by TRANSURANUS was compared with the technological limits known in literature: the possibility of relaxing these limits for low burn-up values and the preponderance of the European fuel rod design in front of PCI emerged from TU analyses. Finally, a good agreement was found between TU evaluations and PIE data, with regard to fission gas release, fuel grain growth, and creep, corrosion and elongation of the cladding. (authors)

  3. Behavior of high burnup fuel rod cladding during long-term dry storage in CASTOR casks

    International Nuclear Information System (INIS)

    Schaberg, A.; Spilker, H.; Goll, W.

    2000-01-01

    Short-time creep and rupture tests were performed to assess the strain potential of cladding of high burnt rods under conditions of dry storage. The tests comprised optimized Zr y-4 cladding samples from fuel rods irradiated to burnups of up to 64 MWd/kg U and were carried out at temperatures of 573 and 643 K at cladding stresses of about 400 and 600 MPa. The stresses, much higher than those occurring in a fuel rod, were chosen to reach circumferential elongations of about 2% within an envisaged testing time of 3-4 days. The creep tests were followed by a low temperature test at 423 K and 100 MPa to assess the long-term behavior of the cladding ductility especially with regard to the effect of a higher hydrogen content in the cladding due to the high burnup. The creep tests showed considerable uniform plastic elongations at these high burnups. It was demonstrated that around 600 K a uniform plastic strain of a least 2% is reached without cladding failure. The low temperature tests at 423 K for up to 5 days revealed no cladding failure under these conditions of reduced cladding ductility. It can be concluded that the increased hydrogen content has no adverse effect on cladding performance. (Authors)

  4. Corrosion performance of optimised and advanced fuel rod cladding in PWRs at high burnups

    International Nuclear Information System (INIS)

    Jourdain, P.; Hallstadius, L.; Pati, S.R.; Smith, G.P.; Garde, A.M.

    1997-01-01

    The corrosion behaviour both in-pile and out-of-pile for a number of cladding alloys developed by ABB to meet the current and future needs for fuel rod cladding with improved corrosion resistance is presented. The cladding materials include: 1) Zircaloy-4 (OPTIN) with optimised composition and processing and Zircaloy-2 optimised for Pressurised Water Reactors (PWR), (Zircaloy-2P), and 2) several alternative zirconium-based alloys with compositions outside the composition range for Zircaloys. The data presented originate from fuel rods irradiated in six PWRs to burnups up to about 66 MWd/kgU and from tests conducted in 360 o water autoclave. Also included are in-pile fuel rod growth measurements on some of the alloys. (UK)

  5. Material operating behaviour of ABB BWR control rods

    International Nuclear Information System (INIS)

    Rebensdorff, B.; Bart, G.

    2000-01-01

    The BWR control rods made by ABB use boron carbide (B 4 C and hafnium as absorber material within a cladding of stainless steel. The general behaviour under operation has proven to be very good. ABB and many of their control rod customers have performed extensive inspection programs of control rod behaviour. However, due to changes in the material properties under fast and thermal neutron irradiation defects may occur in the control rods at high neutron fluences. Examinations of irradiated control rod materials have been performed in hot cell laboratories. The examinations have revealed the defect mechanism Irradiation Assisted Stress Corrosion Cracking (IASCC) to appear in the stainless steel cladding. For IASCC to occur three factors have to act simultaneously. Stress, material sensitization and an oxidising environment. Stress may be obtained from boron carbide swelling due to irradiation. Stainless steel may be sensitized to intergranular stress corrosion cracking under irradiation. Normally the reactor environment in a BWR is oxidising. The presentation focuses on findings from hot cell laboratory work on irradiated ABB BWR control rods and studies of irradiated control rod materials in the hot cells at PSI. Apart from physical, mechanical and microstructural examinations, isotope analyses were performed to describe the local isotopic burnup of boron. Consequences (such as possible B 4 C washout) of a under operation in a ABB BWR, after the occurrence of a crack is discussed based on neutron radiographic examinations of control rods operated with cracks. (author)

  6. The use of eddy current testing for nuclear fuel rods cladding evaluation

    International Nuclear Information System (INIS)

    Silva Junior, Silverio F. da; Alencar, Donizete A.; Brito, Mucio Jose D. de

    2007-01-01

    Nuclear fuel rods cladding must be tested after their manufacture and during their operational life. This paper describes a study about the use of eddy current test method as a nondestructive tool for nuclear fuel rods cladding evaluation. The experiments were carried out using two different probes: an external probe and an internal probe. The main goal was to verify the sensitivity of the eddy current test system, to develop calibration and reference standards and to establish the main capabilities and limitations presented by this test method for this application. (author)

  7. Silver-indium-cadmium control rod behaviour during a severe reactor accident

    International Nuclear Information System (INIS)

    Bowsher, B.R.; Jenkins, R.A.; Nichols, A.L.; Rowe, N.A.; Simpson, J.A.H.

    1986-04-01

    An alloy of silver, indium and cadmium is commonly used as control rod material in pressurised water reactors (PWRs). The behaviour of this alloy has been studied in a series of experiments using an induction furnace to achieve temperatures up to 1900K. The aerosols released from overheated clad and unclad control rod samples have been characterised in both steam and inert atmospheres. Mass balance experiments have been undertaken to determine the distribution of the control rod alloy constituents following rupture of the cladding, and this work has been supported by thermogravimetric studies of silver-indium mixtures. Metallographic studies were also undertaken to assess the failure mode of the stainless steel cladding and the interaction of the molten alloy with Zircaloy. The results of this work are discussed in terms of aerosol/vapour behaviour during severe reactor accidents. (author)

  8. Flow-Induced Vibration Measurement of an Inner Cladding Tube in a Simulated Dual-Cooled Fuel Rod

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Kang Hee; Kim, Hyung Kyu; Yoon, Kyung Ho; Lee, Young Ho; Kim, Jae Yong [Korea Atomic Energy Research Institute, Daejeon (Korea, Republic of)

    2009-05-15

    To create an internal coolant flow passage in a dual cooled fuel rod, an inner cladding tube cannot have intermediate supports enough to relieve its vibration. Thus it can be suffered from a flow-induced vibration (FIV) more severely than an outer cladding tube which will be supported by series of spacer grids. It may cause a fatigue failure at welding joints on the cladding's end plug or fluid elastic instability of long, slender inner cladding due to decrease of a critical flow velocity. This is one of the challenging technical issues when a dual cooled fuel assembly is to be realized into a conventional reactor core To study an actual vibration phenomenon of a dual cooled fuel rod, FIV tests using a small-scale test bundle are being carried out. Measurement results of inner cladding tube of two typically simulated rods are presented. Causes of the differences in the vibration amplitude and response spectrum of the inner cladding tube in terms of intermediate support condition and pellet stacking are discussed.

  9. Correlation of waterside corrosion and cladding microstructure in high-burnup fuel and gadolinia rods

    International Nuclear Information System (INIS)

    Chung, H.M.

    1989-09-01

    Waterside corrosion of the Zircaloy cladding has been examined in high-burnup fuel rods from several BWRs and PWRs, as well as in 3 wt % gadolinia burnable poison rods obtained from a BWR. The corrosion behavior of the high-burnup rods was then correlated with results from a microstructural characterization of the cladding by optical, scanning-electron, and transmission-electron microscopy (OM, SEM, and TEM). OM and SEM examination of the BWR fuel cladding showed both uniform and nodular oxide layers 2 to 45 μm in thickness after burnups of 11 to 30 MWd/kgU. For one of the BWRs, which was operated at 307 degree C rather than the normal 288 degree C, a relatively thick (50 to 70 μm) uniform oxide, rather than nodular oxides, was observed after a burnup of 27 to 30 MWd/kgU. TEM characterization revealed a number of microstructural features that occurred in association with the intermetallic precipitates in the cladding metal, apparently as a result of irradiation-induced or -enhanced processes. The BWR rods that exhibited white nodular oxides contained large precipitates (300 to 700 nm in size) that were partially amorphized during service, indicating that a distribution of the large intermetallic precipitates is conductive to nodular oxidation. 23 refs., 9 figs

  10. Models for the Configuration and Integrity of Partially Oxidized Fuel Rod Cladding at High Temperatures

    International Nuclear Information System (INIS)

    Siefken, L.J.

    1999-01-01

    Models were designed to resolve deficiencies in the SCDAP/RELAP5/MOD3.2 calculations of the configuration and integrity of hot, partially oxidized cladding. These models are expected to improve the calculations of several important aspects of fuel rod behavior. First, an improved mapping was established from a compilation of PIE results from severe fuel damage tests of the configuration of melted metallic cladding that is retained by an oxide layer. The improved mapping accounts for the relocation of melted cladding in the circumferential direction. Then, rules based on PIE results were established for calculating the effect of cladding that has relocated from above on the oxidation and integrity of the lower intact cladding upon which it solidifies. Next, three different methods were identified for calculating the extent of dissolution of the oxidic part of the cladding due to its contact with the metallic part. The extent of dissolution effects the stress and thus the integrity of the oxidic part of the cladding. Then, an empirical equation was presented for calculating the stress in the oxidic part of the cladding and evaluating its integrity based on this calculated stress. This empirical equation replaces the current criterion for loss of integrity which is based on temperature and extent of oxidation. Finally, a new rule based on theoretical and experimental results was established for identifying the regions of a fuel rod with oxidation of both the inside and outside surfaces of the cladding. The implementation of these models is expected to eliminate the tendency of the SCDAP/RELAP5 code to overpredict the extent of oxidation of the upper part of fuel rods and to underpredict the extent of oxidation of the lower part of fuel rods and the part with a high concentration of relocated material. This report is a revision and reissue of the report entitled, Improvements in Modeling of Cladding Oxidation and Meltdown

  11. Control rod

    International Nuclear Information System (INIS)

    Takeda, Toshikazu; Inoue, Kotaro.

    1979-01-01

    Purpose: To flatten the power distribution in the reactor core without impairing neutron economy by disposing pins containing elements of lower atomic number in the central region of a shroud and loading pins containing depleted uranium in the periphery region thereof. Constitution: The shroud has a layer of pins containing depleted uranium in the peripheral region and a layer of pins containing elements of lower atomic number such as beryllium in the central region. Heat removal from those pins containing depleted uranium and elements of lower atomic number (neutron moderator) is effected by sodium flow outside of the cladding material. The control rod operation is conducted by inserting or extracting the central portion (pins containing elements of lower atomic number such as beryllium) inside of the stainless pipe. Upon extraction of the control rod, the moderator in the central region is removed whereby high speed neutrons are no more deccelerated and the absorption rate to the depleted uranium is decreased. This can flatten the power distribution in the reactore core with the disposition of a plurality of control rods at a better neutron economy as compared with the use of neutron absorber such as boron. (Seki, T.)

  12. Parametric Evaluation of SiC/SiC Composite Cladding with UO2 Fuel for LWR Applications: Fuel Rod Interactions and Impact of Nonuniform Power Profile in Fuel Rod

    Science.gov (United States)

    Singh, G.; Sweet, R.; Brown, N. R.; Wirth, B. D.; Katoh, Y.; Terrani, K.

    2018-02-01

    SiC/SiC composites are candidates for accident tolerant fuel cladding in light water reactors. In the extreme nuclear reactor environment, SiC-based fuel cladding will be exposed to neutron damage, significant heat flux, and a corrosive environment. To ensure reliable and safe operation of accident tolerant fuel cladding concepts such as SiC-based materials, it is important to assess thermo-mechanical performance under in-reactor conditions including irradiation and realistic temperature distributions. The effect of non-uniform dimensional changes caused by neutron irradiation with spatially varying temperatures, along with the closing of the fuel-cladding gap, on the stress development in the cladding over the course of irradiation were evaluated. The effect of non-uniform circumferential power profile in the fuel rod on the mechanical performance of the cladding is also evaluated. These analyses have been performed using the BISON fuel performance modeling code and the commercial finite element analysis code Abaqus. A constitutive model is constructed and solved numerically to predict the stress distribution in the cladding under normal operating conditions. The dependence of dimensions and thermophysical properties on irradiation dose and temperature has been incorporated into the models. Initial scoping results from parametric analyses provide time varying stress distributions in the cladding as well as the interaction of fuel rod with the cladding under different conditions of initial fuel rod-cladding gap and linear heat rate. It is found that a non-uniform circumferential power profile in the fuel rod may cause significant lateral bowing in the cladding, and motivates further analysis and evaluation.

  13. Eddy-current inspection of high flux isotope reactor nuclear control rods

    International Nuclear Information System (INIS)

    Smith, J.H.; Chitwood, L.D.

    1981-07-01

    Inner control rods for the High Flux Isotope Reactor were nondestructively inspected for defects by eddy-current techniques. During these examinations aluminum cladding thickness and oxide thickness on the cladding were also measured. Special application techniques were required because of the high-radiation levels (approx. 10 5 R/h at 30 cm) present and the relatively large temperature gradients that occurred on the surface of the control rods. The techniques used to perform the eddy-current inspections and the methods used to reduce the associated data are described

  14. Method for the protection of the cladding tubes of fuel rods

    International Nuclear Information System (INIS)

    Steinberg, E.

    1978-01-01

    To present stress crack corrosion and to protect the cladding tubes of the fuel rods made of a circonium alloy from attack by iodine, the inward surfaces are provided with protective coatings. Therefore the casting tubes already filled with fuel element pellets are put under over-pressure at a temperature range between 300 and 500 0 C, until almost yield-point is reached. A small amount of H 2 O or H 2 O 2 , filled in, reacts with the cladding tube material to form the Zr-O 2 protective coating. Afterwards comes a pressure relief, and the cladding tube reaches its original dimensions. (DG) [de

  15. Performance analysis of LMFBR control rods

    International Nuclear Information System (INIS)

    Pitner, A.L.; Birney, K.R.

    1975-01-01

    Control rods in the FFTF and LMFBR's will consist of pin bundles of stainless steel-clad boron carbide pellets. In the FFTF reference design, sixty-one pins of 0.474-inch diameter each containing a 36-inch stack of 0.362-inch diameter boron carbide pellets comprise a control rod. Reactivity control is provided by the 10 B (n,α) 7 Li reaction in the boron carbide. This reaction is accompanied by an energy release of 2.8 MeV, and heating from this reaction typically approaches 100 watts/cm 3 for natural boron carbide pellets in an LMFBR flux. Performance analysis of LMFBR control rods must include an assessment of the thermal performance of control pins. In addition, irradiation performance with regard to helium release, pellet swelling, and reactivity worth depletion as a function of service time must be evaluated

  16. Pellet clad interaction analysis of AFA 3G fuel rod

    International Nuclear Information System (INIS)

    Liu Tong; Shen Caifen; Jiao Yongjun; Lu Huaquan; Zhou Zhou

    2002-01-01

    The author described Pellet Clad Interaction (PCI) analysis of AFA 3G fuel rod during condition II transients for GNPS 18-months alternating equilibrium cycles. It provided PCI technical limit, analytical methods and computer code used in the analyses of condition II transients and thermal-mechanical. Finally, given main calculation results and the conclusion for GNPS 18-months cycles

  17. Specific features of the determination of the pellet-cladding gap of the fuel rods by non-destructive method

    International Nuclear Information System (INIS)

    Amosov, S.V.; Pavlov, S.V.

    2002-01-01

    This report describes the specific features of determining the pellet-cladding gap of the irradiated WWER-1000 fuel rods by nondestructive method. The method is based on the elastic radial deformation of the cladding up to its contact with the fuel. The value of deformation of cladding till its contacting fuel when radial force changes from F max to 0 is proposed as a measuring parameter for determination of the diametrical gap. Because of the features of compression method, the obtained gap value is not analog of the gap measured on micrograph of the fuel rod cross-section. Results of metallography can provide only qualitative evaluation of its method efficiency. Comparison of the values determined by non-destructive method and metallography for WWER-1000 fuel rods with burnup from 25 to 55 MWd/kg U testified that the results of compression method can be used as a low estimate of the pellet-cladding gap value. (author)

  18. Nuclear fuel rod with burnable plate and pellet-clad interaction fix

    International Nuclear Information System (INIS)

    Boyle, R.F.

    1987-01-01

    This patent describes a nuclear fuel rod comprising a metallic tubular cladding containing nuclear fuel pellets, the pellets containing enriched uranium-235. The improvement described here comprises: ceramic wafers, each wafter comprising a sintered mixture of gadolinium oxide and uranium dioxide, the uranium oxide having no more uranium-235 than is present in natural uranium dioxide. Each of the wafers is axially disposed between a major portion of adjacent the nuclear fuel pellets, whereby the wafers freeze out volatile fission products produced by the nuclear fuel and prevent interaction of the fission products with the metallic tubing cladding

  19. Fuel and control rod failure behavior during degraded core accidents

    International Nuclear Information System (INIS)

    Chung, K.S.

    1984-01-01

    As a part of the pretest and posttest analyses of Light Water Reactor Source Term Experiments (STEP) which are conducted in the Transient Reactor Test (TREAT) facility, this paper investigates the thermodynamic and material behaviors of nuclear fuel pins and control rods during severe core degradation accidents. A series of four STEP tests are being performed to simulate the characteristics of the power reactor accidents and investigate the behavior of fission product release during these accidents. To determine the release rate of the fission products from the fuel pins and the control rod materials, information concerning the timing of the clad failure and the thermodynamic conditions of the fuel pins and control rods are needed to be evaluated. Because the phase change involves a large latent heat and volume expansion, and the phase change is a direct cause of the clad failure, the understanding of the phase change phenomena, particularly information regarding how much of the fuel pin and control rod materials are melted are very important. A simple energy balance model is developed to calculate the temperature profile and melt front in various heat transfer media considering the effects of natural convection phenomena on the melting and freezing front behavior

  20. IFPE/IFA-508 and 515, PCMI Behaviour of Thin Cladding Rods, JAERI and HRP

    International Nuclear Information System (INIS)

    2007-01-01

    Description: To measure the integrated response of UO 2 and its cladding to conditions associated with PCI, the Japan Atomic Energy Research Institute carried out a series of experiments in the Halden BWR. The experiment involved two major objectives. The first was to study the influence of rod design parameters on PCI. Diametral gap, wall cladding thickness, SiO 2 additive, and pellet grain size were used as design parameters. The second objective was to study the influence of pre-irradiation (i.e. burnup) on PCI. The maximum burnup attained in the experiment was 23 MWd/kgU. These research results can be applied to current BWR-type fuel rods. The tests were performed between April 1977 and March 1981

  1. Fracture of Zircaloy cladding by interactions with uranium dioxide pellets in LWR fuel rods. Technical report 10

    International Nuclear Information System (INIS)

    Smith, E.; Ranjan, G.V.; Cipolla, R.C.

    1976-11-01

    Power reactor fuel rod failures can be caused by uranium dioxide fuel pellet-Zircaloy cladding interactions. The report summarizes the current position attained in a detailed theoretical study of Zircaloy cladding fracture caused by the growth of stress corrosion cracks which form near fuel pellet cracks as a consequence of a power increase after a sufficiently high burn-up. It is shown that stress corrosion crack growth in irradiated Zircaloy must be able to proceed at very low stress intensifications if uniform friction effects are operative at the fuel-cladding interface, when the interfacial friction coefficient is less than unity, when a symmetric distribution of fuel cracks exists, and when symmetric interfacial slippage occurs (i.e., ''uniform'' conditions). Otherwise, the observed fuel rod failures must be due to departures from ''uniform'' conditions, and a very high interfacial friction coefficient and particularly fuel-cladding bonding, are means of providing sufficient stess intensification at a cladding crack tip to explain the occurrence of cladding fractures. The results of the investigation focus attention on the necessity for reliable experimental data on the stress corrosion crack growth behavior of irradiated Zircaloy, and for further investigations on the correlation between local fuel-cladding bonding and stress corrosion cracking

  2. Fabrication of control rod system of RSG-GAS

    International Nuclear Information System (INIS)

    Hari-Sudirdjo; Setyono; Hendra-Prasetya

    2003-01-01

    Two unit absorbers, they are part of RSG-GAS control rod system, have been fabricated. One set absorber consist of two absorber plates and absorber casing. Absorber plate is made of Ag In Cd ( 80%, 15%, 5% ) alloy, which is cladded by stainless steel plate SS-316. Ag In Cd absorber plate has size of 625 mm x 60 mm x 3.3 mm, while cladding plat has thickness of 0.8 mm. Fabrication of two set absorbers has been conducted according to the plan

  3. Minimization of PWR reactor control rods wear

    International Nuclear Information System (INIS)

    Ponzoni Filho, Pedro; Moura Angelkorte, Gunther de

    1995-01-01

    The Rod Cluster Control Assemblies (RCCA's) of Pressurized Water Reactors (PWR's) have experienced a continuously wall cladding wear when Reactor Coolant Pumps (RCP's) are running. Fretting wear is a result of vibrational contact between RCCA rodlets and the guide cards which provide lateral support for the rodlets when RCCA's are withdrawn from the core. A procedure is developed to minimize the rodlets wear, by the shuffling and axial reposition of RCCA's every operating cycle. These shuffling and repositions are based on measurement of the rodlet cladding thickness of all RCCA's. (author). 3 refs, 2 figs, 2 tabs

  4. A model for predicting pellet-cladding interaction induced fuel rod failure, based on nonlinear fracture mechanics

    International Nuclear Information System (INIS)

    Jernkvist, L.O.

    1993-01-01

    A model for predicting pellet-cladding mechanical interaction induced fuel rod failure, suitable for implementation in finite element fuel-performance codes, is presented. Cladding failure is predicted by explicitly modelling the propagation of radial cracks under varying load conditions. Propagation is assumed to be due to either iodine induced stress corrosion cracking or ductile fracture. Nonlinear fracture mechanics concepts are utilized in modelling these two mechanisms of crack growth. The novelty of this approach is that the development of cracks, which may ultimately lead to fuel rod failure, can be treated as a dynamic and time-dependent process. The influence of cyclic loading, ramp rates and material creep on the failure mechanism can thereby be investigated. Results of numerical calculations, in which the failure model has been used to study the dependence of cladding creep rate on crack propagation velocity, are presented. (author)

  5. Characteristics and properties of cladding tubes for VVER-1000 higher Uranium content fuel rods

    International Nuclear Information System (INIS)

    Peregud, M.; Markelov, A.; Novikov, V.; Gusev, A.; Konkov, V.; Pimenov, Y.; Agapitov, V.; Shtutsa, M.

    2009-01-01

    To improve the fuel cycle economics and to further increase the VVER fuel usability the work programme is under way to design novel improved fuel, fuel rods and fuel assemblies. Longer FA operation time that is needed to increase the fuel burnup and the related design developments of novel fuel assemblies resulted not only in changing types and sizes of Zirconium items and fuel assembly components but also altered the requirements placed on their technical characteristics. To use fuel rods having a larger charge of fuel, to improve their behaviour in LOCA, to reduce fuel rod damage ability during assembling the work was carried out to perfect the characteristics of both the cladding (reduced wall thickness and more rigid tolerances for geometry) and its material. To meet the more rigid requirements for the geometry dimensions of cladding tubes an improved process flow sheet has been designed and employed for their fabrication and also the finishing treatment of tube surfaces has been improved. The higher and stable properties of the cladding materials were managed through using the special purity in terms of Hafnium Zirconium (not higher than 100 ppm Hf) as a base of the E110 alloy and maintaining within the valid specifications for the alloy the optimized contents of Oxygen and Iron at the levels of (600 - 990) ppm and (250 - 700) ppm, respectively. The work was under way in 2004 - 2008 years; during this period the technology and materials science solutions were mastered that were phased-in introduced into the production of the cladding tubes for the fuels loaded into the of the Kalinin NPP Unit 1

  6. Calculation of hydrogen and oxygen uptake in fuel rod cladding during severe accidents using the integral diffusion method -- Preliminary design report

    International Nuclear Information System (INIS)

    Siefken, L.J.

    1999-01-01

    Preliminary designs are described for models of hydrogen and oxygen uptake in fuel rod cladding during severe accidents. Calculation of the uptake involves the modeling of seven processes: (1) diffusion of oxygen from the bulk gas into the boundary layer at the external cladding surface, (2) diffusion from the boundary layer into the oxide layer, (3) diffusion from the inner surface of the oxide layer into the metallic part of the cladding, (4) uptake of hydrogen in the event that the cladding oxide layer is dissolved in a steam-starved region, (5) embrittlement of cladding due to hydrogen uptake, (6) cracking of cladding during quenching due to its embrittlement and (7) release of hydrogen from the cladding after cracking of the cladding. An integral diffusion method is described for calculating the diffusion processes in the cladding. Experimental results are presented that show a rapid uptake of hydrogen in the event of dissolution of the oxide layer and a rapid release of hydrogen in the event of cracking of the oxide layer. These experimental results are used as a basis for calculating the rate of hydrogen uptake and the rate of hydrogen release. The uptake of hydrogen is limited to the equilibrium solubility calculated by applying Sievert's law. The uptake of hydrogen is an exothermic reaction that accelerates the heatup of a fuel rod. An embrittlement criteria is described that accounts for hydrogen and oxygen concentration and the extent of oxidation. A design is described for implementing the models for hydrogen and oxygen uptake and cladding embrittlement into the programming framework of the SCDAP/RELAP5 code. A test matrix is described for assessing the impact of the proposed models on the calculated behavior of fuel rods in severe accident conditions. This report is a revision and reissue of the report entitled; ''Preliminary Design Report for Modeling of Hydrogen Uptake in Fuel Rod Cladding During Severe Accidents.''

  7. Some aspects of the utilization of zicaloy and austenitic steel as cladding material for PWR reactor fuel rods

    International Nuclear Information System (INIS)

    Teixeira e Silva, A.; Perrotta, J.A.

    1985-01-01

    The behaviour under irradiation of fuel rods for light water reactors was simulated by using fuel performance codes. Two types of cladding were analyzed: zircaloy and austenitic stainless steel. The fuel performance codes, originally made for zircaloy cladding, were adapted for austenitic stainless steel. The simulation results for the two types of cladding are presented, compared and discussed. (F.E.) [pt

  8. Post irradiation examination of control rod assembly of FBTR

    International Nuclear Information System (INIS)

    Anandaraj, V.; Raghu, N.; Venkiteswaran, C.N.; Visweswaran, P.; Vijayakumar, Ran; Jayaraj, V.V.; Padmaprabu, P.; Saravanan, T.; Philip, John; Muralidharan, N.G.; Joseph, Jojo; Kasiviswanathan, K.V.

    2010-01-01

    Six control rods with boron carbide pellets are used in FBTR for shutdown and control of reactor power. One control rod after being subjected to a fluence level of 7.2 x 10 22 n/cm 2 was received for post irradiation examination (PIE) to assess its irradiation behavior and to investigate the incident of dropping of control rod. Examinations carried out include precise dimensional measurements to investigate the possibility of interference between the control rod and outer sheath, Neutron radiography and x-radiograph to assess the integrity of the boron carbide pellets and other internals, density measurements to assess the swelling behaviour of boron carbide pellets and metallographic examinations to study the cracking behaviour and microstructural changes in the pellet and the clad. Depletion of B 10 in the pellet was studied using time of flight mass spectrometry. The paper highlights the examinations and results of the PIE carried out. (author)

  9. Out-of-pile experiments on the high-temperature behavior of Zircaloy-4 clad fuel rods

    International Nuclear Information System (INIS)

    Hagen, S.

    1984-01-01

    Out-of-pile experiments have been performed to investigate the escalation in temperature of Zircaloy-clad fuel rods during heatup in steam due to the exothermal Zircaloy steam reaction. In these tests single Zircaloy/uranium dioxide (UO 2 ) fuel rod simulators surrounded with a Zircaloy shroud--simulating the Zircaloy of neighboring rods--were heated inside a fiber ceramic insulation. The initial heating rates were varied from 0.3 to 2.5 K/s. In every test an escalation of the temperature rise rate was observed. The maximum measured surface temperature was about 2200 0 C. The temperature decreased after the maximum had been reached without decreasing the input electric power. The temperature decreases were due to inherent processes including the runoff of molten Zircaloy. The escalation process was influenced by the temperature behavior of the shroud, which was itself affected by the insulation and steam cooling. Damage to the fuel rods increased with increasing heatup rate. Fro slow heatup rates nearly no interaction between the oxidized cladding and UO 2 was observed, while for fast heatup rates the entire annular pellet was dissolved by molten Zircaloy

  10. The role of cladding material for performance of LWR control assemblies

    International Nuclear Information System (INIS)

    Dewes, P.; Roppelt, A.

    2000-01-01

    The lifetime of control assemblies in LWRs can be limited presently by mechanical failure of the absorber cladding. The major cause of failure is mechanical interaction of the absorber with the cladding due to irradiation induced dimensional changes such as absorber swelling and cladding creep, resulting in cracking of the clad. Such failures occurred in both BWRs and PWRs. Experience and in-reactor tests revealed that cracking can be avoided principally by two ways: First, if strain rates and hence, stresses in the cladding are kept low (well below the yield strength), significant strains can be tolerated. This is the case for the cladding of PWR control assemblies with slowly swelling Ag-In-Cd absorber. Recent examinations of highly exposed PWR control assemblies confirmed the design correlation up to the presently used strain limit. Second, in such cases where strongly swelling absorber material like boron carbide is still preferred, materials which are resistant against irradiation assisted stress corrosion cracking (IASCC) can be used. The influence of material composition and condition on IASCC was studied in-reactor using tubular samples of various stainless steels and Ni-base alloys stressed by swelling mandrels. In several programme steps high purity materials with special features had been identified as resistant to IASCC. Another process of cladding damage which may occur in PWRs is wear caused by friction of the control rods in the surrounding guide structure. For replacement control assemblies this problem is solved by coating of the cladding. There exists meanwhile excellent experience of up to 18 operation cycles with coated claddings. (author)

  11. Postirradiation examination of JOYO MK-II control rod (CRM601). Irradiation performance of shroud type absorber pin

    International Nuclear Information System (INIS)

    Tanaka, Kosuke; Kikuchi, Shin; Katsuyama, Kozo; Nagamine, Tsuyoshi; Mitsugi, Takeshi; Uto, Manabu; Tatebe, Kazuaki; Onose, Shoji; Maruyama, Tadashi

    1998-10-01

    This paper describes the results of postirradiation examination and analysis by CORAL code for irradiation performance of CRM601 control rod, which was the 6th reloaded control rod with shroud type absorber pins for use in JOYO MK-II core. The detailed visual examination indicated that there was no cladding breach in absorber pins. However, sodium ingress from the vent tube was observed in four absorber pins among seven pins. While a remarkable oval deformation occurred in cladding tube of helium bonded absorber pins, a little or no diametral change was observed in the absorber pins in which sodium ingress took place. From metallurgical observations and the analysis by CORAL code, it was estimated that the shroud tube installed in helium bonded absorber pins were irradiated at 720degC, and those in sodium bonded absorber pins were irradiated at 420degC. It was confirmed that diametral change of cladding depended on the initial gap between shroud and cladding tube. The results of present investigation indicate that it is desirable to use the materials with low thermal expansion coefficient for shroud tubes, and that sodium bonded absorber pins were advantageous for obtaining long life control rods. (author)

  12. Design of cladding rods-assisted depressed-core few-mode fibers with improved modal spacing

    Science.gov (United States)

    Han, Jiawei; Zhang, Jie

    2018-03-01

    This paper investigates the design details of cladding rods-assisted (CRA) depressed-core (DC) few-mode fibers (FMFs) that feature more equally spaced linearly polarized (LP) modal effective indices, suitable for high-spatial-density weakly-coupled mode-division multiplexing systems. The influences of the index profile of cladding rods on LP mode-resolved effective index, bending sensitivity, and effective area Aeff, are numerically described. Based on the design considerations of LP modal Aeff-dependent spatial efficiency and LP modal bending loss-dependent robustness, the small LP21-LP02 and LP22-LP03 modal spacing limitations, encountered in state-of-the-art weakly-coupled step-index FMFs, have been substantially improved by at least 25%. In addition, the proposed CRA DC FMFs also show sufficiently large effective areas (in excess of 110 μm2) for all guided LP modes, which are expected to exhibit good nonlinear performance.

  13. Modeling of the PWR fuel mechanical behaviour and particularly study of the pellet-cladding interaction in a fuel rod

    International Nuclear Information System (INIS)

    Hourdequin, N.

    1995-05-01

    In Pressurized Water Reactor (PWR) power plants, fuel cladding constitutes the first containment barrier against radioactive contamination. Computer codes, developed with the help of a large experimental knowledge, try to predict cladding failures which must be limited in order to maintain a maximal safety level. Until now, fuel rod design calculus with unidimensional codes were adequate to prevent cladding failures in standard PWR's operating conditions. But now, the need of nuclear power plant availability increases. That leads to more constraining operating condition in which cladding failures are strongly influenced by the fuel rod mechanical behaviour, mainly at high power level. Then, the pellet-cladding interaction (PCI) becomes important, and is characterized by local effects which description expects a multidimensional modelization. This is the aim of the TOUTATIS 2D-3D code, that this thesis contributes to develop. This code allows to predict non-axisymmetric behaviour too, as rod buckling which has been observed in some irradiation experiments and identified with the help of TOUTATIS. By another way, PCI is influenced by under irradiation experiments and identified with the help of TOUTATIS which includes a densification model and a swelling model. The latter can only be used in standard operating conditions. However, the processing structure of this modulus provides the possibility to include any type of model corresponding with other operating conditions. In last, we show the result of these fuel volume variations on the cladding mechanical conditions. (author). 25 refs., 89 figs., 2 tabs., 12 photos., 5 appends

  14. The fuel-cladding interfacial friction coefficient in water-cooled reactor fuel rods

    International Nuclear Information System (INIS)

    Smith, E.

    1979-01-01

    A central problem in the development of cladding failure criteria and of effective operational, design or material remedies is to know whether the cladding stress is enhanced significantly near cladding ridges, pellet chips or fuel pellet cracks; the latter may also be coincident with cladding ridges at pellet-pellet interfaces. As regards the fuel pellet crack source of cladding stress concentration, the magnitude of the uranium dioxide-Zircaloy interfacial friction coefficient μ governs the magnitude and distribution of the enhanced cladding stress. Considerable discussion, particularly at a Post-Conference Seminar associated with the SMIRT 4 Conference, has focussed on the value of μ, the author taking the view that it is unlikely to be large (< 0.5). The reasoning behind this view is as follows. A fuel pellet should fracture during a power ramp when the tensile hoop stress within the pellet exceeds the fuel's fracture stress. Since the preferred position for a fuel pellet crack to form is at the fuel-cladding interface midway between existing fuel cracks, where the interfacial shear stress changes sign, the pellet segment size after a power ramp provides a limit to the magnitude of the interfacial shear stresses and consequently to the value of μ. With this argument as a basis, the author's early work used the Gittus fuel rod model, in which there is a symmetric distribution of fuel pellet cracks and symmetric interfacial slippage, to show that μ < 0.5 if it is assumed that the average hoop stress within the cladding attains yield levels. It was therefore suggested that a high interfacial friction coefficient is unlikely to be operative during a power ramp; this result was used to support the view that interfacial friction effects do not play a dominant role in stress corrosion crack formation within the cladding. (orig.)

  15. Radiological characterization of spent control rod assemblies

    International Nuclear Information System (INIS)

    Lepel, E.A.; Robertson, D.E.; Thomas, C.W.; Pratt, S.L.; Haggard, D.L.

    1995-10-01

    This document represents the final report of an ongoing study to provide radiological characterizations, classifications, and assessments in support of the decommissioning of nuclear power stations. This report describes the results of non-destructive and laboratory radionuclide measurements, as well as waste classification assessments, of BWR and PWR spent control rod assemblies. The radionuclide inventories of these spent control rods were determined by three separate methodologies, including (1) direct assay techniques, (2) calculational techniques, and (3) by sampling and laboratory radiochemical analyses. For the BWR control rod blade (CRB) and PWR burnable poison rod assembly (BPRA), 60 Co and 63 Ni, present in the stainless steel cladding, were the most abundant neutron activation products. The most abundant radionuclide in the PWR rod cluster control assembly (RCCA) was 108m Ag (130 yr halflife) produced in the Ag-In-Cd alloy used as the neutron poison. This radionuclide will be the dominant contributor to the gamma dose rate for many hundreds of years. The results of the direct assay methods agree very well (±10%) with the sampling/radiochemical measurements. The results of the calculational methods agreed fairly well with the empirical measurements for the BPRA, but often varied by a factor of 5 to 10 for the CRB and the RCCA assemblies. If concentration averaging and encapsulation, as allowed by 10CFR61.55, is performed, then each of the entire control assemblies would be classified as Class C low-level radioactive waste

  16. Investigation of typicality of non-nuclear rod and fuel-clad gap effect during reflood phase, and development of a FEM thermal transient analysis code HETFEM

    International Nuclear Information System (INIS)

    Sudoh, Takashi

    1981-06-01

    The objective of this study are: 1) Evaluate the capability of the electrical heater for simulating the fuel rod during the reflood phase, and 2) To investigate the effect of the clad-fuel gap in the fuel rod on the clad thermal response during the reflood phase. A computer code HETFEM which is the two dimensional transient thermal conductivity analysis code utilized a finite element method is developed for analysing thermal responses of heater and fuel rod. The two kinds of electrical heaters and a fuel rod are calculated with simple boundary conditions. 1) direct heater (former JAERI reflood test heater), 2) indirect heater (FLECHT test heater), 3) fuel rod (15 x 15 type in Westinghouse PWR). The comparison of the clad temperature responses shows the quench time is influenced by the thermal diffusivity and gap conductance. In the conclusion, the ELECHT heater shows atypicality in the clad temperature response and heat releasing rate. But the direct heater responses are similar to those of the fuel rod. For the gap effect on the fuel rod behavior, the lower gap conductance causes sooner quench and less heat releasing rate. This calculation is not considered the precursory cooling which is affected by heat releasing rate at near and below the quench front. Therefore two dimensional calculation with heat transfer related to the local fluid conditions will be needed. (author)

  17. Laboratory simulation of rod-to-rod mechanical interactions during postulated loss-of-coolant accidents in a PWR involving cladding oxidation

    International Nuclear Information System (INIS)

    Hindle, E.D.; Haste, T.J.; Harrison, W.R.

    1987-01-01

    Creep deformation of Zircaloy cladding in postulated PWR loss-of-coolant accidents may lead to rod-to-rod mechanical interactions. Tests have been performed in the electrically heated FOURSQUARE rig at 750 0 C and 850 0 C in steam to investigate this effect. Conservatisms inherent in a simple 'square with rounded corners' coolant channel blockage model have been quantified; about 5-10% flow area may remain even at strains which in ideal circumstances would give total blockage. Reduction of average burst strains produced by an oxide layer (up to 13 μm) has been demonstrated, resulting from strain concentration at oxide cracks. (author)

  18. Development and fabrication of seamless Aluminium finned clad tubes for metallic uranium fuel rods for research reactor

    International Nuclear Information System (INIS)

    Singh, A.K.; Hussain, M.M.; Jayachandran, N.K.; Abdulla, K.K.

    2012-01-01

    Natural uranium metal or its alloy is used as fuel in nuclear reactors. Usually fuel is clad with compatible material to prevent its direct contact with coolant which prevents spread of activity. One of the methods of producing fuel for nuclear reactor is by co-drawing finished uranium rods with aluminum clad tube to develop intimate contact for effective heat removal during reactor operation. Presently seam welded Aluminium tubes are used as clad for Research Reactor fuel. The paper will highlight entire fabrication process followed for the fabrication of seamless Aluminium finned tubes along with relevant characterisation results

  19. The M5 Fuel Rod Cladding

    International Nuclear Information System (INIS)

    Mardon, J.P.; Charquet, D.; Senevat, J.

    1998-01-01

    The large-scale program for the development and irradiation of new Zr alloys started by FRAMATOME and its industrial partners CEZUS and ZIRCOTUBE more than 10 years ago is now enabling FRAGEMA to offer the ternary M5 (ZrNbO) as the cladding material for PWR advanced fuel rods. Compared with the former product (low-tin-Zircaloy-4), this alloy exhibits impressive gains under irradiation at extended burnup (55 GWd/t) relatively to corrosion (factor 3 to 4), hydriding (factor 5 to 6), growth and creep (factor 2 to 3). In this paper, we shall successively address: - the industrial development and manufacturing experience - the corrosion, hydriding, creep and growth performances obtained over a wide range of PWR normal irradiation conditions (France and other countries) up to burnups of 55 GWd/t - The interpretation of these results by means of analytical experiments conducted in test reactors (free growth, creep) and microstructural observations on the irradiated material - and the behaviour under accident (LOCA) and severe environment and irradiation (Li, boiling) conditions. (Author)

  20. An evaluation of the influence of fuel design parameters and burnup on pellet/cladding interaction for boiling water reactor fuel rod through in-core diameter measurement

    International Nuclear Information System (INIS)

    Yanagisawa, K.

    1986-01-01

    The influence of design parameters and burning on pellet/cladding interaction (PCI) of current boiling water reactor fuel rods was studied through in-core diameter measurement. Thinner cladding and a smaller diametral gap enhanced the PCI during startup. At constant power, fuel with SiO 2 added greatly reduced PCI due to relaxation. The fuel with a small grain size greatly reduced PCI due to densification. Preirradiation of rods up to 23 MWd/kgU caused a large PCI not only in a small gap but also in a large gap rod. Relaxation and permanent deformation was small. In the power increase experiment, one rod experienced PCI failure. The spurt times of coolant radioactivity coincided well with the sudden drop of cladding axial strain and marked crack opening at the rod surface. The estimated hoop stress predicted by FEMAXI-III was 350 MPa at the failure

  1. Investigation of axial power gradients near a control rod tip

    Energy Technology Data Exchange (ETDEWEB)

    Loberg, John, E-mail: John.Loberg@fysast.uu.se [Uppsala University, Department of Physics and Astronomy, Division of Applied Nuclear Physics, Box 525, SE-75120 Uppsala (Sweden); Osterlund, Michael, E-mail: Michael.Osterlund@fysast.uu.se [Uppsala University, Department of Physics and Astronomy, Division of Applied Nuclear Physics, Box 525, SE-75120 Uppsala (Sweden); Bejmer, Klaes-Hakan, E-mail: Klaes-Hakan.Bejmer@vattenfall.com [Vattenfall Nuclear Fuel AB, Jaemtlandsgatan 99, 162 60 Vaellingby, Stockholm (Sweden); Blomgren, Jan, E-mail: Jan.Blomgren@vattenfall.com [Vattenfall Nuclear Fuel AB, Jaemtlandsgatan 99, 162 60 Vaellingby, Stockholm (Sweden); Kierkegaard, Jesper, E-mail: Jesper.Kierkegaar@vattenfall.com [Vattenfall Nuclear Fuel AB, Jaemtlandsgatan 99, 162 60 Vaellingby, Stockholm (Sweden)

    2011-07-15

    Highlights: > Pin power gradients near BWR control rod tips have been investigated. > A control rod tip is modeled in MCNP and compared to simplified 2D/3D geometry. > Small nodes increases pin power gradients; standard nodes underestimates gradients. > The MCNP results are validated against axial gamma scan of a controlled fuel pin. - Abstract: Control rod withdrawal in BWRs induces large power steps in the adjacent fuel assemblies. This paper investigates how well a 2D/3D method, e.g., CASMO5/SIMULATE5 computes axial pin power gradients adjacent to an asymmetrical control-rod tip in a BWR. The ability to predict pin power gradients accurately is important for safety considerations whereas large powers steps induced by control rod withdrawal can cause Pellet Cladding Interaction. The computation of axial pin power gradients axially around a control rod tip is a challenging task for any nodal code. On top of that, asymmetrical control rod handles are present in some BWR designs. The lattice code CASMO requires diagonal symmetry of all control rod parts. This introduces an error in computed pin power gradients that has been evaluated by Monte Carlo calculations. The results show that CASMO5/SIMULATE5, despite the asymmetrical control rod handle, is able to predict the axial pin power gradient within 1%/cm for axial nodal sizes of 15-3.68 cm. However, a nodal size of 3.68 cm still causes underestimations of pin power gradients compared with 1 cm nodes. Furthermore, if conventional node sizes are used, {approx}15 cm, pin power gradients can be underestimated by over 50% compared with 1 cm nodes. The detailed axial pin power profiles from MCNP are corroborated by measured gamma scan data on fuel rods irradiated adjacent to control rods.

  2. Investigation of axial power gradients near a control rod tip

    International Nuclear Information System (INIS)

    Loberg, John; Osterlund, Michael; Bejmer, Klaes-Hakan; Blomgren, Jan; Kierkegaard, Jesper

    2011-01-01

    Highlights: → Pin power gradients near BWR control rod tips have been investigated. → A control rod tip is modeled in MCNP and compared to simplified 2D/3D geometry. → Small nodes increases pin power gradients; standard nodes underestimates gradients. → The MCNP results are validated against axial gamma scan of a controlled fuel pin. - Abstract: Control rod withdrawal in BWRs induces large power steps in the adjacent fuel assemblies. This paper investigates how well a 2D/3D method, e.g., CASMO5/SIMULATE5 computes axial pin power gradients adjacent to an asymmetrical control-rod tip in a BWR. The ability to predict pin power gradients accurately is important for safety considerations whereas large powers steps induced by control rod withdrawal can cause Pellet Cladding Interaction. The computation of axial pin power gradients axially around a control rod tip is a challenging task for any nodal code. On top of that, asymmetrical control rod handles are present in some BWR designs. The lattice code CASMO requires diagonal symmetry of all control rod parts. This introduces an error in computed pin power gradients that has been evaluated by Monte Carlo calculations. The results show that CASMO5/SIMULATE5, despite the asymmetrical control rod handle, is able to predict the axial pin power gradient within 1%/cm for axial nodal sizes of 15-3.68 cm. However, a nodal size of 3.68 cm still causes underestimations of pin power gradients compared with 1 cm nodes. Furthermore, if conventional node sizes are used, ∼15 cm, pin power gradients can be underestimated by over 50% compared with 1 cm nodes. The detailed axial pin power profiles from MCNP are corroborated by measured gamma scan data on fuel rods irradiated adjacent to control rods.

  3. Fuel rod simulator effects in flooding experiments single rod tests

    International Nuclear Information System (INIS)

    Nishida, M.

    1984-09-01

    The influence of a gas filled gap between cladding and pellet on the quenching behavior of a PWR fuel rod during the reflood phase of a LOCA has been investigated. Flooding experiments were conducted with a short length electrically heated single fuel rod simulator surrounded by glass housing. The gap of 0.05 mm width between the Zircaloy cladding and the internal Al 2 O 3 pellets of the rod was filled either wit helium or with argon to vary the radial heat resistance across the gap. This report presents some typical data and an evaluation of the reflood behavior of the fuel rod simulator used. The results show that the quench front propagates faster for increasing heat resistance in the gap between cladding and heat source of the rod. (orig.) [de

  4. Monte Carlo simulation of a research reactor with nominal power of 7 MW to design new control safety rods

    Energy Technology Data Exchange (ETDEWEB)

    Shoushtari, M.K.; Kakavand, T. [Faculty of Science, University of Zanjan, Zanjan, P.O. Box 451-313 (Iran, Islamic Republic of); Sadat Kiai, S.M., E-mail: sadatkiai@yahoo.co [Nuclear Science and Technology Research Institute (NSTR), Nuclear Science Research, A.E.O.I., P.O. Box 14155-1339, Tehran (Iran, Islamic Republic of); Ghaforian, H. [Faculty of Science and Technology of Marine, Tehran (Iran, Islamic Republic of)

    2010-03-01

    The Monte Carlo simulation has been established for a research reactor with nominal power of 7 MW. A detailed model of the reactor core was employed including standard and control fuel elements, reflectors, irradiation channels, control rods, reactor pool and thermal column. The following physical parameters of reactor core were calculated for the present LEU core: core reactivity (rho), control rod (CR) worth, thermal and epithermal neutron flux distributions, shutdown margin and delayed neutron fraction. Reduction of unfavorable effects of blockage probability of control safety rod (CSR)s in their interiors because of not enough space in their sites, and lack of suitable capabilities to fabricate very thin plates for CSR cladding, is the main aim of the present study. Making the absorber rod thinner and CSR cladding thicker by introducing a better blackness absorbing material and a new stainless steel alloy, respectively, are two studied ways to reduce the effects of mentioned problems.

  5. Control rod

    International Nuclear Information System (INIS)

    Kawakami, Kazuo; Shimoshige, Takanori; Nishimura, Akira

    1979-01-01

    Purpose: A control rod has been developed, which provided a plurality of through-holes in the vicinity of the sheath fitting position, in order to flatten burn-up, of fuel rods in positions confronting a control rod. Thereby to facilitate the manufacture of the control rods and prevent fuel rod failures. Constitution: A plurality of through-holes are formed in the vicinity of the sheath fitting position of a central support rod to which a sheath for the control rod is fitted. These through-holes are arranged in the axial direction of the central support rod. Accordingly, burn-up of fuel rods confronting the control rods can be reduced by through-holes and fuel rod failures can be prevented. (Yoshino, Y.)

  6. PWR control rods wear by vibrations induced by coolant fluid

    International Nuclear Information System (INIS)

    Reynier, R.

    1997-01-01

    Flow induced vibrations in pressurised water reactors generate the wear of control rods against their guidance systems. Alternate sliding (at 320 deg. C in water) and impact-sliding tests (at room temperature in air) were carried out on 304 L austenitic stainless steel control rods' claddings. Microstructural analysis were made on the wear scars of the tube specimen using Scanning ELectron Microscopy, microhardness measurements and X-ray diffractometry. The alternate sliding leads to an important mass loss, a strong plastic deformation due to the strain hardening of the surface layers and generates strong compressive residual stresses. These results are specific to a severe wear case. Therefore, the impact-sliding mode induces martensitic phase, a cracked oxide layer and a compressive residual stresses weaker than those created in the alternate sliding case. This type of motion leads to a milder wear of the control rods

  7. Calculation of thermoelastic stresses in the rewetting region of the fuel rod cladding during a loss of coolant accident (loca)

    International Nuclear Information System (INIS)

    Roberty, N.C.; Carmo, E.G.D. do; Tanajura, C.A.S.

    1982-01-01

    A one-dimensional model for axial distribution calculation of temperature and thermal stresses in the fuel rod cladding for a Pressurized Water Reactors (PWR) is developed. The effect of the coolant inlet temperaure, the Leidenfrost and the nucleate boiling in the stress distribution are evaluated. A perturbation in the cladding stress state is obtained. (E.G.) [pt

  8. Temperature analysis of the control rods at the scram shutdown of the HTTR. Evaluation by using measurement data at scram test of HTTR

    Energy Technology Data Exchange (ETDEWEB)

    Takada, Eiji; Fujimoto, Nozomu; Nakagawa, Shigeaki [Japan Atomic Energy Research Inst., Oarai, Ibaraki (Japan). Oarai Research Establishment; Matsuda, Atsuko [Toshiba Co., Tokyo (Japan)

    2003-03-01

    In the High Temperature Engineering Test Reactor (HTTR), since the primary coolant temperature become 950 degrees centigrade at the high temperature test operation, the special alloy Alloy800H is used for cladding tubes and spines of the control rods to endure the high temperature. The temperature limitation of control rod is 900 degrees centigrade according to the strength data of Alloy800H. The scram shutdown by loss of off-site electric power at the high temperature test operation was assumed as an transient of the temperature of the control rods cladding might exceed 900 degrees centigrade. In this report, the temperature of the control rods is analyzed by using the measurement data of the rise-to-power test. From the result of this analysis, it was confirmed that the control rod temperature does not exceed the limit even at the transient of the loss of off-site electric power from the high temperature test operation. (author)

  9. Investigation of in-pile formed corrosion films on zircaloy fuel-rod claddings by impedance spectroscopy and galvanostatic anodization

    International Nuclear Information System (INIS)

    Gebhardt, O.

    1993-01-01

    Hot-cell investigations have been executed to study the corrosion behaviour of irradiated Zircaloy fuel-rod claddings by impedance spectroscopy and galvanostatic anodization. The thickness of the compact oxide at the metal/oxide interface and the thickness of the minimum barrier oxide have been determined at different positions along the claddings. As shown by analysis, both quantities first increase and then decrease with increasing thickness of the total oxide. (author) 6 figs., 33 refs

  10. Control rods

    International Nuclear Information System (INIS)

    Maruyama, Hiromi.

    1984-01-01

    Purpose: To realize effective utilization, cost reduction and weight reduction in neutron absorbing materials. Constitution: Residual amount of neutron absorbing material is averaged between the top end region and other regions of a control rod upon reaching to the control rod working life, by using a single kind of neutron absorbing material and increasing the amount of the neutron absorber material at the top end region of the control rod as compared with that in the other regions. Further, in a case of a control rod having control rod blades such as in a cross-like control rod, the amount of the neutron absorbing material is decreased in the middle portion than in the both end portions of the control rod blade along the transversal direction of the rod, so that the residual amount of the neutron absorbing material is balanced between the central region and both end regions upon reaching the working life of the control rod. (Yoshihara, H.)

  11. Numerical solution of the elastic non-axial contact between pellet and cladding of fuel rod in PWR

    International Nuclear Information System (INIS)

    Zymak, J.

    1987-08-01

    Elastic non-axial contacts between the pellet and the cladding of a fuel rod in a pressurized water reactor were calculated. The existence and the uniqueness of the solution were proved. The problem was approximated by the finite element method and quadratic programming was used for the solution. The results will be used in the solution of the probabilistic model of a fuel rod with non-axial pellets in a PWR. (author). 10 figs., 4 tabs., 10 refs

  12. Prevention of nuclear fuel cladding materials corrosion

    International Nuclear Information System (INIS)

    Yang, K.R.; Yang, J.C.; Lee, I.C.; Kang, H.D.; Cho, S.W.; Whang, C.K.

    1983-01-01

    The only way which could be performed by the operator of nuclear power plant to minimizing the degradation of nuclear fuel cladding material is to control the water quality of primary coolant as specified standard conditions which dose not attack the cladding material. If the water quality of reactor coolant does not meet far from the specification, the failure will occure not only cladding material itself but construction material of primary system which contact with the coolant. The corrosion product of system material are circulate through the whole primary system with the coolant and activated by the neutron near the reactor core. The activated corrosion products and fission products which released from fuel rod to the coolant, so called crud, will repeate deposition and redeposition continuously on the fuel rod and construction material surface. As a result we should consider heat transfer problem. In this study following activities were performed; 1. The crud sample was taken from the spent fuel rod surface of Kori unit one and analized for radioactive element and non radioactive chemical species. 2. The failure mode of nuclear fuel cladding material was estimated by the investigation of releasing type of fission products from the fuel rod to the reactor coolant using the iodine isotopes concentration of reactor coolants. 3. A study was carried out on the sipping test results of spent fuel and a discussion was made on the water quality control records through the past three cycle operation period of Kori unit one plant. (Author)

  13. Procedure and apparatus for measuring the radial gap between fuel and surrounding cladding in a fuel rod for a nuclear reactor

    International Nuclear Information System (INIS)

    Olshausen, K.D.

    1976-01-01

    A device is described for measuring non-destructively the annular fuel-cladding gap in an irradiated or fresh fuel rod. The principle applied is that a force is applied to an arm which presses the cladding diametrically, thus deforming it until it touches the fuel pellet. By presenting the values of the force applied and the deformation produced on an XY recorder, the width of the gap is obtained. Alternatively the gap width may be obtained digitally. Since the gap is so small that the deformation is within the elastic range, the fuel rod may be reloaded in the reactor for further irradiation. (JIW)

  14. Analysis of Double-encapsulated Fuel Rods

    Energy Technology Data Exchange (ETDEWEB)

    Hales, Jason Dean [Idaho National Laboratory; Medvedev, Pavel G [Idaho National Laboratory; Novascone, Stephen Rhead [Idaho National Laboratory; Perez, Danielle Marie [Idaho National Laboratory; Williamson, Richard L [Idaho National Laboratory

    2014-09-01

    In an LWR fuel rod, the cladding encapsulates the fuel, contains fission products, and transfers heat directly to the water coolant. In some situations, it may be advantageous to separate the cladding from the coolant through use of a secondary cladding or capsule. This may be done to increase confidence that the fuel or fission products will not mix with the coolant, to provide a mechanism for controlling the rod temperature, or to place multiple experimental rodlets within a single housing. With an axisymmetric assumption, it is possible to derive closed-form expressions for the temperature profile in a fuel rod using radially-constant thermal conductivity in the fuel. This is true for both a traditional fuel-cladding rod and a double-encapsulated fuel (fuel, cladding, capsule) configuration. Likewise, it is possible to employ a fuel performance code to analyse both a traditional and a double-encapsulated fuel. In the case of the latter, two sets of gap heat transfer conditions must be imposed. In this work, we review the equations associated with radial heat transfer in a cylindrical system, present analytic and computational results for a postulated power and gas mixture history for IFA-744, and describe the analysis of the AFC-2A, 2B metallic fuel alloy experiments at the Advanced Test Reactor, including the effect of a release of fission products into the cladding-capsule gap. The computational results for these two cases were obtained using BISON, a fuel performance code under development at Idaho National Laboratory.

  15. Method and apparatus for sizing nuclear fuel rod cladding tubes

    International Nuclear Information System (INIS)

    Koehler, L.

    1976-01-01

    Nuclear fuel rod cladding tubes are sized internally to diameters precisely fitting nuclear fuel pellets with which the tubes are charged by externally applying hydraulic pressure to short lengths of each tube. The pressure is applied while the tube is stationary. The tube is then moved to bring a new length within the hydraulic pressure zone. The volume of the hydraulic liquid used and the pressure applied to this liquid is such that the liquid is compressed slightly so that the length being sized yields, the expansion of the liquid then completing the sizing. The lengths being sized step-by-step are internally supported by either the fuel pellets or a mandrel having the same diameter as the pellets

  16. Accident-tolerant control rod

    International Nuclear Information System (INIS)

    Ohta, Hirokazu; Sawabe, Takashi; Ogata, Takanari

    2013-01-01

    Boron carbide (B 4 C) and hafnium (Hf) metal are used for the neutron absorber materials of control rods in BWRs, and silver-indium-cadmium (Ag-In-Cd) alloy is used in PWRs. These materials are clad with stainless steel. The eutectic point of B 4 C and iron (Fe) is about 1150 deg. C and the melting point of Ag-In-Cd alloy is about 800 deg. C, which are lower than the temperature of zircaloy - steam reaction increases rapidly (∼1200 deg. C). Accordingly, it is possible that the control rods melt and collapse before the reactor core is significantly damaged in the case of severe accidents. Since the neutron absorber would be separated from the fuels, there is a risk of re-criticality, when pure water or seawater is injected for emergency cooling. In order to ensure sub-criticality and extend options of emergency cooling in the course of severe accidents, a concept of accident-tolerant control rod (ACT) has been derived. ACT utilises a new absorber material having the following properties: - higher neutron absorption than current control rod; - higher melting or eutectic temperature than 1200 deg. C where rapid zircaloy oxidation occurs; - high miscibility with molten fuel materials. The candidate of a new absorber material for ATC includes gadolinia (Gd 2 O 3 ), samaria (Sm 2 O 3 ), europia (Eu 2 O 3 ), dysprosia (Dy 2 O 3 ), hafnia (HfO 2 ). The melting point of these materials and the liquefaction temperature with Fe are higher than the rapid zircaloy oxidation temperature. ACT will not collapse before the core melt-down. After the core melt-down, the absorber material will be mixed with molten fuel material. The current absorber materials, such as B 4 C, Hf and Ag-In-Cd, are charged at the tip of ATC in which the neutron flux is high, and a new absorber material is charged in the low-flux region. This design could minimise the degradation of a new absorber material by the neutron absorption and the influence of ATC deployment on reactor control procedure. As a

  17. Control rod drives

    International Nuclear Information System (INIS)

    Nakamura, Akira.

    1984-01-01

    Purpose: To enable to monitor the coupling state between a control rod and a control rod drive. Constitution: After the completion of a control rod withdrawal, a coolant pressure is applied to a control rod drive being adjusted so as to raise only the control rod drive and, in a case where the coupling between the control rod drive and the control rod is detached, the former is elevated till it contacts the control rod and then stopped. The actual stopping position is detected by an actual position detection circuit and compared with a predetermined position stored in a predetermined position detection circuit. If both of the positions are not aligned with each other, it is judged by a judging circuit that the control rod and the control rod drives are not combined. (Sekiya, K.)

  18. Stress corrosion testing of irradiated cladding tubes

    International Nuclear Information System (INIS)

    Lunde, L.; Olshausen, K.D.

    1980-01-01

    Samples from two fuel rods with different cladding have been stress corrosion tested by closed-end argon-iodine pressurization at 320 0 C. The fuel rods with stress relieved and recrystallized Zircaloy-2 had received burnups of 10.000 and 20.000 MWd/ton UO 2 , respectively. It was found that the SCC failure stress was unchanged or slightly higher for the irradiated than for the unirradiated control tubes. The tubes failed consistently in the end with the lowest irradiation dose. The diameter increase of the irradiated cladding during the test was 1.1% for the stress-relieved samples and 0.24% for the recrystallized samples. SEM examination revealed no major differences between irradiated and unirradiated cladding. A ''semi-ductile'' fracture zone in recrystallized material is described in some detail. (author)

  19. Control rod assembly

    International Nuclear Information System (INIS)

    Takahashi, Akio.

    1982-01-01

    Purpose: To enable reliable insertion and drops of control rods, as well as insure a sufficient flow rate of coolants flowing through the control rods for attaining satisfactory cooling thereof to enable relexation of thermal stress resulted to rectifying mechanisms or the likes. Constitution: To the outer circumference of a control rod contained vertically movably within a control rod guide tube, resistive members are retractably provided in such a way as to project to close the gap between outer circumference of the control rod and the inner surface of the control rod guide tube upon engagement of a gripper of control rod drives, and retract upon release of the engagement of the gripper. Thus, since the resistive members project to provide a greater resistance to the coolants flowing between them and the control rod guide tube in the normal operation where the gripper is engaged to drive the control rod by the control rod drives, a major part of the coolant flowing into the control rod guide tube flows into the control rod. This enables to cool the control rod effectively and make the temperature distribution uniform for the coolant flowing from the upper end of the control rod guide tube to thereby attain the relaxation of the thermal stress resulted in the rectifying mechanisms or the likes. (Moriyama, K.)

