  1. Low-temperature electrical transport in B-doped ultrananocrystalline diamond film

    International Nuclear Information System (INIS)

    Li, Lin; Zhao, Jing; Hu, Zhaosheng; Quan, Baogang; Li, Junjie; Gu, Changzhi

    2014-01-01

    B-doped ultrananocrystalline diamond (UNCD) films are grown using hot-filament chemical vapor deposition method, and their electrical transport properties varying with temperature are investigated. When the B-doped concentration of UNCD film is low, a step-like increase feature of the resistance is observed with decreasing temperature, reflecting at least three temperature-modified electronic state densities at the Fermi level according to three-dimensional Mott's variable range hopping transport mechanism, which is very different from that of reported B-doped nanodiamond. With increasing B-doped concentration, a superconductive transformation occurs in the UNCD film and the highest transformation temperature of 5.3 K is observed, which is higher than that reported for superconducting nanodiamond films. In addition, the superconducting coherence length is about 0.63 nm, which breaks a reported theoretical and experimental prediction about ultra-nanoscale diamond's superconductivity

  2. Effect of doping on electronic states in B-doped polycrystalline CVD diamond films

    International Nuclear Information System (INIS)

    Elsherif, O S; Vernon-Parry, K D; Evans-Freeman, J H; May, P W

    2012-01-01

    High-resolution Laplace deep-level transient spectroscopy (LDLTS) and thermal admittance spectroscopy (TAS) have been used to determine the effect of boron (B) concentration on the electronic states in polycrystalline chemical vapour deposition diamond thin films grown on silicon by the hot filament method. A combination of high-resolution LDLTS and direct-capture cross-sectional measurements was used to investigate whether the deep electronic states present in the layers originated from point or extended defects. There was good agreement between data on deep electronic levels obtained from DLTS and TAS experiments. Two hole traps, E1 (0.29 eV) and E2 (0.53 eV), were found in a film with a boron content of 1 × 10 19 cm −3 . Both these levels and an additional level, E3 (0.35 eV), were found when the B content was increased to 4 × 10 19 cm −3 . Direct capture cross-sectional measurements of levels E1 and E2 show an unusual dependence on the fill-pulse duration which is interpreted as possibly indicating that the levels are part of an extended defect. The E3 level found in the more highly doped film consisted of two closely spaced levels, both of which show point-like defect characteristics. The E1 level may be due to B-related extended defects within the grain boundaries, whereas the ionization energy of the E2 level is in agreement with literature values from ab initio calculations for B–H complexes. We suggest that the E3 level is due to isolated B-related centres in bulk diamond. (paper)

  3. Morphological and electrochemical properties of boron-doped diamond films on carbon cloths with enhanced surface area

    International Nuclear Information System (INIS)

    Silva, L.L.G.; Ferreira, N.G.; Corat, E.J.

    2008-01-01

    The electrochemical properties of doped diamond electrodes (10 17 -10 19 B cm -3 ) grown on carbon fiber cloths in H 2 SO 4 0.1 mol L -1 electrolyte were investigated. Cyclic voltammograms of B-doped diamond/carbon fiber cloth and carbon fiber cloth electrodes showed that both kinds of electrodes possess similar working potential windows of about 2.0 V. The electrode capacitance was determined by impedance spectroscopy and chronopotentiometry measurements and very close values were obtained. The capacitance values of the diamond film on carbon fiber cloths were 180 times higher than the ones of diamond films on Si. In this paper we have also discussed the capacitance frequency dependence of diamond/carbon cloth electrodes

  4. OSL and TL dosimeter characterization of boron doped CVD diamond films

    Science.gov (United States)

    Gonçalves, J. A. N.; Sandonato, G. M.; Meléndrez, R.; Chernov, V.; Pedroza-Montero, M.; De la Rosa, E.; Rodríguez, R. A.; Salas, P.; Barboza-Flores, M.

    2005-04-01

    Natural diamond is an exceptional prospect for clinical radiation dosimetry due to its tissue-equivalence properties and being chemically inert. The use of diamond in radiation dosimetry has been halted by the high market price; although recently the capability of growing high quality CVD diamond has renewed the interest in using diamond films as radiation dosimeters. In the present work we have characterized the dosimetric properties of diamond films synthesized by the HFCVD method. The thermoluminescence and the optically stimulated luminescence of beta exposed diamond sample containing a B/C 4000 ppm doping presents excellent properties suitable for dosimetric applications with β-ray doses up to 3.0 kGy. The observed OSL and TL performance is reasonable appropriate to justify further investigation of diamond films as dosimeters for ionizing radiation, specially in the radiotherapy field where very well localized and in vivo and real time radiation dose applications are essential.

  5. Toward deep blue nano hope diamonds: heavily boron-doped diamond nanoparticles.

    Science.gov (United States)

    Heyer, Steffen; Janssen, Wiebke; Turner, Stuart; Lu, Ying-Gang; Yeap, Weng Siang; Verbeeck, Jo; Haenen, Ken; Krueger, Anke

    2014-06-24

    The production of boron-doped diamond nanoparticles enables the application of this material for a broad range of fields, such as electrochemistry, thermal management, and fundamental superconductivity research. Here we present the production of highly boron-doped diamond nanoparticles using boron-doped CVD diamond films as a starting material. In a multistep milling process followed by purification and surface oxidation we obtained diamond nanoparticles of 10-60 nm with a boron content of approximately 2.3 × 10(21) cm(-3). Aberration-corrected HRTEM reveals the presence of defects within individual diamond grains, as well as a very thin nondiamond carbon layer at the particle surface. The boron K-edge electron energy-loss near-edge fine structure demonstrates that the B atoms are tetrahedrally embedded into the diamond lattice. The boron-doped diamond nanoparticles have been used to nucleate growth of a boron-doped diamond film by CVD that does not contain an insulating seeding layer.

  6. Fabrication and characterization of boron-doped nanocrystalline diamond-coated MEMS probes

    Science.gov (United States)

    Bogdanowicz, Robert; Sobaszek, Michał; Ficek, Mateusz; Kopiec, Daniel; Moczała, Magdalena; Orłowska, Karolina; Sawczak, Mirosław; Gotszalk, Teodor

    2016-04-01

    Fabrication processes of thin boron-doped nanocrystalline diamond (B-NCD) films on silicon-based micro- and nano-electromechanical structures have been investigated. B-NCD films were deposited using microwave plasma assisted chemical vapour deposition method. The variation in B-NCD morphology, structure and optical parameters was particularly investigated. The use of truncated cone-shaped substrate holder enabled to grow thin fully encapsulated nanocrystalline diamond film with a thickness of approx. 60 nm and RMS roughness of 17 nm. Raman spectra present the typical boron-doped nanocrystalline diamond line recorded at 1148 cm-1. Moreover, the change in mechanical parameters of silicon cantilevers over-coated with boron-doped diamond films was investigated with laser vibrometer. The increase of resonance to frequency of over-coated cantilever is attributed to the change in spring constant caused by B-NCD coating. Topography and electrical parameters of boron-doped diamond films were investigated by tapping mode AFM and electrical mode of AFM-Kelvin probe force microscopy (KPFM). The crystallite-grain size was recorded at 153 and 238 nm for boron-doped film and undoped, respectively. Based on the contact potential difference data from the KPFM measurements, the work function of diamond layers was estimated. For the undoped diamond films, average CPD of 650 mV and for boron-doped layer 155 mV were achieved. Based on CPD values, the values of work functions were calculated as 4.65 and 5.15 eV for doped and undoped diamond film, respectively. Boron doping increases the carrier density and the conductivity of the material and, consequently, the Fermi level.

  7. Growing of synthetic diamond boron-doped films for analytical applications

    International Nuclear Information System (INIS)

    Barros, Rita de Cassia Mendes de; Suarez-Iha, Maria Encarnacion Vazquez; Corat, Evaldo Jose; Iha, Koshun

    1999-01-01

    Chemical vapor deposition (CVD) technology affords the possibility of producing synthetic diamond film electrodes, with several advantageous properties due the unique characteristics of diamond. In this work, we present the study of boron-doped diamond films growth on molybdenum and silicon substrates, using boron trioxide as dopant in a filament assisted CVD reactor. The objective was to obtain semiconductor diamond for use as electrode. The samples were characterized by scanning electron microscopy and Raman spectroscopy to confirm morphology and doping levels. We have assembled electrodes with the various samples, Pt, Mo, Si and diamond, by utilizing brass and left as base materials. The electrodes were tested in neutralization potentiometric titrations for future use in electroanalysis. Boron-doped electrodes have very good performance compared with Pt, widely used in analytical chemistry. (author)

  8. Morphology and structure of Ti-doped diamond films prepared by microwave plasma chemical vapor deposition

    Science.gov (United States)

    Liu, Xuejie; Lu, Pengfei; Wang, Hongchao; Ren, Yuan; Tan, Xin; Sun, Shiyang; Jia, Huiling

    2018-06-01

    Ti-doped diamond films were deposited through a microwave plasma chemical vapor deposition (MPCVD) system for the first time. The effects of the addition of Ti on the morphology, microstructure and quality of diamond films were systematically investigated. Secondary ion mass spectrometry results show that Ti can be added to diamond films through the MPCVD system using tetra n-butyl titanate as precursor. The spectra from X-ray diffraction, Raman spectroscopy, and X-ray photoelectron spectroscopy and the images from scanning electron microscopy of the deposited films indicate that the diamond phase clearly exists and dominates in Ti-doped diamond films. The amount of Ti added obviously influences film morphology and the preferred orientation of the crystals. Ti doping is beneficial to the second nucleation and the growth of the (1 1 0) faceted grains.

  9. Structural Transformation upon Nitrogen Doping of Ultrananocrystalline Diamond Films by Microwave Plasma CVD

    Directory of Open Access Journals (Sweden)

    Chien-Chung Teng

    2009-01-01

    Full Text Available The molecular properties and surface morphology of undoped and N-doped ultra-nanocrystalline diamond (UNCD films deposited by microwave plasma CVD with addition of nitrogen are investigated with various spectroscopic techniques. The results of spatially resolved Raman scattering, ATR/FT-IR and XPS spectra show more amorphous and sp2/sp3 ratio characteristics in N-doped UNCD films. The surface morphology in AFM scans shows larger nanocrystalline diamond clusters in N-doped UNCD films. Incorporation of nitrogen into UNCD films has promoted an increase of amorphous sp2-bonded carbons in the grain boundaries and the size of nanocrystalline diamond grains that are well correlated to the reported enhancement of conductivity and structural changes of UNCD films.

  10. Combined effect of nitrogen doping and nanosteps on microcrystalline diamond films for improvement of field emission

    International Nuclear Information System (INIS)

    Mengui, U.A.; Campos, R.A.; Alves, K.A.; Antunes, E.F.; Hamanaka, M.H.M.O.; Corat, E.J.; Baldan, M.R.

    2015-01-01

    Highlights: • Hot filament chemical vapor deposition using methane, hydrogen and a solution of urea in methanol produced nitrogen-doped diamond films. • Diamonds had the grain morphology changed for long growth time (28 h), and the nitrogen doping were evaluated by Raman spectroscopy. • Field emission characterization shows a decrease up to 70% in threshold field, related to reference diamond layer. - Abstract: Nitrogen-doped microcrystalline diamond (N-MCD) films were grown on Si substrates using a hot filament reactor with methanol solution of urea as N source. Electrostatic self-assembly seeding of nanocrystalline diamond were used to obtain continuous and uniform films. Simultaneous changes in grains morphology and work function of diamond by nitrogen doping decreased the threshold field and the angular coefficient of Fowler–Nordhein plots. The field emission properties of our N-MCD films are comparable to carbon nanotube films

  11. Combined effect of nitrogen doping and nanosteps on microcrystalline diamond films for improvement of field emission

    Energy Technology Data Exchange (ETDEWEB)

    Mengui, U.A., E-mail: ursulamengui@gmail.com [INPE – Instituto Nacional de Pesquisas Espaciais Laboratório Associado de Sensores e Materiais – LAS, Av. dos Astronautas 1758, CP 515, CEP 12.245-970, São José dos Campos, SP (Brazil); Campos, R.A.; Alves, K.A.; Antunes, E.F. [INPE – Instituto Nacional de Pesquisas Espaciais Laboratório Associado de Sensores e Materiais – LAS, Av. dos Astronautas 1758, CP 515, CEP 12.245-970, São José dos Campos, SP (Brazil); Hamanaka, M.H.M.O. [Centro de Tecnologia da Informação Renato Archer, Divisão de Superfícies de Interação e Displays, Rodovia D. Pedro I (SP 65) km 143.6, CP 6162, CEP 13089-500, Campinas, SP (Brazil); Corat, E.J.; Baldan, M.R. [INPE – Instituto Nacional de Pesquisas Espaciais Laboratório Associado de Sensores e Materiais – LAS, Av. dos Astronautas 1758, CP 515, CEP 12.245-970, São José dos Campos, SP (Brazil)

    2015-04-15

    Highlights: • Hot filament chemical vapor deposition using methane, hydrogen and a solution of urea in methanol produced nitrogen-doped diamond films. • Diamonds had the grain morphology changed for long growth time (28 h), and the nitrogen doping were evaluated by Raman spectroscopy. • Field emission characterization shows a decrease up to 70% in threshold field, related to reference diamond layer. - Abstract: Nitrogen-doped microcrystalline diamond (N-MCD) films were grown on Si substrates using a hot filament reactor with methanol solution of urea as N source. Electrostatic self-assembly seeding of nanocrystalline diamond were used to obtain continuous and uniform films. Simultaneous changes in grains morphology and work function of diamond by nitrogen doping decreased the threshold field and the angular coefficient of Fowler–Nordhein plots. The field emission properties of our N-MCD films are comparable to carbon nanotube films.

  12. Soft X-ray angle-resolved photoemission spectroscopy of heavily boron-doped superconducting diamond films

    Directory of Open Access Journals (Sweden)

    T. Yokoya, T. Nakamura, T. Matushita, T. Muro, H. Okazaki, M. Arita, K. Shimada, H. Namatame, M. Taniguchi, Y. Takano, M. Nagao, T. Takenouchi, H. Kawarada and T. Oguchi

    2006-01-01

    Full Text Available We have performed soft X-ray angle-resolved photoemission spectroscopy (SXARPES of microwave plasma-assisted chemical vapor deposition diamond films with different B concentrations in order to study the origin of the metallic behavior of superconducting diamond. SXARPES results clearly show valence band dispersions with a bandwidth of ~23 eV and with a top of the valence band at gamma point in the Brillouin zone, which are consistent with the calculated valence band dispersions of pure diamond. Boron concentration-dependent band dispersions near the Fermi level (EF exhibit a systematic shift of EF, indicating depopulation of electrons due to hole doping. These SXARPES results indicate that diamond bands retain for heavy boron doping and holes in the diamond band are responsible for the metallic states leading to superconductivity at low temperature. A high-resolution photoemission spectroscopy spectrum near EF of a heavily boron-doped diamond superconductor is also presented.

  13. Superconductivity and low temperature electrical transport in B-doped CVD nanocrystalline diamond

    Directory of Open Access Journals (Sweden)

    Milos Nesladek, Jiri J. Mares, Dominique Tromson, Christine Mer, Philippe Bergonzo, Pavel Hubik and Jozef Kristofik

    2006-01-01

    Full Text Available In this work, we report on superconductivity (SC found in thin B-doped nanocrystalline diamond films, prepared by the PE-CVD technique. The thickness of the films varies from about 100 to 400 nm, the films are grown on low-alkaline glass at substrate temperatures of about 500–700 °C. The SIMS measurements show that films can be heavily doped with boron in concentrations in the range of 3×1021 cm−3. The Raman spectra show Fano resonances, confirming the substitutional B-incorporation. The low temperature magnetotransport measurements reveal a positive magnetoresistance. The SC transition is observed at about Tc=1.66 K. A simple theory exploiting the concept of weak localization accounting for this transition is proposed.

  14. Microwave plasma-assisted photoluminescence enhancement in nitrogen-doped ultrananocrystalline diamond film

    Directory of Open Access Journals (Sweden)

    Yu Lin Liu

    2012-06-01

    Full Text Available Optical properties and conductivity of nitrogen-doped ultrananocrystal diamond (UNCD films were investigated following treatment with low energy microwave plasma at room temperature. The plasma also generated vacancies in UNCD films and provided heat for mobilizing the vacancies to combine with the impurities, which formed the nitrogen-vacancy defect centers. The generated color centers were distributed uniformly in the samples. The conductivity of nitrogen-doped UNCD films treated by microwave plasma was found to decrease slightly due to the reduced grain boundaries. The photoluminescence emitted by the plasma treated nitrogen-doped UNCD films was enhanced significantly compared to the untreated films.

  15. Improvement on p-type CVD diamond semiconducting properties by fabricating thin heavily-boron-doped multi-layer clusters isolated each other in unintentionally boron-doped diamond layer

    Science.gov (United States)

    Maida, Osamu; Tabuchi, Tomohiro; Ito, Toshimichi

    2017-12-01

    We have developed a new fabrication process to decrease the effective activation energy of B atoms doped in diamond without a significant decrease in the carrier mobility by fabricating heavily B-doped clusters with very low mobility which are embedded in lightly-B-doped diamond layers. The resistivities of the heavily B-doped and unintentionally B-doped diamond stacked layers had almost no temperature dependence, suggesting the presence of an impurity-band conduction in these diamond layers. On the other hand, the resistivities of the samples after the embedding growth process of the stacked layers that had been appropriately divided to innumerable small clusters by means of a suitable etching process increased with decreasing the temperature from 330 to 130 K. The effective activation energies and Hall mobilities at room temperature of both samples were estimated to be 0.21 eV, 106 cm2 V-1 s-1 for micron-sized clusters and 0.23 eV, 470 cm2 V-1 s-1 for nano-sized clusters, respectively, indicating that the diamond film structure fabricated in this work is effective for the improvement of the p-type performance for the B-doped CVD diamond.

  16. Effect of boron doping on the wear behavior of the growth and nucleation surfaces of micro- and nanocrystalline diamond films

    NARCIS (Netherlands)

    Buijnsters, J.G.; Tsigkourakos, M.C.; Hantschel, T.; Gomes, F.O.V.; Nuytten, T.; Favia, P.; Bender, H; Arstila, K.; Celis, JP; Vandervorst, W

    2016-01-01

    B-doped diamond has become the ultimate material for applications in the field of microelectromechanical systems (MEMS), which require both highly wear resistant and electrically conductive diamond films and microstructures. Despite the extensive research of the tribological properties of undoped

  17. Electrical conductivity enhancement by boron-doping in diamond using first principle calculations

    Science.gov (United States)

    Ullah, Mahtab; Ahmed, Ejaz; Hussain, Fayyaz; Rana, Anwar Manzoor; Raza, Rizwan

    2015-04-01

    Boron doping in diamond plays a vital role in enhancing electrical conductivity of diamond by making it a semiconductor, a conductor or even a superconductor. To elucidate this fact, partial and total density of states has been determined as a function of B-content in diamond. Moreover, the orbital charge distributions, B-C bond lengths and their population have been studied for B-doping in pristine diamond thin films by applying density functional theory (DFT). These parameters have been found to be influenced by the addition of different percentages of boron atoms in diamond. The electronic density of states, B-C bond situations as well as variations in electrical conductivities of diamond films with different boron content and determination of some relationship between these parameters were the basic tasks of this study. Diamond with high boron concentration (∼5.88% B-atoms) showed maximum splitting of energy bands (caused by acceptor impurity states) at the Fermi level which resulted in the enhancement of electron/ion conductivities. Because B atoms either substitute carbon atoms and/or assemble at grain boundaries (interstitial sites) inducing impurity levels close to the top of the valence band. At very high B-concentration, impurity states combine to form an impurity band which accesses the top of the valence band yielding metal like conductivity. Moreover, bond length and charge distributions are found to decrease with increase in boron percentage in diamond. It is noted that charge distribution decreased from +1.89 to -1.90 eV whereas bond length reduced by 0.04 Å with increasing boron content in diamond films. These theoretical results support our earlier experimental findings on B-doped diamond polycrystalline films which depict that the addition of boron atoms to diamond films gives a sudden fall in resistivity even up to 105 Ω cm making it a good semiconductor for its applications in electrical devices.

  18. Increased charge storage capacity of titanium nitride electrodes by deposition of boron-doped nanocrystalline diamond films

    DEFF Research Database (Denmark)

    Meijs, Suzan; McDonald, Matthew; Sørensen, Søren

    2015-01-01

    The aim of this study was to investigate the feasibility of depositing a thin layer of boron-doped nanocrystalline diamond (B-NCD) on titanium nitride (TiN) coated electrodes and the effect this has on charge injection properties. The charge storage capacity increased by applying the B-NCD film...

  19. Visible sub-band gap photoelectron emission from nitrogen doped and undoped polycrystalline diamond films

    Energy Technology Data Exchange (ETDEWEB)

    Elfimchev, S., E-mail: sergeyel@tx.technion.ac.il; Chandran, M.; Akhvlediani, R.; Hoffman, A.

    2017-07-15

    Highlights: • Nitrogen related centers in diamond film are mainly responsible for visible sub-band-gap photoelectron emission. • The influence of film thickness and substrate on the measured photoelectron emission yields was not found. • Nanocrystalline diamonds have low electron emission yields most likely because of high amount of defects. • Visible sub-band gap photoelectron emission may increase with temperature due to electron trapping/detrapping processes. - Abstract: In this study the origin of visible sub-band gap photoelectron emission (PEE) from polycrystalline diamond films is investigated. The PEE yields as a function of temperature were studied in the wavelengths range of 360–520 nm. Based on the comparison of electron emission yields from diamond films deposited on silicon and molybdenum substrates, with different thicknesses and nitrogen doping levels, we suggested that photoelectrons are generated from nitrogen related centers in diamond. Our results show that diamond film thickness and substrate material have no significant influence on the PEE yield. We found that nanocrystalline diamond films have low electron emission yields, compared to microcrystalline diamond, due to the presence of high amount of defects in the former, which trap excited electrons before escaping into the vacuum. However, the low PEE yield of nanocrystalline diamond films was found to increase with temperature. The phenomenon was explained by the trap assisted photon enhanced thermionic emission (ta-PETE) model. According to the ta-PETE model, photoelectrons are trapped by shallow traps, followed by thermal excitation at elevated temperatures and escape into the vacuum. Activation energies of trap levels were estimated for undoped nanocrystalline, undoped microcrystalline and N-doped diamond films using the Richardson-Dushman equation, which gives 0.13, 0.39 and 0.04 eV, respectively. Such low activation energy of trap levels makes the ta-PETE process very

  20. Electrical characterization of 10B doped diamond irradiated with low thermal neutron fluence

    International Nuclear Information System (INIS)

    Reed, M.L.; Reed, M.J.; Jagannadham, K.; Verghese, K.; Bedair, S.M.; El-Masry, N.; Butler, J.E.

    2004-01-01

    A sample of 10 B isotope doped diamond was neutron irradiated to a thermal fluence of 1.3x10 19 neutron cm -2 . The diamond sample was cooled continuously during irradiation in a nuclear reactor. 7 Li is formed by nuclear transmutation reaction from 10 B. Characterization for electrical conductance in the temperature range of 160 K 10 B doped sample and the 10 B doped and irradiated sample. The unirradiated diamond sample showed p-type conductance at higher temperature (T>200 K) and p-type surface conductance at lower temperature (T 7 Li that is formed by nuclear transmutation reaction from 10 B atoms. Also, compensation of n-type carriers from 7 Li by p-type carriers from 10 B is used to interpret the conductance above 400 K. A low concentration of radiation induced defects, absence of defect complexes, and the low activation energy of n-type 7 Li are thought responsible for the observed variation of conductance in the irradiated diamond. The present results illustrate that neutron transmutation from 10 B doped diamond is a useful method to achieve n-type conductivity in diamond

  1. Concurrent doping effect of Ti and nano-diamond on flux pinning of MgB2

    International Nuclear Information System (INIS)

    Zhao, Y.; Ke, C.; Cheng, C.H.; Feng, Y.; Yang, Y.; Munroe, P.

    2010-01-01

    Nano-diamond and titanium concurrently doped MgB 2 nanocomposites have been prepared by solid state reaction method. The effects of carbon and Ti concurrent doping on J c -H behavior and pinning force scaling features of MgB 2 have been investigated. Although T c was slightly depressed, J c of MgB 2 have been significantly improved by the nano-diamond doping, especially in the high field region. In the mean time, the J c value in low field region is sustained though concurrent Ti doping. Microstructure analysis reveals that when nano-diamond was concurrently doped with titanium in MgB 2 , a unique nanocomposite in which TiB 2 forms a thin layer surrounding MgB 2 grains whereas nano-diamond particles were wrapped inside the MgB 2 grains. Besides, nano-diamond doping results in a high density stress field in the MgB 2 samples, which may take responsibility for the Δκ pinning behavior in the carbon-doped MgB 2 system.

  2. First principles calculation of lithium-phosphorus co-doped diamond

    Directory of Open Access Journals (Sweden)

    Q.Y. Shao

    2013-03-01

    Full Text Available We calculate the density of states (DOS and the Mulliken population of the diamond and the co-doped diamonds with different concentrations of lithium (Li and phosphorus (P by the method of the density functional theory, and analyze the bonding situations of the Li-P co-doped diamond thin films and the impacts of the Li-P co-doping on the diamond conductivities. The results show that the Li-P atoms can promote the split of the diamond energy band near the Fermi level, and improve the electron conductivities of the Li-P co-doped diamond thin films, or even make the Li-P co-doped diamond from semiconductor to conductor. The affection of Li-P co-doping concentration on the orbital charge distributions, bond lengths and bond populations is analyzed. The Li atom may promote the split of the energy band near the Fermi level and also may favorably regulate the diamond lattice distortion and expansion caused by the P atom.

  3. Enhanced field emission characteristics of boron doped diamond films grown by microwave plasma assisted chemical vapor deposition

    Energy Technology Data Exchange (ETDEWEB)

    Koinkar, Pankaj M. [Center for International Cooperation in Engineering Education (CICEE), University of Tokushima, 2-1 Minami-josanjima-cho, Tokushima 770-8506 (Japan); Patil, Sandip S. [Center for Advanced Studies in Materials Science and Condensed Matter Physics, Department of Physics, University of Pune, Pune 411007 (India); Kim, Tae-Gyu [Department of Nano System and Process Engineering, Pusan National University, 50 Cheonghak-ri, Samrangjin-eup, Miryang, Gyeongnam, Pusan 627-706 (Korea, Republic of); Yonekura, Daisuke [Department of Mechanical Engineering, University of Tokushima, 2-1 Minami-josanjima-cho, Tokushima 770-8506 (Japan); More, Mahendra A., E-mail: mam@physics.unipune.ac.in [Center for Advanced Studies in Materials Science and Condensed Matter Physics, Department of Physics, University of Pune, Pune 411007 (India); Joag, Dilip S. [Center for Advanced Studies in Materials Science and Condensed Matter Physics, Department of Physics, University of Pune, Pune 411007 (India); Murakami, Ri-ichi, E-mail: murakami@me.tokushima-u.ac.jp [Department of Mechanical Engineering, University of Tokushima, 2-1 Minami-josanjima-cho, Tokushima 770-8506 (Japan)

    2011-01-01

    Boron doped diamond films were synthesized on silicon substrates by microwave plasma chemical vapor deposition (MPCVD) technique. The effect of B{sub 2}O{sub 3} concentration varied from 1000 to 5000 ppm on the field emission characteristics was examined. The surface morphology and quality of films were characterized by scanning electron microscope (SEM) and Raman spectroscopy. The surface morphology obtained by SEM showed variation from facetted microcrystal covered with nanometric grains to cauliflower of nanocrystalline diamond (NCD) particles with increasing B{sub 2}O{sub 3} concentration. The Raman spectra confirm the formation of NCD films. The field emission properties of NCD films were observed to improve upon increasing boron concentration. The values of the onset field and threshold field are observed to be as low as 0.36 and 0.08 V/{mu}m, respectively. The field emission current stability investigated at the preset value of {approx}1 {mu}A is observed to be good, in each case. The enhanced field emission properties are attributed to the better electrical conductivity coupled with the nanometric features of the diamond films.

  4. Fluorine and boron co-doped diamond-like carbon films deposited by pulsed glow discharge plasma immersion ion processing

    CERN Document Server

    He, X M; Peters, A M; Taylor, B; Nastasi, M

    2002-01-01

    Fluorine (F) and boron (B) co-doped diamond-like carbon (FB-DLC) films were prepared on different substrates by the plasma immersion ion processing (PIIP) technique. A pulse glow discharge plasma was used for the PIIP deposition and was produced at a pressure of 1.33 Pa from acetylene (C sub 2 H sub 2), diborane (B sub 2 H sub 6), and hexafluoroethane (C sub 2 F sub 6) gas. Films of FB-DLC were deposited with different chemical compositions by varying the flow ratios of the C sub 2 H sub 2 , B sub 2 H sub 6 , and C sub 2 F sub 6 source gases. The incorporation of B sub 2 H sub 6 and C sub 2 F sub 6 into PIIP deposited DLC resulted in the formation of F-C and B-C hybridized bonding structures. The levels of the F and B concentrations effected the chemical bonding and the physical properties as was evident from the changes observed in density, hardness, stress, friction coefficient, and contact angle of water on films. Compared to B-doped or F-doped DLC films, the F and B co-doping of DLC during PIIP deposition...

  5. Concurrent doping effect of Ti and nano-diamond on flux pinning of MgB{sub 2}

    Energy Technology Data Exchange (ETDEWEB)

    Zhao, Y., E-mail: yzhao@swjtu.edu.c [Key Laboratory of Magnetic Levitation and Maglev Trains (Ministry of Education of China), Superconductivity R and D Center (SRDC), Mail Stop 165, Southwest Jiaotong University, Chengdu, Sichuan 610031 (China); Superconductivity Research Group, School of Materials Science and Engineering, University of New South Wales, Sydney, 2052 NSW (Australia); Ke, C. [Key Laboratory of Magnetic Levitation and Maglev Trains (Ministry of Education of China), Superconductivity R and D Center (SRDC), Mail Stop 165, Southwest Jiaotong University, Chengdu, Sichuan 610031 (China); Cheng, C.H. [Superconductivity Research Group, School of Materials Science and Engineering, University of New South Wales, Sydney, 2052 NSW (Australia); Feng, Y. [Northwest Institute for Nonferrous Metal Research, P.O. Box 51, Xian, Shaanxi 710016 (China); Western Superconductivity Technology Company, Xian (China); Yang, Y. [Key Laboratory of Magnetic Levitation and Maglev Trains (Ministry of Education of China), Superconductivity R and D Center (SRDC), Mail Stop 165, Southwest Jiaotong University, Chengdu, Sichuan 610031 (China); Munroe, P. [Superconductivity Research Group, School of Materials Science and Engineering, University of New South Wales, Sydney, 2052 NSW (Australia)

    2010-11-01

    Nano-diamond and titanium concurrently doped MgB{sub 2} nanocomposites have been prepared by solid state reaction method. The effects of carbon and Ti concurrent doping on J{sub c}-H behavior and pinning force scaling features of MgB{sub 2} have been investigated. Although T{sub c} was slightly depressed, J{sub c} of MgB{sub 2} have been significantly improved by the nano-diamond doping, especially in the high field region. In the mean time, the J{sub c} value in low field region is sustained though concurrent Ti doping. Microstructure analysis reveals that when nano-diamond was concurrently doped with titanium in MgB{sub 2}, a unique nanocomposite in which TiB{sub 2} forms a thin layer surrounding MgB{sub 2} grains whereas nano-diamond particles were wrapped inside the MgB{sub 2} grains. Besides, nano-diamond doping results in a high density stress field in the MgB{sub 2} samples, which may take responsibility for the {Delta}{kappa} pinning behavior in the carbon-doped MgB{sub 2} system.

  6. Electrochemical reactivity at graphitic micro-domains on polycrystalline boron doped diamond thin-films electrodes

    International Nuclear Information System (INIS)

    Mahe, E.; Devilliers, D.; Comninellis, Ch.

    2005-01-01

    This paper deals with the electrochemical reactivity of boron doped diamond (BDD) electrodes. A comparative study has been carried out to show the influence of the presence of graphitic micro-domains upon the surface of these films. Those graphitic domains are sometimes present on as-grown boron doped diamond electrodes. The effect of doping a pure Csp 3 diamond electrode is established by highly oriented pyrolytic graphite (HOPG) abrasion onto the diamond surface. In order to establish the effect of doping on a pure Csp 3 diamond electrode, the amount of graphitic domains was increased by means of HOPG crystals grafted onto the BDD surface. Indeed that method allows the enrichment of the Csp 2 contribution of the electrode. The presence of graphitic domains can be correlatively associated with the presence of kinetically active redox sites. The electrochemical reactivity of boron doped diamond electrodes shows a distribution of kinetic constants on the whole surface of the electrode corresponding to different active sites. In this paper, we have studied by cyclic voltammetry and electrochemical impedance spectroscopy the kinetics parameters of the ferri/ferrocyanide redox couple in KCl electrolyte. A method is proposed to diagnose the presence of graphitic domains on diamond electrodes, and an electrochemical 'pulse cleaning' procedure is proposed to remove them

  7. Hydrogen doped thin film diamond. Properties and application for electronic devices

    International Nuclear Information System (INIS)

    Looi, H.J.

    2000-01-01

    The face centered cubic allotrope of carbon, diamond, is a semiconducting material which possesses a valuable combination of extreme properties such as super-hardness, highest thermal conductivity, chemical hardness, radiation hardness, wide bandgap and others. Advances in chemical vapour deposition (CVD) technology have lead to diamond becoming available in previously unattainable forms for example over large areas and with controllable purity. This has generated much research interest towards developing the knowledge and processing technology that would be necessary to fully exploit these extreme properties. Electronic devices fabricated on oxidised boron doped polycrystalline CVD diamond (PCD) displayed very poor and inconsistent characteristic. As a result, many electronic applications of polycrystalline diamond films were confined to ultra-violet (UV) and other forms of device which relied on the high intrinsic resistivity on undoped diamond films. If commercially accessible PCD films are to advance in areas which involve sophisticated electronic applications or to compete with existing semiconductors, the need for a more reliable and fully ionised dopant is paramount. This thesis describes a unique dopant discovered within the growth surface of PCD films. This dopant is related to hydrogen which arises during the growth of diamond films. The aim of this study is to characterise and identify possible applications for this form of dopant. The mechanism for carrier generation remains unknown and based on the experimental results in this work, a model is proposed. The Hall measurements conducted on this conductive layer revealed a p-type nature with promising properties for electronic device application. A more detail study based on electrical and surface science methods were carried out to identify the stability and operating conditions for this dopant. The properties of metal-semiconductor contacts on these surfaces were investigated. The fundamental knowledge

  8. Electroluminescence Spectrum Shift with Switching Behaviour of Diamond Thin Films

    Institute of Scientific and Technical Information of China (English)

    王小平; 王丽军; 张启仁; 姚宁; 张兵临

    2003-01-01

    We report a special phenomenon on switching behaviour and the electroluminescence (EL) spectrum shift of doped diamond thin films. Nitrogen and cerium doped diamond thin films were deposited on a silicon substrate by microwave plasma-assisted chemical vapour deposition system and other special techniques. An EL device with a three-layer structure of nitrogen doped diamond/cerium doped diamond/SiO2 thin films was made. The EL device was driven by a direct-current power supply. Its EL character has been investigated, and a switching behaviour was observed. The EL light emission colour of diamond films changes from yellow (590nm) to blue (454 nm) while the switching behaviour appears.

  9. Electrochemical characterization of doped diamond-coated carbon fibers at different boron concentrations

    Energy Technology Data Exchange (ETDEWEB)

    Almeida, E.C. [INPE, CP 515, Sao Jose dos Campos, SP 12201-970 (Brazil)]. E-mail: erica@las.inpe.br; Diniz, A.V. [INPE, CP 515, Sao Jose dos Campos, SP 12201-970 (Brazil); Trava-Airoldi, V.J. [INPE, CP 515, Sao Jose dos Campos, SP 12201-970 (Brazil); Ferreira, N.G. [CTA-Divisao de Materiais, Sao Jose dos Campos, SP 12228-904 (Brazil)

    2005-08-01

    Doped diamond films have been deposited on carbon fibers (felt) obtained from polyacrylonitrile at different levels of boron doping. For a successful coating of the fibers, an ultrasonic pretreatment in a bath of diamond powder dissolved in hexane was required. Films were grown on both sample sides, simultaneously, by hot filament-assisted chemical vapour deposition technique at 750 deg. C from a 0.5% H{sub 2}/CH{sub 4} mixture at a total pressure of 6.5 x 10{sup 3} Pa. Boron was obtained from H{sub 2} forced to pass through a bubbler containing B{sub 2}O{sub 3} dissolved in methanol. The doping level studied corresponds to films with acceptor concentrations in the range of 6.5 x 10{sup 18} to 1.5 x 10{sup 21} cm{sup -} {sup 3}, obtained from Mott-Schottky plots. Scanning electron microscopy analyses evidenced fibers totally covered with high quality polycrystalline boron-doped diamond film, also confirmed by Raman spectroscopy spectra. Diamond electrodes grown on carbon fibers demonstrated similar electrochemical behavior obtained from films on Si substrate, for ferri/ferrocyanide redox couple as a function of boron content. The boron content influences electrochemical surface area. A lower boron concentration provides a higher growth rate that results in a higher surface area.

  10. Measurement of the magnetic penetration depth in p-doped superconducting diamond films

    Energy Technology Data Exchange (ETDEWEB)

    Fuchs, Lorenz; Brunner, Markus C.P.; Schneider, Ina; Kronfeldner, Klaus [University of Regensburg (Germany); Bousquet, Jessica; Bustarret, Etienne; Strunk, Christoph [Institut Neel, Grenoble (France)

    2016-07-01

    Boron-doped diamond becomes superconducting once a critical doping concentration of 4.5 x 10{sup 20} cm{sup -3} is reached. Mutual inductance measurements with a two-coil setup have been performed to determine the magnetic penetration depth λ(T), which is a measure for the superfluid stiffnes θ ∝ 1/λ{sup 2}(T). Two superconducting p-doped diamond films with thicknesses of 145 nm and 345 nm were investigated. At low temperatures these values agree reasonably with the values expected within BCS-theory using T{sub c}, carrier density and mean free path determined from electric transport measurements. Magnetic penetration depths of 3.7 μm for the thinner and 2.6 μm for the thicker film have been found. λ decreases and accordingly θ increases with increasing film thickness. On the other hand, the superfluid stiffness drops by a factor of 2 or even more at T{sub c}/2, i.e., much faster than expected from BCS-theory, but remains finite between T{sub c}/2 < T < T{sub c}. At present it is unclear, whether this behavior results from the proliferation of phase fluctuations already far below T{sub c} or from a spatial inhomogeneity of the films.

  11. Electrochemical reactivity at graphitic micro-domains on polycrystalline boron doped diamond thin-films electrodes

    Energy Technology Data Exchange (ETDEWEB)

    Mahe, E. [LI2C CNRS/UMR 7612, Laboratoire d' Electrochimie, Universite Pierre-et-Marie Curie - case courrier 51, 4, Place Jussieu, 75252 Paris Cedex 05 (France); Devilliers, D. [LI2C CNRS/UMR 7612, Laboratoire d' Electrochimie, Universite Pierre-et-Marie Curie - case courrier 51, 4, Place Jussieu, 75252 Paris Cedex 05 (France); Comninellis, Ch. [Unite de Genie Electrochimique, Institut de sciences des procedes chimiques et biologiques, Ecole Polytechnique Federale de Lausanne, 1015, Lausanne (Switzerland)

    2005-04-01

    This paper deals with the electrochemical reactivity of boron doped diamond (BDD) electrodes. A comparative study has been carried out to show the influence of the presence of graphitic micro-domains upon the surface of these films. Those graphitic domains are sometimes present on as-grown boron doped diamond electrodes. The effect of doping a pure Csp{sup 3} diamond electrode is established by highly oriented pyrolytic graphite (HOPG) abrasion onto the diamond surface. In order to establish the effect of doping on a pure Csp{sup 3} diamond electrode, the amount of graphitic domains was increased by means of HOPG crystals grafted onto the BDD surface. Indeed that method allows the enrichment of the Csp{sup 2} contribution of the electrode. The presence of graphitic domains can be correlatively associated with the presence of kinetically active redox sites. The electrochemical reactivity of boron doped diamond electrodes shows a distribution of kinetic constants on the whole surface of the electrode corresponding to different active sites. In this paper, we have studied by cyclic voltammetry and electrochemical impedance spectroscopy the kinetics parameters of the ferri/ferrocyanide redox couple in KCl electrolyte. A method is proposed to diagnose the presence of graphitic domains on diamond electrodes, and an electrochemical 'pulse cleaning' procedure is proposed to remove them.

  12. Electrical current at micro-/macro-scale of undoped and nitrogen-doped MWPECVD diamond films

    Science.gov (United States)

    Cicala, G.; Velardi, L.; Senesi, G. S.; Picca, R. A.; Cioffi, N.

    2017-12-01

    Chemical, structural, morphological and micro-/macro-electrical properties of undoped and nitrogen-(N-)doped diamond films are determined by X-ray photoelectron spectroscopy, Raman and photoluminescence spectroscopies, field emission scanning electron microscopy, atomic force microscopy, scanning capacitance microscopy (SCM) and two points technique for I-V characteristics, respectively. The characterization results are very useful to examine and understand the relationship among these properties. The effect of the nitrogen incorporation in diamond films is investigated through the evolution of the chemical, structural, morphological and topographical features and of the electrical behavior. The distribution of the electrical current is first assessed at millimeter scale on the surface of diamond films and then at micrometer scale on small regions in order to establish the sites where the carriers preferentially move. Specifically, the SCM images indicate a non-uniform distribution of carriers on the morphological structures mainly located along the grain boundaries. A good agreement is found by comparing the electrical currents at the micro- and macro-scale. This work aims to highlight phenomena such as photo- and thermionic emission from N-doped diamond useful for microelectronic engineering.

  13. Electronic structure of B-doped diamond: A first-principles study

    Directory of Open Access Journals (Sweden)

    T. Oguchi

    2006-01-01

    Full Text Available Electronic structure of B-doped diamond is studied based on first-principles calculations with supercell models for substitutional and interstitial doping at 1.5–3.1 at.% B concentrations. Substitutional doping induces holes around the valence-band maximum in a rigid-band fashion. The nearest neighbor C site to B shows a large energy shift of 1s core state, which may explain reasonably experimental features in recent photoemission and X-ray absorption spectra. Doping at interstitial Td site is found to be unstable compared with that at the substitutional site

  14. Multiple delta doping of single crystal cubic boron nitride films heteroepitaxially grown on (001)diamonds

    Science.gov (United States)

    Yin, H.; Ziemann, P.

    2014-06-01

    Phase pure cubic boron nitride (c-BN) films have been epitaxially grown on (001) diamond substrates at 900 °C. The n-type doping of c-BN epitaxial films relies on the sequential growth of nominally undoped (p-) and Si doped (n-) layers with well-controlled thickness (down to several nanometer range) in the concept of multiple delta doping. The existence of nominally undoped c-BN overgrowth separates the Si doped layers, preventing Si dopant segregation that was observed for continuously doped epitaxial c-BN films. This strategy allows doping of c-BN films can be scaled up to multiple numbers of doped layers through atomic level control of the interface in the future electronic devices. Enhanced electronic transport properties with higher hall mobility (102 cm2/V s) have been demonstrated at room temperature as compared to the normally continuously Si doped c-BN films.

  15. Investigation of Physical Properties and Electrochemical Behavior of Nitrogen-Doped Diamond-Like Carbon Thin Films

    Directory of Open Access Journals (Sweden)

    Rattanakorn Saensak

    2014-03-01

    Full Text Available This work reports characterizations of diamond-like carbon (DLC films used as electrodes for electrochemical applications. DLC thin films are prepared on glass slides and silicon substrates by radio frequency plasma enhanced chemical vapor deposition (RF-PECVD using a gas mixture of methane and hydrogen. In addition, the DLC films are doped with nitrogen in order to reduce electrical resistivity. Compared to the undoped DLC films, the electrical resistivity of nitrogen-doped (N-doped DLC films is decreased by three orders of magnitude. Raman spectroscopy and UV/Vis spectroscopy analyses show the structural transformation in N-doped DLC films that causes the reduction of band gap energy. Contact angle measurement at N-doped DLC films indicates increased hydrophobicity. The results obtained from the cyclic voltammetry measurements with Fe(CN63-/Fe(CN64- redox species exhibit the correlation between the physical properties and electrochemical behavior of DLC films.

  16. Optical and electrical properties of boron doped diamond thin conductive films deposited on fused silica glass substrates

    Energy Technology Data Exchange (ETDEWEB)

    Ficek, M.; Sobaszek, M.; Gnyba, M. [Department of Metrology and Optoelectronics, Gdansk University of Technology, 11/12G. Narutowicza St., 80-233 Gdansk (Poland); Ryl, J. [Department of Electrochemistry, Corrosion and Material Engineering, Gdansk University of Technology, 11/12 Narutowicza St., 80-233 Gdansk (Poland); Gołuński, Ł. [Department of Metrology and Optoelectronics, Gdansk University of Technology, 11/12G. Narutowicza St., 80-233 Gdansk (Poland); Smietana, M.; Jasiński, J. [Institute of Microelectronics and Optoelectronics, Warsaw University of Technology, 75 Koszykowa St., 00-662 Warsaw (Poland); Caban, P. [Institute of Electronic Materials Technology, 133 Wolczynska St., 01-919 Warsaw (Poland); Bogdanowicz, R., E-mail: rbogdan@eti.pg.gda.pl [Department of Metrology and Optoelectronics, Gdansk University of Technology, 11/12G. Narutowicza St., 80-233 Gdansk (Poland); Materials and Process Simulation Center, California Institute of Technology, Pasadena, CA 91125 (United States)

    2016-11-30

    Highlights: • Growth of 60% of transmittance diamond films with resistivity as low as 48 Ω cm. • Two step seeding process of fused silica: plasma hydrogenation and wet seeding. • Nanodiamond seeding density of 2 × 10{sup 10} cm{sup −2} at fused silica substrates. • High refractive index (2.4 @550 nm) was achieved for BDD films deposited at 500 °C. - Abstract: This paper presents boron-doped diamond (BDD) film as a conductive coating for optical and electronic purposes. Seeding and growth processes of thin diamond films on fused silica have been investigated. Growth processes of thin diamond films on fused silica were investigated at various boron doping level and methane admixture. Two step pre-treatment procedure of fused silica substrate was applied to achieve high seeding density. First, the substrates undergo the hydrogen plasma treatment then spin-coating seeding using a dispersion consisting of detonation nanodiamond in dimethyl sulfoxide with polyvinyl alcohol was applied. Such an approach results in seeding density of 2 × 10{sup 10} cm{sup −2}. The scanning electron microscopy images showed homogenous, continuous and polycrystalline surface morphology with minimal grain size of 200 nm for highly boron doped films. The sp{sup 3}/sp{sup 2} ratio was calculated using Raman spectra deconvolution method. A high refractive index (range of 2.0–2.4 @550 nm) was achieved for BDD films deposited at 500 °C. The values of extinction coefficient were below 0.1 at λ = 550 nm, indicating low absorption of the film. The fabricated BDD thin films displayed resistivity below 48 Ohm cm and transmittance over 60% in the visible wavelength range.

  17. Comparison between nano-diamond and carbon nanotube doping effects on critical current density and flux pinning in MgB2

    International Nuclear Information System (INIS)

    Cheng, C H; Yang, Y; Munroe, P; Zhao, Y

    2007-01-01

    Doping effects of nano-diamond and carbon nanotubes (CNTs) on critical current density of bulk MgB 2 have been studied. CNTs are found prone to be doped into the MgB 2 lattice whereas nano-diamond tends to form second-phase inclusions in the MgB 2 matrix, leading to a more significant improvement of J c (H) by doping by nano-diamond than by CNTs in MgB 2 . TEM reveals tightly packed MgB 2 nanograins (50-100 nm) with a dense distribution of diamond nanoparticles (10-20 nm) inside MgB 2 grains in nano-diamond-doped samples. Such a unique microstructure leads to a flux pinning behaviour different from that in CNTs-doped MgB 2

  18. Investigation of corrosion behavior of nitrogen doped and platinum/ruthenium doped diamond-like carbon thin films in Hank's solution

    International Nuclear Information System (INIS)

    Khun, N.W.; Liu, E.

    2011-01-01

    Undoped (DLC), nitrogen-doped (N-DLC) and platinum/ruthenium doped diamond-like carbon (PtRu-DLC) thin films were deposited on p-Si (100) substrates using a DC magnetron sputtering deposition system. The chemical composition, bonding structure, surface morphology and adhesion strength of the films were characterized using X-ray photoelectron spectroscopy (XPS), micro-Raman spectroscopy, atomic force microscopy (AFM) and micro-scratch test, respectively. The corrosion behavior of the films in a Hank's solution was investigated using potentiodynamic polarization test. The corrosion results revealed that the PtRu-DLC film had the highest corrosion potential among the films used in this study. Highlights: → DLC thin films were deposited on Si substrates via dc magnetron sputtering. → Some DLC films were doped with N and/or Pt/Ru. → The film corrosion behavior was studied in a Hank solution with polarization test. → The PtRu-DLC film showed the highest corrosion potential among the films studied.

  19. Electronic structures of B 2p and C 2p levels in boron-doped diamond films studied using soft x-ray absorption and emission spectroscopy

    Science.gov (United States)

    Nakamura, Jin; Kabasawa, Eiki; Yamada, Nobuyoshi; Einaga, Yasuaki; Saito, Daisuke; Isshiki, Hideo; Yugo, Shigemi; Perera, Rupert C. C.

    2004-12-01

    X-ray absorption (XAS) and emission (XES) spectroscopy near B K and C K edges have been performed on metallic ( ˜0.1at.% B, B-diamond) and semiconducting ( ˜0.03at.% B and N, BN-diamond) doped diamond films. Both B K XAS and XES spectra show a metallic partial density of states (PDOS) with the Fermi energy of 185.3eV , and there is no apparent boron-concentration dependence in contrast to the different electric property. In C K XAS spectrum of B-diamond, the impurity state ascribed to boron is clearly observed near the Fermi level. The Fermi energy is found to be almost same with the top of the valence band of nondoped diamond: EV=283.9eV . C K XAS of BN-diamond shows both the B-induced shallow level and N-induced deep and broad levels as the in-gap states, in which the shallow level is in good agreement with the activation energy (Ea=0.37eV) estimated from the temperature dependence of the conductivity; namely, the change in C2p PDOS of impurity-induced metallization is directly observed. The electric property of this diamond is ascribed mainly to the electronic structure of C2p near the Fermi level. The observed XES spectra are compared with the discrete variational Xα ( DVXα ) cluster calculation. The DVXα result supports the strong hybridization between B2p and C2p observed in XAS and XES spectra, and suggests that the small amount of boron (⩽0.1at.%) in diamond occupies the substitutional site rather than interstitial site.

  20. Dependence of reaction pressure on deposition and properties of boron-doped freestanding diamond films

    International Nuclear Information System (INIS)

    Li Liuan; Li Hongdong; Lue Xianyi; Cheng Shaoheng; Wang Qiliang; Ren Shiyuan; Liu Junwei; Zou Guangtian

    2010-01-01

    In this paper, we investigate the reaction pressure-dependent growth and properties of boron-doped freestanding diamond films, synthesized by hot filament chemical vapor deposition (HFCVD) at different boron-doping levels. With the decrease in pressure, the growth feature of the films varies from mixed [1 1 1] and [1 1 0] to dominated [1 1 1] texture. The low reaction pressure, as well as high boron-doping level, results in the increase (decrease) of carrier concentration (resistivity). The high concentration of atomic hydrogen in the ambient and preferable [1 1 1] growth, due to the low reaction pressure, is available for the enhancement of boron doping. The estimated residual stress increases with increase in the introducing boron level.

  1. Single-layer nano-carbon film, diamond film, and diamond/nano-carbon composite film field emission performance comparison

    International Nuclear Information System (INIS)

    Wang, Xiaoping; Wang, Jinye; Wang, Lijun

    2016-01-01

    A series of single-layer nano-carbon (SNC) films, diamond films, and diamond/nano-carbon (D/NC) composite films have been prepared on the highly doped silicon substrate by using microwave plasma chemical vapor deposition techniques. The films were characterised by scanning electron microscopy, Raman spectroscopy, and field emission I-V measurements. The experimental results indicated that the field emission maximum current density of D/NC composite films is 11.8–17.8 times that of diamond films. And the field emission current density of D/NC composite films is 2.9–5 times that of SNC films at an electric field of 3.0 V/μm. At the same time, the D/NC composite film exhibits the advantage of improved reproducibility and long term stability (both of the nano-carbon film within the D/NC composite cathode and the SNC cathode were prepared under the same experimental conditions). And for the D/NC composite sample, a high current density of 10 mA/cm"2 at an electric field of 3.0 V/μm was obtained. Diamond layer can effectively improve the field emission characteristics of nano-carbon film. The reason may be due to the diamond film acts as the electron acceleration layer.

  2. The processing of heteroepitaxial thin-film diamond for electronic applications

    International Nuclear Information System (INIS)

    McGrath, J.

    1998-09-01

    Thin film diamond is of particular interest because of its wide applicability, including its potential use in high temperature electronics. This thesis describes a study of some of the processing stages required to exploit thin film diamond as an electronic device. Initial experiments were carried out to optimise bi-metallic contact schemes on orientated diamond film using electrical measurements and chemical analysis. Temperature stability was also investigated and it was concluded that the most favourable ohmic contact scheme is aluminium-on-titanium. Further electrical measurements confirmed that the contribution of resistance made by the contacts themselves to the metal/diamond/metal system overall was acceptably low, specifically 6 Ω.cm 2 for an undoped diamond system and less than 3 x 10 -6 Ω.cm 2 for boron doped diamond. To improve the as-grown resistivity of diamond films, an oxygen/argon plasma etch process was applied. The input parameters of the plasma system were optimised to give the maximum achievable resistivity of 4 x 10 11 Ω.cm. This was attained using a statistical design procedure via analysis of resistivity and etch rate outputs. Having optimised post growth treatment and contact metallisation, undoped and doped orientated diamond films were characterised via voltage and temperature dependencies. It was concluded that the dominant charge transport mechanisms for undoped diamond, nitrogen and boron doped diamond were variable range hopping at low temperatures up to 523 K and grain boundary effects. At higher temperatures, valence or impurity band conduction appeared to be the probable mechanisms with activation energies of 0.23 eV for nitrogen doped diamond and 0.08 eV for boron doped diamond. Preliminary experiments electrical properties of diamond and initial results suggested the presence of a high density of recombination centres. The final stage of experimental research initiated a study of direct electron beam writing lithography to

  3. Investigation of corrosion behavior of nitrogen doped and platinum/ruthenium doped diamond-like carbon thin films in Hank's solution

    Energy Technology Data Exchange (ETDEWEB)

    Khun, N.W.; Liu, E., E-mail: MEJLiu@ntu.edu.sg

    2011-10-10

    Undoped (DLC), nitrogen-doped (N-DLC) and platinum/ruthenium doped diamond-like carbon (PtRu-DLC) thin films were deposited on p-Si (100) substrates using a DC magnetron sputtering deposition system. The chemical composition, bonding structure, surface morphology and adhesion strength of the films were characterized using X-ray photoelectron spectroscopy (XPS), micro-Raman spectroscopy, atomic force microscopy (AFM) and micro-scratch test, respectively. The corrosion behavior of the films in a Hank's solution was investigated using potentiodynamic polarization test. The corrosion results revealed that the PtRu-DLC film had the highest corrosion potential among the films used in this study. Highlights: {yields} DLC thin films were deposited on Si substrates via dc magnetron sputtering. {yields} Some DLC films were doped with N and/or Pt/Ru. {yields} The film corrosion behavior was studied in a Hank solution with polarization test. {yields} The PtRu-DLC film showed the highest corrosion potential among the films studied.

  4. Iron, nitrogen and silicon doped diamond like carbon (DLC) thin films: A comparative study

    International Nuclear Information System (INIS)

    Ray, Sekhar C.; Pong, W.F.; Papakonstantinou, P.

    2016-01-01

    The X-ray absorption near edge structure (XANES), X-ray photoelectron spectroscopy (XPS), valence band photoemission (VB-PES) and Raman spectroscopy results show that the incorporation of nitrogen in pulsed laser deposited diamond like carbon (DLC) thin films, reverts the sp"3 network to sp"2 as evidenced by an increase of the sp"2 cluster and I_D/I_G ratio in C K-edge XANES and Raman spectra respectively which reduces the hardness/Young's modulus into the film network. Si-doped DLC film deposited in a plasma enhanced chemical vapour deposition process reduces the sp"2 cluster and I_D/I_G ratio that causes the decrease of hardness/Young's modulus of the film structure. The Fe-doped DLC films deposited by dip coating technique increase the hardness/Young's modulus with an increase of sp"3-content in DLC film structure. - Highlights: • Fe, N and Si doped DLC films deposited by dip, PLD and PECVD methods respectively • DLC:Fe thin films have higher hardness/Young's modulus than DLC:N(:Si) thin films. • sp"3 and sp"2 contents are estimated from C K-edge XANES and VB-PES measurements.

  5. Iron, nitrogen and silicon doped diamond like carbon (DLC) thin films: A comparative study

    Energy Technology Data Exchange (ETDEWEB)

    Ray, Sekhar C., E-mail: Raysc@unisa.ac.za [Department of Physics, College of Science, Engineering and Technology, University of South Africa, Private Bag X6, Florida, 1710, Science Campus, Christiaan de Wet and Pioneer Avenue, Florida Park, Johannesburg (South Africa); Pong, W.F. [Department of Physics, Tamkang University, Tamsui 251, New Taipei City, Taiwan (China); Papakonstantinou, P. [Nanotechnology and Integrated Bio-Engineering Centre, University of Ulster, Shore Road, Newtownabbey BT37 0QB (United Kingdom)

    2016-07-01

    The X-ray absorption near edge structure (XANES), X-ray photoelectron spectroscopy (XPS), valence band photoemission (VB-PES) and Raman spectroscopy results show that the incorporation of nitrogen in pulsed laser deposited diamond like carbon (DLC) thin films, reverts the sp{sup 3} network to sp{sup 2} as evidenced by an increase of the sp{sup 2} cluster and I{sub D}/I{sub G} ratio in C K-edge XANES and Raman spectra respectively which reduces the hardness/Young's modulus into the film network. Si-doped DLC film deposited in a plasma enhanced chemical vapour deposition process reduces the sp{sup 2} cluster and I{sub D}/I{sub G} ratio that causes the decrease of hardness/Young's modulus of the film structure. The Fe-doped DLC films deposited by dip coating technique increase the hardness/Young's modulus with an increase of sp{sup 3}-content in DLC film structure. - Highlights: • Fe, N and Si doped DLC films deposited by dip, PLD and PECVD methods respectively • DLC:Fe thin films have higher hardness/Young's modulus than DLC:N(:Si) thin films. • sp{sup 3} and sp{sup 2} contents are estimated from C K-edge XANES and VB-PES measurements.

  6. Morphological and electrochemical studies of spherical boron doped diamond electrodes

    Energy Technology Data Exchange (ETDEWEB)

    Mendes de Barros, R.C. [IQ/USP, Av. Lineu Prestes, 748, Bloco 2 Superior, Cidade Universitaria, Sao Paulo/SP, 05508-900 (Brazil); Ferreira, N.G. [LAS/INPE, Av. dos Astronautas, 1758, Jardim da Granja, Sao Jose dos Campos/SP, 12245-970 (Brazil); Azevedo, A.F. [LAS/INPE, Av. dos Astronautas, 1758, Jardim da Granja, Sao Jose dos Campos/SP, 12245-970 (Brazil); Corat, E.J. [LAS/INPE, Av. dos Astronautas, 1758, Jardim da Granja, Sao Jose dos Campos/SP, 12245-970 (Brazil); Sumodjo, P.T.A. [IQ/USP, Av. Lineu Prestes, 748, Bloco 2 Superior, Cidade Universitaria, Sao Paulo/SP, 05508-900 (Brazil); Serrano, S.H.P. [IQ/USP, Av. Lineu Prestes, 748, Bloco 2 Superior, Cidade Universitaria, Sao Paulo/SP, 05508-900 (Brazil)]. E-mail: shps@iq.usp.br

    2006-08-14

    Morphological and electrochemical characteristics of boron doped diamond electrode in new geometric shape are presented. The main purpose of this study is a comparison among voltammetric behavior of planar glassy carbon electrode (GCE), planar boron doped diamond electrode (PDDE) and spherical boron doped diamond electrode (SDDE), obtained from similar experimental parameters. SDDE was obtained by the growth of boron doped film on textured molybdenum tip. This electrode does not present microelectrode characteristics. However, its voltammetric peak current, determined at low scan rates, is largest associated to the smallest {delta}E {sub p} values for ferrocyanide system when compared with PDDE or GCE. In addition, the capacitance is about 200 times smaller than that for GCE. These results show that the analytical performance of boron doped diamond electrodes can be implemented just by the change of sensor geometry, from plane to spherical shape.

  7. Possible observation of the Berezinskii-Kosterlitz-Thouless transition in boron-doped diamond films

    Science.gov (United States)

    Coleman, Christopher; Bhattacharyya, Somnath

    2017-11-01

    The occurrence of the Berezinskii-Kosterlitz-Thouless (BKT) transition is investigated in heavily boron-doped nanocrystalline diamond films through a combination of current-voltage and resistance measurements. We observe transport features suggesting a robust BKT transition along with transport features related to vortex pinning in nanocrystalline diamond films with smaller grain size. The vortex core energy determined through analysis of the resistance temperature curves was found to be anti-correlated to the BKT transition temperatures. It is also observed that the higher BKT temperature is related to an increased vortex-antivortex binding energy derived from the activated transport regions. Further, the magnetic field induced superconductor insulator transition shows the possibility of the charge glass state. The consequences of granularity such as localization and vortex pinning can lead to tuneable BKT temperatures and strongly affects the field induced insulating state.

  8. Boron-doped diamond electrode: synthesis, characterization, functionalization and analytical applications.

    Science.gov (United States)

    Luong, John H T; Male, Keith B; Glennon, Jeremy D

    2009-10-01

    In recent years, conductive diamond electrodes for electrochemical applications have been a major focus of research and development. The impetus behind such endeavors could be attributed to their wide potential window, low background current, chemical inertness, and mechanical durability. Several analytes can be oxidized by conducting diamond compared to other carbon-based materials before the breakdown of water in aqueous electrolytes. This is important for detecting and/or identifying species in solution since oxygen and hydrogen evolution do not interfere with the analysis. Thus, conductive diamond electrodes take electrochemical detection into new areas and extend their usefulness to analytes which are not feasible with conventional electrode materials. Different types of diamond electrodes, polycrystalline, microcrystalline, nanocrystalline and ultrananocrystalline, have been synthesized and characterized. Of particular interest is the synthesis of boron-doped diamond (BDD) films by chemical vapor deposition on various substrates. In the tetrahedral diamond lattice, each carbon atom is covalently bonded to its neighbors forming an extremely robust crystalline structure. Some carbon atoms in the lattice are substituted with boron to provide electrical conductivity. Modification strategies of doped diamond electrodes with metallic nanoparticles and/or electropolymerized films are of importance to impart novel characteristics or to improve the performance of diamond electrodes. Biofunctionalization of diamond films is also feasible to foster several useful bioanalytical applications. A plethora of opportunities for nanoscale analytical devices based on conducting diamond is anticipated in the very near future.

  9. Investigation of low-resistivity from hydrogenated lightly B-doped diamond by ion implantation

    Directory of Open Access Journals (Sweden)

    Cui Xia Yan et al

    2008-01-01

    Full Text Available We have implanted boron (B ions (dosage: 5×1014 cm-2 into diamond and then hydrogenated the sample by implantating hydrogen ions at room temperature. A p-type diamond material with a low resistivity of 7.37 mΩ cm has been obtained in our experiment, which suggests that the hydrogenation of B-doped diamond results in a low-resistivity p-type material. Interestingly, inverse annealing, in which carrier concentration decreased with increasing annealing temperature, was observed at annealing temperatures above 600 °C. In addition, the formation mechanism of a low-resistivity material has been studied by density functional theory calculation using a plane wave method.

