  1. Randomized controlled split-mouth clinical trial of direct laminate veneers with two micro-hybrid resin composites

    NARCIS (Netherlands)

    Gresnigt, Marco M. M.; Kalk, Warner; Ozcan, M.; Ozcan, Mutlu

    Objectives: This randomized, split-mouth clinical study evaluated the survival rate of direct laminate veneers made of two resin-composite materials. Methods: A total of 23 patients (mean age: 52.4 years old) received 96 direct composite laminate veneers using two micro-hybrid composites in

  2. Wettability and Impact Performance of Wood Veneer/Polyester Composites

    Directory of Open Access Journals (Sweden)

    Shayesteh Haghdan

    2015-07-01

    Full Text Available Fiber-reinforced thermosetting composites have been of interest since the 1940s due to their ease of use in processing, fast curing times, and high specific stiffness and strength. While the use of plant fibers in a polyester matrix has been thoroughly studied, only limited information is available regarding using wood as reinforcement. In this study, composites of thin wood veneer and a polyester matrix were made and the difficulties in the lamination and curing processes were investigated. Sheets of Douglas fir, maple, and oak veneers using a catalyzed polyester resin were assembled as unidirectional, balanced, and unbalanced cross-ply laminates. These were compared to control specimens using glass fiber as reinforcement. The impact properties of the samples, with respect to the laminate thicknesses, were characterized using a drop-weight impact tester. The wettability and surface roughness of unsanded and sanded wood veneers were also investigated. Results showed that Douglas fir cross-ply laminates had an impact energy equivalent to glass fiber laminates, making them an interesting alternative to synthetic fiber composites. Wood/polyester laminates absorbed a considerable amount of energy through a higher number of fracture modes. The balanced lay-up limited twisting of the wood/polyester composites. The lowest contact angle and highest wettability were observed in unsanded Douglas fir veneers.

  3. Effect of Static and Cyclic Loading on Ceramic Laminate Veneers Adhered to Teeth with and Without Aged Composite Restorations

    NARCIS (Netherlands)

    Gresnigt, Marco M. M.; Ozcan, Mutlu; Kalk, Warner; Galhano, Graziela

    2011-01-01

    Purpose: Existing composite restorations on teeth are often remade prior to the cementation of fixed dental prostheses. The aim of this study was to evaluate the effect of static and cyclic loading on ceramic laminate veneers adhered to aged resin composite restorations. Materials and Methods:

  4. Production of laminated veneer lumber LVL using veneer of Schizolobium amazonicum, Eucalyptus saligna and Pinus taeda

    Directory of Open Access Journals (Sweden)

    Setsuo Iwakiri

    2010-12-01

    Full Text Available This research evaluated the quality of laminated veneer lumber - LVL manufactured with veneers of Schizolobium amazonicum (paricá, Eucalyptus saligna and Pinus taeda. The LVL panels were manufactured in the laboratory conditions composed by seven veneers, 2,0 mm thickness, with different structural compositions, using phenol-formaldehyde resin. The veneers of Schizolobium amazonicum- paricá- were pre-classified by using stress wave machine. The veneers of Eucalyptus saligna and Pinus taeda were disposed in the face layer to reinforce the structural strength of LVL panels. The LVL quality was evaluated using glue line shear strength and static bending test (MOE and MOR, edge and flat. Grading of paricá veneers based on MOEd did not affected significantly the results of the glue line shear strength and MOE and MOR edge. For the MOE and MOR flat, the use of veneers of MOEd grade 1 contributed significantly to increasing the average values of these properties. In the same way, using the Eucalyptus saligna veneers on the face of LVL resulted in higher average values of MOE and MOR, edge and flat.

  5. Masking ability of bi- and tri- laminate all-ceramic veneers on tooth-colored ceramic discs.

    Science.gov (United States)

    Farhan, Daniel; Sukumar, Smitha; von Stein-Lausnitz, Axel; Aarabi, Ghazal; Alawneh, Ahmad; Reissmann, Daniel R

    2014-01-01

    A predictable esthetic outcome is imperative when placing ceramic veneers. Discolored teeth pose a major challenge as sufficient material thickness is required to achieve a good esthetic result. There is limited evidence in the literature that compares the masking ability of multi-laminate veneers. The aim of this in-vitro study was to compare the masking ability of bi-laminate (BL) and tri-laminate (TL) all-ceramic veneers cemented on tooth-colored ceramic discs. A total of 40 veneers (shade A1, 10-mm diameter, 0.8-mm thick) were manufactured-20 BL veneers (0.4-mm pressable ceramic coping veneered with 0.4-mm thick enamel layer) and 20 TL veneers (0.4-mm coping veneered with 0.2-mm thick opaque interlayer and 0.2-mm thick enamel layer). A bonding apparatus was utilized to adhesively cement all veneers on the ceramic discs (shade A1), simulating teeth of light and dark color. The resulting groups (N = 10 each) were the reference groups (shade A1 ceramic base) BL-1 and TL-1 veneers, and the test groups (shade A4 ceramic base) BL-4 and TL-4 veneers. The color of the cemented veneers was measured using a spectrophotometer. The data were converted to CIE L*a*b* coordinates, and ΔE* were calculated to allow for statistical analysis. The color differences between the samples with the A1 and A4 ceramic bases were significantly lower when covered with TL veneers (mean ΔE*: 3.2 units) than with BL veneers (mean ΔE*: 4.0 units: p bi-laminate veneers. Patients with discolored/darker teeth may benefit from a more predictable esthetic result when teeth restored with tri-laminate rather than bi-laminate veneers. © 2014 Wiley Periodicals, Inc.

  6. Flexural properties of laminated veneer lumber manufactured from ultrasonically rated red maple veneer : a pilot study.

    Science.gov (United States)

    Xiping Wang; Robert J. Ross; Brian K. Brashaw; Steven A. Verhey; John W. Forsman; John R. Erickson

    2003-01-01

    The study described in this report was conducted to examine the flexural properties of laminated veneer lumber (LVL) manufactured from red maple veneer. Ultrasonically rated veneer, which was peeled from low value red maple saw-logs, was fabricated into 1/2-in.-(1.3-cm-) and 2-in.-(5-cm-) thick LVL billets. The flexural properties of the billets and of corresponding...

  7. Influence of bruxism on survival of porcelain laminate veneers.

    Science.gov (United States)

    Granell-Ruíz, Maria; Agustín-Panadero, Rubén; Fons-Font, Antonio; Román-Rodríguez, Juan-Luis; Solá-Ruíz, María-Fernanda

    2014-09-01

    This study aims to determine whether bruxism and the use of occlusal splints affect the survival of porcelain laminate veneers in patients treated with this technique. Restorations were made in 70 patients, including 30 patients with some type of parafunctional habit. A total of 323 veneers were placed, 170 in patients with bruxism activity, and the remaining 153 in patients without it. A clinical examination determined the presence or absence of ceramic failure (cracks, fractures and debonding) of the restorations; these incidents were analyzed for association with bruxism and the use of splints. Analysis of the ceramic failures showed that of the 13 fractures and 29 debonding that were present in our study, 8 fractures and 22 debonding were related to the presence of bruxism. Porcelain laminate veneers are a predictable treatment option that provides excellent results, recognizing a higher risk of failure in patients with bruxism activity. The use of occlusal splints reduces the risk of fractures.

  8. Cervical and incisal marginal discrepancy in ceramic laminate veneering materials: A SEM analysis

    Directory of Open Access Journals (Sweden)

    Hemalatha Ranganathan

    2017-01-01

    Full Text Available Context: Marginal discrepancy influenced by the choice of processing material used for the ceramic laminate veneers needs to be explored further for better clinical application. Aims: This study aimed to evaluate the amount of cervical and incisal marginal discrepancy associated with different ceramic laminate veneering materials. Settings and Design: This was an experimental, single-blinded, in vitro trial. Subjects and Methods: Ten central incisors were prepared for laminate veneers with 2 mm uniform reduction and heavy chamfer finish line. Ceramic laminate veneers fabricated over the prepared teeth using four different processing materials were categorized into four groups as Group I - aluminous porcelain veneers, Group II - lithium disilicate ceramic veneers, Group III - lithium disilicate-leucite-based veneers, Group IV - zirconia-based ceramic veneers. The cervical and incisal marginal discrepancy was measured using a scanning electron microscope. Statistical Analysis Used: ANOVA and post hoc Tukey honest significant difference (HSD tests were used for statistical analysis. Results: The cervical and incisal marginal discrepancy for four groups was Group I - 114.6 ± 4.3 μm, 132.5 ± 6.5 μm, Group II - 86.1 ± 6.3 μm, 105.4 ± 5.3 μm, Group III - 71.4 ± 4.4 μm, 91.3 ± 4.7 μm, and Group IV - 123.1 ± 4.1 μm, 142.0 ± 5.4 μm. ANOVA and post hoc Tukey HSD tests observed a statistically significant difference between the four test specimens with regard to cervical marginal discrepancy. The cervical and incisal marginal discrepancy scored F = 243.408, P < 0.001 and F = 180.844, P < 0.001, respectively. Conclusion: This study concluded veneers fabricated using leucite reinforced lithium disilicate exhibited the least marginal discrepancy followed by lithium disilicate ceramic, aluminous porcelain, and zirconia-based ceramics. The marginal discrepancy was more in the incisal region than in the cervical region in all the groups.

  9. Interfacial Adhesion and Damping Characteristics of Laminated Veneer Lumber Intercalated with Rubber Sheets

    Directory of Open Access Journals (Sweden)

    Jingquan Han

    2016-06-01

    Full Text Available Laminated wood veneer lumber intercalated with rubber sheets (LLVR was fabricated using a layered adhesive system composed of polyaryl polymethylene isocyanate (PAPI for wood-rubber inter-bonding and phenol formaldehyde (PF resin to glue the wood veneers. The optimized manufacturing process (chloroprene rubber: CR; PAPI: 80 g/m2; PF: 200 g/m2; and silane: 9.0 wt.% was determined. The process as developed was then utilized to fabricate nine-ply LLVRs of five balanced constructions with two or three CR laminates used as various layers. The physico-mechanical properties of the LLVRs were evaluated, and the results showed that LLVRs had strong shear strength, sound dimensional stability, decent bending strength, and favorable toughening and buffering performances. The newly developed product is an interesting potential alternative to traditional laminated veneer lumber or plywood.

  10. Esthetic Rehabilitation of Anterior Teeth with Porcelain Laminates and Sectional Veneers

    NARCIS (Netherlands)

    Gresnigt, Marco; Ozcan, Mutlu

    2011-01-01

    Full-coverage bonded porcelain restorations offer predictable treatment options in dentistry, but a certain amount of tooth material must be removed to allow space for the required thickness of the restorative material. Laminate veneers and inlays are considered minimally invasive, but they also

  11. Randomized Clinical Trial of Indirect Resin Composite and Ceramic Veneers : Up to 3-year Follow-up

    NARCIS (Netherlands)

    Gresnigt, Marco M. M.; Kalk, Warner; Ozcan, Mutlu

    2013-01-01

    Purpose: This randomized controlled split-mouth clinical trial evaluated the short-term survival rate of indirect resin composite and ceramic laminate veneers. Materials and Methods: A total of 10 patients (mean age: 48.6 years) received 46 indirect resin composite (Estenia; n = 23) and ceramic

  12. Esthetic restorations of maxillary anterior teeth with orthodontic treatment and porcelain laminate veneers: a case report.

    Science.gov (United States)

    Moon, Ji-Eun; Kim, Sung-Hun; Han, Jung-Suk; Yang, Jae-Ho; Lee, Jai-Bong

    2010-06-01

    If orthodontists and restorative dentists establish the interdisciplinary approach to esthetic dentistry, the esthetic and functional outcome of their combined efforts will be greatly enhanced. This article describes satisfying esthetic results obtained by the distribution of space for restoration by orthodontic treatment and porcelain laminate veneers in uneven space between maxillary anterior teeth. It is proposed that the use of orthodontic treatment for re-distribution of the space and the use of porcelain laminate veneers to alter crown anatomy provide maximum esthetic and functional correction for patients with irregular interdental spacing.

  13. Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading

    Directory of Open Access Journals (Sweden)

    Leyla Sadighpour

    2018-01-01

    Full Text Available Purpose. Porcelain laminate veneers (PLVs are sometimes required to be used for teeth with composite fillings. This study examined the fracture strength of PLVs bonded to the teeth restored with different sizes of class V composite fillings. Materials and Methods. Thirty-six maxillary central incisors were divided into three groups (n=12: intact teeth (control and teeth with class V composite fillings of one-third or two-thirds of the crown height (small or large group, resp.. PLVs were made by using IPS e.max and bonded with a resin cement (RelyX Unicem. Fracture resistance (N was measured after cyclic loading (1 × 106 cycles, 1.2 Hz. For statistical analyses, one-way ANOVA and Tukey test were used (α=0.05. Results. There was a significant difference between the mean failure loads of the test groups (P=0.004, with the Tukey-HSD test showing lower failure loads in the large-composite group compared to the control (P=0.02 or small group (P=0.05. The control and small-composite groups achieved comparable results (P>0.05. Conclusions. Failure loads of PLVs bonded to intact teeth and to teeth with small class V composite fillings were not significantly different. However, extensive composite fillings could compromise the bonding of PLVs.

  14. A Step-by-Step Conservative Approach for CAD-CAM Laminate Veneers

    Directory of Open Access Journals (Sweden)

    Gerardo Durán Ojeda

    2017-01-01

    Full Text Available The use of CAD/CAM technology has allowed the fabrication of ceramic restorations efficiently and with predictable results. Lithium disilicate is a type of glass ceramic material that can be used for the elaboration of laminate veneers, being monolithic restorations which require characterization through a covering ceramic in order to achieve acceptable esthetic results. The next case report shows a predictable clinical protocol for the rehabilitation of the anterior teeth through the preparation of CAD/CAM veneers (e.max CAD, Ivoclar Vivadent, Liechtenstein which have been characterized by a nanofluorapatite ceramic (e.max Ceram, Ivoclar Vivadent, Liechtenstein through the layering technique.

  15. Fracture strengths of chair-side-generated veneers cemented with glass fibers.

    Science.gov (United States)

    Turkaslan, S; Bagis, B; Akan, E; Mutluay, M M; Vallittu, P K

    2015-01-01

    CAD/CAM (computer-aided design and computer-aided manufacturing) systems have refreshed the idea of chair-side production of restorations, but the fracture of ceramic veneers remains a problem. Cementation with glass fibers may improve the fracture strengths and affect the failure modes of CAD/CAM-generated ceramic veneers. Therefore, this study compared the fracture strengths of ceramic veneers produced at chair side and cemented with or without glass fibers with those of composite veneers. Thirty intact mandibular incisors were randomly divided into three groups ( n = 10) and treated with CAD/CAM-fabricated veneers cemented with dual-cure composite resin luting cement (CRLC; Group 1), CAD/CAM-fabricated veneers cemented with a glass fiber network (GFN) and dual-cure CRLC (Group 2), and a direct particulate filler composite veneer constructed utilizing fiber and a restorative composite resin (Group 3). The specimens were tested with a universal testing machine after thermal cycling treatment. The loads at the start of fracture were the lowest for traditionally fabricated composite veneers and higher for CAD/CAM-generated. Veneers cemented either without or with the GFN. The failure initiation loads (N) for the veneers were 798.92 for Group 1, 836.27 for Group 2, and 585.93 for Group 3. The predominant failure mode is adhesive failure between the laminates and teeth for Group 1, cohesive failure in the luting layer for Group 2, and cohesive laminate failure for Group 3, which showed chipping and small fractures. Ceramic material is a reliable alternative for veneer construction at chair side. Fibers at the cementation interface may improve the clinical longevity and provide higher fracture strength values.

  16. Comparison of Marginal and Internal Adaptation of Heat-Pressed and CAD/CAM Porcelain Laminate Veneers and a 2-Year Follow-Up.

    Science.gov (United States)

    Yuce, Mert; Ulusoy, Mubin; Turk, Ayse Gozde

    2017-12-22

    To compare marginal and internal adaptations of porcelain laminate veneers fabricated with heat-pressed and CAD/CAM techniques, and to evaluate the clinical performances 2 years after cementation. Thirty heat-pressed and 31 CAD/CAM porcelain laminate veneers were fabricated for 12 patients. Silicone replicas of each veneer were obtained. Replicas were sectioned into 4 parts to measure adaptations of the veneers. A stereomicroscope was used to measure from 3 locations of replicas for marginal, and 9 locations for internal adaptations at 40x magnification. Clinical evaluations were done at baseline and 6, 12, 18, and 24 months after cementation according to the modified United States Public Health Service (USPHS) criteria. Independent samples t-test compared the adaptation values between heat-pressed and CAD/CAM groups. Paired t-test was used to evaluate marginal and internal adaptations of each group. Differences between the modified USPHS criteria ratings of heat-pressed and CAD/CAM groups were determined by the Mann-Whitney U test. Kaplan-Meier analysis was used to analyze the survival ratings of the veneers (p CAD/CAM veneers were 295 and 314.98 μm, respectively, and there was no statistically significant difference (p = 0.541). Internal adaptation values of groups were not statistically different either (201.82 μm for heat pressed; 195.47 μm for CAD/CAM p = 0.734). When marginal and internal adaptation values were compared within groups, there were significant differences both for heat-pressed (p CAD/CAM (p CAD/CAM or heat-pressed, had no effect on the marginal and internal adaptation of porcelain laminate veneers. The results showed that both fabrication techniques performed well after 2 years of clinical performance. © 2017 by the American College of Prosthodontists.

  17. Effect of Provisional Cements on Shear Bond Strength of Porcelain Laminate Veneers

    OpenAIRE

    Altintas, Subutay Han; Tak, Onjen; Secilmis, Asli; Usumez, Aslihan

    2011-01-01

    Objectives: The purpose of this study was to evaluate the effect of three provisional cements and two cleaning techniques on the final bond strength of porcelain laminate veneers. Methods: The occlusal third of the crowns of forty molar teeth were sectioned and embedded in autopolymerizing acrylic resin. Dentin surfaces were polished and specimens were randomly divided into four groups (n=10). Provisional restorations were fabricated and two provisional restorations were cemented onto each to...

  18. Influence of Different Types of Resin Luting Agents on Color Stability of Ceramic Laminate Veneers Subjected to Accelerated Artificial Aging.

    Science.gov (United States)

    Silami, Francisca Daniele Jardilino; Tonani, Rafaella; Alandia-Román, Carla Cecilia; Pires-de-Souza, Fernanda de Carvalho Panzeri

    2016-01-01

    The aim of this study was to evaluate the influence of accelerated aging (AAA) on the color stability of resin cements for bonding ceramic laminate veneers of different thicknesses. The occlusal surfaces of 80 healthy human molars were flattened. Ceramic laminate veneers (IPS e-max Ceram) of two thicknesses (0.5 and 1.0 mm) were bonded with three types of luting agents: light-cured, conventional dual and self-adhesive dual cement. Teeth without restorations and cement samples (0.5 mm) were used as control. After initial color evaluations, the samples were subjected to AAA for 580 h. After this, new color readouts were made, and the color stability (ΔE) and luminosity (ΔL) data were analyzed. The greatest color changes (p<0.05) occurred when 0.5 mm veneers were fixed with light-cured cement and the lowest when 1.0 mm veneers were fixed with conventional dual cement. There was no influence of the restoration thickness when the self-adhesive dual cement was used. When veneers were compared with the control groups, it was verified that the cement samples presented the greatest alterations (p<0.05) in comparison with both substrates and restored teeth. Therefore, it was concluded that the thickness of the restoration influences color and luminosity changes for conventional dual and light-cured cements. The changes in self-adhesive cement do not depend on restoration thickness.

  19. Porcelain veneer post-bonding crack repair by resin infiltration

    NARCIS (Netherlands)

    Gresnigt, Marco; Magne, Michel; Magne, Pascal

    2017-01-01

    Ceramic laminate veneer restorations are indicated in several clinical situations. Indirect restorations are usually chosen if the less-invasive options - bleaching, resin infiltration, or composite resin restorations - are not possible, or when it is too difficult to achieve an esthetically

  20. EFFECTS OF PRESS PRESSURE ON GLUE LINE THICKNESS AND PROPERTIES OF LAMINATED VENEER LUMBER GLUED WITH MELAMINE UREA FORMALDEHYDE ADHESIVE

    Directory of Open Access Journals (Sweden)

    Ramazan Kurt,

    2012-07-01

    Full Text Available Laminated veneer lumbers (LVLs were manufactured from half-round sliced I-214 hybrid poplar clone veneers with MUF adhesives using press pressures ranging from 2.5 to 15 kg cm-2. The results showed that the press pressures affected the glue line thickness (GLT and the physical and mechanical properties of the LVLs. Higher specific gravity (SG and mechanical properties, but lower GLT were developed as a result of using higher press pressures. The optimum press pressure was found to be 10 kg cm-2 in relation to GLT, SG, and mechanical properties. Significant linear correlations were found between GLT and mechanical properties. GLT can be used to determine the quality of wood bonding and may become a valuable tool for this purpose. Reliable data on the optimum GLT and press pressures can be used to design safe wood bonding applications in all aspects of wood based composites, as well as wood constructions when appropriate techniques are adopted to measure the GLT.

  1. The clinical microscope and direct composite veneer

    DEFF Research Database (Denmark)

    Pascotto, Renata C; Benetti, Ana Raquel

    2010-01-01

    This paper presents the advantages and limitations related to the use of a clinical microscope in restorative dentistry, and it demonstrates the aid of magnification during preparation and restoration of a direct composite veneer. Good illumination and visibility is important to adequately viewin...... the adjacent dental tissues so that the resin composite buildup can mimic natural teeth. The reproduction of details results in a naturally esthetic direct veneer....

  2. Effect of luting agent on the load to failure and accelerated-fatigue resistance of lithium disilicate laminate veneers

    NARCIS (Netherlands)

    Gresnigt, Marco M. M.; Ozcan, Mutlu; Carualho, Marco; Lazari, Priscilla; Cune, Marco S.; Razavi, Peywand; Magne, Pascal

    2017-01-01

    Objective. The aim of this study was to investigate the influence of the luting agent on the application of laminate veneers (LVs) in an accelerated fatigue and load-to-failure test after thermo-cyclic aging. Methods. Sound maxillary central incisors (N = 40) were randomly divided into four groups

  3. Effect of immediate and delayed dentin sealing on the fracture strength, failure type and Weilbull characteristics of lithiumdisilicate laminate veneers

    NARCIS (Netherlands)

    Gresnigt, Marco M.M.; Cune, Marco S.; de Roos, Joanne G.; Özcan, Mutlu

    OBJECTIVES: Adhesion on dentin is less reliable than on enamel, which could affect the durability of laminate veneers (LV). Immediate dentin sealing (IDS) is suggested instead of delayed dentin sealing (DDS) to overcome hypersensitivity and prevent debonding from dentin. This study evaluated the

  4. The Effect of Veneer Layers on the Bending Shear Strength and Delamination of Laminated Veneer Lumber (LVL) from Oil Palm Trunk (OPT)

    Science.gov (United States)

    Jamaludin, M. A.; Nordin, K.; Bahari, S. A.; Ahmad, M.

    2010-03-01

    The aim of this study was to evaluate the effects of the number of veneer layers on the bending shear strength and delamination of Laminated Veneer Lumber (LVL) from oil palm trunk (OPT). Five (5), Six (6) and Seven (7) veneer layers of OPT LVL were manufactured. The dimension of the boards was 45 cm by 45 cm by 1.9 cm. The boards were hot pressed for 13 minutes at a pressure of 31 kgf per m2. Urea formaldehyde (UF) supplied by a local adhesive manufacturer was used as the binder for the boards. The bending shear tests consisted of the edgewise and flatwise tests, whereas the delamination test consisted of the cold and hot water boil tests. The preparation of the test specimens and tests set-up was in accordance to the Japanese Standards, JAS-1991 [1]. Six replications were used for each test. The results were analyzed by Analysis of Variance (ANOVA) using the Duncan's Multiple Range Test to test for significant differences. The results indicated that as the number of layers increased the strength also increased. All the boards passed the standard. The difference in strength between the different types of samples was significant at 95 percent confidence level. Bending shear failures were primarily in the veneers. It is possible to use the boards as light weight interior building and furniture components. Over the years, the supply of quality timber resources from the natural forest has decrease as the wood-based industry experienced rapid growth. The supply of rubberwood for the furniture industry is also decreasing as a result of increase latex price. Accordingly, OPT LVL can be an alternative or supplementary raw material for the wood-based industry.

  5. Effectiveness of optical illusions 
applied on a single composite resin veneer for the diastema closure 
of maxillary central incisors.

    Science.gov (United States)

    Katsarou, Thomai; Antoniadou, Maria; Papazoglou, Efstratios

    To assess the esthetic effectiveness of four illusion techniques applied to a composite resin veneer for diastema closure between maxillary central incisors. An acrylic model with six natural maxillary anterior teeth was fabricated with a 2-mm diastema between the central incisors. Resin veneers were constructed on the left central incisor and the following cases were derived: V0: no veneer; V1: veneer without optical illusion features; V2: veneer with centralized interproximal ridges; V3: veneer with curved incisal edges; V4: veneer with gray pigment mesially/distally; V5: veneer with gray pigment on the developmental lobes. Digital printed photos of the models (13.2 x 17.8 cm, and 6.1 x 8 cm), with low, medium, and high smile lines and without a smile line (processed by Adobe Photoshop CS6) were shown to three groups of people (faculty members, senior undergraduate students, and patients; n = 25/group) for them to assess the overall size and width of the two central incisors. The results were analyzed by Pearson's and chi-square goodness of fit tests. There was no significant influence in the estimation of the two central incisors as being the same size, according to the technique used (P = 0.869) and group of evaluators (P = 0.209). The estimated probability of assessing the tested incisor as wider was indicatively lower in V2 compared to V1 (adjusted odds ratio = 0.59; P = 0.088). The height of the smile line affected the evaluation of the veneers only in the large-sized photos. No interference is the best esthetic decision concerning a 2-mm diastema closure when restoring only one central incisor with a laminate veneer. The next best option is to deliver a veneer with centralized interproximal ridges.

  6. Simplified treatment of severe dental erosion with ultrathin CAD-CAM composite occlusal veneers and anterior bilaminar veneers.

    Science.gov (United States)

    Schlichting, Luís Henrique; Resende, Tayane Holz; Reis, Kátia Rodrigues; Magne, Pascal

    2016-10-01

    Restorative treatment for patients with dental erosion requires an analysis of the degree of structural damage. Patients affected by moderate to severe dental erosion are particularly challenging because complex occlusal reconstruction will be needed. Ultrathin bonded occlusal veneers represent a conservative alternative to traditional onlays and complete coverage crowns for the treatment of severe erosion. This article describes a complete mouth rehabilitation with ultrathin computer-aided design and computer-aided manufacturing (CAD-CAM) composite resin occlusal veneers in a patient with a severely eroded dentition. In the maxillary anterior teeth, the bilaminar approach was chosen with lingual composite resin veneers and labial porcelain veneers. The main benefit of this approach is the possibility of using additive adhesive techniques, allowing only strategic reduction of sound dental structure or no preparation. Copyright © 2016 Editorial Council for the Journal of Prosthetic Dentistry. Published by Elsevier Inc. All rights reserved.

  7. Main Clinical Outcomes of Feldspathic Porcelain and Glass-Ceramic Laminate Veneers: A Systematic Review and Meta-Analysis of Survival and Complication Rates.

    Science.gov (United States)

    Morimoto, Susana; Albanesi, Rafael Borges; Sesma, Newton; Agra, Carlos Martins; Braga, Mariana Minatel

    2016-01-01

    The aim of this study was to perform a systematic review and meta-analysis based on clinical trials that evaluated the main outcomes of glass-ceramic and feldspathic porcelain laminate veneers. A systematic search was carried out in Cochrane and PubMed databases. From the selected studies, the survival rates for porcelain and glass-ceramic veneers were extracted, as were complication rates of clinical outcomes: debonding, fracture/chipping, secondary caries, endodontic problems, severe marginal discoloration, and influence of incisal coverage and enamel/dentin preparation. The Cochran Q test and the I(2) statistic were used to evaluate heterogeneity. Out of the 899 articles initially identified, 13 were included for analysis. Metaregression analysis showed that the types of ceramics and follow-up periods had no influence on failure rate. The estimated overall cumulative survival rate was 89% (95% CI: 84% to 94%) in a median follow-up period of 9 years. The estimated survival for glass-ceramic was 94% (95% CI: 87% to 100%), and for feldspathic porcelain veneers, 87% (95% CI: 82% to 93%). The meta-analysis showed rates for the following events: debonding: 2% (95% CI: 1% to 4%); fracture/chipping: 4% (95% CI: 3% to 6%); secondary caries: 1% (95% CI: 0% to 3%); severe marginal discoloration: 2% (95% CI: 1% to 10%); endodontic problems: 2% (95% CI: 1% to 3%); and incisal coverage odds ratio: 1.25 (95% CI: 0.33 to 4.73). It was not possible to perform meta-analysis of the influence of enamel/dentin preparation on failure rates. Glass-ceramic and porcelain laminate veneers have high survival rates. Fracture/ chipping was the most frequent complication, providing evidence that ceramic veneers are a safe treatment option that preserve tooth structure.

  8. Effect of stacking sequence on mechanical properties neem wood veneer plastic composites

    Science.gov (United States)

    Nagamadhu, M.; Kumar, G. C. Mohan; Jeyaraj, P.

    2018-04-01

    This study investigates the effect of wood veneer stacking sequence on mechanical properties of neem wood polymer composite (WPC) experimentally. Wood laminated samples were fabricated by conventional hand layup technique in a mold and cured under pressure at room temperature and then post cured at elevated temperature. Initially, the tensile, flexural, and impact test were conducted to understand the effect of weight fraction of fiber on mechanical properties. The mechanical properties have increased with the weight fraction of fiber. Moreover the stacking sequence of neem wood plays an important role. As it has a significant impact on the mechanical properties. The results indicated that 0°/0° WPC shows highest mechanical properties as compared to other sequences (90°/90°, 0°/90°, 45°/90°, 45°/45°). The Fourier Transform Infrared Spectroscopy (FTIR) Analysis were carried out to identify chemical compounds both in raw neem wood and neem wood epoxy composite. The microstructure raw/neat neem wood and the interfacial bonding characteristics of neem wood composite investigated using Scanning electron microscopy images.

  9. Shear bond strength of porcelain laminate veneers to enamel, dentine and enamel-dentine complex bonded with different adhesive luting systems.

    Science.gov (United States)

    Öztürk, Elif; Bolay, Şükran; Hickel, Reinhard; Ilie, Nicoleta

    2013-02-01

    The aim of this study was to evaluate the shear bond strength of porcelain laminate veneers to 3 different surfaces by means of enamel, dentine, and enamel-dentine complex. One hundred thirty-five extracted human maxillary central teeth were used, and the teeth were randomly divided into 9 groups (n=15). The teeth were prepared with 3 different levels for bonding surfaces of enamel (E), dentine (D), and enamel-dentine complex (E-D). Porcelain discs (IPS e.max Press, Ivoclar Vivadent) of 2mm in thickness and 4mm in diameter were luted to the tooth surfaces by using 2 light-curing (RelyX Veneer [RV], 3M ESPE; Variolink Veneer [VV], Ivoclar Vivadent) and a dual-curing (Variolink II [V2], Ivoclar Vivadent) adhesive systems according to the manufacturers' instructions. Shear bond strength test was performed in a universal testing machine at 0.5mm/min until bonding failure. Failure modes were determined under a stereomicroscope, and fracture surfaces were evaluated with a scanning electron microscope. The data were statistically analysed (SPSS 17.0) (p=0.05). Group RV-D exhibited the lowest bond strength value (5.42±6.6MPa). There was statistically no difference among RV-D, V2-D (13.78±8.8MPa) and VV-D (13.84±6.2MPa) groups (p>0.05). Group VV-E exhibited the highest bond strength value (24.76±8.8MPa). The type of tooth structure affected the shear bond strength of the porcelain laminate veneers to the 3 different types of tooth structures (enamel, dentine, and enamel-dentine complex). When dentine exposure is necessary during preparation, enough sound enamel must be protected as much as possible to maintain a good bonding; to obtain maximum bond strength, preparation margins should be on sound enamel. Copyright © 2012 Elsevier Ltd. All rights reserved.

  10. Digital workflow for virtually designing and milling ceramic lithium disilicate veneers: a clinical report.

    Science.gov (United States)

    Zandinejad, A; Lin, W S; Atarodi, M; Abdel-Azim, T; Metz, M J; Morton, D

    2015-01-01

    Laminate veneers have been routinely used to restore and enhance the appearance of natural dentition. The traditional pathway for fabricating veneers consisted of making conventional polyvinyl siloxane impressions, producing stone casts, and fabricating final porcelain prostheses on stone dies. Pressed ceramics have successfully been used for laminate veneer fabrication for several years. Recently, digital computer-aided design/computer-aided manufacturing scanning has become commercially available to make a digital impression that is sent electronically to a dental laboratory or a chairside milling machine. However, technology has been developed to allow digital data acquisition in conjunction with electronically transmitted data that enables virtual design of restorations and milling at a remote production center. Following the aforementioned workflow will provide the opportunity to fabricate a physical cast-free restoration. This new technique has been reported recently for all-ceramic IPS e.max full-coverage pressed-ceramic restorations. However, laminate veneers are very delicate and technique-sensitive restorations when compared with all-ceramic full-coverage ones made from the same material. Complete digital design and fabrication of multiple consecutive laminate veneers seems to be very challenging. This clinical report presents the digital workflow for the virtual design and fabrication of multiple laminate veneers in a patient for enhancing the esthetics of his maxillary anterior teeth. A step-by-step process is presented with a discussion of the advantages and disadvantages of this novel technique. Additionally, the use of lithium disilicate ceramic as the material of choice and the rationale for such a decision is discussed.

  11. Design of pedestrian truss bridge with Sengon-Rubber laminated veneer lumber

    Science.gov (United States)

    Herbudiman, B.; Pranata, Y. A.; Pangestu, L.

    2017-12-01

    Timber bridges are one of the bridge that has long been used, but nowadays, large dimension of sawn timber has limited supply and also it is not environmental-friendly. Laminated veneer lumber (LVL) is a engineered wood that becomes one of the promising alternative, because it is made from lower quality wood that processed to be used as a more quality one. The bridge planned to be a pedestrian truss bridge with length of 9 m, width of 3 m, height of 2.5 m, and using bolt and steel plate as its connection system. Mechanical properties of LVL obtained directly from laboratory test result. Bridge modeling and planning for wood construction refers to SNI 7973:2013, while the loading refers to SNI 1725:2016. Based on the modelling and calculation, the dimension of truss frame and girder beam which are 9 cm x 9 cm and 9 cm x 18 cm have adequate strengths and satisfy deflection requirement.

  12. Surface roughness of composite resin veneer after application of herbal and non-herbal toothpaste

    Science.gov (United States)

    Nuraini, S.; Herda, E.; Irawan, B.

    2017-08-01

    The aim of this study was to find out the surface roughness of composite resin veneer after brushing. In this study, 24 specimens of composite resin veneer are divided into three subgroups: brushed without toothpaste, brushed with non-herbal toothpaste, and brushed with herbal toothpaste. Brushing was performed for one set of 5,000 strokes and continued for a second set of 5,000 strokes. Roughness of composite resin veneer was determined using a Surface Roughness Tester. The results were statistically analyzed using Kruskal-Wallis nonparametric test and Post Hoc Mann-Whitney. The results indicate that the highest difference among the Ra values occurred within the subgroup that was brushed with the herbal toothpaste. In conclusion, the herbal toothpaste produced a rougher surface on composite resin veneer compared to non-herbal toothpaste.

  13. Continuous jute fibre reinforced laminated paper composite

    Indian Academy of Sciences (India)

    Jute fibre; laminated paper composite; plastic bag pollution. Abstract. Plastic bags create a serious environmental problem. The proposed jute fibre reinforced laminated paper composite and reinforcement-fibre free paper laminate may help to combat the war against this pollutant to certain extent. The paper laminate ...

  14. Composite lamination method

    Science.gov (United States)

    Dickerson, G. E. (Inventor)

    1977-01-01

    A process was developed for preparing relatively thick composite laminate structure wherein thin layers of prepreg tapes are assembled, these thin layers are cut into strips that are partially cured, and stacked into the desired thickness with uncured prepreg disposed between each layer of strips. The formed laminate is finally cured and thereafter machined to the desired final dimensions.

  15. Structural properties of laminated Douglas fir/epoxy composite material

    Energy Technology Data Exchange (ETDEWEB)

    Spera, D.A. (National Aeronautics and Space Administration, Cleveland, OH (USA). Lewis Research Center); Esgar, J.B. (Sverdrup Technology, Inc., Cleveland, OH (USA)); Gougeon, M.; Zuteck, M.D. (Gougeon Bros., Bay City, MI (USA))

    1990-05-01

    This publication contains a compilation of static and fatigue and strength data for laminated-wood material made from Douglas fir and epoxy. Results of tests conducted by several organizations are correlated to provide insight into the effects of variables such as moisture, size, lamina-to-lamina joint design, wood veneer grade, and the ratio of cyclic stress to steady stress during fatigue testing. These test data were originally obtained during development of wood rotor blades for large-scale wind turbines of the horizontal-axis (propeller) configuration. Most of the strength property data in this compilation are not found in the published literature. Test sections ranged from round cylinders 2.25 in. in diameter to rectangular slabs 6 in. by 24 in. in cross section and approximately 30 ft long. All specimens were made from Douglas fir veneers 0.10 in. thick, bonded together with the WEST epoxy system developed for fabrication and repair of wood boats. Loading was usually parallel to the grain. Size effects (reduction in strength with increase in test volume) are observed in some of the test data, and a simple mathematical model is presented that includes the probability of failure. General characteristics of the wood/epoxy laminate are discussed, including features that make it useful for a wide variety of applications. 9 refs.

  16. [Interface bond and compatibility between GI-II glass/alumina composite and Vitadur alpha veneering porcelain].

    Science.gov (United States)

    Meng, Yukun; Chao, Yonglie; Liao, Yunmao

    2002-01-01

    Multiple layer techniques were commonly employed in fabricating all-ceramic restorations. Bond and compatibility between layers were vitally important for the clinical success of the restorations. The purposes of this study were to investigate the bond of the interface between the GI-II glass/alumina composite and Vitadur alpha veneering porcelain, and to study the thermal compatibility between them. Prepared a bar shaped specimen of GI-II glass/alumina composite 25 mm x 5 mm x 1 mm in size, with bottom surface pre-notched. The upper surface was veneered with Vitadur alpha veneering porcelain (0.2 mm opaque dentin and 0.6 mm dentin porcelain), then fractured and the fracture surface were examined under scanning electron microscope (SEM) and electron microprobe analyzer (EMPA) with electron beam of 10 micrometer in diameter; ten all-ceramic single crowns for an upper right central incisor were fabricated and the temperatures of thermal shock resistance were tested. SEM observation showed tight bond between the composite and the porcelain; The results of EMPA showed that penetration of Na, Al elements from glass/alumina into veneering porcelain and Si, K, Ca elements from veneering porcelain into glass/alumina occurred after sintering baking; The temperature of thermal shock resistance for anterior crowns in this study was 158 +/- 10.3 degrees C, cracks were mainly distributed in veneering porcelain with thicker layer. Chemical bond exists between the GI-II glass/alumina composite and Vitadur alpha veneering porcelain, and there is good thermal compatibility between them.

  17. Six-year follow-up with Empress veneers.

    Science.gov (United States)

    Fradeani, M

    1998-06-01

    This study reports on 6 years experience with IPS Empress laminate veneers. A total of 83 anterior veneers were positioned in 21 patients from January 1991 to December 1996 in the author's private practice. Final evaluation was carried out in May and June 1997. Color match, marginal discoloration, recurrent caries, contour, and marginal integrity were evaluated using the modified U.S. Public Health Service criteria at baseline and subsequent recall appointments. On the basis of the criteria used, a large percentage of veneers were rated Alfa. Only one failure was recorded, resulting in a success rate of 98.8%. A thorough description of clinical procedures and laboratory techniques through which anterior teeth can be successfully treated with ceramic veneers is supplied. A clinical case is presented to demonstrate the satisfactory esthetic results obtained using this very conservative restorative technique.

  18. Advances in dental veneers: materials, applications, and techniques.

    Science.gov (United States)

    Pini, Núbia Pavesi; Aguiar, Flávio Henrique Baggio; Lima, Débora Alves Nunes Leite; Lovadino, José Roberto; Terada, Raquel Sano Suga; Pascotto, Renata Corrêa

    2012-01-01

    Laminate veneers are a conservative treatment of unaesthetic anterior teeth. The continued development of dental ceramics offers clinicians many options for creating highly aesthetic and functional porcelain veneers. This evolution of materials, ceramics, and adhesive systems permits improvement of the aesthetic of the smile and the self-esteem of the patient. Clinicians should understand the latest ceramic materials in order to be able to recommend them and their applications and techniques, and to ensure the success of the clinical case. The current literature was reviewed to search for the most important parameters determining the long-term success, correct application, and clinical limitations of porcelain veneers.

  19. Yield and ultrasonic modulus of elasticity of red maple veneer

    Science.gov (United States)

    Robert J. Ross; Steven Verhey; John R. Erickson; John W. Forsman; Brian K. Brashaw; Crystal L. Pilon; Xiping Wang

    2004-01-01

    The purpose of the study was to assess the potential for using red maple sawlogs to manufacture laminated veneer lumber (LVL). The primary objective was to determine the yield of ultrasonically graded veneer from red maple logs. A sample of 48 logs was obtained from six Eastern and Lake States in the United States. The logs were visually graded and shipped to a plywood...

  20. Modeling Bistable Composite Laminates for Piezoelectric Morphing Structures

    OpenAIRE

    Darryl V. Murray; Oliver J. Myers

    2013-01-01

    A sequential modeling effort for bistable composite laminates for piezoelectric morphing structures is presented. Thin unsymmetric carbon fiber composite laminates are examined for use of morphing structures using piezoelectric actuation. When cooling from the elevated cure temperature to room temperature, these unsymmetric composite laminates will deform. These postcure room temperature deformation shapes can be used as morphing structures. Applying a force to these deformed laminates will c...

  1. Impact damages modeling in laminated composite structures

    Directory of Open Access Journals (Sweden)

    Kreculj Dragan D.

    2014-01-01

    Full Text Available Laminated composites have an important application in modern engineering structures. They are characterized by extraordinary properties, such as: high strength and stiffness and lightweight. Nevertheless, a serious obstacle to more widespread use of those materials is their sensitivity to the impact loads. Impacts cause initiation and development of certain types of damages. Failures that occur in laminated composite structures can be intralaminar and interlaminar. To date it was developed a lot of simulation models for impact damages analysis in laminates. Those models can replace real and expensive testing in laminated structures with a certain accuracy. By using specialized software the damage parameters and distributions can be determined (at certain conditions on laminate structures. With performing numerical simulation of impact on composite laminates there are corresponding results valid for the analysis of these structures.

  2. Design and evaluation of low-cost laminated wood composite blades for intermediate size wind turbines: Blade design, fabrication concept, and cost analysis

    Science.gov (United States)

    Lieblein, S.; Gaugeon, M.; Thomas, G.; Zueck, M.

    1982-01-01

    As part of a program to reduce wind turbine costs, an evaluation was conducted of a laminated wood composite blade for the Mod-OA 200 kW wind turbine. The effort included the design and fabrication concept for the blade, together with cost and load analyses. The blade structure is composed of laminated Douglas fir veneers for the primary spar and nose sections, and honeycomb cored plywood panels for the trailing edges sections. The attachment of the wood blade to the rotor hub was through load takeoff studs bonded into the blade root. Tests were conducted on specimens of the key structural components to verify the feasibility of the concept. It is concluded that the proposed wood composite blade design and fabrication concept is suitable for Mod-OA size turbines (125-ft diameter rotor) at a cost that is very competitive with other methods of manufacture.

  3. Finite elements modeling of delaminations in composite laminates

    DEFF Research Database (Denmark)

    Gaiotti, m.; Rizzo, C.M.; Branner, Kim

    2011-01-01

    of the buckling strength of composite laminates containing delaminations. Namely, non-linear buckling and post-buckling analyses are carried out to predict the critical buckling load of elementary composite laminates affected by rectangular delaminations of different sizes and locations, which are modelled......The application of composite materials in many structures poses to engineers the problem to create reliable and relatively simple methods, able to estimate the strength of multilayer composite structures. Multilayer composites, like other laminated materials, suffer from layer separation, i.......e., delaminations, which may affect the stiffness and stability of structural components. Especially deep delaminations in the mid surface of laminates are expected to reduce the effective flexural stiffness and lead to collapse, often due to buckling behaviour. This paper deals with the numerical modelling...

  4. Optimal Design of Laminated Composite Beams

    DEFF Research Database (Denmark)

    Blasques, José Pedro Albergaria Amaral

    model for the analysis of laminated composite beams is proposed. The structural analysis is performed in a beam finite element context. The development of a finite element based tool for the analysis of the cross section stiffness properties is described. The resulting beam finite element formulation...... is able to account for the effects of material anisotropy and inhomogeneity in the global response of the beam. Beam finite element models allow for a significant reduction in problem size and are therefore an efficient alternative in computationally intensive applications like optimization frameworks...... design of laminated composite beams. The devised framework is applied in the optimal design of laminated composite beams with different cross section geometries and subjected to different load cases. Design criteria such as beam stiffness, weight, magnitude of the natural frequencies of vibration...

  5. Progressive delamination in polymer matrix composite laminates: A new approach

    Science.gov (United States)

    Chamis, C. C.; Murthy, P. L. N.; Minnetyan, L.

    1992-01-01

    A new approach independent of stress intensity factors and fracture toughness parameters has been developed and is described for the computational simulation of progressive delamination in polymer matrix composite laminates. The damage stages are quantified based on physics via composite mechanics while the degradation of the laminate behavior is quantified via the finite element method. The approach accounts for all types of composite behavior, laminate configuration, load conditions, and delamination processes starting from damage initiation, to unstable propagation, and to laminate fracture. Results of laminate fracture in composite beams, panels, plates, and shells are presented to demonstrate the effectiveness and versatility of this new approach.

  6. Ceramic Veneers and Direct-Composite Cases of Amelogenesis Imperfecta Rehabilitation.

    Science.gov (United States)

    Shibata, S; Taguchi, Cmc; Gondo, R; Stolf, S C; Baratieri, L N

    2016-01-01

    The aim of this article is to present two case reports for the treatment of patients affected with amelogenesis imperfecta. One case was treated with composite resin and the other case with ceramic veneers. Esthetic and functional results were achieved using both treatments, and a review of advantages and disadvantages is presented.

  7. Optimization of Laminated Composite Structures

    DEFF Research Database (Denmark)

    Henrichsen, Søren Randrup

    of the contributions of the PhD project are included in the second part of the thesis. Paper A presents a framework for free material optimization where commercially available finite element analysis software is used as analysis tool. Robust buckling optimization of laminated composite structures by including...... allows for a higher degree of tailoring of the resulting material. To enable better utilization of the composite materials, optimum design procedures can be used to assist the engineer. This PhD thesis is focused on developing numerical methods for optimization of laminated composite structures...... nonlinear analysis of structures, buckling and post-buckling analysis of structures, and formulations for optimization of structures considering stiffness, buckling, and post-buckling criteria. Lastly, descriptions, main findings, and conclusions of the papers are presented. The papers forming the basis...

  8. Evaluation of the use potential of nine species of genus Eucalyptus for production of veneers and plywood panels

    Directory of Open Access Journals (Sweden)

    Setsuo Iwakiri

    2013-06-01

    Full Text Available The objective of thisstudywas to evaluate the use potential of nine species of Eucalyptus for production of veneer sheets and multilaminated plywood panels. Veneers were cut using a pilot laminating lathe to a nominal thickness of 2.0 mm. Analysis included finding values of overall yield and yield according to three quality classes for the nine relevant species. Plywood panels were manufactured in a laboratory, consisting of five 2.0 mm veneer sheets which were bonded together with phenol-formaldehyde resin at a weight of 360 g/m2 (double line. The panels were compressed using a specific pressure of 10 kgf/cm2, a temperature of 140ºC and a pressing time of 10 minutes. Results indicated that, with the exception of E. phaeotricha and E. pellita, all other Eucalyptus species had above 50% average veneer yield after lamination. Results of glue line shear testing and static bending parallel and perpendicular demonstrated that species Eucalyptus grandis, Eucalyptus saligna, Eucalyptus dunnii, Eucalyptus globulus, Eucalyptus viminalis, Eucalyptus robusta and Eucalyptus pellita have great potential within the parameters of this study for use in the production of veneer sheets and plywood panels intended for outdoor use.

  9. Effect of laminate edge conditions on the formation of microvoids in composite laminates

    Science.gov (United States)

    Anderson, J. P.; Altan, M. C.

    2015-05-01

    Manufacturing defects such as microvoids are common in thermoset composite components and are known to negatively affect their strength. The resin pressure developed in and the resin flow out from the laminates during cure have been reported to be the primary factors influencing the final void content of a composite component. In this work, the effect of laminate edge conditions during the cure process on the formation of microvoids was experimentally investigated. This was achieved by fabricating eight-ply laminates from TenCate® BT250/7781 prepreg in a hot-press at a constant cure pressure of 170 kPa while limiting the laminate perimeter available for resin flow by 0%, 25%, 50%, 75%, and 100%. The individual plies of these five laminates were conditioned at 99% relative humidity before curing to maximize the moisture present in the lay-up before fabrication. The presence of moisture in the lay-ups was expected to promote void formation and allow the effect of restricting flow at the edges of a laminate to be better identified. The restriction of resin outflow was found to cause the average characteristic void diameter to decrease by 17% and void content to rise by 33%. This phenomenon was identified to be a result of the outflow restriction increasing the number of voids trapped within the laminate and indicates that for laminates cured at low pressures resin outflow is the dominant mechanism for void reduction.

  10. Process-induced viscoelastic stress in composite laminates

    International Nuclear Information System (INIS)

    Stango, R.J.

    1985-01-01

    In recent years, considerable interest has developed in evaluating the stress response of composite laminates which is associated with cooling the material system from the cure temperature to room temperature. This research examines the fundamental nature of time-dependent residual-thermal stresses in composite laminates which are caused by the extreme temperature reduction encountered during the fabrication process. Viscoelastic stress in finite-width, symmetric composite laminates is examined on the basis of a formulation that employs an incremental hereditary integral approach in conjunction with a quasi-three dimensional finite element analysis. A consistent methodology is developed and employed for the characterization of lamina material properties. Special attention is given to the time-dependent stress response at ply-interface locations near the free-edge. In addition, the influence of cooling path on stress history is examined. Recently published material property data for graphite-epoxy lamina is employed in the analysis. Results of the investigation generally indicate that nominal differences between the thermoelastic and viscoelastic solutions are obtained. Slight changes of the final stress state are observed to result when different cooling paths are selected for the temperature history. The methodology employed is demonstrated to result in an accurate, efficient, and consistent approach for the viscoelastic analysis of advanced composite laminates

  11. Laminated lumber may be more profitable than sawn lumber

    Science.gov (United States)

    P. Koch

    1976-01-01

    By laminating 1/4-in. rotary-cut veneer into structural lumber, manufacturers can expand lumber output by at least 30% without increasing volume logged. The idea merits intensive study. Manufacturing plus raw material costs should total about $142/Mbf; sales price for desirable widths and lengths of the strong laminated product should approach or exceed $200/Mbf.

  12. Porcelain veneer post-bonding crack repair by resin infiltration.

    Science.gov (United States)

    Gresnigt, Marco; Magne, Michel; Magne, Pascal

    Ceramic laminate veneer restorations are indicated in several clinical situations. Indirect restorations are usually chosen if the less-invasive options - bleaching, resin infiltration, or composite resin restorations - are not possible, or when it is too difficult to achieve an esthetically pleasing result in the long term. Bonded indirect partial restorations are highly dependent on their adhesive interface, as these thin restorations have a relatively low cohesive strength. Therefore, preservation of sound enamel, conditioning of the restorations and of the substrate, and luting procedures are of paramount importance for a successful outcome. Even when utmost care is taken during every step of the procedure, failures such as fractures, chipping, or marginal discoloration and defects sometimes occur. Only very few of these cases of failure are presented or are a subject of interest. In this case presentation, a fracture repair is performed using an infiltration technique with a resin composite material.

  13. Laminated Ti-Al composites: Processing, structure and strength

    DEFF Research Database (Denmark)

    Du, Yan; Fan, Guohua; Yu, Tianbo

    2016-01-01

    Laminated Ti-Al composite sheets with different layer thickness ratios have been fabricated through hot pressing followed by multi-pass hot rolling at 500 °C.The laminated sheets show strong bonding with intermetallic interface layers of nanoscale thickness between the layers of Ti and Al....... The mechanical properties of the composites with different volume fractions of Al from 10% to 67% show a good combination of strength and ductility. A constraint strain in the hot-rolled laminated structure between the hard and soft phases introduces an elastic-plastic deformation stage, which becomes more...

  14. Effect of provisional cements on shear bond strength of porcelain laminate veneers.

    Science.gov (United States)

    Altintas, Subutay Han; Tak, Onjen; Secilmis, Asli; Usumez, Aslihan

    2011-08-01

    The purpose of this study was to evaluate the effect of three provisional cements and two cleaning techniques on the final bond strength of porcelain laminate veneers. The occlusal third of the crowns of forty molar teeth were sectioned and embedded in autopolymerizing acrylic resin. Dentin surfaces were polished and specimens were randomly divided into four groups (n=10). Provisional restorations were fabricated and two provisional restorations were cemented onto each tooth. Restorations were fixed with one of three different provisional cements: eugenol-free provisional cement (Cavex), calcium hydroxide (Dycal), and light-cured provisional cement (Tempond Clear). Provisional restorations were removed with either a dental explorer and air-water spray, or a cleaning bur (Opticlean). In the control group, provisional restorations were not used on the surfaces of specimens. IPS Empress 2 ceramic discs were luted with a dual-cured resin cement (Panavia F). Shear bond strength was measured using a universal testing machine. Data were statistically analyzed by ANOVA, Tukey's HSD and Dunnett tests. Surfaces were examined by scanning electronic microscopy. Significant differences were found between the control group and both the light-cured provisional cement groups and the eugenol-free provisional cement-cleaning bur group (Pprovisional cement showed the lowest bond strength values. Selection of the provisional cement is an important factor in the ultimate bond strength of the final restoration. Calcium hydroxide provisional cement and cleaning with a dental explorer are advisable.

  15. Experimental Assessment of Tensile Failure Characteristic for Advanced Composite Laminates

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Myoung Keon [Agency for Defense Development, Daejeon (Korea, Republic of); Lee, Jeong Won; Yoon, Dong Hyun; Kim, Jae Hoon [Chungnam Nat’l Univ., Daejeon (Korea, Republic of)

    2017-10-15

    In recent years, major airplane manufacturers have been using the laminate failure theory to estimate the strain of composite structures for airplanes. The laminate failure theory uses the failure strain of the laminate to analyze composite structures. This paper describes a procedure for the experimental assessment of laminate tensile failure characteristics. Regression analysis was used as the experimental assessment method. The regression analysis was performed with the response variable being the laminate failure strain and with the regressor variables being two-ply orientation (0° and ±45°) variables. The composite material in this study is a carbon/epoxy unidirectional (UD) tape that was cured as a pre-preg at 177°C(350°F). A total of 149 tension tests were conducted on specimens from 14 distinct laminates that were laid up at standard angle layers (0°, 45°, -45°, and 90°). The ASTM-D-3039 standard was used as the test method.

  16. Experimental Assessment of Tensile Failure Characteristic for Advanced Composite Laminates

    International Nuclear Information System (INIS)

    Lee, Myoung Keon; Lee, Jeong Won; Yoon, Dong Hyun; Kim, Jae Hoon

    2017-01-01

    In recent years, major airplane manufacturers have been using the laminate failure theory to estimate the strain of composite structures for airplanes. The laminate failure theory uses the failure strain of the laminate to analyze composite structures. This paper describes a procedure for the experimental assessment of laminate tensile failure characteristics. Regression analysis was used as the experimental assessment method. The regression analysis was performed with the response variable being the laminate failure strain and with the regressor variables being two-ply orientation (0° and ±45°) variables. The composite material in this study is a carbon/epoxy unidirectional (UD) tape that was cured as a pre-preg at 177°C(350°F). A total of 149 tension tests were conducted on specimens from 14 distinct laminates that were laid up at standard angle layers (0°, 45°, -45°, and 90°). The ASTM-D-3039 standard was used as the test method.

  17. Laminated exfoliated graphite composite-metal compositions for fuel cell flow field plate or bipolar plate applications

    Science.gov (United States)

    Zhamu, Aruna; Shi, Jinjun; Guo, Jiusheng; Jang, Bor Z

    2014-05-20

    An electrically conductive laminate composition for fuel cell flow field plate or bipolar plate applications. The laminate composition comprises at least a thin metal sheet having two opposed exterior surfaces and a first exfoliated graphite composite sheet bonded to the first of the two exterior surfaces of the metal sheet wherein the exfoliated graphite composite sheet comprises: (a) expanded or exfoliated graphite and (b) a binder or matrix material to bond the expanded graphite for forming a cohered sheet, wherein the binder or matrix material is between 3% and 60% by weight based on the total weight of the first exfoliated graphite composite sheet. Preferably, the first exfoliated graphite composite sheet further comprises particles of non-expandable graphite or carbon in the amount of between 3% and 60% by weight based on the total weight of the non-expandable particles and the expanded graphite. Further preferably, the laminate comprises a second exfoliated graphite composite sheet bonded to the second surface of the metal sheet to form a three-layer laminate. Surface flow channels and other desired geometric features can be built onto the exterior surfaces of the laminate to form a flow field plate or bipolar plate. The resulting laminate has an exceptionally high thickness-direction conductivity and excellent resistance to gas permeation.

  18. Deflection of Cross-Ply Composite Laminates Induced by Piezoelectric Actuators

    Directory of Open Access Journals (Sweden)

    Chi-Sheng Lin

    2010-01-01

    Full Text Available The coupling effects between the mechanical and electric properties of piezoelectric materials have drawn significant attention for their potential applications as sensors and actuators. In this investigation, two piezoelectric actuators are symmetrically surface bonded on a cross-ply composite laminate. Electric voltages with the same amplitude and opposite sign are applied to the two symmetric piezoelectric actuators, resulting in the bending effect on the laminated plate. The bending moment is derived by using the classical laminate theory and piezoelectricity. The analytical solution of the flexural displacement of the simply supported composite plate subjected to the bending moment is solved by using the plate theory. The analytical solution is compared with the finite element solution to show the validation of present approach. The effects of the size and location of the piezoelectric actuators on the response of the composite laminate are presented through a parametric study. A simple model incorporating the classical laminate theory and plate theory is presented to predict the deformed shape of the simply supported laminate plate.

  19. Preparation of Chitin-PLA laminated composite for implantable application

    Directory of Open Access Journals (Sweden)

    Romana Nasrin

    2017-12-01

    Full Text Available The present study explores the possibilities of using locally available inexpensive waste prawn shell derived chitin reinforced and bioabsorbable polylactic acid (PLA laminated composites to develop new materials with excellent mechanical and thermal properties for implantable application such as in bone or dental implant. Chitin at different concentration (1–20% of PLA reinforced PLA films (CTP were fabricated by solvent casting process and laminated chitin-PLA composites (LCTP were prepared by laminating PLA film (obtained by hot press method with CTP also by hot press method at 160 °C. The effect of variation of chitin concentration on the resulting laminated composite's behavior was investigated. The detailed physico-mechanical, surface morphology and thermal were assessed with different characterization technique such as FT-IR, XRD, SEM and TGA. The FTIR spectra showed the characteristic peaks for chitin and PLA in the composites. SEM images showed an excellent dispersion of chitin in the films and composites. Thermogravimetric analysis (TGA showed that the complete degradation of chitin, PLA film, 5% chitin reinforced PLA film (CTP2 and LCTP are 98%, 95%, 87% and 98% respectively at temperature of 500 °C. The tensile strength of the LCTP was found 25.09 MPa which is significantly higher than pure PLA film (18.55 MPa and CTP2 film (8.83 MPa. After lamination of pure PLA and CTP2 film, the composite (LCTP yielded 0.265–1.061% water absorption from 30 min to 24 h immerse in water that is much lower than PLA and CTP. The increased mechanical properties of the laminated films with the increase of chitin content indicated good dispersion of chitin into PLA and strong interfacial actions between the polymer and chitin. The improvement of mechanical properties and the results of antimicrobial and cytotoxicity of the composites also evaluated and revealed the composite would be a suitable candidate for implant application in biomedical

  20. Preparation of Chitin-PLA laminated composite for implantable application.

    Science.gov (United States)

    Nasrin, Romana; Biswas, Shanta; Rashid, Taslim Ur; Afrin, Sanjida; Jahan, Rumana Akhter; Haque, Papia; Rahman, Mohammed Mizanur

    2017-12-01

    The present study explores the possibilities of using locally available inexpensive waste prawn shell derived chitin reinforced and bioabsorbable polylactic acid (PLA) laminated composites to develop new materials with excellent mechanical and thermal properties for implantable application such as in bone or dental implant. Chitin at different concentration (1-20% of PLA) reinforced PLA films (CTP) were fabricated by solvent casting process and laminated chitin-PLA composites (LCTP) were prepared by laminating PLA film (obtained by hot press method) with CTP also by hot press method at 160 °C. The effect of variation of chitin concentration on the resulting laminated composite's behavior was investigated. The detailed physico-mechanical, surface morphology and thermal were assessed with different characterization technique such as FT-IR, XRD, SEM and TGA. The FTIR spectra showed the characteristic peaks for chitin and PLA in the composites. SEM images showed an excellent dispersion of chitin in the films and composites. Thermogravimetric analysis (TGA) showed that the complete degradation of chitin, PLA film, 5% chitin reinforced PLA film (CTP2) and LCTP are 98%, 95%, 87% and 98% respectively at temperature of 500 °C. The tensile strength of the LCTP was found 25.09 MPa which is significantly higher than pure PLA film (18.55 MPa) and CTP2 film (8.83 MPa). After lamination of pure PLA and CTP2 film, the composite (LCTP) yielded 0.265-1.061% water absorption from 30 min to 24 h immerse in water that is much lower than PLA and CTP. The increased mechanical properties of the laminated films with the increase of chitin content indicated good dispersion of chitin into PLA and strong interfacial actions between the polymer and chitin. The improvement of mechanical properties and the results of antimicrobial and cytotoxicity of the composites also evaluated and revealed the composite would be a suitable candidate for implant application in biomedical sector.

  1. Tunable characteristics of bending resonance frequency in magnetoelectric laminated composites

    Institute of Scientific and Technical Information of China (English)

    Chen Lei; Li Ping; Wen Yu-Mei; Zhu Yong

    2013-01-01

    As the magnetoelectric (ME) effect in piezoelectric/magnetostrictive laminated composites is mediated by mechanical deformation,the ME effect is significantly enhanced in the vicinity of resonance frequency.The bending resonance frequency (fr) of bilayered Terfenol-D/PZT (MP) laminated composites is studied,and our analysis predicts that (i) the bending resonance frequency of an MP laminated composite can be tuned by an applied dc magnetic bias (Hdc) due to the △E effect; (ii) the bending resonance frequency of the MP laminated composite can be controlled by incorporating FeCuNbSiB layers with different thicknesses.The experimental results show that with Hdc increasing from 0Oe (1 Oe=79.5775 A/m)to 700 Oe,the bending resonance frequency can be shifted in a range of 32.68 kHz ≤ fr ≤ 33.96 kHz.In addition,with the thickness of the FeCuNbSiB layer increasing from 0 μm to 90 μm,the bending resonance frequency of the MP laminated composite gradually increases from 33.66 kHz to 39.18 kHz.This study offers a method of adjusting the strength of dc magnetic bias or the thicknesses of the FeCuNbSiB layer to tune the bending resonance frequency for ME composite,which plays a guiding role in the ME composite design for real applications.

  2. Smart damping of laminated fuzzy fiber reinforced composite shells using 1–3 piezoelectric composites

    International Nuclear Information System (INIS)

    Kundalwal, S I; Suresh Kumar, R; Ray, M C

    2013-01-01

    This paper deals with the investigation of active constrained layer damping (ACLD) of smart laminated continuous fuzzy fiber reinforced composite (FFRC) shells. The distinct constructional feature of a novel FFRC is that the uniformly spaced short carbon nanotubes (CNTs) are radially grown on the circumferential surfaces of the continuous carbon fiber reinforcements. The constraining layer of the ACLD treatment is considered to be made of vertically/obliquely reinforced 1–3 piezoelectric composite materials. A finite element (FE) model is developed for the laminated FFRC shells integrated with the two patches of the ACLD treatment to investigate the damping characteristics of the laminated FFRC shells. The effect of variation of the orientation angle of the piezoelectric fibers on the damping characteristics of the laminated FFRC shells has been studied when the piezoelectric fibers are coplanar with either of the two mutually orthogonal vertical planes of the piezoelectric composite layer. It is revealed that radial growth of CNTs on the circumferential surfaces of the carbon fibers enhances the attenuation of the amplitude of vibrations and the natural frequencies of the laminated FFRC shells over those of laminated base composite shells without CNTs. (paper)

  3. Mechanical performance of laminated composites incorporated with nanofibrous membranes

    International Nuclear Information System (INIS)

    Liu, L.; Huang, Z.-M.; He, C.L.; Han, X.J.