  20. Device for coupling a control rod and control rod drive

    International Nuclear Information System (INIS)

    Nishioka, Kazuya.

    1975-01-01

    Object: To obtain simple and reliable coupling between a control rod and control rod drive by equipping the lower end of the control rod with an extension provided with lateral protuberances and forming the upper end of an index tube with a recess provided with lateral holes. Structure: The tapering central extension of the control rod is inserted into the recess by lowering the control rod, and then it is further inserted by causing frictional movement of the inclined surfaces of lateral protuberances in frictional contact with guide surfaces. When the lateral protuberances are brought into contact with a stepped portion, the control rod is rotated to fit the lateral protuberances into the lateral holes. In this way, the control rod is coupled to the index tube of the control rod drive. (Yoshino, Y.)

  1. Thermalhydraulic phenomena governing the quenching of hot rods, and existing models

    International Nuclear Information System (INIS)

    Bestion, D.

    2001-01-01

    After a core dry-out and a period of rod clad overheating, which might occur in some postulated accidental sequences in a PWR, the actuation of safety injections allows to quench the hot rods. Both thermal and mechanical processes control the phenomenon of quenching. Quenching first requires that liquid water is present to release the heat stored in the rod. When water is present, a pre-cooling of the clad is also required before quenching. (author)

  2. Thermalhydraulic phenomena governing the quenching of hot rods, and existing models

    Energy Technology Data Exchange (ETDEWEB)

    Bestion, D. [CEA-Grenoble, DEN/DTP/SMTH (France)

    2001-07-01

    After a core dry-out and a period of rod clad overheating, which might occur in some postulated accidental sequences in a PWR, the actuation of safety injections allows to quench the hot rods. Both thermal and mechanical processes control the phenomenon of quenching. Quenching first requires that liquid water is present to release the heat stored in the rod. When water is present, a pre-cooling of the clad is also required before quenching. (author)

  3. Uncontrolled withdrawal of a control rod without scram

    International Nuclear Information System (INIS)

    Abou-EL-Maaty, Talal

    2008-01-01

    In the present work the thermal-hydraulics of reactivity-induced transients in low enriched uranium (LEU) core of a typical material test research reactor (MTR) are analyzed using the previous program developed by Khater et al. The analysis was done for uncontrolled withdrawal of a control rod with scram-disabled conditions. Initiating reactivity events with and without the influence of reactivity efficiency curve ('S' curve) were considered. The results of the proposed transients are analyzed and compared with each other. In transient without the 'S' curve influence, a high primary peak power of 406.18 MW is attained and a clad melt down takes place after 1.85 s. In the transient with the 'S' curve influence, a high super prompt-critical situation is produced (1.762$ at 0.895 s) with a very high primary peak power of 801.05 MW at 0.912 s. Also, a fast clad melt down is resulted in the hot channel at 1.088 s and a stable film boiling is established. This study indicates that, compared to the application of linear reactivity curve, the application of the reactivity efficiency curve results in the prediction of higher peaks in power and temperatures (fuel, clad and coolant) with a fast clad melt down

  4. Uncontrolled withdrawal of a control rod without SCRAM

    International Nuclear Information System (INIS)

    Abou-El-Maaty, T.

    2007-01-01

    In the present work, the thermal-hydraulic analysis of reactivity-induced transients in a Low Enriched Uranium (LEU) core of a typical material test research reactor is conducted using the previous program developed Khater et al. The analysis was done for the uncontrolled withdrawal of a control rod under scram-disabled conditions. The initiating event reactivity was considered with and without influence of the reactivity efficiency curve (''S'' curve). The results of the transient calculations are analyzed and compared with each other. In the transient without the ''S'' curve influence, a high primary peak power of 406.18 MW is attained and a clad melt down is occurring after 1.85 s. In the transient with the ''S'' curve influence, a super prompt highly critical situation is produced (1.762 $ at 0.895 s) with a very high primary peak power of 801.05 MW at 0.912 s. A fast clad melt down is resulting in the hot channel at 1.088 s and a stable film boiling is occurring. This study shows that the influence of the reactivity efficiency curve results in higher peaks in power and temperatures (fuel, clad and coolant) with a fast clad melt down than that of a linear assumption. (orig.)

  5. Control rod displacement

    International Nuclear Information System (INIS)

    Nakazato, S.

    1987-01-01

    This patent describes a nuclear reactor including a core, cylindrical control rods, a single support means supporting the control rods from their upper ends in spaced apart positions and movable for displacing the control rods in their longitudinal direction between a first end position in which the control rods are fully inserted into the core and a second end position in which the control rods are retracted from the core, and guide means contacting discrete regions of the outer surface of each control rod at least when the control rods are in the vicinity of the second end position. The control rods are supported by the support means for longitudinal movement without rotation into and out of the core relative to the guide means to thereby cause the outer surface of the control rods to experience wear as a result of sliding contact with the guide means. The support means are so arranged with respect to the core and the guide means that it is incapable of rotation relative to the guide means. The improvement comprises displacement means being operatively coupled to a respective one of the control rods for periodically rotating the control rod in a single angular direction through an angle selected to change the locations on the outer surfaces of the control rods at which the control rods are contacted by the guide means during subsequent longitudinal movement of the control rods

  6. Effects of pellet-to-cladding gap design parameters on the reliability of high burnup PWR fuel rods under steady state and transient conditions

    International Nuclear Information System (INIS)

    Tas, Fatma Burcu; Ergun, Sule

    2013-01-01

    Highlights: • Fuel performance of a typical Pressurized Water Reactor rod is analyzed. • Steady state fuel rod behavior is examined to see the effects of pellet to cladding gap thickness and gap gas pressure. • Transient fuel rod behavior is examined to see the effects of pellet to cladding gap thickness and gap gas pressure. • The optimum pellet to cladding gap thickness and gap gas pressure values of the simulated fuel are determined. • The effects of pellet to cladding gap design parameters on nuclear fuel reliability are examined. - Abstract: As an important improvement in the light water nuclear reactor operations, the nuclear fuel burnup rate is increased in recent decades and this increase causes heavier duty for the nuclear fuel. Since the high burnup fuel is exposed to very high thermal and mechanical stresses and since it operates in an environment with high radiation for about 18 month cycles, it carries the risk of losing its integrity. In this study; it is aimed to determine the effects of pellet–cladding gap thickness and gap pressure on reliability of high burnup nuclear fuel in Pressurized Water Reactors (PWRs) under steady state operation conditions and suggest optimum values for the examined parameters only and validate these suggestions for a transient condition. In the presented study, fuel performance was analyzed by examining the effects of pellet–cladding gap thickness and gap pressure on the integrity of high burnup fuels. This work is carried out for a typical Westinghouse type PWR fuel. The steady state conditions were modeled and simulated with FRAPCON-3.4a steady state fuel performance code and the FRAPTRAN-1.4 fuel transient code was used to calculate transient fuel behavior. The analysis included the changes in the important nuclear fuel design limitations such as the centerline temperature, cladding stress, strain and oxidation with the change in pellet–cladding gap thickness and initial pellet–cladding gap gas

  7. Control rod drive

    International Nuclear Information System (INIS)

    Hawke, B.C.

    1986-01-01

    A reactor core, one or more control rods, and a control rod drive are described for selectively inserting and withdrawing the one or more control rods into and from the reactor core, which consists of: a support structure secured beneath the reactor core; control rod positioning means supported by the support structure for movably supporting the control rod for movement between a lower position wherein the control rod is located substantially beneath the reactor core and an upper position wherein at least an upper portion of the control rod extends into the reactor core; transmission means; primary drive means connected with the control rod positioning means by the transmission means for positioning the control rod under normal operating conditions; emergency drive means for moving the control rod from the lower position to the upper position under emergency conditions, the emergency drive means including a weight movable between an upper and a lower position, means for movably supporting the weight, and means for transmitting gravitational force exerted on the weight to the control rod positioning means to move the control rod upwardly when the weight is pulled downwardly by gravity; the transmission means connecting the control rod positioning means with the emergency drive means so that the primary drive means effects movement of the weight and the control rod in opposite directions under normal conditions, thus providing counterbalancing to reduce the force required for upward movement of the control rod under normal conditions; and restraint means for restraining the fall of the weight under normal operating conditions and disengaging the primary drive means to release the weight under emergency conditions

  8. The pellet-cladding contact in a fuel rod and its simulation by finite elements

    International Nuclear Information System (INIS)

    Tanajura, C.A.S.

    1988-01-01

    A model to analyse the mechanical behavior of a fuel rod of a PWR is presented. We drew our attention to the phenomenon of pellet-pellet and pellet-cladding contact by taking advantage of a model which assumes the hypotheses of axisymmetry, elastic behavior with infinitesimal deformations and changes of the material properties with temperature. It also includes the effects of swelling and initial relocation. The problem of contact gives rise to a variational formulation which employs Lagrangian multipliers. With this approach an iterative scheme is constructed to obtain the solution. The finite element method is applied to space discretization. The model sensibility to some parameters and its performance concerning fuel rod behavior is discussed by means of numerical simulations. (author) [pt

  9. Modelling of pellet-cladding interaction in PWR's

    International Nuclear Information System (INIS)

    Esteves, A.M.; Silva, A.T. e.

    1992-01-01

    The pellet-cladding interaction that can occur in a PWR fuel rod design is modelled with the computer codes FRAPCON-1 and ANSYS. The fuel performance code FRAPCON-1 analyses the fuel rod irradiation behavior and generates the initial conditions for the localized fuel rod thermal and mechanical modelling in two and three-dimensional finite elements with ANSYS. In the mechanical modelling, a pellet fragment is placed in the fuel rod gap. Two types of fuel rod cladding materials are considered: Zircaloy and austenitic stainless steel. (author)

  10. Expandable device for a nuclear fuel rod

    International Nuclear Information System (INIS)

    Gesinski, L.T.

    1978-01-01

    A nuclear fuel rod and a device for use within the rod cladding to maintain the axial position of the fuel pellets stacked one atop another within the cladding are described. The device is initially of a smaller external cross-section than the fuel rod cladding internal cross-section so as to accommodate loading into the rod at preselected locations. During power operation the device responds to a rise in temperature, so as to permanently maintain its position and restrain any axial motion of the fuel pellets

  11. 3D finite element analysis of a nuclear fuel rod with gap elements between the pellet and the cladding

    International Nuclear Information System (INIS)

    Kang, Chang-Hak; Lee, Sung-Uk; Yang, Dong-Yol; Kim, Hyo-Chan; Yang, Yong-Sik

    2016-01-01

    Nuclear fuel rods which comprises an important component of a nuclear power plant are composed of nuclear fuel and cladding. Simulating the nuclear fuel rod using a computer program is the universal method to verify its safety. The computer program used for this is called the fuel performance code. The main objective of this study is to simulate the nuclear fuel rod behavior considering the gap conductance using three-dimensional gap elements. Gap elements are used because, unlike other methods, this approach does not require special methods or other variables such as the Lagrange multiplier. In this work, a nuclear fuel rod has been simulated and the results are compared with the experimental results. (author)

  12. Cladding creepdown model for FRAPCON-2

    International Nuclear Information System (INIS)

    Shah, V.N.; Tolli, J.E.

    1985-02-01

    This report presents a cladding deformation model developed to analyze cladding creepdown during steady state operation in both a pressurized water reactor (PWR) and a boiling water reactor (BWR). This model accounts for variations in zircaloy cladding heat treatment; cold worked and stress relieved material, typically used in a PWR, and fully recrystallized material, typically used in a BWR. The model calculates cladding creepdown as a function of hoop stress, fast neutron flux, exposure time, and temperature. This report also presents a comparison between cladding creep calculations by this model and corresponding measurements from the KWU/CE program, ORNL HOBBIE experiments, and EPRI/Westinghouse Engineering cooperative project. The comparisons show that the model calculates cladding creep strains well. The analyses of non-fueled rods by FRAPCON-2 show that the cladding creepdown model was correctly incorporated. Also, analysis of a PWR rod test case shows that the FRAPCON-2 code can analyze pellet-cladding mechanical interaction caused by cladding creepdown and fuel swelling

  13. Deformation of PWR cladding following a loss-of-coolant accident

    International Nuclear Information System (INIS)

    Hindle, E.D.; Mann, C.A.

    1979-07-01

    A review is presented of recent experiments to investigate the deformation behaviour of Zircaloy cladding in simulated loss-of-coolant accidents. The behaviour of Zircaloy cladding is shown to be controlled by a complex interaction of metallurgical and heat transfer variables, with the latter having a major influence. There is a significant increase in both diametral strain and the axial extent of deformation in multi-rod compared with single-rod tests. The extent to which this will occur in nuclear-heated tests is not yet known; however, it is expected that the 'smearing' of the gamma-radiation portion of decay heat in such tests will tend to reduce circumferential temperature variations. Opposing this is the influence of the colder control rods in an assembly. The resolution of this dichotomy will require a series of in-reactor multi-rod tests and attendant code development. (author)

  14. Simulation and operation of the EBR-II automatic control rod drive system

    International Nuclear Information System (INIS)

    Lehto, W.K.; Larson, H.A.; Dean, E.M.; Christensen, L.J.

    1985-01-01

    An automatic control rod drive system (ACRDS) installed at EBR-II produces shaped power transients from 40% to full reactor power at a linear ramp rate of 4 MWt/s. A digital computer and modified control-rod-drive provides this capability. Simulation and analysis of ACRDS experiments establish the safety envelope for reactor transient operation. Tailored transients are required as part of USDOE Operational Reliability Testing program for prototypic fast reactor fuel cladding breach behavior studies. After initial EBR-II driver fuel testing and system checkout, test subassemblies were subjected to both slow and fast transients. In addition, the ACRDS is used for steady-state operation and will be qualified to control power ascent from initial critical to full power

  15. Simulation and operation of the EBR-II automatic control rod drive system

    International Nuclear Information System (INIS)

    Lehto, W.K.; Larson, H.A.; Dean, E.M.; Christensen, L.J.

    1985-01-01

    An automatic control rod drive system (ACRDS) installed at EBR-II produces shaped power transients from 40% to full reactor power at a linear ramp rate of 4 MWt/s. A digital computer and modified control-rod-drive provides this capability. Simulation and analysis of ACRDS experiments establish the safety envelope for reactor transient operation. Tailored transients are required as part of USDOE Operational Reliability Testing program for prototypic fast reactor fuel cladding breach behavior studies. After initial EBR-II driver fuel testing and system checkout, test subassemblies were subjected to both slow and fast transients. In additions, the ACRDS is used for steady-state operation and will be qualified to control power ascent from initial critical to full power

  16. Pellet-clad interaction in water reactor fuels

    Energy Technology Data Exchange (ETDEWEB)

    NONE

    2004-07-01

    The aim of this seminar is was to draw up a comprehensive picture of the pellet clad interaction and its impact on the fuel rod. This document is a detailed abstract of the papers presented during the following five sessions: industrial goals, fuel material behaviour in PCI situation, cladding behaviour relevant to PCI, in pile rod behaviour and modelling of the mechanical interaction between pellet and cladding. (A.L.B.)

  17. Pellet-clad interaction in water reactor fuels

    International Nuclear Information System (INIS)

    2004-01-01

    The aim of this seminar is was to draw up a comprehensive picture of the pellet clad interaction and its impact on the fuel rod. This document is a detailed abstract of the papers presented during the following five sessions: industrial goals, fuel material behaviour in PCI situation, cladding behaviour relevant to PCI, in pile rod behaviour and modelling of the mechanical interaction between pellet and cladding. (A.L.B.)

  18. Development of Cr Electroplated Cladding Tube for preventing Fuel-Cladding Chemical Interaction (FCCI)

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Jun Hwan; Woo, Je Woong; Kim, Sung Ho; Cheon, Jin Sik; Lee, Byung Oon; Lee, Chan Bock [Korea Atomic Energy Research Institute, Daejeon (Korea, Republic of)

    2015-05-15

    Metal fuel has been selected as a candidate fuel in the SFR because of its superior thermal conductivity as well as enhanced proliferation resistance in connection with the pyroprocessing. However, metal fuel suffers eutectic reaction (Fuel Cladding Chemical Interaction, FCCI) with the fuel cladding made of stainless steel at reactor operating temperature so that cladding thickness gradually reduces to endanger reactor safety. In order to mitigate FCCI, barrier concept has been proposed between the fuel and the cladding in designing fuel rod. Regarding this, KAERI has initiated barrier cladding development to prevent interdiffusion process as well as enhance the SFR fuel performance. Previous study revealed that Cr electroplating has been selected as one of the most promising options because of its technical and economic viability. This paper describes the development status of the Cr electroplating technology for the usage of fuel rod in SFR. This paper summarizes the status of Cr electroplating technology to prevent FCCI in metal fuel rod. It has been selected for the ease of practical application at the tube inner surface. Technical scoping, performance evaluation and optimization have been carried out. Application to the tube inner surface and in-pile test were conducted which revealed as effective.

  19. Control rod drives

    International Nuclear Information System (INIS)

    Futatsugi, Masao.

    1980-01-01

    Purpose: To secure the reactor operation safety by the provision of a fluid pressure detecting section for control rod driving fluid and a control rod interlock at the midway of the flow pass for supplying driving fluid to the control rod drives. Constitution: Between a driving line and a direction control valve are provided a pressure detecting portion, an alarm generating device, and a control rod inhibition interlock. The driving fluid from a driving fluid source is discharged by way of a pump and a manual valve into the reactor in which the control rods and reactor fuels are contained. In addition, when the direction control valve is switched and the control rods are inserted and extracted by the control rod drives, the pressure in the driving line is always detected by the pressure detection section, whereby if abnormal pressure is resulted, the alarm generating device is actuated to warn the abnormality and the control rod inhibition interlock is actuated to lock the direction control valve thereby secure the safety operation of the reactor. (Seki, T.)

  20. Contribution to numerical and mechanical modelling of pellet-cladding interaction in nuclear reactor fuel rod

    International Nuclear Information System (INIS)

    Retel, V.

    2002-12-01

    Pressurised water reactor fuel rods (PWR) are the place of nuclear fission, resulting in unstable and radioactive elements. Today, the mechanical loading on the cladding is harder and harder and is partly due to the fuel pellet movement. Then, the mechanical behaviour of the cladding needs to be simulated with models allowing to assess realistic stress and strain fields for all the running conditions. Besides, the mechanical treatment of the fuel pellet needs to be improved. The study is part of a global way of improving the treatment of pellet-cladding interaction (PCI) in the 1D finite elements EDF code named CYRANO3. Non-axisymmetrical multidirectional effects have to be accounted for in a context of unidirectional axisymmetrical finite elements. The aim of this work is double. Firstly a model simulating the effect of stress concentration on the cladding, due to the opening of the radial cracks of fuel, had been added in the code. Then, the fragmented state of fuel material has been taken into account in the thermomechanical calculation, through a model which led the strain and stress relaxation in the pellet due to the fragmentation, be simulated. This model has been implemented in the code for two types of fuel behaviour: elastic and viscoplastic. (author)

  1. A model for hydrogen pickup for BWR cladding materials

    International Nuclear Information System (INIS)

    Hede, G.; Kaiser, U.

    2001-01-01

    It has been observed that rod elongation is driven by the hydrogen pickup but not by corrosion as such. Based on this a non-destructive method to determine clad hydrogen concentration has been developed. The method is based on the observation that there are three different mechanisms behind the rod growth: the effect of neutron irradiation on the Zircaloy microstructure, the volume increase of the cladding as an effect of hydride precipitation and axial pellet-cladding-mechanical-interaction (PCMI). The derived correlation is based on the experience of older cladding materials, inspected at hot-cell laboratories, that obtained high hydrogen levels (above 500 ppm) at lower burnup (assembly burnup below 50 MWd/kgU). Now this experience can be applied, by interpolation, on more modern cladding materials with a burnup beyond 50 MWd/kgU by analysis of the rod growth database of the respective cladding materials. Hence, the method enables an interpolation rather than an extrapolation of present day hydrogen pickup database, which improves the reliability and accuracy. Further, one can get a good estimate of the hydrogen pickup during an ongoing outage based on a non-destructive method. Finally, rod growth measurements are normally performed for a large population of rods, hence giving a good statistics compared to examination of a few rods at a hot cell. (author)

  2. Adaptation of fuel code for light water reactor with austenitic steel rod cladding

    International Nuclear Information System (INIS)

    Gomes, Daniel de Souza; Silva, Antonio Teixeira; Giovedi, Claudia

    2015-01-01

    Light water reactors were used with steel as nuclear fuel cladding from 1960 to 1980. The high performance proved that the use of low-carbon alloys could substitute the current zirconium alloys. Stainless steel is an alternative that can be used as cladding. The zirconium alloys replaced the steel. However, significant experiences in-pile occurred, in commercial units such as Haddam Neck, Indian Point, and Yankee experiences. Stainless Steel Types 347 and 348 can be used as cladding. An advantage of using Stainless Steel was evident in Fukushima when a large number of hydrogens was produced at high temperatures. The steel cladding does not eliminate the problem of accumulating free hydrogen, which can lead to a risk of explosion. In a boiling water reactor, environments easily exist for the attack of intergranular corrosion. The Stainless Steel alloys, Types 321, 347, and 348, are stabilized against attack by the addition of titanium, niobium, or tantalum. The steel Type 348 is composed of niobium, tantalum, and cobalt. Titanium preserves type 321, and niobium additions stabilize type 347. In recent years, research has increased on studying the effects of irradiation by fast neutrons. The impact of radiation includes changes in flow rate limits, deformation, and ductility. The irradiation can convert crystalline lattices into an amorphous structure. New proposals are emerging that suggest using a silicon carbide-based fuel rod cladding or iron-chromium-aluminum alloys. These materials can substitute the classic zirconium alloys. Once the steel Type 348 was chosen, the thermal and mechanical properties were coded in a library of functions. The fuel performance codes contain all features. A comparative analysis of the steel and zirconium alloys was made. The results demonstrate that the austenitic steel alloys are the viable candidates for substituting the zirconium alloys. (author)

  3. Adaptation of fuel code for light water reactor with austenitic steel rod cladding

    Energy Technology Data Exchange (ETDEWEB)

    Gomes, Daniel de Souza; Silva, Antonio Teixeira, E-mail: dsgomes@ipen.br, E-mail: teixeira@ipen.br [Instituto de Pesquisas Energeticas e Nucleares (IPEN/CNEN-SP), Sao Paulo, SP (Brazil); Giovedi, Claudia, E-mail: claudia.giovedi@labrisco.usp.br [Universidade de Sao Paulo (POLI/USP), Sao Paulo, SP (Brazil). Lab. de Analise, Avaliacao e Gerenciamento de Risco

    2015-07-01

    Light water reactors were used with steel as nuclear fuel cladding from 1960 to 1980. The high performance proved that the use of low-carbon alloys could substitute the current zirconium alloys. Stainless steel is an alternative that can be used as cladding. The zirconium alloys replaced the steel. However, significant experiences in-pile occurred, in commercial units such as Haddam Neck, Indian Point, and Yankee experiences. Stainless Steel Types 347 and 348 can be used as cladding. An advantage of using Stainless Steel was evident in Fukushima when a large number of hydrogens was produced at high temperatures. The steel cladding does not eliminate the problem of accumulating free hydrogen, which can lead to a risk of explosion. In a boiling water reactor, environments easily exist for the attack of intergranular corrosion. The Stainless Steel alloys, Types 321, 347, and 348, are stabilized against attack by the addition of titanium, niobium, or tantalum. The steel Type 348 is composed of niobium, tantalum, and cobalt. Titanium preserves type 321, and niobium additions stabilize type 347. In recent years, research has increased on studying the effects of irradiation by fast neutrons. The impact of radiation includes changes in flow rate limits, deformation, and ductility. The irradiation can convert crystalline lattices into an amorphous structure. New proposals are emerging that suggest using a silicon carbide-based fuel rod cladding or iron-chromium-aluminum alloys. These materials can substitute the classic zirconium alloys. Once the steel Type 348 was chosen, the thermal and mechanical properties were coded in a library of functions. The fuel performance codes contain all features. A comparative analysis of the steel and zirconium alloys was made. The results demonstrate that the austenitic steel alloys are the viable candidates for substituting the zirconium alloys. (author)

  4. Control rod drives

    International Nuclear Information System (INIS)

    Hayakawa, Hiroyasu.

    1979-01-01

    Purpose: To enable rapid control in a simple circuit by providing a motor control device having an electric capacity capable of simultaneously driving all of the control rods rapidly only in the inserting direction as well as a motor controlling device capable of fine control for the insertion and extraction at usual operation. Constitution: The control rod drives comprise a first motor control device capable of finely controlling the control rods both in inserting and extracting directions, a second motor control device capable of rapidly driving the control rods only in the inserting direction, and a first motor switching circuit and a second motor switching circuit switched by switches. Upon issue of a rapid insertion instruction for the control rods, the second motor switching circuit is closed by the switch and the second motor control circuit and driving motors are connected. Thus, each of the control rod driving motors is driven at a high speed in the inserting direction to rapidly insert all of the control rods. (Yoshino, Y.)

  5. Control rod drives

    International Nuclear Information System (INIS)

    Oonuki, Koji.

    1981-01-01

    Purpose: To increase the driving speed of control rods at rapid insertion with an elongate control rod and an extension pipe while ensuring sufficient buffering performance in a short buffering distance, by providing a plurality of buffers to an extension pipe between a control rod drive source and a control rod in LMFBR type reactor. Constitution: First, second and third buffers are respectively provided to an acceleration piston, an extension pipe and a control rod respectively and the insertion positions for each of the buffers are displaced orderly from above to below. Upon disconnection of energizing current for an electromagnet, the acceleration piston, the extension pipe and the control rod are rapidly inserted in one body. The first, second and third buffers are respectively actuated at each of their falling strokes upon rapid insertion respectively, and the acceleration piston, the extension pipe and the control rod receive the deceleration effect in the order correspondingly. Although the compression force is applied to the control rod only near the stroke end, it does not cause deformation. (Kawakami, Y.)

  6. Control rod

    International Nuclear Information System (INIS)

    Igarashi, Takao; Yoshimoto, Yuichiro; Sugawara, Satoshi; Fukumoto, Takashi; Endo, Zen-ichiro; Saito, Shozo; Shinpo, Katsutoshi; Nishimura, Akira; Ozawa, Michihiro

    1988-01-01

    Purpose: To provide a sufficient shutdown margin upon reactor shutdown, prevent sheath deformation without decreasing neutron absorbents and prevent impact shocks exerted to structural materials. Constitution: The control rod of the present invention comprises a neutron absorption region, a sheath deformation means attached to the side wall and means for restricting and supporting axial movement of the neutron absorbent rod. Then, the amount of absorptive nuclei chained absorbents in the lower region is reduced than that in the upper region. In this way, effective neutron absorbing performance can be obtained relative to the neutron importance distribution during reactor shutdown. In addition, since the operationability is improved by reducing the weight of the control rod and the absorptive nuclei chained neutron abosrbers are used, mechanical nuclear life of the control rod can be increased. Thus, it is possible to prevent the outward deformation of the sheath, as well as prevent collision between the neutron absorber rod and the structural material on the side of inserting the control rod generated upon reactor scram by a simple structure. (Kamimura, M.)

  7. Control rod position control device

    International Nuclear Information System (INIS)

    Ubukata, Shinji.

    1997-01-01

    The present invention provides a control rod position control device which stores data such as of position signals and driving control rod instruction before and after occurrence of abnormality in control for the control rod position for controlling reactor power and utilized the data effectively for investigating the cause of abnormality. Namely, a plurality of individual control devices have an operation mismatching detection circuit for outputting signals when difference is caused between a driving instruction given to the control rod position control device and the control rod driving means and signals from a detection means for detecting an actual moving amount. A general control device collectively controls the individual control devices. In addition, there is also disposed a position storing circuit for storing position signals at least before and after the occurrence of the control rod operation mismatching. With such procedures, the cause of the abnormality can be determined based on the position signals before and after the occurrence of control rod mismatching operation stored in the position storing circuit. Accordingly, the abnormality cause can be determined to conduct restoration in an early stage. (I.S.)

  8. Oxidation during reflood of reactor core with melting cladding

    Energy Technology Data Exchange (ETDEWEB)

    Siefken, L.J.; Allison, C.M.; Davis, K.L. [and others

    1995-09-01

    Models were recently developed and incorporated into the SCDAP/RELAP5 code for calculating the oxidation of fuel rods during cladding meltdown and reflood. Experiments have shown that a period of intense oxidation may occur when a hot partially oxidized reactor core is reflooded. This paper offers an explanation of the cladding meltdown and oxidation processes that cause this intense period of oxidation. Models for the cladding meltdown and oxidation processes are developed. The models are assessed by simulating a severe fuel damage experiment that involved reflood. The models for cladding meltdown and oxidation were found to improve calculation of the temperature and oxidation of fuel rods during the period in which hot fuel rods are reflooded.

  9. The irradiation performance of austenitic stainless steel clade PWR fuel rods

    International Nuclear Information System (INIS)

    Teixeira e Silva, A.; Esteves, A.M.

    1988-01-01

    The steady state irradiation performance of austenitic stainless steel clad pressurized water reactor fuel rods is modeled with fuel performance codes of the FRAP series. These codes, originally developed to model the thermal-mechanical behavior of zircaloy clad fuel rods, are modified to model stainless steel clad fuel rods. The irradiation thermal-mechanical behavior of type 348 stainless steel and zircaloy fuel rods is compared. (author) [pt

  10. Mechanical modelling of transient- to- failure SFR fuel cladding

    Energy Technology Data Exchange (ETDEWEB)

    Feria, F.; Herranz, L. E.

    2014-07-01

    The response of Sodium Fast Reactor (SFR) fuel rods to transient accident conditions is an important safety concern. During transients the cladding strain caused by the stress due to pellet cladding mechanical interaction (PCMI) can lead to failure. Due to the fact that SFR fuel rods are commonly clad with strengthened material made of stainless steel (SS), cladding is usually treated as an elastic-perfectly-plastic material. However, viscoplastic behaviour can contribute to mechanical strain at high temperature (> 1000 K). (Author)

  11. AgInCd control rod failure in the QUENCH-13 bundle test

    International Nuclear Information System (INIS)

    Sepold, L.; Lind, T.; Csordas, A. Pinter; Stegmaier, U.; Steinbrueck, M.; Stuckert, J.

    2009-01-01

    The QUENCH off-pile experiments performed at the Karlsruhe Research Center are to investigate the high-temperature behavior of Light Water Reactor (LWR) core materials under transient conditions and in particular the hydrogen source term resulting from the water injection into an uncovered LWR core. The typical LWR-type QUENCH test bundle, which is electrically heated, consists of 21 fuel rod simulators with a total length of approximately 2.5 m. The Zircaloy-4 rod claddings and the grid spacers are identical to those used in Pressurized Water Reactors (PWR) whereas the fuel is represented by ZrO 2 pellets. In the QUENCH-13 experiment the single unheated fuel rod simulator in the center of the test bundle was replaced by a PWR-type control rod. The QUENCH-13 experiment consisting of pre-oxidation, transient, and quench water injection at the bottom of the test section investigated the effect of an AgInCd/stainless steel/Zircaloy-4 control rod assembly on early-phase bundle degradation and on reflood behavior. Furthermore, in the frame of the EU 6th Framework Network of Excellence SARNET, release and transport of aerosols of a failed absorber rod were to be studied in QUENCH-13, which was accomplished with help of aerosol measurements performed by PSI-Switzerland and AEKI-Hungary. Control rod failure was initiated by eutectic interaction of steel cladding and Zircaloy-4 guide tube and was indicated at about 1415 K by axial peak absorber and bundle temperature responses and additionally by the on-line aerosol monitoring system. Significant releases of aerosols and melt relocation from the control rod were observed at an axial peak bundle temperature of 1650 K. At a maximum bundle temperature of 1820 K reflood from the bottom was initiated with cold water at a flooding rate of 52 g/s. There was no noticeable temperature escalation during quenching. This corresponds to the small amount of about 1 g in hydrogen production during the quench phase (compared to 42 g of H 2

  12. Experimental determination of temperature fields in sodium-cooled rod bundles with hexagonal rod arrangement and grid spacers

    International Nuclear Information System (INIS)

    Moeller, R.; Tschoeke, H.; Kolodziej, M.

    1977-01-01

    Three-dimensional temperature fields in the claddings of sodium cooled rods were determined experimentally under representative nominal operating conditions for a SNR typical 19-rod bundle model provided with spark-eroded spacers. These experiments are required to verify thermohydraulic computer programs which will provide the output data for strength calculations of the high loaded cladding tubes. In this work the essentials are reported of the measured circumferential distributions of wall temperatures of peripheral rods. In addition the sub-channel temperatures measured over the bundle cross section are indicated, they are required to sustain codes for the global thermohydraulic design of core elements. The most important results are: 1) The whole fuel element is located within the thermal entrance length. 2) High azimuthal temperature differences were measured in the claddings of peripheral rods, which are strongly influenced by the distance between the rod and the shroud, especially for the corner rod. 3) With decreasing Pe-number ( [de

  13. International symposium on fuel rod simulators: development and application

    Energy Technology Data Exchange (ETDEWEB)

    McCulloch, R.W. (comp.)

    1981-05-01

    Separate abstracts are included for each of the papers presented concerning fuel rod simulator operation and performance; simulator design and evaluation; clad heated fuel rod simulators and fuel rod simulators for cladding investigations; fuel rod simulator components and inspection; and simulator analytical modeling. Ten papers have previously been input to the Energy Data Base.

  14. Control rod drive

    International Nuclear Information System (INIS)

    Okutani, Tetsuro.

    1988-01-01

    Purpose: To provide a simple and economical control rod drive using a control circuit requiring no pulse circuit. Constitution: Control rods in a BWR type reactor are driven by hydraulic pressure and inserted or withdrawn in the direction of applying the hydraulic pressure. The direction of the hydraulic pressure is controlled by a direction control valve. Since the driving for the control rod is extremely important in view of the operation, a self diagnosis function is disposed for rapid inspection of possible abnormality. In the present invention, two driving contacts are disposed each by one between the both ends of a solenoid valve of the direction control valve for driving the control rod and the driving power source, and diagnosis is conducted by alternately operating them. Therefore, since it is only necessary that the control circuit issues a driving instruction only to one of the two driving contacts, the pulse circuit is no more required. Further, since the control rod driving is conducted upon alignment of the two driving instructions, the reliability of the control rod drive can be improved. (Horiuchi, T.)

  15. Control rod drive mechanism

    International Nuclear Information System (INIS)

    Nakamura, Akira.

    1981-01-01

    Purpose: To ensure the scram operation of a control rod by the reliable detection for the position of control rods. Constitution: A permanent magnet is provided to the lower portion of a connecting rod in engagement with a control rod and a tube having a plurality of lead switches arranged axially therein in a predetermined pitch is disposed outside of the control rod drives. When the control rod moves upwardly in the scram operation, the lead switches are closed successively upon passage of the permanent magnet to operate the electrical circuit provided by way of each of the lead switches. Thus, the position for the control rod during the scram can reliably be determined and the scram characteristic of the control rod can be recognized. (Furukawa, Y.)

  16. Analysis of pellet cladding mechanical interaction using computational simulation

    Energy Technology Data Exchange (ETDEWEB)

    Berretta, José R.; Suman, Ricardo B.; Faria, Danilo P.; Rodi, Paulo A., E-mail: jose.berretta@marinha.mil.br [Centro Tecnológico da Marinha em São Paulo (CTMSP), São Paulo, SP (Brazil); Giovedi, Claudia, E-mail: claudia.giovedi@labrisco.usp.br [Universidade de Sao Paulo (LabRisco/USP), São Paulo, SP (Brazil). Laboratório de Análise, Avaliação e Gerenciamento de Riscos

    2017-07-01

    During the operation of Pressurized Water Reactors (PWR), specifically under power transients, the fuel pellet experiences many phenomena, such as swelling and thermal expansion. These dimensional changes in the fuel pellet can enable occurrence of contact it and the cladding along the fuel rod. Thus, pellet cladding mechanical interaction (PCMI), due this contact, induces stress increase at the contact points during a period, until the accommodation of the cladding to the stress increases. This accommodation occurs by means of the cladding strain, which can produce failure, if the fuel rod deformation is permanent or the burst limit of the cladding is reached. Therefore, the mechanical behavior of the cladding during the occurrence of PCMI under power transients shall be investigated during the fuel rod design. Considering the Accident Tolerant Fuel program which aims to develop new materials to be used as cladding in PWR, one important design condition to be evaluated is the cladding behavior under PCMI. The purpose of this paper is to analyze the effects of the PCMI on a typical PWR fuel rod geometry with stainless steel cladding under normal power transients using computational simulation (ANSYS code). The PCMI was analyzed considering four geometric situations at the region of interaction between pellet and cladding. The first case, called “perfect fuel model” was used as reference for comparison. In the second case, it was considered the occurrence of a pellet crack with the loss of a chip. The goal for the next two cases was that a pellet chip was positioned into the gap of pellet-cladding, in the situations described in the first two cases. (author)

  17. Internal hydriding in irradiated defected Zircaloy fuel rods: A review (LWBR Development Program)

    International Nuclear Information System (INIS)

    Clayton, J.C.

    1987-10-01

    Although not a problem in recent commercial power reactors, including the Shippingport Light Water Breeder Reactor, internal hydriding of Zircaloy cladding was a persistent cause of gross cladding failures during the 1960s. It occurred in the fuel rods of water-cooled nuclear power reactors that had a small cladding defect. This report summarizes the experimental findings, causes, mechanisms, and methods of minimizing internal hydriding in defected Zircaloy-clad fuel rods. Irradiation test data on the different types of defected fuel rods, intentionally fabricated defected and in-pile operationally defected rods, are compared. Significant factors affecting internal hydriding in defected Zircaloy-clad fuel rods (defect hole size, internal and external sources of hydrogen, Zircaloy cladding surface properties, nickel alloy contamination of Zircaloy, the effect of heat flux and fluence) are discussed. Pertinent in-pile and out-of-pile test results from Bettis and other laboratories are used as a data base in constructing a qualitative model which explains hydrogen generation and distribution in Zircaloy cladding of defected water-cooled reactor fuel rods. Techniques for minimizing internal hydride failures in Zircaloy-clad fuel rods are evaluated

  18. Fuel cladding behavior under rapid loading conditions

    Science.gov (United States)

    Yueh, K.; Karlsson, J.; Stjärnsäter, J.; Schrire, D.; Ledergerber, G.; Munoz-Reja, C.; Hallstadius, L.

    2016-02-01

    A modified burst test (MBT) was used in an extensive test program to characterize fuel cladding failure behavior under rapid loading conditions. The MBT differs from a normal burst test with the use of a driver tube to simulate the expansion of a fuel pellet, thereby producing a partial strain driven deformation condition similar to that of a fuel pellet expansion in a reactivity insertion accident (RIA). A piston/cylinder assembly was used to pressurize the driver tube. By controlling the speed and distance the piston travels the loading rate and degree of sample deformation could be controlled. The use of a driver tube with a machined gauge section localizes deformation and allows for continuous monitoring of the test sample diameter change at the location of maximum hoop strain, during each test. Cladding samples from five irradiated fuel rods were tested between 296 and 553 K and loading rates from 1.5 to 3.5/s. The test rods included variations of Zircaloy-2 with different liners and ZIRLO, ranging in burn-up from 41 to 74 GWd/MTU. The test results show cladding ductility is strongly temperature and loading rate dependent. Zircaloy-2 cladding ductility degradation due to operational hydrogen pickup started to recover at approximately 358 K for test condition used in the study. This recovery temperature is strongly loading rate dependent. At 373 K, ductility recovery was small for loading rates less than 8 ms equivalent RIA pulse width, but longer than 8 ms the ductility recovery increased exponentially with increasing pulse width, consistent with literature observations of loading rate dependent brittle-to-ductile (BTD) transition temperature. The cladding ductility was also observed to be strongly loading rate/pulse width dependent for BWR cladding below the BTD temperature and Pressurized Water Reactor (PWR) cladding at both 296 and 553 K.

  19. Modelling of pellet-clad interaction during power ramps

    International Nuclear Information System (INIS)

    Zhou, G.; Lindback, J.E.; Schutte, H.C.; Jernkvist, L.O.; Massih, A.R.; Massih, A.R.

    2005-01-01

    A computational method to describe the pellet-clad interaction phenomenon is presented. The method accounts for the mechanical contact between fragmented pellets and the zircaloy clad, as well as for chemical reaction of fission products with zircaloy during power ramps. Possible pellet-clad contact states, soft, hard and friction, are taken into account in the computational algorithm. The clad is treated as an elastic-plastic-viscoplastic material with irradiation hardening. Iodine-induced stress corrosion cracking is described by using a fracture mechanics-based model for crack propagation. This integrated approach is used to evaluate two power ramp experiments made on boiling water reactor fuel rods in test reactors. The influence of the pellet-clad coefficient of friction on clad deformation is evaluated and discussed. Also, clad deformations, pellet-clad gap size and fission product gas release for one of the ramped rods are calculated and compared with measured data. (authors)

  20. Control rod calibration including the rod coupling effect

    International Nuclear Information System (INIS)

    Szilard, R.; Nelson, G.W.

    1984-01-01

    In a reactor containing more than one control rod, which includes all reactors licensed in the United States, there will be a 'coupling' or 'shadowing' of control rod flux at the location of a control rod as a result of the flux depression caused by another control rod. It was decided to investigate this phenomenon further, and eventually to put calibration table data or formulae in a small computer in the control room, so once could insert the positions of the three control rods and receive the excess reactivity without referring to separate tables. For this to be accomplished, a 'three control- rod reactivity function' would be used which would include the flux coupling between the rods. The function is design and measured data was fitted into it to determine the calibration constants. The input data for fitting the trial functions consisted of 254 data points, each consisting of the position of the reg, shim, and transient rods, and the total excess reactivity. (About 200 of these points were 'critical balance points', that is the rod positions for which reactor was critical, and the remainder were determined by positive period measurements.) Although this may be unrealistic from a physical viewpoint, the function derived gave a very accurate recalculation of the input data, and thus would faithfully give the excess reactivity for any possible combination of the locations of the three control rods. The next step, incorporation of the three-rod function into the minicomputer, will be pursued in the summer and fall of 1984

  1. Electrically heated ex-reactor pellet-cladding interaction (PCI) simulations utilizing irradiated Zircaloy cladding

    International Nuclear Information System (INIS)

    Barner, J.O.; Fitzsimmons, D.E.

    1985-02-01

    In a program sponsored by the Fuel Systems Research Branch of the US Nuclear Regulatory Commission, a series of six electrically heated fuel rod simulation tests were conducted at Pacific Northwest Laboratory. The primary objective of these tests was to determine the susceptibility of irradiated pressurized-water reactor (PWR) Zircaloy-4 cladding to failures caused by pellet-cladding mechanical interaction (PCMI). A secondary objective was to acquire kinetic data (e.g., ridge growth or relaxation rates) that might be helpful in the interpretation of in-reactor performance results and/or the modeling of PCMI. No cladding failures attributable to PCMI occurred during the six tests. This report describes the testing methods, testing apparatus, fuel rod diametral strain-measuring device, and test matrix. Test results are presented and discussed

  2. Examination of control rod ejection in WWER-440 type reactors at different circumstances using the code DYN3D

    International Nuclear Information System (INIS)

    Petoefi, G.; Aszodi, A.

    2001-01-01

    For nuclear reactors it is very important to examine the reactivity initiated transients caused by the ejection of a control rod. The event is found to be dependent on different thermal and neutronic parameters. In this paper the emphasis is laid on the effect of the power level at which the transient began and on the effect of the heat transfer coefficient measured in the gap between the fuel and the cladding. The most significant transients can be established by the ejection of the most effective control rod. So the first step is to determine the position of this rod. It was done by steady state calculations A calculation was carried out with all the rods inserted to the half level of the core, criticality was reached by adjusting the power level. Seven other calculations were made for each control rod at withdrawn position while the other six rods were inserted to the half plane of the core. From the results the most effective control rod could be determined.(authors)

  3. Axial distribution of deformation in the cladding of pressurized water reactor fuel rods in a loss-of-coolant accident

    International Nuclear Information System (INIS)

    Rose, K.M.; Mann, C.A.; Hindle, E.D.

    1979-01-01

    In the event of a loss-of-coolant accident in a pressurized water reactor, the cladding of the fuel rods would undergo a temperature excursion while being subject to tensile hoop stress. The deformation behavior of 470-mm lengths of Zircaloy-4 fuel cladding has been studied experimentally; under a range of stress levels in the high-alpha range of zirconium (600 to 850 0 C), diametral strains of up to 70% were observed over the greater part of their length. A negative-feedback mechanism is suggested, based on the reduction of secondary creep rate following cooling by enhanced heat loss at swelling areas. An approximate analysis based on this mechanism was found to be in reasonable agreement with the experimental results. A computer modeling code is being developed to predict cladding deformation under realistic conditions

  4. Axial distribution of deformation in the cladding of pressurized water reactor fuel rods in a loss-of-coolant accident

    Energy Technology Data Exchange (ETDEWEB)

    Rose, K.M.; Mann, C.A.; Hindle, E.D.

    1979-12-01

    In the event of a loss-of-coolant accident in a pressurized water reactor, the cladding of the fuel rods would undergo a temperature excursion while being subject to tensile hoop stress. The deformation behavior of 470-mm lengths of Zircaloy-4 fuel cladding has been studied experimentally; under a range of stress levels in the high-alpha range of zirconium (600 to 850/sup 0/C), diametral strains of up to 70% were observed over the greater part of their length. A negative-feedback mechanism is suggested, based on the reduction of secondary creep rate following cooling by enhanced heat loss at swelling areas. An approximate analysis based on this mechanism was found to be in reasonable agreement with the experimental results. A computer modeling code is being developed to predict cladding deformation under realistic conditions.

  5. Analysis of corrosion behavior of KOFA cladding

    International Nuclear Information System (INIS)

    Lee, Chan Bock; Kim, Ki Hang; Seo, Keum Seok; Chung, Jin Gon

    1994-01-01

    The corrosion behavior of KOFA cladding was analyzed using the oxide measurement data of KOFA fuel irradiated up to the fuel rod burnup of 35,000 MWD/MTU for two cycles in Kori-2. Even though KOFA cladding is a standard Zircaloy-4 manufactured by Westinghouse according to the Siemens/KWU's HCW (Highly Cold Worked) standard Zircaloy-4 specification, it was expected that in-pile corrosion behavior of KOFA cladding would not be equivalent to that of Siemens/KWU's cladding due to the differences in such manufacturing processes as cold work and heat treatment. The analysis of measured KOFA cladding oxidation showed that oxidation of KOFA cladding is at least 19 % lower than the design analysis based upon Siemens/KWU's HCW standard Zircaloy-4 cladding. Lower corrosion of KOFA cladding seems to result from the differences in the manufacturing processes and chemical composition although the burnup and oxide layer thickness of the measured fuel rods is relatively low and the amount of the oxidation data base is small

  6. Control rod shutdown system

    International Nuclear Information System (INIS)

    Miyamoto, Yoshiyuki; Higashigawa, Yuichi.

    1996-01-01

    The present invention provides a control rod terminating system in a BWR type nuclear power plant, which stops an induction electric motor as rapidly as possible to terminate the control rods. Namely, the control rod stopping system controls reactor power by inserting/withdrawing control rods into a reactor by driving them by the induction electric motor. The system is provided with a control device for controlling the control rods and a control device for controlling the braking device. The control device outputs a braking operation signal for actuating the braking device during operation of the control rods to stop the operation of the control rods. Further, the braking device has at least two kinds of breaks, namely, a first and a second brakes. The two kinds of brakes are actuated by receiving the brake operation signals at different timings. The brake device is used also for keeping the control rods after the stopping. Even if a stopping torque of each of the breaks is small, different two kinds of brakes are operated at different timings thereby capable of obtaining a large stopping torque as a total. (I.S.)

  7. Technical basis for storage of Zircaloy-clad spent fuel in inert gases

    International Nuclear Information System (INIS)

    Johnson, A.B. Jr.; Gilbert, E.R.

    1983-09-01

    The technical bases to establish safe conditions for dry storage of Zircaloy-clad fuel are summarized. Dry storage of fuel with zirconium alloy cladding has been licensed in Canada, the Federal Republic of Germany, and Switzerland. Dry storage demonstrations, hot cell tests, and modeling have been conducted using Zircaloy-clad fuel. The demonstrations have included irradiated boiling water reactor, pressurized heavy-water reactor, and pressurized water reactor fuel assemblies. Irradiated fuel has been emplaced in and retrieved from metal casks, dry wells, silos, and a vault. Dry storage tests and demonstrations have involved about 15,000 fuel rods, and about 5600 rods have been monitored during dry storage in inert gases with maximum cladding temperatures ranging from 50 to 570 0 C. Although some tests and demonstrations are still in progress, there is currently no evidence that any rods exposed to inert gases have failed (one PWR rod exposed to an air cover gas failed at about 270 0 C). Based on this favorable experience, it is concluded that there is sufficient information on fuel rod behavior, storage conditions, and potential cladding failure mechanisms to support licensing of dry storage in the US. This licensing position includes a requirement for inert cover gases and a maximum cladding temperature guideline of 380 0 C for Zircaloy-clad fuel. Using an inert cover gas assures that even if fuel with cladding defects were placed in dry storage, or if defects develop during storage, the defects would not propagate. Tests and demonstrations involving Zircaloy-clad rods and assemblies with maximum cladding temperatures above 400 0 C are in progress. When the results from these tests have been evaluated, the viability of higher temperature limits should be examined. Acceptable conditions for storage in air and dry storage of consolidated fuel are issues yet to be resolved

  8. SEFLEX - fuel rod simulator effects in flooding experiments. Pt. 2

    International Nuclear Information System (INIS)

    Ihle, P.; Rust, K.

    1986-03-01

    This report presents typical data and a limited heat transfer analysis from unblocked bundle reflood tests of an experimental thermal-hydraulic program. Full-length bundles of 5 x 5 fuel rod simulators having a gas-filled gap between the Zy cladding and the alumina pellets were tested in the test rig designed for the earlier Flooding Experiments with Blocked Arrays (FEBA-program). The 5 x 5 FEBA rod bundle tests were performed with gapless heater rods. These rods have a close thermal contact between the stainless steel cladding and the electric insulation material. A comparison of the SEFLEX data with the reference data of FEBA obtained under identical initial and reflood conditions shows the influence of different fuel rod simulators on the thermal-hydraulic behavior during forced feed bottom reflooding of unblocked and blocked arrays. Compared to bundles of gapless rods, bundles of rods with Zy claddings and a gas filled gap between claddings and pellets, which more closely represent the features that exist in an actual fuel rod geometry, produced higher quench front velocities, enhanced removal of stored heat in the rods, reduced peak cladding temperatures, increased grid spacer effects and absolutely unproblematic coolability of 90 percent blockages with bypass. The data offer the opportunity for further validation of computer codes to make realistic predictions of safety margins during a LOCA in a PWR. (orig./HP) [de

  9. SEFLEX fuel rod simulator effects in flooding experiments. Pt. 3

    International Nuclear Information System (INIS)

    Ihle, P.; Rust, K.

    1986-03-01

    This report presents typical data and a limited heat transfer analysis from blocked bundle reflood tests of an experimental thermal-hydraulic program. Full-length bundles of 5x5 fuel rod simulators having a gas-filled gap between the Zy cladding and the alumina pellets were tested in the test rig designed for the earlier Flooding Experiments with Blocked Arrays (FEBA-program). The 5x5 FEBA rod bundle tests were performed with gapless heater rods. These rods have a close thermal contact between the stainless steel cladding and the electric insulation material. A comparison of the SEFLEX data with the reference data of FEBA obtained under identical initial and reflood conditions shows the influence of different fuel rod simulators on the thermal-hydraulic behavior during forced feed bottom reflooding of unblocked and blocked arrays. Compared to bundles of gapless rods, bundles of rods with Zy claddings and a gas filled gap between claddings and pellets, which more closely represent the features that exist in an actual fuel rod geometry, produced higher quench front velocities, enhanced removal of stored heat in the rods, reduced peak cladding temperatures, increased grid spacer effects and absolutely unproblematic coolability of 90 percent blockages with bypass. The data offer the opportunity for further validation of computer codes to make realistic predictions of safety margins during a LOCA in a PWR. (orig./HP) [de

  10. Control rod

    International Nuclear Information System (INIS)

    Igarashi, Takao; Sugawara, Satoshi; Yoshimoto, Yuichiro; Saito, Shozo; Fukumoto, Takashi.

    1987-01-01

    Purpose: To reduce the weight and thereby obtain satisfactory operationability of control rods by combining absorbing nuclear chain type neutron absorbers and conventional type neutron absorbers in the axial direction of blades. Constitution: Neutron absorber rods and long life type neutron absorber rods are disposed in a tie rod and a sheath. The neutron absorber rod comprises a poison tube made of stainless steels and packed with B 4 C powder. The long life type neutron absorber rod is prepared by packing B-10 enriched boron carbide powder into a hafnium metal rod, hafnium pipe, europium and stainless made poison tube. Since the long life type absorber rod uses HF as the absorbing nuclear chain type neutron absorber, it absorbs neutrons to form new neutron absorbers to increase the nuclear life. (Yoshino, Y.)

  11. Control rod withdrawal monitoring device

    International Nuclear Information System (INIS)

    Ebisuya, Mitsuo.

    1984-01-01

    Purpose: To prevent the power ramp even if a plurality of control rods are subjected to withdrawal operation at a time, by reducing the reactivity applied to the reactor. Constitution: The control rod withdrawal monitoring device is adapted to monitor and control the withdrawal of the control rods depending on the reactor power and the monitoring region thereof is divided into a control rod group monitoring region a transition region and a control group monitoring not interfere region. In a case if the distance between a plurality of control rods for which the withdrawal positions are selected is less than a limiting value, the coordinate for the control rods, distance between the control rods and that the control rod distance is shorter are displayed on a display panel, and the withdrawal for the control rods are blocked. Accordingly, even if a plurality of control rods are subjected successively to the withdrawal operation contrary to the control rod withdrawal sequence upon high power operation of the reactor, the power ramp can be prevented. (Kawakami, Y.)

  12. Temperature distribution determination of JPSR power reactor fuel element and cladding

    International Nuclear Information System (INIS)

    Sudarmono

    1996-01-01

    In order to utilize of fuel rod efficiency, a concept of JAERI passive Safety Reactor (JPSR) has been developed in Japan Atomic Energy Research Institute. In the JPSR design, UO 2 . are adopted as a fuel rod. The temperature distribution in the fuel rod and cladding in the hottest channel is a potential limiting design constraint of the JPSR. In the present determination, temperature distribution of the fuel rod and cladding for JPSR were PET:formed using COBRA-IV-I to evaluate the safety margin of the present JPSR design. In this method, the whole core was represented by the 1/4 sector and divided into 50 subchannels and 40 axial nodes. The temperature become maximum at the elevation of 1.922 and 2.196 m in the typical cell under operating condition. The maximum temperature in the center of the fuel rod surface of the fuel rod and cladding were 1620,4 o C, 722,8 o C, and 348,6 o C. The maximum results of temperature in the center of the fuel rod and cladding; were 2015,28 o C and 550 o C which were observed at 3.1 second in the typical cell

  13. Experimental study of the deformation of Zircaloy PWR fuel rod cladding under mainly convective cooling

    International Nuclear Information System (INIS)

    Hindle, E.D.; Mann, C.A.

    1982-01-01

    Zircaloy-4 cladding specimens 450 mm long were filled with alumina pellets and tested at temperatures between 630 and 915 degree C in flowing steam at atmospheric pressure. Internal test pressures were in the range 0.69 to 11.0 MPa. The length of cladding strained 33 percent or more was greatest (about 20 times the original diameter) when the initial pressure was 1.38/plus or minus/0.17MPa. This results from oxidation strengthening of the surface layers acting as an additional mechanism for stabilizing the deformation or partial superplastic deformation, or both. For adjacent rods in a fuel assembly not to touch at any temperature, the pressure would have to be less than about 1 MPa. These results are compared with those form multirod tests elsewhere, and it is suggested that heat transfer has a dominant effect in determining deformation. The implications for the behavior of fuel elements in a loss-of-coolant accident are outlined. 37 refs

  14. Experimental study of the deformation of Zircaloy PWR fuel rod cladding under mainly convective cooling

    Energy Technology Data Exchange (ETDEWEB)

    Hindle, E.D.; Mann, C.A.

    1982-01-01

    Zircaloy-4 cladding specimens 450 mm long were filled with alumina pellets and tested at temperatures between 630 and 915 degree C in flowing steam at atmospheric pressure. Internal test pressures were in the range 0.69 to 11.0 MPa. The length of cladding strained 33 percent or more was greatest (about 20 times the original diameter) when the initial pressure was 1.38/plus or minus/0.17MPa. This results from oxidation strengthening of the surface layers acting as an additional mechanism for stabilizing the deformation or partial superplastic deformation, or both. For adjacent rods in a fuel assembly not to touch at any temperature, the pressure would have to be less than about 1 MPa. These results are compared with those form multirod tests elsewhere, and it is suggested that heat transfer has a dominant effect in determining deformation. The implications for the behavior of fuel elements in a loss-of-coolant accident are outlined. 37 refs.

  15. Mechanical behaviour of PWR fuel rods during intermediate storage

    International Nuclear Information System (INIS)

    Bouffioux, P.; Dalmas, R.; Bernaudat, C.

    2000-01-01

    EDF, which owns the irradiated fuel coming from its NPPs, has initiated studies regarding the mechanical behaviour of a fuel rod and the integrity of its cladding, in the case where the spent fuel is stored for a significant duration. During the phases following in-reactor irradiation (ageing in a water-pool, transport and intermediate storage), many phenomena, which are strongly coupled, may influence the cladding integrity: - residual power and temperature decay; - helium production and release in the free volume of the rod (especially for MOX fuel); - fuel column swelling; - cladding creep-out under the inner gas pressure of the fuel rod; - metallurgical changes due to high temperatures during transportation. In parallel, the quantification of the radiological risk is based on the definition of a cladding integrity criterion. Up to now, this criterion requires that the clad hoop strain due to creep-out does not exceed 1%. A more accurate criterion is being investigated. The study and modelling of all the phenomena mentioned above are included in a R and D programme. This programme also aims at redefining the cladding integrity criterion, which is assumed to be too conservative. The R and D programme will be presented. In order to predict the overall behaviour of the rod during the intermediate storage phases, the AVACYC code has been developed. It includes the models developed in the R and D programme. The input data of the AVACYC code are provided by the results of in-reactor rod behaviour simulations, using the thermal-mechanical CYRANO3 code. Its main results are the evolution vs. time of hoop stresses in the cladding, rod internal pressure and cladding hoop strains. Chained CYRANO-AVACYC calculations have been used to simulate the behaviour of MOX fuel rods irradiated up to 40 GWd/t and stored under air during 100 years, or under water during 50 years. For such fuels, where the residual power remains high, we show that a large part of the cladding strain

  16. Development of high performance cladding materials

    International Nuclear Information System (INIS)

    Park, Jeong Yong; Jeong, Y. H.; Park, S. Y.

    2010-04-01

    The irradiation test for HANA claddings conducted and a series of evaluation for next-HANA claddings as well as their in-pile and out-of pile performances tests were also carried out at Halden research reactor. The 6th irradiation test have been completed successfully in Halden research reactor. As a result, HANA claddings showed high performance, such as corrosion resistance increased by 40% compared to Zircaloy-4. The high performance of HANA claddings in Halden test has enabled lead test rod program as the first step of the commercialization of HANA claddings. DB has been established for thermal and LOCA-related properties. It was confirmed from the thermal shock test that the integrity of HANA claddings was maintained in more expanded region than the criteria regulated by NRC. The manufacturing process of strips was established in order to apply HANA alloys, which were originally developed for the claddings, to the spacer grids. 250 kinds of model alloys for the next-generation claddings were designed and manufactured over 4 times and used to select the preliminary candidate alloys for the next-generation claddings. The selected candidate alloys showed 50% better corrosion resistance and 20% improved high temperature oxidation resistance compared to the foreign advanced claddings. We established the manufacturing condition controlling the performance of the dual-cooled claddings by changing the reduction rate in the cold working steps

  17. FRACAS: a subcode for the analysis of fuel pellet-cladding mechanical interaction

    International Nuclear Information System (INIS)

    Bohn, M.P.

    1977-04-01

    This report describes FRACAS (Fuel Rod and Cladding Analysis Subcode), a computer code which performs the mechanical analysis in the FRAP fuel rod codes. At each loadstep, FRACAS obtains a complete elastic-plastic-creep solution for the stresses, strains, and displacements in the fuel rod cladding. The cladding is modeled as a thin cylindrical shell with prescribed temperature, pressures, and radial displacement of the inside surface. The displacement of the fuel pellets is assumed to be due to thermal gradients only. Three different regimes of pellet-cladding mechanical interaction are considered: (a) open gap, (b) closed gap, and (c) trapped stack. Both transient and steady state creep calculations are performed. The capabilities of the code are illustrated by an example problem, and comparisons are made with data obtained from two experimental fuel rods

  18. Analysis of fuel rod behaviour within a rod bundle of a pressurized water reactor under the conditions of a loss of coolant accident (LOCA) using probabilistic methodology

    International Nuclear Information System (INIS)

    Sengpiel, W.

    1980-12-01

    The assessment of fuel rod behaviour under PWR LOCA conditions aims at the evaluation of the peak cladding temperatures and the (final) maximum circumferential cladding strains. Moreover, the estimation of the amount of possible coolant channel blockages within a rod bundle is of special interest, as large coplanar clad strains of adjacent rods may result in strong local reductions of coolant channel areas. Coolant channel blockages of large radial extent may impair the long-term coolability of the corresponding rods. A model has been developed to describe these accident consequences using probabilistic methodology. This model is applied to study the behaviour of fuel rods under accident conditions following the double-ended pipe rupture between collant pump and pressure vessel in the primary system of a 1300 MW(el)-PWR. Specifically a rod bundle is considered consisting of 236 fuel rods, that is subjected to severe thermal and mechanical loading. The results obtained indicate that plastic clad deformations with circumferential clad strains of more than 30% cannot be excluded for hot rods of the reference bundle. However, coplanar coolant channel blockages of significant extent seem to be probable within that bundle only under certain boundary conditions which are assumed to be pessimistic. (orig./RW) [de

  19. Cladding axial elongation models for FRAP-T6

    International Nuclear Information System (INIS)

    Shah, V.N.; Carlson, E.R.; Berna, G.A.