  10. Understanding anodic wear at boron doped diamond film electrodes

    International Nuclear Information System (INIS)

    Chaplin, Brian P.; Hubler, David K.; Farrell, James

    2013-01-01

    This research investigated the mechanisms associated with anodic wear of boron-doped diamond (BDD) film electrodes. Cyclic voltammetry (CV), x-ray photoelectron spectroscopy (XPS), scanning electron microscopy (SEM), and electrochemical impedance spectroscopy (EIS) were used to measure changes in electrode response and surface chemistry as a function of the charge passed and applied current density. Density functional theory (DFT) modeling was used to evaluate possible reaction mechanisms. The initial hydrogen-terminated surface was electrochemically oxidized at lower potentials than water oxidation (≤ 1.83 V/SHE), and was not catalyzed by the hydrogen-terminated surface. In the region where water oxidation produces hydroxyl radicals (OH·), the hydrogen-terminated surface may also be oxidized by chemical reaction with OH·. Oxygen atoms became incorporated into the surface via reaction of carbon atoms with OH·, forming both C = O and C-OH functional groups, that were also detected by XPS measurements. Experimental and DFT modeling results indicate that the oxygenated diamond surface lowers the potential for activationless water oxidation from 2.74 V/SHE for the hydrogen terminated surface to 2.29 V/SHE for the oxygenated surface. Electrode wear was accelerated at high current densities (i.e., 500 mA cm −2 ), where SEM results indicated oxidation of the BDD film resulted in significant surface roughening. These results are supported by EIS measurements that document an increase in the double-layer capacitance as a function of the charge passed. DFT simulations provide a possible mechanism that explains the observed diamond oxidation. DFT simulation results indicate that BDD edge sites (=CH 2 ) can be converted to COOH functional groups, which are further oxidized via reactions with OH· to form H 2 CO 3(aq.) with an activation energy of 58.9 kJ mol −1

  11. Gas Permeation, Mechanical Behavior and Cytocompatibility of Ultrathin Pure and Doped Diamond-Like Carbon and Silicon Oxide Films

    Directory of Open Access Journals (Sweden)

    Juergen M. Lackner

    2013-12-01

    Full Text Available Protective ultra-thin barrier films gather increasing economic interest for controlling permeation and diffusion from the biological surrounding in implanted sensor and electronic devices in future medicine. Thus, the aim of this work was a benchmarking of the mechanical oxygen permeation barrier, cytocompatibility, and microbiological properties of inorganic ~25 nm thin films, deposited by vacuum deposition techniques on 50 µm thin polyetheretherketone (PEEK foils. Plasma-activated chemical vapor deposition (direct deposition from an ion source was applied to deposit pure and nitrogen doped diamond-like carbon films, while physical vapor deposition (magnetron sputtering in pulsed DC mode was used for the formation of silicon as well as titanium doped diamond-like carbon films. Silicon oxide films were deposited by radio frequency magnetron sputtering. The results indicate a strong influence of nanoporosity on the oxygen transmission rate for all coating types, while the low content of microporosity (particulates, etc. is shown to be of lesser importance. Due to the low thickness of the foil substrates, being easily bent, the toughness as a measure of tendency to film fracture together with the elasticity index of the thin films influence the oxygen barrier. All investigated coatings are non-pyrogenic, cause no cytotoxic effects and do not influence bacterial growth.

  12. Laser-excited photoemission spectroscopy study of superconducting boron-doped diamond

    Directory of Open Access Journals (Sweden)

    K. Ishizaka, R. Eguchi, S. Tsuda, T. Kiss, T. Shimojima, T. Yokoya, S. Shin, T. Togashi, S. Watanabe, C.-T. Chen, C.Q. Zhang, Y. Takano, M. Nagao, I. Sakaguchi, T. Takenouchi and H. Kawarada

    2006-01-01

    Full Text Available We have investigated the low-energy electronic state of boron-doped diamond thin film by the laser-excited photoemission spectroscopy. A clear Fermi-edge is observed for samples doped above the semiconductor–metal boundary, together with the characteristic structures at 150×n meV possibly due to the strong electron–lattice coupling effect. In addition, for the superconducting sample, we observed a shift of the leading edge below Tc indicative of a superconducting gap opening. We discuss the electron–lattice coupling and the superconductivity in doped diamond.

  13. Improved stability of titanium based boron-doped chemical vapor deposited diamond thin-film electrode by modifying titanium substrate surface

    International Nuclear Information System (INIS)

    Lim, P.Y.; Lin, F.Y.; Shih, H.C.; Ralchenko, V.G.; Varnin, V.P.; Pleskov, Yu.V.; Hsu, S.F.; Chou, S.S.; Hsu, P.L.

    2008-01-01

    The film quality and electrochemical properties of BDD (boron-doped diamond) thin films grown by hot-filament chemical vapor deposition technique on titanium substrates that had been subjected to a range of pre-treatment processes were evaluated. The pre-roughened Ti-substrates are shown to support more adherent BDD films. It is evident that acid-etching the Ti-substrate involves surface hydrogenation that enhances nucleation and formation of diamond thereon. The prepared BDD film exhibits wide potential window and electrochemical reversibility. It also demonstrated a better long-term electrochemical stability based on the low variation in voltametric background current upon the exposing of the electrodes to repeated cycles of electrochemical metal deposition/stripping process

  14. Properties of planar structures based on Policluster films of diamond and AlN

    Science.gov (United States)

    Belyanin, A. F.; Luchnikov, A. P.; Nalimov, S. A.; Bagdasarian, A. S.

    2018-01-01

    AlN films doped with zinc were grown on Si substrates by RF magnetron reactive sputtering of a compound target. Policluster films of diamond doped with boron were formed on layered Si/AlN substrates from the gas phase hydrogen and methane, activated arc discharge. By electron microscopy, X-ray diffraction and Raman spectroscopy the composition and structure of synthetic policluster films of diamond and AlN films were studied. Photovoltaic devices based on the AlN/PFD layered structure are presented.

  15. Boron Doped diamond films as electron donors in photovoltaics: An X-ray absorption and hard X-ray photoemission study

    Energy Technology Data Exchange (ETDEWEB)

    Kapilashrami, M.; Zegkinoglou, I. [Advanced Light Source, Lawrence Berkeley National Laboratory, Berkeley, California 94720 (United States); Department of Physics, University of Wisconsin Madison, Madison, Wisconsin 53706 (United States); Conti, G.; Nemšák, S.; Conlon, C. S.; Fadley, C. S. [Department of Physics, University of California, Davis, California 95616 (United States); Materials Sciences Division, Lawrence Berkeley National Laboratory, Berkeley, California 94720 (United States); Törndahl, T.; Fjällström, V. [Ångström Solar Center, Uppsala University, Box 534, SE-751 21 Uppsala (Sweden); Lischner, J. [Department of Physics, University of California, Berkeley, California 94720 (United States); Louie, Steven G. [Materials Sciences Division, Lawrence Berkeley National Laboratory, Berkeley, California 94720 (United States); Department of Physics, University of California, Berkeley, California 94720 (United States); Hamers, R. J.; Zhang, L. [Department of Chemistry, University of Wisconsin Madison, Madison, Wisconsin 53706 (United States); Guo, J.-H. [Advanced Light Source, Lawrence Berkeley National Laboratory, Berkeley, California 94720 (United States); Himpsel, F. J., E-mail: fhimpsel@wisc.edu [Department of Physics, University of Wisconsin Madison, Madison, Wisconsin 53706 (United States)

    2014-10-14

    Highly boron-doped diamond films are investigated for their potential as transparent electron donors in solar cells. Specifically, the valence band offset between a diamond film (as electron donor) and Cu(In,Ga)Se₂ (CIGS) as light absorber is determined by a combination of soft X-ray absorption spectroscopy and hard X-ray photoelectron spectroscopy, which is more depth-penetrating than standard soft X-ray photoelectron spectroscopy. In addition, a theoretical analysis of the valence band is performed, based on GW quasiparticle band calculations. The valence band offset is found to be small: VBO=VBM{sub CIGS} – VBM{sub diamond}=0.3 eV±0.1 eV at the CIGS/Diamond interface and 0.0 eV±0.1 eV from CIGS to bulk diamond. These results provide a promising starting point for optimizing the band offset by choosing absorber materials with a slightly lower valence band maximum.

  16. Boron Doped Nanocrystalline Diamond Films for Biosensing Applications

    Directory of Open Access Journals (Sweden)

    V. Petrák

    2011-01-01

    Full Text Available With the rise of antibiotic resistance of pathogenic bacteria there is an increased demand for monitoring the functionality of bacteria membranes, the disruption of which can be induced by peptide-lipid interactions. In this work we attempt to construct and disrupt supported lipid membranes (SLB on boron doped nanocrystalline diamond (B-NCD. Electrochemical Impedance Spectroscopy (EIS was used to study in situ changes related to lipid membrane formation and disruption by peptide-induced interactions. The observed impedance changes were minimal for oxidized B-NCD samples, but were still detectable in the low frequency part of the spectra. The sensitivity for the detection of membrane formation and disruption was significantly higher for hydrogenated B-NCD surfaces. Data modeling indicates large changes in the electrical charge when an electrical double layer is formed at the B-NCD/SLB interface, governed by ion absorption. By contrast, for oxidized B-NCD surfaces, these changes are negligible indicating little or no change in the surface band bending profile.

  17. Rhenium Alloys as Ductile Substrates for Diamond Thin-Film Electrodes.

    Science.gov (United States)

    Halpern, Jeffrey M; Martin, Heidi B

    2014-02-01

    Molybdenum-rhenium (Mo/Re) and tungsten-rhenium (W/Re) alloys were investigated as substrates for thin-film, polycrystalline boron-doped diamond electrodes. Traditional, carbide-forming metal substrates adhere strongly to diamond but lose their ductility during exposure to the high-temperature (1000°C) diamond, chemical vapor deposition environment. Boron-doped semi-metallic diamond was selectively deposited for up to 20 hours on one end of Mo/Re (47.5/52.5 wt.%) and W/Re (75/25 wt.%) alloy wires. Conformal diamond films on the alloys displayed grain sizes and Raman signatures similar to films grown on tungsten; in all cases, the morphology and Raman spectra were consistent with well-faceted, microcrystalline diamond with minimal sp 2 carbon content. Cyclic voltammograms of dopamine in phosphate-buffered saline (PBS) showed the wide window and low baseline current of high-quality diamond electrodes. In addition, the films showed consistently well-defined, dopamine electrochemical redox activity. The Mo/Re substrate regions that were uncoated but still exposed to the diamond-growth environment remained substantially more flexible than tungsten in a bend-to-fracture rotation test, bending to the test maximum of 90° and not fracturing. The W/Re substrates fractured after a 27° bend, and the tungsten fractured after a 21° bend. Brittle, transgranular cleavage fracture surfaces were observed for tungsten and W/Re. A tension-induced fracture of the Mo/Re after the prior bend test showed a dimple fracture with a visible ductile core. Overall, the Mo/Re and W/Re alloys were suitable substrates for diamond growth. The Mo/Re alloy remained significantly more ductile than traditional tungsten substrates after diamond growth, and thus may be an attractive metal substrate for more ductile, thin-film diamond electrodes.

  18. Boron Doped diamond films as electron donors in photovoltaics: An X-ray absorption and hard X-ray photoemission study

    International Nuclear Information System (INIS)

    Kapilashrami, M.; Zegkinoglou, I.; Conti, G.; Nemšák, S.; Conlon, C. S.; Fadley, C. S.; Törndahl, T.; Fjällström, V.; Lischner, J.; Louie, Steven G.; Hamers, R. J.; Zhang, L.; Guo, J.-H.; Himpsel, F. J.

    2014-01-01

    Highly boron-doped diamond films are investigated for their potential as transparent electron donors in solar cells. Specifically, the valence band offset between a diamond film (as electron donor) and Cu(In,Ga)Se 2 (CIGS) as light absorber is determined by a combination of soft X-ray absorption spectroscopy and hard X-ray photoelectron spectroscopy, which is more depth-penetrating than standard soft X-ray photoelectron spectroscopy. In addition, a theoretical analysis of the valence band is performed, based on GW quasiparticle band calculations. The valence band offset is found to be small: VBO = VBM CIGS – VBM diamond  = 0.3 eV ± 0.1 eV at the CIGS/Diamond interface and 0.0 eV ± 0.1 eV from CIGS to bulk diamond. These results provide a promising starting point for optimizing the band offset by choosing absorber materials with a slightly lower valence band maximum.

  19. Correlation of CVD Diamond Electron Emission with Film Properties

    Science.gov (United States)

    Bozeman, S. P.; Baumann, P. K.; Ward, B. L.; Nemanich, R. J.; Dreifus, D. L.

    1996-03-01

    Electron field emission from metals is affected by surface morphology and the properties of any dielectric coating. Recent results have demonstrated low field electron emission from p-type diamond, and photoemission measurements have identified surface treatments that result in a negative electron affinity (NEA). In this study, the field emission from diamond is correlated with surface treatment, surface roughness, and film properties (doping and defects). Electron emission measurements are reported on diamond films synthesized by plasma CVD. Ultraviolet photoemission spectroscopy indicates that the CVD films exhibit a NEA after exposure to hydrogen plasma. Field emission current-voltage measurements indicate "threshold voltages" ranging from approximately 20 to 100 V/micron.

  20. Corrosion behavior of aluminum doped diamond-like carbon thin films in NaCl aqueous solution.

    Science.gov (United States)

    Khun, N W; Liu, E

    2010-07-01

    Aluminum doped diamond-like carbon (DLC:Al) thin films were deposited on n-Si(100) substrates by co-sputtering a graphite target under a fixed DC power (650 W) and an aluminum target under varying DC power (10-90 W) at room temperature. The structure, adhesion strength and surface morphology of the DLC:Al films were characterized by X-ray photoelectron spectroscopy (XPS), micro-scratch testing and atomic force microscopy (AFM), respectively. The corrosion performance of the DLC:Al films was investigated by means of potentiodynamic polarization testing in a 0.6 M NaCl aqueous solution. The results showed that the polarization resistance of the DLC:Al films increased from about 18 to 30.7 k(omega) though the corrosion potentials of the films shifted to more negative values with increased Al content in the films.

  1. Hydrogen termination of CVD diamond films by high-temperature annealing at atmospheric pressure

    NARCIS (Netherlands)

    Seshan, V.; Ullien, D.; Castellanos-Gomez, A.; Sachdeva, S.; Murthy, D.H.K.; Savenije, T.J.; Ahmad, H.A.; Nunney, T.S.; Janssens, S.D.; Haenen, K.; Nesládek, M.; Van der Zant, H.S.J.; Sudhölter, E.J.R.; De Smet, L.C.P.M.

    2013-01-01

    A high-temperature procedure to hydrogenate diamond films using molecular hydrogen at atmospheric pressure was explored. Undoped and doped chemical vapour deposited (CVD) polycrystalline diamond films were treated according to our annealing method using a H2 gas flow down to ?50 ml/min (STP) at

  2. Fabrication and electrochemistry characteristics of nickel-doped diamond-like carbon film toward applications in non-enzymatic glucose detection

    Science.gov (United States)

    Liu, Chi-Wen; Chen, Wei-En; Sun, Yin Tung Albert; Lin, Chii-Ruey

    2018-04-01

    This research work focused on the fabrication of nickel-doped diamond-like carbon (DLC) films and their characteristics including of surface morphology, microstructure, and electrochemical aiming at applications in non-enzymatic glucose detection. Novel nanodiamond target was employed in unbalanced magnetron radio-frequency co-sputtering process to prepared high quality Ni-doped DLC thin film at room temperature. TEM analysis reveals a highly uniform distribution of Ni crystallites in amorphous carbon matrix with fraction ranged from 3 to 11.5 at.% which is considered as active sites for the glucose detection. Our cyclic voltammetry measurements using 0.1 M H2SO4 solution demonstrated that the as-prepared Ni-doped DLC films possess large electrochemical potential window of 2.12 V, and this was also observed to be significantly reduced at high Ni doping level owing to lower sp3 fraction. The non-enzymatic glucose detection investigation indicates that the Ni-doped DLC thin film electrode prepared under 7 W of DC sputtering power on Ni target possesses good detecting performance, high stability, and high sensitivity to glucose concentration up to 10 mM, even with the existence of uric acid and ascorbic acid. The peak current was observed to be proportional to glucose concentration and scanning rate, demonstrating highly reversibility redox process of the film electrode and glucose.

  3. Structural characteristics of surface-functionalized nitrogen-doped diamond-like carbon films and effective adjustment to cell attachment

    International Nuclear Information System (INIS)

    Liu Ai-Ping; Liu Min; Yu Jian-Can; Qian Guo-Dong; Tang Wei-Hua

    2015-01-01

    Nitrogen-doped diamond-like carbon (DLC:N) films prepared by the filtered cathodic vacuum arc technology are functionalized with various chemical molecules including dopamine (DA), 3-Aminobenzeneboronic acid (APBA), and adenosine triphosphate (ATP), and the impacts of surface functionalities on the surface morphologies, compositions, microstructures, and cell compatibility of the DLC:N films are systematically investigated. We demonstrate that the surface groups of DLC:N have a significant effect on the surface and structural properties of the film. The activity of PC12 cells depends on the particular type of surface functional groups of DLC:N films regardless of surface roughness and wettability. Our research offers a novel way for designing functionalized carbon films as tailorable substrates for biosensors and biomedical engineering applications. (paper)

  4. Stress reduction of Cu-doped diamond-like carbon films from ab initio calculations

    Directory of Open Access Journals (Sweden)

    Xiaowei Li

    2015-01-01

    Full Text Available Structure and properties of Cu-doped diamond-like carbon films (DLC were investigated using ab initio calculations. The effect of Cu concentrations (1.56∼7.81 at.% on atomic bond structure was mainly analyzed to clarify the residual stress reduction mechanism. Results showed that with introducing Cu into DLC films, the residual compressive stress decreased firstly and then increased for each case with the obvious deterioration of mechanical properties, which was in agreement with the experimental results. Structural analysis revealed that the weak Cu-C bond and the relaxation of both the distorted bond angles and bond lengths accounted for the significant reduction of residual compressive stress, while at the higher Cu concentration the increase of residual stress attributed to the existence of distorted Cu-C structures and the increased fraction of distorted C-C bond lengths.

  5. Experimental studies of N~+ implantation into CVD diamond thin films

    Institute of Scientific and Technical Information of China (English)

    辛火平; 林成鲁; 王建新; 邹世昌; 石晓红; 林梓鑫; 周祖尧; 刘祖刚

    1997-01-01

    The effects of N+ implantation under various conditions on CVD diamond films were analyzed with Raman spectroscopy, four-point probe method, X-ray diffraction (XRD), Rutherford backseattering spectroscopy (RBS), ultraviolet photoluminescence spectroscopy (UV-PL), Fourier transformation infrared absorption spectroscopy (FTIR) and X-ray photoelectron spectroscopy (XPS). The results show that the N+ implantation doping without any graphitization has been successfully realized when 100 keV N+ ions at a dosage of 2 × 1016 cm-2 were implanted into diamond films at 550℃ . UV-PL spectra indicate that the implanted N+ ions formed an electrically inactive deep-level impurity in diamond films. So the sheet resistance of the sample after N+ implantation changed little. Carbon nitride containing C≡N covalent bond has been successfully synthesized by 100 keV, 1.2×1018 N/cm2 N+ implantation into diamond films. Most of the implanted N+ ions formed C≡N covalent bonds with C atoms. The others were free state nitroge

  6. Effect of B doping on optical, electrical properties and defects of ZnO films

    Energy Technology Data Exchange (ETDEWEB)

    Mao, Caiying [State Key Laboratory of Mechanical Transmission, College of Physics, Chongqing University, Chongqing, 400044 (China); Fang, Liang, E-mail: lfang@cqu.edu.cn [State Key Laboratory of Mechanical Transmission, College of Physics, Chongqing University, Chongqing, 400044 (China); Zhang, Hong; Li, Wanjun [Key Laboratory of Optoelectronic Functional Materials of Chongqing, College of Physics and Electronic Engineering, Chongqing Normal University, Chongqing 401331 (China); Wu, Fang, E-mail: fang01234@163.com [State Key Laboratory of Mechanical Transmission, College of Physics, Chongqing University, Chongqing, 400044 (China); Qin, Guoping [Key Laboratory of Optoelectronic Functional Materials of Chongqing, College of Physics and Electronic Engineering, Chongqing Normal University, Chongqing 401331 (China); Ruan, Haibo, E-mail: rhbcqu@aliyun.com [Chongqing Key Laboratory of Micro/Nano Materials Engineering and Technology, Research Center for Materials Interdisciplinary Sciences, Chongqing University of Arts and Sciences, Chongqing, 402160 (China); Kong, Chunyang, E-mail: kchy@163.com [Key Laboratory of Optoelectronic Functional Materials of Chongqing, College of Physics and Electronic Engineering, Chongqing Normal University, Chongqing 401331 (China)

    2016-08-15

    Boron doped ZnO (BZO) films with B content in the range of 0–6 at.% were deposited on quartz glass substrates by RF magnetron sputtering technique. The effects of B doping content on microstructure, optical and electrical properties of BZO films were systematically investigated by XRD, SEM, AFM, XPS, PL, UV–vis–near infrared spectrophotometer and Hall-effect measurement, respectively. It is found that the crystal quality of ZnO films can be improved as B doping content increases to no larger than 4 at.% and will be deteriorated at higher B doping content. The grain size and surface roughness of the films reduce with the increase of B doping content. The BZO films exhibit tensile stress and the stress increases with B content. The transmittance of the BZO films is revealed to be 90% in the visible region. As the B doping content increases from 0 to 6 at.%, the optical band gap of BZO films enhances from 3.28 to 3.57 eV, which is found to increase linearly with the tensile stress in the films. The lowest resistivity of 1.58 × 10{sup −3} (Ω cm) is obtained at 2 at.% B doping content. XPS and PL analyses demonstrated that B doping can promote the formation of defects of zinc interstitials (Zn{sub i}) and oxygen vacancies (V{sub O}). - Highlights: • The relationship of band gap (E{sub g}) and stress (σ) in BZO is deduced. • XPS and PL illustrate B doping can promote the formation of Zn{sub i} and V{sub O} in BZO. • The lowest resistivity (1.58 × 10{sup −3} Ω cm) is obtained at 2 at.% B content.

  7. Effect of sputtering power on structure, adhesion strength and corrosion resistance of nitrogen doped diamond-like carbon thin films.

    Science.gov (United States)

    Khun, N W; Liu, E

    2011-06-01

    Nitrogen doped diamond-like carbon (DLC:N) thin films were deposited on highly conductive p-Si substrates using a DC magnetron sputtering deposition system. The DLC:N films were characterized using X-ray photoelectron spectroscopy (XPS), micro-Raman spectroscopy, atomic force microscopy (AFM), contact angle measurement and micro-scratch test. The XPS and Raman results indicated that the sputtering power significantly influenced the properties of the films in terms of bonding configuration in the films. The corrosion performance of the DLC:N films was investigated in a 0.6 M NaCl solution by means of potentiodynamic polarization testing. It was found that the corrosion performance of the films could be enhanced by higher sputtering powers.

  8. Optically transparent boron-doped nanocrystalline diamond films for spectroelectrochemical measurements on different substrates

    International Nuclear Information System (INIS)

    Sobaszek, M.; Bogdanowicz, R.; Pluciński, J.; Siuzdak, K.; Skowroński, Ł.

    2016-01-01

    Fabrication process of optically transparent boron nanocrystalline diamond (B- NCD) electrode on silicon and quartz substrate was shown. The B-NCD films were deposited on the substrates using Microwave Plasma Assisted Chemical Vapor Deposition (MWPACVD) at glass substrate temperature of 475 °C. A homogenous, continuous and polycrystalline surface morphology with high sp 3 content in B-NCD films and film thickness depending from substrate in the range of 60-300 nm was obtained. The high refraction index and transparency in visible (VIS) wavelength range was achieved. Moreover, cyclic voltammograms (CV) were recorded to determine reaction reversibility at the B-NCD electrode. CV measurements in aqueous media consisting of 1 mM K 3 [Fe(CN) 6 ] in 0.5 M Na 2 SO 4 demonstrated relatively fast kinetics expressed by a redox peak splitting below 503 mV for B-NCD/silicon and 110 mv for B-NCD/quartz

  9. Raman Microscopic Analysis of Internal Stress in Boron-Doped Diamond

    Directory of Open Access Journals (Sweden)

    Kevin E. Bennet

    2015-05-01

    Full Text Available Analysis of the induced stress on undoped and boron-doped diamond (BDD thin films by confocal Raman microscopy is performed in this study to investigate its correlation with sample chemical composition and the substrate used during fabrication. Knowledge of this nature is very important to the issue of long-term stability of BDD coated neurosurgical electrodes that will be used in fast-scan cyclic voltammetry, as potential occurrence of film delaminations and dislocations during their surgical implantation can have unwanted consequences for the reliability of BDD-based biosensing electrodes. To achieve a more uniform deposition of the films on cylindrically-shaped tungsten rods, substrate rotation was employed in a custom-built chemical vapor deposition reactor. In addition to visibly preferential boron incorporation into the diamond lattice and columnar growth, the results also reveal a direct correlation between regions of pure diamond and enhanced stress. Definite stress release throughout entire film thicknesses was found in the current Raman mapping images for higher amounts of boron addition. There is also a possible contribution to the high values of compressive stress from sp2 type carbon impurities, besides that of the expected lattice mismatch between film and substrate.

  10. Conductivity of boron-doped polycrystalline diamond films: influence of specific boron defects

    Czech Academy of Sciences Publication Activity Database

    Ashcheulov, Petr; Šebera, Jakub; Kovalenko, Alexander; Petrák, Václav; Fendrych, František; Nesládek, M.; Taylor, Andrew; Vlčková Živcová, Zuzana; Frank, Otakar; Kavan, Ladislav; Dračínský, Martin; Hubík, Pavel; Vacík, Jiří; Kraus, I.; Kratochvílová, Irena

    2013-01-01

    Roč. 86, č. 10 (2013), , "443-1"-"443-9" ISSN 1434-6028 R&D Projects: GA TA ČR TA01011165; GA ČR(CZ) GAP304/10/1951; GA MŠk(XE) LM2011019; GA ČR GA13-31783S; GA MŠk(CZ) LD11076 EU Projects: European Commission(XE) 238201 - MATCON Institutional support: RVO:68378271 ; RVO:61388955 ; RVO:61388963 ; RVO:61389005 Keywords : polycrystalline diamond layer * conductivity B doping Subject RIV: BM - Solid Matter Physics ; Magnetism; CG - Electrochemistry (UFCH-W) Impact factor: 1.463, year: 2013

  11. In situ boron doping during heteroepitaxial growth of diamond on Ir/YSZ/Si

    Energy Technology Data Exchange (ETDEWEB)

    Sartori, Andre F.; Fischer, Martin; Gsell, Stefan; Schreck, Matthias [Universitaet Augsburg, Institut fuer Physik, 86135 Augsburg (Germany)

    2012-09-15

    In situ boron doping of heteroepitaxial diamond films grown by microwave plasma chemical vapor deposition on Ir/YSZ/Si (001) is investigated. The study comprises the analysis of the gas phase by optical emission spectroscopy (OES) and measurements of B doped films by secondary ion mass spectroscopy (SIMS), cathodoluminescence (CL), and X-ray diffraction (XRD). The OE intensity of BH species scales linearly with the concentration of the boron precursor trimethylboron (TMB) in the feed gas. Addition of CO{sub 2} as an oxygen source causes a proportional reduction of the BH signal. At a ratio C:O = 1, a reduction factor of {proportional_to}50 is obtained. It is shown for two diamond samples that the boron incorporation drops nearly identical to the BH emission intensity. We conclude that the influence of oxygen on boron incorporation is a pure gas phase effect. In contrast, CN and BH emission indicate a negligible interaction between N{sub 2} and TMB added to the feed gas. At the same time, preliminary growth rate measurements show that the boron background pressure in the chamber after growth with TMB completely cancels the growth acceleration by nitrogen up to N{sub 2} concentrations of 100 ppm which points to the dominance of surface processes. Heteroepitaxial diamond films grown on Ir at 50 mbar between 720 and 900 C contain high intrinsic stress that varies from -2.2 GPa compressive at the lowest to slightly tensile at the highest deposition temperature. The observed behavior is similar to former work at 200 mbar in which effective climb of dislocations was suggested as responsible mechanism. Addition of boron rather enhances the stress formation than causing a relaxation. The B concentration in the heteroepitaxial films is deduced by SIMS, CL, and XRD and correlated with the TMB concentration in the gas phase. (Copyright copyright 2012 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  12. The Field Emission Characteristics of Titanium-Doped Nano-Diamonds

    Institute of Scientific and Technical Information of China (English)

    YANG Yan-Ning; ZHANG Zhi-Yong; ZHANG Fu-Chun; DONG Jun-Tang; ZHAO Wu; ZHAI Chun-Xue; ZHANG Wei-Hu

    2012-01-01

    powder. Compared with the undoped nano-diamond cathode, the turn-on fields decline from 6.95 to 5.95 V/bμm. When the electric field strength is 13.80 V/μm, the field emission current density increases to 130.00 μA/cm2. Under the applied fields, the emission current is stable and the luminescence is at its best, while the Held emission characteristics of the 10 mg Ti-doped coating become worse, as does the luminescence. The reason for this could be that an excessive amount of TiC is generated on the surface of the coating.

  13. Ellipsometric investigation of nitrogen doped diamond thin films grown in microwave CH{sub 4}/H{sub 2}/N{sub 2} plasma enhanced chemical vapor deposition

    Energy Technology Data Exchange (ETDEWEB)

    Ficek, Mateusz, E-mail: rbogdan@eti.pg.gda.pl [Department of Metrology and Optoelectronics, Faculty of Electronics, Telecommunications and Informatics, Gdansk University of Technology, 11/12 G. Narutowicza St., 80-233 Gdansk (Poland); Institute for Materials Research (IMO), Hasselt University, Wetenschapspark 1, B-3590 Diepenbeek (Belgium); Sankaran, Kamatchi J.; Haenen, Ken [Institute for Materials Research (IMO), Hasselt University, Wetenschapspark 1, B-3590 Diepenbeek (Belgium); IMOMEC, IMEC vzw, Wetenschapspark 1, B-3590 Diepenbeek (Belgium); Ryl, Jacek; Darowicki, Kazimierz [Department of Electrochemistry, Corrosion and Material Engineering, Gdansk University of Technology, 11/12 Narutowicza St., 80-233 Gdansk (Poland); Bogdanowicz, Robert [Department of Metrology and Optoelectronics, Faculty of Electronics, Telecommunications and Informatics, Gdansk University of Technology, 11/12 G. Narutowicza St., 80-233 Gdansk (Poland); Materials and Process Simulation Center, California Institute of Technology, Pasadena, California 91125 (United States); Lin, I-Nan [Department of Physics, Tamkang University, Tamsui 251, Taiwan (China)

    2016-06-13

    The influence of N{sub 2} concentration (1%–8%) in CH{sub 4}/H{sub 2}/N{sub 2} plasma on structure and optical properties of nitrogen doped diamond (NDD) films was investigated. Thickness, roughness, and optical properties of the NDD films in the VIS–NIR range were investigated on the silicon substrates using spectroscopic ellipsometry. The samples exhibited relatively high refractive index (2.6 ± 0.25 at 550 nm) and extinction coefficient (0.05 ± 0.02 at 550 nm) with a transmittance of 60%. The optical investigation was supported by the molecular and atomic data delivered by Raman studies, bright field transmission electron microscopy imaging, and X-ray photoelectron spectroscopy diagnostics. Those results revealed that while the films grown in CH{sub 4}/H{sub 2} plasma contained micron-sized diamond grains, the films grown using CH{sub 4}/H{sub 2}/(4%)N{sub 2} plasma exhibited ultranano-sized diamond grains along with n-diamond and i-carbon clusters, which were surrounded by amorphous carbon grain boundaries.

  14. Diamond film growth with modification properties of adhesion between substrate and diamond film

    Directory of Open Access Journals (Sweden)

    Setasuwon P.

    2004-03-01

    Full Text Available Diamond film growth was studied using chemical vapor deposition (CVD. A special equipment was build in-house, employing a welding torch, and substrate holder with a water-cooling system. Acetylene and oxygen were used as combustion gases and the substrate was tungsten carbide cobalt. It was found that surface treatments, such as diamond powder scratching or acid etching, increase the adhesion and prevent the film peel-off. Diamond powder scratching and combined diamond powder scratching with acid etching gave the similar diamond film structure with small grain and slightly rough surface. The diamond film obtained with both treatments has high adhesion and can withstand internal stress better than ones obtained by untreated surface or acid etching alone. It was also found that higher substrate temperature produced smoother surface and more uniform diamond grain.

  15. Boron-doped Diamond Electrodes: Electrochemical, Atomic Force Microscopy and Raman Study towards Corrosion-modifications at Nanoscale

    International Nuclear Information System (INIS)

    Kavan, Ladislav; Vlckova Zivcova, Zuzana; Petrak, Vaclav; Frank, Otakar; Janda, Pavel; Tarabkova, Hana; Nesladek, Milos; Mortet, Vincent

    2015-01-01

    Highlights: • B-doped diamond is nanostructured by corrosion-driven modifications occurring at carbonaceous impurity sites (sp 2 -carbons). • The electrochemical oxidation partly transforms a hydrogen-terminated diamond surface to O-terminated one, but the electrocatalytic activity of plasmatically O-terminated diamond is not achieved. • In contrast to all usual sp 2 carbons, the Raman spectra of B-doped diamond electrodes do not change upon electrochemical charging/discharging. - Abstract: Comparative studies of boron-doped diamonds electrodes (polycrystalline, single-crystalline, H-/O-terminated, and with different sp 3 /sp 2 ratios) indicate morphological modifications of diamond which are initiated by corrosion at nanoscale. In-situ electrochemical AFM imaging evidences that the textural changes start at non-diamond carbonaceous impurity sites treated at high positive potentials (>2.2 V vs. Ag/AgCl). The primary perturbations subsequently develop into sub-micron-sized craters. Raman spectroscopy shows that the primary erosion site is graphite-like (sp 2 -carbon), which is preferentially removed by anodic oxidation. Other non-diamond impurity, viz. tetrahedral amorphous carbon (t-aC), is less sensitive to oxidative decomposition. The diamond-related Raman features, including the B-doping-assigned modes, are intact during reversible electrochemical charging/discharging, which is a salient difference from all usual sp 2 -carbons. The electrochemical oxidation partly transforms a hydrogen-terminated diamond surface to O-terminated one, but the electrocatalytic activity of plasmatically O-terminated diamond is not achieved for a model redox couple, Fe 3+/2+ . Electrochemical impedance spectra were fitted to six different equivalent circuits. The determination of acceptor concentrations is feasible even for highly-doped diamond electrodes.

  16. Electron field emission from boron doped microcrystalline diamond

    International Nuclear Information System (INIS)

    Roos, M.; Baranauskas, V.; Fontana, M.; Ceragioli, H.J.; Peterlevitz, A.C.; Mallik, K.; Degasperi, F.T.

    2007-01-01

    Field emission properties of hot filament chemical vapor deposited boron doped polycrystalline diamond have been studied. Doping level (N B ) of different samples has been varied by the B/C concentration in the gas feed during the growth process and doping saturation has been observed for high B/C ratios. Threshold field (E th ) for electron emission as function of B/C concentration has been measured, and the influences of grain boundaries, doping level and surface morphology on field emission properties have been investigated. Carrier transport through conductive grains and local emission properties of surface sites have been figured out to be two independent limiting effects in respect of field emission. Emitter current densities of 500 nA cm -2 were obtained using electric fields less than 8 V/μm

  17. Piezoelectric actuated micro-resonators based on the growth of diamond on aluminum nitride thin films

    International Nuclear Information System (INIS)

    Hees, J; Heidrich, N; Pletschen, W; Sah, R E; Wolfer, M; Lebedev, V; Nebel, C E; Ambacher, O; Williams, O A

    2013-01-01

    Unimorph heterostructures based on piezoelectric aluminum nitride (AlN) and diamond thin films are highly desirable for applications in micro- and nanoelectromechanical systems. In this paper, we present a new approach to combine thin conductive boron-doped as well as insulating nanocrystalline diamond (NCD) with sputtered AlN films without the need for any buffer layers between AlN and NCD or polishing steps. The zeta potentials of differently treated nanodiamond (ND) particles in aqueous colloids are adjusted to the zeta potential of AlN in water. Thereby, the nucleation density for the initial growth of diamond on AlN can be varied from very low (10 8 cm −2 ), in the case of hydrogen-treated ND seeding particles, to very high values of 10 11 cm −2 for oxidized ND particles. Our approach yielding high nucleation densities allows the growth of very thin NCD films on AlN with thicknesses as low as 40 nm for applications such as microelectromechanical beam resonators. Fabricated piezo-actuated micro-resonators exhibit enhanced mechanical properties due to the incorporation of boron-doped NCD films. Highly boron-doped NCD thin films which replace the metal top electrode offer Young’s moduli of more than 1000 GPa. (paper)

  18. Microstructure and property of diamond-like carbon films with Al and Cr co-doping deposited using a hybrid beams system

    International Nuclear Information System (INIS)

    Dai, Wei; Liu, Jingmao; Geng, Dongsen; Guo, Peng; Zheng, Jun; Wang, Qimin

    2016-01-01

    Highlights: • Diamond-like carbon films with Al and Cr doping were deposited. • Alternate multilayered structure consisted of Al-poor layer and Al-rich layer was formed. • The periodic Al-rich layers can greatly improve the residual stress and elastic resilience of the films. - Abstract: DLC films with weak carbide former Al and carbide former Cr co-doping (Al:Cr-DLC) were deposited by a hybrid beams system comprising an anode-layer linear ion beam source (LIS) and high power impulse magnetron sputtering using a gas mixture of C 2 H 2 and Ar as the precursor. The doped Al and Cr contents were controlled via adjusting the C 2 H 2 fraction in the gas mixture. The composition, microstructure, compressive stress, mechanical properties and tribological behaviors of the Al:Cr-DLC films were researched carefully using X-ray photoelectron spectroscopy, transmission electron microscopy, Raman spectroscopy, stress-tester, nanoindentation and ball-on-plate tribometer as function of the C 2 H 2 fraction. The results show that the Al and Cr contents in the films increased continuously as the C 2 H 2 fraction decreased. The doped Cr atoms preferred to bond with the carbon while the Al atoms mainly existed in metallic state. Structure modulation with alternate multilayer consisted of Al-poor DLC layer and Al-rich DLC layer was found in the films. Those periodic Al-rich DLC layers can effectively release the residual stress of the films. On the other hand, the formation of the carbide component due to Cr incorporation can help to increase the film hardness. Accordingly, the residual stress of the DLC films can be reduced without sacrificing the film hardness though co-doping Al and Cr atoms. Furthermore, it was found that the periodic Al-rich layer can greatly improve the elastic resilience of the DLC films and thus decreases the film friction coefficient and wear rate significantly. However, the existence of the carbide component would cause abrasive wear and thus

  19. Structural characteristics of surface-functionalized nitrogen-doped diamond-like carbon films and effective adjustment to cell attachment

    Science.gov (United States)

    Liu, Ai-Ping; Liu, Min; Yu, Jian-Can; Qian, Guo-Dong; Tang, Wei-Hua

    2015-05-01

    Nitrogen-doped diamond-like carbon (DLC:N) films prepared by the filtered cathodic vacuum arc technology are functionalized with various chemical molecules including dopamine (DA), 3-Aminobenzeneboronic acid (APBA), and adenosine triphosphate (ATP), and the impacts of surface functionalities on the surface morphologies, compositions, microstructures, and cell compatibility of the DLC:N films are systematically investigated. We demonstrate that the surface groups of DLC:N have a significant effect on the surface and structural properties of the film. The activity of PC12 cells depends on the particular type of surface functional groups of DLC:N films regardless of surface roughness and wettability. Our research offers a novel way for designing functionalized carbon films as tailorable substrates for biosensors and biomedical engineering applications. Project supported by the National Natural Science Foundation of China (Grant Nos. 51272237, 51272231, and 51010002) and the China Postdoctoral Science Foundation (Grant Nos. 2012M520063, 2013T60587, and Bsh1201016).

  20. Sequential Electrodeposition of Platinum-Ruthenium at Boron-Doped Diamond Electrodes for Methanol Oxidation

    Directory of Open Access Journals (Sweden)

    Ileana González-González

    2011-01-01

    Full Text Available Sequential electrodeposition of Pt and Ru on boron-doped diamond (BDD films, in 0.5 M H2SO4 by cyclic voltammetry, has been prepared. The potential cycling, in the aqueous solutions of the respective metals, was between 0.00 and 1.00 V versus Ag/AgCl. The catalyst composites, Pt and PtRu, deposited on BDD film substrates, were tested for methanol oxidation. The modified diamond surfaces were also characterized by scanning electron microscopy-X-ray fluorescence-energy dispersive spectroscopy, X-ray photoelectron spectroscopy, and Auger electron spectroscopy. The scanning Auger electron spectroscopy mapping showed the ruthenium signal only in areas where platinum was electrodeposited. Ruthenium does not deposit on the oxidized diamond surface of the boron-doped diamond. Particles with 5–10% of ruthenium with respect to platinum exhibited better performance for methanol oxidation in terms of methanol oxidation peak current and chronoamperometric current stability. The electrogenerated •OH radicals on BDD may interact with Pt surface, participating in the methanol oxidation as shown in oxidation current and the shift in the peak position. The conductive diamond surface is a good candidate as the support for the platinum electrocatalyst, because it ensures catalytic activity, which compares with the used carbon, and higher stability under severe anodic and cathodic conditions.

  1. Influence of duty ratio of pulsed bias on structure and properties of silicon-doped diamond-like carbon films by plasma deposition

    International Nuclear Information System (INIS)

    Nakazawa, Hideki; Kamata, Ryosuke; Miura, Soushi; Okuno, Saori

    2013-01-01

    We have investigated the influence of the duty ratio of pulsed substrate bias on the structure and properties of Si-doped diamond-like carbon (Si-DLC) films deposited by radio frequency plasma-enhanced chemical vapor deposition using CH 4 , Ar, and monomethylsilane (CH 3 SiH 3 ) as the Si source. The Si/(Si + C) ratios in the Si-DLC films deposited using pulsed bias were higher than that of the dc-biased Si-DLC film, and the Si fraction increased with decreasing pulse duty ratio. Fourier transform infrared spectroscopy and X-ray photoelectron spectroscopy analyses revealed that Si-C, Si-H n , and C-H n bonds in the Si-DLC films increased with decreasing duty ratio. The internal stress decreased as the duty ratio decreased, which is probably due to the increase in Si-C, Si-H n , and C-H n bonds in the films. The Si-DLC films deposited using pulsed bias had higher adhesion strength than the dc-biased Si-DLC film because of the further reduction of internal stress. At higher duty ratios, although the Si fractions of the pulse-biased Si-DLC films were higher than that of the dc-biased Si-DLC film, the wear rates of the former were less than that of the latter. - Highlights: • The internal stress of Si-doped films was lowered at lower duty ratios. • The adhesion of pulse-biased films was improved compared with that of dc films. • The tribological properties of Si-doped films were improved by the use of pulse bias

  2. Effect of working pressure on corrosion behavior of nitrogen doped diamond-like carbon thin films deposited by DC magnetron sputtering.

    Science.gov (United States)

    Khun, N W; Liu, E

    2011-06-01

    Nitrogen doped diamond-like carbon thin films were deposited on highly conductive p-silicon(100) substrates using a DC magnetron sputtering deposition system by varying working pressure in the deposition chamber. The bonding structure, adhesion strength, surface roughness and corrosion behavior of the films were investigated by using X-ray photoelectron spectroscopy, micro-Raman spectroscopy, micro-scratch test, atomic force microscopy and potentiodynamic polarization test. A 0.6 M NaCl electrolytic solution was used for the corrosion tests. The optimum corrosion resistance of the films was found at a working pressure of 7 mTorr at which a good balance between the kinetics of the sputtered ions and the surface mobility of the adatoms promoted a microstructure of the films with fewer porosities.

  3. Preparation of TiO2/boron-doped diamond/Ta multilayer films and use as electrode materials for supercapacitors

    Science.gov (United States)

    Shi, Chao; Li, Hongji; Li, Cuiping; Li, Mingji; Qu, Changqing; Yang, Baohe

    2015-12-01

    We report nanostructured TiO2/boron-doped diamond (BDD)/Ta multilayer films and their electrochemical performances as supercapacitor electrodes. The BDD films were grown on Ta substrates using electron-assisted hot filament chemical vapor deposition. Ti metal layers were deposited on the BDD surfaces by radio frequency magnetron sputtering, and nanostructured TiO2/BDD/Ta thin films were prepared by electrochemical etching and thermal annealing. The successful formation of TiO2 and Ta layered nanostructures was demonstrated using scanning electron and transmission electron microscopies. The electrochemical responses of these electrodes were evaluated by examining their use as electrical double-layer capacitors, using cyclic voltammetry, and galvanostatic charge/discharge and impedance measurements. When the TiO2/BDD/Ta film was used as the working electrode with 0.1 M Na2SO4 as the electrolyte, the capacitor had a specific capacitance of 5.23 mF cm-2 at a scan rate of 5 mV s-1 for a B/C ratio of 0.1% w/w. Furthermore, the TiO2/BDD/Ta film had improved electrochemical stability, with a retention of 89.3% after 500 cycles. This electrochemical behavior is attributed to the quality of the BDD, the surface roughness and electrocatalytic activities of the TiO2 layer and Ta nanoporous structures, and the synergies between them. These results show that TiO2/BDD/Ta films are promising as capacitor electrodes for special applications.

  4. Deposition of boron doped DLC films on TiNb and characterization of their mechanical properties and blood compatibility.

    Science.gov (United States)

    Liza, Shahira; Hieda, Junko; Akasaka, Hiroki; Ohtake, Naoto; Tsutsumi, Yusuke; Nagai, Akiko; Hanawa, Takao

    2017-01-01

    Diamond-like carbon (DLC) material is used in blood contacting devices as the surface coating material because of the antithrombogenicity behavior which helps to inhibit platelet adhesion and activation. In this study, DLC films were doped with boron during pulsed plasma chemical vapor deposition (CVD) to improve the blood compatibility. The ratio of boron to carbon (B/C) was varied from 0 to 0.4 in the film by adjusting the flow rate of trimethylboron and acetylene. Tribological tests indicated that boron doping with a low B/C ratio of 0.03 is beneficial for reducing friction (μ = 0.1), lowering hardness and slightly increasing wear rate compared to undoped DLC films. The B/C ratio in the film of 0.03 and 0.4 exhibited highly hydrophilic surface owing to their high wettability and high surface energy. An in vitro platelet adhesion experiment was conducted to compare the blood compatibility of TiNb substrates before and after coating with undoped and boron doped DLC. Films with highly hydrophilic surface enhanced the blood compatibility of TiNb, and the best results were obtained for DLC with the B/C ratio of 0.03. Boron doped DLC films are promising surface coatings for blood contacting devices.

  5. Influence of boron concentration on growth characteristic and electro-catalytic performance of boron-doped diamond electrodes prepared by direct current plasma chemical vapor deposition

    International Nuclear Information System (INIS)

    Feng Yujie; Lv Jiangwei; Liu Junfeng; Gao Na; Peng Hongyan; Chen Yuqiang

    2011-01-01

    A series of boron-doped diamond (BDD) electrodes were prepared by direct current plasma chemical vapor deposition (DC-PCVD) with different compositions of CH 4 /H 2 /B(OCH 3 ) 3 gas mixture. A maximum growth rate of 0.65 mg cm -2 h -1 was obtained with CH 4 /H 2 /B(OCH 3 ) 3 radio of 4/190/10 and this growth condition was also a turning point for discharge plasma stability which arose from the addition of B(OCH 3 ) 3 that changed electron energy distribution and influenced the plasma reaction. The surface coating structure and electro-catalytic performance of the BDD electrodes were characterized by scanning electron microscopy (SEM), X-ray diffraction (XRD), Raman spectroscopy, Hall test, and electrochemical measurement and electro-catalytic oxidation in phenol solution. It is suggested that the boron doping level and the thermal stress in the films are the main factors affecting the electro-catalytic characteristics of the electrodes. Low boron doping level with CH 4 /H 2 /B(OCH 3 ) 3 ratio of 4/199/1 decreased the films electrical conductivity and its electro-catalytic activity. When the carrier concentration in the films reached around 10 20 cm -3 with CH 4 /H 2 /B(OCH 3 ) 3 ratio over a range of 4/195/5-4/185/15, the thermal stress in the films was the key reason that influenced the electro-catalytic activity of the electrodes for its effect on diamond lattice expansion. Therefore, the BDD electrode with modest CH 4 /H 2 /B(OCH 3 ) 3 ratio of 4/190/10 possessed the best phenol removal efficiency.

  6. Microstructure and property of diamond-like carbon films with Al and Cr co-doping deposited using a hybrid beams system

    Energy Technology Data Exchange (ETDEWEB)

    Dai, Wei, E-mail: popdw@126.com [School of Electromechanical Engineering, Guangdong University of Technology, Guangzhou 510006 (China); Liu, Jingmao; Geng, Dongsen [School of Electromechanical Engineering, Guangdong University of Technology, Guangzhou 510006 (China); Guo, Peng [Key Laboratory of Marine Materials and Related Technologies, Zhejiang Key Laboratory of Marine Materials and Protective Technologies, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201 (China); Zheng, Jun [Science and Technology on Surface Engineering Laboratory, Lanzhou Institute of Physics, Lanzhou 730000 (China); Wang, Qimin, E-mail: qmwang@gdut.edu.cn [School of Electromechanical Engineering, Guangdong University of Technology, Guangzhou 510006 (China)

    2016-12-01

    Highlights: • Diamond-like carbon films with Al and Cr doping were deposited. • Alternate multilayered structure consisted of Al-poor layer and Al-rich layer was formed. • The periodic Al-rich layers can greatly improve the residual stress and elastic resilience of the films. - Abstract: DLC films with weak carbide former Al and carbide former Cr co-doping (Al:Cr-DLC) were deposited by a hybrid beams system comprising an anode-layer linear ion beam source (LIS) and high power impulse magnetron sputtering using a gas mixture of C{sub 2}H{sub 2} and Ar as the precursor. The doped Al and Cr contents were controlled via adjusting the C{sub 2}H{sub 2} fraction in the gas mixture. The composition, microstructure, compressive stress, mechanical properties and tribological behaviors of the Al:Cr-DLC films were researched carefully using X-ray photoelectron spectroscopy, transmission electron microscopy, Raman spectroscopy, stress-tester, nanoindentation and ball-on-plate tribometer as function of the C{sub 2}H{sub 2} fraction. The results show that the Al and Cr contents in the films increased continuously as the C{sub 2}H{sub 2} fraction decreased. The doped Cr atoms preferred to bond with the carbon while the Al atoms mainly existed in metallic state. Structure modulation with alternate multilayer consisted of Al-poor DLC layer and Al-rich DLC layer was found in the films. Those periodic Al-rich DLC layers can effectively release the residual stress of the films. On the other hand, the formation of the carbide component due to Cr incorporation can help to increase the film hardness. Accordingly, the residual stress of the DLC films can be reduced without sacrificing the film hardness though co-doping Al and Cr atoms. Furthermore, it was found that the periodic Al-rich layer can greatly improve the elastic resilience of the DLC films and thus decreases the film friction coefficient and wear rate significantly. However, the existence of the carbide component would

  7. Thin diamond films for tribological applications

    International Nuclear Information System (INIS)

    Wong, M.S.; Meilunas, R.; Ong, T.P.; Chang, R.P.H.

    1989-01-01

    Diamond films have been deposited on Si, Mo and many other substrates by microwave and radio frequency plasma enhanced chemical vapor deposition. Although the adhesion between the diamond film and most of the metal substrates is poor due to residual thermal stress from the mismatch of thermal expansion coefficients, the authors have developed processes to promote the growth of uniform and continuous diamond films with enhanced adhesion to metal substrates for tribological applications. The tribological properties of these films are measured using a ring-on-block tribotester. The coefficients of friction of diamond films sliding against a 52100 steel ring under the same experimental conditions are found to be significantly different depending on the morphology, grain size and roughness of the diamond films. However, under all cases tested, it is found that for uniform and continuous diamond films with small grain size of 1-3 micrometers, the coefficient of friction of the diamond film sliding against a steel ring under lubrication of a jet of mineral oil is about 0.04

  8. Lateral overgrowth of diamond film on stripes patterned Ir/HPHT-diamond substrate

    Science.gov (United States)

    Wang, Yan-Feng; Chang, Xiaohui; Liu, Zhangcheng; Liu, Zongchen; Fu, Jiao; Zhao, Dan; Shao, Guoqing; Wang, Juan; Zhang, Shaopeng; Liang, Yan; Zhu, Tianfei; Wang, Wei; Wang, Hong-Xing

    2018-05-01

    Epitaxial lateral overgrowth (ELO) of diamond films on patterned Ir/(0 0 1)HPHT-diamond substrates have been carried out by microwave plasma CVD system. Ir/(0 0 1)HPHT-diamond substrates are fabricated by photolithographic and magnetron sputtering technique. The morphology of the as grown ELO diamond film is characterized by optical microscopy and scanning electronic microscopy. The quality and stress of the ELO diamond film are investigated by surface etching pit density and micro-Raman spectroscopy. Two ultraviolet photodetectors are fabricated on ELO diamond area and non-ELO diamond area prepared on same substrate, and that one on ELO diamond area indicates better photoelectric properties. All results indicate quality of ELO diamond film is improved.

  9. Fabrication and Characterization of N-Type Zinc Oxide/P-Type Boron Doped Diamond Heterojunction

    Science.gov (United States)

    Marton, Marián; Mikolášek, Miroslav; Bruncko, Jaroslav; Novotný, Ivan; Ižák, Tibor; Vojs, Marian; Kozak, Halyna; Varga, Marián; Artemenko, Anna; Kromka, Alexander

    2015-09-01

    Diamond and ZnO are very promising wide-bandgap materials for electronic, photovoltaic and sensor applications because of their excellent electrical, optical, physical and electrochemical properties and biocompatibility. In this contribution we show that the combination of these two materials opens up the potential for fabrication of bipolar heterojunctions. Semiconducting boron doped diamond (BDD) thin films were grown on Si and UV grade silica glass substrates by HFCVD method with various boron concentration in the gas mixture. Doped zinc oxide (ZnO:Al, ZnO:Ge) thin layers were deposited by diode sputtering and pulsed lased deposition as the second semiconducting layer on the diamond films. The amount of dopants within the films was varied to obtain optimal semiconducting properties to form a bipolar p-n junction. Finally, different ZnO/BDD heterostructures were prepared and analyzed. Raman spectroscopy, SEM, Hall constant and I-V measurements were used to investigate the quality, structural and electrical properties of deposited heterostructures, respectively. I-V measurements of ZnO/BDD diodes show a rectifying ratio of 55 at ±4 V. We found that only very low dopant concentrations for both semiconducting materials enabled us to fabricate a functional p-n junction. Obtained results are promising for fabrication of optically transparent ZnO/BDD bipolar heterojunction.

  10. Separation of intra- and intergranular magnetotransport properties in nanocrystalline diamond films on the metallic side of the metal-insulator transition

    International Nuclear Information System (INIS)

    Janssens, S D; Pobedinskas, P; Ruttens, B; D'Haen, J; Nesladek, M; Haenen, K; Wagner, P; Vacik, J; Petrakova, V

    2011-01-01

    A systematic study on the morphology and electronic properties of thin heavily boron-doped nanocrystalline diamond (NCD) films is presented. The films have nominally the same thickness (∼150 nm) and are grown with a fixed B/C ratio (5000 ppm) but with different C/H ratios (0.5-5%) in the gas phase. The morphology of the films is investigated by x-ray diffraction and atomic force microscopy measurements, which confirm that lower C/H ratios lead to a larger average grain size. Magnetotransport measurements reveal a decrease in resistivity and a large increase in mobility, approaching the values obtained for single-crystal diamond as the average grain size of the films increases. In all films, the temperature dependence of resistivity decreases with larger grains and the charge carrier density and mobility are thermally activated. It is possible to separate the intra- and intergrain contributions for resistivity and mobility, which indicates that in these complex systems Matthiessen's rule is followed. The concentration of active charge carriers is reduced when the boron-doped NCD is grown with a lower C/H ratio. This is due to lower boron incorporation, which is confirmed by neutron depth profiling.

  11. Diamond anvil cells using boron-doped diamond electrodes covered with undoped diamond insulating layer

    Science.gov (United States)

    Matsumoto, Ryo; Yamashita, Aichi; Hara, Hiroshi; Irifune, Tetsuo; Adachi, Shintaro; Takeya, Hiroyuki; Takano, Yoshihiko

    2018-05-01

    Diamond anvil cells using boron-doped metallic diamond electrodes covered with undoped diamond insulating layers have been developed for electrical transport measurements under high pressure. These designed diamonds were grown on a bottom diamond anvil via a nanofabrication process combining microwave plasma-assisted chemical vapor deposition and electron beam lithography. The resistance measurements of a high-quality FeSe superconducting single crystal under high pressure were successfully demonstrated by just putting the sample and gasket on the bottom diamond anvil directly. The superconducting transition temperature of the FeSe single crystal was increased to up to 43 K by applying uniaxial-like pressure.

  12. Electron field emission for ultrananocrystalline diamond films

    Energy Technology Data Exchange (ETDEWEB)

    Krauss, A. R.; Auciello, O.; Ding, M. Q.; Gruen, D. M.; Huang, Y.; Zhirnov, V. V.; Givargizov, E. I.; Breskin, A.; Chechen, R.; Shefer, E. (and others)

    2001-03-01

    Ultrananocrystalline diamond (UNCD) films 0.1--2.4 {mu}m thick were conformally deposited on sharp single Si microtip emitters, using microwave CH{sub 4}--Ar plasma-enhanced chemical vapor deposition in combination with a dielectrophoretic seeding process. Field-emission studies exhibited stable, extremely high (60--100 {mu}A/tip) emission current, with little variation in threshold fields as a function of film thickness or Si tip radius. The electron emission properties of high aspect ratio Si microtips, coated with diamond using the hot filament chemical vapor deposition (HFCVD) process were found to be very different from those of the UNCD-coated tips. For the HFCVD process, there is a strong dependence of the emission threshold on both the diamond coating thickness and Si tip radius. Quantum photoyield measurements of the UNCD films revealed that these films have an enhanced density of states within the bulk diamond band gap that is correlated with a reduction in the threshold field for electron emission. In addition, scanning tunneling microscopy studies indicate that the emission sites from UNCD films are related to minima or inflection points in the surface topography, and not to surface asperities. These data, in conjunction with tight binding pseudopotential calculations, indicate that grain boundaries play a critical role in the electron emission properties of UNCD films, such that these boundaries: (a) provide a conducting path from the substrate to the diamond--vacuum interface, (b) produce a geometric enhancement in the local electric field via internal structures, rather than surface topography, and (c) produce an enhancement in the local density of states within the bulk diamond band gap.

  13. Fluorination of Boron-Doped Diamond Film Electrodes for Minimization of Perchlorate Formation.

    Science.gov (United States)

    Gayen, Pralay; Chaplin, Brian P

    2017-08-23

    This research investigated the effects of surface fluorination on both rates of organic compound oxidation (phenol and terephthalic acid (TA)) and ClO 4 - formation at boron-doped diamond (BDD) film anodes at 22 °C. Different fluorination methods (i.e., electrochemical oxidation with perfluorooctanoic acid (PFOA), radio frequency plasma, and silanization) were used to incorporate fluorinated moieties on the BDD surface, which was confirmed by X-ray photoelectron spectroscopy (XPS). The silanization method was found to be the most effective fluorination method using a 1H,1H,2H,2H-perfluorodecyltrichlorosilane precursor to form a self-assembled monolayer (SAM) on the oxygenated BDD surface. The ClO 4 - formation decreased from rates of 0.45 ± 0.03 mmol m -2 min -1 during 1 mM NaClO 3 oxidation and 0.28 ± 0.01 mmol m -2 min -1 during 10 mM NaCl oxidation on the BDD electrode to below detectable levels (layer on the BDD surface that inhibited charge transfer via steric hindrance and hydrophobic effects. The surface coverages and thicknesses of the fluorinated films controlled the charge transfer rates, which was confirmed by estimates of film thicknesses using XPS and density functional theory simulations. The aliphatic silanized electrode also showed very high stability during OH • production. Perchlorate formation rates were below the detection limit (<0.12 μmoles m -2 min -1 ) for up to 10 consecutive NaClO 3 oxidation experiments.

  14. Ultraviolet photosensitivity of sulfur-doped micro- and nano-crystalline diamond

    International Nuclear Information System (INIS)

    Mendoza, Frank; Makarov, Vladimir; Hidalgo, Arturo; Weiner, Brad; Morell, Gerardo

    2011-01-01

    The room-temperature photosensitivity of sulfur-doped micro- (MCD), submicro- (SMCD) and nano- (NCD) crystalline diamond films synthesized by hot-filament chemical vapor deposition was studied. The structure and composition of these diamond materials were characterized by Raman spectroscopy, scanning electron microscopy and X-ray diffraction. The UV sensitivity and response time were studied for the three types of diamond materials using a steady state broad UV excitation source and two pulsed UV laser radiations. It was found that they have high sensitivity in the UV region, as high as 10 9 sec -1 mV -1 range, linear response in a broad spectral range below 320 nm, photocurrents around ∼10 -5 A, and short response time better than 100 ns, which is independent of fluency intensity. A phenomenological model was applied to help understand the role of defects and dopant concentration on the materials' photosensitivity

  15. Structure, adhesive strength and electrochemical performance of nitrogen doped diamond-like carbon thin films deposited via DC magnetron sputtering.

    Science.gov (United States)

    Khun, N W; Liu, E; Krishna, M D

    2010-07-01

    Nitrogen doped diamond-like carbon (DLC:N) thin films were deposited on p-Si (100) substrates by DC magnetron sputtering with different nitrogen flow rates at a substrate temperature of about 100 degrees C. The chemical bonding structure of the films was characterized by X-ray photoelectron spectroscopy (XPS) and micro-Raman spectroscopy. The adhesive strength and surface morphology of the films were studied using micro-scratch tester and scanning electron microscope (SEM), respectively. The electrochemical performance of the films was evaluated by potentiodynamic polarization testing and linear sweep voltammetry. The electrolytes used for the electrochemical tests were deaerated and unstirred 0.47 M KCl aqueous solution for potentiodynamic polarization testing and 0.2 M KOH and 0.1 M KCl solutions for voltammetric analysis. It was found that the DLC:N films could well passivate the underlying substrates though the corrosion resistance of the films decreased with increased nitrogen content in the films. The DLC:N films showed wide potential windows in the KOH solution, in which the detection ability of the DLC:N films to trace lead of about 1 x 10(-3) M Pb(2+) was also tested.

  16. Thermal diffusion boron doping of single-crystal natural diamond

    Energy Technology Data Exchange (ETDEWEB)

    Seo, Jung-Hun; Mikael, Solomon; Mi, Hongyi; Venkataramanan, Giri; Ma, Zhenqiang, E-mail: mazq@engr.wisc.edu [Department of Electrical and Computer Engineering, University of Wisconsin-Madison, Madison, Wisconsin 53706 (United States); Wu, Henry; Morgan, Dane [Department of Materials Science and Engineering, University of Wisconsin-Madison, Madison, Wisconsin 53706 (United States); Blanchard, James P. [Department of Nuclear Engineering and Engineering Physics, University of Wisconsin-Madison, Madison, Wisconsin 53706 (United States); Zhou, Weidong [Department of Electrical Engineering, NanoFAB Center, University of Texas at Arlington, Arlington, Texas 76019 (United States); Gong, Shaoqin [Department of Biomedical Engineering and Wisconsin Institute for Discovery, University of Wisconsin-Madison, Madison, Wisconsin 53706 (United States)

    2016-05-28

    With the best overall electronic and thermal properties, single crystal diamond (SCD) is the extreme wide bandgap material that is expected to revolutionize power electronics and radio-frequency electronics in the future. However, turning SCD into useful semiconductors requires overcoming doping challenges, as conventional substitutional doping techniques, such as thermal diffusion and ion implantation, are not easily applicable to SCD. Here we report a simple and easily accessible doping strategy demonstrating that electrically activated, substitutional doping in SCD without inducing graphitization transition or lattice damage can be readily realized with thermal diffusion at relatively low temperatures by using heavily doped Si nanomembranes as a unique dopant carrying medium. Atomistic simulations elucidate a vacancy exchange boron doping mechanism that occurs at the bonded interface between Si and diamond. We further demonstrate selectively doped high voltage diodes and half-wave rectifier circuits using such doped SCD. Our new doping strategy has established a reachable path toward using SCDs for future high voltage power conversion systems and for other novel diamond based electronic devices. The novel doping mechanism may find its critical use in other wide bandgap semiconductors.

  17. Thermal diffusion boron doping of single-crystal natural diamond

    International Nuclear Information System (INIS)

    Seo, Jung-Hun; Mikael, Solomon; Mi, Hongyi; Venkataramanan, Giri; Ma, Zhenqiang; Wu, Henry; Morgan, Dane; Blanchard, James P.; Zhou, Weidong; Gong, Shaoqin

    2016-01-01

    With the best overall electronic and thermal properties, single crystal diamond (SCD) is the extreme wide bandgap material that is expected to revolutionize power electronics and radio-frequency electronics in the future. However, turning SCD into useful semiconductors requires overcoming doping challenges, as conventional substitutional doping techniques, such as thermal diffusion and ion implantation, are not easily applicable to SCD. Here we report a simple and easily accessible doping strategy demonstrating that electrically activated, substitutional doping in SCD without inducing graphitization transition or lattice damage can be readily realized with thermal diffusion at relatively low temperatures by using heavily doped Si nanomembranes as a unique dopant carrying medium. Atomistic simulations elucidate a vacancy exchange boron doping mechanism that occurs at the bonded interface between Si and diamond. We further demonstrate selectively doped high voltage diodes and half-wave rectifier circuits using such doped SCD. Our new doping strategy has established a reachable path toward using SCDs for future high voltage power conversion systems and for other novel diamond based electronic devices. The novel doping mechanism may find its critical use in other wide bandgap semiconductors.