    2006-01-01

    The effect of non-woven nanofibrous membranes as interlaminar interfaces on the mechanical performance of laminated composites was investigated experimentally. The nanofibrous membranes are porous, thin and lightweight, and exhibit toughness and strength to some extent. They give little increase in weight and thickness when incorporated into a laminate. More important, they can be used as a functional agent carrier for the laminate. The nanofiber membranes used in this paper were prepared by electrospinning of Nylon-6 (PA6), Epoxy 609 (EPO 1691-410) and thermoplastic polyurethane (TPU), with a thickness ranging from 20 to 150 μm. The non-woven fabrics were attached to one side of a glass/epoxy fabric lamina prior to lamination and each fabric was arranged in between two adjacent plies of the laminate. The nanofibrous membranes were characterized through scanning electron microscopy (SEM) and tensile testing, whereas the mechanical properties of the laminate were understood in terms of three-point bending and short-beam shear tests. Results have shown that the nanofibrous membranes in the ply interfaces with a proper thickness did not affect the mechanical performance of the composite laminates significantly

  4. Combined tension and bending testing of tapered composite laminates

    Science.gov (United States)

    O'Brien, T. Kevin; Murri, Gretchen B.; Hagemeier, Rick; Rogers, Charles

    1994-11-01

    A simple beam element used at Bell Helicopter was incorporated in the Computational Mechanics Testbed (COMET) finite element code at the Langley Research Center (LaRC) to analyze the responce of tappered laminates typical of flexbeams in composite rotor hubs. This beam element incorporated the influence of membrane loads on the flexural response of the tapered laminate configurations modeled and tested in a combined axial tension and bending (ATB) hydraulic load frame designed and built at LaRC. The moments generated from the finite element model were used in a tapered laminated plate theory analysis to estimate axial stresses on the surface of the tapered laminates due to combined bending and tension loads. Surfaces strains were calculated and compared to surface strains measured using strain gages mounted along the laminate length. The strain distributions correlated reasonably well with the analysis. The analysis was then used to examine the surface strain distribution in a non-linear tapered laminate where a similarly good correlation was obtained. Results indicate that simple finite element beam models may be used to identify tapered laminate configurations best suited for simulating the response of a composite flexbeam in a full scale rotor hub.

  5. Eddy-current effect on resonant magnetoelectric coupling in magnetostrictive-piezoelectric laminated composites

    Science.gov (United States)

    Liu, Guoxi; Zhang, Chunli; Chen, Weiqiu; Dong, Shuxiang

    2013-07-01

    An analytical model of resonant magnetoelectric (ME) coupling in magnetostrictive (MS)-piezoelectric (PE) laminated composites in consideration of eddy-current effect in MS layer using equivalent circuit method is presented. Numerical calculations show that: (1) the eddy-current has a strong effect on ME coupling in MS-PE laminated composites at resonant frequency; and (2) the resonant ME coupling is then significantly dependent on the sizes of ME laminated composites, which were neglected in most previous theoretical analyses. The achieved results provide a theoretical guidance for the practice engineering design, manufacture, and application of ME laminated composites and devices.

  6. Resin infusion of layered metal/composite hybrid and resulting metal/composite hybrid laminate

    Science.gov (United States)

    Cano, Roberto J. (Inventor); Grimsley, Brian W. (Inventor); Weiser, Erik S. (Inventor); Jensen, Brian J. (Inventor)

    2009-01-01

    A method of fabricating a metal/composite hybrid laminate is provided. One or more layered arrangements are stacked on a solid base to form a layered structure. Each layered arrangement is defined by a fibrous material and a perforated metal sheet. A resin in its liquid state is introduced along a portion of the layered structure while a differential pressure is applied across the laminate structure until the resin permeates the fibrous material of each layered arrangement and fills perforations in each perforated metal sheet. The resin is cured thereby yielding a metal/composite hybrid laminate.

  7. Aesthetic composite veneers for an adult patient with amelogenesis imperfecta: a case report.

    Science.gov (United States)

    Brignall, Ian; Mehta, Shamir B; Banerji, Subir; Millar, Brian J

    2011-11-01

    This case has been presented as part of the continual assessment requirement for the MSc in Aesthetic Dentistry, King's College Dental Institute. Amelogenesis imperfecta (AI) is a hereditary disorder of enamel formation, affecting both the permanent and deciduous dentitions. It can be classified into hypoplastic, hypomaturation and hypocalcified types and presents with different hereditary patterns. The aim of this article is to provide an overview of amelogenesis imperfecta, including a detailed case report for an aesthetically concerned adult patient presenting in general practice with a Witkop's Type IA defect managed with the placement of direct, layered resin composite veneers. Amelogenesis imperfecta patients are susceptible to the restorative cycle of replacement restorations like any other patient, but start with a distinct disadvantage.This case report demonstrates a minimally invasive, relatively simple and cost-effective option for the aesthetic correction of a case of hypoplastic amelogenesis imperfecta with layered composite veneers. Dent Update 2011; 38:594-603

  8. Stochastic-Strength-Based Damage Simulation of Ceramic Matrix Composite Laminates

    Science.gov (United States)

    Nemeth, Noel N.; Mital, Subodh K.; Murthy, Pappu L. N.; Bednarcyk, Brett A.; Pineda, Evan J.; Bhatt, Ramakrishna T.; Arnold, Steven M.

    2016-01-01

    The Finite Element Analysis-Micromechanics Analysis Code/Ceramics Analysis and Reliability Evaluation of Structures (FEAMAC/CARES) program was used to characterize and predict the progressive damage response of silicon-carbide-fiber-reinforced reaction-bonded silicon nitride matrix (SiC/RBSN) composite laminate tensile specimens. Studied were unidirectional laminates [0] (sub 8), [10] (sub 8), [45] (sub 8), and [90] (sub 8); cross-ply laminates [0 (sub 2) divided by 90 (sub 2),]s; angled-ply laminates [plus 45 (sub 2) divided by -45 (sub 2), ]s; doubled-edge-notched [0] (sub 8), laminates; and central-hole laminates. Results correlated well with the experimental data. This work was performed as a validation and benchmarking exercise of the FEAMAC/CARES program. FEAMAC/CARES simulates stochastic-based discrete-event progressive damage of ceramic matrix composite and polymer matrix composite material structures. It couples three software programs: (1) the Micromechanics Analysis Code with Generalized Method of Cells (MAC/GMC), (2) the Ceramics Analysis and Reliability Evaluation of Structures Life Prediction Program (CARES/Life), and (3) the Abaqus finite element analysis program. MAC/GMC contributes multiscale modeling capabilities and micromechanics relations to determine stresses and deformations at the microscale of the composite material repeating-unit-cell (RUC). CARES/Life contributes statistical multiaxial failure criteria that can be applied to the individual brittle-material constituents of the RUC, and Abaqus is used to model the overall composite structure. For each FEAMAC/CARES simulation trial, the stochastic nature of brittle material strength results in random, discrete damage events that incrementally progress until ultimate structural failure.

  9. Composite materials from forest biomass : a review of current practices, science, and technology

    Science.gov (United States)

    Roger M. Rowell

    2007-01-01

    Renewable and sustainable composite materials can be produced using forest biomass if we maintain healthy forests. Small diameter trees and other forest biomass can be processed in the forest into small solid wood pieces, sliced veneers, strands, flakes, chips, particles and fiber that can be used to make construction composite products such as glued-laminated lumber,...

  10. Damage Maps of Veneered Zirconia under Simulated Mastication

    Science.gov (United States)

    Kim, Jae-Won; Kim, Joo-Hyung; Janal, Malvin N.; Zhang, Yu

    2016-01-01

    Zirconia based restorations often fracture from chipping and/or delamination of the porcelain veneers. We hypothesize that veneer chipping/delamination is a result of the propagation of near-contact induced partial cone cracks on the occlusal surface under mastication. Masticatory loading involves the opposing tooth sliding along the cuspal inner incline surface with an applied biting force. To test this hypothesis, flat porcelain veneered zirconia plates were cemented to dental composites and cyclically loaded (contact–slide–liftoff) at an inclination angle as a simplified model of zirconia based restorations under occlusion. In the light of in-situ observation of damage evolution in a transparent glass/zirconia/polycarbonate trilayer, postmortem damage evaluation of porcelain/zirconia/composite trilayers using a sectioning technique revealed that deep penetrating occlusal surface partial cone fracture is the predominant fracture mode of porcelain veneers. Clinical relevance is discussed. PMID:19029080

  11. NiCoCrAl/YSZ laminate composites fabricated by EB-PVD

    International Nuclear Information System (INIS)

    Shi Guodong; Wang Zhi; Liang Jun; Wu Zhanjun

    2011-01-01

    Highlights: → The metal-ceramic laminate composites were fabricated by EB-PVD. → Both metal and ceramic layers consisted of straight columns with banded structures. → Columnar grain size was limited by the periodic layer interfaces in the laminates. → Effect of columns on fracture property was decreased by limiting layer thickness. → Laminates showed greater specific strength than monolithic metal foil. - Abstract: Two NiCoCrAl/YSZ laminate composites (A and B) with different metal-layer thickness (∼35 μm and 14 μm, respectively) were fabricated by electron beam physical vapor deposition (EB-PVD). Their microstructure was examined and their mechanical properties were compared with the 289 μm thick NiCoCrAl monolithic foil produced by EB-PVD. Both the YSZ and NiCoCrAl layers of the laminate composites had columnar grain structure. But the periodic layer interfaces limited the columnar grain size. Some pores between the columns were also observed. It was found that the strength of the laminate A was equal approximately to that of the NiCoCrAl monolithic foil, and that laminate B had the greater strength. Moreover, the density of the foils decreased with the increasing thickness ratio of YSZ/NiCoCrAl layers and the increasing the layer number. Thus, comparing with the NiCoCrAl monolithic foil, the NiCoCrAl/YSZ laminate composites not only had the equal or greater strength, but also had the much greater specific strength.

  12. Control of formaldehyde and TVOC emission from wood-based flooring composites at various manufacturing processes by surface finishing.

    Science.gov (United States)

    Kim, Sumin

    2010-04-15

    This paper assesses the reproducibility of testing formaldehyde and TVOC emission behavior from wood flooring composites bonded by urea-formaldehyde resin at various manufacturing steps for surface finishing materials. The surface adhesion step of laminate flooring for this research was divided into two steps; HDF only and HDF with LPMs. In the case of engineered flooring, the manufacturing steps were divided into three steps; plywood only, fancy veneer bonded on plywood and UV coated on fancy veneer with plywood. Formaldehyde and VOCs emission decreased at the process of final surface finishing materials; LPMs were applied on the surface of HDF for laminate flooring. Although emissions increased when fancy veneer was bonded onto plywood in the case of engineered flooring, emission was dramatically reduced up to similar level with plywood only when final surface finishing; UV-curable coating was applied on fancy veneer. This study suggests that formaldehyde and VOCs emission from floorings can be controlled at manufacturing steps for surface finishing. 2009 Elsevier B.V. All rights reserved.

  13. On Poisson's ratio for metal matrix composite laminates. [aluminum boron composites

    Science.gov (United States)

    Herakovich, C. T.; Shuart, M. J.

    1978-01-01

    The definition of Poisson's ratio for nonlinear behavior of metal matrix composite laminates is discussed and experimental results for tensile and compressive loading of five different boron-aluminum laminates are presented. It is shown that there may be considerable difference in the value of Poisson's ratio as defined by a total strain or an incremental strain definition. It is argued that the incremental definition is more appropriate for nonlinear material behavior. Results from a (0) laminate indicate that the incremental definition provides a precursor to failure which is not evident if the total strain definition is used.

  14. BILAM: a composite laminate failure-analysis code using bilinear stress-strain approximations

    Energy Technology Data Exchange (ETDEWEB)

    McLaughlin, P.V. Jr.; Dasgupta, A.; Chun, Y.W.

    1980-10-01

    The BILAM code which uses constant strain laminate analysis to generate in-plane load/deformation or stress/strain history of composite laminates to the point of laminate failure is described. The program uses bilinear stress-strain curves to model layer stress-strain behavior. Composite laminates are used for flywheels. The use of this computer code will help to develop data on the behavior of fiber composite materials which can be used by flywheel designers. In this program the stress-strain curves are modelled by assuming linear response in axial tension while using bilinear approximations (2 linear segments) for stress-strain response to axial compressive, transverse tensile, transverse compressive and axial shear loadings. It should be noted that the program attempts to empirically simulate the effects of the phenomena which cause nonlinear stress-strain behavior, instead of mathematically modelling the micromechanics involved. This code, therefore, performs a bilinear laminate analysis, and, in conjunction with several user-defined failure interaction criteria, is designed to provide sequential information on all layer failures up to and including the first fiber failure. The modus operandi is described. Code BILAM can be used to: predict the load-deformation/stress-strain behavior of a composite laminate subjected to a given combination of in-plane loads, and make analytical predictions of laminate strength.

  15. Bayesian inference model for fatigue life of laminated composites

    DEFF Research Database (Denmark)

    Dimitrov, Nikolay Krasimirov; Kiureghian, Armen Der; Berggreen, Christian

    2016-01-01

    A probabilistic model for estimating the fatigue life of laminated composite plates is developed. The model is based on lamina-level input data, making it possible to predict fatigue properties for a wide range of laminate configurations. Model parameters are estimated by Bayesian inference. The ...

  16. Control of free-edge interlaminar stresses in composite laminates using piezoelectric actuators

    International Nuclear Information System (INIS)

    Huang, Bin; Soo Kim, Heung

    2014-01-01

    The control of free-edge interlaminar stresses in laminated composite structures using a stress function-based approach is proposed. The assumed stress fields satisfy pointwise traction and free boundary conditions at surfaces. Governing equations are derived using the principle of complementary virtual work. A general eigenvalue solution procedure was adopted to obtain accurate stress states of the laminated composite structure. The results obtained from the proposed method were compared with those obtained by three-dimensional finite element analyses. It was found that interlaminar stresses generated by mechanical loadings could be significantly reduced by applying proper electric fields to piezoelectric actuators, which were surface bonded or embedded in composite laminates. Locations of piezoelectric actuators also influenced the distributions of interlaminar stresses. The results provided that piezoelectric actuators have potential in the application to actively control interlaminar stresses in composite laminates. (paper)

  17. Optimum design of laminated composite under axial compressive load

    Indian Academy of Sciences (India)

    In the present study optimal design of composite laminates, with and without rectangular cut-out, is carried out for maximizing the buckling load. Optimization study is carried out for obtaining the maximum buckling load with design variables as ply thickness, cut-out size and orientation of cut-out with respect to laminate.

  18. Damage and Failure of Non-Conventional Composite Laminates

    NARCIS (Netherlands)

    Lopes, C.S.

    2009-01-01

    For a long time, the application of composite materials was restricted to military aircraft and secondary structures of commercial aircraft. Furthermore, the design possibilities offered by composite laminates were narrowed to quasi-isotropic configurations due to their closer behaviour with

  19. Minimum weight design of composite laminates for multiple loads

    International Nuclear Information System (INIS)

    Krikanov, A.A.; Soni, S.R.

    1995-01-01

    A new design method of constructing optimum weight composite laminates for multiple loads is proposed in this paper. A netting analysis approach is used to develop an optimization procedure. Three ply orientations permit development of optimum laminate design without using stress-strain relations. It is proved that stresses in minimum weight laminate reach allowable values in each ply with given load. The optimum ply thickness is defined at maximum value among tensile and compressive loads. Two examples are given to obtain optimum ply orientations, thicknesses and materials. For comparison purposes, calculations of stresses are done in orthotropic material using classical lamination theory. Based upon these calculations, matrix degrades at 30 to 50% of ultimate load. There is no fiber failure and therefore laminates withstand all applied loads in both examples

  20. Fatigue Performance of Composite Laminates After Low-velocity Impact

    Directory of Open Access Journals (Sweden)

    LIANG Xiao-lin

    2016-12-01

    Full Text Available Compression-compression fatigue tests were carried out on T300/5405 composite laminates after low-velocity impact, compression performance of the laminates with different impact damages was studied together with its fatigue life and damage propagation under different stress levels, then the effects of impact energy, stress level and damage propagation on fatigue life of laminates were discussed. The results indicate that impact damage can greatly reduce the residual strength of laminates; under low fatigue load levels, the higher impact energy is, the shorter the fatigue life of laminates with impact damage will be; damage propagation undergoes two stages during the fatigue test, namely the steady propagation and the rapid propagation, accounting for 80% and 20% of the overall fatigue life, respectively; damage propagation rate decreases with the reduction of stress level.

  1. Ballistic Impact Response of Woven Hybrid Coir/Kevlar Laminated Composites

    Directory of Open Access Journals (Sweden)

    Azrin Hani A.R

    2016-01-01

    Full Text Available The effects of different laminated hybrid composites stacking configuration subjected to ballistic impact were investigated. The hybrid composites consist of woven coir (C and woven Kevlar (K layers laminated together. The samples of woven coir were prepared using handloom device. The composites were produced by stacking the laminated woven coir and Kevlar alternately with the presence of the binder. The samples were tested under ballistic impact with different stacking configuration. The results obtained had successfully achieved the National Institute of Justice (NIJ standard level IIA with energy absorption of 435.6 kJ and 412.2 kJ under the projectile speed of between 330 m/s and 321 m/s respectively. Samples that having Kevlar layer at the front face and woven coir layer as back face achieved partial penetration during projectile impact. This orientation is proven to have good impact energy absorption and able to stop projectile at the second panel of the composites.

  2. Natural fabric sandwich laminate composites: development and ...

    Indian Academy of Sciences (India)

    3Department of Production Technology, MIT Campus, Anna University, Chennai 600044, India. MS received ... In this work, eco-friendly natural fabric sandwich laminate (NFSL) composites are formulated using ... and eco-friendly quality [22].

  3. Estimation of physical properties of laminated composites via the method of inverse vibration problem

    Energy Technology Data Exchange (ETDEWEB)

    Balci, Murat [Dept. of Mechanical Engineering, Bayburt University, Bayburt (Turkmenistan); Gundogdu, Omer [Dept. of Mechanical Engineering, Ataturk University, Erzurum (Turkmenistan)

    2017-01-15

    In this study, estimation of some physical properties of a laminated composite plate was conducted via the inverse vibration problem. Laminated composite plate was modelled and simulated to obtain vibration responses for different length-to-thickness ratio in ANSYS. Furthermore, a numerical finite element model was developed for the laminated composite utilizing the Kirchhoff plate theory and programmed in MATLAB for simulations. Optimizing the difference between these two vibration responses, inverse vibration problem was solved to obtain some of the physical properties of the laminated composite using genetic algorithms. The estimated parameters are compared with the theoretical results, and a very good correspondence was observed.

  4. Estimation of physical properties of laminated composites via the method of inverse vibration problem

    International Nuclear Information System (INIS)

    Balci, Murat; Gundogdu, Omer

    2017-01-01

    In this study, estimation of some physical properties of a laminated composite plate was conducted via the inverse vibration problem. Laminated composite plate was modelled and simulated to obtain vibration responses for different length-to-thickness ratio in ANSYS. Furthermore, a numerical finite element model was developed for the laminated composite utilizing the Kirchhoff plate theory and programmed in MATLAB for simulations. Optimizing the difference between these two vibration responses, inverse vibration problem was solved to obtain some of the physical properties of the laminated composite using genetic algorithms. The estimated parameters are compared with the theoretical results, and a very good correspondence was observed

  5. 3D Guided Wave Motion Analysis on Laminated Composites

    Science.gov (United States)

    Tian, Zhenhua; Leckey, Cara; Yu, Lingyu

    2013-01-01

    Ultrasonic guided waves have proved useful for structural health monitoring (SHM) and nondestructive evaluation (NDE) due to their ability to propagate long distances with less energy loss compared to bulk waves and due to their sensitivity to small defects in the structure. Analysis of actively transmitted ultrasonic signals has long been used to detect and assess damage. However, there remain many challenging tasks for guided wave based SHM due to the complexity involved with propagating guided waves, especially in the case of composite materials. The multimodal nature of the ultrasonic guided waves complicates the related damage analysis. This paper presents results from parallel 3D elastodynamic finite integration technique (EFIT) simulations used to acquire 3D wave motion in the subject laminated carbon fiber reinforced polymer composites. The acquired 3D wave motion is then analyzed by frequency-wavenumber analysis to study the wave propagation and interaction in the composite laminate. The frequency-wavenumber analysis enables the study of individual modes and visualization of mode conversion. Delamination damage has been incorporated into the EFIT model to generate "damaged" data. The potential for damage detection in laminated composites is discussed in the end.

  6. Esthetic, occlusal, and periodontal rehabilitation of anterior teeth with minimum thickness porcelain laminate veneers.

    Science.gov (United States)

    da Cunha, Leonardo Fernandes; Pedroche, Lorena Oliveira; Gonzaga, Carla Castiglia; Furuse, Adilson Yoshio

    2014-12-01

    Ceramic veneers of minimum thickness provide satisfactory esthetic outcomes while preserving the dental structure. Dental ceramics can both improve the esthetic appearance and reestablish the strength and function of teeth. In worn anterior teeth, functional surfaces, for example, anterior and lateral guidance, can be restored effectively. The characteristics of dental ceramics, such as color stability and mechanical and optical properties, make this material a good choice for indirect restorations, especially when optimum function and esthetics are required. This clinical report presents an occlusal, periodontal, and restorative solution with minimum thickness glass ceramic veneers for worn anterior teeth with multiple diastemas. Copyright © 2014 Editorial Council for the Journal of Prosthetic Dentistry. Published by Elsevier Inc. All rights reserved.

  7. Irradiation effects in tungsten-copper laminate composite

    Energy Technology Data Exchange (ETDEWEB)

    Garrison, L.M., E-mail: garrisonlm@ornl.gov [Oak Ridge National Laboratory, Oak Ridge, TN 37831 (United States); Katoh, Y. [Oak Ridge National Laboratory, Oak Ridge, TN 37831 (United States); Snead, L.L. [Oak Ridge National Laboratory, Oak Ridge, TN 37831 (United States); Massachusetts Institute of Technology, Cambridge, MA 02139 (United States); Byun, T.S. [Oak Ridge National Laboratory, Oak Ridge, TN 37831 (United States); Pacific Northwest National Laboratory, Richland, WA 99352 (United States); Reiser, J.; Rieth, M. [Karlsruhe Institute of Technology, Karlsruhe (Germany)

    2016-12-01

    Tungsten-copper laminate composite has shown promise as a structural plasma-facing component as compared to tungsten rod or plate. The present study evaluated the tungsten-copper composite after irradiation in the High Flux Isotope Reactor (HFIR) at temperatures of 410–780 °C and fast neutron fluences of 0.02–9.0 × 10{sup 25} n/m{sup 2}, E > 0.1 MeV, 0.0039–1.76 displacements per atom (dpa) in tungsten. Tensile tests were performed on the composites, and the fracture surfaces were analyzed with scanning electron microscopy. Before irradiation, the tungsten layers had brittle cleavage failure, but the overall composite had 15.5% elongation at 22 °C. After only 0.0039 dpa this was reduced to 7.7% elongation, and no ductility was observed after 0.2 dpa at all irradiation temperatures when tensile tested at 22 °C. For elevated temperature tensile tests after irradiation, the composite only had ductile failure at temperatures where the tungsten was delaminating or ductile. - Highlights: • Fusion reactors need a tough, ductile tungsten plasma-facing material. • The unirradiated tungsten-copper laminate is more ductile than tungsten alone. • After neutron irradiation, the composite has significantly less ductility. • The tungsten behavior appears to dominate the overall composite behavior.

  8. Effect of Electrospun Nanofibers on the Short Beam Strength of Laminated Fiberglass Composite

    Science.gov (United States)

    Shinde, Dattaji K.

    High specific modulus and strength are the most desirable properties for the material used in structural applications. Composite materials exhibit these properties and over the last decade, their usage has increased significantly, particularly in automotive, defense, and aerospace applications. The major cause of failures in composite laminates is due to delaminations. Delamination in composite laminates can occur due to fatigue, low velocity impact and other loadings modes. Conventional methods like "through-the-thickness stitching" or "Z-Pinning" have limitations for improving flexural and interlaminar properties in woven composites due to the fact that while improving interlaminar properties, the presence of stitches or Z pins affects in-plane properties. This study investigates the flexural behavior of fiberglass composites interleaved with non-woven Tetra Ethyl Orthosilicate (TEOS) electrsopsun nanofibers (ENFs). TEOS ENFs were manufactured using an electrospinning technique and then sintered. Nanoengineered beams were fabricated by interleaving TEOS ENFs between the laminated fiberglass composites to improve the flexural properties. TEOS ENFs, resin film, and failed fiberglass laminated composites with and without nanofibers were characterized using SEM Imaging and ASTM standard testing methods. A hybrid composite was made by interleaving a non-woven sheet of TEOS ENFs between the fiberglass laminates with additional epoxy resin film and fabricated using the out of autoclave vacuum bagging method. Four commonly used stacking sequences of fiberglass laminates with and without nanofibers were used to study the progressive failure and deformation mechanics under flexural loadings. The experimental study has shown significant improvements in short beam strength and strain energy absorption in the nanoengineered laminated fiberglass composites before complete failure. The modes were investigated by performing detailed fractographic examination of failed specimens

  9. Evaluation of shear-compressive strength properties for laminated GFRP composites in electromagnet system

    Science.gov (United States)

    Song, Jun Hee; Kim, Hak Kun; Kim, Sam Yeon

    2014-07-01

    Laminated fiber-reinforced composites can be applied to an insulating structure of a nuclear fusion device. It is necessary to investigate the interlaminar fracture characteristics of the laminated composites for the assurance of design and structural integrity. The three methods used to prepare the glass fiber reinforced plastic composites tested in this study were vacuum pressure impregnation, high pressure laminate (HPL), and prepreg laminate. We discuss the design criteria for safe application of composites and the shear-compressive test methods for evaluating mechanical properties of the material. Shear-compressive tests could be performed successfully using series-type test jigs that were inclined 0°, 30°, 45°, 60°, and 75° to the normal axis. Shear strength depends strongly on the applied compressive stress. The design range of allowable shear stress was extended by use of the appropriate composite fabrication method. HPL had the largest design range, and the allowable interlaminar shear stress was 0.254 times the compressive stress.

  10. Using lamb waves tomonitor moisture absorption thermally fatigues composite laminates

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Jae Sun; Cho, Youn Ho [School of Mechanical Engineering, Pusan National University, Busan (Korea, Republic of)

    2016-06-15

    Nondestructive evaluation for material health monitoring is important in aerospace industries. Composite laminates are exposed to heat cyclic loading and humid environment depending on flight conditions. Cyclic heat loading and moisture absorption may lead to material degradation such as matrix breaking, debonding, and delamination. In this paper, the moisture absorption ratio was investigated by measuring the Lamb wave velocity. The composite laminates were manufactured and subjected to different thermal aging cycles and moisture absorption. For various conditions of these cycles, not only changes in weight and also ultrasonic wave velocity were measured, and the Lamb wave velocity at various levels of moisture on a carbon-epoxy plate was investigated. Results from the experiment show a linear correlation between moisture absorption ratio and Lamb wave velocity at different thermal fatigue stages. The presented method can be applied as an alternative solution in the online monitoring of composite laminate moisture levels in commercial flights.

  11. Characterization and Formability of Titanium/Aluminum Laminate Composites Fabricated by Hot Pressing

    Science.gov (United States)

    Qin, Liang; Wang, Hui; Cui, Shengqiang; Wu, Qian; Fan, Minyu; Yang, Zonghui; Tao, Jie

    2017-07-01

    The Ti/Al laminate composites were prepared by hot pressing to investigate the forming performance due to the corresponding potential applications in both the aerospace and auto industry. The bonding interface morphology and element distributions were characterized by SEM and EDS. The phase constituent was detected by XRD. It was observed that these composites presented good bonding interfaces between Ti and Al layers, and no low-sized voids and intermetallic compounds formed at the interface. In addition, the formability of these laminate composites was studied by the uniaxial tension tests, the limit drawing ratio (LDR) and the forming limit curve (FLC) experiments, respectively. The results indicated that the flow stress increased along with the strain rate increment. A constitutive equation was developed for deformation behavioral description of these laminate composites. The LDR value was 1.8, and the most susceptible region to present cracks was located at the punch profile radius. The forming limit curve of the laminate composites was located between the curves of titanium and aluminum and intersected with the major strain line at approximately 0.31. The macroscopic cracks of the FLC sample demonstrated a saw-toothed crack feature.

  12. Boron nitride nanoparticle enhanced prepregs: A novel route for manufacturing aerospace structural composite laminate

    Energy Technology Data Exchange (ETDEWEB)

    Kelkar, Ajit D., E-mail: kelkar@ncat.edu [Joint School of Nanoscience and Nanoengineering, North Carolina Agricultural and Technical State University, Greensboro, NC, 27401 (United States); Tian, Qiong [Joint School of Nanoscience and Nanoengineering, North Carolina Agricultural and Technical State University, Greensboro, NC, 27401 (United States); School of Science, Xi' an Jiaotong University, Xi' an, 710049 (China); Yu, Demei [School of Science, Xi' an Jiaotong University, Xi' an, 710049 (China); Zhang, Lifeng, E-mail: lzhang@ncat.edu [Joint School of Nanoscience and Nanoengineering, North Carolina Agricultural and Technical State University, Greensboro, NC, 27401 (United States)

    2016-06-15

    Boron nitride nanoparticles (BNNPs) were surface functionalized and subsequently applied to surface of fiberglass prepregs to fabricate hybrid BNNPs/fiberglass/epoxy composite laminate. A systematic and comparative study on BNNPs functionalization routes and their effects on morphology, mechanical property and thermal conductivity of final BNNPs enhanced composite laminates was performed. The functionalized BNNPs were characterized by Fourier-transform infrared spectroscopy (FT-IR), thermogravimetric analysis (TGA), and scanning electron microscopy (SEM). The composite laminates with surface functionalized BNNPs demonstrated improvement in tensile and flexural strength and modulus as well as in thermal conductivity compared to the composite laminate with pristine BNNPs while physically functionalized BNNPs outperformed chemically functionalized BNNPs in all cases. SEM images indicated better compatibility and dispersion of BNNPs in epoxy matrix following either of functionalization route. BNNPs bear great radiation-shielding capability. This investigation revealed a novel and industrially feasible route to incorporate BNNPs in aerospace structural materials. - Highlights: • BNNPs were surface functionalized and applied onto fiberglass prepreg. • The BNNPs enhanced prepreg was employed to make hybrid BNNPs/fiberglass/epoxy composite laminate. • The hybrid laminate presented significant improvement in mechanical strength and thermal conductivity. • This investigation revealed a novel and industrially feasible route to incorporate BNNPs in aerospace structural materials.

  13. Boron nitride nanoparticle enhanced prepregs: A novel route for manufacturing aerospace structural composite laminate

    International Nuclear Information System (INIS)

    Kelkar, Ajit D.; Tian, Qiong; Yu, Demei; Zhang, Lifeng

    2016-01-01

    Boron nitride nanoparticles (BNNPs) were surface functionalized and subsequently applied to surface of fiberglass prepregs to fabricate hybrid BNNPs/fiberglass/epoxy composite laminate. A systematic and comparative study on BNNPs functionalization routes and their effects on morphology, mechanical property and thermal conductivity of final BNNPs enhanced composite laminates was performed. The functionalized BNNPs were characterized by Fourier-transform infrared spectroscopy (FT-IR), thermogravimetric analysis (TGA), and scanning electron microscopy (SEM). The composite laminates with surface functionalized BNNPs demonstrated improvement in tensile and flexural strength and modulus as well as in thermal conductivity compared to the composite laminate with pristine BNNPs while physically functionalized BNNPs outperformed chemically functionalized BNNPs in all cases. SEM images indicated better compatibility and dispersion of BNNPs in epoxy matrix following either of functionalization route. BNNPs bear great radiation-shielding capability. This investigation revealed a novel and industrially feasible route to incorporate BNNPs in aerospace structural materials. - Highlights: • BNNPs were surface functionalized and applied onto fiberglass prepreg. • The BNNPs enhanced prepreg was employed to make hybrid BNNPs/fiberglass/epoxy composite laminate. • The hybrid laminate presented significant improvement in mechanical strength and thermal conductivity. • This investigation revealed a novel and industrially feasible route to incorporate BNNPs in aerospace structural materials.

  14. Recent developments of discrete material optimization of laminated composite structures

    DEFF Research Database (Denmark)

    Lund, Erik; Sørensen, Rene

    2015-01-01

    This work will give a quick summary of recent developments of the Discrete Material Optimization approach for structural optimization of laminated composite structures. This approach can be seen as a multi-material topology optimization approach for selecting the best ply material and number...... of plies in a laminated composite structure. The conceptual combinatorial design problem is relaxed to a continuous problem such that well-established gradient based optimization techniques can be applied, and the optimization problem is solved on basis of interpolation schemes with penalization...

  15. Numerical Material Model for Composite Laminates in High-Velocity Impact Simulation

    Directory of Open Access Journals (Sweden)

    Tao Liu

    Full Text Available Abstract A numerical material model for composite laminate, was developed and integrated into the nonlinear dynamic explicit finite element programs as a material user subroutine. This model coupling nonlinear state of equation (EOS, was a macro-mechanics model, which was used to simulate the major mechanical behaviors of composite laminate under high-velocity impact conditions. The basic theoretical framework of the developed material model was introduced. An inverse flyer plate simulation was conducted, which demonstrated the advantage of the developed model in characterizing the nonlinear shock response. The developed model and its implementation were validated through a classic ballistic impact issue, i.e. projectile impacting on Kevlar29/Phenolic laminate. The failure modes and ballistic limit velocity were analyzed, and a good agreement was achieved when comparing with the analytical and experimental results. The computational capacity of this model, for Kevlar/Epoxy laminates with different architectures, i.e. plain-woven and cross-plied laminates, was further evaluated and the residual velocity curves and damage cone were accurately predicted.

  16. Laser displacement sensor to monitor the layup process of composite laminate production

    Science.gov (United States)

    Miesen, Nick; Groves, Roger M.; Sinke, Jos; Benedictus, Rinze

    2013-04-01

    Several types of flaw can occur during the layup process of prepreg composite laminates. Quality control after the production process checks the end product by testing the specimens for flaws which are included during the layup process or curing process, however by then these flaws are already irreversibly embedded in the laminate. This paper demonstrates the use of a laser displacement sensor technique applied during the layup process of prepreg laminates for in-situ flaw detection, for typical flaws that can occur during the composite production process. An incorrect number of layers and fibre wrinkling are dominant flaws during the process of layup. These and other dominant flaws have been modeled to determine the requirements for an in-situ monitoring during the layup process of prepreg laminates.

  17. Modeling and Chaotic Dynamics of the Laminated Composite Piezoelectric Rectangular Plate

    Directory of Open Access Journals (Sweden)

    Minghui Yao

    2014-01-01

    Full Text Available This paper investigates the multipulse heteroclinic bifurcations and chaotic dynamics of a laminated composite piezoelectric rectangular plate by using an extended Melnikov method in the resonant case. According to the von Karman type equations, Reddy’s third-order shear deformation plate theory, and Hamilton’s principle, the equations of motion are derived for the laminated composite piezoelectric rectangular plate with combined parametric excitations and transverse excitation. The method of multiple scales and Galerkin’s approach are applied to the partial differential governing equation. Then, the four-dimensional averaged equation is obtained for the case of 1 : 3 internal resonance and primary parametric resonance. The extended Melnikov method is used to study the Shilnikov type multipulse heteroclinic bifurcations and chaotic dynamics of the laminated composite piezoelectric rectangular plate. The necessary conditions of the existence for the Shilnikov type multipulse chaotic dynamics are analytically obtained. From the investigation, the geometric structure of the multipulse orbits is described in the four-dimensional phase space. Numerical simulations show that the Shilnikov type multipulse chaotic motions can occur. To sum up, both theoretical and numerical studies suggest that chaos for the Smale horseshoe sense in motion exists for the laminated composite piezoelectric rectangular plate.

  18. Probabilistic Modelling of Fatigue Life of Composite Laminates Using Bayesian Inference

    DEFF Research Database (Denmark)

    Dimitrov, Nikolay Krasimirov; Kiureghian, Armen Der

    2014-01-01

    A probabilistic model for estimating the fatigue life of laminated composite plates subjected to constant-amplitude or variable-amplitude loading is developed. The model is based on lamina-level input data, making it possible to predict fatigue properties for a wide range of laminate configuratio...

  19. Structural Analysis of Composite Laminates using Analytical and Numerical Techniques

    Directory of Open Access Journals (Sweden)

    Sanghi Divya

    2016-01-01

    Full Text Available A laminated composite material consists of different layers of matrix and fibres. Its properties can vary a lot with each layer’s or ply’s orientation, material property and the number of layers itself. The present paper focuses on a novel approach of incorporating an analytical method to arrive at a preliminary ply layup order of a composite laminate, which acts as a feeder data for the further detailed analysis done on FEA tools. The equations used in our MATLAB are based on analytical study code and supply results that are remarkably close to the final optimized layup found through extensive FEA analysis with a high probabilistic degree. This reduces significant computing time and saves considerable FEA processing to obtain efficient results quickly. The result output by our method also provides the user with the conditions that predicts the successive failure sequence of the composite plies, a result option which is not even available in popular FEM tools. The predicted results are further verified by testing the laminates in the laboratory and the results are found in good agreement.

  20. Discrete Material Buckling Optimization of Laminated Composite Structures considering "Worst" Shape Imperfections

    DEFF Research Database (Denmark)

    Henrichsen, Søren Randrup; Lindgaard, Esben; Lund, Erik

    2015-01-01

    Robust design of laminated composite structures is considered in this work. Because laminated composite structures are often thin walled, buckling failure can occur prior to material failure, making it desirable to maximize the buckling load. However, as a structure always contains imperfections...... and “worst” shape imperfection optimizations to design robust composite structures. The approach is demonstrated on an U-profile where the imperfection sensitivity is monitored, and based on the example it can be concluded that robust designs can be obtained....

  1. Laser irradiation-induced laminated graphene/MoS2 composites with synergistically improved tribological properties

    Science.gov (United States)

    Luo, Ting; Chen, Xinchun; Li, Peisheng; Wang, Ping; Li, Cuncheng; Cao, Bingqiang; Luo, Jianbin; Yang, Shikuan

    2018-06-01

    Engineering lubricant additives that have extraordinary friction reduction and anti-wear performance is critical to almost any modern mechanical machines. Here, we demonstrate the fabrication of laminated lubricant additives that can combine the advantages of zero-dimensional nanospheres and two-dimensional nanosheets. A simple in situ laser irradiation method is developed to prepare the laminated composite structure composed of ideally ultrasmooth MoS2 sub-microspheres embedded within multiple layers of graphene. These ultrasmooth MoS2 spheres within the laminated structure can change sliding friction into rolling friction under strong shear force created by moving contact surfaces to significantly reduce the friction. Meantime, the graphene layers can behave as ‘protection pads’ to efficiently avoid the formation of scars on the metal-to-metal contact surfaces. Overall, the laminated composites as lubricant additives synergistically improve the friction reduction and anti-wear properties. Additionally, due to the unique loosely packed laminated structure, the composites can stably disperse in the lubricant for more than 15 d and work under high temperatures without being oxidized. Such constructed laminated composites with outstanding tribological properties by an in situ laser irradiation method supply a new concept in designing lubricant additives that can combine the advantages of 0D and 2D structures.

  2. Embedding piezoresistive pressure sensors to obtain online pressure profiles inside fiber composite laminates.

    Science.gov (United States)

    Moghaddam, Maryam Kahali; Breede, Arne; Brauner, Christian; Lang, Walter

    2015-03-27

    The production of large and complex parts using fiber composite materials is costly due to the frequent formation of voids, porosity and waste products. By embedding different types of sensors and monitoring the process in real time, the amount of wastage can be significantly reduced. This work focuses on developing a knowledge-based method to improve and ensure complete impregnation of the fibers before initiation of the resin cure. Piezoresistive and capacitive pressure sensors were embedded in fiber composite laminates to measure the real-time the pressure values inside the laminate. A change of pressure indicates resin infusion. The sensors were placed in the laminate and the resin was infused by vacuum. The embedded piezoresistive pressure sensors were able to track the vacuum pressure in the fiber composite laminate setup, as well as the arrival of the resin at the sensor. The pressure increase due to closing the resin inlet was also measured. In contrast, the capacitive type of sensor was found to be inappropriate for measuring these quantities. The following study demonstrates real-time monitoring of pressure changes inside the fiber composite laminate, which validate the use of Darcy's law in porous media to control the resin flow during infusion.

  3. Modelling low velocity impact induced damage in composite laminates

    Science.gov (United States)

    Shi, Yu; Soutis, Constantinos

    2017-12-01

    The paper presents recent progress on modelling low velocity impact induced damage in fibre reinforced composite laminates. It is important to understand the mechanisms of barely visible impact damage (BVID) and how it affects structural performance. To reduce labour intensive testing, the development of finite element (FE) techniques for simulating impact damage becomes essential and recent effort by the composites research community is reviewed in this work. The FE predicted damage initiation and propagation can be validated by Non Destructive Techniques (NDT) that gives confidence to the developed numerical damage models. A reliable damage simulation can assist the design process to optimise laminate configurations, reduce weight and improve performance of components and structures used in aircraft construction.

  4. Feasibility on fiber orientation detection on unidirectional CFRP composite laminates using nondestructive evaluation techniques

    Science.gov (United States)

    Yang, In-Young; Kim, Ji-Hoon; Cha, Cheon-Seok; Lee, Kil-Sung; Hsu, David K.; Im, Kwang-Hee

    2007-07-01

    In particular, CFRP (carbon fiber reinforced plastics) composite materials have found wide applicability because of their inherent design flexibility and improved material properties. CFRP composites were manufactured from uni-direction prepreg sheet in this paper. It is important to assess fiber orientation, material properties and part defect in order to ensure product quality and structural integrity of CFRP because strength and stiffness of composites depend on fiber orientation. It is desirable to perform nondestructive evaluation which is very beneficial. An new method for nondestructively determining the fiber orientation in a composite laminate is presented. A one-sided pitch-catch setup was used in the detection and evaluation of flaws and material anomalies in the unidirectional CFRP composite laminates. Two Rayleigh wave transducers were joined head-to-head and used in the pitch-catch mode on the surface of the composites. The pitch-catch signal was found to be more sensitive than normal incidence backwall echo of longitudinal wave to subtle flaw conditions in the composite. Especially, ultrasonic waves were extensively characterized in the CFRP composite laminates both normal to fiber and along to fiber with using a one-sided direction of Rayleigh wave transducers. Also, one-sided ultrasonic measurement was made with using a Rayleigh wave transducers and a conventional scanner was used in an immersion tank for extracting fiber orientation information from the ultrasonic reflection in the unidirectional laminate. Therefore, it is thought that the proposed method is useful to evaluate integrity of CFRP laminates.

  5. Reliability and Sensitivity Analysis for Laminated Composite Plate Using Response Surface Method

    International Nuclear Information System (INIS)

    Lee, Seokje; Kim, Ingul; Jang, Moonho; Kim, Jaeki; Moon, Jungwon

    2013-01-01

    Advanced fiber-reinforced laminated composites are widely used in various fields of engineering to reduce weight. The material property of each ply is well known; specifically, it is known that ply is less reliable than metallic materials and very sensitive to the loading direction. Therefore, it is important to consider this uncertainty in the design of laminated composites. In this study, reliability analysis is conducted using Callosum and Meatball interactions for a laminated composite plate for the case in which the tip deflection is the design requirement and the material property is a random variable. Furthermore, the efficiency and accuracy of the approximation method is identified, and a probabilistic sensitivity analysis is conducted. As a result, we can prove the applicability of the advanced design method for the stabilizer of an underwater vehicle

  6. Reliability and Sensitivity Analysis for Laminated Composite Plate Using Response Surface Method

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Seokje; Kim, Ingul [Chungnam National Univ., Daejeon (Korea, Republic of); Jang, Moonho; Kim, Jaeki; Moon, Jungwon [LIG Nex1, Yongin (Korea, Republic of)

    2013-04-15

    Advanced fiber-reinforced laminated composites are widely used in various fields of engineering to reduce weight. The material property of each ply is well known; specifically, it is known that ply is less reliable than metallic materials and very sensitive to the loading direction. Therefore, it is important to consider this uncertainty in the design of laminated composites. In this study, reliability analysis is conducted using Callosum and Meatball interactions for a laminated composite plate for the case in which the tip deflection is the design requirement and the material property is a random variable. Furthermore, the efficiency and accuracy of the approximation method is identified, and a probabilistic sensitivity analysis is conducted. As a result, we can prove the applicability of the advanced design method for the stabilizer of an underwater vehicle.

  7. Modal analysis of pre and post impacted nano composite laminates

    Directory of Open Access Journals (Sweden)

    R. Velmurugan

    Full Text Available Modal analysis is carried out on pre and post impacted nano composite laminates. The laminates are prepared using 3, 5 and 8 layers of 610gsm glass woven roving mats(WRM with epoxy resin and montmorillonite(MMT clay content is varied from 1% to 5%. Impulse hammer technique is used to find natural frequency and damping factor of laminates. Medium velocity impact tests are conducted by using a gas gun. The vibration responses of natural frequency and damping factor are obtained and are studied for laminates with all edges clamped boundary conditions. Results show considerable improvement in natural frequency and damping factor due to nano clay addition. It is also seen that the nano clay controls the delamination due to impact loading.

  8. Modeling of a partially debonded piezoelectric actuator in smart composite laminates

    International Nuclear Information System (INIS)

    Huang, Bin; Soo Kim, Heung; Ho Yoon, Gil

    2015-01-01

    A partially debonded piezoelectric actuator in smart composite laminates was modeled using an improved layerwise displacement field and Heaviside unit step functions. The finite element method with four node plate element and the extended Hamilton principle were used to derive the governing equation. The effects of actuator debonding on the smart composite laminate were investigated in both the frequency and time domains. The frequency and transient responses were obtained using the mode superposition method and the Newmark time integration algorithm, respectively. Two partial actuator debonding cases were studied to investigate the debonding effects on the actuation capability of the piezoelectric actuator. The effect of actuator debonding on the natural frequencies was subtler, but severe reductions of the actuation ability were observed in both the frequency and time responses, especially in the edge debonded actuator case. The results provided confirmation that the proposed modeling could be used in virtual experiments of actuator failure in smart composite laminates. (paper)

  9. Ultrathin CAD-CAM Ceramic Occlusal Veneers and Anterior Bilaminar Veneers for the Treatment of Moderate Dental Biocorrosion: A 1.5-Year Follow-Up.

    Science.gov (United States)

    Resende, T H; Reis, K R; Schlichting, L H; Magne, P

    2018-03-27

    Dental biocorrosion can produce a devastating impact on oral health. The restorative phase of the treatment should not cause additional damage of the remaining sound tooth structure. Ultrathin occlusal veneers are a conservative alternative to traditional onlays and complete crowns for the treatment of severe biocorrosive lesions. This strategy is explained in the present case report through a full-mouth rehabilitation of a patient with moderate biocorrosion. Maxillary anterior teeth were restored using the bilaminar technique (lingual direct composite veneers with labial ceramic veneers) and posterior teeth using ultrathin CAD-CAM ceramic occlusal veneers. The technical aspects required for the implementation of this new restorative design are presented with a special emphasis on the control of tooth preparation based on diagnostic wax-up, provisionalization, and the use of CAD-CAM technology.

  10. Local and global nonlinear dynamics of a parametrically excited rectangular symmetric cross-ply laminated composite plate

    International Nuclear Information System (INIS)

    Ye Min; Lu Jing; Zhang Wei; Ding Qian

    2005-01-01

    The present investigation deals with nonlinear dynamic behavior of a parametrically excited simply supported rectangular symmetric cross-ply laminated composite thin plate for the first time. The governing equation of motion for rectangular symmetric cross-ply laminated composite thin plate is derived by using von Karman equation. The geometric nonlinearity and nonlinear damping are included in the governing equations of motion. The Galerkin approach is used to obtain a two-degree-of-freedom nonlinear system under parametric excitation. The method of multiple scales is utilized to transform the second-order non-autonomous differential equations to the first-order averaged equations. Using numerical method, the averaged equations are analyzed to obtain the steady state bifurcation responses. The analysis of stability for steady state bifurcation responses in laminated composite thin plate is also given. Under certain conditions laminated composite thin plate may have two or multiple steady state bifurcation solutions. Jumping phenomenon occurs in the steady state bifurcation solutions. The chaotic motions of rectangular symmetric cross-ply laminated composite thin plate are also found by using numerical simulation. The results obtained here demonstrate that the periodic, quasi-periodic and chaotic motions coexist for a parametrically excited fore-edge simply supported rectangular symmetric cross-ply laminated composite thin plate under certain conditions

  11. Design of Multiple Bolted Connections for Laminated Veneer Lumber

    Science.gov (United States)

    Borjen Yeh; Douglas Rammer; Jeff Linville

    2014-01-01

    The design of multiple bolted connections in accordance with Appendix E of the National Design Specification for Wood Construction (NDS) has incorporated provisions for evaluating localized member failure modes of row and group tear-out when the connections are closely spaced. Originally based on structural glued laminated timber (glulam) members made with all L1...

  12. The influences of contamination during lamination on the properties of composite materials

    Energy Technology Data Exchange (ETDEWEB)

    Hall Beng, G.M. (Univ. of Portsmouth, School of Systems Engineering, Portsmouth (United Kingdom)); Mason, S.E. (Univ. of Portsmouth, School of Systems Engineering, Portsmouth (United Kingdom))

    1993-11-01

    The quality of a fibrous composite laminate can be largely attributed to the laminating process. It is therefore important to control parameters which will ultimately affect the desired quality of the laminate. Although several composite manufacturing organisations have installed clean room facilities with the hope of controlling potential contaminants, which may be detrimental to the process, the unavoidable reductions in productivity, coupled with the initial capital and maintenance costs make it an expensive solution to an unquantified problem. This study investigates the influences of contamination on structural fibre reinforced composites. Initial testing has involved contaminating Carbon/Epoxy (Fiberite 7714B) prepregs on a gross level. Contaminants have been selected on a tactile level in order to be as closely representative of situations likely to be encountered in the laminating process. The research has concentrated on airborne particulates, including fibres, condensation and humidity. Modes of contamination have been proposed for each, and suitable test methods selected to verify the modes. Test methods include the sort beam shear test (interlaminar shear strength), double cantilever beam test (interlaminar fracture data) and tensile tests. Such high levels of contamination enables the identification of those contaminants that are most detrimental to final laminate quality. Strategic reduction in the contamination levels of those identified will enable the clean room operating level to be sought. (orig.).

  13. The influences of contamination during lamination on the properties of composite materials

    International Nuclear Information System (INIS)

    Hall Beng, G.M.; Mason, S.E.

    1993-01-01

    The quality of a fibrous composite laminate can be largely attributed to the laminating process. It is therefore important to control parameters which will ultimately affect the desired quality of the laminate. Although several composite manufacturing organisations have installed clean room facilities with the hope of controlling potential contaminants, which may be detrimental to the process, the unavoidable reductions in productivity, coupled with the initial capital and maintenance costs make it an expensive solution to an unquantified problem. This study investigates the influences of contamination on structural fibre reinforced composites. Initial testing has involved contaminating Carbon/Epoxy (Fiberite 7714B) prepregs on a gross level. Contaminants have been selected on a tactile level in order to be as closely representative of situations likely to be encountered in the laminating process. The research has concentrated on airborne particulates, including fibres, condensation and humidity. Modes of contamination have been proposed for each, and suitable test methods selected to verify the modes. Test methods include the sort beam shear test (interlaminar shear strength), double cantilever beam test (interlaminar fracture data) and tensile tests. Such high levels of contamination enables the identification of those contaminants that are most detrimental to final laminate quality. Strategic reduction in the contamination levels of those identified will enable the clean room operating level to be sought. (orig.)

  14. The performance of integrated active fiber composites in carbon fiber laminates

    International Nuclear Information System (INIS)

    Melnykowycz, M; Brunner, A J

    2011-01-01

    Piezoelectric elements integrated into fiber-reinforced polymer-matrix laminates can provide various functions in the resulting adaptive or smart composite. Active fiber composites (AFC) composed of lead zirconate titanate (PZT) fibers can be used as a component in a smart material system, and can be easily integrated into woven composites. However, the impact of integration on the device and its functionality has not been fully investigated. The current work focuses on the integration and performance of AFC integrated into carbon-fiber-reinforced plastic (CFRP) laminates, focusing on the strain sensor performance of the AFC–CFRP laminate under tensile loading conditions. AFC were integrated into cross-ply CFRP laminates using simple insertion and interlacing of the CFRP plies, with the AFC always placed in the 90° ply cutout area. Test specimens were strained to different strain levels and then cycled with a 0.01% strain amplitude, and the resulting signal from the AFC was monitored. Acoustic emission monitoring was performed during tensile testing to provide insight to the failure characteristics of the PZT fibers. The results were compared to those from past studies on AFC integration; the strain signal of AFC integrated into CFRP was much lower than that for AFC integrated into woven glass fiber laminates. However, the profiles of the degradations of the AFC signal resulting from the strain were nearly identical, showing that the PZT fibers fragmented in a similar manner for a given global strain. The sensor performance recovered upon unloading, which is attributed to the closure of cracks between PZT fiber fragments

  15. Strength and fatigue life evaluation of composite laminate with embedded sensors

    Science.gov (United States)

    Rathod, Vivek T.; Hiremath, S. R.; Roy Mahapatra, D.

    2014-04-01

    Prognosis regarding durability of composite structures using various Structural Health Monitoring (SHM) techniques is an important and challenging topic of research. Ultrasonic SHM systems with embedded transducers have potential application here due to their instant monitoring capability, compact packaging potential toward unobtrusiveness and noninvasiveness as compared to non-contact ultrasonic and eddy current techniques which require disassembly of the structure. However, embedded sensors pose a risk to the structure by acting as a flaw thereby reducing life. The present paper focuses on the determination of strength and fatigue life of the composite laminate with embedded film sensors like CNT nanocomposite, PVDF thin films and piezoceramic films. First, the techniques of embedding these sensors in composite laminates is described followed by the determination of static strength and fatigue life at coupon level testing in Universal Testing Machine (UTM). Failure mechanisms of the composite laminate with embedded sensors are studied for static and dynamic loading cases. The coupons are monitored for loading and failure using the embedded sensors. A comparison of the performance of these three types of embedded sensors is made to study their suitability in various applications. These three types of embedded sensors cover a wide variety of applications, and prove to be viable in embedded sensor based SHM of composite structures.

  16. Determination of Fracture Parameters for Multiple Cracks of Laminated Composite Finite Plate

    Science.gov (United States)

    Srivastava, Amit Kumar; Arora, P. K.; Srivastava, Sharad Chandra; Kumar, Harish; Lohumi, M. K.

    2018-04-01

    A predictive method for estimation of stress state at zone of crack tip and assessment of remaining component lifetime depend on the stress intensity factor (SIF). This paper discusses the numerical approach for prediction of first ply failure load (FL), progressive failure load, SIF and critical SIF for multiple cracks configurations of laminated composite finite plate using finite element method (FEM). The Hashin and Chang failure criterion are incorporated in ABAQUS using subroutine approach user defined field variables (USDFLD) for prediction of progressive fracture response of laminated composite finite plate, which is not directly available in the software. A tensile experiment on laminated composite finite plate with stress concentration is performed to validate the numerically predicted subroutine results, shows excellent agreement. The typical results are presented to examine effect of changing the crack tip distance (S), crack offset distance (H), and stacking fiber angle (θ) on FL, and SIF .

  17. Thermoviscoelastic characterization and prediction of Kevlar/epoxy composite laminates

    Science.gov (United States)

    Gramoll, K. C.; Dillard, D. A.; Brinson, H. F.

    1990-01-01

    The thermoviscoelastic characterization of Kevlar 49/Fiberite 7714A epoxy composite lamina and the development of a numerical procedure to predict the viscoelastic response of any general laminate constructed from the same material were studied. The four orthotropic material properties, S sub 11, S sub 12, S sub 22, and S sub 66, were characterized by 20 minute static creep tests on unidirectional (0) sub 8, (10) sub 8, and (90) sub 16 lamina specimens. The Time-Temperature Superposition-Principle (TTSP) was used successfully to accelerate the characterization process. A nonlinear constitutive model was developed to describe the stress dependent viscoelastic response for each of the material properties. A numerical procedure to predict long term laminate properties from lamina properties (obtained experimentally) was developed. Numerical instabilities and time constraints associated with viscoelastic numerical techniques were discussed and solved. The numerical procedure was incorporated into a user friendly microcomputer program called Viscoelastic Composite Analysis Program (VCAP), which is available for IBM PC type computers. The program was designed for ease of use. The final phase involved testing actual laminates constructed from the characterized material, Kevlar/epoxy, at various temperatures and load level for 4 to 5 weeks. These results were compared with the VCAP program predictions to verify the testing procedure and to check the numerical procedure used in the program. The actual tests and predictions agreed for all test cases which included 1, 2, 3, and 4 fiber direction laminates.

  18. A comparative study on low-velocity impact response of fabric composite laminates

    International Nuclear Information System (INIS)

    Zhang, Diantang; Sun, Ying; Chen, Li; Pan, Ning

    2013-01-01

    Highlights: • We examine the low-velocity behavior of single-ply 3D orthogonal woven fabric composites. • Three-coordinate measuring device was used to acquire the 3D topographies. • Single-ply 3D orthogonal woven fabric composites show better impact performance. • Impact properties will increase if in-plane yarns and Z-yarns of single-ply 3D orthogonal woven fabric are optimized. - Abstract: Impact behaviors at low velocity of composite laminates reinforced with fabrics of different architectures are investigated. Unidirectional prepreg, 2D woven and 3D orthogonal fabrics, all formed of Ultrahigh Molecular Weight Polyethylene (UHMWPE) filaments, were selected as reinforcements to form composite laminates using hot pressing technology. Low velocity impact tests were conducted using a drop-weight impact equipment at the energy level of 35 J. A three-coordinate measuring device was employed to determine the volume of plastic deformation and surface dent diameter. The results show that the composite laminates of single-ply 3D orthogonal woven fabric exhibit better energy absorbed capacity and impact damage resistance as compared to those of unidirectional and 2D plain-woven fabric

  19. Discrete Material and Thickness Optimization of laminated composite structures including failure criteria

    DEFF Research Database (Denmark)

    Lund, Erik

    2017-01-01

    This work extends the Discrete Material and Thickness Optimization approach to structural optimization problems where strength considerations in the form of failure criteria are taken into account for laminated composite structures. It takes offset in the density approaches applied for stress...... constrained topology optimization of single-material problems and develops formulations for multi-material topology optimization problems applied for laminated composite structures. The method can be applied for both stress- and strain-based failure criteria. The large number of local constraints is reduced...

  20. Simulation of delamination crack growth in composite laminates: application of local and non-local interface damage models

    International Nuclear Information System (INIS)

    Ijaz, H.; Asad, M.

    2015-01-01

    The use of composite laminates is increasing in these days due to higher strength and low density values in comparison of metals. Delamination is a major source of failure in composite laminates. Damage mechanics based theories are employed to simulate the delamination phenomena between composite laminates. These damage models are inherently local and can cause the concentration of stresses around the crack tip. In the present study integral type non-local damage formulation is proposed to avoid the localization problem associated to damage formulation. A comprehensive study is carried out for the models and classical local damage model are performed and results are compared with available experimental data for un IMS/924 Carbon/fiber epoxy composite laminate. (author)

  1. A genetic algorithm for the optimization of fiber angles in composite laminates

    International Nuclear Information System (INIS)

    Hwang, Shun Fa; Hsu, Ya Chu; Chen, Yuder

    2014-01-01

    A genetic algorithm for the optimization of composite laminates is proposed in this work. The well-known roulette selection criterion, one-point crossover operator, and uniform mutation operator are used in this genetic algorithm to create the next population. To improve the hill-climbing capability of the algorithm, adaptive mechanisms designed to adjust the probabilities of the crossover and mutation operators are included, and the elite strategy is enforced to ensure the quality of the optimum solution. The proposed algorithm includes a new operator called the elite comparison, which compares and uses the differences in the design variables of the two best solutions to find possible combinations. This genetic algorithm is tested in four optimization problems of composite laminates. Specifically, the effect of the elite comparison operator is evaluated. Results indicate that the elite comparison operator significantly accelerates the convergence of the algorithm, which thus becomes a good candidate for the optimization of composite laminates.

  2. Environmental Effects on Flutter Characteristics of Laminated Composite Rectangular and Skew Panels

    Directory of Open Access Journals (Sweden)

    T.V.R. Chowdary

    1996-01-01

    Full Text Available A finite element method is presented for predicting the flutter response of laminated composite panels subjected to moisture concentration and temperature. The analysis accounts for material properties at elevated temperature and moisture concentration. The analysis is based on the first-order approximation to the linear piston theory and laminated plate theory that includes shear deformation. Both rectangular and skew panels are considered. Stability boundaries at moisture concentrations and temperatures for various lamination schemes and boundary conditions are discussed.

  3. Development of Compressive Failure Strength for Composite Laminate Using Regression Analysis Method

    Energy Technology Data Exchange (ETDEWEB)

    Lee, Myoung Keon [Agency for Defense Development, Daejeon (Korea, Republic of); Lee, Jeong Won; Yoon, Dong Hyun; Kim, Jae Hoon [Chungnam Nat’l Univ., Daejeon (Korea, Republic of)

    2016-10-15

    This paper provides the compressive failure strength value of composite laminate developed by using regression analysis method. Composite material in this document is a Carbon/Epoxy unidirection(UD) tape prepreg(Cycom G40-800/5276-1) cured at 350°F(177°C). The operating temperature is –60°F~+200°F(-55°C - +95°C). A total of 56 compression tests were conducted on specimens from eight (8) distinct laminates that were laid up by standard angle layers (0°, +45°, –45° and 90°). The ASTM-D-6484 standard was used for test method. The regression analysis was performed with the response variable being the laminate ultimate fracture strength and the regressor variables being two ply orientations (0° and ±45°)

  4. Development of Compressive Failure Strength for Composite Laminate Using Regression Analysis Method

    International Nuclear Information System (INIS)

    Lee, Myoung Keon; Lee, Jeong Won; Yoon, Dong Hyun; Kim, Jae Hoon

    2016-01-01

    This paper provides the compressive failure strength value of composite laminate developed by using regression analysis method. Composite material in this document is a Carbon/Epoxy unidirection(UD) tape prepreg(Cycom G40-800/5276-1) cured at 350°F(177°C). The operating temperature is –60°F~+200°F(-55°C - +95°C). A total of 56 compression tests were conducted on specimens from eight (8) distinct laminates that were laid up by standard angle layers (0°, +45°, –45° and 90°). The ASTM-D-6484 standard was used for test method. The regression analysis was performed with the response variable being the laminate ultimate fracture strength and the regressor variables being two ply orientations (0° and ±45°)

  5. Determination of maximum negative Poisson's ratio for laminated fiber composites

    Energy Technology Data Exchange (ETDEWEB)

    Shokrieh, M.M.; Assadi, A. [Composites Research Laboratory, Mechanical Engineering Department, Center of Excellence in Experimental Solid Mechanics and Dynamics, Iran University of Science and Technology, Tehran 16846-13114 (Iran, Islamic Republic of)

    2011-05-15

    Contrary to isotropic materials, composites always show complicated mechanical behavior under external loadings. In this article, an efficient algorithm is employed to obtain the maximum negative Poisson's ratio for laminated composite plates. We try to simplify the problem based on normalization of parameters and some manufacturing constraints to overlook the additional constraint of the optimization procedure. A genetic algorithm is used to find the optimal thickness of each lamina with a specified fiber direction. It is observed that the laminated composite with the configuration of (15/60/15) has the maximum negative Poisson's ratio. (Copyright copyright 2011 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  6. Electrical behavior of laminated composites with intralaminar degradation: A comprehensive micro-meso homogenization procedure

    KAUST Repository

    Selvakumaran, Lakshmi; Lubineau, Gilles

    2014-01-01

    Electrical Resistance Tomography (ERT) is a promising health monitoring technique to assess damage in laminated composites. Yet, the missing link between the various complex degradation mechanisms within the laminate and its global change

  7. Effect of Stacking Layup on Spring-back Deformation of Symmetrical Flat Laminate Composites Manufactured through Autoclave Processing

    Science.gov (United States)

    Nasir, M. N. M.; Seman, M. A.; Mezeix, L.; Aminanda, Y.; Rivai, A.; Ali, K. M.

    2017-03-01

    The residual stresses that develop within fibre-reinforced laminate composites during autoclave processing lead to dimensional warpage known as spring-back deformation. A number of experiments have been conducted on flat laminate composites with unidirectional fibre orientation to examine the effects of both the intrinsic and extrinsic parameters on the warpage. This paper extends the study on to the symmetrical layup effect on spring-back for flat laminate composites. Plies stacked at various symmetrical sequences were fabricated to observe the severity of the resulting warpage. Essentially, the experimental results demonstrated that the symmetrical layups reduce the laminate stiffness in its principal direction compared to the unidirectional laminate thus, raising the spring-back warpage with the exception of the [45/-45]S layup due to its quasi-isotropic property.

  8. Assessment and propagation of mechanical property uncertainties in fatigue life prediction of composite laminates

    DEFF Research Database (Denmark)

    Castro, Oscar; Branner, Kim; Dimitrov, Nikolay Krasimirov

    2018-01-01

    amplitude loading cycles. Fatigue life predictions of unidirectional and multi-directional glass/epoxy laminates are carried out to validate the proposed model against experimental data. The probabilistic fatigue behavior of laminates is analyzed under constant amplitude loading conditions as well as under......A probabilistic model for estimating the fatigue life of laminated composite materials considering the uncertainty in their mechanical properties is developed. The uncertainty in the material properties is determined from fatigue coupon tests. Based on this uncertainty, probabilistic constant life...... diagrams are developed which can efficiently estimate probabilistic É›-N curves at any load level and stress ratio. The probabilistic É›-N curve information is used in a reliability analysis for fatigue limit state proposed for estimating the probability of failure of composite laminates under variable...

  9. Criterion of damage beginning: experimental identification for laminate composite

    International Nuclear Information System (INIS)

    Thiebaud, F.; Perreux, D.; Varchon, D.; Lebras, J.

    1996-01-01

    The aim of this study is to propose a criterion of damage beginning for laminate composite. The materials is a glass-epoxy laminate [+55 deg.,-55 deg.[ n performed by winding filament process. First of all a description of the damage is performed and allows to define a damage variable. Thanks to the potential of free energy, an associated variable is defined. The damage criterion is written by using this last one. The parameter of the criterion is identified using mechanical and acoustical methods. The result is compared and exhibit a good agreement. (authors). 13 refs., 5 figs

  10. Bending analysis of laminated composite plates using finite element ...

    African Journals Online (AJOL)

    user

    theory to analyze the laminated composite plates. They concluded that ...... Aeronautics and Astronautics”, Inc.1801, Chapter 8, pp. 240. Baltacıoğlu A.K .... He is working as Assistant Professor in the Department of Mechanical. Engineering in ...