    1983-01-01

    This paper presents a description of the cladding axial elongation models developed at the Idaho National Engineering Laboratory (INEL) for use by the FRAP-T6 computer code in analyzing the response of fuel rods during reactor transients in light water reactors (LWR). The FRAP-T6 code contains models (FRACAS-II subcode) that analyze the structural response of a fuel rod including pellet-cladding-mechanical-interaction (PCMI). Recently, four models were incorporated into FRACAS-II to calculate cladding axial deformation: (a) axial PCMI, (b) trapped fuel stack, (c) fuel relocation, and (d) effective fuel thermal expansion. Comparisons of cladding axial elongation measurements from two experiments with the corresponding FRAP-T6 calculations are presented

  20. Failure probabilities of SiC clad fuel during a LOCA in public acceptable simple SMR (PASS)

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Youho, E-mail: euo@kaist.ac.kr; Kim, Ho Sik, E-mail: hskim25@kaist.ac.kr; NO, Hee Cheon, E-mail: hcno@kaist.ac.kr

    2015-10-15

    Highlights: • Graceful operating conditions of SMRs markedly lower SiC cladding stress. • Steady-state fracture probabilities of SiC cladding is below 10{sup −7} in SMRs. • PASS demonstrates fuel coolability (T < 1300 °C) with sole radiation in LOCA. • SiC cladding failure probabilities of PASS are ∼10{sup −2} in LOCA. • Cold gas gap pressure controls SiC cladding tensile stress level in LOCA. - Abstract: Structural integrity of SiC clad fuels in reference Small Modular Reactors (SMRs) (NuScale, SMART, IRIS) and a commercial pressurized water reactor (PWR) are assessed with a multi-layered SiC cladding structural analysis code. Featured with low fuel pin power and temperature, SMRs demonstrate markedly reduced incore-residence fracture probabilities below ∼10{sup −7}, compared to those of commercial PWRs ∼10{sup −6}–10{sup −1}. This demonstrates that SMRs can serve as a near-term deployment fit to SiC cladding with a sound management of its statistical brittle fracture. We proposed a novel SMR named Public Acceptable Simple SMR (PASS), which is featured with 14 × 14 assemblies of SiC clad fuels arranged in a square ring layout. PASS aims to rely on radiative cooling of fuel rods during a loss of coolant accident (LOCA) by fully leveraging high temperature tolerance of SiC cladding. An overarching assessment of SiC clad fuel performance in PASS was conducted with a combined methodology—(1) FRAPCON-SiC for steady-state performance analysis of PASS fuel rods, (2) computational fluid dynamics code FLUENT for radiative cooling rate of fuel rods during a LOCA, and (3) multi-layered SiC cladding structural analysis code with previously developed SiC recession correlations under steam environments for both steady-state and LOCA. The results show that PASS simultaneously maintains desirable fuel cooling rate with the sole radiation and sound structural integrity of fuel rods for over 36 days of a LOCA without water supply. The stress level of

  1. Loop capabilities in Rez for water chemistry and corrosion control of cladding and in-core components

    International Nuclear Information System (INIS)

    Kysela, J.; Zmitko, M.; Srank, J.; Vsolak, R.

    1999-01-01

    Main characteristics of LVR-15 research reactor and its irradiation facilities are presented. For testing of cladding, internals and RPV materials specialised loop are used. There are now five high pressure loops modelling PWR, WWER or BWR water environment and chemistry. Loops can be connected with instrumented in-pile channels enable slow strain rate testing, 1CT or 2CT specimens loading and electrically heated rods exposition. Reactor dosimetry including neutronic parameters measurements and calculations and mock-up experiments are used. Water chemistry control involves gas (O 2 , H 2 ) dosing system, Orbisphere H 2 /O 2 measurement, electrochemical potential (ECP) measurements and specialised analytical chemistry laboratory. For cladding corrosion studies in-pile channels with four electrically heated rods with heat flux up to 100 W/cm 2 , void fraction 5 % at the outlet, inlet temperature 320 deg. C and flow velocity 3 m/s were development and tested. For corrosion layer investigation there is eddy current measurements and PIE techniques which use crud thickness measurement, chemical analyses of the crud, optical metallography, hydrogen analysis, SEM and TEM. (author)

  2. The buckling of fuel rods in transportation casks under hypothetical accident conditions

    International Nuclear Information System (INIS)

    Bjorkman, G.S.

    2004-01-01

    The buckling analysis of fuel rods during an end drop impact of a spent fuel transportation cask has traditionally been performed to demonstrate the structural integrity of the fuel rod cladding or the integrity of the fuel geometry in criticality evaluations following a cask drop event. The actual calculation of the fuel rod buckling load, however, has been the subject of some controversy, with estimates of the critical buckling load differing by as much as a factor of 5. Typically, in the buckling analysis of a fuel rod, assumptions are made regarding the percentage of fuel mass that is bonded to or participates with the cladding during the buckling process, with estimates ranging from 0 to 100%. The greater the percentage of fuel mass that is assumed to be bonded to the cladding the higher the inertia loads on the cladding, and, therefore, the lower the ''g'' value at which buckling occurs. Current published solutions do not consider displacement compatibility between the fuel and the cladding. By invoking displacement compatibility between the fuel column and the cladding column, this paper presents an exact solution for the buckling of fuel rods under inertia loading. The results show that the critical inertia load magnitude for the buckling of a fuel rod depends on the weight of the cladding and the total weight of the fuel, regardless of the percentage of fuel mass that is assumed to be attached to or participate with the cladding in the buckling process. Therefore, 100% of the fuel always participates in the buckling of a fuel rod under inertia loading

  3. Control rods

    International Nuclear Information System (INIS)

    Koga, Isao; Masuoka, Ryuzo.

    1979-01-01

    Purpose: To prevent fuel element failures during power conditioning by removing liquid absorbents in poison tubes of control rods in a fast power up step and extracting control rods to slightly increase power in a medium power up step. Constitution: A plurality of poison tubes are disposed in a coaxial or plate-like arrangement and divided into a region capable of compensating the reactivity from the initial state at low temperature to 40% power operation and a region capable of compensating the reactivity in the power up above 40% power operation. Soluble poisons are used as absorbers in the poison tubes corresponding to above 40% power operation and they are adapted to be removed independently from the driving of control rods. The poison tubes filled with the soluble absorbers are responsible for the changes in the reactivity from the initial state at low temperature to the medium power region and the reactivity control is conducted by the elimination of liquid absorbers from the poison tubes. In the succeeding slight power up region above the medium power, power up is proceeding by extracting the control rods having remaining poison tubes filled with solid or liquid absorbers. (Seki, T.)

  4. Fuel rod pressure in nuclear power reactors: Statistical evaluation of the fuel rod internal pressure in LWRs with application to lift-off probability

    Energy Technology Data Exchange (ETDEWEB)

    Jelinek, Tomas

    2001-02-01

    In this thesis, a methodology for quantifying the risk of exceeding the Lift-off limit in nuclear light water power reactors is outlined. Due to fission gas release, the pressure in the gap between the fuel pellets and the cladding increases with burnup of the fuel. An increase in the fuel-clad gap due to clad creep would be expected to result in positive feedback, in the form of higher fuel temperatures, leading to more fission gas release, higher rod pressure, etc, until the cladding breaks. An increase in the fuel-clad gap that leads to this positive feedback is a phenomenon called Lift-off and is a limitation that must be considered in the fuel core management. Lift-off is a consequence of very high internal fuel rod pressure. The internal fuel rod pressure is therefore used as a Lift-off indicator. The internal fuel rod pressure is closely connected to the fission gas release into the fuel rod plenum and is thus used to increase the database. It is concluded that the dominating error source in the prediction of the pressure in Boiling Water Reactors (BWR), is the power history. There is a bias in the fuel pressure prediction that is dependent on the fuel rod position in the fuel assembly for BWRs. A methodology to quantify the risk of the fuel rod internal pressure exceeding a certain limit is developed; the risk is dependent of the pressure prediction and the fuel rod position. The methodology is based on statistical treatment of the discrepancies between predicted and measured fuel rod internal pressures. Finally, a methodology to estimate the Lift-off probability of the whole core is outlined.

  5. Stainless steel clad for light water reactor fuels. Final report

    International Nuclear Information System (INIS)

    Rivera, J.E.; Meyer, J.E.

    1980-07-01

    Proper reactor operation and design guidelines are necessary to assure fuel integrity. The occurrence of fuel rod failures for operation in compliance with existing guidelines suggests the need for more adequate or applicable operation/design criteria. The intent of this study is to develop such criteria for light water reactor fuel rods with stainless steel clad and to indicate the nature of uncertainties in its development. The performance areas investigated herein are: long term creepdown and fuel swelling effects on clad dimensional changes and on proximity to clad failure; and short term clad failure possibilities during up-power ramps

  6. Measurement of the residual stresses in a PWR Control Rod Drive Mechanism nozzle

    OpenAIRE

    Coules, Harry; Smith, David

    2018-01-01

    Residual stress in the welds that attach Control Rod Drive Mechanism nozzles into the upper head of a PWR reactor vessel can influence the vessel's structural integrity and initiate Primary Water Stress Corrosion Cracking. PWSCC at Alloy 600 CRDM nozzles has caused primary coolant leakage in operating PWRs. We have used Deep Hole Drilling to characterise residual stresses in a PWR vessel head. Measurements of the internal cladding and nozzle attachment weld showed that although modest tensile...

  7. IFPE/IFA-432, Fission Gas Release, Mechanical Interaction BWR Fuel Rods, Halden

    International Nuclear Information System (INIS)

    Turnbull, J.A.

    1996-01-01

    Description: It contains data from experiments that have been performed at the IFE/OECD Halden Reactor Project, available for use in fuel performance studies. It covers experiments on thermal performance, fission product release, clad properties and pellet clad mechanical interaction. It includes also experimental data relevant to high burn-up behaviour. IFA-432: Measurements of fuel temperature response, fission gas release and mechanical interaction on BWR-type fuel rods up to high burn-ups. The assembly featured several variations in rod design parameters, including fuel type, fuel/cladding gap size, fill gas composition (He and Xe) and fuel stability. It contained 6 BWR-type fuel rods with fuel centre thermocouples at two horizontal planes, rods were also equipped with pressure transducers and cladding extensometers. Only data from 6 rods are compiled here

  8. Testing device for control rod drives

    International Nuclear Information System (INIS)

    Hayakawa, Toshifumi.

    1992-01-01

    A testing device for control rod drives comprises a logic measuring means for measuring an output signal from a control rod drive logic generation circuit, a control means for judging the operation state of a control rod and a man machine interface means for outputting the result of the judgement. A driving instruction outputted from the control rod operation device is always monitored by the control means, and if the operation instruction is stopped, a testing signal is outputted to the control rod control device to simulate a control rod operation. In this case, the output signal of the control rod drive logic generation circuit is held in a control rod drive memory means and intaken into a logic analysis means for measurement and an abnormality is judged by the control means. The stopping of the control rod drive instruction is monitored and the operation abnormality of the control rod is judged, to mitigate the burden of an operator. Further, the operation of the control rod drive logic generation circuit can be confirmed even during a nuclear plant operation by holding the control rod drive instruction thereby enabling to improve maintenance efficiency. (N.H.)

  9. Control rod velocity limiter

    International Nuclear Information System (INIS)

    Cearley, J.E.; Carruth, J.C.; Dixon, R.C.; Spencer, S.S.; Zuloaga, J.A. Jr.

    1986-01-01

    This patent describes a velocity control arrangement for a reciprocable, vertically oriented control rod for use in a nuclear reactor in a fluid medium, the control rod including a drive hub secured to and extending from one end therefrom. The control device comprises: a toroidally shaped control member spaced from and coaxially positioned around the hub and secured thereto by a plurality of spaced radial webs thereby providing an annular passage for fluid intermediate the hub and the toroidal member spaced therefrom in coaxial position. The side of the control member toward the control rod has a smooth generally conical surface. The side of the control member away from the control rod is formed with a concave surface constituting a single annular groove. The device also comprises inner and outer annular vanes radially spaced from one another and spaced from the side of the control member away from the control rod and positioned coaxially around and spaced from the hub and secured thereto by spaced radial webs thereby providing an annular passage for fluid intermediate the hub and the vanes. The vanes are angled toward the control member, the outer edge of the inner vane being closer to the control member and the inner edge of the outer vane being closer to the control member. When the control rod moves in the fluid in the direction toward the drive hub the vanes direct a flow of fluid turbulence which provides greater resistance to movement of the control rod in the direction toward the drive hub than in the other direction

  10. Integrated control rod monitoring device

    International Nuclear Information System (INIS)

    Saito, Katsuhiro

    1997-01-01

    The present invention provides a device in which an entire control rod driving time measuring device and a control rod position support device in a reactor building and a central control chamber are integrated systematically to save hardwares such as a signal input/output device and signal cables between boards. Namely, (1) functions of the entire control rod driving time measuring device for monitoring control rods which control the reactor power and a control rod position indication device are integrated into one identical system. Then, the entire devices can be made compact by the integration of the functions. (2) The functions of the entire control rod driving time measuring device and the control rod position indication device are integrated in a central operation board and a board in the site. Then, the place for the installation of them can be used in common in any of the cases. (3) The functions of the entire control rod driving time measuring device and the control rod position indication device are integrated to one identical system to save hardware to be used. Then, signal input/output devices and drift branching panel boards in the site and the central operation board can be saved, and cables for connecting both of the boards is no more necessary. (I.S.)

  11. Research on laser cladding control system based on fuzzy PID

    Science.gov (United States)

    Zhang, Chuanwei; Yu, Zhengyang

    2017-12-01

    Laser cladding technology has a high demand for control system, and the domestic laser cladding control system mostly uses the traditional PID control algorithm. Therefore, the laser cladding control system has a lot of room for improvement. This feature is suitable for laser cladding technology, Based on fuzzy PID three closed-loop control system, and compared with the conventional PID; At the same time, the laser cladding experiment and friction and wear experiment were carried out under the premise of ensuring the reasonable control system. Experiments show that compared with the conventional PID algorithm in fuzzy the PID algorithm under the surface of the cladding layer is more smooth, the surface roughness increases, and the wear resistance of the cladding layer is also enhanced.

  12. Control rod drive for vertical movement

    International Nuclear Information System (INIS)

    Suskov, I.I.; Gorjunov, V.S.; Zajcev, B.I.; Derevjankin, N.E.; Petrov, V.A.; Istomin, S.D.; Kovalencik, D.I.; Archipov, E.A.; Serebrjakov, V.I.; Kacalin, V.S.

    1982-01-01

    The control of the rod repositioning gear unit and the control unit of the profile grab of the control rod drive for the alkali metal-cooled fast breeder reactor is achieved by an electromotor being arranged outside the hermetic drive casing. The guide tube is directly repositioned by the rod repositioning gear unit. Coupling control of the drive with the control rod is done in the lower operative position of the control rod and that because of the interaction of the tie rod arranged on the spring-mounted control rod with the induction transmitter for the lower position of the control rod. In the transfer position the rod is fixed within the guide tube. (orig.)

  13. Characteristics of copper-clad aluminum rods prepared by horizontal continuous casting

    Science.gov (United States)

    Zhang, Yubo; Fu, Ying; Jie, Jinchuan; Wu, Li; Svynarenko, Kateryna; Guo, Qingtao; Li, Tingju; Wang, Tongmin

    2017-11-01

    An innovative horizontal continuous casting method was developed and successfully used to prepare copper-clad aluminum (CCA) rods with a diameter of 85 mm and a sheath thickness of 16 mm. The solidification structure and element distribution near the interface of the CCA ingots were investigated by means of a scanning electron microscope, an energy dispersive spectrometer, and an electron probe X-ray microanalyzer. The results showed that the proposed process can lead to a good metallurgical bond between Cu and Al. The interface between Cu and Al was a multilayered structure with a thickness of 200 μm, consisting of Cu9Al4, CuAl2, α-Al/CuAl2 eutectic, and α-Al + α-Al/CuAl2 eutectic layers from the Cu side to the Al side. The mean tensile-shear strength of the CCA sample was 45 MPa, which fulfills the requirements for the further extrusion process. The bonding and diffusion mechanisms are also discussed in this paper.

  14. Control device for the withdrawal of control rod

    International Nuclear Information System (INIS)

    Ando, Masaki.

    1985-01-01

    Purpose: To significantly suppress the maximum value of the control-rod worth upon control rod withdrawal. Constitution: At first, a signal for designating the first class is sent from a class-control section to the group-control section. In the group-control section, the peripheral group among the first class is designated by which the withdrawal of the control rods other than the peripheral group is inhibited and the control-rods in the peripheral group are withdrawn one by one. When all of them have been withdrawn, the group-control section designates the central group of the first class. All the control rods of the central group have been withdrawn, then the group-control section designates the peripheral group of the second class. Thereafter, the central group in the second class is designated. The control rods are thus withdrawn in the same manner hereinafter. The maximum value for the control-rod worth can be decreased by such a withdrawing sequence for the control rods. (Horiuchi, T.)

  15. RodPilotR - The Innovative and Cost-Effective Digital Control Rod Drive Control System for PWRs

    International Nuclear Information System (INIS)

    Baron, Clemens

    2008-01-01

    With RodPilot, AREVA NP offers an innovative and cost-effective system for controlling control rods in Pressurized Water Reactors. RodPilot controls the three operating coils of the control rod drive mechanism (lift, moveable gripper and stationary gripper coil). The rods are inserted into or withdrawn from the core as required by the Reactor Control System. The system combines modern components, state-of-the-art logic and a proven electronic control rod drive control principle to provide enhanced reliability and lower maintenance costs. (author)

  16. Method for automatic filling of nuclear fuel rod cladding tubes

    International Nuclear Information System (INIS)

    Bezold, H.

    1979-01-01

    Prior to welding the zirconium alloy cladding tubes with end caps, they are automatically filled with nuclear fuel tablets and ceramic insulating tablets. The tablets are introduced into magazine drums and led through a drying oven to a discharging station. The empty cladding tubes are removed from this discharging station and filled with tablets. A filling stamp pushes out the columns of tablets in the magazine tubes of the magazine drum into the cladding tube. Weight and measurement of length determine the filled state of the cladding tube. The cladding tubes are then led to the welding station via a conveyor belt. (DG) [de

  17. Change in geometrical parameters of WWER high burnup fuel rods under operational conditions and transient testing

    International Nuclear Information System (INIS)

    Kanashov, B.; Amosov, S.; Lyadov, G.; Markov, D.; Ovchinnikov, V; Polenok, V.; Smirnov, A.; Sukhikh, A.; Bek, E.; Yenin, A.; Novikov, V.

    2001-01-01

    The paper discusses changes in fuel rods geometric parameters as result of operation conditions and burnups. The degree of geometry variability of fuel rods, cladding and column is one of the most important characteristics affecting fuel serviceability. On the other hand, changes in fuel rod geometric parameters influence fuel temperature, fission gas release, fuel-to-cladding stress strained state as well as the degree of interaction with FA skeleton elements and skeleton rigidity. Change in fuel-to-cladding gap is measured using compression technique. The axial distribution of fuel-to-cladding gap demonstrates the largest decrease of the gap in the region 500 to 2000 mm from the bottom of the fuel rod (WWER-440) and in the region of 500 to 3000 mm for WWER-1000. The cladding material creep in WWER fuel rods together with the radiation growth results in fuel rod cladding elongation. A set of transient tests for spent WWER-440 and WWER-1000 fuel rods carried out in SSC RIAR during a period 1995-1999, with the aim to estimate the changes in geometric parameters of FRs. The estimation of changes in outer diameter of cladding and fuel column and fuel-to-cladding gap are performed in transient conditions (changes in linear power range of 180 to 400 W/cm) for both WWER-440 and WWER-1000. WWER-440 fuel rods having the same burnup and close fuel-cladding contact before testing are subjected to considerable hoop cladding strain in testing up to 300 W/cm. But the hoop strain does not grow due to the structural changes in fuel column and decrease in central hole diameter occurred when the power is higher

  18. Digital control rod blocking monitor

    International Nuclear Information System (INIS)

    Funayama, Yoshio.

    1996-01-01

    The present invention system is used for monitoring of a power region of a reactor, and used for monitoring of simultaneous withdrawal of a plurality of control rods without increasing the size or complicating the system. Namely, the system processes signals from a neutron flux detectors at the periphery of control rods controlled for withdrawal. As a result of the processing, the digital monitoring system generates an alarm when the reactor power at the periphery of the control rods fluctuates exceeding an allowable range. In the system, a control rod information forming means prepares frame data comprising front data, positions of the control rods to be withdrawn, frame numbers and completion data. A serial data transmitting means transmits the frame data successively as repeating frame data rows. A control rod information receiving means takes up the frame data of each of control rods to be withdrawn from the transmitted frame data rows. Since the system of the present invention can monitor the withdrawal of a plurality of control rods simultaneously without increasing the size or complicating the system, cost can be saved and the maintenance can be improved. (I.S.)

  19. Evaluation of LWR fuel rod behavior under operational transient conditions

    International Nuclear Information System (INIS)

    Nakamura, M.; Hiramoto, K.; Maru, A.

    1984-01-01

    To evaluate the effects of fission gas flow and diffusion in the fuel-cladding gap on fuel rod thermal and mechanical behaviors in light water reactor (LWR) fuel rods under operational transient conditions, computer sub-programs which can calculate the gas flow and diffusion have been developed and integrated into the LWR fuel rod performance code BEAF. This integrated code also calculates transient temperature distribution in the fuel-pellet and cladding. The integrated code was applied to an analysis of Inter Ramp Project data, which showed that by taking into account the gas flow and diffusion effects, the calculated cladding damage indices predicted for the failed rods in the ramp test were consistent with iodine-SCC (Stress Corrosion Cracking) failure conditions which were obtained from out-of-reactor pressurized tube experiments with irradiated Zircaloy claddings. This consistency was not seen if the gas flow and diffusion effects were neglected. Evaluation were also made for the BWR 8x8 RJ fuel rod temperatures under power ramp conditions. (orig.)

  20. Experimental determination of local temperature field variations due to spacer grids in the cladding tubes of a rod cluster flowed through by sodium

    International Nuclear Information System (INIS)

    Moeller, R.; Tschoeke, H.

    1978-01-01

    If spacer grids are used to keep the fuel rods in their places - as in the fuel elements of the SNR series, exact tests are necessary to find out whether and to what extent temperature peaks near the supporting points affect cladding tube design. To clarify this special problem, experimental investigations have been carried out for the first time in a rod cluster model of the SNR-300 fuel element cross-flowed with sodium. The investigations and findings so far are reported on. (orig./RW) [de

  1. IFPE/NFIR-1, Clad creep-down, power history effect on fission product distribution (6 PWR rods 40-64 MWd/kg in BR-3)

    International Nuclear Information System (INIS)

    Turnbull, J.A.

    2006-01-01

    Description: The NFIR-1 programme was designed to investigate factors likely to affect the fission gas release behaviour of fuel rods operating under normal commercial conditions. The factors which were investigated were: - the effect of fuel/rod design parameters, e.g., wet versus dry route pellet manufacture, fuel-clad gap size and rod pressurization; - the effect of power history i.e., In/Out fuel management strategy; - the effect of burn-up extension. This was accomplished by an extensive PIE campaign on 6 fuel rods irradiated to 40-64 MWd/kg under different prescribed conditions in the BR3 PWR. The examination involved non destructive mensuration and destructive examination using optical, SEM, TEM and EPMA techniques. The dataset is unique in demonstrating the effect of these variables on fuel performance

  2. Development and application of an asymmetric deformation model to describe the fuel rod behaviour during LOCA

    International Nuclear Information System (INIS)

    Chakraborty, A.K.; Schubert, J.D.

    1983-01-01

    For calculation of clad ballooning from single rod and rod bundle experiments a model considering the influences of azimuthal temperature gradients due to the existing eccentricity of the pellets has been developed. This model is based on the secondary creep model of Norton and on the concentric deformation model ending in cladding burst as proposed by F. Erbacher. The new model considers the azimuthal temperature differences along the cladding and the resulting differences in deformations. With this model, calculations of cladding burst deformations from single rod and rod bundle experiments are performed with good agreement

  3. Sturdy on Orbital TIG Welding Properties for Nuclear Fuel Test Rod

    International Nuclear Information System (INIS)

    Joung, Changyoung; Hong, Jintae; Kim, Kahye; Huh, Sungho

    2014-01-01

    We developed a precision TIG welding system that is able to weld the seam between end-caps and a fuel cladding tube for the nuclear fuel test rod and rig. This system can be mainly classified into an orbital TIG welder (AMI, M-207A) and a pressure chamber. The orbital TIG welder can be independently used, and it consists of a power supply unit, a microprocessor, water cooling unit, a gas supply unit and an orbital weld head. In this welder, the power supply unit mainly supplies GTAW power for a welding specimen and controls an arc starting of high frequency, supping of purge gas, arc rotation through the orbital TIG welding head, and automatic timing functions. In addition, the pressure chamber is used to make the welded surface of the cladding specimen clean with the inert gas filled inside the chamber. To precisely weld the cladding tube, a welding process needs to establish a schedule program for an orbital TIG welding. Therefore, the weld tests were performed on a cladding tube and dummy rods under various conditions. This paper describes not only test results on parameters of the purge gas flow rates and the chamber gas pressures for the orbital TIG welding, but also test results on the program establishment of an orbital TIG welding system to weld the fuel test rods. Various welding tests were performed to develop the orbital TIG welding techniques for the nuclear fuel test rod. The width of HAZ of a cladding specimen welded with the identical power during an orbital TIG welding cycle was continuously increased from a welded start-point to a weld end-point because of heat accumulation. The welding effect of the PGFR and CGP shows a relatively large difference for FSS and LSS. Each hole on the cladding specimens was formed in the 1bar CGP with the 20L/min PGFR but not made in the case of the PGFR of 10L/min in the CGP of 2bar. The optimum schedule program of the orbital TIG welding system to weld the nuclear fuel test rod was established through the program

  4. Sturdy on Orbital TIG Welding Properties for Nuclear Fuel Test Rod

    Energy Technology Data Exchange (ETDEWEB)

    Joung, Changyoung; Hong, Jintae; Kim, Kahye; Huh, Sungho [Korea Atomic Energy Research Institute, Daejeon (Korea, Republic of)

    2014-05-15

    We developed a precision TIG welding system that is able to weld the seam between end-caps and a fuel cladding tube for the nuclear fuel test rod and rig. This system can be mainly classified into an orbital TIG welder (AMI, M-207A) and a pressure chamber. The orbital TIG welder can be independently used, and it consists of a power supply unit, a microprocessor, water cooling unit, a gas supply unit and an orbital weld head. In this welder, the power supply unit mainly supplies GTAW power for a welding specimen and controls an arc starting of high frequency, supping of purge gas, arc rotation through the orbital TIG welding head, and automatic timing functions. In addition, the pressure chamber is used to make the welded surface of the cladding specimen clean with the inert gas filled inside the chamber. To precisely weld the cladding tube, a welding process needs to establish a schedule program for an orbital TIG welding. Therefore, the weld tests were performed on a cladding tube and dummy rods under various conditions. This paper describes not only test results on parameters of the purge gas flow rates and the chamber gas pressures for the orbital TIG welding, but also test results on the program establishment of an orbital TIG welding system to weld the fuel test rods. Various welding tests were performed to develop the orbital TIG welding techniques for the nuclear fuel test rod. The width of HAZ of a cladding specimen welded with the identical power during an orbital TIG welding cycle was continuously increased from a welded start-point to a weld end-point because of heat accumulation. The welding effect of the PGFR and CGP shows a relatively large difference for FSS and LSS. Each hole on the cladding specimens was formed in the 1bar CGP with the 20L/min PGFR but not made in the case of the PGFR of 10L/min in the CGP of 2bar. The optimum schedule program of the orbital TIG welding system to weld the nuclear fuel test rod was established through the program

  5. RodPilot{sup R} - The Innovative and Cost-Effective Digital Control Rod Drive Control System for PWRs

    Energy Technology Data Exchange (ETDEWEB)

    Baron, Clemens [AREVA NP GmbH, NLEE-G, Postfach 1199, 91001 Erlangen (Germany)

    2008-07-01

    With RodPilot, AREVA NP offers an innovative and cost-effective system for controlling control rods in Pressurized Water Reactors. RodPilot controls the three operating coils of the control rod drive mechanism (lift, moveable gripper and stationary gripper coil). The rods are inserted into or withdrawn from the core as required by the Reactor Control System. The system combines modern components, state-of-the-art logic and a proven electronic control rod drive control principle to provide enhanced reliability and lower maintenance costs. (author)

  6. Control-rod driving mechanism

    International Nuclear Information System (INIS)

    Jodoi, Takashi.

    1976-01-01

    Purpose: To prevent falling of control rods due to malfunction. Constitution: The device of the present invention has a scram function in particular, and uses principally a fluid pressure as a scram accelerating means. The control rod is held by upper and lower holding devices, which are connected by a connecting mechanism. This connecting mechanism is designed to be detachable only at the lower limit of driving stroke of the control rod so that there occurs no erroneous scram resulting from careless disconnection of the connecting mechanism. Further, scramming operation due to own weight of the scram operating portion such as control rod driving shaft may be effected to increase freedom. (Kamimura, M.)

  7. Design criteria for confidence in the manufacture of BWR fuel rods

    International Nuclear Information System (INIS)

    Anantharaman, K.; Basu, S.; Anand, A.K.; Mehta, S.K.

    Based on the experience of fuel manufacture for BWR type reactors in India, the parameters which need stringent quality control, are discussed. The design specifications of the fuel rods as well as the cladding material and tubes are reported. The defect mechanisms to be taken into account and the fuel failure in reference to the variation of mechanical properties of the cladding are also described. (K.B.)

  8. The BWR Hybrid 4 control rod

    International Nuclear Information System (INIS)

    Gross, H.; Fuchs, H.P.; Lippert, H.J.; Dambietz, W.

    1988-01-01

    The service life of BWR control rods designed in the past has been unsatisfactory. The main reason was irradiation assisted stress corrosion cracking of B 4 C rods caused by external swelling of the B 4 C powder. By this reason KWU developed an improved BWR control rod (Hybrid 4 control rod) with extended service life and increased control rod worth. It also allows the procedure for replacing and rearranging fuel assemblies to be considerably simplified. A complete set of Hydbrid 4 control rods is expected to last throughout the service life of a plant (assumption: ca. 40 years) if an appropriate control rod reshuffling management program is used. (orig.)

  9. Characteristics of WWER-1000 fuel rod claddings and FA components from E635 alloy at burnups up to 72 MWd/kgU

    International Nuclear Information System (INIS)

    Nikulin, A.; Novikov, A.; Peregud, M.; Shishov, V.; Shevyakov, A.; Volkova, I.; Novoselov, A.; Kobylyansky, G.

    2011-01-01

    In this paper operation experience, results of investigated E365 alloy components of Balakovo NPP Unit 1 and Kalinin NPP unit 1 fuel assemblies are presented. Appearance, shape changes and geometric size, corrosion state of guide thimbles, angles and fuel rods, corrosion of fuel claddings are studied. At the end authors concluded that: I) E635 alloy corroborated its high operation reliability as fuel claddings and WWER-1000 FA components during 6 year service to the fuel burnup of 72MWd/kgU; II) Based on the results from the post-irradiation investigations of the fuel rods and other structural elements of WWER-1000 FAA, fabricated from E635 alloy, in terms of the basic operational characteristics, their resources after the 6 year operation cycle have not been exhausted; III) The geometrical parameters, corrosion states, tensile properties of items fabricated from fuel alloy did not attain the values that would prevent their further operation: 1) the elongations of the fuel rods at the mean burnups up to 66.2 MWd/kgU do not exceed 15 mm or 4.9%; 8) the amount of the oxide coat at surface of GT and CT does not exceed 45 μm, the hydrogen content is <0.03% mass; 9) the oxide coat at the surfaces of the frame angles does not exceed 50 μm, the hydrogen content is <0.04% mass

  10. Nuclear fuel rods

    International Nuclear Information System (INIS)

    Wada, Toyoji.

    1979-01-01

    Purpose: To remove failures caused from combination of fuel-cladding interactions, hydrogen absorptions, stress corrosions or the likes by setting the quantity ratio of uranium or uranium and plutonium relative to oxygen to a specific range in fuel pellets and forming a specific size of a through hole at the center of the pellets. Constitution: In a fuel rods of a structure wherein fuel pellets prepared by compacting and sintering uranium dioxide, or oxide mixture consisting of oxides of plutonium and uranium are sealed with a zirconium metal can, the ratio of uranium or uranium and plutonium to oxygen is specified as 1 : 2.01 - 1 : 2.05 in the can and a passing hole of a size in the range of 15 - 30% of the outer diameter of the fuel pellet is formed at the center of the pellet. This increases the oxygen partial pressure in the fuel rod, oxidizes and forms a protection layer on the inner surface of the can to control the hydrogen absorption and stress corrosion. Locallized stress due to fuel cladding interaction (PCMI) can also be moderated. (Horiuchi, T.)

  11. REACTOR CONTROL ROD OPERATING SYSTEM

    Science.gov (United States)

    Miller, G.

    1961-12-12

    A nuclear reactor control rod mechanism is designed which mechanically moves the control rods into and out of the core under normal conditions but rapidly forces the control rods into the core by catapultic action in the event of an emergency. (AEC)

  12. Control rod control device

    International Nuclear Information System (INIS)

    Seiji, Takehiko; Obara, Kohei; Yanagihashi, Kazumi

    1998-01-01

    The present invention provides a device suitable for switching of electric motors for driving each of control rods in a nuclear reactor. Namely, in a control rod controlling device, a plurality of previously allotted electric motors connected in parallel as groups, and electric motors of any selected group are driven. In this case, a voltage of not driving predetermined selected electric motors is at first applied. In this state an electric current supplied to the circuit of predetermined electric motors is detected. Whether integration or failure of a power source and the circuit of the predetermined electric motors are normal or not is judged by the detected electric current supplied. After they are judged normal, the electric motors are driven by a regular voltage. With such procedures, whether the selected circuit is normal or not can be accurately confirmed previously. Since the electric motors are not driven just at the selected time, the control rods are not operated erroneously. (I.S.)

  13. Control rod selecting and driving device

    International Nuclear Information System (INIS)

    Isobe, Hideo.

    1981-01-01

    Purpose: To simultaneously drive a predetermined number of control rods in a predetermined mode by the control of addresses for predetermined number of control rods and read or write of driving codified data to and from the memory by way of a memory controller. Constitution: The system comprises a control rod information selection device for selecting predetermined control rods from a plurality of control rods disposed in a reactor and outputting information for driving them in a predetermined mode, a control rod information output device for codifying the information outputted from the above device and outputting the addresses to the predetermined control rods and driving mode coded data, and a driving device for driving said predetermined control rods in a predetermined mode in accordance with the codified data outputted from the above device, said control rod infromation output device comprising a memory device capable of storing a predetermined number of the codified data and a memory control device for storing the predetermined number of data into the above memory device at a predetermined timing while successively outputting the thus stored predetermined number of data at a predetermined timing. (Seki, T.)

  14. Heat split imbalance study for annular fuel rod

    International Nuclear Information System (INIS)

    He Xiaojun; Ji Songtao; Zhang Yingchao

    2014-01-01

    Annular fuel rod has two gaps at inner and outer side. Under irradiation condition, the dimensional change of pellets is always larger than claddings' due to thermal expansion, swelling and densification, and this tends to enlarge the inner gap and reduce the outer gap. The gap size asymmetry must induce heat split imbalance problem that the heat flux will be larger at outer side of the rod. In this work, computer code AFPAC l.0 is used to simulate this heat split imbalance phenomena. The effect of initial gap size, rod inner pressure, roughness of pellets and cladding is studied, the results reveal that: l) Adjusting initial size of both gaps, reducing inner gap and enlarging outer gap could effectively alleviate heat split imbalance problem; 2) Adjusting the initial roughness of pellets and cladding is another effective approach to reducing heat split imbalance; 3) It seems that changing the rod inner pressure has a little effect on solving the heat flux asymmetry problem. (authors)

  15. Control rod drives

    International Nuclear Information System (INIS)

    Asano, Hiromitsu.

    1979-01-01

    Purpose: To drive control rods at an optimum safety speed corresponding to the reactor core output. Constitution: The reactor power is detected by a neutron detector and the output signal is applied to a process computer. The process computer issues a signal representing the reactor core output, which is converted through a function generator into a signal representing the safety speed of control rods. The converted signal is further supplied to a V/F converter and converted into a pulse signal. The pulse signal is inputted to a step motor driving circuit, which actuates a step motor to operate the control rods always at a safety speed corresponding to the reactor core power. (Furukawa, Y.)

  16. Fuel rod failure detection method and system

    International Nuclear Information System (INIS)

    Assmann, H.; Janson, W.; Stehle, H.; Wahode, P.

    1975-01-01

    The inventor claims a method for the detection of a defective fuel rod cladding tube or of inleaked water in the cladding tube of a fuel rod in the fuel assembly of a pressurized-water reactor. The fuel assembly is not disassembled but examined as a whole. In the examination, the cladding tube is heated near one of its two end plugs, e.g. with an attached high-frequency inductor. The water contained in the cladding tube evaporates, and steam bubbles or a condensate are detected by the ultrasonic impulse-echo method. It is also possible to measure the delay of the temperature rise at the end plug or to determine the cooling energy required to keep the end plug temperature stable and thus to detect water ingression. (DG/AK) [de

  17. In-cell facility for performing mechanical-property tests on irradiated cladding

    International Nuclear Information System (INIS)

    Yaggee, F.L.; Haglund, R.C.; Mattas, R.F.

    1978-11-01

    A new facility was developed for testing cladding sections of LWR fuel rods. This facility and the accompanying test procedures have improved the level of in-cell mechanical-testing capabilities, making them comparable to existing capabilities for unirradiated cladding. The new facility is currently being used to study the susceptibility of irradiated Zircaloy cladding from LWR fuel rods to iodine stress-corrosion cracking. Preliminary testing results indicate a systematic effect of temperature, stress and irradiation on the susceptibility of annealed and stress-relieved Zircaloy-2. Experimental data obtained to date are being used to develop a stress-corrosion cracking model for LWR fuel rod failure. SEM examination of the undisturbed fracture surface of specimens that failed by pinhole leakage provides useful information on crack propagation and morphology

  18. Potential impacts of crud deposits on fuel rod behaviour on high powered PWR fuel rods

    International Nuclear Information System (INIS)

    Wilson, W.; Comstock, R.J.

    1999-01-01

    Fuel assemblies operating with significant sub-cooled boiling are subject to deposition of surface deposits commonly referred to as crud. This crud can potentially cause concentration of chemical species within the deposits which can be detrimental to cladding performance in PWRs. In addition, these deposits on the surface of the cladding can result in power anomalies and erroneous reporting of fuel rod oxide thickness which can substantially hamper corrosion and core performance modeling efforts. Data is presented which illustrates the importance of accounting for the presence of crud on fuel cladding surfaces. Several methods used to correct for this phenomenon when collecting and analyzing zirconium alloy field oxide thickness measurements are described. Various observations related to crud characteristics and its impact on fuel rod performance are also addressed. (author)

  19. End-of-life destructive examination of light water breeder reactor fuel rods (LWBR Development Program)

    International Nuclear Information System (INIS)

    Richardson, K.D.

    1987-10-01

    Destructive examination of 12 representative Light Water Breeder Reactor fuel rods was performed following successful operation in the Shippingport Atomic Power Station for 29,047 effective full power hours, about five years. Light Water Breeder Reactor fuel rods were unique in that the thorium oxide and uranium-233 oxide fuel was contained within Zircaloy-4 cladding. Destructive examinations included analysis of released fission gas; chemical analysis of the fuel to determine depletion, iodine, and cesium levels; chemical analysis of the cladding to determine hydrogen, iodine, and cesium levels; metallographic examination of the cladding, fuel, and other rod components to determine microstructural features and cladding corrosion features; and tensile testing of the irradiated cladding to determine mechanical strength. The examinations confirmed that Light Water Breeder Reactor fuel rod performance was excellent. No evidence of fuel rod failure was observed, and the fuel operating temperature was low (below 2580 0 F at which an increased percentage of fission gas is released). 21 refs., 80 figs., 20 tabs

  20. The effect of mechanical restraint on the deformation of Zircaloy cladding

    International Nuclear Information System (INIS)

    Jones, P.M.; Haste, T.J.

    1980-10-01

    Zircaloy cladding, deformed at temperatures postulated for loss-of-coolant accidents, can exhibit considerable ductility. The actual circumferential strain is governed by the temperature uniformity around the rod during the time at which the major part of the deformation occurs. If the bulges in neighbouring rods in a multi-rod array touch before rupture, and the array is large enough for the outer rods to restrain bulges rather than be pushed away by them, then the stress in such bulges drops. However the stress in adjacent axial regions of the cladding which have not contacted remains high and these continue to strain until they also interact, thus propagating the bulging axially. Meanwhile the non-contacted portions of the interacting bulges continue to strain slowly into the remaining sub-channels. Illustrative calculations suggest that the mechanical restraint of bulging cladding will only be effective in increasing sub-channel blockage when the failure strains are greater than 60-70%. This may occur with temperature differences between neighbouring rods of 10-25 0 C if the deformation process is thermally stabilised. (author)

  1. Examination of Zircaloy-clad spent fuel after extended pool storage

    International Nuclear Information System (INIS)

    Bradley, E.R.; Bailey, W.J.; Johnson, A.B. Jr.; Lowry, L.M.

    1981-09-01

    This report presents the results from metallurgical examinations of Zircaloy-clad fuel rods from two bundles (0551 and 0074) of Shippingport PWR Core 1 blanket fuel after extended water storage. Both bundles were exposed to water in the reactor from late 1957 until discharge. The estimated average burnups were 346 GJ/kgU (4000 MWd/MTU) for bundle 0551 and 1550 GJ/kgU (18,000 MWd/MTU) for bundle 0074. Fuel rods from bundle 0551 were stored in deionized water for nearly 21 yr prior to examination in 1980, representing the world's oldest pool-stored Zircaloy-clad fuel. Bundle 0074 has been stored in deionized water since reactor discharge in 1964. Data from the current metallurgical examinations enable a direct assessment of extended pool storage effects because the metallurgical condition of similar fuel rods was investigated and documented soon after reactor discharge. Data from current and past examinations were compared, and no significant degradation of the Zircaloy cladding was indicated after almost 21 yr in water storage. The cladding dimensions and mechanical properties, fission gas release, hydrogen contents of the cladding, and external oxide film thicknesses that were measured during the current examinations were all within the range of measurements made on fuel bundles soon after reactor discharge. The appearance of the external surfaces and the microstructures of the fuel and cladding were also similar to those reported previously. In addition, no evidence of accelerated corrosion or hydride redistribution in the cladding was observed

  2. Process and apparatus for controlling control rods

    International Nuclear Information System (INIS)

    Gebelin, B.; Couture, R.

    1987-01-01

    This process and apparatus is characterized by 2 methods, for examination of cluster of nuclear control rods. Foucault current analyzer which examines fraction by fraction all the control rods. This examination is made by rotation of the cluster. Doubtful rods are then analysed by ultrasonic probe [fr

  3. Fuel cladding tube and fuel rod for BWR type reactor

    International Nuclear Information System (INIS)

    Urata, Megumu; Mitani, Shinji.

    1995-01-01

    A fuel cladding tube has grooves fabricated, on the surface thereof, with a predetermined difference between crest and bottom (depth of the groove) in the circumferential direction. The cross sectional shape thereof is sinusoidal. The distribution of the grain size of iron crud particles in coolants is within a range about from 2μm to 12μm. If the surface roughness of the fuel cladding tube (depth of the groove) is determined greater than 1.6μm and less than 12.5, iron cruds in coolants can be positively deposited on the surface of the fuel cladding tube. In addition, once deposited iron cruds can be prevented from peeling from the surface of the fuel cladding tube. With such procedures, iron cruds deposited and radioactivated on the fuel cladding tube can be prevented from peeling, to prevent and reduce the increase of radiation dose on the surface of the pipelines without providing any additional device. (I.N.)

  4. Analysis of the Behavior of CAREM-25 Fuel Rods Using Computer Code BACO

    International Nuclear Information System (INIS)

    Estevez, Esteban; Markiewicz, Mario; Marino, Armando

    2000-01-01

    The thermo-mechanical behavior of a fuel rod subjected to irradiation is a complex process, on which a great quantity of interrelated physical-chemical phenomena are coupled.The code BACO simulates the thermo-mechanical behavior and the evolution of fission gases of a cylindrical rod in operation.The power history of fuel rods, arising from neutronic calculations, is the program input.The code calculates, among others, the temperature distribution and the principal stresses in the pellet and cladding, changes in the porosity and restructuring of pellet, the fission gases release, evolution of the internal gas pressure.In this work some of design limits of CAREM-25's fuel rods are analyzed by means of the computer code BACO.The main variables directly related with the integrity of the fuel rod are: Maximum temperature of pellet; Cladding hoop stresses; Gases pressure in the fuel rod; Cladding axial and radial strains, etc.The analysis of results indicates that, under normal operation conditions, the maximum fuel pellet temperature, cladding stresses, pressure of gases at end of life, etc, are below the design limits considered for the fuel rod of CAREM-25 reactor

  5. Control rod position detection device

    International Nuclear Information System (INIS)

    Akita, Haruo; Ogiwara, Sakae.

    1996-01-01

    The device of the present invention is used in a back-up shut down system of an LMFBR type reactor which is easy for maintenance, has high reliability and can recognize the position of control rods accurately. Namely, a permanent magnet is disposed to a control rod extension tube connected to the lower portion of the control rod. The detector guide tube is disposed in the vicinity of the control rod extension tube. A detector having a detection coil is inserted into a detector tube. With such constitution, the control rod can be detected at one position using the following method. (1) the movement of the magnetic field of the permanent magnet is detected by the detection coil. (2) a plurality of grooves are formed on the control rod extension tube, and the movement of the grooves is detected. In addition, the detection coil is inserted into the detector guide tube, and the signals from the detection coil are inputted to a signal processing circuit disposed at the outside of the reactor vessel using an MI cable to enable the maintenance of the detector. Further, if the detector comprises a detection coil and an excitation coil, the position of a dropped control rod can be recognized at a plurality of points. (I.S.)

  6. Modelling the gas transport and chemical processes related to clad oxidation and hydriding

    Energy Technology Data Exchange (ETDEWEB)

    Montgomery, R O; Rashid, Y R [ANATECH Research Corp., San Diego, CA (United States)

    1997-08-01

    Models are developed for the gas transport and chemical processes associated with the ingress of steam into a LWR fuel rod through a small defect. These models are used to determine the cladding regions in a defective fuel rod which are susceptible to massive hydriding and the creation of sunburst hydrides. The brittle nature of zirconium hydrides (ZrH{sub 2}) in these susceptible regions produces weak spots in the cladding which can act as initiation sites for cladding cracks under certain cladding stress conditions caused by fuel cladding mechanical interaction. The modeling of the axial gas transport is based on gaseous bimolar diffusion coupled with convective mass transport using the mass continuity equation. Hydrogen production is considered from steam reaction with cladding inner surface, fission products and internal components. Eventually, the production of hydrogen and its diffusion along the length results in high hydrogen concentration in locations remote from the primary defect. Under these conditions, the hydrogen can attack the cladding inner surface and breakdown the protective ZrO{sub 2} layer locally, initiating massive localized hydriding leading to sunburst hydride. The developed hydrogen evolution model is combined with a general purpose fuel behavior program to integrate the effects of power and burnup into the hydriding kinetics. Only in this manner can the behavior of a defected fuel rod be modeled to determine the conditions the result in fuel rod degradation. (author). 14 refs, 6 figs.

  7. 3D Finite Element Simulation of Pellet-Cladding Mechanical Interaction

    International Nuclear Information System (INIS)

    Seo, Sang Kyu; Lee, Sung Uk; Lee, Eun Ho; Yang, Dong Yol; Kim, Hyo Chan; Yang, Dong Yol

    2016-01-01

    In a nuclear power plant, the fuel assembly, which is composed of fuel rods, burns, and the high temperature can generate power. The fuel rod consists of pellets and a cladding that covers the pellets. It is important to understand the pellet-cladding mechanical interaction with regard to nuclear safety. This paper proposes simulation of the PCMI. The gap between the pellets and the cladding, and the contact pressure are very important for conducting thermal analysis. Since the gap conductance is not known, it has to be determined by a suitable method. This paper suggests a solution. In this study, finite element (FE) contact analysis is conducted considering thermal expansion of the pellets. As the contact causes plastic deformation, this aspect is considered in the analysis. A 3D FE module is developed to analyze the PCMI using FORTRAN 90. The plastic deformation due to the contact between the pellets and the cladding is the major physical phenomenon. The simple analytical solution of a cylinder is proposed and compared with the fuel rod performance code results

  8. Cladding For Transversely-Pumped Laser Rod

    Science.gov (United States)

    Byer, Robert L.; Fan, Tso Yee

    1989-01-01

    Combination of suitable dimensioning and cladding of neodymium:yttrium aluminum garnet of similar solid-state laser provides for more efficient utilization of transversely-incident pump light from diode lasers. New design overcomes some of limitations of longitudinal- and older transverse-pumping concepts and promotes operation at higher output powers in TEM00 mode.

  9. Inspecting method for fuel rods

    International Nuclear Information System (INIS)

    Watanabe, Masaaki; Kogure, Sumio.

    1976-01-01

    Purpose: To precisely detect the response of flaw in clad tube and submerged fuel pellets from a relationship between the surface of fuel rod and internal signal. Constitution: Ultrasonic reflected waves from the surface of fuel rods and the interior are detected and either one of fuel rod or ultrasonic flaw detecting contact is rotated to thereby precisely detect the response of the flaw of clad tube and submerged fuel pellets from a relationship between said surface and the interior. It will be noted that the ultrasonic flaw detecting contact used is of the line-focus type, the incident angle of ultrasonic wave from the ultrasonic flaw detecting contact relative to the fuel rod is the angle of skew, that is, the ultrasonic flaw detecting contact is not perpendicular to a center axis of the fuel rod but is slightly displace. That is, the use of the aforesaid contact may facilitate discrimination between the surface flaw of the fuel rod and the response of submergence, and in addition, the employment of the aforesaid incident angle makes it hard to receive reflected waves from the surface of the fuel rod which is great in terms of energy to facilitate discrimination of waves responsive to submergence. (Kawakami, Y.)

  10. Control rod drives

    International Nuclear Information System (INIS)

    Ikakura, Hiroaki.

    1986-01-01

    Purpose: To enable to direct disconnection of control rods upon abnormal temperature rise in the reactor thereby improve the reliability for the disconnecting operation in control rod drives for FBR type reactors upon emergency. Constitution: A diaphragm is disposed to the upper opening of a sealing vessel inserted to the hollow portion of an electromagnet and a rod is secured to the central position of the upper surface. A spring contacts are attached by way of an insulator to the inner surface at the lower portion of an extension pipe and connected with cables for supplying electric power sources respectively to a magnet. If the temperature in the reactor abnormally rises, liquid metals in the sealing vessel are expanded tending to extend the bellows downwardly. However, since they are attracted by the electromagnet, the thermal expansion of the liquid metals exert on the diaphragm prior to the bellows. Thus, the switch between the spring contacts is made open to attain the deenergized state to thereby disconnect the control rod and shutdown the neclear reactor. (Horiuchi, T.)

  11. Control rod testing apparatus

    International Nuclear Information System (INIS)

    Gaunt, R.R.; Ashman, C.M.

    1987-01-01

    A control rod testing apparatus is described comprising: a first guide means having a vertical cylindrical opening for grossly guiding a control rod; a second guide means having a vertical cylindrical opening for grossly guiding a control rod. The first and second guide means are supported at axially spaced locations with the openings coaxial; and a substantially cylindrical subassembly having a vertical cylindrical opening therethrough. The subassembly is trapped coaxial with and between the first and second guide means, and the subassembly radially floats with respect to the first and second guide means

  12. Measuring device for control rod driving time

    International Nuclear Information System (INIS)

    Tanaka, Kazuhiko; Hanabusa, Masatoshi.

    1993-01-01

    The present invention concerns a measuring device for control driving time having a function capable of measuring a selected control rod driving time and measuring an entire control rod driving time simultaneously. A calculation means and a store means for the selected rod control rod driving time, and a calculation means and a store means for the entire control rod driving time are disposed individually. Each of them measures the driving time and stores the data independent of each other based on a selected control rod insert ion signal and an entire control rod insertion signal. Even if insertion of selected and entire control rods overlaps, each of the control rod driving times can be measured reliably to provide an advantageous effect capable of more accurately conducting safety evaluation for the nuclear reactor based on the result of the measurement. (N.H.)

  13. Estimation of penetration depth of fission products in cladding Hull

    International Nuclear Information System (INIS)

    Kim, Hee Moon; Jung, Yang Hong; Yoo, Byong Ok; Choo, Yong Sun; Hong, Kwon Pyo

    2005-01-01

    A disposal and a reprocessing for spent fuel rod with high burnup need de-cladding procedure. Pellet in this rod has been separated from a cladding hull to reduce a radioactivity of hull by chemical and mechanical methods. But fission products and actinides(U,Pu) still remain inside of cladding hull by chemical bonding and fission spike, which is called as 'contamination'. More specific removal of this contamination would have been considered. In this study, the sorts of fission products and penetration depth in hull were observed by EPMA test. To analyze this behavior, SRIM 2000 code was also used as energies of fission products and an oxide thickness of hull

  14. FRAPCON-2: A Computer Code for the Calculation of Steady State Thermal-Mechanical Behavior of Oxide Fuel Rods

    Energy Technology Data Exchange (ETDEWEB)

    Berna, G. A; Bohn, M. P.; Rausch, W. N.; Williford, R. E.; Lanning, D. D.

    1981-01-01

    FRAPCON-2 is a FORTRAN IV computer code that calculates the steady state response of light Mater reactor fuel rods during long-term burnup. The code calculates the temperature, pressure, deformation, and tai lure histories of a fuel rod as functions of time-dependent fuel rod power and coolant boundary conditions. The phenomena modeled by the code include (a) heat conduction through the fuel and cladding, (b) cladding elastic and plastic deformation, (c) fuel-cladding mechanical interaction, (d) fission gas release, (e} fuel rod internal gas pressure, (f) heat transfer between fuel and cladding, (g) cladding oxidation, and (h) heat transfer from cladding to coolant. The code contains necessary material properties, water properties, and heat transfer correlations. FRAPCON-2 is programmed for use on the CDC Cyber 175 and 176 computers. The FRAPCON-2 code Is designed to generate initial conditions for transient fuel rod analysis by either the FRAP-T6 computer code or the thermal-hydraulic code, RELAP4/MOD7 Version 2.

  15. Monitoring device for withdrawing control rods

    International Nuclear Information System (INIS)

    Higashigawa, Yuichi.

    1985-01-01

    Purpose: To improve the sensitivity and the responsivity to an equivalent extent to those in the case where local power range monitors are densely arranged near each of the control rods, with no actual but pseudo increase of the number of local power range monitors. Constitution: The monitor arrangement is patterned by utilizing the symmetricity of the reactor core and stored in a monitor designating device. The symmetricity of control rods to be selected and withdrawn by an operator is judged by a control rod symmetry monitoring device, while the symmetricity of the withdrawn control rods is judged by a control rod withdrawal state monitoring device. Then, only when both of the devices judge the symmetricity, the control rods are subjected to gang driving by the control rod drive mechanisms. In this way, monitoring at a high sensitivity and responsivity is enabled with no increase for the number of monitors. (Yoshino, Y.)

  16. Rope wind-up type control rod

    International Nuclear Information System (INIS)

    Tsuji, Teruaki; Watanabe, Shigeru.

    1979-01-01

    Purpose: To hold a control rod at a certain position even if the sealed cover of the rod drive mechanism should fail. Constitution: A plurality of friction plates, engaging wheels and a threaded shaft are provided to the wind-up drum for winding up a rope which moves the control rod up and down. While the control rod is adapted to drop by its own weight upon insertion, it is adapted to stop at a predetermined position exactly with no shocks by gradually increasing braking force by the sliding friction caused from the friction plates or the like. A ratch mechanism is provided to the upper portion of the control rod so that the top of the ratch piece may automatically engage the guide passage wall of the control rod upon uncontrolled running of the control rod to prevent further uncontrolled running thereof. (Ikeda, J.)

  17. Control rod drive shaft latch

    International Nuclear Information System (INIS)

    Thorp, A.G. II.

    1976-01-01

    A latch mechanism is operated by differential pressure on a piston to engage the drive shaft for a control rod in a nuclear reactor, thereby preventing the control rod from being ejected from the reactor in case of failure of the control rod drive mechanism housing which is subjected to the internal pressure in the reactor vessel. 6 claims, 4 drawing figures

  18. A comparison of thermal algorithms of fuel rod performance code systems

    International Nuclear Information System (INIS)

    Park, C. J.; Park, J. H.; Kang, K. H.; Ryu, H. J.; Moon, J. S.; Jeong, I. H.; Lee, C. Y.; Song, K. C.

    2003-11-01

    The goal of the fuel rod performance is to identify the robustness of a fuel rod with cladding material. Computer simulation of the fuel rod performance becomes one of important parts to designed and evaluate new nuclear fuels and claddings. To construct a computing code system for the fuel rod performance, several algorithms of the existing fuel rod performance code systems are compared and are summarized as a preliminary work. Among several code systems, FRAPCON, and FEMAXI for LWR, ELESTRES for CANDU reactor, and LIFE for fast reactor are reviewed. Thermal algorithms of the above codes are investigated including methodologies and subroutines. This work will be utilized to construct a computing code system for dry process fuel rod performance

  19. A comparison of thermal algorithms of fuel rod performance code systems

    Energy Technology Data Exchange (ETDEWEB)

    Park, C. J.; Park, J. H.; Kang, K. H.; Ryu, H. J.; Moon, J. S.; Jeong, I. H.; Lee, C. Y.; Song, K. C

    2003-11-01

    The goal of the fuel rod performance is to identify the robustness of a fuel rod with cladding material. Computer simulation of the fuel rod performance becomes one of important parts to designed and evaluate new nuclear fuels and claddings. To construct a computing code system for the fuel rod performance, several algorithms of the existing fuel rod performance code systems are compared and are summarized as a preliminary work. Among several code systems, FRAPCON, and FEMAXI for LWR, ELESTRES for CANDU reactor, and LIFE for fast reactor are reviewed. Thermal algorithms of the above codes are investigated including methodologies and subroutines. This work will be utilized to construct a computing code system for dry process fuel rod performance.

  20. Development of the automatic control rod operation system for JOYO. Verification of automatic control rod operation guide system

    International Nuclear Information System (INIS)

    Terakado, Tsuguo; Suzuki, Shinya; Kawai, Masashi; Aoki, Hiroshi; Ohkubo, Toshiyuki

    1999-10-01

    The automatic control rod operation system was developed to control the JOYO reactor power automatically in all operation modes(critical approach, cooling system heat up, power ascent, power descent), development began in 1989. Prior to applying the system, verification tests of the automatic control rod operation guide system was conducted during 32nd duty cycles of JOYO' from Dec. 1997 to Feb. 1998. The automatic control rod operation guide system consists of the control rod operation guide function and the plant operation guide function. The control rod operation guide function provides information on control rod movement and position, while the plant operation guide function provide guidance for plant operations corresponding to reactor power changes(power ascent or power descent). Control rod insertion or withdrawing are predicted by fuzzy algorithms. (J.P.N.)

  1. Damage and failure of unirradiated and irradiated fuel rods tested under film boiling conditions

    International Nuclear Information System (INIS)

    Mehner, A.S.; Hobbins, R.R.; Seiffert, S.L.; MacDonald, P.E.; McCardell, R.K.

    1979-01-01

    Power-cooling-mismatch experiments are being conducted as part of the Thermal Fuels Behavior Program in the Power Burst Facility at the Idaho National Engineering Laboratory to evaluate the behavior of unirradiated and previously irradiated light water reactor fuel rods tested under stable film boiling conditions. The observed damage that occurs to the fuel rod cladding and the fuel as a result of film boiling operation is reported. Analyses performed as a part of the study on the effects of operating failed fuel rods in film boiling, and rod failure mechanisms due to cladding embrittlement and cladding melting upon being contacted by molten fuel are summarized

  2. Control rod excess withdrawal prevention device

    International Nuclear Information System (INIS)

    Takayama, Yoshihito.

    1992-01-01

    Excess withdrawal of a control rod of a BWR type reactor is prevented. That is, the device comprises (1) a speed detector for detecting the driving speed of a control rod, (2) a judging circuit for outputting an abnormal signal if the driving speed is greater than a predetermined level and (3) a direction control valve compulsory closing circuit for controlling the driving direction of inserting and withdrawing a control rod based on an abnormal signal. With such a constitution, when the with drawing speed of a control rod is greater than a predetermined level, it is detected by the speed detector and the judging circuit. Then, all of the direction control valve are closed by way of the direction control valve compulsory closing circuit. As a result, the operation of the control rod is stopped compulsorily and the withdrawing speed of the control rod can be lowered to a speed corresponding to that upon gravitational withdrawal. Accordingly, excess withdrawal can be prevented. (I.S)

  3. Rod consolidation of RG and E's [Rochester Gas and Electric Corporation] spent PWR [pressurized water reactor] fuel

    International Nuclear Information System (INIS)

    Bailey, W.J.