  18. Electrochemical Biosensor Based on Boron-Doped Diamond Electrodes with Modified Surfaces

    OpenAIRE

    Yu, Yuan; Zhou, Yanli; Wu, Liangzhuan; Zhi, Jinfang

    2012-01-01

    Boron-doped diamond (BDD) thin films, as one kind of electrode materials, are superior to conventional carbon-based materials including carbon paste, porous carbon, glassy carbon (GC), carbon nanotubes in terms of high stability, wide potential window, low background current, and good biocompatibility. Electrochemical biosensor based on BDD electrodes have attracted extensive interests due to the superior properties of BDD electrodes and the merits of biosensors, such as specificity, sensitiv...

  19. Structure and properties of diamond and diamond-like films

    Energy Technology Data Exchange (ETDEWEB)

    Clausing, R.E. [Oak Ridge National Lab., TN (United States)

    1993-01-01

    This section is broken into four parts: (1) introduction, (2) natural IIa diamond, (3) importance of structure and composition, and (4) control of structure and properties. Conclusions of this discussion are that properties of chemical vapor deposited diamond films can compare favorably with natural diamond, that properties are anisotropic and are a strong function of structure and crystal perfection, that crystal perfection and morphology are functions of growth conditions and can be controlled, and that the manipulation of texture and thereby surface morphology and internal crystal perfection is an important step in optimizing chemically deposited diamond films for applications.

  20. Microstructure and high-temperature tribological properties of Si-doped hydrogenated diamond-like carbon films

    Science.gov (United States)

    Zhang, Teng Fei; Wan, Zhi Xin; Ding, Ji Cheng; Zhang, Shihong; Wang, Qi Min; Kim, Kwang Ho

    2018-03-01

    Si-doped DLC films have attracted great attention for use in tribological applications. However, their high-temperature tribological properties remain less investigated, especially in harsh oxidative working conditions. In this study, Si-doped hydrogenated DLC films with various Si content were synthesized and the effects of the addition of Si on the microstructural, mechanical and high-temperature tribological properties of the films were investigated. The results indicate that Si doping leads to an obvious increase in the sp3/sp2 ratio of DLC films, likely due to the silicon atoms preferentially substitute the sp2-hybridized carbon atoms and augment the number of sp3 sites. With Si doping, the mechanical properties, including hardness and adhesion strength, were improved, while the residual stress of the DLC films was reduced. The addition of Si leads to higher thermal and mechanical stability of DLC films because the Si atoms inhibit the graphitization of the films at an elevated temperature. Better high-temperature tribological properties of the Si-DLC films under oxidative conditions were observed, which can be attributed to the enhanced thermal stability and formation of a Si-containing lubricant layer on the surfaces of the wear tracks. The nano-wear resistance of the DLC films was also improved by Si doping.

  1. Preparation of TiO{sub 2}/boron-doped diamond/Ta multilayer films and use as electrode materials for supercapacitors

    Energy Technology Data Exchange (ETDEWEB)

    Shi, Chao, E-mail: sc_sq1988@163.com [Tianjin Key Laboratory of Film Electronic and Communicate Devices, School of Electronics Information Engineering, Tianjin University of Technology, Tianjin 300384 (China); Li, Hongji, E-mail: hongjili@yeah.net [Tianjin Key Laboratory of Organic Solar Cells and Photochemical Conversion, School of Chemistry and Chemical Engineering, Tianjin University of Technology, Tianjin 300384 (China); Li, Cuiping, E-mail: licp226@126.com [Tianjin Key Laboratory of Film Electronic and Communicate Devices, School of Electronics Information Engineering, Tianjin University of Technology, Tianjin 300384 (China); Li, Mingji, E-mail: limingji@163.com [Tianjin Key Laboratory of Film Electronic and Communicate Devices, School of Electronics Information Engineering, Tianjin University of Technology, Tianjin 300384 (China); Qu, Changqing, E-mail: quchangqing@tjut.edu.cn [Tianjin Key Laboratory of Film Electronic and Communicate Devices, School of Electronics Information Engineering, Tianjin University of Technology, Tianjin 300384 (China); Yang, Baohe, E-mail: bhyang207@163.com [Tianjin Key Laboratory of Film Electronic and Communicate Devices, School of Electronics Information Engineering, Tianjin University of Technology, Tianjin 300384 (China)

    2015-12-01

    Highlights: • BDD film was deposited on Ta substrate by hot filament CVD method. • Ti layer was deposited on BDD film by radio frequency magnetron sputtering. • Nanostructured TiO{sub 2}/BDD/nanoporous Ta films were prepared. • The films exhibit good capacitance performance and excellent stability. - Abstract: We report nanostructured TiO{sub 2}/boron-doped diamond (BDD)/Ta multilayer films and their electrochemical performances as supercapacitor electrodes. The BDD films were grown on Ta substrates using electron-assisted hot filament chemical vapor deposition. Ti metal layers were deposited on the BDD surfaces by radio frequency magnetron sputtering, and nanostructured TiO{sub 2}/BDD/Ta thin films were prepared by electrochemical etching and thermal annealing. The successful formation of TiO{sub 2} and Ta layered nanostructures was demonstrated using scanning electron and transmission electron microscopies. The electrochemical responses of these electrodes were evaluated by examining their use as electrical double-layer capacitors, using cyclic voltammetry, and galvanostatic charge/discharge and impedance measurements. When the TiO{sub 2}/BDD/Ta film was used as the working electrode with 0.1 M Na{sub 2}SO{sub 4} as the electrolyte, the capacitor had a specific capacitance of 5.23 mF cm{sup −2} at a scan rate of 5 mV s{sup −1} for a B/C ratio of 0.1% w/w. Furthermore, the TiO{sub 2}/BDD/Ta film had improved electrochemical stability, with a retention of 89.3% after 500 cycles. This electrochemical behavior is attributed to the quality of the BDD, the surface roughness and electrocatalytic activities of the TiO{sub 2} layer and Ta nanoporous structures, and the synergies between them. These results show that TiO{sub 2}/BDD/Ta films are promising as capacitor electrodes for special applications.

  2. Hole states in diamond p-delta-doped field effect transistors

    International Nuclear Information System (INIS)

    Martinez-Orozco, J C; Rodriguez-Vargas, I; Mora-Ramos, M E

    2009-01-01

    The p-delta-doping in diamond allows to create high density two-dimensional hole gases. This technique has already been applied in the design and fabrication of diamond-based field effect transistors. Consequently, the knowledge of the electronic structure is of significant importance to understand the transport properties of diamond p-delta-doped systems. In this work the hole subbands of diamond p-type delta-doped quantum wells are studied within the framework of a local-density Thomas-Fermi-based approach for the band bending profile. The calculation incorporates an independent three-hole-band scheme and considers the effects of the contact potential, the delta-channel to contact distance, and the ionized impurity density.

  3. Hole states in diamond p-delta-doped field effect transistors

    Energy Technology Data Exchange (ETDEWEB)

    Martinez-Orozco, J C; Rodriguez-Vargas, I [Unidad Academica de Fisica, Universidad Autonoma de Zacatecas, Calzada Solidaridad Esquina con Paseo la Bufa S/N, CP 98060 Zacatecas, ZAC. (Mexico); Mora-Ramos, M E, E-mail: jcmover@correo.unam.m [Facultad de Ciencias, Universidad Autonoma del Estado de Morelos, Av. Universidad 1001, Col. Chamilpa, CP 62209 Cuernavaca, MOR. (Mexico)

    2009-05-01

    The p-delta-doping in diamond allows to create high density two-dimensional hole gases. This technique has already been applied in the design and fabrication of diamond-based field effect transistors. Consequently, the knowledge of the electronic structure is of significant importance to understand the transport properties of diamond p-delta-doped systems. In this work the hole subbands of diamond p-type delta-doped quantum wells are studied within the framework of a local-density Thomas-Fermi-based approach for the band bending profile. The calculation incorporates an independent three-hole-band scheme and considers the effects of the contact potential, the delta-channel to contact distance, and the ionized impurity density.

  4. Toroidal plasma enhanced CVD of diamond films

    International Nuclear Information System (INIS)

    Zvanya, John; Cullen, Christopher; Morris, Thomas; Krchnavek, Robert R.; Holber, William; Basnett, Andrew; Basnett, Robert; Hettinger, Jeffrey

    2014-01-01

    An inductively coupled toroidal plasma source is used as an alternative to microwave plasmas for chemical vapor deposition of diamond films. The source, operating at a frequency of 400 kHz, synthesizes diamond films from a mixture of argon, methane, and hydrogen. The toroidal design has been adapted to create a highly efficient environment for diamond film deposition: high gas temperature and a short distance from the sample to the plasma core. Using a toroidal plasma geometry operating in the medium frequency band allows for efficient (≈90%) coupling of AC line power to the plasma and a scalable path to high-power and large-area operation. In test runs, the source generates a high flux of atomic hydrogen over a large area, which is favorable for diamond film growth. Using a deposition temperature of 900–1050 °C and a source to sample distance of 0.1–2.0 cm, diamond films are deposited onto silicon substrates. The results showed that the deposition rate of the diamond films could be controlled using the sample temperature and source to sample spacing. The results also show the films exhibit good-quality polycrystalline diamond as verified by Raman spectroscopy, x-ray diffraction, and scanning electron microscopy. The scanning electron microscopy and x-ray diffraction results show that the samples exhibit diamond (111) and diamond (022) crystallites. The Raman results show that the sp 3 peak has a narrow spectral width (FWHM 12 ± 0.5 cm −1 ) and that negligible amounts of the sp 2 band are present, indicating good-quality diamond films

  5. Superconductivity and low temperature electrical transport in B-doped CVD nanocrystalline diamond

    Czech Academy of Sciences Publication Activity Database

    Nesládek, M.; Mareš, Jiří J.; Tromson, D.; Mer, Ch.; Bergonzo, P.; Hubík, Pavel; Krištofik, Jozef

    2006-01-01

    Roč. 7, Suppl. 1 (2006), S41-S44 ISSN 1468-6996 R&D Projects: GA ČR(CZ) GA202/06/0040 Institutional research plan: CEZ:AV0Z10100521 Keywords : superconductivity * electrical transport * doping * CVD diamond Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 1.124, year: 2006

  6. Surface smoothening effects on growth of diamond films

    Science.gov (United States)

    Reshi, Bilal Ahmad; Kumar, Shyam; Kartha, Moses J.; Varma, Raghava

    2018-04-01

    We have carried out a detailed study of the growth dynamics of the diamond film during initial time on diamond substrates. The diamond films are deposited using Microwave Plasma Chemical Vapor Deposition (MPCVD) method for different times. Surface morphology and its correlation with the number of hours of growth of thin films was invested using atomic force microscopy (AFM). Diamond films have smooth interface with average roughness of 48.6873nm. The initial growth dynamics of the thin film is investigated. Interestingly, it is found that there is a decrease in the surface roughness of the film. Thus a smoothening effect is observed in the grown films. The film enters into the growth regime in the later times. Our results also find application in building diamond detector.

  7. Growth, characterization, and device development in monocrystalline diamond films

    Science.gov (United States)

    Davis, Robert F.

    1991-12-01

    The nucleation of diamond grains on an unscratched silicon wafer is enhanced by four order of magnitude relative to scratched substrates by using negative bias enhanced microwave plasma CVD in a 2 percent methane/hydrogen plasma for an initial period. In vacuo surface analysis has revealed that the actual nucleation occurs on the amorphous C coating present on the thin SiC layer which forms as the product of the initial reaction with the Si surface. It is believed that the C forms critical clusters which are favorable for diamond nucleation. Similar enhancement was observed together with the occurrence of textured diamond films in the use of bias pretreatment of cubic Beta SiC substrates. Approximately 50 percent of the initial diamond nuclei were aligned with the SiC substrate. In contrast, the use of the biasing pretreatment for one hour on polycrystalline substrates resulted in only about 7 percent coverage with diamond particles. Numerous techniques have been used to analyze the nucleation and growth phenomena, especially micro Raman and scanning tunneling microscopy. The latter technique has shown that the morphology of doped and undoped diamond nuclei are similar, as well as the fact that significant concentrations of vacancy related defects are present. In device related-studies, UV-photoemission studies have shown that TiC occurs at the Ti-diamond (100) interface after a 400 C anneal. The Schottky barrier height from this metal on p-type diamond was determined to be 1.0 eV. Indications of negative electron affinity (NEA) was observed and attributed to emission of electrons that are quasi-thermalized to the bottom of the conduction band. A disordered surface removes the NEA. The microwave performance of p-type (beta-doped) diamond MESFET's at 10 GHz has been further investigated. Elevated temperatures may be necessary to obtain sufficient free charge densities in the conducting channel but this will result in degraded device performance. Each of these

  8. Nanocrystalline diamond films for biomedical applications

    DEFF Research Database (Denmark)

    Pennisi, Cristian Pablo; Alcaide, Maria

    2014-01-01

    Nanocrystalline diamond films, which comprise the so called nanocrystalline diamond (NCD) and ultrananocrystalline diamond (UNCD), represent a class of biomaterials possessing outstanding mechanical, tribological, and electrical properties, which include high surface smoothness, high corrosion...... performance of nanocrystalline diamond films is reviewed from an application-specific perspective, covering topics such as enhancement of cellular adhesion, anti-fouling coatings, non-thrombogenic surfaces, micropatterning of cells and proteins, and immobilization of biomolecules for bioassays. In order...

  9. Mercury-free sono-electroanalytical detection of lead in human blood by use of bismuth-film-modified boron-doped diamond electrodes

    Energy Technology Data Exchange (ETDEWEB)

    Kruusma, Jaanus [Institute of Physical Chemistry, University of Tartu, Jakobi 2, 51013, Tartu (Estonia); Banks, Craig E.; Compton, Richard G. [Physical and Theoretical Chemistry Laboratory, Oxford University, South Parks Road, OX1 3QZ, Oxford (United Kingdom)

    2004-06-01

    We report the electroanalytical determination of lead by anodic stripping voltammetry at in-situ-formed, bismuth-film-modified, boron-doped diamond electrodes. Detection limits in 0.1 mol L{sup -1} nitric acid solution of 9.6x10{sup -8} mol L{sup -1} (0.2 ppb) and 1.1x10{sup -8} mol L{sup -1} (2.3 ppb) were obtained after 60 and 300 s deposition times, respectively. An acoustically assisted deposition procedure was also investigated and found to result in improved limits of detection of 2.6 x 10{sup -8} mol L{sup -1} (5.4 ppb) and 8.5 x 10{sup -10} mol L{sup -1} (0.18 ppb) for 60 and 300 s accumulation times, respectively. Furthermore, the sensitivity obtained under quiescent and insonated conditions increased from 5.5 (quiescent) to 76.7 A mol{sup -1} L (insonated) for 60 s accumulation and from 25.8 (quiescent) to 317.6 A mol{sup -1} L (insonated) for 300 s accumulation. Investigation of the use of ultrasound with diluted blood revealed detection limits of the order of 10{sup -8} mol L{sup -1} were achievable with excellent inter- and intra-reproducibility and sensitivity of 411.9 A mol{sup -1} L. For the first time, electroanalytical detection of lead in diluted blood is shown to be possible by use of insonated in-situ-formed bismuth-film-modified boron-doped diamond electrodes. This method is a rapid, sensitive, and non-toxic means of clinical sensing of lead in whole human blood. (orig.)

  10. Energy gap and surface structure of superconducting diamond films probed by scanning tunneling microscopy

    International Nuclear Information System (INIS)

    Nishizaki, Terukazu; Takano, Yoshihiko; Nagao, Masanori; Takenouchi, Tomohiro; Kawarada, Hiroshi; Kobayashi, Norio

    2007-01-01

    We have performed scanning tunneling microscopy/spectroscopy (STM/STS) experiments on (1 1 1)-oriented epitaxial films of heavily boron-doped diamond at T = 0.47 K. The STM topography shows two kinds of atomic structures: a hydrogenated 1 x 1 structure, C(1 1 1)1 x 1:H, and an amorphous structure. On the C(1 1 1)1 x 1:H region, the tunneling spectra show superconducting property with the energy gap Δ = 0.83 meV. The obtained gap ratio 2Δ/k B T c = 3.57 is consistent with the weak-coupling BCS theory

  11. Boron doped diamond electrode for the wastewater treatment

    International Nuclear Information System (INIS)

    Quiroz Alfaro, Marco Antonio; Ferro, Sergio; Martinez-Huitle, Carlos Alberto; Vong, Yunny Meas

    2006-01-01

    Electrochemical studies of diamond were started more than fifteen years ago with the first paper on diamond electrochemistry published by Pleskov. After that, work started in Japan, United States of America, France, Switzerland and other countries. Over the last few years, the number of publications has increased considerably. Diamond films have been the subject of applications and fundamental research in electrochemistry, opening up a new branch known as the electrochemistry of diamond electrodes. Here, we first present a brief history and the process of diamond film synthesis. The principal objective of this work is to summarize the most important results in the electrochemical oxidation using diamond electrodes. (author)

  12. Boron doped diamond electrode for the wastewater treatment

    Directory of Open Access Journals (Sweden)

    Alfaro Marco Antonio Quiroz

    2006-01-01

    Full Text Available Electrochemical studies of diamond were started more than fifteen years ago with the first paper on diamond electrochemistry published by Pleskov. After that, work started in Japan, United States of America, France, Switzerland and other countries. Over the last few years, the number of publications has increased considerably. Diamond films have been the subject of applications and fundamental research in electrochemistry, opening up a new branch known as the electrochemistry of diamond electrodes. Here, we first present a brief history and the process of diamond film synthesis. The principal objective of this work is to summarize the most important results in the electrochemical oxidation using diamond electrodes.

  13. Effects of ultraviolet light on B-doped CdS thin films prepared by spray pyrolysis method using perfume atomizer

    Science.gov (United States)

    Novruzov, V. D.; Keskenler, E. F.; Tomakin, M.; Kahraman, S.; Gorur, O.

    2013-09-01

    Boron doped CdS thin films were deposited by spray pyrolysis method using perfume atomizer. The effects of ultraviolet light on the structural, optical and electrical properties of B-doped CdS thin films were investigated as a function of dopant concentration (B/Cd). X-ray diffraction studies showed that all samples were polycrystalline nature with hexagonal structure. It was determined that the preferred orientation of non-illuminated samples changes from (1 0 1) to (0 0 2) with B concentration. The c lattice constant of films decreases from 6.810 Å to 6.661 Å with boron doping. The XRD peak intensity increased with the illumination for almost all the samples. The lattice parameters of B-doped samples remained nearly constant after illumination. It was found that the optical transmittance, photoluminescence spectra, resistivity and carrier concentration of the B-doped samples are stable after the illumination with UV light. Also the effects of UV light on B-doped CdS/Cu2S solar cell were investigated and it was determined that photoelectrical parameters of B-doped solar cell were more durable against the UV light.

  14. Effects of ultraviolet light on B-doped CdS thin films prepared by spray pyrolysis method using perfume atomizer

    Energy Technology Data Exchange (ETDEWEB)

    Novruzov, V.D. [Department of Physics, Recep Tayyip Erdogan University, Rize (Turkey); Keskenler, E.F., E-mail: keskenler@gmail.com [Department of Nanotechnology Engineering, Recep Tayyip Erdogan University, Rize (Turkey); Tomakin, M. [Department of Physics, Recep Tayyip Erdogan University, Rize (Turkey); Kahraman, S. [Department of Physics, Mustafa Kemal University, Hatay (Turkey); Gorur, O. [Department of Physics, Abant Izzet Baysal University, Bolu (Turkey)

    2013-09-01

    Boron doped CdS thin films were deposited by spray pyrolysis method using perfume atomizer. The effects of ultraviolet light on the structural, optical and electrical properties of B-doped CdS thin films were investigated as a function of dopant concentration (B/Cd). X-ray diffraction studies showed that all samples were polycrystalline nature with hexagonal structure. It was determined that the preferred orientation of non-illuminated samples changes from (1 0 1) to (0 0 2) with B concentration. The c lattice constant of films decreases from 6.810 Å to 6.661 Å with boron doping. The XRD peak intensity increased with the illumination for almost all the samples. The lattice parameters of B-doped samples remained nearly constant after illumination. It was found that the optical transmittance, photoluminescence spectra, resistivity and carrier concentration of the B-doped samples are stable after the illumination with UV light. Also the effects of UV light on B-doped CdS/Cu{sub 2}S solar cell were investigated and it was determined that photoelectrical parameters of B-doped solar cell were more durable against the UV light.

  15. Electrochemically assisted deposition of hydroxyapatite on Ti6Al4V substrates covered by CVD diamond films — Coating characterization and first cell biological results

    Energy Technology Data Exchange (ETDEWEB)

    Strąkowska, Paulina [Gdańsk University of Technology, Mechanical Engineering Faculty (Poland); Gdańsk University of Technology, Faculty of Electronics, Telecommunications, and Informatics (Poland); Beutner, René [Max Bergmann Center, Technische Universität Dresden (Germany); Gnyba, Marcin [Gdańsk University of Technology, Faculty of Electronics, Telecommunications, and Informatics (Poland); Zielinski, Andrzej [Gdańsk University of Technology, Mechanical Engineering Faculty (Poland); Scharnweber, Dieter, E-mail: Dieter.Scharnweber@tu-dresden.de [Max Bergmann Center, Technische Universität Dresden (Germany)

    2016-02-01

    Although titanium and its alloys are widely used as implant material for orthopedic and dental applications they show only limited corrosion stability and osseointegration in different cases. The aim of the presented research was to develop and characterize a novel surface modification system from a thin diamond base layer and a hydroxyapatite (HAp) top coating deposited on the alloy Ti6Al4V widely used for implants in contact with bone. This coating system is expected to improve both the long-term corrosion behavior and the biocompatibility and bioactivity of respective surfaces. The diamond base films were obtained by Microwave Plasma Assisted Chemical Vapor Deposition (MW-PACVD); the HAp coatings were formed in aqueous solutions by electrochemically assisted deposition (ECAD) at varying polarization parameters. Scanning electron microscopy (SEM), Raman microscopy, and electrical conductivity measurements were applied to characterize the generated surface states; the calcium phosphate coatings were additionally chemically analyzed for their composition. The biological properties of the coating system were assessed using hMSC cells analyzing for cell adhesion, proliferation, and osteogenic differentiation. Varying MW-PACVD process conditions resulted in composite coatings containing microcrystalline diamond (MCD/Ti-C), nanocrystalline diamond (NCD), and boron-doped nanocrystalline diamond (B-NCD) with the NCD coatings being dense and homogeneous and the B-NCD coatings showing increased electrical conductivity. The ECAD process resulted in calcium phosphate coatings from stoichiometric and non-stoichiometric HAp. The deposition of HAp on the B-NCD films run at lower cathodic potentials and resulted both in the highest coating mass and the most homogenous appearance. Initial cell biological investigations showed an improved cell adhesion in the order B-NCD > HAp/B-NCD > uncoated substrate. Cell proliferation was improved for both investigated coatings whereas ALP

  16. Electrochemically assisted deposition of hydroxyapatite on Ti6Al4V substrates covered by CVD diamond films — Coating characterization and first cell biological results

    International Nuclear Information System (INIS)

    Strąkowska, Paulina; Beutner, René; Gnyba, Marcin; Zielinski, Andrzej; Scharnweber, Dieter

    2016-01-01

    Although titanium and its alloys are widely used as implant material for orthopedic and dental applications they show only limited corrosion stability and osseointegration in different cases. The aim of the presented research was to develop and characterize a novel surface modification system from a thin diamond base layer and a hydroxyapatite (HAp) top coating deposited on the alloy Ti6Al4V widely used for implants in contact with bone. This coating system is expected to improve both the long-term corrosion behavior and the biocompatibility and bioactivity of respective surfaces. The diamond base films were obtained by Microwave Plasma Assisted Chemical Vapor Deposition (MW-PACVD); the HAp coatings were formed in aqueous solutions by electrochemically assisted deposition (ECAD) at varying polarization parameters. Scanning electron microscopy (SEM), Raman microscopy, and electrical conductivity measurements were applied to characterize the generated surface states; the calcium phosphate coatings were additionally chemically analyzed for their composition. The biological properties of the coating system were assessed using hMSC cells analyzing for cell adhesion, proliferation, and osteogenic differentiation. Varying MW-PACVD process conditions resulted in composite coatings containing microcrystalline diamond (MCD/Ti-C), nanocrystalline diamond (NCD), and boron-doped nanocrystalline diamond (B-NCD) with the NCD coatings being dense and homogeneous and the B-NCD coatings showing increased electrical conductivity. The ECAD process resulted in calcium phosphate coatings from stoichiometric and non-stoichiometric HAp. The deposition of HAp on the B-NCD films run at lower cathodic potentials and resulted both in the highest coating mass and the most homogenous appearance. Initial cell biological investigations showed an improved cell adhesion in the order B-NCD > HAp/B-NCD > uncoated substrate. Cell proliferation was improved for both investigated coatings whereas ALP

  17. Undoped CVD diamond films for electrochemical applications

    International Nuclear Information System (INIS)

    Mosinska, Lidia; Fabisiak, Kazimierz; Paprocki, Kazimierz; Kowalska, Magdalena; Popielarski, Pawel; Szybowicz, Miroslaw

    2013-01-01

    By using different deposition conditions, the CVD diamond films with different qualities and orientation were grown by the hot-filament CVD technique. The object of this article is to summarize and discuss relation between structural, physical and electrochemical properties of different diamond electrodes. The physical properties of the Hot Filament CVD microcrystalline diamond films are analyzed by scanning electron microscopy and Raman spectroscopy. In presented studies two different electrodes were used of the diamond grain sizes around 200 nm and 10 μm, as it was estimated from SEM picture. The diamond layers quality was checked on basis of FWHM (Full width at Half Maximum) of 1332 cm −1 diamond Raman peak. The ratio of sp 3 /sp 2 carbon bonds was determined by 1550 cm −1 G band and 1350 cm −1 D band in the Raman spectrum. The electrochemical properties were analyzed using (CV) cyclic voltammetry measurements in aqueous solutions. The sensitivity of undoped diamond electrodes depends strongly on diamond film quality and concentration of amorphous carbon phase in the diamond layer

  18. Investigation of structure, adhesion strength, wear performance and corrosion behavior of platinum/ruthenium/nitrogen doped diamond-like carbon thin films with respect to film thickness

    Energy Technology Data Exchange (ETDEWEB)

    Khun, N.W. [School of Mechanical and Aerospace Engineering, Nanyang Technological University, 50 Nanyang Avenue, Singapore 639798 (Singapore); Liu, E., E-mail: MEJLiu@ntu.edu.sg [School of Mechanical and Aerospace Engineering, Nanyang Technological University, 50 Nanyang Avenue, Singapore 639798 (Singapore)

    2011-03-15

    Research highlights: {yields} Sputtered PtRuN-DLC thin films were fabricated with different film thicknesses. {yields} The graphitization of the films increased with increased film thickness. {yields} The wear resistance of the films increased though their adhesion strength decreased. {yields} The corrosion potentials of the films shifted to more negative values. {yields} However, the corrosion currents of the films decreased. - Abstract: In this study, the corrosion performance of platinum/ruthenium/nitrogen doped diamond-like carbon (PtRuN-DLC) thin films deposited on p-Si substrates using a DC magnetron sputtering deposition system in a 0.1 M NaCl solution was investigated using potentiodynamic polarization test in terms of film thickness. The effect of the film thickness on the chemical composition, bonding structure, surface morphology, adhesion strength and wear resistance of the PtRuN-DLC films was studied using X-ray photoelectron spectroscopy (XPS), micro-Raman spectroscopy, atomic force microscopy (AFM), micro-scratch test and ball-on-disc tribotest, respectively. It was found that the wear resistance of the PtRuN-DLC films apparently increased with increased film thickness though the adhesion strength of the films decreased. The corrosion results revealed that the increased concentration of sp{sup 2} bonds in the PtRuN-DLC films with increased film thickness shifted the corrosion potentials of the films to more negative values but the decreased porosity density in the films significantly decreased the corrosion currents of the films.

  19. Investigation of structure, adhesion strength, wear performance and corrosion behavior of platinum/ruthenium/nitrogen doped diamond-like carbon thin films with respect to film thickness

    International Nuclear Information System (INIS)

    Khun, N.W.; Liu, E.

    2011-01-01

    Research highlights: → Sputtered PtRuN-DLC thin films were fabricated with different film thicknesses. → The graphitization of the films increased with increased film thickness. → The wear resistance of the films increased though their adhesion strength decreased. → The corrosion potentials of the films shifted to more negative values. → However, the corrosion currents of the films decreased. - Abstract: In this study, the corrosion performance of platinum/ruthenium/nitrogen doped diamond-like carbon (PtRuN-DLC) thin films deposited on p-Si substrates using a DC magnetron sputtering deposition system in a 0.1 M NaCl solution was investigated using potentiodynamic polarization test in terms of film thickness. The effect of the film thickness on the chemical composition, bonding structure, surface morphology, adhesion strength and wear resistance of the PtRuN-DLC films was studied using X-ray photoelectron spectroscopy (XPS), micro-Raman spectroscopy, atomic force microscopy (AFM), micro-scratch test and ball-on-disc tribotest, respectively. It was found that the wear resistance of the PtRuN-DLC films apparently increased with increased film thickness though the adhesion strength of the films decreased. The corrosion results revealed that the increased concentration of sp 2 bonds in the PtRuN-DLC films with increased film thickness shifted the corrosion potentials of the films to more negative values but the decreased porosity density in the films significantly decreased the corrosion currents of the films.

  20. Synthesis and characterization of boron incorporated diamond-like carbon thin films

    International Nuclear Information System (INIS)

    Zhang, L.L.; Yang, Q.; Tang, Y.; Yang, L.; Zhang, C.; Hu, Y.; Cui, X.

    2015-01-01

    Boron incorporated diamond-like carbon (B-DLC) (up to 8 wt.% boron) thin films were synthesized on silicon wafers using biased target ion beam deposition technique, where diamond-like carbon (DLC) was deposited by ion beam deposition and boron (B) was simultaneously incorporated by biased target sputtering of a boron carbide (B 4 C) target under different conditions. Pure DLC films and B–C films were also synthesized by ion beam deposition and biased target sputtering of B 4 C under similar conditions, respectively, as reference samples. The microstructure and mechanical properties of the synthesized films have been characterized by various technologies. It has been found that B exists in different states in B-DLC, including carbon-rich and B-rich boron carbides, boron suboxide and boron oxide, and the oxidation of B probably occurs during the film deposition. The incorporation of B into DLC leads to the increase of sp 3 bonded carbon in the films, the increase of both film hardness and elastic modulus, and the decrease of both surface roughness and friction coefficient. Furthermore, the content of sp 3 bonded carbon, film hardness and elastic modulus increase, and the film surface roughness and friction coefficient decrease with the increase of B-rich carbide in the B-DLC films. - Highlights: • Biased target ion beam deposition technique is promising to produce high quality DLC based thin films; • Boron exists in different states in B-DLC thin films; • The incorporation of B to DLC with different levels leads to improved film properties; • The fraction of sp 3 bonded C in B-DLC thin films increase with the increase of B-rich carbide content in the films

  1. Beta Radiation Enhanced Thermionic Emission from Diamond Thin Films

    Directory of Open Access Journals (Sweden)

    Alex Croot

    2017-11-01

    Full Text Available Diamond-based thermionic emission devices could provide a means to produce clean and renewable energy through direct heat-to-electrical energy conversion. Hindering progress of the technology are the thermionic output current and threshold temperature of the emitter cathode. In this report, we study the effects on thermionic emission caused by in situ exposure of the diamond cathode to beta radiation. Nitrogen-doped diamond thin films were grown by microwave plasma chemical vapor deposition on molybdenum substrates. The hydrogen-terminated nanocrystalline diamond was studied using a vacuum diode setup with a 63Ni beta radiation source-embedded anode, which produced a 2.7-fold increase in emission current compared to a 59Ni-embedded control. The emission threshold temperature was also examined to further assess the enhancement of thermionic emission, with 63Ni lowering the threshold temperature by an average of 58 ± 11 °C compared to the 59Ni control. Various mechanisms for the enhancement are discussed, with a satisfactory explanation remaining elusive. Nevertheless, one possibility is discussed involving excitation of preexisting conduction band electrons that may skew their energy distribution toward higher energies.

  2. Boron-doped nanocrystalline diamond microelectrode arrays monitor cardiac action potentials.

    Science.gov (United States)

    Maybeck, Vanessa; Edgington, Robert; Bongrain, Alexandre; Welch, Joseph O; Scorsone, Emanuel; Bergonzo, Philippe; Jackman, Richard B; Offenhäusser, Andreas

    2014-02-01

    The expansion of diamond-based electronics in the area of biological interfacing has not been as thoroughly explored as applications in electrochemical sensing. However, the biocompatibility of diamond, large safe electrochemical window, stability, and tunable electronic properties provide opportunities to develop new devices for interfacing with electrogenic cells. Here, the fabrication of microelectrode arrays (MEAs) with boron-doped nanocrystalline diamond (BNCD) electrodes and their interfacing with cardiomyocyte-like HL-1 cells to detect cardiac action potentials are presented. A nonreductive means of structuring doped and undoped diamond on the same substrate is shown. The resulting BNCD electrodes show high stability under mechanical stress generated by the cells. It is shown that by fabricating the entire surface of the MEA with NCD, in patterns of conductive doped, and isolating undoped regions, signal detection may be improved up to four-fold over BNCD electrodes passivated with traditional isolators. Copyright © 2014 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

  3. Front and back side SIMS analysis of boron-doped delta-layer in diamond

    Energy Technology Data Exchange (ETDEWEB)

    Pinault-Thaury, M.-A., E-mail: marie-amandine.pinault-thaury@uvsq.fr [Groupe d’Etude de la Matière Condensée, CNRS, University of Paris Saclay, University of Versailles St Quentin, 45 Avenue des Etats-Unis, 78035 Versailles Cedex (France); Jomard, F. [Groupe d’Etude de la Matière Condensée, CNRS, University of Paris Saclay, University of Versailles St Quentin, 45 Avenue des Etats-Unis, 78035 Versailles Cedex (France); Mer-Calfati, C.; Tranchant, N.; Pomorski, M.; Bergonzo, P.; Arnault, J.-C. [CEA, LIST, Diamond Sensors Laboratory, 91191 Gif-sur-Yvette (France)

    2017-07-15

    Highlights: • Front and back side SIMS analysis of delta-layer boron-doped is a first for diamond. • Combination of front and back side depth profiling improves delta-layer analyses. • Sharp interfaces are evidenced on both sides of the delta-layer boron-doped diamond. • The growth of delta-layer boron doped diamond is now well controlled. - Abstract: Nowadays the availability of very thin diamond layers in the range of nanometers as well as the possibility to characterize such delta-layer structures are required for the field of photonics and spintronics, but also for the development of next generation high power devices involving boron doping. The fabrication of diamond structures with abrupt interfaces such as superlattices and quantum wells has been recently improved. A very accurate characterization is then essential even though the analysis of such structures is arduous and challenging. SIMS analyses are commonly used to obtain depth profiles of dopants. However, below 10 nm in thickness, SIMS induced ion mixing effects which are no longer negligible. Then the raw SIMS profile might differ from the real dopant profile. In this study, we have analyzed a diamond structure containing a thin boron epilayer, especially synthesized to achieve SIMS analysis on both sides and to overcome the effects of ion mixing. We evidence the ion mixing induced by primary ions. Such a structure is a delta diamond layer, comparable to classical boron-doped delta-layer in silicon. Our results show that the growth of boron-doped delta-layer in diamond is now well controlled in terms of thickness and interfaces.

  4. Diamond films: Historical perspective

    Energy Technology Data Exchange (ETDEWEB)

    Messier, R. [Pennsylvania State Univ., University Park (United States)

    1993-01-01

    This section is a compilation of notes and published international articles about the development of methods of depositing diamond films. Vapor deposition articles are included from American, Russian, and Japanese publications. The international competition to develop new deposition methodologies is stressed. The current status of chemical vapor deposition of diamond is assessed.

  5. Ti-doped hydrogenated diamond like carbon coating deposited by hybrid physical vapor deposition and plasma enhanced chemical vapor deposition

    Science.gov (United States)

    Lee, Na Rae; Sle Jun, Yee; Moon, Kyoung Il; Sunyong Lee, Caroline

    2017-03-01

    Diamond-like carbon films containing titanium and hydrogen (Ti-doped DLC:H) were synthesized using a hybrid technique based on physical vapor deposition (PVD) and plasma enhanced chemical vapor deposition (PECVD). The film was deposited under a mixture of argon (Ar) and acetylene gas (C2H2). The amount of Ti in the Ti-doped DLC:H film was controlled by varying the DC power of the Ti sputtering target ranging from 0 to 240 W. The composition, microstructure, mechanical and chemical properties of Ti-doped DLC:H films with varying Ti concentrations, were investigated using Raman spectroscopy, X-ray photoelectron spectroscopy (XPS), nano indentation, a ball-on-disk tribometer, a four-point probe system and dynamic anodic testing. As a result, the optimum composition of Ti in Ti-doped DLC:H film using our hybrid method was found to be a Ti content of 18 at. %, having superior electrical conductivity and high corrosion resistance, suitable for bipolar plates. Its hardness value was measured to be 25.6 GPa with a low friction factor.

  6. The origin of magnetism in transition metal-doped ZrO2 thin films: Experiment and theory

    KAUST Repository

    Hong, Nguyenhoa

    2013-10-04

    We have investigated the magnetic properties of Fe/Co/Ni-doped ZrO 2 laser ablated thin films in comparison with the known results of Mn-doped ZrO2, which is thought to be a promising material for spintronics applications. It is found that doping with a transition metal can induce room temperature ferromagnetism in \\'fake\\' diamond. Theoretical analysis based on density functional theory confirms the experimental measurements, by revealing that the magnetic moments of Mn- and Ni-doped ZrO2 thin films are much larger than that of Fe- or Co-doped ZrO2 thin films. Most importantly, our calculations confirm that Mn- and Ni-doped ZrO2 show a ferromagnetic ground state in comparison to Co- and Fe-doped ZrO 2, which favor an antiferromagnetic ground state. © 2013 IOP Publishing Ltd.

  7. Synthesis and electrochemical properties of Ti-doped DLC films by a hybrid PVD/PECVD process

    Science.gov (United States)

    Jo, Yeong Ju; Zhang, Teng Fei; Son, Myoung Jun; Kim, Kwang Ho

    2018-03-01

    Low electrical conductivity and poor adhesion to metallic substrates are the main drawbacks of diamond-like carbon (DLC) films when used in electrode applications. In this study, Ti-doped DLC films with various Ti contents were synthesized on metal Ti substrates by a hybrid PVD/PECVD process, where PECVD was used for deposition of DLC films and PVD was used for Ti doping. The effects of the Ti doping ratio on the microstructure, adhesion strength, and electrical and electrochemical properties of the DLC films were systematically investigated. An increase in the Ti content led to increased surface roughness and a higher sp2/sp3 ratio of the Ti-DLC films. Ti atoms existed as amorphous-phase Ti carbide when the Ti doping ratio was less than 2.8 at.%, while the nanocrystalline TiC phase was formed in DLC films when the Ti doping ratio was exceeded 4.0 at.%. The adhesion strength, electrical resistivity, electrochemical activity and reversibility of the DLC films were greatly improved by Ti doping. The influence of Ti doping ratio on the electrical and electrochemical properties of the DLC films were also investigated and the best performance was obtained at a Ti content of 2.8 at.%.

  8. n-type diamond growth by phosphorus doping on (0 0 1)-oriented surface

    International Nuclear Information System (INIS)

    Kato, Hiromitsu; Makino, Toshiharu; Yamasaki, Satoshi; Okushi, Hideyo

    2007-01-01

    The properties of phosphorus incorporation for n-type doping of diamond are discussed and summarized. Doping of (0 0 1)-oriented diamond is introduced and compared with results achieved on (1 1 1) diamond. This review describes detailed procedures and conditions of plasma-enhanced chemical vapour deposition (CVD) growth and characteristics of electrical properties of phosphorus-doped diamond. The phosphorus incorporation was characterized by SIMS analysis including mapping. n-type conductivity is evaluated by Hall-effect measurements over a temperature regime of 300-1000 K. The crystal perfection of (0 0 1)-oriented n-type diamond is also evaluated by x-ray diffraction, Raman spectroscopy, reflection high-energy electron diffraction and cathodoluminescence analyses. The results show that phosphorus atoms are incorporated into the diamond network during (0 0 1) CVD diamond growth and that phosphorus acts as a donor as in (1 1 1)-oriented diamond. This result eliminates the restriction on substrate orientation, which had previously created a bottleneck in the development of diamond electronic devices. (review article)

  9. Workshop on diamond and diamond-like-carbon films for the transportation industry

    Energy Technology Data Exchange (ETDEWEB)

    Nichols, F.A.; Moores, D.K. [eds.

    1993-01-01

    Applications exist in advanced transportation systems as well as in manufacturing processes that would benefit from superior tribological properties of diamond, diamond-like-carbon and cubic boron nitride coatings. Their superior hardness make them ideal candidates as protective coatings to reduce adhesive, abrasive and erosive wear in advanced diesel engines, gas turbines and spark-ignited engines and in machining and manufacturing tools as well. The high thermal conductivity of diamond also makes it desirable for thermal management not only in tribological applications but also in high-power electronic devices and possibly large braking systems. A workshop has been recently held at Argonne National Laboratory entitled ``Diamond and Diamond-Like-Carbon Films for Transportation Applications`` which was attended by 85 scientists and engineers including top people involved in the basic technology of these films and also representatives from many US industrial companies. A working group on applications endorsed 18 different applications for these films in the transportation area alone. Separate abstracts have been prepared.

  10. Polarized Raman spectroscopy of chemically vapour deposited diamond films

    International Nuclear Information System (INIS)

    Prawer, S.; Nugent, K.W.; Weiser, P.S.

    1994-01-01

    Polarized micro-Raman spectra of chemically vapour deposited diamond films are presented. It is shown that important parameters often extracted from the Raman spectra such as the ratio of the diamond to non-diamond component of the films and the estimation of the level of residual stress depend on the orientation of the diamond crystallites with respect to the polarization of the incident laser beam. The dependence originates from the fact that the Raman scattering from the non-diamond components in the films is almost completely depolarized whilst the scattering from the diamond components is strongly polarized. The results demonstrate the importance of taking polarization into account when attempting to use Raman spectroscopy in even a semi-quantitative fashion for the assessment of the purity, perfection and stress in CVD diamond films. 8 refs., 1 tab. 2 figs

  11. Spectrally dependent photovoltages in Schottky photodiode based on (100) B-doped diamond

    Science.gov (United States)

    Čermák, Jan; Koide, Yasuo; Takeuchi, Daisuke; Rezek, Bohuslav

    2014-02-01

    Spectrally and spatially resolved photovoltages were measured by Kelvin probe force microscopy (KPFM) on a Schottky photo-diode made of a 4 nm thin tungsten-carbide (WC) layer on a 500 nm oxygen-terminated boron-doped diamond epitaxial layer (O-BDD) that was grown on a Ib (100) diamond substrate. The diode was grounded by the sideways ohmic contact (Ti/WC), and the semitransparent Schottky contact was let unconnected. The electrical potentials across the device were measured in dark (only 650 nm LED of KPFM being on), under broad-band white light (halogen lamp), UV (365 nm diode), and deep ultraviolet (deuterium lamp) illumination. Illumination induced shift of the electrical potential remains within 210 mV. We propose that the photovoltage actually corresponds to a shift of Fermi level inside the BDD channel and thereby explains orders of magnitude changes in photocurrent.

  12. Pulsed laser deposition of metallic films on the surface of diamond particles for diamond saw blades

    International Nuclear Information System (INIS)

    Jiang Chao; Luo Fei; Long Hua; Hu Shaoliu; Li Bo; Wang Youqing

    2005-01-01

    Ti or Ni films have been deposited on the diamond particle surfaces by pulsed laser deposition. Compressive resistance of the uncoated and coated diamond particles was measured, respectively, in the experiments. The compressive resistance of the Ti-coated diamonds particles was found much higher than that of the uncoated ones. It increased by 39%. The surface morphology is observed by the metallography microscope. The surface of the uncoated diamonds particles had many hollows and flaws, while the surface of Ni-coated diamond particles was flat and smooth, and the surface of Ti-coated diamond particles had some metal masses that stood out of the surface of the Ti-coated film. The components of the metallic films of diamond particles were examined by X-ray diffractometry (XRD). TiC was found formed on the Ti-coated diamond surface, which resulted in increased surface bonding strength between the diamond particles and the Ti films. Meanwhile, TiC also favored improving the bonding strength between the coated diamond particles and the binding materials. Moreover, the bending resistance of the diamond saw blade made of Ti-coated diamond was drastically higher than that of other diamond saw blades, which also played an important role in improving the blade's cutting ability and lifetime. Therefore, it was most appropriate that the diamond saw blade was made of Ti-coated diamond particles rather than other materials

  13. Amorphous Si layers co-doped with B and Mn: Thin film growth and steering of magnetic properties

    International Nuclear Information System (INIS)

    Drera, G.; Mozzati, M.C.; Colombi, P.; Salvinelli, G.; Pagliara, S.; Visentin, D.; Sangaletti, L.

    2015-01-01

    Amorphous silicon thin films co-doped with manganese (5% at.) and boron (1.8% at.) have been prepared by RF sputtering on Al 2 O 3 substrates held at room temperature (RT). The films, with an average thickness of about 0.9 μm, were carefully characterized by micro-Raman and X-ray photoemission spectroscopies. A ferromagnetic (FM) behavior up to RT was observed. In order to discuss and possibly rule out extrinsic effects usually related to segregations of ferromagnetic impurities in the samples, magnetization measurements were carried out on the Al 2 O 3 substrates, as well as on Si:B and Si:Mn films grown with the same RF sputtering system. Only the Si:B:Mn films displayed a FM behavior up to RT. Since amorphous films doped with Mn alone did not display any signature of FM ordering, boron co-doping results to be crucial for the onset of the FM behavior. The conductivity of the samples is not affected by boron doping that, therefore, does not appear to significantly contribute to a possible carrier-mediated FM interaction between Mn ions by supplying extra charges to the system. On this basis, the capability of B to hinder the quenching of the Mn 3d magnetic moments has also to be regarded as a possible role of this co-dopant in the observed magnetization. - Highlights: • We successfully deposited amorphous silicon thin films co-doped with Mn and B. • Structural, electronic, and magnetic properties have been carefully characterized. • A ferromagnetic behavior up to room temperature was detected. • The extrinsic origin of magnetism is excluded. • Boron can play a relevant role to avoid quenching of magnetic moment in Mn ions

  14. Amorphous Si layers co-doped with B and Mn: Thin film growth and steering of magnetic properties

    Energy Technology Data Exchange (ETDEWEB)

    Drera, G. [I-LAMP, Dipartimento di Matematica e Fisica, Università Cattolica del Sacro Cuore, Via dei Musei 41, 25121 Brescia (Italy); Mozzati, M.C. [CNISM, Dipartimento di Fisica, Università di Pavia, Via Bassi 6, 27100 Pavia (Italy); Colombi, P. [CSMT Gestione s.c.a.r.l, Via Branze 45, 25123 Brescia (Italy); Salvinelli, G.; Pagliara, S.; Visentin, D. [I-LAMP, Dipartimento di Matematica e Fisica, Università Cattolica del Sacro Cuore, Via dei Musei 41, 25121 Brescia (Italy); Sangaletti, L., E-mail: sangalet@dmf.unicatt.it [I-LAMP, Dipartimento di Matematica e Fisica, Università Cattolica del Sacro Cuore, Via dei Musei 41, 25121 Brescia (Italy)

    2015-09-01

    Amorphous silicon thin films co-doped with manganese (5% at.) and boron (1.8% at.) have been prepared by RF sputtering on Al{sub 2}O{sub 3} substrates held at room temperature (RT). The films, with an average thickness of about 0.9 μm, were carefully characterized by micro-Raman and X-ray photoemission spectroscopies. A ferromagnetic (FM) behavior up to RT was observed. In order to discuss and possibly rule out extrinsic effects usually related to segregations of ferromagnetic impurities in the samples, magnetization measurements were carried out on the Al{sub 2}O{sub 3} substrates, as well as on Si:B and Si:Mn films grown with the same RF sputtering system. Only the Si:B:Mn films displayed a FM behavior up to RT. Since amorphous films doped with Mn alone did not display any signature of FM ordering, boron co-doping results to be crucial for the onset of the FM behavior. The conductivity of the samples is not affected by boron doping that, therefore, does not appear to significantly contribute to a possible carrier-mediated FM interaction between Mn ions by supplying extra charges to the system. On this basis, the capability of B to hinder the quenching of the Mn 3d magnetic moments has also to be regarded as a possible role of this co-dopant in the observed magnetization. - Highlights: • We successfully deposited amorphous silicon thin films co-doped with Mn and B. • Structural, electronic, and magnetic properties have been carefully characterized. • A ferromagnetic behavior up to room temperature was detected. • The extrinsic origin of magnetism is excluded. • Boron can play a relevant role to avoid quenching of magnetic moment in Mn ions.

  15. Voltammetric and impedance behaviours of surface-treated nano-crystalline diamond film electrodes

    International Nuclear Information System (INIS)

    Liu, F. B.; Jing, B.; Cui, Y.; Di, J. J.; Qu, M.

    2015-01-01

    The electrochemical performances of hydrogen- and oxygen-terminated nano-crystalline diamond film electrodes were investigated by cyclic voltammetry and AC impedance spectroscopy. In addition, the surface morphologies, phase structures, and chemical states of the two diamond films were analysed by scanning probe microscopy, Raman spectroscopy, and X-ray photoelectron spectroscopy, respectively. The results indicated that the potential window is narrower for the hydrogen-terminated nano-crystalline diamond film than for the oxygen-terminated one. The diamond film resistance and capacitance of oxygen-terminated diamond film are much larger than those of the hydrogen-terminated diamond film, and the polarization resistances and double-layer capacitance corresponding to oxygen-terminated diamond film are both one order of magnitude larger than those corresponding to the hydrogen-terminated diamond film. The electrochemical behaviours of the two diamond film electrodes are discussed

  16. Enhanced selectivity of boron doped diamond electrodes for the detection of dopamine and ascorbic acid by increasing the film thickness

    Energy Technology Data Exchange (ETDEWEB)

    Qi, Yao; Long, Hangyu [School of Material Science and Engineering, Central South University, Changsha 410083 (China); Ma, Li, E-mail: marycsupm@csu.edu.cn [State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083 (China); Wei, Quiping, E-mail: qiupwei@csu.edu.cn [School of Material Science and Engineering, Central South University, Changsha 410083 (China); State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083 (China); Li, Site [School of Material Science and Engineering, Central South University, Changsha 410083 (China); Yu, Zhiming [School of Material Science and Engineering, Central South University, Changsha 410083 (China); State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083 (China); Hu, Jingyuan [School of Material Science and Engineering, Central South University, Changsha 410083 (China); Liu, Peizhi [Key laboratory of interface science and engineering in advanced materials, Ministry of Education, Taiyuan University of Technology, Taiyuan 030024,PR China (China); Wang, Yijia [School of Material Science and Engineering, Central South University, Changsha 410083 (China); Meng, Lingcong [Department of Chemistry, University of Warwick, Coventry, West Midlands CV4 7AL (United Kingdom)

    2016-12-30

    Highlights: • BDD electrodes with different thickness have been fabricated. • BDD electrodes are used for simultaneous detection of DA and AA. • Anodic pretreatment enhance the separation of DA and AA oxidation peak potential. • Thicker BDD electrode show better performance for DA detection coexisting with AA. - Abstract: In this paper, boron doped diamond (BDD) with different thickness were prepared by hot filament chemical vapor deposition. The performance of BDD electrodes for detecting dopamine (DA) and ascorbic acid (AA) were investigated. Scanning electron microscopy and Raman spectra reveal the grain size increases and the film quality improves with the increase of film thickness. Electrochemical test show that the transfer coefficient in [Fe{sub 3} (CN) {sub 6}]{sup 3−/4−} redox system increases with the increase of the film thickness. The results of selectivity and sensitivity for DA mixed with AA detection show that 8h-BDD and 12h-BDD electrodes possess well selective separated oxidation peaks of DA and AA, and the 12h-BDD electrode exhibits optimal sensitivity until the DA concentration drops to 1 μ M.

  17. Surface structuring of boron doped CVD diamond by micro electrical discharge machining

    Science.gov (United States)

    Schubert, A.; Berger, T.; Martin, A.; Hackert-Oschätzchen, M.; Treffkorn, N.; Kühn, R.

    2018-05-01

    Boron doped diamond materials, which are generated by Chemical Vapor Deposition (CVD), offer a great potential for the application on highly stressed tools, e. g. in cutting or forming processes. As a result of the CVD process rough surfaces arise, which require a finishing treatment in particular for the application in forming tools. Cutting techniques such as milling and grinding are hardly applicable for the finish machining because of the high strength of diamond. Due to its process principle of ablating material by melting and evaporating, Electrical Discharge Machining (EDM) is independent of hardness, brittleness or toughness of the workpiece material. EDM is a suitable technology for machining and structuring CVD diamond, since boron doped CVD diamond is electrically conductive. In this study the ablation characteristics of boron doped CVD diamond by micro electrical discharge machining are investigated. Experiments were carried out to investigate the influence of different process parameters on the machining result. The impact of tool-polarity, voltage and discharge energy on the resulting erosion geometry and the tool wear was analyzed. A variation in path overlapping during the erosion of planar areas leads to different microstructures. The results show that micro EDM is a suitable technology for finishing of boron doped CVD diamond.

  18. Anodic oxidation of wastewater containing the Reactive Orange 16 Dye using heavily boron-doped diamond electrodes

    International Nuclear Information System (INIS)

    Migliorini, F.L.; Braga, N.A.; Alves, S.A.; Lanza, M.R.V.; Baldan, M.R.; Ferreira, N.G.

    2011-01-01

    Highlights: → Electrochemical advanced oxidation process was studied using BDD based anodes with different boron concentrations. → The difference between the non-active and active anodes for organics degradation. → The influence of morphologic and structural properties of BDD electrodes on the RO-16 dye degradation. - Abstract: Boron-doped diamond (BDD) films grown on the titanium substrate were used to study the electrochemical degradation of Reactive Orange (RO) 16 Dye. The films were produced by hot filament chemical vapor deposition (HFCVD) technique using two different boron concentrations. The growth parameters were controlled to obtain heavily doped diamond films. They were named as E1 and E2 electrodes, with acceptor concentrations of 4.0 and 8.0 x 10 21 atoms cm -3 , respectively. The boron levels were evaluated from Mott-Schottky plots also corroborated by Raman's spectra, which characterized the film quality as well as its physical property. Scanning Electron Microscopy showed well-defined microcrystalline grain morphologies with crystal orientation mixtures of (1 1 1) and (1 0 0). The electrode efficiencies were studied from the advanced oxidation process (AOP) to degrade electrochemically the Reactive Orange 16 azo-dye (RO16). The results were analyzed by UV/VIS spectroscopy, total organic carbon (TOC) and high-performance liquid chromatography (HPLC) techniques. From UV/VIS spectra the highest doped electrode (E2) showed the best efficiency for both, the aromaticity reduction and the azo group fracture. These tendencies were confirmed by the TOC and chromatographic measurements. Besides, the results showed a direct relationship among the BDD morphology, physical property, and its performance during the degradation process.

  19. High-temperature Infrared Transmission of Free-standing Diamond Films

    Directory of Open Access Journals (Sweden)

    HEI Li-fu

    2017-02-01

    Full Text Available The combination of low absorption and extreme mechanical and thermal properties make diamond a compelling choice for some more extreme far infrared (8-12 μm window applications. The optical properties of CVD diamond at elevated temperatures are critical to many of these extreme applications. The infrared transmission of free-standing diamond films prepared by DC arc plasma jet were studied at temperature varied conditions. The surface morphology, structure feature and infrared optical properties of diamond films were tested by optical microscope, X-ray diffraction, laser Raman and Fourier-transform infrared spectroscopy. The results show that the average transmittance for 8-12μm is decreased from 65.95% at 27℃ to 52.5% at 500℃,and the transmittance drop is in three stages. Corresponding to the drop of transmittance with the temperature, diamond film absorption coefficient increases with the rise of temperature. The influence of the change of surface state of diamond films on the optical properties of diamond films is significantly greater than the influence on the internal structure.

  20. Effect of boron incorporation on the structure and electrical properties of diamond-like carbon films deposited by femtosecond and nanosecond pulsed laser ablation

    Energy Technology Data Exchange (ETDEWEB)

    Sikora, A. [Laboratoire Hubert Curien, UMR 5516 CNRS, Universite Jean Monnet, 18 Rue Pr. Benoit Lauras, 42000 Saint-Etienne (France); Bourgeois, O. [Institut Neel, UPR 2940 CNRS, 25 Avenue des Martyrs, 38042 Grenoble Cedex 9 (France); Sanchez-Lopez, J.C. [Instituto de Ciencia de Materiales de Sevilla, Avda. Americo Vespucio, 49 41092 Sevilla (Spain); Rouzaud, J.-N. [Laboratoire de Geologie, UMR 8538 CNRS, Ecole Normale Superieure, 45 Rue d' Ulm, 75230 Paris Cedex 05 (France); Rojas, T.C. [Instituto de Ciencia de Materiales de Sevilla, Avda. Americo Vespucio, 49 41092 Sevilla (Spain); Loir, A.-S. [Laboratoire Hubert Curien, UMR 5516 CNRS, Universite Jean Monnet, 18 Rue Pr. Benoit Lauras, 42000 Saint-Etienne (France); Garden, J.-L. [Institut Neel, UPR 2940 CNRS, 25 Avenue des Martyrs, 38042 Grenoble Cedex 9 (France); Garrelie, F. [Laboratoire Hubert Curien, UMR 5516 CNRS, Universite Jean Monnet, 18 Rue Pr. Benoit Lauras, 42000 Saint-Etienne (France); Donnet, C., E-mail: christophe.donnet@univ-st-etienne.f [Laboratoire Hubert Curien, UMR 5516 CNRS, Universite Jean Monnet, 18 Rue Pr. Benoit Lauras, 42000 Saint-Etienne (France)

    2009-12-31

    The influence of the incorporation of boron in diamond-like carbon (DLC) films on the microstructure of the coatings has been investigated. The boron-containing DLC films (a-C:B) have been deposited by pulsed laser deposition (PLD) at room temperature in high vacuum conditions, by ablating graphite and boron targets either with a femtosecond pulsed laser (800 nm, 150 fs, fs-DLC) or with a nanosecond pulsed laser (248 nm, 20 ns, ns-DLC). Alternative ablation of the graphite and boron targets has been carried out to deposit the a-C:B films. The film structure and composition have been highlighted by coupling Field Emission Scanning Electron Microscopy, Electron Energy Loss Spectroscopy and High Resolution Transmission Electron Microscopy. Using the B K-edge, EELS characterization reveals the boron effect on the carbon bonding. Moreover, the plasmon energy reveals a tendency of graphitization associated to the boron doping. Pure boron particles have been characterized by HRTEM and reveal that those particles are amorphous or crystallized. The nanostructures of the boron-doped ns-DLC and the boron-doped fs-DLC are thus compared. In particular, the incorporation of boron in the DLC matrix is highlighted, depending on the laser used for deposition. Electrical measurements show that some of these films have potentialities to be used in low temperature thermometry, considering their conductivity and temperature coefficient of resistance (TCR) estimated within the temperature range 160-300 K.

  1. Metal-doped diamond-like carbon films synthesized by filter-arc deposition

    International Nuclear Information System (INIS)

    Weng, K.-W.; Chen, Y.-C.; Lin, T.-N.; Wang, D.-Y.

    2006-01-01

    Diamond-like carbon (DLC) thin films are extensively utilized in the semiconductor, electric and cutting machine industries owing to their high hardness, high elastic modulus, low friction coefficients and high chemical stability. DLC films are prepared by ion beam-assisted deposition (BAD), sputter deposition, plasma-enhanced chemical vapor deposition (PECVD), cathodic arc evaporation (CAE), and filter arc deposition (FAD). The major drawbacks of these methods are the degraded hardness associated with the low sp 3 /sp 2 bonding ratio, the rough surface and poor adhesion caused by the presence of particles. In this study, a self-developed filter arc deposition (FAD) system was employed to prepare metal-containing DLC films with a low particle density. The relationships between the DLC film properties, such as film structure, surface morphology and mechanical behavior, with variation of substrate bias and target current, are examined. Experimental results demonstrate that FAD-DLC films have a lower ratio, suggesting that FAD-DLC films have a greater sp 3 bonding than the CAE-DLC films. FAD-DLC films also exhibit a low friction coefficient of 0.14 and half of the number of surface particles as in the CAE-DLC films. Introducing a CrN interfacial layer between the substrate and the DLC films enables the magnetic field strength of the filter to be controlled to improve the adhesion and effectively eliminate the contaminating particles. Accordingly, the FAD system improves the tribological properties of the DLC films

  2. Progress of Diamond-like Carbon Films

    Directory of Open Access Journals (Sweden)

    CHEN Qing-yun

    2017-03-01

    Full Text Available Diamond-like carbon(DLC films had many unique and outstanding properties such as high thermal conductivity, high hardness, excellent chemical inertness, low friction coefficients and wear coefficients. The properties and combinations were very promising for heat sink, micro-electromechanical devices, radiation hardening, biomedical devices, automotive industry and other technical applications, more research and a lot of attention were attracted in recent years. The research progress of diamond-like films and the nucleation mechanism of film were summarized, and application prospect of DLC films were demonstrated. The aim of this paper is to provide insights on the research trend of DLC films and the industry applications.

  3. Modifying thin film diamond for electronic applications

    International Nuclear Information System (INIS)

    Baral, B.

    1999-01-01

    The unique combination of properties that diamond possesses are being exploited in both electronic and mechanical applications. An important step forward in the field has been the ability to grow thin film diamond by chemical vapour deposition (CVD) methods and to control parameters such as crystal orientation, dopant level and surface roughness. An extensive understanding of the surface of any potential electronic material is vital to fully comprehend its behaviour within device structures. The surface itself ultimately controls key aspects of device performance when interfaced with other materials. This study has provided insight into important chemical reactions on polycrystalline CVD diamond surfaces, addressing how certain surface modifications will ultimately affect the properties of the material. A review of the structure, bonding, properties and potential of diamond along with an account of the current state of diamond technology and CVD diamond growth is provided. The experimental chapter reviews bulk material and surface analytical techniques employed in this work and is followed by an investigation of cleaning treatments for polycrystalline CVD diamond aimed at removing non-diamond carbon from the surface. Selective acid etch treatments are compared and contrasted for efficacy with excimer laser irradiation and hydrogen plasma etching. The adsorption/desorption kinetics of potential dopant-containing precursors on polycrystalline CVD diamond surfaces have been investigated to compare their effectiveness at introducing dopants into the diamond during the growth stage. Both boron and sulphur-containing precursor compounds have been investigated. Treating polycrystalline CVD diamond in various atmospheres / combination of atmospheres has been performed to enhance electron field emission from the films. Films which do not emit electrons under low field conditions can be modified such that they emit at fields as low as 10 V/μm. The origin of this enhancement

  4. Assessment of Electrodes Prepared from Wafers of Boron-doped Diamond for the Electrochemical Oxidation of Waste Lubricants

    International Nuclear Information System (INIS)

    Taylor, G.T.; Sullivan, I.A.; Newey, A.W.E.