  11. Vibrations of laminated composite thick shells of revolution having meridionally varying curvature

    International Nuclear Information System (INIS)

    Suzuki, Katsuyoshi; Shikanai, Genji; Baba, Iwato

    1998-01-01

    An exact solution is presented for solving free vibrations of laminated composite thick shells of revolution having meridionally varying curvature. Based on the thick lamination theory considering the shear deformation and rotary inertia, equations of motion and boundary conditions are obtained from the stationary conditions of the Lagrangian. The equations of motion are solved exactly by using a power series expansion for symmetrically laminated cross-ply shells. Frequencies and mode shapes of shells of revolution having elliptical and parabolical meridians are presented for both ends clamped, and the effects of shear deformation and rotary inertia are discussed by comparing the results from the present theory with those from the thin lamination theory. (author)

  12. A Novel Procedure for Prediction of Mixed Mode I/II in Fracture Toughness of Laminate Composites

    Directory of Open Access Journals (Sweden)

    M. Mahmood Shokrieh

    2014-06-01

    Full Text Available Delamination is one of the important modes of failure in laminated composite materials. In this respect, the mixed mode I/II fracture is the most major mode of delamination incidence in laminated composite. In the present research, a relation between the fracture toughness of double cantilever beam (DCB and asymmetric double cantilever beam (ADCB specimens is presented. The DCB and ADCB samples are used for measuring the mode I and mixed mode I/II fracture toughness (G of laminated composite materials, respectively. By considering the diversity of the stacking sequence of lay-ups, the test performance on all different types of lay-ups in order to measure the fracture toughness of laminated composites is a tedious, costly and time consuming task. The purpose of deriving this relation is to estimate the value of the strain energy release rate of laminated composite ADCB specimens by testing a unidirectional DCB. To develop this relationship, the geometry of DCB and ADCB specimens are considered to obtain fracture toughness of multi-directional laminate composites of ADCB samples with arbitrary ply sequence which may be used for design purposes. The procedure presented here reduces the calculation costs of the finite element modeling and its corresponding test significantly. The results obtained by this method are compared with those of experimental and numerical methods. It is shown that the fracture toughness of multi-directional lay-ups can be predicted by measuring the unidirectional ply with an error less than 10% demonstrating the accuracy of the procedure developed in the present research.

  13. Analysis of Usability in Furniture Production of Wood Plastic Laminated Board

    Directory of Open Access Journals (Sweden)

    Abdullah Cemil Ilçe

    2015-05-01

    Full Text Available The objective of this study was to manufacture a lightweight and easily producible wood plastic laminate (WPL board that could be used in the furniture sector. Eastern beech (Fagus orientalis L. veneer papels (A and hollow polycarbonate boards (B, both with a thickness of 4 mm, were laminated in different combinations using polyurethane (PUR and polychloroprene (PCR adhesives. The physical and mechanical properties of the WPL boards obtained were determined according to the principles specified in the EN 326-1, EN 317, EN 310, ASTM D1037, and ASTM D1761 standards. Subsequently, the specimens were compared with particle boards (PB, medium density fiberboards (MDF, and okoume plywoods (PW. According to the results, the AABAA, ABABA, and ABBBA combinations of the WPL materials had better physical properties, such as weight, water absorption, and swelling thickness, compared to the other composites. Furthermore, because the WPL materials had a high bending resistance, modulus of elasticity, and nail and screw withdrawal strength, they could be used instead of PB and MDF. The WPL material obtained within the scope of this study are suitable for furniture making.

  14. The fatigue behavior of composite laminates under various mean stresses

    Science.gov (United States)

    Rotem, A.

    1991-01-01

    A method is developed for predicting the S-N curve of a composite laminate which is subjected to an arbitrary stress ratio, R (minimum stress/maximum stress). The method is based on the measuring of the S-N behavior of two distinct cases, tension-tension and compression-compression fatigue loadings. Using these parameters, expressions are formulated that estimate the fatigue behavior under any stress ratio loading. Experimental results from the testing of graphite/epoxy laminates, with various structures, are compared with the predictions and show good agreement.

  15. Current injection phase thermography for low-velocity impact damage identification in composite laminates

    International Nuclear Information System (INIS)

    Grammatikos, S.A.; Kordatos, E.Z.; Matikas, T.E.; David, C.; Paipetis, A.S.

    2014-01-01

    Highlights: • A novel Current injection phase thermography NDE method has been developed. • Blind impact damage has been successfully detected in composite laminates. • Carbon nanotubes enhance detection by improving of through thickness conductivity. • Detection is feasible with considerably less energy than for IR excited thermography. - Abstract: An innovative non-destructive evaluation (NDE) technique is presented based on current stimulated thermography. Modulated electric current is injected to Carbon Fibre Reinforced Plastics (CFRP) laminates as an external source of thermal excitation. Pulsed Phase Thermography (PPT) is concurrently employed to identify low velocity impact induced (LVI) damage. The efficiency of the proposed method is demonstrated for both plain and with Carbon Nanotubes (CNTs) modified laminates, which are subjected to low-velocity impact damaged composite laminates at different energy levels. The presence of the nano reinforcing phase is important in achieving a uniform current flow along the laminate, as it improves the through thickness conductivity. The acquired thermographs are compared with optical PPT, C-scan images and Computer Tomography (CT) representations. The typical energy input for successful damage identification with current injection is three to four orders of magnitude less compared to the energy required for optical PPT

  16. Fabrication and characterization of laminated Ti-(TiB+La2O3/Ti composite

    Directory of Open Access Journals (Sweden)

    Yuanfei Han

    2015-10-01

    Full Text Available The incorporation of ceramic particulate reinforcements into titanium alloys can improve the specific strength and specific stiffness, while inevitably reduce the plasticity and ductility. In this study, in situ synthesized multilayer Ti-(TiB+La2O3/Ti composite was designed by learning from the microstructure of nature biological materials with excellent mechanical properties. The Ti-(TiB+La2O3/Ti composite with unique characteristic of laminated structure was prepared by combined powder metallurgy and hot rolling. The method has the synthesize advantages with in-situ reaction of Ti and LaB6 at high temperature and controllability of reinforcements size and constituent phases in composites. The result shows that the pores in the as sintered laminated structure composite completely disappeared after hot rolling at 1050 °C. The agglomerated reinforcement particles were well dispersed and distributed uniformly along the rolling direction. The thickness of pure Ti layer and (TiB+La2O3/Ti composite layer decreased from 1 mm to about 200 μm. Meanwhile, the grains size was refined obviously after rolling deformation. The room temperature tensile test indicates that the elongation of the laminated Ti-(TiB+La2O3/Ti composite improved from 13% to 17% in comparison with the uniform (TiB+La2O3/Ti composite, while the tensile strength had little change. It provides theoretical and experimental basis for fabricating the novel high performance laminated Ti-(TiB+La2O3/Ti composites.

  17. Scarf Repair of Composite Laminates

    Directory of Open Access Journals (Sweden)

    Xie Zonghong

    2016-01-01

    Full Text Available The use of composite materials, such as carbon-fiber reinforced plastic (CFRP composites, aero-structures has led to an increased need of advanced assembly joining and repair technologies. Adhesive bonded repairs as an alternative to recover full or part of initial strength were investigated. Tests were conducted with the objective of evaluating the effectiveness of techniques used for repairing damage fiber reinforced laminated composites. Failure loads and failure modes were generated and compared with the following parameters: scarf angles, roughness of grind tool and number of external plies. Results showed that scarf angle was the critical parameter and the largest tensile strength was observed with the smallest scarf angle. Besides, the use of external plies at the outer surface could not increase the repairs efficiency for large scarf angle. Preparing the repair surfaces by sanding them with a sander ranging from 60 to 100 grit number had significant effect on the failure load. These results allowed the proposal of design principles for repairing CFRP structures.

  18. Curing of Thick Thermoset Composite Laminates: Multiphysics Modeling and Experiments

    Science.gov (United States)

    Anandan, S.; Dhaliwal, G. S.; Huo, Z.; Chandrashekhara, K.; Apetre, N.; Iyyer, N.

    2017-11-01

    Fiber reinforced polymer composites are used in high-performance aerospace applications as they are resistant to fatigue, corrosion free and possess high specific strength. The mechanical properties of these composite components depend on the degree of cure and residual stresses developed during the curing process. While these parameters are difficult to determine experimentally in large and complex parts, they can be simulated using numerical models in a cost-effective manner. These simulations can be used to develop cure cycles and change processing parameters to obtain high-quality parts. In the current work, a numerical model was built in Comsol MultiPhysics to simulate the cure behavior of a carbon/epoxy prepreg system (IM7/Cycom 5320-1). A thermal spike was observed in thick laminates when the recommended cure cycle was used. The cure cycle was modified to reduce the thermal spike and maintain the degree of cure at the laminate center. A parametric study was performed to evaluate the effect of air flow in the oven, post cure cycles and cure temperatures on the thermal spike and the resultant degree of cure in the laminate.

  19. Pitch catch ultrasonic study on unidirectional CFRP composite laminates using rayleigh wave transducers

    International Nuclear Information System (INIS)

    Park, Je Woong; Yang, In Young; Im, Kwang Hee; Hsu, David K.; Jung, Jong An

    2012-01-01

    The importance of carbon fiber reinforced plastics (CFRP) has been generally recognized, and CFRP composite laminates have become widely used. Thus, a nondestructive technique would be very useful for evaluating CF/epoxy composite laminates. A pitch catch UT signal is more sensitive than is a normal incidence backwall echo of a longitudinal wave in composites. The depth of the sampling volume where the pitch catch UT signal came from is relatively shallow, but the depth can be increased by increasing the separation distance of the transmitting and receiving probes. Moreover, a method is utilized to determine the porosity content of a composite lay up by processing micrograph images of the laminate. The porosity content of a composite structure is critical to the overall strength and performance of the structure. The image processing method developed utilizes software to process micrograph images of the test sample. The results from the image processing method are compared with existing data. Beam profile is characterized in unidirectional CFRP using pitch catch Rayleigh probes. The one sided and two sided pitch catch techniques are utilized to produce C scan images with the aid of an automatic scanner. The pitch catch ultrasonic signal corresponds with the simulated results of unidirectional CFRP composites

  20. Guided Wave Propagation Study on Laminated Composites by Frequency-Wavenumber Technique

    Science.gov (United States)

    Tian, Zhenhua; Yu, Lingyu; Leckey, Cara A. C.

    2014-01-01

    Toward the goal of delamination detection and quantification in laminated composites, this paper examines guided wave propagation and wave interaction with delamination damage in laminated carbon fiber reinforced polymer (CFRP) composites using frequency-wavenumber (f-kappa) analysis. Three-dimensional elastodynamic finite integration technique (EFIT) is used to acquire simulated time-space wavefields for a CFRP composite. The time-space wavefields show trapped waves in the delamination region. To unveil the wave propagation physics, the time-space wavefields are further analyzed by using two-dimensional (2D) Fourier transforms (FT). In the analysis results, new f-k components are observed when the incident guided waves interact with the delamination damage. These new f-kappa components in the simulations are experimentally verified through data obtained from scanning laser Doppler vibrometer (SLDV) tests. By filtering the new f-kappa components, delamination damage is detected and quantified.

  1. Modeling the kinematics of multi-axial composite laminates as a stacking of 2D TIF plies

    Science.gov (United States)

    Ibañez, Ruben; Abisset-Chavanne, Emmanuelle; Chinesta, Francisco; Huerta, Antonio

    2016-10-01

    Thermoplastic composites are widely considered in structural parts. In this paper attention is paid to sheet forming of continuous fiber laminates. In the case of unidirectional prepregs, the ply constitutive equation is modeled as a transversally isotropic fluid, that must satisfy both the fiber inextensibility as well as the fluid incompressibility. When the stacking sequence involves plies with different orientations the kinematics of each ply during the laminate deformation varies significantly through the composite thickness. In our former works we considered two different approaches when simulating the squeeze flow induced by the laminate compression, the first based on a penalty formulation and the second one based on the use of Lagrange multipliers. In the present work we propose an alternative approach that consists in modeling each ply involved in the laminate as a transversally isotropic fluid - TIF - that becomes 2D as soon as incompressibility constraint and plane stress assumption are taken into account. Thus, composites laminates can be analyzed as a stacking of 2D TIF models that could eventually interact by using adequate friction laws at the inter-ply interfaces.

  2. ESTIMATING THE SIZE OF LATE VENEER IMPACTORS FROM IMPACT-INDUCED MIXING ON MERCURY

    International Nuclear Information System (INIS)

    Rivera-Valentin, E. G.; Barr, A. C.

    2014-01-01

    Late accretion of a ''veneer'' of compositionally diverse planetesimals may introduce chemical heterogeneity in the mantles of the terrestrial planets. The size of the late veneer objects is an important control on the angular momenta, eccentricities, and inclinations of the terrestrial planets, but current estimates range from meter-scale bodies to objects with diameters of thousands of kilometers. We use a three-dimensional global Monte Carlo model of impact cratering, excavation, and ejecta blanket formation to show that evidence of mantle heterogeneity can be preserved within ejecta blankets of mantle-exhuming impacts on terrestrial planets. Compositionally distinct provinces implanted at the time of the late veneer are most likely to be preserved in bodies whose subsequent geodynamical evolution is limited. Mercury may have avoided intensive mixing by solid-state convection during much of its history. Its subsequent bombardment may have then excavated evidence of primordial mantle heterogeneity introduced by the late veneer. Simple geometric arguments can predict the amount of mantle material in the ejecta blanket of mantle-exhuming impacts, and deviations in composition relative to geometric predictions can constrain the length-scale of chemical heterogeneities in the subsurface. A marked change in the relationship between mantle and ejecta composition occurs when chemically distinct provinces are ∼250 km in diameter; thus, evidence of bombardment by thousand-kilometer-sized objects should be readily apparent from the variation in compositions of ejecta blankets in Mercury's ancient cratered terrains

  3. Enhanced laminated composite phase change material for energy storage

    Energy Technology Data Exchange (ETDEWEB)

    Darkwa, J.; Zhou, T. [Centre for Sustainable Energy Technologies (CSET), The University of Nottingham Ningbo, 199 Taikang East Road, Ningbo 315100 (China)

    2011-02-15

    This paper summarises studies undertaken towards the development of a laminated composite aluminium/hexadecane phase change material (PCM) drywall based on previous analytical work. The study also covered the selection and testing of various types of adhesive materials and identified Polyvinyl acetate (PVA) material as a suitable bonding material. For the purpose of comparison pure hexadecane and composite aluminium/hexadecane samples were developed and tested. The test results revealed faster thermal response by the aluminium/hexadecane sample regarding the rate of heat flux and also achieved about 10% and 15% heat transfer enhancements during the charging and discharging periods respectively. Its measured effective thermal conductivity also increased remarkably to 1.25 W/mK as compared with 0.15 W/mK for pure hexadecane. However there was about 5% less total cumulative thermal energy discharged at the end of the test which indicates that its effective thermal capacity was reduced by the presence of the aluminium particles. The study has shown that some of the scientific and technical barriers associated with the development of laminated composite PCM drywall systems can be overcome but further investigations of effects of adhesive materials are needed. (author)

  4. Nonlinear vibrations of thin arbitrarily laminated composite plates subjected to harmonic excitations using DKT elements

    Science.gov (United States)

    Chiang, C. K.; Xue, David Y.; Mei, Chuh

    1993-04-01

    A finite element formulation is presented for determining the large-amplitude free and steady-state forced vibration response of arbitrarily laminated anisotropic composite thin plates using the Discrete Kirchhoff Theory (DKT) triangular elements. The nonlinear stiffness and harmonic force matrices of an arbitrarily laminated composite triangular plate element are developed for nonlinear free and forced vibration analyses. The linearized updated-mode method with nonlinear time function approximation is employed for the solution of the system nonlinear eigenvalue equations. The amplitude-frequency relations for convergence with gridwork refinement, triangular plates, different boundary conditions, lamination angles, number of plies, and uniform versus concentrated loads are presented.

  5. Influence of stacking sequence on scattering characteristics of the fundamental anti-symmetric Lamb wave at through holes in composite laminates.

    Science.gov (United States)

    Veidt, Martin; Ng, Ching-Tai

    2011-03-01

    This paper investigates the scattering characteristics of the fundamental anti-symmetric (A(0)) Lamb wave at through holes in composite laminates. Three-dimensional (3D) finite element (FE) simulations and experimental measurements are used to study the physical phenomenon. Unidirectional, bidirectional, and quasi-isotropic composite laminates are considered in the study. The influence of different hole diameter to wavelength aspect ratios and different stacking sequences on wave scattering characteristics are investigated. The results show that amplitudes and directivity distribution of the scattered Lamb wave depend on these parameters. In the case of quasi-isotropic composite laminates, the scattering directivity patterns are dominated by the fiber orientation of the outer layers and are quite different for composite laminates with the same number of laminae but different stacking sequence. The study provides improved physical insight into the scattering phenomena at through holes in composite laminates, which is essential to develop, validate, and optimize guided wave damage detection and characterization techniques. © 2011 Acoustical Society of America

  6. A Mixed-Mode (I-II) Fracture Criterion for AS4/8552 Carbon/Epoxy Composite Laminate

    Science.gov (United States)

    Karnati, Sidharth Reddy

    A majority of aerospace structures are subjected to bending and stretching loads that introduce peel and shear stresses between the plies of a composite laminate. These two stress components cause a combination of mode I and II fracture modes in the matrix layer of the composite laminate. The most common failure mode in laminated composites is delamination that affects the structural integrity of composite structures. Damage tolerant designs of structures require two types of materials data: mixed-mode (I-II) delamination fracture toughness that predicts failure and delamination growth rate that predicts the life of the structural component. This research focuses determining mixed-mode (I-II) fracture toughness under a combination of mode I and mode II stress states and then a fracture criterion for AS4/8552 composite laminate, which is widely used in general aviation. The AS4/8552 prepreg was supplied by Hexcel Corporation and autoclave fabricated into a 20-ply unidirectional laminate with an artificial delamination by a Fluorinated Ethylene Propylene (FEP) film at the mid-plane. Standard split beam specimens were prepared and tested in double cantilever beam (DCB) and end notched flexure modes to determine mode I (GIC) and II (GIIC) fracture toughnesses, respectively. The DCB specimens were also tested in a modified mixed-mode bending apparatus at GIIm /GT ratios of 0.18, 0.37, 0.57 and 0.78, where GT is total and GIIm is the mode II component of energy release rates. The measured fracture toughness, GC, was found to follow the locus a power law equation. The equation was validated for the present and literature experimental data.

  7. Shade evaluation of ceramic laminates according to different try-in materials.

    Science.gov (United States)

    Lopes, Lawrence Gonzaga; Vaz, Maysa Magalhaes; de Magalhaes, Ana Paula Rodrigues; Cardoso, Paula Carvalho; de Souza, Joao Batista; de Torres, Erica Miranda

    2014-01-01

    The porcelain laminate replaces the visible portion of enamel with a ceramic, which is attached to the dental surface. To enhance cosmetic results, a preliminary color matching procedure is performed prior to cementing the veneers. This procedure can be performed using water, water-soluble gel, or try-in paste. The different shades of cement and try-in pastes are intended to obtain better color and esthetics of the final restoration. This study sought to evaluate the shade of ceramic veneers produced by different try-in materials. Forty bovine teeth and 40 ceramic discs (0.6 mm thick) were prepared. The samples were divided into 4 groups (n = 10). For Group 1 samples, no material was used between the tooth and the ceramic, Group 2 interposed samples with water, Group 3 used a water-soluble gel, and Group 4 used try-in paste (value 0). The color was measured with a spectrophotometer, obtaining L*, a*, and b* values to calculate the color difference (ΔE*). The data were subjected to normality tests and 1-way ANOVA. No significant statistical differences were found among the groups, indicating that the different try-in materials had similar effects on the color of the ceramic laminates.

  8. Elastic-plastic analysis of AS4/PEEK composite laminate using a one-parameter plasticity model

    Science.gov (United States)

    Sun, C. T.; Yoon, K. J.

    1992-01-01

    A one-parameter plasticity model was shown to adequately describe the plastic deformation of AS4/PEEK (APC-2) unidirectional thermoplastic composite. This model was verified further for unidirectional and laminated composite panels with and without a hole. The elastic-plastic stress-strain relations of coupon specimens were measured and compared with those predicted by the finite element analysis using the one-parameter plasticity model. The results show that the one-parameter plasticity model is suitable for the analysis of elastic-plastic deformation of AS4/PEEK composite laminates.

  9. Nonlinear analysis of AS4/PEEK thermoplastic composite laminate using a one parameter plasticity model

    Science.gov (United States)

    Sun, C. T.; Yoon, K. J.

    1990-01-01

    A one-parameter plasticity model was shown to adequately describe the orthotropic plastic deformation of AS4/PEEK (APC-2) unidirectional thermoplastic composite. This model was verified further for unidirectional and laminated composite panels with and without a hole. The nonlinear stress-strain relations were measured and compared with those predicted by the finite element analysis using the one-parameter elastic-plastic constitutive model. The results show that the one-parameter orthotropic plasticity model is suitable for the analysis of elastic-plastic deformation of AS4/PEEK composite laminates.

  10. Evaluation of the retentive means, opacifiers and veneering materials for veneered crowns using 137 Cs

    International Nuclear Information System (INIS)

    Nour, A.M.; El-Sadeek; M.E.; Ramadan, F.A.; Eskander, M.

    1991-01-01

    The purpose of this investigation is to evaluate the best plastic veneering material, which affords initial sealing and adaptation to the metal backing. Cs chloride is used for this purpose. The effect of different retentive means, namely, under cuts, wire loops, stainless steel grills, and acrylic beads, as well as the effect of different opaquers were studied. The influence of time factor and changing temperature was considered as well. The results obtained showed the following: 1- A quantitative method for the evaluation of micro leakage is essential parallel to the semiquantitative one. 2- The tested opaquer exhibits a better sealing ability. 3- The leakage increases significantly by temperature cycling, and by time duration with all the veneering materials tested. Composite is the least leak-sensitive material to changes in temperature. 4- Beads offered the best means of retention, to obtain the best sealing qualities.1 tab., 2 fig

  11. Analysis on and Optimization of a Circular Piezoelectric Composite Laminate for a Micro-Pump Driver

    International Nuclear Information System (INIS)

    Jia, Jianyuan; Wang, Weidong; Huang, Xinbo

    2002-01-01

    Among the various micro-pump actuation devices, piezoelectric composite laminate actuation has become an effective method. Due to lacking of analysis treatments, the design of this type micro-pump is in a great limitation. In this paper, an electromechanical-coupled mechanics model is established for the circle-flake micro-actuator. A kind of analysis and design method is presented that piezoelectric plate's radial strain induced by inverse piezoelectric effect is equivalently substituted with transverse stress on piezoelectric composite laminates. It is pointed out that the equivalent transverse load depends on the edge electric field distribution of parallel plate capacitor. The question has been solved that where the neutral plane in the piezoelectric composite laminates lies. Finally, an optimization design is developed on the radius ratio of piezoelectric-to-silicon plate radius by utilizing of FEA modeling

  12. Fabrication of laminated ZrC-SiC composite by vacuum hot-pressing sintering

    Directory of Open Access Journals (Sweden)

    Yuanyuan Li

    2015-03-01

    Full Text Available Laminated ZrC-SiC ceramic was prepared through tape casting and hot pressing. The green tapes of ZrC and SiC were prepared at room temperature. In order to improve the density of composite, the binder of green tapes were removed at 550 °C for 1 h. The laminated structure and the cracks propagation path, which is not a straight line, are observed by optical metalloscope. The compact laminated ZrC-SiC composite sintered by vacuum hot-pressing at 1650 °C for 90 min under pressure of 20 MPa was researched by X-ray diffraction and scanning electron microscopy (SEM equipped with energy dispersive X-ray analysis. The results showed that interlayer bonding is tight, and no disordered phase has formed in the interlayers of ZrC or SiC, and the combination mode is physical mechanism.

  13. Analysis of a hybrid balanced laminate as a structural material for thick composite beams with axial stiffeners

    Energy Technology Data Exchange (ETDEWEB)

    Modak, Partha; Hossain, M. Jamil, E-mail: jamil917@gmail.com; Ahmed, S. Reaz [Department of Mechanical Engineering, Bangladesh University of Engineering and Technology, Dhaka 1000 (Bangladesh)

    2016-07-12

    An accurate stress analysis has been carried out to investigate the suitability of a hybrid balanced laminate as a structural material for thick composite beams with axial stiffeners. Three different balanced laminates composed of dissimilar ply material as well as fiber orientations are considered for a thick beam on simple supports with stiffened lateral ends. A displacement potential based elasticity approach is used to obtain the numerical solution of the corresponding elastic fields. The overall laminate stresses as well as individual ply stresses are analysed mainly in the perspective of laminate hybridization. Both the fiber material and ply angle of individual laminas are found to play dominant roles in defining the design stresses of the present composite beam.

  14. Modeling the Mechanical Behavior of Aluminum Laminated Metal Composites During High Temperature Deformation

    National Research Council Canada - National Science Library

    Grishber, R

    1997-01-01

    A constitutive model for deformation of a novel laminated metal composite (LMC) which is comprised of 21 alternating layers of Al 5182 alloy and Al 6090/SiC/25p metal matrix composite (MMC) has been proposed...

  15. Influence of veneer thickness on residual stress profile in veneering ceramic: measurement by hole-drilling.

    Science.gov (United States)

    Mainjot, Amélie K; Schajer, Gary S; Vanheusden, Alain J; Sadoun, Michaël J

    2012-02-01

    The veneering process of frameworks induces residual stresses and can initiate cracks when combined with functional stresses. The stress distribution within the veneering ceramic as a function of depth is a key factor influencing failure by chipping. This is a well-known problem with Yttria-tetragonal-zirconia-polycrystal based fixed partial dentures. The objective of this study is to investigate the influence of veneer thickness on the stress profile in zirconia- and metal-based structures. The hole-drilling method, often used for engineering measurements, was adapted for use with veneering ceramic. The stress profile was measured in bilayered disc samples of 20 mm diameter, with a 1 mm thick zirconia or metal framework. Different veneering ceramic thicknesses were performed: 1 mm, 1.5 mm, 2 mm, 2.5 mm and 3 mm. All samples exhibited the same type of stress vs. depth profile, starting with compressive at the ceramic surface, decreasing with depth up to 0.5-1.0 mm from the surface, and then becoming compressive again near the framework, except for the 1.5 mm-veneered zirconia samples which exhibited interior tensile stresses. Stresses in the surface of metal samples were not influenced by veneer thickness. Variation of interior stresses at 1.2 mm from the surface in function of veneer thickness was inverted for metal and zirconia samples. Veneer thickness influences in an opposite way the residual stress profile in metal- and in zirconia-based structures. A three-step approach and the hypothesis of the crystalline transformation are discussed to explain the less favorable residual stress development in zirconia samples. Copyright © 2011 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

  16. Meshfree modeling in laminated composites

    KAUST Repository

    Simkins, Daniel Craig; Collier, Nathan; Alford, Joseph B.

    2012-01-01

    A problem of increasing importance in the aerospace industry is in detailed modeling of explicit fracture in laminated composite materials. For design applications, the simulation must be capable of initiation and propagation of changes in the problem domain. Further, these changes must be able to be incorporated within a design-scale simulation. The use of a visibility condition, coupled with the local and dynamic nature of meshfree shape function construction allows one to initiate and explicitly open and propagate holes inside a previously continuous problem domain. The method to be presented naturally couples to a hierarchical multi-scale material model incorporating external knowldege bases to achieve the goal of a practical explicit fracture modeling capability for full-scale problems. © 2013 Springer-Verlag.

  17. Meshfree modeling in laminated composites

    KAUST Repository

    Simkins, Daniel Craig

    2012-09-27

    A problem of increasing importance in the aerospace industry is in detailed modeling of explicit fracture in laminated composite materials. For design applications, the simulation must be capable of initiation and propagation of changes in the problem domain. Further, these changes must be able to be incorporated within a design-scale simulation. The use of a visibility condition, coupled with the local and dynamic nature of meshfree shape function construction allows one to initiate and explicitly open and propagate holes inside a previously continuous problem domain. The method to be presented naturally couples to a hierarchical multi-scale material model incorporating external knowldege bases to achieve the goal of a practical explicit fracture modeling capability for full-scale problems. © 2013 Springer-Verlag.

  18. Bending Response of Cross-Ply Laminated Composite Plates with Diagonally Perturbed Localized Interfacial Degeneration

    Directory of Open Access Journals (Sweden)

    Chee Zhou Kam

    2013-01-01

    Full Text Available A laminated composite plate element with an interface description is developed using the finite element approach to investigate the bending performance of two-layer cross-ply laminated composite plates in presence of a diagonally perturbed localized interfacial degeneration between laminae. The stiffness of the laminate is expressed through the assembly of the stiffnesses of lamina sub-elements and interface element, the latter of which is formulated adopting the well-defined virtually zero-thickness concept. To account for the extent of both shear and axial weak bonding, a degeneration ratio is introduced in the interface formulation. The model has the advantage of simulating a localized weak bonding at arbitrary locations, with various degeneration areas and intensities, under the influence of numerous boundary conditions since the interfacial description is expressed discretely. Numerical results show that the bending behavior of laminate is significantly affected by the aforementioned parameters, the greatest effect of which is experienced by those with a localized total interface degeneration, representing the case of local delamination.

  19. Investigation of actuator debonding effects on active control in smart composite laminates

    Directory of Open Access Journals (Sweden)

    Bin Huang

    2015-04-01

    Full Text Available This article presents a numerical study of active vibration control of smart composite laminates in the presence of actuator debonding failures. A comparison between the smart composite laminates with healthy actuator and various partially debonded actuator cases is performed to investigate the debonding effects on the vibration suppression. The improved layerwise theory with Heaviside’s unit step function is adopted to model the displacement field with actuator debonding failure. The higher order electric potential field is adopted to describe the potential variation through the thickness. The finite element method–based formulations are derived using the plate element, taking into consideration the electro-mechanical coupling effect. The reduced-order model is represented by the state-space form and further for the vibration suppression using a simple constant gain velocity feedback control strategy. For the purpose of demonstration, a 16-layer cross-ply substrate laminate ([0/90]4s is employed for the numerical study. The results show that the actuator debonding affects the closed-loop frequencies, active damping ratios, and efficiency of vibration suppression.

  20. Origin and mixing timescale of Earth's late veneer

    Science.gov (United States)

    Prescher, C.; Allu Peddinti, D.; Bell, E. A.; Bello, L.; Cernok, A.; Ghosh, N.; Tucker, J.; Wielicki, M. M.; Zahnle, K. J.

    2012-12-01

    Experimental studies on the partitioning behavior of highly siderophile elements (HSE) between silicate and metallic melts imply that the Earth's mantle should have been highly depleted in these elements by core formation in an early magma ocean. However, present HSE contents of the Earth's mantle are ~3 orders of magnitude higher than that expected by experiments. The apparent over-abundance of HSE has commonly been explained by the addition of meteoritic material in the "late veneer" which describes the exogenous mass addition following the moon forming impact and concluding with the late heavy bombardment at ~3.8-3.9 Ga. The strongest evidence for this theory is that the platinum group element (PGE) contents in today's mantle are present in chondritic relative abundances, as opposed to a fractionated pattern expected with metal-silicate partitioning. Archean komatiites indicate that the PGE content of the Earth's mantle increased from about half their present abundances at 3.5 Ga to their present abundances at 2.9 Ga. This secular increase in PGE content suggests a progressive mixing of the late veneer material into the Earth's mantle. However, this time scale also implies that the whole mantle was relatively well mixed by 2.9 Ga. We use a compilation of existing isotopic and trace element data in order to constrain the origin and composition of the late veneer. We use PGE abundances, W abundances and W isotopic compositions in chondritic meteorites and the primitive upper mantle to compute the amount of mass delivered during the late veneer and find the late veneer mass to be ~0.6 % the mass of the bulk silicate Earth (consistent with earlier estimates). We also use the 187Re-187Os and 190Pt-186Os systems to constrain the composition and timing of delivery of the impacting population. We model the efficiency of mantle mixing in this time frame by using 3-dimensional numerical geodynamical simulations and geochemical constraints. Initial parameters include the

  1. Performance analysis of smart laminated composite plate integrated with distributed AFC material undergoing geometrically nonlinear transient vibrations

    Science.gov (United States)

    Shivakumar, J.; Ashok, M. H.; Khadakbhavi, Vishwanath; Pujari, Sanjay; Nandurkar, Santosh

    2018-02-01

    The present work focuses on geometrically nonlinear transient analysis of laminated smart composite plates integrated with the patches of Active fiber composites (AFC) using Active constrained layer damping (ACLD) as the distributed actuators. The analysis has been carried out using generalised energy based finite element model. The coupled electromechanical finite element model is derived using Von Karman type nonlinear strain displacement relations and a first-order shear deformation theory (FSDT). Eight-node iso-parametric serendipity elements are used for discretization of the overall plate integrated with AFC patch material. The viscoelastic constrained layer is modelled using GHM method. The numerical results shows the improvement in the active damping characteristics of the laminated composite plates over the passive damping for suppressing the geometrically nonlinear transient vibrations of laminated composite plates with AFC as patch material.

  2. Arab Societal Awareness of Dental Veneers.

    Science.gov (United States)

    Alfouzan, Afnan; Al-Sanie, Aisha A; Al-Dhafiri, Reem A

    2018-03-01

    The aim of this study is to assess the Arab society's knowledge, awareness, and attitudes toward dental veneers. A cross-sectional study was performed by collecting data through an online questionnaire created using the Survey Monkey website and distributed among Middle Eastern societies through social media to ascertain participants' knowledge and awareness regarding dental veneers. The sample included Arab laypeople who were over 18 years old, to represent the awareness of the majority regarding dental veneers. The sample of this study included 1,332 subjects from different Middle Eastern nationalities, mainly Saudis, Kuwaitis, and Emiratis (15.6% of males and 84.4% of females). The results of this study showed that the total knowledge of dental veneers is 50.12%. The respondents with the highest level of knowledge acquired their information mainly from newspapers and magazines, followed by the Internet, then dentists, then social media, and, finally, friends and relatives. Cost was the only factor limiting 38.4% of subjects from receiving veneers, and 56% of the subjects would receive veneers if they were free of cost. In total, 72.6% of the respondents believed that veneers are currently overused. The knowledge and awareness of dental veneers were below a satisfactory level. Participants who relied on social media as a source of information had lower knowledge levels. This study emphasized the need for continual societal education regarding dental veneers.

  3. A low frequency vibration energy harvester using magnetoelectric laminate composite

    International Nuclear Information System (INIS)

    Ju, Suna; Chae, Song Hee; Choi, Yunhee; Lee, Seungjun; Ji, Chang-Hyeon; Lee, Hyang Woon

    2013-01-01

    In this paper, we present a vibration energy harvester using magnetoelectric laminate composite and a springless spherical permanent magnet as a proof mass. The harvester utilizes a freely movable spherical permanent magnet to transform external vibration into a time varying magnetic field applied to the magnetoelectric transducer. The laminate composite consists of a Ni–Mn–Ga-based MSMA (magnetic shape memory alloy) element and a PZT (lead zirconate titanate) plate. A proof-of-concept harvester has been fabricated and characterized at various input accelerations and frequencies. A maximum open circuit voltage of 1.18 V has been obtained in response to a 3g vibration at 17 Hz with the fabricated device. Moreover, a maximum output voltage of 10.24 V and output power of 4.1 μW have been achieved on a 950 Ω load, when the fabricated energy harvester was mounted on a smartphone and shaken by hand. (paper)

  4. Mechanical behavior of glass/epoxy composite laminate with varying amount of MWCNTs under different loadings

    Science.gov (United States)

    Singh, K. K.; Rawat, Prashant

    2018-05-01

    This paper investigates the mechanical response of three phased (glass/MWCNTs/epoxy) composite laminate under three different loadings. Flexural strength, short beam strength and low-velocity impact (LVI) testing are performed to find an optimum doping percentage value for maximum enhancement in mechanical properties. In this work, MWCNTs were used as secondary reinforcement for three-phased composite plate. MWCNT doping was done in a range of 0–4 wt% of the thermosetting matrix system. Symmetrical design eight layered glass/epoxy laminate with zero bending extension coupling laminate was fabricated using a hybrid method i.e. hand lay-up technique followed by vacuum bagging method. Ranging analysis of MWCNT mixing highlighted the enhancement in flexural, short beam strength and improvement in damage tolerance under LVI loading. While at higher doping wt%, agglomeration of MWCNTs are observed. Results of mechanical testing proposed an optimized doping value for maximum strength and damage resistance of the laminate.

  5. Ply-based Optimization of Laminated Composite Shell Structures under Manufacturing Constraints

    DEFF Research Database (Denmark)

    Sørensen, Rene; Lund, Erik

    2012-01-01

    This work concerns a new ply-based parameterization for performing simultaneous material selection and topology optimization of fiber reinforced laminated composite structures while ensuring that a series of different manufacturing constraints are fulfilled. The material selection can either...

  6. High energy ballistic and fracture comparison between multilayered armor systems using non-woven curaua fabric composites and aramid laminates

    Directory of Open Access Journals (Sweden)

    Fábio de Oliveira Braga

    2017-10-01

    Full Text Available For personal protection against high kinetic energy projectiles, multilayered armor systems (MAS are usually the best option. They combine synergistically the properties of different materials such as ceramics, composites and metals. In the present work, ballistic tests were performed to evaluate multilayered armor systems (MAS using curaua non-woven fabric epoxy composites as second layer. A comparison to a MAS using aramid (Kevlar™ fabric laminates was made. The results showed that the curaua non-woven fabric composites are suitable to the high ballistic applications, and are promising substitutes for aramid fabric laminates. Keywords: Composite, Natural fiber, Curaua fiber, Non-woven fabric, Aramid laminate, Ballistic test

  7. Analysis of Thermo-Acoustic Emission from Damage in Composite Laminates under Thermal Cyclic Loading

    International Nuclear Information System (INIS)

    Kim, Young Bok; Min, Dae Hong; Lee, Deok Bo; Choi, Nak Sam

    2001-01-01

    An investigation on nondestructive evaluation of thermal stress-reduced damage in the composite laminates (3mm in thickness and [+45 6 /-45 6 ] S lay-up angles) has been performed using the thermo-acoustic emission technique. Reduction of thermo-AE events due to repetitive thermal load cycles showed a Kaiser effect. An analysis of the thermo-AE behavior determined the stress free temperature of composite laminates. Fiber fracture and matrix cracks were observed using the optical microscopy, scanning electron microscopy and ultrasonic C-sean. Short-Time Fourier Transform of thermo-AE signals offered the time-frequency characteristics which might classify the thermo-AE as three different types to estimate the damage processes of the composites

  8. Damping mathematical modelling and dynamic responses for FRP laminated composite plates with polymer matrix

    Science.gov (United States)

    Liu, Qimao

    2018-02-01

    This paper proposes an assumption that the fibre is elastic material and polymer matrix is viscoelastic material so that the energy dissipation depends only on the polymer matrix in dynamic response process. The damping force vectors in frequency and time domains, of FRP (Fibre-Reinforced Polymer matrix) laminated composite plates, are derived based on this assumption. The governing equations of FRP laminated composite plates are formulated in both frequency and time domains. The direct inversion method and direct time integration method for nonviscously damped systems are employed to solve the governing equations and achieve the dynamic responses in frequency and time domains, respectively. The computational procedure is given in detail. Finally, dynamic responses (frequency responses with nonzero and zero initial conditions, free vibration, forced vibrations with nonzero and zero initial conditions) of a FRP laminated composite plate are computed using the proposed methodology. The proposed methodology in this paper is easy to be inserted into the commercial finite element analysis software. The proposed assumption, based on the theory of material mechanics, needs to be further proved by experiment technique in the future.

  9. Design Optimization of Laminated Composite Structures with Many Local Strength Criteria

    DEFF Research Database (Denmark)

    Lund, Erik

    2012-01-01

    This paper presents different strategies for handling very many local strength criteria in structural optimization of laminated composites. Global strength measures using Kreisselmeier-Steinhauser or p-norm functions are introduced for patch-wise parameterizations, and the efficiency of the metho...

  10. Statistical damage analysis of transverse cracking in high temperature composite laminates

    International Nuclear Information System (INIS)

    Sun Zuo; Daniel, I.M.; Luo, J.J.

    2003-01-01

    High temperature polymer composites are receiving special attention because of their potential applications to high speed transport airframe structures and aircraft engine components exposed to elevated temperatures. In this study, a statistical analysis was used to study the progressive transverse cracking in a typical high temperature composite. The mechanical properties of this unidirectional laminate were first characterized both at room and high temperatures. Damage mechanisms of transverse cracking in cross-ply laminates were studied by X-ray radiography at room temperature and in-test photography technique at high temperature. Since the tensile strength of unidirectional laminate along transverse direction was found to follow Weibull distribution, Monte Carlo simulation technique based on experimentally obtained parameters was applied to predict transverse cracking at different temperatures. Experiments and simulation showed that they agree well both at room temperature and 149 deg. C (stress free temperature) in terms of applied stress versus crack density. The probability density function (PDF) of transverse crack spacing considering statistical strength distribution was also developed, and good agreements with simulation and experimental results are reached. Finally, a generalized master curve that predicts the normalized applied stress versus normalized crack density for various lay-ups and various temperatures was established

  11. Analysis of spring-in in U-shaped composite laminates: Numerical and experimental results

    Science.gov (United States)

    Bellini, Costanzo; Sorrentino, Luca; Polini, Wilma; Parodo, Gianluca

    2018-05-01

    The phenomena that happen during the cure process of a composite material laminate are responsible for the rise of residual stresses and, consequently, for the deformation at the end of the manufacturing process. The most analyzed deformation is the spring-in, that represent the flange-to-flange angle deviance from the theoretical value. In this work, the influence of some parameters, such as the laminate thickness, the stacking sequence and the mold radius, on the spring-in angle of a U-shaped laminate was studied exploring a full factorial plan through numerical simulations. First of all, a numerical model proper for cure simulation was introduced and its suitability to simulate the deformation behavior was demonstrated. As a result, only the stacking sequence influenced the spring-in value, while the effect of the tool radius and laminate thickness was minimal.

  12. Autoclave processing for composite material fabrication. 1: An analysis of resin flows and fiber compactions for thin laminate

    Science.gov (United States)

    Hou, T. H.

    1985-01-01

    High quality long fiber reinforced composites, such as those used in aerospace and industrial applications, are commonly processed in autoclaves. An adequate resin flow model for the entire system (laminate/bleeder/breather), which provides a description of the time-dependent laminate consolidation process, is useful in predicting the loss of resin, heat transfer characteristics, fiber volume fraction and part dimension, etc., under a specified set of processing conditions. This could be accomplished by properly analyzing the flow patterns and pressure profiles inside the laminate during processing. A newly formulated resin flow model for composite prepreg lamination process is reported. This model considers viscous resin flows in both directions perpendicular and parallel to the composite plane. In the horizontal direction, a squeezing flow between two nonporous parallel plates is analyzed, while in the vertical direction, a poiseuille type pressure flow through porous media is assumed. Proper force and mass balances have been made and solved for the whole system. The effects of fiber-fiber interactions during lamination are included as well. The unique features of this analysis are: (1) the pressure gradient inside the laminate is assumed to be generated from squeezing action between two adjacent approaching fiber layers, and (2) the behavior of fiber bundles is simulated by a Finitely Extendable Nonlinear Elastic (FENE) spring.

  13. Properties of composite laminates based on basalt fibers with epoxidized vegetable oils

    International Nuclear Information System (INIS)

    Samper, M.D.; Petrucci, R.; Sanchez-Nacher, L.; Balart, R.; Kenny, J.M.

    2015-01-01

    Highlights: • New environmentally friendly composites from biobased epoxies and basalt fibers. • Improved performance with conventional silane treatment on basalt fabrics. • Composites with excellent appearance due to basalt shiny brown color. • Potential applications as substitute of glass fiber reinforced composites in engineering design. • Processing with conventional resin transfer molding (RTM) techniques. - Abstract: This paper deals with the development of polymeric materials derived from epoxidized vegetable oils which have been used in the manufacture of laminated composite materials with basalt fabrics. Epoxidized linseed oil (ELO) and epoxidized soybean oil (ESBO) were used as biobased matrices. The basalt fabrics were modified with amino-silane and glycidyl-silane to increase fiber–matrix interactions. The curing behavior of both resins was evaluated by differential scanning calorimetry (DSC) and oscillatory rheometry (OR). The evaluation of mechanical properties was made by tensile, flexural and Charpy tests. The extent of the fiber–matrix interactions among interface was evaluated by scanning electron microscopy (SEM). The obtained results revealed that surface modification of basalt fibers with glycidyl-silane clearly improves the mechanical properties of the composites. The use of the ELO resin as matrix for composite laminates improved substantially the mechanical performance compared to composites made with ESBO

  14. Towards mechanisms-guided resistivity-based monitoring of damage evolution in laminated composites

    KAUST Repository

    Lubineau, Gilles; Nouri, Hedi; Selvakumaran, Lakshmi

    2013-01-01

    A convenient health monitoring technique for detecting degradation in laminated composite is to monitor the change of electrical resistance along multiple conduction paths within the structure. Yet, the relations between the global modification

  15. Western hemlock as a veneer resource.

    Science.gov (United States)

    Thomas D. Fahey; Jr. Woodfin

    1982-01-01

    Presents recovery of veneer grade and volume from western hemlock from Oregon and Washington. Veneer grade recovery varied by grade and size of logs. Veneer volume recovered was about 45 percent of the cubic volume of the log and varied somewhat with log diameter.

  16. Theoretical modeling and experimental analyses of laminated wood composite poles

    Science.gov (United States)

    Cheng Piao; Todd F. Shupe; Vijaya Gopu; Chung Y. Hse

    2005-01-01

    Wood laminated composite poles consist of trapezoid-shaped wood strips bonded with synthetic resin. The thick-walled hollow poles had adequate strength and stiffness properties and were a promising substitute for solid wood poles. It was necessary to develop theoretical models to facilitate the manufacture and future installation and maintenance of this novel...

  17. Experimental verification of a progressive damage model for composite laminates based on continuum damage mechanics. M.S. Thesis Final Report

    Science.gov (United States)

    Coats, Timothy William

    1994-01-01

    Progressive failure is a crucial concern when using laminated composites in structural design. Therefore the ability to model damage and predict the life of laminated composites is vital. The purpose of this research was to experimentally verify the application of the continuum damage model, a progressive failure theory utilizing continuum damage mechanics, to a toughened material system. Damage due to tension-tension fatigue was documented for the IM7/5260 composite laminates. Crack density and delamination surface area were used to calculate matrix cracking and delamination internal state variables, respectively, to predict stiffness loss. A damage dependent finite element code qualitatively predicted trends in transverse matrix cracking, axial splits and local stress-strain distributions for notched quasi-isotropic laminates. The predictions were similar to the experimental data and it was concluded that the continuum damage model provided a good prediction of stiffness loss while qualitatively predicting damage growth in notched laminates.

  18. Sound Insulation Property Study on Nylon 66 Scrim Reinforced PVF Laminated Membranes and their Composite Sound Proof Structure

    Science.gov (United States)

    Chen, Lihe; Chen, Zhaofeng; Zhang, Xinyang; Wang, Weiwei

    2018-01-01

    In this paper, we investigated the sound insulation property of nylon 66 scrim reinforced PVF laminated membranes and their corresponding composite structures with glass fiber felt and carbon fiber board. Sound transmission loss (STL) was measured by standing wave tube method. The results show that, with the decrease of nylon 66 gridlines spacing, STL of nylon 66 scrim reinforced PVF laminated membranes was improved. The sound insulation performance of laminated membranes with gridlines spacing of 3mm is the best, whose STL was up to 10dB at 6.3 kHz. Besides, STL was improved effectively as air layers were embedded into the composite sound proof construction consist of laminated membrane, glass fiber felt and carbon fiber board.

  19. Large deflection analysis of laminated composite plates resting on nonlinear elastic foundations by the method of discrete singular convolution

    International Nuclear Information System (INIS)

    Baltacioglu, A.K.; Civalek, O.; Akgoez, B.; Demir, F.

    2011-01-01

    This paper presents nonlinear static analysis of a rectangular laminated composite thick plate resting on nonlinear two-parameter elastic foundation with cubic nonlinearity. The plate formulation is based on first-order shear deformation theory (FSDT). The governing equation of motion for a rectangular laminated composite thick plate is derived by using the von Karman equation. The nonlinear static deflections of laminated plates on elastic foundation are investigated using the discrete singular convolution method. The effects of foundation and geometric parameters of plates on nonlinear deflections are investigated. The validity of the present method is demonstrated by comparing the present results with those available in the literature. - Highlights: → Large deflection analysis of laminated composite plates are investigated. → As foundation, nonlinear elastic models have been used firstly. → The effects of three-parameter foundation are investigated in detail.

  20. Damping mathematical modelling and dynamic responses for FRP laminated composite plates with polymer matrix

    Directory of Open Access Journals (Sweden)

    Liu Qimao

    2018-02-01

    Full Text Available This paper proposes an assumption that the fibre is elastic material and polymer matrix is viscoelastic material so that the energy dissipation depends only on the polymer matrix in dynamic response process. The damping force vectors in frequency and time domains, of FRP (Fibre-Reinforced Polymer matrix laminated composite plates, are derived based on this assumption. The governing equations of FRP laminated composite plates are formulated in both frequency and time domains. The direct inversion method and direct time integration method for nonviscously damped systems are employed to solve the governing equations and achieve the dynamic responses in frequency and time domains, respectively. The computational procedure is given in detail. Finally, dynamic responses (frequency responses with nonzero and zero initial conditions, free vibration, forced vibrations with nonzero and zero initial conditions of a FRP laminated composite plate are computed using the proposed methodology. The proposed methodology in this paper is easy to be inserted into the commercial finite element analysis software. The proposed assumption, based on the theory of material mechanics, needs to be further proved by experiment technique in the future.

  1. The effect of bulk-resin CNT-enrichment on damage and plasticity in shear-loaded laminated composites

    KAUST Repository

    Ventura, Isaac Aguilar

    2013-07-01

    One way to improve multi functionality of epoxy-based laminated composites is to dope the resin with carbon nanotubes. Many investigators have focused on the elastic and fracture behavior of such nano-modified polymers under tensile loading. Yet, in real structural applications, laminated composites can exhibit plasticity and progressive damage initiated mainly by shear loading. We investigated the damage and plasticity induced by the addition of carbon nanotubes to the matrix of a glass fiber/epoxy composite system. We characterized both the modified epoxy resin and the associated modified laminates using classical mesoscale analysis. We used dynamic mechanical analysis, scanning electron microscopy, atomic force microscopy and classical mechanical testing to characterize samples with different concentrations of nanofillers. Since the samples were prepared using the solvent evaporation technique, we also studied the influence of this process. We found that in addition to the global increase in elastic regime properties, the addition of carbon nanotubes also accelerates the damage process in both the bulk resin and its associated glass-fiber composite. © 2013 Elsevier Ltd.

  2. On micro-meso relations homogenizing electrical properties of transversely cracked laminated composites

    KAUST Repository

    Lubineau, Gilles; Nouri, Hedi; Roger, Frederic

    2013-01-01

    A practical way to track the development of transverse cracking in a laminated composite is to monitor the change of its electrical resistance. Yet, the relations between transverse cracking and the global modification of resistivity is still

  3. Tensile and compressive failure modes of laminated composites loaded by fatigue with different mean stress

    Science.gov (United States)

    Rotem, Assa

    1990-01-01

    Laminated composite materials tend to fail differently under tensile or compressive load. Under tension, the material accumulates cracks and fiber fractures, while under compression, the material delaminates and buckles. Tensile-compressive fatigue may cause either of these failure modes depending on the specific damage occurring in the laminate. This damage depends on the stress ratio of the fatigue loading. Analysis of the fatigue behavior of the composite laminate under tension-tension, compression-compression, and tension-compression had led to the development of a fatigue envelope presentation of the failure behavior. This envelope indicates the specific failure mode for any stress ratio and number of loading cycles. The construction of the fatigue envelope is based on the applied stress-cycles to failure (S-N) curves of both tensile-tensile and compressive-compressive fatigue. Test results are presented to verify the theoretical analysis.

  4. Vibration Analysis of Inclined Laminated Composite Beams under Moving Distributed Masses

    Directory of Open Access Journals (Sweden)

    E. Bahmyari

    2014-01-01

    Full Text Available The dynamic response of laminated composite beams subjected to distributed moving masses is investigated using the finite element method (FEM based on the both first-order shear deformation theory (FSDT and the classical beam theory (CLT. Six and ten degrees of freedom beam elements are used to discretize the CLT and FSDT equations of motion, respectively. The resulting spatially discretized beam governing equations including the effect of inertial, Coriolis, and centrifugal forces due to moving distributed mass are evaluated in time domain by applying Newmark’s scheme. The presented approach is first validated by studying its convergence behavior and comparing the results with those of existing solutions in the literature. Then, the effect of incline angle, mass, and velocity of moving body, layer orientation, load length, and inertial, Coriolis, and centrifugal forces due to the moving distributed mass and friction force between the beam and the moving distributed mass on the dynamic behavior of inclined laminated composite beams are investigated.

  5. Evaluation of a novel multiple phase veneering ceramic.

    Science.gov (United States)

    Sinthuprasirt, Pannapa; van Noort, Richard; Moorehead, Robert; Pollington, Sarah

    2015-04-01

    To produce a new veneering ceramic based on the production of a multiple phase glass-ceramic with improved performance in terms of strength and toughness. A composition of 60% leucite, 20% diopside and 20% feldspathic glass was prepared, blended and a heat treatment schedule of 930°C for 5 min was derived from differential thermal analysis (DTA) of the glasses. X-ray diffraction (XRD) and SEM analysis determined the crystalline phases and microstructure. Chemical solubility, biaxial flexural strength (BFS), fracture toughness, hardness, total transmittance and coefficient of thermal expansion (CTE) were all measured in comparison to a commercial veneering ceramic (VITA VM9). Thermal shock resistance of the leucite-diopside and VITA VM9 veneered onto a commercial high strength zirconia (Vita In-Ceram YZ) was also assessed. Statistical analysis was undertaken using Independent Samples t-test. Weibull analysis was employed to examine the reliability of the strength data. The mean chemical solubility was 6 μg/cm(2) for both ceramics (P=1.00). The mean BFS was 109 ± 8 MPa for leucite-diopside ceramic and 79 ± 11 MPa for VITA VM9 ceramic (P=0.01). Similarly, the leucite-diopside ceramic demonstrated a significantly higher fracture toughness and hardness. The average total transmittance was 46.3% for leucite-diopside ceramic and 39.8% for VITA VM9 (P=0.01). The leucite-diopside outperformed the VITA VM9 in terms of thermal shock resistance. Significance This novel veneering ceramic exhibits significant improvements in terms of mechanical properties, yet retains a high translucency and is the most appropriate choice as a veneering ceramic for a zirconia base core material. Copyright © 2015 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

  6. Deformation behavior of an electrodeposited nano-Ni/amorphous Fe78Si9B13 laminated composite sheet

    Directory of Open Access Journals (Sweden)

    Zhang Kaifeng

    2015-01-01

    Full Text Available A nano-Ni/amorphous Fe78Si9B13 composite sheet was prepared in the form of three-ply (Ni-Fe78Si9B13-Ni laminated structure by an electrodeposition method. The average grain size of Ni layers is about 50 nm. The interface of laminated composite was investigated with SEM equipped with energy dispersive scanning (EDS and line analysis technique. The laminated composite has a good interfacial bonding between amorphous layer and nano-Ni layers due to the mutual diffusion of atoms in Fe78Si9B13 and Ni layers during the process of electrodeposition. A maximum elongation of 115.5% was obtained when the volume fraction of nano-Ni layers (VNi was 0.77, which is greatly higher than that of monolithic amorphous Fe78Si9B13 ribbon (36.3% tested under the same conditions. Bulging tests were carried out to evaluate plastic forming properties of the Fe78Si9B13/Ni laminated composite. Under the condition of 450 °C, 4.0 MPa and 30 min, a good bulging part with the relative bulging height (RBH of 0.4 was obtained.

  7. Self-Healing Laminate System

    Science.gov (United States)

    Beiermann, Brett A. (Inventor); Keller, Michael W. (Inventor); White, Scott R. (Inventor); Sottos, Nancy R. (Inventor)

    2016-01-01

    A laminate material may include a first flexible layer, and a self-healing composite layer in contact with the first flexible layer. The composite layer includes an elastomer matrix, a plurality of first capsules including a polymerizer, and a corresponding activator for the polymerizer. The laminate material may self-heal when subjected to a puncture or a tear.

  8. Fracture strengths of chair‑side‑generated veneers cemented with ...

    African Journals Online (AJOL)

    2014-06-09

    Jun 9, 2014 ... Group 1), CAD/CAM‑fabricated veneers cemented with a glass fiber ... specimens were tested with a universal testing machine after thermal cycling treatment. ... The purpose of the current in vitro study is to determine the ..... fracture resistance of fiber reinforced cups‑replacing composite restorations.

  9. Microcracking in composite laminates under thermal and mechanical loading. Thesis

    Science.gov (United States)

    Maddocks, Jason R.

    1995-01-01

    Composites used in space structures are exposed to both extremes in temperature and applied mechanical loads. Cracks in the matrix form, changing the laminate thermoelastic properties. The goal of the present investigation is to develop a predictive methodology to quantify microcracking in general composite laminates under both thermal and mechanical loading. This objective is successfully met through a combination of analytical modeling and experimental investigation. In the analysis, the stress and displacement distributions in the vicinity of a crack are determined using a shear lag model. These are incorporated into an energy based cracking criterion to determine the favorability of crack formation. A progressive damage algorithm allows the inclusion of material softening effects and temperature-dependent material properties. The analysis is implemented by a computer code which gives predicted crack density and degraded laminate properties as functions of any thermomechanical load history. Extensive experimentation provides verification of the analysis. AS4/3501-6 graphite/epoxy laminates are manufactured with three different layups to investigate ply thickness and orientation effects. Thermal specimens are cooled to progressively lower temperatures down to -184 C. After conditioning the specimens to each temperature, cracks are counted on their edges using optical microscopy and in their interiors by sanding to incremental depths. Tensile coupons are loaded monotonically to progressively higher loads until failure. Cracks are counted on the coupon edges after each loading. A data fit to all available results provides input parameters for the analysis and shows them to be material properties, independent of geometry and loading. Correlation between experiment and analysis is generally very good under both thermal and mechanical loading, showing the methodology to be a powerful, unified tool. Delayed crack initiation observed in a few cases is attributed to a

  10. Assessment of various failure theories for weight and cost optimized laminated composites using genetic algorithm

    Energy Technology Data Exchange (ETDEWEB)

    Goyal, T. [Indian Institute of Technology Kanpur. Dept. of Aerospace Engineering, UP (India); Gupta, R. [Infotech Enterprises Ltd., Hyderabad (India)

    2012-07-01

    In this work, minimum weight-cost design for laminated composites is presented. A genetic algorithm has been developed for the optimization process. Maximum-Stress, Tsai-Wu and Tsai-Hill failure criteria have been used along with buckling analysis parameter for the margin of safety calculations. The design variables include three materials; namely Carbon-Epoxy, Glass-Epoxy, Kevlar-Epoxy; number of plies; ply orientation angles, varying from -75 deg. to 90 deg. in the intervals of 15 deg. and ply thicknesses which depend on the material in use. The total cost is a sum of material cost and layup cost. Layup cost is a function of the ply angle. Validation studies for solution convergence and weight-cost inverse proportionality are carried out. One set of results for shear loading are also validated from literature for a particular case. A Pareto-Optimal solution set is demonstrated for biaxial loading conditions. It is then extended to applied moments. It is found that global optimum for a given loading condition is a function of the failure criteria for shear loading, with Maximum Stress criteria giving the lightest-cheapest and Tsai-Wu criteria giving the heaviest-costliest optimized laminates. Optimized weight results are plotted from the three criteria to do a comparative study. This work gives a global optimized laminated composite and also a set of other local optimum laminates for a given set of loading conditions. The current algorithm also provides with adequate data to supplement the use of different failure criteria for varying loadings. This work can find use in the industry and/or academia considering the increased use of laminated composites in modern wind blades. (Author)

  11. A review of strategies for improving the degradation properties of laminated continuous-fiber/epoxy composites with carbon-based nanoreinforcements

    KAUST Repository

    Lubineau, Gilles

    2012-06-01

    Continuous-fiber/epoxy-matrix laminated composites are a key structural material for aeronautical and aerospace applications. Introducing nanoscale reinforcements to these materials is a possible way to achieve improved mechanical properties. To date, much work has been done on nano-reinforced polymers. However, few systematic studies concerning the effect of the nanoreinforcements on the mechanical properties on laminated composites were conducted. This paper presents a systematic review of the mechanisms of degradation in laminated structures and considers various nanoreinforcement strategies in the light of well-known mechanisms of degradation and phenomenologies in classical laminated composites. We also discuss various nanoreinforcement strategies in terms of their potential to reduce degradation on every scale. In addition, we review studies conducted on the role that nanoreinforcements play in mechanical properties involved in structural simulation and design. The degradation mechanisms are systematically considered to provide a full picture of each reinforcement strategy. © 2012 Elsevier Ltd. All rights reserved.

  12. Ceramic (Feldspathic & IPS Empress II) vs. laboratory composite (Gradia) veneers; a comparison between their shear bond strength to enamel; an in vitro study.

    Science.gov (United States)

    Nikzad, S; Azari, Abbas; Dehgan, S

    2010-07-01

    Patient demand for aesthetic dentistry is steadily growing. Laminates and free metal restorations have evolved in an attempt to overcome the invasiveness nature of full veneer restorations. Although many different materials have been used for making these restorations, there is no single material that fits best for all purposes. Two groups of ceramic material (Feldspathic and IPS Empress II) and one group of laboratory composite (Gradia) discs (10 discs in each group; 4 mm in diameter and 2 mm in thickness) were prepared according to the manufacturer's instruction. The surface of ceramic discs were etched and silanized. In Gradia group, liquid primer was applied on composite surfaces. Thirty freshly extracted sound human molars and premolars were randomly divided into three groups. The enamel surface of each tooth was slightly flattened (0.3 mm) on the buccal or lingual side and then primed and cemented to the prepared discs with the aid of a dental surveyor. The finishing specimens were thermocycled between 5 degrees C and 55 degrees C for 2500 cycles and then prepared for shear bond strength testing. The resulting data were analyzed by one-way anova and Tukey HSD test. The fractured surfaces of each specimen were inspected by means of stereomicroscope and SEM. There is significant difference between the bond strength of materials tested. The mean bond strengths obtained with Feldspathic ceramic, IPS Empress II and Gradia were 33.10 +/- 4.31 MPa, 26.04 +/- 7.61 MPa and 14.42 +/- 5.82 MPa, respectively. The fracture pattern was mainly mixed for ceramic groups. More scientific evidence needed for standardization of bonding protocols.

  13. Estimate of compressive strength of an unidirectional composite lamina using cross-ply and angle-ply laminates

    Directory of Open Access Journals (Sweden)

    M. Scafè

    2014-07-01

    Full Text Available In this work has been estimated the compressive strength of a unidirectional lamina of a carbon/epoxy composite material, using the cross-ply and angle-ply laminates. Over the years various methods have been developed to deduce compressive properties of composite materials reinforced with long fibres. Each of these methods is characterized by a specific way of applying load to the specimen. The method chosen to perform the compression tests is the Wyoming Combined Loading Compression (CLC Test Method, described in ASTM D 6641 / D 6641M-09. This method presents many advantages, especially: the load application on the specimen (end load combined with shear load, the reproducibility of measurements and the experimental equipment quite simplified. Six different laminates were tested in compressive tests. They were realized by the same unidirectional prepreg, but with different stacking sequences: two cross-ply [0/90]ns, two angle-ply [0/90/±45]ns and two unidirectional laminates [0]ns and [90]ns. The estimate of the compressive strength of the unidirectional laminates at 0°, was done by an indirect analytical method, developed from the classical lamination theory, and which uses a multiplicative parameter known as Back-out Factor (BF. The BF is determined by using the experimental values obtained from compression tests.

  14. Free material stiffness design of laminated composite structures using commercial finite element analysis codes

    DEFF Research Database (Denmark)

    Henrichsen, Søren Randrup; Lindgaard, Esben; Lund, Erik

    2015-01-01

    In this work optimum stiffness design of laminated composite structures is performed using the commercially available programs ANSYS and MATLAB. Within these programs a Free Material Optimization algorithm is implemented based on an optimality condition and a heuristic update scheme. The heuristic...... update scheme is needed because commercially available finite element analysis software is used. When using a commercial finite element analysis code it is not straight forward to implement a computationally efficient gradient based optimization algorithm. Examples considered in this work are a clamped......, where full access to the finite element analysis core is granted. This comparison displays the possibility of using commercially available programs for stiffness design of laminated composite structures....

  15. Thermoelastic wave propagation in laminated composites plates

    Directory of Open Access Journals (Sweden)

    Verma K. L.

    2012-12-01

    Full Text Available The dispersion of thermoelastic waves propagation in an arbitrary direction in laminated composites plates is studied in the framework of generalized thermoelasticity in this article. Three dimensional field equations of thermoelasticity with relaxation times are considered. Characteristic equation is obtained on employing the continuity of displacements, temperature, stresses and thermal gradient at the layers’ interfaces. Some important particular cases such as of free waves on reducing plates to single layer and the surface waves when thickness tends to infinity are also discussed. Uncoupled and coupled thermoelasticity are the particular cases of the obtained results. Numerical results are also obtained and represented graphically.

  16. Effect of core/veneer thickness ratio and veneer translucency on absolute and relative translucency of CAD-On restorations

    Directory of Open Access Journals (Sweden)

    Mennatallah Mohie el-Din Wahba, (BDS, MSc

    2017-06-01

    Conclusions: Only veneer translucency had significant effect over contrast ratio values, while on the other hand, absolute translucency values were significantly affected by the core/veneer thickness ratio, veneer translucency and interaction between them. It was clear that absolute translucency measurements showed higher translucency values for the restorations than contrast ratio measurements.

  17. [Wear intensity and surface roughness of microhybrid composite and ceramic occlusal veneers on premolars after the thermocycling and cyclic mechanical loading tests].