    1987-05-01

    The rod consolidation demonstration involved pulling the fuel rods from five fuel assemblies from Unit 1 of RG and E's R.E. Ginna Nuclear Power Plant. Slow and careful rod pulling efforts were used for the first and second fuel assemblies. Rod pulling then proceeded smoothly and rapidly after some minor modifications were made to the UST and D consolidation equipment. The compaction ratios attained ranged from 1.85 to 2.00 (rods with collapsed cladding were replaced by dummy rods in one fuel assembly to demonstrate the 2:1 compaction ratio capability). This demonstration involved 895 PWR fuel rods, among which there were some known defective rods (over 50 had collapsed cladding); no rods were broken or dropped during the demonstration. However, one of the rods with collapsed cladding unexplainably broke during handling operations (i.e., reconfiguration in the failed fuel canister), subsequent to the rod consolidation demonstration. The broken rod created no facility problems; the pieces were encapsulated for subsequent storage. Another broken rod was found during postdemonstration cutting operations on the nonfuel-bearing structural components from the five assemblies; evidence indicates it was broken prior to any rod consolidation operations. During the demonstration, burnish-type lines or scratches were visible on the rods that were pulled; however, experience indicates that such lines are generally produced when rods are pulled (or pushed) through the spacer grids. Rods with collapsed cladding would not enter the funnel (the transition device between the fuel assembly and the canister that aids in obtaining high compaction ratios). Reforming of the flattened areas of the cladding on those rods was attempted to make the rod cross sections more nearly circular; some of the reformed rods passed through the funnel and into the canister

  4. NEUTRONIC REACTOR CONTROL ROD DRIVE APPARATUS

    Science.gov (United States)

    Oakes, L.C.; Walker, C.S.

    1959-12-15

    ABS>A suspension mechanism between a vertically movable nuclear reactor control rod and a rod extension, which also provides information for the operator or an automatic control signal, is described. A spring connects the rod extension to a drive shift. The extension of the spring indicates whether (1) the rod is at rest on the reactor, (2) the rod and extension are suspended, or (3) the extension alone is suspended, the spring controlling a 3-position electrical switch.

  5. Mechanical and temperature contact in fuel rod cladding

    International Nuclear Information System (INIS)

    Fredriksson, B.E.; Rydholm, S.G.

    1977-01-01

    The paper presents results for the effect of different types of slip rules on the contact stress distribution. It is shown that the contact shear stress is smaller for the hardening model than for the ideal model. It is also shown that a crack in the fuel increases the contact stresses and that at temperature decrease high tensile stresses arise after eventual welding. It is also shown how particles between fuel and cladding influence the stresses. Also here the effect of eventual welding is studied. The present method is well suited to study cracks and crack propagation. The surfaces of the existing cracks are defined as contact surfaces and the crack extension work is calculated by releasing the nodes at the crack tip. As the crack surfaces are defined as contact surfaces eventual crack closure is automatically taken into account. Crack extension work is calculated for existing cracks in the cladding. It is shown that cracks in the fuel and particles between fuel and cladding will increase the crack extension work

  6. Seismic scrammability of HTTR control rods

    International Nuclear Information System (INIS)

    Nishiguchi, I.; Iyoku, T.; Ito, N.; Watanabe, Y.; Araki, T.; Katagiri, S.

    1990-01-01

    Scrammability tests on HTTR (High-Temperature Engineering Test Reactor) control rods under seismic conditions have been carried out and seismic conditions influences on scram time as well as functional integrity were examined. A control rod drive located in a stand-pipe at the top of a reactor vessel, raises and lowers a pair of control rods by suspension cables. Each flexible control rod consists of 10 neutron absorber sections held together by a metal spine passing through the center. It falls into a hole in graphite blocks due to gravity at scram. In the tests, a full scale control rod drive and a pair of control rods were employed with a column of graphite blocks in which holes for rods were formed. Blocks misalignment and contact with the hole surface during earthquakes were considered as major causes of disturbance in scram time. Therefore, the following parameters were set up in the tests: excitation direction, combination or horizontal and vertical excitation, acceleration, frequency and block to block gaps. Main results obtained from tests are as follow. 1) Every scram time obtained under the design conditions was within 6 seconds. On the contrary, the scram times were 5.2 seconds when there were no vibration. Therefore, it was concluded that the seismic effects on scram time were not significant. 2) Scram time became longer with increase in both acceleration and horizontal excitation frequency, and control rods fell very smoothly without any jerkiness. This suggests that collision between control rods and hole surface is the main disturbing factor of falling motion. 3) Mechanical and functional integrity of control rod drive mechanism, control rods and graphite blocks was confirmed after 140 seismic scrammability tests. (author). 10 figs, 1 tab

  7. B4C control rod behavior during severe accident sequences

    International Nuclear Information System (INIS)

    Steinbrueck, M.

    2003-01-01

    The oxidation kinetics of various types of boron carbides (pellets, powder) as well as the degradation of B 4 C control rod segments were investigated in the temperature range between 800 and 1600 deg C. Mass spectrometric gas analysis was used to determine oxidation rates in transient and isothermal tests. The oxidation kinetics of boron carbide are determined by the formation of a liquid boron oxide layer and its loss due to the reaction with surplus steam to form volatile boric acids and at temperatures above 1500 deg C by direct evaporation. Under these test conditions linear oxidation kinetics are established soon after oxidation has initiated. The oxidation kinetics are strongly influenced by the thermal-hydraulic boundary conditions, in particular by the steam flow rate. Only very low amounts of methane were ever produced in these tests. Enhanced degradation of B 4 C control rods starts with the rapid formation of eutectic melts in the systems B 4 C-stainless steel (SS) and SS-Zircaloy at temperatures above 1250 deg C. Initially, this melt is kept within a ZrO 2 scale externally formed at the Zircaloy guide tube. The absorber melt is rapidly oxidized after failure of the oxide shell and aggressively attacks adjacent fuel claddings. (author)

  8. Control rod

    International Nuclear Information System (INIS)

    Fukumoto, Takashi; Hirakawa, Hiromasa; Kawashima, Norio; Goto, Yasuyuki.

    1994-01-01

    Neutron absorbers are contained in a tubular member comprising, integrally a tubular portion and four corners disposed at the outer circumference of the tubular portion at every 90deg, to provide a neutron absorbing tube. A plurality of neutron absorbing tubes are arranged in parallel in the lateral direction, and adjacent corners are joined, into a blade to constitute a control rod. Such a control rod has a great structural strength, simple in the structure and relatively light in weight and can contain a great amount of neutron absorbers. Upon formation of the control rod by arranging the blades in a cross-like shape, at least a portion thereof is constituted with short neutron absorbing tubes shorter than the entire length of the blade, and gaps are formed at positions in adjacent in the axial direction. With such a constitution, there is no worry that a wing end of the blade collides against or be abraded with a fuel channel box or a fuel support. Even if fuel channels are vibrated upon scram of the reactor, such as occurrence of earthquakes, it can be inserted to the reactor easily. (N.H.)

  9. Multidimensional simulations of hydrides during fuel rod lifecycle

    International Nuclear Information System (INIS)

    Stafford, D.S.

    2015-01-01

    In light water reactor fuel rods, waterside corrosion of zirconium-alloy cladding introduces hydrogen into the cladding, where it is slightly soluble. When the solubility limit is reached, the hydrogen precipitates into crystals of zirconium hydride which decrease the ductility of the cladding and may lead to cladding failure during dry storage or transportation events. The distribution of the hydride phase and the orientation of the crystals depend on the history of the spatial temperature and stress profiles in the cladding. In this work, we have expanded the existing hydride modeling capability in the BISON fuel performance code with the goal of predicting both global and local effects on the radial, azimuthal and axial distribution of the hydride phase. We compare results from 1D simulations to published experimental data. We demonstrate the new capability by simulating in 2D a fuel rod throughout a lifecycle that includes irradiation, short-term storage in the spent fuel pool, drying, and interim storage in a dry cask. Using the 2D simulations, we present qualitative predictions of the effects of the inter-pellet gap and the drying conditions on the growth of a hydride rim. - Highlights: • We extend BISON fuel performance code to simulate lifecycle of fuel rods. • We model hydrogen evolution in cladding from reactor through dry storage. • We validate 1D simulations of hydrogen evolution against experiments. • We show results of 2D axisymmetric simulations predicting hydride formation. • We show how our model predicts formation of a hydride rim in the cladding.

  10. Simulation of fuel rod behaviour during various break LOCAs in PWRs

    International Nuclear Information System (INIS)

    Gadalla, A.A.; El-Fawal, M.M.

    1996-01-01

    During loss of coolant accident (LOCAs) course of events, attention focuses on fuel rod cladding temperature behaviour. In this study, the DRUFAN analytical model and LOBI-MOD2 experimental modeling scheme for fuel rod temperature behaviour during C L-Break LOCA in PWRs, are described and discussed. These models are applied for the investigation of fuel rod cladding temperature behaviour during LOCA blowdown phase. A spectrum of selected values representing small, intermediate and large CL- Break sizes are considered in the predictions. The results of the predictions demonstrated that calculated heater rod temperature at steady state as well as the transient period up to 1000 sec are going in good agreement with the measured values. However above 1000 sec the calculated temperatures are higher than the measured values. This indicates that code predictions in this period are conservative. The results indicated also that, in case of small CL-break LOCA (0.01 A and 0.01 and 0.03 A), the heater rod cladding temperature don't rise above saturation temperature. However, on the top of the heater rod, DNB is occurred in case of 0.03 A CL break, while for 0.01 A break, DNB didn't occur. In case of intermediate and large CL-break; (0.05 A, 0.10 A and 1 A), the results showed that, the heater rod cladding temperature exceeded the saturation temperature and DNB prevailed in upper and intermediate sections of the core. 15 figs., 2 tabs

  11. BISON Fuel Performance Analysis of FeCrAl cladding with updated properties

    Energy Technology Data Exchange (ETDEWEB)

    Sweet, Ryan [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States); George, Nathan M. [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States); Terrani, Kurt A. [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States); Wirth, Brian [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)

    2016-08-30

    In order to improve the accident tolerance of light water reactor (LWR) fuel, alternative cladding materials have been proposed to replace zirconium (Zr)-based alloys. Of these materials, there is a particular focus on iron-chromium-aluminum (FeCrAl) alloys due to much slower oxidation kinetics in high-temperature steam than Zr-alloys. This should decrease the energy release due to oxidation and allow the cladding to remain integral longer in the presence of high temperature steam, making accident mitigation more likely. As a continuation of the development for these alloys, suitability for normal operation must also be demonstrated. This research is focused on modeling the integral thermo-mechanical performance of FeCrAl-cladded fuel during normal reactor operation. Preliminary analysis has been performed to assess FeCrAl alloys (namely Alkrothal 720 and APMT) as a suitable fuel cladding replacement for Zr-alloys, using the MOOSE-based, finite-element fuel performance code BISON and the best available thermal-mechanical and irradiation-induced constitutive properties. These simulations identify the effects of the mechanical-stress and irradiation response of FeCrAl, and provide a comparison with Zr-alloys. In comparing these clad materials, fuel rods have been simulated for normal reactor operation and simple steady-state operation. Normal reactor operating conditions target the cladding performance over the rod lifetime (~4 cycles) for the highest-power rod in the highest-power fuel assembly under reactor power maneuvering. The power histories and axial temperature profiles input into BISON were generated from a neutronics study on full-core reactivity equivalence for FeCrAl using the 3D full core simulator NESTLE. Evolution of the FeCrAl cladding behavior over time is evaluated by using steady-state operating conditions such as a simple axial power profile, a constant cladding surface temperature, and a constant fuel power history. The fuel rod designs and

  12. Sensitivity Analysis of Gap Conductance for Heat Split in an Annular Fuel Rod

    International Nuclear Information System (INIS)

    Chun, Kun Ho; Chun, Tae Hyun; In, Wang Kee; Song, Keun Woo

    2006-01-01

    To increase of the core power density in the current PWR cores, an annular fuel rod was proposed by MIT. This annular fuel rod has two coolant channels and two cladding-pellet gaps unlike the current solid fuel rod. It's important to predict the heat split reasonably because it affects coolant enthalpy rise in each channel and Departure from Nuclear Boiling Ratio (DNBR) in each channel. Conversely, coolant conditions affect fuel temperature and heat split. In particular if the heat rate leans to either inner or outer channel, it is out of a thermal equilibrium. To control a thermal imbalance, placing another gap in the pellet is introduced. The heat flow distribution between internal and external channels as well as fuel and cladding temperature profiles is calculated with and without the fuel gap between the inner and outer pellets

  13. Status and development of RBMK fuel rods and reactor materials

    International Nuclear Information System (INIS)

    Bibilashvili, Yu.K.; Reshetnikov, F.G.; Ioltukhovsky, A.G.

    1998-01-01

    The paper presents current status and development of RBMK fuel rods and reactor materials. With regard to fuel rod cladding the following issues have been discussed: corrosion, tensile properties, welding technology and testing of an alternative cladding alloy with a composition of Zr-Nb-Sn-Fe. Erbium doped fuel has been suggested for safety improvement. Also analysis of fuel reliability is presented in the paper. (author)

  14. Hydraulic burst tests at elevated temperatures on Zircaloy cladding from fuel rods irradiated in the Winfrith SGHWR

    International Nuclear Information System (INIS)

    Garlick, A.; Hindmarch, P.

    1980-09-01

    Closed-end hydraulic burst tests have been carried out at 613K on lengths of cladding cut from fuel rods that had been irradiated in the SGHWR to 25 n/m 2 . The effects of reactor exposure on the mechanical properties of the Zircaloy cladding, initially in the stress-relieved and fully recrystallised conditions, have been evaluated from measurements of the 0.2% proof stress, the ultimate burst stress, the total circumferential elongation and the reduction in wall thickness at fracture. It is shown that after irradiation, the measured strength properties of stress-relieved cladding remained higher than for that in the fully recrystallised condition, although the large differences observed before irradiation were considerably reduced. The irradiation-induced increase in proof stress measured during these tests was compared with US results from uniaxial tensile tests and, after correcting for the effect of stress-ratio, it is concluded that close agreement exists between the two sets of data for Zircaloy in the fully recrystallised condition. In contrast, the agreement for stress-relieved Zircaloy is less good, although the maximum increase in proof stress after high neutron doses for this material is similar for data from the two sources. After irradiation, the ductility of fully recrystallised Zircaloy remained higher than that of stress-relieved material and there was no evidence to suggest that a serious loss of ductility had occurred for Zircaloy in either condition of heat-treatment as a result of reactor exposure. (author)

  15. Control rod housing alignment

    International Nuclear Information System (INIS)

    Dixon, R.C.; Deaver, G.A.; Punches, J.R.; Singleton, G.E.; Erbes, J.G.; Offer, H.P.

    1990-01-01

    This patent describes a process for measuring the vertical alignment between a hole in a core plate and the top of a corresponding control rod drive housing within a boiling water reactor. It comprises: providing an alignment apparatus. The alignment apparatus including a lower end for fitting to the top of the control rod drive housing; an upper end for fitting to the aperture in the core plate, and a leveling means attached to the alignment apparatus to read out the difference in angularity with respect to gravity, and alignment pin registering means for registering to the alignment pin on the core plate; lowering the alignment device on a depending support through a lattice position in the top guide through the hole in the core plate down into registered contact with the top of the control rod drive housing; registering the upper end to the sides of the hole in the core plate; registering the alignment pin registering means to an alignment pin on the core plate to impart to the alignment device the required angularity; and reading out the angle of the control rod drive housing with respect to the hole in the core plate through the leveling devices whereby the angularity of the top of the control rod drive housing with respect to the hole in the core plate can be determined

  16. Mechanical stress analysis for a fuel rod under normal operating conditions

    International Nuclear Information System (INIS)

    Pino, Eddy S.; Giovedi, Claudia; Serra, Andre da Silva; Abe, Alfredo Y.

    2013-01-01

    Nuclear reactor fuel elements consist mainly in a system of a nuclear fuel encapsulated by a cladding material subject to high fluxes of energetic neutrons, high operating temperatures, pressure systems, thermal gradients, heat fluxes and with chemical compatibility with the reactor coolant. The design of a nuclear reactor requires, among a set of activities, the evaluation of the structural integrity of the fuel rod submitted to different loads acting on the fuel rod and the specific properties (dimensions and mechanical and thermal properties) of the cladding material and coolant, including thermal and pressure gradients produced inside the rod due to the fuel burnup. In this work were evaluated the structural mechanical stresses of a fuel rod using stainless steel as cladding material and UO 2 with a low degree of enrichment as fuel pellet on a PWR (pressurized water reactor) under normal operating conditions. In this sense, tangential, radial and axial stress on internal and external cladding surfaces considering the orientations of 0 deg, 90 deg and 180 deg were considered. The obtained values were compared with the limit values for stress to the studied material. From the obtained results, it was possible to conclude that, under the expected normal reactor operation conditions, the integrity of the fuel rod can be maintained. (author)

  17. A novel contra propagating ultrasonic flowmeter using glad buffer rods for high temperature measurement. Application to the oil and gas industries

    Energy Technology Data Exchange (ETDEWEB)

    Franca, Demartonne R. [Brasilia Univ., DF (Brazil). Dept. de Engenharia Eletrica; Cheng-Kuei Jen; Yuu Ono [National Research Council (NRC), Quebec (Canada). Industrial Materials Institute

    2005-07-01

    Ultrasonic techniques are attractive for process monitoring and control because they are non-intrusive, robust and inexpensive. Two common concerns limiting the high temperature performance of conventional ultrasonic systems for flow measurement are related to transducers and couplants. A suitable approach to overcoming this drawback is to insert a thermal isolating buffer rod with good ultrasonic performance (e.g., high signal-to-noise ratio). This requirement is important because, a priori, the noises generated in the buffer rod may bury the desired signals, so that no meaningful information is extracted. Besides protecting the ultrasonic transducers from overheating in applications such as high temperature flow measurements, buffer rods are also a solution for the couplant between the probe and tested sample, since their probing end can be directly wetted by fluids. Here, we propose clad buffer rods driven by shear transducers as the main building block of contra propagating ultrasonic flowmeters for high temperature application. It is demonstrated that the superior signal-to-noise ratio exhibit by clad buffer rods compared to the reported non-clad counterparts improve precision in transit-time measurement, leading to more accurate flow speed determination. In addition, it is shown that clad buffer rods generate specific ultrasonic signals for temperature calibration of flowmeters, allowing temperature variation while still measuring accurately the flow speed. These results are of interest for the oil and gas industries. (author)

  18. Real-time laser cladding control with variable spot size

    Science.gov (United States)

    Arias, J. L.; Montealegre, M. A.; Vidal, F.; Rodríguez, J.; Mann, S.; Abels, P.; Motmans, F.

    2014-03-01

    Laser cladding processing has been used in different industries to improve the surface properties or to reconstruct damaged pieces. In order to cover areas considerably larger than the diameter of the laser beam, successive partially overlapping tracks are deposited. With no control over the process variables this conduces to an increase of the temperature, which could decrease mechanical properties of the laser cladded material. Commonly, the process is monitored and controlled by a PC using cameras, but this control suffers from a lack of speed caused by the image processing step. The aim of this work is to design and develop a FPGA-based laser cladding control system. This system is intended to modify the laser beam power according to the melt pool width, which is measured using a CMOS camera. All the control and monitoring tasks are carried out by a FPGA, taking advantage of its abundance of resources and speed of operation. The robustness of the image processing algorithm is assessed, as well as the control system performance. Laser power is decreased as substrate temperature increases, thus maintaining a constant clad width. This FPGA-based control system is integrated in an adaptive laser cladding system, which also includes an adaptive optical system that will control the laser focus distance on the fly. The whole system will constitute an efficient instrument for part repair with complex geometries and coating selective surfaces. This will be a significant step forward into the total industrial implementation of an automated industrial laser cladding process.

  19. Investigation of control rod worth and nuclear end of life of BWR control rods

    International Nuclear Information System (INIS)

    Magnusson, Per

    2008-01-01

    This work has investigated the Control Rod Worth (CRW) and Nuclear End of Life (NEOL) values for BWR control rods. A study of how different parameters affect NEOL was performed with the transport code PHOENIX4. It was found that NEOL, expressed in terms of 10 B depletion, can be generalized beyond the conditions for which the rod is depleted, such as different power densities and void fractions, the corresponding variation in the NEOL will be about 0.2-0.4% 10 B. It was also found that NEOL results for different fuel types and different fuel enrichments have a variation of about 2-3% in 10 B depletion. A comparative study on NHOL and CRW was made between PHOENIX4 and the stochastic Monte Carlo code MCNP. It was found that there is a significant difference, both due to differences in the codes and to limitations in the geometrical modeling in PHOENIX4. Since MCNP is considered more physically correct, a methodology was developed to calculate the nuclear end of life of BWR control rods with MCNP. The advantages of the methodology are that it does not require other codes to perform the depletion of the absorber material, it can describe control rods of any design and it can deplete the control rod absorber material without burning the fuel. The disadvantage of the method is that is it time-consuming

  20. A study of friction and axial effects in pellet-clad mechanical interaction

    International Nuclear Information System (INIS)

    Harriague, Santiago; Mayer, J.E.

    1982-01-01

    An analysis is made of the effect of friction and axial forces along the fuel rod in the pellet-cladding mechanical interaction in a commercial reactor under a power-up ramp. The effect of different pellet and rod shapes on their behaviour was also determined. A linear thermoelastic computer program was used in order to obtain the stiffness matrix of a compound structure from the stiffness of its components. Pellet-cladding displacements, localized deformations of the cladding in the interfaces between pellets, as well as pellet and cladding axial deformations were determined for different power axial profiles as well as for pellets with and without dishing and with height/diameter ratios of 1.7, 1 and 0.5. (M.E.L.) [es

  1. Zirconium-barrier cladding attributes

    International Nuclear Information System (INIS)

    Rosenbaum, H.S.; Rand, R.A.; Tucker, R.P.; Cheng, B.; Adamson, R.B.; Davies, J.H.; Armijo, J.S.; Wisner, S.B.

    1987-01-01

    This metallurgical study of Zr-barrier fuel cladding evaluates the importance of three salient attributes: (1) metallurgical bond between the zirconium liner and the Zircaloy substrate, (2) liner thickness (roughly 10% of the total cladding wall), and (3) softness (purity). The effect that each of these attributes has on the pellet-cladding interaction (PCI) resistance of the Zr-barrier fuel was studied by a combination of analytical model calculations and laboratory experiments using an expanding mandrel technique. Each of the attributes is shown to contribute to PCI resistance. The effect of the zirconium liner on fuel behavior during off-normal events in which steam comes in contact with the zirconium surface was studied experimentally. Simulations of loss-of-coolant accident (LOCA) showed that the behavior of Zr-barrier cladding is virtually indistinguishable from that of conventional Zircaloy cladding. If steam contacts the zirconium liner surface through a cladding perforation and the fuel rod is operated under normal power conditions, the zirconium liner is oxidized more rapidly than is Zircaloy, but the oxidation rate returns to the rate of Zircaloy oxidation when the oxide phase reaches the zirconium-Zircaloy metallurgical bond

  2. Semi-empirical corrosion model for Zircaloy-4 cladding

    International Nuclear Information System (INIS)

    Nadeem Elahi, Waseem; Atif Rana, Muhammad

    2015-01-01

    The Zircaloy-4 cladding tube in Pressurize Water Reactors (PWRs) bears corrosion due to fast neutron flux, coolant temperature, and water chemistry. The thickness of Zircaloy-4 cladding tube may be decreased due to the increase in corrosion penetration which may affect the integrity of the fuel rod. The tin content and inter-metallic particles sizes has been found significantly in the magnitude of oxide thickness. In present study we have developed a Semiempirical corrosion model by modifying the Arrhenius equation for corrosion as a function of acceleration factor for tin content and accumulative annealing. This developed model has been incorporated into fuel performance computer code. The cladding oxide thickness data obtained from the Semi-empirical corrosion model has been compared with the experimental results i.e., numerous cases of measured cladding oxide thickness from UO 2 fuel rods, irradiated in various PWRs. The results of the both studies lie within the error band of 20μm, which confirms the validity of the developed Semi-empirical corrosion model. Key words: Corrosion, Zircaloy-4, tin content, accumulative annealing factor, Semi-empirical, PWR. (author)

  3. Integration of post-irradiation examination results of failed WWER fuel rods

    International Nuclear Information System (INIS)

    Smirnov, A.; Markov, D.; Smirnov, V.; Polenok, V.; Perepelkin, S.

    2003-01-01

    The aim of the work is to investigate the causes of WWER fuel rod failures and to reveal the dependence of the failed fuel rod behaviour and state on the damage characteristics and duration of their operation in the core. The post-irradiation examination of 12 leaky fuel assemblies (5 for WWER-440 and 7 for WWER-1000) has been done at SSC RF RIAR. The results show that the main mechanism responsible for the majority of cases of the WWER fuel rod perforation is debris-damage of the claddings. Debris fretting of the claddings spread randomly over the fuel assembly cross-section and they are registered in the area of the bundle supporting grid or under the lower spacer grids along the fuel assembly height. In the WWER fuel rods, the areas of secondary hydrogenating of cladding are spaced from the primary defects by ∼2500-3000 mm, as a rule, and are often adjacent closely to the upper welded joints. There is no pronounced dependence of the distance between the primary and secondary cladding defects neither on the linear power, at which the fuel rods were operated, nor on the period of their operation in the leaky state. The time period of the significant secondary damage formation is about 250 ± 50 calendar days for the WWER fuel rods with slight through primary defects (∼0.1 - 0.5 mm 2 ) operated in the linear power range 170-215 W/cm. Cladding degradation, taking place due to the secondary hydrogenating, does not occur in case of large through debris-defects during operation up to 600 calendar days

  4. Structural analysis and modeling of water reactor fuel rod behavior

    International Nuclear Information System (INIS)

    Roshan Zamir, M.

    2000-01-01

    An important aspect of the design and analysis of nuclear reactor is the ability to predict the behavior of fuel elements in the adverse environment of a reactor system under normal and emergency operating conditions. To achieve these objectives and in order to provide a suitable computer code based on fundamental material properties for design and study of the thermal-mechanical behavior of water reactor fuel rods during their irradiation life and also to demonstrate the fuel rod design and modeling for students, The KIANA-1 computer program has been developed by the writer at Amir-Kabir university of technology with support of Atomic Energy Organization of Iran. KIANA-1 is an integral one-dimensional computer program for the thermal and mechanical analysis in order to predict fuel rods performance and also parameter study of Zircaloy-clad UO 2 fuel rod during steady state conditions. The code has been designed for the following main objectives: To give a solution for the steady state heat conduction equation for fuel as a heat source and clad by using finite difference, control volume and semi-analytical methods in order to predict the temperature profile in the fuel and cladding. To predict the inner gas pressures due to the filling gases and released gaseous fission products. To predict the fission gas production and release by using a simple diffusion model based on the Booth models and an empirical model. To calculate the fuel-clad gap conductance for cracked fuel with partial contact zones to a closed gap with strong contact. To predict the distribution of stress in three principal directions in the fuel and sheet by assuming one-dimensional plane strain and asymmetric idealization. To calculate the strain distribution in three principal directions and the corresponding deformation in the fuel and cladding. For this purpose the permanent strain such as creep or plasticity as well as the thermoelastic deformation and also the swelling, densification, cracking

  5. Detection of defective fuel rods in water reactors - a review

    International Nuclear Information System (INIS)

    Hartog, J.M.

    1980-01-01

    Consideration of the fundamental processes of fission product release within fuel pellets and at the pellet surface, and its transport in the fuel/cladding interspace and from fuel rod to coolant, indicates what radio-nuclides will be detectable in the coolant from small and large cladding failures. A better understanding of the aggregate fission product transport is required to allow reactor operators to interpret signals from detection systems in terms of quantitative cladding deterioration. This needs experimental investigation in a specially instrumented loop, as well as development of a technique to cause a rod to defect deliberately during steady power operation. (author)

  6. 5.4W cladding-pumped Nd:YAG silica fiber laser

    OpenAIRE

    Yoo, S.; Webb, A.S.; Standish, R.J.; May-Smith, T.C.; Sahu, J.K.

    2012-01-01

    We report on the spectroscopy and laser characteristics of Nd-doped fiber, fabricated by rod-in-tube from Nd:YAG as a core material with silica cladding. A cladding-pumped CW laser operation at 1058nm with 52% slope-efficiency is demonstrated.

  7. Control rod drive mechanism

    International Nuclear Information System (INIS)

    Mizuno, Katsuyuki.

    1976-01-01

    Object: To restrict the reduction in performance due to stress corrosion cracks by making use of condensate produced in a turbine steam condenser. Structure: Water produced in a turbine steam condenser is forced into a condensed water desalting unit by low pressure condensate pump. The condensate is purified and then forced by a high pressure condensate pump into a feedwater heater for heating before it is returned to the reactor by a feedwater pump. Part of the condensate issuing from the condensate desalting unit is branched from the remaining portion at a point upstream the pump and is withdrawn into a control rod drive water pump after passing through a motordriven bypass valve, an orifice and a condenser water level control valve, is pressurized in the control rod drive water desalting unit and supplied to a control rod drive water pressure system. The control rod is vertically moved by the valve operation of the water pressure system. Since water of high oxygen concentration does not enter during normal operation, it is possible to prevent the stress cracking of the stainless steel apparatus. (Nakamura, S.)

  8. Determination and microscopic study of incipient defects in irradiated power reactor fuel rods. Final report

    International Nuclear Information System (INIS)

    Pasupathi, V.; Perrin, J.S.; Roberts, E.

    1978-05-01

    This report presents the results of nondestructive and destructive examinations carried out on the Point Beach-1 (PWR) and Dresden-3 (BWR) candidate fuel rods selected for the study of pellet-clad interaction (PCI) induced incipient defects. In addition, the report includes results of examination of sections from Oskarshamn-1 (BWR) fuel rods. Eddy current examination of Point Beach-1 rods showed indications of possible incipient defects in the fuel rods. The profilometry and the gamma scan data also indicated that the source of the eddy current indications may be incipient defects. No failed rods or rods with incipient failure were found in the sample from Point Beach-1. Despite the lack of success in finding incipient defects and filed rods, the mechanism for fuel rod failures in Point Beach-1 is postulated to be PCI-related, with high startup rates and fuel handling being the key elements. Nine out of the 10 candidate fuel rods from Dresden-3 (BWR) were failed, and all the failed rods had leaked water so that the initial mechanism was observed. Examination of clad inner surfaces of the specimens from failed and unfailed rods showed fuel deposits of widely varying appearance. The deposits were found to contain uranium, cesium, and tellurium. Transmission electron microscopy of clad specimens showed evidence of microscopic strain. Metallographic examination of fuel pellets from the peak transient power location showed extensive grain boundary separation and axial movement of the fuel indicative of rapid release of fission products. Examination of Oskarshamn clad specimens did not show any stress corrosion crack (SCC) type defects. The defects found in the examinations appear to be related to secondary hydriding. The clad inner surface of the Oskarshamn specimens also showed uranium-rich deposits of varying features

  9. Method of inspecting control rod drive mechanism

    International Nuclear Information System (INIS)

    Sato, Tomomi; Tatemichi, Shin-ichiro; Hasegawa, Hidenobu.

    1988-01-01

    Purpose: To conduct inspection for control rod drives and fuel handling operations in parallel without taking out the entire fuel, while maintaining the reactor in a subcritical state. Method: Control rod drives are inspected through the release of connection between control rods and control rod drives, detachment and dismantling of control rod drives, etc. In this case, structural materials having neutron absorbing power equal to or greater than the control rods are inserted into the gap after taking out fuels. Since the structural materials have neutron absorbing portion, subcriticality is maintained by the neutron absorbing effect. Accordingly, there is no requirement for taking out all of the fuels, thereby enabling to check the control rod drives and conduct handling for the fuels in parallel. As a result, the number of days required for the inspection can be shortened and it is possible to improve the working efficiency for the decomposition, inspection, etc. of the control rod drives and, thus, improve the operation efficiency of the nuclear power plant thereby attaining the predetermined purpose. (Kawakami, Y.)

  10. Fuel rod behavior of a PWR during load following

    International Nuclear Information System (INIS)

    Perrotta, J.A.; Andrade, G.G. de

    1982-01-01

    The behavior of a PWR fuel rod when operating in normal power cycles, excluding in case of accidents, is analysed. A computer code, that makes the mechanical analysis of the cladding using the finite element method was developed. The ramps and power cycles were simulated suposing the existence of cracks in pellets when the cladding-pellet interaction are done. As a result, an operation procedure of the fuel rod in power cycle is recommended. (E.G.) [pt

  11. A new physics design of control safety rods for prototype fast breeder reactor

    International Nuclear Information System (INIS)

    Devan, K.; Riyas, A.; Alagan, M.; Mohanakrishnan, P.

    2008-01-01

    The absorber rods of 500 MWe prototype fast breeder reactor (PFBR), which is under construction at Kalpakkam, have been designed to provide sufficient shutdown margin during normal and accidental conditions for ensuring the safe shut down. There are nine control and safety rods (CSR) and 3 diverse safety rods (DSR). Absorber material used is initially 65% enriched B 4 C. Based on the reported experiments in PHENIX reactor and design of absorber rods in SUPERPHENIX, the design of CSR is modified by introducing 20 cm length natural B 4 C at the top and bottom of absorber column and maintaining the remaining portion with 65% enriched B 4 C. This design ensures sufficient shutdown margin (SDM) during normal operation and also during the one stuck rod condition. For comparison of the above two designs, a CSR of 57% of enrichment was considered which gives the same worth as the revised CSR design with natural B 4 C sections in top and bottom. There is significant savings in the initial inventory of enriched B 4 C for CSR. The annual requirement of enriched boron also reduces. This new CSR can last for about 5 cycles, based on its clad life. But, it is planned to be replaced after every 3 cycles (1 cycle equals 180 efpd) of operation due to radiation damage effects in hexcan D9 steel. Use of ferritic steel for hexcan can extend the life of CSR to 5 cycles

  12. Irradiation of pressurized water reactor fuel rods in the Forschungsreaktor Juelich 2

    International Nuclear Information System (INIS)

    Gaertner, M.

    1978-10-01

    Test fuel rods have been irradiated in FRJ-2 to study the interaction between fuel and cladding as well as hydride orientation stability in the prehydrided cladding. The fuel rods achieved burn-ups of 3.500 to 10.000 MWd/tU at surface temperatures of 333 0 C and power levels up to 620 W/cm. (orig.) [de

  13. Examination of stainless steel-clad Connecticut Yankee fuel assembly S004 after storage in borated water

    International Nuclear Information System (INIS)

    Langstaff, D.C.; Bailey, W.J.; Johnson, A.B. Jr.; Landow, M.P.; Pasupathi, V.; Klingensmith, R.W.

    1982-09-01

    A Connecticut Yankee fuel assembly (S004) was tested nondestructively and destructively. It was concluded that no obvious degradation of the 304L stainless steel-clad spent fuel from assembly S004 occurred during 5 y of storage in borated water. Furthermore, no obvious degradation due to the pool environment occurred on 304 stainless steel-clad rods in assemblies H07 and G11, which were stored for shorter periods but contained operationally induced cladding defects. The seam welds in the cladding on fuel rods from assembly S004, H07, and G11 were similar in that they showed a wrought microstructure with grains noticeably smaller than those in the cladding base metal. The end cap welds showed a dendritically cored structure, typical of rapidly quenched austenitic weld metal. Some intergranular melting may have occurred in the heat-affected zone (HAZ) in the cladding adjacent to the end cap welds in rods from assemblies S004 and H07. However, the weld areas did not show evidence of corrosion-induced degradation

  14. Control rod driving hydraulic pressure device

    International Nuclear Information System (INIS)

    Ishida, Kazuo.

    1990-01-01

    Discharged water after actuating control rod drives in a BWR type reactor is once discharged to a discharging header, then returned to a master control unit and, subsequently, discharged to a reactor by way of a cooling water header. The radioactive level in the discharging header and the master control unit is increased by the reactor water to increase the operator's exposure. In view of the above, a riser is disposed for connecting a hydraulic pressure control unit incorporating a directional control valve and the cooling water head. When a certain control rod is inserted, the pressurized driving water is supplied through a hydraulic pressure control unit to the control rod drives. The discharged water from the control rod drives is entered by way of the hydraulic pressure control unit into the cooling water header and then returned to the reactor by way of other hydraulic pressure control unit and the control rod drives. Thus, the reactor water is no more recycled to the master control unit to reduce the radioactive exposure. (N.H.)

  15. Control rod for HTGR type reactor

    International Nuclear Information System (INIS)

    Mogi, Haruyoshi; Saito, Yuji; Fukamichi, Kenjiro.

    1990-01-01

    Upon dropping control rod elements into the reactor core, impact shocks are applied to wire ropes or spines to possibly deteriorate the integrity of the control rods. In view of the above in the present invention, shock absorbers such as springs or bellows are disposed between a wire rope and a spine in a HTGR type reactor control rod comprising a plurality of control rod elements connected axially by means of a spine that penetrates the central portion thereof, and is suspended at the upper end thereof by a wire rope. Impact shocks of about 5 kg are applied to the wire rope and the spine and, since they can be reduced by the shock absorbers, the control rod integrity can be maintained and the reactor safety can be improved. (T.M.)

  16. Influence of manufacturing process on the in-reactor creep anisotropy of stress-relieved Zircaloy-2 cladding

    International Nuclear Information System (INIS)

    Shann, S.H.; Van Swam, L.F.

    1995-01-01

    A procedure to determine the axial/radial and circumferential/radial contractile strain ratios (the R and P factors respectively in the Backofen-modified von Mises-Hill yield criterion) from post-irradiation dimensional measurements of Zircaloy-2 cladding of BWR fuel rods, tie rods and water rods was developed and has been described previously (S.H. Shann and L.F. van Swam, Creep anisotropy of Zircaloy-2 cladding during irradiation, Trans. SMiRT-11, Vol. C, 1991). The present study employs the procedure to determine the anisotropy factors R and P for textured cold-worked stress-relieved (CWSR) Zircaloy-2 cladding fabricated by various manufacturing processes. The analysis indicates that the cladding manufacturing process can have a pronounced effect on the anisotropy of irradiation-induced creep. Cladding types with identical yield and ultimate tensile strengths but fabricated by different manufacturing processes have different values of R and P during in-reactor creep. ((orig.))

  17. Shielding device for control rod in nuclear reactor

    International Nuclear Information System (INIS)

    Sakamaki, Kazuo; Tomatsu, Tsutomu.

    1995-01-01

    The device of the present invention shields radiation emitted from control rods to greatly reduce an operator's radiation exposure even if reactor water level is lowered and the upper portion of the control rod is exposed upon inspection of a BWR type reactor. Namely, a shield assembly has a structure comprising a set of four columnar shields in a two-row and two-column arrangement, which can be inserted into a control rod guide tube. Upon conducting inspection, the control rod is lowered into the control rod guide tube, and in this state, the columnar shields of the shield assembly are inserted to the control rod in the control rod guide tube. With such procedures, the upper portion of the control rod protruded from the control rod guide tube is covered with the shield assembly. As a result, radiation leaked from the control rod is shielded. Accordingly, irradiation in the reactor due to leaked radiation can be prevented thereby enabling to reduce an operator's radiation exposure. (I.S.)

  18. Detection device for control rod interference

    International Nuclear Information System (INIS)

    Saito, Noboru.

    1984-01-01

    Purpose: To enable to detect the mechanical interference or friction between a control rod and a channel box automatically, simply and rapidly. Constitution: A signal from a gate circuit and a signal from a comparison mechanism are inputted into an AND circuit if a control rod has not been displaced by a predetermined distance within a prescribed time Δt after the output of an insertion or withdrawal signal for the control rod, by which a control-rod-interference signal is outputted from the AND circuit. Accordingly, the interference between the control rod and the channel box can be detected automatically, easily and rapidly. Furthermore, by properly adjusting the prescribed time Δt set by the gate circuit, the degree of the interference can also be detected, whereby the safety and the reliability of the reactor can be improved significantly. (Horiuchi, T.)

  19. The development of the fuel rod transient performance analysis code FTPAC

    International Nuclear Information System (INIS)

    Han Zhijie; Ji Songtao

    2014-01-01

    Fuel rod behavior, especially the integrity of cladding, played an important role in fuel safety research during reactor transient and hypothetical accidents conditions. In order to study fuel rod performance under transient accidents, FTPAC (Fuel Transient Performance Analysis Code) has been developed for simulating light water reactor fuel rod transient behavior when power or coolant boundary conditions are rapidly changing. It is composed of temperature, mechanical deformation, cladding oxidation and gas pressure model. The assessment was performed by comparing FTPAC code analysis result to experiments data and FRAPTRAN code calculations. Comparison shows that, the FTPAC gives reasonable agreement in temperature, deformation and gas pressure prediction. And the application of slip coefficient is more suitable for simulating the sliding between pellet and cladding when the gap is closed. (authors)

  20. Control rods in LMFBRs: a physics assessment

    International Nuclear Information System (INIS)

    McFarlane, H.F.; Collins, P.J.

    1982-08-01

    This physics assessment is based on roughly 300 control rod worth measurements in ZPPR from 1972 to 1981. All ZPPR assemblies simulated mixed-oxide LMFBRs, representing sizes of 350, 700, and 900 MWe. Control rod worth measurements included single rods, various combinations of rods, and Ta and Eu rods. Additional measurements studied variations in B 4 C enrichment, rod interaction effects, variations in rod geometry, neutron streaming in sodium-filled channels, and axial worth profiles. Analyses were done with design-equivalent methods, using ENDF/B Version IV data. Some computations for the sensitivities to approximations in the methods have been included. Comparisons of these analyses with the experiments have allowed the status of control rod physics in the US to be clearly defined

  1. Snubber assembly for a control rod drive

    International Nuclear Information System (INIS)

    1976-01-01

    A snubber cartridge assembly is described which is mounted to the nozzle of a control rod drive mechanism to insure that it will be located within the liquid filled section of a nuclear reactor vessel whenever the control rod drive is assembled thereto. The snubber assembly includes a piston-mounted proximate to the control rod connecting end of the control rod drive leadscrew to allow the piston to travel within the liquid filled snubber cartridge and controllable exhaust the liquid during a 'scram' condition. The snubber cartridge provides three separate areas of increasing resistance to piston travel to insure a speedy but safe 'scram' of the control rod into the reactor

  2. Snubber assembly for a control rod drive

    International Nuclear Information System (INIS)

    Matthews, J.C.

    1978-01-01

    A snubber cartridge assembly is mounted to the nozzle of a control rod drive mechanism to insure that the snubber assembly will be located within the liquid filled section of a nuclear reactor vessel whenever the control rod drive is assembled thereto. The snubber assembly includes a piston mounted proximate to the control rod connecting end of the control rod drive leadscrew to allow the piston to travel within the liquid filled snubber cartridge and controllably exhaust liquid therefrom during a ''scram'' condition. The snubber cartridge provides three separate areas of increasing resistance to piston travel to insure a speedy but safe ''scram'' of the control rod into the reactor

  3. Apparatus for inspecting a irradiated nuclear fuel rod

    International Nuclear Information System (INIS)

    Saura, Hideaki; Yonemura, Eizo.

    1975-01-01

    Object: To increase safety and inspection efficiency by operating irradiated fuel rods, which are accommodated in a water-filled pool after being taken out from the reactor. Structure: When making inspection of irradiated fuel rods, particularly the cladding tube thereof, a fuel box which stores irradiated fuel rods in a water pool is secured to a securement mechanism with slime removal apparatus and inspection apparatus on either side capable of being vertically moved, and it is then stopped at a water depth of about 2 meters. When the lid of the box is opened, irradiated fuel rods are taken out with gripping means and then secured together with the gripping means to an operation base provided on the outside of the pool. Thereafter, the box is lowered by operating pedals on the operation base to completely pull out the irradiated fuel rods from the box, and the irradiated fuel rods are then horizontally moved and then held in a suspended state. Next a slime removal apparatus in raised by operating pedals and an inspection element assembly are progressively raised for inspection of the state of the cladding tube of each fuel rod after removal of slime therefrom. (Nakamura, S.)

  4. Reconstitutable control rod spider assembly

    International Nuclear Information System (INIS)

    Shallenberger, J.M.; Ferian, S.J.

    1990-01-01

    A reconstitutable control rod/spider assembly includes a hollow connecting finger of the spider having a pair of opposing flat segments formed on the interior thereof and engaging a pair of opposing flat sectors formed on the exterior of a stem extending form the upper end of control rod. The stem also has an externally-threaded portion engaging a nut and a pilot aligning portion for the nut. The nut has a radially flexible and expandable thread-defining element captured in its bore. The segments and sectors allow the rod to be removed and reattached after turning through 180 0 to allow more even wear on the rod. (author)

  5. Strengthening effect of reduced graphene oxide in steel clad copper rod

    Science.gov (United States)

    Gao, Haitao; Liu, Xianghua; Ai, Zhengrong; Zhang, Shilong; Liu, Lizhong

    2016-11-01

    Reduced graphene oxide has been extensively used as reinforcing agent owing to their high mechanical properties. In this work, an attempt is made to synthesize steel clad copper rod reinforced with reduced graphene oxide (RGO) by the combination of powder-in-tube and intermediate annealing (IA). Experiments show that the Fe/RGO/Cu composites manifest better mechanical properties than Fe/Cu composites. In the process of groove rolling, RGO acts as effective binder, which can greatly improve the adhesive strength of copper scrap and two metals. Moreover, the strengthening effect of RGO is tightly related to its dispersion state. The RGO diffuses much more uniformly on the metallic substrate under the IA temperature of 1100 °C than 800 °C, which can be characterized by less deformation twins appearing at the interface of core copper and the formation of Fe-RGO-Cu transition belt at the bonding interface. In this case, the peak hardness, tensile strength and shear strength of Fe/RGO/Cu composites are 52 HV, 125 and 41 MPa higher than those of the Fe/Cu composites, respectively. The difference of strengthening effect and mechanisms of RGO under 800 and 1100 °C of IA are systematically discussed by referring to experimental results.

  6. Control rod driving mechanism

    International Nuclear Information System (INIS)

    Ooshima, Yoshio.

    1983-01-01

    Purpose: To perform reliable scram operation, even if abnormality should occur in a system instructing scram operation in FBR type reactors. Constitution: An aluminum alloy member to be melt at a predetermined temperature (about 600sup(o)C) is disposed to a connection part between a control rod and a driving mechanism, whereby the control rod is detached from the driving mechanism and gravitationally fallen to the reactor core. (Ikeda, J.)

  7. Control rod driving hydraulic device

    International Nuclear Information System (INIS)

    Sugano, Hiroshi.

    1993-01-01

    In a control rod driving hydraulic device for an improved BWR type reactor, a bypass pipeline is disposed being branched from a scram pipeline, and a control orifice and a throttle valve are interposed to the bypass pipeline for restricting pressure. Upon occurrence of scram, about 1/2 of water quantity flowing from an accumulator of a hydraulic control unit to the lower surface of a piston of control rod drives by way of a scram pipeline is controlled by the restricting orifice and the throttle valve, by which the water is discharged to a pump suction pipeline or other pipelines by way of the bypass pipeline. With such procedures, a function capable of simultaneously conducting scram for two control rod drives can be attained by one hydraulic control unit. Further, an excessive peak pressure generated by a water hammer phenomenon in the scram pipeline or the control rod drives upon occurrence of scram can be reduced. Deformation and failure due to the excessive peak pressure can be prevented, as well as vibrations and degradation of performance of relevant portions can be prevented. (N.H.)

  8. Corrosion behavior of duplex and reference cladding in NPP Grohnde

    International Nuclear Information System (INIS)

    Besch, O.A.; Yagnik, S.K.; Eucken, C.M.; Bradley, E.R.

    1996-01-01

    The Nuclear Fuel Industry Research (NFIR) Group undertook a lead test assembly (LTA) program in NPP Grohnde PWR in Germany to assess the corrosion performance of duplex and reference cladding. Two identical 16 by 16 LTAs, each containing 32 peripheral test rods, completed four reactor cycles, reaching a peak rod burnup of 46 MWd/kgU. The results from poolside examinations performed at the end of each cycle, together with power histories and coolant chemistry, are reported. Five different cladding materials were characterized during fabrication. The corrosion performance of the cladding materials was tracked in long-term tests in high-pressure, high-temperature autoclaves. The relative ranking of corrosion behavior in such tests corresponded well with the in-reactor corrosion performance. The extent and distribution of hydriding in duplex and reference specimens during the autoclave testing has been characterized. The in-reactor corrosion data indicate that the low-tin Zircaloy-4 reference cladding, R2, had an improved corrosion resistance compared to high-tin Zircaloy-4 reference cladding, R1. Two types of duplex cladding, D1 (Zr-2.5% Nb) and D2 (Zr-0.4% Fe-0.5% Sn), showed an even further improvement in corrosion resistance compared to R2 cladding. The third duplex cladding, D3 (Zr-4 + 1.0% Nb), had significantly less corrosion resistance, which was inferior to R1. The in-reactor and out-reactor corrosion performances have been ranked

  9. Fuel rod-grid interaction wear: in-reactor tests (LWBR development program)

    International Nuclear Information System (INIS)

    Stackhouse, R.M.

    1979-11-01

    Wear of the Zircaloy cladding of LWBR irradiation test fuel rods, resulting from relative motion between rod and rod support contacts, is reported. Measured wear depths were small, 0.0 to 2.7 mils, but are important in fuel element behavior assessment because of the local loss of cladding thickness, as well as the effect on grid spring forces that laterally restrain the rods. An empirical wear analysis model, based on out-of-pile tests, is presented. The model was used to calculate the wear on the irradiation test fuel rods attributed to a combination of up-and-down motions resulting from power and pressure/temperature cycling of the test reactor, flow-induced vibrations, and assembly handling scratches. The calculated depths are generally deeper than the measured depths

  10. First interim examination of defected BWR and PWR rods tested in unlimited air at 2290C

    International Nuclear Information System (INIS)

    Einziger, R.E.; Cook, J.A.

    1983-01-01

    A five-year whole rod test was initiated to investigate the long-term stability of spent fuel rods under a variety of possible dry storage conditions. Both PWR and BWR rods were included in the test. The first interim examination was conducted after three months of testing to determine if there was any degradation in those defected rods stored in an unlimited air atmosphere. Visual observations, diametral measurements and radiographic smears were used to assess the degree of cladding deformation and particulate dispersal. The PWR rod showed no measurable change from the pre-test condition. The two original artificial defects had not changed in appearance and there was no diametral growth of the cladding. One of the defects in BWR rod showed significant deformation. There was approximately 10% cladding strain at the defect site and a small axial crack had formed. The fuel in the defect did not appear to be friable. The second defect showed no visible change and no cladding strain. Following examination, the test was continued at 230 0 C. Another interim examination is planned during the summer of 1983. This paper discusses the details and meaning of the data from the first interim examination

  11. Implementation of CTRLPOS, a VENTURE module for control rod position criticality searches, control rod worth curve calculations, and general criticality searches

    Energy Technology Data Exchange (ETDEWEB)

    Smith, L.A.; Renier, J.P.

    1994-06-01

    A module in the VENTURE reactor analysis code system, CTRLPOS, is developed to position control rods and perform control rod position criticality searches. The module is variably dimensioned so that calculations can be performed with any number of control rod banks each having any number of control rods. CTRLPOS can also calculate control rod worth curves for a single control rod or a bank of control rods. Control rod depletion can be calculated to provide radiation source terms. These radiation source terms can be used to predict radiation doses to personnel and estimate the shielding and long-term storage requirements for spent control rods. All of these operations are completely automated. The numerous features of the module are discussed in detail. The necessary input data for the CTRLPOS module is explained. Several sample problems are presented to show the flexibility of the module. The results presented with the sample problems show that the CTRLPOS module is a powerful tool which allows a wide variety of calculations to be easily performed.

  12. Estimation of irradiated control rod worth

    International Nuclear Information System (INIS)

    Varvayanni, M.; Catsaros, N.; Antonopoulos-Domis, M.

    2009-01-01

    When depleted control rods are planned to be used in new core configurations, their worth has to be accurately predicted in order to deduce key design and safety parameters such as the available shutdown margin. In this work a methodology is suggested for the derivation of the distributed absorbing capacity of a depleted rod, useful in the case that the level of detail that is known about the irradiation history of the control rod does not allow an accurate calculation of the absorber's burnup. The suggested methodology is based on measurements of the rod's worth carried out in the former core configuration and on corresponding calculations based on the original (before first irradiation) absorber concentration. The methodology is formulated for the general case of the multi-group theory; it is successfully tested for the one-group approximation, for a depleted control rod of the Greek Research Reactor, containing five neutron absorbers. The computations reproduce satisfactorily the irradiated rod worth measurements, practically eliminating the discrepancy of the total rod worth, compared to the computations based on the nominal absorber densities.

  13. Control rod for FBR type reactor

    International Nuclear Information System (INIS)

    Nakai, Koichi.

    1993-01-01

    In a control rod for an LMFBR type reactor, a thermal resistor is disposed between a temperature sensitive cylinder and a cam unit support rod. A thermal expansion difference due to the temperature difference is caused between the temperature sensitive cylinder and the cam unit support rod only upon abrupt temperature change of coolants. A control rod shaft extending mechanism of downwardly depressing an absorbent portion by amplifying the thermal expansion difference by an extension link mechanism and the cam unit is provided. The thermal resistor comprises inconel 625 or like other steel of small heat conductivity. If a certain abnormality should cause to the reactor system to elevate the coolant temperature in the reactor elevates abruptly and the reactor shutdown system does not actuate, since the control rod extension shaft extends to urge the absorbent and lower the reactor core reactivity, so that leading to serious accident can be prevented surely. Further, the control rod extension shaft does not extend upon moderate temperature elevation in the usual startup and causes no unnecessary reactivity change. (N.H.)

  14. LOFT fuel rod surface temperature measurement testing

    International Nuclear Information System (INIS)

    Eaton, A.M.; Tolman, E.L.; Solbrig, C.W.

    1978-01-01

    Testing of the LOFT fuel rod cladding surface thermocouples has been performed to evaluate how accurately the LOFT thermocouples measure the cladding surface temperature during a loss-of-coolant accident (LOCA) sequence and what effect, if any, the thermocouple would have on core performance. Extensive testing has been done to characterize the thermocouple design. Thermal cycling and corrosion testing of the thermocouple weld design have provided an expected lifetime of 6000 hours when exposed to reactor coolant conditions of 620 K and 15.9 MPa and to sixteen thermal cycles with an initial temperature of 480 K and peak temperatures ranging from 870 to 1200K. Departure from nucleate boiling (DNB) tests have indicated a DNB penalty (5 to 28% lower) during steady state operation and negligible effects during LOCA blowdown caused by the LOFT fuel rod surface thermocouple arrangement. Experience with the thermocouple design in Power Burst Facility (PBF) and LOFT nonnuclear blowdown testing has been quite satisfactory. Tests discussed here were conducted using both stainless steel and zircaloy-clad electrically heated rod in the LOFT Test Support Facility (LTSF) blowdown simulation loop

  15. Control rod for a nuclear reactor

    Science.gov (United States)

    Roman, Walter G.; Sutton, Jr., Harry G.

    1979-01-01

    A control rod assembly for a nuclear reactor is disclosed having a remotely disengageable coupling between the control rod and the control rod drive shaft. The coupling is actuated by first lowering then raising the drive shaft. The described motion causes axial repositioning of a pin in a grooved rotatable cylinder, each being attached to different parts of the drive shaft which are axially movable relative to each other. In one embodiment, the relative axial motion of the parts of the drive shaft is used either to couple or to uncouple the connection by forcing resilient members attached to the drive shaft into or out of shouldered engagement, respectively, with an indentation formed in the control rod.

  16. Control rod for a nuclear reactor

    International Nuclear Information System (INIS)

    Roman, W.G.; Sutton, H.G. Jr.

    1976-01-01

    A control rod assembly for a nuclear reactor is disclosed having a remotely disengageable coupling between the control rod and the control rod drive shaft. The coupling is actuated by first lowering then raising the drive shaft. The described motion causes axial repositioning of a pin in a grooved rotatable cylinder, each being attached to different parts of the drive shaft which are axially movable relative to each other. In one embodiment, the relative axial motion of the parts of the drive shaft is used either to couple or to uncouple the connection by forcing resilent members attached to the drive shaft into or out of shouldered engagement, respectively, with an indentation formed in the control rod

  17. Control rod for a nuclear reactor

    International Nuclear Information System (INIS)

    Roman, W.G.; Sutton, H.G. Jr.

    1979-01-01

    A control rod assembly for a nuclear reactor is disclosed having a remotely disengageable coupling between the control rod and the control rod drive shaft. The coupling is actuated by first lowering then raising the drive shaft. The described motion causes axial repositioning of a pin in a grooved rotatable cylinder, each being attached to different parts of the drive shaft which are axially movable relative to each other. In one embodiment, the relative axial motion of the parts of the drive shaft is used either to couple or to uncouple the connection by forcing resilient members attached to the drive shaft into or out of shouldered engagement, respectively, with an indentation formed in the control rod

  18. Advanced gray rod control assembly

    Science.gov (United States)

    Drudy, Keith J; Carlson, William R; Conner, Michael E; Goldenfield, Mark; Hone, Michael J; Long, Jr., Carroll J; Parkinson, Jerod; Pomirleanu, Radu O

    2013-09-17

    An advanced gray rod control assembly (GRCA) for a nuclear reactor. The GRCA provides controlled insertion of gray rod assemblies into the reactor, thereby controlling the rate of power produced by the reactor and providing reactivity control at full power. Each gray rod assembly includes an elongated tubular member, a primary neutron-absorber disposed within the tubular member said neutron-absorber comprising an absorber material, preferably tungsten, having a 2200 m/s neutron absorption microscopic capture cross-section of from 10 to 30 barns. An internal support tube can be positioned between the primary absorber and the tubular member as a secondary absorber to enhance neutron absorption, absorber depletion, assembly weight, and assembly heat transfer characteristics.

  19. Reactor control rod supporting structure

    International Nuclear Information System (INIS)

    Akimoto, Tokuzo; Miyata, Hiroshi.

    1984-01-01

    Purpose: To enable stable reactor core control even in extremely great vertical earthquakes, as well as under normal operation conditions in FBR type reactors. Constitution: Since a mechanism for converting the rotational movement of a control rod into vertical movement is placed at the upper portion of the reactor core at high temperature, the mechanism should cause fusion or like other danger after the elapse of a long period of time. In view of the above, the conversion mechanism is disposed to the lower portion of the reactor core at a lower temperature region. Further, the connection between the control rod and the control rod drive can be separated upon great vertical earthquakes. (Seki, T.)

  20. Development of a control rod drive

    International Nuclear Information System (INIS)

    1991-01-01

    In the period under review, the computer codes required for transients calculation have been completed, as well as the programs for modelling and testing the hot-gas temperature control by means of combined core rod and reflector rod operation. The specification of requirements to be fulfilled by the rod drive computer and the neutron flux measuring system has been done relying essentially on the data obtained by the transients calculations performed and the resulting informations on operating conditions. The work for optimization of the core rod drive with regard to rod driving speeds and the 'three-point switch' with hysteresis for controlled, automatic core rod operation has been concentrating on the case of specified, normal operation of the reactor. (orig./DG) [de

  1. A Study on the Structural Integrity Issues of a Dual-Cooled Fuel Rod

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Hyung-Kyu; Lee, Kang-Hee; Lee, Young-Ho; Yoon, Kyung-Ho; Kim, Jae-Yong; Song, Kun-Woo [Korea Atomic Energy Research Institute, 1045 Daedeokdaero Yuseong Daejeon 305-353 (Korea, Republic of)

    2009-06-15

    A dual-cooled fuel rod has an internal coolant flow passage in addition to the external one. A remarkable power up-rate can be achieved due to the increased surface area, which may draw great interests from the fuel researchers, designers and vendors. However, it requires effective resolution to the difficult technical issues when a fuel assembly is to be realized. It becomes much more difficult if a tough boundary condition needs to be satisfied such as a compatibility with the existing reactor internal structures. This kind of challenge is tackled through a national R and D project in Korea: to develop the structural components of a dual-cooled fuel that should be compatible with the current OPR 1000 (Korea Standard Nuclear Power Plant) internal structures. Fuel rod supporting structures, top and bottom end pieces and guide tubes are the components. Besides, the fuel rod components have to be developed as well since the fuel rod's geometry becomes much different from the conventional rod's one. The dimension change may well affect the above mentioned structural components. As a part of the work, structural integrity of the components of a dual-cooled fuel rod is studied in this paper. The investigated topics are: i) the thickness determination of a cladding tube (especially outer tube of a large diameter), ii) vibration issue of an inner cladding tube, iii) design concern of plenum spring and spacer. The cladding thickness issue arises due to the increased outside diameter of a fuel rod, which is caused by an internal flow passage formation. Among the criteria for the thickness determination, an elastic buckling criteria was focused on. Theoretical background for the well-known formula (such as a stability problem) was revisited. Verification tests were carried out independently with using a cladding tube of PHWR fuel rod. Results showed that the formula was not conservative to apply for the cladding thickness determination. Minimum thickness for the

  2. Development of nuclear fuel rod inspection technique using ultrasonic resonance phenomenon

    Energy Technology Data Exchange (ETDEWEB)

    Choi, Myung Sun; Lee, Jong Po; Ju, Young Sang [Korea Atomic Energy Research Institute, Taejon (Korea, Republic of)

    1995-11-01

    Acoustic resonance scattering from a nuclear fuel rod in water is analyzed. A new model for the background which is attributed to the interference of reflected wave and diffracted wave is found and here named {sup t}he inherent background{sup .} The resonance spectrum of a fuel rod is obtained by subtracting the inherent background from the scattered pressure. And also analyzed are the effect of material damping of cladding tube and pellet on the resonance spectrum of a fuel rod. The propagation characteristics of circumferential waves which cause the resonances of cladding tube is produced and the appropriate resonance modes for the application to the inspection of assembled fuel rods are selected. The resonance modes are experimentally measured for pre- and post-irradiated fuel rods and the validation of the fuel rod inspection using ultrasonic resonance phenomenon is examined. And thin ultrasonic sensors accessible into the narrow interval (about 2-3mm) between assembled fuel rods are designed and manufactured. 14 refs. (Author).

  3. Control rod supporting device in reactor

    International Nuclear Information System (INIS)

    Seki, Osamu; Itooka, Satoshi; Harada, Kiyoshi; Jodoi, Takashi.