    2006-01-01

    Electrochemical oxidation using boron-doped diamond electrodes is being investigated as a treatment process for radioactively contaminated oily wastes. Previously, it was shown that electrodes coated with a thin film of diamond were able to oxidise a cutting oil but not a mineral oil. These tests were inconclusive, because the electrodes lost their diamond coating during operation. Accordingly, an electrode prepared from a 'solid' wafer of boron-doped diamond is being investigated to determine whether it will oxidise mineral oils. The electrode has been tested with sucrose, a cutting oil and an emulsified mineral oil. Before and after each test, the state of the electrode was assessed by cyclic voltammetry with the ferro/ferricyanide redox couple. Analysis of the cyclic voltammogram suggested that material accumulated on the surface of the electrode during the tests. The magnitude of the effect was in the order: - emulsified mineral oil > cutting oil > sucrose. Despite this, the results indicated that the electrode was capable of oxidising the emulsified mineral oil. Confirmatory tests were undertaken in the presence of alkali to trap the carbon dioxide, but they had to be abandoned when the adhesive holding the diamond in the electrode was attacked by the alkali. Etching of the diamond wafer was also observed at the end of the tests. Surface corrosion is now regarded as an intrinsic part of the electrochemical oxidation on diamond, and it is expected that the rate of attack will determine the service life of the electrodes. (authors)

  5. Polycrystalline Diamond Schottky Diodes and Their Applications.

    Science.gov (United States)

    Zhao, Ganming

    In this work, four-hot-filament CVD techniques for in situ boron doped diamond synthesis on silicon substrates were extensively studied. A novel tungsten filament shape and arrangement used to obtain large-area, uniform, boron doped polycrystalline diamond thin films. Both the experimental results and radiative heat transfer analysis showed that this technique improved the uniformity of the substrate temperature. XRD, Raman and SEM studies indicate that large area, uniform, high quality polycrystalline diamond films were obtained. Schottky diodes were fabricated by either sputter deposition of silver or thermal evaporation of aluminum or gold, on boron doped diamond thin films. High forward current density and a high forward-to-reverse current ratio were exhibited by silver on diamond Schottky diodes. Schottky barrier heights and the majority carrier concentrations of both aluminum and gold contacted diodes were determined from the C-V measurements. Furthermore, a novel theoretical C-V-f analysis of deep level boron doped diamond Schottky diodes was performed. The analytical results agree well with the experimental results. Compressive stress was found to have a large effect on the forward biased I-V characteristics of the diamond Schottky diodes, whereas the effect on the reverse biased characteristics was relatively small. The stress effect on the forward biased diamond Schottky diode was attributed to piezojunction and piezoresistance effects. The measured force sensitivity of the diode was as high as 0.75 V/N at 1 mA forward bias. This result shows that CVD diamond device has potential for mechanical transducer applications. The quantitative photoresponse characteristics of the diodes were studied in the spectral range of 300 -1050 nm. Semi-transparent gold contacts were used for better photoresponse. Quantum efficiency as high as 50% was obtained at 500 nm, when a reverse bias of over 1 volt was applied. The Schottky barrier heights between either gold or

  6. Spectrally dependent photovoltages in Schottky photodiode based on (100) B-doped diamond

    International Nuclear Information System (INIS)

    Čermák, Jan; Rezek, Bohuslav; Koide, Yasuo; Takeuchi, Daisuke

    2014-01-01

    Spectrally and spatially resolved photovoltages were measured by Kelvin probe force microscopy (KPFM) on a Schottky photo-diode made of a 4 nm thin tungsten-carbide (WC) layer on a 500 nm oxygen-terminated boron-doped diamond epitaxial layer (O-BDD) that was grown on a Ib (100) diamond substrate. The diode was grounded by the sideways ohmic contact (Ti/WC), and the semitransparent Schottky contact was let unconnected. The electrical potentials across the device were measured in dark (only 650 nm LED of KPFM being on), under broad-band white light (halogen lamp), UV (365 nm diode), and deep ultraviolet (deuterium lamp) illumination. Illumination induced shift of the electrical potential remains within 210 mV. We propose that the photovoltage actually corresponds to a shift of Fermi level inside the BDD channel and thereby explains orders of magnitude changes in photocurrent

  7. Spectrally dependent photovoltages in Schottky photodiode based on (100) B-doped diamond

    Energy Technology Data Exchange (ETDEWEB)

    Čermák, Jan, E-mail: cermakj@fzu.cz; Rezek, Bohuslav [Institute of Physics, Academy of Sciences of the Czech Republic, Cukrovarnická 10, 16200 Prague 6 (Czech Republic); Koide, Yasuo [Sensor Materials Center, National Institute for Material Science (NIMS), 1-1 Namiki, Tsukuba 305-0044 (Japan); Takeuchi, Daisuke [Energy Technology Research Institute, National Institute of Advanced Industrial Science and Technology (AIST), 1-1-1 Umezono, Tsukuba 305-8568 (Japan)

    2014-02-07

    Spectrally and spatially resolved photovoltages were measured by Kelvin probe force microscopy (KPFM) on a Schottky photo-diode made of a 4 nm thin tungsten-carbide (WC) layer on a 500 nm oxygen-terminated boron-doped diamond epitaxial layer (O-BDD) that was grown on a Ib (100) diamond substrate. The diode was grounded by the sideways ohmic contact (Ti/WC), and the semitransparent Schottky contact was let unconnected. The electrical potentials across the device were measured in dark (only 650 nm LED of KPFM being on), under broad-band white light (halogen lamp), UV (365 nm diode), and deep ultraviolet (deuterium lamp) illumination. Illumination induced shift of the electrical potential remains within 210 mV. We propose that the photovoltage actually corresponds to a shift of Fermi level inside the BDD channel and thereby explains orders of magnitude changes in photocurrent.

  8. Encapsulation of electroless copper patterns into diamond films

    Energy Technology Data Exchange (ETDEWEB)

    Pimenov, S.M.; Shafeev, G.A.; Lavrischev, S.V. [General Physics Institute, Moscow (Russian Federation)] [and others

    1995-12-31

    The results are reported on encapsulating copper lines into diamond films grown by a DC plasma CVD. The process includes the steps of (i) laser activation of diamond for electroless metal plating, (ii) electroless copper deposition selectively onto the activated surface regions, and (iii) diamond regrowth on the Cu-patterned diamond films. The composition and electrical properties of the encapsulated copper lines were examined, revealing high purity and low electrical resistivity of the encapsulated electroless copper.

  9. Chemical vapor deposition of nanocrystalline diamond films

    International Nuclear Information System (INIS)

    Vyrovets, I.I.; Gritsyna, V.I.; Dudnik, S.F.; Opalev, O.A.; Reshetnyak, O.M.; Strel'nitskij, V.E.

    2008-01-01

    The brief review of the literature is devoted to synthesis of nanocrystalline diamond films. It is shown that the CVD method is an effective way for deposition of such nanostructures. The basic technological methods that allow limit the size of growing diamond crystallites in the film are studied.

  10. X-ray beam monitor made by thin-film CVD single-crystal diamond.

    Science.gov (United States)

    Marinelli, Marco; Milani, E; Prestopino, G; Verona, C; Verona-Rinati, G; Angelone, M; Pillon, M; Kachkanov, V; Tartoni, N; Benetti, M; Cannatà, D; Di Pietrantonio, F

    2012-11-01

    A novel beam position monitor, operated at zero bias voltage, based on high-quality chemical-vapor-deposition single-crystal Schottky diamond for use under intense synchrotron X-ray beams was fabricated and tested. The total thickness of the diamond thin-film beam monitor is about 60 µm. The diamond beam monitor was inserted in the B16 beamline of the Diamond Light Source synchrotron in Harwell (UK). The device was characterized under monochromatic high-flux X-ray beams from 6 to 20 keV and a micro-focused 10 keV beam with a spot size of approximately 2 µm × 3 µm square. Time response, linearity and position sensitivity were investigated. Device response uniformity was measured by a raster scan of the diamond surface with the micro-focused beam. Transmissivity and spectral responsivity versus beam energy were also measured, showing excellent performance of the new thin-film single-crystal diamond beam monitor.

  11. TL and LOE dosimetric evaluation of diamond films exposed to beta and ultraviolet radiation

    International Nuclear Information System (INIS)

    Preciado F, S.; Melendrez, R.; Chernov, V.; Barboza F, M.; Schreck, M.; Cruz Z, E.

    2005-01-01

    The diamond possesses a privileged position regarding other materials of great technological importance. Their applications go from the optics, microelectronics, metals industry, medicine and of course as dosemeter, in the registration and detection of ionizing and non ionizing radiation. In this work the results of TL/LOE obtained in two samples of diamond of 10 μm thickness grown by the chemical vapor deposition method (CVD) assisted by microwave plasma. The films were deposited in a silicon substrate (001) starting from a mixture of gases composed of CH 4 /H 2 and 750 ppm of molecular nitrogen as dopant. The samples were exposed to beta radiation (Sr 90 / Y 90 ) and ultraviolet, being stimulated later on thermal (TL) and optically (LOE) to evaluate their dosimetric properties. The sample without doping presented high response TL/LOE to the ultraviolet and beta radiation. The TL glow curve of the sample without doping showed two TL peaks with second order kinetics in the range of 520 to 550 K, besides a peak with first order kinetics of more intensity around 607 K. The TL efficiency of the non doped sample is bigger than the doped with nitrogen; however the LOE efficiency is similar in both samples. The results indicate that the CVD diamond possesses excellent perspectives for dosimetric applications, with special importance in radiotherapy due to it is biologically compatible with the human tissue. (Author)

  12. Friction Properties of Polished Cvd Diamond Films Sliding against Different Metals

    Science.gov (United States)

    Lin, Zichao; Sun, Fanghong; Shen, Bin

    2016-11-01

    Owing to their excellent mechanical and tribological properties, like the well-known extreme hardness, low coefficient of friction and high chemical inertness, chemical vapor deposition (CVD) diamond films have found applications as a hard coating for drawing dies. The surface roughness of the diamond films is one of the most important attributes to the drawing dies. In this paper, the effects of different surface roughnesses on the friction properties of diamond films have been experimentally studied. Diamond films were fabricated using hot filament CVD. The WC-Co (Co 6wt.%) drawing dies were used as substrates. A gas mixture of acetone and hydrogen gas was used as the feedstock gas. The CVD diamond films were polished using mechanical polishing. Polished diamond films with three different surface roughnesses, as well as the unpolished diamond film, were fabricated in order to study the tribological performance between the CVD diamond films and different metals with oil lubrication. The unpolished and polished CVD diamond films are characterized with scanning electron microscope (SEM), atomic force microscope (AFM), surface profilometer, Raman spectrum and X-ray diffraction (XRD). The friction examinations were carried out by using a ball-on-plate type reciprocating friction tester. Low carbide steel, stainless steel, copper and aluminum materials were used as counterpart balls. Based on this study, the results presented the friction coefficients between the polished CVD films and different metals. The friction tests demonstrate that the smooth surface finish of CVD diamond films is beneficial for reducing their friction coefficients. The diamond films exhibit low friction coefficients when slid against the stainless steel balls and low carbide steel ball, lower than that slid against copper ball and aluminum ball, attributed to the higher ductility of copper and aluminum causing larger amount of wear debris adhering to the sliding interface and higher adhesive

  13. STRUCTURING OF DIAMOND FILMS USING MICROSPHERE LITHOGRAPHY

    Directory of Open Access Journals (Sweden)

    Mária Domonkos

    2014-10-01

    Full Text Available In this study, the structuring of micro- and nanocrystalline diamond thin films is demonstrated. The structuring of the diamond films is performed using the technique of microsphere lithography followed by reactive ion etching. Specifically, this paper presents a four-step fabrication process: diamond deposition (microwave plasma assisted chemical vapor deposition, mask preparation (by the standard Langmuir-Blodgett method, mask modification and diamond etching. A self-assembled monolayer of monodisperse polystyrene (PS microspheres with close-packed ordering is used as the primary template. Then the PS microspheres and the diamond films are processed in capacitively coupled radiofrequency plasma  using different plasma chemistries. This fabrication method illustrates the preparation of large arrays of periodic and homogeneous hillock-like structures. The surface morphology of processed diamond films is characterized by scanning electron microscopy and atomic force microscope. The potential applications of such diamond structures in various fields of nanotechnology are also briefly discussed.

  14. Thermal diffusivity of diamond films using a laser pulse technique

    International Nuclear Information System (INIS)

    Albin, S.; Winfree, W.P.; Crews, B.S.

    1990-01-01

    Polycrystalline diamond films were deposited using a microwave plasma-enhanced chemical vapor deposition process. A laser pulse technique was developed to measure the thermal diffusivity of diamond films deposited on a silicon substrate. The effective thermal diffusivity of a diamond film on silicon was measured by observing the phase and amplitude of the cyclic thermal waves generated by laser pulses. An analytical model is presented to calculate the effective inplane (face-parallel) diffusivity of a two-layer system. The model is used to reduce the effective thermal diffusivity of the diamond/silicon sample to a value for the thermal diffusivity and conductivity of the diamond film

  15. Phenomenological effets of tantalum incorporation into diamond films: Experimental and first principle studies

    Energy Technology Data Exchange (ETDEWEB)

    Ullah, Mahtab, E-mail: mahtabullah@bzu.edu.pk [Department of Physics, Bahauddin Zakariya University Multan (Pakistan); Rana, Anwar Manzoor; Ahmad, E. [Department of Physics, Bahauddin Zakariya University Multan (Pakistan); Raza, Rizwan [Department of Physics, COMSATS Institute of Information Technology, Lahore-54000 (Pakistan); Hussain, Fayyaz [Department of Physics, Bahauddin Zakariya University Multan (Pakistan); Hussain, Akhtar; Iqbal, Muhammad [Theoretical Physics Division, PINSTECH, P.O. Nilore, Islamabad (Pakistan)

    2016-09-01

    Graphical abstract: - Highlights: • Fabrication of tantalum incorporated diamonds films using HFCVD technique. • Decrease in resistivity by increasing tantalum content in diamond thin films. • Electronic structure calculations of tantalum incorporated diamonds films through VASP code. • A rise of bond length and bond angles by addition of tantalum in the diamond lattice. • Confirmation of decrease of resistivity by adding tantalum due to creation of impurity states in the bandgap. - Abstract: Tantalum (Ta) incorporated diamond films are synthesized on silicon substrate by chemical vapor deposition under gas mixture of CH{sub 4} + H{sub 2}. Characterizations of the resulting films indicate that morphology and resistivity of as-grown diamond films are significantly influenced by the process parameters and the amount of tantalum incorporated in the diamond films. XRD plots reveal that diamond films are composed of TaC along with diamond for higher concentration of tantalum and Ta{sub 2}C phases for lower concentration of tantalum. EDS spectra confirms the existence of tantalum in the diamond films. Resistivity measurements illustrate a sudden fall of about two orders of magnitude by the addition of tantalum in the diamond films. Band structure of Ta-incorporated diamond has been investigated based on density functional theory (DFT) using VASP code. Band structure calculations lead to the semiconducting behavior of Ta-incorporated diamond films because of the creation of defects states inside the band gap extending towards conduction band minimum. Present DFT results support experimental trend of resistivity that with the incorporation of tantalum into diamond lattice causes a decrease in the resistivity of diamond films so that tantalum-incorporated diamond films behave like a good semiconductor.

  16. Substitutional Boron in Nanodiamond, Bucky-Diamond, and Nanocrystalline Diamond Grain Boundaries

    Energy Technology Data Exchange (ETDEWEB)

    Barnard, Amanda S.; Sternberg, Michael G.

    2006-10-05

    Although boron has been known for many years to be a successful dopant in bulk diamond, efficient doping of nanocrystalline diamond with boron is still being developed. In general, the location, configuration, and bonding structure of boron in nanodiamond is still unknown, including the fundamental question of whether it is located within grains or grain boundaries of thin films and whether it is within the core or at the surface of nanoparticles. Presented here are density functional tight-binding simulations examining the configuration, potential energy surface, and electronic charge of substitutional boron in various types of nanocrystalline diamond. The results predict that boron is likely to be positioned at the surface of isolated particles and at the grain boundary of thin-film samples.

  17. Electrochemically assisted deposition of hydroxyapatite on Ti6Al4V substrates covered by CVD diamond films - Coating characterization and first cell biological results.

    Science.gov (United States)

    Strąkowska, Paulina; Beutner, René; Gnyba, Marcin; Zielinski, Andrzej; Scharnweber, Dieter

    2016-02-01

    Although titanium and its alloys are widely used as implant material for orthopedic and dental applications they show only limited corrosion stability and osseointegration in different cases. The aim of the presented research was to develop and characterize a novel surface modification system from a thin diamond base layer and a hydroxyapatite (HAp) top coating deposited on the alloy Ti6Al4V widely used for implants in contact with bone. This coating system is expected to improve both the long-term corrosion behavior and the biocompatibility and bioactivity of respective surfaces. The diamond base films were obtained by Microwave Plasma Assisted Chemical Vapor Deposition (MW-PACVD); the HAp coatings were formed in aqueous solutions by electrochemically assisted deposition (ECAD) at varying polarization parameters. Scanning electron microscopy (SEM), Raman microscopy, and electrical conductivity measurements were applied to characterize the generated surface states; the calcium phosphate coatings were additionally chemically analyzed for their composition. The biological properties of the coating system were assessed using hMSC cells analyzing for cell adhesion, proliferation, and osteogenic differentiation. Varying MW-PACVD process conditions resulted in composite coatings containing microcrystalline diamond (MCD/Ti-C), nanocrystalline diamond (NCD), and boron-doped nanocrystalline diamond (B-NCD) with the NCD coatings being dense and homogeneous and the B-NCD coatings showing increased electrical conductivity. The ECAD process resulted in calcium phosphate coatings from stoichiometric and non-stoichiometric HAp. The deposition of HAp on the B-NCD films run at lower cathodic potentials and resulted both in the highest coating mass and the most homogenous appearance. Initial cell biological investigations showed an improved cell adhesion in the order B-NCD>HAp/B-NCD>uncoated substrate. Cell proliferation was improved for both investigated coatings whereas ALP

  18. Anodic oxidation with doped diamond electrodes: a new advanced oxidation process

    International Nuclear Information System (INIS)

    Kraft, Alexander; Stadelmann, Manuela; Blaschke, Manfred

    2003-01-01

    Boron-doped diamond anodes allow to directly produce OH· radicals from water electrolysis with very high current efficiencies. This has been explained by the very high overvoltage for oxygen production and many other anodic electrode processes on diamond anodes. Additionally, the boron-doped diamond electrodes exhibit a high mechanical and chemical stability. Anodic oxidation with diamond anodes is a new advanced oxidation process (AOP) with many advantages compared to other known chemical and photochemical AOPs. The present work reports on the use of diamond anodes for the chemical oxygen demand (COD) removal from several industrial wastewaters and from two synthetic wastewaters with malic acid and ethylenediaminetetraacetic (EDTA) acid. Current efficiencies for the COD removal between 85 and 100% have been found. The formation and subsequent removal of by-products of the COD oxidation has been investigated for the first time. Economical considerations of this new AOP are included

  19. One step deposition of highly adhesive diamond films on cemented carbide substrates via diamond/β-SiC composite interlayers

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Tao; Zhuang, Hao; Jiang, Xin, E-mail: xin.jiang@uni-siegen.de

    2015-12-30

    Graphical abstract: - Highlights: • Novel diamond/beta-silicon carbide composite gradient interlayers were synthesized. • The interlayer features a cross-sectional gradient with increasing diamond content. • Diamond top layers and the interlayers were deposited in one single process. • The adhesion of the diamond film is drastically improved by employing the interlayer. • The stress was suppressed by manipulating the distribution of diamond and silicon carbide. - Abstract: Deposition of adherent diamond films on cobalt-cemented tungsten carbide substrates has been realized by application of diamond/beta-silicon carbide composite interlayers. Diamond top layers and the interlayers were deposited in one single process by hot filament chemical vapor deposition technique. Two different kinds of interlayers have been employed, namely, gradient interlayer and interlayer with constant composition. The distribution of diamond and beta-silicon carbide phases was precisely controlled by manipulating the gas phase composition. X-ray diffraction and Raman spectroscopy were employed to determine the existence of diamond, beta-silicon carbide and cobalt silicides (Co{sub 2}Si, CoSi) phases, as well as the quality of diamond crystal and the residual stress in the films. Rockwell-C indentation tests were carried out to evaluate the film adhesion. It is revealed that the adhesion of the diamond film is drastically improved by employing the interlayer. This is mainly influenced by the residual stress in the diamond top layer, which is induced by the different thermal expansion coefficient of the film and the substrate. It is even possible to further suppress the stress by manipulating the distribution of diamond and beta-silicon carbide in the interlayer. The most adhesive diamond film on cemented carbide is thus obtained by employing a gradient composite interlayer.

  20. Optical and electrical properties of transparent conducting B-doped ZnO thin films prepared by various deposition methods

    International Nuclear Information System (INIS)

    Nomoto, Jun-ichi; Miyata, Toshihiro; Minami, Tadatsugu

    2011-01-01

    B-doped ZnO (BZO) thin films were prepared with various thicknesses up to about 500 nm on glass substrates at 200 deg. C by dc or rf magnetron sputtering deposition, pulsed laser deposition (PLD), and vacuum arc plasma evaporation (VAPE) methods. Resistivities of 4-6 x 10 -4 Ω cm were obtained in BZO thin films prepared with a B content [B/(B + Zn) atomic ratio] around 1 at. % by PLD and VAPE methods: Hall mobilities above 40 cm 2 /Vs and carrier concentrations on the order of 10 20 cm -3 . All 500-nm-thick-BZO thin films prepared with a resistivity on the order of 10 -3 -10 -4 Ω cm exhibited an averaged transmittance above 80% in the wavelength range of 400-1100 nm. The resistivity in BZO thin films prepared with a thickness below about 500 nm was found to increase over time with exposure to various high humidity environments. In heat-resistance tests, the resistivity stability of BZO thin films was found to be nearly equal to that of Ga-doped ZnO thin films, so these films were judged suitable for use as a transparent electrode for thin-film solar cells.

  1. Raman and EPR spectroscopic studies of chromium-doped diamond-like carbon films

    Czech Academy of Sciences Publication Activity Database

    Savchenko, Dariia; Vorlíček, Vladimír; Prokhorov, Andriy; Kalabukhova, E.; Lančok, Ján; Jelínek, Miroslav

    2018-01-01

    Roč. 83, Mar (2018), s. 30-37 ISSN 0925-9635 R&D Projects: GA MŠk(CZ) LO1409; GA MŠk(CZ) LM2015088; GA ČR(CZ) GA15-05864S Institutional support: RVO:68378271 Keywords : EPR * micro-Raman spectroscopy * diamond-like films * carbon-related defects * chromium Subject RIV: BM - Solid Matter Physics ; Magnetism OBOR OECD: Condensed matter physics (including formerly solid state physics, supercond.) Impact factor: 2.561, year: 2016

  2. Plasma etching treatment for surface modification of boron-doped diamond electrodes

    Energy Technology Data Exchange (ETDEWEB)

    Kondo, Takeshi [Department of Industrial Chemistry, Faculty of Engineering, Tokyo University of Science, 1-3 Kagurazaka, Shinjuku-ku, Tokyo 162-8601 (Japan); Ito, Hiroyuki [Department of Industrial Chemistry, Faculty of Engineering, Tokyo University of Science, 1-3 Kagurazaka, Shinjuku-ku, Tokyo 162-8601 (Japan); Kusakabe, Kazuhide [Department of Applied Physics, Faculty of Science, Tokyo University of Science, 1-3 Kagurazaka, Shinjuku-ku, Tokyo 162-8601 (Japan); Ohkawa, Kazuhiro [Department of Applied Physics, Faculty of Science, Tokyo University of Science, 1-3 Kagurazaka, Shinjuku-ku, Tokyo 162-8601 (Japan); Einaga, Yasuaki [Department of Chemistry, Faculty of Science and Technology, Keio University, 3-14-1 Hiyoshi, Yokohama 223-8522 (Japan); Fujishima, Akira [Kanagawa Academy of Science and Technology (KAST), 3-2-1 Sakado, Takatsu-ku, Kawasaki, Kanagawa 213-0012 (Japan); Kawai, Takeshi [Department of Industrial Chemistry, Faculty of Engineering, Tokyo University of Science, 1-3 Kagurazaka, Shinjuku-ku, Tokyo 162-8601 (Japan)]. E-mail: kawai@ci.kagu.tus.ac.jp

    2007-03-01

    Boron-doped diamond (BDD) thin film surfaces were modified by brief plasma treatment using various source gases such as Cl{sub 2}, CF{sub 4}, Ar and CH{sub 4}, and the electrochemical properties of the surfaces were subsequently investigated. From X-ray photoelectron spectroscopy analysis, Cl and F atoms were detected on the BDD surfaces after 3 min of Cl{sub 2} and CF{sub 4} plasma treatments, respectively. From the results of cyclic voltammetry and electrochemical AC impedance measurements, the electron-transfer rate for Fe(CN){sub 6} {sup 3-/4-} and Fe{sup 2+/3+} at the BDD electrodes was found to decrease after Cl{sub 2} and CF{sub 4} plasma treatments. However, the electron-transfer rate for Ru(NH{sub 3}){sub 6} {sup 2+/3+} showed almost no change after these treatments. This may have been related to the specific interactions of surface halogen (C-Cl and C-F) moieties with the redox species because no electrical passivation was observed after the treatments. In addition, Raman spectroscopy showed that CH{sub 4} plasma treatment of diamond surfaces formed an insulating diamond-like carbon thin layer on the surfaces. Thus, by an appropriate choice of plasma source, short-duration plasma treatments can be an effective way to functionalize diamond surfaces in various ways while maintaining a wide potential window and a low background current.

  3. Superconductive B-doped nanocrystalline diamond thin films: Electrical transport and Raman spectra

    Czech Academy of Sciences Publication Activity Database

    Nesládek, M.; Tromson, D.; Mer, Ch.; Bergonzo, P.; Hubík, Pavel; Mareš, Jiří J.

    2006-01-01

    Roč. 88, č. 23 (2006), 232111/1-232111/3 ISSN 0003-6951 R&D Projects: GA ČR(CZ) GA202/06/0040 Institutional research plan: CEZ:AV0Z10100521 Keywords : nanocrystalline diamond * superconductivity * magnetoresistance * Raman spectroscopy * Fano resonance Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 3.977, year: 2006

  4. Depth profiling of fluorine-doped diamond-like carbon (F-DLC) film: Localized fluorine in the top-most thin layer can enhance the non-thrombogenic properties of F-DLC

    Energy Technology Data Exchange (ETDEWEB)

    Hasebe, Terumitsu [Center for Science of Environment, Resources and Energy, Keio University Faculty of Science and Technology, 3-14-1 Hiyoshi, Kohoku-ku, Yokohama, Kanagawa 223-8522 (Japan); Department of Radiology, Tachikawa Hospital, 4-2-22, Nishiki-cho, Tachikawa, Tokyo 190-8531 (Japan)], E-mail: teru_hasebe@hotmail.com; Nagashima, So [Center for Science of Environment, Resources and Energy, Keio University Faculty of Science and Technology, 3-14-1 Hiyoshi, Kohoku-ku, Yokohama, Kanagawa 223-8522 (Japan); Kamijo, Aki [Department of Transfusion Medicine, the University of Tokyo Hospital, 7-3-1 Hongo, Bunkyo-ku, Tokyo 113-8655 (Japan); Yoshimura, Taichi; Ishimaru, Tetsuya; Yoshimoto, Yukihiro; Yohena, Satoshi; Kodama, Hideyuki; Hotta, Atsushi [Center for Science of Environment, Resources and Energy, Keio University Faculty of Science and Technology, 3-14-1 Hiyoshi, Kohoku-ku, Yokohama, Kanagawa 223-8522 (Japan); Takahashi, Koki [Department of Transfusion Medicine, the University of Tokyo Hospital, 7-3-1 Hongo, Bunkyo-ku, Tokyo 113-8655 (Japan); Suzuki, Tetsuya [Center for Science of Environment, Resources and Energy, Keio University Faculty of Science and Technology, 3-14-1 Hiyoshi, Kohoku-ku, Yokohama, Kanagawa 223-8522 (Japan)

    2007-12-03

    Fluorine-doped diamond-like carbon (F-DLC) has recently drawn a great deal of attention as a more non-thrombogenic coating than conventional DLC for blood-contacting medical devices. We conducted quantitative depth profiling of F-DLC film by X-ray photoelectron spectroscopy (XPS) in order to elucidate the effects of fluorine and fluorine distribution in F-DLC film in connection with the prevention of surface blood adhesion. F-DLC films were prepared on silicon substrates using the radio frequency plasma enhanced chemical vapor deposition method, and the thickness of films was {approx} 50 nm. 50-nm-thick F-DLC film samples were etched at 10-nm thickness intervals using argon plasma, and each surface was examined by XPS. Thereafter, each etched film layer was incubated with platelet-rich plasma isolated from human whole blood, and the platelet-covered area per unit area was evaluated for each surface. XPS spectra showed the localization of doped fluorine in the top-most thin layer of the film. Platelet-covered areas represented progressively larger portions of the surfaces of deeper etched layers, corresponding to the decreasing fluorine content in such sample surfaces. These results indicate that the localized fluorine in the top-most thin layer is one of the key factors in the promotion of the non-thrombogenicity of F-DLC film.

  5. Influence of sulfidation treatment on the structure and tribological properties of nitrogen-doped diamond-like carbon films

    International Nuclear Information System (INIS)

    Zeng Qunfeng; Dong Guangneng; Xie Youbai

    2008-01-01

    The nitrogen-doped diamond-like carbon (DLC) films were deposited on high speed steel (HSS) substrates in the direct current unbalanced magnetron sputtering system. Sulphurized layer was formed on the surface of DLC films by means of liquid sulfidation in the intermixture of urea and thiourea solution in order to improve the tribological properties of DLC films. The influence of sulfidation treatment on the structure and tribological properties of DLC films was investigated in this work. The structure and wear surface morphology of DLC films were analyzed by Raman spectroscopy, XPS and SEM, respectively. It reveals that the treated films are smooth and uniform; and sulfur atoms are bonded chemically. The treated films have broader distribution of Raman spectra in the range of 1000-1800 cm -1 and higher I D /I G ratio than the untreated films as a result of the appearance of the crystalline graphite structure after the sulfidation treatment. It is showed that the sp 2 relative content increase in the treated films from the XPS measurement. The Raman results are consistent with the XPS results. The tribological properties of DLC films were investigated using a ball-on-disk rotating friction and wear tester under dry friction conditions. It is found that the sulfidation concentration plays an important part in the tribological properties of the treated DLC films. The results showed the treated films with low sulfidation concentration have a lower friction coefficient (0.1) than the treated films with high sulfidation concentration (0.26) and the untreated films (0.27) under the same friction testing conditions, which can be attributed to both the presence of sulfur-containing materials and the forming of the mechanical alloyed layer on the wear surface. Adding the dry nitrogen to the sliding surface in the testing system helps the friction coefficient of the treated films with low sulfidation concentration to decrease to 0.04 further in this work. On the basis of the

  6. High-performance thermal sensitive W-doped VO{sub 2}(B) thin film and its identification by first-principles calculations

    Energy Technology Data Exchange (ETDEWEB)

    Wan, Dongyun; Xiong, Ping; Chen, Lanli [School of Materials Science and Engineering, Shanghai University, Shanghai 200444 (China); Shi, Siqi, E-mail: sqshi@shu.edu.cn [School of Materials Science and Engineering, Shanghai University, Shanghai 200444 (China); Materials Genome Institute, Shanghai University, Shanghai 200444 (China); Ishaq, Ahmad [National Center for Physics, Quaid-I-Azam University, Islamabad 44000 (Pakistan); Luo, Hongjie [School of Materials Science and Engineering, Shanghai University, Shanghai 200444 (China); Materials Genome Institute, Shanghai University, Shanghai 200444 (China); Gao, Yanfeng, E-mail: yfgao@shu.edu.cn [School of Materials Science and Engineering, Shanghai University, Shanghai 200444 (China)

    2017-03-01

    Graphical abstract: VO{sub 2}(B) thin films with high TCR and suitable resistance were first achieved by W doping. The mechanism for performance improvement was studied by first-principles calculations. The two-dimensional octahedral structure of VO{sub 2}(B) favors the strain control with W-doping for achieving a large TCR, which overcomes the contradiction between the high conductivity and large TCR generated by dopants in VO{sub 2}(M). - Highlights: • High performance W-doped VO{sub 2}(B) thin films were first achieved by co-sputtering. • Mechanism for performance improvement was studied by first-principles calculations. • The two-dimensional octahedral structure of VO{sub 2} (B) favors the strain control. • Achieved VO{sub 2} films possess high thermal sensitivity (TCR: −3.9%/K & R{sub 0}: 32.7 kΩ). - Abstract: VO{sub 2}(B) is currently a preferred phase structure for the application as bolometer material, which, however, suffers from low temperature-coefficient-of-resistance (TCR) values and large resistances. Here we present the combined experimental and first-principles calculations study on both doped and undoped VO{sub 2}(B) thin films enabling us to attain high TCR (−3.9%/k) and suitable square-resistance (32.7 kΩ) by controlled W doping employing the widely used magnetron sputtering technique. The TCR value is 50% larger than reported ones at the similar resistance. The underlying microscopic mechanism for the performance improvement was studied and results indicated that the introduction of extra electrons and the variation in the band structure resulting from the incorporation of W{sup 6+} ions in the VO{sub 2}(B) crystal lattice contribute to the enhancement of the electronic conductivity. Moreover, the special two-dimensional octahedral structure of monoclinic (C2/m) B-phase VO{sub 2} favors the strain control with W-doping for achieving a large TCR, which overcomes the analogous predicament between the high conductivity and large TCR

  7. Characterization of boron doped nanocrystalline diamonds

    International Nuclear Information System (INIS)

    Peterlevitz, A C; Manne, G M; Sampaio, M A; Quispe, J C R; Pasquetto, M P; Iannini, R F; Ceragioli, H J; Baranauskas, V

    2008-01-01

    Nanostructured diamond doped with boron was prepared using a hot-filament assisted chemical vapour deposition system fed with an ethyl alcohol, hydrogen and argon mixture. The reduction of the diamond grains to the nanoscale was produced by secondary nucleation and defects induced by argon and boron atoms via surface reactions during chemical vapour deposition. Raman measurements show that the samples are nanodiamonds embedded in a matrix of graphite and disordered carbon grains, while morphological investigations using field electron scanning microscopy show that the size of the grains ranges from 20 to 100 nm. The lowest threshold fields achieved were in the 1.6 to 2.4 V/μm range

  8. Repulsive effects of hydrophobic diamond thin films on biomolecule detection

    Energy Technology Data Exchange (ETDEWEB)

    Ruslinda, A. Rahim, E-mail: ruslindarahim@gmail.com [Institute of Nano Electronic Engineering, Universiti Malaysia Perlis, Jln Kgr-Alor Setar, Seriab, 01000 Kangar, Perlis (Malaysia); Department of Nano Science and Nano Engineering, School of Advance Science and Engineering, Ohkubo 3-4-1, Shinjuku, 169-8555 Tokyo (Japan); Ishiyama, Y. [Department of Nano Science and Nano Engineering, School of Advance Science and Engineering, Ohkubo 3-4-1, Shinjuku, 169-8555 Tokyo (Japan); Penmatsa, V. [Department of Mechanical and Materials Engineering, Florida International University, 10555 West Flagler Street, Miami, FL 33174 (United States); Ibori, S.; Kawarada, H. [Department of Nano Science and Nano Engineering, School of Advance Science and Engineering, Ohkubo 3-4-1, Shinjuku, 169-8555 Tokyo (Japan)

    2015-02-15

    Highlights: • We report the effect of fluorine plasma treatment on diamond thin film to resist the nonspecific adsorption of biomolecules. • The diamond thin film were highly hydrophobic with a surface energy value of ∼25 mN/m. • The repulsive effect shows excellent binding efficiency for both DNA and HIV-1 Tat protein. - Abstract: The repulsive effect of hydrophobic diamond thin film on biomolecule detection, such as single-nucleotide polymorphisms and human immunodeficiency virus type 1 trans-activator of transcription peptide protein detection, was investigated using a mixture of a fluorine-, amine-, and hydrogen-terminated diamond surfaces. These chemical modifications lead to the formation of a surface that effectively resists the nonspecific adsorption of proteins and other biomolecules. The effect of fluorine plasma treatment on elemental composition was also investigated via X-ray photoelectron spectroscopy (XPS). XPS results revealed a fluorocarbon layer on the diamond thin films. The contact angle measurement results indicated that the fluorine-treated diamond thin films were highly hydrophobic with a surface energy value of ∼25 mN/m.

  9. Repulsive effects of hydrophobic diamond thin films on biomolecule detection

    International Nuclear Information System (INIS)

    Ruslinda, A. Rahim; Ishiyama, Y.; Penmatsa, V.; Ibori, S.; Kawarada, H.

    2015-01-01

    Highlights: • We report the effect of fluorine plasma treatment on diamond thin film to resist the nonspecific adsorption of biomolecules. • The diamond thin film were highly hydrophobic with a surface energy value of ∼25 mN/m. • The repulsive effect shows excellent binding efficiency for both DNA and HIV-1 Tat protein. - Abstract: The repulsive effect of hydrophobic diamond thin film on biomolecule detection, such as single-nucleotide polymorphisms and human immunodeficiency virus type 1 trans-activator of transcription peptide protein detection, was investigated using a mixture of a fluorine-, amine-, and hydrogen-terminated diamond surfaces. These chemical modifications lead to the formation of a surface that effectively resists the nonspecific adsorption of proteins and other biomolecules. The effect of fluorine plasma treatment on elemental composition was also investigated via X-ray photoelectron spectroscopy (XPS). XPS results revealed a fluorocarbon layer on the diamond thin films. The contact angle measurement results indicated that the fluorine-treated diamond thin films were highly hydrophobic with a surface energy value of ∼25 mN/m

  10. Adherence of diamond films on refractory metal substrates for thermionic applications

    International Nuclear Information System (INIS)

    Tsao, B.H.; Ramalingam, M.L.; Adams, S.F.; Cloyd, J.S.

    1991-01-01

    Diamond films are currently being considered as electrical insulation material for application in the thermionic fuel element of a power producing nuclear reactor system. The function of the diamond insulator in this application is to electrically isolate the collector of each cell in the TFE from the coolant and outer sheath. Deposition of diamond films on plane surfaces of Si/SiO 2 have already been demonstrated to be quite effective. However, the diamond films on refractory metal surfaces tend to spall off in the process of deposition revealing an inefficient adherence characteristic between the film and the substrate. This paper is geared towards explaining this deficiency by way of selected experimentation and the use of analytical tools to predict uncertainties such as the mismatch in coefficient of expansion, micrographic study of the interface between the film and the substrate and X-ray diffraction spectra. The investigation of the adherence characteristics of several diamond films on Mo and Nb substrates revealed that there was an allowable stress that resulted in the formation of the critical thickness for the diamond film

  11. Thermoluminescence properties of undoped and nitrogen-doped CVD diamond exposed to gamma radiation

    International Nuclear Information System (INIS)

    Barboza-Flores, M.; Gastelum, S.; Cruz-Zaragoza, E.; Melendrez, R.; Chernov, V.; Pedroza-Montero, M.; Favalli, A.

    2008-01-01

    It is known that the thermoluminescence (TL) performance of CVD diamond depends on the impurity concentration and doping materials introduced during growing. We report on the TL properties of undoped and 750 ppm nitrogen-doped CVD diamond grown on (0 0 1) silicon substrate. The samples were exposed to gamma radiation from a Gammacell 200 Nordion irradiator in the 10-500 Gy dose range at 627 mGy/min dose rate. The nitrogen-doped CVD diamond sample exhibited a TL glow curve peaked around 537 K and a small shoulder about 411 K and a linear dose behavior in the 10-60 Gy dose range. In contrast, the undoped specimen showed a 591 K peaked TL glow curve and linear dose response for 10-100 Gy doses. However, both samples displayed a non-linear dose response for doses higher than 100 Gy. The doping effects seem to cause a higher TL efficiency, which may be attributed to the differences in the diamond bonding and amorphous carbon on the CVD samples as well as to the presence of nitrogen. In addition, the nitrogen content may produce some structural and morphological surface effects, which may account for the distinctive TL features and dose response of the diamond samples

  12. Study on the Microstructure and Electrical Properties of Boron and Sulfur Codoped Diamond Films Deposited Using Chemical Vapor Deposition

    Directory of Open Access Journals (Sweden)

    Zhang Jing

    2014-01-01

    Full Text Available The atomic-scale microstructure and electron emission properties of boron and sulfur (denoted as B-S codoped diamond films grown on high-temperature and high-pressure (HTHP diamond and Si substrates were investigated using atom force microscopy (AFM, scanning tunneling microscopy (STM, secondary ion mass spectroscopy (SIMS, and current imaging tunneling spectroscopy (CITS measurement techniques. The films grown on Si consisted of large grains with secondary nucleation, whereas those on HTHP diamond are composed of well-developed polycrystalline facets with an average size of 10–50 nm. SIMS analyses confirmed that sulfur was successfully introduced into diamond films, and a small amount of boron facilitated sulfur incorporation into diamond. Large tunneling currents were observed at some grain boundaries, and the emission character was better at the grain boundaries than that at the center of the crystal. The films grown on HTHP diamond substrates were much more perfect with higher quality than the films deposited on Si substrates. The local I-V characteristics for films deposited on Si or HTHP diamond substrates indicate n-type conduction.

  13. Synthesis and characterization of p-type boron-doped IIb diamond large single crystals

    International Nuclear Information System (INIS)

    Li Shang-Sheng; Li Xiao-Lei; Su Tai-Chao; Jia Xiao-Peng; Ma Hong-An; Huang Guo-Feng; Li Yong

    2011-01-01

    High-quality p-type boron-doped IIb diamond large single crystals are successfully synthesized by the temperature gradient method in a china-type cubic anvil high-pressure apparatus at about 5.5 GPa and 1600 K. The morphologies and surface textures of the synthetic diamond crystals with different boron additive quantities are characterized by using an optical microscope and a scanning electron microscope respectively. The impurities of nitrogen and boron in diamonds are detected by micro Fourier transform infrared technique. The electrical properties including resistivities, Hall coefficients, Hall mobilities and carrier densities of the synthesized samples are measured by a four-point probe and the Hall effect method. The results show that large p-type boron-doped diamond single crystals with few nitrogen impurities have been synthesized. With the increase of quantity of additive boron, some high-index crystal faces such as {113} gradually disappear, and some stripes and triangle pits occur on the crystal surface. This work is helpful for the further research and application of boron-doped semiconductor diamond. (cross-disciplinary physics and related areas of science and technology)

  14. Optical and electrical properties of transparent conducting B-doped ZnO thin films prepared by various deposition methods

    Energy Technology Data Exchange (ETDEWEB)

    Nomoto, Jun-ichi; Miyata, Toshihiro; Minami, Tadatsugu [Optoelectronic Device System R and D Center, Kanazawa Institute of Technology, 7-1 Ohgigaoka, Nonoichi, Ishikawa 921-8501 (Japan)

    2011-07-15

    B-doped ZnO (BZO) thin films were prepared with various thicknesses up to about 500 nm on glass substrates at 200 deg. C by dc or rf magnetron sputtering deposition, pulsed laser deposition (PLD), and vacuum arc plasma evaporation (VAPE) methods. Resistivities of 4-6 x 10{sup -4}{Omega} cm were obtained in BZO thin films prepared with a B content [B/(B + Zn) atomic ratio] around 1 at. % by PLD and VAPE methods: Hall mobilities above 40 cm{sup 2}/Vs and carrier concentrations on the order of 10{sup 20} cm{sup -3}. All 500-nm-thick-BZO thin films prepared with a resistivity on the order of 10{sup -3}-10{sup -4}{Omega} cm exhibited an averaged transmittance above 80% in the wavelength range of 400-1100 nm. The resistivity in BZO thin films prepared with a thickness below about 500 nm was found to increase over time with exposure to various high humidity environments. In heat-resistance tests, the resistivity stability of BZO thin films was found to be nearly equal to that of Ga-doped ZnO thin films, so these films were judged suitable for use as a transparent electrode for thin-film solar cells.

  15. Modified diamond electrodes for electrolysis and electroanalysis applications

    International Nuclear Information System (INIS)

    Einaga, Yasuaki; Sato, Rika; Olivia, Herlambang; Shin, Dongchan; Ivandini, T.A.; Fujishima, Akira

    2004-01-01

    The outstanding properties of diamond make it a very attractive material for use in many potential applications. In particular, the superior electrochemical properties of highly boron-doped conductive diamond films, prepared by the chemical vapor deposition (CVD) process, have received attention from electrochemists. This paper reports several diversified applications of boron-doped diamond electrodes; highly sensitive and interference-free microfiber electrodes with over-oxidized polypyrrole modification, integrated electrochemical detector for microchip capillary electrophoresis (CE), and smoothing treatments of micro-polycrystalline surface. Studies have been made of the electrochemical properties of each system and their application in electroanalysis is discussed

  16. [Influence of deposition time on chromatics during nitrogen-doped diamond like carbon coating on pure titanium].

    Science.gov (United States)

    Yin, Lu; Yao, Jiang-wu; Xu, De-wen

    2010-10-01

    The aim of this study was to observed the influence of deposition time on chromatics during nitrogen-doped diamond like carbon coating (N-DLC) on pure titanium by multi impulse are plasma plating machine. Applying multi impulse are plasma plating machine to produce TiN coatings on pure titanium in nitrogen atmosphere, then filming with nitrogen-doped DLC on TiN in methane (10-80 min in every 5 min). The colors of N-DLC were evaluated in the CIE1976 L*a*b* uniform color scale and Mussell notation. The surface morphology of every specimen was analyzed using scanning electron microscope (SEM) and X-ray photoelectron spectroscopy (XPS). When changing the time of N-DLC coating deposition, N-DLC surface showed different color. Golden yellow was presented when deposition time was 30 min. SEM showed that crystallization was found in N-DLC coatings, the structure changed from stable to clutter by varying the deposition time. The chromatics of N-DLC coatings on pure titanium could get golden yellow when deposition time was 30 min, then the crystallized structure was stable.

  17. In-situ boron doping of chemical-bath deposited CdS thin films

    International Nuclear Information System (INIS)

    Khallaf, Hani; Park, S.; Schulte, Alfons; Chai, Guangyu; Lupan, Oleg; Chow, Lee; Heinrich, Helge

    2009-01-01

    In-situ boron doping of CdS using chemical-bath deposition (CBD) is reported. The effect of B doping on optical properties, as well as electrical properties, crystal structure, chemistry, and morphology of CdS films is studied. We present a successful approach towards B doping of CdS using CBD, where a resistivity as low as 1.7 x 10 -2 Ωcm and a carrier density as high as 1.91 x 10 19 cm -3 were achieved. The bandgap of B-doped films was found to slightly decrease as the[B]/[Cd] ratio in the solution increases. X-ray diffraction studies showed B 3+ ions likely enter the lattice substitutionally. A phase transition, due to annealing, as well as induced lattice defects, due to B doping, were detected by micro-Raman spectroscopy and transmission electron microscopy. The chemistry and morphology of films were unaffected by B doping. (copyright 2009 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim) (orig.)

  18. Microstructure and mechanical properties of Ti/Al co-doped DLC films: Dependence on sputtering current, source gas, and substrate bias

    International Nuclear Information System (INIS)

    Guo, Ting; Kong, Cuicui; Li, Xiaowei; Guo, Peng; Wang, Zhenyu; Wang, Aiying

    2017-01-01

    Highlights: • Ti/Al co-doped diamond-like carbon films were fabricated by a hybrid ion beam method. • Process parameters affected the structure and chemical state of co-doped Ti and Al. • The relation between microstructure and properties was investigated systematically. • The guidance to tailor the Ti/Al-DLC films with high performance was provided. - Abstract: Co-doping two metal elements into diamond-like carbon (DLC) films can reach the desirable combined properties, but the preparation and commercialized application of metal co-doped DLC films with well-defined structural properties are currently hindered by the non-comprehensive understanding of structural evolutions under different process parameters. Here, we fabricated the Ti/Al-DLC films using a unique hybrid ion beam system which enabled the independent control of metal content and carbon structure. The evolutions of microstructure, residual compressive stress and mechanical properties induced by the different process parameters including sputtering currents, C_2H_2 or CH_4 source gases and bias voltages were investigated systematically in order to perform in-depth analysis on the relation between the structure and properties in Ti/Al-DLC films. Results revealed that the variations of process parameters seriously affected the concentration and chemical bond state of co-doped Ti/Al atoms in amorphous carbon matrix or incident energies of C ions, which brought the complicated effect on amorphous carbon structures, accounting for the change of residual compressive stress, hardness and toughness. The present results provide the guidance for suitable, effective parameters selection to tailor the Ti/Al-DLC films with high performance for further applications.

  19. Microstructure and mechanical properties of Ti/Al co-doped DLC films: Dependence on sputtering current, source gas, and substrate bias

    Energy Technology Data Exchange (ETDEWEB)

    Guo, Ting [Key Laboratory of Marine Materials and Related Technologies, Zhejiang Key Laboratory of Marine Materials and Protective Technologies, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201 (China); School of Materials Science and Engineering, Shanghai University, Shanghai 200444 (China); Kong, Cuicui [Key Laboratory of Marine Materials and Related Technologies, Zhejiang Key Laboratory of Marine Materials and Protective Technologies, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201 (China); Ningbo University, Ningbo 315201 (China); Li, Xiaowei, E-mail: lixw@nimte.ac.cn [Key Laboratory of Marine Materials and Related Technologies, Zhejiang Key Laboratory of Marine Materials and Protective Technologies, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201 (China); Guo, Peng; Wang, Zhenyu [Key Laboratory of Marine Materials and Related Technologies, Zhejiang Key Laboratory of Marine Materials and Protective Technologies, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201 (China); Wang, Aiying, E-mail: aywang@nimte.ac.cn [Key Laboratory of Marine Materials and Related Technologies, Zhejiang Key Laboratory of Marine Materials and Protective Technologies, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201 (China)

    2017-07-15

    Highlights: • Ti/Al co-doped diamond-like carbon films were fabricated by a hybrid ion beam method. • Process parameters affected the structure and chemical state of co-doped Ti and Al. • The relation between microstructure and properties was investigated systematically. • The guidance to tailor the Ti/Al-DLC films with high performance was provided. - Abstract: Co-doping two metal elements into diamond-like carbon (DLC) films can reach the desirable combined properties, but the preparation and commercialized application of metal co-doped DLC films with well-defined structural properties are currently hindered by the non-comprehensive understanding of structural evolutions under different process parameters. Here, we fabricated the Ti/Al-DLC films using a unique hybrid ion beam system which enabled the independent control of metal content and carbon structure. The evolutions of microstructure, residual compressive stress and mechanical properties induced by the different process parameters including sputtering currents, C{sub 2}H{sub 2} or CH{sub 4} source gases and bias voltages were investigated systematically in order to perform in-depth analysis on the relation between the structure and properties in Ti/Al-DLC films. Results revealed that the variations of process parameters seriously affected the concentration and chemical bond state of co-doped Ti/Al atoms in amorphous carbon matrix or incident energies of C ions, which brought the complicated effect on amorphous carbon structures, accounting for the change of residual compressive stress, hardness and toughness. The present results provide the guidance for suitable, effective parameters selection to tailor the Ti/Al-DLC films with high performance for further applications.

  20. Boron doped diamond synthesized from detonation nanodiamond in a C-O-H fluid at high pressure and high temperature

    Science.gov (United States)

    Shakhov, Fedor M.; Abyzov, Andrey M.; Takai, Kazuyuki

    2017-12-01

    Boron doped diamond (BDD) was synthesized under high pressure and high temperature (HPHT) of 7 GPa, 1230 °C in a short time of 10 s from a powder mixtures of detonation nanodiamond (DND), pentaerythritol C5H8(OH)4 and amorphous boron. SEM, TEM, XRD, XPS, FTIR and Raman spectroscopy indicated that BDD nano- and micro-crystals have formed by consolidation of DND particles (4 nm in size). XRD showed the enlargement of crystallites size to 6-80 nm and the increase in diamond lattice parameter by 0.02-0.07% without appearance of any microstrains. Raman spectroscopy was used to estimate the content of boron atoms embedded in the diamond lattice. It was found that the Raman diamond peak shifts significantly from 1332 cm-1 to 1290 cm-1 without appearance of any non-diamond carbon. The correlation between Raman peak position, its width, and boron content in diamond is proposed. Hydrogenated diamond carbon in significant amount was detected by IR spectroscopy and XPS. Due to the doping with boron content of about 0.1 at%, the electrical conductivity of the diamond achieved approximately 0.2 Ω-1 cm-1. Reaction mechanism of diamond growth (models of recrystallization and oriented attachment) is discussed, including the initial stages of pentaerythritol pyrolysis and thermal desorption of functional groups from the surface of DND particles with the generation of supercritical fluid of low-molecular substances (H2O, CH4, CO, CO2, etc.), as well as byproducts formation (B2O3, B4C).

  1. Transient photoresponse of nitrogen-doped ultrananocrystalline diamond electrodes in saline solution

    Energy Technology Data Exchange (ETDEWEB)

    Ahnood, Arman, E-mail: arman.ahnood@unimelb.edu.au; Ganesan, Kumaravelu; Stacey, Alastair; Prawer, Steven [School of Physics, University of Melbourne, Melbourne, Victoria 3010 (Australia); Simonov, Alexandr N.; Spiccia, Leone [School of Chemistry and the ARC Centre of Excellence for Electromaterials Science, Monash University, Melbourne, Victoria 3800 (Australia); Laird, Jamie S. [CSIRO, Minerals Resources Flagship, School of Physics, University of Melbourne, Melbourne, Victoria 3010 (Australia); Maturana, Matias I. [National Vision Research Institute, Australian College of Optometry, Carlton, Victoria 3053 (Australia); NeuroEngineering Laboratory, Department of Electrical and Electronic Engineering, University of Melbourne, Parkville, Victoria 3010 (Australia); Ibbotson, Michael R. [National Vision Research Institute, Australian College of Optometry, Carlton, Victoria 3053 (Australia); ARC Centre of Excellence for Integrative Brain Function, Department of Optometry and Vision Sciences, University of Melbourne, Parkville, Victoria 3010 (Australia)

    2016-03-07

    Beyond conventional electrically-driven neuronal stimulation methods, there is a growing interest in optically-driven approaches. In recent years, nitrogen-doped ultrananocrystalline diamond (N-UNCD) has emerged as a strong material candidate for use in electrically-driven stimulation electrodes. This work investigates the electrochemical activity of N-UNCD in response to pulsed illumination, to assess its potential for use as an optically-driven stimulation electrode. Whilst N-UNCD in the as-grown state exhibits a weak photoresponse, the oxygen plasma treated film exhibits two orders of magnitude enhancement in its sub-bandgap open circuit photovoltage response. The enhancement is attributed to the formation of a dense network of oxygen-terminated diamond nanocrystals at the N-UNCD surface. Electrically connected to the N-UNCD bulk via sub-surface graphitic grain boundaries, these diamond nanocrystals introduce a semiconducting barrier between the sub-surface graphitic semimetal and the electrolyte solution, leading to a photovoltage under irradiation with wavelengths of λ = 450 nm and shorter. Within the safe optical exposure limit of 2 mW mm{sup −2}, charge injection capacity of 0.01 mC cm{sup −2} is achieved using a 15 × 15 μm electrode, meeting the requirements for extracellular and intercellular stimulation. The nanoscale nature of processes presented here along with the diamond's biocompatibility and biostability open an avenue for the use of oxygen treated N-UNCD as optically driven stimulating electrodes.

  2. Transient photoresponse of nitrogen-doped ultrananocrystalline diamond electrodes in saline solution

    International Nuclear Information System (INIS)

    Ahnood, Arman; Ganesan, Kumaravelu; Stacey, Alastair; Prawer, Steven; Simonov, Alexandr N.; Spiccia, Leone; Laird, Jamie S.; Maturana, Matias I.; Ibbotson, Michael R.

    2016-01-01

    Beyond conventional electrically-driven neuronal stimulation methods, there is a growing interest in optically-driven approaches. In recent years, nitrogen-doped ultrananocrystalline diamond (N-UNCD) has emerged as a strong material candidate for use in electrically-driven stimulation electrodes. This work investigates the electrochemical activity of N-UNCD in response to pulsed illumination, to assess its potential for use as an optically-driven stimulation electrode. Whilst N-UNCD in the as-grown state exhibits a weak photoresponse, the oxygen plasma treated film exhibits two orders of magnitude enhancement in its sub-bandgap open circuit photovoltage response. The enhancement is attributed to the formation of a dense network of oxygen-terminated diamond nanocrystals at the N-UNCD surface. Electrically connected to the N-UNCD bulk via sub-surface graphitic grain boundaries, these diamond nanocrystals introduce a semiconducting barrier between the sub-surface graphitic semimetal and the electrolyte solution, leading to a photovoltage under irradiation with wavelengths of λ = 450 nm and shorter. Within the safe optical exposure limit of 2 mW mm"−"2, charge injection capacity of 0.01 mC cm"−"2 is achieved using a 15 × 15 μm electrode, meeting the requirements for extracellular and intercellular stimulation. The nanoscale nature of processes presented here along with the diamond's biocompatibility and biostability open an avenue for the use of oxygen treated N-UNCD as optically driven stimulating electrodes.

  3. Tribological properties of nanocrystalline diamond films

    Energy Technology Data Exchange (ETDEWEB)

    Erdemir, A.; Fenske, G.R.; Krauss, A.R.; Gruen, D.M.; McCauley, T.; Csencsits, R.T. [Argonne National Lab., IL (United States). Energy Technology Div.

    1999-11-01

    In this paper, we present the friction and wear properties of nanocrystalline diamond (NCD) films grown in Ar-fullerene (C{sub 60}) and Ar-CH{sub 4} microwave plasmas. Specifically, we will address the fundamental tribological issues posed by these films during sliding against Si{sub 3}N{sub 4} counterfaces in ambient air and inert gases. Grain sizes of the films grown by the new method are very small (10-30 nm) and are much smoother (20-40 nm, root mean square) than those of films grown by the conventional H{sub 2}-CH{sub 4} microwave-assisted chemical vapor deposition process. Transmission electron microscopy (TEM) revealed that the grain boundaries of these films are very sharp and free of nondiamond phases. The microcrystalline diamond films grown by most conventional methods consist of large grains and a rough surface finish, which can cause severe abrasion during sliding against other materials. The friction coefficients of films grown by the new method (i.e. in Ar-C{sub 60} and Ar-CH{sub 4} plasmas) are comparable with those of natural diamond, and wear damage on counterface materials is minimal. Fundamental tribological studies indicate that these films may undergo phase transformation during long-duration, high-speed and/or high-load sliding tests and that the transformation products trapped at the sliding interfaces can intermittently dominate friction and wear performance. Using results from a combination of TEM, electron diffraction, Raman spectroscopy, and electron energy loss spectroscopy, we describe the structural chemistry of the debris particles trapped at the sliding interfaces and elucidate their possible effects on friction and wear of NCD films in dry N{sub 2}. Finally, we suggest a few potential applications in which NCD films can improve performance and service lives. (orig.)

  4. Morphology modulating the wettability of a diamond film.

    Science.gov (United States)

    Tian, Shibing; Sun, Weijie; Hu, Zhaosheng; Quan, Baogang; Xia, Xiaoxiang; Li, Yunlong; Han, Dong; Li, Junjie; Gu, Changzhi

    2014-10-28

    Control of the wetting property of diamond surface has been a challenge because of its maximal hardness and good chemical inertness. In this work, the micro/nanoarray structures etched into diamond film surfaces by a maskless plasma method are shown to fix a surface's wettability characteristics, and this means that the change in morphology is able to modulate the wettability of a diamond film from weakly hydrophilic to either superhydrophilic or superhydrophobic. It can be seen that the etched diamond surface with a mushroom-shaped array is superhydrophobic following the Cassie mode, whereas the etched surface with nanocone arrays is superhydrophilic in accordance with the hemiwicking mechnism. In addition, the difference in cone densities of superhydrophilic nanocone surfaces has a significant effect on water spreading, which is mainly derived from different driving forces. This low-cost and convenient means of altering the wetting properties of diamond surfaces can be further applied to underlying wetting phenomena and expand the applications of diamond in various fields.

  5. Synthetic diamond in electrochemistry

    International Nuclear Information System (INIS)

    Pleskov, Yurii V

    1999-01-01

    The results of studies on the electrochemistry of diamond carried out during the last decade are reviewed. Methods for the preparation, the crystalline structure and the main electrophysical properties of diamond thin films are considered. Depending on the doping conditions, the diamond behaves as a superwide-gap semiconductor or as a semimetal. It is shown that the 'metal-like' diamond is corrosion-resistant and can be used advantageously as an electrode in the electrosynthesis (in particular, for the electroreduction of compounds that are difficult to reduce) and electroanalysis. Kinetic characteristics of some redox reactions and the impedance parameters for diamond electrodes are presented. The results of comparative studies of the electrodes made of diamond single crystals, polycrystalline diamond and amorphous diamond-like carbon, which reveal the effect of the crystalline structure (e.g., the influence of intercrystallite boundaries) on the electrochemical properties of diamond, are presented. The bibliography includes 99 references.

  6. New route to the fabrication of nanocrystalline diamond films

    International Nuclear Information System (INIS)

    Varshney, Deepak; Morell, Gerardo; Palomino, Javier; Resto, Oscar; Gil, Jennifer; Weiner, Brad R.

    2014-01-01

    Nanocrystalline diamond (NCD) thin films offer applications in various fields, but the existing synthetic approaches are cumbersome and destructive. A major breakthrough has been achieved by our group in the direction of a non-destructive, scalable, and economic process of NCD thin-film fabrication. Here, we report a cheap precursor for the growth of nanocrystalline diamond in the form of paraffin wax. We show that NCD thin films can be fabricated on a copper support by using simple, commonplace paraffin wax under reaction conditions of Hot Filament Chemical Vapor Deposition (HFCVD). Surprisingly, even the presence of any catalyst or seeding that has been conventionally used in the state-of-the-art is not required. The structure of the obtained films was analyzed by scanning electron microscopy and transmission electron microscopy. Raman spectroscopy and electron energy-loss spectroscopy recorded at the carbon K-edge region confirm the presence of nanocrystalline diamond. The process is a significant step towards cost-effective and non-cumbersome fabrication of nanocrystalline diamond thin films for commercial production

  7. Nanodiamond Films for Applications in Electrochemical Systems

    Directory of Open Access Journals (Sweden)

    A. F. Azevedo

    2012-01-01

    Full Text Available The purpose of the present paper is to give an overview on the current development status of nanocrystalline diamond electrodes for electrochemical applications. Firstly, we describe a brief comparison between the general properties of nanocrystalline diamond (undoped and boron-doped and boron-doped microcrystalline diamond films. This is followed by a summary of the nanodiamond preparation methods. Finally, we present a discussion about the undoped and boron-doped nanocrystalline diamond and their characteristics, electrochemical properties, and practical applications.

  8. THIN DIAMOND FILMS FOR SNS H INJECTIONS STRIPPING

    International Nuclear Information System (INIS)

    SHAW, R.W.; HERR, A.D.; FEIGERLE, C.S.; CUTLER, R.J.; LIAW, C.J.; LEE, Y.Y.

    2004-01-01

    We have investigated the preparation and testing of thin diamond foils for use in stripping the SNS H - Linac beam. A long useful lifetime for these foils is desirable to improve operational efficiency. Preliminary data presented at PAC 2001 indicated that diamond foils were superior to conventional evaporated carbon foils, exhibiting lifetimes approximately five-fold longer [1]. That work employed a fully supported diamond foil, a format that is not acceptable for the SNS application; at least two edges of the approximately 1 x 1 cm foils must be free standing to allow for beam rastering. Residual stress in a chemical vapor deposited (CVD) diamond foil results in film distortion (scrolling) when the film is released from its silicon growth substrate. We have attacked this problem by initially patterning the surface of CVD growth substrates with a 50 or 100 line/inch trapezoidal grating, followed by conformal diamond film growth on the patterned substrate. Then removal of the substrate by chemical etching produced a foil that possessed improved mechanical integrity due to its corrugation. The high nucleation density required to grow continuous, pinhole free diamond foils of the desired thickness (1 (micro)m, 350 (micro)g/cm 2 ) was achieved by a combination of substrate surface scratching and seeding. A variety of diamond foils have been tested using the BNL 750 keV Radio Frequency Quadrupole H - beam to simulate energy loss in the SNS. Those include flat, corrugated, microcrystalline, and nanocrystalline foils. Foil lifetimes are reported

  9. Electrochemical oxidation of biological pretreated and membrane separated landfill leachate concentrates on boron doped diamond anode

    Energy Technology Data Exchange (ETDEWEB)

    Zhou, Bo, E-mail: 357436235@qq.com [School of Materials Science and Engineering, Central South University, Changsha 410083 (China); Yu, Zhiming, E-mail: zhiming@csu.edu.cn [School of Materials Science and Engineering, Central South University, Changsha 410083 (China); State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083 (China); Wei, Qiuping, E-mail: qiupwei@csu.edu.cn [School of Materials Science and Engineering, Central South University, Changsha 410083 (China); State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083 (China); Long, HangYu, E-mail: 55686385@qq.com [School of Materials Science and Engineering, Central South University, Changsha 410083 (China); Xie, Youneng, E-mail: 1187272844@qq.com [School of Materials Science and Engineering, Central South University, Changsha 410083 (China); Wang, Yijia, E-mail: 503630433@qq.com [School of Materials Science and Engineering, Central South University, Changsha 410083 (China)

    2016-07-30

    Highlights: • High quality boron-doped diamond film electrodes were synthesized on Nb substrates. • Electrochemical oxidation on boron-doped diamond anode is an effective method for treating landfill leachate concentrates. • Optimal operating conditions for electrochemical oxidation of landfill leachate concentrates is determined. • 87.5% COD removal and 74.06% NH{sub 3}−N removal were achieved after 6 h treatment. - Abstract: In the present study, the high quality boron-doped diamond (BDD) electrodes with excellent electrochemical properties were deposited on niobium (Nb) substrates by hot filament chemical vapor deposition (HFCVD) method. The electrochemical oxidation of landfill leachate concentrates from disc tube reverse osmosis (DTRO) process over a BDD anode was investigated. The effects of varying operating parameters, such as current density, initial pH, flow velocity and cathode material on degradation efficiency were also evaluated following changes in chemical oxygen demand (COD) and ammonium nitrogen (NH{sub 3}−N). The instantaneous current efficiency (ICE) was used to appraise different operating conditions. As a result, the best conditions obtained were as follows, current density 50 mA cm{sup −2}, pH 5.16, flow velocity 6 L h{sup −1}. Under these conditions, 87.5% COD and 74.06% NH{sub 3}−N removal were achieved after 6 h treatment, with specific energy consumption of 223.2 kWh m{sup −3}. In short, these results indicated that the electrochemical oxidation with BDD/Nb anode is an effective method for the treatment of landfill leachate concentrates.