    Science.gov (United States)

    Zhang, H Y; Jiang, T; Cheng, M X; Zhang, Y W

    2018-02-18

    To evaluate the wear intensity and surface roughness of occlusal veneers on premolars made of microhybrid composite resin or two kinds of ceramics in vitro after the thermocycling and cyclic mechanical loading tests. In the study,24 fresh extracted human premolars without root canal treatment were prepared (cusps reduction of 1.5 mm in thickness to simulate middle to severe tooth wear, the inclinations of cusps were 20°). The prepared teeth were restored with occlusal veneers made of three different materials: microhybrid composite, heat-pressed lithium disilicate ceramic and computer-aided design/computer-aided manufacturing (CAD/CAM) lithium disilicate ceramic in the thickness of 1.5 mm. The occlusal veneers were cemented with resin cement. The specimens were fatigued using the thermocycling and cyclic mechanical loading tests after being stored in water for 72 h. The wear of specimens was measured using gypsum replicas and 3D laser scanner before and after the thermocycling and cyclic mechanical loading tests and the mean lost distance (mm) was used to indicate the level of wear. The surfaces of occlusal contact area were observed and the surface roughness was recorded using 3D laser scanning confocal microscope before and after the fatigue test. Differences between the groups were compared using ONE-way ANOVA(Pcomposite group, heat-pressed lithium disilicate ceramic group, and CAD/CAM lithium disilicate ceramic group was (-0.13±0.03) mm, (-0.05±0.01) mm and (-0.05±0.01) mm, the wear of microhybrid composite was significantly higher than the two ceramic groups(Pcomposite was significantly higher than the two ceramic groups(Pcomposite(P=0.005) and CAD/CAM lithium disilicate ceramic (P=0.010). From the view of wear speed, microhybrid composite was significantly higher than the two kinds of ceramics, but it was similar to enamel when the opposing tooth was natural. The surface roughness before the themocycling and cyclic mechanical loading test of microhybrid

  18. Static and dynamic strain energy release rates in toughened thermosetting composite laminates

    Science.gov (United States)

    Cairns, Douglas S.

    1992-01-01

    In this work, the static and dynamic fracture properties of several thermosetting resin based composite laminates are presented. Two classes of materials are explored. These are homogeneous, thermosetting resins and toughened, multi-phase, thermosetting resin systems. Multi-phase resin materials have shown enhancement over homogenous materials with respect to damage resistance. The development of new dynamic tests are presented for composite laminates based on Width Tapered Double Cantilevered Beam (WTDCB) for Mode 1 fracture and the End Notched Flexure (ENF) specimen. The WTDCB sample was loaded via a low inertia, pneumatic cylinder to produce rapid cross-head displacements. A high rate, piezo-electric load cell and an accelerometer were mounted on the specimen. A digital oscilloscope was used for data acquisition. Typical static and dynamic load versus displacement plots are presented. The ENF specimen was impacted in three point bending with an instrumented impact tower. Fracture initiation and propagation energies under static and dynamic conditions were determined analytically and experimentally. The test results for Mode 1 fracture are relatively insensitive to strain rate effects for the laminates tested in this study. The test results from Mode 2 fracture indicate that the toughened systems provide superior fracture initiation and higher resistance to propagation under dynamic conditions. While the static fracture properties of the homogeneous systems may be relatively high, the apparent Mode 2 dynamic critical strain energy release rate drops significantly. The results indicate that static Mode 2 fracture testing is inadequate for determining the fracture performance of composite structures subjected to conditions such as low velocity impact. A good correlation between the basic Mode 2 dynamic fracture properties and the performance is a combined material/structural Compression After Impact (CAI) test is found. These results underscore the importance of

  19. INFLUENCE OF SILANE HEAT TREATMENT ON THE TENSILE BOND STRENGTH BETWEEN EX-3 SYNTHETIC VENEERING PORCELAIN AND COMPOSITE RESIN USING FIVE DIFFERENT ACTIVATION TEMPERATURES

    Directory of Open Access Journals (Sweden)

    Spartak Yanakiev

    2017-02-01

    Full Text Available Purpose: The purpose of the present study is to assess the effect of five different silane activation temperatures and eight activation methods on the tensile bond strength between one veneering porcelain and one composite resin material. Material and methods: A total of 81 ceramic rods were made of EX-3 veneering ceramic (Kuraray Noritake Dental, Japan. Sintered ceramic bars were grinded with diamond disks to size 10x2x2mm ± 0,05mm. The front part of each bar was polished. After ultrasonic cleaning in distilled water, the specimens were divided into nine groups. Silane was activated with air at room temperature, 38º С, 50º С, 100º С, 120º С using a custom made blow drier. In a silicone mold, a composite resin Z250 (3М ESPE, St. Paul, USA was condensed toward the bond ceramic surface. A total of 81 specimens approximately 2,0 cm long were prepared for tensile bond testing. One way ANOVA, followed by Bonferroni and Games-Howell tests were used for statistical analysis. Results: The lowest tensile bond strength was observed in the control group (3,51MPa. Group 2 yielded the highest bond strength among all groups (19,54MPa. Silane heat treatment enhanced the bond strength for all treatment methods. Within the polished specimens, the highest bond strength was yielded with warm air at 120ºС (11,31MPa. Conclusion: The most effective method for bonding Z250 composite resin to EX-3 veneering ceramic includes HF etching, silane, and adhesive resin. The most effective heat treatment method for bonding is hot air at 120ºС.

  20. Standard test method for translaminar fracture toughness of laminated and pultruded polymer matrix composite materials

    CERN Document Server

    American Society for Testing and Materials. Philadelphia

    2004-01-01

    1.1 This test method covers the determination of translaminar fracture toughness, KTL, for laminated and pultruded polymer matrix composite materials of various ply orientations using test results from monotonically loaded notched specimens. 1.2 This test method is applicable to room temperature laboratory air environments. 1.3 Composite materials that can be tested by this test method are not limited by thickness or by type of polymer matrix or fiber, provided that the specimen sizes and the test results meet the requirements of this test method. This test method was developed primarily from test results of various carbon fiber – epoxy matrix laminates and from additional results of glass fiber – epoxy matrix, glass fiber-polyester matrix pultrusions and carbon fiber – bismaleimide matrix laminates (1-4, 6, 7). 1.4 A range of eccentrically loaded, single-edge-notch tension, ESE(T), specimen sizes with proportional planar dimensions is provided, but planar size may be variable and adjusted, with asso...

  1. Effect of Sandblasting on Shear Bond Strength Composite Resin Veneer

    Directory of Open Access Journals (Sweden)

    Octarina Octarina

    2013-07-01

    Full Text Available Attachment between restoration and enamel surface in indirect resin composite veneer restoration (IRCV is obtained using multi-step (MS resin cement. Recently, a one step self-adhesive dual-cured resin cement (SADRC was introduced. Objective: To determine the effect of sandblasting on shear bond strength (SBS of IRCV to enamel using MS resin cement and SADRC. Methods: Forty specimens of buccal surface of enamel human were light-cured in Solidilite chamber and were divided into two groups: IRCV without sandblasting (n=20 and with sandblasting for 10 seconds (n=20 and then bonded to enamel using MS (n=10 and SADRC (n=10, respectively. After 24h SBS of specimens were tested using a Universal Testing Machine. Data were analyzed statistically by one-way ANOVA. Results: The average SBS value of IRCV without SB and bonded with MS was 18.95+7.80MPa and MS with SB was 19.30+ SB (4.85+2.12MPa and SADRC with SB (9.57+3.45MPa(p<0.05. Conclusion: increased SBS VIRK to enamel using MS resin cement than SADRC.  

  2. [Veneer computer aided design based on reverse engineering technology].

    Science.gov (United States)

    Liu, Ming-li; Chen, Xiao-dong; Wang, Yong

    2012-03-01

    To explore the computer aided design (CAD) method of veneer restoration, and to assess if the solution can help prosthesis meet morphology esthetics standard. A volunteer's upper right central incisor needed to be restored with veneer. Super hard stone models of patient's dentition (before and after tooth preparation) were scanned with the three-dimensional laser scanner. The veneer margin was designed as butt-to-butt type. The veneer was constructed using reverse engineering (RE) software. The technique guideline of veneers CAD was explore based on RE software, and the veneers was smooth, continuous and symmetrical, which met esthetics construction needs. It was a feasible method to reconstruct veneer restoration based on RE technology.

  3. Analysis of elastic nonlinearity for impact damage detection in composite laminates

    International Nuclear Information System (INIS)

    Frau, A; Porcu, M C; Aymerich, F; Pieczonka, L; Staszewski, W J

    2015-01-01

    This paper concerns the experimental analysis of nonlinear response features of a composite laminate plate for impact damage detection. The measurement procedure is based on the Scaling Subtraction Method (SSM) and consists in exciting the damaged specimen with two sinusoidal signals at different amplitude. The linearly rescaled response signal at low amplitude excitation is subtracted from the response at large amplitude excitation to extract the nonlinear signatures. The latter are analysed in the time domain to infer the presence of damage. Results are compared with frequency domain analyses using the nonlinear vibro-acoustic modulation technique (NWMS). Changes in amplitude and phase as well as modulation effects of the acquired responses are also monitored. Surface-bonded, low profile piezoceramic transducers are used for excitation and sensing. Both measurements techniques are applied to detect barely visible impact damage in laminate composite plate. Non-destructive penetrant-enhanced X-ray inspections are carried out to characterize the extent of internal damage. The behavior of the nonlinear features and the sensitivity of each technique are also investigated in the paper. (paper)

  4. Incorporation of plasma-functionalized carbon nanostructures in composite laminates for interlaminar reinforcement and delamination crack monitoring

    Science.gov (United States)

    Kravchenko, O. G.; Pedrazzoli, D.; Kovtun, D.; Qian, X.; Manas-Zloczower, I.

    2018-01-01

    A new approach employing carbon nanostructure (CNS) buckypapers (BP) was used to prepare glass fiber/epoxy composite materials with enhanced resistance to delamination along with damage monitoring capability. The CNS-BP was subjected to plasma treatment to improve its wettability by epoxy and to promote stronger interfacial bonding. An increase up to 20% in interlaminar fracture toughness in mode I and mode II was observed in composite laminates incorporating CNS BP. Morphological analysis of the fracture surfaces indicated that failure in the conductive CNS layer provided a more effective energy dissipation mechanism, resulting in interlaminar fracture toughness increase. Moreover, fracture of the conductive CNS layer enabled damage monitoring of the composite by electrical resistance measurements upon delamination. The proposed approach provides multifunctional ply interphases, allowing to couple damage monitoring with interlaminar reinforcement of composite laminates.

  5. DESIGN ALTERNATIVES ON THE LAMINATES

    Directory of Open Access Journals (Sweden)

    Gökay Nemli

    2004-04-01

    Full Text Available Wood based panel manufacturers use increasing volumes of laminates. Laminates are resistant to the water, humidity, scratch, abrasion, burning and chemicals. These products consist of printed decor papers that have been saturated with thermosetting resin. In this study, laminate types, composition form and design alternatives were investigated.

  6. Fracture toughness of Ceramic-Fiber-Reinforced Metallic-Intermetallic-Laminate (CFR-MIL) composites

    International Nuclear Information System (INIS)

    Vecchio, Kenneth S.; Jiang, Fengchun

    2016-01-01

    Novel Ceramic-Fiber-Reinforced-Metal-Intermetallic-Laminate (CFR-MIL) composites, Ti–Al 3 Ti–Al 2 O 3 –Al, were synthesized by reactive foil sintering in air. Microstructure controlled material architectures were achieved with continuous Al 2 O 3 fibers oriented in 0° and 90° layers to form fully dense composites in which the volume fractions of all four component phases can be tailored. Bend fracture specimens were cut from the laminate plates in divider orientation, and bend tests were performed to study the fracture behavior of CFR-MIL composites under three-point and four-point bending loading conditions. The microstructures and fractured surfaces of the CFR-MIL composites were examined using optical microscopy and scanning electron microscopy to establish a correlation between the fracture toughness, fracture surface morphology and microstructures of CFR-MIL composites. The fracture and toughening mechanisms of the CFR-MIL composites are also addressed. The present experimental results indicate that the fracture toughness of CFR-MIL composites determined by three- and four-point bend loading configurations are quite similar, and increased significantly compared to MIL composites without ceramic fiber reinforcement. The interface cracking behavior is related to the volume fraction of the brittle Al 3 Ti phase and residual ductile Al, but the fracture toughness values appear to be insensitive to the ratio of these two phases. The toughness appears to be dominated by the ductility/strength of the Ti layers and the strength and crack bridging effect of the ceramic fibers.

  7. Effect of bleaching and repolishing procedures on coffee and tea stain removal from three anterior composite veneering materials.

    Science.gov (United States)

    Türkün, L Sebnem; Türkün, Murat

    2004-01-01

    Discolored teeth can be treated with resin veneers, but their color changes when confronted with staining solutions. Polishing procedures can provide a remedy for highly stained composites, but they tend to remove some materials as well. However, bleaching procedures are an effective, nondestructive method for solving the problem. The aim of this study was to compare the color change of three veneer composites exposed to staining solutions and to evaluate the effectiveness of a 15% hydrogen peroxide bleaching agent and three polishing systems to remove the stain. Forty-five disks (12 x 2 mm) each of Clearfil ST (Kuraray Co. Ltd., Osaka, Japan), Esthet-X (Dentsply/Caulk, Milford DE, USA), and Filtek A110 (3M ESPE, St. Paul, MN, USA) were prepared. The specimens were polished with Sof-Lex (3M ESPE), Enhance (Dentsply/Caulk), or PoGo (Dentsply/Caulk). Five specimens for each material-polishing system combination were immersed in coffee (Nescafe Classic, Nestle SA, Vevey, Switzerland) or tea (Earl Grey, Lipton, Blackfriars-London, England) for 7 days. The remaining disks were stored in water. Color measurements were made with a spectrophotometer (X-Rite Seroice SP78, Loaner, Köln, Germany) at baseline; after 1, 3, 5, and 7 days; and after bleaching and repolishing. After 1 week, one side of the specimens was bleached with Illuminé-office (Dentsply De Trey GmbH, Konstanz, Germany) for 1 hour, and the other side was repolished for 30 seconds. All comparisons of color change for the polishing systems, times, and staining solutions were subjected to repeated measurements of analysis of variance. Paired t-test was used to examine whether significant color differences (deltaE*) occurred during immersion at the specified time intervals (p < or = .05). Filtek A110 was the least stained resin composite. Its color remained under a deltaE* value of 2 during the study. Clearfil ST exhibited the most color change after 1 week. All specimens polished with Enhance showed less

  8. Effects of the shock duration on the response of CFRP composite laminates

    International Nuclear Information System (INIS)

    Gay, Elise; Berthe, Laurent; Boustie, Michel; Arrigoni, Michel; Buzaud, Eric

    2014-01-01

    Shock loads induce a local tensile stress within a sample. The location and amplitude of this high strain rate stress can be monitored respectively by the duration and intensity of the shock. The process is applied to carbon fibre reinforced polymer (CFRP) composites, involved in aeronautic or defense industry. This paper describes the response of CFRP laminates of different thicknesses to a shock load normal to the fibres direction. The effects of the shock duration on the wave propagation are key issues of this work. Experiments have been performed on high power laser facilities and on a high power pulsed generator to get a wide range of pulse duration from fs to µs. Numerical simulation provides a comprehensive approach of the wave propagation and tensile stress generation within these complex materials. The main result concerns the relation between the load duration, the tensile stress and the induced delamination within 1, 4 and 8 ply composite laminates. (paper)

  9. Permeability After Impact Testing of Composite Laminates

    Science.gov (United States)

    Nettles, Alan T.

    2003-01-01

    Since composite laminates are beginning to be identified for use in reusable launch vehicle propulsion systems, an understanding of their permeance is needed. A foreign object impact event can cause a localized area of permeability (leakage) in a polymer matrix composite and it is the aim of this study to assess a method of quantifying permeability-after-impact results. A simple test apparatus is presented and variables that could affect the measured values of permeability-after-impact were assessed. Once it was determined that valid numbers were being measured, a fiber/resin system was impacted at various impact levels and the resulting permeability measured, first with a leak check solution (qualitative) then using the new apparatus (quantitative). The results showed that as the impact level increased, so did the measured leakage. As the pressure to the specimen was increased, the leak rate was seen to increase in a non-linear fashion for almost all of the specimens tested.

  10. Low pressure process for continuous fiber reinforced polyamic acid resin matrix composite laminates

    Science.gov (United States)

    Druyun, Darleen A. (Inventor); Hou, Tan-Hung (Inventor); Kidder, Paul W. (Inventor); Reddy, Rakasi M. (Inventor); Baucom, Robert M. (Inventor)

    1994-01-01

    A low pressure processor was developed for preparing a well-consolidated polyimide composite laminate. Prepreg plies were formed from unidirectional fibers and a polyamic acid resin solution. Molding stops were placed at the sides of a matched metal die mold. The prepreg plies were cut shorter than the length of the mold in the in-plane lateral direction and were stacked between the molding stops to a height which was higher than the molding stops. The plies were then compressed to the height of the stops and heated to allow the volatiles to escape and to start the imidization reaction. After removing the stops from the mold, the heat was increased and 0 - 500 psi was applied to complete the imidization reaction. The heat and pressure were further increased to form a consolidated polyimide composite laminate.

  11. Investigation of the Mechanical Properties of Hybrid Carbon-Hemp Laminated Composites Used as Thermal Insulation for Different Industrial Applications

    Directory of Open Access Journals (Sweden)

    M. L. Scutaru

    2014-04-01

    Full Text Available Carbon-hemp composite laminate provides good thermal properties. For this reason this type of material is presently being used for various applications like insulator for airplanes, spaceships, nuclear reactors, and so forth. Unfortunately their mechanical properties are less studied. These characteristics are very important since they should be guaranteed also for important mechanical stress in addition to the thermal one. The present paper presents a study regarding the impact testing of some hybrid composite laminate panels based on polyester resin reinforced with both carbon and hemp fabric. The effects of different impact speeds on the mechanical behavior of these panels have been analyzed. The paper lays stress on the characterization of this hybrid composite laminate regarding the impact behavior of these panels by dropping a weight with low velocity.

  12. 3D quantification of clinical marginal and internal gap of porcelain laminate veneers with minimal and without tooth preparation and 2-year clinical evaluation.

    Science.gov (United States)

    Karagözoğlu, İrem; Toksavul, Suna; Toman, Muhittin

    2016-01-01

    The aims of this clinical study were to compare internal three-dimensional (3D) adaptation of porcelain laminate veneers (PLV) with minimal tooth preparation and without tooth preparation (prepless) and to evaluate the clinical outcomes at baseline and following 6, 12, and 24 months after luting. Thirty-one prepless PLV and 31 PLV with minimal tooth preparation were fabricated using lithium disilicate glass-ceramic material and placed in 12 patients (8 women, 4 men; 18 to 40 years old). All PLV were luted with an adhesive luting system (Variolink veneer). A silicone replica was obtained to measure internal adaptation of each PLV using a low viscosity polyvinyl siloxane impression material just before luting. Silicone replicas were scanned in x-ray micro computerized tomography (micro CT). Clinical evaluations took place at baseline (2 days after luting) and following 6, 12, and 24 months after luting. Marginal integrity, marginal discoloration, secondary caries, tooth sensitivity, and fracture were evaluated following FDI criteria. Replica scores were analyzed using Mann-Whitney U and Student's t test (α = .05). Kaplan-Meier statistical analysis was done for the survival rate of PLV. FDI criteria scores were analyzed using Pearson's chi-square test (α = .05). The median marginal gaps for PLV-without-tooth-preparation and PLV-with-minimal-tooth-preparation groups were 100 μm and 140 μm respectively. There was a statistically significant difference between the two groups with respect to marginal gap (P = .04). The mean internal adaptation for the PLV-without-tooth-preparation group was 217.17 ± 54.72 μm, and was 170.67 ± 46.54 μm for the PLV-with-minimaltooth- preparation group. There was a statistically significant difference between the two groups (P = .001). Based on FDI criteria, 100% of the PLV were rated satisfactory during the 2-year period. In this in-vivo study, mean and median values of marginal gap and internal adaptation for PLV with minimal tooth

  13. Numerical simulating and experimental study on the woven carbon fiber-reinforced composite laminates under low-velocity impact

    Science.gov (United States)

    Liu, Hanyang; Tang, Zhanwen; Pan, Lingying; Zhao, Weidong; Sun, Baogang; Jiang, Wenge

    2016-05-01

    Impact damage has been identified as a critical form of the defects that constantly threatened the reliability of composite structures, such as those used in the aerospace structures and systems. Low energy impacts can introduce barely visible damage and cause the degradation of structural stiffness, furthermore, the flaws caused by low-velocity impact are so dangerous that they can give rise to the further extended delaminations. In order to improve the reliability and load carrying capacity of composite laminates under low-velocity impact, in this paper, the numerical simulatings and experimental studies on the woven fiber-reinforced composite laminates under low-velocity impact with impact energy 16.7J were discussed. The low velocity impact experiment was carried out through drop-weight system as the reason of inertia effect. A numerical progressive damage model was provided, in which the damages of fiber, matrix and interlamina were considered by VUMT subroutine in ABAQUS, to determine the damage modes. The Hashin failure criteria were improved to cover the failure modes of fiber failure in the directions of warp/weft and delaminations. The results of Finite Element Analysis (FEA) were compared with the experimental results of nondestructive examination including the results of ultrasonic C-scan, cross-section stereomicroscope and contact force - time history curves. It is found that the response of laminates under low-velocity impact could be divided into stages with different damage. Before the max-deformation of the laminates occurring, the matrix cracking, fiber breakage and delaminations were simulated during the impactor dropping. During the releasing and rebounding period, matrix cracking and delaminations areas kept increasing in the laminates because of the stress releasing of laminates. Finally, the simulating results showed the good agreements with the results of experiment.

  14. Laminated electrospun nHA/PHB-composite scaffolds mimicking bone extracellular matrix for bone tissue engineering

    Energy Technology Data Exchange (ETDEWEB)

    Chen, Zhuoyue [Lab of Tissue Engineering, Faculty of Life Science, Northwest University, 229 TaiBai North Road, Xi' an, Shaanxi Province 710069 (China); Provincial Key Laboratory of Biotechnology of Shaanxi, Northwest University, 229 TaiBai North Road, Xi' an, Shaanxi Province 710069 (China); Song, Yue [Lab of Tissue Engineering, Faculty of Life Science, Northwest University, 229 TaiBai North Road, Xi' an, Shaanxi Province 710069 (China); Zhang, Jing [Lab of Tissue Engineering, Faculty of Life Science, Northwest University, 229 TaiBai North Road, Xi' an, Shaanxi Province 710069 (China); Provincial Key Laboratory of Biotechnology of Shaanxi, Northwest University, 229 TaiBai North Road, Xi' an, Shaanxi Province 710069 (China); Key Laboratory of Resource Biology and Modern Biotechnology in Western China, Ministry of Education, Northwest University, 229 TaiBai North Road, Xi' an, Shaanxi Province, 710069 (China); Liu, Wei [Lab of Tissue Engineering, Faculty of Life Science, Northwest University, 229 TaiBai North Road, Xi' an, Shaanxi Province 710069 (China); Cui, Jihong, E-mail: cjh@nwu.edu.cn [Lab of Tissue Engineering, Faculty of Life Science, Northwest University, 229 TaiBai North Road, Xi' an, Shaanxi Province 710069 (China); Provincial Key Laboratory of Biotechnology of Shaanxi, Northwest University, 229 TaiBai North Road, Xi' an, Shaanxi Province 710069 (China); Key Laboratory of Resource Biology and Modern Biotechnology in Western China, Ministry of Education, Northwest University, 229 TaiBai North Road, Xi' an, Shaanxi Province, 710069 (China); and others

    2017-03-01

    Electrospinning is an effective means to generate nano- to micro-scale polymer fibers resembling native extracellular matrix for tissue engineering. However, a major problem of electrospun materials is that limited pore size and porosity may prevent adequate cellular infiltration and tissue ingrowth. In this study, we first prepared thin layers of hydroxyapatite nanoparticle (nHA)/poly-hydroxybutyrate (PHB) via electrospinning. We then laminated the nHA/PHB thin layers to obtain a scaffold for cell seeding and bone tissue engineering. The results demonstrated that the laminated scaffold possessed optimized cell-loading capacity. Bone marrow mesenchymal stem cells (MSCs) exhibited better adherence, proliferation and osteogenic phenotypes on nHA/PHB scaffolds than on PHB scaffolds. Thereafter, we seeded MSCs onto nHA/PHB scaffolds to fabricate bone grafts. Histological observation showed osteoid tissue formation throughout the scaffold, with most of the scaffold absorbed in the specimens 2 months after implantation, and blood vessels ingrowth into the graft could be observed in the graft. We concluded that electrospun and laminated nanoscaled biocomposite scaffolds hold great therapeutic potential for bone regeneration. - Highlights: • We laminated the nHA/PHB layers to obtain a scaffold for bone tissue engineering. • The laminated scaffold performed optimized cell-loading capacity. • MSCs exhibited osteogenic phenotypes on the laminated scaffold. • Osteoid tissue formed throughout the laminated scaffold after 2 months in vivo. The laminated bio-composite scaffolds can be applied to bone regeneration.

  15. Laminated electrospun nHA/PHB-composite scaffolds mimicking bone extracellular matrix for bone tissue engineering

    International Nuclear Information System (INIS)

    Chen, Zhuoyue; Song, Yue; Zhang, Jing; Liu, Wei; Cui, Jihong

    2017-01-01

    Electrospinning is an effective means to generate nano- to micro-scale polymer fibers resembling native extracellular matrix for tissue engineering. However, a major problem of electrospun materials is that limited pore size and porosity may prevent adequate cellular infiltration and tissue ingrowth. In this study, we first prepared thin layers of hydroxyapatite nanoparticle (nHA)/poly-hydroxybutyrate (PHB) via electrospinning. We then laminated the nHA/PHB thin layers to obtain a scaffold for cell seeding and bone tissue engineering. The results demonstrated that the laminated scaffold possessed optimized cell-loading capacity. Bone marrow mesenchymal stem cells (MSCs) exhibited better adherence, proliferation and osteogenic phenotypes on nHA/PHB scaffolds than on PHB scaffolds. Thereafter, we seeded MSCs onto nHA/PHB scaffolds to fabricate bone grafts. Histological observation showed osteoid tissue formation throughout the scaffold, with most of the scaffold absorbed in the specimens 2 months after implantation, and blood vessels ingrowth into the graft could be observed in the graft. We concluded that electrospun and laminated nanoscaled biocomposite scaffolds hold great therapeutic potential for bone regeneration. - Highlights: • We laminated the nHA/PHB layers to obtain a scaffold for bone tissue engineering. • The laminated scaffold performed optimized cell-loading capacity. • MSCs exhibited osteogenic phenotypes on the laminated scaffold. • Osteoid tissue formed throughout the laminated scaffold after 2 months in vivo. The laminated bio-composite scaffolds can be applied to bone regeneration.

  16. Influence of Thinning and Pruning on Southern Pine Veneer Quality

    Science.gov (United States)

    Mark D. Gibson; Terry R. Clason; Gary L. Hill; George A. Grozdits

    2002-01-01

    This paper presents the effects of intensive pine plantation management on veneer yields, veneer grade distribution and veneer MOE as measured by ultrasonic stress wave transmission (Metriguard). Veneer production trials were done at a commercial southern pine plywood plant to elucidate the effects of silvicultural treatments on veneer quality, yield, and modulus of...

  17. Structural and Chemical Analysis of the Zirconia-Veneering Ceramic Interface.

    Science.gov (United States)

    Inokoshi, M; Yoshihara, K; Nagaoka, N; Nakanishi, M; De Munck, J; Minakuchi, S; Vanmeensel, K; Zhang, F; Yoshida, Y; Vleugels, J; Naert, I; Van Meerbeek, B

    2016-01-01

    The interfacial interaction of veneering ceramic with zirconia is still not fully understood. This study aimed to characterize morphologically and chemically the zirconia-veneering ceramic interface. Three zirconia-veneering conditions were investigated: 1) zirconia-veneering ceramic fired on sandblasted zirconia, 2) zirconia-veneering ceramic on as-sintered zirconia, and 3) alumina-veneering ceramic (lower coefficient of thermal expansion [CTE]) on as-sintered zirconia. Polished cross-sectioned ceramic-veneered zirconia specimens were examined using field emission gun scanning electron microscopy (Feg-SEM). In addition, argon-ion thinned zirconia-veneering ceramic interface cross sections were examined using scanning transmission electron microscopy (STEM)-energy dispersive X-ray spectrometry (EDS) at high resolution. Finally, the zirconia-veneering ceramic interface was quantitatively analyzed for tetragonal-to-monoclinic phase transformation and residual stress using micro-Raman spectroscopy (µRaman). Feg-SEM revealed tight interfaces for all 3 veneering conditions. High-resolution transmission electron microscopy (HRTEM) disclosed an approximately 1.0-µm transformed zone at sandblasted zirconia, in which distinct zirconia grains were no longer observable. Straight grain boundaries and angular grain corners were detected up to the interface of zirconia- and alumina-veneering ceramic with as-sintered zirconia. EDS mapping disclosed within the zirconia-veneering ceramic a few nanometers thick calcium/aluminum-rich layer, touching the as-sintered zirconia base, with an equally thick silicon-rich/aluminum-poor layer on top. µRaman revealed t-ZrO2-to-m-ZrO2 phase transformation and residual compressive stress at the sandblasted zirconia surface. The difference in CTE between zirconia- and the alumina-veneering ceramic resulted in residual tensile stress within the zirconia immediately adjacent to its interface with the veneering ceramic. The rather minor chemical

  18. Modeling two-phase ferroelectric composites by sequential laminates

    International Nuclear Information System (INIS)

    Idiart, Martín I

    2014-01-01

    Theoretical estimates are given for the overall dissipative response of two-phase ferroelectric composites with complex particulate microstructures under arbitrary loading histories. The ferroelectric behavior of the constituent phases is described via a stored energy density and a dissipation potential in accordance with the theory of generalized standard materials. An implicit time-discretization scheme is used to generate a variational representation of the overall response in terms of a single incremental potential. Estimates are then generated by constructing sequentially laminated microgeometries of particulate type whose overall incremental potential can be computed exactly. Because they are realizable, by construction, these estimates are guaranteed to conform with any material constraints, to satisfy all pertinent bounds and to exhibit the required convexity properties with no duality gap. Predictions for representative composite and porous systems are reported and discussed in the light of existing experimental data. (paper)

  19. Shear bond strength of veneering porcelain to zirconia: Effect of surface treatment by CNC-milling and composite layer deposition on zirconia.

    Science.gov (United States)

    Santos, R L P; Silva, F S; Nascimento, R M; Souza, J C M; Motta, F V; Carvalho, O; Henriques, B

    2016-07-01

    The purpose of this study was to evaluate the shear bond strength of veneering feldspathic porcelain to zirconia substrates modified by CNC-milling process or by coating zirconia with a composite interlayer. Four types of zirconia-porcelain interface configurations were tested: RZ - porcelain bonded to rough zirconia substrate (n=16); PZ - porcelain bonded to zirconia substrate with surface holes (n=16); RZI - application of a composite interlayer between the veneering porcelain and the rough zirconia substrate (n=16); PZI - application of a composite interlayer between the porcelain and the zirconia substrate treated by CNC-milling (n=16). The composite interlayer was composed of zirconia particles reinforced porcelain (30%, vol%). The mechanical properties of the ceramic composite have been determined. The shear bond strength test was performed at 0.5mm/min using a universal testing machine. The interfaces of fractured and untested specimens were examined by FEG-SEM/EDS. Data was analyzed with Shapiro-Wilk test to test the assumption of normality. The one-way ANOVA followed by Tukey HSD multiple comparison test was used to compare shear bond strength results (α=0.05). The shear bond strength of PZ (100±15MPa) and RZI (96±11MPa) specimens were higher than that recorded for RZ (control group) specimens (89±15MPa), although not significantly (p>0.05). The highest shear bond strength values were recorded for PZI specimens (138±19MPa), yielding a significant improvement of 55% relative to RZ specimens (p<0.05). This study shows that it is possible to highly enhance the zirconia-porcelain bond strength - even by ~55% - by combining surface holes in zirconia frameworks and the application of a proper ceramic composite interlayer. Copyright © 2016 Elsevier Ltd. All rights reserved.

  20. Characterization of damaged composite laminates by an optical measurement of the displacement field

    International Nuclear Information System (INIS)

    Loukil, M S; Ayadi, Z; Varna, J

    2012-01-01

    The degradation of the elastic properties of composite laminates with intralaminar cracks is caused by reduced stress in the damaged layer which is mainly due to two parameters: the crack opening displacement (COD) and the crack sliding displacement (CSD). In this paper these parameters are measured experimentally providing laminate stiffness reduction models with valuable information for validation of used assumptions and for defining limits of their application. In particular, the displacement field on the edges of a [0/ +70 4 / −70 4 ] s glass fiber/epoxy laminate specimens with multiple intralaminar cracks is studied and the COD and CSD dependence on the applied mechanical load is measured. The specimen full-field displacement measurement is carried out using ESPI (Electronic Speckle Pattern Interferometry). By studying the displacement discontinuities, the crack face displacements were measured. A comparison between the COD and the CSD (for the same crack) is performed.

  1. Finite element modeling of small-scale tapered wood-laminated composite poles with biomimicry features

    Science.gov (United States)

    Cheng Piao; Todd F. Shupe; R.C. Tang; Chung Y. Hse

    2008-01-01

    Tapered composite poles with biomimicry features as in bamboo are a new generation of wood laminated composite poles that may some day be considered as an alternative to solid wood poles that are widely used in the transmission and telecommunication fields. Five finite element models were developed with ANSYS to predict and assess the performance of five types of...

  2. Thickness filters for gradient based multi-material and thickness optimization of laminated composite structures

    DEFF Research Database (Denmark)

    Sørensen, Rene; Lund, Erik

    2015-01-01

    This paper presents a new gradient based method for performing discrete material and thickness optimization of laminated composite structures. The novelty in the new method lies in the application of so-called casting constraints, or thickness filters in this context, to control the thickness...... variation throughout the laminate. The filters replace the layerwise density variables with a single continuous through-the-thickness design variable. Consequently, the filters eliminate the need for having explicit constraints for preventing intermediate void through the thickness of the laminate....... Therefore, the filters reduce both the number of constraints and design variables in the optimization problem. Based upon a continuous approximation of a unit step function, the thickness filters are capable of projecting discrete 0/1 values to the underlying layerwise or ”physical” density variables which...

  3. Optimization of sensor introduction into laminated composite materials

    Science.gov (United States)

    Schaaf, Kristin; Nemat-Nasser, Sia

    2008-03-01

    This work seeks to extend the functionality of the composite material beyond that of simply load-bearing and to enable in situ sensing, without compromising the structural integrity of the host composite material. Essential to the application of smart composites is the issue of the mechanical coupling of the sensor to the host material. Here we present various methods of embedding sensors within the host composite material. In this study, quasi-static three-point bending (short beam) and fatigue three-point bending (short beam) tests are conducted in order to characterize the effects of introducing the sensors into the host composite material. The sensors that are examined include three types of polyvinylidene fluoride (PVDF) thin film sensors: silver ink with a protective coating of urethane, silver ink without a protective coating, and nickel-copper alloy without a protective coating. The methods of sensor integration include placement at the midplane between the layers of prepreg material as well as a sandwich configuration in which a PVDF thin film sensor is placed between the first and second and nineteenth and twentieth layers of prepreg. Each PVDF sensor is continuous and occupies the entire layer, lying in the plane normal to the thickness direction in laminated composites. The work described here is part of an ongoing effort to understand the structural effects of integrating microsensor networks into a host composite material.

  4. The analysis of composite laminated beams using a 2D interpolating meshless technique

    Science.gov (United States)

    Sadek, S. H. M.; Belinha, J.; Parente, M. P. L.; Natal Jorge, R. M.; de Sá, J. M. A. César; Ferreira, A. J. M.

    2018-02-01

    Laminated composite materials are widely implemented in several engineering constructions. For its relative light weight, these materials are suitable for aerospace, military, marine, and automotive structural applications. To obtain safe and economical structures, the modelling analysis accuracy is highly relevant. Since meshless methods in the recent years achieved a remarkable progress in computational mechanics, the present work uses one of the most flexible and stable interpolation meshless technique available in the literature—the Radial Point Interpolation Method (RPIM). Here, a 2D approach is considered to numerically analyse composite laminated beams. Both the meshless formulation and the equilibrium equations ruling the studied physical phenomenon are presented with detail. Several benchmark beam examples are studied and the results are compared with exact solutions available in the literature and the results obtained from a commercial finite element software. The results show the efficiency and accuracy of the proposed numeric technique.

  5. Evaluation of Force-Time Changes During Impact of Hybrid Laminates Made of Titanium and Fibrous Composite

    Directory of Open Access Journals (Sweden)

    Jakubczak P.

    2016-06-01

    Full Text Available Fibre metal laminates (FML are the modern hybrid materials with potential wide range of applications in aerospace technology due to their excellent mechanical properties (particularly fatigue strength, resistance to impacts and also excellent corrosion resistance. The study describes the resistance to low velocity impacts in Ti/CFRP laminates. Tested laminates were produced in autoclave process. The laminates were characterized in terms of their response to impacts in specified energy range (5J, 10J, 20J. The tests were performed in accordance with ASTM D7137 standard. The laminates were subjected to impacts by means of hemispherical impactor with diameter of 12,7 mm. The following values have been determined: impact force vs. time, maximum force and the force at which the material destruction process commences (Pi. It has been found that fibre titanium laminates are characterized by high resistance to impacts. This feature is associated with elasto-plastic properties of metal and high rigidity of epoxy - fibre composite. It has been observed that Ti/CFRP laminates are characterized by more instable force during impact in stage of stabilization of impactor-laminate system and stage of force growth that glass fibre laminates. It has been observed more stable force decrease in stage of stress relaxation and withdrawal of the impactor. In energy range under test, the laminates based on titanium with glass and carbon fibres reinforcement demonstrate similar and high resistance to low-velocity impact, measured by means of failure initiation force and impact maximum force.

  6. Bath temperature effect on magnetoelectric performance of Ni-lead zirconate titanate-Ni laminated composites synthesized by electroless deposition

    Energy Technology Data Exchange (ETDEWEB)

    Wu, W. [College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016 (China); Wang, Y.G., E-mail: yingang.wang@nuaa.edu.c [College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016 (China); Bi, K. [College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016 (China)

    2011-03-15

    Magnetoelectric (ME) Ni-lead zirconate titanate-Ni laminated composites have been prepared by electroless deposition at various bath temperatures. The structure of the Ni layers deposited at various bath temperatures was characterized by X-ray diffraction, and microstructures were investigated by transmission electron microscopy. The magnetostrictive coefficients were measured by means of a resistance strain gauge. The transverse ME voltage coefficient {alpha}{sub E,31} was measured with the magnetic field applied parallel to the sample plane. The deposition rate of Ni increases with bath temperature. Ni layer with smaller grain size is obtained at higher bath temperature and shows higher piezomagnetic coefficient, promoting the ME effect of corresponding laminated composites. It is advantageous to increase the bath temperature, while trying to avoid the breaking of bath constituents. - Research Highlights: Laminated composites without interlayer are prepared by electroless deposition. Bath temperature affects the grain size of the deposited Ni layers. Higher bath temperature is beneficial to obtain stronger ME response.

  7. Optimum stacking sequence design of laminated composite circular plates with curvilinear fibres by a layer-wise optimization method

    Science.gov (United States)

    Guenanou, A.; Houmat, A.

    2018-05-01

    The optimum stacking sequence design for the maximum fundamental frequency of symmetrically laminated composite circular plates with curvilinear fibres is investigated for the first time using a layer-wise optimization method. The design variables are two fibre orientation angles per layer. The fibre paths are constructed using the method of shifted paths. The first-order shear deformation plate theory and a curved square p-element are used to calculate the objective function. The blending function method is used to model accurately the geometry of the circular plate. The equations of motion are derived using Lagrange's method. The numerical results are validated by means of a convergence test and comparison with published values for symmetrically laminated composite circular plates with rectilinear fibres. The material parameters, boundary conditions, number of layers and thickness are shown to influence the optimum solutions to different extents. The results should serve as a benchmark for optimum stacking sequences of symmetrically laminated composite circular plates with curvilinear fibres.

  8. Equivalent circuit method research of resonant magnetoelectric characteristic in magnetoelectric laminate composites using nonlinear magnetostrictive constitutive model

    International Nuclear Information System (INIS)

    Zhou, Hao-Miao; Li, Chao; Xuan, Li-Ming; Zhao, Ji-Xiang; Wei, Jing

    2011-01-01

    This paper analyzes the magnetoelectric (ME) response around the resonance frequency in the magnetostrictive/piezoelectric/magnetostrictive (MPM) magnetoelectric laminate composites. Following the equivalent circuit method and considering the mechanical loss, we select the nonlinear magnetostrictive constitutive model to present a novel explicit nonlinear expression for the resonant magnetoelectric (ME) coefficient of the magnetoelectric laminate composites. Compared with the experimental results, the predicted resonant ME coefficient of the explicit expression shows a good agreement both qualitatively and quantitatively. Also, when the electromechanical coupling factor of the piezoelectric material, k 31 p , is small, this explicit expression can be reduced to the existing model. On this basis, this paper considers and predicts the magnetoelectric conversion characteristics of the magnetoelectric laminate composites, calculates and analyzes the influences of the thickness ratio of magnetostrictive layer and piezoelectric material, bias magnetic field, and saturation magnetostrictive coefficient on the resonant ME coefficient. This research can provide a theoretical basis for the preparation of magnetoelectric devices with good magnetoelectric conversion characteristics, such as magnetoelectric sensors, energy harvesting transducers, microwave devices etc

  9. Relative translucency of six all-ceramic systems. Part II: core and veneer materials.

    Science.gov (United States)

    Heffernan, Michael J; Aquilino, Steven A; Diaz-Arnold, Ana M; Haselton, Debra R; Stanford, Clark M; Vargas, Marcos A

    2002-07-01

    STATEMENT OF PROBLEM All-ceramic core materials with various strengthening compositions have a range of translucencies. It is unknown whether translucency differs when all-ceramic materials are fabricated similarly to the clinical restoration with a veneered core material. This study compared the translucency of 6 all-ceramic materials veneered and glazed at clinically appropriate thicknesses. Core specimens (n = 5 per group) of Empress dentin, Empress 2 dentin, In-Ceram Alumina, In-Ceram Spinell, In-Ceram Zirconia, and Procera AllCeram were fabricated as described in Part I of this study and veneered with their corresponding dentin porcelain to a final thickness of 1.47 +/- 0.01 mm. These specimens were compared with veneered Vitadur Alpha opaque dentin (as a standard), a clear glass disc (positive control), and a high-noble metal-ceramic alloy (Porc. 52 SF) veneered with Vitadur Omega dentin (negative control). Specimen reflectance was measured with an integrating sphere attached to a spectrophotometer across the visible spectrum (380 to 700 nm); 0-degree illumination and diffuse viewing geometry were used. Measurements were repeated after a glazing cycle. Contrast ratios were calculated from the luminous reflectance (Y) of the specimens with a black (Yb) and a white backing (Yw) to give Yb/Yw with CIE illuminant D65 and a 2-degree observer function (0.0 = transparent, 1.0 = opaque). One-way analysis of variance and Tukey's multiple-comparison test were used to analyze the data (P<.05). Significant differences in contrast ratios were found among the ceramic systems tested when they were veneered (P<.0001) and after the glazing cycle (P<.0001). Significant changes in contrast ratios (P<.0001) also were identified when the veneered specimens were glazed. Within the limitations of this study, a range of translucency was identified in the veneered all-ceramic systems tested. Such variability may affect their ability to match natural teeth. The glazing cycle resulted

  10. The Effect of Core and Veneering Design on the Optical Properties of Polyether Ether Ketone.

    Science.gov (United States)

    Zeighami, S; Mirmohammadrezaei, S; Safi, M; Falahchai, S M

    2017-12-01

    This study aimed to evaluate the effect of core shade and core and veneering thickness on color parameters and translucency of polyether ether ketone (PEEK). Sixty PEEK discs (0.5 and 1 mm in thickness) with white and dentine shades were veneered with A2 shade indirect composite resin with 0.5, 1 and 1.5 mm thickness (n=5). Cores without the veneering material served as controls for translucency evaluation. Color parameters were measured by a spectroradiometer. Color difference (ΔE₀₀) and translucency parameters (TP) were computed. Data were analyzed using one-way ANOVA and Tukey's test (for veneering thickness) and independent t-test (for core shade and thickness) via SPSS 20.0 (p⟨0.05). Regarding the veneering thickness, white cores of 0.5 mm thickness showed significant differences in all color parameters. In white cores of 1 mm thickness and dentine cores of 0.5 and 1 mm thickness, there were statistically significant differences only in L∗, a∗ and h∗. The mean TP was significantly higher in all white cores of 1 mm thickness than dentine cores of 1 mm. Considering ΔE₀₀=3.7 as clinically unacceptable, only three groups had higher mean ΔE₀₀ values. Core shade, core thickness, and the veneering thickness affected the color and translucency of PEEK restorations. Copyright© 2017 Dennis Barber Ltd.

  11. Mechanical characterisation of hybrid composite laminates based on basalt fibres in combination with flax, hemp and glass fibres manufactured by vacuum infusion

    International Nuclear Information System (INIS)

    Petrucci, R.; Santulli, C.; Puglia, D.; Sarasini, F.; Torre, L.; Kenny, J.M.

    2013-01-01

    Highlights: ► For the first time, hybrid laminates with three different fibres were produced. ► Concerns are confirmed on the brittleness of hybrid laminates with basalt fibre core. ► An optimal configuration (FHB) for flexural properties was singled out. ► Differences between tensile and flexural properties of hybrids were identified. ► In general, the specific mechanical properties of the hybrids are quite high. - Abstract: This work concerns the production by vacuum infusion and the comparison of the properties of different hybrid composite laminates, based on basalt fibre composites as the inner core, and using also glass, flax and hemp fibre laminates to produce symmetrical configurations, all of them with a 21–23% fibre volume, in an epoxy resin. The laminates have been subjected to tensile, three-point flexural and interlaminar shear strength tests and their fracture surfaces have been characterised by scanning electron microscopy. The mechanical performance of all the hybrid laminates appears superior to pure hemp and flax fibre reinforced laminates and inferior to basalt fibre laminates. Among the hybrids, the best properties are offered by those obtained by adding glass and flax to basalt fibre reinforced laminates. Scanning electron microscopy (SEM) observation of hybrid laminates showed the diffuse presence of fibre pull-out in hemp and flax fibre reinforced layers and a general trend of brittle failure

  12. Friction Properties of Laminated Composite Materials of Alpha-Tricalcium Phosphate–Filled Poly (Vinyl Alcohol) Hydrogels

    OpenAIRE

    Yamamoto, Kanae; Iwai, Tomoaki; Shoukaku, Yutaka

    2015-01-01

    The aim of this study was to examine the mechanical characteristics of a polyvinyl alcohol hydrogel (PVA-H) as a candidate material for artificial joint cartilage. In the study, PVA-H was filled with α-tricalcium phosphate (α-TCP) in order to improve its mechanical properties. In addition, laminated composite materials with 3 layers were prepared by laminating α-TCP–filled PVA-H and unfilled PVA-H. The samples were prepared with different numbers of repeated freeze–thaw cycles and several con...

  13. On the detectability of transverse cracks in laminated composites using electrical potential change measurements

    KAUST Repository

    Selvakumaran, Lakshmi; Long, Quan; Prudhomme, Serge M.; Lubineau, Gilles

    2015-01-01

    Real-time health monitoring of structures made of laminated composites is necessary as significant damage may occur without any visible signs on the surface. Inspection by electrical tomography (ET) seems a viable approach that relies on voltage

  14. Thermographic Non-Destructive Evaluation for Natural Fiber-Reinforced Composite Laminates

    Directory of Open Access Journals (Sweden)

    Hai Zhang

    2018-02-01

    Full Text Available Natural fibers, including mineral and plant fibers, are increasingly used for polymer composite materials due to their low environmental impact. In this paper, thermographic non-destructive inspection techniques were used to evaluate and characterize basalt, jute/hemp and bagasse fibers composite panels. Different defects were analyzed in terms of impact damage, delaminations and resin abnormalities. Of particular interest, homogeneous particleboards of sugarcane bagasse, a new plant fiber material, were studied. Pulsed phase thermography and principal component thermography were used as the post-processing methods. In addition, ultrasonic C-scan and continuous wave terahertz imaging were also carried out on the mineral fiber laminates for comparative purposes. Finally, an analytical comparison of different methods was given.

  15. Mechanical properties of laminated composites of Al 1100/Al 2024 in three aging states

    International Nuclear Information System (INIS)

    Pessoa, C.S.

    1984-01-01

    Laminated composites consisting of alternating layers of Al 2024 were produced by hot rolling, with a volume fraction of 49% of Al 2024. These composites used in nuclear reactor tecnology, were given under-aging, aging and over-aging heat treatments at 448k for 1h, 4h and 96h, respectively. Tests of microhardness, tension and fatigue in the divider orientation were performed. (Author) [pt

  16. Fracture Strength of Indirect Resin Composite Laminates to Teeth with Existing Restorations : An Evaluation of Conditioning Protocols

    NARCIS (Netherlands)

    Mese, Ayse; Ozcan, Mutlu

    2009-01-01

    Purpose: This study evaluated the fracture strength and failure types of indirect resin-based composite laminates bonded to teeth with aged Class III composite restorations that were conditioned according to various protocols. Materials and Methods: Maxillary central incisors (N = 60) with

  17. Effect of nanomodified polyester resin on hybrid sandwich laminates

    International Nuclear Information System (INIS)

    Anbusagar, NRR.; Giridharan, P.K.; Palanikumar, K.

    2014-01-01

    Highlights: • Effect of nanomodified polyester resin on hybrid sandwich laminates is evaluated. • The hybrid sandwich laminates are fabricated with varying wt% of nanoclay. • Flexural, impact and moisture absorbtion properties are evaluated for hybrid composites. • Scanning electron microscopy is utilized to analyze the dispersion of clay and fractured surfaces of the nanocomposites. - Abstract: Effect of nanoclay modified polyester resin on flexural, impact, hardness and water absorption properties of untreated woven jute and glass fabric hybrid sandwich laminates have been investigated experimentally. The hybrid sandwich laminates are prepared by hand lay-up manufacturing technique (HL) for investigation. All hybrid sandwich laminates are fabricated with a total of 10 layers, by varying the extreme layers and wt% of nanoclay in polyester resin so as to obtain four different combinations of hybrid sandwich laminates. For comparison of the composite with hybrid composite, jute fiber reinforced composite laminate also fabricated. X-ray diffraction (XRD) results obtained from samples with nanoclay indicated that intergallery spacing of the layered clay increases with matrix. Scanning electron microscopy (SEM) gave a morphological picture of the cross-sections and energy dispersive X-ray spectroscopy (EDS) allowed investigating the elemental composition of matrix in composites. The testing results indicated that the flexural properties are greatly increased at 4% of nanoclay loading while impact, hardness and water absorption properties are increased at 6% of nanoclay loading. A plausible explanation for high increase of properties has also been discussed

  18. Effect of Ultrasonic Versus Manual Cementation on the Fracture Strength of Resin Composite Laminates

    NARCIS (Netherlands)

    Ozcan, M.; Mese, A.

    2009-01-01

    This study evaluated the effect of conventional versus ultrasonic cementation techniques on the fracture strength of resin composite laminates. In addition, the failure modes were assessed. Window-type preparations I mm above the cemento-enamel junction were made on intact human maxillary central

  19. Effect of the interface in laminated composites of Al-1100 and Al-2024

    International Nuclear Information System (INIS)

    Godefroid, L.B.

    1983-01-01

    Laminated composites consisting of alternating layers of Al-1100 and Al-2024 were produced by hot rolling, with 45% Al-2024 volume fraction. These composites were subjected to cyclic thermal treatment (various numbers of cycles) and to isothermal treatment (various numbers of cycles) and to isothermal treatment (at peak temperature and for times equivalent to those of the thermal cycles. Microhardness, tensile and fatigue crack arrester modes) were studied in the initial state and after treatments. (E.G.) [pt

  20. Electrical impedance spectroscopy for measuring the impedance response of carbon-fiber-reinforced polymer composite laminates

    KAUST Repository

    Almuhammadi, Khaled; Bera, Tushar Kanti; Lubineau, Gilles

    2017-01-01

    impedance spectroscopy response at various frequencies of laminates chosen to be representative of classical layups employed in composite structures. We clarify the relationship between the frequency of the electrical current, the conductivity of the surface

  1. Dynamic tensile stress–strain characteristics of carbon/epoxy laminated composites in through-thickness direction

    Directory of Open Access Journals (Sweden)

    Nakai Kenji

    2015-01-01

    Full Text Available The effect of strain rate up to approximately ε̇ = 102/s on the tensile stress–strain properties of unidirectional and cross-ply carbon/epoxy laminated composites in the through-thickness direction is investigated. Waisted cylindrical specimens machined out of the laminated composites in the through-thickness direction are used in both static and dynamic tests. The dynamic tensile stress–strain curves up to fracture are determined using the split Hopkinson bar (SHB. The low and intermediate strain-rate tensile stress–strain relations up to fracture are measured on an Instron 5500R testing machine. It is demonstrated that the ultimate tensile strength and absorbed energy up to fracture increase significantly, while the fracture strain decreases slightly with increasing strain rate. Macro- and micro-scopic examinations reveal a marked difference in the fracture surfaces between the static and dynamic tension specimens.

  2. Development and verification of local/global analysis techniques for laminated composites

    Science.gov (United States)

    Griffin, O. Hayden, Jr.

    1989-01-01

    Analysis and design methods for laminated composite materials have been the subject of considerable research over the past 20 years, and are currently well developed. In performing the detailed three-dimensional analyses which are often required in proximity to discontinuities, however, analysts often encounter difficulties due to large models. Even with the current availability of powerful computers, models which are too large to run, either from a resource or time standpoint, are often required. There are several approaches which can permit such analyses, including substructuring, use of superelements or transition elements, and the global/local approach. This effort is based on the so-called zoom technique to global/local analysis, where a global analysis is run, with the results of that analysis applied to a smaller region as boundary conditions, in as many iterations as is required to attain an analysis of the desired region. Before beginning the global/local analyses, it was necessary to evaluate the accuracy of the three-dimensional elements currently implemented in the Computational Structural Mechanics (CSM) Testbed. It was also desired to install, using the Experimental Element Capability, a number of displacement formulation elements which have well known behavior when used for analysis of laminated composites.

  3. Sensitivity Analysis of a CPAM Inverse Algorithm for Composite Laminates Characterization

    Directory of Open Access Journals (Sweden)

    Farshid Masoumi

    2017-01-01

    Full Text Available Using experimental data and numerical simulations, a new combined technique is presented for characterization of thin and thick orthotropic composite laminates. Four or five elastic constants, as well as ply orientation angles, are considered as the unknown parameters. The material characterization is first examined for isotropic plates under different boundary conditions to evaluate the method’s accuracy. The proposed algorithm, so-called CPAM (Combined Programs of ABAQUS and MATLAB, utilizes an optimization procedure and makes simultaneous use of vibration test data together with their corresponding numerical solutions. The numerical solutions are based on a commercial finite element package for efficiently identifying the material properties. An inverse method based on particle swarm optimization algorithm is further provided using MATLAB software. The error function to be minimized is the sum of squared differences between experimental and simulated data of eigenfrequencies. To evaluate the robustness of the model’s results in the presence of uncertainty and unwanted noises, a sensitivity analysis that employs Gaussian disorder model is directly applied to the measured frequencies. The results with high accuracy confirm the validity and capability of the present method in simultaneous determination of mechanical constants and fiber orientation angles of composite laminates as compared to prior methods.

  4. On the detectability of transverse cracks in laminated composites through measurements of electrical potential change

    KAUST Repository

    Selvakumaran, Lakshmi; Long, Quan; Prudhomme, Serge; Lubineau, Giles

    2015-01-01

    For structures made of laminated composites, real-time structural health monitoring is necessary as significant damage may occur without any visible signs on the surface. Inspection by electrical tomography seems a viable approach as the technique

  5. Defining Hardwood Veneer Log Quality Attributes

    Science.gov (United States)

    Jan Wiedenbeck; Michael Wiemann; Delton Alderman; John Baumgras; William Luppold

    2004-01-01

    This publication provides a broad spectrum of information on the hardwood veneer industry in North America. Veneer manufacturers and their customers impose guidelines in specifying wood quality attributes that are very discriminating but poorly defined (e.g., exceptional color, texture, and/or figure characteristics). To better understand and begin to define the most...

  6. Study of fatigue crack propagation in laminated metal composites alluminium 1100/alluminium 2024

    International Nuclear Information System (INIS)

    Tavares, R.I.

    1984-01-01

    A study has been made of fatigue crack propagation in laminated metal composites with different volume fraction of constituents. The composites were produced by hot rolling, combining 1100 and 2024 aluminum alloys in crack divider orientation. Mechanical and metallurgical properties of the composites and original alloys sheets have been evaluated. Paris type relationship, corresponding to stage II of fatigue crack propagation curves, has been determined by two different methods, wich have shown to be equivalent. A computer software in FORTRAN language was developed for all the mathematical manipulation of fatigue data including statistical analysis and graphics. (Author) [pt

  7. An indirect veneer technique for simple and esthetic treatment of anterior hypoplastic teeth

    Directory of Open Access Journals (Sweden)

    Amit Khatri

    2010-01-01

    Full Text Available This study describes a technique for treating anterior hypoplastic teeth using indirect nanocomposite veneer restoration. The prime advantage of an indirect veneer technique is that it provides an esthetic and conservative result. One of the most frequent reasons that patients seek dental care is discolored anterior teeth. Although treatment options such as removal of surface stains, bleaching, microabrasion or macroabrasion, veneering, and placement of porcelain crowns are available, conservative approach such as veneer preserves the natural tooth as much as possible. Full veneers are recommended for the restoration of localized defects or areas of intrinsic discoloration, which are caused by deeper internal stains or enamel defects. Indirectly fabricated veneers are much less sensitive compared to a operator′s technique and if multiple teeth are to be veneered, indirect veneers can be usually placed much more expeditiously. Indirect veneers last much longer than the direct veneers. Therefore, indirectly fabricated veneers are more advantageous than directly fabricated veneers in many cases.

  8. Static Analysis of Laminated Composite Plate using New Higher Order Shear Deformation Plate Theory

    Directory of Open Access Journals (Sweden)

    Ibtehal Abbas Sadiq

    2017-02-01

    Full Text Available In the present work a theoretical analysis depending on the new higher order . element in shear deformation theory for simply supported cross-ply laminated plate is developed. The new displacement field of the middle surface expanded as a combination of exponential and trigonometric function of thickness coordinate with the transverse displacement taken to be constant through the thickness. The governing equations are derived using Hamilton’s principle and solved using Navier solution method to obtain the deflection and stresses under uniform sinusoidal load. The effect of many design parameters such as number of laminates, aspect ratio and thickness ratio on static behavior of the laminated composite plate has been studied. The modal of the present work has been verified by comparing the results of shape functions with that were obtained by other workers. Result shows the good agreement with 3D elasticity solution and that published by other researchers.

  9. A multiscale and multiphysics numerical framework for modelling of hygrothermal ageing in laminated composites

    NARCIS (Netherlands)

    Barcelos Carneiro M Rocha, Iuri; van der Meer, F.P.; Nijssen, RPL; Sluijs, Bert

    2017-01-01

    In this work, a numerical framework for modelling of hygrothermal ageing in laminated composites is proposed. The model consists of a macroscopic diffusion analysis based on Fick's second law coupled with a multiscale FE2 stress analysis in order to take microscopic degradation

  10. On micro-meso relations homogenizing electrical properties of transversely cracked laminated composites

    KAUST Repository

    Lubineau, Gilles

    2013-11-01

    A practical way to track the development of transverse cracking in a laminated composite is to monitor the change of its electrical resistance. Yet, the relations between transverse cracking and the global modification of resistivity is still unclear that makes difficult to interpret these non-destructive-testing results. Here, we introduce the homogenization process that defines at the meso scale an equivalent homogeneous ply that is energetically equivalent to the cracked one. It is shown that this equivalent ply mainly depends on the cracking level while it can be considered independent on the rest of the laminated structure. The direct consequence is that the meso scale is a pertinent one to perform the homogenization. Then, non-destructive electrical measurements can be considered as a reliable technique to access meso scale damage indicators. © 2013 Elsevier Ltd.

  11. On the lamb wave propagation in anisotropic laminated composite plates

    International Nuclear Information System (INIS)

    Park, Soo Keun; Jeong, Hyun Jo; Kim, Moon Saeng

    1998-01-01

    This paper examines the propagation of Lamb (or plate) waves in anisotropic laminated composite plates. The dispersion relations are explicitly derived using the classical plate theory (CLT), the first-order shear deformation theory (FSDT) and the exact solution (ES), Attention is paid to the lowest antisymmetric (flexural) and lowest symmetric(extensional) modes in the low frequency, long wavelength limit. Different values of shear correction factor were tested in FSDT and comparisons between flexural wave dispersion curves were made with exact results to asses the range of validity of approximate plate theories in the frequency domain.

  12. Prediction of process induced shape distortions and residual stresses in large fibre reinforced composite laminates

    DEFF Research Database (Denmark)

    Nielsen, Michael Wenani

    to their accuracy in predicting process induced strain and stress development in thick section laminates during curing, and more precisely regarding the evolution of the composite thermoset polymer matrix mechanical behaviour during the phase transitions experienced during curing. The different constitutive...

  13. A Novel Rational Design Method for Laminated Composite Structures Exhibiting Complex Geometrically Nonlinear Buckling Behaviour

    DEFF Research Database (Denmark)

    Lindgaard, Esben; Lund, Erik

    2012-01-01

    This paper presents a novel FEM-based approach for fiber angle optimal design of laminated composite structures exhibiting complicated nonlinear buckling behavior, thus enabling design of lighter and more cost-effective structures. The approach accounts for the geometrically nonlinear behavior of...

  14. Compression of laminated composite beams with initial damage

    Science.gov (United States)

    Breivik, Nicole L.; Gurdal, Zafer; Griffin, O. H., Jr.

    1993-01-01

    The effect of isolated damage modes on the compressive strength and failure characteristics of laminated composite test specimens were evaluated experimentally and numerically. In addition to specimens without initial damage, specimens with three types of initial damage were considered: (1) specimens with short delaminations distributed evenly through the specimen thickness, (2) specimens with few long delaminations, and (3) specimens with local fiber damage in the surface plies under the three-point bend contact point. It was found that specimens with short multiple delamination experienced the greatest reduction in compression strength compared to the undamaged specimens. Single delaminations far from the specimen surface had little effect on the final compression strength, and moderate strength reduction was observed for specimens with localized surface ply damage.

  15. Meshless Solution of the Problem on the Static Behavior of Thin and Thick Laminated Composite Beams

    Science.gov (United States)

    Xiang, S.; Kang, G. W.

    2018-03-01

    For the first time, the static behavior of laminated composite beams is analyzed using the meshless collocation method based on a thin-plate-spline radial basis function. In the approximation of a partial differential equation by using a radial basis function, the shape parameter has an important role in ensuring the numerical accuracy. The choice of a shape parameter in the thin plate spline radial basis function is easier than in other radial basis functions. The governing differential equations are derived based on Reddy's third-order shear deformation theory. Numerical results are obtained for symmetric cross-ply laminated composite beams with simple-simple and cantilever boundary conditions under a uniform load. The results found are compared with available published ones and demonstrate the accuracy of the present method.

  16. Stress and strain field singularities, micro-cracks, and their role in failure initiation at the composite laminate free-edge

    Science.gov (United States)

    Dustin, Joshua S.

    A state-of-the-art multi-scale analysis was performed to predict failure initiation at the free-edge of an angle-ply laminate using the Strain Invariant Failure Theory (SIFT), and multiple improvements to this analysis methodology were proposed and implemented. Application of this analysis and theory led to the conclusion that point-wise failure criteria which ignore the singular stress and strain fields from a homogenized analysis and the presence of free-edge damage in the form of micro-cracking, may do so at the expense of failure prediction capability. The main contributions of this work then are made in the study of the laminate free-edge singularity and in the effects of micro-cracking at the composite laminate free-edge. Study of both classical elasticity and finite element solutions of the laminate free-edge stress field based upon the assumption of homogenized lamina properties reveal that the order of the free-edge singularity is sufficiently small such that the domain of dominance of this term away from the laminate free-edge is much smaller than the relevant dimensions of the microstructure. In comparison to a crack-tip field, these free-edge singularities generate stress and strain fields which are half as intense as those at the crack-tip, leading to the conclusion that existing flaws at the free-edge in the form of micro-cracks would be more prone to the initiation of free-edge failure than the existence of a singularity in the free-edge elasticity solutions. A methodical experiment was performed on a family of [±25°/90°] s laminates made of IM7/8552 carbon/epoxy composite, to both characterize micro-cracks present at the laminate free-edge and to study their behavior under the application of a uniform extensional load. The majority of these micro-cracks were of length on the order of a few fiber diameters, though larger micro-cracks as long as 100 fiber diameters were observed in thicker laminates. A strong correlation between the application of

  17. Computational Fatigue Life Analysis of Carbon Fiber Laminate

    Science.gov (United States)

    Shastry, Shrimukhi G.; Chandrashekara, C. V., Dr.

    2018-02-01

    In the present scenario, many traditional materials are being replaced by composite materials for its light weight and high strength properties. Industries like automotive industry, aerospace industry etc., are some of the examples which uses composite materials for most of its components. Replacing of components which are subjected to static load or impact load are less challenging compared to components which are subjected to dynamic loading. Replacing the components made up of composite materials demands many stages of parametric study. One such parametric study is the fatigue analysis of composite material. This paper focuses on the fatigue life analysis of the composite material by using computational techniques. A composite plate is considered for the study which has a hole at the center. The analysis is carried on (0°/90°/90°/90°/90°)s laminate sequence and (45°/-45°)2s laminate sequence by using a computer script. The life cycles for both the lay-up sequence are compared with each other. It is observed that, for the same material and geometry of the component, cross ply laminates show better fatigue life than that of angled ply laminates.

  18. Analysis of Mode I and Mode II Crack Growth Arrest Mechanism with Z-Fibre Pins in Composite Laminated Joint

    Science.gov (United States)

    Jeevan Kumar, N.; Ramesh Babu, P.