    1990-01-01

    Since coolants flowing from a reactor core hit against a control rod and a control rod connection pipe, a considerable amount of bending moment for separating an attracting surface between an electromagnet and an armature is formed. Then, a plurality of grooves are formed on a heat sensitive material to dispose a heat collecting fin, and each of upper and lower contact portions of a control rod supporting portion in which the flanged portion of T-like cross section does not slip out is made into a partial spheric surface and a portion between the electromagnet and the attracted member are engaged by the unevenness. With such a constitution, even if a bending moment is applied, the control rod only swings and the bending moment is not transmitted to the attracted member. Further, since the temperature of the heat sensitive material can be rapidly made closer to the peripheral temperature by using the heat collecting fin, the timing for separation is made accurate. Further, since the engaging portion is brought into contact at the spheric surface, the load distribution on the control rod is made uniform, and the positional relationship is made accurate, to support the control rod reliably and the separation depends only on the temperature of the coolants. (N.H.)

  4. Zircaloy sheathed thermocouples for PWR fuel rod temperature measurements

    International Nuclear Information System (INIS)

    Anderson, J.V.; Wesley, R.D.; Wilkins, S.C.

    1979-01-01

    Small diameter zircaloy sheathed thermocouples have been developed by EG and G Idaho, Inc., at the Idaho National Engineering Laboratory. Surface mounted thermocouples were developed to measure the temperature of zircaloy clad fuel rods used in the Thermal Fuels Behavior Program (TFBP), and embedded thermocouples were developed for use by the Loss-of-Fluid Test (LOFT) Program for support tests using zircaloy clad electrically heated nuclear fuel rod simulators. The first objective of this developmental effort was to produce zircaloy sheathed thermocouples to replace titanium sheathed thermocouples and thereby eliminate the long-term corrosion of the titanium-to-zircaloy attachment weld. The second objective was to reduce the sheath diameter to obtain faster thermal response and minimize cladding temperature disturbance due to thermocouple attachment

  5. Analysis of photonic band gaps in two-dimensional photonic crystals with rods covered by a thin interfacial layer

    International Nuclear Information System (INIS)

    Trifonov, T.; Marsal, L.F.; Pallares, J.; Rodriguez, A.; Alcubilla, R.

    2004-01-01

    We investigate different aspects of the absolute photonic band gap (PBG) formation in two-dimensional photonic structures consisting of rods covered with a thin dielectric film. Specifically, triangular and honeycomb lattices in both complementary arrangements, i.e., air rods drilled in silicon matrix and silicon rods in air, are studied. We consider that the rods are formed of a dielectric core (silicon or air) surrounded by a cladding layer of silicon dioxide (SiO 2 ), silicon nitride (Si 3 N 4 ), or germanium (Ge). Such photonic lattices present absolute photonic band gaps, and we study the evolution of these gaps as functions of the cladding material and thickness. Our results show that in the case of air rods in dielectric media the existence of dielectric cladding reduces the absolute gap width and may cause complete closure of the gap if thick layers are considered. For the case of dielectric rods in air, however, the existence of a cladding layer can be advantageous and larger absolute PBG's can be achieved

  6. FREC-4A: a computer program to predict fuel rod performance under normal reactor operation

    International Nuclear Information System (INIS)

    Harayama, Yasuo; Izumi, Fumio

    1981-10-01

    The program FREC-4A (Fuel Reliability Evaluation Code-version 4A) is used for predicting fuel rod performance in normal reactor operation. The performance is calculated in accordance with the irradiation history of fuel rods. Emphasis is placed on the prediction of the axial elongation of claddings induced by pellet-cladding mechanical interaction, including the influence of initially preloaded springs inserted in fuel rod lower plenums. In the FREC-4A, an fuel rod is divided into axial segments. In each segment, it is assumed that the temperature, stress and strain are axi-symmetrical, and the axial strain in constant in fuel pellets and in a cladding, though the values in the pellets and in the cladding are different. The calculation of the contact load and the clearance along the length of a fuel rod and the stress and strain in each segment is explained. The method adopted in the FREC-4A is simple, and suitable to predict the deformation of fuel rods over their full length. This report is described on the outline of the program, the method of solving the stiffness equations, the calculation models, the input data such as irradiation history, output distribution, material properties and pores, the printing-out of input data and calculated results. (Kako, I.)

  7. Utilization of carbon/carbon composites in nuclear simulation fuel rods

    International Nuclear Information System (INIS)

    Polidoro, H.A.; Otani, S.; Rezende, M.C.; Ferreira, S.R.; Otani, C.

    1988-01-01

    Thermo-hydraulic problems, in nuclear plants are normally analysed by using electrically heated rods. Carbon/carbon composites were used to make heating elements for testing by indirect heating up to a heat flux of 100 W/cm 2 . It is easy to verify that this value can be exceed if the choice of the complementary materials for insulator and cladding were improved. The swaging process used to reduce the cladding diameter prevented the fabrication of graphite heater rods. (author) [pt

  8. Results of the Gallium-Clad Phase 3 and Phase 4 tasks (canceled prior to completion)

    International Nuclear Information System (INIS)

    Morris, R.N.

    1998-08-01

    This report summarizes the results of the Gallium-Clad interactions Phase 3 and 4 tasks. Both tasks were to involve examining the out-of-pile stability of residual gallium in short fuel rods with an imposed thermal gradient. The thermal environment was to be created by an electrical heater in the center of the fuel rod and coolant flow on the rod outer cladding. Both tasks were canceled due to difficulties with fuel pellet fabrication, delays in the preparation of the test apparatus, and changes in the Fissile Materials Disposition program budget

  9. MABEL-2: a code to analyse cladding deformation in a loss-of-coolant accident: status February 1980

    International Nuclear Information System (INIS)

    Gittus, J.H.; Haste, T.J.; Bowring, R.W.; Cooper, C.A.

    1980-02-01

    MABEL-2 calculates the deformation of a single fuel rod. This rod is surrounded by 8 other rods on a square lattice whose behaviour is specified via Input Data options. A 2-D (r,theta) conduction model is used for the fuel rod, the cladding creep is calculated from the CANSWEL-2 model and the feedback effect of clad strain on heat transfer to the coolant is obtained from subchannel analysis of the coolant passages surrounding the rod. The coding of the first version of MABEL-2 has been completed except for work to optimise the iteration convergence, minimise the running time and generally tidy up the coding. (author)

  10. Investigations of the interaction between ballooning Zircaloy cladding and emergency core cooling

    International Nuclear Information System (INIS)

    Wiehr, K.; Barth, S.; Erbacher, F.; Hame, W.; Harten, U.; Just, W.; Megerle, A.; Mueller, S.; Neitzel, H.J.; Reimann; Schaeffner, P.; Schmidt, H.

    1975-01-01

    The development of fabrication methods for the production of fuel rod simulators has been largely terminated. For welding of Zircaloy-4 and inconel 600 explosive welding has proved to be promissory in preliminary tests. A prototype fuel rod simulator was tested at full power. Its performance was faultless and the fuel rod and ring pellets could be easily dismantled and reused after the experiment. Planning of the test rig and electricity supply were terminated. Most of the assembly work has been finished. For electric heating of the fuel rod simulators a special device was built and tested which allows to program the power control. The radiographic system recording ballooning of the Zircaloy clad was erected outside the test space and put into operation. First trial pictures yielded good results. (orig.) [de

  11. Control rod cluster with removable rods for nuclear fuel assembly

    International Nuclear Information System (INIS)

    Denizou, J.P.

    1989-01-01

    For each removable control rod, the open end section of the sleeve has a certain length of reduced diameter with openings in its wall. The top end of the rod is joined to an extension tube that surrounds the shaft over part of its lenght. This extension tube fits over the reduced part of the sleeve when the shaft is screwed into the bore of the sleeve. Rotation of the rod in the sleeve is prevented by deforming the extension tube locally in the openings of the end part of the sleeve. The rod is dismantled by exerting a torque on it using a gripping area near the end of the rod [fr

  12. RODSWELL: a computer code for the thermomechanical analysis of fuel rods under LOCA conditions

    International Nuclear Information System (INIS)

    Casadei, F.; Laval, H.; Donea, J.; Jones, P.M.; Colombo, A.

    1984-01-01

    The present report is the user's manual for the computer code RODSWELL developed at the JRC-Ispra for the thermomechanical analysis of LWR fuel rods under simulated loss-of-coolant accident (LOCA) conditions. The code calculates the variation in space and time of all significant fuel rod variables, including fuel, gap and cladding temperature, fuel and cladding deformation, cladding oxidation and rod internal pressure. The essential characteristics of the code are briefly outlined here. The model is particularly designed to perform a full thermal and mechanical analysis in both the azimuthal and radial directions. Thus, azimuthal temperature gradients arising from pellet eccentricity, flux tilt, arbitrary distribution of heat sources in the fuel and the cladding and azimuthal variation of coolant conditions can be treated. The code combines a transient 2-dimensional heat conduction code and a 1-dimentional mechanical model for the cladding deformation. The fuel rod is divided into a number of axial sections and a detailed thermomechanical analysis is performed within each section in radial and azimuthal directions. In the following sections, instructions are given for the definition of the data files and the semi-variable dimensions. Then follows a complete description of the input data. Finally, the restart option is described

  13. In-core failure of the instrumented BWR rod by locally induced high coolant temperature

    International Nuclear Information System (INIS)

    Yanagisawa, Kazuaki

    1985-12-01

    In the BWR type light water loop instrumented in HBWR, a current BWR type fuel rod pre-irradiated up to 5.6 MWd/kgU was power ramped to 50 kW/m. During the ramp, the diameter of the rod was expanded significantly at the bottom end. The behaviour was different from which caused by pellet-cladding interaction (PCI). In the post-irradiation examination, the rod was found to be failed. In this paper, the cause of the failure was studied and obtained the followings. (1) The significant expansion of the rod diameter was attributed to marked oxidation of cladding outer diameter, appeared in the direction of 0 0 -180 0 degree with a shape of nodular. (2) The cladding in the place was softened by high coolant temperature. Coolant pressure, 7MPa intruded the cladding into inside chamfer void at pellet interface. (3) At the place of the significant oxidation, an instrumented transformer was existed and the coolant flow area was very little. The reduction of the coolant flow was enhanced by the bending of the cladding which was caused in pre-irradiation stage. They are considered to be a principal cause of local closure of coolant flow and resultant high temperature in the place. (author)

  14. Gray rod for a nuclear reactor

    International Nuclear Information System (INIS)

    Francis, T.A.; Cerni, Samuel.

    1986-01-01

    The invention relates to an improved gray rod for insertion in a nuclear fuel assembly having an array of fuel rods. The gray rod includes a thin-walled cladding tube a first longitudinal section of which is positioned within, and a second longitudinal section of which is positioned essentially without, the array of fuel rods when the gray rod is inserted in the fuel assembly. The first longitudinal section defines a pellet-receiving space having detained therein a stack of annular pellets with an outer diameter sufficient to lend radial support to the wall of the first longitudinal tube section. The second longitudinal section defines a hollow space devoid of pellets and having means to resist radial collapse under external pressure. This means may be a partially compressed spiral spring which serves the dual purpose of retaining the stack of pellets in the pellet-receiving space and of lending radial support to the wall of the second longitudinal tube section or it may be holes through the wall to allow pressure equalisation. The cladding tube is composed of stainless-steel material having a low neutron-capture cross-section, and the annular pellets preferably being composed of Zircaloy or Zirconia material. (author)

  15. Microcomputer system for controlling fuel rod length

    International Nuclear Information System (INIS)

    Meyer, E.R.; Bouldin, D.W.; Bolfing, B.J.

    1979-01-01

    A system is being developed at the Oak Ridge National Laboratory (ORNL) to automatically measure and control the length of fuel rods for use in a high temperature gas-cooled reactor (HTGR). The system utilizes an LSI-11 microcomputer for monitoring fuel rod length and for adjusting the primary factor affecting length. Preliminary results indicate that the automated system can maintain fuel rod length within the specified limits of 1.940 +- 0.040 in. This system provides quality control documentation and eliminates the dependence of the current fuel rod molding process on manual length control. In addition, the microcomputer system is compatible with planned efforts to extend control to fuel rod fissile and fertile material contents

  16. FRAPCON-3: A computer code for the calculation of steady-state, thermal-mechanical behavior of oxide fuel rods for high burnup

    International Nuclear Information System (INIS)

    Berna, G.A.; Beyer, G.A.; Davis, K.L.; Lanning, D.D.

    1997-12-01

    FRAPCON-3 is a FORTRAN IV computer code that calculates the steady-state response of light water reactor fuel rods during long-term burnup. The code calculates the temperature, pressure, and deformation of a fuel rod as functions of time-dependent fuel rod power and coolant boundary conditions. The phenomena modeled by the code include (1) heat conduction through the fuel and cladding, (2) cladding elastic and plastic deformation, (3) fuel-cladding mechanical interaction, (4) fission gas release, (5) fuel rod internal gas pressure, (6) heat transfer between fuel and cladding, (7) cladding oxidation, and (8) heat transfer from cladding to coolant. The code contains necessary material properties, water properties, and heat-transfer correlations. The codes' integral predictions of mechanical behavior have not been assessed against a data base, e.g., cladding strain or failure data. Therefore, it is recommended that the code not be used for analyses of cladding stress or strain. FRAPCON-3 is programmed for use on both mainframe computers and UNIX-based workstations such as DEC 5000 or SUN Sparcstation 10. It is also programmed for personal computers with FORTRAN compiler software and at least 8 to 10 megabytes of random access memory (RAM). The FRAPCON-3 code is designed to generate initial conditions for transient fuel rod analysis by the FRAPTRAN computer code (formerly named FRAP-T6)

  17. CONTROL ROD

    Science.gov (United States)

    Walker, D.E.; Matras, S.

    1963-04-30

    This patent shows a method of making a fuel or control rod for a nuclear reactor. Fuel or control material is placed within a tube and plugs of porous metal wool are inserted at both ends. The metal wool is then compacted and the tube compressed around it as by swaging, thereby making the plugs liquid- impervious but gas-pervious. (AEC)

  18. Fuel rod failure due to marked diametral expansion and fuel rod collapse occurred in the HBWR power ramp experiment

    International Nuclear Information System (INIS)

    Yanagisawa, Kazuaki

    1985-12-01

    In the power ramp experiment with the BWR type light water loop at the HBWR, the two pre-irradiated fuel rods caused an unexpected pellet-cladding interaction (PCI). One occurred in the fuel rod with small gap of 0.10 mm, which was pre-irradiated up to the burn-up of 14 MWd/kgU. At high power, the diameter of the rod was increased markedly without accompanying significant axial elongation. The other occurred in the rod with a large gap of 0.23 mm, which was pre-irradiated up to the burn-up of 8 MWd/kgU. The diameter of the rod collapsed during a diameter measurement at the maximum power level. The causes of those were investigated in the present study by evaluating in-core data obtained from equipped instruments in the experiment. It was revealed from the investigation that these behaviours were attributed to the local reduction of the coolant flow occurred in the region of a transformer in the ramp rig. The fuel cladding material is seemed to become softened due to temperature increase caused by the local reduction of the coolant flow, and collapsed by the coolant pressure, either locally or wholly depending on the rod diametral gap existed. (author)

  19. Fuel-rod response during the large-break LOCA Test LOC-6

    International Nuclear Information System (INIS)

    Vinjamuri, K.; Cook, B.A.; Hobbins, R.R.

    1981-01-01

    The large break Loss of Coolant Accident (LOCA) Test LOC-6 was conducted in the Power Burst Facility (PBF) at the Idaho National Engineering Laboratory by EG and G Idaho, Inc. The objectives of the PBF LOCA tests are to obtain in-pile cladding ballooning data under blowdown and reflood conditions and assess how well out-of-pile ballooning data represent in-pile fuel rod behavior. The primary objective of the LOC-6 test was to determine the effects of internal rod pressures and prior irradiation on the deformation behavior of fuel rods that reached cladding temperatures high in the alpha phase of zircaloy. Test LOC-6 was conducted with four rods of PWR 15 x 15 design with the exception of fuel stack length (89 cm) and enrichment (12.5 W% 235 U). Each rod was surrounded by an individual flow shroud

  20. Behavior of four PWR rods subjected to a simulated loss-of-coolant accient in the power burst facility

    International Nuclear Information System (INIS)

    Cook, T.F.; Hagrman, D.L.; Sepold, L.K.

    1978-01-01

    Cladding deformation characteristics resulting from the first nuclear blowdown tests (LOC-11) conducted in the Power Burst Facility (PBF) are emphasized in this paper. The objective of the LOC-11 tests was to obtain data on the thermal, mechanical, and materials behavior of pressurized and unpressurized fuel rods when exposed to a blowdown similiar to that expected in a pressurized water reactor (PWR) during a hypothesized double-ended cold-leg break. The test hardware consisted of four separately shrouded fresh fuel rods of PWR 15 x 15 design. Initial plenum pressures ranged from atmospheric to 4.8 MPa (representative of end-of-life). During LOC-11C, the four fuel rods were subjected to 6.5 hours of nuclear operation at approximately 67 kW/m average rod power to cause decay heat build-up. Just before the start of blowdown, cladding surface temperatures were about 620 K and fuel centerline temperatures were in the 2500 to 2600 K range. During the 30-second blowdown transient, CHF occurred 2 seconds after initiation. Fuel centerline temperature dropped continuously, while cladding surface temperatures increased. Maximum cladding temperatures of 1030 to 1050 K occurred 15 seconds into the transient. Posttest destructive examination revealed cladding microstructures and oxide thicknesses consistent with the measured cladding temperatures. The cladding surface thermocouples did not appreciably affect cladding temperature distributuion (fin cooling effect) in the vicinity of the thermocouples

  1. Control Rod Malfunction at the NRAD Reactor

    Energy Technology Data Exchange (ETDEWEB)

    Thomas L. Maddock

    2010-05-01

    The neutron Radiography Reactor (NRAD) is a training, research, and isotope (TRIGA) reactor located at the INL. The reactor is normally shut down by the insertion of three control rods that drop into the core when power is removed from electromagnets. During a routine shutdown, indicator lights on the console showed that one of the control rods was not inserted. It was initially thought that the indicator lights were in error because of a limit switch that was out of adjustment. Through further testing, it was determined that the control rod did not drop when the scram switch was initially pressed. The control rod anomaly led to a six month shutdown of the reactor and an in depth investigation of the reactor protective system. The investigation looked into: scram switch operation, console modifications, and control rod drive mechanisms. A number of latent issues were discovered and corrected during the investigation. The cause of the control rod malfunction was found to be a buildup of corrosion in the control rod drive mechanism. The investigation resulted in modifications to equipment, changes to both operation and maintenance procedures, and additional training. No reoccurrences of the problem have been observed since corrective actions were implemented.

  2. Control rod experiments in Racine

    International Nuclear Information System (INIS)

    Stanculescu, A.; Humbert, G.

    1981-09-01

    A survey of the control-rod experiments planned within the joint CEA/CNEN-DeBeNe critical experiment RACINE is given. The applicability to both heterogeneous and homogeneous large power LMFBR-cores is discussed. Finally, the most significant results of the provisional design calculations performed on behalf of the RACINE control-rod programme are presented

  3. Experimental studies of resistance fretting-wear of fuel rods for VVER-1000 and TVS-KVADRAT fuel assemblies

    International Nuclear Information System (INIS)

    Makarov, V.; Afanasiev, A.; Egorov, Yu.; Matvienko, I.

    2015-01-01

    The paper covers the results of the studies performed to justify the wear resistance of fuel rods in contact with the spacer grids of TVS VVER-1000 fuel assembly and TVS-KVADRAT square fuel assembly of Russian design for PWR-900 reactor. The presented results of three testing stages comprise: Testing of mockup fuel rods of VVER TVS fuel assembly for fretting wear under the conditions of the water chemistry of VVER reactor; Testing models of different design embodiments of the fuel rods for VVER TVS fuel assembly for fretting wear in still cold water; Testing mockup fuel rods of TVS-KVADRAT square fuel assembly for PWR reactor for frettingwear under the conditions of PWR water chemistry. The effect of structural and operational factors was determined (amplitudes, fuel rod vibration frequencies, values of cladding-to-spacer grid cell gap for the depth of fuel rod cladding wear etc.), an assessment was made of the threshold values of fuel rod vibration parameters, which, if not exceeded, provide the absence of the fuel rod cladding fretting wear in the fuel rod-to spacer grid contact area. Key words: fretting wear, fuel rod, spacer grid, VVER, PWR (author)

  4. Control rod housing alignment and repair apparatus

    International Nuclear Information System (INIS)

    Dixon, R.C.; Deaver, G.A.; Punches, J.R.; Singleton, G.E.; Erbes, J.G.; Offer, H.P.

    1991-01-01

    This patent describes a welding a repair device for precisely locating and welding the position of the top of a control rod drive housing attached from a stub tube from a corresponding aperture and alignment pin in a core plate within a boiling water nuclear reactor, the welding and repair device. It comprises: a shaft, the shaft extending from the vicinity of the top of the control rod drive housing up to and through the aperture in the core plate; means for registering to the aperture and the alignment pin on the core plate; a fixture attached to the bottom end of the shaft for mating to the top of the control rod drive housing in precise mating relationship; the fixture attached to the bottom end of the shaft whereby the fixture, when mated to the control rod drove housing and the registering means when registered to the alignment pin and aperture on the core plate imparts to the shaft, and angularity between the top of the control rod drive housing and the hole in the core plate; a hollow cylinder, the cylinder mounted for depending and sealed support with respect to the shaft above, about and below the control rod drive housing top; the cylinder depending down below the control rod drive housing to an elevation below the top of the sub tube; a rotating welding apparatus with a welding head for dispensing weldment mounted for rotation with respect to the shaft; the welding head disposed at the juncture between the side of the control rod drive housing and the stub tube; and means for flooding the cylinder with gas whereby the cylinder may be lowered. flooded in a gas environment and effect a weld between the top of the stub tube and the control rod drive housing

  5. Control rod housing alignment and repair method

    International Nuclear Information System (INIS)

    Dixon, R.C.; Deaver, G.A.; Punches, J.R.; Singleton, G.E.; Erbes, J.G.; Offer, H.P.

    1992-01-01

    This patent describes a method for underwater welding of a control rod drive housing inserted through a stub tube to maintain requisite alignment and elevation of the top of the control rod drive housing to an overlying and corresponding aperture in a core plate as measured by an alignment device which determines the relative elevation and angularity with respect to the aperture. It comprises providing a welding cylinder dependent from the alignment device such that the elevation of the top of the welding cylinder is in a fixed relationship to the alignment device and is gas-proof; pressurizing the welding cylinder with inert welding gas sufficient to maintain the interior of the welding cylinder dry; lowering the welding cylinder through the aperture in the core plate by depending the cylinder with respect to the alignment device, the lowering including lowering through and adjusting the elevation relationship of the welding cylinder to the alignment device such that when the alignment device is in position to measure the elevation and angularity of the new control rod drive housing, the lower distal end of the welding cylinder extends below the upper periphery of the stub where welding is to occur; inserting a new control rod drive housing through the stub tube and positioning the control rod drive housing to a predetermined relationship to the anticipated final position of the control rod drive housing; providing welding implements transversely rotatably mounted interior of the welding cylinder relative to the alignment device such that the welding implements may be accurately positioned for dispensing weldment around the periphery of the top of the stub tube and at the side of the control rod drive housing; measuring the elevation and angularity of the control rod drive housing; and dispensing weldment along the top of the stub tube and at the side of the control rod drive housing

  6. Shock analysis on hydraulic drive control rod during scram

    International Nuclear Information System (INIS)

    Song Wei; Qin Benke; Bo Hanliang

    2013-01-01

    Control rod hydraulic drive mechanism (CRHDM) is a new invention of Institute of Nuclear and New Energy Technology of Tsinghua University. The hydraulic absorber buffers the control rod when it scrams. The control rod fast drop impact experiment was conducted and the key parameters of control rod hydraulic buffering performance were obtained. Based on the test results and according to D'Alembert principle, the maximum inertial impact force on the control rod during the fast drop period was applied as equivalent static load force on the control rod. The deformations and stress distributions on the control rod in this worst case were calculated by using finite element software ABAQUS. Calculation results were compared with the experiment results, and it was verified that nonlinear transient dynamics analysis in this problem can be simplified as static analysis. Damage criterion of the control rod fast drop impact process was also given. And it lays foundation for optimal design of the control rod and hydraulic absorber. (authors)

  7. Thermal performance of the nuclear fuel rods submitted to angular variation of the heat exchanger coefficients

    International Nuclear Information System (INIS)

    Carvalho, A.M.M. de.

    1984-01-01

    Generally, LMFBR fuel rods consist of fuel pellets encapsulated in cladding tubes. These tubes are wrapped by a helical wire, working as a spacer. Distortions in the rod temperature distribution and in the external heat flux can be generated by angular variations in the local heat transfer coefficients due to the wire, by excentricity between pellet and clad or by ovalization of the cladding tube. Also, the temperature distributions can be affected by fuel densification, reestructuring and swelling. The present work consists of the development of a computer code in order to analyse the fuel rod performance as function of geometrical and operational effects, in steady state regime. (Author) [pt

  8. Control-rod scram device

    International Nuclear Information System (INIS)

    Matsui, Yoshiro; Saito, Koji.

    1986-01-01

    Purpose: To eliminate the requirement for the nitrogen gas system in a scram device and enable safety and reliable shutdown of a water-cooled reactor power plant. Constitution: A piston and a spring are contained within a hydraulic vessel, and the piston is driven by the energy stored in the spring so as to supply hydraulic water to control mechanisms. During usual reactor operation, a scram valve is closed and a high water pressure of about 130 kg/cm 2 is applied to the water filled in the vessel through a check valve. Upon occurrence of abnormal conditions and generation of scram signals, the scram valve is opened to supply the water filled in the vessel through the scram valve to the control rod drive mechanisms. When the water pressure in the vessel is decreased, since the piston is urged upwardly by the energy stored in the spring, the water filled in the vessel is intermitently supplied to the control rod drive mechanisms. Thus, control rods can be inserted into the nuclear reactor to shutdown the same. (Horiuchi, T.)

  9. Experimental and calculation results of the integral reflood test QUENCH-14 with M5 (registered) cladding tubes

    International Nuclear Information System (INIS)

    Stuckert, J.; Birchley, J.; Grosse, M.; Jaeckel, B.; Steinbrueck, M.

    2010-01-01

    The QUENCH-14 experiment investigated the effect of M5 (registered) cladding material on bundle oxidation and core reflood, in comparison with tests QUENCH-06 (ISP-45) that used standard Zircaloy-4 and QUENCH-12 that used VVER E110-claddings. The PWR bundle configuration of QUENCH-14 with a single unheated rod, 20 heated rods, and four corner rods was otherwise identical to QUENCH-06. The test was conducted in principle with the same protocol as QUENCH-06, so that the effects of the change of cladding material could be observed more easily. Pre-test calculations were performed by the Paul Scherrer Institut (Switzerland) using the SCDAPSIM, SCDAP/RELAP5 and MELCOR codes. Follow-on post-test analyses were performed using SCDAP/RELAP5 and MELCOR as part of an ongoing programme of model validation and code assessment. Alternative oxidation correlations were used to examine the possible influence of the M5 (registered) cladding material on hydrogen generation, in comparison with Zircaloy-4. The experiment started with a pre-oxidation phase in steam, lasting ∼3000 s at ∼1500 K peak bundle temperature. After a further temperature increase to maximum bundle temperature of 2073 K the bundle was flooded with 2 g/s/rod water from the bottom. The peak temperature of ∼2300 K was measured on the bundle shroud, shortly after quench initiation. The electrical power was reduced to average value of 2 W/cm during the reflood phase to simulate effective decay heat level. Complete bundle cooling was reached in 300 s after reflood initiation. The development of the oxide layer growth during the test was essentially defined by measurements performed on the three Zircaloy-4 corner rods withdrawn successively from the bundle. The withdrawal of Zircaloy-4 and E110 corner rods after the test allowed a comparison of the different alloys in one test. One heated rod with M5 cladding was withdrawn after the test for a detailed analysis of oxidation degree and measurement of absorbed

  10. Optimized Control Rods of the BR2 Reactor

    Energy Technology Data Exchange (ETDEWEB)

    Kalcheva, Silva; Koonen, E.

    2007-09-15

    At the present time the BR-2 reactor uses control elements with cadmium as neutron absorbing part. The lower section of the control element is a beryllium assembly cooled by light water. Due to the burn up of the lower end of the cadmium section during the reactor operation, the presently used rods for reactivity control of the BR-2 reactor have to be replaced by new ones. Considered are various types Control Rods with full active part of the following materials: cadmium (Cd), hafnium (Hf), europium oxide (Eu2O3) and gadolinium (Gd2O3). Options to decrease the burn up of the control rod material in the hot spot, such as use of stainless steel in the lower active part of the Control Rod are discussed. Comparison with the characteristics of the presently used Control Rods types is performed. The changing of the characteristics of different types Control Rods and the perturbation effects on the reactor neutronics during the BR-2 fuel cycle are investigated. The burn up of the Control Rod absorbing material, total and differential control rods worth, macroscopic and effective microscopic absorption cross sections, fuel and reactivity evolution are evaluated during approximately 30 operating cycles.

  11. Optimized Control Rods of the BR2 Reactor

    International Nuclear Information System (INIS)

    Kalcheva, Silva; Koonen, E.

    2007-01-01

    At the present time the BR-2 reactor uses control elements with cadmium as neutron absorbing part. The lower section of the control element is a beryllium assembly cooled by light water. Due to the burn up of the lower end of the cadmium section during the reactor operation, the presently used rods for reactivity control of the BR-2 reactor have to be replaced by new ones. Considered are various types Control Rods with full active part of the following materials: cadmium (Cd), hafnium (Hf), europium oxide (Eu2O3) and gadolinium (Gd2O3). Options to decrease the burn up of the control rod material in the hot spot, such as use of stainless steel in the lower active part of the Control Rod are discussed. Comparison with the characteristics of the presently used Control Rods types is performed. The changing of the characteristics of different types Control Rods and the perturbation effects on the reactor neutronics during the BR-2 fuel cycle are investigated. The burn up of the Control Rod absorbing material, total and differential control rods worth, macroscopic and effective microscopic absorption cross sections, fuel and reactivity evolution are evaluated during approximately 30 operating cycles.

  12. Fabrication Of Control Rod System Of The RSG-GAS

    International Nuclear Information System (INIS)

    Sudirdjo, Hari; Setyono; Prasetya, Hendra

    2001-01-01

    Eight units of control rod mechanical system of RSG-GAS has been fabricated. The control rod mechanical system of RSG-GAS consist of guide tube and lifting rod. Complete construction of the control rod mechanical system of RSG-GAS are guide tube, lifting rod, absorber, and absorber casing. The eight units of the control rod mechanical system of RSG-GAS has been fabricated according to the mechanical engineering design

  13. Zircaloy cladding degradation under repository conditions

    International Nuclear Information System (INIS)

    Santanam, L.; Raghavan, S.; Chin, B.A.

    1990-12-01

    Creep, a potential degradation mechanism of Zircaloy cladding after repository disposal of spent nuclear fuel, has been investigated. The deformation and fracture map methodology has been used to predict maximum allowable initial storage temperatures to achieve a thousand year life without rupture as a function of spent-fuel history. Maximum allowable temperatures are 340 degree C (613 K) for typically stressed rods (70--100 MPa) and 300 degree C (573 K) for highly stressed rods (140--160 MPa). 10 refs., 2 figs

  14. Review of experimental data for modelling LWR fuel cladding behaviour under loss of coolant accident conditions

    Energy Technology Data Exchange (ETDEWEB)

    Massih, Ali R. [Quantum Technologies AB, Uppsala Science Park (Sweden)

    2007-02-15

    Extensive range of experiments has been conducted in the past to quantitatively identify and understand the behaviour of fuel rod under loss-of-coolant accident (LOCA) conditions in light water reactors (LWRs). The obtained experimental data provide the basis for the current emergency core cooling system acceptance criteria under LOCA conditions for LWRs. The results of recent experiments indicate that the cladding alloy composition and high burnup effects influence LOCA acceptance criteria margins. In this report, we review some past important and recent experimental results. We first discuss the background to acceptance criteria for LOCA, namely, clad embrittlement phenomenology, clad embrittlement criteria (limitations on maximum clad oxidation and peak clad temperature) and the experimental bases for the criteria. Two broad kinds of test have been carried out under LOCA conditions: (i) Separate effect tests to study clad oxidation, clad deformation and rupture, and zirconium alloy allotropic phase transition during LOCA. (ii) Integral LOCA tests, in which the entire LOCA sequence is simulated on a single rod or a multi-rod array in a fuel bundle, in laboratory or in a tests and results are discussed and empirical correlations deduced from these tests and quantitative models are conferred. In particular, the impact of niobium in zirconium base clad and hydrogen content of the clad on allotropic phase transformation during LOCA and also the burst stress are discussed. We review some recent LOCA integral test results with emphasis on thermal shock tests. Finally, suggestions for modelling and further evaluation of certain experimental results are made.

  15. Hydraulic pressure control unit for control rod drive

    International Nuclear Information System (INIS)

    Watabe, Yukio.

    1990-01-01

    The pressure invention concerns a hydraulic pressure control unit for control rod drives in BWR type reactors. The space above a floating piston possessed by an accumulator and the housing of control rod drives are connected by means of a pipeline. The pipeline has a scram valve which is opened upon occurrence of reactor scram. A pump is disposed between the accumulator and the scram valve for communicating a discharge port to apply a high pressure water to the accumulator. According to the present invention, a control unit is disposed between the scram valve and the housing of the control rod drives in the hydraulic pressure control unit for maintaining the cross sectional area of the flow channel of the pipeline to a usual size when the pressure in a pressure vessel is under a rated operation pressure, while limiting the cross sectional area of the flow channel when the pressure is lower than that in the rated operation. Thus, whole insertion of the control rod substantially at a constant speed is enabled irrespective of the level of the pressure in the pressure vessel. (I.S.)

  16. Detection device for control rod scram

    International Nuclear Information System (INIS)

    Ishiyama, Satoshi.

    1989-01-01

    The device of the present invention comprises a control rod dropping separately from a control rod driving mechanism main body, a following tube falling separately accompanying therewith and a guide tube for guiding the dropping of the control rod and the following tube. Further, rare earth permanent magnets are embedded with the pole being axially oriented in the following tube and bobbins each mounted with an inner flange made of high magnetic permeability material are disposed to the guide tube. Coils are wound in the bobbin. In this control rod scram detection device, since magnetic fluxes can effectively be supplied to the coils, it is possible to obtain stable and highly reliable scram detection signals. Further, since the coils and the bobbins can be manufactured separately from the guide tube, their assemblies can be tested independently from the guide tube. (K.M.)

  17. Behavior of defective LWR-type fuel rods irradiated under postulated accident conditions

    International Nuclear Information System (INIS)

    Hobbins, R.R.; Croucher, D.W.; Seiffert, S.L.; Cook, B.A.; Kerwin, D.K.; Mehner, A.S.; Ploger, S.A.

    1979-05-01

    The irradiation experiments reported here have been conducted by the Thermal Fuels Behavior Program of EG and G Idaho, Inc., for the United States Nuclear Regulatory Commission in the Power Burst Facility (PBF) at the Idaho National Engineering Laboratory. Five of the rods were irradiated in PCM tests and one in a LOC test. During these tests, the six rods lost cladding integrity prior to or during the transient phase of the test due to either manufacturing defects or intentional rod design and operation. Of the five defective rods tested under PCM conditions, one (Rod IE-008, Test IE-1) had a hydride rupture below the region of the rod, which was in film boiling during the transient; two (Rod A-0021, Test PCM-3 and Rod IE-019, Test IE-5) contained defects (a pin hole and a small axial crack, respectively) within the film boiling zone; and two (Rod 201-1, Test PCM-1 and Rod 205-8, Test PCM-5) failed by cladding embrittlement within the film boiling zone. Rod 312-3 was waterlogged before being subjected to LOC conditions in Test LLR-3

  18. PHEBUS/test-218, Behaviour of a Fuel Rod Bundle during a Large Break LOCA Transient with a two Peaks Temperature History

    International Nuclear Information System (INIS)

    1987-01-01

    1 - Description of test facility: PHEBUS test facility operated at CEA Research Center Cadarache consists of a pressurized circuit involving pumps, heat exchangers and a blowdown tank - 25 nuclear fuel rod bundle, coupled to a separate driver core; - active length 0.8 m, cosine axial power profile; - pressurized and un-pressurized fuel rods; - controlled cooling conditions at the bundle inlet (blowdown, refill and reflood period); - de-pressurized test rig volume 0.22 m 3 . The following 'as measured' boundary conditions (B.C.) were offered to participants as options with decreasing challenge to their analytical approach: Boundary conditions B.C.0: - full thermal-hydraulic analysis of PHEBUS test rig (was not recommended). Boundary conditions B.C.1: - thermal power level of fuel bundle; - fluid inlet conditions to bundle section. Boundary conditions B.C.2: - local cladding temperatures of rods; - heat transfer coefficients. Boundary conditions B.C.3: - cladding temperatures of rods; - internal pressure of rods. 2 - Description of test: Post-test investigation into the response of a nuclear fuel bundle to a large break loss of coolant accident with respect to - local fuel temperatures, - cladding strain at the time of burst, - time to burst and under given thermal-hydraulic boundary conditions of PHEBUS-test 218

  19. Model investigation of fuel rod behaviour

    International Nuclear Information System (INIS)

    Girgis, M.M.; Wiesenack, W.; Stegemann, D.

    1985-06-01

    Thermal and mechanical behaviour of fuel rods can be explained but unsatisfactorily by models based of an axial symmetry concept. Recently developed models include, with respect to their thermal components, a simple method for the computation of the temperature distribution within the fuel, and they also take into account the influence of excentrically placed pellets for the computation of heat transfer in the cold gap. Additionally, a finite-element model is used to evaluate the effects of cracking and fragmentation on the thermal behaviour of pellets. The reaction of fuel and fuel cladding to external and internal loadings and the axial interaction between fuel and cladding are described in the mechanical portion of the model. A special case of axial coupling is the so-called random stacking interaction caused by fuel pellets placed excentrically at the cladding and sliding radially and axially. In the comparison of measurement results, both thermal and mechanical behaviour of different rods from the OECD Halden Reactor Project are subject to investigations. (RF) [de

  20. Temperature escalation in PWR fuel rod simulators due to the zircaloy/steam reaction ESSI-4 ESSI-11

    International Nuclear Information System (INIS)

    Hagen, S.; Kapulla, H.; Malauscheck, H.; Wallenfels, K.P.; Buescher, B.J.

    1985-03-01

    The tests had the initial heatup rate as main parameter. The experimental arrangement consisted of a fuel rod simulator (central tungsten heater, UO 2 ring pellets and zircaloy cladding), a zircaloy shroud and the fiber ceramic insulation. A steam flow of ca. 20 g/min was introduced at the lower end of the bundle. A temperature escalation was observed in every test. The maximum cladding surface temperature in the single rod tests never exceeded 2200 0 C. The escalation began in the upper region of the rods and moved down the rods, opposite to the direction of steam flow. For fast initial heatup rates, the runoff of molten zircaloy was a limiting process for the escalation. For slow heatup rates, the formation of a protective oxide layer reduced the reaction rate. The test with less insulation thickness showed a reduction of the escalation. A stronger influence was found for the gap between shroud and insulation. This is caused by convection heat losses to the steam circulating in this gap by natural convection. Removal of the gap between shroud and insulation in essentially the same experimental arrangement produced a faster escalation. The posttest appearance of the fuel rod simulators showed that, at slow heatup rates oxidation of the cladding was complete, and the fuel rod was relatively intact. Conversely, at fast heatup rates, relatively little cladding oxidation with extensive dissolution of the UO 2 pellets and runoff of molten cladding was observed. (orig./HP) [de

  1. RODSWELL: a computer code for the thermomechanical analysis of fuel rods under LOCA conditions

    International Nuclear Information System (INIS)

    Casadei, F.; Laval, H.; Donea, J.; Jones, P.M.; Colombo, A.

    1984-01-01

    The code calculates the variation in space and time of all significant fuel rod variables, including fuel, gap and cladding temperature, fuel and cladding deformation, cladding oxidation and rod internal pressure. The code combines a transient 2-dimensional heat conduction code and a 1-dimensional mechanical model for the cladding deformation. The first sections of this report deal with the heat conduction model and the finite element discretization used for the thermal analysis. The mechanical deformation model is presented next: modelling of creep, phase change and oxidation of the zircaloy cladding is discussed in detail. A model describing the effect of oxidation and oxide cracking on the mechanical strength of the cladding is presented too. Next a mechanical restraint model, which allows the simulation of the presence of the neighbouring rods and is particularly important in assessing the amount of channel blockage during a transient, is presented. A description of the models used for the coolant conditions and for the power generation follows. The heat source can be placed either in the fuel or in the cladding, and direct or indirect clad heating by electrical power can be simulated. Then a section follows, dealing with the steady-state and transient types of calculation and with the automatic variable time step selection during the transient. The last sections deal with presentation of results, graphical output, test problems and an example of general application of the code

  2. Controlling a nuclear reactor with dropped control rods

    International Nuclear Information System (INIS)

    Mc Atee, K.R.; Alsop, B.H.

    1987-01-01

    A control system is described for a nuclear power plant including a reactor with a core having an upper portion and a lower portion and control rods which are inserted into and withdrawn from the core of the reactor vertically to control reactivity in the core. The system comprises: means to measure neutron flux separately in the upper portion and the lower portion of the reactor and to generate from such measurements a signal representative of axial distribution of power between the upper and lower portions of the reactor core; means to detect a dropped control rod in the reactor and to generate a dropped rod signal in response thereto; means to generate an axial power distribution limit signal representative of a critical axial power distribution for a dropped rod condition; means to compare the axial power distribution signal to the axial power distribution limit signal and to generate an axial power distribution out of limits signal when the axial power distribution signal exceeds the axial power distribution limit signal; and means responsive only to the presence of both the dropped rod signal and the axial power distribution out of limits signal to generate a signal for shutting the reactor down

  3. Simulation of nuclear fuel rods by using process computer-controlled power for indirect electrically heated rods

    International Nuclear Information System (INIS)

    Malang, S.

    1975-11-01

    An investigation was carried out to determine how the simulation of nuclear fuel rods with indirect electrically heated rods could be improved by use of a computer to control the electrical power during a loss-of-coolant accident (LOCA). To aid in the experiment, a new version of the HETRAP code was developed which simulates a LOCA with heater rod power controlled by a computer that adjusts rod power during a blowdown to minimize the difference in heat flux of the fuel and heater rods. Results show that without computer control of heater rod power, only the part of a blowdown up to the time when the heat transfer mode changes from nucleate boiling to transition or film boiling can be simulated well and then only for short times. With computer control, the surface heat flux and temperature of an electrically heated rod can be made nearly identical to that of a reactor fuel rod with the same cooling conditions during much of the LOCA. A small process control computer can be used to achieve close simulation of a nuclear fuel rod with an indirect electrically heated rod

  4. Microstructural examination of fuel rods subjected to a simulated large-break loss of coolant accident in reactor

    International Nuclear Information System (INIS)

    Garlick, A.

    1985-01-01

    A series of tests has been conducted in the National Research Universal (NRU) reactor, Chalk River, Canada, to investigate the behaviour of full-length 32-rod PWR fuel bundles during a simulated large-break loss of coolant accident (LOCA). In one of these tests (MT-3), 12 central rods were pre-pressurized in order to evaluate the ballooning and rupture of cladding in the Zircaloy high-α/α+β temperature region. All 12 rods ruptured after experiencing < 90% diametral strain but there was no suggestion of coplanar blockage. Post-irradiation examination was carried out on cross-sections of cladding from selected rods to determine the aximuthal distribution of wall thinning along the ballooned regions. These data are assessed to check whether they are consistent with a mechanism in which fuel stack eccentricity generates temperature gradients around the ballooning cladding and leads to premature rupture during a LOCA. After anodizing, the cladding microstructures were examined for the presence of prior-beta phase that would indicate the α/α+β transformation temperature (1078K) had been exceeded. These results were compared with isothermal annealing test data on unirradiated cladding from the same manufacturing batch

  5. Analysis of control rod behavior based on numerical simulation

    International Nuclear Information System (INIS)

    Ha, D. G.; Park, J. K.; Park, N. G.; Suh, J. M.; Jeon, K. L.

    2010-01-01

    The main function of a control rod is to control core reactivity change during operation associated with changes in power, coolant temperature, and dissolved boron concentration by the insertion and withdrawal of control rods from the fuel assemblies. In a scram, the control rod assemblies are released from the CRDMs (Control Rod Drive Mechanisms) and, due to gravity, drop rapidly into the fuel assemblies. The control rod insertion time during a scram must be within the time limits established by the overall core safety analysis. To assure the control rod operational functions, the guide thimbles shall not obstruct the insertion and withdrawal of the control rods or cause any damage to the fuel assembly. When fuel assembly bow occurs, it can affect both the operating performance and the core safety. In this study, the drag forces of the control rod are estimated by a numerical simulation to evaluate the guide tube bow effect on control rod withdrawal. The contact condition effects are also considered. A full scale 3D model is developed for the evaluation, and ANSYS - commercial numerical analysis code - is used for this numerical simulation. (authors)

  6. Modeling of the PWR fuel mechanical behaviour and particularly study of the pellet-cladding interaction in a fuel rod; Contribution a la modelisation du comportement mecanique des combustibles REP sous irradiation, avec en particulier le traitement de l`interaction pastille-gaine dans un crayon combustible

    Energy Technology Data Exchange (ETDEWEB)

    Hourdequin, N.

    1995-05-01

    In Pressurized Water Reactor (PWR) power plants, fuel cladding constitutes the first containment barrier against radioactive contamination. Computer codes, developed with the help of a large experimental knowledge, try to predict cladding failures which must be limited in order to maintain a maximal safety level. Until now, fuel rod design calculus with unidimensional codes were adequate to prevent cladding failures in standard PWR`s operating conditions. But now, the need of nuclear power plant availability increases. That leads to more constraining operating condition in which cladding failures are strongly influenced by the fuel rod mechanical behaviour, mainly at high power level. Then, the pellet-cladding interaction (PCI) becomes important, and is characterized by local effects which description expects a multidimensional modelization. This is the aim of the TOUTATIS 2D-3D code, that this thesis contributes to develop. This code allows to predict non-axisymmetric behaviour too, as rod buckling which has been observed in some irradiation experiments and identified with the help of TOUTATIS. By another way, PCI is influenced by under irradiation experiments and identified with the help of TOUTATIS which includes a densification model and a swelling model. The latter can only be used in standard operating conditions. However, the processing structure of this modulus provides the possibility to include any type of model corresponding with other operating conditions. In last, we show the result of these fuel volume variations on the cladding mechanical conditions. (author). 25 refs., 89 figs., 2 tabs., 12 photos., 5 appends.

  7. RODMOD: a code for control rod positioning

    International Nuclear Information System (INIS)

    Vondy, D.R.; Fowler, T.B.

    1978-11-01

    The report documents a computer code which has been implemented to position control rods according to a prescribed schedule during the calculation of a reactor history. Control rods may be represented explicitly with or without internal black absorber conditions in selected energy groups, or fractional insertion may be done, or both, in a problem. There is provision for control rod follower, movement of materials through a series of zones in a closed loop, and shutdown rod insertion and subsequent removal to allow the reactor history calculation to be continued. This code is incorporated in the system containing the VENTURE diffusion theory neutronics and the BURNER exposure codes for routine use. The implemented automated procedures cause the prescribed control rod insertion schedule to be applied without the access of additional user input data during the calculation of a reactor operating history

  8. Assessment of stainless steel 348 fuel rod performance against literature available data using TRANSURANUS code

    Directory of Open Access Journals (Sweden)

    Giovedi Claudia

    2016-01-01

    Full Text Available Early pressurized water reactors were originally designed to operate using stainless steel as cladding material, but during their lifetime this material was replaced by zirconium-based alloys. However, after the Fukushima Daiichi accident, the problems related to the zirconium-based alloys due to the hydrogen production and explosion under severe accident brought the importance to assess different materials. In this sense, initiatives as ATF (Accident Tolerant Fuel program are considering different material as fuel cladding and, one candidate is iron-based alloy. In order to assess the fuel performance of fuel rods manufactured using iron-based alloy as cladding material, it was necessary to select a specific stainless steel (type 348 and modify properly conventional fuel performance codes developed in the last decades. Then, 348 stainless steel mechanical and physics properties were introduced in the TRANSURANUS code. The aim of this paper is to present the obtained results concerning the verification of the modified TRANSURANUS code version against data collected from the open literature, related to reactors which operated using stainless steel as cladding. Considering that some data were not available, some assumptions had to be made. Important differences related to the conventional fuel rods were taken into account. Obtained results regarding the cladding behavior are in agreement with available information. This constitutes an evidence of the modified TRANSURANUS code capabilities to perform fuel rod investigation of fuel rods manufactured using 348 stainless steel as cladding material.

  9. Influence of texture on fracture toughness of zircaloy cladding

    International Nuclear Information System (INIS)

    Grigoriev, V.; Andersson, Stefan

    1997-06-01

    The correlation between texture and fracture toughness of Zircaloy 2 cladding has been investigated in connection with axial cracks in fuel rods. The texture of the cladding determines the anisotropy of plasticity of the cladding which, in turn, should influence the strain conditions at the crack-tip. Plastic strains in the cladding under uniaxial tension were characterised by means of the anisotropy constants F, G and H calculated according to Hill's theory. Test temperatures between 20 and 300 deg C do not influence the F, G and H values. Any significant effect of hydrogen (about 500 wtppm) on the anisotropy constants F, G and H has not been revealed at a test temperature of 300 deg C. The results, obtained for stress-relieved and recrystallized cladding with different texture, show an obvious influence of texture on the fracture toughness of Zircaloy cladding. A higher fracture toughness has been found for cladding with more radial texture

  10. Influence of texture on fracture toughness of zircaloy cladding

    Energy Technology Data Exchange (ETDEWEB)

    Grigoriev, V. [Studsvik Material AB, Nykoeping (Sweden); Andersson, Stefan [Royal Inst. of Tech., Stockholm (Sweden)

    1997-06-01

    The correlation between texture and fracture toughness of Zircaloy 2 cladding has been investigated in connection with axial cracks in fuel rods. The texture of the cladding determines the anisotropy of plasticity of the cladding which, in turn, should influence the strain conditions at the crack-tip. Plastic strains in the cladding under uniaxial tension were characterised by means of the anisotropy constants F, G and H calculated according to Hill`s theory. Test temperatures between 20 and 300 deg C do not influence the F, G and H values. Any significant effect of hydrogen (about 500 wtppm) on the anisotropy constants F, G and H has not been revealed at a test temperature of 300 deg C. The results, obtained for stress-relieved and recrystallized cladding with different texture, show an obvious influence of texture on the fracture toughness of Zircaloy cladding. A higher fracture toughness has been found for cladding with more radial texture. With a 2 page summary in Swedish. 32 refs, 18 figs.

  11. Method of driving control rod in reactor

    International Nuclear Information System (INIS)

    Osa, Hirotaka.

    1986-01-01

    Purpose: To improve security and safety of the reactor by reducing reactor output automatically and quickly when circulation of cooling water is stopped. Constitution: When the circulating pump is under operation, fluid pressure in the discharge pipe is transferred to the fluid room of fluid pressure cylinder via the control rod drive pipe and lift up the piston, and then the control rod is drawn out of the reactor core. When the circulating pump is lowered in its functions, discharge pipe fluid pressure decreases, fluid pressure in the fluid room decreases, and with less force of piston movement, the control rod gets lowered by its own weight. At this time, the blocked state of the opening by the piston is released, fluid flows into the room. Lowering of pressure and the control rod is promoted by transferring out fluid below the piston in the fluid room to the upper part of the piston via a small gap when the control rod falls by gravity. (Horiuchi, T.)

  12. Status of rod consolidation

    International Nuclear Information System (INIS)

    Bailey, W.J.

    1985-04-01

    Two of the factors that need to be taken into account with rod consolidation are (1) the effects on rods from their removal from the fuel assembly and (2) the effects on rods as a result of the consolidation process. Potential components of both factors are described in the report. Discussed under (1) are scratches on the fuel rod surfaces, rod breakage, crud, extended burnup, and possible cladding embrittlement due to hydrogen injection at BWRs. Discussed under (2) are the increased water temperature (less than 10 0 C) because of closer packing of the rods, formation of crevices between rods in the close-packed mode, contact with dissimilar metals, and the potential for rapid heating of fuel rods following the loss of water from a spent fuel storage pool. Another factor that plays an important role in rod consolidation is the cost of disposal of the nonfuel-bearing components of the fuel assembly. Also, the dose rate from the components - especially Inconel spacer grids - can affect the handling procedures. Several licensing issues that exist are described. A list of recommendations is provided. 98 refs., 5 figs., 5 tabs

  13. Apparatus for handling control rod drives

    International Nuclear Information System (INIS)

    Akimoto, A.; Watanabe, M.; Yoshida, T.; Sugaya, Z.; Saito, T.; Ishii, Y.

    1979-01-01

    An apparatus for handling control rod drives (CRD's) attached by detachable fixing means to housings mounted in a reactor pressure vessel and each coupled to one of control rods inserted in the reactor pressure vessel is described. The apparatus for handling the CRD's comprise cylindrical housing means, uncoupling means mounted in the housing means for uncoupling each of the control rods from the respective CRD, means mounted on the housing means for effecting attaching and detaching of the fixing means, means for supporting the housing means, and means for moving the support means longitudinally of the CRD

  14. Analysis of buffering process of control rod hydraulic absorber

    International Nuclear Information System (INIS)

    Bao Jishi; Qin Benke; Bo Hanliang

    2011-01-01

    Control Rod Hydraulic Drive Mechanism(CRHDM) is a newly invented build-in control rod drive mechanism. Hydraulic absorber is the key part of this mechanism, and is used to cushion the control rod when the rod scrams. Thus, it prevents the control rod from being deformed and damaged. In this paper dynamics program ANSYS CFX is used to calculate all kinds of flow conditions in hydraulic absorber to obtain its hydraulic characteristics. Based on the flow resistance coefficients obtained from the simulation results, fluid mass and momentum equations were developed to get the trend of pressure change in the hydraulic cylinder and the displacement of the piston rod during the buffering process of the control rod. The results obtained in this paper indicate that the hydraulic absorber meets the design requirement. The work in this paper will be helpful for the design and optimization of the control rod hydraulic absorber. (author)

  15. FEMAXI-III, a computer code for fuel rod performance analysis

    International Nuclear Information System (INIS)

    Ito, K.; Iwano, Y.; Ichikawa, M.; Okubo, T.

    1983-01-01

    This paper presents a method of fuel rod thermal-mechanical performance analysis used in the FEMAXI-III code. The code incorporates the models describing thermal-mechanical processes such as pellet-cladding thermal expansion, pellet irradiation swelling, densification, relocation and fission gas release as they affect pellet-cladding gap thermal conductance. The code performs the thermal behavior analysis of a full-length fuel rod within the framework of one-dimensional multi-zone modeling. The mechanical effects including ridge deformation is rigorously analyzed by applying the axisymmetric finite element method. The finite element geometrical model is confined to a half-pellet-height region with the assumption that pellet-pellet interaction is symmetrical. The 8-node quadratic isoparametric ring elements are adopted for obtaining accurate finite element solutions. The Newton-Raphson iteration with an implicit algorithm is applied to perform the analysis of non-linear material behaviors accurately and stably. The pellet-cladding interaction mechanism is exactly treated using the nodal continuity conditions. The code is applicable to the thermal-mechanical analysis of water reactor fuel rods experiencing variable power histories. (orig.)

  16. Investigating mechanical behavior and radiation resistant of fuel rods clad in nuclear power plant

    International Nuclear Information System (INIS)

    Sedgh Kerdar, A.

    1999-01-01

    interstitials in metal lattice under irradiation causes increased strength and hardness but decreases ductility in metals.The increase in strength and hardness depends on obstacles that prevent the motion of dislocations. The clustering of point defects are responsible for these changes. Irradiation also induces instabilities in phases due to enhancement of diffusion, solute segregation, precipitate formation, order- disorder transformation and resolution of small precipitates. From the microscopic point of view accumulation of vacancies accompanied by formation of He and H 2 gases under irradiation cause an increase in volume which results in swelling and eventually ends up with embrittlement of metals. This subject was described in chapter three Zirconium and its alloys are the best structural materials for fuel cladding of BWR and PWR reactors core. The working condition in the core of nuclear reactor are very serve, respect temperature and radiation dose. It should be realized that, if fuel cladding receive damage and get cracked, the first cooling cycle and the maine equipment will be contaminated with active materials which cause additional environmental problems. Furthermore, replacement of fuel rods are very costly. Therefore, for increasing life time of fuel cladding and minimizing damage, the effect of radiation and heat on Zirconium and its alloys must be investigated. This subject was described in chapter four.The mechanical behavior and radiation resistant of fuel cladding in PWR reactor (specifically WWER ) have been investigated which is described in chapter five. Result, discussion and final conclusion are summarized in last chapter and also several points for improvement have been offered

  17. Means for driving control rod

    International Nuclear Information System (INIS)

    Sato, Haruo; Sasaki, Masayoshi.

    1974-01-01

    Object: To enable wire rope to be readily removed from guide pulleys for the inspection or replacement of control rods. Structure: A pair of guide pulleys disposed to oppose each other are provided on their periphery with respective notches which are arranged in a staggered fashion. In this way, the rope is made to be removed from the notches for inspection of the control rod or for other purposes. (Kamimura, M.)

  18. Fuel followed control rod installation at AFRRI

    International Nuclear Information System (INIS)

    Moore, Mark; Owens, Chris; Forsbacka, Matt

    1992-01-01

    Fuel Followed Control Rods (FFCRs) were installed at the Armed Forces Radiobiology Research Institute's 1 MW TRIGA Reactor. The procedures for obtaining, shipping, and installing the FFCRs is described. As part of the FFCR installation, the transient rod drive was relocated. Core performance due to the addition of the fuel followed control rods is discussed. (author)

  19. Control rod repositioning considerations in core design analysis

    International Nuclear Information System (INIS)

    Armstrong, B.C.; Buechel, R.J.

    1990-01-01

    Control rod repositioning is a method for minimizing rod cluster control assembly (RCCA) wear in the upper internals area where the guide cards interface with the rodlets of the RCCAs. A number of utilities have implemented strategies for rod repositioning, which often has no impact on the nuclear analysis for cases where the control rods are never repositioned into the active fuel. Other strategies involve repositioning the control rods several steps into the active fuel. The impact of this type of repositioning on the axial power shape and consequently the total peaking factor F Q T varies, depending on the method in which the repositioning is implemented at the plant. Operating for long periods with all the control and shutdown rods inserted several steps in the active fuel followed by withdrawing them fully from the core results in a shifting of the power distribution toward the top of the core and must be accounted for in the design analysis. On the other hand, an optional plan for control rod repositioning that considers margins available in related design parameters can be devised that minimizes the effects of the repositioning for the reload. This paper summarizes a rod repositioning strategy implemented for a recent reload and some calculated power shape results for this strategy and other scenarios

  20. Control rod drives for FBR type reactor

    International Nuclear Information System (INIS)

    Ikakura, Hiroaki.

    1990-01-01

    The control rod drives for an FBR type reactor of the present invention eliminate obstacles deposited on attracting surfaces between an electromagnet and an armature which connect control rods to recover their retaining power. That is, a sealed chamber capable of controlling its inner pressure by an operation from the outside of a reactor is disposed in an extension pipe, and a nozzle connected to the sealed chamber and facing at the lower end thereof to the attracting surface is disposed. Liquid sodium sucked by evacuating the sealed chamber is jetted out from the nozzle by pressurizing the chamber to simultaneously eliminate obstacles deposited to the attracting surfaces of the electromagnet and the control rod. Alternatively, a nozzle protruding from and retracting to the lower surface of the electromagnet is disposed opposing to each of the attracting surfaces of the electromagnet and the control rod. Similar effect can also be obtained if gases are jetted out in this state. As a result, control rod drives of high reliability for a FBR type reactor can be obtained. (I.S.)

  1. Protective guide structure for reactor control rod

    International Nuclear Information System (INIS)

    Ban, Minoru; Umeda, Kenji; Kubo, Noboru; Ito, Tomohiro.

    1996-01-01

    The present invention provides an improved protective guide structure for control rods, which does not cause swirling of coolants and resonance even though a slit is formed on a protective tube which surrounds a control rod element in a PWR type reactor. Namely, a reactor control rod is constituted with elongated control elements collectively bundled in the form of a cluster. The protective guide structure protectively guides the collected constituent at the upper portion of a reactor container. The protective structure comprises a plurality of protective tubes each having a C-shaped cross section disposed in parallel for receiving control rod elements individually in which the corners of the opening of the cross section of the protective tube are chamfered to an appropriate configuration. With such a constitution, even if coolant flows in a circumferential direction along the protective tubes surrounding the control rod elements, no shearing stream is caused to the coolants flow since the corners of the cross sectional opening (slit) of the tube are chamfered. Accordingly, occurrence of swirlings can be suppressed. (I.S.)

  2. Radionuclide release from PWR spent fuel specimens with induced cladding defects

    International Nuclear Information System (INIS)

    Wilson, C.N.; Oversby, V.M.