  10. Low-temperature synthesis of diamond films by photoemission-assisted plasma-enhanced chemical vapor deposition

    Energy Technology Data Exchange (ETDEWEB)

    Kawata, Mayuri, E-mail: kawata@mail.tagen.tohoku.ac.jp; Ojiro, Yoshihiro; Ogawa, Shuichi; Takakuwa, Yuji [Institute of Multidisciplinary Research for Advanced Materials, Tohoku University, 2-1-1 Katahira, Aoba-ku, Sendai 980-8577 (Japan); Masuzawa, Tomoaki; Okano, Ken [International Christian University, 3-10-2 Osawa, Mitaka 181-8585 (Japan)

    2014-03-15

    Photoemission-assisted plasma-enhanced chemical vapor deposition (PA-PECVD), a process in which photoelectrons emitted from a substrate irradiated with ultraviolet light are utilized as a trigger for DC discharge, was investigated in this study; specifically, the DC discharge characteristics of PA-PECVD were examined for an Si substrate deposited in advance through hot-filament chemical vapor deposition with a nitrogen-doped diamond layer of thickness ∼1 μm. Using a commercially available Xe excimer lamp (hν = 7.2 eV) to illuminate the diamond surface with and without hydrogen termination, the photocurrents were found to be 3.17 × 10{sup 12} and 2.11 × 10{sup 11} electrons/cm{sup 2}/s, respectively. The 15-fold increase in photocurrent was ascribed to negative electron affinity (NEA) caused by hydrogen termination on the diamond surfaces. The DC discharge characteristics revealed that a transition bias voltage from a Townsend-to-glow discharge was considerably decreased because of NEA (from 490 to 373 V for H{sub 2} gas and from 330 to 200 V for Ar gas), enabling a reduction in electric power consumption needed to synthesize diamond films through PA-PECVD. In fact, the authors have succeeded in growing high-quality diamond films of area 2.0 cm{sup 2} at 540 °C with a discharge power of only 1.8 W, plasma voltage of 156.4 V, and discharge current of 11.7 mA under the glow discharge of CH{sub 4}/H{sub 2}/Ar mixed gases. In addition to having only negligible amounts of graphite and amorphous carbon, the diamond films exhibit a relatively high diamond growth rate of 0.5 μm/h at temperatures as low as 540 °C, which is attributed to Ar{sup +} ions impinging on the diamond surface, and causing the removal of hydrogen atoms from the surface through sputtering. This process leads to enhanced CH{sub x} radical adsorption, because the sample was applied with a negative potential to accelerate photoelectrons in PA-PECVD.

  11. Laser Raman microprobe spectroscopy as a diagnostic for the characterisation of diamond and diamond like carbon (DLC) thin films

    International Nuclear Information System (INIS)

    Johnston, C.

    1990-10-01

    Invariably when manufacturing an artificial diamond film a mixture of carbon is deposited - tetragonally bonded (diamond), trigonally bonded (graphite) and other allotropic crystalline forms and amorphous carbons. This imposes a need for careful analysis to determine exactly what carbon types constitute the films. Raman spectroscopy is particularly sensitive to crystal and atomic structure and has a number of advantages which make it one of the most useful techniques for interrogating diamond and DLC thin films. Although Raman spectroscopy alone cannot fully characterise the film, it can give more information than simply what particular form of carbon or other impurities are present in the film. It can be used to determine the ratio of sp 2 to sp 3 bonding within the film, and to some extent the crystallite or domain size and the internal stress of the film. The use of laser Raman microprobe spectroscopy as a diagnostic tool in the analysis of diamond and DLC thin films is demonstrated for a variety of carbon films on various substrates and the characterisation of these films is discussed. (author)

  12. Characterization of chemical vapour deposited diamond films: correlation between hydrogen incorporation and film morphology and quality

    International Nuclear Information System (INIS)

    Tang, C J; Neves, A J; Carmo, M C

    2005-01-01

    In order to tailor diamond synthesized through chemical vapour deposition (CVD) for different applications, many diamond films of different colours and variable quality were deposited by a 5 kW microwave plasma CVD reactor under different growth conditions. The morphology, quality and hydrogen incorporation of these films were characterized using scanning electron microscopy (SEM), Raman and Fourier-transform infrared (FTIR) spectroscopy, respectively. From this study, a general trend between hydrogen incorporation and film colour, morphology and quality was found. That is, as the films sorted by colour gradually become darker, ranging from white through grey to black, high magnification SEM images illustrate that the smoothness of the well defined crystalline facet gradually decreases and second nucleation starts to appear on it, indicating gradual degradation of the crystalline quality. Correspondingly, Raman spectra evidence that the diamond Raman peak at 1332 cm -1 becomes broader and the non-diamond carbon band around 1500 cm -1 starts to appear and becomes stronger, confirming increase of the non-diamond component and decrease of the phase purity of the film, while FTIR spectra show that the CH stretching band and the two CVD diamond specific peaks around 2830 cm -1 rise rapidly, and this indicates that the total amount of hydrogen incorporated into the film increases significantly

  13. Measurement setup for the magnetic penetration depth and superfluid stiffness in thin superconducting films

    Energy Technology Data Exchange (ETDEWEB)

    Fuchs, Lorenz; Brunner, Markus Christopher Paul; Schneider, Ina; Kronfeldner, Klaus; Strunk, Christoph [Institute for exp. and appl. Physics, University of Regensburg (Germany); Bousquet, Jessica; Bustarret, Etienne [Institut NEEL, Grenoble (France)

    2015-07-01

    A mutual inductance measurement setup has been established in order to determine the magnetic penetration depths of thin film superconductors. By measuring the variation of the mutual inductance M, the temperature dependent penetration depth can be evaluated. The setup has been characterized using thin aluminum and niobium films as a reference. Temperature dependence of λ of B-doped diamond films is determined down to 0.3 K and compared with theoretical expectations. The impact of the doping ratio B/C and film thickness on λ and T{sub c} is investigated. Correlation between the film impedance σ = σ{sub 1} - i σ{sub 2} and λ is examined.

  14. UV detectors based on epitaxial diamond films grown on single-crystal diamond substrates by vapor-phase synthesis

    International Nuclear Information System (INIS)

    Sharonov, G.V.; Petrov, S.A.; Bol'shakov, A.P.; Ral'chenko, V.G.; Kazyuchits, N.M.

    2010-01-01

    The prospects for use of CVD-technology for epitaxial growth of single-crystal diamond films of instrumental quality in UHF plasma for the production of optoelectronic devices are discussed. A technology for processing diamond single crystals that provides a perfect surface crystal structure with roughness less than 0,5 nm was developed. It was demonstrated that selective UV detectors based on synthetic single-crystal diamond substrates coated with single-crystal films can be produced. A criterion for selecting clean and structurally perfect single crystals of synthetic diamond was developed for the epitaxial growth technology. (authors)

  15. Optical characterization of hydrogen-free CeO2 doped DLC films deposited by unbalanced magnetron sputtering

    International Nuclear Information System (INIS)

    Zhang Zhenyu; Zhou Hongxiu; Guo Dongming; Gao Hang; Kang Renke

    2008-01-01

    A novel kind of hydrogen-free CeO 2 doped diamond-like carbon (DLC) films with thickness of 180-200 nm were deposited on silicon by unbalanced magnetron sputtering. Reduced reflectance and increased lifetime are expected with respect to pure DLC films, making these coatings good candidates as optical protective coatings for IR windows and solar cells. X-ray photoelectron spectroscopy confirms that CeO 2 is formed within the DLC films. Auger electron spectroscopy exhibits that the C, O, and Ce elements distribute uniformly across the film thickness, and C element diffuses into the Si substrate at the interface between the substrate and film. AFM shows that nanoparticles with diameter of around 50 nm are formed on the surface of deposited films, whose surface roughness is in the range of 1.3-2.3 nm. Raman spectra show the CeO 2 doped DLC films are amorphous DLC films, and both the G frequency and relative intensity ratio I D /I G are higher than those of pure DLC films. The photoluminescence of CeO 2 doped DLC films is obviously more intense than that of a pure DLC film, which indicates a promising potential as optical protective films for solar cells and IR window

  16. N-type doped nano-diamond in a first MEMS application

    Energy Technology Data Exchange (ETDEWEB)

    Dipalo, M.; Kusterer, J.; Janischowsky, K.; Kohn, E. [Dept. of Electron Devices and Circuits, University of Ulm, Albert Einstein Allee 45, 89081 Ulm (Germany)

    2006-09-15

    Nanocrystalline diamond is an interesting material for MEMS applications especially due to its outstanding mechanical, electrical and electrochemical properties. The current choice for doping is boron, resulting in p-type conduction. It has two difficulties: firstly, at high concentration (as needed for full activation) the lattice becomes highly stressed and may degrade the material's quality. Secondly, it contaminates the growth chamber, resulting in a memory effect. A recent alternative is n-type nitrogen doping, avoiding these disadvantages. However, nitrogen is mainly incorporated in the grain boundaries and thus inhomogeneously distributed. In turn this may limit the material's stability. Here we present a first trial to use nitrogen-doped nanocrystalline diamond (NCD), grown by hot filament CVD, in a water microjet as heater element. No stability problems were encountered even at high overdrive power. (copyright 2006 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim) (orig.)

  17. Investigation of laser ablation of CVD diamond film

    Science.gov (United States)

    Chao, Choung-Lii; Chou, W. C.; Ma, Kung-Jen; Chen, Ta-Tung; Liu, Y. M.; Kuo, Y. S.; Chen, Ying-Tung

    2005-04-01

    Diamond, having many advanced physical and mechanical properties, is one of the most important materials used in the mechanical, telecommunication and optoelectronic industry. However, high hardness value and extreme brittleness have made diamond extremely difficult to be machined by conventional mechanical grinding and polishing. In the present study, the microwave CVD method was employed to produce epitaxial diamond films on silicon single crystal. Laser ablation experiments were then conducted on the obtained diamond films. The underlying material removal mechanisms, microstructure of the machined surface and related machining conditions were also investigated. It was found that during the laser ablation, peaks of the diamond grains were removed mainly by the photo-thermal effects introduced by excimer laser. The diamond structures of the protruded diamond grains were transformed by the laser photonic energy into graphite, amorphous diamond and amorphous carbon which were removed by the subsequent laser shots. As the protruding peaks gradually removed from the surface the removal rate decreased. Surface roughness (Ra) was improved from above 1μm to around 0.1μm in few minutes time in this study. However, a scanning technique would be required if a large area was to be polished by laser and, as a consequence, it could be very time consuming.

  18. Adherent diamond film deposited on Cu substrate by carbon transport from nanodiamond buried under Pt interlayer

    Energy Technology Data Exchange (ETDEWEB)

    Liu Xuezhang [School of Materials Science and Engineering, Central South University, Changsha, 410083 (China); Wei Qiuping, E-mail: qiupwei@csu.edu.cn [School of Materials Science and Engineering, Central South University, Changsha, 410083 (China); State Key Laboratory of Powder Metallurgy, Central South University, Changsha, 410083 (China); Yu Zhiming, E-mail: zhiming@csu.edu.cn [School of Materials Science and Engineering, Central South University, Changsha, 410083 (China); State Key Laboratory of Powder Metallurgy, Central South University, Changsha, 410083 (China); Yang Taiming; Zhai Hao [School of Materials Science and Engineering, Central South University, Changsha, 410083 (China)

    2013-01-15

    Highlights: Black-Right-Pointing-Pointer Adherent polycrystalline diamond films were grown on copper substrate by carbon transport. Black-Right-Pointing-Pointer The nucleation density was increased to 10{sup 11} cm{sup -2}. Black-Right-Pointing-Pointer Diamond films were a composite structure of nano-crystalline diamond layer and micro-crystalline diamond layer. Black-Right-Pointing-Pointer Diamond nucleation was based by carbon dissolving from UDDs to Pt interlayer and formation of sp{sup 3}-bonded diamond clusters at the Pt surface. - Abstract: Diamond film deposited on Cu suffered from poor adhesion mainly due to the large mismatch of thermal expansion coefficients and the lack of affinity between carbon and Cu. Enhancing diamond nucleation by carbon transport from buried nanodiamond through a Pt ultrathin interlayer, adherent diamond film was then deposited on Cu substrate without distinctly metallic interlayer. This novel nucleation mechanism increased diamond nucleation density to 10{sup 11} cm{sup -2}, and developed diamond film with a composite structure of nano-crystalline diamond (NCD) layer and micro-crystalline diamond layer. Diamond film was characterized by the scanning electron microscope (SEM) and Raman spectroscope, respectively. The composition of diamond film/Cu substrate interface was examined by electron probe microanalysis (EPMA). The adhesion of diamond film was evaluated by indentation test. Those results show that a Pt ultrathin interlayer provides stronger chemically bonded interfaces and improve film adhesion.

  19. Adherent diamond film deposited on Cu substrate by carbon transport from nanodiamond buried under Pt interlayer

    International Nuclear Information System (INIS)

    Liu Xuezhang; Wei Qiuping; Yu Zhiming; Yang Taiming; Zhai Hao

    2013-01-01

    Highlights: ► Adherent polycrystalline diamond films were grown on copper substrate by carbon transport. ► The nucleation density was increased to 10 11 cm −2 . ► Diamond films were a composite structure of nano-crystalline diamond layer and micro-crystalline diamond layer. ► Diamond nucleation was based by carbon dissolving from UDDs to Pt interlayer and formation of sp 3 -bonded diamond clusters at the Pt surface. - Abstract: Diamond film deposited on Cu suffered from poor adhesion mainly due to the large mismatch of thermal expansion coefficients and the lack of affinity between carbon and Cu. Enhancing diamond nucleation by carbon transport from buried nanodiamond through a Pt ultrathin interlayer, adherent diamond film was then deposited on Cu substrate without distinctly metallic interlayer. This novel nucleation mechanism increased diamond nucleation density to 10 11 cm −2 , and developed diamond film with a composite structure of nano-crystalline diamond (NCD) layer and micro-crystalline diamond layer. Diamond film was characterized by the scanning electron microscope (SEM) and Raman spectroscope, respectively. The composition of diamond film/Cu substrate interface was examined by electron probe microanalysis (EPMA). The adhesion of diamond film was evaluated by indentation test. Those results show that a Pt ultrathin interlayer provides stronger chemically bonded interfaces and improve film adhesion.

  20. γ radiation thermoluminescence performance of HFCVD diamond films

    International Nuclear Information System (INIS)

    Gastelum, S.; Cruz-Zaragoza, E.; Melendrez, R.; Chernov, V.; Barboza-Flores, M.

    2006-01-01

    Polycrystalline chemically vapor deposited (CVD) diamond films have been proposed as detectors and dosimeters of ionizing radiation with prospective applications in high-energy photon dosimetry applications. We present a comparison study on the thermoluminescence (TL) properties of two diamond film samples grown by the hot filament CVD method having thickness of 180 and 500 μm and exposed to γ radiation in the 1-300 Gy dose range. The 180 μm thick sample deposited on silicon substrate displayed a TL glow curve peaked at 145 deg. C. The 500 μm, which was a free standing sample, exhibited higher intensity and a well defined first order kinetics TL glow peak around 289 deg. C. Both diamond samples showed a linear dose behavior in the 1-50 Gy range and sublinear behavior for higher doses. The 180 and 500 μm samples presented about 80% and 30% TL losses in a 24 h period, respectively, with both samples showing excellent TL reproducibility. The results indicate that the 500 μm CVD diamond film exhibited a good TL behavior adequate for γ radiation dosimetry

  1. Electrolyte influence on the Cu nanoparticles electrodeposition onto boron doped diamond electrode

    International Nuclear Information System (INIS)

    Matsushima, Jorge Tadao; Santos, Laura Camila Diniz; Couto, Andrea Boldarini; Baldan, Mauricio Ribeiro; Ferreira, Neidenei Gomes

    2012-01-01

    This paper presents the electrolyte influence on deposition and dissolution processes of Cu nanoparticles on boron doped diamond electrodes (DDB). Morphological, structural and electrochemical analysis showed BDD films with good reproducibility, quality and reversible in a specific redox system. Electrodeposition of Cu nanoparticles on DDB electrodes in three different solutions was influenced by pH and ionic strength of the electrolytic medium. Analyzing the process as function of the scan rate, it was verified a better efficiency in 0,5 mol L -1 Na 2 SO 4 solution. Under the influence of the pH and ionic strength, Cu nanoparticles on DDB may be obtained with different morphologies and it was important for defining the desired properties. (author)

  2. Microstructure and mechanical properties of diamond films on titanium-aluminum-vanadium alloy

    Science.gov (United States)

    Catledge, Shane Aaron

    The primary focus of this dissertation is the investigation of the processing-structure-property relationships of diamond films deposited on Ti-6Al-4V alloy by microwave plasma chemical vapor deposition (MPCVD). By depositing a well-adhered protective layer of diamond on an alloy component, its hardness, wear-resistance, performance, and overall lifetime could be significantly increased. However, due to the large thermal expansion mismatch between the diamond film and metal (and the corresponding residual stress induced in the film), film adhesion is typically unsatisfactory and often results in immediate delamination after processing. Therefore, it is a major goal of this research to improve adhesion of the diamond film to the alloy substrate. Through the use of innovative processing techniques involving MPCVD deposition conditions and methane (CH4), nitrogen (N2), and hydrogen (H2) chemistry, we have achieved diamond films which consistently adhere to the alloy substrate. In addition, we have discovered that, with the appropriate choice of deposition conditions, the film structure can be tailored to range from highly crystalline, well-faceted diamond to nanocrystalline diamond with extremely low surface roughness (as low as 27 nm). The relationship between processing and structure was studied using in-situ optical emission spectroscopy, micro-Raman spectroscopy, surface profilometry, glancing-angle x-ray diffraction, and scanning electron microscopy. We observe that when nitrogen is added to the H2/CH4 feedgas mixture, a carbon-nitrogen (CN) emission band arises and its relative abundance to the carbon dimer (C2) gas species is shown to have a pronounced influence on the diamond film structure. By appropriate choice of deposition chemistry and conditions, we can tailor the diamond film structure and its corresponding properties. The mechanical properties of interest in this thesis are those relating to the integrity of the film/substrate interface, as well as the

  3. A Review on the Low-Dimensional and Hybridized Nanostructured Diamond Films

    Directory of Open Access Journals (Sweden)

    Hongdong Li

    2015-01-01

    Full Text Available In the last decade, besides the breakthrough of high-rate growth of chemical vapor deposited single-crystal diamonds, numerous nanostructured diamond films have been rapidly developed in the research fields of the diamond-based sciences and industrial applications. The low-dimensional diamonds of two-dimensional atomic-thick nanofilms and nanostructural diamond on the surface of bulk diamond films have been theoretically and experimentally investigated. In addition, the diamond-related hybrid nanostructures of n-type oxide/p-type diamond and n-type nitride/p-type diamond, having high performance physical and chemical properties, are proposed for further applications. In this review, we first briefly introduce the three categories of diamond nanostructures and then outline the current advances in these topics, including their design, fabrication, characterization, and properties. Finally, we address the remaining challenges in the research field and the future activities.

  4. Doping site dependent thermoelectric properties of epitaxial strontium titanate thin films

    KAUST Repository

    Abutaha, Anas I.; Sarath Kumar, S. R.; Mehdizadeh Dehkordi, Arash; Tritt, Terry M.; Alshareef, Husam N.

    2014-01-01

    We demonstrate that the thermoelectric properties of epitaxial strontium titanate (STO) thin films can be improved by additional B-site doping of A-site doped ABO3 type perovskite STO. The additional B-site doping of A-site doped STO results in increased electrical conductivity, but at the expense of Seebeck coefficient. However, doping on both sites of the STO lattice significantly reduces the lattice thermal conductivity of STO by adding more densely and strategically distributed phononic scattering centers that attack wider phonon spectra. The additional B-site doping limits the trade-off relationship between the electrical conductivity and total thermal conductivity of A-site doped STO, leading to an improvement in the room-temperature thermoelectric figure of merit, ZT. The 5% Pr3+ and 20% Nb5+ double-doped STO film exhibits the best ZT of 0.016 at room temperature. This journal is

  5. Panel 2 - properties of diamond and diamond-like-carbon films

    Energy Technology Data Exchange (ETDEWEB)

    Blau, P.J.; Clausing, R.E. [Oak Ridge National Lab., TN (United States); Ajayi, O.O.; Liu, Y.Y.; Purohit, A. [Argonne National Lab., IL (United States); Bartelt, P.F. [Deere & Co., Moline, IL (United States); Baughman, R.H. [Allied Signal, Morristown, NJ (United States); Bhushan, B. [Ohio State Univ., Columbus (United States); Cooper, C.V. [United Technologies Research Center, East Hartford, CT (United States); Dugger, M.T. [Sandia National Laboratories, Albuquerque, NM (United States); Freedman, A. [Aerodyne Research, Inc., Billerica, MA (United States); Larsen-Basse, J. [National Science Foundation, Washington, DC (United States); McGuire, N.R. [Caterpillar, Peoria, IL (United States); Messier, R.F. [Pennsylvania State Univ., University Park (United States); Noble, G.L.; Ostrowki, M.H. [John Crane, Inc., Morton Grove, IL (United States); Sartwell, B.D. [Naval Research Lab., Washington, DC (United States); Wei, R. [Colorado State Univ., Fort Collins (United States)

    1993-01-01

    This panel attempted to identify and prioritize research and development needs in determining the physical, mechanical and chemical properties of diamond and diamond-like-carbon films (D/DLCF). Three specific goals were established. They were: (1) To identify problem areas which produce concern and require a better knowledge of D/DLCF properties. (2) To identify and prioritize key properties of D/DLCF to promote transportation applications. (3) To identify needs for improvement in properties-measurement methods. Each of these goals is addressed subsequently.

  6. Cell adhesion and growth on ultrananocrystalline diamond and diamond-like carbon films after different surface modifications

    Czech Academy of Sciences Publication Activity Database

    Mikšovský, Jan; Voss, A.; Kozarova, R.; Kocourek, Tomáš; Písařík, Petr; Ceccone, G.; Kulisch, W.; Jelínek, Miroslav; Apostolova, M.D.; Reithmaier, J.P.; Popov, C.

    2014-01-01

    Roč. 297, APR (2014), s. 95-102 ISSN 0169-4332 R&D Projects: GA MŠk LD12069 Institutional support: RVO:68378271 Keywords : ultrananocrystalline diamond films * diamond -like carbon films * surface modification * direct contact cell tests Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 2.711, year: 2014 http://www.sciencedirect.com/science/article/pii/S0169433214001251

  7. Grain boundaries and mechanical properties of nanocrystalline diamond films.

    Energy Technology Data Exchange (ETDEWEB)

    Busmann, H.-G.; Pageler, A.; Gruen, D. M.

    1999-08-06

    Phase-pure nanocrystalline diamond thin films grown from plasmas of a hydrogen-poor carbon argon gas mixture have been analyzed regarding their hardness and elastic moduli by means of a microindentor and a scanning acoustic microscope.The films are superhard and the moduli rival single crystal diamond. In addition, Raman spectroscopy with an excitation wavelength of 1064 nm shows a peak at 1438 l/cm and no peak above 1500 l/cm, and X-ray photoelectron spectroscopy a shake-up loss at 4.2 eV. This gives strong evidence for the existence of solitary double bonds in the films. The hardness and elasticity of the films then are explained by the assumption, that the solitary double bonds interconnect the nanocrystals in the films, leading to an intergrain boundary adhesion of similar strength as the intragrain diamond cohesion. The results are in good agreement with recent simulations of high-energy grain boundaries.

  8. Protein-modified nanocrystalline diamond thin films for biosensor applications.

    Science.gov (United States)

    Härtl, Andreas; Schmich, Evelyn; Garrido, Jose A; Hernando, Jorge; Catharino, Silvia C R; Walter, Stefan; Feulner, Peter; Kromka, Alexander; Steinmüller, Doris; Stutzmann, Martin

    2004-10-01

    Diamond exhibits several special properties, for example good biocompatibility and a large electrochemical potential window, that make it particularly suitable for biofunctionalization and biosensing. Here we show that proteins can be attached covalently to nanocrystalline diamond thin films. Moreover, we show that, although the biomolecules are immobilized at the surface, they are still fully functional and active. Hydrogen-terminated nanocrystalline diamond films were modified by using a photochemical process to generate a surface layer of amino groups, to which proteins were covalently attached. We used green fluorescent protein to reveal the successful coupling directly. After functionalization of nanocrystalline diamond electrodes with the enzyme catalase, a direct electron transfer between the enzyme's redox centre and the diamond electrode was detected. Moreover, the modified electrode was found to be sensitive to hydrogen peroxide. Because of its dual role as a substrate for biofunctionalization and as an electrode, nanocrystalline diamond is a very promising candidate for future biosensor applications.

  9. Boron-doped nanocrystalline diamond electrodes for neural interfaces: in vivo biocompatibility evaluation

    Czech Academy of Sciences Publication Activity Database

    Alcaide, M.; Taylor, Andrew; Fjorback, M.; Zachar, V.; Pennisi, C.P.

    2016-01-01

    Roč. 10, Mar (2016), 1-9, č. článku 87. ISSN 1662-453X Institutional support: RVO:68378271 Keywords : nanocrystalline diamond * neuroprosthetic interfaces * neural electrodes * boron-doped diamond * titanium nitride * foreign body reaction Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 3.566, year: 2016

  10. Effect of Nano-Ni Catalyst on the Growth and Characterization of Diamond Films by HFCVD

    Directory of Open Access Journals (Sweden)

    Chien-Chung Teng

    2010-01-01

    Full Text Available Four different catalysts, nanodiamond seed, nano-Ni, diamond powder, and mixture of nano-Ni/diamond powder, were used to activate Si wafers for diamond film growth by hot-filament CVD (HFCVD. Diamond crystals were shown to grow directly on both large diamond powder and small nanodiamond seed, but a better crystallinity of diamond film was observed on the ultrasonicated nanodiamond seeded Si substrate. On the other hand, nano-Ni nanocatalysts seem to promote the formation of amorphous carbon but suppress transpolyacetylene (t-PA phases at the initial growth of diamond films. The subsequent nucleation and growth of diamond crystals on the amorphous carbon layer leads to generation of the spherical diamond particles and clusters prior to coalescence into continuous diamond films based on the CH3 addition mechanism as characterized by XRD, Raman, ATR/FT-IR, XPS, TEM, SEM, and AFM techniques. Moreover, a 36% reduction in surface roughness of diamond film assisted by nano-Ni catalyst is quite significant.

  11. CVD of alternated microcrystalline (MCD) and nanocrystalline (NCD) diamond films on WC-TIC-CO substrates

    International Nuclear Information System (INIS)

    Campos, Raonei Alves; Contin, Andre; Trava-Airoldi, Vladimir J.; Corat, Evaldo Jose; Barquete, Danilo Maciel

    2010-01-01

    CVD Diamond coating of WC-TiC-Co cutting tools has been an alternative to increase tool lifetime. Experiments have shown that residual stresses produced during films growth on WC-TiC-Co substrates significantly increases with increasing film thickness up to 20 μm and usually leads to film delamination. In this work alternated micro- and nanocrystalline CVD diamond films have been used to relax interface stresses and to increase diamond coatings performance. WC-TiC-Co substrates have been submitted to a boronizing thermal diffusion treatment prior to CVD diamond films growth. After reactive heat treatment samples were submitted to chemical etching in acid and alkaline solution. The diamond films deposition was performed using HFCVD reactor with different gas concentrations for microcrystalline (MCD) and nano-crystalline (NCD) films growth. As a result, we present the improvement of diamond films adherence on WC-TiC-Co, evaluated by indentation and machining tests. Samples were characterized by Scanning Electron Microscopy (SEM) and Energy Dispersive X-ray (EDX) for qualitative analysis of diamond films. X-ray Diffraction (XRD) was used for phases identification after boronizing process. Diamond film compressive residual stresses were analyzed by Raman Scattering Spectroscopy (RSS). (author)

  12. Boron doped nanostructure ZnO films deposited by ultrasonic spray pyrolysis

    Energy Technology Data Exchange (ETDEWEB)

    Karakaya, Seniye, E-mail: seniyek@ogu.edu.tr; Ozbas, Omer

    2015-02-15

    Highlights: • Nanostructure undoped and boron doped ZnO films were deposited by USP technique. • Influences of doping on the surface and optical properties of the ZnO films were investigated. • XRD spectra of the films exhibited a variation in crystalline quality depending on the B content. - Abstract: ZnO is an II–VI compound semiconductor with a wide direct band gap of 3.3 eV at room temperature. Doped with group III elements (B, Al or Ga), it becomes an attractive candidate to replace tin oxide (SnO{sub 2}) or indium tin oxide (ITO) as transparent conducting electrodes in solar cell devices and flat panel display due to competitive electrical and optical properties. In this work, ZnO and boron doped ZnO (ZnO:B) films have been deposited onto glass substrates at 350 ± 5 °C by a cost-efficient ultrasonic spray pyrolysis technique. The optical, structural, morphological and electrical properties of nanostructure undoped and ZnO:B films have been investigated. Electrical resistivity of films has been analyzed by four-probe technique. Optical properties and thicknesses of the films have been examined in the wavelength range 1200–1600 nm by using spectroscopic ellipsometry (SE) measurements. The optical constants (refractive index (n) and extinction coefficient (k)) and the thicknesses of the films have been fitted according to Cauchy model. The optical method has been used to determine the band gap value of the films. Transmission spectra have been taken by UV spectrophotometer. It is found that both ZnO and ZnO:B films have high average optical transmission (≥80%). X-ray diffraction (XRD) patterns indicate that the obtained ZnO has a hexagonal wurtzite type structure. The morphological properties of the films were studied by atomic force microscopy (AFM). The surface morphology of the nanostructure films is found to depend on the concentration of B. As a result, ZnO:B films are promising contender for their potential use as transparent window layer and

  13. Ferromagnetism appears in nitrogen implanted nanocrystalline diamond films

    Energy Technology Data Exchange (ETDEWEB)

    Remes, Zdenek [Institute of Physics ASCR v.v.i., Cukrovarnicka 10, 162 00 Prague 6 (Czech Republic); Sun, Shih-Jye, E-mail: sjs@nuk.edu.tw [Department of Applied Physics, National University of Kaohsiung, Kaohsiung 811, Taiwan (China); Varga, Marian [Department of Applied Physics, National University of Kaohsiung, Kaohsiung 811, Taiwan (China); Chou, Hsiung [Department of Physics, National Sun Yat-Sen University, Kaohsiung 804, Taiwan (China); Hsu, Hua-Shu [Department of Applied Physics, National Pingtung University of Education, Pingtung 900, Taiwan (China); Kromka, Alexander [Department of Applied Physics, National University of Kaohsiung, Kaohsiung 811, Taiwan (China); Horak, Pavel [Nuclear Physics Institute, 250 68 Rez (Czech Republic)

    2015-11-15

    The nanocrystalline diamond films turn to be ferromagnetic after implanting various nitrogen doses on them. Through this research, we confirm that the room-temperature ferromagnetism of the implanted samples is derived from the measurements of magnetic circular dichroism (MCD) and superconducting quantum interference device (SQUID). Samples with larger crystalline grains as well as higher implanted doses present more robust ferromagnetic signals at room temperature. Raman spectra indicate that the small grain-sized samples are much more disordered than the large grain-sized ones. We propose that a slightly large saturated ferromagnetism could be observed at low temperature, because the increased localization effects have a significant impact on more disordered structure. - Highlights: • Nitrogen implanted nanocrystalline diamond films exhibit ferromagnetism at room temperature. • Nitrogen implants made a Raman deviation from the typical nanocrystalline diamond films. • The ferromagnetism induced from the structure distortion is dominant at low temperature.

  14. Biological responses of diamond-like carbon (DLC) films with different structures in biomedical application.

    Science.gov (United States)

    Liao, T T; Zhang, T F; Li, S S; Deng, Q Y; Wu, B J; Zhang, Y Z; Zhou, Y J; Guo, Y B; Leng, Y X; Huang, N

    2016-12-01

    Diamond-like carbon (DLC) films are potential candidates for artificial joint surface modification in biomedical applications, and the influence of the structural features of DLC surfaces on cell functions has attracted attention in recent decades. Here, the biocompatibility of DLC films with different structures was investigated using macrophages, osteoblasts and fibroblasts. The results showed that DLC films with a low ratio of sp(2)/sp(3), which tend to have a structure similar to that of diamond, led to less inflammatory, excellent osteogenic and fibroblastic reactions, with higher cell viability, better morphology, lower release of TNF-α (tumor necrosis factor-α) and IL-6 (interleukin-6), and higher release of IL-10 (interleukin-10). The results also demonstrated that the high-density diamond structure (low ratio of sp(2)/sp(3)) of DLC films is beneficial for cell adhesion and growth because of better protein adsorption without electrostatic repulsion. These findings provide valuable insights into the mechanisms underlying inhibition of an inflammatory response and the promotion of osteoblastogenesis and fibrous propagation, and effectively build a system for evaluating the biocompatibility of DLC films. Copyright © 2016 Elsevier B.V. All rights reserved.

  15. Method for producing fluorinated diamond-like carbon films

    Science.gov (United States)

    Hakovirta, Marko J.; Nastasi, Michael A.; Lee, Deok-Hyung; He, Xiao-Ming

    2003-06-03

    Fluorinated, diamond-like carbon (F-DLC) films are produced by a pulsed, glow-discharge plasma immersion ion processing procedure. The pulsed, glow-discharge plasma was generated at a pressure of 1 Pa from an acetylene (C.sub.2 H.sub.2) and hexafluoroethane (C.sub.2 F.sub.6) gas mixture, and the fluorinated, diamond-like carbon films were deposited on silicon substrates. The film hardness and wear resistance were found to be strongly dependent on the fluorine content incorporated into the coatings. The hardness of the F-DLC films was found to decrease considerably when the fluorine content in the coatings reached about 20%. The contact angle of water on the F-DLC coatings was found to increase with increasing film fluorine content and to saturate at a level characteristic of polytetrafluoroethylene.

  16. Chemical Vapor-Deposited (CVD) Diamond Films for Electronic Applications

    Science.gov (United States)

    1995-01-01

    Diamond films have a variety of useful applications as electron emitters in devices such as magnetrons, electron multipliers, displays, and sensors. Secondary electron emission is the effect in which electrons are emitted from the near surface of a material because of energetic incident electrons. The total secondary yield coefficient, which is the ratio of the number of secondary electrons to the number of incident electrons, generally ranges from 2 to 4 for most materials used in such applications. It was discovered recently at the NASA Lewis Research Center that chemical vapor-deposited (CVD) diamond films have very high secondary electron yields, particularly when they are coated with thin layers of CsI. For CsI-coated diamond films, the total secondary yield coefficient can exceed 60. In addition, diamond films exhibit field emission at fields orders of magnitude lower than for existing state-of-the-art emitters. Present state-of-the-art microfabricated field emitters generally require applied fields above 5x10^7 V/cm. Research on field emission from CVD diamond and high-pressure, high-temperature diamond has shown that field emission can be obtained at fields as low as 2x10^4 V/cm. It has also been shown that thin layers of metals, such as gold, and of alkali halides, such as CsI, can significantly increase field emission and stability. Emitters with nanometer-scale lithography will be able to obtain high-current densities with voltages on the order of only 10 to 15 V.

  17. Study of the diamond and diamond like films formation and technology development for the films precipitation on solid surface for wear resistance increasing of tools, machine and mechanism parts

    International Nuclear Information System (INIS)

    Imanbekov, Z.; Bekmuhambetov, E.

    1996-01-01

    Purpose of the project: The purpose of the project is a development and a creation of an effective technology of the diamond and diamond like films precipitation on materials, including refractory metals, semiconductors and composite on the carbon fibers base. The study method includes the experimental investigation of the base surface structure and properties, preparation of the surface for diamond and diamond like coats growing. The precipitation of above mentioned films will be carried out from the plasma being formed from carbon gas medium at low pressure. The main purposes of the project are: - development of the technology for obtaining the films with specified properties; provision of required rate -of the precipitation; - decreasing of temperature; - manufacturing of the functioning laboratory stand with further developing of a pilot- - commercial plant for diamond and diamond like coating. It is supposed to develop a method of the monocrystal diamond films growing, that are useful for semiconductor devices manufacturing The methods: A thermo-emission and ECR methods will be used for investigation of the diamond and diamond like films formation and growth processes. The plant that will be used for the first method is a two electrode construction. Refractory metals (W,Re) being heated up to 2500 Kelvin degrees, are usually used as an actuating electrode. The second one is a base on which the precipitation is carrying out. Refractory metals, steel, silicon can be used as the base. Actuating medium is a mixture of carbon and inert gases. The second method is based on a principle of a plasma formation with use of 2.45 GHz Shf radiation power. An ECR-plasma is formed in conjunction with magnetic field in the actuating chamber. This method allows to precipitate high quality films at lower pressure. Expected results: The main purpose of the project is to assimilate the high effective technology of the diamond and diamond like films precipitation on different

  18. Influence of electroformation regime on the specific properties of cobalt oxide‒platinum composite films deposited on conductive diamond

    Energy Technology Data Exchange (ETDEWEB)

    Spătaru, Tanţa; Osiceanu, Petre; Preda, Loredana; Munteanu, Cornel [Institute of Physical Chemistry “Ilie Murgulescu”, 202 Spl. Independenţei 060021, Bucharest (Romania); Spătaru, Nicolae, E-mail: nspataru@icf.ro [Institute of Physical Chemistry “Ilie Murgulescu”, 202 Spl. Independenţei 060021, Bucharest (Romania); Fujishima, Akira [Tokyo University of Science, 1-3 Kagurazaka, Shinjuku-ku Tokyo 162-8601 (Japan)

    2014-04-01

    Two straightforward electrochemical methods were used in the present work for depositing cobalt oxide-platinum composite films on boron-doped diamond substrates in order to put into evidence the effect of the electroformation regime on the morphological and electrochemical features of these hybrid systems. The shift from potentiostatic to potentiodynamic deposition enabled not only a significant improvement of the Pt particles dispersion but also a much higher surface concentration of oxygenated species of platinum. For similar Co{sub 3}O{sub 4} and Pt loadings, the specific capacitance of the composite films deposited by cyclic voltammetry was with ca. 8% higher than that of the potentiostatically obtained ones. Additional advantage of potentiodynamic deposition is the improved resistance to fouling during methanol anodic oxidation of Pt particles, tentatively ascribed to the higher surface concentration of oxygenated species of platinum. - Highlights: • Cobalt oxide-platinum composite films were electrodeposited on conductive diamond. • Composite films formed by cyclic voltammetry exhibit enhanced specific capacitance. • Potentiodynamic deposition enables higher concentration of oxygenated Pt species. • Co{sub 3}O{sub 4}–Pt films prepared by cyclic voltammetry are less susceptible to CO poisoning.

  19. Electrochemical Biosensor Based on Boron-Doped Diamond Electrodes with Modified Surfaces

    Directory of Open Access Journals (Sweden)

    Yuan Yu

    2012-01-01

    Full Text Available Boron-doped diamond (BDD thin films, as one kind of electrode materials, are superior to conventional carbon-based materials including carbon paste, porous carbon, glassy carbon (GC, carbon nanotubes in terms of high stability, wide potential window, low background current, and good biocompatibility. Electrochemical biosensor based on BDD electrodes have attracted extensive interests due to the superior properties of BDD electrodes and the merits of biosensors, such as specificity, sensitivity, and fast response. Electrochemical reactions perform at the interface between electrolyte solutions and the electrodes surfaces, so the surface structures and properties of the BDD electrodes are important for electrochemical detection. In this paper, the recent advances of BDD electrodes with different surfaces including nanostructured surface and chemically modified surface, for the construction of various electrochemical biosensors, were described.

  20. Structure and giant magnetoresistance of carbon-based amorphous films prepared by magnetron sputtering

    International Nuclear Information System (INIS)

    Ma, L.; He, M.F.; Liu, Z.W.; Zeng, D.C.; Gu, Z.F.; Cheng, G.

    2014-01-01

    Pure amorphous carbon (a-C) and Co-doped Co x C 1−x films were prepared on n-Si(100) substrates by dc magnetron sputtering. In Co–C films, the nano-sized amorphous Co particles were homogeneously dispersed in the amorphous cross-linked carbon matrix. The structures of a-C and Co x C 1−x films were investigated by X-ray photoelectron spectroscopy and Raman spectroscopy. The results showed that the a-C films were diamond-like carbon (DLC) films. After doping cobalt into DLC film, the sp 3 -hybridized carbon content in DLC composite films almost had no change. The as-deposited Co x C 1−x granular films had larger value of magnetoresistance (MR) than the amorphous carbon film. A very high positive MR, up to 15.5% at magnetic field B = 0.8 T and x = 2.5 at.% was observed in a Co x C 1−x granular film with thickness of 80 nm at room temperature when the external magnetic field was perpendicular to the electric current and the film surface. With increase of the film thickness and Co-doped content, the MR decreased gradually. It remains a challenge to well explain the observed MR effect in the Co x C 1−x granular films. - Highlights: • The amorphous carbon films were diamond-like carbon films. • No carbide appearing, the Co–C composite films form a good metal/insulator system. • A high positive magnetoresistance, up to 15.5% at B = 0.8 T was observed in Co–C films

  1. Homo-epitaxial diamond film growth on ion implanted diamond substrates

    Energy Technology Data Exchange (ETDEWEB)

    Weiser, P S; Prawer, S; Nugent, K W; Bettiol, A A; Kostidis, L I; Jamieson, D N [Melbourne Univ., Parkville, VIC (Australia). School of Physics

    1997-12-31

    The nucleation of CVD diamond is a complicated process, governed by many interrelated parameters. In the present work we attempt to elucidate the effect of strain on the growth of a homo-epitaxial CVD diamond. We have employed laterally confined high dose (MeV) Helium ion implantation to produce surface swelling of the substrate. The strain is enhanced by the lateral confinement of the implanted region to squares of 100 x 100 {mu}m{sup 2}. After ion implantation, micro-Raman spectroscopy was employed to map the surface strain. The substrates were then inserted into a CVD reactor and a CVD diamond film was grown upon them. Since the strained regions were laterally confined, it was then possible to monitor the effect of strain on diamond nucleation. The substrates were also analysed using Rutherford Backscattering Spectroscopy (RBS), Proton induced X-ray Emission (PIXE) and Ion Beam induced Luminescence (IBIL). 7 refs., 5 figs.

  2. Homo-epitaxial diamond film growth on ion implanted diamond substrates

    Energy Technology Data Exchange (ETDEWEB)

    Weiser, P.S.; Prawer, S.; Nugent, K.W.; Bettiol, A.A.; Kostidis, L.I.; Jamieson, D.N. [Melbourne Univ., Parkville, VIC (Australia). School of Physics

    1996-12-31

    The nucleation of CVD diamond is a complicated process, governed by many interrelated parameters. In the present work we attempt to elucidate the effect of strain on the growth of a homo-epitaxial CVD diamond. We have employed laterally confined high dose (MeV) Helium ion implantation to produce surface swelling of the substrate. The strain is enhanced by the lateral confinement of the implanted region to squares of 100 x 100 {mu}m{sup 2}. After ion implantation, micro-Raman spectroscopy was employed to map the surface strain. The substrates were then inserted into a CVD reactor and a CVD diamond film was grown upon them. Since the strained regions were laterally confined, it was then possible to monitor the effect of strain on diamond nucleation. The substrates were also analysed using Rutherford Backscattering Spectroscopy (RBS), Proton induced X-ray Emission (PIXE) and Ion Beam induced Luminescence (IBIL). 7 refs., 5 figs.

  3. Homo-epitaxial diamond film growth on ion implanted diamond substrates

    International Nuclear Information System (INIS)

    Weiser, P.S.; Prawer, S.; Nugent, K.W.; Bettiol, A.A.; Kostidis, L.I.; Jamieson, D.N.

    1996-01-01

    The nucleation of CVD diamond is a complicated process, governed by many interrelated parameters. In the present work we attempt to elucidate the effect of strain on the growth of a homo-epitaxial CVD diamond. We have employed laterally confined high dose (MeV) Helium ion implantation to produce surface swelling of the substrate. The strain is enhanced by the lateral confinement of the implanted region to squares of 100 x 100 μm 2 . After ion implantation, micro-Raman spectroscopy was employed to map the surface strain. The substrates were then inserted into a CVD reactor and a CVD diamond film was grown upon them. Since the strained regions were laterally confined, it was then possible to monitor the effect of strain on diamond nucleation. The substrates were also analysed using Rutherford Backscattering Spectroscopy (RBS), Proton induced X-ray Emission (PIXE) and Ion Beam induced Luminescence (IBIL). 7 refs., 5 figs

  4. Metastable State Diamond Growth and its Applications to Electronic Devices.

    Science.gov (United States)

    Jeng, David Guang-Kai

    Diamond which consists of a dense array of carbon atoms joined by strong covalent bonds and formed into a tetrahedral crystal structure has remarkable mechanical, thermal, optical and electrical properties suitable for many industrial applications. With a proper type of doping, diamond is also an ideal semiconductor for high performance electronic devices. Unfortunately, natural diamond is rare and limited by its size and cost, it is not surprising that people continuously look for a synthetic replacement. It was believed for long time that graphite, another form of carbon, may be converted into diamond under high pressure and temperature. However, the exact condition of conversion was not clear. In 1939, O. I. Leipunsky developed an equilibrium phase diagram between graphite and diamond based on thermodynamic considerations. In the phase diagram, there is a low temperature (below 1000^ circC) and low pressure (below 1 atm) region in which diamond is metastable and graphite is stable, therefore establishes the conditions for the coexistence of the two species. Leipunsky's pioneer work opened the door for diamond synthesis. In 1955, the General Electric company (GE) was able to produce artificial diamond at 55k atm pressure and a temperature of 2000^ circC. Contrary to GE, B. Derjaguin and B. V. Spitzyn in Soviet Union, developed a method of growing diamonds at 1000^circC and at a much lower pressure in 1956. Since then, researchers, particularly in Soviet Union, are continuously looking for methods to grow diamond and diamond film at lower temperatures and pressures with slow but steady progress. It was only in the early 80's that the importance of growing diamond films had attracted the attentions of researchers in the Western world and in Japan. Recent progress in plasma physics and chemical vapor deposition techniques in integrated electronics technology have pushed the diamond growth in its metastable states into a new era. In this research, a microwave plasma

  5. Applications of diamond films and related materials; Proceedings of the 1st International Conference, Auburn, AL, Aug. 17-22, 1991

    Science.gov (United States)

    Tzeng, Yonhua (Editor); Yoshikawa, Manasori (Editor); Murakawa, Masao (Editor); Feldman, Albert (Editor)

    1991-01-01

    The present conference discusses the nucleation and growth of diamond from hydrocarbons, the cutting tool performance of CVD thick-film diamond, the characterization of CVD diamond grinding powder, industrial applications of crystalline diamond-coated tools, standardized SEM tribometry of diamond-coated substrates, residual stress in CVD diamond films, the optical properties of CVD diamond films, polycrystalline diamond films for optical applications, and diamond growth on ferrous metals. Also discussed are ion beam-irradiation smoothing of diamond films, electronic circuits on diamond substrates, diamond-laminated surfaces for evaporative spray cooling, electron devices based on the unique properties of diamond, diamond cold cathodes, thin-film diamond microstructure applications, Schottky diodes from flame-grown diamond, diamond films for thermionic applications, methods of diamond nucleation and selective deposition, high-rate/large-area diamond film production, halogen-assisted diamond growth, the economics of diamond technology, and the optical and mechanical properties of diamondlike films.

  6. Hydrogen content and density in nanocrystalline carbon films of a predominant diamond character

    International Nuclear Information System (INIS)

    Hoffman, A.; Heiman, A.; Akhvlediani, R.; Lakin, E.; Zolotoyabko, E.; Cyterman, C.

    2003-01-01

    Nanocrystalline carbon films possessing a prevailing diamond or graphite character, depending on substrate temperature, can be deposited from a methane hydrogen mixture by the direct current glow discharge plasma chemical vapor deposition method. While at a temperature of ∼880 deg. C, following the formation of a thin precursor graphitic film, diamond nucleation occurs and a nanodiamond film grows, at higher and lower deposition temperatures the films maintain their graphitic character. In this study the hydrogen content, density and nanocrystalline phase composition of films deposited at various temperatures are investigated. We aim to elucidate the role of hydrogen in nanocrystalline films with a predominant diamond character. Secondary ion mass spectroscopy revealed a considerable increase of the hydrogen concentration in the films that accompanies the growth of nanodiamond. It correlates with near edge x-ray adsorption spectroscopy measurements, that showed an appearance of spectroscopic features associated with the diamond structure, and with a substantial increase of the film density detected by x-ray reflectivity. Electron energy loss spectroscopy showed that nanocrystalline diamond films can be deposited from a CH 4 /H 2 mixture with hydrogen concentration in the 80%-95% range. For a deposition temperature of 880 deg. C, the highest diamond character of the films was found for a hydrogen concentration of 91% of H 2 . The deposition temperature plays an important role in diamond formation, strongly influencing the content of adsorbed hydrogen with an optimum at 880 deg. C. It is suggested that diamond nucleation and growth of the nanodiamond phase is driven by densification of the deposited graphitic films which results in high local compressive stresses. Nanodiamond formation is accompanied by an increase of hydrogen concentration in the films. It is suggested that hydrogen retention is critical for stabilization of nanodiamond crystallites. At lower

  7. Resistance to protein adsorption and adhesion of fibroblasts on nanocrystalline diamond films: the role of topography and boron doping

    Czech Academy of Sciences Publication Activity Database

    Alcaide, M.; Papaioannou, S.; Taylor, Andrew; Fekete, Ladislav; Gurevich, L.; Zachar, V.; Pennisi, C.P.

    2016-01-01

    Roč. 27, č. 5 (2016), s. 90-1-12 ISSN 0957-4530 R&D Projects: GA MŠk LO1409 Grant - others:FUNBIO(XE) CZ.2.16/3.1.00/21568 Institutional support: RVO:68378271 Keywords : protein adsorption * fibroblasts adhesion * nanocrystalline diamond * boron doping * topography Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 2.325, year: 2016

  8. Metal ion analysis in contaminated water samples using anodic stripping voltammetry and a nanocrystalline diamond thin-film electrode

    International Nuclear Information System (INIS)

    Sonthalia, Prerna; McGaw, Elizabeth; Show, Yoshiyuki; Swain, Greg M.

    2004-01-01

    Boron-doped nanocrystalline diamond thin-film electrodes were employed for the detection and quantification of Ag (I), Cu (II), Pb (II), Cd (II), and Zn (II) in several contaminated water samples using anodic stripping voltammetric (ASV). Diamond is an alternate electrode that possesses many of the same attributes as Hg and, therefore, appears to be a viable material for this electroanalytical measurement. The nanocrystalline form has been found to perform slightly better than the more conventional microcrystalline form of diamond in this application. Differential pulse voltammetry (DPASV) was used to detect these metal ions in lake water, well water, tap water, wastewater treatment sludge, and soil. The electrochemical results were compared with data from inductively coupled plasma mass spectrometric (ICP-MS) and or atomic absorption spectrometric (AAS) measurements of the same samples. Diamond is shown to function well in this electroanalytical application, providing a wide linear dynamic range, a low limit of quantitation, excellent response precision, and good response accuracy. For the analysis of Pb (II), bare diamond provided a response nearly identical to that obtained with a Hg-coated glassy carbon electrode

  9. Electrochemical treatment of wastewaters containing 4-chlororesorcinol using boron doped diamond anodes

    International Nuclear Information System (INIS)

    Nasr, B.; Abdelatif, G.

    2009-01-01

    The electrochemical oxidation of aqueous wastes polluted with 4-chlororesorcinol has been studied on boron-doped diamond electrodes on acidic medium. The voltammetric results showed that in the potential region where the supporting electrolyte is stable, reactions occur, resulting in the loss of activity due to electrode fouling. Galvanostatic electrolysis study showed that the oxidation of these wastes in single-compartment electrochemical flow cell with boron doped diamond anodes deal to the complete mineralization of the organics but is no indication of electrode fouling. Resorcinol, 1,2,4-trihydroxybenzene, benzoquinone, maleic, fumaric, and oxalic acids have been detected as soluble organics and chlorides (Cl - ) and hypochlorites (ClO - ) as mineral products during the electrolysis of 4-chlororesorcinol. The electrochemical oxidation of 4-chlororesorcinol consists of a sequence of steps: Release of Cl and/or hydroxylation of the aromatic ring; formation of quinonic compounds; oxidative opening of aromatic ring to form carboxylic acids; and oxidation of carboxylic acids to carbon dioxide. Both, direct oxidation at boron doped diamond surface and mediated oxidation by powerful oxidants electrogenerated from electrolyte oxidation at anode surface are involved in these stages. (author)

  10. Defining B-c, B* and B-phi for YBCO Thin Films

    DEFF Research Database (Denmark)

    Paturi, Petriina; Irjala, Matti; Abrahamsen, Asger Bech

    2009-01-01

    of superconducting films. Similarly, the characteristic field, B c, can be obtained from magneto-optical (MO) images from when the flux fronts meet in the middle of the film. The matching field, B phi, at which there is one vortex line per pinning site, is sometimes thought to be the same as B*, but in BaZrO3-doped...... YBa2Cu3O7 films the calculated B phi is much higher than the observed B*. B phi can be determined from angular dependent transport measurements. All of the field values correspond to some special case in the flux pinning in the film and relate to J c. In this work we have determined B c, B* and B phi...

  11. Influence of grain boundaries on elasticity and thermal conductivity of nanocrystalline diamond films

    International Nuclear Information System (INIS)

    Mohr, Markus; Daccache, Layal; Horvat, Sebastian; Brühne, Kai; Jacob, Timo; Fecht, Hans-Jörg

    2017-01-01

    Diamond combines several outstanding material properties such as the highest thermal conductivity and highest elastic moduli of all materials. This makes diamond an interesting candidate for a multitude of applications. Nonetheless, nanocrystalline diamond films, layers and coatings, usually show properties different to those of single crystalline diamond. This is usually attributed to the larger volume fraction of the grain boundaries with atomic structure different from the single crystal. In this work we measured Young's modulus and thermal conductivity of nanocrystalline diamond films with average grain sizes ranging from 6 to 15 nm. The measured thermal conductivities are modeled considering the thermal boundary conductance between grains as well as a grain size effect on the phonon mean free path. We make a comparison between elastic modulus and thermal boundary conductance of the grain boundaries G_k for different nanocrystalline diamond films. We conclude that the grain boundaries thermal boundary conductance G_k is a measure of the cohesive energy of the grain boundaries and therefore also of the elastic modulus of the nanocrystalline diamond films.

  12. Infrared absorption study of hydrogen incorporation in thick nanocrystalline diamond films

    International Nuclear Information System (INIS)

    Tang, C.J.; Neves, A.J.; Carmo, M.C.

    2005-01-01

    We present an infrared (IR) optical absorbance study of hydrogen incorporation in nanocrystalline diamond films. The thick nanocrystalline diamond films were synthesized by microwave plasma-assisted chemical vapor deposition and a high growth rate about 3.0 μm/h was achieved. The morphology, phase quality, and hydrogen incorporation were assessed by means of scanning electron microscopy, Raman spectroscopy, and Fourier-transform infrared spectroscopy (FTIR). Large amount of hydrogen bonded to nanocrystalline diamond is clearly evidenced by the huge CH stretching band in the FTIR spectrum. The mechanism of hydrogen incorporation is discussed in light of the growth mechanism of nanocrystalline diamond. This suggests the potential of nanocrystalline diamond for IR electro-optical device applications

  13. Thermal Transport in Diamond Films for Electronics Thermal Management

    Science.gov (United States)

    2018-03-01

    AFRL-RY-WP-TR-2017-0219 THERMAL TRANSPORT IN DIAMOND FILMS FOR ELECTRONICS THERMAL MANAGEMENT Samuel Graham Georgia Institute of Technology MARCH... ELECTRONICS THERMAL MANAGEMENT 5a. CONTRACT NUMBER FA8650-15-C-7517 5b. GRANT NUMBER 5c. PROGRAM ELEMENT NUMBER 61101E 6. AUTHOR(S) Samuel...seeded sample (NRL 010516, Die A5). The NCD membrane and Al layer thicknesses, tNCD, were measured via transmission electron microscopy (TEM). The

  14. Porous boron doped diamonds as metal-free catalysts for the oxygen reduction reaction in alkaline solution

    Science.gov (United States)

    Suo, Ni; Huang, Hao; Wu, Aimin; Cao, Guozhong; Hou, Xiaoduo; Zhang, Guifeng

    2018-05-01

    Porous boron doped diamonds (BDDs) were obtained on foam nickel substrates with a porosity of 80%, 85%, 90% and 95% respectively by hot filament chemical vapor deposition (HFCVD) technology. Scanning electron microscopy (SEM) reveals that uniform and compact BDDs with a cauliflower-like morphology have covered the overall frame of the foam nickel substrates. Raman spectroscopy shows that the BDDs have a poor crystallinity due to heavily doping boron. X-ray photoelectron spectroscopy (XPS) analysis effectively demonstrates that boron atoms can be successfully incorporated into the crystal lattice of diamonds. Electrochemical measurements indicate that the oxygen reduction potential is unaffected by the specific surface area (SSA), and both the onset potential and the limiting diffusion current density are enhanced with increasing SSA. It is also found that the durability and methanol tolerance of the boron doped diamond catalysts are attenuated as the increasing of SSA. The SSA of the catalyst is directly proportional to the oxygen reduction activity and inversely to the durability and methanol resistance. These results provide a reference to the application of porous boron doped diamonds as potential cathodic catalysts for the oxygen reduction reaction in alkaline solution by adjusting the SSA.

  15. Initial damage processes for diamond film exposure to hydrogen plasma

    International Nuclear Information System (INIS)

    Deslandes, A.; Guenette, M.C.; Samuell, C.M.; Karatchevtseva, I.; Ionescu, M.; Cohen, D.D.; Blackwell, B.; Corr, C.; Riley, D.P.

    2013-01-01

    Graphical abstract: -- Highlights: • Exposing chemical vapour deposited (CVD) diamond films in a recently constructed device, MAGPIE, specially commissioned to simulate fusion plasma conditions. • Non-diamond material is etched from the diamond. • There is no hydrogen retention observed, which suggests diamond is an excellent candidate for plasma facing materials. • Final structure of the surface is dependent on synergistic effects of etching and ion-induced structural change. -- Abstract: Diamond is considered to be a possible alternative to other carbon based materials as a plasma facing material in nuclear fusion devices due to its high thermal conductivity and resistance to chemical erosion. In this work CVD diamond films were exposed to hydrogen plasma in the MAGnetized Plasma Interaction Experiment (MAGPIE): a linear plasma device at the Australian National University which simulates plasma conditions relevant to nuclear fusion. Various negative sample stage biases of magnitude less than 500 V were applied to control the energies of impinging ions. Characterisation results from SEM, Raman spectroscopy and ERDA are presented. No measureable quantity of hydrogen retention was observed, this is either due to no incorporation of hydrogen into the diamond structure or due to initial incorporation as a hydrocarbon followed by subsequent etching back into the plasma. A model is presented for the initial stages of diamond erosion in fusion relevant hydrogen plasma that involves chemical erosion of non-diamond material from the surface by hydrogen radicals and damage to the subsurface region from energetic hydrogen ions. These results show that the initial damage processes in this plasma regime are comparable to previous studies of the fundamental processes as reported for less extreme plasma such as in the development of diamond films

  16. RBS and XRD analysis of silicon doped titanium diboride films

    International Nuclear Information System (INIS)

    Mollica, S.; Sood, D.K.; Ghantasala, M.K.; Kothari, R.

    1999-01-01

    Titanium diboride is a newly developed material suitable for protective coatings. Its high temperature oxidation resistance at temperatures of 700 deg C and beyond is limited due to its poor oxidative behaviour. This paper presents a novel approach to improving the coatings' oxidative characteristics at temperatures of 700 deg C by doping with silicon. Titanium diboride films were deposited onto Si(100) wafer substrates using a DC magnetron sputtering system. Films were deposited in two different compositions, one at pure TiB 2 and the other with 20 % Si doping. These samples were vacuum annealed at 700 deg C at 1x10 -6 Torr to investigate the anaerobic behaviour of the material at elevated temperatures and to ensure that they were crystalline. Samples were then oxidised in air at 700 deg C to investigate their oxidation resistance. Annealing the films at 700 deg C in air results in the oxidation of the film as titanium and boron form TiO 2 and B 2 O 3 . Annealing is seen to produce only minor changes in the films. There is some silicon diffusion from the substrate at elevated temperatures, which is related to the porous nature of the deposited film and the high temperature heat treatments. However, silicon doped films showed relatively less oxidation characteristics after annealing in air compared with the pure TiB 2 samples

  17. Graphene grown out of diamond

    Science.gov (United States)

    Gu, Changzhi; Li, Wuxia; Xu, Jing; Xu, Shicong; Lu, Chao; Xu, Lifang; Li, Junjie; Zhang, Shengbai

    2016-10-01

    Most applications of graphene need a suitable support substrate to present its excellent properties. But transferring graphene onto insulators or growing graphene on foreign substrates could cause properties diminishing. This paper reports the graphene growth directly out of diamond (111) by B doping, guided by first-principles calculations. The spontaneous graphene formation occurred due to the reconstruction of the diamond surface when the B doping density and profile are adequate. The resulting materials are defect free with high phase purity/carrier mobility, controllable layer number, and good uniformity, which can be potentially used directly for device fabrication, e.g., high-performance devices requiring good thermal conductivity.

  18. Enhanced surface transfer doping of diamond by V{sub 2}O{sub 5} with improved thermal stability

    Energy Technology Data Exchange (ETDEWEB)

    Crawford, Kevin G., E-mail: k.crawford.2@research.gla.ac.uk; Moran, David A. J. [School of Engineering, University of Glasgow, Glasgow G12 8LT (United Kingdom); Cao, Liang [High Magnetic Field Laboratory, Chinese Academy of Sciences, 350 Shushanhu Road, Hefei 230031, Anhui (China); Department of Physics, National University of Singapore, 2 Science Drive 3, Singapore, Singapore 117542 (Singapore); Qi, Dongchen, E-mail: d.qi@latrobe.edu.au [Department of Chemistry and Physics, La Trobe Institute for Molecular Science, La Trobe University, Melbourne, Victoria 3086 (Australia); Tallaire, Alexandre [LSPM-CNRS, Université Paris 13, Villetaneuse 93430 (France); Limiti, E.; Verona, C. [Department of Industrial Engineering, “Tor Vergata” University, Rome 00173 (Italy); Wee, Andrew T. S. [Department of Physics, National University of Singapore, 2 Science Drive 3, Singapore, Singapore 117542 (Singapore)

    2016-01-25

    Surface transfer doping of hydrogen-terminated diamond has been achieved utilising V{sub 2}O{sub 5} as a surface electron accepting material. Contact between the oxide and diamond surface promotes the transfer of electrons from the diamond into the V{sub 2}O{sub 5} as revealed by the synchrotron-based high resolution photoemission spectroscopy. Electrical characterization by Hall measurement performed before and after V{sub 2}O{sub 5} deposition shows an increase in hole carrier concentration in the diamond from 3.0 × 10{sup 12} to 1.8 × 10{sup 13 }cm{sup −2} at room temperature. High temperature Hall measurements performed up to 300 °C in atmosphere reveal greatly enhanced thermal stability of the hole channel produced using V{sub 2}O{sub 5} in comparison with an air-induced surface conduction channel. Transfer doping of hydrogen-terminated diamond using high electron affinity oxides such as V{sub 2}O{sub 5} is a promising approach for achieving thermally stable, high performance diamond based devices in comparison with air-induced surface transfer doping.

  19. Surface analytical investigation of diamond coatings and nucleation processes by secondary ion mass spectrometry

    International Nuclear Information System (INIS)

    Steiner, R.