    2018-04-01

    This paper presents the numerical study of the mode I and mode II interlaminar crack growth arrest in hybrid laminated curved composite stiffened joint with Z-fibre reinforcement. A FE model of hybrid laminated skin-stiffener joint reinforced with Z-pins is developed to investigate the effect of Z- fibre pins on mode I and mode II crack growth where the delamination is embedded inbetween the skin and stiffener interface. A finite element model was developed using S4R element of a 4-node doubly curved thick shell elements to model the composite laminates and non linear interface elements to simulate the reinforcements. The numerical analyses revealed that Z-fibre pinning were effective in suppressing the delamination growth when propagated due to applied loads. Therefore, the Z-fibre technique effectively improves the crack growth resistance and hence arrests or delays crack growth extension.

  19. Deposition of aluminum coatings on bio-composite laminates

    Science.gov (United States)

    Boccarusso, L.; Viscusi, A.; Durante, M.; Astarita, A.; De Fazio, D.; Sansone, R.; Caraviello, A.; Carrino, L.

    2018-05-01

    As a result of the increasing environmental awareness, the concern for environmental sustainability and the growing global waste problem, the interest of bio-composites materials is growing rapidly in the last years in order to use them in various engineering fields. Tremendous advantages and opportunities are associated with the use of these materials. On the other hand, some issues are related to the superficial properties of the bio-laminates, in particular the wear properties, the flame resistance and the aesthetic appearance have to be improved in order to extend the application fields of these materials. Aiming to these goals this paper deals with the study of the deposition of aluminum coating through cold spray process on hemp/PLA bio-composites manufactured by using the compression molding technique. Therefore, SEM observations, roughness analyses, bending tests, pin on disk and scratch tests were carried out in order to study the feasibility of the process and to investigate on the properties of the coated samples. The experimental results proved that when the process parameters of the deposition process are properly set, no damages are induced in the composite panel and that the aluminum coating, under specific load conditions, resulted to be able to protect the substrate.

  20. Guided wave and damage detection in composite laminates using different fiber optic sensors.

    Science.gov (United States)

    Li, Fucai; Murayama, Hideaki; Kageyama, Kazuro; Shirai, Takehiro

    2009-01-01

    Guided wave detection using different fiber optic sensors and their applications in damage detection for composite laminates were systematically investigated and compared in this paper. Two types of fiber optic sensors, namely fiber Bragg gratings (FBG) and Doppler effect-based fiber optic (FOD) sensors, were addressed and guided wave detection systems were constructed for both types. Guided waves generated by a piezoelectric transducer were propagated through a quasi-isotropic carbon fiber reinforced plastic (CFRP) laminate and acquired by these fiber optic sensors. Characteristics of these fiber optic sensors in ultrasonic guided wave detection were systematically compared. Results demonstrated that both the FBG and FOD sensors can be applied in guided wave and damage detection for the CFRP laminates. The signal-to-noise ratio (SNR) of guided wave signal captured by an FOD sensor is relatively high in comparison with that of the FBG sensor because of their different physical principles in ultrasonic detection. Further, the FOD sensor is sensitive to the damage-induced fundamental shear horizontal (SH(0)) guided wave that, however, cannot be detected by using the FBG sensor, because the FOD sensor is omnidirectional in ultrasound detection and, in contrast, the FBG sensor is severely direction dependent.

  1. Edge delamination of composite laminates subject to combined tension and torsional loading

    Science.gov (United States)

    Hooper, Steven J.

    1990-01-01

    Delamination is a common failure mode of laminated composite materials. Edge delamination is important since it results in reduced stiffness and strength of the laminate. The tension/torsion load condition is of particular significance to the structural integrity of composite helicopter rotor systems. Material coupons can easily be tested under this type of loading in servo-hydraulic tension/torsion test stands using techniques very similar to those used for the Edge Delamination Tensile Test (EDT) delamination specimen. Edge delamination of specimens loaded in tension was successfully analyzed by several investigators using both classical laminate theory and quasi-three dimensional (Q3D) finite element techniques. The former analysis technique can be used to predict the total strain energy release rate, while the latter technique enables the calculation of the mixed-mode strain energy release rates. The Q3D analysis is very efficient since it produces a three-dimensional solution to a two-dimensional domain. A computer program was developed which generates PATRAN commands to generate the finite element model. PATRAN is a pre- and post-processor which is commonly used with a variety of finite element programs such as MCS/NASTRAN. The program creates a sufficiently dense mesh at the delamination crack tips to support a mixed-mode fracture mechanics analysis. The program creates a coarse mesh in those regions where the gradients in the stress field are low (away from the delamination regions). A transition mesh is defined between these regions. This program is capable of generating a mesh for an arbitrarily oriented matrix crack. This program significantly reduces the modeling time required to generate these finite element meshes, thus providing a realistic tool with which to investigate the tension torsion problem.

  2. The effect of bulk-resin CNT-enrichment on damage and plasticity in shear-loaded laminated composites

    KAUST Repository

    Ventura, Isaac Aguilar; Lubineau, Gilles

    2013-01-01

    One way to improve multi functionality of epoxy-based laminated composites is to dope the resin with carbon nanotubes. Many investigators have focused on the elastic and fracture behavior of such nano-modified polymers under tensile loading. Yet

  3. A Progressive Damage Model for Predicting Permanent Indentation and Impact Damage in Composite Laminates

    Science.gov (United States)

    Ji, Zhaojie; Guan, Zhidong; Li, Zengshan

    2017-10-01

    In this paper, a progressive damage model was established on the basis of ABAQUS software for predicting permanent indentation and impact damage in composite laminates. Intralaminar and interlaminar damage was modelled based on the continuum damage mechanics (CDM) in the finite element model. For the verification of the model, low-velocity impact tests of quasi-isotropic laminates with material system of T300/5228A were conducted. Permanent indentation and impact damage of the laminates were simulated and the numerical results agree well with the experiments. It can be concluded that an obvious knee point can be identified on the curve of the indentation depth versus impact energy. Matrix cracking and delamination develops rapidly with the increasing impact energy, while considerable amount of fiber breakage only occurs when the impact energy exceeds the energy corresponding to the knee point. Predicted indentation depth after the knee point is very sensitive to the parameter μ which is proposed in this paper, and the acceptable value of this parameter is in range from 0.9 to 1.0.

  4. Synthesis and characterization of laminated Si/SiC composites

    Science.gov (United States)

    Naga, Salma M.; Kenawy, Sayed H.; Awaad, Mohamed; Abd El-Wahab, Hamada S.; Greil, Peter; Abadir, Magdi F.

    2012-01-01

    Laminated Si/SiC ceramics were synthesized from porous preforms of biogenous carbon impregnated with Si slurry at a temperature of 1500 °C for 2 h. Due to the capillarity infiltration with Si, both intrinsic micro- and macrostructure in the carbon preform were retained within the final ceramics. The SEM micrographs indicate that the final material exhibits a distinguished laminar structure with successive Si/SiC layers. The produced composites show weight gain of ≈5% after heat treatment in air at 1300 °C for 50 h. The produced bodies could be used as high temperature gas filters as indicated from the permeability results. PMID:25685404

  5. Synthesis and characterization of laminated Si/SiC composites

    Directory of Open Access Journals (Sweden)

    Salma M. Naga

    2013-01-01

    Full Text Available Laminated Si/SiC ceramics were synthesized from porous preforms of biogenous carbon impregnated with Si slurry at a temperature of 1500 °C for 2 h. Due to the capillarity infiltration with Si, both intrinsic micro- and macrostructure in the carbon preform were retained within the final ceramics. The SEM micrographs indicate that the final material exhibits a distinguished laminar structure with successive Si/SiC layers. The produced composites show weight gain of ≈5% after heat treatment in air at 1300 °C for 50 h. The produced bodies could be used as high temperature gas filters as indicated from the permeability results.

  6. Geometrically nonlinear transient vibrations of actively damped anti-symmetric angle ply laminated composite shallow shell using active fibre composite (AFC) actuators

    Science.gov (United States)

    Ashok, M. H.; Shivakumar, J.; Nandurkar, Santosh; Khadakbhavi, Vishwanath; Pujari, Sanjay

    2018-02-01

    In present work, the thin laminated composite shallow shell as smart structure with AFC material’s ACLD treatment is analyzed for geometrically nonlinear transient vibrations. The AFC material is used to make the constraining layer of the ACLD treatment. Golla-Hughes-McTavish (GHM) is used to model the constrained viscoelastic layer of the ACLD treatment in time domain. Along with a simple first-order shear deformation theory the Von Kármán type non-linear strain displacement relations are used for deriving this electromechanical coupled problem. A 3-dimensional finite element model of smart composite panels integrated with the ACLD treated patches has been modelled to reveal the performance of ACLD treated patches on improving the damping properties of slender anti-symmetric angle-ply laminated shallow shell, in controlling the transient vibrations which are geometrically nonlinear. The mathematical results explain that the ACLD treated patches considerably enhance the damping properties of anti-symmetric angle-ply panels undergoing geometrically nonlinear transient vibrations.

  7. Converse magnetoelectric effect in laminated composite of Metglas and Pb(Zr,TiO3 with screen-printed interdigitated electrodes

    Directory of Open Access Journals (Sweden)

    Yuan Zhang

    2014-06-01

    Full Text Available In this study, we investigate the converse magnetoelectric (CME effect in a laminated composite consisting of Metglas ribbons and Pb(Zr,TiO3 (PZT plate with screen-printed interdigitated electrodes and operating in longitudinal magnetization and longitudinal polarization (L-L mode. Large CME coefficients of 0.134 G·cm/V at frequency of 1 kHz and 2.75 G·cm/V at resonance frequency of 43.5 kHz under a small bias magnetic field of 7 Oe are achieved. The large CME effect can be attributed to the L-L mode and low mechanical loss of the Metglas/PZT laminated composite.

  8. Evaluation of Interlaminar Stresses in Composite Laminates with a Bolt-Filled Hole Using a Linear Elastic Traction-Separation Description

    Directory of Open Access Journals (Sweden)

    Yong Cao

    2017-01-01

    Full Text Available Determination of the local interlaminar stress distribution in a laminate with a bolt-filled hole is helpful for optimal bolted joint design, due to the three-dimensional (3D nature of the stress field near the bolt hole. A new interlaminar stress distribution phenomenon induced by the bolt-head and clamp-up load, which occurs in a filled-hole composite laminate, is investigated. In order to efficiently evaluate interlaminar stresses under the complex boundary condition, a calculation strategy that using zero-thickness cohesive interface element is presented and validated. The interface element is based on a linear elastic traction-separation description. It is found that the interlaminar stress concentrations occur at the hole edge, as well as the interior of the laminate near the periphery of the bolt head. In addition, the interlaminar stresses near the periphery of the bolt head increased with an increase in the clamp-up load, and the interlaminar normal and shear stresses are not at the same circular position. Therefore, the clamp-up load cannot improve the interlaminar stress distribution in the laminate near the periphery of the bolt head, although it can reduce the magnitude of the interlaminar shear stress at the hole edge. Thus, the interlaminar stress distribution phenomena may lead to delamination initiation in the laminate near the periphery of the bolt head, and should be considered in composite bolted joint design.

  9. Residual stress measurement in veneering ceramic by hole-drilling.

    Science.gov (United States)

    Mainjot, Amélie K; Schajer, Gary S; Vanheusden, Alain J; Sadoun, Michaël J

    2011-05-01

    Mismatch in thermal expansion properties between veneering ceramic and metallic or high-strength ceramic cores can induce residual stresses and initiate cracks when combined with functional stresses. Knowledge of the stress distribution within the veneering ceramic is a key factor for understanding and predicting chipping failures, which are well-known problems with Yttria-tetragonal-zirconia-polycrystal based fixed partial dentures. The objectives of this study are to develop a method for measuring the stress profile in veneering ceramics and to compare ceramic-fused-to-metal compounds to veneered Yttria-tetragonal-zirconia-polycrystal ceramic. The hole-drilling method, often used for engineering measurements, was adapted for use with veneering ceramic. Because of the high sensitivity needed in comparison with industrial applications, a high sensitivity electrical measurement chain was developed. All samples exhibited the same type of stress vs. depth profile, starting with compressive at the ceramic surface, decreasing with depth and becoming tensile at 0.5-1.0mm from the surface, and then becoming slightly compressive again. The zirconia samples exhibited a stress depth profile of larger magnitude. The hole drilling method was shown be a practical tool for measuring residual stresses in veneering ceramics. Copyright © 2010 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

  10. Characterization of fracture properties of thin aluminum inclusions embedded in anisotropic laminate composites

    Directory of Open Access Journals (Sweden)

    Gabriella Bolzon

    2012-01-01

    Full Text Available The fracture properties of thin aluminum inclusions embedded in anisotropic paperboard composites, of interest for food and beverage packaging industry, can be determined by performing tensile tests on non-conventional heterogeneous specimens. The region of interest of the investigated material samples is monitored all along the experiment by digital image correlation techniques, which allow to recover qualitative and quantitative information about the metal deformation and about the evolution of the damaging processes leading to the detachment of the inclusion from the surrounding laminate composite. The interpretation of the laboratory results is supported by the numerical simulation of the tests.

  11. Standard Guide for Acousto-Ultrasonic Assessment of Composites, Laminates, and Bonded Joints

    CERN Document Server

    American Society for Testing and Materials. Philadelphia

    2007-01-01

    1.1 This guide explains the rationale and basic technology for the acousto-ultrasonic (AU) method. Guidelines are given for nondestructive evaluation (NDE) of flaws and physical characteristics that influence the mechanical properties and relative strength of composite structures (for example, filament-wound pressure vessels), adhesive bonds (for example, joints between metal plates), and interlaminar and fiber/matrix bonds in man-made composites and natural composites (for example, wood products). 1.2 This guide covers technical details and rules that must be observed to ensure reliable and reproducible quantitative AU assessments of laminates, composites, and bonded structures. The underlying principles, prototype apparatus, instrumentation, standardization, examination methods, and data analysis for such assessments are covered. Limitations of the AU method and guidelines for taking advantage of its capabilities are cited. 1.3 The objective of AU is to assess subtle flaws and associated strength variations...

  12. Concurrent material-fabrication optimization of metal-matrix laminates under thermo-mechanical loading

    Science.gov (United States)

    Saravanos, D. A.; Morel, M. R.; Chamis, C. C.

    1991-01-01

    A methodology is developed to tailor fabrication and material parameters of metal-matrix laminates for maximum loading capacity under thermomechanical loads. The stresses during the thermomechanical response are minimized subject to failure constrains and bounds on the laminate properties. The thermomechanical response of the laminate is simulated using nonlinear composite mechanics. Evaluations of the method on a graphite/copper symmetric cross-ply laminate were performed. The cross-ply laminate required different optimum fabrication procedures than a unidirectional composite. Also, the consideration of the thermomechanical cycle had a significant effect on the predicted optimal process.

  13. Mechanically programmed shape change in laminated elastomeric composites.

    Science.gov (United States)

    Robertson, Jaimee M; Torbati, Amir H; Rodriguez, Erika D; Mao, Yiqi; Baker, Richard M; Qi, H Jerry; Mather, Patrick T

    2015-07-28

    Soft, anisotropic materials, such as myocardium in the heart and the extracellular matrix surrounding cells, are commonly found in nature. This anisotropy leads to specialized responses and is imperative to material functionality, yet few soft materials exhibiting similar anisotropy have been developed. Our group introduced an anisotropic shape memory elastomeric composite (A-SMEC) composed of non-woven, aligned polymer fibers embedded in an elastomeric matrix. The composite exhibited shape memory (SM) behavior with significant anisotropy in room-temperature shape fixing. Here, we exploit this anisotropy by bonding together laminates with oblique anisotropy such that tensile deformation at room temperature - mechanical programming - results in coiling. This response is a breakthrough in mechanical programming, since non-affine shape change is achieved by simply stretching the layered A-SMECs at room temperature. We will show that pitch and curvature of curled geometries depend on fiber orientations and the degree of strain programmed into the material. To validate experimental results, a model was developed that captures the viscoplastic response of A-SMECs. Theoretical results correlated well with experimental data, supporting our conclusions and ensuring attainability of predictable curling geometries. We envision these smart, soft, shape changing materials will have aerospace and medical applications.

  14. Effects of core-to-dentin thickness ratio on the biaxial flexural strength, reliability, and fracture mode of bilayered materials of zirconia core (Y-TZP) and veneer indirect composite resins.

    Science.gov (United States)

    Su, Naichuan; Liao, Yunmao; Zhang, Hai; Yue, Li; Lu, Xiaowen; Shen, Jiefei; Wang, Hang

    2017-01-01

    Indirect composite resins (ICR) are promising alternatives as veneering materials for zirconia frameworks. The effects of core-to-dentin thickness ratio (C/Dtr) on the mechanical property of bilayered veneer ICR/yttria-tetragonal zirconia polycrystalline (Y-TZP) core disks have not been previously studied. The purpose of this in vitro study was to assess the effects of C/Dtr on the biaxial flexural strength, reliability, and fracture mode of bilayered veneer ICR/ Y-TZP core disks. A total of 180 bilayered 0.6-mm-thick composite resin disks in core material and C/Dtr of 2:1, 1:1, and 1:2 were tested with either core material placed up or placed down for piston-on-3-ball biaxial flexural strength. The mean biaxial flexural strength, Weibull modulus, and fracture mode were measured to evaluate the variation trend of the biaxial flexural strength, reliability, and fracture mode of the bilayered disks with various C/Dtr. One-way analysis of variance (ANOVA) and chi-square tests were used to evaluate the variation tendency of fracture mode with the C/Dtr or material placed down during testing (α=.05). Light microscopy was used to identify the fracture mode. The mean biaxial flexural strength and reliability improved with the increase in C/Dtr when specimens were tested with the core material either up and down, and depended on the materials that were placed down during testing. The rates of delamination, Hertzian cone cracks, subcritical radial cracks, and number of fracture fragments partially depended on the C/Dtr and the materials that were placed down during testing. The biaxial flexural strength, reliability, and fracture mode in bilayered structures of Y-TZP core and veneer ICR depend on both the C/Dtr and the material that was placed down during testing. Copyright © 2016 Editorial Council for the Journal of Prosthetic Dentistry. Published by Elsevier Inc. All rights reserved.

  15. Processing and impact properties of steel based laminated composites

    International Nuclear Information System (INIS)

    Carreno, F.; Pozuelo, M.; Chao, J.; Ruano, O. A.

    2001-01-01

    A seven layers steel based laminated composite (four ultra-high carbon steel, UHCS, layers and three mild steel, MS layers) has been processed by rolling bonding and its microstructure and impact properties have been studied. Suitable parameters of temperature and thickness reduction were selected to obtain a finer microstructure relative to the original materials components. This finer microstructure induces improved mechanical properties. Charpy impact tests values in both crack arrester and crack divider orientations improve the values of the UHCS constituent materials. Furthermore, the crack arrester orientation value exceed that of the MS material. The delamination, which is controlled by interface bonding, plays a key role defecting the crack, absorbing energy and imposing the nucleation of new cracks in the next materials layers. (Author) 10 refs

  16. Design and manufacturing of skins based on composite corrugated laminates for morphing aerodynamic surfaces

    Science.gov (United States)

    Airoldi, Alessandro; Fournier, Stephane; Borlandelli, Elena; Bettini, Paolo; Sala, Giuseppe

    2017-04-01

    The paper discusses the approaches for the design and manufacturing of morphing skins based on rectangular-shaped composite corrugated laminates and proposes a novel solution to prevent detrimental effects of corrugation on aerodynamic performances. Additionally, more complex corrugated shapes are presented and analysed. The manufacturing issues related to the production of corrugated laminates are discussed and tests are performed to compare different solutions and to assess the validity of analytical and numerical predictions. The solution presented to develop an aerodynamically efficient skin consists in the integration of an elastomeric cover in the corrugated laminate. The related manufacturing process is presented and assessed, and a fully nonlinear numerical model is developed and characterized to study the behaviour of this skin concept in different load conditions. Finally, configurations based on combinations of individual rectangular-shaped corrugated panels are considered. Their structural properties are numerically investigated by varying geometrical parameters. Performance indices are defined to compare structural stiffness contributions in non-morphing directions with the ones of conventional panels of the same weight. Numerical studies also show that the extension of the concept to complex corrugated shapes may improve both the design flexibility and some specific performances with respect to rectangular shaped corrugations. The overall results validate the design approaches and manufacturing processes to produce corrugated laminates and indicate that the solution for the integration of an elastomeric cover is a feasible and promising method to enhance the aerodynamic efficiency of corrugated skins.

  17. Robust buckling optimization of laminated composite structures using discrete material optimization considering “worst” shape imperfections

    DEFF Research Database (Denmark)

    Henrichsen, Søren Randrup; Lindgaard, Esben; Lund, Erik

    2015-01-01

    Robust buckling optimal design of laminated composite structures is conducted in this work. Optimal designs are obtained by considering geometric imperfections in the optimization procedure. Discrete Material Optimization is applied to obtain optimal laminate designs. The optimal geometric...... imperfection is represented by the “worst” shape imperfection. The two optimization problems are combined through the recurrence optimization. Hereby the imperfection sensitivity of the considered structures can be studied. The recurrence optimization is demonstrated through a U-profile and a cylindrical panel...... example. The imperfection sensitivity of the optimized structure decreases during the recurrence optimization for both examples, hence robust buckling optimal structures are designed....

  18. The modelling and control of failure in bi-material ceramic laminates

    International Nuclear Information System (INIS)

    Phillipps, A.J.; Howard, S.J.; Clegg, W.J.; Clyne, T.W.

    1993-01-01

    Recent experimental and theoretical work on simple, single phase, laminated systems has indicated that failure resistant ceramics can be produced using an elegant method that avoids many of the problems and limitations of comparable fibrous ceramic composites. Theoretical work on these laminated systems has shown good agreement with experiment and simulated the effects of material properties and laminate structure on the composite performance. This work has provided guidelines for optimised laminate performance. In the current study, theoretical work has been simply extended to predict the behaviour of bi-material laminates with alternating layers of weak and strong material with different stiffnesses. Expressions for the strain energy release rates of internal advancing cracks are derived and combined with existing criteria to predict the failure behaviour of these laminates during bending. The modelling indicates three modes of failure dictated by the relative proportions, thicknesses and interfacial properties of the weak and strong phases. A critical percentage of strong phase is necessary to improve failure behaviour, in an identical argument to that for fibre composites. Incorporation of compliant layers is also investigated and implications for laminate design discussed. (orig.)

  19. Micromechanics approach to the magnetoelectric properties of laminate and fibrous piezoelectric/magnetostrictive composites

    International Nuclear Information System (INIS)

    Huang Haitao; Zhou, L.M.

    2004-01-01

    We use a micromechanics approach to study the magnetoelectric (ME) properties of the piezoelectric/magnetostrictive composite with a 2-2 laminate structure and a 3-1 fibrous structure. It is found that the 3-1 composite has a higher ME coefficient than the 2-2 one, if the volume ratio of piezoelectric material is the same. The reason is that the 3-1 fibrous composite makes use of the longitudinal piezoelectric response and the piezoelectric voltage constant g 33 is 2-3 times that of g 31 . Generally, a smaller volume ratio of the piezoelectric material will generate a higher ME response. The tensile stress at the piezoelectric/magnetostrictive interface of the 3-1 fibrous composite, however, could be high enough to induce plastic deformation or microcracks, which leads to a ME coefficient lower than the theoretically predicted one

  20. Graphene and poly(methyl methacrylate) composite laminates on flexible substrates for volatile organic compound detection

    Science.gov (United States)

    Rattanabut, Chanoknan; Wongwiriyapan, Winadda; Muangrat, Worawut; Bunjongpru, Win; Phonyiem, Mayuree; Song, Young Jae

    2018-04-01

    In this paper, we present a gas sensor for volatile organic compound (VOC) detection based on graphene and poly(methyl methacrylate) (GR/PMMA) composite laminates fabricated using CVD-grown graphene. Graphene was transferred to a poly(ethylene terephthalate) (PET) substrate by PMMA-supported wet transfer process without PMMA removal in order to achieve the deposition of GR/PMMA composite laminates on PET. The GR/PMMA and graphene sensors show completely different sensitivities to VOC vapors. The GR/PMMA and graphene sensors showed the highest sensitivities to dichloromethane (DCM). The response of the GR/PMMA sensor to DCM was 3 times higher than that of the graphene sensor but the GR/PMMA sensor hardly responded to acetone, chloroform, or benzene. The sensing mechanism of the graphene sensor can be based on the dielectric constant of VOCs, the size of VOC molecule, and electron hopping effects on defect graphene, while that of the GR/PMMA sensor can be explained in terms of the polymer swelling owing to the Hansen solubility parameter.

  1. On the detectability of transverse cracks in laminated composites through measurements of electrical potential change

    KAUST Repository

    Selvakumaran, Lakshmi

    2015-01-07

    For structures made of laminated composites, real-time structural health monitoring is necessary as significant damage may occur without any visible signs on the surface. Inspection by electrical tomography seems a viable approach as the technique relies on voltage measurements from a network of electrodes over the boundary of the inspected domain to infer the change in conductivity within the bulk material. The change in conductivity, if significant, can be correlated to the degradation state of the material, allowing damage detection. We focus here on the detection of the transverse cracking mechanism which modifies the in-plane transverse conductivity of ply. The quality of detection is directly related to the sensitivity of the voltage measurements with respect to the presence of cracks. We demonstrate here from numerical experiments that the sensitivity depends on several parameters, such as the anisotropy in the electrical conductivity of the baseline composite ply or the geometricalparameters of the structure. Based on these results, applicability of electrical tomography to detect transverse cracks in a laminate is discussed.

  2. Flutter and Thermal Buckling Analysis for Composite Laminated Panel Embedded with Shape Memory Alloy Wires in Supersonic Flow

    Directory of Open Access Journals (Sweden)

    Chonghui Shao

    2016-01-01

    Full Text Available The flutter and thermal buckling behavior of laminated composite panels embedded with shape memory alloy (SMA wires are studied in this research. The classical plate theory and nonlinear von-Karman strain-displacement relation are employed to investigate the aeroelastic behavior of the smart laminated panel. The thermodynamic behaviors of SMA wires are simulated based on one-dimensional Brinson SMA model. The aerodynamic pressure on the panel is described by the nonlinear piston theory. Nonlinear governing partial differential equations of motion are derived for the panel via the Hamilton principle. The effects of ply angle of the composite panel, SMA layer location and orientation, SMA wires temperature, volume fraction and prestrain on the buckling, flutter boundary, and amplitude of limit cycle oscillation of the panel are analyzed in detail.

  3. Detecting closing delaminations in laminated composite plates using nonlinear structural intensity and time reversal mirrors

    International Nuclear Information System (INIS)

    Lamberti, Alfredo; Semperlotti, Fabio

    2013-01-01

    Closing delaminations in composite laminated structures exhibit a nonlinear dynamic response when excited by high frequency elastic waves. The contact acoustic nonlinear effects taking place at the damage interface act as a mechanism of energy redistribution from the driving frequency to the nonlinear harmonic frequencies. In this paper, we extend the concept of nonlinear structural intensity (NSI) to the analysis of closing delaminations in composite laminated plates. NSI is calculated using a method based on a combination of finite element and finite difference techniques, which is suitable for processing both numerical and experimental data. NSI is proven to be an effective metric to identify the presence and location of closing delaminations. The highly directional nature of orthotropic composites results in vibrational energy propagating in a different direction from that of the initial elastic wave. This aspect reduces the ability to effectively interrogate the damage and, therefore, the sensitivity to the damage. The time reversal mirror technique is explored as a possible approach to overcome the effect of the material directionality and increase the ability to interrogate the damage. Numerical simulations show that this technique is able to overcome the material directionality and to drastically enhance the ability to interrogate the damage. (paper)

  4. 3D-characterization of the veneer-zirconia interface using FIB nano-tomography.

    Science.gov (United States)

    Mainjot, Amélie K; Douillard, Thierry; Gremillard, Laurent; Sadoun, Michaël J; Chevalier, Jérôme

    2013-02-01

    The phenomena occurring during zirconia frameworks veneering process are not yet fully understood. In particular the study of zirconia behavior at the interface with the veneer remains a challenge. However this interface has been reported to act on residual stress in the veneering ceramic, which plays a significant role in clinical failures such as chipping. The objective of this study was thus to investigate the veneer-zirconia interface using a recent 3D-analysis tool and to confront these observations to residual stress measurements in the veneering ceramic. Two cross-sectioned bilayered disc samples (veneer on zirconia), exhibiting different residual stress profiles in the veneering ceramic, were investigated using 2D and 3D imaging (respectively Scanning Electron Microscopy (SEM) and Focused Ion Beam nanotomography (FIB-nt), associated with chemical analysis by Energy Dispersive X-ray Spectroscopy (EDS). The observations did not reveal any structural change in the bulk of zirconia layer of both samples. However the presence of structural alterations and sub-surface microcracks were highlighted in the first micrometer of zirconia surface, exclusively for the sample exhibiting interior tensile stress in the veneering ceramic. No interdiffusion phenomena were observed. FIB nanotomography was proven to be a powerful technique to study the veneer-zirconia interface. The determination of the origin and the nature of zirconia alterations need to be further studied. The results of the present study support the hypothesis that zirconia surface property changes could be involved in the development of tensile stress in the veneering ceramic, increasing the risk of chipping. Copyright © 2012 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

  5. Fracture mechanics analyses of ceramic/veneer interface under mixed-mode loading.

    Science.gov (United States)

    Wang, Gaoqi; Zhang, Song; Bian, Cuirong; Kong, Hui

    2014-11-01

    Few studies have focused on the interface fracture performance of zirconia/veneer bilayered structure, which plays an important role in dental all-ceramic restorations. The purpose of this study was to evaluate the fracture mechanics performance of zirconia/veneer interface in a wide range of mode-mixities (at phase angles ranging from 0° to 90°), and to examine the effect of mechanical properties of the materials and the interface on the fracture initiation and crack path of an interfacial crack. A modified sandwich test configuration with an oblique interfacial crack was proposed and calibrated to choose the appropriate geometry dimensions by means of finite element analysis. The specimens with different interface inclination angles were tested to failure under three-point bending configuration. Interface fracture parameters were obtained with finite element analyses. Based on the interfacial fracture mechanics, three fracture criteria for crack kinking were used to predict crack initiation and propagation. In addition, the effects of residual stresses due to coefficient of thermal expansion mismatch between zirconia and veneer on the crack behavior were evaluated. The crack initiation and propagation were well predicted by the three fracture criteria. For specimens at phase angle of 0, the cracks propagated in the interface; whereas for all the other specimens the cracks kinked into the veneer. Compressive residual stresses in the veneer can improve the toughness of the interface structure. The results suggest that, in zirconia/veneer bilayered structure the veneer is weaker than the interface, which can be used to explain the clinical phenomenon that veneer chipping rate is larger than interface delamination rate. Consequently, a veneer material with larger fracture toughness is needed to decrease the failure rate of all-ceramic restorations. And the coefficient of thermal expansion mismatch of the substrates can be larger to produce larger compressive

  6. UV curing of teak veneers for decorative panel

    International Nuclear Information System (INIS)

    Gatot Trimulyadi Rekso; Darsono

    1999-01-01

    The radiation curing of surface coating of teak veneers for decorative panels has been conducted by using ultra violet (UV) as radiation source. In this experiment teak wood veneer was use as a substrate. Epoxy acrylate (import product,) and unsaturated polyester (locally product) were used as coating materials after being added with difunctional monomer TPGDA, and photo-initiator darocur 1173 or irgacure 184. Irradiation was conducted using 80 watt/cm LTV source at conveyor speed of 3,0 m/min. Parameters observed were viscosity of coating materials, hardness, adhesion, appearance, abrasion and chemical resistance of cured films. In general the results showed that viscosity of the formulations based on epoxy acrylate and unsaturated polyester resin were effected by the storage. Film cured by LTV made of epoxy acrylate and unsaturated polyester on the teak veneer wood have the same adhesion and abrasion resistant properties but the hardness and chemical resistant of epoxy acrylate are better than unsaturated polyester. From the experiment result it can be concluded the unsaturated polyester (locally product) can be used as radiation curable material for coating teak veneer panels

  7. Laminate mechanics for balanced woven fabrics

    NARCIS (Netherlands)

    Akkerman, Remko

    2006-01-01

    Laminate mechanics equations are presented for composites with balanced woven fabric reinforcements. It is shown that mimicking these textile composites with equivalent transversely isotropic (‘unidirectional’) layers requires disputable manipulations. Various micromechanics predictions of textile

  8. Design feasibility study of a divertor component reinforced with fibrous metal matrix composite laminate

    International Nuclear Information System (INIS)

    You, J.-H.

    2005-01-01

    Fibrous metal matrix composites possess advanced mechanical properties compared to conventional alloys. It is expected that the application of these composites to a divertor component will enhance the structural reliability. A possible design concept would be a system consisting of tungsten armour, copper composite interlayer and copper heat sink where the composite interlayer is locally inserted into the highly stressed domain near the bond interface. For assessment of the design feasibility of the composite divertor concept, a non-linear multi-scale finite element analysis was performed. To this end, a micro-mechanics algorithm was implemented into a finite element code. A reactor-relevant heat flux load was assumed. Focus was placed on the evolution of stress state, plastic deformation and ductile damage on both macro- and microscopic scales. The structural response of the component and the micro-scale stress evolution of the composite laminate were investigated

  9. Design feasibility study of a divertor component reinforced with fibrous metal matrix composite laminate

    Energy Technology Data Exchange (ETDEWEB)

    You, J.-H. [Max-Planck-Institut fuer Plasmaphysik, EURATOM Association, Boltzmannstr. 2, D-85748 Garching (Germany)]. E-mail: j.h.you@ipp.mpg.de

    2005-01-01

    Fibrous metal matrix composites possess advanced mechanical properties compared to conventional alloys. It is expected that the application of these composites to a divertor component will enhance the structural reliability. A possible design concept would be a system consisting of tungsten armour, copper composite interlayer and copper heat sink where the composite interlayer is locally inserted into the highly stressed domain near the bond interface. For assessment of the design feasibility of the composite divertor concept, a non-linear multi-scale finite element analysis was performed. To this end, a micro-mechanics algorithm was implemented into a finite element code. A reactor-relevant heat flux load was assumed. Focus was placed on the evolution of stress state, plastic deformation and ductile damage on both macro- and microscopic scales. The structural response of the component and the micro-scale stress evolution of the composite laminate were investigated.

  10. Estimate of compressive strength of an unidirectional composite lamina using cross-ply and angle-ply laminates

    OpenAIRE

    Scafè, M.; Raiteri, G.; Brentari, A.; Dlacic, R.; Troiani, E.; Falaschetti, M. P.; Besseghini, E.

    2014-01-01

    In this work has been estimated the compressive strength of a unidirectional lamina of a carbon/epoxy composite material, using the cross-ply and angle-ply laminates. Over the years various methods have been developed to deduce compressive properties of composite materials reinforced with long fibres. Each of these methods is characterized by a specific way of applying load to the specimen. The method chosen to perform the compression tests is the Wyoming Combined Loading Compr...

  11. Cure Cycle Design Methodology for Fabricating Reactive Resin Matrix Fiber Reinforced Composites: A Protocol for Producing Void-free Quality Laminates

    Science.gov (United States)

    Hou, Tan-Hung

    2014-01-01

    For the fabrication of resin matrix fiber reinforced composite laminates, a workable cure cycle (i.e., temperature and pressure profiles as a function of processing time) is needed and is critical for achieving void-free laminate consolidation. Design of such a cure cycle is not trivial, especially when dealing with reactive matrix resins. An empirical "trial and error" approach has been used as common practice in the composite industry. Such an approach is not only costly, but also ineffective at establishing the optimal processing conditions for a specific resin/fiber composite system. In this report, a rational "processing science" based approach is established, and a universal cure cycle design protocol is proposed. Following this protocol, a workable and optimal cure cycle can be readily and rationally designed for most reactive resin systems in a cost effective way. This design protocol has been validated through experimental studies of several reactive polyimide composites for a wide spectrum of usage that has been documented in the previous publications.

  12. Experimental investigation of defect criticality in FRP laminate composites

    Science.gov (United States)

    Joyce, Peter James

    1999-11-01

    This work examines the defect criticality of fiber reinforced polymer Composites. The objective is to determine the sensitivity of the finished composite to various process-induced defects. This work focuses on two different classes of process-induced defects; (1) fiber waviness in high performance carbon-fiber reinforced unidirectional composites and (2) void volume in low cost glass-fabric reinforced composites. The role of fiber waviness in the compressive response of unidirectional composites has been studied by a number of other investigators. Because of difficulties associated with producing real composites with varying levels of fiber waviness, most experimental studies of fiber waviness have evaluated composites with artificially induced fiber waviness. Furthermore, most experimental studies have been concentrated on the effects of out-of-plane fiber waviness. The objective of this work is to evaluate the effects of in-plane fiber waviness naturally occurring in autoclave consolidated thermoplastic laminates. The first phase of this project involved the development of a simple technique for measuring the resulting fiber waviness levels. An experimental investigation of the compression strength reduction in composites with in-plane fiber waviness followed. The experimental program included carbon-fiber reinforced thermoplastic composites manufactured from prepreg tape by hand layup, and carbon-fiber and glass-fiber reinforced composites manufactured from an experimental powder towpreg by filament winding and autoclave consolidation. The compression specimens exhibited kink band failure in the prepreg composite and varying amounts of longitudinal splitting and kink banding in the towpreg composites. The compression test results demonstrated the same trend as predicted by microbudding theory but the overall quantitative correlation was poor. The second thrust of this research evaluated void effects in resin transfer molded composites. Much of the existing

  13. Computational Homogenization of Mechanical Properties for Laminate Composites Reinforced with Thin Film Made of Carbon Nanotubes

    Science.gov (United States)

    El Moumen, A.; Tarfaoui, M.; Lafdi, K.

    2018-06-01

    Elastic properties of laminate composites based Carbone Nanotubes (CNTs), used in military applications, were estimated using homogenization techniques and compared to the experimental data. The composite consists of three phases: T300 6k carbon fibers fabric with 5HS (satin) weave, baseline pure Epoxy matrix and CNTs added with 0.5%, 1%, 2% and 4%. Two step homogenization methods based RVE model were employed. The objective of this paper is to determine the elastic properties of structure starting from the knowledge of those of constituents (CNTs, Epoxy and carbon fibers fabric). It is assumed that the composites have a geometric periodicity and the homogenization model can be represented by a representative volume element (RVE). For multi-scale analysis, finite element modeling of unit cell based two step homogenization method is used. The first step gives the properties of thin film made of epoxy and CNTs and the second is used for homogenization of laminate composite. The fabric unit cell is chosen using a set of microscopic observation and then identified by its ability to enclose the characteristic periodic repeat in the fabric weave. The unit cell model of 5-Harness satin weave fabric textile composite is identified for numerical approach and their dimensions are chosen based on some microstructural measurements. Finally, a good comparison was obtained between the predicted elastic properties using numerical homogenization approach and the obtained experimental data with experimental tests.

  14. Process Modelling of Curing Process-Induced Internal Stress and Deformation of Composite Laminate Structure with Elastic and Viscoelastic Models

    Science.gov (United States)

    Li, Dongna; Li, Xudong; Dai, Jianfeng

    2018-06-01

    In this paper, two kinds of transient models, the viscoelastic model and the linear elastic model, are established to analyze the curing deformation of the thermosetting resin composites, and are calculated by COMSOL Multiphysics software. The two models consider the complicated coupling between physical and chemical changes during curing process of the composites and the time-variant characteristic of material performance parameters. Subsequently, the two proposed models are implemented respectively in a three-dimensional composite laminate structure, and a simple and convenient method of local coordinate system is used to calculate the development of residual stresses, curing shrinkage and curing deformation for the composite laminate. Researches show that the temperature, degree of curing (DOC) and residual stresses during curing process are consistent with the study in literature, so the curing shrinkage and curing deformation obtained on these basis have a certain referential value. Compared the differences between the two numerical results, it indicates that the residual stress and deformation calculated by the viscoelastic model are more close to the reference value than the linear elastic model.

  15. Sustainability of fiber reinforced laminate and honeycomb composites in manufacturing industries

    Science.gov (United States)

    Asmatulu, Eylem; Alonayni, Abdullah; Alamir, Mohammed; Rahman, Muhammad M.

    2018-03-01

    Fiber reinforced polymer (FRP) composites provide a lot of benefits, including strength-to-weight ratio / light weight, superior mechanical properties, low maintenance, prolonged service life, as well as corrosion, fatigue and creep resistance. However, sustainability of the FRP composites have not been studied in detail in terms of long term productions in various industries, such as aerospace, wind energy, automotive and defense. Carbon fibers are relatively expensive because of the energy intensive production systems, and lack of easy production options, which forces many companies to recycle and reuse the FRP composites in the same or different manufacturing industries. This study mainly deals with two important issues, including the disposal of composite wastes generated during the manufacturing of composite parts, and the disposal of the products at the end of their useful life. It is believed that the carbon fibers in the used composites will have still high mechanical strengths to use in different composite manufacturing after its end of life. The major manufacturing costs come from the labor and raw materials, so using the recycled carbon fibers will make sustainable composite productions in other industries. This paper presents the current status and outlook of the FRP composite recycling and re-manufacturing techniques in the same or different industries. A future vision of the FRP composites will be investigated with sustainability point of views. This study will also mention about the sustainability issues in laminate and honeycomb composites, new product design and developments and potential applications in different manufacturing industries.

  16. Progressive Damage and Failure Analysis of Composite Laminates

    Science.gov (United States)

    Joseph, Ashith P. K.

    Composite materials are widely used in various industries for making structural parts due to higher strength to weight ratio, better fatigue life, corrosion resistance and material property tailorability. To fully exploit the capability of composites, it is required to know the load carrying capacity of the parts made of them. Unlike metals, composites are orthotropic in nature and fails in a complex manner under various loading conditions which makes it a hard problem to analyze. Lack of reliable and efficient failure analysis tools for composites have led industries to rely more on coupon and component level testing to estimate the design space. Due to the complex failure mechanisms, composite materials require a very large number of coupon level tests to fully characterize the behavior. This makes the entire testing process very time consuming and costly. The alternative is to use virtual testing tools which can predict the complex failure mechanisms accurately. This reduces the cost only to it's associated computational expenses making significant savings. Some of the most desired features in a virtual testing tool are - (1) Accurate representation of failure mechanism: Failure progression predicted by the virtual tool must be same as those observed in experiments. A tool has to be assessed based on the mechanisms it can capture. (2) Computational efficiency: The greatest advantages of a virtual tools are the savings in time and money and hence computational efficiency is one of the most needed features. (3) Applicability to a wide range of problems: Structural parts are subjected to a variety of loading conditions including static, dynamic and fatigue conditions. A good virtual testing tool should be able to make good predictions for all these different loading conditions. The aim of this PhD thesis is to develop a computational tool which can model the progressive failure of composite laminates under different quasi-static loading conditions. The analysis

  17. Resonant responses and chaotic dynamics of composite laminated circular cylindrical shell with membranes

    Science.gov (United States)

    Zhang, W.; Liu, T.; Xi, A.; Wang, Y. N.

    2018-06-01

    This paper is focused on the resonant responses and chaotic dynamics of a composite laminated circular cylindrical shell with radially pre-stretched membranes at both ends and clamped along a generatrix. Based on the two-degree-of-freedom non-autonomous nonlinear equations of this system, the method of multiple scales is employed to obtain the four-dimensional nonlinear averaged equation. The resonant case considered here is the primary parametric resonance-1/2 subharmonic resonance and 1:1 internal resonance. Corresponding to several selected parameters, the frequency-response curves are obtained. From the numerical results, we find that the hardening-spring-type behaviors and jump phenomena are exhibited. The jump phenomena also occur in the amplitude curves of the temperature parameter excitation. Moreover, it is found that the temperature parameter excitation, the coupling degree of two order modes and the detuning parameters can effect the nonlinear oscillations of this system. The periodic and chaotic motions of the composite laminated circular cylindrical shell clamped along a generatrix are demonstrated by the bifurcation diagrams, the maximum Lyapunov exponents, the phase portraits, the waveforms, the power spectrums and the Poincaré map. The temperature parameter excitation shows that the Pomeau-Manneville type intermittent chaos occur under the certain initial conditions. It is also found that there exist the twin phenomena between the Pomeau-Manneville type intermittent chaos and the period-doubling bifurcation.

  18. Analysis of metal-matrix composite structures. I - Micromechanics constitutive theory. II - Laminate analyses

    Science.gov (United States)

    Arenburg, R. T.; Reddy, J. N.

    1991-01-01

    The micromechanical constitutive theory is used to examine the nonlinear behavior of continuous-fiber-reinforced metal-matrix composite structures. Effective lamina constitutive relations based on the Abouli micromechanics theory are presented. The inelastic matrix behavior is modeled by the unified viscoplasticity theory of Bodner and Partom. The laminate constitutive relations are incorporated into a first-order deformation plate theory. The resulting boundary value problem is solved by utilizing the finite element method. Attention is also given to computational aspects of the numerical solution, including the temporal integration of the inelastic strains and the spatial integration of bending moments. Numerical results the nonlinear response of metal matrix composites subjected to extensional and bending loads are presented.

  19. Buckling-driven delamination growth in composite laminates: Guidelines for assessing the threat posed by interlaminar matrix delamination

    DEFF Research Database (Denmark)

    Bhushan, Karihaloo; Stang, Henrik

    2008-01-01

    This paper is concerned with development of a simple procedure to assess the threat posed by interlaminar matrix delaminations to the integrity of composite laminates when they are situated in a compressive stress field. Depending upon the size of the delamination, its location below the surface...

  20. [An in vitro study of the fracture strength of tooth preparations for Empress 2 veneers and crowns and mandibular incisors restored with Empress 2 veneers and crowns].

    Science.gov (United States)

    Wei, Xue; Li, Yan

    2009-12-01

    To compare the fracture resistance of mandibular incisors' preparations for veneers and crowns, mandibular incisors restored with Empress 2 veneers and crowns. 50 human mandibular incisors were randomly divided into five groups. Each group consisted of ten teeth and the treatment obtained as follows: A, tooth preparations for veneers; B, tooth preparations for crowns; C, teeth restored with veneers; D, teeth restored with crowns; E, untreated group. The teeth received standardized preparation and the restorations were manufactured with Empress 2 system and cemented with resin luting agent. The fracture resistances of teeth were measured by Instron universal testing machine and statistically analyzed with one-way ANOVA. The fracture resistances of A, B, C, D, E were (576.11 +/- 91.53), (204.13 +/- 85.88), (451.50 +/- 116.81), (386.16 +/- 117.75) and (566.05 +/- 121.37) N, respectively. The statistical analysis demonstrated significant differences between five groups. There were no significant differences between group A and E, group C and D. Tooth preparations for veneers did not significantly reduce the fracture resistance of mandibular incisor. The fracture resistance of teeth restored with Empress 2 veneers and crowns did not significantly differ from each other.

  1. Viscoelastic characterization and self-heating behavior of laminated fiber composite driveshafts

    International Nuclear Information System (INIS)

    Henry, Todd C.; Bakis, Charles E.; Smith, Edward C.

    2015-01-01

    Highlights: • Carbon fiber composites with different matrix moduli were manufactured. • The composites are of interest for flexible driveshaft applications. • The composites are viscoelastically characterized using dynamic mechanical analysis. • The viscoelastic properties are used to predict self-heating in spinning shafts. • Measured and predicted temperatures of shafts agreed within 0.7 °C. - Abstract: The high cyclic strain capacity of fiber reinforced polymeric composites presents an opportunity to design driveshafts that can transmit high power under imperfect alignment conditions without the use of flexible couplers. In weight sensitive applications such as rotorcraft, the design of highly optimized driveshafts requires a general modeling capability that can predict a number of shaft performance characteristics—one of which is self-heating due to dynamic loading conditions. The current investigation developed three new flexible matrix composite materials of intermediate matrix modulus that, together with previously developed composites, cover the full range of material properties that are of potential interest in driveshaft design. An analytical model for the self-heating of spinning, misaligned, laminated composite shafts was refined to suit the full range of materials. Inputs to the model include ply-level dynamic material properties of the composite, cyclic strain amplitude and frequency, and various heat transfer constants related to conduction, radiation, and convection. Predictions of the surface temperature of spinning shafts correspond well with experimental measurements for bending strains of up to 2000 με, which encompasses the range of strains expected in rotorcraft driveshaft applications

  2. Investigation of translaminar fracture in fibrereinforced composite laminates---applicability of linear elastic fracture mechanics and cohesive-zone model

    Science.gov (United States)

    Hou, Fang

    With the extensive application of fiber-reinforced composite laminates in industry, research on the fracture mechanisms of this type of materials have drawn more and more attentions. A variety of fracture theories and models have been developed. Among them, the linear elastic fracture mechanics (LEFM) and cohesive-zone model (CZM) are two widely-accepted fracture models, which have already shown applicability in the fracture analysis of fiber-reinforced composite laminates. However, there remain challenges which prevent further applications of the two fracture models, such as the experimental measurement of fracture resistance. This dissertation primarily focused on the study of the applicability of LEFM and CZM for the fracture analysis of translaminar fracture in fibre-reinforced composite laminates. The research for each fracture model consisted of two sections: the analytical characterization of crack-tip fields and the experimental measurement of fracture resistance parameters. In the study of LEFM, an experimental investigation based on full-field crack-tip displacement measurements was carried out as a way to characterize the subcritical and steady-state crack advances in translaminar fracture of fiber-reinforced composite laminates. Here, the fiber-reinforced composite laminates were approximated as anisotropic solids. The experimental investigation relied on the LEFM theory with a modification with respect to the material anisotropy. Firstly, the full-field crack-tip displacement fields were measured by Digital Image Correlation (DIC). Then two methods, separately based on the stress intensity approach and the energy approach, were developed to measure the crack-tip field parameters from crack-tip displacement fields. The studied crack-tip field parameters included the stress intensity factor, energy release rate and effective crack length. Moreover, the crack-growth resistance curves (R-curves) were constructed with the measured crack-tip field parameters

  3. A review of strategies for improving the degradation properties of laminated continuous-fiber/epoxy composites with carbon-based nanoreinforcements

    KAUST Repository

    Lubineau, Gilles; Rahaman, Ariful

    2012-01-01

    . To date, much work has been done on nano-reinforced polymers. However, few systematic studies concerning the effect of the nanoreinforcements on the mechanical properties on laminated composites were conducted. This paper presents a systematic review

  4. Numerical evaluation of delamination in CFRP laminates by stereo X-ray pictures

    International Nuclear Information System (INIS)

    Kunoo, Kazuo; Uda, Nobuhide; Ono, Kousei; Onohara, Kaoru; Takahashi, Toshiaki; Tanaka, Hisahiro.

    1989-01-01

    This paper presents a method for quantifying damage in composite laminates by stereo X-ray pictures. A three dimensional image of delamination, which is one of the characteristic types of damage in composite laminates can be reconstructed with this method. A digital image processing technique is used to analyze X-ray pictures. Experimental results of reconstructing delaminations in carbon/epoxy cross-ply laminates show that this method is accurate enough for practical usage. (author)

  5. [A preliminary study on the color effect of IPS Empress all-ceramic veneers].

    Science.gov (United States)

    Li, Zhi-yong; Cheng, Xiang-rong; Wang, Yi-ning

    2004-09-01

    To evaluate the opaquing capacity, color compatibility and stability of IPS Empress all-ceramic veneers. A total of 86 IPS Empress all-ceramic veneers were made for 18 patients. The patients were divided into three groups: Group A was tetracycline teeth, 64 veneers for 5 patients; Group B was non-tetracycline teeth, 22 veneers for 13 patients; Group C was 22 natural vital teeth with normal color as control group. Before and after veneers were inserted, ShadeEye NCC was employed to obtain L * a * b * values of each tooth. The values of cemented veneers used as the baseline, the L * a * b * values of each veneer were measured half a year, 1 year, and 2 years after restoration respectively. All L * a * b * values at different evaluation times were analyzed by SPSS 10.0. Before and after veneers were restored, the L * a * b * values of both Group A and Group B were significantly different, the color difference being 5.01 and 4.15 respectively. The color difference between Group A and selected shade guides was 2.45. Compared with the baseline value, the L * value of Group A significantly decreased 2 years after restoration, but the DeltaE of different evaluation times was not significantly different. The color difference between Group B and Group C was 0.22 and there was no significant color difference after restoration. IPS Empress all-ceramic veneers have excellent opaquing capacity, color compatibility and stability to non-tetracycline teeth. To tetracycline teeth IPS Empress all-ceramic veneers have a certain opaquing capacity, but they cannot completely match with shade guides; the L * value is significantly different after restoration and further studies are needed to evaluate its color effect.

  6. Analysis of interlaminar stresses in symmetric and unsymmetric laminates under various loadings

    Science.gov (United States)

    Leger, C. A.; Chan, W. S.

    1993-04-01

    A quasi-three-dimensional finite-element model is developed to investigate the interlaminar stresses in a composite laminate under combined loadings. An isoparametric quadrilateral element with eight nodes and three degrees of freedom per node is the finite element used in this study. The element is used to model a composite laminate cross section loaded by tension, torsion, transverse shear, and both beam and chord bending which are representative of loading in a helicopter rotor system. Symmetric and unsymmetric laminates are examined with comparisons made between the interlaminar stress distributions and magnitudes for each laminate. Unsymmetric results are compared favorably to limited results found in literature. The unsymmetric interlaminar normal stress distribution in a symmetric laminate containing a free edge delamination is also examined.

  7. Fracture toughness of Ti-Al3Ti-Al-Al3Ti laminate composites under static and cyclic loading conditions

    Science.gov (United States)

    Patselov, A. M.; Gladkovskii, S. V.; Lavrikov, R. D.; Kamantsev, I. S.

    2015-10-01

    The static and cyclic fracture toughnesses of a Ti-Al3Ti-Al-Al3Ti laminate composite material containing at most 15 vol % intermetallic compound are studied. Composite specimens are prepared by terminating reaction sintering of titanium and aluminum foils under pressure. The fracture of the titanium layers is quasi-cleavage during cyclic crack growth and is ductile during subsequent static loading.

  8. Numerical simulation of hot-pressed veneer products: Forming - Spring back – Distortion

    DEFF Research Database (Denmark)

    Ormarsson, Sigurdur; Sandberg, Dick

    2007-01-01

    Customers demand very high quality of veneered furniture products with regard to surface appearance, shape stability and stiffness. To meet these requirements, it is important to improve the manufacturing process by a better understanding of the thermo-hygro-mechanical behaviour of the individual...... veneers. During the manufacture of strongly curved products, the veneers are exposed to large membrane and bending deformations and to high pressure in the radial fibre direction. When hot-press forming is used, the veneers are also exposed to a high surface temperature during the pressing time (curing...... time). These severe conditions can result in plastic deformation perpendicular to the veneer surface as well as mechano-sorptive strains in the curved regions, since the heating can have a significant influence on the moisture distribution. How strong an influence these factors have on the distortion...

  9. Microstructural Evolution and Fracture Behavior of Friction-Stir-Welded Al-Cu Laminated Composites

    Science.gov (United States)

    Beygi, R.; Kazeminezhad, Mohsen; Kokabi, A. H.

    2014-01-01

    In this study, we attempt to characterize the microstructural evolution during friction stir butt welding of Al-Cu-laminated composites and its effect on the fracture behavior of the joint. Emphasis is on the material flow and particle distribution in the stir zone. For this purpose, optical microscopy and scanning electron microscopy (SEM) images, energy-dispersive spectroscopy EDS and XRD analyses, hardness measurements, and tensile tests are carried out on the joints. It is shown that intermetallic compounds exist in lamellas of banding structure formed in the advancing side of the welds. In samples welded from the Cu side, the banding structure in the advancing side and the hook formation in the retreating side determine the fracture behavior of the joint. In samples welded from the Al side, a defect is formed in the advancing side of the weld, which is attributed to insufficient material flow. It is concluded that the contact surface of the laminate (Al or Cu) with the shoulder of the FSW tool influences the material flow and microstructure of welds.

  10. Electrical behavior of laminated composites with intralaminar degradation: A comprehensive micro-meso homogenization procedure

    KAUST Repository

    Selvakumaran, Lakshmi

    2014-03-01

    Electrical Resistance Tomography (ERT) is a promising health monitoring technique to assess damage in laminated composites. Yet, the missing link between the various complex degradation mechanisms within the laminate and its global change in resistivity prevents ERT from being used as a quantitative technique. We propose an electrical mesomodel that can establish this link between the various microscale degradations and the resistivity changes in the measurements. The mesoscale homogenization of transverse cracks with local delamination of the ply is first described for in-plane electrical loading for both the outer and the inner plies. The mesoscale model is then extended to include the out-of-plane loading. The relationship between the mesoscale damage indicators and the degradation morphology is identified. These damage indicators are found to be intrinsic to the ply. As such, this defines the first step towards the interpretation of resistivity measurement in terms of micromechanical damage. © 2013 Elsevier Ltd.

  11. [Preliminary study of bonding strength between diatomite-based dental ceramic and veneering porcelains].

    Science.gov (United States)

    Lu, Xiao-li; Gao, Mei-qin; Cheng, Yu-ye; Zhang, Fei-min

    2015-04-01

    In order to choose the best veneering porcelain for diatomite-based dental ceramic substrate, the bonding strength between diatomite-based dental ceramics and veneering porcelains was measured, and the microstructure and elements distribution of interface were analyzed. The coefficient of thermal expansion (CTE) of diatomite-based dental ceramics was detected by dilatometry. Three veneering porcelain materials were selected with the best CTE matching including alumina veneering porcelain (group A), titanium porcelain veneering porcelain (group B), and E-max veneering porcelain (group C). Shear bonding strength was detected. SEM and EDS were used to observe the interface microstructure and element distribution. Statistical analysis was performed using SPSS 17.0 software package. The CTE of diatomite-based dental ceramics at 25-500 degrees centigrade was 8.85×10-6K-1. The diatomite-based substrate ceramics combined best with group C. Shear bonding strength between group A and C and group B and C both showed significant differences(P<0.05). SEM and EDS showed that the interface of group C sintered tightly and elements permeated on both sides of the interface. The diatomite-based substrate ceramics combines better with E-max porcelain veneer.

  12. Drilling of Hybrid Titanium Composite Laminate (HTCL) with Electrical Discharge Machining.

    Science.gov (United States)

    Ramulu, M; Spaulding, Mathew

    2016-09-01

    An experimental investigation was conducted to determine the application of die sinker electrical discharge machining (EDM) as it applies to a hybrid titanium thermoplastic composite laminate material. Holes were drilled using a die sinker EDM. The effects of peak current, pulse time, and percent on-time on machinability of hybrid titanium composite material were evaluated in terms of material removal rate (MRR), tool wear rate, and cut quality. Experimental models relating each process response to the input parameters were developed and optimum operating conditions with a short cutting time, achieving the highest workpiece MRR, with very little tool wear were determined to occur at a peak current value of 8.60 A, a percent on-time of 36.12%, and a pulse time of 258 microseconds. After observing data acquired from experimentation, it was determined that while use of EDM is possible, for desirable quality it is not fast enough for industrial application.

  13. Drilling of Hybrid Titanium Composite Laminate (HTCL with Electrical Discharge Machining

    Directory of Open Access Journals (Sweden)

    M. Ramulu

    2016-09-01

    Full Text Available An experimental investigation was conducted to determine the application of die sinker electrical discharge machining (EDM as it applies to a hybrid titanium thermoplastic composite laminate material. Holes were drilled using a die sinker EDM. The effects of peak current, pulse time, and percent on-time on machinability of hybrid titanium composite material were evaluated in terms of material removal rate (MRR, tool wear rate, and cut quality. Experimental models relating each process response to the input parameters were developed and optimum operating conditions with a short cutting time, achieving the highest workpiece MRR, with very little tool wear were determined to occur at a peak current value of 8.60 A, a percent on-time of 36.12%, and a pulse time of 258 microseconds. After observing data acquired from experimentation, it was determined that while use of EDM is possible, for desirable quality it is not fast enough for industrial application.

  14. The influence of lathe check depth and orientation on the bond quality of phenol-formaldehyde-bonded birch plywood

    Science.gov (United States)

    Anti Rohumaa; Christopher G. Hunt; Mark Hughes; Charles R. Frihart; Janne Logren

    2013-01-01

    During the rotary peeling of veneer for plywood or the laminated veneer lumber manufacture, checks are formed in the veneer that are as deep as 70 – 80 % of the veneer thickness. The results of this study show that, during adhesive bond testing, deep lathe checks in birch (Betula pendula Roth.) veneer significantly reduce the shear strength and the...

  15. A Practical Method of Acoustic Emission Source Location in Anisotropic Composite Laminates

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Jeong Kon; Kang, Yong Kyu; Kwon, Oh Yang [Inha University, Incheon (Korea, Republic of)

    2003-06-15

    Since the velocity is dependent on the fiber orientation in anisotropic composites, the application of traditional acoustic emission (AE) source location techniques based on the constant velocity to composite structures has been practically impossible. The anisotropy makes the source location procedure complicated and deteriorates the accuracy of the location. In this study, we have divided the region of interest(ROI) into a set of finite elements, taken each element as a virtual source, and calculated the arrival time differences between sensors by using the velocities at every degree from 0 to 90. The calculated and the experimentally measured values of the arrival time difference aye then compared to minimize the location error. The results from two different materials, namely AA6061-T6 and CFRP(uni-directional; UD, [0]{sub 32}4 ) laminate confirmed the practical usefulness of the proposed method

  16. Veneer industry and timber use, North Central Region, 1980.

    Science.gov (United States)

    James E. Blyth; W. Brad Smith

    1984-01-01

    Shows 1980 veneer-log production and receipts by species in the Lake State (Michigan, Minnesota, and Wisconsin) and in the Central States (Illinois, Indiana, Iowa, and Missouri). Comparisons are made with similar data collected in 1976. Includes tables showing veneer-log production and receipts (for selected years) since 1946 in the Lake States and since 1956 in the...

  17. Veneer-log production and receipts, North Central Region, 1976.

    Science.gov (United States)

    James E. Blyth; Jerold T. Hahn

    1978-01-01

    Shows 1976 veneer-log production and receipts by species in the Lake States (Michigan, Minnesota, and Wisconsin) and in the Central States (Illinois, Indiana, Iowa, and Missouri). Comparisons are made with similar data for 1974. Includes tables showing veneer-log production and receipts (for selected years) since 1946 in the Lake States and since 1956 in the Central...

  18. Veneer-log production and receipts, North Central Region, 1974.

    Science.gov (United States)

    James E. Blyth; Jerold T. Hahn

    1976-01-01

    Shows 1974 veneer-log production and receipts by species in the Lake States (Michigan, Minnesota, and Wisconsin) and in the Central States (Illinois, Indiana, Iowa, and Missouri). Comparisons are made with similar data for 1972. Includes tables showing veneer-log production and receipts (for selected years) since 1946 in the Lake States and since 1956 in the Central...

  19. Experimental Studies on Strength Behaviour of Notched Glass/Epoxy Laminated Composites under Uni-axial and Bi-axial Loading

    Science.gov (United States)

    Guptha, V. L. Jagannatha; Sharma, Ramesh S.

    2017-11-01

    The use of FRP composite materials in aerospace, aviation, marine, automotive and civil engineering industry has increased rapidly in recent years due to their high specific strength and stiffness properties. The structural members contrived from such composite materials are generally subjected to complex loading conditions and leads to multi-axial stress conditions at critical surface localities. Presence of notches, much required for joining process of composites, makes it further significant. The current practice of using uni-axial test data alone to validate proposed material models is inadequate leading to evaluation and consideration of bi-axial test data. In order to correlate the bi-axial strengths with the uni-axial strengths of GFRP composite laminates in the presence of a circular notch, bi-axial tests using four servo-hydraulic actuators with four load cells were carried out. To determine the in-plane strength parameters, bi-axial cruciform test specimen model was considered. Three different fibre orientations, namely, 0°, 45°, and 90° are considered with a central circular notch of 10 mm diameter in the present investigation. From the results obtained, it is observed that there is a reduction in strength of 5.36, 2.41 and 13.92% in 0°, 45°, and 90° fibre orientation, respectively, under bi-axial loading condition as compared to that of uni-axial loading in laminated composite.

  20. Hybrid Laminates for Application in North Conditions

    Science.gov (United States)

    Antipov, V. V.; Oreshko, E. I.; Erasov, V. S.; Serebrennikova, N. Yu.

    2016-11-01

    A hybrid aluminum-lithium alloy/SIAL laminate as a possible material for application in structures operated in North conditions is considered. The finite-element method is used for a buckling stability analysis of hybrid panels, bars, and plates. A technique allowing one to compare the buckling stability of multilayered hybrid plates is offered. Compression tests were run on a hybrid laminate wing panel as a prototype of the top panel of TU-204SM airplane made from a high-strength B95T2 aluminum alloy. It turned out that the lighter composite panel had a higher load-carrying capacity than the aluminum one. Results of investigation into the properties the hybrid aluminum-lithium alloy/SIAL laminate and an analysis of scientific-technical data on this subject showed that this composite material could be used in the elements of airframes, including those operated in north conditions.

  1. Fracture and Fatigue Resistance of Cemented versus Fused CAD-on Veneers over Customized Zirconia Implant Abutments.

    Science.gov (United States)

    Nossair, Shereen Ahmed; Aboushelib, Moustafa N; Morsi, Tarek Salah

    2015-01-05

    To evaluate the fracture mechanics of cemented versus fused CAD-on veneers on customized zirconia implant abutments. Forty-five identical customized CAD/CAM zirconia implant abutments (0.5 mm thick) were prepared and seated on short titanium implant abutments (Ti base). A second scan was made to fabricate 45 CAD-on veneers (IPS Empress CAD, A2). Fifteen CAD-on veneers were cemented on the zirconia abutments (Panavia F2.0). Another 15 were fused to the zirconia abutments using low-fusing glass, while manually layered veneers served as control (n = 15). The restorations were subjected to artificial aging (3.2 million cycles between 5 and 10 kg in a water bath at 37°C) before being axially loaded to failure. Fractured specimens were examined using scanning electron microscopy to detect fracture origin, location, and size of critical crack. Stress at failure was calculated using fractography principles (alpha = 0.05). Cemented CAD-on restorations demonstrated significantly higher (F = 72, p CAD-on and manually layered restorations. Fractographic analysis of fractured specimens indicated that cemented CAD-on veneers failed due to radial cracks originating from the veneer/resin interface. Branching of the critical crack was observed in the bulk of the veneer. Fused CAD-on veneers demonstrated cohesive fracture originating at the thickest part of the veneer ceramic, while manually layered veneers failed due to interfacial fracture at the zirconia/veneer interface. Within the limitations of this study, cemented CAD-on veneers on customized zirconia implant abutments demonstrated higher fracture than fused and manually layered veneers. © 2014 by the American College of Prosthodontists.