    1984-03-01

    Radionuclide releases from pressurized water reactor (PWR) spent fuel rod specimens containing various artificially induced cladding defects were compared by leach testing. The study was conducted in support of the Nevada Nuclear Waste Storage Investigations (NNWSI) Waste Package Task to evaluate the effectiveness of failed cladding as a barrier to radionuclide release. Test description and results are presented

  3. Evolutionary developments of advanced PWR nuclear fuels and cladding materials

    International Nuclear Information System (INIS)

    Kim, Kyu-Tae

    2013-01-01

    Highlights: • PWR fuel and cladding materials development processes are provided. • Evolution of PWR advanced fuel in U.S.A. and in Korea is described. • Cutting-edge design features against grid-to-rod fretting and debris are explained. • High performance data of advanced grids, debris filters and claddings are given. -- Abstract: The evolutionary developments of advanced PWR fuels and cladding materials are explained with outstanding design features of nuclear fuel assembly components and zirconium-base cladding materials. The advanced PWR fuel and cladding materials development processes are also provided along with verification tests, which can be used as guidelines for newcomers planning to develop an advanced fuel for the first time. The up-to-date advanced fuels with the advanced cladding materials may provide a high level of economic utilization and reliable performance even under current and upcoming aggressive operating conditions. To be specific, nuclear fuel vendors may achieve high fuel burnup capability of between 45,000 and 65,000 MWD/MTU batch average, overpower thermal margin of as much as 15% and longer cycle length up to 24 months on the one hand and fuel failure rates of around 10 −6 on the other hand. However, there is still a need for better understanding of grid-to-rod fretting wear mechanisms leading to major PWR fuel defects in the world and subsequently a driving force for developing innovative spacer grid designs with zero fretting wear-induced fuel failure

  4. Effects of cold worked and fully annealed claddings on fuel failure behaviour

    International Nuclear Information System (INIS)

    Saito, Shinzo; Hoshino, Hiroaki; Shiozawa, Shusaku; Yanagihara, Satoshi

    1979-12-01

    Described are the results of six differently heat-treated Zircaloy clad fuel rod tests in NSRR experiments. The purpose of the test is to examine the extent of simulating irradiated claddings in mechanical properties by as-cold worked ones and also the effect of fully annealing on the fuel failure bahaviour in a reactivity initiated accident (RIA) condition. As-cold worked cladding does not properly simulated the embrittlement of the irradiated one in a RIA condition, because the cladding is fully annealed before the fuel failure even in the short transient. Therefore, the fuel behaviour such as fuel failure threshold energy, failure mechanism, cladding deformation and cladding oxidation of the fully annealed cladding fuel, as well as that of the as-cold worked cladding fuel, are not much different from that of the standard stress-relieved cladding fuel. (author)

  5. Control rod drives for HTGR type reactor

    International Nuclear Information System (INIS)

    Nishiguchi, Isoharu; Katagiri, Shigeo.

    1991-01-01

    The device of the present invention has a feature of having stable braking characteristics upon scram operation of control rods. That is, control rod drives are moved upon and down by a dram which rotates the control rod suspended from to a wire rope, and the dram is disconnected from the driving mechanism by a crutch mechanism upon scram, to rapidly insert the control rod in the reactor by its own weight. An electric generator is used as a braking mechanism for controlling the scram speed of the control rod. A plurality of resistors disposed outside of the reactor coolants boundary are connected in parallel between input/output terminals of the electric generator. With such a constitution, braking characteristics are determined by the intensity of the permanent magnet, number of the coil windings and values of the resistors constituting the power generator. Accordingly, the braking characteristics are less changed relative to the working circumstantial conditions, the history of use and the state of mounting. As a result, stable braking characteristics can always be obtained. Further, braking characteristics can easily be controlled by varying the resistance value. (I.S.)

  6. A study of friction and axial effects in pellet-clad mechanical interaction

    International Nuclear Information System (INIS)

    Harriague, S.; Meyer, J.E.

    1983-01-01

    An analysis is made of the effect of friction forces at the pellet-cladding contact points on the behaviour of a fuel rod under a power-up ramp. A thermoelastic description of the pellets is given; the stiffness matrix and initial displacements are obtained from a finite element calculation. The cladding is considered to behave as a thermoelastic thin shell. A method is developed to assemble the stiffness of each pellet and corresponding cladding section on a fuel rod, resulting in an explicit description of the whole stack. The assumption of thermoelasticity allows for a very fast calculation, even when including hundreds of pellets under an arbitrary axial distribution of power. Results showing the pattern of friction and axial forces, and relative and localized displacements along the rod, are presented. In most cases, pellets at the top of the stack slide with respect to the clad. As a result of the build-up of axial forces due to friction, pellets at lower positions in the fuel column may show, at the contact positions, no relative displacements with respect to the cladding. The effect of pellet dishing and L/D ratio on the axial strains and local deformations are shown. The predictions are consistent with the experimental observations on the effect of pellet shape. Finally, a discussion is made of the results of this study. The use of these results as a guideline for establishing proper boundary conditions in a non-linear PCMI model (i.e., including plasticity and pellet cracking) are also discussed. (author)

  7. Comparison of two analytical methods for the local quantitative determination of lithium and boron contents in cladding materials

    International Nuclear Information System (INIS)

    Gavillet, D.; Guenther-Leopold, I.; Martin, M.; Guillong, M.; Hellwig, Ch.; Sell, H.J.

    2008-01-01

    Pressurized water reactors contain boric acid for reactivity control. As the acidic coolant conditions result in an increased attack of the circuit materials, LiOH is added to render the coolant slightly alkaline. However, LiOH can affect corrosion of the Zr alloy cladding. Thus the Li content in the oxide layers of irradiated fuel rods is of high interest, especially for new alloys (pathfinder rods). At the 'Paul Scherrer Institut' the lithium as well as the boron content in the oxide layers of claddings are determined by Secondary Ion Mass Spectrometry (SIMS). Quantification is performed by direct comparison with a Zircaloy-oxide layer implanted with B and Li. A new and independent method using Laser Ablation Inductively Coupled Plasma Mass Spectrometry was applied to cross-check the SIMS data. (authors)

  8. Hydraulically centered control rod

    International Nuclear Information System (INIS)

    Horlacher, W.R.; Sampson, W.T.; Schukei, G.E.

    1981-01-01

    A control rod suspended to reciprocate in a guide tube of a nuclear fuel assembly has a hydraulic bearing formed at its lower tip. The bearing includes a plurality of discrete pockets on its outer surface into which a flow of liquid is continuously provided. In one embodiment the flow is induced by the pressure head in a downward facing chamber at the end of the bearing. In another embodiment the flow originates outside the guide tube. In both embodiments the flow into the pockets produces pressure differences across the bearing which counteract forces tending to drive the rod against the guide tube wall. Thus contact of the rod against the guide tube is avoided

  9. Overview of Japanese control rods development program

    International Nuclear Information System (INIS)

    Koyama, M.

    1984-01-01

    The Japanese control rods development program was established based on the fast breeder reactor program. Therefore, PNC's efforts have been made mainly for the development of analysis, design and fabrication technologies for ''JOYO'' and ''MONJU'' control rods. Laboratory studies were performed to obtain the information for absorber materials. The design and fabrication of the sealed and vented type control rod pins were completed, and water loop tests and in-sodium tests were carried out. Irradiation behavior of enriched B 4 C pellets with low and high density in DFR was examined. Japan's experimental fast reactor, JOYO, has been operated at the rated power of 50MWt and 75MWt since April 1977 when the MK-I core (breeder core) attained initial criticality. Post irradiation examinations on control rod, removed from the reactor, were carried out and their performance behavior were evaluated. In the MK-II core, a control rods monitoring program has been in investigation. Absorber Materials Irradiation Rigs (AMIR) are scheduled to be loaded and irradiated in the JOYO MK-II core from 1984. (author)

  10. Stress analysis and collapse time prediction of nuclear fuel cladding tube with wear scar

    International Nuclear Information System (INIS)

    Lee, J. S.; Kim, O. H.; Kim, H. K.; Hu, Y. H.; Kim, J. I.; Kim, K. T.

    2004-01-01

    In this analysis, the stress and collapse time analysis models for nuclear fuel rod with the fretting wear scar were developed in order to evaluate the effects of the wear depth on the integrity of nuclear fuel rod. The stress analysis result shows that the nuclear fuel rod with approximately 60% deep wear scar of the clad wall thickness, meets the allowable stress criteria and the collapse time analysis indicates that the fuel rod with less than roughly 56% deep wear scar of the clad wall thickness has longer collapse time than the expected fuel life-time. The both stress and collapse time results are evaluated to be very reasonable on considering the comparison with the outputs of existing design code for the simple model. However, the developed analysis models and the results will be confirmed by the tests

  11. FARST: A computer code for the evaluation of FBR fuel rod behavior under steady-state/transient conditions

    International Nuclear Information System (INIS)

    Nakamura, M.; Sakagami, M.

    1984-01-01

    FARST, a computer code for the evaluation of fuel rod thermal and mechanical behavior under steady-state/transient conditions has been developed. The code characteristics are summarized as follows: (I) FARST evaluates the fuel rod behavior under the transient conditions. The code analyzes thermal and mechanical phenomena within a fuel rod, taking into account the temperature change in coolant surrounding the fuel rod. (II) Permanent strains such as plastic, creep and swelling strains as well as thermoelastic deformations can be analyzed by using the strain increment method. (III) Axial force and contact pressure which act on the fuel stack and cladding are analyzed based on the stick/slip conditions. (IV) FARST used a pellet swelling model which depends on the contact pressure between pellet and cladding, and an empirical pellet relocation model, designated as 'jump relocation model'. The code was successfully applied to analyses of the fuel rod irradiation data from pulse reactor for nuclear safety research in Cadarache (CABRI) and pulse reactor for nuclear safety research in Japan Atomic Energy Research Institute (NSRR). The code was further applied to stress analysis of a 1000 MW class large FBR plant fuel rod during transient conditions. The steady-state model which was used so far gave the conservative results for cladding stress during overpower transient, but underestimated the results for cladding stress during a rapid temperature decrease of coolant. (orig.)

  12. Probabilistic assessment of spent-fuel cladding breach

    International Nuclear Information System (INIS)

    Foadian, H.; Rashid, Y.R.; Seager, K.D.

    1991-01-01

    A methodology for determining the probability spent-fuel cladding breach due to normal and accident class B cask transport conditions is introduced. This technique uses deterministic stress analysis results as well as probabilistic cladding material properties, initial flaws, and breach criteria. Best estimates are presented for the probability distributions of irradiated Zircaloy properties such as ductility and fracture toughness, and for fuel rod initial conditions such as manufacturing flaws and PCI part-wall cracks. Example analyses are used to illustrate the implementation of this methodology for a BWR (GE 7 x 7) and a PWR (B ampersand W 15 x 15) assembly. The cladding breach probabilities for each assembly are tabulated for regulatory normal and accident transport conditions including fire

  13. Probabilistic assessment of spent-fuel cladding breach

    International Nuclear Information System (INIS)

    Foadian, H.; Rashid, Y.R.; Seager, K.D.

    1992-01-01

    In this paper a methodology for determining the probability of spent-fuel cladding breach due to normal and accident class B cask transport conditions is introduced. This technique uses deterministic stress analysis results as well as probabilistic cladding material properties, initial flaws, and breach criteria. Best estimates are presented for the probability distributions of irradiated Zircaloy properties such as ductility and fracture toughness, and for fuel rod initial conditions such as manufacturing flaws and PCI part-wall cracks. Example analyses are used to illustrate the implementation of this methodology for a BWR (GE 7 x 7) and a PWR (B and W 15 x 15) assembly. The cladding breach probabilities for each assembly are tabulated for regulatory normal and accident transport conditions including fire

  14. French LMFBR's control rods experience and development

    International Nuclear Information System (INIS)

    Arnaud, G.; Guigon, A.; Verset, L.

    1983-06-01

    Since the last ten years, the French program has been, first of all, directed to the setting up, and then the development of, at once, the Phenix control rods, and next, the Super-Phenix ones. The vented pin design, with porous plug and sodium bonding, which allows the choices of large diameters, has been taken, since the Rapsodie experience was decisive. The absorber material is sintered, 10 B enriched, boron carbide. The can is made of 316 type stainless steel, stabilised, or not, with titanium. The experience gained in Phenix up to now is important, and deals with about six loads of control rods. Results confirm the validity of the design of the absorber pins. Some difficulties has been encountered for the guiding devices, due to the swelling of the steel. They have required design and material improvements. Such difficulties are discarded by a new design of the bearing, for the Super-Phenix control rods. The other parts of these rods, from the Primary Shut-Down System, are strictly derived from Phenix. The design of the rods from the Secondary Shut-Down System is rather different, but it's not the case for the design of the absorber pins: in many a way, they are derived from Phenix pins and from Rapsodie control rods. Both types of rods irradiation tests are in progress in Phenix [fr

  15. Development of advanced zirconium fuel cladding

    International Nuclear Information System (INIS)

    Jeong, Young Hwan; Park, S. Y.; Lee, M. H.

    2007-04-01

    This report includes the manufacturing technology developed for HANA TM claddings, a series of their characterization results as well as the results of their in-pile and out-of pile performances tests which were carried out to develop some fuel claddings for a high burn-up (70,000MWd/mtU) which are competitive in the world market. Some of the HANA TM claddings, which had been manufactured based on the results from the 1st and 2nd phases of the project, have been tested in a research reactor in Halden of Norway for an in-pile performance qualification. The results of the in-pile test showed that the performance of the HANA TM claddings for corrosion and creep was better than 50% compared to that of Zircaloy-4 or A cladding. It was also found that the out-of pile performance of the HANA TM claddings for such as LOCA and RIA in some accident conditions corrosion creep, tensile, burst and fatigue was superior or equivalent to that of the Zircaloy-4 or A cladding. The project also produced the other many data which were required to get a license for an in-pile test of HANA TM claddings in a commercial reactor. The data for the qualification or characterization were provided for KNFC to assist their activities to get the license for the in-pile test of HANA TM Lead Test Rods(LTR) in a commercial reactor

  16. Radionuclide release from PWR spent fuel specimens with induced cladding defects

    International Nuclear Information System (INIS)

    Wilson, C.N.; Oversby, V.M.

    1984-03-01

    Radionuclide releases from pressurized water reactor (PWR) spent fuel rod specimens containing various artificially induced cladding defects were compared by leach testing. The study was conducted in support of the Nevada Nuclear Waste Storage Investigations (NNWSI) Waste Package Task to evaluate the effectiveness of failed cladding as a barrier to radionuclide release. Test description and results are presented. 6 references, 4 figures

  17. Comparison of the cladding deformation measured during the Power Burst Facility loss-of-coolant accident in-pile experiments with recent Oak Ridge National Laboratory out-of-pile results

    International Nuclear Information System (INIS)

    Broughton, J.M.; McCardell, R.K.; MacDonald, P.E.

    1981-01-01

    A series of four large break loss-of-coolant accident fuel behavior experiments have been performed in the Power Burst Facility. The results of these experiments are briefly reviewed and compared with results from the ORNL multirod burst test program. The effect of cladding burst temperature and prior irradiation were investigated. The cladding strain of the previously irradiated test rods was more uniformly distributed around the cladding circumference and larger than for similar unirradiated test rods. The ORNL out-of-pile single rod test results are in good agreement with the Power Burst Facility (PBF) test results with unirradiated test rods, and the ORNL out-of-pile, single-rod test results with heated shrouds and the PBF test results with previously irradiated test rods are comparable

  18. Control rod homogenization in heterogeneous sodium-cooled fast reactors

    International Nuclear Information System (INIS)

    Andersson, Mikael

    2016-01-01

    The sodium-cooled fast reactor is one of the candidates for a sustainable nuclear reactor system. In particular, the French ASTRID project employs an axially heterogeneous design, proposed in the so-called CFV (low sodium effect) core, to enhance the inherent safety features of the reactor. This thesis focuses on the accurate modeling of the control rods, through the homogenization method. The control rods in a sodium-cooled fast reactor are used for reactivity compensation during the cycle, power shaping, and to shutdown the reactor. In previous control rod homogenization procedures, only a radial description of the geometry was implemented, hence the axially heterogeneous features of the CFV core could not be taken into account. This thesis investigates the different axial variations the control rod experiences in a CFV core, to determine the impact that these axial environments have on the control rod modeling. The methodology used in this work is based on previous homogenization procedures, the so-called equivalence procedure. The procedure was newly implemented in the PARIS code system in order to be able to use 3D geometries, and thereby be take axial effects into account. The thesis is divided into three parts. The first part investigates the impact of different neutron spectra on the homogeneous control-rod cross sections. The second part investigates the cases where the traditional radial control-rod homogenization procedure is no longer applicable in the CFV core, which was found to be 5-10 cm away from any material interface. In the third part, based on the results from the second part, a 3D model of the control rod is used to calculate homogenized control-rod cross sections. In a full core model, a study is made to investigate the impact these axial effects have on control rod-related core parameters, such as the control rod worth, the capture rates in the control rod, and the power in the adjacent fuel assemblies. All results were compared to a Monte

  19. Verification test of control rod system for HTR-10

    International Nuclear Information System (INIS)

    Zhou Huizhong; Diao Xingzhong; Huang Zhiyong; Cao Li; Yang Nianzu

    2002-01-01

    There are 10 sets of control rods and driving devices in 10 MW High Temperature Gas-cooled Test Reactor (HTR-10). The control rod system is the controlling and shutdown system of HTR-10, which is designed for reactor criticality, operation, and shutdown. In order to guarantee technical feasibility, a series of verification tests were performed, including room temperature test, thermal test, test after control rod system installed in HTR-10, and test of control rod system before HTR-10 first criticality. All the tests data showed that driving devices working well, control rods running smoothly up and down, random position settling well, and exactly position indicating

  20. Automatic operation device for control rods

    International Nuclear Information System (INIS)

    Sekimizu, Koichi

    1984-01-01

    Purpose: To enable automatic operation of control rods based on the reactor operation planning, and particularly, to decrease the operator's load upon start up and shutdown of the reactor. Constitution: Operation plannings, demand for the automatic operation, break point setting value, power and reactor core flow rate change, demand for operation interrupt, demand for restart, demand for forecasting and the like are inputted to an input device, and an overall judging device performs a long-term forecast as far as the break point by a long-term forecasting device based on the operation plannings. The automatic reactor operation or the like is carried out based on the long-term forecasting and the short time forecasting is performed by the change in the reactor core status due to the control rod operation sequence based on the control rod pattern and the operation planning. Then, it is judged if the operation for the intended control rod is possible or not based on the result of the short time forecasting. (Aizawa, K.)

  1. Ejected control rod and rods drop measurements during Mochovce startup physical tests

    International Nuclear Information System (INIS)

    Minarcin, Miroslav; Elko, Marek

    1998-01-01

    Paper deals with measurements of asymmetric reactivity insertion into the reactor core that were carried out during physical startup tests of Mochovce Unit 1 in June 1998. Control rods worth measurements with one and two rods s tucked in upper limit and worth measurement of one control rod from group 6 'ejected' from the reactor core are discussed. During the experiments neutron flux was measured by four ionisation chambers (three of them were placed symmetrically around the reactor core). Results of measurements and influence of asymmetric reactivity influence on ionisation chambers response are presented in the paper. (Authors)

  2. Review of Current Criteria of Spent Fuel Rod Integrity during Dry Storage

    International Nuclear Information System (INIS)

    Yang, Yong Sik; Kim, Sun Ki; Bang, Je Geon; Song, Kun Woo

    2006-01-01

    A PWR spent fuel has been stored in a wet storage pool in Korea. However, the amount of spent fuel is expected to exceed the capacity of a wet storage pool within 10∼15 years. From the early 1970's, a research on the PWR spent fuel dry storage started because the dry storage system has been economical compared with the wet storage system. The dry storage technology for Zircaloy-clad fuel was assessed and licensed in many countries such as USA, Canada, FRG and Switzerland. In the dry storage system, a clad temperature may be higher than in the wet storage system and can reach up to 400 .deg.. A higher clad temperature can cause cladding failures during the period of dry storage, and thus a dry storage related research has essentially dealt with the prevention of clad degradation. It is temperature and rod internal pressure that cause cladding failures through the mechanisms such as clad creep rupture, hydride re-orientation, and stress-corrosion cracking etc.. In this paper, the current licensing criteria are summarized for the PWR spent fuel dry storage system, especially on spent fuel rod integrity. And it is investigated that an application propriety of existing criteria to Korea spent fuel dry storage system

  3. Installing and detaching apparatus for a control rod drive mechanism

    International Nuclear Information System (INIS)

    Akimoto, Seiichi; Watanabe, Mitsuhiro; Yoshida, Tomiharu; Sugaya, Jun-ichi; Saito, Takashi.

    1976-01-01

    Object: To facilitate maintenance and repair of a control rod drive mechanism. Structure: The apparatus comprises a means moving in a moving direction of a control rod within a reactor vessel, said moving means having a housing mounted thereon, a means mounted on the reactor vessel to release a connection between a control rod drive mechanism connected to the control rod and the control rod, and a means for mounting and removing a fixing means which connects the reactor vessel to the control rod drive means. With this arrangement, cooling water of high radioactivity level may not be leaked outside to thereby notably reduce dangerousness of exposure and materially cut time required for mounting and removing the control rod drive mechanism. (Ohara, T.)

  4. The modeling of fuel rod behaviour under RIA conditions in the code DYN3D

    International Nuclear Information System (INIS)

    Rohde, U.

    2001-01-01

    A description of the fuel rod behaviour and heat transfer model used in the code DYN3D for nuclear reactor core dynamic simulations is given. Besides the solution of heat conduction equations in fuel and cladding, the model comprises a detailed description of heat transfer in the gas gap by conduction, radiation and fuel-cladding contact. The gas gap behaviour is modeled in a mechanistic way taking into account transient changes of the gas gap parameters based on given conditions for the initial state. Thermal, elastic and plastic deformations of fuel and cladding are taken into account within 1D approximation. A creeping law for time-dependent estimation of plastic deformations is implemented. Metal-water reaction of the cladding material in the high temperature region is considered. The cladding-coolant heat transfer regime map covers the region from one-phase liquid convection to dispersed flow with superheated steam. Special emphasis is put on taking into account the impact of thermodynamic non-equilibrium conditions on heat transfer. For the validation of the model, experiments on fuel rod behaviour during RIAs carried out in Russian and Japanese pulsed research reactors with shortened probes of fresh fuel rods are calculated. Comparisons between calculated and measured results are shown and discussed. It is shown, that the fuel rod behaviour is significantly influenced by plastic deformation of the cladding, post crisis heat transfer with sub-cooled liquid conditions and heat release from the metal-water reaction. Numerical studies concerning the fuel rod behaviour under RIA conditions in power reactors are reported on. It is demonstrated, that the fuel rod behaviour at high pressures and flow rates in power reactors is different from the behaviour under atmospheric pressure and stagnant flow conditions in the experiments. The mechanisms of fuel rod failure for fresh and burned fuel reported from the literature can be qualitatively reproduced by the DYN3D

  5. Gas sealing welding method and device for nuclear fuel rod

    International Nuclear Information System (INIS)

    Seki, Masayuki; Nishiyama, Motokuni; Kamimura, Katsuichiro; Yagi, Eiji; Nakase, Tsuyoshi; Kobogata, Sadao; Taniguchi, Jun-ichi; Uesugi, Yoshisaku.

    1995-01-01

    An end plug and a cladding tube are held by clamping, respectively, by opposing movable electrode and static electrode. The movable electrode is forwarded toward the static electrode. The end plug and the cladding tube are abutted and held at a slight gap between their end faces. A region to be welded is surrounded by a pressurizing chamber and the side of the chamber is evacuated and He gas is filled in the cladding tube. Then, one of the electrodes is forwarded, to seal the abutted end faces of the end plug and the cladding tube. Then, pressure and welding current required for welding are applied to the abutted ends, and He gas is sealed in the vessel. The displacement of pressurization caused by slipping when the required pressure is applied to the abutted ends is detected by a sensor, and the operation of the welding control device for starting current supply is terminated by the detection signals. Abutment accuracy between the abutment of the cladding tube and the end plug as a nuclear fuel rod can be ensured, to further improve and stabilize the welding quality. (N.H.)

  6. Device and method of cooling control rod drives

    International Nuclear Information System (INIS)

    Togashi, Hidetoshi; Mase, Noriaki; Matsumura, Yuichi.

    1985-01-01

    Purpose: To prevent the generation of local temperature rise depending on the reactor core position of the control rod drives and control the temperature to an averaged state in BWR type reactors. Method: Control rod drives having a large charging length of the housing in the pressure vessel involve such a factor that the temperature of the control rod drives is increased by the synergistic effect due to the radiation heat from the reactor core and to the unevenness of the cooling water flow rate, which renders an appropriate temperature control difficult for the reactor core position. A cooling water flow rate controlling device having a restriction mechanism is disposed on the cooling water feed path for each of the hydraulic control units of the control rod drives, so that flow rate to the control rod drives is increased at the center of the reactor core and decreased at the periphery thereof. As a result, average temperature state can be set, temperature increase due to cloggings can be prevented and the thermal effect can be eliminated to thereby improve the reliability. (Moriyama, K.)

  7. Simulation of a pellet-clad mechanical interaction with ABAQUS and its verification

    International Nuclear Information System (INIS)

    Cheon, J.-S.; Lee, B.-H.; Koo, Y.-H.; Sohn, D.-S.; Oh, J.-Y.

    2003-01-01

    Pellet-clad mechanical interaction (PCMI) during power transients for MOX fuel is modelled by a FE method. The PCMI model predicts well clad elongation during power ramp and relaxation during power hold except the fuel behaviour during a power decrease. Higher fiction factor results in the earlier occurrence of PCMI and more enhanced clad elongation. The relaxation is dependent on the irradiation creep rate of the pellet and axial compressive force. Verification of the PCMI model was done using recent MOX experimental data. Temperature and clad elongation for the fuel rod can be evaluated in a reasonable way

  8. Fuel-cladding interaction. Framatome CEA experiment on pencils preirradiated in nuclear power plants

    International Nuclear Information System (INIS)

    Atabek, Rosemarie; Vignesoult, Nicole

    1979-01-01

    The study of the fuel-cladding interaction is the subject of an important joint research programme between Framatome and the CEA. Tests are performed either on whole fuel rods, not exceeding two metres in length, from BR3 or the CAP (PRISCA experiment) or on fuel rods refabricated in hot cells from fuel rods of power reactors (FABRICE experiment). The first results reveal the two mechanical and chemical aspects of the interaction phenomenon: the permissible power surge of the fuel elements passes through a minimum for an integrated fast dose (E>1MeV) of around 1.5x10 21 n/cm 2 ; a study made with the electronic microprobe and the scanning microscope shows that the Te, I and Cs fission products are the corrosive agents of the cladding [fr

  9. Implications and control of fuel-cladding chemical interaction for LMFBR fuel pin design

    International Nuclear Information System (INIS)

    Roake, W.E.

    1977-01-01

    Fuel-cladding-chemical-interaction (FCCI) is typically incorporated into the design of an LMFBR fuel pin as a wastage allowance. Several interrelated factors are considered during the evolution of an LMFBR fuel pin design. Those which are indirectly affected by FCCI include: allowable pin power, fuel restructuring, fission gas migration and release from the fuel, fuel cracking, fuel swelling, in-reactor cladding creep, cladding swelling, and the cladding mechanical strain. Chemical activity of oxygen is the most readily controlled factor in FCCI. Two methods are being investigated: control of total oxygen inventory by limiting fuel O/M, and control of oxygen activity with buffer metals

  10. Implications and control of fuel-cladding chemical interaction for LMFBR fuel pin design

    Energy Technology Data Exchange (ETDEWEB)

    Roake, W E [Westinghouse-Hanford Co., Richland, WA (United States)

    1977-04-01

    Fuel-cladding-chemical-interaction (FCCI) is typically incorporated into the design of an LMFBR fuel pin as a wastage allowance. Several interrelated factors are considered during the evolution of an LMFBR fuel pin design. Those which are indirectly affected by FCCI include: allowable pin power, fuel restructuring, fission gas migration and release from the fuel, fuel cracking, fuel swelling, in-reactor cladding creep, cladding swelling, and the cladding mechanical strain. Chemical activity of oxygen is the most readily controlled factor in FCCI. Two methods are being investigated: control of total oxygen inventory by limiting fuel O/M, and control of oxygen activity with buffer metals.

  11. Seismic analysis of hydraulic control rod driving system

    International Nuclear Information System (INIS)

    Zheng, Yanhua; Bo, Hanliang; Dong, Duo

    2002-01-01

    A simplified mathematical model was developed for the Hydraulic Control Rod Driving System (HCRDS) of a 200 MW nuclear heating reactor, which incorporated the design of its chamfer-hole step cylinder, to analyze its seismic response characteristics. The control rod motion was analyzed for different sine-wave vibration loadings on platform vibrator. The vibration frequency domain and the minimum acceleration amplitude of the control rod needed to cause the control rod to step to its next setting were compared with the design acceleration amplitude spectrum. The system design was found to be safety within the calculated limits. The safety margin increased with increasing frequency. (author)

  12. Fuel Rod Performance Evaluation of CE 16 x 16 LTA Operated at Steady State Using Transuranus and Pad Codes

    Energy Technology Data Exchange (ETDEWEB)

    Krasnorutskyy, V.; Slyeptsov, O. [Nuclear Fuel Cycle Science and Technology Establishment (NFCSTE), National Science Center, Kharkhov Institute of Physics and Technology (NSC KIPT), Kharkhov (Ukraine)

    2013-03-15

    The report performed under IAEA research contract No. 15370 describes the results of fuel performance evaluation of PWR fuel rods operated at steady state up to discharge burnup of {approx}60 GWD/MTU using the codes of TRANSURANUS designed by ITU and PAD designed by Westinghouse. The experimental results from US-PWR 16x16 LTA Extended Burnup Demonstration Program presented in the IFPE database of the OECD/NEA have been utilized for assessing the codes themselves during simulation of such properties as rod burnup, cladding corrosion, fuel densification and swelling, cladding irradiation growth and strain, FGR and RIP. The results obtained by PAD showed that the code properly simulates rod burnup, cladding irradiation growth and cladding oxidation with Standard Zr-4 material. The calculated burnup values along the fuel stack vary within {+-} 5% of the rod average burnup. The predicted values of the rod axial growth are (0.88-0.94) % and within the measured ones obtained in the burnup range of (50 - 60) GWD/MTU. With allowance made for probability of crud deposition and hot channel hydraulic diameter variation, the axial distribution of oxide layer is predicted well. For the nominal rod dimensions and operation conditions, the calculated peak oxide thickness is slightly overestimated based on the BE corrosion model parameters. The WEC fuel swelling and densification model together with the US NRC one, which is incorporated in the code, were used to assess the change in fuel pellet density ({Delta}{rho}) and fuel volume ({Delta}V{sub F}/V) vs. burnup as well as the rod void volume change, {Delta}V{sub V}/V, and the cladding outer diameter (OD) variation along the fuel stack. (author)

  13. Method for installing a control rod driving device in a reactor

    International Nuclear Information System (INIS)

    Sato, Haruo; Watanabe, Masatoshi.

    1975-01-01

    Object: To install a device using a wire rope, including individually moving up and down a control rod and a control rod driving device thereby enabling to install them within a low house and to reduce time required for installing operation. Structure: The control rod is temporarily attached to a support structure for the control rod driving device, the control rod driving device is suspended on a crane positioned upwardly of the support structure, a rope connected to the control rod driving device is connected to the control rod, a sagged portion of the rope is then wound about a rotary cylinder, the control rod is disconnected from its temporary attachment, and the wound rope is wound back while the rotary cylinder is rotated to move down the control rod. After the rope has been released from the rotary cylinder, the control rod driving device is moved down by the crane. (Kamimura, M.)

  14. Postirradiation examination results for the Irradiation Effects Test Series IE-ST-2, Rod IE-002

    International Nuclear Information System (INIS)

    Murdock, B.A.

    1977-12-01

    A postirradiation examination was conducted on a zircaloy-clad, UO 2 -fueled, pressurized water reactor (PWR) type rod which had been tested in the Power Burst Facility as part of the Irradiation Effects Test Series of the Thermal Fuels Behavior Program. The fuel rod, previously irradiated to a burnup of 15,800 MWd/t was subjected to a power ramp from 28 to 55 kW/m peak power at an average ramp rate of 4 kW/m/min. Posttest fuel restructuring and relocation, fission product redistribution, and fuel rod cladding deformation were evaluated and analyzed

  15. Lumped-parameter fuel rod model for rapid thermal transients

    International Nuclear Information System (INIS)

    Perkins, K.R.; Ramshaw, J.D.

    1975-07-01

    The thermal behavior of fuel rods during simulated accident conditions is extremely sensitive to the heat transfer coefficient which is, in turn, very sensitive to the cladding surface temperature and the fluid conditions. The development of a semianalytical, lumped-parameter fuel rod model which is intended to provide accurate calculations, in a minimum amount of computer time, of the thermal response of fuel rods during a simulated loss-of-coolant accident is described. The results show good agreement with calculations from a comprehensive fuel-rod code (FRAP-T) currently in use at Aerojet Nuclear Company

  16. Stabilizing device for control rod tip

    International Nuclear Information System (INIS)

    Verdone, G.F.

    1982-01-01

    A control rod has a spring device on its lower end for eliminating oscillatory contact of the rod against its adjacent guide tube wall. The base of the device is connected to the lower tip of the rod. A plurality of elongated extensions are cantilevered downward from the base. Each extension has a shoulder for contacting the guide tube, and the plurality of shoulders as a group has a transverse dimension that is preset to be larger than the inner diameter of the guide tube such that an interference fit is obtained when the control rod is inserted in the tube. The elongated extensions form an open-ended, substantially hollow member through which most of the liquid coolant flows, and the spaces between adjacent extensions allow the flow to bypass the shoulders without experiencing a significant pressure drop

  17. Position control device for a control rod

    International Nuclear Information System (INIS)

    Ono, Takehiko; Kusaka, Shuji.

    1976-01-01

    Purpose: To reliably prevent dangerous operation in the control of the position of the control rod by checking for abnormal pulse motor coil excitation voltage and, at the time of occurrence of abnormality, immediately holding the control rod stationary lest it should be moved to an unsafe position, this being accomplished excitation from a compensating excitation system. Constitution: In an FBR reactor, a circuit for memorizing the correct output states of individual drive signals at arbitrary instants and consequtively producing the memorized results is provided, and the output of the circuit and the actual drive signal are compared at all times to discriminate whether the drive signal being compared is normal or not. When the actual drive signal is abnormal, a series signal varying after a predetermined pattern is shifted to enable replacement of the actual drive signal, so that irrespective of whether the problem drive signal is ''on'' or ''off'', a drive signal of the correct pattern may be supplied to the pulse motor to hold the control rod and prevent it from being moved toward the dangerous side due to its own weight or other causes. (Horiuchi, T.)

  18. Initial Cladding Condition

    International Nuclear Information System (INIS)

    Siegmann, E.

    2000-01-01

    The purpose of this analysis is to describe the condition of commercial Zircaloy clad fuel as it is received at the Yucca Mountain Project (YMP) site. Most commercial nuclear fuel is encased in Zircaloy cladding. This analysis is developed to describe cladding degradation from the expected failure modes. This includes reactor operation impacts including incipient failures, potential degradation after reactor operation during spent fuel storage in pool and dry storage and impacts due to transportation. Degradation modes include cladding creep, and delayed hydride cracking during dry storage and transportation. Mechanical stresses from fuel handling and transportation vibrations are also included. This Analysis and Model Report (AMR) does not address any potential damage to assemblies that might occur at the YMP surface facilities. Ranges and uncertainties have been defined. This analysis will be the initial boundary condition for the analysis of cladding degradation inside the repository. In accordance with AP-2.13Q, ''Technical Product Development Planning'', a work plan (CRWMS M andO 2000c) was developed, issued, and utilized in the preparation of this document. There are constraints, caveats and limitations to this analysis. This cladding degradation analysis is based on commercial Pressurized Water Reactor (PWR) fuel with Zircaloy cladding but is applicable to Boiling Water Reactor (BWR) fuel. Reactor operating experience for both PWRs and BWRs is used to establish fuel reliability from reactor operation. It is limited to fuel exposed to normal operation and anticipated operational occurrences (i.e. events which are anticipated to occur within a reactor lifetime), and not to fuel that has been exposed to severe accidents. Fuel burnup projections have been limited to the current commercial reactor licensing environment with restrictions on fuel enrichment, oxide coating thickness and rod plenum pressures. The information provided in this analysis will be used in

  19. Control rod position detector for nuclear reactor

    International Nuclear Information System (INIS)

    Kudo, Mitsuru; Fujiwara, Hiroshi.

    1981-01-01

    Purpose: To improve the reliability of a control rod position detector by detecting a reactive code with a combination of control rod position change signals produced from vertical and horizontal axis decoders, generation an error signal and thus simultaneously detecting the operation of more than two lead switches. Constitution: Horizontal and vertical axis position signals responsive to changes in the control rod position are applied from lead switches connected in a predetermined matrix connection corresponding to the notches of the positions of respective position detecting probes, the reactive output from the decoder is detected by a reactive code detecting circuit, which in turn generates a fault signal, and the control rod position code converted in a notch number generating circuit is converted to a predetermined value indicating invalidity. Accordingly, a fault caused by the simultaneous operation of a plurality of failed lead switches can be effectively detected. (Yoshino, Y.)

  20. Core design and fuel rod analyses of a super fast reactor with high power density

    International Nuclear Information System (INIS)

    Ju, Haitao; Cao, Liangzhi; Lu, Haoliang; Oka, Yoshiaki; Ikejiri, Satoshi; Ishiwatari, Yuki

    2009-01-01

    A Super Fast Reactor is a pressure-vessel type, fast spectrum SuperCritical Water Reactor (SCWR) that is presently researched in a Japanese project. One of the most important advantages of the Super Fast Reactor is the higher power density compared to the thermal spectrum SCWR, which reduces the capital cost. A preliminary core has an average power density of 158.8W/cc. In this paper, the principle of improving the average power density is studied and the core design is improved. After the sensitivity analyses on the fuel rod configurations, the fuel assembly configurations and the core configurations, an improved core with an average power density of 294.8W/cc is designed by 3-D neutronic/thermal-hydraulic coupled calculations. This power density is competitive with that of typical Liquid Metal Fast Breeder Reactors (LMFBR). In order to ensure the fuel rod integrity of this core design, the fuel rod behaviors on the normal operating condition are analyzed using FEMAXI-6 code. The power histories of each fuel rod are taken from the neutronics calculation results in the core design. The cladding surface temperature histories are taken from the thermal-hydraulic calculation results in the core design. Four types of the limiting fuel rods, with the Maximum Cladding Surface Temperature (MCST), Maximum Power Peak(MPP), Maximum Discharge Burnup(MDB) and Different Coolant Flow Pattern (DCFP), are chosen to cover all the fuel rods in the core. The available design range of the fuel rod design parameters, such as initial gas plenum pressure, gas plenum position, gas plenum length, grain size and gap size, are found out in order to satisfy the following design criteria: (1) Maximum fuel centerline temperature should be less than 1900degC. (2) Maximum cladding stress in circumstance direction should be less than 100MPa. (3) Pressure difference on the cladding should be less than 1/3 of buckling collapse pressure. (4) Cumulative damage faction (CDF) of the cladding should be

  1. A systematic approach for development of a PWR cladding corrosion model

    International Nuclear Information System (INIS)

    Quecedo, M.; Serna, J.J.; Weiner, R.A.; Kersting, P.J.

    2001-01-01

    A new model for the in-reactor corrosion of Improved (low-tin) Zircaloy-4 cladding irradiated in commercial pressurized water reactors (PWRs) is described. The model is based on an extensive database of PWR fuel cladding corrosion data from fuel irradiated in commercial reactors, with a range of fuel duty and coolant chemistry control strategies which bracket current PWR fuel management practices. The fuel thermal duty with these current fuel management practices is characterized by a significant amount of sub-cooled nucleate boiling (SNB) during the fuel's residence in-core, and the cladding corrosion model is very sensitive to the coolant heat transfer models used to calculate the coolant temperature at the oxide surface. The systematic approach to developing the new corrosion model therefore began with a review and evaluation of several alternative models for the forced convection and SNB coolant heat transfer. The heat transfer literature is not sufficient to determine which of these heat transfer models is most appropriate for PWR fuel rod operating conditions, and the selection of the coolant heat transfer model used in the new cladding corrosion model has been coupled with a statistical analysis of the in-reactor corrosion enhancement factors and their impact on obtaining the best fit to the cladding corrosion data. The in-reactor corrosion enhancement factors considered in this statistical analysis are based on a review of the current literature for PWR cladding corrosion phenomenology and models. Fuel operating condition factors which this literature review indicated could have a significant effect on the cladding corrosion performance were also evaluated in detail in developing the corrosion model. An iterative least squares fitting procedure was used to obtain the model coefficients and select the coolant heat transfer models and in-reactor corrosion enhancement factors. This statistical procedure was completed with an exhaustive analysis of the model

  2. BWR control rod drive scram pilot valve monitoring system

    International Nuclear Information System (INIS)

    Soden, R.A.; Kelly, V.

    1984-01-01

    The control rod drive system in a Boiling Water Reactor is the most important safety system in the power plant. All components of the system can be verified except the solenoid operated, scram pilot valves without scramming a rod. The pilot valve mechancial works is the weak link to the control rod drive system. These pilot valves control the hydraulic system which applies pressure to the ''insert'' side of the control rod piston and vents the ''withdraw'' side of the piston causing the rods to insert during a scam. The only verification that the valve is operating properly is to scram the rod. The concern for this portion of the system is demonstrated by the high number of redundant components and complete periodic testing of the electrical circuits. The pilot valve can become hung-up through wear, fracture of internal components, mechanical binding, foreign material or chemicals left in the valve during maintenance, etc. If the valve becomes hung-up the electrical tests performed will not indicate this condition and scramming the rod is in jeopardy. Only an attempt to scram a rod will indicate the hung-up valve. While this condition exists the rod is considered inoperative. This paper describes a system developed at a nuclear power plant that monitors the pilot valves on the control rod drive system. This system utilizes pattern recognition to assure proper internal workings of the scram pilot valves to plant operators. The system is totally automatic such that each time the valve is operated on a ''half scram'', a printout is available to the operator along with light indication that each of the 370 valves (on one unit of a BWR) is operating properly. With this monitoring system installed, all components of the control rod drive system including the solenoid pilot valves can be verified as operational without scramming any rods

  3. BWR control rod drive scram pilot valve monitoring program

    International Nuclear Information System (INIS)

    Soden, R.A.; Kelly, V.

    1986-01-01

    The control rod drive system in a Boiling Water Reactor is the most important safety system in the power plant. All components of the system can be verified except the solenoid operated, scram pilot valves without scramming a rod. The pilot valve mechanical works is the weak link to the control rod drive system. These pilot valves control the hydraulic system which applies pressure to the insert side of the control rod piston and vents the withdraw side of the piston causing the rods to insert during a scram. The only verification that the valve is operating properly is to scram the rod. The concern for this portion of the system is demonstrated by the high number of redundant components and complete periodic testing of the electrical circuits. The pilot valve can become hung-up through wear, fracture of internal components, mechanical binding, foreign material or chemicals left in the valve during maintenance, etc. If the valve becomes hung-up the electrical tests performed will not indicate this condition and scramming the rod is in jeopardy. Only an attempt to scram a rod will indicate the hung-up valve. While this condition exists the rod is considered inoperative. This paper describes a system developed at a nuclear power plant that monitors the pilot valves on the control rod drive system. This system utilizes pattern recognition to assure proper internal workings of the scram pilot valves to plant operators. The system is totally automatic such that each time the valve is operated on a half scram, a printout is available to the operator along with light indication that each of the 370 valves (on one unit of a BWR) is operating properly. With this monitoring system installed, all components of the control rod drive system including the solenoid pilot valves can be verified as operational without scramming any rods

  4. Control rod driving mechanism of reactor, control device and operation method therefor

    International Nuclear Information System (INIS)

    Ariyoshi, Masahiko; Matsumoto, Fujio; Matsumoto, Koji; Kinugasa, Kunihiko; Nara, Yoshihiko; Otama, Kiyomaro; Mikami, Takao

    1998-01-01

    The present invention provides a device for and a method of directly driving control rods of an FBR type reactor linearly by a cylinder type linear motor while having a driving shaft as an electric conductor. Namely, a linear induction motor drives a driving shaft connected with a control rod and vertically moving the control rod by electromagnetic force as an electric conductor. The position of the control rod is detected by a position detector. The driving shaft is hung by a wire by way of an electromagnet which is attachably/detachably held. With such a constitution, the driving shaft connected with the control rod can be vertically moved linearly, stopped or kept. Since they can be driven smoothly at a wide range speed, the responsibility and reliability of the reactor operation can be improved. In addition, since responsibility of the control rod operation is high, scram can be conducted by the linear motor. Since the driving mechanism can be simplified, maintenance and inspection operation can be mitigated. (I.S.)

  5. Axisym finite element code: modifications for pellet-cladding mechanical interaction analysis

    International Nuclear Information System (INIS)

    Engelman, G.P.

    1978-10-01

    Local strain concentrations in nuclear fuel rods are known to be potential sites for failure initiation. Assessment of such strain concentrations requires a two-dimensional analysis of stress and strain in both the fuel and the cladding during pellet-cladding mechanical interaction. To provide such a capability in the FRAP (Fuel Rod Analysis Program) codes, the AXISYM code (a small finite element program developed at the Idaho National Engineering Laboratory) was modified to perform a detailed fuel rod deformation analysis. This report describes the modifications which were made to the AXISYM code to adapt it for fuel rod analysis and presents comparisons made between the two-dimensional AXISYM code and the FRACAS-II code. FRACAS-II is the one-dimensional (generalized plane strain) fuel rod mechanical deformation subcode used in the FRAP codes. Predictions of these two codes should be comparable away from the fuel pellet free ends if the state of deformation at the pellet midplane is near that of generalized plane strain. The excellent agreement obtained in these comparisons checks both the correctness of the AXISYM code modifications as well as the validity of the assumption of generalized plane strain upon which the FRACAS-II subcode is based

  6. Corrugated thimble tube for controlling control rod descent in nuclear reactor

    International Nuclear Information System (INIS)

    Luetzow, H.J.

    1981-01-01

    A thimble tube construction is described which will provide a controlled descent for a control rod while minimizing the reaction forces which must be absorbed by the thimble tube and reducing the possibility that a foreign particle could interfere with the free descent of a control rod. A thimble tube is formed with helically-corrugate internal walls which cooperate with a control rod contained in the tube in an emergency situation to provide a progressively-increasing hydraulic restraining force as each adjacent corrugation is encountered

  7. The modeling of fuel rod behaviour under RIA conditions in the code DYN3D

    International Nuclear Information System (INIS)

    Rohde, U.

    1998-01-01

    A description of the fuel rod behaviour and heat transfer model used in the code DYN3D for nuclear reactor core dynamic simulations is given. Besides the solution of heat conduction equations in fuel and cladding, the model comprises detailed description of heat transfer in the gas gap by conduction, radiation and fuel-cladding contact. The gas gap behaviour is modeled in a mechanistic way taking into account transient changes of the gas gap parameters based on given conditions for the initial state. Thermal, elastic and plastic deformations of fuel and cladding are taken into account within 1D approximation. Numerical studies concerning the fuel rod behaviour under RIA conditions in power reactors are reported. Fuel rod behaviour at high pressures and flow rates in power reactors is different from the behaviour under atmospheric pressure and stagnant flow conditions in the experiments. The mechanisms of fuel rod failure for fresh and burned fuel reported from the literature can be qualitatively reproduced by the DYN3D model. (author)

  8. Control rod drives

    International Nuclear Information System (INIS)

    Yamanaka, Toshikatsu.

    1979-01-01

    Purpose: To protect bellows against failures due to negative pressure to prevent the loss of pressure balance caused by the expansion of the bellows upon scram. Constitution: An expansion pipe connected to the control rod drive is driven along a guide pipe to insert a control rod into the reactor core. Expansible bellows are provided at the step between the expansion pipe and the guide pipe. Further, a plurality of bore holes or slits are formed on the side wall of the guide pipe corresponding to the expansion portion of the bellows. In such an arrangement, when the expansion pipe falls rapidly and the bellows are expanded upon scram, the volume between each of the pipes of the bellows and the guide pipe is increased to produce a negative pressure, but the effect of the negative pressure on the bellows can be eliminated by the flowing-in of coolants corresponding to that pressure through the bore holes or the slits. (Furukawa, Y.)

  9. Welding of stainless steel clad fuel rods for nuclear reactors

    International Nuclear Information System (INIS)

    Neves, Mauricio David Martins das

    1986-01-01

    This work describes the obtainment of austenitic stainless steel clad fuel rods for nuclear reactors. Two aspects have been emphasized: (a) obtainment and qualification of AISI 304 and 304 L stainless steel tubes; b) the circumferential welding of pipe ends to end plugs of the same alloy followed by qualification of the welds. Tubes with special and characteristic dimensions were obtained by set mandrel drawing. Both, seamed and seamless tubes of 304 and 304 L were obtained.The dimensional accuracy, surface roughness, mechanical properties and microstructural characteristics of the tubes were found to be adequate. The differences in the properties of the tubes with and without seams were found to be insignificant. The TIG process of welding was used. The influence of various welding parameters were studied: shielding gas (argon and helium), welding current, tube rotation speed, arc length, electrode position and gas flow. An inert gas welding chamber was developed and constructed with the aim of reducing surface oxidation and the heat affected zone. The welds were evaluated with the aid of destructive tests (burst-test, microhardness profile determination and metallographic analysis) and non destructive tests (visual inspection, dimensional examination, radiography and helium leak detection). As a function of the results obtained, two different welding cycles have been suggested; one for argon and another for helium. The changes in the microstructure caused by welding have been studied in greater detail. The utilization of work hardened tubes, permitted the identification by optical microscopy and microhardness measurements, of the different zones: weld zone; heat affected zone (region of grain growth, region of total and partial recrystallization) and finally, the zone not affected by heat. Some correlations between the welding parameters and metallurgical phenomena such as: solidification, recovery, recrystallization, grain growth and precipitation that occurred

  10. MABEL-2: a code to analyse cladding deformation in a loss-of-coolant accident

    International Nuclear Information System (INIS)

    Bowring, R.W.; Cooper, C.A.

    1982-04-01

    MABEL-2 has been developed to predict the extent of cladding deformation in PWR fuel rods during a loss of coolant accident. The user notes describe how to run MABEL. They include case preparation and input data, the job control language, a description of the output tables available, and aids to debugging. The input data and results for two sample cases are given. (U.K.)

  11. Power ramp tests of MOX fuel rods. HBWR irradiation with the instrument rig, IFA-591

    International Nuclear Information System (INIS)

    Ozawa, Takayuki; Abe, Tomoyuki

    2006-03-01

    Plutonium-uranium mixed oxide (MOX) fuel rods of instrumental rig IFA-591 were ramped in HBWR to study the Advanced Thermal Reactor (ATR) MOX fuel behavior during transient operation and to determine a failure threshold of the MOX fuel rods. Eleven segments were base-irradiated in ATR 'FUGEN' up to 18.4 GWd/t. Zirconium liner claddings were adopted for four segments of them. As the results of non-destructive post irradiation examinations (PIEs) after the base-irradiation and before the ramp tests, no remarkable behavior affecting the integrity of fuel assembly and fuel rod was confirmed. All segments to be used for the ramp tests, which consisted of the multi-step ramp tests and the single-step ramp tests, had instrumentations for in-pile measurements of cladding elongation or plenum pressure, and heated up to the maximum linear power of 58.3-68.4 kW/m without failure. The major results of ramp tests are as follows: There is no difference in PCMI behaviors between two type rods of Zry-2 and Zirconium liner claddings from the in-pile measurements of cladding elongation and plenum pressure. The computations of cladding elongation and inner pressure gave slightly lower elongation and pressure than the in-pile measurements during the ramp-test. However, the cladding relaxation during the power hold was in good agreement, and the fission gas release behavior during cooling down could be evaluated by taking into account the relaxation of contact pressure between pellet and cladding. Although the final power during IFA-591 ramp tests reached the higher linear power than the failure threshold power of UO 2 fuel rods, no indication of fuel failure was observed during the ramp tests. The cladding relaxation due to the creep deformation of the MOX pellets at high temperature could be confirmed at the power steps during the multi-ramp test. The fission gas release due to the emancipation from PCMI stress was observed during the power decreasing. The burn-up dependence could be

  12. Cladding embrittlement during postulated loss-of-coolant accidents.

    Energy Technology Data Exchange (ETDEWEB)

    Billone, M.; Yan, Y.; Burtseva, T.; Daum, R.; Nuclear Engineering Division

    2008-07-31

    The effect of fuel burnup on the embrittlement of various cladding alloys was examined with laboratory tests conducted under conditions relevant to loss-of-coolant accidents (LOCAs). The cladding materials tested were Zircaloy-4, Zircaloy-2, ZIRLO, M5, and E110. Tests were performed with specimens sectioned from as-fabricated cladding, from prehydrided (surrogate for high-burnup) cladding, and from high-burnup fuel rods which had been irradiated in commercial reactors. The tests were designed to determine for each cladding material the ductile-to-brittle transition as a function of steam oxidation temperature, weight gain due to oxidation, hydrogen content, pre-transient cladding thickness, and pre-transient corrosion-layer thickness. For short, defueled cladding specimens oxidized at 1000-1200 C, ring compression tests were performed to determine post-quench ductility at {le} 135 C. The effect of breakaway oxidation on embrittlement was also examined for short specimens oxidized at 800-1000 C. Among other findings, embrittlement was found to be sensitive to fabrication processes--especially surface finish--but insensitive to alloy constituents for these dilute zirconium alloys used as cladding materials. It was also demonstrated that burnup effects on embrittlement are largely due to hydrogen that is absorbed in the cladding during normal operation. Some tests were also performed with longer, fueled-and-pressurized cladding segments subjected to LOCA-relevant heating and cooling rates. Recommendations are given for types of tests that would identify LOCA conditions under which embrittlement would occur.

  13. Key developments of a rod control system - 15101

    International Nuclear Information System (INIS)

    Pouillot, M.; Jegou, H.; Duthou, A.

    2015-01-01

    The aim of the Rod Control System is to carry out the insertion and withdrawal of control rod clusters to provide the power required by the grid (G-mode control), to control the temperature of the reactor, or to provide negative reactivity margin when the reactor is shut down. The rod control system is not classified important for safety, but its correct operation is essential for the availability of the reactor, as the spurious drop of a single cluster usually results in a reactor trip. Rolls-Royce has been designing, manufacturing and providing rod control systems since 1977, in France, China, Belgium, Korea, and South Africa, as an original manufacturer and for modernization projects. All the corresponding nuclear units share the following features, key points for the system design: -) The power source is a three-phased 260 Vac with neutral, provided by zigzag-coupled alternators; -) The Control Rod Drive Mechanisms (CRDM) are 'three-coil type': Stationary Gripper (SG), Movable Gripper (MG) and Lift Coil (LC); -) Rod clusters are arranged in banks and sub-banks, the bank being composed of one or two sub-banks and a sub-bank is a set of 4 clusters moved simultaneously, the central cluster being an exception; and -) Most of those reactors are operated in G-mode (load following). (authors)

  14. Post-irradiation examination of Al-61 wt% U3Si fuel rods from the NRU reactor

    International Nuclear Information System (INIS)

    Sears, D.F.; Wang, N.

    1997-01-01

    This paper describes the post-irradiation examination of 4 intact low enrichment uranium (LEU) fuel rods from the national research universal (NRU) reactor at the Chalk River Laboratories of AECL. The rods were irradiated during the period 1993 through 1995, under typical driver fuel operating conditions in NRU, i.e., nominal D 2 O coolant inlet temperature 37E C, inlet pressure 654 kPa and mass flow 12.4 L/s. Irradiation exposures ranged from 147 to 251 full-power days, corresponding to 40 to 84 atom % 235 U burnup. The maximum rod power was ∼2 MW, with element linear power ratings up to 68 kW/m. Post-irradiation examinations, conducted in 1997, focused on optical metallography to measure cladding oxide thickness and fuel core and cladding microstructural examinations. The cladding oxide was approximately 24 : m thick at the mid-plane of fuel rods irradiated to 251 full-power days, with small areas up to 34 : m thick on the fins. The cladding retained significant ductility after irradiation, and its microstructure appeared unchanged. Fuel core diametral increases were small (up to 4%) and within the range previously observed on Al-61 wt% U 3 Si fuel irradiated in the NRU reactor. (author)

  15. Rapid and accurate control rod calibration measurement and analysis

    International Nuclear Information System (INIS)

    Nelson, George W.; Doane, Harry J.

    1990-01-01

    In order to reduce the time needed to perform control rod calibrations and improve the accuracy of the results, a technique for a measurement, analysis, and tabulation of integral rod worths has been developed. A single series of critical rod positions are determined at constant low power to reduce the waiting time between positive period measurements and still assure true stable reactor period data. Reactivity values from positive period measurements and control rod drop measurements are used as input data for a non-linear fit to the expected control rod integral worth shape. With this method, two control rods can be calibrated in about two hours, and integral and differential calibration tables for operator use are printed almost immediately. Listings of the BASIC computer programs for the non-linear fitting and calibration table preparation are provided. (author)

  16. Some insights into the role of axial gas flow in fuel rod behaviour during the LOCA based on Halden tests and calculations with the FALCON-PSI code

    International Nuclear Information System (INIS)

    Khvostov, G.; Wiesenack, W.; Zimmermann, M.A.; Ledergerber, G.

    2011-01-01

    Highlights: → A model for the dynamics of axial gas redistribution in fuel rods during the LOCA is developed and coupled to the FALCON fuel behaviour code. → The first verification of the model is carried out using the data of the selected Halden LOCA tests. → According to calculation, the short rods used in the Halden tests show a small effect of the delayed gas redistribution during the clad ballooning. → The predicted effect is significant in the full length rods, eventually resulting in a considerable delay of the predicted moment of cladding rupture. → The predicted delay of cladding burst may be large enough to eventually affect the efficiency of the emergency core cooling system. - Abstract: A model for axial gas flow in a fuel rod during the LOCA is integrated into the FRELAX model that deals with the thermal behaviour and fuel relocation in the fuel rods of the Halden LOCA test series. The first verification was carried out using the experimental data for the inner pressure during the gas outflow after cladding rupture in tests 3, 4 and 5. Furthermore, the modified FRELAX model is implicitly coupled to the FALCON fuel behaviour code. The analysis with the new methodology shows that the dynamics of axial gas-flow along the rod and through the cladding rupture can have a strong influence on the fuel rod behaviour. Specifically, a delayed axial gas redistribution during the heat-up phase of the LOCA can result in a drop of local pressure in the ballooned area, which is eventually able to affect the cladding burst. The results of the new model seem to be useful when analysing some of the Halden LOCA tests (showing considerable fuel relocation) and selected cases of LOCA in full-length fuel rods. While the short rods used in the Halden tests only show a very small effect of the delayed gas redistribution during the clad ballooning, such an effect is predicted to be significant in the full-scale rods - with a power peak located sufficiently away from

  17. Control rod studies in small and medium sized fast reactors

    International Nuclear Information System (INIS)

    John, T.M.; Mohanakrishnan, P.; Mahalakshmi, B.; Singh, R.S.

    1988-01-01

    Control rods are the primary safety mechanism in the operation of fast reactors. Neutronic parameters associated with the control rods have to be evaluated precisely for studying the behaviour of the reactor under various operating conditions. Control rods are strong neutron absorbers discretely distributed in the reactor core. Accurate estimation of control rod parameters demand, in principle transport theory solutions in exact geometry. But computer codes for such evaluations usually consume exorbitantly large computer time and memory for even a single parameter evaluation. During the design of reactors, evaluation of these parameters will be required for many configurations of control rods. In this paper, the method used at Indira Gandhi Centre for Atomic Research for estimating the parameters associated with control rods is presented. Diffusion theory solutions were used for computations. A scheme using three dimensional geometry represented by triangular meshes and diffusion theory solutions in few energy groups for control rod parameter evaluation is presented. This scheme was employed in estimating the control rod parameters in a 500 Mw(e) fast reactor. Error due to group collapsing is estimated by comparing with 25 group calculations in three dimensions for typical cases. (author). 5 refs, 4 figs, 3 tabs

  18. A pellet-clad interaction failure criterion

    International Nuclear Information System (INIS)

    Howl, D.A.; Coucill, D.N.; Marechal, A.J.C.

    1983-01-01

    A Pellet-Clad Interaction (PCI) failure criterion, enabling the number of fuel rod failures in a reactor core to be determined for a variety of normal and fault conditions, is required for safety analysis. The criterion currently being used for the safety analysis of the Pressurized Water Reactor planned for Sizewell in the UK is defined and justified in this paper. The criterion is based upon a threshold clad stress which diminishes with increasing fast neutron dose. This concept is consistent with the mechanism of clad failure being stress corrosion cracking (SCC); providing excess corrodant is always present, the dominant parameter determining the propagation of SCC defects is stress. In applying the criterion, the SLEUTH-SEER 77 fuel performance computer code is used to calculate the peak clad stress, allowing for concentrations due to pellet hourglassing and the effect of radial cracks in the fuel. The method has been validated by analysis of PCI failures in various in-reactor experiments, particularly in the well-characterised power ramp tests in the Steam Generating Heavy Water Reactor (SGHWR) at Winfrith. It is also in accord with out-of-reactor tests with iodine and irradiated Zircaloy clad, such as those carried out at Kjeller in Norway. (author)

  19. Model for incorporating fuel swelling and clad shrinkage effects in diffusion theory calculations (LWBR Development Program)

    International Nuclear Information System (INIS)

    Schick, W.C. Jr.; Milani, S.; Duncombe, E.

    1980-03-01

    A model has been devised for incorporating into the thermal feedback procedure of the PDQ few-group diffusion theory computer program the explicit calculation of depletion and temperature dependent fuel-rod shrinkage and swelling at each mesh point. The model determines the effect on reactivity of the change in hydrogen concentration caused by the variation in coolant channel area as the rods contract and expand. The calculation of fuel temperature, and hence of Doppler-broadened cross sections, is improved by correcting the heat transfer coefficient of the fuel-clad gap for the effects of clad creep, fuel densification and swelling, and release of fission-product gases into the gap. An approximate calculation of clad stress is also included in the model

  20. Test plan for spent fuel cladding containment credit tests

    International Nuclear Information System (INIS)

    Wilson, C.N.

    1983-11-01

    Lawrence Livermore National Laboratory has chosen Westinghouse Hanford Company as a subcontractor to assist them in determining the requirements for successful disposal of spent fuel rods in the proposed Nevada Test Site repository. An initial scoping test, with the objective of determining whether or not the cladding of a breached fuel rod can be given any credit as an effective barrier to radionuclide release, is described in this test plan. 8 references, 2 figures, 4 tables

  1. CANSWEL-2: a computer model of the creep deformation of Zircaloy cladding under loss-of-coolant accident conditions

    International Nuclear Information System (INIS)

    Haste, T.J.