    1993-10-01

    Imaging SIMS for the investigation of substrate surfaces: the influence of the substrate surface on diamond nucleation is a major topic in the investigation of the chemical vapour deposition (CVD) of diamond. It is well known that the nucleation density can be enhanced by scratching the substrate surface with abrasive powders. Diamond can nucleate at scratches or at residues of the polishing material. In the present work the surface of refractory metals (Mo, Nb, Ta, W) polished with silicon carbide and diamond powder is studied by imaging (2- or 3-D) secondary ion mass spectrometry (SIMS). In first experiments the distribution of SiC and/or diamond residues after polishing was determined. The reaction of diamond with the substrate during heating to deposition temperatures was investigated. Investigation of WC/Co hardmetal substrates: it is well known that Co contained in the binder phase of the hard metal inhibits a strong adhesion between the diamond film and the substrate, which is need for an application as cutting tool. Several attempts to improve the adhesion have been reported up to now. In this work a pre-treatment procedure leading to the formation of Co compounds (borides and silicides) which are stable under diamond deposition conditions were investigated. Furthermore, the application of intermediate sputter layers consisting of chromium and titanium were studied. Investigation of P-doped diamond coatings: in the quaternary phase diagram C-P-B-N exist some phases with diamond structure and superhard phases (e.g BP, c-BN). Also a hypothetical superhard phase of the composition C 3 N 4 is predicted. A scientific objective is the synthesis of such phases by chemical vapour deposition. An increase of the phosphorus concentration effects a distinct change in the morphology of the deposited coatings. A major advantage of SIMS is that the concentration profiles can be measured through the whole film, due to the sputter removal of the sample, and the interface

  20. Field electron emission characteristics of chemical vapour deposition diamond films with controlled sp2 phase concentration

    International Nuclear Information System (INIS)

    Lu, X.; Yang, Q.; Xiao, C.; Hirose, A.

    2008-01-01

    Diamond films were synthesized in a microwave plasma-enhanced chemical vapour deposition reactor. The microstructure and surface morphology of deposited films were characterized by Raman spectroscope and scanning electron microscope. The sp 2 phase concentration in diamond films was varied and its effect on the field electron emission (FEE) properties was investigated. Diamond films deposited under higher methane concentration exhibit better FEE property including lower turn-on electric field and larger emission current. The predominating factor modifying the FEE property is presumed to be the increase of sp 2 phase concentration. The influence of bias voltage on the FEE property of diamond films is not monotonic. Postgrowth acid treatment reduces the sp 2 phase content in diamond films without changing diamond grain sizes. The corresponding FEE property was degraded

  1. Stratigraphy of a diamond epitaxial three-dimensional overgrowth using doping superlattices

    Science.gov (United States)

    Lloret, F.; Fiori, A.; Araujo, D.; Eon, D.; Villar, M. P.; Bustarret, E.

    2016-05-01

    The selective doped overgrowth of 3D mesa patterns and trenches has become an essential fabrication step of advanced monolithic diamond-based power devices. The methodology here proposed combines the overgrowth of plasma-etched cylindrical mesa structures with the sequential growth of doping superlattices. The latter involve thin heavily boron doped epilayers separating thicker undoped epilayers in a periodic fashion. Besides the classical shape analysis under the scanning electron microscope relying on the appearance of facets corresponding to the main crystallographic directions and their evolution toward slow growing facets, the doping superlattices were used as markers in oriented cross-sectional lamellas prepared by focused ion beam and observed by transmission electron microscopy. This stratigraphic approach is shown here to be applicable to overgrown structures where faceting was not detectable. Intermediate growth directions were detected at different times of the growth process and the periodicity of the superlattice allowed to calculate the growth rates and parameters, providing an original insight into the planarization mechanism. Different configurations of the growth front were obtained for different sample orientations, illustrating the anisotropy of the 3D growth. Dislocations were also observed along the lateral growth fronts with two types of Burger vector: b 01 1 ¯ = /1 2 [ 01 1 ¯ ] and b 112 = /1 6 [ 112 ] . Moreover, the clustering of these extended defects in specific regions of the overgrowth prompted a proposal of two different dislocation generation mechanisms.

  2. Electrochemical and morphological characterization of gold nanoparticles deposited on boron-doped diamond electrode

    Energy Technology Data Exchange (ETDEWEB)

    Limat, Meriadec; El Roustom, Bahaa [Ecole Polytechnique Federale de Lausanne (EPFL), Institute of Chemical Sciences and Engineering, CH-1015 Lausanne (Switzerland); Jotterand, Henri [Ecole Polytechnique Federale de Lausanne (EPFL), Institute of Physics of the Complex Matter, CH-1015 Lausanne (Switzerland); Foti, Gyoergy [Ecole Polytechnique Federale de Lausanne (EPFL), Institute of Chemical Sciences and Engineering, CH-1015 Lausanne (Switzerland)], E-mail: gyorgy.foti@epfl.ch; Comninellis, Christos [Ecole Polytechnique Federale de Lausanne (EPFL), Institute of Chemical Sciences and Engineering, CH-1015 Lausanne (Switzerland)

    2009-03-30

    A novel two-step method was employed to synthesize gold nanoparticles dispersed on boron-doped diamond (BDD) electrode. It consisted of sputter deposition at ambient temperature of maximum 15 equivalent monolayers of gold, followed by a heat treatment in air at 600 deg. C. Gold nanoparticles with an average diameter between 7 and 30 nm could be prepared by this method on polycrystalline BDD film electrode. The obtained Au/BDD composite electrode appeared stable under conditions of electrochemical characterization performed using ferri-/ferrocyanide and benzoquinone/hydroquinone redox couples in acidic medium. The electrochemical behavior of Au/BDD was compared to that of bulk Au and BDD electrodes. Finally, the Au/BDD composite electrode was regarded as an array of Au microelectrodes dispersed on BDD substrate.

  3. Electrochemical and morphological characterization of gold nanoparticles deposited on boron-doped diamond electrode

    International Nuclear Information System (INIS)

    Limat, Meriadec; El Roustom, Bahaa; Jotterand, Henri; Foti, Gyoergy; Comninellis, Christos

    2009-01-01

    A novel two-step method was employed to synthesize gold nanoparticles dispersed on boron-doped diamond (BDD) electrode. It consisted of sputter deposition at ambient temperature of maximum 15 equivalent monolayers of gold, followed by a heat treatment in air at 600 deg. C. Gold nanoparticles with an average diameter between 7 and 30 nm could be prepared by this method on polycrystalline BDD film electrode. The obtained Au/BDD composite electrode appeared stable under conditions of electrochemical characterization performed using ferri-/ferrocyanide and benzoquinone/hydroquinone redox couples in acidic medium. The electrochemical behavior of Au/BDD was compared to that of bulk Au and BDD electrodes. Finally, the Au/BDD composite electrode was regarded as an array of Au microelectrodes dispersed on BDD substrate

  4. Metallization and superconductivity in a multizone doped semiconductor: boron-doped diamond

    International Nuclear Information System (INIS)

    Loktev, V.M.; Pogorelov, Yu.G.

    2005-01-01

    Within the framework of Anderson's s - d hybride model, metallization of a semiconductor at collectivization of impurity states is discussed. Taking in mind the description of boron-doped diamond CB x , the model is generalized for the case of the multiband initial spectrum and cluster acceptor states, due to the pairs of the nearest neighbor impurities ('impurity dumbbells'). The parameters of the calculated band of collective impurity states are compared to those observed in metallized and superconducting CB x

  5. Application of heat treatment and dispersive strengthening concept in interlayer deposition to enhance diamond film adherence

    Energy Technology Data Exchange (ETDEWEB)

    Lin Chiiruey [Tatung Inst. of Technol., Taipei (Taiwan, Province of China). Dept. of Mech. Eng.; Kuo Chengtzu; Chang Rueyming [Institute of Materials Science and Engineering, National Chiao Tung University, 1001 Ta-Hsueh Road, Hsinchu 30050 (Taiwan, Province of China)

    1997-10-31

    Two different deposition processes were carried out to enhance adherence of diamond films on WC+3-5%Co substrate with Ti-Si as the interlayer. One process can be called two-step diamond deposition process. Another process can be called interlayer heat treatment process. Diamond films were deposited by a microwave plasma chemical vapor deposition system. Ti and Si interlayer are deposited by DC sputter and an E-gun, respectively. Film morphologies, interface structure and film quality were examined by SEM, XRD, Auger electron spectroscopy and Raman spectroscopy. The residual stresses and adhesion strengths of the films were determined by Raman spectroscopy and indentation adhesion testing, respectively. Comparing the regular one-step diamond deposition process with the present two different new processes, the average dP/dX values, which are a measure of the adherence of the film, are 354 kgf/mm, 494 kgf/mm and 787 kgf/mm, respectively. In other words, the interlayer heat treatment process gives the best film adherence on average. For the two-step diamond deposition process, the interlayer thickness and the percent diamond surface coverage of the first diamond deposition step are the main parameters, and there exists an optimum Ti thickness and percent diamond coverage for the best film adherence. The main contribution to better film adherence is not a large difference in residual stress, but is due to the following reasons. The interlayer heat treatment can transform amorphous Si to polycrystalline Si, and may form strong TiC and SiC bonding. The polycrystalline Si and the diamond particles from the first diamond deposition step can be an effective seeds to enhance diamond nucleation. (orig.) 11 refs.

  6. RF characteristic of MESFET on H-terminated DC arc jet CVD diamond film

    International Nuclear Information System (INIS)

    Liu, J.L.; Li, C.M.; Zhu, R.H.; Guo, J.C.; Chen, L.X.; Wei, J.J.; Hei, L.F.; Wang, J.J.; Feng, Z.H.; Guo, H.; Lv, F.X.

    2013-01-01

    Diamond has been considered to be a potential material for high-frequency and high-power electronic devices due to the excellent electrical properties. In this paper, we reported the radio frequency (RF) characteristic of metal-semiconductor field effect transistor (MESFET) on polycrystalline diamond films prepared by direct current (DC) arc jet chemical vapor deposition (CVD). First, 4 in polycrystalline diamond films were deposited by DC arc jet CVD in gas recycling mode with the deposition rate of 14 μm/h. Then the polished diamond films were treated by microwave hydrogen plasma and the 0.2 μm-gate-length MESFET was fabricated by using Au mask photolithography and electron beam (EB) lithography. The surface conductivity of the H-terminated diamond film and DC and RF performances of the MESFET were characterized. The results demonstrate that, the carrier mobility of 24.6 cm 2 /V s and the carrier density of 1.096 × 10 13 cm −2 are obtained on the surface of H-terminated diamond film. The FET shows the maximum transition frequency (f T ) of 5 GHz and the maximum oscillation frequency (f max ) of 6 GHz at V GS = −0.5 V and V DS = −8 V, which indicates that H-terminated DC arc jet CVD polycrystalline diamond is suitable for the development of high frequency devices.

  7. P-type diamond stripper foils for tandem ion accelerators

    International Nuclear Information System (INIS)

    Phelps, A.W.; Koba, R.

    1989-01-01

    The authors are developing a stripper foil composed of a p-type diamond membrane. This diamond stripper foil should have a significantly longer lifetime than any conventional stripper foil material. To be useful for stripper foils, the boron-doped blue diamond films must be thinner than 0.8 μm and pore-free. Two methods are compared for their ability to achieve a high nucleation areal density on a W substrate. Some W substrates were first coated with think layer of boron (≤20 nm) in order to enhance nucleation. Other W substrates were scratched with submicron diamond particles. A schematic diagram of the stripper foil is shown. Stripper foils were created by etching away the central area of W substrates. The diamond membrane was then supported by an annulus of W. Tungsten was selected as a ring-support material because of its high electrical and thermal conductivity, relatively low thermal expansion, and proven suitability as a substrate for diamond CVD. Warping or fracture of the diamond film after substrate etch-back was investigated

  8. Ultra-nanocrystalline diamond nanowires with enhanced electrochemical properties

    International Nuclear Information System (INIS)

    Shalini, Jayakumar; Lin, Yi-Chieh; Chang, Ting-Hsun; Sankaran, Kamatchi Jothiramalingam; Chen, Huang-Chin; Lin, I.-Nan; Lee, Chi-Young; Tai, Nyan-Hwa

    2013-01-01

    The effects of N 2 incorporation in Ar/CH 4 plasma on the electrochemical properties and microstructure of ultra-nanocrystalline diamond (UNCD) films are reported. While the electrical conductivity of the films increased monotonously with increasing N 2 content (up to 25%) in the plasma, the electrochemical behavior was optimized for UNCD films grown in (Ar–10% N 2 )/CH 4 plasma. Transmission electron microscopy showed that the main factor resulting in high conductivity in the films was the formation of needle-like nanodiamond grains and the induction graphite layer encapsulating these grains. The electrochemical process for N 2 -incorporated UNCD films can readily be activated due to the presence of nanographite along the grain boundaries of the films. The formation of needle-like diamond grains was presumably due to the presence of CN species that adhered to the existing nanodiamond clusters, which suppressed radial growth of the nanodiamond crystals, promoting anisotropic growth and the formation of needle-like nanodiamond. The N 2 -incorporated UNCD films outperformed other electrochemical electrode materials, such as boron-doped diamond and glassy carbon, in that the UNCD electrodes could sense dopamine, urea, and ascorbic acid simultaneously in the same mixture with clear resolution

  9. The Immunosuppressive drug – Rapamycin – Electroanalytical Sensing Using Boron- Doped Diamond electrode

    International Nuclear Information System (INIS)

    Stanković, Dalibor M.; Kalcher, Kurt

    2015-01-01

    Graphical abstract: Display Omitted -- Abstract: This paper presents for the first time the study of electrochemical behavior of well known immunosuppressant drug – rapamycin (sirolimus) using boron-doped diamond electrode. Rapamycin provided single and oval-shaped oxidation peak at +1.1 V vs. Ag/AgCl electrode in Britton–Robinson buffer solution at pH 3 confirming highly irreversible behavior of analyte at boron-doped diamond electrode. A differential pulse voltammetry was used for quantification of tested drug under the optimum experimental conditions. The calibration curve was linear over the range from 0.5 to 19.5 μM (R 2 = 0.9976) with detection limit of 0.22 μM. Repeatability of ten successfully measurements of three different concentrations (5, 10 and 15 μM) was 2.5, 1.9 and 1,7 %, respectively. Influence of most common biomolecules presented in urine samples was evaluated. The suggested analytical methodology was successfully applied for determination of rapamycin in four urine samples with excellent recoveries. The developed approach could be beneficial in analysis of rapamycin in biological samples using boron-doped diamond electrode as up-to-date electrochemical sensor and could represent inexpensive analytical alternative to separation methods

  10. Deposition and Tribological Properties of Sulfur-Doped DLC Films Deposited by PBII Method

    Directory of Open Access Journals (Sweden)

    Nutthanun Moolsradoo

    2010-01-01

    Full Text Available Sulfur-doped diamond-like carbon films (S-DLC fabricated from C2H2 and SF6 mixtures were used to study the effects of sulfur content and negative pulse bias voltage on the deposition and tribological properties of films prepared by plasma-based ion implantation (PBII. The structure and relative concentration of the films were analyzed by Raman spectroscopy and Auger electron spectroscopy. Hardness and elastic modulus of films were measured by nanoindentation hardness testing. Tribological characteristics of films were performed using a ball-on-disk friction tester. The results indicate that with the increasing sulfur content, the hardness and elastic modulus decrease. Additionally, by changing the negative pulse bias voltage from 0 kV to −5 kV, the hardness and elastic modulus increase, while the friction coefficient and specific wear rate tends to decrease. Moreover, at a negative pulse bias voltage of −5 kV and flow-rate ratio of 1 : 2, there is considerable improvement in friction coefficient of 0.05 under ambient air is due to the formation of a transfer films on the interface. The decrease in the friction coefficient of films doped with 4.9 at.% sulfur is greater under high vacuum (0.03 than under ambient air (>0.1.

  11. TSC response of irradiated CVD diamond films

    CERN Document Server

    Borchi, E; Bucciolini, M; Guasti, A; Mazzocchi, S; Pirollo, S; Sciortino, S

    1999-01-01

    CVD diamond films have been irradiated with electrons, sup 6 sup 0 Co photons and protons in order to study the dose response to exposure to different particles and energies and to investigate linearity with dose. The Thermally Stimulated Current (TSC) has been studied as a function of the dose delivered to polymethilmetacrilate (PMMA) in the range from 1 to 12 Gy with 20 MeV electrons from a linear accelerator. The TSC spectrum has revealed the presence of two components with peak temperatures of about 470 and 520 K, corresponding to levels lying in the diamond band gap with activation energies of the order of 0.7 - 1 eV. After the subtraction of the exponential background the charge emitted during the heating scan has been evaluated and has been found to depend linearly on the dose. The thermally emitted charge of the CVD diamond films has also been studied using different particles. The samples have been irradiated with the same PMMA dose of about 2 Gy with 6 and 20 MeV electrons from a Linac, sup 6 sup 0 ...

  12. Anomalous behavior of B1g mode in highly transparent anatase nano-crystalline Nb-doped Titanium Dioxide (NTO thin films

    Directory of Open Access Journals (Sweden)

    Subodh K. Gautam

    2015-12-01

    Full Text Available The effect of Niobium doping and size of crystallites on highly transparent nano-crystalline Niobium doped Titanium Dioxide (NTO thin films with stable anatase phase are reported. The Nb doping concentration is varied within the solubility limit in TiO2 lattice. Films were annealed in controlled environment for improving the crystallinity and size of crystallites. Elemental and thickness analysis were carried out using Rutherford backscattering spectrometry and cross sectional field emission scanning electron microscopy. Structural characteristics reveal a substitutional incorporation of Nb+5 in the TiO2 lattice which inhibits the anatase crystallites growth with increasing the doping percentage. The micro-Raman (MR spectra of films with small size crystallites shows stiffening of about 4 cm−1 for the Eg(1 mode and is ascribed to phonon confinement and non-stoichiometry. In contrast, B1g mode exhibits a large anomalous softening of 20 cm−1 with asymmetrical broadening; which was not reported for the case of pure TiO2 crystallites. This anomalous behaviour is explained by contraction of the apical Ti-O bonds at the surface upon substitutional Nb5+ doping induced reduction of Ti4+ ions also known as hetero-coordination effect. The proposed hypotheses is manifested through studying the electronic structure and phonon dynamics by performing the near edge x-ray absorption fine structure (NEXAFS and temperature dependent MR down to liquid nitrogen temperature on pure and 2.5 at.% doped NTO films, respectively.

  13. Laser Cutting of Thick Diamond Films Using Low-Power Laser

    Energy Technology Data Exchange (ETDEWEB)

    Park, Y.J.; Baik, Y.J. [Korea Institute of Science and Technology, Seoul (Korea)

    2000-02-01

    Laser cutting of thick diamond films is studied rising a low-power(10 W) copper vapor laser. Due to the existence of the saturation depth in laser cutting, thick diamond films are not easily cut by low-power lasers. In this study, we have adopted a low thermal- conductivity underlayer of alumina and a heating stage (up to 500 deg. C in air) to prevent the laser energy from consuming-out and, in turn, enhance the cutting efficiency. Aspect ratio increases twice from 3.5 to 7 when the alumina underlayer used. Adopting a heating stage also increases aspect ratio and more than 10 is obtained at higher temperatures than 400 deg. C. These results show that thick diamond films can be cut, with low-power lasers, simply by modifying the thermal property of underlayer. (author). 13 refs., 5 figs.

  14. Electronic and optical properties of diamond/organic semiconductor heterostructures

    Energy Technology Data Exchange (ETDEWEB)

    Gajewski, Wojciech; Garrido, Jose; Niedermeier, Martin; Stutzmann, Martin [Walter Schottky Institute, TU Muenchen, Am Coulombwall 3, 85748 Garching (Germany); Williams, Oliver; Haenen, Ken [Institute for Materials Research, University of Hasselt, Wetenschapspark 1, BE-3590 Diepenbeek (Belgium)

    2007-07-01

    Different diamond substrates (single crystalline: SCD, poly-crystalline: PCD and nano-crystalline: NCD) were used to investigate the electronic and optical properties of the diamond/organic semiconductor heterostructures. Layers of a poly[ethynyl-(2-decyloxy-5methoxy)benzene] - PEB, pentacene and 4-nitro-biphenyl-4-diazonium cations - Ph-Ph-NO{sub 2} were prepared by spin coating, thermal evaporation and grafting, respectively. The measurements of the electronic transport along the organic layer were performed using a Hg probe as well as Hall effect measurements in the temperature range 70-400 K. The I-V characteristics of the B-doped diamond/organic semiconductor heterostructures were measured at room temperature by means of the Hg probe. Undoped IIa and undoped PCD films were used for a study of the optical and optoelectronic properties of prepared heterostructures. The influence of the organic layer homogeneity and layer thickness on the optical properties will be discussed. Furthermore, preliminary data on perpendicular and parallel transport in the heterostructures layer will be reported.

  15. Tl and OSL dosimetry of diamond films CVD pure and unpurified with boron-carbon

    International Nuclear Information System (INIS)

    Melendrez, R.; Pedroza M, M.; Chernov, V.; Ochoa N, J.D.; Bernal, R.; Barboza F, M.; Castaneda, B.; Goncalves, J.A.N.; Sandonato, G.M.; Cruz Z, E.; Preciado F, S.; Cruz V, C.; Brown, F.; Schreck, M.

    2004-01-01

    The diamond is a material that possesses extreme physical properties, such as its hardness to the radiation, its low chemical reactivity besides its equivalence to the human tissue, which qualify him as an ideal material for radiation dosimetry. In this work, it was studied the thermal and optically stimulated response (Tl and OSL) of polycrystalline diamond films grown by the technique of CVD pure and contaminated with Boron-carbon (B/C) with the intention of characterizing their efficiency like a dosemeter for radiation in a range of 0 - 3000 Gy. For the case of the films without impurities, the Tl curve presents four main peaks, two of them in an interval of temperatures of 150-200 C and other two additional around of 250-400 C. The dependence of the response of integrated Tl and that of OSL always maintained a lineal relationship with the exhibition dose up to 100 Gy. The behavior of the films contaminated with B/C (2000 - 20000 ppm) was established through experiments that involved the signal of OSL and their relationship with the Tl response. It was found that this processes are correlated, since the electrons caught in the traps of low temperature (50 - 250 C) of the Tl they are the electrons that recombining with more probability to provide the signal of OSL. According to these results it is possible to propose the diamond films as a good candidate for dosimetry to, using the traditional technique of Tl so much as well as the but recent of OSL. (Author)

  16. Electrochemical mineralization pathway of quinoline by boron-doped diamond anodes.

    Science.gov (United States)

    Wang, Chunrong; Ma, Keke; Wu, Tingting; Ye, Min; Tan, Peng; Yan, Kecheng

    2016-04-01

    Boron-doped diamond anodes were selected for quinoline mineralization, and the resulting intermediates, phenylpropyl aldehyde, phenylpropionic acid, and nonanal were identified and followed during quinoline oxidation by gas chromatography-mass spectrometry and high-performance liquid chromatography. The evolutions of formic acid, acetic acid, oxalic acid, NO2(-), NO3(-), and NH4(+) were quantified. A new reaction pathway for quinoline mineralization by boron-doped diamond anodes has been proposed, where the pyridine ring in quinoline is cleaved by a hydroxyl radical giving phenylpropyl aldehyde and NH4(+). Phenylpropyl aldehyde is quickly oxidized into phenylpropionic acid, and the benzene ring is cleaved giving nonanal. This is further oxidized to formic acid, acetic acid, and oxalic acid. Finally, these organic intermediates are mineralized to CO2 and H2O. NH4(+) is also oxidized to NO2(-) and on to NO3(-). The results will help to gain basic reference for clearing intermediates and their toxicity. Copyright © 2016 Elsevier Ltd. All rights reserved.

  17. Atomic layer deposition of B-doped ZnO using triisopropyl borate as the boron precursor and comparison with Al-doped ZnO

    NARCIS (Netherlands)

    Garcia - Alonso, D.; Potts, S.E.; Helvoirt, van C.A.A.; Verheijen, M.A.; Kessels, W.M.M.

    2015-01-01

    Doped ZnO films are an important class of transparent conductive oxides, with many applications demanding increased growth control and low deposition temperatures. Therefore, the preparation of B-doped ZnO films by atomic layer deposition (ALD) at 150 °C was studied. The B source was triisopropyl

  18. Low-temperature phenomena in highly doped grained diamond

    Czech Academy of Sciences Publication Activity Database

    Mareš, Jiří J.; Hubík, Pavel; Krištofik, Jozef; Nesládek, Miloš

    2009-01-01

    Roč. 9, č. 6 (2009), s. 3689-3694 ISSN 1533-4880 Institutional research plan: CEZ:AV0Z10100521 Keywords : nanocrystalline diamond films * granular structure * superconductivity Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 1.435, year: 2009

  19. Doping and cluster formation in diamond

    KAUST Repository

    Schwingenschlö gl, Udo; Chroneos, Alexander; Grimes, R. W.; Schuster, Cosima

    2011-01-01

    Introducing a cluster formation model, we provide a rational fundamental viewpoint for the difficulty to achieve n-type dopeddiamond. We argue that codoping is the way forward to form appropriately doped shallow regions in diamond and other forms of carbon such as graphene. The electronegativities of the codopants are an important design criterion for the donor atom to efficiently donate its electron. We propose that the nearest neighbour codopants should be of a considerably higher electronegativity compared to the donor atom. Codoping strategies should focus on phosphorous for which there are a number of appropriate codopants.

  20. Doping and cluster formation in diamond

    KAUST Repository

    Schwingenschlögl, Udo

    2011-09-09

    Introducing a cluster formation model, we provide a rational fundamental viewpoint for the difficulty to achieve n-type dopeddiamond. We argue that codoping is the way forward to form appropriately doped shallow regions in diamond and other forms of carbon such as graphene. The electronegativities of the codopants are an important design criterion for the donor atom to efficiently donate its electron. We propose that the nearest neighbour codopants should be of a considerably higher electronegativity compared to the donor atom. Codoping strategies should focus on phosphorous for which there are a number of appropriate codopants.

  1. Grating-assisted coupling to nanophotonic circuits in microcrystalline diamond thin films

    Directory of Open Access Journals (Sweden)

    Patrik Rath

    2013-05-01

    Full Text Available Synthetic diamond films can be prepared on a waferscale by using chemical vapour deposition (CVD on suitable substrates such as silicon or silicon dioxide. While such films find a wealth of applications in thermal management, in X-ray and terahertz window design, and in gyrotron tubes and microwave transmission lines, their use for nanoscale optical components remains largely unexplored. Here we demonstrate that CVD diamond provides a high-quality template for realizing nanophotonic integrated optical circuits. Using efficient grating coupling devices prepared from partially etched diamond thin films, we investigate millimetre-sized optical circuits and achieve single-mode waveguiding at telecoms wavelengths. Our results pave the way towards broadband optical applications for sensing in harsh environments and visible photonic devices.

  2. Electrochemical properties of N-doped hydrogenated amorphous carbon films fabricated by plasma-enhanced chemical vapor deposition methods

    Energy Technology Data Exchange (ETDEWEB)

    Tanaka, Yoriko; Furuta, Masahiro; Kuriyama, Koichi; Kuwabara, Ryosuke; Katsuki, Yukiko [Division of Environmental Science and Engineering, Graduate School of Science and Engineering, Yamaguchi University, 1677-1 Yoshida, Yamaguchi-shi, Yamaguchi 753-8512 (Japan); Kondo, Takeshi [Department of Pure and Applied Chemistry, Faculty of Science and Technology, Tokyo University of Science, 2641 Yamazaki, Noda 278-8510 (Japan); Fujishima, Akira [Kanagawa Advanced Science and Technology (KAST), 3-2-1, Sakato, Takatsu-ku, Kawasaki-shi, Kanagawa 213-0012 (Japan); Honda, Kensuke, E-mail: khonda@yamaguchi-u.ac.j [Division of Environmental Science and Engineering, Graduate School of Science and Engineering, Yamaguchi University, 1677-1 Yoshida, Yamaguchi-shi, Yamaguchi 753-8512 (Japan)

    2011-01-01

    Nitrogen-doped hydrogenated amorphous carbon thin films (a-C:N:H, N-doped DLC) were synthesized with microwave-assisted plasma-enhanced chemical vapor deposition widely used for DLC coating such as the inner surface of PET bottles. The electrochemical properties of N-doped DLC surfaces that can be useful in the application as an electrochemical sensor were investigated. N-doped DLC was easily fabricated using the vapor of nitrogen contained hydrocarbon as carbon and nitrogen source. A N/C ratio of resulting N-doped DLC films was 0.08 and atomic ratio of sp{sup 3}/sp{sup 2}-bonded carbons was 25/75. The electrical resistivity and optical gap were 0.695 {Omega} cm and 0.38 eV, respectively. N-doped DLC thin film was found to be an ideal polarizable electrode material with physical stability and chemical inertness. The film has a wide working potential range over 3 V, low double-layer capacitance, and high resistance to electrochemically induced corrosion in strong acid media, which were the same level as those for boron-doped diamond (BDD). The charge transfer rates for the inorganic redox species, Fe{sup 2+/3+} and Fe(CN){sub 6}{sup 4-/3-} at N-doped DLC were sufficiently high. The redox reaction of Ce{sup 2+/3+} with standard potential higher than H{sub 2}O/O{sub 2} were observed due to the wider potential window. At N-doped DLC, the change of the kinetics of Fe(CN){sub 6}{sup 3-/4-} by surface oxidation is different from that at BDD. The rate of Fe(CN){sub 6}{sup 3-/4-} was not varied before and after oxidative treatment on N-doped DLC includes sp{sup 2} carbons, which indicates high durability of the electrochemical activity against surface oxidation.

  3. Polycrystalline diamond film UV detectors for excimer lasers

    International Nuclear Information System (INIS)

    Ralchenko, V G; Savel'ev, A V; Konov, Vitalii I; Mazzeo, G; Spaziani, F; Conte, G; Polyakov, V I

    2006-01-01

    Photoresistive metal-semiconductor-metal detectors based on polycrystalline diamond films are fabricated for recording cw and pulsed UV radiation. The detectors have a high spectral selectivity (the UV-to-VIS response ratio is ∼10 5 ) and a temporal resolution of the order of 10 9 s. 'Solar-blind' photostable diamond detectors are promising for applications in UV lithography, laser micromachining, medicine, and space research. (letters)

  4. Radiation defects and electron disordering in proton-irradiated diamond films

    International Nuclear Information System (INIS)

    Maschenko, V.E.; Soloviev, G.G.

    1991-01-01

    The absorption spectra are studied in the region of the fundamental absorption band and its longwave boundary for the 0.6 μm thick diamond films deposited onto Al 2 O 3 single crystal underlayers and irradiated by 100 keV and 50 keV protons at fluences of 10 13 -10 16 cm -2 . The E 0 β (6.10-5.9eV) and E 0 α (5.51-5.43eV) maxima and the exponential tails towards lower energies are resolved in the spectra of initial films. The halfwidths of the maxima and a weak temperature dependence of their parameters and of the Urbach tail slope are indicative of disordering of the film structure. The intrinsic maxima near and above the indirect absorption boundary in diamond Γ 25 '-Δ are identified with transitions in the disordered cubic and hexagonal phases of the diamond films. The proton irradiation stimulates the intensity redistribution of the intrinsic maxima, the absorption enhancement, and the change of the Urbach tail slope. The character of radiolysis has been found to depend on the composition of the nonirradiated carbon films and on proton fluence. (author). 8 refs.; 3 figs

  5. Ultrananocrystalline diamond film as an optimal cell interface for biomedical applications.

    Science.gov (United States)

    Bajaj, Piyush; Akin, Demir; Gupta, Amit; Sherman, Debby; Shi, Bing; Auciello, Orlando; Bashir, Rashid

    2007-12-01

    Surfaces of materials that promote cell adhesion, proliferation, and growth are critical for new generation of implantable biomedical devices. These films should be able to coat complex geometrical shapes very conformally, with smooth surfaces to produce hermetic bioinert protective coatings, or to provide surfaces for cell grafting through appropriate functionalization. Upon performing a survey of desirable properties such as chemical inertness, low friction coefficient, high wear resistance, and a high Young's modulus, diamond films emerge as very attractive candidates for coatings for biomedical devices. A promising novel material is ultrananocrystalline diamond (UNCD) in thin film form, since UNCD possesses the desirable properties of diamond and can be deposited as a very smooth, conformal coating using chemical vapor deposition. In this paper, we compared cell adhesion, proliferation, and growth on UNCD films, silicon, and platinum films substrates using different cell lines. Our results showed that UNCD films exhibited superior characteristics including cell number, total cell area, and cell spreading. The results could be attributed to the nanostructured nature or a combination of nanostructure/surface chemistry of UNCD, which provides a high surface energy, hence promoting adhesion between the receptors on the cell surface and the UNCD films.

  6. High energy ion beam induced modifications in diamond and diamond like carbon thin films

    International Nuclear Information System (INIS)

    Dilawar, N.; Sah, S.; Mehta, B.R.; Vankar, V.D.

    1996-01-01

    Diamond and DLC films deposited using hot-filament chemical vapour deposition technique at various parameters were irradiated with 50 MeV Si 4+ ions. The resulting microstructural changes were studied using X-ray diffraction and scanning electron microscopy. All the samples showed the development of β-SiC and hexagonal carbon phases at the expense of the diamond/DLC phase. The ERD analysis was carried out to determine the hydrogen concentration and its distribution in DLC films. The absolute hydrogen concentration in DLC samples is of the order of 10 22 atoms/cm 3 which gets depleted on irradiation. The DLC samples show a clear dependence of hydrogen content on the deposition parameters. (author)

  7. Metal-insulator transition and superconductivity in heavily boron-doped diamond and related materials

    Energy Technology Data Exchange (ETDEWEB)

    Achatz, Philipp

    2009-05-15

    During this PhD project, the metal-insulator transition and superconductivity of highly boron-doped single crystal diamond and related materials have been investigated. The critical boron concentration n{sub c} for the metal-insulator transition was found to be the same as for the normal-superconductor transition. All metallic samples have been found to be superconducting and we were able to link the occurence of superconductivity to the proximity to the metal-insulator transition. For this purpose, a scaling law approach based on low temperature transport was proposed. Furthermore, we tried to study the nature of the superconductivity in highly boron doped single crystal diamond. Raman spectroscopy measurements on the isotopically substituted series suggest that the feature occuring at low wavenumbers ({approx} 500 cm{sup -1}) is the A1g vibrational mode associated with boron dimers. Usual Hall effect measurements yielded a puzzling situation in metallic boron-doped diamond samples, leading to carrier concentrations up to a factor 10 higher than the boron concentration determined by secondary ion mass spectroscopy (SIMS). The low temperature transport follows the one expected for a granular metal or insulator, depending on the interplay of intergranular and intragranular (tunneling) conductance. The metal-insulator transition takes place at a critical conductance g{sub c}. The granularity also influences significantly the superconducting properties by introducing the superconducting gap {delta} in the grain and Josephson coupling J between superconducting grains. A peak in magnetoresistance is observed which can be explained by superconducting fluctuations and the granularity of the system. Additionally we studied the low temperature transport of boron-doped Si samples grown by gas immersion laser doping, some of which yielded a superconducting transition at very low temperatures. Furthermore, preliminary results on the LO-phonon-plasmon coupling are shown for the

  8. Metal-insulator transition and superconductivity in heavily boron-doped diamond and related materials

    International Nuclear Information System (INIS)

    Achatz, Philipp

    2009-01-01

    During this PhD project, the metal-insulator transition and superconductivity of highly boron-doped single crystal diamond and related materials have been investigated. The critical boron concentration n c for the metal-insulator transition was found to be the same as for the normal-superconductor transition. All metallic samples have been found to be superconducting and we were able to link the occurence of superconductivity to the proximity to the metal-insulator transition. For this purpose, a scaling law approach based on low temperature transport was proposed. Furthermore, we tried to study the nature of the superconductivity in highly boron doped single crystal diamond. Raman spectroscopy measurements on the isotopically substituted series suggest that the feature occuring at low wavenumbers (∼ 500 cm -1 ) is the A1g vibrational mode associated with boron dimers. Usual Hall effect measurements yielded a puzzling situation in metallic boron-doped diamond samples, leading to carrier concentrations up to a factor 10 higher than the boron concentration determined by secondary ion mass spectroscopy (SIMS). The low temperature transport follows the one expected for a granular metal or insulator, depending on the interplay of intergranular and intragranular (tunneling) conductance. The metal-insulator transition takes place at a critical conductance g c . The granularity also influences significantly the superconducting properties by introducing the superconducting gap Δ in the grain and Josephson coupling J between superconducting grains. A peak in magnetoresistance is observed which can be explained by superconducting fluctuations and the granularity of the system. Additionally we studied the low temperature transport of boron-doped Si samples grown by gas immersion laser doping, some of which yielded a superconducting transition at very low temperatures. Furthermore, preliminary results on the LO-phonon-plasmon coupling are shown for the first time in aluminum-doped

  9. Diamond films deposited by oxygen-enhanced linear plasma chemistry

    Czech Academy of Sciences Publication Activity Database

    Kromka, Alexander; Babchenko, Oleg; Ižák, Tibor; Varga, Marián; Davydova, Marina; Krátká, Marie; Rezek, Bohuslav

    2013-01-01

    Roč. 5, č. 6 (2013), s. 509-514 ISSN 2164-6627 R&D Projects: GA ČR(CZ) GBP108/12/G108; GA ČR GAP108/12/0996 Institutional support: RVO:68378271 Keywords : diamond films * process gas chemistry * pulsed microwave plasma * surface conductivity of diamond Subject RIV: BM - Solid Matter Physics ; Magnetism

  10. Impacts of doping on epitaxial germanium thin film quality and Si-Ge interdiffusion

    KAUST Repository

    Zhou, Guangnan

    2018-04-03

    Ge-on-Si structures with three different dopants (P, As and B) and those without intentional doping were grown, annealed and characterized by several different material characterization methods. All samples have a smooth surface (roughness < 1.5 nm), and the Ge films are almost entirely relaxed. B doped Ge films have threading dislocations above 1 × 10 cm, while P and As doping can reduce the threading dislocation density to be less than 10 cm without annealing. The interdiffusion of Si and Ge of different films have been investigated experimentally and theoretically. A quantitative model of Si-Ge interdiffusion under extrinsic conditions across the full x range was established including the dislocationmediated diffusion. The Kirkendall effect has been observed. The results are of technical significance for the structure, doping, and process design of Ge-on-Si based devices, especially for photonic applications.

  11. Impacts of doping on epitaxial germanium thin film quality and Si-Ge interdiffusion

    KAUST Repository

    Zhou, Guangnan; Lee, Kwang Hong; Anjum, Dalaver H.; Zhang, Qiang; Zhang, Xixiang; Tan, Chuan Seng; Xia, Guangrui

    2018-01-01

    Ge-on-Si structures with three different dopants (P, As and B) and those without intentional doping were grown, annealed and characterized by several different material characterization methods. All samples have a smooth surface (roughness < 1.5 nm), and the Ge films are almost entirely relaxed. B doped Ge films have threading dislocations above 1 × 10 cm, while P and As doping can reduce the threading dislocation density to be less than 10 cm without annealing. The interdiffusion of Si and Ge of different films have been investigated experimentally and theoretically. A quantitative model of Si-Ge interdiffusion under extrinsic conditions across the full x range was established including the dislocationmediated diffusion. The Kirkendall effect has been observed. The results are of technical significance for the structure, doping, and process design of Ge-on-Si based devices, especially for photonic applications.

  12. Diamond-like carbon films deposited on polycarbonates by plasma-enhanced chemical vapor deposition

    Energy Technology Data Exchange (ETDEWEB)

    Guo, C.T. [Department of Computer and Communication, Diwan College of Management, 72141 Taiwan (China)], E-mail: ctguo@dwu.edu.tw

    2008-04-30

    Diamond-like carbon films were coated on optical polycarbonate using plasma-enhanced chemical vapor deposition. A mixture of SiH{sub 4} and CH{sub 4}/H{sub 2} gases was utilized to reduce the internal compressive stress of the deposited films. The structure of the DLC films was characterized as a function of film thickness using Raman spectroscopy. The dependence of G peak positions and the intensity ratio of I{sub D}/I{sub G} on the DLC film thicknesses was analyzed in detail. Other studies involving atomic force microscopy, ultraviolet visible spectrometry, and three adhesion tests were conducted. Good transparency in the visible region, and good adhesion between diamond-like carbon films and polycarbonate were demonstrated. One-time recordings before and after a DLC film was coated on compact rewritable disc substrates were analyzed as a case study. The results reveal that the diamond-like carbon film overcoating the optical polycarbonates effectively protects the storage media.

  13. Thermoluminescence properties of undoped diamond films deposited using HF CVD technique

    Directory of Open Access Journals (Sweden)

    Paprocki K.

    2018-03-01

    Full Text Available Natural diamond has been considered as a perspective material for clinical radiation dosimetry due to its tissuebiocompatibility and chemical inertness. However, the use of natural diamond in radiation dosimetry has been halted by the high market price. The recent progress in the development of CVD techniques for diamond synthesis, offering the capability of growing high quality diamond layers, has renewed the interest in using this material in radiation dosimeters having small geometricalsizes. Polycrystalline CVD diamond films have been proposed as detectors and dosimeters of β and α radiation with prospective applications in high-energy photon dosimetry. In this work, we present a study on the TL properties of undoped diamond film samples grown by the hot filament CVD (HF CVD method and exposed to β and α radiation. The glow curves for both types of radiation show similar character and can be decomposed into three components. The dominant TL peaks are centered at around 610 K and exhibit activation energy of the order of 0.90 eV.

  14. Planarization of the diamond film surface by using the hydrogen plasma etching with carbon diffusion process

    International Nuclear Information System (INIS)

    Kim, Sung Hoon

    2001-01-01

    Planarization of the free-standing diamond film surface as smooth as possible could be obtained by using the hydrogen plasma etching with the diffusion of the carbon species into the metal alloy (Fe, Cr, Ni). For this process, we placed the free-standing diamond film between the metal alloy and the Mo substrate like a metal-diamond-molybdenum (MDM) sandwich. We set the sandwich-type MDM in a microwave-plasma-enhanced chemical vapor deposition (MPECVD) system. The sandwich-type MDM was heated over ca. 1000 .deg. C by using the hydrogen plasma. We call this process as the hydrogen plasma etching with carbon diffusion process. After etching the free-standing diamond film surface, we investigated surface roughness, morphologies, and the incorporated impurities on the etched diamond film surface. Finally, we suggest that the hydrogen plasma etching with carbon diffusion process is an adequate etching technique for the fabrication of the diamond film surface applicable to electronic devices

  15. Model for the boron-doping dependence of the critical temperature of superconducting boron-doped diamond

    Czech Academy of Sciences Publication Activity Database

    Šopík, Břetislav

    2009-01-01

    Roč. 11, č. 10 (2009), 103026/1-103026/10 ISSN 1367-2630 R&D Projects: GA AV ČR IAA100100712 Grant - others:GAČR(CZ) GA202/07/0597 Institutional research plan: CEZ:AV0Z10100521 Keywords : superconductivity * boron-doped diamond Subject RIV: BE - Theoretical Physics Impact factor: 3.312, year: 2009

  16. Cathodoluminescence characteristics of polycrystalline diamond films grown by cyclic deposition method

    International Nuclear Information System (INIS)

    Seo, Soo-Hyung; Park, Chang-Kyun; Park, Jin-Seok

    2002-01-01

    Polycrystalline diamond films were deposited using a cyclic deposition method where the H 2 plasma for etching (t E ) and the CH 4 +H 2 plasma for growing (t G ) are alternately modulated with various modulation ratios (t E /t G ). From the measurement of full width at half maximum and I D /I G intensity ratio obtained from the Raman spectra, it was found that diamond defects and non-diamond carbon phases were reduced a little by adopting the cyclic deposition method. From the cathodoluminescence (CL) characteristics measured for deposited films, the nitrogen-related band (centered at approximately 590 nm) as well as the so-called band-A (centered at approximately 430 nm) were observed. As the cyclic ratio t E /t G increased, the relative intensity ratio of band-A to nitrogen-related band (I A /I N ) was found to monotonically decrease. In addition, analysis of X-ray diffraction spectra and scanning electron microscope morphologies showed that CL characteristics of deposited diamond films were closely related to their crystal orientations and morphologies

  17. Thin film diamond microstructure applications

    Science.gov (United States)

    Roppel, T.; Ellis, C.; Ramesham, R.; Jaworske, D.; Baginski, M. E.; Lee, S. Y.

    1991-01-01

    Selective deposition and abrasion, as well as etching in atomic oxygen or reduced-pressure air, have been used to prepare patterned polycrystalline diamond films which, on further processing by anisotropic Si etching, yield the microstructures of such devices as flow sensors and accelerometers. Both types of sensor have been experimentally tested in the respective functions of hot-wire anemometer and both single- and double-hinged accelerometer.

  18. Study of the effects of focused high-energy boron ion implantation in diamond

    Science.gov (United States)

    Ynsa, M. D.; Agulló-Rueda, F.; Gordillo, N.; Maira, A.; Moreno-Cerrada, D.; Ramos, M. A.

    2017-08-01

    Boron-doped diamond is a material with a great technological and industrial interest because of its exceptional chemical, physical and structural properties. At modest boron concentrations, insulating diamond becomes a p-type semiconductor and at higher concentrations a superconducting metal at low temperature. The most conventional preparation method used so far, has been the homogeneous incorporation of boron doping during the diamond synthesis carried out either with high-pressure sintering of crystals or by chemical vapour deposition (CVD) of films. With these methods, high boron concentration can be included without distorting significantly the diamond crystalline lattice. However, it is complicated to manufacture boron-doped microstructures. A promising alternative to produce such microstructures could be the implantation of focused high-energy boron ions, although boron fluences are limited by the damage produced in diamond. In this work, the effect of focused high-energy boron ion implantation in single crystals of diamond is studied under different irradiation fluences and conditions. Micro-Raman spectra of the sample were measured before and after annealing at 1000 °C as a function of irradiation fluence, for both superficial and buried boron implantation, to assess the changes in the diamond lattice by the creation of vacancies and defects and their degree of recovery after annealing.

  19. Modification of fluorescence and optical properties of Rhodamine B dye doped PVA/Chitosan polymer blend films

    Science.gov (United States)

    Padmakumari, R.; Ravindrachary, V.; Mahantesha, B. K.; Sagar, Rohan N.; Sahanakumari, R.; Bhajantri, R. F.

    2018-05-01

    Pure and Rhodamine B doped Poly (vinyl alcohol)/Chitosan composite films are prepared using solution casting method. Fourier transforms infrared spectra (FTIR), Ultraviolet-Visible (UV-Vis), fluorescence studies were used to characterize the prepared polymer films. The FT-IR results show that the appearance of new peaks along with shift in peak positions indicates the interaction of Rhodamine B with PVA-CS blend. Optical absorption edge, band gap and activation energy were determined from UV-Visible studies. The optical absorption edge increases, band gap decreases and activation energy increases with dopant concentration respectively. The corresponding emission spectra were studied using fluorescence spectroscopy. From the fluorescence study the quenching phenomena are observed in emission wavelength range of 607nm-613nm upon excitation with absorption maxima 443nm.

  20. Cell adhesion and growth on ultrananocrystalline diamond and diamond-like carbon films after different surface modifications

    Energy Technology Data Exchange (ETDEWEB)

    Miksovsky, J. [Institute of Nanostructure Technologies and Analytics, Center for Interdisciplinary Nanostructure Science and Technology, University of Kassel (Germany); Institute of Physics ASCR, Prague (Czech Republic); Czech Technical University in Prague, Faculty of Biomedical Engineering, Kladno (Czech Republic); Voss, A. [Institute of Nanostructure Technologies and Analytics, Center for Interdisciplinary Nanostructure Science and Technology, University of Kassel (Germany); Kozarova, R. [Institute of Molecular Biology, Bulgarian Academy of Sciences, Sofia (Bulgaria); Kocourek, T.; Pisarik, P. [Institute of Physics ASCR, Prague (Czech Republic); Czech Technical University in Prague, Faculty of Biomedical Engineering, Kladno (Czech Republic); Ceccone, G. [Unit Nanobiosciences, European Commission Joint Research Centre, Ispra (Italy); Kulisch, W. [Institute of Nanostructure Technologies and Analytics, Center for Interdisciplinary Nanostructure Science and Technology, University of Kassel (Germany); Jelinek, M. [Institute of Physics ASCR, Prague (Czech Republic); Czech Technical University in Prague, Faculty of Biomedical Engineering, Kladno (Czech Republic); Apostolova, M.D. [Institute of Molecular Biology, Bulgarian Academy of Sciences, Sofia (Bulgaria); Reithmaier, J.P. [Institute of Nanostructure Technologies and Analytics, Center for Interdisciplinary Nanostructure Science and Technology, University of Kassel (Germany); Popov, C., E-mail: popov@ina.uni-kassel.de [Institute of Nanostructure Technologies and Analytics, Center for Interdisciplinary Nanostructure Science and Technology, University of Kassel (Germany)

    2014-04-01

    Graphical abstract: - Highlights: • UNCD and DLC films were modified by UV/O{sub 3} treatments, O{sub 2} or NH{sub 3}-containing plasmas. • Surface composition, wettability and surface energy change upon modifications. • Higher efficiency of UNCD modifications was observed. • Cell attachment and growth were influenced by the surface termination and roughness. - Abstract: Diamond and diamond-like carbon (DLC) films possess a set of excellent physical and chemical properties which together with a high biocompatibility make them attractive candidates for a number of medical and biotechnological applications. In the current work thin ultrananocrystalline diamond (UNCD) and DLC films were comparatively investigated with respect to cell attachment and proliferation after different surface modifications. The UNCD films were prepared by microwave plasma enhanced chemical vapor deposition, the DLC films by pulsed laser deposition (PLD). The films were comprehensively characterized with respect to their basic properties, e.g. crystallinity, morphology, chemical bonding nature, etc. Afterwards the UNCD and DLC films were modified applying O{sub 2} or NH{sub 3}/N{sub 2} plasmas and UV/O{sub 3} treatments to alter their surface termination. The surface composition of as-grown and modified samples was studied by X-ray photoelectron spectroscopy (XPS). Furthermore the films were characterized by contact angle measurements with water, formamide, 1-decanol and diiodomethane; from the results obtained the surface energy with its dispersive and polar components was calculated. The adhesion and proliferation of MG63 osteosarcoma cells on the different UNCD and DLC samples were assessed by measurement of the cell attachment efficiency and MTT assays. The determined cell densities were compared and correlated with the surface properties of as-deposited and modified UNCD and DLC films.

  1. Raman spectroscopy study of the influence of processing conditions on the structure of polycrystalline diamond films

    International Nuclear Information System (INIS)

    Ramamurti, R.; Shanov, V.; Singh, R.N.; Mamedov, S.; Boolchand, P.

    2006-01-01

    Diamond films are prepared by microwave plasma-enhanced chemical-vapor deposition on Si (100) substrates using the H 2 -Ar-CH 4 gases. Raman scattering data, including the peak position, intensity, area, and width, are analyzed in depth and used to obtain the sp 3 - and sp 2 -bonded carbon contents and the nature of internal stresses in the films. Polarization behavior of the Raman peaks is analyzed to assess its role on the quantitative analysis of the diamond films, which suggested that the 1150 cm -1 Raman peak in nanocrystalline diamond films could be attributed to sp 2 -bonded carbon. The role of the H 2 /Ar content in the gas mixture and substrate temperature on the characteristics of the diamond film is studied. Thickness and grain size of diamond films are also determined by scanning electron microscopy and related to the deposition conditions and Raman results. Deposition conditions, which led to highest sp 3 -bonded carbon content and growth rate, are identified

  2. Controlled surface chemistry of diamond/β-SiC composite films for preferential protein adsorption.

    Science.gov (United States)

    Wang, Tao; Handschuh-Wang, Stephan; Yang, Yang; Zhuang, Hao; Schlemper, Christoph; Wesner, Daniel; Schönherr, Holger; Zhang, Wenjun; Jiang, Xin

    2014-02-04

    Diamond and SiC both process extraordinary biocompatible, electronic, and chemical properties. A combination of diamond and SiC may lead to highly stable materials, e.g., for implants or biosensors with excellent sensing properties. Here we report on the controllable surface chemistry of diamond/β-SiC composite films and its effect on protein adsorption. For systematic and high-throughput investigations, novel diamond/β-SiC composite films with gradient composition have been synthesized using the hot filament chemical vapor deposition (HFCVD) technique. As revealed by scanning electron microscopy (SEM), the diamond/β-SiC ratio of the composite films shows a continuous change from pure diamond to β-SiC over a length of ∼ 10 mm on the surface. X-ray photoelectron spectroscopy (XPS) and time-of-flight secondary ion mass spectrometry (ToF-SIMS) was employed to unveil the surface termination of chemically oxidized and hydrogen treated surfaces. The surface chemistry of the composite films was found to depend on diamond/β-SiC ratio and the surface treatment. As observed by confocal fluorescence microscopy, albumin and fibrinogen were preferentially adsorbed from buffer: after surface oxidation, the proteins preferred to adsorb on diamond rather than on β-SiC, resulting in an increasing amount of proteins adsorbed to the gradient surfaces with increasing diamond/β-SiC ratio. By contrast, for hydrogen-treated surfaces, the proteins preferentially adsorbed on β-SiC, leading to a decreasing amount of albumin adsorbed on the gradient surfaces with increasing diamond/β-SiC ratio. The mechanism of preferential protein adsorption is discussed by considering the hydrogen bonding of the water self-association network to OH-terminated surfaces and the change of the polar surface energy component, which was determined according to the van Oss method. These results suggest that the diamond/β-SiC gradient film can be a promising material for biomedical applications which

  3. SERS activity of Ag decorated nanodiamond and nano-β-SiC, diamond-like-carbon and thermally annealed diamond thin film surfaces.

    Science.gov (United States)

    Kuntumalla, Mohan Kumar; Srikanth, Vadali Venkata Satya Siva; Ravulapalli, Satyavathi; Gangadharini, Upender; Ojha, Harish; Desai, Narayana Rao; Bansal, Chandrahas

    2015-09-07

    In the recent past surface enhanced Raman scattering (SERS) based bio-sensing has gained prominence owing to the simplicity and efficiency of the SERS technique. Dedicated and continuous research efforts have been made to develop SERS substrates that are not only stable, durable and reproducible but also facilitate real-time bio-sensing. In this context diamond, β-SiC and diamond-like-carbon (DLC) and other related thin films have been promoted as excellent candidates for bio-technological applications including real time bio-sensing. In this work, SERS activities of nanodiamond, nano-β-SiC, DLC, thermally annealed diamond thin film surfaces were examined. DLC and thermally annealed diamond thin films were found to show SERS activity without any metal nanostructures on their surfaces. The observed SERS activities of the considered surfaces are explained in terms of the electromagnetic enhancement mechanism and charge transfer resonance process.

  4. The infrared optical properties of heavily B-doped nanocrystalline diamond films on low alkaline glass substrates

    Czech Academy of Sciences Publication Activity Database

    Remeš, Zdeněk; Nesladek, M.

    2006-01-01

    Roč. 203, č. 12 (2006), s. 3016-3020 ISSN 0031-8965 R&D Projects: GA AV ČR KJB100100623 Institutional research plan: CEZ:AV0Z10100521 Keywords : diamond * boron * dielectric function * glass Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 1.221, year: 2006

  5. Transmission photocathodes based on stainless steel mesh and quartz glass coated with N-doped DLC thin films prepared by reactive magnetron sputtering

    Science.gov (United States)

    Balalykin, N. I.; Huran, J.; Nozdrin, M. A.; Feshchenko, A. A.; Kobzev, A. P.; Arbet, J.

    2016-03-01

    The influence was investigated of N-doped diamond-like carbon (DLC) films properties on the quantum efficiency of a prepared transmission photocathode. N-doped DLC thin films were deposited on a silicon substrate, a stainless steel mesh and quartz glass (coated with 5 nm thick Cr adhesion film) by reactive magnetron sputtering using a carbon target and gas mixture Ar, 90%N2+10%H2. The elements' concentration in the films was determined by RBS and ERD. The quantum efficiency was calculated from the measured laser energy and the measured cathode charge. For the study of the vectorial photoelectric effect, the quartz type photocathode was irradiated by intensive laser pulses to form pin-holes in the DLC film. The quantum efficiency (QE), calculated at a laser energy of 0.4 mJ, rose as the nitrogen concentration in the DLC films was increased and rose dramatically after the micron-size perforation in the quartz type photocathodes.

  6. Mechanical design of thin-film diamond crystal mounting apparatus with optimized thermal contact and crystal strain for coherence preservation x-ray optics

    Science.gov (United States)

    Shu, Deming; Shvydko, Yury; Stoupin, Stanislav; Kim, Kwang-Je

    2018-05-08

    A method and mechanical design for a thin-film diamond crystal mounting apparatus for coherence preservation x-ray optics with optimized thermal contact and minimized crystal strain are provided. The novel thin-film diamond crystal mounting apparatus mounts a thin-film diamond crystal supported by a thick chemical vapor deposition (CVD) diamond film spacer with a thickness slightly thicker than the thin-film diamond crystal, and two groups of thin film thermal conductors, such as thin CVD diamond film thermal conductor groups separated by the thick CVD diamond spacer. The two groups of thin CVD film thermal conductors provide thermal conducting interface media with the thin-film diamond crystal. A piezoelectric actuator is integrated into a flexural clamping mechanism generating clamping force from zero to an optimal level.

  7. Use of B{sub 2}O{sub 3} films grown by plasma-assisted atomic layer deposition for shallow boron doping in silicon

    Energy Technology Data Exchange (ETDEWEB)

    Kalkofen, Bodo, E-mail: bodo.kalkofen@ovgu.de; Amusan, Akinwumi A.; Bukhari, Muhammad S. K.; Burte, Edmund P. [Institute of Micro and Sensor Systems, Otto-von-Guericke University, Universitätsplatz 2, 39106 Magdeburg (Germany); Garke, Bernd [Institute for Experimental Physics, Otto-von-Guericke University, Universitätsplatz 2, 39106 Magdeburg (Germany); Lisker, Marco [IHP, Im Technologiepark 25, 15236 Frankfurt (Oder) (Germany); Gargouri, Hassan [SENTECH Instruments GmbH, Schwarzschildstraße 2, 12489 Berlin (Germany)

    2015-05-15

    Plasma-assisted atomic layer deposition (PALD) was carried for growing thin boron oxide films onto silicon aiming at the formation of dopant sources for shallow boron doping of silicon by rapid thermal annealing (RTA). A remote capacitively coupled plasma source powered by GaN microwave oscillators was used for generating oxygen plasma in the PALD process with tris(dimethylamido)borane as boron containing precursor. ALD type growth was obtained; growth per cycle was highest with 0.13 nm at room temperature and decreased with higher temperature. The as-deposited films were highly unstable in ambient air and could be protected by capping with in-situ PALD grown antimony oxide films. After 16 weeks of storage in air, degradation of the film stack was observed in an electron microscope. The instability of the boron oxide, caused by moisture uptake, suggests the application of this film for testing moisture barrier properties of capping materials particularly for those grown by ALD. Boron doping of silicon was demonstrated using the uncapped PALD B{sub 2}O{sub 3} films for RTA processes without exposing them to air. The boron concentration in the silicon could be varied depending on the source layer thickness for very thin films, which favors the application of ALD for semiconductor doping processes.

  8. Growth of carbon fibres, sheets and tubes on diamond films under high power plasma etching conditions

    Energy Technology Data Exchange (ETDEWEB)

    Villalpando, I. [Centro de Investigacion de los Recursos Naturales, Antigua Normal Rural, Salaices, Lopez, Chihuahua (Mexico); John, P.; Wilson, J. I. B., E-mail: isaelav@hotmail.com [School of Engineering and Physical Sciences, Heriot-Watt University, Riccarton, Edinburgh, EH14-4AS (United Kingdom)

    2017-11-01

    The application of diamond as a plasma facing material for fusion reactors can be limited by unknown reactions between diamond and the chamber materials transported by the plasma. Transformation of diamond to other structures can cause problems such as contamination of the plasma with loose particles or retention of gases. We have seen that diamond thin films are eroded under hydrogen plasma etching, but if silicon is present the growth of various carbon structures on diamond films is observed. We have produced carbon with different morphologies on diamond films including fibres, sheets with flower-like shapes and tubes and proposed growth mechanisms based on the results of scanning electron microscopy, X-ray photoelectron spectroscopy and Raman spectroscopy. Sample surfaces contain silicon and are oxidised having COO and CO groups as seen by XP S analysis. Raman analyses revealed a spectrum typical for graphite combined with that from diamond that remains on the surface after hydrogen bombardment. The results of this sturdy show the experimental conditions in which carbon fibres, sheets and tubes are produced under high-power hydrogen etching of diamond films and open the possibility to other applications such as catalysts, sensors and the production of electrodes. (Author)

  9. Growth of carbon fibres, sheets and tubes on diamond films under high power plasma etching conditions

    International Nuclear Information System (INIS)

    Villalpando, I.; John, P.; Wilson, J. I. B.

    2017-01-01

    The application of diamond as a plasma facing material for fusion reactors can be limited by unknown reactions between diamond and the chamber materials transported by the plasma. Transformation of diamond to other structures can cause problems such as contamination of the plasma with loose particles or retention of gases. We have seen that diamond thin films are eroded under hydrogen plasma etching, but if silicon is present the growth of various carbon structures on diamond films is observed. We have produced carbon with different morphologies on diamond films including fibres, sheets with flower-like shapes and tubes and proposed growth mechanisms based on the results of scanning electron microscopy, X-ray photoelectron spectroscopy and Raman spectroscopy. Sample surfaces contain silicon and are oxidised having COO and CO groups as seen by XP S analysis. Raman analyses revealed a spectrum typical for graphite combined with that from diamond that remains on the surface after hydrogen bombardment. The results of this sturdy show the experimental conditions in which carbon fibres, sheets and tubes are produced under high-power hydrogen etching of diamond films and open the possibility to other applications such as catalysts, sensors and the production of electrodes. (Author)

  10. doped ZnO thick film resistors

    Indian Academy of Sciences (India)

    The characterization and ethanol gas sensing properties of pure and doped ZnO thick films were investigated. Thick films of pure zinc oxide were prepared by the screen printing technique. Pure zinc oxide was almost insensitive to ethanol. Thick films of Al2O3 (1 wt%) doped ZnO were observed to be highly sensitive to ...

  11. Characterization of the Diamond-like Carbon Based Functionally Gradient Film

    Institute of Scientific and Technical Information of China (English)

    2002-01-01

    Diamond-like carbon coatings have been used as solid lubricating coatings in vacuum technology for their goodphysical and chemical properties. In this paper, the hybrid technique of unbalanced magnetron sputtering and plasmaimmersion ion implantation (PIll) was adopted to fabricate diamond-like carbon-based functionally gradient film,N/TiN/Ti(N,C)/DLC, on the 304 stainless steel substrate. The film was characterized by using Raman spectroscopyand glancing X-ray diffraction (GXRD), and the topography and surface roughness of the film was observed usingAFM. The mechanical properties of the film were evaluated by nano-indentation. The results showed that the surfaceroughness of the film was approximately 0.732 nm. The hardness and elastic modulus, fracture toughness andinterfacial fracture toughness of N/TiN/Ti(N,C)/DLC functionally gradient film were about 19.84 GPa, 190.03 GPa,3.75 MPa.m1/2 and 5.68 MPa@m1/2, respectively. Compared with that of DLC monolayer and C/TiC/DLC multilayer,this DLC gradient film has better qualities as a solid lubricating coating.

  12. Boron-Doped Diamond Electrodes for the Electrochemical Oxidation and Cleavage of Peptides

    NARCIS (Netherlands)

    Roeser, Julien; Alting, Niels F. A.; Permentier, Hjalmar P.; Bruins, Andries P.; Bischoff, Rainer

    2013-01-01

    Electrochemical oxidation of peptides and proteins is traditionally performed on carbon-based electrodes. Adsorption caused by the affinity of hydrophobic and aromatic amino acids toward these surfaces leads to electrode fouling. We compared the performance of boron-doped diamond (BDD) and glassy

  13. Electrical characteristics of thermal CVD B-doped Si films on highly strained Si epitaxially grown on Ge(100) by plasma CVD without substrate heating

    International Nuclear Information System (INIS)

    Sugawara, Katsutoshi; Sakuraba, Masao; Murota, Junichi

    2010-01-01

    Using an 84% relaxed Ge(100) buffer layer formed on Si(100) by electron cyclotron resonance (ECR) plasma enhanced chemical vapor deposition (CVD), influence of strain upon electrical characteristics of B-doped Si film epitaxially grown on the Ge buffer have been investigated. For the thinner B-doped Si film, surface strain amount is larger than that of the thicker film, for example, strain amount reaches 2.0% for the thickness of 2.2 nm. It is found that the hole mobility is enhanced by the introduction of strain to Si, and the maximum enhancement of about 3 is obtained. This value is higher than that of the usually reported mobility enhancement by strain using Si 1 -x Ge x buffer. Therefore, introduction of strain using relaxed Ge film formed by ECR plasma enhanced CVD is useful to improve future Si-based device performance.

  14. Diamond thin films: giving biomedical applications a new shine.

    Science.gov (United States)

    Nistor, P A; May, P W

    2017-09-01

    Progress made in the last two decades in chemical vapour deposition technology has enabled the production of inexpensive, high-quality coatings made from diamond to become a scientific and commercial reality. Two properties of diamond make it a highly desirable candidate material for biomedical applications: first, it is bioinert, meaning that there is minimal immune response when diamond is implanted into the body, and second, its electrical conductivity can be altered in a controlled manner, from insulating to near-metallic. In vitro, diamond can be used as a substrate upon which a range of biological cells can be cultured. In vivo , diamond thin films have been proposed as coatings for implants and prostheses. Here, we review a large body of data regarding the use of diamond substrates for in vitro cell culture. We also detail more recent work exploring diamond-coated implants with the main targets being bone and neural tissue. We conclude that diamond emerges as one of the major new biomaterials of the twenty-first century that could shape the way medical treatment will be performed, especially when invasive procedures are required. © 2017 The Authors.