  2. The analysis of thin walled composite laminated helicopter rotor with hierarchical warping functions and finite element method

    Science.gov (United States)

    Zhu, Dechao; Deng, Zhongmin; Wang, Xingwei

    2001-08-01

    In the present paper, a series of hierarchical warping functions is developed to analyze the static and dynamic problems of thin walled composite laminated helicopter rotors composed of several layers with single closed cell. This method is the development and extension of the traditional constrained warping theory of thin walled metallic beams, which had been proved very successful since 1940s. The warping distribution along the perimeter of each layer is expanded into a series of successively corrective warping functions with the traditional warping function caused by free torsion or free bending as the first term, and is assumed to be piecewise linear along the thickness direction of layers. The governing equations are derived based upon the variational principle of minimum potential energy for static analysis and Rayleigh Quotient for free vibration analysis. Then the hierarchical finite element method is introduced to form a numerical algorithm. Both static and natural vibration problems of sample box beams are analyzed with the present method to show the main mechanical behavior of the thin walled composite laminated helicopter rotor.

  3. Study on long term creep of two different types of compressed wood sheets used in library shelves

    Directory of Open Access Journals (Sweden)

    Saeid Azimi

    2016-12-01

    Full Text Available In this study, the creep behaviors of composite panels used in library shelves were investigated. For this purpose, two types of wood-composite panels (medium density fiberboard and particleboard, and three types of covering including synthetic laminates, natural veneer, and without cove, and two types of wood joints (fixed and detachable were used. Dimensions of the book-shelves were in actual shelf size, that is, 1,000 × 300 mm. Totally, 48 shelf specimens were prepared. For the creep test, a 23.5 kg loading level was applied in the center part of the shelves. Measurements on the creep behavior were carried out over 155 days at different intervals. Results indicated that the type of wood-composite as well as the type of veneer had statistically significant effect on the creep behaviors of panels. The lowest creep was observed in MDF panels. Moreover, those panels covered with natural veneer demonstrated significantly lower creep values. The type of joint also had a significant effect on the creeping behavior of the shelves, though not as conspicuous as the type of panels and veneers. Based on the results of the present research project, it is suggested that in order to increase the service life of library shelves it would be better to produce the shelves from MDF panels covered with natural veneers; these shelves should be fixed on supports.

  4. Color management of porcelain veneers: influence of dentin and resin cement colors.

    Science.gov (United States)

    Dozic, Alma; Tsagkari, Maria; Khashayar, Ghazal; Aboushelib, Moustafa

    2010-01-01

    Porcelain veneers have become an interesting treatment option to correct the shape and color of anterior teeth. Because of their limited thickness and high translucency, achieving a good color match is influenced by several variables. The aim of this work was to investigate the influence of natural dentin and resin cement colors on final color match of porcelain veneers. A preselected shade tab (A1) was chosen as the target color for a maxillary central incisor, and its color parameters (L*a*b*) were measured using a digital spectrophotometer (SpectroShade, MHT). Nine natural dentin colors (Natural Die Material, Ivoclar Vivadent) representing a wide range of tooth colors were used to prepare resin replicas of the maxillary central incisor with a standard preparation for porcelain veneers. The prepared porcelain veneers (IPS Empress Esthetic, A1, 0.6 mm thick, Ivoclar Vivadent) were cemented on the resin dies (nine groups of natural dentin colors) using seven shades of resin cement (Variolink Veneers, Ivoclar Vivadent). The L*a*b* values of the cemented veneers were measured, and DE values were calculated against the preselected target color (A1). DE greater than 3.3 was considered as a significant color mismatch detectable by the human eye. The seven shades of resin cement had no significant influence on the final color of the veneers, as the measured DE values were almost identical for every test group. On the other hand, the color of natural dentin was a significant factor that influenced final color match. None of the 63 tested combinations (nine natural dentin colors and seven resin cement colors) produced an acceptable color match. Thin porcelain veneers cannot mask underlying tooth color even when different shades of resin cement are used. Incorporation of opaque porcelain (high chroma) may improve final color match.

  5. Damage prognosis of adhesively-bonded joints in laminated composite structural components of unmanned aerial vehicles

    Energy Technology Data Exchange (ETDEWEB)

    Farrar, Charles R [Los Alamos National Laboratory; Gobbato, Maurizio [UCSD; Conte, Joel [UCSD; Kosmatke, John [UCSD; Oliver, Joseph A [UCSD

    2009-01-01

    The extensive use of lightweight advanced composite materials in unmanned aerial vehicles (UAVs) drastically increases the sensitivity to both fatigue- and impact-induced damage of their critical structural components (e.g., wings and tail stabilizers) during service life. The spar-to-skin adhesive joints are considered one of the most fatigue sensitive subcomponents of a lightweight UAV composite wing with damage progressively evolving from the wing root. This paper presents a comprehensive probabilistic methodology for predicting the remaining service life of adhesively-bonded joints in laminated composite structural components of UAVs. Non-destructive evaluation techniques and Bayesian inference are used to (i) assess the current state of damage of the system and, (ii) update the probability distribution of the damage extent at various locations. A probabilistic model for future loads and a mechanics-based damage model are then used to stochastically propagate damage through the joint. Combined local (e.g., exceedance of a critical damage size) and global (e.g.. flutter instability) failure criteria are finally used to compute the probability of component failure at future times. The applicability and the partial validation of the proposed methodology are then briefly discussed by analyzing the debonding propagation, along a pre-defined adhesive interface, in a simply supported laminated composite beam with solid rectangular cross section, subjected to a concentrated load applied at mid-span. A specially developed Eliler-Bernoulli beam finite element with interlaminar slip along the damageable interface is used in combination with a cohesive zone model to study the fatigue-induced degradation in the adhesive material. The preliminary numerical results presented are promising for the future validation of the methodology.

  6. Development and qualification of polymeric matrix laminated composites for repair for piping and pipelines; Desenvolvimento e qualificacao de compositos laminados de matriz polimerica para o reparo de dutos e tubulacoes industriais

    Energy Technology Data Exchange (ETDEWEB)

    Rohem, N.R.F.; Sampaio, E.M.; Queiroz, R.A.; Cortines, V.J. [Universidade do Estado do Rio de Janeiro (LAA/UERJ), Campus Regional - Instituto Politecnico (IPRJ) - Laboratorio de Adesao e Aderencia, Nova Friburgo, RJ (Brazil)], e-mail: nrohem@iprj.uerj.br

    2010-07-01

    The use of polymeric matrix composites to repair and strengthen structures in the oil industry has become a common industry practice. In the year of 2006 the ISO/PDTS 24817 'Petroleum, petrochemical and natural gas industries - Qualification, design, installation, testing and inspection' was presented. This study presents the development of a new laminate, manual lamination process, and some of the certifying tests in accordance with ISO, for through-wall damage repairs. The test consists of applying the composite laminate repair in 9 carbon steel tubes, NPS6, with 600mm of length, with drilled holes of 10, 15, and 25mm. After the curing time a hydrostatic test is performed. The laminate must fail by delamination at the substrate/composite interface. With this test we obtain the {lambda}LCL (energy release rate), used to determine the thickness of the repair applied in tubes with through-wall damage. (author)

  7. Comparison of Open-Hole Compression Strength and Compression After Impact Strength on Carbon Fiber/Epoxy Laminates for the Ares I Composite Interstage

    Science.gov (United States)

    Hodge, Andrew J.; Nettles, Alan T.; Jackson, Justin R.

    2011-01-01

    Notched (open hole) composite laminates were tested in compression. The effect on strength of various sizes of through holes was examined. Results were compared to the average stress criterion model. Additionally, laminated sandwich structures were damaged from low-velocity impact with various impact energy levels and different impactor geometries. The compression strength relative to damage size was compared to the notched compression result strength. Open-hole compression strength was found to provide a reasonable bound on compression after impact.

  8. Teaching learning algorithm based optimization of kerf deviations in pulsed Nd:YAG laser cutting of Kevlar-29 composite laminates

    Science.gov (United States)

    Gautam, Girish Dutt; Pandey, Arun Kumar

    2018-03-01

    Kevlar is the most popular aramid fiber and most commonly used in different technologically advanced industries for various applications. But the precise cutting of Kevlar composite laminates is a difficult task. The conventional cutting methods face various defects such as delamination, burr formation, fiber pullout with poor surface quality and their mechanical performance is greatly affected by these defects. The laser beam machining may be an alternative of the conventional cutting processes due to its non-contact nature, requirement of low specific energy with higher production rate. But this process also faces some problems that may be minimized by operating the machine at optimum parameters levels. This research paper examines the effective utilization of the Nd:YAG laser cutting system on difficult-to-cut Kevlar-29 composite laminates. The objective of the proposed work is to find the optimum process parameters settings for getting the minimum kerf deviations at both sides. The experiments have been conducted on Kevlar-29 composite laminates having thickness 1.25 mm by using Box-Benkhen design with two center points. The experimental data have been used for the optimization by using the proposed methodology. For the optimization, Teaching learning Algorithm based approach has been employed to obtain the minimum kerf deviation at bottom and top sides. A self coded Matlab program has been developed by using the proposed methodology and this program has been used for the optimization. Finally, the confirmation tests have been performed to compare the experimental and optimum results obtained by the proposed methodology. The comparison results show that the machining performance in the laser beam cutting process has been remarkably improved through proposed approach. Finally, the influence of different laser cutting parameters such as lamp current, pulse frequency, pulse width, compressed air pressure and cutting speed on top kerf deviation and bottom kerf

  9. Parametric study on patch repaired CFRP laminates using FEA

    Energy Technology Data Exchange (ETDEWEB)

    Kashfuddoja, M.; Ramji, M. [Indian Institute of Technology. Engineering Optics Lab. Dept. of Mechanical Engineering, Hyderabad (India)

    2012-07-01

    Carbon fibre reinforced plastic (CFRP) composite laminates have become popular for structural applications as they are lighter, stronger and tougher. Composite structures are also susceptible to damage while in service. For improved service life, the damage needs to be repaired so that repair structure integrity is enhanced. Various parameters like patch size and shape, it's layup sequence and adhesive thickness would influence the performance of the repaired structure. In present work, a parametric study is carried out using finite element analysis (FEA) to investigate the influence of various parameters involved in composite repair. The panel is made of carbon / epoxy composite laminate with stacking sequence of (0/{+-}45/900)s and is subjected to tensile load. Damaged CFRP laminates is repaired by symmetrical patch adhesively bonded over the damaged area. Circular patch of different stacking sequence and size is considered. Influence of adhesive material and it's thickness on repair efficiency is also investigated. The influence of various repair parameters on peel stress is also analysed. (Author)

  10. Damage in woven CFRP laminates subjected to low velocity impacts

    International Nuclear Information System (INIS)

    Ullah, H; Abdel-Wahab, A A; Harland, A R; Silberschmidt, V V

    2012-01-01

    Carbon fabric-reinforced polymer (CFRP) composites used in sports products can be exposed to different in-service conditions such as large dynamic bending deformations caused by impact loading. Composite materials subjected to such loads demonstrate various damage modes such as matrix cracking, delamination and, ultimately, fabric fracture. Damage evolution in these materials affects both their in-service properties and performance that can deteriorate with time. These processes need adequate means of analysis and investigation, the major approaches being experimental characterisation and non-destructive examination of internal damage in composite laminates. This research deals with a deformation behaviour and damage in woven composite laminates due to low-velocity dynamic out-of-plane bending. Experimental tests are carried out to characterise the behaviour of such laminates under large-deflection dynamic bending in un-notched specimens in Izod tests using a Resil Impactor. A series of low-velocity impact tests is carried out at various levels of impact energy to assess the energy absorbed and force-time response of CFRP laminates. X-ray micro computed tomography (micro-CT) is used to investigate material damage modes in the impacted specimens. X-ray tomographs revealed that through-thickness matrix cracking, inter-ply delamination and intra-ply delamination, such as tow debonding and fabric fracture, were the prominent damage modes.

  11. INFLUÊNCIA DE DIFERENTES COMBINAÇÕES DE LÂMINAS DE Eucalyptus saligna E Pinus taeda EM PAINÉIS LVL

    Directory of Open Access Journals (Sweden)

    Marcos Theodoro Müller

    2015-01-01

    Full Text Available This research aimed to investigate the influence of the positioning of Eucalyptus saligna and Pinus taeda wood veneers on layers of laminated veneer lumber (LVL panels. The compositions were manufactured in six different combinations of five veneers of 3.2 mm thickness, glued with phenol-formaldehyde, resulting in treatments composed of wood of the same species or with a combination of two wood types. The evaluation of the proposed arrangements was performed under the characterization of physical properties (moisture content and density and mechanical properties (modulus of elasticity – MOE and modulus of rupture – MOR verified in flatwise and edgewise static bending tests. The results obtained indicated that, in most situations, the different positions of the veneers with higher density (in the outer, intermediate and inner layers influenced the mechanical properties of the panels. The influence detected was varied for MOE and MOR, especially when comparing the flatwise and edgewise test values. In certain positions, on the layers of the LVL compositions, the presence of eucalypt veneers resulted in stiffness and strength increases. However, the treatments formed by interposed veneers of eucalypt and pine demonstrated interesting performances for structural use, in either flatwise or edgewise position, once they present values of MOE and MOR that allow to distinguish them as 1st class, according to the North American standard APA/EWS PRL–501 (2001.

  12. Three-unit posterior zirconia-ceramic fixed dental prostheses (FDPs) veneered with layered and milled (CAD-on) veneering ceramics: 1-year follow-up of a randomized controlled clinical trial.

    Science.gov (United States)

    Grohmann, Philipp; Bindl, Andreas; Hämmerle, Christoph; Mehl, Albert; Sailer, Irena

    2015-01-01

    The aim of this multicenter randomized controlled clinical trial was to test posterior zirconia-ceramic fixed dental prostheses (FDPs) veneered with a computer-aided design/computer- assisted manufacture (CAD/CAM) lithium disilicate veneering ceramic (CAD-on) and manually layered zirconia veneering ceramic with respect to survival of the FDPs, and technical and biologic outcomes. Sixty patients in need of one posterior three-unit FDP were included. The zirconia frameworks were produced with a CAD/CAM system (Cerec inLab 3D/Cerec inEOS inLab). Thirty FDPs were veneered with a CAD/CAM lithium disilicate veneering ceramic (Cad-on) (test) and 30 were veneered with a layered zirconia veneering ceramic (control). For the clinical evaluation at baseline, 6, and 12 months, the United States Public Health Service (USPHS) criteria were used. The biologic outcome was judged by comparing the plaque control record (PCR), bleeding on probing (BOP), and probing pocket depth (PPD). Data were statistically analyzed. Fifty-six patients were examined at a mean follow-up of 13.9 months. At the 1-year follow-up the survival rate was 100% in the test and in the control group. No significant differences of the technical outcomes occurred. Major chipping occurred in the control group (n = 3) and predominantly minor chipping in the test group (minor n = 2, major n = 1). No biologic problems or differences were found. Both types of zirconia-ceramic FDPs exhibited very good clinical outcomes without differences between groups. Chipping occurred in both types of FDPs at small amounts, yet the extension of the chippings differed. The test FDPs predominantly exhibited minor chipping, the control FDPs major chipping.

  13. Cyclic testing of porcelain laminiate veneers on superficial enamel and dentin: Pressed vs. conventional layered porcelain

    Science.gov (United States)

    Tawde, Shweta

    Statement of Problem: Clinicians are inclined towards more aggressive teeth preparations to accommodate the thickness of the veneering material. The principle of conservative tooth preparation is compromised. Purpose: By using a conservative approach to treatment with porcelain veneers, long-lasting, esthetic and functional results may be achieved. Sacrificing as little tooth structure as possible and conserving the supporting tissues will facilitate prospective patients. Materials and Methods: Forty extracted human maxillary and mandibular canines were selected. The teeth were divided into one of two groups (pressable and stackable) and further subdivided according to tooth substrate (all-enamel or mixed enamel-dentin exposure). Twenty canine teeth were allotted to the pressable veneer group and 20 were allotted to the stackable veneer group. Of the 20 teeth in the pressable group, all were pressed with a lithium disilicate ceramic system (IPS e.max Press), 10 with labial tooth reduction of 0.3-0.5 mm maintaining superficial enamel (PEN) and the remaining 10 teeth with labial veneer reduction of 0.8-1.0 mm exposing superficial dentin (PDN). Of the 20 teeth in the stackable group, all were stacked/ layered with conventional feldspathic porcelain (Fortune; Williams/ Ivoclar); with labial veneer reduction of 0.3-0.5 mm maintaining superficial enamel (SEN) and the remaining 10 teeth with labial veneer reduction of 0.8-1.0 mm exposing superficial dentin (SDN). Silicon putty matrix was fabricated prior to teeth preparation to estimate the teeth reduction. The prepared facial reduction was limited to the incisal edge. No incisal or palatal/lingual reduction was performed. Impressions of the prepared teeth were taken in medium/light-bodied PVS. Master casts were made in Resin Rock. The stackable group specimens were made with fabricating refractory dies and after following the recommended steps of laboratory procedure, stackable veneers were processed. The pressable group

  14. Enhancement of Gas Barrier Properties of CFRP Laminates Fabricated Using Thin-Ply Prepregs

    Science.gov (United States)

    横関, 智弘; 高木, 智宏; 吉村, 彰記; Ogasawara, Toshio; 荻原, 慎二

    Composite laminates manufactured using thin-ply prepregs are expected to have superior resistance properties against microcracking compared to those using standard prepregs. In this study, comparative investigations are presented on the microcrack accumulation and gas leakage characteristics of CFRP laminates fabricated using standard and thin-ply prepregs, consisting of high-performance carbon fiber and toughened epoxy, as a fundamental research on the cryogenic composite tanks for future space vehicles. It was shown that laminates using thin-ply prepregs exhibited much higher strain at microcrack initiation compared to those using standard prepregs at room and cryogenic temperatures. In addition, helium gas leak tests using CFRP laminated tubular specimens subjected to quasi-static tension loadings were performed. It was demonstrated that CFRP laminates using thin-ply prepregs have higher gas barrier properties than those using standard prepregs.

  15. Developing and Evaluating Composites Based on Plantation Eucalyptus Rotary-cut Veneer and High-density Polyethylene Film as Novel Building Materials

    Directory of Open Access Journals (Sweden)

    Wei Song

    2016-02-01

    Full Text Available To achieve value-added utilizations of plantation timbers, eucalyptus veneer/high-density polyethylene film composites were prepared, with process-factors (PF (hot-pressing temperature, HT; hot-pressing duration, HD; hot-pressing pressure, HP; HDPE-film content, HC and composite-properties (CP (water-resistant bonding-strength, BS; modulus of rupture, MOR; modulus of elasticity, MOE investigated. According to thermal analyses, 140 to 180 °C was appropriate for HT. Based on statistical analyses, HD was easier to affect CP, while MOE was easier to be affected by PF. Quantitative relationships between PF and CP were determined by the neural-network (ANN modeling. In ANN simulation surveys, CP displayed Gaussian distributions (R2 > 0.9 when PF changed in current ranges, with positive correlations between BS and MOR (R2 ≈ 0.5. Combining ANN and the genetic-algorithm, optimal processes (HT, 160 °C; HD, 50 s/mm; HP, 1.3 MPa; HC, 6 layers were found, and optimal results (BS, 1.30 MPa; MOR, 86.94 MPa; MOE, 8.33 GPa were comparable to various reported poplar-plywoods. Microscopic images demonstrated that composite interfaces were formed by the mechanical interlocking. The optimal BS attained Chinese standards for water-resistant plywoods, so proposed composites can serve as water-resistant and formaldehyde-free building materials for furniture and interior design.

  16. Effects of interface roughness on the annealing behaviour of laminated Ti-Al composite deformed by hot rolling

    DEFF Research Database (Denmark)

    Du, Y.; Fan, G.H.; Yu, Tianbo

    2015-01-01

    A laminated Ti-Al composite has been fabricated by hot compaction and hot rolling of alternate layers of commercial purity Ti and Al sheets with a thickness of 200 μm. The hot compaction temperature was 500˚C and in a following step the composite has been reduced 50% in thickness by hot rolling....... The fully consolidated composite has been annealed at 300˚C and 500˚C for different length of time. As a result of the differences in crystal structure and mechanical properties between Ti and Al protrusions and retrusions formed at the interface. A heterogeneous interface has thereby been created...

  17. A novel adaptive sun tracker for spacecraft solar panel based on hybrid unsymmetric composite laminates

    Science.gov (United States)

    Wu, Zhangming; Li, Hao

    2017-11-01

    This paper proposes a novel adaptive sun tracker which is constructed by hybrid unsymmetric composite laminates. The adaptive sun tracker could be applied on spacecraft solar panels to increase their energy efficiency through decreasing the inclined angle between the sunlight and the solar panel normal. The sun tracker possesses a large rotation freedom and its rotation angle depends on the laminate temperature, which is affected by the light condition in the orbit. Both analytical model and finite element model (FEM) are developed for the sun tracker to predict its rotation angle in different light conditions. In this work, the light condition of the geosynchronous orbit on winter solstice is considered in the numerical prediction of the temperatures of the hybrid laminates. The final inclined angle between the sunlight and the solar panel normal during a solar day is computed using the finite element model. Parametric study of the adaptive sun tracker is conducted to improve its capacity and effectiveness of sun tracking. The improved adaptive sun tracker is lightweight and has a state-of-the-art design. In addition, the adaptive sun tracker does not consume any power of the solar panel, since it has no electrical driving devices. The proposed adaptive sun tracker provides a potential alternative to replace the traditional sophisticated electrical driving mechanisms for spacecraft solar panels.

  18. Gravity Effects of Curing Angle on Laminated Composite Structures: A Review on Novel Study

    Directory of Open Access Journals (Sweden)

    T. T. T. Jennise

    2013-01-01

    Full Text Available Composites manufactured by small and medium industries/entrepreneurs (SMI/E are conventionally cured in the horizontal position. Hence, the confined space restricts optimum productivity. Besides, SMI/E is unable to allocate high budget for high-end technology such as autoclave and vacuum mechanical oven which limits the development of SMI/E as a result of high capital cost. Through a series of literature review, the review confirmed that there is no similar scientific study has been conducted. Consequently, the review is carried out to facilitate the investigation of the feasibility of a gravity cured glass fiber laminated thermosetting composites via vacuum bagging at angle position from horizontal (0° to vertical (90° to enhance the curing space required.

  19. Three-Point Bending Tests of Zirconia Core/Veneer Ceramics for Dental Restorations

    Directory of Open Access Journals (Sweden)

    Massimo Marrelli

    2013-01-01

    Full Text Available Introduction. The mechanical strength and the surface hardness of commercially available yttrium-doped zirconia were investigated. Furthermore, a comparative study of eight different ceramic veneers, to be used for the production of two-layered all-ceramic restorative systems, was carried out. Materials and Methods. Four types of zirconia specimens were analyzed, according to a standard ISO procedure (ISO 6872. Besides, two-layered zirconia-veneer specimens were prepared for three-point bending tests. Results. A strong effect of the surface roughness on the mechanical strength of zirconia specimens was observed. Finally, a comparative study of eight commercially available veneering ceramics shows different modes of failure between the selected veneers. Conclusion. The results indicate that close attention should be paid to the preparation of zirconia-based crowns and bridges by CAD/CAM process, because surface roughness has an important effect on the mechanical strength of the material. Finally, the results of the mechanical tests on two-layered specimens represent an important support to the choice of the veneering ceramic.

  20. Static and dynamic through thickness lamina properties of thick laminates

    NARCIS (Netherlands)

    Lahuerta, F.; Nijssen, R.P.L.; Van der Meer, F.P.; Sluys, L.J.

    2015-01-01

    Thick laminates are increasingly present in large composites structures such as wind turbine blades. Different factors are suspected to be involved in the decreased static and dynamic performance of thick laminates. These include the effect of self-heating, the scaling effect, and the manufacturing

  1. Fabrication of Hydrophobic Surface on Wood Veneer via Electroless Nickel Plating Combined with Chemical Corrosion

    Directory of Open Access Journals (Sweden)

    Zhaojun Tang

    2015-12-01

    Full Text Available Birch veneers were coated with Ni-P films by a combined process of KBH4 activation and electroless plating. The plated veneers were further chemically corroded to obtain hydrophobic surfaces on wood. The effect of chemical corrosion on the contact angle of the veneers was investigated. The hydrophobic veneers were characterized by X-ray photo electron spectroscopy (XPS, scanning electron microscopy (SEM, and X-ray diffraction (XRD. The surface contact angle of birch veneer before and after it was plated with Ni-P alloy coating was 41º and 121º, respectively. The contact angle reached 136.7º when the nickel-coated veneers were corroded in CuSO4 aqueous solution for 30 min. XPS analysis showed that Cu0 cluster doped with little CuO formed on the corroded surface of Ni-P alloy film after chemical corrosion. SEM and XRD showed that rough copper clusters formed on the surface of the wood veneer and revealed the reason of the surface hydrophobicity. This study provides a new pathway for fabricating hydrophobic wood.

  2. Experimental Study and Numerical Modelling of Low Velocity Impact on Laminated Composite Reinforced with Thin Film Made of Carbon Nanotubes

    Science.gov (United States)

    El Moumen, A.; Tarfaoui, M.; Hassoon, O.; Lafdi, K.; Benyahia, H.; Nachtane, M.

    2018-04-01

    In this work, polymer laminated composites based on Epon 862 Epoxy resin, T300 6 k carbon fibers and carbon nanotubes (CNTs) were tested with the aim to elucidate the effect of CNTs on impact properties including impact force and capacity to absorb impact energy. The polymer matrix was reinforced by a random distribution of CNTs with fraction ranging from 0.5 to 4.wt%. Composite panels were manufactured by using the infusion process. Taylor impact test was used to obtain the impact response of specimens. Projectile manufactured from a high strength and hardened steel with a diameter of 20 mm and 1.5 kg of mass was launched by a compressed gas gun within the velocity of 3 m/s. Impact force histories and absorbed energy of specimens were recorded. A numerical model was employed to simulate the impact performance. This model has been accomplished by forming a user established subroutine (VUMAT) and executing it in ABAQUS software. Finally, the effect of CNTs amount on dynamic properties of laminated composites was discussed.

  3. Composites

    International Nuclear Information System (INIS)

    Kasen, M.B.

    1983-01-01

    This chapter discusses the roles of composite laminates and aggregates in cryogenic technology. Filamentary-reinforced composites are emphasized because they are the most widely used composite materials. Topics considered include composite systems and terminology, design and fabrication, composite failure, high-pressure reinforced plastic laminates, low-pressure reinforced plastics, reinforced metals, selectively reinforced structures, the effect of cryogenic temperatures, woven-fabric and random-mat composites, uniaxial fiber-reinforced composites, composite joints in cryogenic structures, joining techniques at room temperature, radiation effects, testing laminates at cryogenic temperatures, static and cyclic tensile testing, static and cyclic compression testing, interlaminar shear testing, secondary property tests, and concrete aggregates. It is suggested that cryogenic composite technology would benefit from the development of a fracture mechanics model for predicting the fitness-for-purpose of polymer-matrix composite structures

  4. Permeability Testing of Impacted Composite Laminates for Use on Reusable Launch Vehicles

    Science.gov (United States)

    Nettles, A. T.

    2001-01-01

    Since composite laminates are beginning to be identified for use in reusable launch vehicle propulsion systems, an understanding of their permeance is needed. A foreign object impact event can cause a localized area of permeability (leakage) in a polymer matrix composite, and it is the aim of this study to assess a method of quantifying permeability-after-impact results. A simple test apparatus is presented, and variables that could affect the measured values of permeability-after-impact were assessed. Once it was determined that valid numbers were being measured, a fiber/resin system was impacted at various impact levels and the resulting permeability measured, first with a leak check solution (qualitative) then using the new apparatus (quantitative). The results showed that as the impact level increased, so did the measured leakage. As the pressure to the specimen was increased, the leak rate was seen to increase in a nonlinear fashion for almost all the specimens tested.

  5. Self-heating forecasting for thick laminates testing coupons in fatigue

    NARCIS (Netherlands)

    Lahuerta, F.; Westphal, T.; Nijssen, R.P.L.

    2012-01-01

    Thick laminate sections can be found from the tip to the root in most common wind turbine blade designs. Obtaining accurate and reliable design data for thick laminates is subject of investigations. Due to the poor thermal conductivity properties of composites and the material self-heating that

  6. In situ polymerization of polyaniline in wood veneers.

    Science.gov (United States)

    Trey, Stacy; Jafarzadeh, Shadi; Johansson, Mats

    2012-03-01

    The present study describes the possibility to polymerize aniline within wood veneers to obtain a semi-conducting material with solid wood acting as the base template. It was determined that it is possible to synthesize the intrinsically conductive polymer (ICP) polyaniline in situ within the wood structure of Southern yellow pine veneers, combining the strength of the natural wood structure with the conductivity of the impregnated polymer. It was found that polyaniline is uniformly dispersed within the wood structure by light microscopy and FT-IR imaging. A weight percent gain in the range of 3-12 wt % was obtained with a preferential formation in the wood structure and cell wall, rather than in the lumen. The modified wood was found to be less hydrophilic with the addition of phosphate doped polyaniline as observed by equilibrium water swelling studies. While wood itself is insulating, the modified veneers had conductivities of 1 × 10(-4) to 1 × 10(-9) S cm(-1), demonstrating the ability to tune the conductivity and allowing for materials with a wide range of applications, from anti-static to charge-dispersing materials. Furthermore, the modified veneers had lower total and peak heat releases, as determined by cone calorimetry, because of the char properties of the ICP. This is of interest if these materials are to be used in building and furniture applications where flame retardance is of importance. © 2012 American Chemical Society

  7. Bioinspired Transparent Laminated Composite Film for Flexible Green Optoelectronics.

    Science.gov (United States)

    Lee, Daewon; Lim, Young-Woo; Im, Hyeon-Gyun; Jeong, Seonju; Ji, Sangyoon; Kim, Yong Ho; Choi, Gwang-Mun; Park, Jang-Ung; Lee, Jung-Yong; Jin, Jungho; Bae, Byeong-Soo

    2017-07-19

    Herein, we report a new version of a bioinspired chitin nanofiber (ChNF) transparent laminated composite film (HCLaminate) made of siloxane hybrid materials (hybrimers) reinforced with ChNFs, which mimics the nanofiber-matrix structure of hierarchical biocomposites. Our HCLaminate is produced via vacuum bag compressing and subsequent UV-curing of the matrix resin-impregnated ChNF transparent paper (ChNF paper). It is worthwhile to note that this new type of ChNF-based transparent substrate film retains the strengths of the original ChNF paper and compensates for ChNF paper's drawbacks as a flexible transparent substrate. As a result, compared with high-performance synthetic plastic films, such as poly(ethylene terephthalate), poly(ether sulfone), poly(ethylene naphthalate), and polyimide, our HCLaminate is characterized to exhibit extremely smooth surface topography, outstanding optical clarity, high elastic modulus, high dimensional stability, etc. To prove our HCLaminate as a substrate film, we use it to fabricate flexible perovskite solar cells and a touch-screen panel. As far as we know, this work is the first to demonstrate flexible optoelectronics, such as flexible perovskite solar cells and a touch-screen panel, actually fabricated on a composite film made of ChNF. Given its desirable macroscopic properties, we envision our HCLaminate being utilized as a transparent substrate film for flexible green optoelectronics.

  8. Self-heating forecasting for thick laminate specimens in fatigue

    Science.gov (United States)

    Lahuerta, F.; Westphal, T.; Nijssen, R. P. L.

    2014-12-01

    Thick laminate sections can be found from the tip to the root in most common wind turbine blade designs. Obtaining accurate and reliable design data for thick laminates is subject of investigations, which include experiments on thick laminate coupons. Due to the poor thermal conductivity properties of composites and the material self-heating that occurs during the fatigue loading, high temperature gradients may appear through the laminate thickness. In the case of thick laminates in high load regimes, the core temperature might influence the mechanical properties, leading to premature failures. In the present work a method to forecast the self-heating of thick laminates in fatigue loading is presented. The mechanical loading is related with the laminate self-heating, via the cyclic strain energy and the energy loss ratio. Based on this internal volumetric heat load a thermal model is built and solved to obtain the temperature distribution in the transient state. Based on experimental measurements of the energy loss factor for 10mm thick coupons, the method is described and the resulting predictions are compared with experimental surface temperature measurements on 10 and 30mm UD thick laminate specimens.

  9. Relationship between stress wave velocities of green and dry veneer

    Science.gov (United States)

    Brian K. Brashaw; Xiping Wang; Robert J. Ross; Roy F. Pellerin

    2004-01-01

    This paper evaluates the relationship between the stress wave velocities of green and dry southern pine and Douglas-fir veneers. A commercial stress wave timer and a laboratory signal analysis system were used to measure the transit time required for an induced stress wave to travel the longitudinal length of each veneer. Stress wave transit times were measured in the...

  10. Vibration suppression of composite laminated beams using distributed piezoelectric patches

    International Nuclear Information System (INIS)

    Foda, M A; Almajed, A A; ElMadany, M M

    2010-01-01

    The focus of this paper is to develop an analytical and straightforward approach to suppress the steady state transverse vibration of a symmetric cross-ply laminated composite beam that is excited by an external harmonic force. This is achieved by bonding patches of piezoelectric material at selected locations along the beam. The governing equations for the system are formulated and the dynamic Green's functions are used to obtain an exact solution for the problem. A scheme is proposed for determining the values of the driving voltages, the dimensions of the PZT patches and their locations along the beam, in order to confine the vibration in a certain chosen region where the vibration is not harmful and leave the other chosen region stationary or vibrating with very small amplitudes. Beams with different boundary conditions are considered. Numerical case studies are presented to verify the utility of the proposed scheme

  11. Influence of heat treatment and veneering on the storage modulus and surface of zirconia ceramic

    NARCIS (Netherlands)

    Siavikis, G.; Behr, M.; van der Zel, J.M.; Feilzer, A.J.; Rosentritt, M.

    2011-01-01

    Objectives: Glass-ceramic veneered zirconia is used for the application as fixed partial dentures. The aim of this investigation was to evaluate whether the heat treatment during veneering, the application of glass-ceramic for veneering or long term storage has an influence on the storage modulus of

  12. Geometry effect on the behaviour of single and glue-laminated glass fibre reinforced polymer composite sandwich beams loaded in four-point bending

    International Nuclear Information System (INIS)

    Awad, Ziad K.; Aravinthan, Thiru; Manalo, Allan

    2012-01-01

    Highlights: ► Investigated the behaviour of single and glue-laminated GFRP sandwich beam. ► Effect of shear span to depth was a key factor affecting the overall behaviour. ► Comparison with prediction models gave reasonable results in specific regions. ► A failure map was developed to identify the shear and flexural failures of panels. -- Abstract: The research investigated the behaviour of single and glue laminated glass fibre reinforced polymer (GFRP) composite sandwich beams considering different spans and beam cross sections. The composite sandwich beams with different thicknesses (1, 2, 3, 4, and 5 sandwich layers) have been tested in four-point static flexural test with different shear span to depth ratio (a/d). The a/d ratios showed a direct effect on the flexural and shear behaviour. The capacity of the beam decreased with increasing a/d. Various failure modes were observed including core crushing, core shear, and top skin compression failure. The failure mode map developed based on the experimental finding and analytical prediction indicated that the failure mode is affected by the a/d with the number of glue laminated panels.

  13. Effect of saliva and blood contamination after etching upon the shear bond strength between composite resin and enamel

    Science.gov (United States)

    Armadi, A. S.; Usman, M.; Suprastiwi, E.

    2017-08-01

    The aim of this study was to find out the surface roughness of composite resin veneer after brushing. In this study, 24 specimens of composite resin veneer are divided into three subgroups: brushed without toothpaste, brushed with non-herbal toothpaste, and brushed with herbal toothpaste. Brushing was performed for one set of 5,000 strokes and continued for a second set of 5,000 strokes. Roughness of composite resin veneer was determined using a Surface Roughness Tester. The results were statistically analyzed using Kruskal-Wallis nonparametric test and Post Hoc Mann-Whitney. The results indicate that the highest difference among the Ra values occurred within the subgroup that was brushed with the herbal toothpaste. In conclusion, the herbal toothpaste produced a rougher surface on composite resin veneer compared to non-herbal toothpaste.

  14. Fabrication of Silicon Nitride Dental Core Ceramics with Borosilicate Veneering material

    International Nuclear Information System (INIS)

    Wananuruksawong, R; Jinawath, S; Wasanapiarnpong, T; Padipatvuthikul, P

    2011-01-01

    Silicon nitride (Si 3 N 4 ) ceramic is a great candidate for clinical applications due to its high fracture toughness, strength, hardness and bio-inertness. This study has focused on the Si 3 N 4 ceramic as a dental core material. The white Si 3 N 4 was prepared by pressureless sintering at relative low sintering temperature of 1650 deg. C in nitrogen atmosphere. The coefficient of thermal expansion (CTE) of Si 3 N 4 ceramic is lower than that of Zirconia and Alumina ceramic which are popular in this field. The borosilicate glass veneering was employed due to its compatibility in thermal expansion. The sintered Si 3 N 4 specimens represented the synthetic dental core were paintbrush coated by a veneer paste composed of borosilicate glass powder ( 2 O 3 - partial stabilized zirconia) and 30 wt% of polyvinyl alcohol (5 wt% solution). After coating the veneer on the Si 3 N 4 specimens, the firing was performed in electric tube furnace between 1000-1200 deg. C. The veneered specimens fired at 1100 deg. C for 15 mins show good bonding, smooth and glossy without defect and crazing. The veneer has thermal expansion coefficient as 3.98x10 -6 deg. C -1 , rather white and semi opaque, due to zirconia addition, the Vickers hardness as 4.0 GPa which is closely to the human teeth.

  15. Interfacial characterization of ceramic core materials with veneering porcelain for all-ceramic bi-layered restorative systems.

    Science.gov (United States)

    Tagmatarchis, Alexander; Tripodakis, Aris-Petros; Filippatos, Gerasimos; Zinelis, Spiros; Eliades, George

    2014-01-01

    The aim of the study was to characterize the elemental distribution at the interface between all-ceramic core and veneering porcelain materials. Three groups of all-ceramic cores were selected: A) Glass-ceramics (Cergo, IPS Empress, IPS Empress 2, e-max Press, Finesse); B) Glass-infiltrated ceramics (Celay Alumina, Celay Zirconia) and C) Densely sintered ceramics (Cercon, Procera Alumina, ZirCAD, Noritake Zirconia). The cores were combined with compatible veneering porcelains and three flat square test specimens were produced for each system. The core-veneer interfaces were examined by scanning electron microscopy and energy dispersive x-ray microanalysis. The glass-ceramic systems showed interfacial zones reach in Si and O, with the presence of K, Ca, Al in core and Ca, Ce, Na, Mg or Al in veneer material, depending on the system tested. IPS Empress and IPS Empress 2 demonstrated distinct transitional phases at the core-veneer interface. In the glassinfiltrated systems, intermixing of core (Ce, La) with veneer (Na, Si) elements occurred, whereas an abrupt drop of the core-veneer elemental concentration was documented at the interfaces of all densely sintered ceramics. The results of the study provided no evidence of elemental interdiffusion at the core-veneer interfaces in densely sintered ceramics, which implies lack of primary chemical bonding. For the glass-containing systems (glassceramics and glass-infiltrated ceramics) interdiffusion of the glass-phase seems to play a critical role in establishing a primary bonding condition between ceramic core and veneering porcelain.

  16. Durability of feldspathic veneering ceramic on glass-infiltrated alumina ceramics after long-term thermocycling.

    Science.gov (United States)

    Mesquita, A M M; Ozcan, M; Souza, R O A; Kojima, A N; Nishioka, R S; Kimpara, E T; Bottino, M A

    2010-01-01

    This study compared the bond strength durability of a feldspathic veneering ceramic to glass-infiltrated reinforced ceramics in dry and aged conditions. Disc shaped (thickness: 4 mm, diameter: 4 mm) of glass-infiltrated alumina (In-Ceram Alumina) and glass-infiltrated alumina reinforced by zirconia (In-Ceram Zirconia) core ceramic specimens (N=48, N=12 per groups) were constructed according to the manufacturers' recommendations. Veneering ceramic (VITA VM7) was fired onto the core ceramics using a mold. The core-veneering ceramic assemblies were randomly divided into two conditions and tested either immediately after specimen preparation (Dry) or following 30000 thermocycling (5-55 ºC±1; dwell time: 30 seconds). Shear bond strength test was performed in a universal testing machine (cross-head speed: 1 mm/min). Failure modes were analyzed using optical microscope (x20). The bond strength data (MPa) were analyzed using ANOVA (α=0.05). Thermocycling did not decrease the bond strength results for both In-Ceram Alumina (30.6±8.2 MPa; P=0.2053) and In-Ceram zirconia (32.6±9 MPa; P=0.3987) core ceramic-feldspathic veneering ceramic combinations when compared to non-aged conditions (28.1±6.4 MPa, 29.7±7.3 MPa, respectively). There were also no significant differences between adhesion of the veneering ceramic to either In-Ceram Alumina or In-Ceram Zirconia ceramics (P=0.3289). Failure types were predominantly a mixture of adhesive failure between the veneering and the core ceramic together with cohesive fracture of the veneering ceramic. Long-term thermocycling aging conditions did not impair the adhesion of the veneering ceramic to the glass-infiltrated alumina core ceramics tested.

  17. Opalescence of all-ceramic core and veneer materials.

    Science.gov (United States)

    Cho, Moon-Sang; Yu, Bin; Lee, Yong-Keun

    2009-06-01

    The enamel of natural teeth is opalescent, where there is light scattering of the shorter wavelengths of the visible spectrum, giving a tooth a bluish appearance in the reflected color and an orange/brown appearance in the transmitted color. The objective of this study was to determine the opalescence of all-ceramic core, veneer and layered specimens with a color measuring spectrophotometer. Colors of core (A2-corresponding shade), veneer (A2- and A3-corresponding shades) and layered (A2- and A3-layered) ceramics for all-ceramic restorations in clinically relevant thicknesses were measured in the reflectance and transmittance modes. The opalescence parameter (OP), which was calculated as the difference in blue-yellow coordinate (Deltab(*)) and red-green coordinate (Deltaa(*)), and the differences in blue-yellow coordinate (Deltab(*)) and in color (DeltaE(ab)(*)) between the reflected and transmitted colors were calculated. One-way ANOVA was performed for the OP values of the core, veneer and layered specimens by the kind of materials. Regression analysis was performed between the OP and Deltab(*), and the OP and DeltaE(ab)(*) values. The range of the OP value was 1.6-6.1, 2.0-7.1, 1.3-5.0 and 1.6-4.2 for the core, veneer, A2- and A3-layered specimens, respectively, all of which were significantly influenced by the kind of materials (pOpalescence varied by kind of ceramics. The OP values of ceramics were lower than those of tooth enamel. All-ceramic materials that can simulate the opalescence of natural teeth should be developed.

  18. Assessment of damage in composite laminates through dynamic, full-spectral interrogation of fiber Bragg grating sensors

    International Nuclear Information System (INIS)

    Propst, A; Peters, K; Zikry, M A; Schultz, S; Kunzler, W; Zhu, Z; Wirthlin, M; Selfridge, R

    2010-01-01

    In this study, we demonstrate the full-spectral interrogation of a fiber Bragg grating (FBG) sensor at 535 Hz. The sensor is embedded in a woven, graphite fiber–epoxy composite laminate subjected to multiple low-velocity impacts. The measurement of unique, time dependent spectral features from the FBG sensor permits classification of the laminate lifetime into five regimes. These damage regimes compare well with previous analysis of the same material system using combined global and local FBG sensor information. Observed transient spectral features include peak splitting, wide spectral broadening and a strong single peak at the end of the impact event. Such features could not be measured through peak wavelength interrogation of the FBG sensor. Cross-correlation of the measured spectra with the original embedded FBG spectrum permitted rapid visualization of average strains and the presence of transverse compressive strain on the optical fiber, but smeared out the details of the spectral profile

  19. An Investigation on Tensile Properties of Glass Fiber/Aluminium Laminates

    Directory of Open Access Journals (Sweden)

    M. Sadighi

    2009-12-01

    Full Text Available The idea of combining low weight and good mechanical properties has led to efforts to develop a new light fiber/metal laminate (FML in the last decade. FMLs are hybrid composites consisting of alternating thin layers of metal sheets and fiber-reinforced epoxy prepregs. In this study, the effect of fiber orientation on tensile properties of this material is investigated both analytically and experimentally. An analytical constitutive model based on classical lamination theory by using Kirchhoff-Love assumption, which incorporates the elastic-plastic behavior of the aluminium alloy was applied. Test results show that fiber sheet, with zero angle in laminates, improve the tensile strength. The composite layers with different fiber orientation change specimens' mode of fracture. Good agreement is obtained between the model predictions and experimental results.

  20. Laminates

    Science.gov (United States)

    Lepedat, Karin; Wagner, Robert; Lang, Jürgen

    The use of phenolic resin for the impregnation of a carrier material such as paper or fabric based on either organic or inorganic fibers was and still is one of the most important application areas for liquid phenolic resins. Substrates like paper, cotton, or glass fabric impregnated with phenolic resins are used as core layers for decorative and technical laminates and for many other different industrial applications. Nowadays, phenolic resins for decorative laminates used for furniture, flooring, or in the construction and transportation industry have gained significant market share. The Laminates chapter mainly describes the manufacture of decorative laminates especially the impregnation and pressing process with special emphasis to new technological developments and recent trends. Moreover, the different types of laminates are introduced, combined with some brief comments as they relate to the market for decorative surfaces.

  1. A study of an influence of a fiber arrangement of a laminate ply on the distribution and values of stresses in the multi-layered composite material

    Directory of Open Access Journals (Sweden)

    Herbuś Krzysztof

    2017-01-01

    Full Text Available In the work are presented studies related with the influence of a fiber arrangement of a laminate ply on the distribution and values of stresses in the multi-layered composite material. For this purpose, the characteristics of the three-point bending test, according to the standard PN-EN ISO 7438, of specimens made from the composite material, where a single ply is a composition of epoxy resin and glass fibres, was mapped. The modelling process of the multi-layered composite material and its strength verification was performed in the PLM Siemens NX system. Based on the results of performed numerical studies, the relation between the value of the main angle of an arrangement of fibers in each plies of the laminate, and the distribution and values of stresses, occurring in the examined specimens has been determined.

  2. Effect of bulk-fill base material on fracture strength of root-filled teeth restored with laminate resin composite restorations.

    Science.gov (United States)

    Taha, N A; Maghaireh, G A; Ghannam, A S; Palamara, J E

    2017-08-01

    To evaluate the effect of using a bulk-fill flowable base material on fracture strength and fracture patterns of root-filled maxillary premolars with MOD preparations restored with laminate restorations. Fifty extracted maxillary premolars were selected for the study. Standardized MOD cavities with endodontic treatment were prepared for all teeth, except for intact control. The teeth were divided randomly into five groups (n=10); (Group 1) sound teeth, (Group 2) unrestored teeth; (Group 3) MOD cavities with Vitrebond base and resin-based composite (Ceram. X One Universal); (Group 4) MOD cavities with 2mm GIC base (Fuji IX GP) and resin-based composite (Ceram. X One Universal) open laminate, (Group 5) MOD cavities were restored with 4mm of bulk-fill flowable base material (SDR) and resin-based composite (Ceram. X One Universal). All teeth were thermocycled and subjected to a 45° ramped oblique load in a universal testing machine. Fracture load and fracture patterns were recorded. Data were analyzed using one-way ANOVA and Dunnett's T3 test. Restoration in general increased the fracture strength compared to unrestored teeth. The fracture strength of group 5 (bulk-fill) was significantly higher than the fracture strength of the GIC laminate groups and not significantly different from the intact teeth (355±112N, P=0.118). The type of failure was unfavorable for most of the groups, with the majority being mixed failures. The use of a bulk-fill flowable base material significantly increased the fracture strength of extracted root-filled teeth with MOD cavities; however it did not improve fracture patterns to more favorable ones. Investigating restorative techniques that may improve the longevity of root-filled premolar teeth restored with direct resin restorations. Copyright © 2017 Elsevier Ltd. All rights reserved.

  3. [Effect of ceramic thickness and resin cement shades on final color of heat-pressed ceramic veneers].

    Science.gov (United States)

    Ren, D F; Zhan, K R; Chen, X D; Xing, W Z

    2017-02-09

    Objective: To analyze the effect of ceramic materials thickness and resin cement shades on the final color of ceramic veneers in the discolored teeth, and to investigate the color agreement of try-in pastes to the corresponding resin cements. Methods: Sixty artificial maxillary central incisor teeth (C2 shade) were used to simulate the natural discolored teeth and prepared according to veneer tooth preparation protocol. Veneers of different thickness in the body region (0.50 and 0.75 mm) were fabricated using ceramic materials (LT A2 shade, IPS e.max Press). The ceramic veneer specimens were bonded to the artificial teeth using the 6 shades of resin cements (Variolink Veneer: shades of LV-3, LV-2, HV+3; RelyX™ Veneer: shades of TR, A3, WO) ( n= 5). A clinical spectrophotometer was used to measure the color parameters of ceramic veneers at the cervical, body and incisal regions. Color changes of veneers before and after cementation were calculated and registered as ΔE1, and the changes between try-in paste and the corresponding resin cements were registered as ΔE2. Results: Three-way ANOVA indicated that ΔE1 and ΔE2 values were significantly affected by the ceramic thickness, resin cement shades and measuring regions ( Pceramic veneers were cemented with resin cements in shades of HV+3 and WO. The ΔE2 values of six shades ranged from 0.60-2.56. The shades of HV+3, WO and A3 resin cements were more than 1.60. Conclusions: Different thickness of ceramic materials, resin cement shades and measuring regions could affect the final color of ceramic veneers. The color differences of some resin cements and corresponding try-in pastes might be observed in clinical practice.

  4. Stiffness and Density Analysis of Rotary Veneer Recovered from Six Species of Australian Plantation Hardwoods

    Directory of Open Access Journals (Sweden)

    Robert Lee McGavin

    2015-08-01

    Full Text Available Commercial interest in Australian hardwood plantations is increasing. The timber industry is investigating alternative supplies of forest resources, and the plantation growing industry is eager to explore alternative markets to maximize financial returns. Identifying suitable processing strategies and high-value products that suit young, plantation-grown hardwoods have proven challenging; however, recent veneer processing trials using simple veneer technology have demonstrated more acceptable recoveries of marketable products. The recovered veneers have visual qualities that are suitable for structurally-based products; however, the mechanical properties of the veneer are largely unknown. Veneers resulting from processing trials of six commercially important Australian hardwood species were used to determine key wood properties (i.e., density, dynamic modulus of elasticity (MoE, and specific MoE. The study revealed that a wide variation of properties existed between species and also within species. Simple mathematical modeling, using sigmoidal curves, was demonstrated to be an effective method to model the evolution of key wood properties across the billet radius and along the resulting veneer ribbon with benefits for tree breeders and processors.

  5. Detection of layup errors in prepreg laminates using shear ultrasonic waves

    Science.gov (United States)

    Hsu, David K.; Fischer, Brent A.

    1996-11-01

    The highly anisotropic elastic properties of the plies in a composite laminate manufactured from unidirectional prepregs interact strongly with the polarization direction of shear ultrasonic waves propagating through its thickness. The received signals in a 'crossed polarizer' transmission configuration are particularly sensitive to ply orientation and layup sequence in a laminate. Such measurements can therefore serve as an NDE tool for detecting layup errors. For example, it was shown experimentally recently that the sensitivity for detecting the presence of misoriented plies is better than one ply out of a 48-ply laminate of graphite epoxy. A physical model based on the decomposition and recombination of the shear polarization vector has been constructed and used in the interpretation and prediction of test results. Since errors should be detected early in the manufacturing process, this work also addresses the inspection of 'green' composite laminates using electromagnetic acoustic transducers (EMAT). Preliminary results for ply error detection obtained with EMAT probes are described.

  6. Static aeroelastic behavior of an adaptive laminated piezoelectric composite wing

    Science.gov (United States)

    Weisshaar, T. A.; Ehlers, S. M.

    1990-01-01

    The effect of using an adaptive material to modify the static aeroelastic behavior of a uniform wing is examined. The wing structure is idealized as a laminated sandwich structure with piezoelectric layers in the upper and lower skins. A feedback system that senses the wing root loads applies a constant electric field to the piezoelectric actuator. Modification of pure torsional deformaton behavior and pure bending deformation are investigated, as is the case of an anisotropic composite swept wing. The use of piezoelectric actuators to create an adaptive structure is found to alter static aeroelastic behavior in that the proper choice of the feedback gain can increase or decrease the aeroelastic divergence speed. This concept also may be used to actively change the lift effectiveness of a wing. The ability to modify static aeroelastic behavior is limited by physical limitations of the piezoelectric material and the manner in which it is integrated into the parent structure.

  7. Rehabilitation of a patient with amelogenesis imperfecta using porcelain veneers and CAD/CAM polymer restorations: A clinical report.

    Science.gov (United States)

    Saeidi Pour, Reza; Edelhoff, Daniel; Prandtner, Otto; Liebermann, Anja

    2015-01-01

    The complete dental rehabilitation of patients with a vertical dimension loss (VDL) caused by structural enamel deficits associated with amelogenesis imperfecta (AI) represents a difficult challenge for restorative teams. Accurate analysis and treatment planning that includes esthetic and functional evaluations and adequate material selection are important prerequisites for successful results. Long-term provisional restorations play an important role in exploring and elucidating the patients' esthetic demands and functional needs. Restorative treatment options can vary from requiring only oral hygiene instructions to extensive dental restorations that include composite fillings, ceramic veneers, metal-ceramic, or all-ceramic crowns. This case report describes a full-mouth rehabilitation of a patient with amelogenesis imperfecta including the case planning, bite replacement, preparation, and restoration setting steps with an experimental CAD/CAM polymer and porcelain veneers.

  8. Development of a Higher Order Laminate Theory for Modeling Composites with Induced Strain Actuators

    Science.gov (United States)

    Chattopadhyay, Aditi; Seeley, Charles E.

    1996-01-01

    A refined higher order plate theory is developed to investigate the actuation mechanism of piezoelectric materials surface bonded or embedded in composite laminates. The current analysis uses a displacement field which accurately accounts for transverse shear stresses. Some higher order terms are identified by using the conditions that shear stresses vanish at all free surfaces. Therefore, all boundary conditions for displacements and stresses are satisfied in the present theory. The analysis is implemented using the finite element method which provides a convenient means to construct a numerical solution due to the discrete nature of the actuators. The higher order theory is computationally less expensive than a full three dimensional analysis. The theory is also shown to agree well with published experimental results. Numerical examples are presented for composite plates with thicknesses ranging from thin to very thick.

  9. Damage in woven CFRP laminates under impact loading

    Science.gov (United States)

    Ullah, H.; Harland, A. R.; Silberschmidt, V. V.

    2012-08-01

    Carbon fibre-reinforced polymer (CFRP) composites used in sports products can be exposed to different in-service conditions such as large dynamic bending deformations caused by impact loading. Composite materials subjected to such loads demonstrate various damage modes such as matrix cracking, delamination and, ultimately, fabric fracture. Damage evolution affects both in-service properties and performance of CFRP that can deteriorate with time. These failure modes need adequate means of analysis and investigation, the major approaches being experimental characterisation and numerical simulations. This research deals with a deformation behaviour and damage in composite laminates due to dynamic bending. Experimental tests are carried out to characterise the behaviour of a woven CFRP material under large-deflection dynamic bending in impact tests carried out to obtain the force-time and absorbed energy profiles for CFRP laminates. Damage in the impacted laminates is analysed using optical microscopy. Numerical simulations are performed to study the deformation behaviour and damage in CFRP for cases of large-deflection bending based on three-dimensional finite-element models implemented in the commercial code Abaqus/Explicit. Multiple layers of bilinear cohesive-zone elements are employed to model the initiation and progression of inter-ply delamination observed in the microscopy studies. The obtained results of simulations show good agreement with experimental data.

  10. Micro/nanoscale mechanical characterization and in situ observation of cracking of laminated Si3N4/BN composites

    International Nuclear Information System (INIS)

    Li Xiaodong; Zou Linhua; Ni Hai; Reynolds, Anthony P.; Wang Changan; Huang Yong

    2008-01-01

    Micro/nanoscale mechanical characterization of laminated Si 3 N 4 /BN composites was carried out by nanoindentation techniques. A custom-designed micro mechanical tester was integrated with an optical microscope and an atomic force microscope to perform in situ three-point bending tests on notched Si 3 N 4 /BN composite bend specimens where the crack initiation and propagation were imaged simultaneously with the optical microscope and atomic force microscope during bending loading. The whole fracture process was in situ captured. It was found that crack deflection was initiated/induced by the pre-existing microvoids and microcracks in BN interfacial layers. New fracture mechanisms were proposed to provide guidelines for the design of biomimetic nacre-like composites

  11. Enhanced Magnetoelectric Effect in Permendur/Pb(Zr0.52Ti0.48O3 Laminated Magnetostrictive/Piezoelectric Composite

    Directory of Open Access Journals (Sweden)

    Yanmin Jia

    2015-09-01

    Full Text Available In this work, after investigating three typical magneto-electric (ME composites, Permendur/Pb(Zr0.52Ti0.48O3(PZT, Metglas/PZT, and Tefenol-D/PZT, with the same dimensions and different saturation magnetostriction and magnetic permeability, the most excellent ME performance is observed in the Permendur/PZT laminates, which agrees well with the predicted results from the figure of merit. The low-frequency and resonance ME coefficients of Permendur/PZT composite are ~23.1 V/Oe.cm and ~309 V/Oe.cm at the optimal dc bias magnetic field of ~250 Oe, respectively. The strong ME effect of Permendur/PZT composite gives it potential in practical magnetic sensitive device applications.

  12. Lamination cooling system

    Science.gov (United States)

    Rippel, Wally E.; Kobayashi, Daryl M.

    2005-10-11

    An electric motor, transformer or inductor having a lamination cooling system including a stack of laminations, each defining a plurality of apertures at least partially coincident with apertures of adjacent laminations. The apertures define a plurality of cooling-fluid passageways through the lamination stack, and gaps between the adjacent laminations are sealed to prevent a liquid cooling fluid in the passageways from escaping between the laminations. The gaps are sealed by injecting a heat-cured sealant into the passageways, expelling excess sealant, and heat-curing the lamination stack. The apertures of each lamination can be coincident with the same-sized apertures of adjacent laminations to form straight passageways, or they can vary in size, shape and/or position to form non-axial passageways, angled passageways, bidirectional passageways, and manifold sections of passageways that connect a plurality of different passageway sections. Manifold members adjoin opposite ends of the lamination stack, and each is configured with one or more cavities to act as a manifold to adjacent passageway ends. Complex manifold arrangements can create bidirectional flow in a variety of patterns.

  13. Healable Composites

    Science.gov (United States)

    2012-03-28

    oriented fibers and healable polymer matrix 4. Laminate pre-preg layers to form composite panels with minimal voids & defects 5. Characterize the...composites: determine mechanical and crack healing properties (4, 5) Composite (3) Prepreg (2) Polymer (1) Furan (1) Maleimide Healable Composites...Develop pre-preg system of oriented fibers and healable polymer matrix 4. Laminate pre-preg layers to form composite panels with minimal voids & defects

  14. Thermal analysis of smart composite laminated angle-ply using higher order shear deformation theory with zig zag function

    Science.gov (United States)

    YagnaSri, P.; Siddiqui, Maimuna; Vijaya Nirmala, M.

    2018-03-01

    The objective of the work is to develop the higher order theory for piezoelectric composite laminated plates with zigzag function and to determine the thermal characteristics of piezoelectric laminated plate with zig zag function for different aspect ratios (a/h), thickness ratios (z/h) and voltage and also to evaluate electric potential function by solving second order differential equation satisfying electric boundary conditions along the thickness direction of piezoelectric layer. The related functions and derivations for equation of motion are obtained using the dynamic version of the principle of virtual work or Hamilton’s principle. The solutions are obtained by using Navier’s stokes method for anti-symmetric angle-ply with specific type of simply supported boundary conditions. Computer programs have been developed for realistic prediction of stresses and deflections for various sides to thickness ratios (a/h) and voltages.

  15. Connections: Superplasticity, Damascus Steels, Laminated Steels, and Carbon Dating

    Science.gov (United States)

    Wadsworth, Jeffrey

    2016-12-01

    In this paper, a description is given of the connections that evolved from the initial development of a family of superplastic plain carbon steels that came to be known as Ultra-High Carbon Steels (UHCS). It was observed that their very high carbon contents were similar, if not identical, to those of Damascus steels. There followed a series of attempts to rediscover how the famous patterns found on Damascus steels blades were formed. At the same time, in order to improve the toughness at room temperature of the newly-developed UHCS, laminated composites were made of alternating layers of UHCS and mild steel (and subsequently other steels and other metals). This led to a study of ancient laminated composites, the motives for their manufacture, and the plausibility of some of the claims relating to the number of layers in the final blades. One apparently ancient laminated composite, recovered in 1837 from the great pyramid of Giza which was constructed in about 2750 B.C., stimulated a carbon dating study of ancient steels. The modern interest in "Bladesmithing" has connections back to many of these ancient weapons.

  16. Free vibration of fully functionally graded carbon nanotube reinforced graphite/epoxy laminates

    Science.gov (United States)

    Kuo, Shih-Yao

    2018-03-01

    This study provides the first-known vibration analysis of fully functionally graded carbon nanotube reinforced hybrid composite (FFG-CNTRHC) laminates. CNTs are non-uniformly distributed to reinforce the graphite/epoxy laminates. Some CNT distribution functions in the plane and thickness directions are proposed to more efficiently increase the stiffening effect. The rule of mixtures is modified by considering the non-homogeneous material properties of FFG-CNTRHC laminates. The formulation of the location dependent stiffness matrix and mass matrix is derived. The effects of CNT volume fraction and distribution on the natural frequencies of FFG-CNTRHC laminates are discussed. The results reveal that the FFG layout may significantly increase the natural frequencies of FFG-CNTRHC laminate.

  17. Fabrication of Silicon Nitride Dental Core Ceramics with Borosilicate Veneering material

    Science.gov (United States)

    Wananuruksawong, R.; Jinawath, S.; Padipatvuthikul, P.; Wasanapiarnpong, T.

    2011-10-01

    Silicon nitride (Si3N4) ceramic is a great candidate for clinical applications due to its high fracture toughness, strength, hardness and bio-inertness. This study has focused on the Si3N4 ceramic as a dental core material. The white Si3N4 was prepared by pressureless sintering at relative low sintering temperature of 1650 °C in nitrogen atmosphere. The coefficient of thermal expansion (CTE) of Si3N4 ceramic is lower than that of Zirconia and Alumina ceramic which are popular in this field. The borosilicate glass veneering was employed due to its compatibility in thermal expansion. The sintered Si3N4 specimens represented the synthetic dental core were paintbrush coated by a veneer paste composed of borosilicate glass powder (tube furnace between 1000-1200°C. The veneered specimens fired at 1100°C for 15 mins show good bonding, smooth and glossy without defect and crazing. The veneer has thermal expansion coefficient as 3.98×10-6 °C-1, rather white and semi opaque, due to zirconia addition, the Vickers hardness as 4.0 GPa which is closely to the human teeth.

  18. Synergetic effects of thin plies and aligned carbon nanotube interlaminar reinforcement in composite laminates

    OpenAIRE

    Arteiro, Albertino; Borstnar, Gregor; Mavrogordato, Mark N.; Sinclair, Ian; Spearing, S. Mark; Camanho, Pedro P.; Cohen, Estelle; Kopp, Reed Alan; Furtado Pereira da Silva, Carolina; Ni, Xinchen; Wardle, Brian L

    2017-01-01

    Thin-ply carbon fiber laminates have exhibited superior mechanical properties, including higher initiation and ultimate strength, when compared to standard thickness plies and enable greater flexibility in laminate design. However, the increased ply count in thin-ply laminates also increases the number of ply-ply interfaces, thereby increasing the number of relatively weak and delamination-prone interlaminar regions. In this study, we report the first experimental realization of aligned carbo...

  19. Identification of impact force acting on composite laminated plates using the radiated sound measured with microphones

    Science.gov (United States)

    Atobe, Satoshi; Nonami, Shunsuke; Hu, Ning; Fukunaga, Hisao

    2017-09-01

    Foreign object impact events are serious threats to composite laminates because impact damage leads to significant degradation of the mechanical properties of the structure. Identification of the location and force history of the impact that was applied to the structure can provide useful information for assessing the structural integrity. This study proposes a method for identifying impact forces acting on CFRP (carbon fiber reinforced plastic) laminated plates on the basis of the sound radiated from the impacted structure. Identification of the impact location and force history is performed using the sound pressure measured with microphones. To devise a method for identifying the impact location from the difference in the arrival times of the sound wave detected with the microphones, the propagation path of the sound wave from the impacted point to the sensor is examined. For the identification of the force history, an experimentally constructed transfer matrix is employed to relate the force history to the corresponding sound pressure. To verify the validity of the proposed method, impact tests are conducted by using a CFRP cross-ply laminate as the specimen, and an impulse hammer as the impactor. The experimental results confirm the validity of the present method for identifying the impact location from the arrival time of the sound wave detected with the microphones. Moreover, the results of force history identification show the feasibility of identifying the force history accurately from the measured sound pressure using the experimental transfer matrix.