    1982-07-01

    The CANSWEL-2 code models cladding creep deformation under conditions relevant to a loss-of-coolant accident (LOCA) in a pressurised water reactor (PWR). It considers in detail the centre rod of a 3 x 3 nominally square array, taking into account azimuthal non-uniformities in cladding thickness and temperature, and the mechanical restraint imposed on contact with neighbouring rods. Any of the rods in the array may assume a non-circular shape. Models are included for primary and secondary creep, dynamic phase change and superplasticity when both alpha- and beta-phase Zircaloy are present. A simple treatment of oxidation strengthening is incorporated. Account is taken of the anisotropic creep behaviour of alpha-phase Zircaloy which leads to cladding bowing. The CANSWEL-2 model is used both as a stand-alone code and also as part of the LOCA analysis code MABEL-2. (author)

  2. Influence of fuel-cladding system deviations from the model of continuous cylinders on the parameters of WWER fuel element working ability

    International Nuclear Information System (INIS)

    Scheglov, A.

    1994-01-01

    In the programs of fuel rod computation, fuel and cladding are usually presented in the form of coaxial cylinders, which can change their sizes, mechanical and thermal-physical properties. The real fuel element has some typical deviations from this continuous coaxial cylinders (CCC) model as: axial asymmetry of fuel-cladding system (due to the oval form of the cladding, cracking and other type of fuel pallet damage, axial asymmetry of the volumetric heat release), gaps between the pallets (and heat release peaking in fuel near the gap), chambers in the pallets. As a result of these deviations actual fuel rod parameters of working ability - temperature, stresses, thermal fluxes relieved from the cladding, geometry changes - in some locations can greatly vary from the ones calculated according to CCC model. The influence of these deviations is extremely important while calculating the fuel rod, because they are a part of the mechanical excess coefficient. The author reviews the influence of these factors using specific examples. He applies his own two-dimensional codes based on the Finite Elements Method for calculations of temperature fields, stresses and deformation in the fuel rod elements. It is shown that consideration of these deviations, as a rule, leads to the increase of the maximum fuel temperature in the WWER pellets (characterized by a large central hole), temperature of the cladding, thermal flux, relieved by the coolant from the cladding, and stresses in the cladding. It is necessary to consider these factors for both validation of the fuel element working ability and interpretation of the experimental results. 4 tabs., 3 figs., 5 refs

  3. Influence of fuel-cladding system deviations from the model of continuous cylinders on the parameters of WWER fuel element working ability

    Energy Technology Data Exchange (ETDEWEB)

    Scheglov, A [Russian Research Centre Kurchatov Inst., Moscow (Russian Federation)

    1994-12-31

    In the programs of fuel rod computation, fuel and cladding are usually presented in the form of coaxial cylinders, which can change their sizes, mechanical and thermal-physical properties. The real fuel element has some typical deviations from this continuous coaxial cylinders (CCC) model as: axial asymmetry of fuel-cladding system (due to the oval form of the cladding, cracking and other type of fuel pallet damage, axial asymmetry of the volumetric heat release), gaps between the pallets (and heat release peaking in fuel near the gap), chambers in the pallets. As a result of these deviations actual fuel rod parameters of working ability - temperature, stresses, thermal fluxes relieved from the cladding, geometry changes - in some locations can greatly vary from the ones calculated according to CCC model. The influence of these deviations is extremely important while calculating the fuel rod, because they are a part of the mechanical excess coefficient. The author reviews the influence of these factors using specific examples. He applies his own two-dimensional codes based on the Finite Elements Method for calculations of temperature fields, stresses and deformation in the fuel rod elements. It is shown that consideration of these deviations, as a rule, leads to the increase of the maximum fuel temperature in the WWER pellets (characterized by a large central hole), temperature of the cladding, thermal flux, relieved by the coolant from the cladding, and stresses in the cladding. It is necessary to consider these factors for both validation of the fuel element working ability and interpretation of the experimental results. 4 tabs., 3 figs., 5 refs.

  4. Method of operating control rods for BWR type reactors

    International Nuclear Information System (INIS)

    Shirakawa, Toshihisa.

    1979-01-01

    Purpose: To eliminate the danger such as fuel element failures due to rapid power increase and form a control rod pattern for obtaining a required power level in a relatively short time. Method: Control rods are disposed so as to vertically enter into and retract from the central region of each four fuel assemblies adjacent to each other respectively. Upon operation of the control rods, every other control rods in the lateral and longitudinal directions among the entire control rods that are inserted completely are extracted completely at the lower flow limit of coolants. Then, the control rods completely inserted are divided into groups inserted deeply and groups inserted less deeply. The less deeply inserted groups are extracted just before the excess of thermal limit value successively in the lower flow limit of the coolants and then the deeply inserted groups are extracted successively till a predetermined power level in the same manner. Therefore, the coolant flow to the reactor core is increased and the power level is raised. (Furukawa, Y.)

  5. Calculation method for control rod dropping time in reactor

    International Nuclear Information System (INIS)

    Nogami, Takeki; Kato, Yoshifumi; Ishino, Jun-ichi; Doi, Isamu.

    1996-01-01

    If a control rod starts dropping, the dropping speed is rapidly increased, then settled substantially constant, rapidly decreased when it reaches a dash pot. A second detection signal generated by removing an AC component from a first detection signal is differentiated twice. The time when the maximum value among the twice differentiated values is generated is determined as a time when the control rods starts dropping. The time when minimum value among the twice differentiated values is generated is determined as a time when the control rod reaches the dash pot of the reactor. The measuring time within a range from the time when the control rod starts dropping to the time when the control rod reaches the dash pot of the reactor is determined. As a result, processing for the calculation of the dropping start time and dash pot reaching time of the control rod can be automatized. Further, it is suffice to conduct differentiation twice till the reaching time, which can facilitate the processing thereby enabling to determine a reliable time range. (N.H.)

  6. In-reactor performance of methods to control fuel-cladding chemical interaction

    International Nuclear Information System (INIS)

    Weber, E.T.; Gibby, R.L.; Wilson, C.N.; Lawrence, L.A.; Adamson, M.G.

    1979-01-01

    Inner surface corrosion of austenitic stainless steel cladding by oxygen and reactive fission product elements requires a 50 μm wastage allowance in current FBR reference oxide fuel pin design. Elimination or reduction of this wastage allowance could result in better reactor efficiency and economics through improvements in fuel pin performance and reliability. Reduction in cladding thickness and replacement of equivalent volume with fuel result in improved breeding capability. Of the factors affecting fuel-cladding chemical interaction (FCCI), oxygen activity within the fuel pin can be most readily controlled and/or manipulated without degrading fuel pin performance or significantly increasing fuel fabrication costs. There are two major approaches to control oxygen activity within an oxide fuel pin: (1) control of total oxygen inventory and chemical activity (Δ anti GO 2 ) by use of low oxygen-to-metal ratio (O/M) fuel; and (2) incorporation of a material within the fuel pin to provide in-situ control of oxygen activity (Δ anti GO 2 ) and fixation of excess oxygen prior to, or in preference to reaction with the cladding. The paper describes irradiation tests which were conducted in EBR-II and GETR incorporating oxygen buffer/getter materials and very low O/M fuel to control oxygen activity in sealed fuel pins

  7. Method for automatic control rod operation using rule-based control

    International Nuclear Information System (INIS)

    Kinoshita, Mitsuo; Yamada, Naoyuki; Kiguchi, Takashi

    1988-01-01

    An automatic control rod operation method using rule-based control is proposed. Its features are as follows: (1) a production system to recognize plant events, determine control actions and realize fast inference (fast selection of a suitable production rule), (2) use of the fuzzy control technique to determine quantitative control variables. The method's performance was evaluated by simulation tests on automatic control rod operation at a BWR plant start-up. The results were as follows; (1) The performance which is related to stabilization of controlled variables and time required for reactor start-up, was superior to that of other methods such as PID control and program control methods, (2) the process time to select and interpret the suitable production rule, which was the same as required for event recognition or determination of control action, was short (below 1 s) enough for real time control. The results showed that the method is effective for automatic control rod operation. (author)

  8. Tensile and burst tests in support of the cadmium safety rod failure evaluation

    International Nuclear Information System (INIS)

    Thomas, J.K.

    1992-02-01

    The reactor safety rods may be subjected to high temperatures due to gamma heating after the core coolant level has dropped during the ECS phase of hypothetical LOCA event. Accordingly, an experimental safety rod testing subtask was established as part of a task to address the response of reactor core components to this accident. This report discusses confirmatory separate effects tests conducted to support the evaluation of failures observed in the safety rod thermal tests. As part of the failure evaluation, the potential for liquid metal embrittlement (LME) of the safety rod cladding by cadmium (Cd) -- aluminum (Al) solutions was examined. Based on the test conditions, literature data, and U-Bend tests, its was concluded that the SS304 safety rod cladding would not be subject to LME by liquid Cd-Al solutions under conditions relevant to the safety rod thermal tests or gamma heating accident. To confirm this conclusion, tensile tests on SS304 specimens were performed in both air and liquid Cd-Al solutions with the range of strain rates, temperatures, and loading conditions spanning the range relevant to the safety rod thermal tests and gamma heating accident

  9. Hydraulic system for the drive of control rod

    International Nuclear Information System (INIS)

    Niwano, Masao.

    1978-01-01

    Purpose: To remove thermal stress and improve safety by utilizing water discharged a driving device as a part of cooling water for the device upon driving of control rods. Constitution: A water drain valve is wholly closed and a flow stabilization valve is supplied with an amount of water necessary for driving control rods. Upon driving one control rod, an amount of water required for the driving is caused to flow to the relivant hydraulic control unit and the flow rate in the stabilization valve is reduced by an amount required for the driving to keep the flow rate constant in the flow control valve. Since Excess water conventionally returned to the pressure vessel is utilized as cooling water for the driving device of control rods, the pressure vessel nozzle can be saved. Accordingly, the thermal stress in the nozzle portion can be removed to significantly improve the safety. (Seki, T.)

  10. Impact loading of a BWR control rod during braking

    International Nuclear Information System (INIS)

    Heeschen, U.

    1977-01-01

    In an emergency case the control rods of a boiling water reactor are shot into the RPV from below against the weight of the rods with drive motors. According to the position of the control rods between the fuel elements the rods can reach in that case velocities up to 4 m/s. The moved masses of the control rods and of the pistons (both of them are connected by a coupling) are braked through a cup spring which transfers its forces to the RPV-bottom sphere. The spring has to be designed that in this case tthe complete kinetic energy of he control rods of about 1000Nm can be taken up. The spring power and the inertia of the moved masses cause extremely high loadings during and shortly after the impact onto the spring. The shock-like loading propagates along the whole rod at the speed of sound, and this is also the reason why the weaker cross-sections have to endure considerable short-term stress peaks. (Auth.)

  11. Models for fuel rod behaviour at high burnup

    Energy Technology Data Exchange (ETDEWEB)

    Jernkvist, Lars O.; Massih, Ali R. [Quantum Technologies AB, Uppsala Science Park, Uppsala (Sweden)

    2004-12-01

    This report deals with release of fission product gases and irradiation-induced restructuring in uranium dioxide nuclear fuel. Waterside corrosion of zirconium alloy clad tubes to light water reactor fuel rods is also discussed. Computational models, suitable for implementation in the FRAPCON-3.2 computer code, are proposed for these potentially life-limiting phenomena. Hence, an integrated model for the calculation or thermal fission gas release by intragranular diffusion, gas trapping in grain boundaries, irradiation-induced re-solution, grain boundary saturation, and grain boundary sweeping in UO{sub 2} fuel, under time varying temperature loads, is formulated. After a brief review of the status of thermal fission gas release modelling, we delineate the governing equations for the aforementioned processes. Grain growth kinetic modelling is briefly reviewed and pertinent data on grain growth of high burnup fuel obtained during power ramps in the Third Risoe Fission Gas Release Project are evaluated. Sample computations are performed, which clearly show the connection between fission gas release and gram growth as a function of time at different isotherms. Models are also proposed for the restructuring of uranium dioxide fuel at high burnup, the so-called rim formation, and its effect on fuel porosity build-up, fuel thermal conductivity and fission gas release. These models are assessed by use of recent experimental data from the High Burnup Rim Project, as well as from post irradiation examinations of high-burnup fuel, irradiated in power reactors. Moreover, models for clad oxide growth and hydrogen pickup in PWRs, applicable to Zircaloy-4, ZIRLO or M5 cladding, are formulated, based on recent in-reactor corrosion data for high-burnup fuel rods. Our evaluation of these data indicates that the oxidation rate of ZIRLO-type materials is about 20% lower than for standard Zircaloy-4 cladding under typical PWR conditions. Likewise, the oxidation rate of M5 seems to be

  12. Method of changing the control rod pattern in BWR type reactors

    International Nuclear Information System (INIS)

    Yoshida, Kenji.

    1984-01-01

    Purpose: To enable to change the control rod pattern in a short time with ease, as well as improve the availability factor of the reactor. Method: Control rods other than those being inserted into the reactor core are inserted into the reactor core to reduce the power by the reduction in the reactor core flow rate. Then, the control rod to be operated is operated partially for the change of the control rod pattern to restrict the linear heat rating of the fuels to less than 0.1 kW/ft per one hour to change the control pattern to the aimed control rod pattern. Then, the reactor core flow rate is increased after the pattern exchange for the control rod to increase the power. Since only the control rod operation is performed without adjusting the reactor core flow rate upon change of the control rod pattern, procedures can be made simply in a short time to thereby improve the availability factor of the reactor. (Moriyama, K.)

  13. Thermal hydraulic performance of naturally aspirated control rod housing assemblies

    International Nuclear Information System (INIS)

    Geiger, G.T.; Randolph, H.W.; Paik, I.K.; Foti, D.J.

    1992-01-01

    Savannah River Site reactors are comprised of heat generating fuel/target assemblies, control rods which regulate reactor power, and heavy water which acts as the coolant and as a moderator. The fuel/target assemblies are cooled by the downflow of heavy water while the control rods are cooled via upflow. Five control rods are grouped with two safety rods in seven-channel assemblies called septifoils. Under normal operating conditions, the reactor power level, radial shape flux and axial power flux are regulated by the positioning of the control rods. The control rods are solid rods of a lithium-aluminum alloy with an thin aluminum outer sheath. Lithium is a good absorber of neutrons and, thus control rod temperatures rise with reactor power. At conditions of sufficiently high reactor power and degraded coolant flow, the control rods could heat sufficiently to cause a metallurigical failure of the sheath leading to molten material coming in contact with water and the possibility of a steam explosion. An accident has been postulated as part of the analysis involving the safety upgrade of Savannah River Site reactors in which the housing is not seated on the pin. Coolant from the upflow pin would not be directed into the housing but, into the moderator space surrounding the housing. Only naturally aspirated cooling due to buoyancy effects would be available to cool the control rods and the coolant mass flow rate would drop significantly from its nominal value. In this study, the mechanisms and limits of cooling heated rods housed in an unseated septifoil are addressed. Experiments were conducted on a shortened, prototypic housing with electrically heated rods to gain an understanding of the phenomena governing the cooling in such a case and develop data which can be used to evaluate predictive models. These experiments are described, their results discussed, and the predictions of current models is presented

  14. Design requirement on KALIMER control rod assembly duct

    International Nuclear Information System (INIS)

    Hwang, W.; Kang, H. Y.; Nam, C.; Kim, J. O.; Kim, Y. J.

    1998-03-01

    This document establishes the design guidelines which are needs for designing the control rod assembly duct of the KALIMER as design requirements. it describes control rod assembly duct of the KALIMER and its requirements that includes functional requirements, performance requirements, interfacing systems, design limits and strength requirements, seismic requirements, structural requirements, environmental requirements, reliability and safety requirements, standard and codes, QA programs, and other requirements. The control rod system consists of three parts, which are drive mechanism, drive-line, and absorber bundle. This report deals with the absorber bundle and its outer duct only because the others are beyond the scope of fuel system design. The guidelines for design requirements intend to be used for an improved design of the control rod assembly duct of the KALIMER. (author). 19 refs

  15. Design requirement on KALIMER control rod assembly duct

    Energy Technology Data Exchange (ETDEWEB)

    Hwang, W.; Kang, H. Y.; Nam, C.; Kim, J. O.; Kim, Y. J

    1998-03-01

    This document establishes the design guidelines which are needs for designing the control rod assembly duct of the KALIMER as design requirements. it describes control rod assembly duct of the KALIMER and its requirements that includes functional requirements, performance requirements, interfacing systems, design limits and strength requirements, seismic requirements, structural requirements, environmental requirements, reliability and safety requirements, standard and codes, QA programs, and other requirements. The control rod system consists of three parts, which are drive mechanism, drive-line, and absorber bundle. This report deals with the absorber bundle and its outer duct only because the others are beyond the scope of fuel system design. The guidelines for design requirements intend to be used for an improved design of the control rod assembly duct of the KALIMER. (author). 19 refs.

  16. Pulsed eddy current inspection system for nondestructive examination of irradiated fuel rods

    International Nuclear Information System (INIS)

    Yancey, M.E.

    1979-01-01

    An inspection system has been developed for nondestructive examination of irradiated fuel rods utilizing pulsed eddy current techniques. The system employs an encircling type pulsed eddy current transducer capable of sensing small defects located on both the inner and outer diameter fuel rod surfaces during a single scan. Pulsed eddy current point probes are used to provide fuel rod wall thikness data and an indication of radial defect location. Two linear variable differential transformers are used to provide information on fuel rod diameter variation. A microprocessor based control system is used to automatically scan fuel rods up to 4.06 meters in length at predetermined radial locations. Defects as small as 0.005 cm deep by 0.254 cm long by 0.005 cm wide have been detected on outside diameter surfaces of a 1.43 cm outside diameter fuel rod cladding with a 0.094 cm wall thickness and 0.010 cm deep by 0.254 cm long by 0.005 cm wide on the inside diameter surface

  17. Rod consolidation at the West Valley Demonstration Project

    International Nuclear Information System (INIS)

    Bailey, W.J.

    1986-12-01

    A rod consolidation demonstration with irradiated pressurized water reactor fuel was recently conducted by personnel from Nuclear Assurance Corporation and West Valley Nuclear Services Company at the West Valley Demonstration Project in West Valley, New York. The rod consolidation demonstration involved pulling all of the fuel rods from six fuel Assemblies. In general, the rod pulling proceeded smoothly. The highest compaction ratio attained was 1:8:1. Among the total of 1074 fuel rods were some known degraded rods (they had collapsed cladding, a result of in-reactor fuel densification), but no rods were broken or dropped during the demonstration. One aim was to gather information on the effect of rod consolidation operations on the integrity of the fuel rods during subsequent handling and storage. Another goal was to collect information on the condition and handling of intact, damaged, and failed fuel that has been in storage for an extended period. 9 refs., 8 figs., 1 tab

  18. State of fuel rods spent in the VVER-1000 reactor up to a fuel burnup of 75 MW·Day/KgU

    International Nuclear Information System (INIS)

    Markov, D.; Zvir, E.; Polenok, V.; Zhitelev, V.; Strozhuk, A.; Volkova, I.

    2011-01-01

    The presented material contains the data on change in form, corrosion state and mechanical properties of fuel rod claddings, change in fuel structure and release of gaseous fission products (GFP) under the cladding. The results of PIEs of the VVER-1000 fuel rods with the high burnup of fuel (average value is 72.3 MW·day/kgU and maximum is 75 MW·day/kgU) carried out in JSC 'SSC RIAR' show that by the basic operational characteristics the lifetime of fuel rods with such burnup of fuel is not exhausted. The state of fuel rods is characterized by following key parameters. The fuel-to-cladding gap on the most part of the fuel meat is absent. With the burnup growth, diameter of the fuel rod increases due to fuel meat swelling. In so doing, the reverse strain achieves the values of 0.40-0.47 %. Ridges on the cladding are formed practically along the entire length of the fuel meat, average height of ridges makes up 25 μm, maximum - 40 μm. At burnups exceeding 55 MW·day/kgU, the rate of the fuel rod elongation is less than at low and average burnups. So if within a burnup range of 20-55 MW·day/kgU, the rate of the fuel rod elongation makes up about 0.330mm per 1 MW·day/kgU, at burnups exceeding 55 MW·day/kgU it is only 0.085mm per 1 MW·day/kgU. Corrosion state of the claddings of fuel rods with high burnup of fuel is satisfactory. The oxide film, as a rule, is uniform, dense, without cracks and exfoliation, its thickness on the external surface does not exceed 13 μm, while on the internal surface - 15 μm. Hydrogenation is insignificant, mass fraction of hydrogen does not exceed 0.01 %. Interaction of fuel rods with spacer grids does not result in significant fretting-corrosion. Based of the results of tests, short-term mechanical properties of the claddings of fuel rods with high burnup of fuel remain at high level. The state of fuel is characterized by absence of the fuel-to-cladding gap on the most part of the fuel meat, fuel is tightly fixed to the cladding

  19. Post-irradiation examination of A1-61 wt % U3Si fuel rods from the NRU reactor

    International Nuclear Information System (INIS)

    Sears, D.F.; Wang, N.

    1997-09-01

    This paper describes the post-irradiation examination of 4 intact low-enrichment uranium (LEU) fuel rods from the national research universal (NRU) reactor at the Chalk River Laboratories of AECL. The rods were irradiated during the period 1993 through 1995, under typical driver fuel operating conditions in NRU, i.e., nominal D 2 0 coolant inlet temperature 37 degrees C, inlet pressure 654 kPa and mass flow 12.4 L/s. Irradiation exposures ranged from 147 to 251 full-power days, corresponding to 40 to 84 atom % 235 U burnup. The maximum rod power was ∼2 MW, with element linear power ratings up to 68 kW/m. Post-irradiation examinations, conducted in 1997, focused on optical metallography to measure cladding oxide thickness and fuel core and cladding microstructural examinations. The cladding oxide was approximately 24 μm thick at the mid-plane of fuel rods irradiated to 251 full-power days, with small areas up to 34 μm thick on the fins. The cladding retained significant ductility after irradiation, and its microstructure appeared unchanged. Fuel core diametral increases were small (up to 4%) and within the range previously observed on A1-61 wt % U 3 Si fuel irradiated in the NRU reactor. (author)

  20. BISON Fuel Performance Analysis of IFA-796 Rod 3 & 4 and Investigation of the Impact of Fuel Creep

    Energy Technology Data Exchange (ETDEWEB)

    Wirth, Brian [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States); Terrani, Kurt A. [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States); Sweet, Ryan T. [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)

    2017-08-01

    In order to improve the accident tolerance of light water reactor (LWR) fuel, alternative cladding materials have been proposed to replace the currently used zirconium (Zr)-based alloys. Of these materials, there is a particular focus on iron-chromiumaluminum (FeCrAl) alloys because they exhibit slower oxidation kinetics in high-temperature steam than Zr-alloys. This should decrease the energy release due to oxidation and slow cladding consumption in the presence of high temperature steam. These alloys should also exhibit increased “coping time” in the event of an accident scenario by improving the mechanical performance at high temperatures, allowing greater flexibility to achieve core cooling. As a continuation of the development of these alloys, in-reactor irradiation testing of FeCrAl cladded fuel rods has started. In order to provide insight on the possible behavior of these fuel rods as they undergo irradiation in the Halden Boiling Water Reactor, engineering analysis has been performed using FeCrAl material models implemented into the BISON fuel performance code. This milestone report provides an update on the ongoing development of modeling capability to predict FeCrAl cladding fuel performance and to provide an early look at the possible behavior of planned in-reactor FeCrAl cladding experiments. In particular, this report consists of two separate analyses. The first analysis consists of fuel performance simulations of IFA-796 rod 4 and two segments of rod 3. These simulations utilize previously implemented material models for the C35M FeCrAl alloy and UO2 to provide a bounding behavior analysis corresponding to variation of the initial fuel cladding gap thickness within the fuel rod. The second analysis is an assessment of the fuel and cladding stress states after modification of the fuel creep model that is currently implemented in the BISON fuel performance code. Effects from modifying the fuel creep model were identified for the BISON simulations

  1. Annealing studies of Zircaloy-2 cladding at 580-850 deg C

    International Nuclear Information System (INIS)

    Hindle, E.D.

    1983-01-01

    For fuel rod cladding it is important to determine if prior metallurgical condition combined with irradiation damage can influence high temperature deformation, because studies of such deformation are required to produce data for the cladding ballooning models which are used in analysing loss-of-coolant (LOCA). If the behaviour of all cladding conditions during a LOCA can be represented by, say, the annealed condition, then a great deal of experimental work on a multiplicity of cladding conditions can be avoided. By examining the metallographic structure and hardness, the present study determines the time required in the range 580 to 850 deg C for returning Zircaloy cladding to the annealed condition, so that for any transient a point can be specified where the material should have annealed. An equation has been derived to give this information. (author)

  2. Dynamic insertion analysis of control rods of BWR under seismic excitation

    International Nuclear Information System (INIS)

    Nakagawa, Masaki; Koide, Yuichi; Fukushi, Naoki; Ishigaki, Hirokuni; Okumura, Kazue

    2007-01-01

    The dynamic insertion characteristics of the control rods for the boiling water reactors under the seismic excitation are investigated using non-linear analytical models. The control rod insertion capability is one of the most important items for the safety of nuclear power plants under the seismic events. Predicting the control rod insertion behavior during the earthquake is important in the course of the control rod seismic design. We developed the analytical models using the finite element method (FEM). The effect of the interaction force between the control rod and the fuel assemblies is considered in the non-linear analysis. This interaction force courses the resistance force to the control rod during its insertion behavior. The validity of analytical methods was confirmed by comparing the analytical results with the experimental ones. Using the analytical models, the effects of input seismic motion and structural parameters of the control rods and the fuel assemblies, such as the thickness of the channel box, on the insertion time are investigated. These analytical methods can predict insertion time of the control rod, and are useful for the seismic design of the control rod assemblies. (author)

  3. A two-dimensional finite element method for analysis of solid body contact problems in fuel rod mechanics

    International Nuclear Information System (INIS)

    Nissen, K.L.

    1988-06-01

    Two computer codes for the analysis of fuel rod behavior have been developed. Fuel rod mechanics is treated by a two-dimensional, axisymmetric finite element method. The program KONTAKT is used for detailed examinations on fuel rod sections, whereas the second program METHOD2D allows instationary calculations of whole fuel rods. The mechanical contact of fuel and cladding during heating of the fuel rod is very important for it's integrity. Both computer codes use a Newton-Raphson iteration for the solution of the nonlinear solid body contact problem. A constitutive equation is applied for the dependency of contact pressure on normal approach of the surfaces which are assumed to be rough. If friction is present on the contacting surfaces, Coulomb's friction law is used. Code validation is done by comparison with known analytical solutions for special problems. Results of the contact algorithm for an elastic ball pressing against a rigid surface are confronted with Hertzian theory. Influences of fuel-pellet geometry as well as influences of discretisation of displacements and stresses of a single fuel pellet are studied. Contact of fuel and cladding is calculated for a fuel rod section with two fuel pellets. The influence of friction forces between fuel and cladding on their axial expansion is demonstrated. By calculation of deformations and temperatures during an instationary fuel rod experiment of the CABRI-series the feasibility of two-dimensional finite element analysis of whole fuel rods is shown. (orig.) [de

  4. Rebirth of a control rod at the Phenix power plant

    International Nuclear Information System (INIS)

    De Carvalho, Corinne; Vignau, Bernard; Masson, Marc

    2007-01-01

    This paper outlines the operations involved in cleaning the control rod for the complementary shutdown system in the Phenix Power Plant, the French sodium-cooled fast reactor. The Phenix reactor is controlled by six control rods and a complementary shutdown system. The latter comprises a control rod and a mechanism maintaining the rod in position by means of an electromagnet. The electromagnet is continuously supplied with power and holds the rod control assembly in position by magnetisation on a plane circular surface made from pure iron. The bearing capacity of the mechanism on the rod was initially 80 daN with a rod weight of 26.3 daN. This deteriorated progressively over time. The bearing surface of the rod and the electromagnet became contaminated with a deposit of sodium oxides and metallic particles, thus creating an air gap. This reached a figure of 36 daN in 2005 and was deemed not to be sufficient to prevent the rod from dropping at the wrong time during reactor operation. The Power Plant thus decided to replace the rod mechanism in the reactor in an initial phase, followed by the control rod itself. As the Phenix Power Plant had no spare control rods left, they initiated a 'salvage' plan, over two stages, for the rod removed from the reactor and placed in the fuel storage drum: - Inspection of the bearing surface of the rod by means of a borescope to check whether the rod could be salvaged, - A cleaning operation on the bearing face and checks on the bearing capacity of the rod. The operation is subject to very stringent requirements: the rod must not be taken out of the sodium to ensure that it can be reused in the reactor. The operation must thus take place in the fuel storage drum where there are no facilities for such an operation and where operating conditions are very hostile: high temperatures (the sodium in the fuel storage drum is at a temperature of 150 deg. C, high dose rate (3 mGy/h on the bearing surface) and the bearing surface is submerged

  5. Freely suspended rod fall dampener, especially for control rod of liquid-cooled nuclear reactor

    International Nuclear Information System (INIS)

    Becvar, J.; Saroch, V.

    1977-01-01

    A shock absorber is described whose advantage is that the space required for the movement of the shock absorber in the operating travel of the system suspension rod-control rod bundle may be reduced. The design allows the automatic disconnection of the system and the removal of the suspension rod from the reactor without dismantling. The braking force reaction is transmitted to the structure above the core. The system fall energy is absorbed on the side of the suspension rod which has a bigger mass. (J.B.)

  6. Nuclear reactor internals and control rod handling device

    International Nuclear Information System (INIS)

    Betancourt, G.N.; Etzel, W.W.

    1981-01-01

    A method and apparatus for removing, in an essentially continuous operation, the control rods and the upper guide structure from a nuclear reactor vessel during refueling. The apparatus includes a rigid frame which is secured to the upper guide structure after the vessel head is removed. A platform is vertically reciprocable within the frame and is adapted to engage and lift simultaneously all control rod drive shafts to a maximum elevation within the frame. A mechanical interface between the platform and the frame is provided so that continuation of the lifting force on the platform transfers the lift force to the frame whereby the upper guide structure is lifted out of the vessel. Automatically operated stop means are provided to lock the platform and rods in the maximum elevation within the frame in order to prevent accidental dropping of the rods during transfer of the upper guide structure and control rods to a temporary storage area

  7. Regulatory perspective on incomplete control rod insertions

    International Nuclear Information System (INIS)

    Chatterton, M.

    1997-01-01

    The incomplete control rod insertions experienced at South Texas Unit 1 and Wolf Creek are of safety concern to the NRC staff because they represent potential precursors to loss of shutdown margin. Even before it was determined if these events were caused by the control rods or by the fuel there was an apparent correlation of the problem with high burnup fuel. It was determined that there was also a correlation between high burnup and high drag forces as well as with rod drop time histories and lack of rod recoil. The NRC staff initial actions were aimed at getting a perspective on the magnitude of the problem as far as the number of plants and the amount of fuel that could be involved, as well as the safety significance in terms of shutdown margin. As tests have been performed and data has been analyzed the focus has shifted more toward understanding the problem and the ways to eliminate it. At this time the staff's understanding of the phenomena is that it was a combination of factors including burnup, power history and temperature. The problem appears to be very sensitive to these factors, the interaction of which is not clearly understood. The model developed by Westinghouse provides a possible explanation but there is not sufficient data to establish confidence levels and sensitivity studies involving the key parameters have not been done. While several fixes to the problem have been discussed, no definitive fixes have been proposed. Without complete understanding of the phenomena, or fixes that clearly eliminate the problem the safety concern remains. The safety significance depends on the amount of shutdown margin lost due to incomplete insertion of the control rods. Were the control rods to stick high in the core, the reactor could not be shutdown by the control rods and other means such as emergency boration would be required

  8. Performance of cladding on MOX fuel with low 240Pu/239Pu ratio

    International Nuclear Information System (INIS)

    McCoy, K.; Blanpain, P.; Morris, R.

    2015-01-01

    The U.S. Department of Energy has decided to dispose of a portion of its surplus plutonium by reconstituting it into mixed oxide (MOX) fuel and irradiating it in commercial power reactors. As part of fuel qualification, four lead assemblies were manufactured and irradiated to a maximum fuel rod average burnup of 47.3 MWd/kg heavy metal. This was the world's first commercial irradiation of MOX fuel with a 240 Pu/ 239 Pu ratio less than 0.10. Five fuel rods with varying burnups and plutonium contents were selected from one of the assemblies and shipped to Oak Ridge National Laboratory for hot cell examination. This paper discusses the results of those examinations with emphasis on cladding performance. Exams relevant to the cladding included visual and eddy current exams, profilometry, microscopy, hydrogen analysis, gallium analysis, and mechanical testing. There was no discernible effect of the type of MOX fuel on the performance of the cladding. (authors)

  9. Control rod housing alignment apparatus

    International Nuclear Information System (INIS)

    Dixon, R.C.; Deaver, G.A.; Punches, J.R.; Singleton, G.E.; Erbes, J.G.; Offer, H.P.

    1991-01-01

    This paper discusses an alignment device for precisely locating the position of the top of a control rod drive housing from an overlying and corresponding hole and alignment pin in a core plate within a boiling water nuclear reactor. It includes a shaft, the shaft having a length sufficient to extend from the vicinity of the top of the control rod drive housing up to and through the hole in the core plate; means for registering the top of the shaft to the hole in the core plate, the registering means including means for registering with an alignment pin in the core plate adjacent the hole

  10. Control rod guide tube assemblies

    International Nuclear Information System (INIS)

    Jabsen, F.S.

    1979-01-01

    A nuclear fuel assembly including sleeves telescoped over end portions of control rod guide tubes which bear against internal shoulders of the sleeves. Upper ends of the sleeves protrude beyond a control rod guide tube spider and are locked in place by means of a resilient cellular lattice or lock that is seated in mating grooves in the outer surfaces of the sleeves. A grapple is provided for disengaging the entire lock structure spider and associated washers, springs and a grill from the end of the fuel assembly in order to enable these components to be removed and subsequently replaced on the fuel assembly after inspection and repair. (UK)

  11. Effect of laser power on clad metal in laser-TIG combined metal cladding

    Science.gov (United States)

    Utsumi, Akihiro; Hino, Takanori; Matsuda, Jun; Tasoda, Takashi; Yoneda, Masafumi; Katsumura, Munehide; Yano, Tetsuo; Araki, Takao

    2003-03-01

    TIG arc welding has been used to date as a method for clad welding of white metal as bearing material. We propose a new clad welding process that combines a CO2 laser and a TIG arc, as a method for cladding at high speed. We hypothesized that this method would permit appropriate control of the melted quantity of base metal by varying the laser power. We carried out cladding while varying the laser power, and investigated the structure near the boundary between the clad layer and the base metal. Using the laser-TIG combined cladding, we found we were able to control appropriately the degree of dilution with the base metal. By applying this result to subsequent cladding, we were able to obtain a clad layer of high quality, which was slightly diluted with the base metal.

  12. A deformation and thermodynamic model for hydride precipitation kinetics in spent fuel cladding

    International Nuclear Information System (INIS)

    Stout, R.B.

    1989-10-01

    Hydrogen is contained in the Zircaloy cladding of spent fuel rods from nuclear reactors. All the spent fuel rods placed in a nuclear waste repository will have a temperature history that decreases toward ambient; and as a result, most all of the hydrogen in the Zircaloy will eventually precipitate as zirconium hydride platelets. A model for the density of hydride platelets is a necessary sub-part for predicting Zircaloy cladding failure rate in a nuclear waste repository. A model is developed to describe statistically the hydride platelet density, and the density function includes the orientation as a physical attribute. The model applies concepts from statistical mechanics to derive probable deformation and thermodynamic functionals for cladding material response that depend explicitly on the hydride platelet density function. From this model, hydride precipitation kinetics depend on a thermodynamic potential for hydride density change and on the inner product of a stress tensor and a tensor measure for the incremental volume change due to hydride platelets. The development of a failure response model for Zircaloy cladding exposed to the expected conditions in a nuclear waste repository is supported by the US DOE Yucca Mountain Project. 19 refs., 3 figs

  13. A device for the hydraulic control of nuclear reactor control rods

    International Nuclear Information System (INIS)

    Frisch, Erling; Frisch, D.R.; Andrews, H.N.

    1974-01-01

    A device for driving and locking the control rods of a nuclear reactor. This device comprises a hydraulic driving piston mounted in a cylinder provided with a construction for absorbing shocks. The piston is provided, at is extremity, with a locking device adapted to engage a stationary lock, it being possible to control the latter for freeing said piston locking device; with such an arrangement, the control rod is normally maintained in position, and it can be freed only by a positive signal. Moreover, the control rod movements are slowed down, so as to prevent the gripping device from being damaged. This device can be used in the nuclear industry [fr

  14. On-line fuel and control rod integrity management in BWRs

    International Nuclear Information System (INIS)

    Larsson, Irina; Sihver, Lembit

    2011-01-01

    Surveillance of fuel and control rod integrity in a BWR core is essential to maintain a safe and reliable operation of a nuclear power plant. An accurate and prompt way to monitor fuel integrity in a reactor core during reactor operation is by using on-line measurements of the gamma emitting noble gas activities in the off-gas system. The integrity of control rods can be efficiently followed by on-line measurements of the helium (He) concentration in the off-gases. This method also gives information about fuel rod failures since He is used as a fill gas in the fuel rods. To survey fuel and control rod integrity during reactor operation, a system consisting of combined gamma and He on-line measurements in the off-gases should be used. Such a system can detect and follow the behavior of fuel and control rod failures. In addition, it can separate fuel failures from control rod failures since fuel rods contain both He and gamma emitting noble gases, while control rods only contain He. Moreover, the system is able to distinguish primary fuel failures from degradation of already existing ones. In this paper we present a combined system for on-line measurements of He and gamma emitting noble gases in the reactor off-gas system and measuring experiences from different BWRs. (author)

  15. A statistical analysis of pellet-clad interaction failures in water reactor fuel

    International Nuclear Information System (INIS)

    McDonald, S.G.; Fardo, R.D.; Sipush, P.J.; Kaiser, R.S.

    1981-01-01

    The primary objective of the statistical analysis was to develop a mathematical function that would predict PCI fuel rod failures as a function of the imposed operating conditions. Linear discriminant analysis of data from both test and commercial reactors was performed. The initial data base used encompassed 713 data points (117 failures and 596 non-failures) representing a wide variety of water cooled reactor fuel (PWR, BWR, CANDU, and SGHWR). When applied on a best-estimate basis, the resulting function simultaneously predicts approximately 80 percent of both the failure and non-failure data correctly. One of the most significant predictions of the analysis is that relatively large changes in power can be tolerated when the pre-ramp irradiation power is low, but that only small changes in power can be tolerated when the pre-ramp irradiation power is high. However, it is also predicted that fuel rods irradiated at low power will fail at lower final powers than those irradiated at high powers. Other results of the analysis are that fuel rods with high clad operating temperatures can withstand larger power increases that fuel rods with low clad operating temperatures, and that burnup has only a minimal effect on PCI performance after levels of approximately 10000 MWD/MTU have been exceeded. These trends in PCI performance and the operating parameters selected are believed to be consistent with mechanistic considerations. Published PCI data indicate that BWR fuel usually operates at higher local powers and changes in power, lower clad temperatures, and higher local ramp rates than PWR fuel

  16. The development and validation of control rod calculation methods

    International Nuclear Information System (INIS)

    Rowlands, J.L.; Sweet, D.W.; Franklin, B.M.

    1979-01-01

    Fission rate distributions have been measured in the zero power critical facility, ZEBRA, for a series of eight different arrays of boron carbide control rods. Diffusion theory calculations have been compared with these measurements. The normalised fission rates differ by up to about 30% in some regions, between the different arrays, and these differences are well predicted by the calculations. A development has been made to a method used to produce homogenised cross sections for lattice regions containing control rods. Calculations show that the method also reproduces the reaction rate within the rod and the fission rate dip at the surface of the rod in satisfactory agreement with the more accurate calculations which represent the fine structure of the rod. A comparison between diffusion theory and transport theory calculations of control rod reactivity worths in the CDFR shows that for the standard design method the finite mesh approximation and the difference between diffusion theory and transport theory (the transport correction) tend to cancel and result in corrections to be applied to the standard mesh diffusion theory calculations of about +- 2% or less. This result applies for mesh centred finite difference diffusion theory codes and for the arrays of natural boron carbide control rods for which the calculations were made. Improvements have also been made to the effective diffusion coefficients used in diffusion theory calculations for control rod followers and these give satisfactory agreement with transport theory calculations. (U.K.)

  17. Control rod drive mechanism

    International Nuclear Information System (INIS)

    Futatsugi, Masao; Goto, Mikihiko.

    1976-01-01

    Purpose: To provide a control rod drive mechanism using water as an operating source, which prevents a phenomenon for forming two-layers of water in the neighbourhood of a return nozzle in a reactor to limit formation of excessive thermal stress to improve a safety. Constitution: In the control rod drive mechanism of the present invention, a heating device is installed in the neighbourhood of a pressure container for a reactor. This heating device is provided to heat return water in the reactor to a level equal to the temperature of reactor water thereby preventing a phenomenon for forming two-layers of water in the reactor. This limits formation of thermal stress in the return nozzle in the reactor. Accordingly, it is possible to minimize damages in the return nozzle portion and yet a possibility of failure in reactor water. (Kawakami, Y.)

  18. Experimental study of effect of initial clad temperature on reflood phenomena during PWR-LOCA

    International Nuclear Information System (INIS)

    Sugimoto, Jun; Murao, Yoshio

    1983-01-01

    Integral system tests with the Cylindrical Core Test Facility (CCTF) were performed to investigate the effect of the initial clad temperature on the reflood phenomena in a PWR-LOCA. The initial peak clad temperatures in these three tests were 871, 968 and 1,047K, respectively. The feedback of the system on the core inlet mass flow rate was estimated to be little influenced by the variation of the initial clad temperature except for the first 20s in the transient. The observed temperature rise from the reflood initiation was lower with the higher initial clad temperature. This qualitatively agreed with the results of the small scale forced feed reflood experiments. However, the magnitude of the temperature rise in CCTF was significantly low due to the high initial core inlet mass flow rate. Also observed were the multi-dimensional thermal behaviors for the three cases in the CCTF wide core. The analysis codes REFLA and TRAC reasonably predicted the effect of the initial clad temperature on the core thermo-hydraulics under the simulated core inlet flow conditions. However, the calculated temperature rise of the maximum powered rod based on the one-dimensional core analysis was higher than that of the average powered rod, which contradicts the tendency observed in CCTF tests. (author)

  19. Models of multi-rod code FRETA-B for transient fuel behavior analysis

    International Nuclear Information System (INIS)

    Uchida, Masaaki; Otsubo, Naoaki.

    1984-11-01

    This paper is a final report of the development of FRETA-B code, which analyzes the LWR fuel behavior during accidents, particularly the Loss-of-Coolant Accident (LOCA). The very high temperature induced by a LOCA causes oxidation of the cladding by steam and, as a combined effect with low external pressure, extensive swelling of the cladding. The latter may reach a level that the rods block the coolant channel. To analyze these phenomena, single-rod model is insufficient; FRETA-B has a capability to handle multiple fuel rods in a bundle simultaneously, including the interaction between them. In the development work, therefore, efforts were made for avoiding the excessive increase of calculation time and core memory requirement. Because of the strong dependency of the in-LOCA fuel behavior on the coolant state, FRETA-B has emphasis on heat transfer to the coolant as well as the cladding deformation. In the final version, a capability was added to analyze the fuel behavior under reflooding using empirical models. The present report describes the basic models of FRETA-B, and also gives its input manual in the appendix. (author)

  20. Control rod guide tube cleaning device

    International Nuclear Information System (INIS)

    Tsuji, Tadashi; Shiota, Yoshiaki.

    1990-01-01

    Since there was no exclusive device for cleaning control rods, no effective cleaning could not be conducted and there was a possibility that obstacles may not be recovered. Then, there are disposed a first pump for supplying pressurized water, a spray nozzle for forming a swirling flow in a control rod guide tube, a second pump for pressurizing water introduced by a sucking pipeline and a collecting device for recovering obstacles intruding to water from the second pump. The pressurized water supplied from the first pump is introduced to a head passing through a blowing pipe and jetted from the spray nozzle to the control rod guide tube. In this case, a swirling stream occurs and obstacles in the control guide tube are mixed into water. The water containing the obstacles passes from the sucking port through a pipeline, introduced to the second pump and recovered to the collecting device. Since there is no water staying portion upon cleaning operation, the obstacles accumulating over the entire region of the bottom of the guide tube can be recovered reliably and efficiently. (N.H.)

  1. The analytic method for calculating the control rod worth

    International Nuclear Information System (INIS)

    Kim, Han Gon; Lee, Byeong Ho; Chang, Soon Heung

    1989-01-01

    We calculated the control rod worth in this paper. To avoid complexity, we did not consider burnable poisons and soluble boron. The system was localized within one assembly. The control rod was treated as not an absorber but an another boundary. Thus all of the group constants were unchanged before and after control rod insertion. And we discussed the method for calculation of the reactivity of the whole core

  2. Linear motion device and method for inserting and withdrawing control rods

    International Nuclear Information System (INIS)

    Smith, J. E.

    1984-01-01

    A linear motion device, more specifically a control rod drive mechanism (CRDM) for inserting and withdrawing control rods into a reactor core, is capable of independently and sequentially positioning two sets of control rods with a single motor stator and rotor. The CRDM disclosed can control more than one control rod lead screw without incurring a substantial increase in the size of the mechanism

  3. Effects of thermocouple installation and location on fuel rod temperature measurements

    International Nuclear Information System (INIS)

    McCormick, R.D.

    1983-01-01

    This paper describes the results of analyses of nuclear fuel rod cladding temperature data obtained during in-reactor experiments under steady state and transient (simulated loss-of-coolant accident) operating conditions. The objective of the analyses was to determine the effect of thermocouple attachment method and location on measured thermal response. The use of external thermocouples increased the time to critical heat flux (CHF), reduced the blowdown peak temperature, and enhanced rod quench. A comparison of laser welded and resistance welded external thermocouple responses showed that the laser welding technique reduced the indicated cladding steady state temperatures and provided shorter time-to-CHF. A comparison of internal welded and embedded thermocouples indicated that the welded technique gave generally unsatisfactory cladding temperature measurements. The embedded thermocouple gave good, consistent results, but was possibly more fragile than the welded thermocouples. Detailed descriptions of the thermocouple designs, attachment methods and locations, and test conditions are provided

  4. FRAPCON analysis of cladding performance during dry storage operations

    Energy Technology Data Exchange (ETDEWEB)

    Richmond, David J.; Geelhood, Kenneth J.

    2018-03-01

    There is an increasing need in the U.S. and around the world to move used nuclear fuel from wet storage in fuel pools to dry storage in casks stored at independent spent fuel storage installations (ISFSI) or interim storage sites. The NRC limits cladding temperature to 400°C while maintaining cladding hoop stress below 90 MPa in an effort to avoid radial hydride reorientation. An analysis was conducted with FRAPCON-4.0 on three modern fuel designs with three representative used nuclear fuel storage temperature profiles that peaked at 400 °C. Results were representative of the majority of U.S. LWR fuel. They conservatively showed that hoop stress remains below 90 MPa at the licensing temperature limit. Results also show that the limiting case for hoop stress may not be at the highest rod internal pressure in all cases but will be related to the axial temperature and oxidation profiles of the rods at the end of life and in storage.

  5. Results of examinations of safety experimental rods of trap-like type irradiated in the BN-600 reactor

    International Nuclear Information System (INIS)

    Tarasikov, V.P.; Voznesenskij, R.M.; Rudenko, V.A.

    2001-01-01

    The results of post-irradiation examination are reported for three trap-like scram rods having been in operation in BN-600 reactor for 311, 331 and 348 EFPD (effective full power days). Compacted boron carbide enriched with 80 at.% 10 B is used as an absorber, zirconium hydride serves as a moderator; cladding are fabricated from steel 06Kh16N15M3B. The results obtained show that two zones are formed in the absorber material which are different in fracture mode and positioned at different distances from the moderator. Radiation damages of steel cladding are noted to be arranged nonuniformly through the height of the rod. The cladding-absorber interaction manifests itself in various ways, this is associated with various absorber burnups. The area of cladding-zirconium hydride interaction constitutes ∼ 30-80 μm. The swelling of the moderator is 4-5% and does not result in a loss of a cladding-moderator clearance [ru

  6. Multi-rod burst test under a loss-of coolant accident condition, (4)

    International Nuclear Information System (INIS)

    Otomo, Takashi; Hashimoto, Masao; Kawasaki, Satoru; Furuta, Teruo; Uetsuka, Hiroshi

    1983-06-01

    Multi-rod burst test of No.7808 bundle was performed in steam to estimate quantitative coolant flow channel restriction caused by the ballooning of zircaloy claddings in a fuel assembly during a LOCA transient in LWRs. The test was conducted under the condition that the initial internal pressure in each rod was 35kg/cm 2 (RT) and the heating rate was 9 0 C/s in steam with flow rate of 0.4g/cm 2 .min. The following results were obtained; (1) Maximum and burst pressures in rods were in the range 45 to 48kg/cm 2 and 41 to 45kg/cm 2 , respectively. The burst temperature of cladding were estimated to be 850 to 880 0 C. (2) Axial portions of tubes with greater than 34% strain were observed in the range 0 to 40mm in most rod. The mean length was 19mm in the bundle. (3) The degree of maximum increase in cross-sectional area is 54.2% in the bundle(7 x 7) and 66.9% in the internal rods(5 x 5). (4) Maximum channel area restriction was 40.5% in the bundle(7 x 7) and 51.4% in the internal rods(5 x 5). (author)

  7. Effect of PWR Re-start ramp rate on pellet-cladding interactions

    International Nuclear Information System (INIS)

    Yagnik, S.K.; Chang, B.C.; Sunderland, D.J.

    2005-01-01

    To mitigate pellet-cladding interaction (PCI) leading to fuel rod failures, fuel suppliers specify reactor power ramp rate limitations during reactor start-up after an outage. Typical re-start ramp rates are restricted and range between 3-4% per hour of full reactor power above a threshold power level. Relaxation of threshold power and ramp rate restrictions has the potential to improve plant economics. The paper will compare known re-start power ascension procedures employed in the US, German, French and Korean PWRs after a refuelling outage. A technical basis for optimising power ascension procedures during reactor start-up can be developed using analytical modelling. The main objective of the modelling is to determine the potential for PCI failure for various combinations of threshold power levels and ramp rate levels. A key element of our analysis is to estimate the decrease in margin to cladding failure by ISCC based on a time-temperature-stress failure criterion fashioned Act a cumulative cladding damage index. The analysis approach and the cladding damage model will be described and the results from three case studies based on the FALCON fuel rod behaviour code will be reported. We conclude that the PCI behaviour is more affected by ramp rate and threshold power than by the fuel design and that the fuel power history is the most important parameter. (authors)

  8. Linear motion device and method for inserting and withdrawing control rods

    Science.gov (United States)

    Smith, J.E.

    Disclosed is a linear motion device and more specifically a control rod drive mechanism (CRDM) for inserting and withdrawing control rods into a reactor core. The CRDM and method disclosed is capable of independently and sequentially positioning two sets of control rods with a single motor stator and rotor. The CRDM disclosed can control more than one control rod lead screw without incurring a substantial increase in the size of the mechanism.

  9. Thermal gradient effects on the oxidation of Zircaloy fuel cladding

    International Nuclear Information System (INIS)

    Klein, A.C.; Reyes, J.N. Jr.; Maguire, M.A.

    1990-01-01

    A Thermal Gradient Test Facility (TGTF) has been designed and constructed to measure the thermal gradient effect on pressurized water reactor (PWR) fuel rod cladding. The TGTF includes a heat flux simulator assembly capable of producing a wide range of PWR operating conditions including water flow velocities and temperatures, water chemistry conditions, cladding temperatures, and heat fluxes ranging to 160 W/cm 2 . It is fully instrumented including a large number of thermocouples both inside the water flow channel and inside the cladding. Two test programs are in progress. First, cladding specimens are pre-oxidized in air at 500 deg. C and in 400 deg. C steam for various lengths of time to develop a range of uniform oxide thicknesses from 1 to 60 micrometers. The pre-oxidized specimens are placed in the TGTF to characterize the oxide thermal conductivity under a variety of water flow and heat flux conditions. Second, to overcome the long exposure times required under typical PWR conditions a series of tests with the addition of high concentrations of lithium hydroxide to the water are being considered. Static autoclave tests have been conducted with lithium hydroxide concentrations ranging from 0 to 2 moles per liter at 300, 330, and 360 deg. C for up to 36 hours. Results for zircaloy-4 show a considerable increase in the weight gain for the exposed samples with oxidation rate enhancement factors as high as 70 times that of pure water. Operation of the TGTF with elevated lithium hydroxide levels will yield real-time information concerning the effects of a heat flux on the oxidation kinetics of zircaloy fuel rod cladding. (author). 5 refs, 5 figs, 2 tabs

  10. Investigation of water-logged spent fuel rods under dry storage conditions

    International Nuclear Information System (INIS)

    Kohli, R.; Pasupathi, V.

    1986-09-01

    Tests were conducted to determine the amount of moisture contained in breached, water-logged spent fuel rods and the rate of release. Two well-characterized BWR fuel rods with reactor-induced breaches were tested in a hot cell. These rods contained approximately 6 to 10 g of moisture, most of which was released during heating tests simulating normal cask drying operations. Additional testing with two intentionally defected fuel rods (BWR and PWR) was performed to evaluate the effect of the cladding breach on migration of moisture along the length of the fuel rod. The results showed that the moisture released from reactor-breached spent fuel rods was insufficient to cause degradation of fuel or dry storage system components

  11. A model for asymmetric ballooning and analyses of ballooning behaviour of single rods with probabilistic methods

    International Nuclear Information System (INIS)

    Keusenhoff, J.G.; Schubert, J.D.; Chakraborty, A.K.

    1985-01-01

    Plastic deformation behaviour of Zircaloy cladding has been extensively examined in the past and can be described best by a model for asymmetric deformation. Slight displacement between the pellet and cladding will always exist and this will lead to the formation of azimuthal temperature differences. The ballooning process is strongly temperature dependent and, as a result of the built up temperature differences, differing deformation behaviours along the circumference of the cladding result. The calculated ballooning of cladding is mainly influenced by its temperature, the applied burst criterion and the parameters used in the deformation model. All these influencing parameters possess uncertainties. In order to quantify these uncertainties and to estimate distribution functions of important parameters such as temperature and deformation the response surface method was applied. For a hot rod the calculated standard deviation of cladding temperature amounts to 50 K. From this high value the large influence of the external cooling conditions on the deformation and burst behaviour of cladding can be estimated. In an additional statistical examination the parameters of deformation and burst models have been included and their influence on the deformation of the rod has been studied. (author)

  12. Knowledge based system for control rod programming of BWRs

    International Nuclear Information System (INIS)

    Fukuzaki, Takaharu; Yoshida, Ken-ichi; Kobayashi, Yasuhiro

    1988-01-01

    A knowledge based system has been developed to support designers in control rod programming of BWRs. The programming searches through optimal control rod patterns to realize safe and effective burning of nuclear fuel. Knowledge of experienced designers plays the main role in minimizing the number of calculations by the core performance evaluation code. This code predicts power distibution and thermal margins of the nuclear fuel. This knowledge is transformed into 'if-then' type rules and subroutines, and is stored in a knowledge base of the knowledge based system. The system consists of working area, an inference engine and the knowledge base. The inference engine can detect those data which have to be regenerated, call those subroutine which control the user's interface and numerical computations, and store competitive sets of data in different parts of the working area. Using this system, control rod programming of a BWR plant was traced with about 500 rules and 150 subroutines. Both the generation of control rod patterns for the first calculation of the code and the modification of a control rod pattern to reflect the calculation were completed more effectively than in a conventional method. (author)

  13. Fuel assemblies for PWR type reactors: fuel rods, fuel plates. CEA work presentation

    International Nuclear Information System (INIS)

    Delafosse, Jacques.

    1976-01-01

    French work on PWR type reactors is reported: basic knowledge on Zr and its alloys and on uranium oxide; experience gained on other programs (fast neutron and heavy water reactors); zircaloy-2 or zircaloy-4 clad UO 2 fuel rods; fuel plates consisting of zircaloy-2 clad UO 2 squares of thickness varying between 2 and 4mm [fr

  14. The results of postirradiation examinations of VVER-1000 and VVER-440 fuel rods

    Science.gov (United States)

    Dubrovin, K. P.; Ivanov, E. G.; Strijov, P. N.; Yakovlev, V. V.

    1991-02-01

    The paper presents the results of postirradiation examination of the fuel rods having different fuel-cladding gaps, pellet densities, pellet inner diameters and so on. The fuel rods were irradiated in the material science reactor (MR) of the Kurchatov Institute of Atomic Energy and at 4 unit of the Novo-Voronezh nuclear powerplant. Some data on fission gas release and rod geometry and compared with computer code predictions.

  15. Inlet for fuel assembly having finger control rods

    International Nuclear Information System (INIS)

    Berglund, A.; Suvanto, A.; Tornblom, L.

    1975-01-01

    A nuclear reactor with vertically arranged fuel assemblies positioned on supporting members and with control rods displaceably arranged in guide tubes between the fuel rods inside the fuel assemblies is described. The supporting plate is provided with a transverse end piece with throttling means for the liquid flow which passes from below up through the supporting member and past the fuel rods in the fuel assembly. The inlets for the guide tubes for the control rods are located below the end piece and the throttling means. In this way a higher pressure prevails at the inlet to the guide tubes than above the end piece, so that a stronger flow of coolant is produced through guide tubes than through the fuel assembly. (U.S.)

  16. Pre-test prediction and post-test analysis of PWR fuel rod ballooning in the MT-3 in-pile LOCA simulation experiment in the NRU reactor

    International Nuclear Information System (INIS)

    Donaldson, A.T.; Horwood, R.A.; Healey, T.

    1983-01-01

    The USNRC and the UKAEA have jointly funded a series of in-pile LOCA simulation experiments in the Canadian NRU reactor in order to secure further information on the thermal hydraulic and clad deformation response of PWR fuel rod bundles. Test MT-3 in the series was performed using reflood rate and rod internal pressure conditions specified by the UK nuclear industry. The parameters were selected to ensure the development of a near-isothermal clad temperature history during which zircaloy was required to balloon and rupture near the alpha-alpha/beta phase transition. Specification of the reflood rate conditions was assisted by the performance of a precursor test on an unpressurised rod bundle and by complementary application of appropriate thermal hydraulic analyses. Identification of the rod internal pressure needed to cause ballooning and rupture was achieved using a creep deformation model, BALLOON, in conjunction with the clad thermal history defined by the prior thermal hydraulic test. This paper presents the basis of the BALLOON analysis and describes its application in calculating the fill gas pressure for rods MT-3, their axial ballooning profile and the clad temperature at peak radial strain elevations. (author)

  17. SUMMARY OF CHARACTERISATION DATA ON CLADDING MATERIALS USED IN THE CORROSION TEST IFA-638 AND IN THE CREEP TEST IFA-617

    International Nuclear Information System (INIS)

    Nakata, M.; Hauso, E.

    1998-10-01

    Modern PWR cladding materials are being tested in two joint programme tests; the cladding corrosion test IFA-638 and in the creep test IFA-617. The materials for the two tests, have been provided by four organisations: ABB-Atom, ENUSA, Framatome and Mitsubishi Heavy Industries. This report gives an overview of the different materials being tested as fuelled test rods and unfuelled cladding coupons in IFA-638. For IFA-638, cladding has been used for fabrication of both fresh and pre-irradiated test rods. The coupon materials, all in the unirradiated condition, comprise a range of alloys of different chemical composition, heat treatment, pre-filming and /or pre-hydriding treatment. Four pre-irradiated cladding materials of the same type of those used in IFA-638, have also been used to prepare the four fuelled subsegments that are being studied in the creep rig IFA-617. All currently available information related to the IFA-638 and IFA-617 material characterisation and properties are summarised in this report. (author)

  18. Fuel Performance Calculations for FeCrAl Cladding in BWRs

    Energy Technology Data Exchange (ETDEWEB)

    George, Nathan [Univ. of Tennessee, Knoxville, TN (United States). Dept. of Nuclear Engineering; Sweet, Ryan [Univ. of Tennessee, Knoxville, TN (United States). Dept. of Nuclear Engineering; Maldonado, G. Ivan [Univ. of Tennessee, Knoxville, TN (United States). Dept. of Nuclear Engineering; Wirth, Brian D. [Univ. of Tennessee, Knoxville, TN (United States). Dept. of Nuclear Engineering; Powers, Jeffrey J. [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States); Worrall, Andrew [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)

    2015-01-01

    This study expands upon previous neutronics analyses of the reactivity impact of alternate cladding concepts in boiling water reactor (BWR) cores and directs focus toward contrasting fuel performance characteristics of FeCrAl cladding against those of traditional Zircaloy. Using neutronics results from a modern version of the 3D nodal simulator NESTLE, linear power histories were generated and supplied to the BISON-CASL code for fuel performance evaluations. BISON-CASL (formerly Peregrine) expands on material libraries implemented in the BISON fuel performance code and the MOOSE framework by providing proprietary material data. By creating material libraries for Zircaloy and FeCrAl cladding, the thermomechanical behavior of the fuel rod (e.g., strains, centerline fuel temperature, and time to gap closure) were investigated and contrasted.

  19. Expert system for control rod programming of boiling water reactors

    International Nuclear Information System (INIS)

    Fukuzaki, T.; Yoshida, K.; Kobayashi, Y.; Matsuura, H.; Hoshi, K.

    1986-01-01

    Control rod programming, one of the main tasks in reactor core management of boiling water reactors (BWRs), can be successfully accomplished by well-experienced engineers. By use of core performance evaluation codes, their knowledge plays the main role in searching through optimal control rod patterns and exposure points for adjusting notch positions and exchanging rod patterns. An expert system has been developed, based on a method of knowledge engineering, to lighten the engineer's load in control rod programming. This system utilizes an inference engine suited for planning/designing problems, and stores the knowledge of well-experienced engineers in its knowledge base. In this report, the inference engine, developed considering the characteristics of the control rod programming, is introduced. Then the constitution and function of the expert system are discussed

  20. PIN99W, Modelling of VVER and PWR Fuel Rod Thermomechanical Behaviour

    International Nuclear Information System (INIS)

    Valach, M.; Strizhov, P.; Svoboda, R.