  15. Nanostructured diamond film deposition on curved surfaces of metallic temporomandibular joint implant

    Energy Technology Data Exchange (ETDEWEB)

    Fries, Marc D; Vohra, Yogesh K [Department of Physics, University of Alabama at Birmingham (UAB), Birmingham, AL (United States)

    2002-10-21

    Microwave plasma chemical vapour deposition of nanostructured diamond films was carried out on curved surfaces of Ti-6Al-4V alloy machined to simulate the shape of a temporomandibular joint (TMJ) dental implant. Raman spectroscopy shows that the deposited films are uniform in chemical composition along the radius of curvature of the TMJ condyle. Thin film x-ray diffraction reveals an interfacial carbide layer and nanocrystalline diamond grains in this coating. Nanoindentation hardness measurements show an ultra-hard coating with a hardness value of 60{+-}5 GPa averaged over three samples. (rapid communication)

  16. Synthesis of thick diamond films by direct current hot-cathode plasma chemical vapour deposition

    CERN Document Server

    Jin Zeng Sun; Bai Yi Zhen; Lu Xian Yi

    2002-01-01

    The method of direct current hot-cathode plasma chemical vapour deposition has been established. A long-time stable glow discharge at large discharge current and high gas pressure has been achieved by using a hot cathode in the temperature range from 1100 degree C to 1500 degree C and non-symmetrical configuration of the poles, in which the diameter of the cathode is larger than that of anode. High-quality thick diamond films, with a diameter of 40-50 mm and thickness of 0.5-4.2 mm, have been synthesized by this method. Transparent thick diamond films were grown over a range of growth rates between 5-10 mu m/h. Most of the thick diamond films have thermal conductivities of 10-12 W/K centre dot cm. The thick diamond films with high thermal conductivity can be used as a heat sink of semiconducting laser diode array and as a heat spreading and isolation substrate of multichip modules. The performance can be obviously improved

  17. Structural characteristics of single crystalline GaN films grown on (111) diamond with AlN buffer

    DEFF Research Database (Denmark)

    Pécz, Béla; Tóth, Lajos; Barna, Árpád

    2013-01-01

    Hexagonal GaN films with the [0001] direction parallel to the surface normal were grown on (111) oriented single crystalline diamond substrates by plasma-assisted molecular beam epitaxy. Pre-treatments of the diamond surface with the nitrogen plasma beam, prior the nucleation of a thin AlN layer......, eliminated the inversion domains and reduced the density of threading dislocations in the GaN epilayers. The films have an in-plane epitaxial relationship [1010]GaN//[110]diamond. Thus GaN (0001) thin films of single epitaxial relationship and of single polarity were realised on diamond with AlN buffer....

  18. Quantum transport in boron-doped nanocrystalline diamond

    Czech Academy of Sciences Publication Activity Database

    Mareš, Jiří J.; Hubík, Pavel; Krištofik, Jozef; Kindl, Dobroslav; Nesládek, Miloš

    2008-01-01

    Roč. 14, č. 7-8 (2008), s. 161-172 ISSN 0948-1907 R&D Projects: GA ČR GA202/07/0525; GA AV ČR IAA1010404; GA ČR(CZ) GA202/06/0040 Institutional research plan: CEZ:AV0Z10100521 Keywords : nanocrystalline diamond film * ballistic transport * superconductivity * Josephson’s effects Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 1.483, year: 2008

  19. Thermoluminescence characterization of CVD diamond film exposed to UV and beta radiation

    International Nuclear Information System (INIS)

    Barboza-Flores, M.; Melendrez, R.; Gastelum, S.; Chernov, V.; Bernal, R.; Cruz-Vazquez, C.; Brown, F.; Pedroza-Montero, M.; Gan, B.; Ahn, J.; Zhang, Q.; Yoon, S.F.

    2003-01-01

    Thermoluminescence (TL) properties of diamond films grown by microwave and hot filament CVD techniques were studied. The main purpose of the present work was to characterize the thermoluminescence response of diamond films to ultraviolet and beta radiation. The thermoluminescence excitation spectrum exhibits maximum TL efficiency around 210-215 nm. All samples presented a glow curve composed of at least one TL peak and showed regions of linear as well as supralinear behavior as a function or irradiation dose. The linear dose dependence was found for up to sixteen minutes of monochromatic UV irradiation and 300 Gy for beta irradiated samples. The activation energy and the frequency factor were determined and found in the range of 0.33-1.7 eV and 5.44 x 10 2 -5.67 x 10 16 s -1 , respectively. The observed TL performance is reasonable appropriate to justify further investigation of diamond films as radiation dosimeters keeping in mind that diamond is an ideal TL dosemeter since it is tissue-equivalent and biological compatible. (copyright 2003 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim) (orig.)

  20. Electron field emission from undoped and doped DLC films

    International Nuclear Information System (INIS)

    Chakhovskoi, A G; Evtukh, A A; Felter, T E; Klyui, N I; Kudzinovsky, S Y; Litovchenko, V G; Litvin, Y M

    1999-01-01

    Electron field emission and electrical conductivity of undoped and nitrogen doped DLC films have been investigated. The films were grown by the PE CVD method from CH(sub 4):H(sub 2) and CH(sub 4):H(sub 2):N(sub 2) gas mixtures, respectively. By varying nitrogen content in the gas mixture over the range 0 to 45%, corresponding concentrations of 0 to 8% (atomic) could be achieved in the films. Three different gas pressures were used in the deposition chamber: 0.2, 0.6 and 0.8 Torr. Emission current measurements were performed at approximately 10(sup -6) Torr using the diode method with emitter-anode spacing set at 20(micro)m. The current - voltage characteristics of the Si field electron emission arrays covered with DLC films show that threshold voltage (V(sub th)) varies in a complex manner with nitrogen content. As a function of nitrogen content, V(sub th) initially increases rapidly, then decreases and finally increases again for the highest concentration. Corresponding Fowler-Nordheim (F-N) plots follow F-N tunneling over a wide range. The F-N plots were used for determination of the work function, threshold voltage, field enhancement factor and effective emission area. For a qualitative explanation of experimental results, we treat the DLC film as a diamond-like (sp(sup 3) bonded) matrix with graphite-like inclusions

  1. Synthesis of Antimony Doped Amorphous Carbon Films

    Science.gov (United States)

    Okuyama, H.; Takashima, M.; Akasaka, H.; Ohtake, N.

    2013-06-01

    We report the effects of antimony (Sb) doping on the electrical and optical properties of amorphous carbon (a-C:H) films grown on silicon and copper substrates by magnetron sputtering deposition. For film deposition, the mixture targets fabricated from carbon and antimony powders was used. The atomic concentration of carbon, hydrogen, and antimony, in the film deposited from the 1.0 mol% Sb containing target were 81, 17, 2 at.%, respectively. These elements were homogeneously distributed in the film. On the structural effect, the average continuous sp2 carbon bonding networks decreased with Sb concentration increasing, and defects in the films were increased with the Sb incorporation because atomic radius of Sb atoms is twice larger size than that of carbon. The optical gap and the electrical resistivity were carried out before and after the Sb doping. The results show that optical gap dropped from 3.15 to 3.04 eV corresponding to non-doping to Sb-doping conditions, respectively. The electrical resistivity reduced from 10.5 to 1.0 MΩm by the Sb doping. These results suggest the doping level was newly formed in the forbidden band.

  2. Synthesis of Antimony Doped Amorphous Carbon Films

    International Nuclear Information System (INIS)

    Okuyama, H; Takashima, M; Akasaka, H; Ohtake, N

    2013-01-01

    We report the effects of antimony (Sb) doping on the electrical and optical properties of amorphous carbon (a-C:H) films grown on silicon and copper substrates by magnetron sputtering deposition. For film deposition, the mixture targets fabricated from carbon and antimony powders was used. The atomic concentration of carbon, hydrogen, and antimony, in the film deposited from the 1.0 mol% Sb containing target were 81, 17, 2 at.%, respectively. These elements were homogeneously distributed in the film. On the structural effect, the average continuous sp 2 carbon bonding networks decreased with Sb concentration increasing, and defects in the films were increased with the Sb incorporation because atomic radius of Sb atoms is twice larger size than that of carbon. The optical gap and the electrical resistivity were carried out before and after the Sb doping. The results show that optical gap dropped from 3.15 to 3.04 eV corresponding to non-doping to Sb-doping conditions, respectively. The electrical resistivity reduced from 10.5 to 1.0 MΩm by the Sb doping. These results suggest the doping level was newly formed in the forbidden band.

  3. X-ray diffraction characterization of epitaxial CVD diamond films with natural and isotopically modified compositions

    Energy Technology Data Exchange (ETDEWEB)

    Prokhorov, I. A., E-mail: igor.prokhorov@mail.ru [Russian Academy of Sciences, Space Materials Science Laboratory, Shubnikov Institute of Crystallography, Federal Scientific Research Centre “Crystallography and Photonics”, Kaluga Branch (Russian Federation); Voloshin, A. E. [Russian Academy of Sciences, Shubnikov Institute of Crystallography, Federal Scientific Research Centre “Crystallography and Photonics” (Russian Federation); Ralchenko, V. G.; Bolshakov, A. P. [Russian Academy of Sciences, Prokhorov General Physics Institute (Russian Federation); Romanov, D. A. [Bauman Moscow State Technical University, Kaluga Branch (Russian Federation); Khomich, A. A. [Russian Academy of Sciences, Prokhorov General Physics Institute (Russian Federation); Sozontov, E. A. [National Research Centre “Kurchatov Institute” (Russian Federation)

    2016-11-15

    Comparative investigations of homoepitaxial diamond films with natural and modified isotopic compositions, grown by chemical vapor deposition (CVD) on type-Ib diamond substrates, are carried out using double-crystal X-ray diffractometry and topography. The lattice mismatch between the substrate and film is precisely measured. A decrease in the lattice constant on the order of (Δa/a){sub relax} ∼ (1.1–1.2) × 10{sup –4} is recorded in isotopically modified {sup 13}C (99.96%) films. The critical thicknesses of pseudomorphic diamond films is calculated. A significant increase in the dislocation density due to the elastic stress relaxation is revealed by X-ray topography.

  4. Effect of grain boundary on electrical characteristics in B- and P-doped polycrystalline Si1-x-yGe xC y film deposited by ultraclean LPCVD

    International Nuclear Information System (INIS)

    Shim, Hyunyoung; Sakuraba, Masao; Murota, Junichi

    2006-01-01

    The effect of grain boundary on electrical characteristics in B- and P-doped polycrystalline (poly) Si 1-x -y Ge x C y films was investigated. Poly-Si 1-x -y Ge x C y films were deposited on thermally oxidized Si(100) at 500-650 deg. C in a SiH 4 -GeH 4 -SiH 3 CH 3 -H 2 gas mixture by an ultraclean hot-wall low-pressure chemical vapor deposition. B and P were doped into the films by ion implantation and diffusion by heat-treatment. The electrical properties are characterized by grain size, width of disordered region near grain boundaries, carrier trap density and the amount of impurity segregation at grain boundaries. In the B-doped poly-Si 1-x -y Ge x C y films heat-treated at 900 deg. C, the increase of carrier concentration n poly and the decrease of resistivity ρ poly with Ge addition are caused by the narrowing of the width of disordered regions, i.e., crystallization of disordered regions induced by Ge atoms. The decrease of n poly and the increase of ρ poly with C addition are explained by the suppression of crystallization of disordered region due to C atom segregation at grain boundaries. In the P-doped poly-Si 1-x -y Ge x C y films, it is found that n poly and ρ poly are influenced by P atom segregation at grain boundaries due to lowering solid solubility of P in grain by the existence of Ge

  5. Potential barrier heights at metal on oxygen-terminated diamond interfaces

    Energy Technology Data Exchange (ETDEWEB)

    Muret, P., E-mail: pierre.muret@neel.cnrs.fr; Traoré, A.; Maréchal, A.; Eon, D. [Inst. NEEL, Univ. Grenoble Alpes, F-38042 Grenoble, France and CNRS, Inst. NEEL, F-38042 Grenoble (France); Pernot, J. [Univ. Grenoble Alpes, Inst. NEEL, F-38042 Grenoble, (France); CNRS, Inst. NEEL, F-38042 Grenoble, (France); Institut Universitaire de France, 103 Boulevard Saint-Michel, F-75005 Paris (France); Pinero, J. C.; Villar, M. P.; Araujo, D., E-mail: daniel.araujo@uca.es [Dpto. Ciencias de los Materiales, Universidad de Cádiz, 11510 Puerto Real (Cádiz) (Spain)

    2015-11-28

    Electrical properties of metal-semiconductor (M/SC) and metal/oxide/SC structures built with Zr or ZrO{sub 2} deposited on oxygen-terminated surfaces of (001)-oriented diamond films, comprised of a stack of lightly p-doped diamond on a heavily doped layer itself homoepitaxially grown on an Ib substrate, are investigated experimentally and compared to different models. In Schottky barrier diodes, the interfacial oxide layer evidenced by high resolution transmission electron microscopy and electron energy losses spectroscopy before and after annealing, and barrier height inhomogeneities accounts for the measured electrical characteristics until flat bands are reached, in accordance with a model which generalizes that by Tung [Phys. Rev. B 45, 13509 (1992)] and permits to extract physically meaningful parameters of the three kinds of interface: (a) unannealed ones, (b) annealed at 350 °C, (c) annealed at 450 °C with the characteristic barrier heights of 2.2–2.5 V in case (a) while as low as 0.96 V in case (c). Possible models of potential barriers for several metals deposited on well defined oxygen-terminated diamond surfaces are discussed and compared to experimental data. It is concluded that interface dipoles of several kinds present at these compound interfaces and their chemical evolution due to annealing are the suitable ingredients that are able to account for the Mott-Schottky behavior when the effect of the metal work function is ignored, and to justify the reverted slope observed regarding metal work function, in contrast to the trend always reported for all other metal-semiconductor interfaces.

  6. Highly-focused boron implantation in diamond and imaging using the nuclear reaction {sup 11}B(p, α){sup 8}Be

    Energy Technology Data Exchange (ETDEWEB)

    Ynsa, M.D., E-mail: m.ynsa@uam.es [Centro de Micro-Análisis de Materiales, Universidad Autónoma de Madrid, E-28049 Madrid (Spain); Departamento de Física Aplicada, Universidad Autónoma de Madrid, E-28049 Madrid (Spain); Ramos, M.A. [Centro de Micro-Análisis de Materiales, Universidad Autónoma de Madrid, E-28049 Madrid (Spain); Departamento de Física de la Materia Condensada and Instituto Nicolás Cabrera, Universidad Autónoma de Madrid, E-28049 Madrid (Spain); Skukan, N. [Laboratory for Ion Beam Interactions, Ruđer Bošković Institute, Bijenička 54, HR-10000 Zagreb (Croatia); Torres-Costa, V. [Centro de Micro-Análisis de Materiales, Universidad Autónoma de Madrid, E-28049 Madrid (Spain); Departamento de Física Aplicada, Universidad Autónoma de Madrid, E-28049 Madrid (Spain); Jakšić, M. [Laboratory for Ion Beam Interactions, Ruđer Bošković Institute, Bijenička 54, HR-10000 Zagreb (Croatia)

    2015-04-01

    Diamond is an especially attractive material because of its gemological value as well as its unique mechanical, chemical and physical properties. One of these properties is that boron-doped diamond is an electrically p-type semiconducting material at practically any boron concentration. This property makes it possible to use diamonds for multiple industrial and technological applications. Boron can be incorporated into pure diamond by different techniques including ion implantation. Although typical energies used to dope diamond by ion implantation are about 100 keV, implantations have also been performed with energies above MeV. In this work CMAM microbeam setup has been used to demonstrate capability to implant boron with high energies. An 8 MeV boron beam with a size of about 5 × 3 μm{sup 2} and a beam current higher than 500 pA has been employed while controlling the beam position and fluence at all irradiated areas. The subsequent mapping of the implanted boron in diamond has been obtained using the strong and broad nuclear reaction {sup 11}B(p, α){sup 8}Be at E{sub p} = 660 keV. This reaction has a high Q-value (8.59 MeV for α{sub 0} and 5.68 MeV for α{sub 1}) and thus is almost interference-free. The sensitivity of the technique is studied in this work.

  7. Deposition and properties of Al-containing diamond-like carbon films by a hybrid ion beam sources

    International Nuclear Information System (INIS)

    Dai Wei; Wang Aiying

    2011-01-01

    Research highlights: → Weak carbide former, Al element, was incorporated into DLC films using a hybrid ion beams system comprising an anode-layer ion source and a magnetron sputtering unit. → The structure disorder of the films tended to decrease with Al atoms doping, which resulted in the distinct reduction of the film internal stress and hardness, but the internal stress dropped faster than the hardness. → The DLC films with low internal stress and high hardness can be acquired by Al incorporation. - Abstract: Metal incorporation is one of the most effective methods for relaxing internal stress in diamond-like carbon (DLC) films. It was reported that the chemical state of the incorporated metal atoms has a significant influence on the film internal stress. The doped atoms embedding in the DLC matrix without bonding with C atoms can reduce the structure disorder of the DLC films through bond angle distortion and thus relax the internal stress of the films. In present paper, Al atoms, which are inert to carbon, were incorporated into the DLC films deposited by a hybrid ion beams system comprising an anode-layer ion source and a magnetron sputtering unit. The film composition, microstructure and atomic bond structure were characterized using X-ray photoelectron spectroscopy, transmission electron microscopy and Raman spectroscopy. The internal stress, mechanical properties and tribogoical behavior were studied as a function of Al concentration using a stress-tester, nanoindentation and ball-on-disc tribo-tester, respectively. The results indicated that the incorporated Al atoms were dissolved in the DLC matrix without bonding with C atoms and the films exhibited the feature of amorphous carbon. The structure disorder of the films tended to decrease with Al atoms incorporation. This resulted in the distinct reduction of the internal stress in the films. All Al-DLC films exhibited a lower friction coefficient compared with pure DLC film. The formation of the

  8. Effect of TiO2/Al2O3 film coated diamond abrasive particles by sol-gel technique

    Science.gov (United States)

    Hu, Weida; Wan, Long; Liu, Xiaopan; Li, Qiang; Wang, Zhiqi

    2011-04-01

    The diamond abrasive particles were coated with the TiO2/Al2O3 film by the sol-gel technique. Compared with the uncoated diamonds, the TiO2/Al2O3 film was excellent material for the protection of the diamonds. The results showed that the incipient oxidation temperature of the TiO2/Al2O3 film coated diamonds in air atmosphere was 775 °C, which was higher 175 °C than that of the uncoated diamonds. And the coated diamonds also had better the diamond's single particle compressive strength and the impact toughness than that of uncoated diamonds after sintering at 750 °C. For the vitrified bond grinding wheels, replacing the uncoated diamonds with the TiO2/Al2O3 film coated diamonds, the volume expansion of the grinding wheels decreased from 6.2% to 3.4%, the porosity decreased from 35.7% to 25.7%, the hardness increased from 61.2HRC to 66.5HRC and the grinding ratio of the vitrified bond grinding wheels to carbide alloy (YG8) increased from 11.5 to 19.1.

  9. Chemical Analysis of Impurity Boron Atoms in Diamond Using Soft X-ray Emission Spectroscopy

    Energy Technology Data Exchange (ETDEWEB)

    Muramatsu, Yasuji; Iihara, Junji; Takebe, Toshihiko; Denlinger, Jonathan D.

    2008-03-29

    To analyze the local structure and/or chemical states of boron atoms in boron-doped diamond, which can be synthesized by the microwave plasma-assisted chemical vapor deposition method (CVD-B-diamond) and the temperature gradient method at high pressure and high temperature (HPT-B-diamond), we measured the soft X-ray emission spectra in the CK and BK regions of B-diamonds using synchrotron radiation at the Advanced Light Source (ALS). X-ray spectral analyses using the fingerprint method and molecular orbital calculations confirm that boron atoms in CVD-B-diamond substitute for carbon atoms in the diamond lattice to form covalent B-C bonds, while boron atoms in HPT-B-diamond react with the impurity nitrogen atoms to form hexagonal boron nitride. This suggests that the high purity diamond without nitrogen impurities is necessary to synthesize p-type B-diamond semiconductors.

  10. Biomineralized diamond-like carbon films with incorporated titanium dioxide nanoparticles improved bioactivity properties and reduced biofilm formation.

    Science.gov (United States)

    Lopes, F S; Oliveira, J R; Milani, J; Oliveira, L D; Machado, J P B; Trava-Airoldi, V J; Lobo, A O; Marciano, F R

    2017-12-01

    Recently, the development of coatings to protect biomedical alloys from oxidation, passivation and to reduce the ability for a bacterial biofilm to form after implantation has emerged. Diamond-like carbon films are commonly used for implanted medical due to their physical and chemical characteristics, showing good interactions with the biological environment. However, these properties can be significantly improved when titanium dioxide nanoparticles are included, especially to enhance the bactericidal properties of the films. So far, the deposition of hydroxyapatite on the film surface has been studied in order to improve biocompatibility and bioactive behavior. Herein, we developed a new route to obtain a homogeneous and crystalline apatite coating on diamond-like carbon films grown on 304 biomedical stainless steel and evaluated its antibacterial effect. For this purpose, films containing two different concentrations of titanium dioxide (0.1 and 0.3g/L) were obtained by chemical vapor deposition. To obtain the apatite layer, the samples were soaked in simulated body fluid solution for up to 21days. The antibacterial activity of the films was evaluated by bacterial eradication tests using Staphylococcus aureus biofilm. Scanning electron microscopy, X-ray diffraction, Raman scattering spectroscopy, and goniometry showed that homogeneous, crystalline, and hydrophilic apatite films were formed independently of the titanium dioxide concentration. Interestingly, the diamond-like films containing titanium dioxide and hydroxyapatite reduced the biofilm formation compared to controls. A synergism between hydroxyapatite and titanium dioxide that provided an antimicrobial effect against opportunistic pathogens was clearly observed. Copyright © 2017 Elsevier B.V. All rights reserved.

  11. Ion beam deposition of DLC and nitrogen doped DLC thin films for enhanced haemocompatibility on PTFE

    International Nuclear Information System (INIS)

    Srinivasan, S.; Tang, Y.; Li, Y.S.; Yang, Q.; Hirose, A.

    2012-01-01

    Diamond-like carbon (DLC) and N-doped DLC (DLC:N) thin films have been synthesized on polytetrafluroethylene (PTFE) and silicon wafers using ion beam deposition. Raman spectroscopy, atomic force microscopy, X-ray photoelectron spectroscopy and scanning electron microscopy were used to study the structural and morphological properties of the coated surface. The results show that the ion beam deposited DLC thin films exhibit high hardness and Young's modulus, low coefficient of friction and high adhesion to the substrate. Low concentration of nitrogen doping in DLC improves the mechanical properties and reduces the surface roughness. DLC coating decreases the surface energy and improves the wettability of PTFE. The platelet adhesion results show that the haemocompatibility of DLC coated PTFE, especially DLC:N coated PTFE, has been significantly enhanced as compared with uncoated PTFE. SEM observations show that the platelet reaction on the DLC and DLC:N coated PTFE was minimized as the platelets were much less aggregated and activated.

  12. Temperature dependence of stress in CVD diamond films studied by Raman spectroscopy

    Directory of Open Access Journals (Sweden)

    Dychalska Anna

    2015-09-01

    Full Text Available Evolution of residual stress and its components with increasing temperature in chemical vapor deposited (CVD diamond films has a crucial impact on their high temperature applications. In this work we investigated temperature dependence of stress in CVD diamond film deposited on Si(100 substrate in the temperature range of 30 °C to 480 °C by Raman mapping measurement. Raman shift of the characteristic diamond band peaked at 1332 cm-1 was studied to evaluate the residual stress distribution at the diamond surface. A new approach was applied to calculate thermal stress evolution with increasing tempera­ture by using two commonly known equations. Comparison of the residts obtained from the two methods was presented. The intrinsic stress component was calculated from the difference between average values of residual and thermal stress and then its temperature dependence was discussed.

  13. Effect of pulse biasing on the morphology of diamond films grown by hot filament CVD

    International Nuclear Information System (INIS)

    Beake, B.D.; Hussain, I.U.; Rego, C.; Ahmed, W.

    1999-01-01

    There has been considerable interest in the chemical vapour deposition (CVD) of diamond due to its unique mechanical, optical and electronic properties, which make it useful for many applications. For use in optical and electronic applications further developments in the CVD process are required to control the surface morphology and crystal size of the diamond films. These will require a detailed understanding of both the nucleation and growth processes that effect the properties. The technique of bias enhanced nucleation (BEN) of diamond offers better reproducibility than conventional pre-treatment methods such as mechanical abrasion. Atomic force microscopy (AFM) and scanning electron microscopy (SEM) have been used study the surface modification of diamond films on silicon substrates during pulse biased growth in a hot filament CVD reactor. Pre-abraded silicon substrates were subjected to a three-step sequential growth process: (i) diamond deposition under standard CVD conditions, (ii) bias pre-treatment and (iii) deposition under standard conditions. The results show that the bias pre-treatment time is a critical parameter controlling the surface morphology and roughness of the diamond films deposited. Biasing reduces the surface roughness from 152 nm for standard CVD diamond to 68 nm for the 2.5 minutes pulse biased film. Further increase in the bias time results in an increase in surface roughness and crystallite size. (author)

  14. Nucleation and adhesion of diamond films on Co cemented tungsten carbide

    Energy Technology Data Exchange (ETDEWEB)

    Polini, R.; Santarelli, M.; Traversa, E.

    1999-12-01

    Diamond deposits were grown using hot filament chemical vapor deposition (CVD) on pretreated Co cemented tungsten carbide (WC-Co) substrates with an average grain size of 6 {micro}m. Depositions were performed with 0.5 or 1.0% methane concentration and with substrate temperatures ranging from 750 to 1,000 C. Diamond nucleation densities were measured by scanning electron microscopy. Scratched and bias-enhanced nucleation pretreated substrates showed the larger nucleation densities. Etching of the WC performed by Murakami's reagent, followed by surface-Co dissolution (MP pretreatment), led to a roughened but scarcely nucleating surface. The performance of a scratching prior to the MP pretreatment allowed one to increase the nucleation density, due scratching-induced defects, confined in the outermost layer of WC grains, which act as nucleation sites. Smaller nucleation densities were observed with increasing the substrate temperature and reducing the methane concentration, confirming that diamond nucleates via a heterogeneous process. The adhesion of continuous films was evaluated by the reciprocal of the slope of crack radius-indentation load functions. The substrate pretreatments mainly affected the film adhesion, while the influence of CVD process conditions was minor. The two main factors that improve the diamond film adhesion are the coating-substrate contact area and the surface-Co removal.

  15. Growth, characterization and device development in monocrystalline diamond films

    Science.gov (United States)

    Davis, R. F.; Glass, J. T.; Nemanich, R. J.; Bozeman, S. P.; Sowers, A. T.

    1995-06-01

    Experimental and theoretical studies concerned with interface interactions of diamond with Si, Ni, and Ni3Si substrates have been conducted. Oriented diamond films deposited on (100) Si were characterized by polar Raman, polar x-ray diffraction (XRD), and cross-sectional high resolution transmission electron microscopy (HRTEM). These sutides showed that the diamond(100)/Si(100) interface adopted the 3:2-match arrangement rather than a 45 deg rotation. Extended Hueckel tight-binding (EHTB) electronic structure calculations for a model system revealed that the interface interaction favors the 3:2-match arrangement. Growth on polycrystalline Ni3Si resulted in oriented diamond particles; under the same growth conditions, graphite was formed on the nickel substrate. Our EHTB electronic structure calculations showed that the (111) and (100) surfaces of Ni3Si have a strong preference for diamond nucleation over graphite nucleation, but this was not the case for the (111) and (100) surfaces of Ni.

  16. Study on tribological behavior and cutting performance of CVD diamond and DLC films on Co-cemented tungsten carbide substrates

    International Nuclear Information System (INIS)

    Zhang Dongcan; Shen Bin; Sun Fanghong

    2010-01-01

    The tribological behaviors of diamond and diamond-like carbon (DLC) films play a major role on their machining and mechanical applications. In this study, diamond and diamond-like carbon (DLC) films are deposited on the cobalt cemented tungsten carbide (WC-Co) substrate respectively adopting the hot filament chemical vapor deposition (HFCVD) technique and the vacuum arc discharge with a graphite cathode, and their friction properties are evaluated on a reciprocating ball-on-plate tribometer with counterfaces of silicon nitride (Si 3 N 4 ) ceramic, cemented tungsten carbide (WC) and ball-bearing steel materials, under the ambient air without lubricating condition. Moreover, to evaluate their cutting performance, comparative turning tests are conducted using the uncoated WC-Co and as-fabricated CVD diamond and DLC coated inserts, with glass fiber reinforced plastics (GFRP) composite materials as the workpiece. The as-deposited HFCVD diamond and DLC films are characterized with energy-dispersive X-ray spectroscopy (EDX), scanning electron microscope (SEM), X-ray diffraction spectroscopy (XRD), Raman spectroscopy and 3D surface topography based on white-light interferometry. Furthermore, Rocwell C indentation tests are conducted to evaluate the adhesion of HFCVD diamond and DLC films grown onto WC-Co substrates. SEM and 3D surface topography based on white-light interferometry are also used to investigate the worn region on the surfaces of diamond and DLC films. The friction tests suggest that the obtained friction coefficient curves that of various contacts exhibit similar evolution tendency. For a given counterface, DLC films present lower stable friction coefficients than HFCVD diamond films under the same sliding conditions. The cutting tests results indicate that flank wear of the HFCVD diamond coated insert is lower than that of DLC coated insert before diamond films peeling off.

  17. Origin, state of the art and some prospects of the diamond CVD

    CERN Document Server

    Spitsyn, B V; Alexenko, A E

    2000-01-01

    A short review on the diamond CVD origin, together with its state of the art and some prospects was given. New hybrid methods of the diamond CVD permit to gain 1.2 to 6 times of growth rate in comparison with ordinary diamond CVD's. Recent results on n-type diamond film synthesis through phosphorus doping in the course of the CVD process are briefly discussed. In comparison with high-pressure diamond synthesis, the CVD processes open new facets of the diamond as ultimate crystal for science and technology evolution. It was stressed that, mainly on the basis of new CVDs of diamond, the properties of natural diamond are not only reproduced, but can be surpassed. As examples, mechanical (fracture resistance), physical (thermal conductivity), and chemical (oxidation stability) properties are mentioned. Some present issues in the field are considered.

  18. Electrochemical evaluation and determination of antiretroviral drug fosamprenavir using boron-doped diamond and glassy carbon electrodes.

    Science.gov (United States)

    Gumustas, Mehmet; Ozkan, Sibel A

    2010-05-01

    Fosamprenavir is a pro-drug of the antiretroviral protease inhibitor amprenavir and is oxidizable at solid electrodes. The anodic oxidation behavior of fosamprenavir was investigated using cyclic and linear sweep voltammetry at boron-doped diamond and glassy carbon electrodes. In cyclic voltammetry, depending on pH values, fosamprenavir showed one sharp irreversible oxidation peak or wave depending on the working electrode. The mechanism of the oxidation process was discussed. The voltammetric study of some model compounds allowed elucidation of the possible oxidation mechanism of fosamprenavir. The aim of this study was to determine fosamprenavir levels in pharmaceutical formulations and biological samples by means of electrochemical methods. Using the sharp oxidation response, two voltammetric methods were described for the determination of fosamprenavir by differential pulse and square-wave voltammetry at the boron-doped diamond and glassy carbon electrodes. These two voltammetric techniques are 0.1 M H(2)SO(4) and phosphate buffer at pH 2.0 which allow quantitation over a 4 x 10(-6) to 8 x 10(-5) M range using boron-doped diamond and a 1 x 10(-5) to 1 x 10(-4) M range using glassy carbon electrodes, respectively, in supporting electrolyte. All necessary validation parameters were investigated and calculated. These methods were successfully applied for the analysis of fosamprenavir pharmaceutical dosage forms, human serum and urine samples. The standard addition method was used in biological media using boron-doped diamond electrode. No electroactive interferences from the tablet excipients or endogenous substances from biological material were found. The results were statistically compared with those obtained through an established HPLC-UV technique; no significant differences were found between the voltammetric and HPLC methods.

  19. Thermal shock resistance of thick boron-doped diamond under extreme heat loads

    NARCIS (Netherlands)

    De Temmerman, G.; Dodson, J.; Linke, J.; Lisgo, S.; Pintsuk, G.; Porro, S.; Scarsbrook, G.

    2011-01-01

    Thick free-standing boron-doped diamonds were prepared by microwave plasma assisted chemical vapour deposition. Samples with a final thickness close to 5 mm and with lateral dimensions 25 x 25 mm were produced. The thermal shock resistance of the material was tested by exposure in the JUDITH

  20. Growth of high quality AlN films on CVD diamond by RF reactive magnetron sputtering

    Science.gov (United States)

    Chen, Liang-xian; Liu, Hao; Liu, Sheng; Li, Cheng-ming; Wang, Yi-chao; An, Kang; Hua, Chen-yi; Liu, Jin-long; Wei, Jun-jun; Hei, Li-fu; Lv, Fan-xiu

    2018-02-01

    A highly oriented AlN layer has been successfully grown along the c-axis on a polycrystalline chemical vapor deposited (CVD) diamond by RF reactive magnetron sputtering. Structural, morphological and mechanical properties of the heterostructure were investigated by Scanning Electron Microscopy (SEM), Atomic Force Microscopy (AFM), Transmission Electron Microscopy (TEM), X-ray diffraction (XRD), Nano-indentation and Four-probe meter. A compact AlN film was demonstrated on the diamond layer, showing columnar grains and a low surface roughness of 1.4 nm. TEM results revealed a sharp AlN/diamond interface, which was characterized by the presence of a distinct 10 nm thick buffer layer resulting from the initial AlN growth stage. The FWHM of AlN (002) diffraction peak and its rocking curve are as low as 0.41° and 3.35° respectively, indicating a highly preferred orientation along the c-axis. AlN sputtered films deposited on glass substrates show a higher bulk resistivity (up to 3 × 1012 Ω cm), compared to AlN films deposited on diamond (∼1010 Ω cm). Finally, the film hardness and Young's modulus of AlN films on diamond are 25.8 GPa and 489.5 GPa, respectively.

  1. Tribological performance of polycrystalline tantalum-carbide-incorporated diamond films on silicon substrates

    Science.gov (United States)

    Ullah, Mahtab; Rana, Anwar Manzoor; Ahmed, E.; Malik, Abdul Sattar; Shah, Z. A.; Ahmad, Naseeb; Mehtab, Ujala; Raza, Rizwan

    2018-05-01

    Polycrystalline tantalum-carbide-incorporated diamond coatings have been made on unpolished side of Si (100) wafer by hot filament chemical vapor deposition process. Morphology of the coatings has been found to vary from (111) triangular-facetted to predominantly (111) square-faceted by increasing the concentration of tantalum carbide. The results have been compared to those of a diamond reference coating with no tantalum content. An increase in roughness has been observed with the increase of tantalum carbide (TaC) due to change in morphology of the diamond films. It is noticed that roughness of the coatings increases as grains become more square-faceted. It is found that diamond coatings involving tantalum carbide are not as resistant as diamond films with no TaC content and the coefficient of friction for such coatings with microcrystalline grains can be manipulated to 0·33 under high vacuum of 10-7 Torr. Such a low friction coefficient value enhances tribological behavior of unpolished Si substrates and can possibly be used in sliding applications.

  2. Mechanical properties of phosphorus-doped polysilicon films

    CERN Document Server

    Lee, S W; Kim, J P; Park, S J; Yi, S W; Cho, D I; Kim, J J

    1998-01-01

    Polysilicon films deposited by low pressure chemical vapor deposition (LPCVD) are the most widely used structural material in microelectromechanical systems (MEMS). However, the structural properties of LPCVD polysilicon films are known to vary significantly, depending on deposition conditions as well as post-deposition processes. This paper investigates the effects of phosphorus doping and texture on Young's modulus of polysilicon films. Polysilicon films are deposited at 585 .deg. C, 605 .deg. C, and 625 .deg. C to a thickness of 2 mu m. Specimens with varying phosphorus doping levels are prepared by the diffusion process at various temperatures and times using both POCl sub 3 and phosphosilicate glass (PSG) source. Texture is measured using an X-ray diffractometer. Young's modulus is estimated from the average values of the resonant frequencies measured from four-different size lateral resonators. Our results show that Young's modulus of diffusion doped polysilicon films decreases with increasing doping co...

  3. Novel morphology of chemical vapor deposited diamond films

    Energy Technology Data Exchange (ETDEWEB)

    Tang, C.J. [I3N and Department of Physics, University of Aveiro (Portugal); Jiangsu Key Laboratory for Advanced Functional Materials and Department of Physics, Changshu Institute of Technology, Changshu (China); TEMA and Department of Mechanical Engineering, University of Aveiro (Portugal); Fernandes, A.J.S.; Abe, I.; Pinto, J.L. [I3N and Department of Physics, University of Aveiro (Portugal); Gracio, J. [TEMA and Department of Mechanical Engineering, University of Aveiro (Portugal); Buijnsters, J.G. [Institute for Molecules and Materials (IMM), Radboud University Nijmegen (Netherlands)

    2010-04-15

    We have obtained simultaneously nanocrystalline and {l_brace}100{r_brace} faceted large-grained polycrystalline diamond films not only on different substrates but also on the same substrate in only one deposition run using a novel approach for substrate arrangement. Furthermore, interesting unusual morphologies and microstructures composed by non-faceted nanostructures and terminated with large smooth {l_brace}100{r_brace} facet-like belt are found near the edges of the top square sample. The morphology variation is likely caused by the so called edge effect, where a strong variation in temperature is also present. We have modelled the temperature distribution on the substrates by computer simulations using the finite element method. The novel feature, namely the coexistence of oval non-faceted nanocrystalline diamond grains and large smooth {l_brace}100{r_brace} facet-like belt in one diamond grain, is in the transition from {l_brace}100{r_brace} faceted polycrystalline diamond to cauliflower-like nanocrystalline diamond. The formation mechanism is discussed based on the temperature analysis and other simulation results described in the literature. (copyright 2010 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim) (orig.)

  4. Electrochemical protein cleavage in a microfluidic cell with integrated boron doped diamond electrodes

    NARCIS (Netherlands)

    van den Brink, Floris Teunis Gerardus; Zhang, Tao; Ma, Liwei; Odijk, Mathieu; Olthuis, Wouter; Permentier, Hjalmar P.; Bischoff, Rainer P.H.; van den Berg, Albert

    2015-01-01

    We present a microfluidic electrochemical cell with integrated boron doped diamond (BDD) electrodes which is designed for high electrochemical conversion efficiencies. With our newest developments, we aim to exploit the benefits of BDD as a novel electrode material to conduct tyrosine- and

  5. Combined addition of nano diamond and nano SiO2, an effective method to improve the in-field critical current density of MgB2 superconductor

    International Nuclear Information System (INIS)

    Rahul, S.; Varghese, Neson; Vinod, K.; Devadas, K.M.; Thomas, Syju; Anees, P.; Chattopadhyay, M.K.; Roy, S.B.; Syamaprasad, U.

    2011-01-01

    Highlights: → Both nano diamond and nano SiO 2 caused significant modifications in the structural properties of pure MgB 2 sample. → Reduction in T C for the best codoped sample was approximately 2 K. → The best codoped sample yielded a J C , an order of magnitude more than the undoped one at 5 K and 8 T. → The enhanced flux pinning capability provided by the additives is responsible for the improved in-field J C . -- Abstract: MgB 2 bulk samples added with nano SiO 2 and/or nano diamond were prepared by powder-in-sealed-tube (PIST) method and the effects of addition on structural and superconducting properties were studied. X-ray diffraction (XRD) analysis revealed that the addition caused systematic reduction in 'a' lattice parameter due to the substitution of C atoms at B sites and the strain caused by reacted intragrain nano particles of Mg 2 Si as evinced by transmission electron microscope image. Scanning electron microscopy images showed distinct microstructural variations with SiO 2 /diamond addition. It was evident from DC magnetization measurements that the in-field critical current density [J C (H)] of doped samples did not fall drastically like the undoped sample. Among the doped samples the J C (H) of co-doped samples were significantly higher and the best co-doped sample yielded a J C , an order of magnitude more than the undoped one at 5 K and 8 T.

  6. Factors influencing voltammetric reduction of 5-nitroquinoline at boron-doped diamond electrodes

    Czech Academy of Sciences Publication Activity Database

    Vosáhlová, J.; Zavázalová, J.; Petrák, Václav; Schwarzová-Pecková, K.

    2016-01-01

    Roč. 147, č. 1 (2016), s. 21-29 ISSN 0026-9247 Institutional support: RVO:68378271 Keywords : voltammetry * boron-doped diamond electrode * boron concentration * reduction * electrochemistry Subject RIV: BM - Solid Matter Physics ; Magnetism OBOR OECD: Condensed matter physics (including formerly solid state physics, supercond.) Impact factor: 1.282, year: 2016

  7. Fabrication and Characterization of FeNiCr Matrix-TiC Composite for Polishing CVD Diamond Film

    Institute of Scientific and Technical Information of China (English)

    Zhuji Jin; Zewei Yuan; Renke Kang; Boxian Dong

    2009-01-01

    Dynamic friction polishing (DFP) is one of the most promising methods appropriate for polishing CVD diamond film with high efficiency and low cost.By this method CVD diamond film is polished through being simply pressed against a metal disc rotating at a high speed utilizing the thermochemical reaction occurring as a result of dynamic friction between them in the atmosphere.However, the relatively soft materials such as stainless steel, cast iron and nickel alloy widely used for polishing CVD diamond film are easy to wear and adhere to diamond film surface, which may further lead to low efficiency and poor polishing quality.In this paper, FeNiCr matrix-TiC composite used as grinding wheel for polishing CVD diamond film was obtained by combination of mechanical alloying (MA) and spark plasma sintering (SPS).The process of ball milling,composition, density, hardness, high-temperature oxidation resistance and wear resistance of the sintered piece were analyzed.The results show that TiC was introduced in MA-SPS process and had good combination with FeNiCr matrix and even distribution in the matrix.The density of composite can be improved by mechanical alloying.The FeNiCr matrix-TiC composite obtained at 1273 K was found to be superior to at 1173 K sintering in hardness, high-temperature oxidation resistance and wearability.These properties are more favorable than SUS304 for the preparation of high-performance grinding wheel for polishing CVD diamond film.

  8. Enhanced B doping in CVD-grown GeSn:B using B δ-doping layers

    Science.gov (United States)

    Kohen, David; Vohra, Anurag; Loo, Roger; Vandervorst, Wilfried; Bhargava, Nupur; Margetis, Joe; Tolle, John

    2018-02-01

    Highly doped GeSn material is interesting for both electronic and optical applications. GeSn:B is a candidate for source-drain material in future Ge pMOS device because Sn adds compressive strain with respect to pure Ge, and therefore can boost the Ge channel performances. A high B concentration is required to obtain low contact resistivity between the source-drain material and the metal contact. To achieve high performance, it is therefore highly desirable to maximize both the Sn content and the B concentration. However, it has been shown than CVD-grown GeSn:B shows a trade-off between the Sn incorporation and the B concentration (increasing B doping reduces Sn incorporation). Furthermore, the highest B concentration of CVD-grown GeSn:B process reported in the literature has been limited to below 1 × 1020 cm-3. Here, we demonstrate a CVD process where B δ-doping layers are inserted in the GeSn layer. We studied the influence of the thickness between each δ-doping layers and the δ-doping layers process conditions on the crystalline quality and the doping density of the GeSn:B layers. For the same Sn content, the δ-doping process results in a 4-times higher B doping than the co-flow process. In addition, a B doping concentration of 2 × 1021 cm-3 with an active concentration of 5 × 1020 cm-3 is achieved.

  9. Wafer bowing control of free-standing heteroepitaxial diamond (100) films grown on Ir(100) substrates via patterned nucleation growth

    International Nuclear Information System (INIS)

    Yoshikawa, Taro; Kodama, Hideyuki; Kono, Shozo; Suzuki, Kazuhiro; Sawabe, Atsuhito

    2015-01-01

    The potential of patterned nucleation growth (PNG) technique to control the wafer bowing of free-standing heteroepitaxial diamond films was investigated. The heteroepitaxial diamond (100) films were grown on an Ir(100) substrate via PNG technique with different patterns of nucleation regions (NRs), which were dot-arrays with 8 or 13 μm pitch aligned to < 100 > or < 110 > direction of the Ir(100) substrate. The wafer bows and the local stress distributions of the free-standing films were measured using a confocal micro-Raman spectrometer. For each NR pattern, the stress evolutions within the early stage of diamond growth were also studied together with a scanning electron microscopic observation of the coalescing diamond particles. These investigations revealed that the NR pattern, in terms of pitch and direction of dot-array, strongly affects the compressive stress on the nucleation side of the diamond film and dominantly contributes to the elastic deformation of the free-standing film. This indicates that the PNG technique with an appropriate NR pattern is a promising solution to fabricate free-standing heteroepitaxial diamond films with extremely small bows. - Highlights: • Wafer bowing control of free-standing heteroepitaxial diamond (100) films • Effect of patterned nucleation and growth (PNG) technique on wafer bowing reduction • Influence of nucleation region patterns of PNG on wafer bowing • Internal stress analysis of PNG films via confocal micro-Raman spectroscopy

  10. Role of high microwave power on growth and microstructure of thick nanocrystalline diamond films: A comparison with large grain polycrystalline diamond films

    Science.gov (United States)

    Tang, C. J.; Fernandes, A. J. S.; Girão, A. V.; Pereira, S.; Shi, Fa-Nian; Soares, M. R.; Costa, F.; Neves, A. J.; Pinto, J. L.

    2014-03-01

    In this work, we study the growth habit of nanocrystalline diamond (NCD) films by exploring the very high power regime, up to 4 kW, in a 5 kW microwave plasma chemical vapour deposition (MPCVD) reactor, through addition of a small amount of nitrogen and oxygen (0.24%) into 4% CH4 in H2 plasma. The coupled effect of high microwave power and substrate temperature on NCD growth behaviour is systematically investigated by varying only power, while fixing the remaining operating parameters. When the power increases from 2 kW to 4 kW, resulting also in rise of the Si substrate temperature higher than 150 °C, the diamond films obtained maintain the NCD habit, while the growth rate increases significantly. The highest growth rate of 4.6 μm/h is achieved for the film grown at 4 kW, which represents a growth rate enhancement of about 15 times compared with that obtained when using 2 kW power. Possible factors responsible for such remarkable growth rate enhancement of the NCD films are discussed. The evolution of NCD growth characteristics such as morphology, microstructure and texture is studied by growing thick films and comparing it with that of large grain polycrystalline (PCD) films. One important characteristic of the NCD films obtained, in contrast to PCD films, is that irrespective of deposition time (i.e. film thickness), their grain size and surface roughness remain in the nanometer range throughout the growth. Finally, based on our present and previous experimental results, a potential parameter window is established for fast growth of NCD films under high power conditions.

  11. Investigation of the nucleation process of chemical vapour deposited diamond films

    International Nuclear Information System (INIS)

    Katai, S.

    2001-01-01

    The primary aim of this work was to contribute to the understanding of the bias enhanced nucleation (BEN) process during the chemical vapour deposition (CVD) of diamond on silicon. The investigation of both the gas phase environment above the substrate surface, by in situ mass selective energy analysis of ions, and of the surface composition and structure by in vacuo surface analytic methods (XPS, EELS) have been carried out. In both cases, the implementation of these measurements required the development and construction of special experimental apparatus as well. The secondary aim of this work was to give orientation to our long term goal of growing diamond films with improved quality. For this reason, (1) contaminant levels at the diamond-silicon interface after growth were studied by SIMS, (2) the internal stress distribution of highly oriented free-standing diamond films were studied by Raman spectroscopy, and (3) an attempt was made to produce spatially regular oriented nuclei formation by nucleating on a pattern created by laser treatment on silicon substrates. (orig.)

  12. Structural evolution of Ti destroyable interlayer in large-size diamond film deposition by DC arc plasma jet

    Science.gov (United States)

    Guo, Jianchao; Li, Chengming; Liu, Jinlong; Wei, Junjun; Chen, Liangxian; Hua, Chenyi; Yan, Xiongbo

    2016-05-01

    The addition of titanium (Ti) interlayer was verified to reduce the residual stress of diamond films by self-fracturing and facilitate the harvest of a crack-free free-standing diamond film prepared by direct current (DC) arc plasma jet. In this study, the evolution of the Ti interlayer between large-area diamond film and substrate was studied and modeled in detail. The evolution of the interlayer was found to be relevant to the distribution of the DC arc plasma, which can be divided into three areas (arc center, arc main, and arc edge). The formation rate of titanium carbide (TiC) in the arc main was faster than in the other two areas and resulted in the preferred generation of crack in the diamond film in the arc main during cooling. Sandwich structures were formed along with the growth of TiC until the complete transformation of the Ti interlayer. The interlayer released stress via self-fracture. Avoiding uneven fragile regions that formed locally in the interlayer and achieving cooperatively released stress are crucial for the preparation of large crack-free diamond films.

  13. Diamond nanoparticles as a support for Pt and PtRu catalysts for direct methanol fuel cells.

    Science.gov (United States)

    La-Torre-Riveros, Lyda; Guzman-Blas, Rolando; Méndez-Torres, Adrián E; Prelas, Mark; Tryk, Donald A; Cabrera, Carlos R

    2012-02-01

    Diamond in nanoparticle form is a promising material that can be used as a robust and chemically stable catalyst support in fuel cells. It has been studied and characterized physically and electrochemically, in its thin film and powder forms, as reported in the literature. In the present work, the electrochemical properties of undoped and boron-doped diamond nanoparticle electrodes, fabricated using the ink-paste method, were investigated. Methanol oxidation experiments were carried out in both half-cell and full fuel cell modes. Platinum and ruthenium nanoparticles were chemically deposited on undoped and boron doped diamond nanoparticles through the use of NaBH(4) as reducing agent and sodium dodecyl benzene sulfonate (SDBS) as a surfactant. Before and after the reduction process, samples were characterized by electron microscopy and spectroscopic techniques. The ink-paste method was also used to prepare the membrane electrode assembly with Pt and Pt-Ru modified undoped and boron-doped diamond nanoparticle catalytic systems, to perform the electrochemical experiments in a direct methanol fuel cell system. The results obtained demonstrate that diamond supported catalyst nanomaterials are promising for methanol fuel cells.

  14. Subtle Raman signals from nano-diamond and β-SiC thin films

    International Nuclear Information System (INIS)

    Kuntumalla, Mohan Kumar; Ojha, Harish; Srikanth, Vadali Venkata Satya Siva

    2013-01-01

    Micro Raman scattering experiments are carried out in pursuit of subtle but discernable signals from nano-diamond and β-SiC thin films. The thin films are synthesized using microwave plasma assisted chemical vapor deposition technique. Raman scattering experiments in conjunction with scanning electron microscopy and x-ray diffraction were carried out to extract microstructure and phase information of the above mentioned thin films. Certain subtle Raman signals have been identified in this work. In the case of nanodiamond thin films, Raman bands at ∼ 485 and ∼ 1220 cm −1 are identified. These bands have been assigned to the nanodiamond present in nanodiamond thin films. In the case of nano β-SiC thin films, optical phonons are identified using surface enhanced Raman scattering. - Highlights: ► Subtle Raman signals from nano-diamond and β-silicon carbide related thin films. ► Raman bands at ∼ 485 and ∼ 1220 cm −1 from nanodiamond thin films are identified. ► Longitudinal optical phonon from nano β-silicon carbide thin films is identified

  15. Comparison of the influence of boron and aluminium doping on the material properties of electrochemically deposited ZnO films

    Energy Technology Data Exchange (ETDEWEB)

    Calnan, Sonya [Helmholtz-Zentrum für Materialien und Energie GmbH, Hahn-Meitner Platz 1, 14109 Berlin (Germany); Riedel, Wiebke; Gledhill, Sophie [Helmholtz-Zentrum für Materialien und Energie GmbH, Hahn-Meitner Platz 1, 14109 Berlin (Germany); Fachbereich Physik, Freie Universitaet Berlin, Arnimallee 14, 14195 Berlin (Germany); Stannowski, Bernd [Helmholtz-Zentrum für Materialien und Energie GmbH, Hahn-Meitner Platz 1, 14109 Berlin (Germany); Lux-Steiner, Martha Ch. [Helmholtz-Zentrum für Materialien und Energie GmbH, Hahn-Meitner Platz 1, 14109 Berlin (Germany); Fachbereich Physik, Freie Universitaet Berlin, Arnimallee 14, 14195 Berlin (Germany); Schlatmann, Rutger [Helmholtz-Zentrum für Materialien und Energie GmbH, Hahn-Meitner Platz 1, 14109 Berlin (Germany); Fachbereich 1 Ingenieurwissenschaften I, University of Applied Science (HTW) Berlin, Wilhelminenhofstraße 75 A, 12459 Berlin (Germany)

    2015-11-02

    The effect of varying the boron and aluminium content of the starting electrolyte for extrinsically doped ZnO films grown on SnO{sub 2}:F substrates by electrochemical deposition was investigated. The ZnO:B film surface was characterized by grains with mainly hexagonal faces exposed while the exposed faces of the ZnO:Al grains were rectangular. Whereas a B{sup 3+}/Zn{sup 2+} ratio of up to 10 at.% in the electrolyte had no significant effect on the crystalline structure of the ZnO films, an Al{sup 3+}/Zn{sup 2+} ratio above 0.25 at.% increased the disorder in the crystalline structure. All the boron doped films exhibit a strong E{sub 2}-high Raman mode related to wurtzite ZnO structure but this peak was much weaker for ZnO:Al and diminished with increasing Al incorporation in the films. Exposing the films to ultra-violet light reduced their effective sheet resistance from values beyond measurement range to values between 40 and 5000 kΩ/sq for film thicknesses of 200–550 nm. Inspection of the optical spectra near the bandgap edge and the plasma edge in the mid infrared range, showed that the Al-doping resulted in a higher carrier concentration ~ 10{sup 20} cm{sup −3} than B-doping. X-ray electron spectroscopy showed that the dopant efficiency was limited by the absence of dopant atoms near the surface of all the ZnO:B films and of the lightly doped ZnO:Al and, by the formation of aluminium oxide at the surface of the more highly doped ZnO:Al films. - Highlights: • Crystalline ZnO grown by electrochemical deposition. • Comparison of influence of H{sub 3}BO{sub 3} and Al(NO{sub 3}){sub 3} as dopant sources. • Different ZnO crystalline orientation for Al and boron doping. • Film surface chemical composition suppressed electrical conductivity.

  16. Electrophoretic preparation and characterization of porous electrodes from diamond nanoparticles

    Energy Technology Data Exchange (ETDEWEB)

    Riveros, Lyda La Torre; Soto, Keyla; Tryk, Donald A; Cabrera, Carlos R [Department of Chemistry and Center of Nanoscale Materials, University of Puerto Rico, Rio Piedras, PO Box 23346 San Juan, PR 00931-3346 (Puerto Rico)

    2007-04-15

    We carried out chemical purification of commercially available diamond nanoparticles by refluxing in aqueous HNO{sub 3} and characterized the samples by spectroscopic and surface techniques before and after purification. As a first step in the preparation of electrodes for electrochemistry, we have electrophoretically deposited thin, highly uniform films of controlled thickness (1-8 {mu}m) on silicon substrates using the purified diamond nanoparticles. These have been characterized by scanning electron microscopy (SEM). All films obtained were homogeneous in thickness and without macroscopic holes or cracks. Such structures could also be used in many other applications such as fuel cells or lithium batteries. We have performed cyclic voltammetry experiments with these electrodes. The voltammograms of diamond nanoparticles electrophoretically deposited on silicon indicate hydrogen evolution. This demonstrates that the material is useful as electrocatalitic support. This conclusion is supported by the cyclic voltammograms obtained using ferrycyanide (III) chloride and hexaamineruthenium (III) chloride complexes as redox probes. However, these redox probes showed very small peak currents. This behavior could be improved by doping the diamond nanoparticles with an impurity such as boron.

  17. Electrophoretic preparation and characterization of porous electrodes from diamond nanoparticles

    International Nuclear Information System (INIS)

    Riveros, Lyda La Torre; Soto, Keyla; Tryk, Donald A; Cabrera, Carlos R

    2007-01-01

    We carried out chemical purification of commercially available diamond nanoparticles by refluxing in aqueous HNO 3 and characterized the samples by spectroscopic and surface techniques before and after purification. As a first step in the preparation of electrodes for electrochemistry, we have electrophoretically deposited thin, highly uniform films of controlled thickness (1-8 μm) on silicon substrates using the purified diamond nanoparticles. These have been characterized by scanning electron microscopy (SEM). All films obtained were homogeneous in thickness and without macroscopic holes or cracks. Such structures could also be used in many other applications such as fuel cells or lithium batteries. We have performed cyclic voltammetry experiments with these electrodes. The voltammograms of diamond nanoparticles electrophoretically deposited on silicon indicate hydrogen evolution. This demonstrates that the material is useful as electrocatalitic support. This conclusion is supported by the cyclic voltammograms obtained using ferrycyanide (III) chloride and hexaamineruthenium (III) chloride complexes as redox probes. However, these redox probes showed very small peak currents. This behavior could be improved by doping the diamond nanoparticles with an impurity such as boron

  18. Potential and pH dependence of photocurrent transients for boron-doped diamond electrodes in aqueous electrolyte

    International Nuclear Information System (INIS)

    Green, S.J.; Mahe, L.S.A.; Rosseinsky, D.R.; Winlove, C.P.

    2013-01-01

    Using illumination at energies below the intrinsic diamond energy gap, photocurrent transients have been recorded for boron-doped diamond (BDD) as an electrode in an aqueous electrolyte of 0.1 M KH 2 PO 4 . The commercially-supplied BDD was in the form of a free-standing, polycrystalline film grown by chemical vapour deposition (CVD), with a boron acceptor concentration of ≥10 20 cm −3 . The effects of mechanical polishing of the BDD, of electrochemical hydrogen evolution and of electrochemical oxygen evolution (in 0.1 M KH 2 PO 4 ), on the potential dependence of the photocurrent transients have been examined. Measurements of the cathodic photocurrent at light switch-on have been used to determine the photocurrent onset potential as a measure of the flatband potential. Comparison with and between related literature observations has shown broad agreement across considerably varying BDD/electrolyte systems. The flatband potential shifted positively following electrochemical oxygen evolution, indicating the formation of oxygen-containing groups on the diamond surface, these increasing the potential drop across the Helmholtz layer. For the electrochemically oxidised electrode, the cathodic photocurrent transient at a fixed potential changed reproducibly with changing solution pH, owing to the participation of the oxygen-containing surface groups in acid–base equilibrium with the solution. This clear demonstration of BDD as a photoelectrochemical pH sensor is in principle extendable to mapping the spatial variation in pH across a BDD surface by use of a focussed light spot

  19. Growth of boron doped hydrogenated nanocrystalline cubic silicon carbide (3C-SiC) films by Hot Wire-CVD

    Energy Technology Data Exchange (ETDEWEB)

    Pawbake, Amit [School of Energy Studies, Savitribai Phule Pune University, Pune 411 007 (India); Tata Institute of Fundamental Research, Colaba, Mumbai 400 005 (India); Mayabadi, Azam; Waykar, Ravindra; Kulkarni, Rupali; Jadhavar, Ashok [School of Energy Studies, Savitribai Phule Pune University, Pune 411 007 (India); Waman, Vaishali [Modern College of Arts, Science and Commerce, Shivajinagar, Pune 411 005 (India); Parmar, Jayesh [Tata Institute of Fundamental Research, Colaba, Mumbai 400 005 (India); Bhattacharyya, Somnath [Department of Metallurgical and Materials Engineering, IIT Madras, Chennai 600 036 (India); Ma, Yuan‐Ron [Department of Physics, National Dong Hwa University, Hualien 97401, Taiwan (China); Devan, Rupesh; Pathan, Habib [Department of Physics, Savitribai Phule Pune University, Pune 411007 (India); Jadkar, Sandesh, E-mail: sandesh@physics.unipune.ac.in [Department of Physics, Savitribai Phule Pune University, Pune 411007 (India)

    2016-04-15

    Highlights: • Boron doped nc-3C-SiC films prepared by HW-CVD using SiH{sub 4}/CH{sub 4}/B{sub 2}H{sub 6}. • 3C-Si-C films have preferred orientation in (1 1 1) direction. • Introduction of boron into SiC matrix retard the crystallanity in the film structure. • Film large number of SiC nanocrystallites embedded in the a-Si matrix. • Band gap values, E{sub Tauc} and E{sub 04} (E{sub 04} > E{sub Tauc}) decreases with increase in B{sub 2}H{sub 6} flow rate. - Abstract: Boron doped nanocrystalline cubic silicon carbide (3C-SiC) films have been prepared by HW-CVD using silane (SiH{sub 4})/methane (CH{sub 4})/diborane (B{sub 2}H{sub 6}) gas mixture. The influence of boron doping on structural, optical, morphological and electrical properties have been investigated. The formation of 3C-SiC films have been confirmed by low angle XRD, Raman spectroscopy, X-ray photoelectron spectroscopy (XPS), Fourier transform infra-red (FTIR) spectroscopy and high resolution-transmission electron microscopy (HR-TEM) analysis whereas effective boron doping in nc-3C-SiC have been confirmed by conductivity, charge carrier activation energy, and Hall measurements. Raman spectroscopy and HR-TEM analysis revealed that introduction of boron into the SiC matrix retards the crystallanity in the film structure. The field emission scanning electron microscopy (FE-SEM) and non contact atomic force microscopy (NC-AFM) results signify that 3C-SiC film contain well resolved, large number of silicon carbide (SiC) nanocrystallites embedded in the a-Si matrix having rms surface roughness ∼1.64 nm. Hydrogen content in doped films are found smaller than that of un-doped films. Optical band gap values, E{sub Tauc} and E{sub 04} decreases with increase in B{sub 2}H{sub 6} flow rate.

  20. Modeling flux pinning in thin undoped and BazRo3-doped YBCO films

    DEFF Research Database (Denmark)

    Paturi, P.; Irjala, M.; Huhtinen, H.

    2009-01-01

    A simple model based on distributions of twin boundaries, dislocations, and BaZrO3 nanorods is presented to describe the Jc properties of undoped and BaZrO3 (BZO)-doped YBa2Cu3Ox thin films. The model accurately describes the shape of Jc(B,T) curves of the films, when the pinning site distributions...... are taken from distributions of twin spacings and BZO nanorods from transmission electron microscope images. Thus, assuming that the model can be used for prediction of the Jc properties, we conclude that for enhancement of undoped films more crystalline defects are needed and for doped films a dopant...

  1. Boron-doped zinc oxide thin films for large-area solar cells grown by metal organic chemical vapor deposition

    International Nuclear Information System (INIS)

    Chen, X.L.; Xu, B.H.; Xue, J.M.; Zhao, Y.; Wei, C.C.; Sun, J.; Wang, Y.; Zhang, X.D.; Geng, X.H.

    2007-01-01

    Boron-doped zinc oxide (ZnO:B) films were grown by metal organic chemical vapor deposition using diethylzinc (DEZn), and H 2 O as reactant gases and diborane (B 2 H 6 ) as an n-type dopant gas. The structural, electrical and optical properties of ZnO films doped at different B 2 H 6 flow rates were investigated. X-ray diffraction spectra and scanning electron microscopy images indicate that boron-doping plays an important role on the microstructure of ZnO films, which induced textured morphology. With optimized conditions, low sheet resistance (∼ 30 Ω/□), high transparency (> 85% in the visible light and infrared range) and high mobility (17.8 cm 2 V -1 s -1 ) were obtained for 700-nm ZnO:B films deposited on 20 cm x 20 cm glass substrates at the temperature of 443 K. After long-term exposure in air, the ZnO:B films also showed a better electrical stability than the un-doped samples. With the application of ZnO:B/Al back contacts, the short circuit current density was effectively enhanced by about 3 mA/cm 2 for a small area a-Si:H cell and a high efficiency of 9.1% was obtained for a large-area (20 cm x 20 cm) a-Si solar module

  2. Electronic and physico-chemical properties of nanometric boron delta-doped diamond structures

    International Nuclear Information System (INIS)

    Chicot, G.; Fiori, A.; Tran Thi, T. N.; Bousquet, J.; Delahaye, J.; Grenet, T.; Eon, D.; Omnès, F.; Bustarret, E.; Volpe, P. N.; Tranchant, N.; Mer-Calfati, C.; Arnault, J. C.; Gerbedoen, J. C.; Soltani, A.; De Jaeger, J. C.; Alegre, M. P.; Piñero, J. C.; Araújo, D.; Jomard, F.