  20. Fabrication of Silicon Nitride Dental Core Ceramics with Borosilicate Veneering material

    Energy Technology Data Exchange (ETDEWEB)

    Wananuruksawong, R; Jinawath, S; Wasanapiarnpong, T [Research Unit of Advanced Ceramic, Department of Materials Science, Faculty of Science, Chulalongkorn University, Bangkok (Thailand); Padipatvuthikul, P, E-mail: raayaa_chula@hotmail.com [Faculty of Dentistry, Srinakharinwirot University, Bangkok (Thailand)

    2011-10-29

    Silicon nitride (Si{sub 3}N{sub 4}) ceramic is a great candidate for clinical applications due to its high fracture toughness, strength, hardness and bio-inertness. This study has focused on the Si{sub 3}N{sub 4} ceramic as a dental core material. The white Si{sub 3}N{sub 4} was prepared by pressureless sintering at relative low sintering temperature of 1650 deg. C in nitrogen atmosphere. The coefficient of thermal expansion (CTE) of Si{sub 3}N{sub 4} ceramic is lower than that of Zirconia and Alumina ceramic which are popular in this field. The borosilicate glass veneering was employed due to its compatibility in thermal expansion. The sintered Si{sub 3}N{sub 4} specimens represented the synthetic dental core were paintbrush coated by a veneer paste composed of borosilicate glass powder (<150 micrometer, Pyrex) with 5 wt% of zirconia powder (3 wt% Y{sub 2}O{sub 3} - partial stabilized zirconia) and 30 wt% of polyvinyl alcohol (5 wt% solution). After coating the veneer on the Si{sub 3}N{sub 4} specimens, the firing was performed in electric tube furnace between 1000-1200 deg. C. The veneered specimens fired at 1100 deg. C for 15 mins show good bonding, smooth and glossy without defect and crazing. The veneer has thermal expansion coefficient as 3.98x10{sup -6} deg. C{sup -1}, rather white and semi opaque, due to zirconia addition, the Vickers hardness as 4.0 GPa which is closely to the human teeth.

  1. Modeling delamination of FRP laminates under low velocity impact

    Science.gov (United States)

    Jiang, Z.; Wen, H. M.; Ren, S. L.

    2017-09-01

    Fiber reinforced plastic laminates (FRP) have been increasingly used in various engineering such as aeronautics, astronautics, transportation, naval architecture and their impact response and failure are a major concern in academic community. A new numerical model is suggested for fiber reinforced plastic composites. The model considers that FRP laminates has been constituted by unidirectional laminated plates with adhesive layers. A modified adhesive layer damage model that considering strain rate effects is incorporated into the ABAQUS / EXPLICIT finite element program by the user-defined material subroutine VUMAT. It transpires that the present model predicted delamination is in good agreement with the experimental results for low velocity impact.

  2. Evaluation of contact resistance between carbon fiber/epoxy composite laminate and printed silver electrode for damage monitoring

    International Nuclear Information System (INIS)

    Jeon, Eun Beom; Kim, Hak Sung; Takahashi, Kosuke

    2014-01-01

    An addressable conducting network (ACN) makes it possible to monitor the condition of a structure using the electrical resistance between electrodes on the surface of a carbon fiber reinforced plastics (CFRP) structure. To improve the damage detection reliability of the ACN, the contact resistances between the electrodes and CFRP laminates needs to be minimized. In this study, silver nanoparticle electrodes were fabricated via printed electronics techniques on a CFRP composite. The contact resistance between the silver electrodes and CFRP were measured with respect to various fabrication conditions such as the sintering temperature of the silver nano-ink and the surface roughness of the CFRP laminates. The interfaces between the silver electrode and carbon fibers were observed using a scanning electron microscope (SEM). Based on this study, it was found that the lowest contact resistance of 0.3664Ω could be achieved when the sintering temperature of the silver nano-ink and surface roughness were 120 degree C and 0.230 a, respectively.

  3. LAMINATES

    Directory of Open Access Journals (Sweden)

    Gökay Nemli

    2004-04-01

    Full Text Available Wood based panel producers afford to present their products either in sized semi-finished form or as covered in general by the in additional investments realized. The fact that the laminated material has a certain market share as well as the increase in demand for furniture types finished in various profiles have put the laminated sheets which provide very comprehensive design facilities at the top place and caused such boards to spread over the market rather more quickly. In line with this development, great developments have also been recorded during recent years in laminate utilization in furniture factoring sector and fast steps taken towards a more rational working environment. In this study, laminates types and manufacturing technologies were investigated.

  4. Study on Flexural Creep Parameters of Overlayed Particleboard by Natural and Melaminated Veneers

    Directory of Open Access Journals (Sweden)

    Abdollah Najafi

    2012-06-01

    Full Text Available In this study, effects of natural and artificial veneer on flexural creep behavior of particleboard was investigated. Particleboard panels were prepared from Pars Neopan industries with 660 kg/m3 density and then overlaid by natural and melamine veneers. Their creep behavior was compared to control particleboard. For evaluating maximum bending load in static flexural test, specimens were cut from panels according to ASTM D 1037 with dimensions of 370×50×16 mm. Then, The flexural creep tests at 20% and 40% of failure bending load was applied to test specimens. Results of flexural tests indicated that the MOR and MOE values of veneered particleboard were highest. Results of creep showed that levels of stresses are effective on all creep parameters, but showed less effect on relative creep. Also, creep parameters less effective on specimens overlaid by natural veneer.

  5. Influence of abutment type and esthetic veneering on preload maintenance of abutment screw of implant-supported crowns.

    Science.gov (United States)

    Delben, Juliana Aparecida; Barão, Valentim Adelino Ricardo; Dos Santos, Paulo Henrique; Assunção, Wirley Gonçalves

    2014-02-01

    The effect of veneering materials on screw joint stability remains inconclusive. Thus, this study evaluated the preload maintenance of abutment screws of single crowns fabricated with different abutments and veneering materials. Sixty crowns were divided into five groups (n = 12): UCLA abutment in gold alloy with ceramic (group GC) and resin (group GR) veneering, UCLA abutment in titanium with ceramic (group TiC) and resin (group TiR) veneering, and zirconia abutment with ceramic veneering (group ZiC). Abutment screws made of gold were used with a 35 Ncm insertion torque. Detorque measurements were obtained initially and after mechanical cycling. Data were analyzed by ANOVA and Fisher's exact test at a significance level of 5%. For the initial detorque means (in Ncm), group TiC (21.4 ± 1.78) exhibited statistically lower torque maintenance than groups GC (23.9 ± 0.91), GR (24.1 ± 1.34), and TiR (23.2 ± 1.33) (p abutment type and veneering material. More irregular surfaces in the hexagon area of the castable abutments were observed. The superiority of any veneering material concerning preload maintenance was not established. © 2013 by the American College of Prosthodontists.

  6. Modeling of Nonlinear Mechanical Response in CFRP Angle-Ply Laminates

    Science.gov (United States)

    Ogihara, Shinji

    2014-03-01

    It is known that the failure process in angle-ply laminate involves matrix cracking and delamination and that they exhibit nonlinear stress-strain relation. There may be a significant effect of the constituent blocked ply thickness on the mechanical behavior of angle-ply laminates. These days, thin prepregs whose thickness is, for example 50 micron, are developed and commercially available. Therefore, we can design wide variety of laminates with various constituent ply thicknesses. In this study, effects of constituent ply thickness on the nonlinear mechanical behavior and the damage behavior of CFRP angle-ply laminates are investigated experimentally. Based on the experimental results, the mechanical response in CFRP angle-ply laminates is modeled by using the finite strain viscoplasticity model. We evaluated the mechanical behavior and damage behavior in CFRP angle-ply laminates with different constituent ply thickness under tensile loading experimentally. It was found that as the constituent ply thickness decreases, the strength and failure strain increases. We also observed difference in damage behavior. The preliminary results of finite strain viscoplasticity model considering the damage effect for laminated composites are shown. A qualitative agreement is obtained.

  7. Fatigue Analysis of Notched Laminates: A Time-Efficient Macro-Mechanical Approach

    Science.gov (United States)

    Naghipour, P.; Pineda, E. J.; Bednarcyk, B. A.; Arnold, S. M.; Waas, A. M.

    2016-01-01

    A coupled transversely isotropic deformation and damage fatigue model is implemented within the finite element method and was utilized along with a static progressive damage model to predict the fatigue life, stiffness degradation as a function of number of cycles, and post-fatigue tension and compression response of notched, multidirectional laminates. Initially, the material parameters for the fatigue model were obtained utilizing micromechanics simulations and the provided [0], [90] and [plus or minus 45] experimental composite laminate S-N (stress-cycle) data. Within the fatigue damage model, the transverse and shear properties of the plies were degraded with an isotropic scalar damage variable. The damage in the longitudinal (fiber) ply direction was suppressed, and only the strength of the fiber was degraded as a function of fatigue cycles. A maximum strain criterion was used to capture the failure in each element, and once this criterion was satisfied, the longitudinal stiffness of the element was decreased by a factor of 10 (sup 4). The resulting, degraded properties were then used to calculate the new stress state. This procedure was repeated until final failure of the composite laminate was achieved or a specified number of cycles reached. For post-fatigue tension and compression behavior, four internal state variables were used to control the damage and failure. The predictive capability of the above-mentioned approach was assessed by performing blind predictions of the notched multidirectional IM7/977-3 composite laminates response under fatigue and post-fatigue tensile and compressive loading, followed by a recalibration phase. Although three different multidirectional laminates were analyzed in the course of this study, only detailed results (i.e., stiffness degradation and post-fatigue stress-train curves as well as damage evolution states for a single laminate ([30/60/90/minus 30/minus 60] (sub 2s)) are discussed in detail here.

  8. On the detectability of transverse cracks in laminated composites using electrical potential change measurements

    KAUST Repository

    Selvakumaran, Lakshmi

    2015-03-01

    Real-time health monitoring of structures made of laminated composites is necessary as significant damage may occur without any visible signs on the surface. Inspection by electrical tomography (ET) seems a viable approach that relies on voltage measurements from a network of electrodes across the inspected domain to infer conductivity change within the bulk material. If conductivity decreases significantly with increasing damage, the obtained conductivity map can be correlated to the degradation state of the material. We focus here on detection of transverse cracks. As transverse cracks modify the in-plane transverse conductivity of a single ply, we expect them to be detectable by electrical measurements. Yet, the quality of detection is directly related to the sensitivity of the measurements to the presence of cracks. We use numerical experiments to demonstrate that the sensitivity depends on several material and geometrical parameters. Based on the results, the applicability of ET to detect transverse cracks is discussed. One conclusion from the study is that detecting transverse cracks using ET is more reliable in some laminate configurations than in others. Recommendations about the properties of either the pristine material or the inspected structures are provided to establish if ET is reliable in detecting transverse cracks.

  9. Equivalent Circuit Model of Low-Frequency Magnetoelectric Effect in Disk-Type Terfenol-D/PZT Laminate Composites Considering a New Interface Coupling Factor.

    Science.gov (United States)

    Lou, Guofeng; Yu, Xinjie; Lu, Shihua

    2017-06-15

    This paper describes the modeling of magnetoelectric (ME) effects for disk-type Terfenol-D (Tb 0.3 Dy 0.7 Fe 1.92 )/PZT (Pb(Zr,Ti)O₃) laminate composite at low frequency by combining the advantages of the static elastic model and the equivalent circuit model, aiming at providing a guidance for the design and fabrication of the sensors based on magnetoelectric laminate composite. Considering that the strains of the magnetostrictive and piezoelectric layers are not equal in actual operating due to the epoxy resin adhesive bonding condition, the magnetostrictive and piezoelectric layers were first modeled through the equation of motion separately, and then coupled together with a new interface coupling factor k c , which physically reflects the strain transfer between the phases. Furthermore, a theoretical expression containing k c for the transverse ME voltage coefficient α v and the optimum thickness ratio n optim to which the maximum ME voltage coefficient corresponds were derived from the modified equivalent circuit of ME laminate, where the interface coupling factor acted as an ideal transformer. To explore the influence of mechanical load on the interface coupling factor k c , two sets of weights, i.e., 100 g and 500 g, were placed on the top of the ME laminates with the same thickness ratio n in the sample fabrication. A total of 22 T-T mode disk-type ME laminate samples with different configurations were fabricated. The interface coupling factors determined from the measured α v and the DC bias magnetic field H bias were 0.11 for 500 g pre-mechanical load and 0.08 for 100 g pre-mechanical load. Furthermore, the measured optimum thickness ratios were 0.61 for k c = 0.11 and 0.56 for k c = 0.08. Both the theoretical ME voltage coefficient α v and optimum thickness ratio n optim containing k c agreed well with the measured data, verifying the reasonability and correctness for the introduction of k c in the modified equivalent circuit model.

  10. Equivalent Circuit Model of Low-Frequency Magnetoelectric Effect in Disk-Type Terfenol-D/PZT Laminate Composites Considering a New Interface Coupling Factor

    Directory of Open Access Journals (Sweden)

    Guofeng Lou

    2017-06-01

    Full Text Available This paper describes the modeling of magnetoelectric (ME effects for disk-type Terfenol-D (Tb0.3Dy0.7Fe1.92/PZT (Pb(Zr,TiO3 laminate composite at low frequency by combining the advantages of the static elastic model and the equivalent circuit model, aiming at providing a guidance for the design and fabrication of the sensors based on magnetoelectric laminate composite. Considering that the strains of the magnetostrictive and piezoelectric layers are not equal in actual operating due to the epoxy resin adhesive bonding condition, the magnetostrictive and piezoelectric layers were first modeled through the equation of motion separately, and then coupled together with a new interface coupling factor kc, which physically reflects the strain transfer between the phases. Furthermore, a theoretical expression containing kc for the transverse ME voltage coefficient αv and the optimum thickness ratio noptim to which the maximum ME voltage coefficient corresponds were derived from the modified equivalent circuit of ME laminate, where the interface coupling factor acted as an ideal transformer. To explore the influence of mechanical load on the interface coupling factor kc, two sets of weights, i.e., 100 g and 500 g, were placed on the top of the ME laminates with the same thickness ratio n in the sample fabrication. A total of 22 T-T mode disk-type ME laminate samples with different configurations were fabricated. The interface coupling factors determined from the measured αv and the DC bias magnetic field Hbias were 0.11 for 500 g pre-mechanical load and 0.08 for 100 g pre-mechanical load. Furthermore, the measured optimum thickness ratios were 0.61 for kc = 0.11 and 0.56 for kc = 0.08. Both the theoretical ME voltage coefficient αv and optimum thickness ratio noptim containing kc agreed well with the measured data, verifying the reasonability and correctness for the introduction of kc in the modified equivalent circuit model.

  11. Fatigue damage mechanics of notched graphite-epoxy laminates

    Science.gov (United States)

    Spearing, Mark; Beaumont, Peter W. R.; Ashby, Michael F.

    A modeling approach is presented that recognizes that the residual properties of composite laminates after any form of loading depend on the damage state. Therefore, in the case of cyclic loading, it is necessary to first derive a damage growth law and then relate the residual properties to the accumulated damage. The propagation of fatigue damage in notched laminates is investigated. A power law relationship between damage growth and the strain energy release rate is developed. The material constants used in the model have been determined in independent experiments and are invariant for all the layups investigated. The strain energy release rates are calculated using a simple finite element representation of the damaged specimen. The model is used to predict the effect of tension-tension cyclic loading on laminates of the T300/914C carbon-fiber epoxy system. The extent of damage propagation is successfully predicted in a number of cross-ply laminates.

  12. Evidence of yttrium silicate inclusions in YSZ-porcelain veneers.

    Science.gov (United States)

    Stoner, Brian R; Griggs, Jason A; Neidigh, John; Piascik, Jeffrey R

    2014-04-01

    This report introduces the discovery of crystalline defects that can form in the porcelain veneering layer when in contact with yttria-stabilized zirconia (YSZ). The focus was on dental prostheses and understanding the defects that form in the YSZ/porcelain system; however the data reported herein may have broader implications toward the use and stability of YSZ-based ceramics in general. Specimens were cut from fully sintered YSZ plates and veneering porcelain was applied (X-ray (EDAX) was used for microstructural and elemental analysis. EDAX, for chemical analysis and transmission electron diffraction (TED) for structural analysis were both performed in the transmission electron microscope (TEM). Additionally, in order to spatially resolve Y-rich precipitates, micro-CT scans were conducted at varying depths within the porcelain veneer. Local EDAX (SEM) was performed in the regions of visible inclusions and showed significant increases in yttrium concentration. TEM specimens also showed apparent inclusions in the porcelain and selected area electron diffraction was performed on these regions and found the inclusions to be crystalline and identified as either yttrium-silicate (Y2 SiO5 ) or yttrium-disilicate (Y2 Si2 O7 ). Micro-CT data showed that yttrium-silicate precipitates were distributed throughout the thickness of the porcelain veneer. Future studies are needed to determine whether many of the premature failures associated with this materials system may be the result of crystalline flaws that form as a result of high temperature yttrium diffusion near the surfaces of YSZ. © 2013 Wiley Periodicals, Inc.

  13. Bending analyses for 3D engineered structural panels made from laminated paper and carbon fabric

    Science.gov (United States)

    Jinghao Li; John F. Hunt; Zhiyong Cai; Xianyan Zhou

    2013-01-01

    This paper presents analysis of a 3-dimensional engineered structural panel (3DESP) having a tri-axial core structure made from phenolic impregnated laminated-paper composites with and without high strength composite carbon-fiber fabric laminated to the outside of both faces. Both I-beam equations and finite element method were used to analyze four-point bending of the...

  14. Laminated articles

    International Nuclear Information System (INIS)

    Ridgway, P.C.; Case, D.F.

    1979-01-01

    In a method of bonding laminations of a magnetic core, photo-resist material consisting of a co-polymer is applied as a film to a sheet of magnetic material to define lamination shapes to enable the laminations to be formed by etching. The film of photo-resist material on the laminations is then utilised to bond the laminations together in a stack. In order to permit the core to operate at temperatures higher than the softening temperature of the photo-resist material, the bonded stack is irradiated with 1 - 2 Mer gamma radiation to a dose of 1 - 5 Mrads in 2 - 10 hrs to cause changes to the bonding material such that the material does not soften at the operating temperature of the core. (U.K.)

  15. A MEMS lamination technology based on sequential multilayer electrodeposition

    International Nuclear Information System (INIS)

    Kim, Minsoo; Kim, Jooncheol; Herrault, Florian; Schafer, Richard; Allen, Mark G

    2013-01-01

    A MEMS lamination technology based on sequential multilayer electrodeposition is presented. The process comprises three main steps: (1) automated sequential electrodeposition of permalloy (Ni 80 Fe 20 ) structural and copper sacrificial layers to form multilayer structures of significant total thickness; (2) fabrication of polymeric anchor structures through the thickness of the multilayer structures and (3) selective removal of copper. The resulting structure is a set of air-insulated permalloy laminations, the separation of which is sustained by insulating polymeric anchor structures. Individual laminations have precisely controllable thicknesses ranging from 500 nm to 5 µm, and each lamination layer is electrically isolated from adjacent layers by narrow air gaps of similar scale. In addition to air, interlamination insulators based on polymers are investigated. Interlamination air gaps with very high aspect ratio (>1:100) can be filled with polyvinylalcohol and polydimethylsiloxane. The laminated structures are characterized using scanning electron microscopy and atomic force microscopy to directly examine properties such as the roughness and the thickness uniformity of the layers. In addition, the quality of the electrical insulation between the laminations is evaluated by quantifying the eddy current within the sample as a function of frequency. Fabricated laminations are comprised of uniform, smooth (surface roughness <100 nm) layers with effective electrical insulation for all layer thicknesses and insulator approaches studied. Such highly laminated structures have potential uses ranging from energy conversion to applications where composite materials with highly anisotropic mechanical or thermal properties are required. (paper)

  16. Free edge effects study in laminated composites using Digital Image Correlation: effect of material and geometrical singularities

    Directory of Open Access Journals (Sweden)

    Brieu M.

    2010-06-01

    Full Text Available Composite materials are today used for various industrial applications. However, delamination on free edges, where stress gradients are strong, still remain a problem. In the aim of a better understanding of such phenomenons, Digital Image Correlation (DIC measurements have been carried out on [(15n/-15n2]s laminates under uniaxial tensile strain. Three different composites with different mechanical properties and microstructure have been tested as well as two samples geometries: flat and with ply drop. Experimental results show high shear strain concentrations near 15°/-15° interlaminar interfaces on free edges which depend on material mechanical properties and microstructure and increase in the vicinity of a geometrical singularity.

  17. Morphological and mechanical analyses of laminates manufactured from randomly positioned carbon fibre/epoxy resin prepreg scraps

    Science.gov (United States)

    Souza, Christiane S. R.; Cândido, Geraldo M.; Alves, Wellington; Marlet, José Maria F.; Rezende, Mirabel C.

    2017-10-01

    This study aims to contribute to sustainability by proposing the reuse of composite prepreg scrap as an added value from discards. The research evaluates the microstructure and mechanical properties of laminates processed by the reuse of uncured carbon fibre/F155-epoxy resin prepreg scraps, waste from the ply cutting area of an aeronautical industry. The composite scraps were used as collected and were randomly positioned to produce laminates to be cured at an autoclave. The mechanical characterization shows a decrease of 39% for the compression property due to the discontinuous fibres in the laminate and an increase of 34% for the interlaminar shear strength, when compared to continuous fibre laminates. This increase is attributed to the higher crosslink density of the epoxy resin, as a result of the cure temperature used in autoclave (60 °C higher than suggested by supplier) and also to the randomly positioned scraps. Microscopic analyses confirm the consolidation of laminates, although show resin rich areas with different sizes and shapes attributed to the overlapping of the scraps with different sizes and shapes. These resin rich areas may contribute to decrease the mechanical properties of laminates. The correlation between mechanical and morphological results shows potential to be used on non-critical structural application, as composite jigs, contributing to sustainability.

  18. Predictions of Poisson's ratio in cross-ply laminates containing matrix cracks and delaminations

    Science.gov (United States)

    Harris, Charles E.; Allen, David H.; Nottorf, Eric W.

    1989-01-01

    A damage-dependent constitutive model for laminated composites has been developed for the combined damage modes of matrix cracks and delaminations. The model is based on the concept of continuum damage mechanics and uses second-order tensor valued internal state variables to represent each mode of damage. The internal state variables are defined as the local volume average of the relative crack face displacements. Since the local volume for delaminations is specified at the laminate level, the constitutive model takes the form of laminate analysis equations modified by the internal state variables. Model implementation is demonstrated for the laminate engineering modulus E(x) and Poisson's ratio nu(xy) of quasi-isotropic and cross-ply laminates. The model predictions are in close agreement to experimental results obtained for graphite/epoxy laminates.

  19. Influence of firing time and framework thickness on veneered Y-TZP discs curvature.

    Science.gov (United States)

    Jakubowicz-Kohen, Boris D; Sadoun, Michaël J; Douillard, Thierry; Mainjot, Amélie K

    2014-02-01

    The objective of the present work was to study the curvature of very thinly, veneered Y-TZP discs of different framework thicknesses submitted to different firing times. Fifteen 20-mm-wide Y-TZP discs were produced in three different thicknesses: 0.75, 1, 1.5mm. One disc from each group was left unveneered while the others were layered with a 0.1mm veneering ceramic layer. All discs underwent five firing cycles for a total cumulative firing time of 30 min, 1, 2, 5 and 10h at 900°C. The curvature profile was measured using a profilometer after the veneering process and after each firing cycle respectively. A fitted curve was then used to estimate the, curvature radius. The coefficient of thermal expansion (CTE) measurements were taken on veneering, ceramic and Y-TZP beam samples that underwent the same firing schedule. Those data were used to calculate the curvature generated by CTE variations over firing time. All bilayered samples exhibited a curvature that increased over firing time inversely to framework thickness. However non-veneered samples did not exhibit any curvature modification. The results of the present study reveal that even a very thin veneer layer (0.1mm) can induce a significant curvature of Y-TZP discs. The dilatometric results showed that Tg and CTE, variations are not sufficient to explain this curvature. A chemical-induced zirconia volume, augmentation located at the framework sub-surface near the interface could explain the sample, curvature and its increase with firing time. Copyright © 2013 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

  20. The effects of embedded piezoelectric fiber composite sensors on the structural integrity of glass-fiber–epoxy composite laminate

    International Nuclear Information System (INIS)

    Konka, Hari P; Wahab, M A; Lian, K

    2012-01-01

    Piezoelectric fiber composite sensors (PFCSs) made from micro-sized lead zirconate titanate (PZT) fibers have many advantages over the traditional bulk PZT sensors for embedded sensor applications. PFCSs as embedded sensors will be an ideal choice to continuously monitor the stress/strain levels and health conditions of composite structures. PFCSs are highly flexible, easily embeddable, have high compatibility with composite structures, and also provides manufacturing flexibility. This research is focused on examining the effects of embedding PFCS sensors (macro-fiber composite (MFC) and piezoelectric fiber composite (PFC)) on the structural integrity of glass-fiber–epoxy composite laminates. The strengths of composite materials with embedded PFCSs and conventional PZT sensors were compared, and the advantages of PFCS sensors over PZTs were demonstrated. Initially a numerical simulation study is performed to understand the local stress/strain field near the embedded sensor region inside a composite specimen. High stress concentration regions were observed near the embedded sensor corner edge. Using PFCS leads to a reduction of 56% in longitudinal stress concentration and 38% in transverse stress concentration, when compared to using the conventional PZTs as embedded sensors. In-plane tensile, in-plane tension–tension fatigue, and short beam strength tests are performed to evaluate the strengths/behavior of the composite specimens containing embedded PFCS. From the tensile test it is observed that embedding PFCS and PZT sensors in the composite structures leads to a reduction in ultimate strength by 3 and 6% respectively. From the fatigue test results it is concluded that both embedded PFCS and PZT sensors do not have a significant effect on the fatigue behavior of the composite specimens. From the short beam strength test it is found that embedding PFCS and PZT sensors leads to a reduction in shear strength by 7 and 15% respectively. Overall the pure PZT

  1. The effects of embedded piezoelectric fiber composite sensors on the structural integrity of glass-fiber-epoxy composite laminate

    Science.gov (United States)

    Konka, Hari P.; Wahab, M. A.; Lian, K.

    2012-01-01

    Piezoelectric fiber composite sensors (PFCSs) made from micro-sized lead zirconate titanate (PZT) fibers have many advantages over the traditional bulk PZT sensors for embedded sensor applications. PFCSs as embedded sensors will be an ideal choice to continuously monitor the stress/strain levels and health conditions of composite structures. PFCSs are highly flexible, easily embeddable, have high compatibility with composite structures, and also provides manufacturing flexibility. This research is focused on examining the effects of embedding PFCS sensors (macro-fiber composite (MFC) and piezoelectric fiber composite (PFC)) on the structural integrity of glass-fiber-epoxy composite laminates. The strengths of composite materials with embedded PFCSs and conventional PZT sensors were compared, and the advantages of PFCS sensors over PZTs were demonstrated. Initially a numerical simulation study is performed to understand the local stress/strain field near the embedded sensor region inside a composite specimen. High stress concentration regions were observed near the embedded sensor corner edge. Using PFCS leads to a reduction of 56% in longitudinal stress concentration and 38% in transverse stress concentration, when compared to using the conventional PZTs as embedded sensors. In-plane tensile, in-plane tension-tension fatigue, and short beam strength tests are performed to evaluate the strengths/behavior of the composite specimens containing embedded PFCS. From the tensile test it is observed that embedding PFCS and PZT sensors in the composite structures leads to a reduction in ultimate strength by 3 and 6% respectively. From the fatigue test results it is concluded that both embedded PFCS and PZT sensors do not have a significant effect on the fatigue behavior of the composite specimens. From the short beam strength test it is found that embedding PFCS and PZT sensors leads to a reduction in shear strength by 7 and 15% respectively. Overall the pure PZT sensors

  2. Hygrothermal effects on the tensile strength of carbon/epoxy laminates with molded edges

    Directory of Open Access Journals (Sweden)

    Cândido Geraldo Maurício

    2000-01-01

    Full Text Available The interlaminar stresses are confined to a region near the free edge. Therefore, the laminate stacking sequence and the free edge finishing are some of the factors that affect the strength of the laminate and limit its life. The use of molded edges eliminates the need for trimming and machining the laminates edges thus improving productivity. However, this fabrication technique may have a detrimental effect on the laminate strength for certain stacking sequences. This effect in the presence of moisture has not been characterized. This work presents the results of a comparative study of the resistance to delamination of laminates with machined edges and molded edges. Additionally, two environmental conditions were considered: dry laminates and laminates saturated with moisture. The tensile strength of the laminates were measured and micrographs were used to analyze the microstructure of the laminates near the free edges. It is concluded that the mechanical properties of advanced composites depend on the environmental conditions and the fabrication techniques used to produce the laminates. Therefore, it is necessary to account for these factors when experimentally determining the design allowables.

  3. Specific contribution of lamin A and lamin C in the development of laminopathies

    International Nuclear Information System (INIS)

    Sylvius, Nicolas; Hathaway, Andrea; Boudreau, Emilie; Gupta, Pallavi; Labib, Sarah; Bolongo, Pierrette M.; Rippstein, Peter; McBride, Heidi; Bilinska, Zofia T.; Tesson, Frederique

    2008-01-01

    Mutations in the lamin A/C gene are involved in multiple human disorders for which the pathophysiological mechanisms are partially understood. Conflicting results prevail regarding the organization of lamin A and C mutants within the nuclear envelope (NE) and on the interactions of each lamin to its counterpart. We over-expressed various lamin A and C mutants both independently and together in COS7 cells. When expressed alone, lamin A with cardiac/muscular disorder mutations forms abnormal aggregates inside the NE and not inside the nucleoplasm. Conversely, the equivalent lamin C organizes as intranucleoplasmic aggregates that never connect to the NE as opposed to wild type lamin C. Interestingly, the lamin C molecules present within these aggregates exhibit an abnormal increased mobility. When co-expressed, the complex formed by lamin A/C aggregates in the NE. Lamin A and C mutants for lipodystrophy behave similarly to the wild type. These findings reveal that lamins A and C may be differentially affected depending on the mutation. This results in multiple possible physiological consequences which likely contribute in the phenotypic variability of laminopathies. The inability of lamin C mutants to join the nuclear rim in the absence of lamin A is a potential pathophysiological mechanism for laminopathies

  4. Physical, mechanical, and fire properties of oriented strandboard with fire retardant treated veneers

    Science.gov (United States)

    Nadir Ayrilmis; Zeki Candan; Robert White

    2007-01-01

    This study evaluated physical, mechanical and fire properties of oriented strand boards (OSB) covered with fire retardant treated veneers. The beech (Fagus orientalis Lipsky) veneers were treated with either monoammonium phosphate, diammonium phosphate, lime water or a borax/boric acid (1 : 1 by weight) mixture. Physical and mechanical properties of the specimens were...

  5. DMTO – a method for Discrete Material and Thickness Optimization of laminated composite structures

    DEFF Research Database (Denmark)

    Sørensen, Søren Nørgaard; Sørensen, Rene; Lund, Erik

    2014-01-01

    This paper presents a gradient based topology optimization method for Discrete Material and Thickness Optimization of laminated composite structures, labelled the DMTOmethod. The capabilities of the proposed method are demonstrated on mass minimization, subject to constraints on the structural...... criteria; buckling load factors, eigenfrequencies, and limited displacements. Furthermore, common design guidelines or rules, referred to as manufacturing constraints, are included explicitly in the optimization problem as series of linear inequalities. The material selection and thickness variation...... to manufacturability. The results will thus give insight into the relation between potential weight saving and design complexity. The results show that the DMTO method is capable of solving the problems robustly with only few intermediate valued design variables....

  6. Effect of layering sequence and chemical treatment on the mechanical properties of woven kenaf–aramid hybrid laminated composites

    International Nuclear Information System (INIS)

    Yahaya, R.; Sapuan, S.M.; Jawaid, M.; Leman, Z.; Zainudin, E.S.

    2015-01-01

    Highlights: • The mechanical properties of woven kenaf/Kevlar hybrid composites were analysed. • The layering sequences affect the mechanical properties of hybrid composites. • Treated kenaf improves the mechanical properties of hybrid composites. - Abstract: This work aims to evaluate the effect of layering sequence and chemical treatment on mechanical properties of woven kenaf–Kevlar composites. Woven kenaf–aramid hybrid laminated composites fabricated through hand lay-up techniques by arranging woven kenaf and Kevlar fabrics in different layering sequences and by using treated kenaf mat. To evaluate the effect of chemical treatment on hybrid composites, the woven kenaf mat was treated with 6% sodium hydroxide (NaOH) diluted solution and compared mechanical properties with untreated kenaf hybrid composites. Results shows that the tensile properties of hybrid composites improved in 3-layer composites compared to 4-layer composites. Hybrid composite with Kevlar as outer layers display a better mechanical properties as compared to other hybrid composites. Tensile and flexural properties of treated hybrid composites are better than non-treated hybrid composites. The fractured surface of hybrid composites was investigated by scanning electron microscopy. This study is a part of exploration of potential application of the hybrid composite in high velocity impact application

  7. Normalization of Impact Energy by Laminate Thickness for Compression After Impact Testing

    Science.gov (United States)

    Nettles, A. T.; Hromisin, S. M.

    2013-01-01

    The amount of impact energy used to damage a composite laminate is a critical parameter when assessing residual strength properties. The compression after impact (CAI) strength of impacted laminates is dependent upon how thick the laminate is and this has traditionally been accounted for by normalizing (dividing) the impact energy by the laminate's thickness. However, when comparing CAI strength values for a given lay-up sequence and fiber/resin system, dividing the impact energy by the specimen thickness has been noted by the author to give higher CAI strength values for thicker laminates. A study was thus undertaken to assess the comparability of CAI strength data by normalizing the impact energy by the specimen thickness raised to a power to account for the higher strength of thicker laminates. One set of data from the literature and two generated in this study were analyzed by dividing the impact energy by the specimen thickness to the 1, 1.5, 2, and 2.5 powers. Results show that as laminate thickness and damage severity decreased, the value which the laminate thickness needs to be raised to in order to yield more comparable CAI data increases.

  8. 3D Progressive Damage Modeling for Laminated Composite Based on Crack Band Theory and Continuum Damage Mechanics

    Science.gov (United States)

    Wang, John T.; Pineda, Evan J.; Ranatunga, Vipul; Smeltzer, Stanley S.

    2015-01-01

    A simple continuum damage mechanics (CDM) based 3D progressive damage analysis (PDA) tool for laminated composites was developed and implemented as a user defined material subroutine to link with a commercially available explicit finite element code. This PDA tool uses linear lamina properties from standard tests, predicts damage initiation with an easy-to-implement Hashin-Rotem failure criteria, and in the damage evolution phase, evaluates the degradation of material properties based on the crack band theory and traction-separation cohesive laws. It follows Matzenmiller et al.'s formulation to incorporate the degrading material properties into the damaged stiffness matrix. Since nonlinear shear and matrix stress-strain relations are not implemented, correction factors are used for slowing the reduction of the damaged shear stiffness terms to reflect the effect of these nonlinearities on the laminate strength predictions. This CDM based PDA tool is implemented as a user defined material (VUMAT) to link with the Abaqus/Explicit code. Strength predictions obtained, using this VUMAT, are correlated with test data for a set of notched specimens under tension and compression loads.

  9. Thermoelectrically induced nonlinear free vibration analysis of piezo laminated composite conical shell panel with random fiber orientation

    Directory of Open Access Journals (Sweden)

    Lal Achchhe

    2017-09-01

    Full Text Available This paper presents the free vibration response of piezo laminated composite geometrically nonlinear conical shell panel subjected to a thermo-electrical loading. The temperature field is assumed to be a uniform distribution over the shell surface and through the shell thickness and the electric field is assumed to be the transverse component E2 only. The material properties are assumed to be independent of the temperature and the electric field. The basic formulation is based on higher order shear deformation plate theory (HSDT with von-Karman nonlinearity. A C0 nonlinear finite element method based on direct iterative approach is outlined and applied to solve nonlinear generalized eigenvalue problem. Parametric studies are carried out to examine the effect of amplitude ratios, stacking sequences, cone angles, piezoelectric layers, applied voltages, circumferential length to thickness ratios, change in temperatures and support boundary conditions on the nonlinear natural frequency of laminated conical shell panels. The present outlined approach has been validated with those available results in the literature.

  10. A 2D Daubechies finite wavelet domain method for transient wave response analysis in shear deformable laminated composite plates

    Science.gov (United States)

    Nastos, C. V.; Theodosiou, T. C.; Rekatsinas, C. S.; Saravanos, D. A.

    2018-03-01

    An efficient numerical method is developed for the simulation of dynamic response and the prediction of the wave propagation in composite plate structures. The method is termed finite wavelet domain method and takes advantage of the outstanding properties of compactly supported 2D Daubechies wavelet scaling functions for the spatial interpolation of displacements in a finite domain of a plate structure. The development of the 2D wavelet element, based on the first order shear deformation laminated plate theory is described and equivalent stiffness, mass matrices and force vectors are calculated and synthesized in the wavelet domain. The transient response is predicted using the explicit central difference time integration scheme. Numerical results for the simulation of wave propagation in isotropic, quasi-isotropic and cross-ply laminated plates are presented and demonstrate the high spatial convergence and problem size reduction obtained by the present method.

  11. Hygrotermal effects evaluation using the losipescu shear test for glare laminates

    OpenAIRE

    Botelho, Edson Cocchieri [UNESP; Rezende, Mirabel C.; Pardini, Luis Claudio

    2008-01-01

    Fiber-metal laminates (FML) composed of alternating layers of unidirectional fibers-reinforced plastic (FRP) laminae and aluminum-alloy sheets offer some superior mechanical properties, compared with either conventional laminates consisting of only, FRP laminae or high-strength monolithic aluminum alloys. The environmental factors can limit the applications of composites by deteriorating the mechanical properties during service. Usually, polymeric matrix absorbs moisture when exposed to humid...

  12. Hygrotermal effects evaluation using the iosipescu shear test for glare laminates

    OpenAIRE

    Botelho, Edson C.; Rezende, Mirabel C.; Pardini, Luis Claudio

    2008-01-01

    Fiber-metal laminates (FML) composed of alternating layers of unidirectional fiber-reinforced plastic (FRP) laminae and aluminum-alloy sheets offer some superior mechanical properties, compared with either conventional laminates consisting of only FRP laminae or high-strength monolithic aluminum alloys. The environmental factors can limit the applications of composites by deteriorating the mechanical properties during service. Usually, polymeric matrix absorbs moisture when exposed to humid e...

  13. Wear Behavior of Cold Pressed and Sintered Al2O3/TiC/CaF2Al2O3/TiC Laminated Ceramic Composite

    Institute of Scientific and Technical Information of China (English)

    Xuefeng YANG; Jian CHENG; Peilong SONG; Shouren WANG; Liying YANG; Yanjun WANG; Ken MAO

    2013-01-01

    A novel laminated Al2O3/TiC/CaF2-Al2O3/TiC sandwich ceramic composite was fabricated through cold pressing and sintering to achieve better anti-wear performance,such as low friction coefficient and low wear rate.Al2O3/TiC/CaF2 and Al2O3/TiC composites were alternatively built layer-by-layer to obtain a sandwich structure.Solid lubricant CaF2 was added evenly into the Al2O3/TiC/CaF2 layer to reduce the friction and wear.Al2O3/TiC ceramic was also cold pressed and sintered for comparison.Friction analysis of the two ceramics was then conducted via a wear-and-tear machine.Worn surface and surface compositions were examined by scanning electron microscopy and energy dispersion spectrum,respectively.Results showed that the laminated Al2O3/TiC/CaF2-Al2O3/TiC sandwich ceramic composite has lower friction coefficient and lower wear rate than those of Al2O3/TiC ceramic alone because of the addition of CaF2 into the laminated Al2O3/TiC/CaF2-Al2O3/TiC sandwich ceramic composite.Under the friction load,the tiny CaF2 particles were scraped from the Al2O3/TiC/CaF2 layer and spread on friction pairs before falling off into micropits.This process formed a smooth,self-lubricating film,which led to better anti-wear properties.Adhesive wear is the main wear mechanism of Al2O3/TiC/CaF2 layer and abrasive wear is the main wear mechanism of Al2O3/TiC layer.

  14. Low-cost, environmentally friendly route for producing CFRP laminates with microfibrillated cellulose interphase

    Directory of Open Access Journals (Sweden)

    B. E. B. Uribe

    2017-01-01

    Full Text Available In this paper, a cost-effective and eco-friendly method to improve mechanical performance in continuous carbon fiber-reinforced polymer (CFRP matrix composites is presented. Unsized fiber fabric preforms are coated with self-assembling sugarcane bagasse microfibrillated cellulose, and undergo vacuum-assisted liquid epoxy resin infusion to produce solid laminates after curing at ambient temperature. Quasi-static tensile, flexural and short beam testing at room temperature indicated that the stiffness, ultimate strength and toughness at ultimate load of the brand-new two-level hierarchical composite are substantially higher than in baseline, unsized fiber-reinforced epoxy laminate. Atomic force microscopy for height and phase imaging, along with scanning electron microscopy for the fracture surface survey, revealed a 400 nm-thick fiber/matrix interphase wherein microfibrillated cellulose exerts strengthening and toughening roles in the hybrid laminate. Market expansion of this class of continuous fiber-reinforced-polymer matrix composites exhibiting remarkable mechanical performance/cost ratios is thus conceivable.

  15. Analysis of the low-frequency magnetoelectric performance in three-phase laminate composites with Fe-based nanocrystalline ribbon

    International Nuclear Information System (INIS)

    Chen, Lei; Li, Ping; Wen, Yumei; Zhu, Yong

    2013-01-01

    The theoretical analysis of magnetoelectric (ME) performance in three-phase Terfenol-D/PZT/FeCuNbSiB (MPF) laminate composite is presented in this paper. The ME couplings at low frequency for ideal and less than ideal interface couplings are studied, respectively, and our analysis predicts that (i) the ME voltage coefficient for ideal interface coupling increases with the increasing layers (n) of Fe-based nanocrystalline ribbon FeCuNbSiB (Fe 73.5 Cu 1 Nb 3 Si 13.5 B 9 ) while the sizes of PZT (Pb(Zr 1−x Ti x )O 3 ) and Terfenol-D (Tb 1−x Dy x Fe 2−y ) are kept constant, and then it tends to be a constant when the layers of FeCuNbSiB are >100; (ii) by introducing the interface coupling factor k and considering the degradation of d 33m,f with n, the ME voltage coefficient for a less than ideal interface condition is predicted. As the FeCuNbSiB layer increases, it first increases and reaches to a maximum value, and then slowly decreases. Various MPF laminates are fabricated and tested. It is found that the theoretical predictions for the consideration of actual boundary conditions at the interface are in agreement with the experimental observations. This study plays a guiding role for the design of MPF composite in real applications. (paper)

  16. Invertebrate lamins

    International Nuclear Information System (INIS)

    Melcer, Shai; Gruenbaum, Yosef; Krohne, Georg

    2007-01-01

    Lamins are the main component of the nuclear lamina and considered to be the ancestors of all intermediate filament proteins. They are localized mainly at the nuclear periphery where they form protein complexes with integral proteins of the nuclear inner membrane, transcriptional regulators, histones and chromatin modifiers. Studying lamins in invertebrate species has unique advantages including the smaller number of lamin genes in the invertebrate genomes and powerful genetic analyses in Caenorhabditis elegans and Drosophila melanogaster. These simpler nuclear lamina systems allow direct analyses of their structure and functions. Here we give an overview of recent advances in the field of invertebrate nuclear lamins with special emphasis on their evolution, assembly and functions

  17. High Pressure Laminates with Antimicrobial Properties

    Directory of Open Access Journals (Sweden)

    Sandra Magina

    2016-02-01

    Full Text Available High-pressure laminates (HPLs are durable, resistant to environmental effects and good cost-benefit decorative surface composite materials with special properties tailored to meet market demand. In the present work, polyhexamethylene biguanide (PHMB was incorporated for the first time into melamine-formaldehyde resin (MF matrix on the outer layer of HPLs to provide them antimicrobial properties. Chemical binding of PHMB to resin matrix was detected on the surface of produced HPLs by attenuated total reflection Fourier transform infrared spectroscopy (ATR-FTIR. Antimicrobial evaluation tests were carried out on the ensuing HPLs doped with PHMB against gram-positive Listeria innocua and gram-negative Escherichia coli bacteria. The results revealed that laminates prepared with 1.0 wt % PHMB in MF resin were bacteriostatic (i.e., inhibited the growth of microorganisms, whereas those prepared with 2.4 wt % PHMB in MF resin exhibited bactericidal activity (i.e., inactivated the inoculated microorganisms. The results herein reported disclose a promising strategy for the production of HPLs with antimicrobial activity without affecting basic intrinsic quality parameters of composite material.

  18. Role of core support material in veneer failure of brittle layer structures.

    Science.gov (United States)

    Hermann, Ilja; Bhowmick, Sanjit; Lawn, Brian R

    2007-07-01

    A study is made of veneer failure by cracking in all-ceramic crown-like layer structures. Model trilayers consisting of a 1 mm thick external glass layer (veneer) joined to a 0.5 mm thick inner stiff and hard ceramic support layer (core) by epoxy bonding or by fusion are fabricated for testing. The resulting bilayers are then glued to a thick compliant polycarbonate slab to simulate a dentin base. The specimens are subjected to cyclic contact (occlusal) loading with spherical indenters in an aqueous environment. Video cameras are used to record the fracture evolution in the transparent glass layer in situ during testing. The dominant failure mode is cone cracking in the glass veneer by traditional outer (Hertzian) cone cracks at higher contact loads and by inner (hydraulically pumped) cone cracks at lower loads. Failure is deemed to occur when one of these cracks reaches the veneer/core interface. The advantages and disadvantages of the alumina and zirconia core materials are discussed in terms of mechanical properties-strength and toughness, as well as stiffness. Consideration is also given to the roles of interface strength and residual thermal expansion mismatch stresses in relation to the different joining methods. Copyright 2006 Wiley Periodicals, Inc.

  19. Effects of stacking sequence on impact damage resistance and residual strength for quasi-isotropic laminates

    Science.gov (United States)

    Dost, Ernest F.; Ilcewicz, Larry B.; Avery, William B.; Coxon, Brian R.

    1991-01-01

    Residual strength of an impacted composite laminate is dependent on details of the damage state. Stacking sequence was varied to judge its effect on damage caused by low-velocity impact. This was done for quasi-isotropic layups of a toughened composite material. Experimental observations on changes in the impact damage state and postimpact compressive performance were presented for seven different laminate stacking sequences. The applicability and limitations of analysis compared to experimental results were also discussed. Postimpact compressive behavior was found to be a strong function of the laminate stacking sequence. This relationship was found to depend on thickness, stacking sequence, size, and location of sublaminates that comprise the impact damage state. The postimpact strength for specimens with a relatively symmetric distribution of damage through the laminate thickness was accurately predicted by models that accounted for sublaminate stability and in-plane stress redistribution. An asymmetric distribution of damage in some laminate stacking sequences tended to alter specimen stability. Geometrically nonlinear finite element analysis was used to predict this behavior.

  20. Effect of various intermediate ceramic layers on the interfacial stability of zirconia core and veneering ceramics.

    Science.gov (United States)

    Yoon, Hyung-In; Yeo, In-Sung; Yi, Yang-Jin; Kim, Sung-Hun; Lee, Jai-Bong; Han, Jung-Suk

    2015-01-01

    The purposes of this study were to evaluate the effects of intermediate ceramics on the adhesion between the zirconia core and veneer ceramics. The polished surfaces of fully sintered Y-TZP blocks received three different treatments: (1) connector (C), (2) liner (L) or (3) wash layer (W). All the treated zirconia blocks were veneered with either (a) fluorapatite glass-ceramic (E) or (b) feldspathic porcelain (V) and divided into four groups (CE, CV, LE and WV). For the control group, the testing surfaces of metal blocks were veneered with feldspathic porcelain (VM). A half of the samples in each group (n = 21) were exposed to thermocycling, while the other half of the specimens were stored at room temperature under dry conditions. All specimens were subjected to the shear test and the failed surfaces were microscopically examined. The elemental distribution at the zirconia core/veneer interface was analyzed. The specimens in Groups CE and CV exhibited significantly greater mean bond strength values than those in Groups LE and WV, respectively (p ceramic substances into the zirconia surface. A glass-ceramic based connector is significantly more favorable to core/veneer adhesion than the other intermediate ceramics evaluated in the study. However, thermal cycling affected the bond strength at the core/veneer interface differently according to the intermediate ceramics.

  1. Influence of framework color and layering technique on the final color of zirconia veneered restorations

    NARCIS (Netherlands)

    Aboushelib, M.N.; Dozic, A.; Liem, J.K.

    2010-01-01

    Objective: To investigate the influence of colored zirconia frameworks on the overall color match of zirconia- veneered restorations. Method and Materials: Identical natural and colored zirconia frameworks (Cercon Base, Degudent) were layered using a veneer ceramic (IPS e.max Ceram Dentin, Ivoclar

  2. Polymer Composites Corrosive Degradation: A Computational Simulation

    Science.gov (United States)

    Chamis, Christos C.; Minnetyan, Levon

    2007-01-01

    A computational simulation of polymer composites corrosive durability is presented. The corrosive environment is assumed to manage the polymer composite degradation on a ply-by-ply basis. The degradation is correlated with a measured pH factor and is represented by voids, temperature and moisture which vary parabolically for voids and linearly for temperature and moisture through the laminate thickness. The simulation is performed by a computational composite mechanics computer code which includes micro, macro, combined stress failure and laminate theories. This accounts for starting the simulation from constitutive material properties and up to the laminate scale which exposes the laminate to the corrosive environment. Results obtained for one laminate indicate that the ply-by-ply degradation degrades the laminate to the last one or the last several plies. Results also demonstrate that the simulation is applicable to other polymer composite systems as well.

  3. Influence of cooling rate on residual stress profile in veneering ceramic: measurement by hole-drilling.

    Science.gov (United States)

    Mainjot, Amélie K; Schajer, Gary S; Vanheusden, Alain J; Sadoun, Michaël J

    2011-09-01

    The manufacture of dental crowns and bridges generates residual stresses within the veneering ceramic and framework during the cooling process. Residual stress is an important factor that control the mechanical behavior of restorations. Knowing the stress distribution within the veneering ceramic as a function of depth can help the understanding of failures, particularly chipping, a well-known problem with Yttria-tetragonal-zirconia-polycrystal based fixed partial dentures. The objective of this study is to investigate the cooling rate dependence of the stress profile in veneering ceramic layered on metal and zirconia frameworks. The hole-drilling method, often used for engineering measurements, was adapted for use with veneering ceramic. The stress profile was measured in bilayered disc samples 20 mm in diameter, with a 0.7 mm thick metal or Yttria-tetragonal-zirconia-polycrystal framework and a 1.5mm thick veneering ceramic. Three different cooling procedures were investigated. The magnitude of the stresses in the surface of the veneering ceramic was found to increase with cooling rate, while the interior stresses decreased. At the surface, compressive stresses were observed in all samples. In the interior, compressive stresses were observed in metal samples and tensile in zirconia samples. Cooling rate influences the magnitude of residual stresses. These can significantly influence the mechanical behavior of metal-and zirconia-based bilayered systems. The framework material influenced the nature of the interior stresses, with zirconia samples showing a less favorable stress profile than metal. Copyright © 2011 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

  4. Method and Apparatus for High-Permeability Magnetostrictive/Piezo-Fiber Laminates Having Colossal, Near-Ideal Magnetoelectricity

    OpenAIRE

    2007-01-01

    An ME composite laminate of at least one (1-3) piezo-fiber layer coupled with high-permeability alloy magnetostrictive layers, optionally formed of FeBSiC or equivalent. The composite laminate alternates the (1-3) piezo-fiber and high-permeability alloy magnetostrictive layers in a stacked manner. Optionally, the magnetization direction of the high-permeability alloy magnetostrictive layers and polarization direction of the piezo-fiber layer are an (L-L) arrangement. Optionally, thin film pol...

  5. Fatigue of cord-rubber composites for tires

    Science.gov (United States)

    Song, Jaehoon

    Fatigue behaviors of cord-rubber composite materials forming the belt region of radial pneumatic tires have been characterized to assess their dependence on stress, strain and temperature history as well as materials composition and construction . Using actual tires, it was found that interply shear strain is one of the crucial parameters for damage assessment from the result that higher levels of interply shear strain of actual tires reduce the fatigue lifetime. Estimated at various levels of load amplitude were the fatigue life, the extent and rate of resultant strain increase ("dynamic creep"), cyclic strains at failure, and specimen temperature. The interply shear strain of 2-ply 'tire belt' composite laminate under circumferential tension was affected by twisting of specimen due to tension-bending coupling. However, a critical level of interply shear strain, which governs the gross failure of composite laminate due to the delamination, appeared to be independent of different lay-up of 2-ply vs. symmetric 4-ply configuration. Reflecting their matrix-dominated failure modes such as cord-matrix debonding and delamination, composite laminates with different cord reinforcements showed the same S-N relationship as long as they were constructed with the same rubber matrix, the same cord angle, similar cord volume, and the same ply lay-up. Because of much lower values of single cycle strength (in terms of gross fracture load per unit width), the composite laminates with larger cord angle and the 2-ply laminates exhibited exponentially shorter fatigue lifetime, at a given stress amplitude, than the composite laminates with smaller cord angle and 4-ply symmetric laminates, respectively. The increase of interply rubber thickness lengthens their fatigue lifetime at an intermediate level of stress amplitude. However, the increase in the fatigue lifetime of the composite laminate becomes less noticeable at very low stress amplitude. Even with small compressive cyclic

  6. On micro to mesoscale homogenization of electrical properties for damaged laminated composites (and their potential applications in electrical tomography)

    KAUST Repository

    Selvakumaran, Lakshmi

    2015-12-01

    Efficient and optimal use of composites in structures requires tools to monitor and capture the complex degradation that can occur within the laminates over time. Structural health monitoring (SHM) techniques uses sensors/actuators on the structure to progressively monitor the health of the structure with minimal manual intervention. Electrical tomography (ET) is a SHM technique that uses voltage measurements from the surface of the laminate to reconstruct a conductivity map of the structure. Since damage has been shown to modify the conductivity of the laminate, the conductivity map can provide an indirect measure of the damage within the material. Studies have shown the capability of ET to identify macroscale damage due to impact. But, little has been done to quantitatively assess damage using ET. In this work, we present a theoretical framework to link degradation mechanisms occuring at the microscale to the conductivity at the mesoscale through damage indicators. The mesoscale damage indicators are then shown to be intrinsic to the ply. Next, we use the knowledge obtained through mesoscale homogenization to study the detectability of transverse cracks. Last, we show how the mesoscale homogenization participates in regularization of the inverse problem and in the quantitative assessment of the reconstructed conductivity map. This is as such the first step towards turning ET into a viable quantitative health monitoring technique.

  7. Simulation of guided-wave ultrasound propagation in composite laminates: Benchmark comparisons of numerical codes and experiment.

    Science.gov (United States)

    Leckey, Cara A C; Wheeler, Kevin R; Hafiychuk, Vasyl N; Hafiychuk, Halyna; Timuçin, Doğan A

    2018-03-01

    Ultrasonic wave methods constitute the leading physical mechanism for nondestructive evaluation (NDE) and structural health monitoring (SHM) of solid composite materials, such as carbon fiber reinforced polymer (CFRP) laminates. Computational models of ultrasonic wave excitation, propagation, and scattering in CFRP composites can be extremely valuable in designing practicable NDE and SHM hardware, software, and methodologies that accomplish the desired accuracy, reliability, efficiency, and coverage. The development and application of ultrasonic simulation approaches for composite materials is an active area of research in the field of NDE. This paper presents comparisons of guided wave simulations for CFRP composites implemented using four different simulation codes: the commercial finite element modeling (FEM) packages ABAQUS, ANSYS, and COMSOL, and a custom code executing the Elastodynamic Finite Integration Technique (EFIT). Benchmark comparisons are made between the simulation tools and both experimental laser Doppler vibrometry data and theoretical dispersion curves. A pristine and a delamination type case (Teflon insert in the experimental specimen) is studied. A summary is given of the accuracy of simulation results and the respective computational performance of the four different simulation tools. Published by Elsevier B.V.

  8. Bovine laminitis: clinical aspects, pathology and pathogenesis with reference to acute equine laminitis.

    Science.gov (United States)

    Boosman, R; Németh, F; Gruys, E

    1991-07-01

    This review deals with the features of clinical and subclinical laminitis in cattle. Prominent clinical signs of acute laminitis are a tender gait and arched back. The sole horn reveals red and yellowish discolourations within five days. In subacute and chronic cases clinical signs are less severe. In chronic laminitis the shape of the claws is altered. Laminitis is frequently followed by sole ulceration and white zone lesions. Blood tests showed no significant changes for laminitic animals. Arteriographic studies of claws affected by laminitis indicated that blood vessels had narrowed lumens. Gross pathology revealed congestion of the corium and rotation of the distal phalanx. Histopathologic studies indicate that laminitis is associated with changes of the vasculature. Peripartum management and nutrition are important factors in its aetiology. It is hypothesised that laminitis is evoked by disturbed digital circulation. In the pathogenesis of acute laminitis three factors are considered important: the occurrence of thrombosis, haemodynamic aspects of the corium, and endotoxins which trigger these pathologic events.

  9. Towards mechanisms-guided resistivity-based monitoring of damage evolution in laminated composites

    KAUST Repository

    Lubineau, Gilles

    2013-04-05

    A convenient health monitoring technique for detecting degradation in laminated composite is to monitor the change of electrical resistance along multiple conduction paths within the structure. Yet, the relations between the global modification of resistivity and the exact underlying damage map is still unclear that makes diffcult to interpret these nondestructive-testing results. The challenge is then to be able to reconstruct from these global observation the underlying damage map. This is even more diffcult due to the numerous underlying damage mechanisms that can take place either at the inter laminar of intra laminar level. This paper intends to provide some preliminary insights about strategies to recover the damage state based only on global measurements. We focus here on transverse cracking detection. We introduce the homogenization process that defines at the meso scale an equivalent homogeneous ply that is energetically equivalent to the cracked one. This can be used as a first tool to reconstruct damage maps based on global resistivity measurements.

  10. Influence of thermal expansion mismatch on residual stress profile in veneering ceramic layered on zirconia: Measurement by hole-drilling.

    Science.gov (United States)

    Mainjot, Amélie K; Najjar, Achref; Jakubowicz-Kohen, Boris D; Sadoun, Michaël J

    2015-09-01

    Mismatch in thermal expansion coefficient between core and veneering ceramic (Δα=αcore-αveneer, ppm/°C) is reported as a crucial parameter influencing veneer fractures with Yttria-tetragonal-zirconia-polycrystal (Y-TZP) prostheses, which still constitutes a misunderstood problem. However, the common positive Δα concept remains empirical. The objective of this study is to investigate the Δα dependence of residual stress profiles in veneering ceramic layered on Y-TZP frameworks. The stress profile was measured with the hole-drilling method in bilayered disc samples of 20mm diameter with a 0.7mm thick Y-TZP framework and a 1.5mm thick veneer layer. 3 commercial and 4 experimental veneering ceramics (n=3 per group) were used to obtain different Δα varying from -1.3ppm/°C to +3.2ppm/°C, which were determined by dilatometric analyses. Veneer fractures were observed in samples with Δα≥+2.3 or ≤-0.3ppm/°C. Residual stress profiles measured in other groups showed compressive stresses in the surface, these stresses decreasing with depth and then becoming more compressive again near the interface. Small Δα variations were shown to induce significant changes in residual stress profiles. Compressive stress near the framework was found to decrease inversely to Δα. Veneer CTE close to Y-TZP (+0.2ppm/°C Δα) gived the most favorable stress profile. Yet, near the framework, Δα-induced residual stress varied inversely to predictions. This could be explained by the hypothesis of structural changes occurrence within the Y-TZP surface. Consequently, the optimum Δα value cannot be determined before understanding Y-TZP's particular behavior when veneered. Copyright © 2015 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

  11. Steel skin - SMC laminate structures for lightweight automotive manufacturing

    Science.gov (United States)

    Quagliato, Luca; Jang, Changsoon; Murugesan, Mohanraj; Kim, Naksoo

    2017-09-01

    In the present research work an innovative material, made of steel skin and sheet molding compound core, is presented and is aimed to be utilized for the production of automotive body frames. For a precise description of the laminate structure, the material properties of all the components, including the adhesive utilized as an interlayer, have been carried out, along with the simple tension test of the composite material. The result have shown that the proposed laminate structure has a specific yield strength 114% higher than 6061 T6 aluminum, 34% higher than 7075 T6 aluminum, 186% higher than AISI 304 stainless steel (30HRC) and 42% than SK5 high-strength steel (52HRC), showing its reliability and convenience for the realization of automotive components. After calibrating the material properties of the laminate structure, and utilizing as reference the simple tension results of the laminate structure, the derived material properties have been utilized for the simulation of the mechanical behavior of an automotive B-pillar. The results have been compared with those of a standard B-pillar made of steel, showing that the MS-SMC laminate structure manifests load and impact carry capacity comparable with those of high strength steel, while granting, at least, an 11% weight reduction.

  12. Comparison of Bending Creep Behavior of Bamboo-based Composites Manufactured by Two Types of Stacking Sequences

    Directory of Open Access Journals (Sweden)

    Xinxin Ma

    2014-07-01

    Full Text Available The study of viscoelastic and mechano-sorptive creep on bamboo laminated veneer lumber (BLVL and bamboo/poplar plywood (BPP is described in this paper. Bending creep tests parallel to the grain were carried out on two bamboo-based composites for a length of 90 days. The specimens measured 500 mm × 20 mm × 12 mm. Based on the experimental data, the creep curves of two boards were evaluated. The results are summarized as follows: (1 the anti-creep property of BLVL was better than that of BPP; (2 two creep curves were successfully approximated using the Burgers model and the power law model. The required experimental term for the creep test to estimate an accurate long-term curve is 2 or 3 years when the power law is used for the estimation; and (3 compared with the creep curve in a constant environment, the creep deformation changed more dramatically under varying environment.

  13. Effects of vertically aligned carbon nanotubes on shear performance of laminated nanocomposite bonded joints

    Directory of Open Access Journals (Sweden)

    Davood Askari and Mehrdad N Ghasemi-Nejhad

    2012-01-01

    Full Text Available The main objective is to improve the most commonly addressed weakness of the laminated composites (i.e. delamination due to poor interlaminar strength using carbon nanotubes (CNTs as reinforcement between the laminae and in the transverse direction. In this work, a chemical vapor deposition technique has been used to grow dense vertically aligned arrays of CNTs over the surface of chemically treated two-dimensionally woven cloth and fiber tows. The nanoforest-like fabrics can be used to fabricate three-dimensionally reinforced laminated nanocomposites. The presence of CNTs aligned normal to the layers and in-between the layers of laminated composites is expected to considerably enhance the properties of the laminates. To demonstrate the effectiveness of our approach, composite single lap-joint specimens were fabricated for interlaminar shear strength testing. It was observed that the single lap-joints with through-the-thickness CNT reinforcement can carry considerably higher shear stresses and strains. Close examination of the test specimens showed that the failure of samples with CNT nanoforests was completely cohesive, while the samples without CNT reinforcement failed adhesively. This concludes that the adhesion of adjacent carbon fabric layers can be considerably improved owing to the presence of vertically aligned arrays of CNT nanoforests.

  14. Effects of vertically aligned carbon nanotubes on shear performance of laminated nanocomposite bonded joints.

    Science.gov (United States)

    Askari, Davood; Ghasemi-Nejhad, Mehrdad N

    2012-08-01

    The main objective is to improve the most commonly addressed weakness of the laminated composites (i.e. delamination due to poor interlaminar strength) using carbon nanotubes (CNTs) as reinforcement between the laminae and in the transverse direction. In this work, a chemical vapor deposition technique has been used to grow dense vertically aligned arrays of CNTs over the surface of chemically treated two-dimensionally woven cloth and fiber tows. The nanoforest-like fabrics can be used to fabricate three-dimensionally reinforced laminated nanocomposites. The presence of CNTs aligned normal to the layers and in-between the layers of laminated composites is expected to considerably enhance the properties of the laminates. To demonstrate the effectiveness of our approach, composite single lap-joint specimens were fabricated for interlaminar shear strength testing. It was observed that the single lap-joints with through-the-thickness CNT reinforcement can carry considerably higher shear stresses and strains. Close examination of the test specimens showed that the failure of samples with CNT nanoforests was completely cohesive, while the samples without CNT reinforcement failed adhesively. This concludes that the adhesion of adjacent carbon fabric layers can be considerably improved owing to the presence of vertically aligned arrays of CNT nanoforests.

  15. Straight studs from southern pine veneer cores and cordwood

    Science.gov (United States)

    Peter Koch

    1968-01-01

    An economically feasible system has been developed for converting southern pine veneer cores into straight 8-foot studs (2). Prototype studs - two per core - were 100 percent SPIB stud grade and better.

  16. Indirect veneer treatment of anterior maxillary teeth with enamel hypoplasia

    Directory of Open Access Journals (Sweden)

    Devi Eka Juniarti

    2010-09-01

    Full Text Available Background: Nowadays, aesthetic rehabilitation becomes a necessity. It is affected by patient’s background, especially career, social and economic status. The aesthetic abnormality of anterior teeth i.e discoloration, malposition and malformation can affect patient’s appearance, especially during smile. These dental abnormalities, as a result, can decrease patient’s performance. Dental malformation, for instance, can be caused by developmental tooth defect, such as enamel hypoplasia. Enamel hypoplasia is a developmental defect caused by the lack of matrix amount which leads to thin and porous enamel. Enamel hypoplasia can also be caused by matrix calcification disturbance starting from the formation and development of enamel matrix causing defect and permanent changes which can occur on one or more tooth. Purpose: The aim of the study is to improve dental discoloration and tooth surface texture on anterior maxillary teeth with enamel hypoplasia by using indirect veneer with porcelain material. Case: A 20 years-old woman with enamel hypoplasia came to the Dental Hospital, Faculty of Dentistry Airlangga University. The patient wanted to improve her anterior maxillary teeth. It is clinically known that there were some opaque white spots (chalky spotted and porous on anterior teeth’s surface. Case management: Indirect veneer with porcelain material had been chosen as a restoration treatment which has excellent aesthetics and strength, and did not cause gingival irritation. As a result, the treatment could improve the confidence of the patient, and could also make their function normal. Conclusion: Indirect veneer is an effective treatment, which can improve patient’s appearance and self confidence.Latar belakang: Saat ini perbaikan estetik menjadi suatu kebutuhan. Kebutuhan akan estetik dipengaruhi latar belakang penderita, terutama karir, status sosial dan ekonomi. Hal ini disebabkan, kelainan estetik seperti diskolorasi, malposisi

  17. Detection and Evaluation of Pre-Preg Gaps and Overlaps in Glare Laminates

    Science.gov (United States)

    Nardi, Davide; Abouhamzeh, Morteza; Leonard, Rob; Sinke, Jos

    2018-03-01

    Gaps and overlaps between pre-preg plies represent common flaws in composite materials that can be introduced easily in an automated fibre placement manufacturing process and are potentially detrimental for the mechanical performances of the final laminates. Whereas gaps and overlaps have been addressed for full composite material, the topic has not been extended to a hybrid composite material such as Glare, a member of the family of Fibre Metal Laminates (FMLs). In this paper/research, the manufacturing, the detection, and the optical evaluation of intraply gaps and overlaps in Glare laminates are investigated. As part of an initial assessment study on the effect of gaps and overlaps on Glare, only the most critical lay-up has been considered. The experimental investigation started with the manufacturing of specimens having gaps and overlaps with different widths, followed by a non-destructive ultrasonic-inspection. An optical evaluation of the gaps and overlaps was performed by means of microscope image analysis of the cross sections of the specimens. The results from the non-destructive evaluations show the effectiveness of the ultrasonic detection of gaps and overlaps both in position, shape, width, and severity. The optical inspections confirm the accuracy of the non-destructive evaluation also adding useful insights about the geometrical features due to the presence of gaps and overlaps in the final Glare laminates. All the results justify the need for a further investigation on the effect of gaps and overlaps on the mechanical properties.