    2000-01-01

    1 - Description of program or function: The Code is developed to describe fuel rod thermomechanical behaviour in operational conditions. The main goal of this code is to calculate fuel temperature, gap conductivity, fission gas release and inner gas pressure. 2 - Methods: - fuel rod temperature response is solved by using one-dimensional finite element method combined with weighted residuals method; - the code involves models describing physical phenomena typical for the fuel irradiated in Light Water Power Reactors (densification, restructuring, fission gas release, swelling and relocation) ; - this code is updated and improves PIN-micro code. 3 - Restrictions on the complexity of the problem: - simplified mechanistic solution; - only steady-state solution; - no cladding failure criterion; - no model for axial fuel-cladding interaction

  1. Water pressure control device for control rod drive

    International Nuclear Information System (INIS)

    Sato, Hideyuki.

    1981-01-01

    Purpose: To minimize the fluctuations in the reactor water level upon occurrence of abnormality by inputting the level signal of the reactor to an arithmetic unit for controlling the pressure of control rod drive water to thereby enable effective reactor level control. Constitution: Signal from a flow rate transmitter is inputted into an arithmetic unit to perform constant flow rate control upon normal operation. While on the other hand, if abnormality occurs such as feedwater pump trips, the arithmetic unit is switched from the constant flow rate control to the reactor water level control. Reactor water level signal is inputted into the arithmetic unit and the control valve is most suitably controlled, whereby water is fed from CST to the reactor by way of control rod drive water system to secure the reactor water level if feedwater to the reactor is interrupted by loss of coolants on the feedwater system. Since this enables to minimize the fluctuations in the reactor water level upon abnormality, the reactor water level can be controlled most suitably by the reactor water level signal. (Moriyama, K.)

  2. Thermal performance of a buried nuclear waste storage container storing a hybrid mix of PWR and BWR spent fuel rods

    International Nuclear Information System (INIS)

    Johnson, G.L.

    1991-11-01

    Lawrence Livermore National Laboratory will design, model, and test nuclear waste packages for use at the Nevada Nuclear Waste Storage Repository at Yucca Mountain, Nevada. On such package would store tightly packed spent fuel rods from both pressurized and boiling water reactors. The storage container provides the primary containment of the nuclear waste and the spent fuel rod cladding provides secondary containment. A series of transient conduction and radiation heat transfer analyses was run to determine for the first 1000 yr of storage if the temperature of the tuff at the borehole wall ever falls below 97 degrees C and whether the cladding of the stored spent fuel ever exceeds 350 degrees C. Limiting the borehole to temperatures of 97 degrees C or greater helps minimize corrosion by assuring that no condensed water collects on the container. The 350 degrees C cladding limit minimizes the possibility of creep- related failure in the spent fuel rod cladding. For a series of packages stored in a 8 x 30 m borehole grid where each package contains 10-yr-old spent fuel rods generating 4.74 kW or more, the borehole wall stays above 97 degrees C for the full 10000-yr analysis period. For the 4.74-kW load, the peak cladding temperature rises to just below the 350 degrees C limit about 4 years after emplacement. If the packages are stored using the spacing specified in the Site Characterization Plan (15 ft x 126 ft), a maximum of 4.1 kW per container may be stored. If the 0.05-m-thick void between the container and the borehole wall is filled with loosely packed bentonite, the peak cladding temperature rises more than 40 degrees C above the allowed cladding limit. In all cases the dominant heat transfer mode between container components is thermal radiation

  3. Review of FFTF and CRBRP control rod systems designs

    International Nuclear Information System (INIS)

    Pitterle, T.A.; Lagally, H.O.

    1977-01-01

    The evolution of the primary control rod system design for FFTF and CRBR, beginning with the initial choice of the basic concepts, is described. The significant component and systems tests are reviewed together with the test results which referenced the development of the CRBR primary control rod system design. Modifications to the concepts and detail designs of the FFTF control rod system were required principally to satisfy the requirements of CRBR, and at the same time incorporating design refinements shown desirable by the tests

  4. Thermal creep behavior of N36 zirconium alloy cladding tube

    International Nuclear Information System (INIS)

    Wang, P.; Zhao, W.; Dai, X.

    2015-01-01

    N36 is an alloy containing Zr, Sn, Nb and Fe that is developed by China as a superior cladding material to meet the performance of PWR fuel assembly at the maximum fuel rod burn-up. The creep characteristics of N36 zirconium alloy cladding tube were investigated at temperature from 593 K to 723 K with stress ranging from 20 MPa to 160 MPa. Transitions in creep mechanisms were noted, showing the distinct three rate-controlled creep mechanisms for the alloy at test conditions. In the region of low stresses with stress exponent n ∼ 1 and activation energy Q ∼ (104±4) kJ.mol -1 , Coble creep, based on diffusion of materials through grain boundaries, is the dominant rate-controlling mechanism, which contributes to the creep deformation. The formation of slip bands acts as an accommodation mechanism. In the region of middle stress with stress exponent n ∼ 3 and activation energy Q ∼ (195±7) kJ.mol -1 , micro-creep, caused by viscous gliding of dislocations due to the interaction of O atoms with dislocations, controls the deformation. In the high stress region with stress exponent n ∼ 5-6 and activation energy Q ∼ (210±10) kJ.mol -1 , two mechanisms of the climb of edge dislocations (EDC) and the motion of jogged screw dislocation (MJS) contribute to rate controlling process. In test conditions N36 alloy cladding tube behaves a type of creep similar to that noted in class-I (A) alloys

  5. Review of control rod calibration methods for irradiated AGRs

    Energy Technology Data Exchange (ETDEWEB)

    Telford, A. R.R.

    1975-10-15

    Methods of calibrating control rods with particular reference to irradiated CAGR are surveyed. Some systematic spatial effects are found and an estimate of their magnitude made. It is concluded that control rod oscillation provides a promising method of calibrating rods at power which is as yet untried on CAGR. Also the rod drop using inverse kinetics provides a rod calibration but spatial effects may be large and these would be difficult to correct theoretically. The pulsed neutron technique provides a calibration route with small errors due to spatial effects provided a suitable K-tube can be developed. The xenon transient method is shown to have spatial effects which have not needed consideration in earlier reactors but which in CAGR would need very careful evaluation.

  6. Reactor core and control rod assembly in FBR type reactor

    International Nuclear Information System (INIS)

    Fujimura, Koji; Kawashima, Katsuyuki; Itooka, Satoshi.

    1993-01-01

    Fuel assemblies and control rod assemblies are attached respectively to reactor core support plates each in a cantilever fashion. Intermediate spacer pads are disposed to the lateral side of a wrapper tube just above the fuel rod region. Intermediate space pads are disposed to the lateral side of a control rod guide tube just above a fuel rod region. The thickness of the intermediate spacer pad for the control rod assembly is made smaller than the thickness of the intermediate spacer pad for the fuel assembly. This can prevent contact between intermediate spacer pads of the control guide tube and the fuel assembly even if the temperature of coolants is elevated to thermally expand the intermediate spacer pad, by which the radial displacement amount of the reactor core region along the direction of the height of the control guide tube is reduced substantially to zero. Accordingly, contribution of the control rod assembly to the radial expansion reactivity can be reduced to zero or negative level, by which the effect of the negative radial expansion reactivity of the reactor is increased to improve the safety upon thermal transient stage, for example, loss of coolant flow rate accident. (I.N.)

  7. Evaluation of control rod motion simulator research reactors

    International Nuclear Information System (INIS)

    Sanda

    2010-01-01

    Motion simulator has been carried out testing of the reactor control rod using a servomotor. Reactor control rod motion at any point should be in the right position, one of the motors that can move in a precise and correct the servo motor. To ensure that the servo motor to move in accordance with the desired program, then the servomotor function test for motor work to ensure the performance of the appliance. Tests carried out on meshes stress disorder, the load is stable within a certain period and travel time safety control rod up and down, travel time regulating control rods up and down and travel time compensation control rods up and down. In testing the breakdown voltage Vout nets at 24 V, 6.5 A with 12 Ω load deviation obtained V0 = V1 = 0.1% and 0.65% and for the stability of the load in a certain time deviation V = 0.7125%, next to the breakdown voltage Vout nets at 12V, 4.2 A with a 6 Ω load deviation obtained V0 = V1 = 0.275% and 1.158% for the stability of the load in a certain time deviation V = 1.463% and the net-voltage noise nets on Vout 24 V, 4.5 A with 12 Ω load deviation obtained V0 = V1 = 0.196% and 0.496% and for the stability of the load in a certain time deviation V = 0.3625%. While the travel time of a safety control rod up and down, up and down the regulator and compensation rise and fall showed a steady linear graph. The results show that the performance of the servo motor is very stable with the working area below the tolerance limit, it is 5% - 10%. (author)

  8. Experimental Breeder Reactor-II automatic control-rod-drive system

    International Nuclear Information System (INIS)

    Christensen, L.J.

    1983-01-01

    A computer-controlled automatic control rod drive system (ACRDS) was designed and operated in EBR-II during reactor runs 121 and 122. The ACRDS was operated in a checkout mode during run 121 using a low worth control rod. During run 122 a high worth control rod was used to perform overpower transient tests as part of the LMFBR oxide fuels transient testing program. The testing program required an increase in power of 4 MW/s, a hold time of 12 minutes and a power decrease of 4 MW/s. During run 122, 13 power transients were performed

  9. Control rod for the operation of nuclear reactor

    International Nuclear Information System (INIS)

    Ishida, Hiromi

    1987-01-01

    Purpose: To conduct spectrum shift operation without complicating the reactor core structures, reducing the probability of failures. Constitution: An operation control rod which is driven while passed vertically in the reactor core comprises a strong absorption portion, moderation portion and weak moderation portion defined orderly from above to below and the length for each of the portions is greater than the effective reactor core height. If the operation control rod is lifted to the maximum limit in the upward direction of the reactor core, the weak moderation portion is corresponded over the effective length of the reactor core. Since the weak moderation portion is filled with zirconium and moderators are not present in the operation control rod, water draining gap is formed, neutron spectral shift is formed, excess reactivity is suppressed, absorption of neutrons to fuel fertile material is increased and the formation of nuclear fission material is increased. From the middle to the final stage of the cycle, the control rod is lowered, by which the moderator/fuel effective volume ratio is increased to increase the reactivity. (Kamimura, M.)

  10. Influence of specimen design on the ductility of zircaloy cladding: Experiment and analysis

    International Nuclear Information System (INIS)

    Bates, D. W.; Majumdar, S.; Koss, D. A.; Motta, A. T.

    1999-01-01

    In a reactivity-initiated accident (RIA), a control rod ejection or drop causes a sudden increase in reactor power, which in turn deposits a large amount of energy into the fuel. The resulting thermal expansion and fission gas release loads the cladding into the plastic regime and may cause it to fail. In order to predict cladding survivability, there has been considerable interest and effort in supplementing integral WA tests with separate-effects ring tests of cladding tubes. Such tests can give one insight into failure mechanisms and measure relevant mechanical properties (such as yield strength, uniform elongation, uniaxial stress-strain curve, etc.), for use in computer codes that attempt to predict cladding response during an RIA. The accuracy of such model predictions obviously depends on appropriate and accurate failure data. This study concerns itself with the proper development of ring tensile tests that (i) are similar to the loading conditions present in an RIA, (ii) measure the relevant mechanical properties and (iii) provide insight regarding the influence of the strain paths on the failure mechanisms present if Zircaloy cladding. Based on both experiments and computational modeling, the authors investigate the failure of Zircaloy tubing as a function of specimen geometry, and discuss the limitations of certain ring-test geometries in yielding failure ductility data that are applicable to RIA situations

  11. RODDRP - A FORTRAN program for use in control rod calibration by the rod drop method

    International Nuclear Information System (INIS)

    Wilson, W.E.

    1972-01-01

    The different methods to measure reactivity which are applicable to control rod calibration are discussed. They include: 1) the positive period method, 2) the rod drop method, 3) the source-jerk method, 4) the rod oscillation method, and 5) the pulsed neutron method. The instrument setup used at WSU for rod drop measurements is presented. To speed up the analysis of power fall-off trace, a FORTRAN IV program called RODDRP was written to simultaneously solve the in-hour equation and relative neutron flux. The procedure for calculating the worth of the rod that produced the power trace is given. The reactivity for each time relative flux point is obtained. Conclusions about the status of the equipment are made

  12. Thermal performance of a buried nuclear waste storage container storing a hybrid mix of PWR and BWR spent fuel rods

    International Nuclear Information System (INIS)

    Johnson, G.L.

    1988-09-01

    Lawrence Livermore National Laboratory will design, model, and test nuclear waste packages for use at the Nevada Nuclear Waste Storage Repository at Yucca Mountain, Nevada. One such package would store lightly packed spent fuel rods from both pressurized and boiling water reactors. The storage container provides the primary containment of the nuclear waste and the spent fuel rod cladding provides secondary containment. A series of transient conduction and radiation heat transfer analyses was run to determine for the first 1000 yr of storage if the temperature of the tuff at the borehole wall ever falls below 97/degree/C and whether the cladding of the stored spent fuel ever exceeds 350/degree/C. Limiting the borehole to temperatures of 97/degree/C or greater helps minimize corrosion by assuring that no condensed water collects on the container. The 350/degree/C cladding limit minimizes the possibility of creep-related failure in the spent fuel rod cladding. For a series of packages stored in a 8 x 30 m borehole grid where each package contains 10-yr-old spent fuel rods generating 4.74 kW or more, the borehole wall stays above 97/degree/C for the full 1000-yr analysis period

  13. PWR fuel rod corrosion in Japan

    International Nuclear Information System (INIS)

    Inoue, S.; Mori, K.; Murata, K.; Kobasyashi, S.

    1997-01-01

    Many particular appearance were observed on the fuel rod surfaces during fuel inspection at reactor outage in 1991. The appearances looked like small black circular nodules. The size was approximately 1 mm. This kind of appearances were found on fuel rods of which burnup exceeded approximately 30 GWd/t and at the second or third spans of the fuel assembly from the top. In order to clarify the cause, PIE was performed. The black nodules were confirmed to be oxide film spalling by visual inspection. Maximum oxide film thickness was 70 μm and spalling was observed where oxide thickness exceeded 40 t0 50 μm. Oxide film thickness was greater than expected. Many small pores were found in the oxide film when the oxide film had become thicker. Many circumferential cracks were also found in the film. It was speculated that these cracks caused the spalling of the oxide film. Hydride precipitates were mainly oriented circumferentially. Dense hydrides were observed near the outer rim of the cladding. No concentrated hydrides were observed near the spalling area. Maximum hydrogen content was 315 ppm. It was confirmed that the results of tensile test showed no significant effects by corrosion. The mechanism of accelerated corrosion was studied in detail. Water chemistry during irradiation was examined. Lithium content was maintained below 2.2 ppm. pH value was kept between 6.9 and 7.2. There was no anomalies in water chemistry during reactor operation. Cladding fabrication record clarified that heat treatment parameter was smaller than the optimum value. In Japan, heat treatment of the cladding was already optimized by improved fabrication process. Also chemical composition optimization of the cladding, such as low Tin and high Silicon content, was adopted for high burnup fuel. These remedies has already reduced fuel cladding corrosion and we believe we have solved this problem. (author). 6 figs, 1 tab

  14. PWR fuel rod corrosion in Japan

    Energy Technology Data Exchange (ETDEWEB)

    Inoue, S [Kansai Electric Power Co., Inc., Osaka (Japan); Mori, K; Murata, K; Kobasyashi, S [Nuclear Fuel Industries, Ltd, Osaka (Japan)

    1997-02-01

    Many particular appearance were observed on the fuel rod surfaces during fuel inspection at reactor outage in 1991. The appearances looked like small black circular nodules. The size was approximately 1 mm. This kind of appearances were found on fuel rods of which burnup exceeded approximately 30 GWd/t and at the second or third spans of the fuel assembly from the top. In order to clarify the cause, PIE was performed. The black nodules were confirmed to be oxide film spalling by visual inspection. Maximum oxide film thickness was 70 {mu}m and spalling was observed where oxide thickness exceeded 40 t0 50 {mu}m. Oxide film thickness was greater than expected. Many small pores were found in the oxide film when the oxide film had become thicker. Many circumferential cracks were also found in the film. It was speculated that these cracks caused the spalling of the oxide film. Hydride precipitates were mainly oriented circumferentially. Dense hydrides were observed near the outer rim of the cladding. No concentrated hydrides were observed near the spalling area. Maximum hydrogen content was 315 ppm. It was confirmed that the results of tensile test showed no significant effects by corrosion. The mechanism of accelerated corrosion was studied in detail. Water chemistry during irradiation was examined. Lithium content was maintained below 2.2 ppm. pH value was kept between 6.9 and 7.2. There was no anomalies in water chemistry during reactor operation. Cladding fabrication record clarified that heat treatment parameter was smaller than the optimum value. In Japan, heat treatment of the cladding was already optimized by improved fabrication process. Also chemical composition optimization of the cladding, such as low Tin and high Silicon content, was adopted for high burnup fuel. These remedies has already reduced fuel cladding corrosion and we believe we have solved this problem. (author). 6 figs, 1 tab.

  15. Force analysis of the advanced neutron source control rod drive latch mechanism

    International Nuclear Information System (INIS)

    Damiano, B.

    1989-01-01

    The Advanced Neutron Source reactor (ANS), a proposed Department of Energy research reactor currently undergoing conceptual design at the Oak Ridge National Laboratory (ORNL), will generate a thermal neutron flux approximating 10 30 M -2 emdash S -1 . The compact core necessary to produce this flux provides little space for the shim safety control rods, which are located in the central annulus of the core. Without proper control rod drive design, the control rod drive magnets (which hold the control rod latch in a ready-to-scram position) may be unable to support the required load due to their restricted size. This paper describes the force analysis performed on the control rod latch mechanism to determine the fraction of control rod weight transferred to the drive magnet. This information will be useful during latch, control rod drive and magnet design. 5 refs., 12 figs

  16. Cleaning and excavating tool for control rod canopy seals

    International Nuclear Information System (INIS)

    Kucera, R.A.

    1991-01-01

    This patent describes a device for servicing a weld site about the periphery of a control rod drive mechanism. It comprises a housing adapted to be rotated about the periphery of the control rod drive mechanism; a carriage reciprocably received within the housing; first movement means for reciprocating the carriage in a first direction; a tool attachment reciprocably received within the carriage; and second movement means for reciprocating the tool in a second direction; wherein the tool attachment is positioned relative to the control rod drive mechanism by the first and second movement means

  17. Reconstitutable control assembly having removable control rods with detachable split upper end plugs

    International Nuclear Information System (INIS)

    Gjertsen, R.K.; Knott, R.P.; Sparrow, J.A.

    1989-01-01

    This patent describes, in a reconstitutable control assembly for use with a nuclear fuel assembly, the control assembly including a spider structure and at least one control rod, an attachment joint for detachable fastening the control rod to the spider structure. The attachment joint comprising: a hollow connecting finger on the spider structure; and an elongated detachable split upper end plug on the control rod having a pair of separate upper and lower plug portions, the upper plug portion having integrally-connected tandemly- arranged upper, middle and lower sections. The lower plug portion having integrally-connected tandemly-arranged upper, middle and lower segments

  18. Influence of fuel pin bowing on the temperature distribution in fuel pin cladding tubes in case of sodium cooling; experimental results

    International Nuclear Information System (INIS)

    Moeller, R.; Tschoeke, H.; Kolodziej, M.

    1978-09-01

    The influence of rod bowing on the local temperature distribution was measured with turbulent sodium flow in the cladding tubes of a 19-rod bundle mock-up of the SNR 300 Mark Ia fuel element. Such measurements have been carried out for the first time. The results presented in this report are part 1 of the experimental evaluation not yet completed. The major results are: 1. When a rod on the first ring gets deformed towards a neighbour on the second ring with a gap reduction from the nominal value of 100 % down to 20 %, the maximum azimuthal temperature difference of the outer rod increases by about 60 %. 2. The maximum azimuthal temperature difference of a rod on the first ring increases by a factor of 2, if it is approached by a neighbour on the same ring. 3. The reduction in cross section of a subchannel by rod bowing results only locally in distinct temperature rises, i.e. in the adjacent cladding tubes. Rods of the next but one row are no more subject to noticeable changes in temperature [de

  19. Theoretical investigations of the gas flow in ballooning LWR-fuel rods

    International Nuclear Information System (INIS)

    Gaballah, I.

    1978-09-01

    A theory is developed for the calculation of gas flow in a fuel rod simulator or in a fuel rod with round- or cracked pellets. The fundamental equations are formulated, simplified, reformed, and then numerically solved. The numerical investigations show, that a quasi steady incompressible flow model can be used without great error. The effect of the deformation form is studied. A uniform deformation along the whole length causes small pressure difference. A power profile and rod spacers cause non-uniform clad deformation of the fuel rod simulator or the fuel rod. This deformation leads to greater pressure differences. Finally the effect of the cracked pellets is studied. The cracked pellets cause great pressure differences along the fuel rod. (orig.) 891 HP [de

  20. Calculation of drop course of control rod assembly in PWR

    International Nuclear Information System (INIS)

    Zhou Xiaojia; Mao Fei; Min Peng; Lin Shaoxuan

    2013-01-01

    The validation of control rod drop performance is an important part of safety analysis of nuclear power plant. Development of computer code for calculating control rod drop course will be useful for validating and improving the design of control rod drive line. Based on structural features of the drive line, the driving force on moving assembly was analyzed and decomposed, the transient value of each component of the driving force was calculated by choosing either theoretical method or numerical method, and the simulation code for calculating rod cluster control assembly (RCCA) drop course by time step increase was achieved. The analysis results of control rod assembly drop course calculated by theoretical model and numerical method were validated by comparing with RCCA drop test data of Qinshan Phase Ⅱ 600 MW PWR. It is shown that the developed RCCA drop course calculation code is suitable for RCCA in PWR and can correctly simulate the drop course and the stress of RCCA. (authors)

  1. Components inspection of Monju, a sodium bonded type control rod

    International Nuclear Information System (INIS)

    Harada, Kiyoshi; Matsushita, Yuichi; Lee, Chunchan; Abe, Hideaki; Watahiki, Naohisa

    2002-03-01

    This Report addresses a result of a sodium test conducted on components of a Double Poral Filter Sodium Bonded Type Control Rod that is expected to be a next generation, long life Control Rod. Upper and lower Poral Filter Sodium Bonded Type Control Rod components were mocked up to conduct a sodium test. During the test, sodium chargeability, formation of Gas Plenum at the upper part of the components, sodium drain-ability and NaOH clean-ability were recognized under actual plant condition. The following are results obtained: (1) Sodium Chargeability at Control Rod Insertion to EVST. Sodium was charged into the components when the mocked-up was inserted in sodium of 190degC, with insertion speed of 6 m/min which is an actual insertion speed to EVST. (2) Formation of Upper Gas Plenum by Helium Gas generated in Control Rod Components Gas Plenum formation within deviation of 9% was confirmed by releasing helium gas into the mocked-up which is immersed in sodium of 620degC and 190degC. Length of Gas Plenum is confirmed to be retained in certain length even if helium gas is further released into formed Gas Plenum. (3) Sodium Drain-ability of Control Rod Components when Drawing from EVST. Drain-ability was confirmed to be sufficient and no sodium residue was found in the mocked-up when the mocked-up was drawn out from sodium of 190degC, with drawing speed of 6 m/min which is an actual drawing speed from EVST. (4) Clean-ability of NaOH Solution against Sodium Residue in Control Rod Components. Sodium and NaOH solution reacted calmly, however, clean-ability was not sufficient. When Sodium fully remained in Control Rod Components, it made circulation of NaOH solution not enough. (author)

  2. Control rod drive of nuclear reactor

    International Nuclear Information System (INIS)

    Zhuchkov, I.I.; Gorjunov, V.S.; Zaitsev, B.I.

    1980-01-01

    This invention relates to nuclear reactors and, more particularly, to a drive of a control rod of a nuclear reactor and allows power control, excess reactivity compensation, and emergency shut-down of a reactor. (author)

  3. Eutectic reaction analysis between TRU-50%Zr alloy fuel and HT-9 cladding, and temperature prediction of eutectic reaction under steady-state

    Energy Technology Data Exchange (ETDEWEB)

    Hwang, Woan; Lee, Byoung Oon; Lee, Bong Sang; Park, Won Seok

    2001-02-01

    Blanket fuel assembly for HYPER contains a bundle of pins arrayed in triangular pitch, which has hexagonal bundle structure. The reference blanket fuel pin consists of the fuel slug of TRU-50wt%Zr alloy and the cladding material of ferritic martensite steel, HT-9. Chemical interaction between fuel slug and cladding is one of the major concerns in metallic fuel rod design. The contact of metallic fuel slug and stainless steel cladding in a fuel rod forms a complex multi-component diffusion couple at elevated temperatures. The potential problem of inter-diffusion of fuel and cladding components is essentially two-fold weakening of cladding mechanical strength due to the formation of diffusion zones in the cladding, and the formation of comparatively low melting point phases in the fuel/cladding interface to develop eutectic reaction. The main components of fuel slug are composed of zirconium alloying element in plutonium matrix, including neptunium, americium and uranium additionally. Therefore basic eutectic reaction change of Pu-Fe binary system can be assessed, while it is estimated how much other elements zirconium, uranium, americium and neptunium influence on plutonium phase stability. Afterwards it is needed that eutectic reaction is verified through experimental necessarily.

  4. Eutectic reaction analysis between TRU-50%Zr alloy fuel and HT-9 cladding, and temperature prediction of eutectic reaction under steady-state

    International Nuclear Information System (INIS)

    Hwang, Woan; Lee, Byoung Oon; Lee, Bong Sang; Park, Won Seok

    2001-02-01

    Blanket fuel assembly for HYPER contains a bundle of pins arrayed in triangular pitch, which has hexagonal bundle structure. The reference blanket fuel pin consists of the fuel slug of TRU-50wt%Zr alloy and the cladding material of ferritic martensite steel, HT-9. Chemical interaction between fuel slug and cladding is one of the major concerns in metallic fuel rod design. The contact of metallic fuel slug and stainless steel cladding in a fuel rod forms a complex multi-component diffusion couple at elevated temperatures. The potential problem of inter-diffusion of fuel and cladding components is essentially two-fold weakening of cladding mechanical strength due to the formation of diffusion zones in the cladding, and the formation of comparatively low melting point phases in the fuel/cladding interface to develop eutectic reaction. The main components of fuel slug are composed of zirconium alloying element in plutonium matrix, including neptunium, americium and uranium additionally. Therefore basic eutectic reaction change of Pu-Fe binary system can be assessed, while it is estimated how much other elements zirconium, uranium, americium and neptunium influence on plutonium phase stability. Afterwards it is needed that eutectic reaction is verified through experimental necessarily

  5. Thermoelastic analysis for the fuel claddings of the nuclear power reactor at Atucha in the skid's region

    International Nuclear Information System (INIS)

    Sanchez Sarmiento, Gustavo; Basombrio, F.G.

    1979-01-01

    For the fuel elements of the Nuclear Power Reactor at Atucha, a two-dimensional thermoelastic analysis has been made in the region of the skids of the fuel cladding, when the gap between them and the fuel rod separator's support becomes zero. In such a case the latter forces exert on the skids an elastic reaction opposite to the cladding's expansion. The internal pressure reaching the yield stress for the cladding material has been calculated, as a function of the initial gap; for several possible fuel rod locations within the separator; for the actual dimensions and also for reduced thickness of the cladding; with a given external pressure and, with a known temperature spatial distribution. The latter has been calculated by solving the heat conduction equation along the fuel element for a certain power level in the reactor. The calculations are made with two FORTRAN IV computer codes developed at C.A.B., using the finite-element method: the NOLICUARM, to solve the nonlinear quasi-harmonic equation, and the ELASTEF 3, for the solution of thermoelastic problems with plane symmetry. (author) [es

  6. Using Finite Model Analysis and Out of Hot Cell Surrogate Rod Testing to Analyze High Burnup Used Nuclear Fuel Mechanical Properties

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Jy-An John [ORNL; Jiang, Hao [ORNL; Wang, Hong [ORNL

    2014-07-01

    Based on a series of FEA simulations, the discussions and the conclusions concerning the impact of the interface bonding efficiency to SNF vibration integrity are provided in this report; this includes the moment carrying capacity distribution between pellets and clad, and the impact of cohesion bonding on the flexural rigidity of the surrogate rod system. As progressive de-bonding occurs at the pellet-pellet interfaces and at the pellet-clad interface, the load ratio of the bending moment carrying capacity gradually shifts from the pellets to the clad; the clad starts to carry a significant portion of the bending moment resistance until reaching the full de-bonding state at the pellet-pellet interface regions. This results in localized plastic deformation of the clad at the pellet-pellet-clad interface region; the associated plastic deformations of SS clad leads to a significant degradation in the stiffness of the surrogate rod. For instance, the flexural rigidity was reduced by 39% from the perfect bond state to the de-bonded state at the pellet-pellet interfaces.

  7. Code Package to Analyze Parameters of the WWER Fuel Rod. TOPRA-2 Code - Verification Data

    International Nuclear Information System (INIS)

    Scheglov, A.; Proselkov, V.; Passage, G.; Stefanova, S.

    2009-01-01

    Presented are the data for computer codes to analyze WWER fuel rods, used in the WWER department of RRC 'Kurchatov Institute'. Presented is the description of TOPRA-2 code intended for the engineering analysis of thermophysical and strength parameters of the WWER fuel rod - temperature distributions along the fuel radius, gas pressures under the cladding, stresses in the cladding, etc. for the reactor operation in normal conditions. Presented are some results of the code verification against test problems and the data obtained in the experimental programs. Presented are comparison results of the calculations with TOPRA-2 and TRANSURANUS (V1M1J06) codes. Results obtained in the course of verification demonstrate possibility of application of the methodology and TOPRA-2 code for the engineering analysis of the WWER fuel rods

  8. A survey of blockage measurement methods used in PWR multi-rod experiments

    Energy Technology Data Exchange (ETDEWEB)

    Hindle, E.D.; Jones, C.; Whitty, S. (AEA Reactor Services, Springfield (UK))

    1986-05-01

    The deformation characteristics of Zircaloy multi-rod arrays are being investigated in laboratory and in-reactor tests, and heat transfer experiments are being carried out on pre-deformed arrays. The primary objective is to demonstrate that cladding distension occurring under hypothetical loss-of-coolant accident (LOCA) conditions will not impede the PWR emergency coolant flow during the reflood stage to the extent that unacceptably high cladding temperatures are reached, i.e. that a coolable geometry is maintained. This Report critically reviews the current methods for measuring blockage in multi-rod arrays and discusses their application. A new definition which overcomes the deficiencies of the previous methods is proposed even though it still has drawbacks in the case of overall blockage measurement. A method for automatically measuring the individual rod strain, general cluster blockage sub-channel blockage and sub-channel perimeter changes is described and the results from a deformed array presented. (author).

  9. A survey of blockage measurement methods used in PWR multi-rod experiments

    International Nuclear Information System (INIS)

    Hindle, E.D.; Jones, C.; Whitty, S.

    1986-05-01

    The deformation characteristics of Zircaloy multi-rod arrays are being investigated in laboratory and in-reactor tests, and heat transfer experiments are being carried out on pre-deformed arrays. The primary objective is to demonstrate that cladding distension occurring under hypothetical loss-of-coolant accident (LOCA) conditions will not impede the PWR emergency coolant flow during the reflood stage to the extent that unacceptably high cladding temperatures are reached, i.e. that a coolable geometry is maintained. This Report critically reviews the current methods for measuring blockage in multi-rod arrays and discusses their application. A new definition which overcomes the deficiencies of the previous methods is proposed even though it still has drawbacks in the case of overall blockage measurement. A method for automatically measuring the individual rod strain, general cluster blockage sub-channel blockage and sub-channel perimeter changes is described and the results from a deformed array presented. (author)

  10. End plug for fuel rod and welding method therefor

    International Nuclear Information System (INIS)

    Yoneda, Hiroshi; Murakami, Kazuo; Oyama, Jun-ichi.

    1996-01-01

    An end plug of a fuel rod comprises a pressure-insertion portion having a diameter somewhat greater than the inner diameter of a fuel cladding tube and a welding portion having a diameter substantially the same as the outer diameter of the cladding tube. A V-shaped recess having an outer diameter smaller than the greatest outer diameter of the pressure-insertion portion is formed over the entire circumferential surface of the outer circumference of the connection portion of the pressure-insertion portion and the welding portion. The pressure-insertion portion of the end plug is inserted to the end of the cladding tube till the end of the cladding tube abuts against the inclined surface of the V-shaped recess. The abutting surfaces of the end plug and the cladding tube are subjected to resistance welding in this state. The inner portion bulged from the inclined surface of the V-shaped recess is filled in the recess in a molten state. Lowering of temperature of the cladding tube in the vicinity of the welded portion is decreased by γ heat during reactor operation. Accordingly, lowering of ductility of the cladding tube and degradation of material of the welded region due to segregation of hydrogen in the cladding tube can be suppressed. (I.N.)

  11. Removable control rod drive shaft guide

    International Nuclear Information System (INIS)

    Ales, M.W.; Brown, S.K.; Dixon, L.D.

    1988-01-01

    A removable control rod drive shaft guide is described for a control rod ''guide'' structure card, comprising: a. a substantially annular shaped main body portion having a central axial bore for receiving a control rod drive shaft and an upper exterior groove for receiving removal tooling; b. the main body portion having a reduced outer diameter at its lower section; c. a shoulder portion integral with the main body portion for supporting the main body portion on the guide structure card; d. the shoulder portion having a substantially radial bore and the reduced outer diameter lower section having a slot in alignment with the radial bore; e. a locking arm ''pivotaly'' mounted in the radial bore which protrudes into the slot and is movable between a first normal locking position for engaging the guide structure card and a second release position; f. a spring received within a second axial bore in the main body portion and biased against the locking arm for urging and locking arm into the first normal locking position; and g. a release tab at one end of the locking arm for moving the locking arm into the second release position

  12. FEMAXI-III: a computer code for the analysis of thermal and mechanical behavior of fuel rods

    International Nuclear Information System (INIS)

    Nakajima, Tetsuo; Ichikawa, Michio; Iwano, Yoshihiko; Ito, Kenichi; Saito, Hiroaki; Kashima, Koichi; Kinoshita, Motoyasu; Okubo, Tadatsune.

    1985-12-01

    FEMAXI-III is a computer code to predict the thermal and mechanical behavior of a light water fuel rod during its irradiation life. It can analyze the integral behavior of a whole fuel rod throughout its life, as well as the localized behavior of a small part of fuel rod. The localized mechanical behavior such as the cladding ridge deformation is analyzed by the two-dimensional axisymmetric finite element method. FEMAXI-III calculates, in particular, the temperature distribution, the radial deformation, the fission gas release, and the inner gas pressure as a function of irradiation time and axial position, and the stresses and strains in the fuel and cladding at a small part of fuel rod as a function of irradiation time. For this purpose, Elasto-plasticity, creep, thermal expansion, fuel cracking and crack healing, relocation, densification, swelling, hot pressing, heat generation distribution, fission gas release, and fuel-cladding mechanical interaction are modelled and their interconnected effects are considered in the code. Efforts have been made to improve the accuracy and stability of finite element solution and to minimize the computer memory and running time. This report describes the outline of the code and the basic models involved, and also includes the application of the code and its input manual. (author)

  13. Renovating process for Pressurized Water Reactor control rod assemblies and corresponding control

    International Nuclear Information System (INIS)

    Jahnke, S.; Ple, P.

    1989-01-01

    In the first PWRs the control rods are moving by the intermediary of electromagnetic mechanisms where the power fed to the electromagnets is selected by a hard wired logic circuit connected to the controldesh by another logic control. For renovating the control rod assemblies each power assembly is replaced by an electronic assembly containing an ordinator and power supply interfaces [fr

  14. Anti-ejection device, which can be released, for control rods of nuclear reactor

    International Nuclear Information System (INIS)

    Belz, G.

    1983-01-01

    The present invention proposes an anti-ejection device which allows to withdraw the control rod out of a PWR reactor core if the locking systems of the rod translation are streck. This device prohibits the control rod ejection as long as an effort lower than a predetermined value is not applied on the control rod. This limit value is determined with regard of the efforts which may be applied on the control rod in case of an external accidental source. Nevertheless, if the anti-ejection mechanism remains stuck, it is however possible to withdraw the control rod out of the core applying on its control rod drives an effort higher than the limit value [fr

  15. Analysis of control rod worth in experimental fast reactor JOYO

    International Nuclear Information System (INIS)

    Arii, Y.; Aoyama, T.; Okimoto, Y.; Yoshida, A.; Mizoo, N.

    1988-01-01

    In JOYO, the measurement of control rod worths have been carried out in the beginning of the each cycle, using both period method and neutron source multiplication method. In this paper, the calculational method of control rod worths in the design stage and the comparison with the design values and measured ones are shown. The reasons that the control rod worths change slightly in each cycle, are also investigated. (author). 13 figs, 12 tabs

  16. The estimation of the control rods absorber burn-up during the VVER-1000 operation

    Energy Technology Data Exchange (ETDEWEB)

    Bolshagin, Sergey N.; Gorodkov, Sergey S.; Sukhino-Khomenko, Evgeniya A. [National Research Centre ' Kurchatov Institute' , Moscow (Russian Federation)

    2013-09-15

    The isotopic composition of the control rods absorber changes under the neutron flux influence, so the control rods efficiency can decrease. In the VVER-1000 control rods boron carbide and dysprosium titanate are used as absorbing materials. In boric part the efficiency decreases due to the {sup 10}B isotope burn-up. Dysprosium isotopes turn into other absorbing isotopes, so the absorbing properties of dysprosium part decrease to a lesser degree. Also the control rod's shells may be deformed as a consequence of boron carbide radiation swelling. This fact should be considered in substantiation of control rods durability. For the estimation of the control rods absorber burn-up two models are developed: VVER-1000 3-D fuel assembly with control rods partially immersed (imitation of the control rods operation in the working group) and VVER-1000 3-D fuel assembly with control rods, located at the upper limit switch (imitation of the control rods operation in groups of the emergency shutdown system). (orig.)

  17. Optimization of boiling water reactor control rod patterns using linear search

    International Nuclear Information System (INIS)

    Kiguchi, T.; Doi, K.; Fikuzaki, T.; Frogner, B.; Lin, C.; Long, A.B.

    1984-01-01

    A computer program for searching the optimal control rod pattern has been developed. The program is able to find a control rod pattern where the resulting power distribution is optimal in the sense that it is the closest to the desired power distribution, and it satisfies all operational constraints. The search procedure consists of iterative uses of two steps: sensitivity analyses of local power and thermal margins using a three-dimensional reactor simulator for a simplified prediction model; linear search for the optimal control rod pattern with the simplified model. The optimal control rod pattern is found along the direction where the performance index gradient is the steepest. This program has been verified to find the optimal control rod pattern through simulations using operational data from the Oyster Creek Reactor

  18. Assessment of the prediction capability of the TRANSURANUS fuel performance code on the basis of power ramp tested LWR fuel rods

    International Nuclear Information System (INIS)

    Pastore, G.; Botazzoli, P.; Di Marcello, V.; Luzzi, L.

    2009-01-01

    The present work is aimed at assessing the prediction capability of the TRANSURANUS code for the performance analysis of LWR fuel rods under power ramp conditions. The analysis refers to all the power ramp tested fuel rods belonging to the Studsvik PWR Super-Ramp and BWR Inter-Ramp Irradiation Projects, and is focused on some integral quantities (i.e., burn-up, fission gas release, cladding creep-down and failure due to pellet cladding interaction) through a systematic comparison between the code predictions and the experimental data. To this end, a suitable setup of the code is established on the basis of previous works. Besides, with reference to literature indications, a sensitivity study is carried out, which considers the 'ITU model' for fission gas burst release and modifications in the treatment of the fuel solid swelling and the cladding stress corrosion cracking. The performed analyses allow to individuate some issues, which could be useful for the future development of the code. Keywords: Light Water Reactors, Fuel Rod Performance, Power Ramps, Fission Gas Burst Release, Fuel Swelling, Pellet Cladding Interaction, Stress Corrosion Cracking

  19. The thermo-mechanics of the PWR fuel rod

    International Nuclear Information System (INIS)

    Barral, J.C.; Gautier, B.; Chaigne, G.

    1999-01-01

    The fuel rod mechanics is of a great importance in the safety and performance of the reactors. In this domain a meeting has been organized by the SFEN the 18 march 1998 at Paris. With the participation of scientists from CEA, EDF and Framatome, the physics of the fuel rods was presented based on four main aspects. Two first papers dealt with the solicitations of the fuel rod in normal and accidental conditions. The physical phenomena under irradiation were then detailed in the four following talks. Three papers presented the simulation and the codes of the fuel-cladding interactions with the diabolo effect. The last paper was devoted to the experiment feedback and the research programs. (A.L.B.)

  20. Apparatus for decelerating the dropping speed of a control rod

    International Nuclear Information System (INIS)

    Shirakawa, Toshihisa.

    1975-01-01

    Object: To reduce the dropping speed (i.e. withdrawal) of a control rod of the upward insertion type in a BWR type reactor without reducing the speed of insertion. Structure: A control rod is provided with a flaring lower end so as to constitute a speed limiter which is penerated by vertically extending and upwardly open flow ducts that each have a narrow opening and flare upwardly. Thus, at the time of insertion of the control rod, the resistance offered thereto by the surrounding fluid is reduced to provide increased insertion speed. On the other hand, at the time of withdrawal the resistance offered by the fluid is increased to reduce the dropping speed of the control rod. (Ikeda, J.)

  1. Large test rigs verify Clinch River control rod reliability

    International Nuclear Information System (INIS)

    Michael, H.D.; Smith, G.G.

    1983-01-01

    The purpose of the Clinch River control test programme was to use multiple full-scale prototypic control rod systems for verifying the system's ability to perform reliably during simulated reactor power control and emergency shutdown operations. Two major facilities, the Shutdown Control Rod and Maintenance (Scram) facility and the Dynamic and Seismic Test (Dast) facility, were constructed. The test programme of each facility is described. (UK)

  2. Development and testing of control rod drives for ship reactors

    International Nuclear Information System (INIS)

    Bruelheide, K.; Mundt, D.; Peters, C.-H.; Manthey, H.-J.

    1978-01-01

    The following paper deals with the development and testings of a new control rod drive design for marine reactors. Starting from the good operating experience with the advanced pressurized water reactor (FDR) of the NS OTTO HAHN a control rod drive system with an hermetically sealed drive principle was developed. A prototype control rod drive system was put through extensive tests and developed ready for standard production at the 'Gesellschaft fuer Kernenergieverwertung in Schiffbau und Schiffahrt'

  3. Study on the quantitative rod internal pressure design criterion

    International Nuclear Information System (INIS)

    Kim, Kyu Tae; Kim, Oh Hwan; Han, Hee Tak

    1991-01-01

    The current rod internal pressure criterion permits fuel rods to operate with internal pressures in excess of system pressure only if internal overpressure does not cause the diametral gap enlargement. In this study, the generic allowable internal gas pressure not violating this criterion is estimated as a function of rod power. The results show that the generic allowable internal gas pressure decreases linearly with the increase of rod power. Application of the generic allowable internal gas pressure for the rod internal pressure design criterion will result in the simplication of the current design procedure for checking the diametral gap enlargement caused by internal overpressure because according to the current design procedure the cladding creepout rate should be compared with the fuel swelling rate at each axial node at each time step whenever internal pressure exceeds the system pressure. (Author)

  4. Results of VVER fuel rods tests in the MIR.M1 reactor under power cycling conditions

    International Nuclear Information System (INIS)

    Burukin, A.; Izhutov, A.; Ovchinnikov, V.; Kalygin, V.; Markov, D.; Pimenov, Y.; Novikov, V.; Medvedev, A.; Nesterov, B.

    2011-01-01

    The paper presents the main results of the 50 ... 60 MWd/kgU burnup VVER fuel rods tests performed in the MIR.M1 reactor loop facilities under power cycling. The non-destructive PIE results are presented as well. A series of experiments was performed, including overall measurement of fuel rod parameters test, in one of which 300 cycles were done. Irradiation under power cycling conditions and PIE of high-burnup VVER fuel rods showed the following: 1) all fuel rods claddings preserved their integrity under irradiation at linear heat rate (LHR) higher than the NPP operating one; 2) experimental data were obtained on the axial and radial cladding strain and fission gas release (FGR) from 50 ... 60 MWd/kgU burnup VVER-440 and VVER-1000 fuel rods as well as on the kinetics of the change in these parameters and fuel temperature under the power cycling; 3) non-destructive PIE results are in a satisfactory correlation with the data obtained by means of in-pile measurement gages during irradiation. (authors)

  5. Quivers For Special Fuel Rods-Disposal Of Special Fuel Rods In CASTOR V Casks

    International Nuclear Information System (INIS)

    Bannani, Amin; Cebula, Wojciech; Buchmuller, Olga; Huggenberg, Roland; Helmut Kuhl

    2015-01-01

    While GNS casks of the CASTOR family are a suitable means to transfer fuel assemblies (FA) from the NPP to an interim dry storage site, Germanys phase-out of nuclear energy has triggered the demand for an additional solution to dispose of special fuel rods (SFR), normally remaining in the fuel pond until the final shutdown of the NPP. SFR are fuel rods that had to be removed from fuel assemblies mainly due to their special condition, e. g. damages in the cladding of the fuel rods which may have occurred during reactor operations. SFR are usually stored in the spent fuel pond after they are removed from the FA. The quiver for special fuel rods features a robust yet simple design, with a high mechanical stability, a reliable leak-tightness and large safety margins for future requirements on safety analysis. The quiver for special fuel rods can be easily adapted to a large variety of different damaged fuel rods and tailored to the specific need of the customer. The quiver for special fuel rods is adaptable e.g. in length and diameter for use in other types of transport and storage casks and is applicable in other countries as well. The overall concept presented here is a first of its kind solution for the disposal of SFRs via Castor V-casks. This provides an important precondition in achieving the status 'free from nuclear fuel' of the shut down German NPPs

  6. Quivers For Special Fuel Rods-Disposal Of Special Fuel Rods In CASTOR V Casks

    Energy Technology Data Exchange (ETDEWEB)

    Bannani, Amin; Cebula, Wojciech; Buchmuller, Olga; Huggenberg, Roland [GNS, Essen (Germany); Helmut Kuhl [WTI, Julich (Germany)

    2015-05-15

    While GNS casks of the CASTOR family are a suitable means to transfer fuel assemblies (FA) from the NPP to an interim dry storage site, Germanys phase-out of nuclear energy has triggered the demand for an additional solution to dispose of special fuel rods (SFR), normally remaining in the fuel pond until the final shutdown of the NPP. SFR are fuel rods that had to be removed from fuel assemblies mainly due to their special condition, e. g. damages in the cladding of the fuel rods which may have occurred during reactor operations. SFR are usually stored in the spent fuel pond after they are removed from the FA. The quiver for special fuel rods features a robust yet simple design, with a high mechanical stability, a reliable leak-tightness and large safety margins for future requirements on safety analysis. The quiver for special fuel rods can be easily adapted to a large variety of different damaged fuel rods and tailored to the specific need of the customer. The quiver for special fuel rods is adaptable e.g. in length and diameter for use in other types of transport and storage casks and is applicable in other countries as well. The overall concept presented here is a first of its kind solution for the disposal of SFRs via Castor V-casks. This provides an important precondition in achieving the status 'free from nuclear fuel' of the shut down German NPPs.

  7. Drive-in device for long thin rods into narrow cavitations, especially for control-shutdown rods e.g. of nuclear reactors

    International Nuclear Information System (INIS)

    Flessner, H.; Paeserack, U.

    1974-01-01

    The auxiliary device serves as holder for long and thin rods, e.g. control rods, transported hanging in bundles, when these are lowered into narrow cavities. It is constructed as a rod grab vertically movable at the end of a guide tube. A comb-shaped trap in connection with a guide rod serves for lateral support of the lower ends of the rods hanging on the grab. This guide rod can be moved in vertical direction by means of two pairs of convex rollers resting on the inner guide tube. In addition, the guide rod has a prolongation carrying a traverse by means of an abutment on the lower end. With these auxiliaries amongst others, the trap can be brought into a horizontal position by turning around an axis with the control rods meshing with the teeth of the trap while the parallelism of the rods is kept up during transport. (DG) [de

  8. Vibrational characteristics and wear of fuel rods

    International Nuclear Information System (INIS)

    Schmugar, K.L.

    1977-01-01

    Fuel rod wear, due to vibration, is a continuing concern in the design of liquid-cooled reactors. In my report, the methodology and models that are used to predict fuel rod vibrational response and vibratory wear, in a light water reactor environment, are discussed. This methodology is being followed at present in the design of Westinghouse Nuclear Fuel. Fuel rod vibrations are expressed as the normal bending modes, and sources of rod vibration are examined with special emphasis on flow-induced mechanisms in the stable flow region. In a typical Westinghouse PWR fuel assembly design, each fuel rod is supported at multiple locations along the rod axis by a square-shaped 'grid cell'. For a fuel rod /grid support system, the development of small oscillatory motions, due to fluid flow at the rod/grid interface, results in material wear. A theoretical wear mode is developed using the Archard Theory of Adhesive Wear as the basis. Without question certainty, fretting wear becomes a serious problem if it progresses to the stage where the fuel cladding is penetrated and fuel is exposed to the coolant. Westinghouse fuel is designed to minimize fretting wear by limiting the relative motion between the fuel rod and its supports. The wear producing motion between the fuel rod and its supports occurs when the vibration amplitude exceeds the slippage threshold amplitude

  9. Liquid-metal fast breeder reactor fuel rod performance and modeling at high burnup

    International Nuclear Information System (INIS)

    Verbeek, P.; Toebbe, H.; Hoppe, N.; Steinmetz, B.

    1978-01-01

    The fuel rod modeling codes IAMBUS and COMETHE were used in the analysis and interpretation of postirradiation examination results of mixed-oxide fuel pins. These codes were developed in the framework of the SNR-300 research and development (R and D) program at Interatom and Belgonucleaire, respectively. SNR-300 is a liquid-metal fast breeder reactor demonstration plant designed and presently constructed in consortial cooperation by Germany, Belgium, and the Netherlands. RAPSODIE I, the two-bundle irradiation experiment, was irradiated in the French test FBR RAPSODIE FORTISSIMO and is one of the key irradiation experiments within the SNR-300 R and D program. The comparison of code predictions with postirradiation examination results concentrates on clad diameter expansions, clad total axial elongations, fuel differential and total axial elongations, fuel restructuring, and fission gas release. Fuel rod modeling was considered in the light of benchmarking of the codes, and there was consideration of fuel rod design for operation at low and high burnup

  10. Magnetic switch for reactor control rod

    International Nuclear Information System (INIS)

    Germer, J.H.

    1986-01-01

    This patent describes a control rod system for a nuclear reactor utilizing an electromagnetic grapple mechanism for holding and releasing a control rod, the improvement comprising a magnetic reed switch assembly having a Curie-point magnetic shunt and responsive to reactor coolant temperature for short circuiting the electromagnetic grapple mechanism causing release of the control rod when the coolant temperature reaches the Curie-point of the magnetic shunt. The magnetic reed switch assembly includes a: a permanent magnet, a pair of magnetic pole pieces located at and in contact with opposite ends of the permanent magnet, the Curie-point magnetic shunt being positioned adjacent the permanent magnet and in contact with the pair of magnetic pole pieces, and a reed switch positioned intermediate the pole pieces and provided with a pair of ferromagnetic reeds, a nonmagnetic enclosure around the reeds, a first of the reeds being secured at one end to a first of the pair of pole pieces, a second of the reeds having one end extending into and secured to a hollow member positioned in and extending through a second of the pair of pole pieces, the one end of the second of the reeds secured to a condector adapted to be connected to the electromagnetic grapple mechanism

  11. Degradation resistant fuel cladding materials and manufacturing

    Energy Technology Data Exchange (ETDEWEB)

    Marlowe, M.O. [GE Nuclear Energy, Wilmington, NC (United States); Montes, J. [ENUSA, Madrid (Spain)

    1995-12-31

    GE has been producing the degradation resistant cladding (zirconium liner and zircaloy-2 surface larger) described here with the cooperation of its primary zirconium vendors since the beginning of 1994. Approximately 24 fuel reloads, or in excess of 250,000 fuel rods, have been produced using this material by GE. GE has also produced tubing for one reload of fuel that is currently being produced by its technology affiliate ENUSA. (orig./HP)

  12. Leaked water detection device for control rod drive and BWR type reactor

    International Nuclear Information System (INIS)

    Takahashi, Ken.

    1995-01-01

    The device of the present invention can specify a control rod drive causing great amount of water leakage among a large number of control rod drives. Namely, water leaked from the control rod drives is introduced to each of leaked water pipelines. Further, it is introduced from the leaked water pipelines to flow glasses at which leaked water can visually be recognized individually, and then discharged through a drain pipeline. With such procedures, the amount of leaked water from the leaked water pipelines can visually be recognized at the flow glasses. As a result, the control rod drives which cause a great amount of leakage can be specified among large number of control rod drives. Accordingly, an accurate inspection schedule for a shaft-sealing portion of the control rod drives can be formed. The shaft-sealing portion degradated in the sealing property can reliably be inspected and repaired. Purge water can be ensured to improve reliability of the operation of equipments. (I.S.)

  13. Control Rod Driveline Reactivity Feedback Model for Liquid Metal Reactors

    International Nuclear Information System (INIS)

    Kwon, Young-Min; Jeong, Hae-Yong; Chang, Won-Pyo; Cho, Chung-Ho; Lee, Yong-Bum

    2008-01-01

    The thermal expansion of the control rod drivelines (CRDL) is one important passive mitigator under all unprotected accident conditions in the metal and oxide cores. When the CRDL are washed by hot sodium in the coolant outlet plenum, the CRDL thermally expands and causes the control rods to be inserted further down into the active core region, providing a negative reactivity feedback. Since the control rods are attached to the top of the vessel head and the core attaches to the bottom of the reactor vessel (RV), the expansion of the vessel wall as it heats will either lower the core or raise the control rods supports. This contrary thermal expansion of the reactor vessel wall pulls the control rods out of the core somewhat, providing a positive reactivity feedback. However this is not a safety factor early in a transient because its time constant is relatively large. The total elongated length is calculated by subtracting the vessel expansion from the CRDL expansion to determine the net control rod expansion into the core. The system-wide safety analysis code SSC-K includes the CRDL/RV reactivity feedback model in which control rod and vessel expansions are calculated using single-nod temperatures for the vessel and CRDL masses. The KALIMER design has the upper internal structures (UIS) in which the CRDLs are positioned outside the structure where they are exposed to the mixed sodium temperature exiting the core. A new method to determine the CRDL expansion is suggested. Two dimensional hot pool thermal hydraulic model (HP2D) originally developed for the analysis of the stratification phenomena in the hot pool is utilized for a detailed heat transfer between the CRDL mass and the hot pool coolant. However, the reactor vessel wall temperature is still calculated by a simple lumped model

  14. The physical and chemical degradation of PWR fuel rods in severe accident conditions

    International Nuclear Information System (INIS)

    Parsons, P.D.; Mowat, J.A.S.; Dewhurst, D.W.F.; Hughes, T.E.

    1983-01-01

    An experimental study of the interaction between Zircaloy-4 cladding and UO 2 in PWR fuel rods heated to high temperatures with a negligible differential pressure across the cladding wall is described. The fuel rods were of dimensions appropriate to the 17x17 PWR fuel sub-assembly and were heated in a non-oxidising environment (vacuum) up to approx. 1850 deg. C either isothermally or through heating ramps. Observations were made concerning the extent and nature of the reaction zone between Zircaloy-4 and UO 2 over the temperature range 1500-1850 deg. C for times ranging from 1 min to 125 min. The location, morphology and the chemical composition of the phases formed are described along with the kinetics of their formation. (author)

  15. Control rod ejection analysis during a depressurization accident and the development of a rod-ejection-preventing device

    International Nuclear Information System (INIS)

    Mitake, S.; Itoh, K.; Fukushima, H.; Inoue, T.

    1982-01-01

    The control rods used for the experimental VHTR are suspended in the core by means of flexible steel cables and it is conceivable that an accidental rod ejection could occur due to a depressurization accident. The computer code AFLADE was developed in order to analyze the possibility of accidental rod ejection, and several studies were performed. The parametric study results showed that the adopted design condition for the VHTR core will not cause a rod ejection accident. In parallel with these accident analyses, a rod-ejection-preventing device was developed in preparation for a hypothetical accident, and its function was verified by the component tests

  16. Rolls-Royce digital Rod Control System

    International Nuclear Information System (INIS)

    Pouillot, M.

    2010-01-01

    Full text of publication follows: Rolls-Royce has developed a new generation of Rod Control System, based on 40 years of experience. The fifth-generation Rod Control System (RCS) from Rolls-Royce offers a reliable, modular design with adaptability to your preferred platform, for modernization projects or new reactors. Flexible implementation provides the option for you to keep existing cabinets, which permits you to optimize installation approach. Main features for the power part: - Control Rod Drive Mechanism (CRDM) type: 3-coil. - Independent control of each sub-bank. - Each sub-bank is controlled by a cycler unit and 3 identical power racks, each including 4 identical power modules and a common power-supply module. - Coil-per-coil digital control: each power module embeds power-conversion, current-control, and current-monitoring functions for one coil. Control and monitoring are carried out by separate electronics in the module. Current is digitized and fully monitored by means of min-max templates. - A double-hold function is included: a power module assigned to a gripper will activate its coil if a fault risking to cause a reactor trip occurs. - Power modules are standardized, hot-pluggable and self-configured: a power module includes a set of parameters for each type of coil SG, MG, LC. The module recognizes the rack it is plugged in, and chooses automatically parameters to be used. Main benefits: - Reduced operational, maintenance, training, and inventory costs: standardization of power modules and integration of control and monitoring on the same PC-card lead to a drastic reduction of spare part types, and simplification of the system. - Easy maintenance: - Replacement of a power module solves nearly all failures due to current control or monitoring for a coil. It is done instantly thanks to hot-plug capability. - On the front plate of power-modules, LEDs provide useful information for diagnostic: current setpoint from cycler, output current bar

  17. In-reactor fuel cladding external corrosion measurement process and results

    International Nuclear Information System (INIS)

    Thomazet, J.; Musante, Y.; Pigelet, J.

    1999-01-01

    Analysis of the zirconium alloy cladding behaviour calls for an on-site corrosion measurement device. In the 80's, a FISCHER probe was used and allowed oxide layer measurements to be taken along the outer generating lines of the peripheral fuel rods. In order to allow measurements on inner rods, a thin Eddy current probe called SABRE was developed by FRAMATOME. The SABRE is a blade equipped with two E.C coils is moved through the assembly rows. A spring allows the measurement coil to be clamped on each of the generating lines of the scanned rods. By inserting this blade on all four assembly faces, measurements can also be performed along several generating lines of the same rod. Standard rings are fitted on the device and allow on-line calibration for each measured row. Signal acquisition and processing are performed by LAGOS, a dedicated software program developed by FRAMATOME. The measurements are generally taken at the cycle outage, in the spent fuel pool. On average, data acquisition calls for one shift per assembly (eight hours): this corresponds to more than 2500 measurement points. These measurements are processed statistically by the utility program SAN REMO. All the results are collected in a database for subsequent behaviour analysis: examples of investigated parameters are the thermal/hydraulic conditions of the reactors, the irradiation history, the cladding material, the water chemistry This analysis can be made easier by comparing the behaviour measurement and prediction by means of the COROS-2 corrosion code. (author)

  18. Investigation of likely causes of white patch formation on irradiated WWER fuel rod claddings

    International Nuclear Information System (INIS)

    Bibilashvili, Yu.K.; Velioukhanov, V.P.; Ioltoukhovski, A.Y.; Pogodin, V.P.

    1999-01-01

    The information concerning white patches observed on fuel cladding surfaces has been analytically treated. The analysis shows at least three kinds of the white patch appearance: bright white spots which appear to be loose corrosion product deposits disclosing corrosion pits upon spalling; indistinct streaks with separate pronounced spots 1-2 in dia. The spots seem to be thin superficial deposits; light-coloured dense uniform crud distributed over the surface of fuel claddings and fuel assembly jackets. (author)

  19. Two-group Current-equivalent Parameters for Control Rod Cells. Autocode Programme CRCC

    Energy Technology Data Exchange (ETDEWEB)

    Norinder, O; Nyman, K

    1962-06-15

    In two-group neutron diffusion calculations there is mostly necessary to describe the influence of control rods by equivalent homogeneous two-group parameters in regions about the control rods. The problem is solved for a control rod in a medium characterized by two-group parameters. The property of fast and thermal neutr. on current equivalence is selected to obtain equivalent two-group parameters for a homogeneous cell with the same radius as the control rod cell. For the parameters determined one obtains the same fast and thermal neutron current into the rod cell and the equivalent cell independent of the fast and thermal flux amplitudes on the cell boundaries. The equivalent parameters are obtained as a solution of a system of transcendental equations. A Ferranti Mercury Autocode performing the solution is described. Calculated equivalent parameters for control rods in a heavy water lattice are given for some representative cases.

  20. Detection and mitigating rod drive control system degradation in Westinghouse PWRs

    International Nuclear Information System (INIS)

    Gunther, W.; Sullivan, K.

    1990-01-01

    A study of the effects of aging on the Westinghouse Control Rod Drive (CRD) System was performed as part of the US NRC's Nuclear Plant aging Research (NPAR) Program. For the study, the CRD system boundary includes the power and logic cabinets associated with the manual control rod movement, and the control rod mechanism itself. The aging-related degradation of the interconnecting cables and connectors and the rod position indicating system also were considered. This paper presents the results of that study pertaining to the electrical and instrumentation portions of the CRD system including ways to detect and mitigate system degradation