  18. Secondary overprinting of S-Se-Te signatures in the Earth's mantle: Implications for the Late Veneer

    Science.gov (United States)

    Koenig, S.; Luguet, A.; Lorand, J.; Pearson, D.

    2013-12-01

    Sulphur, Selenium and Tellurium are both chalcophile and highly siderophile elements (HSE) with near-chondritic ratios and absolute abundances in the terrestrial mantle that exceed those predicted by core-mantle differentiation[1]. These 'excess' HSE abundances have been attributed to addition of ca. 0.5% of chondrite-like material that hit the Earth in its accretionary stage between 4 to 3.8 billion years ago after core-mantle differentiation (Late Veneer[2]). Therefore, like other HSE, S, Se and Te are considered potential tracers for the composition of the Late Veneer, provided that their bulk silicate Earth abundances are properly constrained. In contrast to ca. 250 ppm S, Se and Te are ultra-trace elements in the terrestrial mantle. Like all HSE, they are furthermore controlled by base metal sulphides (BMS) and micrometric platinum group minerals (PGMs)[3]. This strong control exerted by the host mineralogy and petrology on the S-Se-Te systematics at both the micro-scale and the whole-rock scale makes detailed mineralogical and petrological studies of BMS and PGM a pre-requisite to fully understand and accurately interpret the whole-rock signatures. Here we combine in-situ sulphide data and detailed mineralogical observations with whole-rock S-Se-Te-HSE signatures of both lherzolites and harburgites from different geodynamic settings. We demonstrate that the near-chondritic Se and Te signature of 'fertile' mantle rocks (Se/Te ≈9×5) is not a primitive signature of the Earth's mantle, but rather reflects strong enrichment in metasomatic HSE host phases, which erased previous pristine signatures. Consequently, current attempts to identify a potential Late Veneer composition are seriously flawed because, neither refertilisation/metasomatism nor true melt depletion (e.g. harzburgitic residues) have been taken into account for the Primitive Upper Mantle composition estimate[4]. Our combined whole rock and in-situ sulphide data indicate a refertilisation trend

  19. Effect of shallow angles on compressive strength of biaxial and triaxial laminates.

    Science.gov (United States)

    Jia, Hongli; Yang, Hyun-Ik

    2016-01-01

    Biaxial (BX) and triaxial (TX) composite laminates with ±45° angled plies have been widely used in wind turbine blades. As the scale of blades increases, BX and TX laminates with shallow-angled plies (i.e. off-axis ply angle shallow-angled BX and TX laminates are critical considering their locations in a wind turbine blade, and therefore in this study, the uniaxial static compression tests were conducted using BX and TX laminates with angled-plies of ±45°, ±35°, and ±25°, for the purpose of evaluation. On the other hand, Mori-Tanaka mean field homogenization method was employed to predict elastic constants of plies in BX and TX laminates involved in tests; linear regression analyses of experimentally measured ply strengths collected from various sources were then performed to estimate strengths of plies in BX and TX laminates; finally, Tsai-Wu, Hashin, and Puck failure criteria were chosen to predict compressive strengths of BX and TX laminates. Comparison between theoretical predictions and test results were carried out to illustrate the effectiveness of each criterion. The compressive strength of BX laminate decreases as ply angle increases, and the trend was successfully predicted by all three failure criteria. For TX laminates, ±35° angled plies rather than ±45° angled plies led to the lowest laminate compressive strength. Hashin and Puck criteria gave good predictions at certain ply angles for TX laminates, but Tsai-Wu criterion was able to capture the unexpected strength variation of TX laminates with ply angle. It was concluded that the transverse tensile stress in 0° plies of TX laminates, which attains its maximum when the off-axis ply angle is 35°, is the dominant factor in failure determination if using Tsai-Wu criterion. This explains the unexpected strength variation of TX laminates with ply angle, and also indicates that proper selection of ply angle is the key to fully utilizing the advantages of shallow-angled laminates.

  20. Minimally invasive restoration of a maxillary central incisor with a partial veneer.

    Science.gov (United States)

    Horvath, Sebastian; Schulz, Claus-Peter

    2012-01-01

    Minimally invasive treatment modalities allow for the preservation of sound tooth substance. However, by limiting the preparation to the extent of a defect, the transition between restoration and natural tooth may be moved to more visible areas. The materials available for the restoration of a limited defect in the anterior area are either resin composite materials or porcelain. A patient was presented who asked for the replacement of a discolored filling on the maxillary right central incisor. Tooth preparation was limited to the extent of the old filling, and a porcelain partial veneer restoration was fabricated. Despite the horizontal finish line in the middle of the clinical crown, a result could be achieved that was regarded as a success by the patient. This type of restoration proves to be a suitable alternative to direct composite restorations in the anterior area for the reconstruction of a limited defect, eg, due to a dental trauma.

  1. [The effect of core veneer thickness ratio on the flexural strength of diatomite-based dental ceramic].

    Science.gov (United States)

    Jiang, Jie; Zhang, Xin; Gao, Mei-qin; Zhang, Fei-min; Lu, Xiao-li

    2015-06-01

    To evaluate the effect of different core veneer thickness ratios on the flexural strength and failure mode of bilayered diatomite-based dental ceramics. Diatomite-based dental ceramics blocks (16 mm×5.4 mm×1 mm) were sintered with different thickness of veneer porcelains: 0 mm (group A), 0.6 mm (group B), 0.8 mm (group C) and 1.0 mm (group D). Flexural strength was detected and scanning electron microscope was used to observe the interface microstructure. Statistical analysis was performed using SPSS 17.0 software package. With the increase of the thickness of the veneer porcelain, flexural strength of group C showed highest flexural strength up to (277.24±5.47) MPa. Different core veneer thickness ratios can significantly influence the flexural strength of bilayered diatomite-based dental ceramics. Supported by Science and Technology Projects of Nantong City (HS2013010).

  2. Composite materials for cryogenic structures

    International Nuclear Information System (INIS)

    Kasen, M.B.

    1978-01-01

    The paper is concerned with the composition, mechanical properties and capabilities of various types of composite materials for cryogenic structures. Attention is given to high-pressure plastic laminates, low-pressure plastic laminates, metal-matrix laminates, and aggregates (low-temperature concretes). The ability of these materials to match the strength and modulus of stainless steels suggests that their usage will substantially increase as alloying elements become scarce and more expensive

  3. Reliability and failure modes of implant-supported zirconium-oxide fixed dental prostheses related to veneering techniques

    Science.gov (United States)

    Baldassarri, Marta; Zhang, Yu; Thompson, Van P.; Rekow, Elizabeth D.; Stappert, Christian F. J.

    2011-01-01

    Summary Objectives To compare fatigue failure modes and reliability of hand-veneered and over-pressed implant-supported three-unit zirconium-oxide fixed-dental-prostheses(FDPs). Methods Sixty-four custom-made zirconium-oxide abutments (n=32/group) and thirty-two zirconium-oxide FDP-frameworks were CAD/CAM manufactured. Frameworks were veneered with hand-built up or over-pressed porcelain (n=16/group). Step-stress-accelerated-life-testing (SSALT) was performed in water applying a distributed contact load at the buccal cusp-pontic-area. Post failure examinations were carried out using optical (polarized-reflected-light) and scanning electron microscopy (SEM) to visualize crack propagation and failure modes. Reliability was compared using cumulative-damage step-stress analysis (Alta-7-Pro, Reliasoft). Results Crack propagation was observed in the veneering porcelain during fatigue. The majority of zirconium-oxide FDPs demonstrated porcelain chipping as the dominant failure mode. Nevertheless, fracture of the zirconium-oxide frameworks was also observed. Over-pressed FDPs failed earlier at a mean failure load of 696 ± 149 N relative to hand-veneered at 882 ± 61 N (profile I). Weibull-stress-number of cycles-unreliability-curves were generated. The reliability (2-sided at 90% confidence bounds) for a 400N load at 100K cycles indicated values of 0.84 (0.98-0.24) for the hand-veneered FDPs and 0.50 (0.82-0.09) for their over-pressed counterparts. Conclusions Both zirconium-oxide FDP systems were resistant under accelerated-life-time-testing. Over-pressed specimens were more susceptible to fatigue loading with earlier veneer chipping. PMID:21557985

  4. Composite materials design and applications

    CERN Document Server

    Gay, Daniel; Tsai, Stephen W

    2002-01-01

    PART ONE. PRINCIPLES OF CONSTRUCTIONCOMPOSITE MATERIALS, INTEREST AND PROPERTIESWhat is Composite Material Fibers and MatrixWhat can be Made Using Composite Materials?Typical Examples of Interest on the Use of Composite MaterialsExamples on Replacing Conventional Solutions with CompositesPrincipal Physical PropertiesFABRICATION PROCESSESMolding ProcessesOther Forming ProcessesPractical Hints in the Manufacturing ProcessesPLY PROPERTIESIsotropy and AnisotropyCharacteristics of the Reinforcement-Matrix MixtureUnidirectional PlyWoven FabricsMats and Reinforced MatricesMultidimensional FabricsMetal Matrix CompositesTestsSANDWICH STRUCTURES:What is a Sandwich Structure?Simplified FlexureA Few Special AspectsFabrication and Design ProblemsNondestructive Quality ControlCONCEPTION AND DESIGNDesign of a Composite PieceThe LaminateFailure of LaminatesSizing of LaminatesJOINING AND ASSEMBLYRiveting and BoltingBondingInsertsCOMPOSITE MATERIALS AND AEROSPACE CONSTRUCTIONAircraftHelicoptersPropeller Blades for AirplanesTur...

  5. Additively Manufactured Titanium and Cobalt-Chromium Implant Frameworks: Fit and Effect of Ceramic Veneering.

    Science.gov (United States)

    Svanborg, Per; Eliasson, Alf; Stenport, Victoria

    The purpose of this study was to evaluate the fit of additively manufactured cobalt-chromium and titanium and CNC-milled titanium frameworks before and after ceramic veneering. Ten stone casts simulating an edentulous maxilla provided with six abutment analogs were produced. For each stone cast, one additively manufactured cobalt-chromium framework (AM CoCr) and one titanium framework (AM Ti) were fabricated. The fit was analyzed with a coordinate measuring machine in three dimensions (x, y, and z axes) using best-fit virtual matching of center point coordinates, before and after ceramic veneering. CNC-milled titanium frameworks (CNC Ti) and earlier results from CNC-milled cobalt-chromium frameworks (CNC CoCr) were used for comparison. All frameworks presented minor misfit before and after veneering in the horizontal plane (x- and y-axes) between 2.9 and 13.5 μm and in the vertical plane (z-axis) between 1.6 and 5.4 μm. Ceramic veneering affected the fit of all groups of frameworks. Both AM Ti and AM CoCr presented significantly smaller distortion in the vertical plane compared with the CNC-milled frameworks. Implant-supported frameworks can be produced in either Ti or CoCr using either CNC milling or additive manufacturing with a fit well within the range of 20 μm in the horizontal plane and 10 μm in the vertical plane. The fit of frameworks of both materials and production techniques are affected by the ceramic veneering procedure to a small extent.

  6. Effects of stacking sequence on fracture mechanisms in quasi-isotropic Carbon/epoxy laminates under tensile loading

    International Nuclear Information System (INIS)

    Hessabi, Z. R.; Majidi, B.; Aghazadeh, J.

    2006-01-01

    The progress of damage in quasi-isotropic carbon/epoxy laminates under tensile loading has been Investigated microscopically. One significant mode of failure in laminated composites is delamination initiating at free edges. The interlaminar stress in the boundary ply along the free edges of a laminated composite is the main factor to cause delamination. The laminate stacking sequence affects the interlaminar stress distribution and consequently may change the mode of failure. It is of design importance to determine a suitable criterion based on stress analysis to obtain the best stacking sequence. In the present work, tensile properties of six samples with different stacking sequences have been examined. Results showed that stress analysis at distance very close to the free edges is a suitable criterion to predict the initiation of delamination and the stacking sequence of [90/45/0/-45] s , has the highest strength among the others. Furthermore finite element analysis showed that the adjacent ±45 plies cause premature delamination during tensile loading

  7. Visco-piezo-elastic parameter estimation in laminated plate structures

    DEFF Research Database (Denmark)

    Araujo, A. L.; Mota Soares, C. M.; Herskovits, J.

    2009-01-01

    A parameter estimation technique is presented in this article, for identification of elastic, piezoelectric and viscoelastic properties of active laminated composite plates with surface-bonded piezoelectric patches. The inverse method presented uses experimental data in the form of a set of measu...

  8. A novel damage index for damage identification using guided waves with application in laminated composites

    International Nuclear Information System (INIS)

    Torkamani, Shahab; Roy, Samit; Barkey, Mark E; Sazonov, Edward; Burkett, Susan; Kotru, Sushma

    2014-01-01

    In the current investigation, an innovative time-domain damage index is introduced for the first time which is based on local statistical features of the waveform. This damage index is called the ‘normalized correlation moment’ (NCM) and is composed of the nth moment of the cross-correlation of the baseline and comparison waves. The performance of this novel damage index is compared for some synthetic signals with that of an existing damage index based on the Pearson correlation coefficient (signal difference coefficient, SDC). The proposed damage index is shown to have significant advantages over the SDC, including sensitivity to the attenuation of the signal and lower sensitivity to the signal’s noise level. Numerical simulations using Abaqus finite element (FE) software show that this novel damage index is not only capable of detecting the delamination type of damage, but also exhibits a good ability in the assessment of this type of damage in laminated composite structures. The NCM damage index is also validated using experimental data for identification of delamination in composites. (paper)

  9. Relation between interlaminar fracture toughness and pressure condition in autoclave molding process of GFRP composite laminates; GFRP sekisoban no autoclave seikei ni okeru atsuryoku joken to sokan hakai jinseichi tono kankei

    Energy Technology Data Exchange (ETDEWEB)

    Jiang, J. [Osaka City University, Osaka (Japan); Motogi, S.; Fukuda, T. [Osaka City University, Osaka (Japan). Faculty of Engineering

    1998-06-15

    Relation between fracture toughness and pressure condition in autoclave molding of GF composite laminates is investigated. Glass/epoxy prepregs are molded under different curing pressures, and UD laminates of [O{sub 8}]T and [O{sub 16}]T are fabricated. The results of the double cantilever beam (DCB) test show that the curing pressure has certain influences on the interlaminar fracture toughness via the change in morphology of matrix resin and fibers between laminae, and via the change in interfacial strength of fiber and matrix. It is also found that the fiber/matrix interfacial strength increases as the curing pressure increases by SEM photographs of the fracture surface in GF UD laminates. 13 refs., 12 figs.

  10. Lamination cooling system formation method

    Science.gov (United States)

    Rippel, Wally E [Altadena, CA; Kobayashi, Daryl M [Monrovia, CA

    2009-05-12

    An electric motor, transformer or inductor having a cooling system. A stack of laminations have apertures at least partially coincident with apertures of adjacent laminations. The apertures define straight or angled cooling-fluid passageways through the lamination stack. Gaps between the adjacent laminations are sealed by injecting a heat-cured sealant into the passageways, expelling excess sealant, and heat-curing the lamination stack. Manifold members adjoin opposite ends of the lamination stack, and each is configured with one or more cavities to act as a manifold to adjacent passageway ends. Complex manifold arrangements can create bidirectional flow in a variety of patterns.

  11. Investigation on the Tribological Behavior and Wear Mechanism of Five Different Veneering Porcelains.

    Directory of Open Access Journals (Sweden)

    Jie Min

    Full Text Available The primary aim of this research was to investigate the wear behavior and wear mechanism of five different veneering porcelains.Five kinds of veneering porcelains were selected in this research. The surface microhardness of all the samples was measured with a microhardness tester. Wear tests were performed on a ball-on-flat PLINT fretting wear machine, with lubrication of artificial saliva at 37°C. The friction coefficients were recorded by the testing system. The microstructure features, wear volume, and damage morphologies were recorded and analyzed with a confocal laser scanning microscope and a scanning electron microscope. The wear mechanism was then elucidated.The friction coefficients of the five veneering porcelains differ significantly. No significant correlation between hardness and wear volume was found for these veneering porcelains. Under lubrication of artificial saliva, the porcelain with higher leucite crystal content exhibited greater wear resistance. Additionally, leucite crystal size and distribution in glass matrix influenced wear behavior. The wear mechanisms for these porcelains were similar: abrasive wear dominates the early stage, whereas delamination was the main damage mode at the later stage. Furthermore, delamination was more prominent for porcelains with larger crystal sizes.Wear compatibility between porcelain and natural teeth is important for dental restorative materials. Investigation on crystal content, size, and distribution in glass matrix can provide insight for the selection of dental porcelains in clinical settings.

  12. Probabilistic Simulation of Multi-Scale Composite Behavior

    Science.gov (United States)

    Chamis, Christos C.

    2012-01-01

    A methodology is developed to computationally assess the non-deterministic composite response at all composite scales (from micro to structural) due to the uncertainties in the constituent (fiber and matrix) properties, in the fabrication process and in structural variables (primitive variables). The methodology is computationally efficient for simulating the probability distributions of composite behavior, such as material properties, laminate and structural responses. Bi-products of the methodology are probabilistic sensitivities of the composite primitive variables. The methodology has been implemented into the computer codes PICAN (Probabilistic Integrated Composite ANalyzer) and IPACS (Integrated Probabilistic Assessment of Composite Structures). The accuracy and efficiency of this methodology are demonstrated by simulating the uncertainties in composite typical laminates and comparing the results with the Monte Carlo simulation method. Available experimental data of composite laminate behavior at all scales fall within the scatters predicted by PICAN. Multi-scaling is extended to simulate probabilistic thermo-mechanical fatigue and to simulate the probabilistic design of a composite redome in order to illustrate its versatility. Results show that probabilistic fatigue can be simulated for different temperature amplitudes and for different cyclic stress magnitudes. Results also show that laminate configurations can be selected to increase the redome reliability by several orders of magnitude without increasing the laminate thickness--a unique feature of structural composites. The old reference denotes that nothing fundamental has been done since that time.

  13. TREATMENT APPROACHES FOR TRAUMATIZED ANTERIOR TEETH WITH EXCESSIVE TISSUE LOSS: THREE CASE REPORTS

    Directory of Open Access Journals (Sweden)

    Zuhal YILDIRIM

    2017-04-01

    Full Text Available Use of direct composite and indirect laminate veneers has been an alternative to metal- and all-ceramic crowns for anterior teeth restorations. Dental traumas are the most common reasons for excessive tissue loss. Treatment options depend on the amount of remaining tissue, the extent of the damage to dental pulp and periapical tissues and the time elapsed before dental treatment. The aim of this case report was to evaluate the direct and indirect techniques used in the treatments of traumatically fractured anterior teeth. In Case 1, a 29-year-old male patient attended to the clinics of the Department of Restorative Dentistry, Faculty of Dentistry, Istanbul University for the replacement of old composite restorations. According to anamnesis, the anterior teeth had fractured because of falling from bicycle. Dentinal pins used to retain the composite restorations were screwed out and indirect composite laminate veneers were placed. In Case 2, a 27-year-old male patient attended to our clinic for the treatment of his anterior teeth which were fractured due to a fall. A different type of technique, a silicon guide, was used to mimic the natural teeth surfaces precisely. In Case 3, a 16-year-old female patient attended to our clinic for the treatment of her anterior teeth which were fractured in a car accident. On clinical evaluation, related teeth were found to be non-vital and application of fiber posts was considered suitable before direct composite restorations. In conclusion, all of these techniques may be used for traumatized anterior teeth. Esthetical necessities and functional forces should be taken into consideration in material choice.

  14. Improved compression molding technology for continuous fiber reinforced composite laminates. Part 2: AS-4/Polyimidesulfone prepreg system

    Science.gov (United States)

    Baucom, Robert M.; Hou, Tan-Hung; Kidder, Paul W.; Reddy, Rakasi M.

    1991-01-01

    AS-4/polyimidesulfone (PISO2) composite prepreg was utilized for the improved compression molding technology investigation. This improved technique employed molding stops which advantageously facilitate the escape of volatile by-products during the B-stage curing step, and effectively minimize the neutralization of the consolidating pressure by intimate interply fiber-fiber contact within the laminate in the subsequent molding cycle. Without the modifying the resin matrix properties, composite panels with both unidirectional and angled plies with outstanding C-scans and mechanical properties were successfully molded using moderate molding conditions, i.e., 660 F and 500 psi, using this technique. The size of the panels molded were up to 6.00 x 6.00 x 0.07 in. A consolidation theory was proposed for the understanding and advancement of the processing science. Processing parameters such as vacuum, pressure cycle design, prepreg quality, etc. were explored.

  15. Vibration and Energy Dissipation of Nanocomposite Laminates for Below Ballistic Impact Loading

    Directory of Open Access Journals (Sweden)

    G. Balaganesan

    Full Text Available Abstract Composite laminates are made of glass woven roving mats of 610gsm, epoxy resin and nano clay which are subjected to projectile impact. Nano clay dispersion is varied from 1% to 5%. Impact tests are conducted in a gas gun setup with a spherical nose cylindrical projectile of diameter 9.5 mm of mass 7.6 g. The energy absorbed by the laminates when subjected to impact loading is studied, the velocity range is below ballistic limit. The effect of nano clay on energy absorption in vibration, delamination and matrix crack is studied for different weight % of nano clay and for different thickness values of the laminates. The natural frequencies and damping factors are obtained for the laminates during impact and the effect of nano clay is studied. The results show considerable improvement in energy absorption due to the presence of nano clay

  16. EVALUATION OF STRENGTH TO SHEAR AND DELAMINATION IN GLUED LAMINATED WOOD

    Directory of Open Access Journals (Sweden)

    Carlito Calil Neto

    2014-12-01

    Full Text Available The Glued Laminated Wood has a large range of applications. In Brazil, its employment as cross-piece poles for overhead electrical power has attracted the attention of companies in the industry, motivated by the potential use of this material. Among the factors that influence the mechanical performance of Glulam solutions stand out efficiency and affinity of the adhesives to the species of wood used, the type of treatment and moisture content of wood veneer, motivating the development of new research on this topic. This research aimed to investigate, by Design of Experiments (DOE, the influence of wood (pinus, teca, eucalipto, adhesive (Purbond; Cascophen and treatment (CCA, CCB, CCBS in the variable responses shear strength and delamination, consisting in the same combination factors evaluated in ANEEL/EESC-PD220-07 project: Head Crosshead Glulam Series. The results of the statistical analysis showed that the species factor expressed significant effect for both response variables evaluated, did not occur with adhesive and treatment factors. Moisture content was significant in the wood evaluated when analyzed the shear strength, and the teca wood showed the highest shear strength and also relating to the delamination.

  17. Lamins of the sea lamprey (Petromyzon marinus) and the evolution of the vertebrate lamin protein family.

    Science.gov (United States)

    Schilf, Paul; Peter, Annette; Hurek, Thomas; Stick, Reimer

    2014-07-01

    Lamin proteins are found in all metazoans. Most non-vertebrate genomes including those of the closest relatives of vertebrates, the cephalochordates and tunicates, encode only a single lamin. In teleosts and tetrapods the number of lamin genes has quadrupled. They can be divided into four sub-types, lmnb1, lmnb2, LIII, and lmna, each characterized by particular features and functional differentiations. Little is known when during vertebrate evolution these features have emerged. Lampreys belong to the Agnatha, the sister group of the Gnathostomata. They split off first within the vertebrate lineage. Analysis of the sea lamprey (Petromyzon marinus) lamin complement presented here, identified three functional lamin genes, one encoding a lamin LIII, indicating that the characteristic gene structure of this subtype had been established prior to the agnathan/gnathostome split. Two other genes encode lamins for which orthology to gnathostome lamins cannot be designated. Search for lamin gene sequences in all vertebrate taxa for which sufficient sequence data are available reveals the evolutionary time frame in which specific features of the vertebrate lamins were established. Structural features characteristic for A-type lamins are not found in the lamprey genome. In contrast, lmna genes are present in all gnathostome lineages suggesting that this gene evolved with the emergence of the gnathostomes. The analysis of lamin gene neighborhoods reveals noticeable similarities between the different vertebrate lamin genes supporting the hypothesis that they emerged due to two rounds of whole genome duplication and makes clear that an orthologous relationship between a particular vertebrate paralog and lamins outside the vertebrate lineage cannot be established. Copyright © 2014 Elsevier GmbH. All rights reserved.

  18. Multi-material topology design of laminates with strength criteria

    DEFF Research Database (Denmark)

    Lund, Erik

    2012-01-01

    The objective of this paper is to present a novel approach for multi-material topology optimization of laminated composite structures where strength constraints are taken into account together with other global structural performance measures. The topology design problem considered contains very...... many design variables, and when strength criteria are included in the problem, a very large number of criteria functions must be considered in the optimization problem to be solved. Thus, block aggregation methods are introduced, such that global strength measures are obtained. These formulations...... are illustrated for multi-material laminated design problems where the maximum failure index is minimized while compliance and mass constraints are taken into account....

  19. The effect of different surface treatments of stainless steel crown and different bonding agents on shear bond strength of direct composite resin veneer

    Directory of Open Access Journals (Sweden)

    Ajami B

    2007-01-01

    Full Text Available Background and Aim: Stainless steel crown (SSC is the most durable and reliable restoration for primary teeth with extensive caries but its metalic appearance has always been a matter of concern. With advances in restorative materials and metal bonding processes, composite veneer has enhanced esthetics of these crowns in clinic. The aim of this study was to evaluate the shear bond strength of SSC to composite resin using different surface treatments and adhesives. Materials and Methods: In this experimental study, 90 stainless steel crowns were selected. They were mounted in molds and divided into 3 groups of 30 each (S, E and F. In group S (sandblast, buccal surfaces were sandblasted for 5 seconds. In group E (etch acidic gel was applied for 5 minutes and in group F (fissure bur surface roughness was created by fissure diamond bur. Each group was divided into 3 subgroups (SB, AB, P based on different adhesives: Single Bond, All Bond2 and Panavia F. Composite was then bonded to specimens. Cases were incubated in 100% humidity at 37°C for 24 hours. Shear bond strength was measured by Zwick machine with crosshead speed of 0.5 mm/min. Data were analyzed by ANOVA test with p0.05 so the two variables were studied separately. No significant difference was observed in mean shear bond strength of composite among the three kinds of adhesives (P>0.05. Similar results were obtained regarding surface treatments (P>0.05. Conclusion: Based on the results of this study, treating the SSC surface with bur and using single bond adhesive and composite can be used successfully to obtain esthetic results in pediatric restorative treatments.

  20. Influence of bress laminate volume fraction on electromechanical properties of externally laminated coated conductor tapes

    Energy Technology Data Exchange (ETDEWEB)

    Bautista, Zhierwinjay M.; Shin, Hyung Seop [Dept. of Mechanical Design Engineering, Andong National University, Andong (Korea, Republic of); Lee, Jae Hun; Lee, Hun Ju; Moon, Seung Hyun [SuNAM Co Ltd., Anseong (Korea, Republic of)

    2016-09-15

    The enhancement of mechanical properties of coated conductor (CC) tapes in practical application are usually achieved by reinforcing through lamination or electroplating metal layers on either sides of the CC tape. Mechanical or electromechanical properties of the CC tapes have been largely affected by the lamination structure under various loading modes such as tension, bending or even cyclic. In this study, the influence of brass laminate volume fraction on electromechanical properties of RCE-DR processed Gadolinium-barium-copper-oxide (GdBCO) CC tapes was investigated. The samples used were composed of single-side and both-side laminate of brass layer to the Cu-stabilized CC tape and their Ic behaviors were compared to those of the Cu-stabilized CC tape without external lamination. The stress/strain dependences of Ic in laminated CC tapes under uniaxial tension were analyzed and the irreversible stress/strain limits were determined. As a result, the increase of brass laminate volume fraction initially increased the irreversible strain limit and became gradual. The corresponding irreversible stress limit, however, showed no difference even though the brass laminate volume fraction increased to 3.4. But the irreversible load limit linearly increased with the brass laminate volume fraction.

  1. An analytical study of composite laminate lay-up using search algorithms for maximization of flexural stiffness and minimization of springback angle

    Science.gov (United States)

    Singh, Ranjan Kumar; Rinawa, Moti Lal

    2018-04-01

    The residual stresses arising in fiber-reinforced laminates during their curing in closed molds lead to changes in the composites after their removal from the molds and cooling. One of these dimensional changes of angle sections is called springback. The parameters such as lay-up, stacking sequence, material system, cure temperature, thickness etc play important role in it. In present work, it is attempted to optimize lay-up and stacking sequence for maximization of flexural stiffness and minimization of springback angle. The search algorithms are employed to obtain best sequence through repair strategy such as swap. A new search algorithm, termed as lay-up search algorithm (LSA) is also proposed, which is an extension of permutation search algorithm (PSA). The efficacy of PSA and LSA is tested on the laminates with a range of lay-ups. A computer code is developed on MATLAB implementing the above schemes. Also, the strategies for multi objective optimization using search algorithms are suggested and tested.

  2. Hygrothermal Effect on Mechanical and Fatigue Properties of laminated Lower Limb Socket and Bacteria Growth

    Directory of Open Access Journals (Sweden)

    Fadhel Abbas Abdullah

    2016-12-01

    Full Text Available In this work, hygrothermal effect on the mechanical and fatigue properties of prosthetic socket lamination and its effect on the bacteria growth were studied. Two laminations composite materials were used in manufacturing prosthetic socket by using vacuum device. The reinforced materials of these laminations were perlon and carbon nanopowder (CNP while the matrix material was polyurethane resin. Tests performed in this work were the moisture absorption properties test to calculate percent moisture content according to ASTM 5229, tensile and fatigue tests with and without the hygrothermal effect to find the mechanical and fatigue properties, and the bacteria growth test under the hygrothermal effect to calculate the number of bacteria on the laminations. The results showed that the lamination (10 perlon+1 wt % CNP has mechanical properties than lamination (10 perlon with and without hygrothermal effect. The mechanical and fatigue properties for the two laminations were decreasing with increasing temperature and moisture.. Adding carbon nanopowder to the lamination (10 perlon increased ultimate stress, modulus of elastic, and endurance limit by (1.36, 2.35, and2.72 time respectively. Finally, the results showed that the Staphylococcus aureus growth increases with increasing temperature and moisture on the two laminations used in manufacturing prosthetic socket, and adding carbon nanopowder also increased the Staphylococcus aureus growth on the lamination.

  3. Hygrothermal effects on the mechanical behaviour of graphite fibre-reinforced epoxy laminates beyond initial failure

    Science.gov (United States)

    Ishai, O.; Garg, A.; Nelson, H. G.

    1986-01-01

    The critical load levels and associated cracking beyond which a multidirectional laminate can be considered as structurally failed has been determined by loading graphite fiber-reinforced epoxy laminates to different strain levels up to ultimate failure. Transverse matrix cracking was monitored by acoustic and optical methods. The residual stiffness and strength parallel and perpendicular to the cracks were determined and related to the environmental/loading history. Within the range of experimental conditions studied, it is concluded that the transverse cracking process does not have a crucial effect on the structural performance of multidirectional composite laminates.

  4. Electrical impedance spectroscopy for measuring the impedance response of carbon-fiber-reinforced polymer composite laminates

    KAUST Repository

    Almuhammadi, Khaled

    2017-02-16

    Techniques that monitor the change in the electrical properties of materials are promising for both non-destructive testing and structural health monitoring of carbon-fiber-reinforced polymers (CFRPs). However, achieving reliable monitoring using these techniques requires an in-depth understanding of the impedance response of these materials when subjected to an alternating electrical excitation, information that is only partially available in the literature. In this work, we investigate the electrical impedance spectroscopy response at various frequencies of laminates chosen to be representative of classical layups employed in composite structures. We clarify the relationship between the frequency of the electrical current, the conductivity of the surface ply and the probing depth for different CFRP configurations for more efficient electrical signal-based inspections. We also investigate the effect of the amplitude of the input signal.

  5. Development and Application of Optimization Techniques for Composite Laminates.

    Science.gov (United States)

    1983-09-01

    Institute of Technolgy Air University in Partial Fulfillment of the Requirements for the Degree of Master of Science by Gerald V. Flanagan, S.B. Lt. USAF...global minima [9]. An informal definition of convexity is that any two points in the space can be connected by a straight line which does not pass out of...question. A quick look at gradient information suggests that too few angles (2 for example) will make the laminate sensitive to small changes in

  6. Cone calorimeter testing of foam core sandwich panels treated with intumescent paper underneath the veneer (FRV)

    Science.gov (United States)

    Mark A. Dietenberger; Ali Shalbafan; Johannes Welling

    2017-01-01

    Surfaces of novel foam core sandwich panels were adhered with intumescent fire‐retardant paper underneath the veneers (FRV) to improve their flammability properties. The panels were evaluated by means of cone calorimeter test (ASTM E 1354). Variables tested were different surface layer treatments, adhesives used for veneering, surface layer thicknesses, and processing...

  7. Validation of Micro-Meso Electrical Relations for Laminates with Varying Anisotropy

    KAUST Repository

    Selvakumaran, Lakshmi

    2015-08-01

    For electrical impedance tomography (EIT) to be useful in monitoring transverse cracks in composites, it is imperative to establish the relation between conductivity and cracking density. Micro to meso scale homogenization has been developed for classical carbon fiber reinforced polymer (CFRP) laminate which provides such a relationship. However, we have shown in previous studies that the detectability of transverse cracks in such CFRP, which are characterized by very anisotropic electrical properties, is poor. Then, it is better to lower the electrical anisotropy, which can be achieved by various technologies including doping the polymeric resin by conductive nanoparticles. However, the validity of mesoscale homogenization for laminates with such low anisotropy has not been tested before. Here, we show that the mesoscale damage indicator is intrinsic for composites with varying anisotropy.

  8. Evaluation of the color durability of acrylic resin veneer materials after immersion in common beverages at different time intervals: A spectrophotometric study.

    Science.gov (United States)

    Kohli, Shivani; Bhatia, Shekhar

    2015-01-01

    Proper function, esthetics, and cost are the prime factors to be considered while selecting bridge veneering materials. The purpose of the study is to evaluate color durability of acrylic veneer materials after immersion in common beverages at different time intervals. Spectrophotometer was used for taking color measurements based on the transmission of light through the specimens made of the selected materials which were Tooth moulding powder (DPI) and Acrylux (Ruthinium). Thirty specimens of standardized dimensions were prepared from each material. The specimens were divided into three groups of 10 each. One group of each material was immersed in tea (TajMahal) and another group of each material in cola (Pepsi) as the staining solutions. The remaining group of 10 from each material served as control and was stored in distilled water. Color measurements were obtained pre-immersion, and after 1, 15, and 30 days of immersion. Tooth moulding powder displayed better color durability than Acrylux over the 1 month immersion period in both staining solutions. Tea resulted in more discoloration compared to cola (Pepsi). The difference in the color durability of Acrylux and Tooth moulding powder may be attributed to the differences in the composition of tested resin veneering materials, i.e. their polar properties, which contribute to the absorption of staining solution, and the different brands and the strengths of the solutions.

  9. Evaluation of the color durability of acrylic resin veneer materials after immersion in common beverages at different time intervals: A spectrophotometric study

    Directory of Open Access Journals (Sweden)

    Shivani Kohli

    2015-06-01

    Full Text Available Background: Proper function, esthetics, and cost are the prime factors to be considered while selecting bridge veneering materials. The purpose of the study is to evaluate color durability of acrylic veneer materials after immersion in common beverages at different time intervals. Methods: Spectrophotometer was used for taking color measurements based on the transmission of light through the specimens made of the selected materials which were Tooth moulding powder (DPI and Acrylux (Ruthinium. Thirty specimens of standardized dimensions were prepared from each material. The specimens were divided into three groups of 10 each. One group of each material was immersed in tea (TajMahal and another group of each material in cola (Pepsi as the staining solutions. The remaining group of 10 from each material served as control and was stored in distilled water. Color measurements were obtained pre-immersion, and after 1, 15, and 30 days of immersion. Results: Tooth moulding powder displayed better color durability than Acrylux over the 1 month immersion period in both staining solutions. Tea resulted in more discoloration compared to cola (Pepsi. Conclusion: The difference in the color durability of Acrylux and Tooth moulding powder may be attributed to the differences in the composition of tested resin veneering materials, i.e. their polar properties, which contribute to the absorption of staining solution, and the different brands and the strengths of the solutions.

  10. Evaluation of veneer yields and grades from yellow-poplar, white oak, and sweetgum from the southeast

    Science.gov (United States)

    Robert H. McAlister

    1980-01-01

    Dry volume yields and standard grades of veneer are given for yellow-poplar, sweetgum, and white oak by tree diameter and location within the stem. Results show that the typical stands of mixed southern pine and hardwood timer yield enough veneer to utilize almost 90 percent of the stand volume in the production of COM-PLY lumber and panels

  11. The influence of felling season and log-soaking temperature on the wetting and phenol formaldehyde adhesive bonding characteristics of birch veneer

    Science.gov (United States)

    Anti Rohumaa; Christopher G. Hunt; Charles R. Frihart; Pekka Saranpää; Martin Ohlmeyer; Mark Hughes

    2014-01-01

    Most adhesive studies employing wood veneer as the substrate assume that it is a relatively uniform material if wood species and veneer thickness are constant. In the present study, veneers from rotary cut birch (Betula pendula Roth) were produced from logs harvested in spring, autumn and winter, and soaked at 20°C and 70°C prior to peeling. Firstly...

  12. Micromechanisms in tension-compression fatigue of composite laminates containing transverse plies

    DEFF Research Database (Denmark)

    Gamstedt, E.K.; Sjögren, B.A.

    1999-01-01

    to optimise fatigue resistance. In this study, glass-fibre-reinforced vinyl-ester was used. The adverse effect of compressive load excursions was verified by counting the transverse cracks in cross-ply laminates. The mechanisms were studied in low-cycle fatigue of a specimen containing a single transverse...

  13. The effect of core material, veneering porcelain, and fabrication technique on the biaxial flexural strength and weibull analysis of selected dental ceramics.

    Science.gov (United States)

    Lin, Wei-Shao; Ercoli, Carlo; Feng, Changyong; Morton, Dean

    2012-07-01

    The objective of this study was to compare the effect of veneering porcelain (monolithic or bilayer specimens) and core fabrication technique (heat-pressed or CAD/CAM) on the biaxial flexural strength and Weibull modulus of leucite-reinforced and lithium-disilicate glass ceramics. In addition, the effect of veneering technique (heat-pressed or powder/liquid layering) for zirconia ceramics on the biaxial flexural strength and Weibull modulus was studied. Five ceramic core materials (IPS Empress Esthetic, IPS Empress CAD, IPS e.max Press, IPS e.max CAD, IPS e.max ZirCAD) and three corresponding veneering porcelains (IPS Empress Esthetic Veneer, IPS e.max Ceram, IPS e.max ZirPress) were selected for this study. Each core material group contained three subgroups based on the core material thickness and the presence of corresponding veneering porcelain as follows: 1.5 mm core material only (subgroup 1.5C), 0.8 mm core material only (subgroup 0.8C), and 1.5 mm core/veneer group: 0.8 mm core with 0.7 mm corresponding veneering porcelain with a powder/liquid layering technique (subgroup 0.8C-0.7VL). The ZirCAD group had one additional 1.5 mm core/veneer subgroup with 0.7 mm heat-pressed veneering porcelain (subgroup 0.8C-0.7VP). The biaxial flexural strengths were compared for each subgroup (n = 10) according to ISO standard 6872:2008 with ANOVA and Tukey's post hoc multiple comparison test (p≤ 0.05). The reliability of strength was analyzed with the Weibull distribution. For all core materials, the 1.5 mm core/veneer subgroups (0.8C-0.7VL, 0.8C-0.7VP) had significantly lower mean biaxial flexural strengths (p Empress and e.max groups, regardless of core thickness and fabrication techniques. Comparing fabrication techniques, Empress Esthetic/CAD, e.max Press/CAD had similar biaxial flexural strength (p= 0.28 for Empress pair; p= 0.87 for e.max pair); however, e.max CAD/Press groups had significantly higher flexural strength (p Empress Esthetic/CAD groups. Monolithic core

  14. Achieving ICME with Multiscale Modeling: The Effects of Constituent Properties and Processing on the Performance of Laminated Polymer Matrix Composite Structures

    Science.gov (United States)

    Pineda, Evan Jorge; Bednarcyk, Brett A.; Arnold, Steven M.

    2014-01-01

    Integrated computational materials engineering (ICME) is a useful approach for tailoring the performance of a material. For fiber-reinforced composites, not only do the properties of the constituents of the composite affect the performance, but so does the architecture (or microstructure) of the constituents. The generalized method of cells is demonstrated to be a viable micromechanics tool for determining the effects of the microstructure on the performance of laminates. The micromechanics is used to predict the inputs for a macroscale model for a variety of different fiber volume fractions, and fiber architectures. Using this technique, the material performance can be tailored for specific applications by judicious selection of constituents, volume fraction, and architectural arrangement given a particular manufacturing scenario

  15. Illuminating light-dependent color shifts in core and veneer layers of dental all-ceramics

    Science.gov (United States)

    Lee, Yong-Keun; Cha, Hyun-Suk; Yu, Bin

    2014-09-01

    The color of an object is perceived differently depending on the ambient light conditions. Since dental all-ceramic restorations are fabricated by building up several layers to reproduce the tooth shade, the optical properties of each layer should be optimized for successful shade reproduction. This study aimed to determine the separate contributions of the color shifts in each of the core and veneer layers of all-ceramics by switching the illuminating lights on the color shifts of layered ceramics. Specimens of seven kinds of core ceramics and the corresponding veneer ceramics for each core were fabricated with a layered thickness of 1.5 mm. A sintering ceramic was used as a reference core material. The Commission Internationale de l'Eclairage (CIE) color coordinates of core, veneer, and layered specimens were measured with a spectroradiometer under the CIE illuminant D65 (daylight), A (incandescent lamp), and F9 (fluorescent lamp) simulating lights. Color shifts of the layered specimens were primarily determined by the CIE a* shifts (D65 to A switch) or by the CIE b* shifts (D65 to F9 switch) of the veneer layer. The color coordinates shifts in the constituent layers differentially influenced those of the layered specimens by the kind of switched lights. Therefore, the optical properties of the constituent layers of all-ceramics should be controlled to reflect these findings.

  16. Fatigue and fracture of fibre metal laminates

    CERN Document Server

    Alderliesten, René

    2017-01-01

    This book contributes to the field of hybrid technology, describing the current state of knowledge concerning the hybrid material concept of laminated metallic and composite sheets for primary aeronautical structural applications. It is the only book to date on fatigue and fracture of fibre metal laminates (FMLs). The first section of the book provides a general background of the FML technology, highlighting the major FML types developed and studied over the past decades in conjunction with an overview of industrial developments based on filed patents. In turn, the second section discusses the mechanical response to quasi-static loading, together with the fracture phenomena during quasi-static and cyclic loading. To consider the durability aspects related to strength justification and certification of primary aircraft structures, the third section discusses thermal aspects related to FMLs and their mechanical response to various environmental and acoustic conditions.

  17. Electrospun Fibers for Composites Applications

    Science.gov (United States)

    2014-02-01

    in traditional woven mat composites. Nanofibrous interlayers were used to increase the impact and shear performance of a prepregged carbon fiber...Nylon 66 Nanofibrilmat Interleaved Carbon/Epoxy Laminates . Polymer Composites 2011, 32, 1781–1789. 21 13. Chen, Q.; Zhang, L.; Rahman, A.; Zhou...Resistance in Laminated Composites With Electrospun Nano-Interlayers. Comp. Sci. Tech. 2008, 68, 673– 683. 15. Zhang, J.; Lin, T.; Wang, X. Electrospun

  18. Fracture strengths of chair‑side‑generated veneers cemented with ...

    African Journals Online (AJOL)

    Introduction: CAD/CAM (computer‑aided design and computer‑aided manufacturing) systems have refreshed the idea of chair‑side production of restorations, but the fracture of ceramic veneers remains a problem. Cementation with glass fibers may improve the fracture strengths and affect the failure modes of ...

  19. Kubelka-Munk reflectance theory applied to porcelain veneer systems using a colorimeter.

    Science.gov (United States)

    Davis, B K; Johnston, W M; Saba, R F

    1994-01-01

    The purpose of this study was to demonstrate the ability of Kubelka-Munk reflectance theory to predict color parameters of veneer porcelain on various backings using colorimetric measurements. Tristimulus absorption and scattering coefficients were used to predict the respective tristimulus reflectance values of A1, D3, and translucent porcelain samples after they had been bonded to light and dark substrates using universal, opaque, and untinted shades of bonding resin. Observed and predicted reflectance values exhibited high correlation (r2 > or = 0.93 for each porcelain shade). Kubelka-Munk theory offers an accurate prediction for the resultant colorimetric reflectance parameters of veneer porcelain bonded to variously colored backings.

  20. Compression of thick laminated composite beams with initial impact-like damage

    Science.gov (United States)

    Breivik, N. L.; Guerdal, Z.; Griffin, O. H., Jr.

    1992-01-01

    While the study of compression after impact of laminated composites has been under consideration for many years, the complexity of the damage initiated by low velocity impact has not lent itself to simple predictive models for compression strength. The damage modes due to non-penetrating, low velocity impact by large diameter objects can be simulated using quasi-static three-point bending. The resulting damage modes are less coupled and more easily characterized than actual impact damage modes. This study includes the compression testing of specimens with well documented initial damage states obtained from three-point bend testing. Compression strengths and failure modes were obtained for quasi-isotropic stacking sequences from 0.24 to 1.1 inches thick with both grouped and interspersed ply stacking. Initial damage prior to compression testing was divided into four classifications based on the type, extent, and location of the damage. These classifications are multiple through-thickness delaminations, isolated delamination, damage near the surface, and matrix cracks. Specimens from each classification were compared to specimens tested without initial damage in order to determine the effects of the initial damage on the final compression strength and failure modes. A finite element analysis was used to aid in the understanding and explanation of the experimental results.

  1. Simulation of Stress Concentration Problems in Laminated Plates by Quasi-Trefftz Finite Element Models

    Directory of Open Access Journals (Sweden)

    Flávio Luiz de Silva Bussamra

    Full Text Available Abstract Hybrid quasi-Trefftz finite elements have been applied with success to the analysis of laminated plates. Two independent fields are approximated by linearly independent, hierarchical polynomials: the stress basis in the domain, adapted from Papkovitch-Neuber solution of Navier equations, and the displacement basis, defined on element surface. The stress field that satisfies the Trefftz constraint a priori for isotropic material is adapted for orthotropic materials, which leads to the term "quasi". In this work, the hexahedral hybrid quasi-Trefftz stress element is applied to the modeling of nonsymmetric laminates and laminated composite plates with geometric discontinuities. The hierarchical p-refinement is exploited.

  2. Interlaminar Fracture Toughness of CFRP Laminates Incorporating Multi-Walled Carbon Nanotubes

    Directory of Open Access Journals (Sweden)

    Elisa Borowski

    2015-06-01

    Full Text Available Carbon fiber reinforced polymer (CFRP laminates exhibit limited fracture toughness due to characteristic interlaminar fiber-matrix cracking and delamination. In this article, we demonstrate that the fracture toughness of CFRP laminates can be improved by the addition of multi-walled carbon nanotubes (MWCNTs. Experimental investigations and numerical modeling were performed to determine the effects of using MWCNTs in CFRP laminates. The CFRP specimens were produced using an epoxy nanocomposite matrix reinforced with carboxyl functionalized multi-walled carbon nanotubes (COOH–MWCNTs. Four MWCNTs contents of 0.0%, 0.5%, 1.0%, and 1.5% per weight of the epoxy resin/hardener mixture were examined. Double cantilever beam (DCB tests were performed to determine the mode I interlaminar fracture toughness of the unidirectional CFRP composites. This composite material property was quantified using the critical energy release rate, GIC. The experimental results show a 25%, 20%, and 17% increase in the maximum interlaminar fracture toughness of the CFRP composites with the addition of 0.5, 1.0, and 1.5 wt% MWCNTs, respectively. Microstructural investigations using Fourier transform infrared (FTIR spectroscopy and X-ray photoelectron spectroscopy (XPS verify that chemical reactions took place between the COOH–MWCNTs and the epoxy resin, supporting the improvements experimentally observed in the interlaminar fracture toughness of the CFRP specimens containing MWCNTs. Finite element (FE simulations show good agreement with the experimental results and confirm the significant effect of MWCNTs on the interlaminar fracture toughness of CFRP.

  3. "Subclinical" laminitis in dairy cattle.

    Science.gov (United States)

    Vermunt, J J

    1992-12-01

    In dairying countries worldwide, the economic importance of lameness in cattle is now recognised. Laminitis is regarded as a major predisposing factor in lameness caused by claw disorders such as white zone lesions, sole ulcer, and heel horn erosion. The existence of subclinical laminitis was first suggested in the late 1970s by Dutch workers describing the symptoms of sole haemorrhages and yellowish-coloured, soft sole horn. In an attempt to clarify some of the confusing and often conflicting terminology, the literature on laminitis is reviewed. Disturbed haemodynamics, in particular repeated or prolonged dilation of arteriovenous anastomoses, have been implicated in the pathogenesis of both equine and bovine laminitis. Some characteristics of the vascular system of the bovine claw which may be of importance in the pathophysiology of the subclinical laminitis syndrome are therefore discussed. Clinical observations suggest that subclinical laminitis is a multifactorial disease. The different factors that are or may be involved in its aetiology vary in complexity and severity according to the management protocol of the animals. The possible involvement of subclinical laminitis in claw lesions is assessed.

  4. Processing and Characterization of Needled Carbon Composites

    Science.gov (United States)

    2015-12-01

    needle is used to insert high strength yarns (i.e., threads) through the dry fabric or prepreg laminate , leaving a loose thread loop underneath [9-11...capability which uses commercially-available felting needles to insert z-fibers into composite laminates at different angles (±45/90°) relative to the... laminate plane. Previous work with needled glass/epoxy composites has shown a 270% improvement in Mode I interlaminar fracture toughness when needled

  5. Ballistic Impact Resistance of Plain Woven Kenaf/Aramid Reinforced Polyvinyl Butyral Laminated Hybrid Composite

    Directory of Open Access Journals (Sweden)

    Suhad D. Salman

    2016-07-01

    Full Text Available Traditionally, the helmet shell has been used to provide protection against head injuries and fatalities caused by ballistic threats. In this study, because of the high cost of aramid fibres and the necessity for environmentally friendly alternatives, a portion of aramid was replaced with plain woven kenaf fibre, with different arrangements and thicknesses, without jeopardising the requirements demanded by U.S. Army helmet specifications. Furthermore, novel helmets were produced and tested to reduce the dependency on the ballistic resistance components. Their use could lead to helmets that are less costly and more easily available than conventional helmet armour. The hybrid materials subjected to ballistic tests were composed of 19 layers and were fabricated by the hot press technique using different numbers and configurations of plain woven kenaf and aramid layers. In the case of ballistic performance tests, a positive effect was found for the hybridisation of kenaf and aramid laminated composites.

  6. Sound insulation of composite cylindrical shells: a comparison between a laminated and a sandwich cylinder

    OpenAIRE

    Yuan, Chongxin; Roozen, Bert; Bergsma, Otto; Beukers, Adriaan

    2012-01-01

    The fuselages of aircraft are modeled as a cylinder in this paper, and the sound insulations of a sandwich cylinder and a laminated cylinder are studied both experimentally and numerically. The cylinders are excited by an acoustic pressure and a mechanical force respectively. Results show that under acoustic excitation, the sandwich cylinder and the laminated one have a similar sound insulation below 3000 Hz, but the sandwich cylinder has a much larger sound insulation at higher frequencies. ...

  7. Survival of ceramic veneers made of different materials after a minimum follow-up period of five years: a systematic review and meta-analysis.

    Science.gov (United States)

    Petridis, Haralampos P; Zekeridou, Alkisti; Malliari, Maria; Tortopidis, Dimitrios; Koidis, Petros

    2012-01-01

    The purpose of this systematic review was to compare the survival and complication rates of ceramic veneers produced with different techniques and materials after a minimum follow-up time of 5 years. A literature search was conducted, using electronic databases, relevant references, citations and journal researching, for clinical studies reporting on the survival of ceramic veneers fabricated with different techniques and materials with a mean followup time of at least 5 years. The search period spanned from January 1980 up to October 2010. Event rates were calculated for the following complications associated with ceramic veneers: fracture, debonding, marginal discoloration, marginal integrity, and caries. Summary estimates, and 5-year event rates were reported. Comparison between subgroups of different materials, as well as statistical significance, was calculated using a mixed effects model. Nine studies were selected for final analysis over an initial yield of 409 titles. No study directly compared the incidence of complications between ceramic veneers fabricated from different materials. Four of the included studies reported on the survival of ceramic veneers made out of feldspathic ceramics; four studies were on glass-ceramic veneers and one study included veneers fabricated from both materials. The mean observation time ranged between 5 and 10 years. Overall, the 5-year complication rates were low, with the exception of studies reporting on extended ceramic veneers. The most frequent complication reported was marginal discoloration (9% at 5 years), followed by marginal integrity (3.9-7.7% at 5 years). There was no statistically significant difference in the event rates between the subgroups of different materials (feldspathic vs. glass-ceramic). The results of this systematic review showed that ceramic veneers fabricated from feldspathic or glass-ceramics have an adequate clinical survival for at least 5 years of clinical service, with very low complication

  8. Front-facing fluoropolymer-coated armor composite

    OpenAIRE

    Gamache, Raymond M.; Roland, Charles M.; Fragiadakis, Daniel M.

    2018-01-01

    Patent A front-facing armor system utilizing a composite laminate backed by a high hardness substrate. The composite laminate comprises a series of first and second layers. The first layer of the bi-layer laminate system is a polymer with a density of at least 1.8 g/ᵌ and having both an amorphous and crystalline phase, and having phase transformation pressure of at least 0.5 GPa at a temperature of 20° C. The second layer of each bi-layer provides acoustic impedance ...

  9. Improving sensitivity of the polyurethane/CNT laminate strain sensor by controlled mechanical preload

    International Nuclear Information System (INIS)

    Slobodian, Petr; Olejnik, Robert; Matyas, Jiri; Babar, Dipak Gorakh

    2016-01-01

    This article describes strain detection potential of polyurethane/CNT layered composite and further possible enhance of its sensitivity to strain, expressed by value of gauge factor, GF, employing its controlled mechanical preload. In course of its fabrication a non-woven polyurethane membrane made by electro spinning was used as filtering membrane for CNT aqueous dispersion. Final CNT polyurethane laminate composite is prepared by compression molding. Produced polyurethane/CNT composite laminate is electrically conductive and high elastic. Its elongation leads to change of its macroscopic electrical resistance. Changes in resistance are further reversible, reproducible and can monitor deformation in real time. Gauge factor reaches very high values around 8 for strain reaching 3.5% comparing with conventional metallic strain gauges. Finally, controlled mechanical preload significantly increases value of GF. For example for value of 8.1% of preload value of GF reaches 23.3 for strain 3.5%. (paper)

  10. Multi-Material and Thickness Optimization Utilizing Casting Filters for Laminated Composite Structures

    DEFF Research Database (Denmark)

    Sørensen, Rene; Lund, Erik

    2013-01-01

    . The reformulation eliminates the need for having explicit constraint for ensuring that intermediate void does not appear in between layers of the laminate. This is achieved by utilizing a filtering technique known as a casting constraint from traditional topology optimization with isotropic materials....

  11. Composite smile designs: the key to dental artistry.

    Science.gov (United States)

    Portalier, L

    1997-01-01

    Patients seeking to improve the appearance of their smiles have driven the profession toward more challenges in esthetic dentistry to answer their needs. Better smiles are being equated with better living. Direct composite veneering has gained tremendous popularity over the past few years because the procedure can be done in one single appointment for a reasonable fee with acceptable results. Materials recently put on the market require stratification build-up techniques to allow for the best natural results. In addition, the procedure gives patients the freedom of live communication and dentists the emotive artistic recreation of a smile composition in which anterior teeth can be designed and redesigned through freehand craftmanship, until both patient and dentist are pleased with the results. This review highlights the benefits of direct composite veneering, a very unique process to investigate more about tooth and smile designs, and suggests more effective communication between patient and dentist in order to achieve predictable results.

  12. Hygrothermal influence on delamination behavior of graphite/epoxy laminates

    Science.gov (United States)

    Garg, A.; Ishai, O.

    1985-01-01

    The hygrothermal effect on the fracture behavior of graphite-epoxy laminates was investigated to develop a methodology for damage tolerance predictions in advanced composite materials. Several T300/934 laminates were tested using a number of specimen configurations to evaluate the effects of temperature and humidity on delamination fracture toughness under mode 1 and mode 2 loading. It is indicated that moisture has a slightly beneficial influence on fracture toughness or critical strain energy release rate during mode 1 delamination, but has a slightly deleterious effect on mode 2 delamination, and mode 1 transverse cracking. The failed specimens are examined by SEM and topographical differences due to fracture modes are identified. It is concluded that the effect of moisture on fracture topography can not be distinguished.

  13. Effect of various veneering techniques on mechanical strength of computer-controlled zirconia framework designs.

    Science.gov (United States)

    Kanat, Burcu; Cömlekoğlu, Erhan M; Dündar-Çömlekoğlu, Mine; Hakan Sen, Bilge; Ozcan, Mutlu; Ali Güngör, Mehmet

    2014-08-01

    The objectives of this study were to evaluate the fracture resistance (FR), flexural strength (FS), and shear bond strength (SBS) of zirconia framework material veneered with different methods and to assess the stress distributions using finite element analysis (FEA). Zirconia frameworks fabricated in the forms of crowns for FR, bars for FS, and disks for SBS (N = 90, n = 10) were veneered with either (a) file splitting (CAD-on) (CD), (b) layering (L), or (c) overpressing (P) methods. For crown specimens, stainless steel dies (N = 30; 1 mm chamfer) were scanned using the labside contrast spray. A bilayered design was produced for CD, whereas a reduced design (1 mm) was used for L and P to support the veneer by computer-aided design and manufacturing. For bar (1.5 × 5 × 25 mm(3) ) and disk (2.5 mm diameter, 2.5 mm height) specimens, zirconia blocks were sectioned under water cooling with a low-speed diamond saw and sintered. To prepare the suprastructures in the appropriate shapes for the three mechanical tests, nano-fluorapatite ceramic was layered and fired for L, fluorapatite-ceramic was pressed for P, and the milled lithium-disilicate ceramics were fused with zirconia by a thixotropic glass ceramic for CD and then sintered for crystallization of veneering ceramic. Crowns were then cemented to the metal dies. All specimens were stored at 37°C, 100% humidity for 48 hours. Mechanical tests were performed, and data were statistically analyzed (ANOVA, Tukey's, α = 0.05). Stereomicroscopy and scanning electron microscopy (SEM) were used to evaluate the failure modes and surface structure. FEA modeling of the crowns was obtained. Mean FR values (N ± SD) of CD (4408 ± 608) and L (4323 ± 462) were higher than P (2507 ± 594) (p mechanical tests, whereas a layering technique increased the FR when an anatomical core design was employed. File splitting (CAD-on) or layering veneering ceramic on zirconia with a reduced framework design may reduce ceramic chipping

  14. The use of wood for wind turbine blade construction

    Science.gov (United States)

    Gougeon, M.; Zuteck, M.

    1979-01-01

    The interrelationships between moisture and wood, conditions for dry rot spore activity, the protection of wood fibers from moisture, wood resin composites, wood laminating, quality control, and the mechanical properties of wood are discussed. The laminated veneer and the bonded sawn stock fabrication techniques, used in the construction of a turbine blade with a monocoque 'D' section forming the leading edge and a built up trailing edge section, are described. A 20 foot root end sample complete with 24 bonded-in studs was successfully subjected to large onetime loads in both the flatwise and edgewise directions, and to fatigue tests. Results indicate that wood is both a viable and advantageous material for use in wind turbine blades. The basic material is reasonably priced, domestically available, ecologically sound, and easily fabricated with low energy consumption.

  15. A theory of piezoelectric laminates

    International Nuclear Information System (INIS)

    Giangreco, E.

    1997-01-01

    A theory of piezoelectric laminates is rationally derived from the three-dimensional Voigt theory of piezoelectricity. The present theory is a generalization to piezoelectric laminates of the Reissner-Mindlin-type layer-wise theory of elastic laminates. Both a differential formulation and a variational formulation of the piezoelectric laminate problem are presented. The proposed theory is adopted in the analysis of simple problems, in order to verify its effectiveness. The results it provides turn out to be in good agreement with the results supplied by the Voigt theory of piezoelectricity

  16. Criterion for matrix cracking in glass fiber reinforced cross-ply laminates. GFRP chokko sekisoban ni okeru matrix kiretsu no hattatsu kijun

    Energy Technology Data Exchange (ETDEWEB)

    Motoki, S.; Fukuda, T. (Osaka City Univ., Osaka (Japan). Faculty of Engineering); Tanaka, M. (Kobe City College of Technology, Kobe (Japan))

    1992-05-15

    In this research, with regard to GFRP cross-ply laminates, which were the most basic lamination composition, the factors governing the progress of matrix cracks at the 90{degree} layer were studied, in particular the criterion for not depending on the thickness of the 90{degree} layer was examined. For the experiment concerning the above, GFRP prepreg was laminated and three kinds of cross-ply laminates were made for use. A quasistatic tensile load was applied to these specimens and a load-displacement curve was measured, and at the same time, the matrix crack numbers generated in the 90{degree} layer were counted. As a result, it was found that the maximum value of the vertical stress in the loading direction of 90{degree} layer did not depend on the lamination composition, hence could become the criterion for the crack progress. Also it was found that in case when this stress surpassed a certain threshold value, cracks were formed, but in case when it was smaller than the threshold value, no crack was formed. 12 refs., 14 figs.

  17. Stochastic analysis of laminated composite plates on elastic foundation: The cases of post-buckling behavior and nonlinear free vibration

    International Nuclear Information System (INIS)

    Singh, B.N.; Lal, Achchhe

    2010-01-01

    This study deals with the stochastic post-buckling and nonlinear free vibration analysis of a laminated composite plate resting on a two parameters Pasternak foundation with Winkler cubic nonlinearity having uncertain system properties. The system properties are modeled as basic random variables. A C 0 nonlinear finite element formulation of the random problem based on higher-order shear deformation theory in the von Karman sense is presented. A direct iterative method in conjunction with a stochastic nonlinear finite element method proposed earlier by the authors is extended to analyze the effect of uncertainty in system properties on the post-buckling and nonlinear free vibration of the composite plates having Winler type of geometric nonlinearity. Mean as well as standard deviation of the responses have been obtained for various combinations of geometric parameters, foundation parameters, stacking sequences and boundary conditions and compared with those available in the literature and Monte Carlo simulation.

  18. Behavior of fiber reinforced metal laminates at high strain rate

    Science.gov (United States)

    Newaz, Golam; Sasso, Marco; Amodio, Dario; Mancini, Edoardo

    2018-05-01

    Carbon Fiber Reinforced Aluminum Laminate (CARALL) is a good system for energy absorption through plastic deformation in aluminum and micro-cracking in the composite layers. Moreover, CARALL FMLs also provide excellent impact resistance due to the presence of aluminum layer. The focus of this research is to characterize the CARALL behavior under dynamic conditions. High strain rate tests on sheet laminate samples have been carried out by means of direct Split Hopkinson Tension Bar. The sample geometry and the clamping system were optimized by FEM simulations. The clamping system has been designed and optimized in order reduce impedance disturbance due to the fasteners and to avoid the excessive plastic strain outside the gauge region of the samples.

  19. Estimation of stepwise crack propagation in ceramic laminates with strong interfaces

    Directory of Open Access Journals (Sweden)

    K. Štegnerová

    2015-10-01

    Full Text Available During the last years many researchers put so much effort to design layered structures combining different materials in order to improve low fracture toughness and mechanical reliability of the ceramics. It has been proven, that an effective way is to create layered ceramics with strongly bonded interfaces. After the cooling process from the sintering temperature, due to the different coefficients of thermal expansion of individual constituents of the composite, significant internal residual stresses are developed within the layers. These stresses can change the crack behaviour. This results to the higher value of so-called apparent fracture toughness, i.e. higher resistance of the ceramic laminate to the crack propagation. The contribution deals with a description of the specific crack behaviour in the layered alumina-zirconia ceramic laminate. The main aim is to clarify crack behaviour in the compressive layer and provide computational tools for estimation of crack behaviour in the field of strong residual stresses. The crack propagation was investigated on the basis of linear elastic fracture mechanics. Fracture parameters were computed numerically and by author’s routines. Finite element models were developed in order to obtain a stress distribution in the laminate containing a crack and to simulate crack propagation. The sharp change of the crack propagation direction was estimated using Sih’s criterion based on the strain energy density factor. Estimated crack behaviour is qualitatively in a good agreement with experimental observations. Presented approach contributes to the better understanding of the toughening mechanism of ceramic laminates and can be advantageously used for design of new layered ceramic composites and for better prediction of their failure.

  20. Natural frequencies and an atlas of mode shapes for generally-laminated, thick, skew, trapezoidal plates

    OpenAIRE

    Lovejoy, Andrew Elwyn

    1994-01-01

    Composite materials are increasingly finding use in structures, such as aircraft components, and thus, an accurate method of predicting response is required. Even laminated structures that are considered thin can be significantly affected by transverse shear effects, and as a result, transverse shear should not be neglected. The free vibration response of generally-laminated, thick, skew, trapezoidal plates is investigated as there appears to be a lack of information in this ar...