    2014-01-01

    Heavily boron doped diamond epilayers with thicknesses ranging from 40 to less than 2 nm and buried between nominally undoped thicker layers have been grown in two different reactors. Two types of [100]-oriented single crystal diamond substrates were used after being characterized by X-ray white beam topography. The chemical composition and thickness of these so-called delta-doped structures have been studied by secondary ion mass spectrometry, transmission electron microscopy, and spectroscopic ellipsometry. Temperature-dependent Hall effect and four probe resistivity measurements have been performed on mesa-patterned Hall bars. The temperature dependence of the hole sheet carrier density and mobility has been investigated over a broad temperature range (6 K  2 /Vs, independently of the layer thickness and the substrate type. Comparison with previously published data and theoretical calculations showed that scattering by ionized impurities explained only partially this low common value. None of the delta-layers showed any sign of confinement-induced mobility enhancement, even for thicknesses lower than 2 nm

  3. Study of Nitrogen Effect on the Boron Diffusion during Heat Treatment in Polycrystalline Silicon/Nitrogen-Doped Silicon Thin Films

    Science.gov (United States)

    Saci, Lynda; Mahamdi, Ramdane; Mansour, Farida; Boucher, Jonathan; Collet, Maéva; Bedel Pereira, Eléna; Temple-Boyer, Pierre

    2011-05-01

    The present paper studies the boron (B) diffusion in nitrogen (N) doped amorphous silicon (a-Si) layer in original bi-layer B-doped polycrystalline silicon (poly-Si)/in-situ N-doped Si layers (NIDOS) thin films deposited by low pressure chemical vapor deposition (LPCVD) technique. The B diffusion in the NIDOS layer was investigated by secondary ion mass spectrometry (SIMS) and Fourier transform infrared spectroscopy (FTIR) analysis. A new extended diffusion model is proposed to fit the SIMS profile of the bi-layer films. This model introduces new terms which take into account the effect of N concentration on the complex diffusion phenomena of B atoms in bi-layer films. SIMS results show that B diffusion does not exceed one third of NIDOS layer thickness after annealing. The reduction of the B diffusion in the NIDOS layer is due to the formation of complex B-N as shown by infrared absorption measurements. Electrical measurements using four-probe and Hall effect techniques show the good conductivity of the B-doped poly-Si layer after annealing treatment.

  4. Structural, optical and magnetic properties of Mn doped ZnO thin films prepared by pulsed laser deposition

    Energy Technology Data Exchange (ETDEWEB)

    Aravind, Arun, E-mail: aruncusat@gmail.com [Nanophotonic and Optoelectronic Devices Laboratory, Department of Physics, Cochin University of Science and Technology, Kochi 682 022, Kerala (India); Jayaraj, M.K., E-mail: mkj@cusat.ac.in [Nanophotonic and Optoelectronic Devices Laboratory, Department of Physics, Cochin University of Science and Technology, Kochi 682 022, Kerala (India); Kumar, Mukesh; Chandra, Ramesh [Nano Science Laboratory, Institute Instrumentation Centre, IIT Roorkee, Roorkee 247 667, Uttarakhand (India)

    2012-08-01

    Highlights: Black-Right-Pointing-Pointer Defect induced Raman active modes in Mn doped ZnO thin films. Black-Right-Pointing-Pointer Room temperature ferromagnetism. Black-Right-Pointing-Pointer Morphological variations of ZnO thin films with Mn doping. Black-Right-Pointing-Pointer Variation of refractive index of ZnO thin films with Mn doping. - Abstract: Zn{sub 1-x}Mn{sub x}O thin films were grown by pulsed laser deposition. The phase purity and the structure were confirmed by X-ray diffraction studies. The films have a transmittance more than 80% in the visible region. The refractive index of Zn{sub 0.90}Mn{sub 0.10}O films is found to be 1.77 at 550 nm. The presence of non-polar E{sub 2}{sup high} and E{sub 2}{sup low} Raman modes in thin films indicates that 'Mn' doping does not change the wurtzite structure of ZnO. Apart from the normal modes of ZnO the Zn{sub 1-x}Mn{sub x}O ceramic targets show two additional modes at 332 cm{sup -1} (I{sub 1}) and 524 cm{sup -1} (I{sub 2}). The broad Raman peaks (340-600 cm{sup -1}) observed Zn{sub 0.90}Mn{sub 0.10}O thin films can be deconvoluted into five peaks, denoted as P{sub 1}-P{sub 5}. The possible origins of Raman peaks in Zn{sub 1-x}Mn{sub x}O films are the structural disorder and morphological change caused by the Mn dopant. The B{sub 1}{sup low}, {sup 2}B{sub 1}{sup low}, B{sub 1}{sup high} and A{sub 1}{sup LO} modes as well as the surface phonon mode have been observed in heavily Mn-doped ZnO films. Zn{sub 0.98}Mn{sub 0.02}O thin film shows room temperature ferromagnetism. The saturation magnetic moment of the Zn{sub 0.98}Mn{sub 0.02}O thin film is 0.42{mu}{sub B}/Mn atom. The undoped ZnO film prepared under the same condition shows diamagnetic nature. At higher doping concentrations the formation of Mn clusters suppress the room temperature ferromagnetism in Zn{sub 1-x}Mn{sub x}O thin films and shows paramagnetism. XPS confirms the incorporation of Mn{sup 2+} into the ZnO lattice.

  5. Optoelectronic properties of doped hydrothermal ZnO thin films

    KAUST Repository

    Mughal, Asad J.

    2017-03-10

    Group III impurity doped ZnO thin films were deposited on MgAl2O3 substrates using a simple low temperature two-step deposition method involving atomic layer deposition and hydrothermal epitaxy. Films with varying concentrations of either Al, Ga, or In were evaluated for their optoelectronic properties. Inductively coupled plasma atomic emission spectroscopy was used to determine the concentration of dopants within the ZnO films. While Al and Ga-doped films showed linear incorporation rates with the addition of precursors salts in the hydrothermal growth solution, In-doped films were shown to saturate at relatively low concentrations. It was found that Ga-doped films showed the best performance in terms of electrical resistivity and optical absorbance when compared to those doped with In or Al, with a resistivity as low as 1.9 mΩ cm and an optical absorption coefficient of 441 cm−1 at 450 nm.

  6. Nanostructured Diamond-Like Carbon Films Grown by Off-Axis Pulsed Laser Deposition

    Directory of Open Access Journals (Sweden)

    Seong Shan Yap

    2015-01-01

    Full Text Available Nanostructured diamond-like carbon (DLC films instead of the ultrasmooth film were obtained by pulsed laser ablation of pyrolytic graphite. Deposition was performed at room temperature in vacuum with substrates placed at off-axis position. The configuration utilized high density plasma plume arriving at low effective angle for the formation of nanostructured DLC. Nanostructures with maximum size of 50 nm were deposited as compared to the ultrasmooth DLC films obtained in a conventional deposition. The Raman spectra of the films confirmed that the films were diamond-like/amorphous in nature. Although grown at an angle, ion energy of >35 eV was obtained at the off-axis position. This was proposed to be responsible for subplantation growth of sp3 hybridized carbon. The condensation of energetic clusters and oblique angle deposition correspondingly gave rise to the formation of nanostructured DLC in this study.

  7. Low-temperature magnetoresistance study of electrical transport in N- and B-doped ultrananocrystalline and nanocrystalline diamond films

    Czech Academy of Sciences Publication Activity Database

    Nesládek, M.; Tromson, D.; Bergonzo, P.; Hubík, Pavel; Mareš, Jiří J.; Krištofik, Jozef; Kindl, Dobroslav; Williams, O.A.; Gruen, D.

    2006-01-01

    Roč. 15, - (2006), s. 607-613 ISSN 0925-9635 R&D Projects: GA AV ČR(CZ) IAA1010404; GA ČR(CZ) GA202/06/0040 Institutional research plan: CEZ:AV0Z10100521 Keywords : U-NCD * NCD * doping * low-temperature doping * weak localisation Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 1.935, year: 2006

  8. Adhesion analysis of polycrystalline diamond films on molybdenum by means of scratch, indentation and sand abrasion testing

    Energy Technology Data Exchange (ETDEWEB)

    Buijnsters, J.G. [Applied Physics, IMM, Department of Applied Physics, Radboud University Nijmegen, Toernooiveld 1, 6525 ED Nijmegen (Netherlands); Shankar, P. [Metallurgy and Materials Group, Indira Gandhi Centre for Atomic Research, Kalpakkam-603 102 (India); Enckevort, W.J.P. van [Solid State Chemistry, IMM, Radboud University Nijmegen, Toernooiveld 1, 6525 ED Nijmegen (Netherlands); Schermer, J.J. [Experimental Solid State Physics III, IMM, Radboud University Nijmegen, Toernooiveld 1, 6525 ED Nijmegen (Netherlands); Meulen, J.J. ter [Applied Physics, IMM, Department of Applied Physics, Radboud University Nijmegen, Toernooiveld 1, 6525 ED Nijmegen (Netherlands)]. E-mail: htmeulen@sci.kun.nl

    2005-03-01

    Diamond films have been grown by hot-filament chemical vapour deposition (CVD) on molybdenum substrates under different growth conditions. The films grown with increasing substrate temperatures show a higher interconnection of diamond grains, whereas increasing methane concentrations in the 0.5-4.0% range lead to a transition from micro- towards nanocrystalline films. X-ray diffraction analysis shows Mo{sub 2}C interlayer formation. Indentation, scratch and sand erosion tests are used to evaluate the adhesion strength of the diamond films. Using steel ball indenters (diameter 750 {mu}m), indentation and scratch adhesion tests are performed up to final loads of 200 N. Upon indentation, the load values at which diamond film failure such as flaking and detachment is first observed, increase for increasing temperatures in the deposition temperature range of 450-850 deg C. The scratch adhesion tests show critical load values in the range of 16-40 N normal load for films grown for 4 h. In contrast, diamond films grown for 24 h at a methane concentration of 0.5% do not show any failure at all upon scratching up to 75 N. Film failure upon indenting and scratching is also found to decrease for increasing methane concentration in the CVD gas mixture. The sand abrasion tests show significant differences in coating failure for films grown at varying CH{sub 4}/H{sub 2} ratios. In contrast to the other tests, here best coating performance is observed for the films deposited with a methane concentration of 4%.

  9. On single doping and co-doping of spray pyrolysed ZnO films: Structural, electrical and optical characterisation

    International Nuclear Information System (INIS)

    Vimalkumar, T.V.; Poornima, N.; Jinesh, K.B.; Kartha, C. Sudha; Vijayakumar, K.P.

    2011-01-01

    In this paper we present studies on ZnO thin films (prepared using Chemical Spray pyrolysis (CSP) technique) doped in two different ways; in one set, 'single doping' using indium was done while in the second set, 'co-doping' using indium and fluorine was adopted. In the former case, effect of in-situ as well as ex-situ doping using In was analyzed. Structural (XRD studies), electrical (I-V measurements) and optical characterizations (through absorption, transmission and photoluminescence studies) of the films were done. XRD analysis showed that, for spray-deposited ZnO films, ex-situ doping using Indium resulted in preferred (0 0 2) plane orientation, while in-situ doping caused preferred orientation along (1 0 0), (0 0 2), (1 0 1) planes; however for higher percentage of in-situ doping, orientation of grains changed from (0 0 2) plane to (1 0 1) plane. The co-doped films had (0 0 2) and (1 0 1) planes. Lowest resistivity (2 x 10 -3 Ω cm) was achieved for the films, doped with 1% Indium through in-situ method. Photoluminescence (PL) emissions of ex-situ doped and co-doped samples had two peaks; one was the 'near band edge' emission (NBE) and the other was the 'blue-green' emission. But interestingly the PL emission of in-situ doped samples exhibited only the 'near band edge' emission. Optical band gap of the films increased with doping percentage, in all cases of doping.

  10. Structure and wettability property of the growth and nucleation surfaces of thermally treated freestanding CVD diamond films

    Science.gov (United States)

    Pei, Xiaoqiang; Cheng, Shaoheng; Ma, Yibo; Wu, Danfeng; Liu, Junsong; Wang, Qiliang; Yang, Yizhou; Li, Hongdong

    2015-08-01

    This paper reports the surface features and wettability properties of the (1 0 0)-textured freestanding chemical vapor deposited (CVD) diamond films after thermal exposure in air at high temperature. Thermal oxidation at proper conditions eliminates selectively nanodiamonds and non-diamond carbons in the films. The growth side of the films contains (1 0 0)-oriented micrometer-sized columns, while its nucleation side is formed of nano-sized tips. The examined wettability properties of the as-treated diamond films reveal a hydrophilicity and superhydrophilicity on the growth surface and nucleation surface, respectively, which is determined by oxygen termination and geometry structure of the surface. When the surface termination is hydrogenated, the wettability of nucleation side converted from superhydrophilicity to high hydrophobicity, while the hydrophilicity of the growth side does not change significantly. The findings open a possibility for realizing freestanding diamond films having not only novel surface structures but also multifunction applications, especially proposed on the selected growth side or nucleation side in one product.

  11. TL and LOE dosimetric evaluation of diamond films exposed to beta and ultraviolet radiation; Evaluacion dosimetrica TL y LOE de peliculas de diamante expuestas a radiacion beta y ultravioleta

    Energy Technology Data Exchange (ETDEWEB)

    Preciado F, S.; Melendrez, R.; Chernov, V.; Barboza F, M. [Universidad de Sonora, A.P. 13 y A.P. 5-088, 83000 Hermosillo, Sonora (Mexico); Schreck, M. [Universitaet Augsburg, Institut fuer Physik D-86135 (Germany); Cruz Z, E. [ICN, UNAM, 04500 Mexico D.F. (Mexico)

    2005-07-01

    The diamond possesses a privileged position regarding other materials of great technological importance. Their applications go from the optics, microelectronics, metals industry, medicine and of course as dosemeter, in the registration and detection of ionizing and non ionizing radiation. In this work the results of TL/LOE obtained in two samples of diamond of 10 {mu}m thickness grown by the chemical vapor deposition method (CVD) assisted by microwave plasma. The films were deposited in a silicon substrate (001) starting from a mixture of gases composed of CH{sub 4}/H{sub 2} and 750 ppm of molecular nitrogen as dopant. The samples were exposed to beta radiation (Sr{sup 90}/ Y{sup 90}) and ultraviolet, being stimulated later on thermal (TL) and optically (LOE) to evaluate their dosimetric properties. The sample without doping presented high response TL/LOE to the ultraviolet and beta radiation. The TL glow curve of the sample without doping showed two TL peaks with second order kinetics in the range of 520 to 550 K, besides a peak with first order kinetics of more intensity around 607 K. The TL efficiency of the non doped sample is bigger than the doped with nitrogen; however the LOE efficiency is similar in both samples. The results indicate that the CVD diamond possesses excellent perspectives for dosimetric applications, with special importance in radiotherapy due to it is biologically compatible with the human tissue. (Author)

  12. Insight into boron-doped diamond Raman spectra characteristic features

    Czech Academy of Sciences Publication Activity Database

    Mortet, Vincent; Vlčková Živcová, Zuzana; Taylor, Andrew; Frank, Otakar; Hubík, Pavel; Trémouilles, D.; Jomard, F.; Barjon, J.; Kavan, Ladislav

    2017-01-01

    Roč. 115, May (2017), s. 279-284 ISSN 0008-6223 R&D Projects: GA ČR GA13-31783S; GA MŠk 7AMB16FR004 Grant - others:AV ČR(CZ) Fellowship J. E. Purkyně Institutional support: RVO:68378271 ; RVO:61388955 Keywords : diamond * boron doping * Raman spectroscopy Subject RIV: BM - Solid Matter Physics ; Magnetism; CG - Electrochemistry (UFCH-W) OBOR OECD: Condensed matter physics (including formerly solid state physics, supercond.); Electrochemistry (dry cells, batteries, fuel cells, corrosion metals, electrolysis) (UFCH-W) Impact factor: 6.337, year: 2016

  13. Nanoparticles doped film sensing based on terahertz metamaterials

    Science.gov (United States)

    Liu, Weimin; Fan, Fei; Chang, Shengjiang; Hou, Jiaqing; Chen, Meng; Wang, Xianghui; Bai, Jinjun

    2017-12-01

    A nanoparticles concentration sensor based on doped film and terahertz (THz) metamaterial has been proposed. By coating the nanoparticles doped polyvinyl alcohol (PVA) film on the surface of THz metamaterial, the effects of nanoparticle concentration on the metamaterial resonances are investigated through experiments and numerical simulations. Results show that resonant frequency of the metamaterial linearly decreases with the increment of doping concentration. Furthermore, numerical simulations illustrate that the redshift of resonance results from the changes of refractive index of the doped film. The concentration sensitivity of this sensor is 3.12 GHz/0.1%, and the refractive index sensitivity reaches 53.33 GHz/RIU. This work provides a non-contact, nondestructive and sensitive method for the detection of nanoparticles concentration and brings out a new application on THz film metamaterial sensing.

  14. Adhesion enhancement of diamond-like carbon thin films on Ti alloys by incorporation of nanodiamond particles

    International Nuclear Information System (INIS)

    Zhang, C.Z.; Tang, Y.; Li, Y.S.; Yang, Q.

    2013-01-01

    Coating adherent diamond-like carbon (DLC) thin films directly on Ti alloys is technologically difficult. This research incorporates nanodiamond particles to form a diamond/DLC composite interlayer to enhance the adhesion of DLC thin films on Ti6Al4V substrates. Initially, nanodiamond particles were deposited on Ti6Al4V substrates by microwave plasma enhanced chemical vapor deposition from a methane–hydrogen gas mixture. A DLC thin film was then deposited, on top of the nanodiamond particles, by direct ion beam deposition. Scanning electron microscopy, Atomic force microscopy, X-ray Diffraction and Raman spectroscopy were used to characterize the microstructure and chemical bonding of the deposited particles and films, and Rockwell indentation testing was used to evaluate the adhesion of the deposited films. The results indicate that the pre-deposited nanodiamond particles significantly enhance the interfacial adhesion between the DLC thin film and the Ti6Al4V substrate, possibly by enhanced interfacial bonding, mechanical interlocking, and stress relief. - Highlights: ► Nanodiamond particles were deposited on Ti6Al4V before DLC deposition. ► Diamond/DLC composite film was formed by incorporation of nanodiamond particles. ► Greatly enhanced adhesion of diamond/DLC composite film on Ti6Al4V was achieved. ► Enhanced adhesion is by increased interfacial bonding and mechanical interlocking

  15. Adhesion enhancement of diamond-like carbon thin films on Ti alloys by incorporation of nanodiamond particles

    Energy Technology Data Exchange (ETDEWEB)

    Zhang, C.Z.; Tang, Y. [Department of Mechanical Engineering, University of Saskatchewan, 57 Campus Drive, Saskatoon, SK, Canada S7N 5A9 (Canada); Li, Y.S. [Plasma Physics Laboratory, University of Saskatchewan, 116 Science Place, Saskatoon, SK, Canada S7N 5E2 (Canada); Yang, Q., E-mail: qiaoqin.yang@usask.ca [Department of Mechanical Engineering, University of Saskatchewan, 57 Campus Drive, Saskatoon, SK, Canada S7N 5A9 (Canada)

    2013-01-01

    Coating adherent diamond-like carbon (DLC) thin films directly on Ti alloys is technologically difficult. This research incorporates nanodiamond particles to form a diamond/DLC composite interlayer to enhance the adhesion of DLC thin films on Ti6Al4V substrates. Initially, nanodiamond particles were deposited on Ti6Al4V substrates by microwave plasma enhanced chemical vapor deposition from a methane–hydrogen gas mixture. A DLC thin film was then deposited, on top of the nanodiamond particles, by direct ion beam deposition. Scanning electron microscopy, Atomic force microscopy, X-ray Diffraction and Raman spectroscopy were used to characterize the microstructure and chemical bonding of the deposited particles and films, and Rockwell indentation testing was used to evaluate the adhesion of the deposited films. The results indicate that the pre-deposited nanodiamond particles significantly enhance the interfacial adhesion between the DLC thin film and the Ti6Al4V substrate, possibly by enhanced interfacial bonding, mechanical interlocking, and stress relief. - Highlights: ► Nanodiamond particles were deposited on Ti6Al4V before DLC deposition. ► Diamond/DLC composite film was formed by incorporation of nanodiamond particles. ► Greatly enhanced adhesion of diamond/DLC composite film on Ti6Al4V was achieved. ► Enhanced adhesion is by increased interfacial bonding and mechanical interlocking.

  16. Visible-light sensitization of boron-doped nanocrystalline diamond through non-covalent surface modification

    Czech Academy of Sciences Publication Activity Database

    Krýsová, Hana; Vlčková Živcová, Zuzana; Bartoň, Jan; Petrák, Václav; Nesladek, M.; Cígler, Petr; Kavan, Ladislav

    2015-01-01

    Roč. 17, č. 2 (2015), s. 1165-1172 ISSN 1463-9076 R&D Projects: GA ČR GA13-31783S Institutional support: RVO:61388955 ; RVO:61388963 ; RVO:68378271 Keywords : nanocrystallines * visible-light sensitization * boron-doped diamond Subject RIV: CF - Physical ; Theoretical Chemistry Impact factor: 4.449, year: 2015

  17. Substrate effect on the room-temperature ferromagnetism in un-doped ZnO films

    Science.gov (United States)

    Zhan, Peng; Wang, Weipeng; Xie, Zheng; Li, Zhengcao; Zhang, Zhengjun; Zhang, Peng; Wang, Baoyi; Cao, Xingzhong

    2012-07-01

    Room-temperature ferromagnetism was achieved in un-doped ZnO films on silicon and quartz substrates. Photoluminescence measurement and positron annihilation analysis suggested that the ferromagnetism was originated from singly occupied oxygen vacancies (roughly estimated as ˜0.55 μB/vacancy), created in ZnO films by annealing in argon. The saturated magnetization of ZnO films was enhanced from ˜0.44 emu/g (on quartz) to ˜1.18 emu/g (on silicon) after annealing at 600 °C, as silicon acted as oxygen getter and created more oxygen vacancies in ZnO films. This study clarified the origin of ferromagnetism in un-doped ZnO and provides an idea to enhance the ferromagnetism.

  18. Dosimetric characterization of chemical-vapor-deposited diamond film irradiated with UV and beta radiation

    Science.gov (United States)

    Meléndrez, R.; Chernov, V.; Pedroza-Montero, M.; Barboza-Flores, M.

    2003-03-01

    Diamond is an excellent prospect for clinical radiation dosimetry due to its tissue-equivalence properties and being chemically inert. The use of diamond in radiation dosimetry has been halted by the high market price; although recently the capability of growing high quality polycrystalline has renewed the interest in using diamond films as detectors and dosimeters. In the present work we have characterized the dosimetric properties of diamond films synthesized by using chemical vapor deposition. The thermoluminescence (TL) of UV and beta exposed samples shows a glow curve composed of at least four peaks; one located around 587 K presents excellent TL properties suitable for dosimetric applications with ionizing and non ionizing radiation. The TL excitation spectrum exhibits maximum TL efficiency at 220 nm. The samples show regions of linear as well as supralinear behavior as a function or irradiation dose. The linear dose dependence was found for up to sixteen minutes of UV irradiation and 300 Gy for beta irradiated samples. The activation energy and the frequency factor were determined and found in the range of 0.32 - 0.89 eV and 1.1x10^2 - 2x10^8s_-1, respectively. The observed TL performance is reasonable appropriate to justify further investigation of diamond films as radiation dosimeters.

  19. Flexible diamond-like carbon film coated on rubber

    NARCIS (Netherlands)

    Pei, Y.T.; Bui, X.L.; Pal, J.P. van der; Martinez-Martinez, D.; Hosson, J.Th.M. De

    2013-01-01

    Dynamic rubber seals are major sources of friction of lubrication systems and bearings, which may take up to 70% of the total friction. The solution we present is to coat rubbers with diamond-like carbon (DLC) thin films by which the coefficient of friction is reduced to less than one tenth. Coating

  20. Adhesion analysis of polycrystalline diamond films on molybdenum by means of scratch, indentation and sand abrasion testing

    NARCIS (Netherlands)

    Buijnsters, J.G.; Shankar, P.; Enckevort, W.J.P. van; Schermer, J.J.; Meulen, J.J. ter

    2005-01-01

    Diamond films have been grown by hot-filament chemical vapour deposition (CVD) on molybdenum substrates under different growth conditions. The films grown with increasing substrate temperatures show a higher interconnection of diamond grains, whereas increasing methane concentrations in the 0.5-4.0%

  1. Thermoluminescence in CVD diamond films: application to actinometric dosimetry

    International Nuclear Information System (INIS)

    Barboza-Flores, M.; Melendrez, R.; Chernov, V.; Castaneda, B.; Pedroza-Montero, M.; Gan, B.; Ahn, J.; Zhang, Q.; Yoon, S.F.

    2002-01-01

    Diamond is considered a tissue-equivalent material since its atomic number (Z=6) is close to the effective atomic number of biological tissue (Z=7.42). Such a situation makes it suitable for radiation detection purposes in medical applications. In the present work the analysis is reported of the thermoluminescence (TL) and dosimetric features of chemically vapour deposited (CVD) diamond film samples subjected to ultraviolet (UV) irradiation in the actinometric region. The TL glow curve shows peaks at 120, 220, 320 and 370 deg. C. The 120 and 370 deg. C peaks are too weak and the first one fades away in a few seconds after exposure. The overall room temperature fading shows a 50% TL decay 30 min after exposure. The 320 deg. C glow peak is considered to be the most adequate for dosimetric applications due to its low fading and linear TL behaviour as a function of UV dose in the 180-260 nm range. The TL excitation spectrum presents a broad band with at least two overlapped components around 205 and 220 nm. The results indicate that the TL behaviour of CVD diamond film can be a good alternative to the currently available dosemeter and detector in the actinometric region as well as in clinical and medical applications. (author)

  2. Study of Ho-doped Bi{sub 2}Te{sub 3} topological insulator thin films

    Energy Technology Data Exchange (ETDEWEB)

    Harrison, S. E. [Department of Physics, Clarendon Laboratory, University of Oxford, Oxford OX1 3PU (United Kingdom); Department of Electrical Engineering, Stanford University, Stanford, California 94305 (United States); Collins-McIntyre, L. J.; Zhang, S. L.; Chen, Y. L.; Hesjedal, T., E-mail: Thorsten.Hesjedal@physics.ox.ac.uk [Department of Physics, Clarendon Laboratory, University of Oxford, Oxford OX1 3PU (United Kingdom); Baker, A. A. [Department of Physics, Clarendon Laboratory, University of Oxford, Oxford OX1 3PU (United Kingdom); Magnetic Spectroscopy Group, Diamond Light Source, Didcot OX11 0DE (United Kingdom); Figueroa, A. I.; Laan, G. van der [Magnetic Spectroscopy Group, Diamond Light Source, Didcot OX11 0DE (United Kingdom); Kellock, A. J.; Pushp, A.; Parkin, S. S. P. [IBM Almaden Research Center, 650 Harry Road, San Jose, California 95120 (United States); Harris, J. S. [Department of Electrical Engineering, Stanford University, Stanford, California 94305 (United States)

    2015-11-02

    Breaking time-reversal symmetry through magnetic doping of topological insulators has been identified as a key strategy for unlocking exotic physical states. Here, we report the growth of Bi{sub 2}Te{sub 3} thin films doped with the highest magnetic moment element Ho. Diffraction studies demonstrate high quality films for up to 21% Ho incorporation. Superconducting quantum interference device magnetometry reveals paramagnetism down to 2 K with an effective magnetic moment of ∼5 μ{sub B}/Ho. Angle-resolved photoemission spectroscopy shows that the topological surface state remains intact with Ho doping, consistent with the material's paramagnetic state. The large saturation moment achieved makes these films useful for incorporation into heterostructures, whereby magnetic order can be introduced via interfacial coupling.

  3. Enhanced flux-pinning in fluorine-free MOD YBCO films by chemical doping

    Energy Technology Data Exchange (ETDEWEB)

    Wang, W.T.; Pu, M.H.; Yang, Y. [Key Laboratory of Magnetic Levitation and Maglev Trains (Ministry of Education of China), Superconductivity R and D Center (SRDC), Mail Stop 165, Southwest Jiaotong University, Chengdu, Sichuan 610031 (China); Zhang, H. [Department of Physics, Peking University, Beijing 100871 (China); Cheng, C.H. [Superconductivity Research Group, School of Materials Science and Engineering, University of New South Wale, Sydney, 2052 NSW (Australia); Zhao, Y., E-mail: yzhao@swjtu.edu.c [Key Laboratory of Magnetic Levitation and Maglev Trains (Ministry of Education of China), Superconductivity R and D Center (SRDC), Mail Stop 165, Southwest Jiaotong University, Chengdu, Sichuan 610031 (China); Superconductivity Research Group, School of Materials Science and Engineering, University of New South Wale, Sydney, 2052 NSW (Australia)

    2010-11-01

    YBCO films without and with dilute cobalt and zinc doping were prepared on (0 0 l) LaAlO{sub 3} substrate by non-fluorine metal organic deposition method. Effects of dilute cobalt and zinc doping on biaxial texture, microstructure and flux-pinning properties of YBCO films were investigated. The surface density and smoothness of the doped YBCO films have been distinctly improved compared with that of the pure film. Dilute cobalt- and zinc-doped YBCO films exhibit significantly enhanced J{sub c} values in the magnetic field. The best result is achieved in the cobalt-doped YBCO film. At 77 K, J{sub c} values of cobalt-doped film are 1.7 and 5.4 times higher than that of pure film in 0.5 T and 1.5 T, respectively. These results strongly suggest that dilute cobalt and zinc doping is a promising way to increase the current carrying capability of YBCO films.

  4. Synthesis of diamonds in Fe–C systems using nitrogen and hydrogen co-doped impurities under HPHT

    International Nuclear Information System (INIS)

    Sun Shi-Shuai; Xu Zhi-Hui; Cui Wen; Jia Xiao-Peng; Ma Hong-An

    2017-01-01

    In this study, we investigate the effect of nitrogen and hydrogen impurities on colors, morphologies, impurity structures and synthesis conditions of diamond crystals in Fe–C systems with C 3 N 6 H 6 additives at pressures in the range 5.0–6.5 GPa and temperatures of 1400–1700 °C in detail. Our results reveal that the octahedron diamond nucleation in a Fe–C system is evidently inhibited by co-doped N–H elements, thereby resulting in the increase of minimum pressure and temperature of diamond synthesis by spontaneous nucleation. The octahedron diamond crystals synthesized from a pure Fe–C system are colorless, while they become green in the system with C 3 N 6 H 6 additive. The surface defects of diamond will deteriorate when the nitrogen and hydrogen atoms simultaneously incorporate in the diamond growth environment in the Fe–C system. We believe that this study will provide some important information and be beneficial for the deep understanding of the crystallization of diamonds from different component systems. (paper)

  5. Highly transparent and conducting boron doped zinc oxide films for window of Dye Sensitized Solar Cell applications

    Energy Technology Data Exchange (ETDEWEB)

    Kumar, Vinod, E-mail: vinod.phy@gmail.com [Materials Science Group, Inter University Accelerator Centre, Aruna Asaf Ali Marg, New Delhi 110067 (India); Department of Physics, Gurukula Kangri University, Haridwar 249404 (India); Singh, R.G. [Department of Electronic Science, Maharaja Agrasen College University of Delhi, New Delhi 110096 (India); Singh, Fouran [Materials Science Group, Inter University Accelerator Centre, Aruna Asaf Ali Marg, New Delhi 110067 (India); Purohit, L.P. [Department of Physics, Gurukula Kangri University, Haridwar 249404 (India)

    2012-12-15

    Highlights: Black-Right-Pointing-Pointer Synthesis of Boron doped ZnO (ZnO:B) films. Black-Right-Pointing-Pointer Minimum of resistivity is observed to be 7.9 Multiplication-Sign 10{sup -4} {Omega} cm. Black-Right-Pointing-Pointer Maximum transmittance {approx}91% for 450 Degree-Sign C annealed films. Black-Right-Pointing-Pointer Applicable for window materials in Dye Sensitized Solar Cell. - Abstract: Highly transparent and conducting boron doped zinc oxide (ZnO:B) films grown by sol-gel method are reported. The annealing temperature is varied from 350 to 550 Degree-Sign C and doping concentration of boron is kept fixed for 0.6 at.% for all the films. At low temperature the stress in the films is compressive, which becomes tensile for the films annealed at higher temperature. A minimum resistivity of 7.9 Multiplication-Sign 10{sup -4} {Omega} cm and maximum transmittance of {approx}91% are observed for the film annealed at 450 Degree-Sign C. This could be attributed to minimum stress of films, which is further evident by the evolution of A{sub 1} and defect related Raman modes without any shifting in its position. Such kind of highly transparent and conducting ZnO:B thin film could be used as window material in Dye Sensitized Solar Cell (DSSC).

  6. Low resistance polycrystalline diamond thin films deposited by hot ...

    Indian Academy of Sciences (India)

    Administrator

    silicon wafers using a hydrocarbon gas (CH4) highly diluted with H2 at low pressure in a hot filament chemi- cal vapour ... the laser spot was focused on the sample surface using a ... tative spectra of diamond thin films with a typical dia-.

  7. Diamond and Diamond-Like Materials as Hydrogen Isotope Barriers

    International Nuclear Information System (INIS)

    Foreman, L.R.; Barbero, R.S.; Carroll, D.W.; Archuleta, T.; Baker, J.; Devlin, D.; Duke, J.; Loemier, D.; Trukla, M.

    1999-01-01

    This is the final report of a two-year, Laboratory Directed Research and Development (LDRD) project at Los Alamos National Laboratory (LANL). The purpose of this project was to develop diamond and diamond-like thin-films as hydrogen isotope permeation barriers. Hydrogen embrittlement limits the life of boost systems which otherwise might be increased to 25 years with a successful non-reactive barrier. Applications in tritium processing such as bottle filling processes, tritium recovery processes, and target filling processes could benefit from an effective barrier. Diamond-like films used for low permeability shells for ICF and HEDP targets were also investigated. Unacceptable high permeabilities for hydrogen were obtained for plasma-CVD diamond-like-carbon films

  8. Electrochemical Incineration of Phenolic Compounds from the Hydrocarbon Industry Using Boron-Doped Diamond Electrodes

    Directory of Open Access Journals (Sweden)

    Alejandro Medel

    2012-01-01

    Full Text Available Electrochemical incineration using boron-doped diamond electrodes was applied to samples obtained from a refinery and compared to the photo-electro-Fenton process in order to selectively eliminate the phenol and phenolic compounds from a complex matrix. Due to the complex chemical composition of the sample, a pretreatment to the sample in order to isolate the phenolic compounds was applied. The effects of the pretreatment and of pH on the degradation of the phenolic compounds were evaluated. The results indicate that the use of a boron-doped diamond electrode in an electrochemical incineration process mineralizes 99.5% of the phenolic sample content. Working in acidic medium (pH = 1, and applying 2 A at 298 K under constant stirring for 2 hours, also results in the incineration of the reaction intermediates reflected by 97% removal of TOC. In contrast, the photo-electro-Fenton process results in 99.9% oxidation of phenolic compounds with only a 25.69% removal of TOC.

  9. VOx effectively doping CVD-graphene for transparent conductive films

    Science.gov (United States)

    Ji, Qinghua; Shi, Liangjing; Zhang, Qinghong; Wang, Weiqi; Zheng, Huifeng; Zhang, Yuzhi; Liu, Yangqiao; Sun, Jing

    2016-11-01

    Chemical vapor deposition(CVD)-synthesized graphene is potentially an alternative for tin-doped indium oxide (ITO) transparent conductive films (TCFs), however its sheet resistance is still too high to meet many demands. Vanadium oxide has been widely applied as smart window materials, however, no study has been reported to use it as dopant to improve the conductivity of graphene TCFs. In this study, we firstly reported that VOx doping can effectively lower the sheet resistance of CVD-graphene films while keeping its good optical properties, whose transmittance is as high as 86-90%. The optimized VOx-doped graphene exhibits a sheet resistance as low as 176 Ω/□, which decreases by 56% compared to the undoped graphene films. The doping process is convenient, stable, economical and easy to operate. What is more, VOx can effectively increase the work function(WF) of the film, making it more appropriate for use in solar cells. The evolution of the VOx species annealed at different temperatures below 400 °C has been detailed studied for the first time, based on which the doping mechanism is proposed. The prepared VOx doped graphene is expected to be a promising candidate for transparent conductive film purposes.

  10. Application of printed nanocrystalline diamond film for electron emission cathode

    International Nuclear Information System (INIS)

    Zhang Xiuxia; Wei Shuyi; Lei Chongmin; Wei Jie; Lu Bingheng; Ding Yucheng; Zhu Changchun

    2011-01-01

    The low-cost and large area screen-printed nano-diamond film (NDF) for electronic emission was fabricated. The edges and corners of nanocrystalline diamond are natural field-emitters. The nano-diamond paste for screen-printing was fabricated of mixing nano-graphite and other inorganic or organic vehicles. Through enough disperse in isopropyl alcohol by ultrasonic nano-diamond paste was screen-printed on the substrates to form NDF. SEM images showed that the surface morphology of NDF was improved, and the nano-diamond emitters were exposed from NDF through the special thermal-sintering technique and post-treatment process. The field emission characteristics of NDF were measured under all conditions with 10 -6 Pa pressure. The results indicated that the field emission stability and emission uniformity of NDF were improved through hydrogen plasma post-treatment process. The turn-on field decreased from 1.60 V/μm to 1.25 V/μm. The screen-printed NDF can be applied to the displays electronic emission cathode for low-cost outdoor in large area.

  11. X-ray magnetic spectroscopy of MBE-grown Mn-doped Bi2Se3 thin films

    Directory of Open Access Journals (Sweden)

    L. J. Collins-McIntyre

    2014-12-01

    Full Text Available We report the growth of Mn-doped Bi2Se3 thin films by molecular beam epitaxy (MBE, investigated by x-ray diffraction (XRD, atomic force microscopy (AFM, SQUID magnetometry and x-ray magnetic circular dichroism (XMCD. Epitaxial films were deposited on c-plane sapphire substrates by co-evaporation. The films exhibit a spiral growth mechanism typical of this material class, as revealed by AFM. The XRD measurements demonstrate a good crystalline structure which is retained upon doping up to ∼7.5 atomic-% Mn, determined by Rutherford backscattering spectrometry (RBS, and show no evidence of the formation of parasitic phases. However an increasing interstitial incorporation of Mn is observed with increasing doping concentration. A magnetic moment of 5.1 μB/Mn is obtained from bulk-sensitive SQUID measurements, and a much lower moment of 1.6 μB/Mn from surface-sensitive XMCD. At ∼2.5 K, XMCD at the Mn L2,3 edge, reveals short-range magnetic order in the films and indicates ferromagnetic order below 1.5 K.

  12. Guided assembly of nanoparticles on electrostatically charged nanocrystalline diamond thin films

    Directory of Open Access Journals (Sweden)

    Verveniotis Elisseos

    2011-01-01

    Full Text Available Abstract We apply atomic force microscope for local electrostatic charging of oxygen-terminated nanocrystalline diamond (NCD thin films deposited on silicon, to induce electrostatically driven self-assembly of colloidal alumina nanoparticles into micro-patterns. Considering possible capacitive, sp2 phase and spatial uniformity factors to charging, we employ films with sub-100 nm thickness and about 60% relative sp2 phase content, probe the spatial material uniformity by Raman and electron microscopy, and repeat experiments at various positions. We demonstrate that electrostatic potential contrast on the NCD films varies between 0.1 and 1.2 V and that the contrast of more than ±1 V (as detected by Kelvin force microscopy is able to induce self-assembly of the nanoparticles via coulombic and polarization forces. This opens prospects for applications of diamond and its unique set of properties in self-assembly of nano-devices and nano-systems.

  13. Optical modelling of photoluminescence emitted by thin doped films

    International Nuclear Information System (INIS)

    Pigeat, P.; Easwarakhanthan, T.; Briancon, J.L.; Rinnert, H.

    2011-01-01

    Photoluminescence (PL) spectra emitted by doped films are deformed owing to film thickness-dependent wave interference. This hampers knowing well their PL generating mechanisms as well as designing photonic devices with suitable geometries that improve their PL efficiency. We develop in this paper an energy model for PL emitted by doped films considering the interaction between the wavelength-differing incident standing and emitted waves, their energy transfer in-between, and the interferences undergone by both. The film optical constants are estimated fitting the model to the measured PL. This simple model has thus allowed us to interpret the evolution of PL emitted by Er-doped AlN films prepared on Si substrates by reactive magnetron sputtering. The shapes, the amplitudes, and the illusive sub-spectral features of the PL spectra depend essentially on the film thickness. The model further predicts high sensitivity for PL emitted by non-homogenously doped stacked-films to incident light wavelengths and film-thickness variations. This property has potential applications in tracking wavelength variations and in measuring physical quantities producing thickness variations. This model may be used to optimise PL efficiency of photonic devices through different film geometries and optical properties.

  14. Nanostructured titanium/diamond-like carbon multilayer films: deposition, characterization, and applications.

    Science.gov (United States)

    Dwivedi, Neeraj; Kumar, Sushil; Malik, Hitendra K

    2011-11-01

    Titanium/diamond-like carbon multilayer (TDML) films were deposited using a hybrid system combining radio frequency (RF)-sputtering and RF-plasma enhanced chemical vapor deposition (PECVD) techniques under a varied number of Ti/diamond-like carbon (DLC) bilayers from 1 to 4, at high base pressure of 1 × 10(-3) Torr. The multilayer approach was used to create unique structures such as nanospheres and nanorods in TDML films, which is confirmed by scanning electron microscopy (SEM) analysis and explained by a hypothetical model. Surface composition was evaluated by X-ray photoelectron spectroscopy (XPS), whereas energy dispersive X-ray analysis (EDAX) and time-of-flight secondary ion mass spectrometer (ToF-SIMS) measurements were performed to investigate the bulk composition. X-ray diffraction (XRD) was used to evaluate the phase and crystallinity of the deposited TDML films. Residual stress in these films was found to be significantly low. These TDML films were found to have excellent nanomechanical properties with maximum hardness of 41.2 GPa. In addition, various nanomechanical parameters were calculated and correlated with each other. Owing to metallic interfacial layer of Ti in multilayer films, the optical properties, electrical properties, and photoluminescence were improved significantly. Due to versatile nanomechanical properties and biocompatibility of DLC and DLC based films, these TDML films may also find applications in biomedical science.

  15. Low-Concentration Indium Doping in Solution-Processed Zinc Oxide Films for Thin-Film Transistors

    Directory of Open Access Journals (Sweden)

    Xue Zhang

    2017-07-01

    Full Text Available We investigated the influence of low-concentration indium (In doping on the chemical and structural properties of solution-processed zinc oxide (ZnO films and the electrical characteristics of bottom-gate/top-contact In-doped ZnO thin-film transistors (TFTs. The thermogravimetry and differential scanning calorimetry analysis results showed that thermal annealing at 400 °C for 40 min produces In-doped ZnO films. As the In content of ZnO films was increased from 1% to 9%, the metal-oxygen bonding increased from 5.56% to 71.33%, while the metal-hydroxyl bonding decreased from 72.03% to 9.63%. The X-ray diffraction peaks and field-emission scanning microscope images of the ZnO films with different In concentrations revealed a better crystalline quality and reduced grain size of the solution-processed ZnO thin films. The thickness of the In-doped ZnO films also increased when the In content was increased up to 5%; however, the thickness decreased on further increasing the In content. The field-effect mobility and on/off current ratio of In-doped ZnO TFTs were notably affected by any change in the In concentration. Considering the overall TFT performance, the optimal In doping concentration in the solution-processed ZnO semiconductor was determined to be 5% in this study. These results suggest that low-concentration In incorporation is crucial for modulating the morphological characteristics of solution-processed ZnO thin films and the TFT performance.

  16. Fabrication of boron-doped nanocrystalline diamond nanoflowers based on 3D Cu(OH)2 dendritic architectures

    International Nuclear Information System (INIS)

    Sim, Huijun; Hong, Sukin; Lee, Seungkoo; Lim, Daesoon; Jin, Juneon; Hwang, Sungwoo

    2012-01-01

    Hot-filament chemical vapor deposition (HFCVD) was used to prepare boron-doped nanocrystalline diamond (BDND) nanoflowers on a Cu substrate with a Cu(OH) 2 dendritic architecture that had been formed by using electrostatic self-assembly (ESA) method with nanodiamond particles. The formation of diamond nanoflowers is controlled by the reaction time between the Cu(OH) 2 nanoflowers and the polymeric linker for the electrostatic attachment of nanodiamonds and by the deposition time for CVD diamond growth with a high nucleation density. Through analysis by field emission scanning electron microscopy (FESEM) and Raman spectroscopy, the optimal conditions for the synthesis of BDND nanoflowers are determined, and a possible explanation is provided.

  17. Polycrystalline ZnO: B grown by LPCVD as TCO for thin film silicon solar cells

    International Nuclear Information System (INIS)

    Fay, Sylvie; Steinhauser, Jerome; Nicolay, Sylvain; Ballif, Christophe

    2010-01-01

    Conductive zinc oxide (ZnO) grown by low pressure chemical vapor deposition (LPCVD) technique possesses a rough surface that induces an efficient light scattering in thin film silicon (TF Si) solar cells, which makes this TCO an ideal candidate for contacting such devices. IMT-EPFL has developed an in-house LPCVD process for the deposition of nanotextured boron doped ZnO films used as rough TCO for TF Si solar cells. This paper is a general review and synthesis of the study of the electrical, optical and structural properties of the ZnO:B that has been performed at IMT-EPFL. The influence of the free carrier absorption and the grain size on the electrical and optical properties of LPCVD ZnO:B is discussed. Transport mechanisms at grain boundaries are studied. It is seen that high doping of the ZnO grains facilitates the tunnelling of the electrons through potential barriers that are located at the grain boundaries. Therefore, even if these potential barriers increase after an exposition of the film to a humid atmosphere, the heavily doped LPCVD ZnO:B layers show a remarkable stable conductivity. However, the introduction of diborane in the CVD reaction induces also a degradation of the intra-grain mobility and increases over-proportionally the optical absorption of the ZnO:B films. Hence, the necessity to finely tune the doping level of LPCVD ZnO:B films is highlighted. Finally, the next challenges to push further the optimization of LPCVD ZnO:B films for thin film silicon solar cells are discussed, as well as some remarkable record cell results achieved with LPCVD ZnO:B as front electrode.

  18. Elastic properties of ultrathin diamond/AlN membranes

    International Nuclear Information System (INIS)

    Zuerbig, V.; Hees, J.; Pletschen, W.; Sah, R.E.; Wolfer, M.; Kirste, L.; Heidrich, N.; Nebel, C.E.; Ambacher, O.; Lebedev, V.

    2014-01-01

    Nanocrystalline diamond- (NCD) and AlN-based ultrathin single layer and bilayer membranes are investigated towards their mechanical properties. It is shown that chemo-mechanical polishing and heavy boron doping of NCD thin films do not impact the elastic properties of NCD layers as revealed by negligible variations of the NCD Young's modulus (E). In addition, it is demonstrated that the combination of NCD elastic layer and AlN piezo-actuator is highly suitable for the fabrication of mechanically stable ultrathin membranes in comparison to AlN single layer membranes. The elastic parameters of NCD/AlN heterostructures are mainly determined by the outstanding high Young's modulus of NCD (E = 1019 ± 19 GPa). Such ultrathin unimorph membranes allow for fabrication of piezo-actuated AlN/NCD microlenses with tunable focus length. - Highlights: • Mechanical properties of nanocrystalline diamond (NCD) and AlN circular membranes • No influence of polishing of NCD thin films on the mechanical properties of NCD • No influence of heavy boron-doping on the mechanical properties of NCD • Demonstration of mechanically stable piezo-actuated NCD/AlN membranes • Reported performance of AlN/NCD microlenses with adjustable focus length

  19. Combined addition of nano diamond and nano SiO{sub 2}, an effective method to improve the in-field critical current density of MgB{sub 2} superconductor

    Energy Technology Data Exchange (ETDEWEB)

    Rahul, S.; Varghese, Neson; Vinod, K.; Devadas, K.M.; Thomas, Syju; Anees, P. [National Institute for Interdisciplinary Science and Technology (CSIR), Trivandrum 695019 (India); Chattopadhyay, M.K.; Roy, S.B. [Magnetic and Superconducting Materials Section, Raja Ramanna Centre for Advanced Technology, Indore 452013 (India); Syamaprasad, U., E-mail: syamcsir@gmail.com [National Institute for Interdisciplinary Science and Technology (CSIR), Trivandrum 695019 (India)

    2011-11-15

    Highlights: {yields} Both nano diamond and nano SiO{sub 2} caused significant modifications in the structural properties of pure MgB{sub 2} sample. {yields} Reduction in T{sub C} for the best codoped sample was approximately 2 K. {yields} The best codoped sample yielded a J{sub C}, an order of magnitude more than the undoped one at 5 K and 8 T. {yields} The enhanced flux pinning capability provided by the additives is responsible for the improved in-field J{sub C}. -- Abstract: MgB{sub 2} bulk samples added with nano SiO{sub 2} and/or nano diamond were prepared by powder-in-sealed-tube (PIST) method and the effects of addition on structural and superconducting properties were studied. X-ray diffraction (XRD) analysis revealed that the addition caused systematic reduction in 'a' lattice parameter due to the substitution of C atoms at B sites and the strain caused by reacted intragrain nano particles of Mg{sub 2}Si as evinced by transmission electron microscope image. Scanning electron microscopy images showed distinct microstructural variations with SiO{sub 2}/diamond addition. It was evident from DC magnetization measurements that the in-field critical current density [J{sub C}(H)] of doped samples did not fall drastically like the undoped sample. Among the doped samples the J{sub C}(H) of co-doped samples were significantly higher and the best co-doped sample yielded a J{sub C}, an order of magnitude more than the undoped one at 5 K and 8 T.

  20. Sandblasting induced stress release and enhanced adhesion strength of diamond films deposited on austenite stainless steel

    Science.gov (United States)

    Li, Xiao; Ye, Jiansong; Zhang, Hangcheng; Feng, Tao; Chen, Jianqing; Hu, Xiaojun

    2017-08-01

    We firstly used sandblasting to treat austenite stainless steel and then deposited a Cr/CrN interlayer by close field unbalanced magnetron sputtering on it. After that, diamond films were prepared on the interlayer. It is found that the sandblasting process induces phase transition from austenite to martensite in the surface region of the stainless steel, which decreases thermal stress in diamond films due to lower thermal expansion coefficient of martensite phase compared with that of austenite phase. The sandblasting also makes stainless steel's surface rough and the Cr/CrN interlayer film inherits the rough surface. This decreases the carburization extent of the interlayer, increases nucleation density and modifies the stress distribution. Due to lower residual stress and small extent of the interlayer's carburization, the diamond film on sandblast treated austenite stainless steel shows enhanced adhesion strength.

  1. Bias-enhanced post-treatment process for enhancing the electron field emission properties of ultrananocrystalline diamond films

    International Nuclear Information System (INIS)

    Saravanan, A.; Huang, B. R.; Sankaran, K. J.; Tai, N. H.; Dong, C. L.; Lin, I. N.

    2015-01-01

    The electron field emission (EFE) properties of ultrananocrystalline diamond films were markedly improved via the bias-enhanced plasma post-treatment (bep) process. The bep-process induced the formation of hybrid-granular structure of the diamond (bep-HiD) films with abundant nano-graphitic phase along the grain boundaries that increased the conductivity of the films. Moreover, the utilization of Au-interlayer can effectively suppress the formation of resistive amorphous-carbon (a-C) layer, thereby enhancing the transport of electrons crossing the diamond-to-Si interface. Therefore, bep-HiD/Au/Si films exhibit superior EFE properties with low turn-on field of E 0  = 2.6 V/μm and large EFE current density of J e  = 3.2 mA/cm 2 (at 5.3 V/μm)

  2. Highly sensitive electrochemical biosensor for bisphenol A detection based on a diazonium-functionalized boron-doped diamond electrode modified with a multi-walled carbon nanotube-tyrosinase hybrid film.

    Science.gov (United States)

    Zehani, Nedjla; Fortgang, Philippe; Saddek Lachgar, Mohamed; Baraket, Abdoullatif; Arab, Madjid; Dzyadevych, Sergei V; Kherrat, Rochdi; Jaffrezic-Renault, Nicole

    2015-12-15

    A highly sensitive electrochemical biosensor for the detection of Bisphenol A (BPA) in water has been developed by immobilizing tyrosinase onto a diazonium-functionalized boron doped diamond electrode (BDD) modified with multi-walled carbon nanotubes (MWCNTs). The fabricated biosensor exhibits excellent electroactivity towards o-quinone, a product of this enzymatic reaction of BPA oxidation catalyzed by tyrosinase. The developed BPA biosensor displays a large linear range from 0.01 nM to 100 nM, with a detection limit (LOD) of 10 pM. The feasibility of the proposed biosensor has been demonstrated on BPA spiked water river samples. Therefore, it could be a promising and reliable analytical tool for on-site monitoring of BPA in waste water. Copyright © 2015 Elsevier B.V. All rights reserved.

  3. Tribochemical interactions of Si-doped DLC film against steel in sliding contact

    International Nuclear Information System (INIS)

    Yoon, Eui Sung; Pham, Duc Cuong; Ahn, Hyo Sok; Oh, Jae Eung

    2007-01-01

    This study concerns the effects of tribochemical interactions at the interface of Si-DLC (silicon-doped diamond-like carbon) film and steel ball in sliding contact on tribological properties of the film. The Si-DLC film was over-coated on pure DLC coating by radio frequency plasma-assisted chemical vapor deposition (r.f. PACVD) with different Si concentration. Friction tests against steel ball using a reciprocating type tribotester were performed in ambient environment. X-Ray photoelectron spectroscopy (XPS) and auger electron spectroscopy (AES) were used to study the chemical characteristics and elemental composition of the films and mating balls after tests. Results showed a darkgray film consisting of carbon, oxygen and silicon on the worn steel ball surface with different thickness. On the contrary, such film was not observed on the surface of the ball slid against pure DLC coating. The oxidation of Si-DLC surface and steel ball was also found at particular regions of contact area. This demonstrates that tribochemical interactions occurred at the contact area of Si-DLC and steel ball during sliding to form a tribofilm (so called transfer film) on the ball specimen. While the pure DLC coating exhibited high coefficient of friction (∼0.06), the Si-DLC film showed a significant lower coefficient of friction (∼0.022) with the presence of tribofilm on mating ball surface. However, the Si-DLC film possesses a very high wear rate in comparison with the pure DLC. It was found that the tribochemical interactions strongly affected tribological properties of the Si-DLC film in sliding against steel

  4. Doping graphene films via chemically mediated charge transfer

    Directory of Open Access Journals (Sweden)

    Ishikawa Ryousuke

    2011-01-01

    Full Text Available Abstract Transparent conductive films (TCFs are critical components of a myriad of technologies including flat panel displays, light-emitting diodes, and solar cells. Graphene-based TCFs have attracted a lot of attention because of their high electrical conductivity, transparency, and low cost. Carrier doping of graphene would potentially improve the properties of graphene-based TCFs for practical industrial applications. However, controlling the carrier type and concentration of dopants in graphene films is challenging, especially for the synthesis of p-type films. In this article, a new method for doping graphene using the conjugated organic molecule, tetracyanoquinodimethane (TCNQ, is described. Notably, TCNQ is well known as a powerful electron accepter and is expected to favor electron transfer from graphene into TCNQ molecules, thereby leading to p-type doping of graphene films. Small amounts of TCNQ drastically improved the resistivity without degradation of optical transparency. Our carrier doping method based on charge transfer has a huge potential for graphene-based TCFs.

  5. Defect mediated reversible ferromagnetism in Co and Mn doped zinc oxide epitaxial films

    Energy Technology Data Exchange (ETDEWEB)

    Mal, Siddhartha; Nori, Sudhakar; Narayan, J. [Department of Material Science and Engineering, North Carolina State University, Raleigh, North Carolina 27695 (United States); Mula, Suhrit [Department of Material Science and Engineering, North Carolina State University, Raleigh, North Carolina 27695 (United States); Department of Metallurgical and Materials Engineering, National Institute of Technology, Rourkela 769008 (India); Prater, J. T. [Materials Science Division, Army Research Office, Research Triangle Park, North Carolina 27709 (United States)

    2012-12-01

    We have introduced defects in ZnO (undoped and doped with Co and Mn) epitaxial thin films using laser irradiation from nanosecond laser pulses and thermal annealing in oxygen ambient. In contrast to the as grown samples, the laser irradiated films show a significant increase in conductivity, enhancement in UV emission, while maintaining the same wurtzite crystal structure. Room-temperature ferromagnetism (RTFM) is observed in laser-irradiated samples, which increased with the number of laser pulses up to a certain value where magnetic moment saturates. The induced ferromagnetism as well as the enhanced electrical conductivity can be reversed with thermal annealing in oxygen ambient. The magnetization in Co and Mn doped films was found to be strong function of growth conditions and defect concentration. X-ray diffraction and optical absorption experiments suggested a 2+ valance state and tetrahedral coordination for both Co and Mn ions. There is a simultaneous increase in n-type electrical conductivity with the number of laser pulses and continue to exhibit semiconducting behavior in both undoped and doped films. The saturation magnetization was found to be 0.08 {mu}{sub B}/Co and 0.05 {mu}{sub B}/Mn, much lower than 3.0 {mu}{sub B}/Co and 5.0 {mu}{sub B}/Mn, indicating the prominent role of intrinsic defects in RTFM with some contribution from Co{sup 2+}-oxygen vacancy complexes. We propose a unified mechanism based upon introduction of intrinsic defects to explain RTFM and n-type conductivity enhancements during pulsed laser and thermal annealing.

  6. Simulation optimization of filament parameters for uniform depositions of diamond films on surfaces of ultra-large circular holes

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Xinchang, E-mail: wangxinchangz@163.com; Shen, Xiaotian; Sun, Fanghong; Shen, Bin

    2016-12-01

    Highlights: • A verified simulation model using a novel filament arrangement is constructed. • Influences of filament parameters are clarified. • A coefficient between simulated and experimental results is proposed. • Orthogonal simulations are adopted to optimize filament parameters. • A general filament arrangement suitable for different conditions is determined. - Abstract: Chemical vapor deposition (CVD) diamond films have been widely applied as protective coatings on varieties of anti-frictional and wear-resistant components, owing to their excellent mechanical and tribological properties close to the natural diamond. In applications of some components, the inner hole surface will serve as the working surface that suffers severe frictional or erosive wear. It is difficult to realize uniform depositions of diamond films on surfaces of inner holes, especially ultra-large inner holes. Adopting a SiC compact die with an aperture of 80 mm as an example, a novel filament arrangement with a certain number of filaments evenly distributed on a circle is designed, and specific effects of filament parameters, including the filament number, arrangement direction, filament temperature, filament diameter, circumradius and the downward translation, on the substrate temperature distribution are studied by computational fluid dynamics (CFD) simulations based on the finite volume method (FVM), adopting a modified computational model well consistent with the actual deposition environment. Corresponding temperature measurement experiments are also conducted to verify the rationality of the computational model. From the aspect of depositing uniform boron-doped micro-crystalline, undoped micro-crystalline and undoped fine-grained composite diamond (BDM-UMC-UFGCD) film on such the inner hole surface, filament parameters as mentioned above are accurately optimized and compensated by orthogonal simulations. Moreover, deposition experiments adopting compensated optimized

  7. Studies of internal stress in diamond films prepared by DC plasma chemical vapour deposition

    International Nuclear Information System (INIS)

    Wang Wanlu; Gao Jinying; Liao Kejun; Liu Anmin

    1992-01-01

    The internal stress in diamond thin films deposited by DC plasma CVD was studied as a function of methane concentration and deposited temperature. Experimental results have shown that total stress in diamond thin films is sensitive to the deposition conditions. The results also indicate that the compressive stress can be explained in terms of amorphous state carbon and hydrogen, and tensile stress is ascribed to the grain boundary relaxation model due to high internal surface area and microstructure with voids

  8. Plasma CVD reactor with two-microwave oscillators for diamond film synthesis

    International Nuclear Information System (INIS)

    Nagatsu, M.; Miyake, M.; Maeda, J.

    2006-01-01

    In this study, we present the experimental results of a new type of microwave plasma CVD system, where two of 1.5 kW microwave sources were used for enlarging the plasma discharge and the diamond film growth. One of the microwave oscillators was used to produce the microwave plasma as in the conventional microwave plasma CVD device, while the second one was used to enlarge the plasma by introducing microwave from the launcher mounted at the substrate stage. We demonstrated the enlargement of plasma discharge area from 60 mm to 100 mm in diameter by using the two-microwave oscillators system. Characteristics of diamond films deposited using H 2 /CH 4 plasmas were also investigated using a scanning electron microscope (SEM) and Raman spectroscopy

  9. Characteristics of ZnO/diamond thin films prepared by RF magnetron sputtering

    CERN Document Server

    Park, Y W; Lee, J G; Baik, Y J; Kim, H J; Jung, H J; Choi, W K; Cho, B H; Park, C Y

    1999-01-01

    Due to its high Young's modulus, diamond has the highest acoustic wave velocity among all materials and is expected to be a candidate substrate for high-frequency surface acoustic wave(SAW) devices. In this study, the deposition of ZnO, as a piezoelectric layer, on a diamond substrate is investigated. ZnO has been fabricated by using RF magnetron sputtering with a ZnO target and various Ar/O sub 2 gas ratios, RF powers, and substrate temperatures at a vacuum of 10 sup - sup 5 Torr. The sputtered ZnO films are characterized by X-ray diffraction (XRD), Rutherford backscattering spectroscopy (RBS), X-ray photoelectron spectroscopy (XPS), and I-V characteristics. All the films show only a (002) orientation. The atomic concentration of the sputtered ZnO films is changed by the oxygen gas ratio, and the ZnO films are grown with a homogeneous composition over their entire thickness. The electrical resistivity of the films varied from 4x10 sup 3 to 7x10 sup 8 OMEGA cm, depending on the Ar/O sub 2 gas ratio. The phase...

  10. Functionalization of nanocrystalline diamond films with phthalocyanines

    Energy Technology Data Exchange (ETDEWEB)

    Petkov, Christo [Institute of Nanostructure Technologies and Analytics (INA), Center for Interdisciplinary Nanostructure Science and Technology (CINSaT), University of Kassel (Germany); Reintanz, Philipp M. [Institute of Chemistry, Center for Interdisciplinary Nanostructure Science and Technology (CINSaT), University of Kassel (Germany); Kulisch, Wilhelm [Institute of Nanostructure Technologies and Analytics (INA), Center for Interdisciplinary Nanostructure Science and Technology (CINSaT), University of Kassel (Germany); Degenhardt, Anna Katharina [Institute of Chemistry, Center for Interdisciplinary Nanostructure Science and Technology (CINSaT), University of Kassel (Germany); Weidner, Tobias [Max Planck Institute for Polymer Research, Mainz (Germany); Baio, Joe E. [School of Chemical, Biological and Environmental Engineering, Oregon State University, Corvallis, OR (United States); Merz, Rolf; Kopnarski, Michael [Institut für Oberflächen- und Schichtanalytik (IFOS), Kaiserslautern (Germany); Siemeling, Ulrich [Institute of Chemistry, Center for Interdisciplinary Nanostructure Science and Technology (CINSaT), University of Kassel (Germany); Reithmaier, Johann Peter [Institute of Nanostructure Technologies and Analytics (INA), Center for Interdisciplinary Nanostructure Science and Technology (CINSaT), University of Kassel (Germany); Popov, Cyril, E-mail: popov@ina.uni-kassel.de [Institute of Nanostructure Technologies and Analytics (INA), Center for Interdisciplinary Nanostructure Science and Technology (CINSaT), University of Kassel (Germany)

    2016-08-30

    Highlights: • Grafting of phthalocyanines on nanocrystalline diamond films with different terminations. • Pc with different central atoms and side chains synthesized and characterized. • Attachment of Pc on H- and O-terminated NCD studied by XPS and NEXAFS spectroscopy. • Orientation order of phthalocyanine molecules on NCD surface. - Abstract: Phthalocyanine (Pc) derivatives containing different central metal atoms (Mn, Cu, Ti) and different peripheral chains were synthesized and comprehensively characterized. Their interaction with nanocrystalline diamond (NCD) films, as-grown by hot-filament chemical vapor deposition or after their modification with oxygen plasma to exchange the hydrogen termination with oxygen-containing groups, was studied by X-ray photoelectron spectroscopy (XPS) and near-edge X-ray absorption fine structure (NEXAFS) spectroscopy. The elemental composition as determined by XPS showed that the Pc were grafted on both as-grown and O-terminated NCD. Mn, Cu and Ti were detected together with N stemming from the Pc ring and S in case of the Ti-Pc from the peripheral ligands. The results for the elemental surface composition and the detailed study of the N 1s, S 2p and O 1s core spectra revealed that Ti-Pc grafted better on as-grown NCD but Cu-Pc and Mn-Pc on O-terminated films. Samples of Mn-Pc on as-grown and O-terminated NCD were further investigated by NEXAFS spectroscopy. The results showed ordering of the grafted molecules, laying flat on the H-terminated NCD surface while only the macrocycles were oriented parallel to the O-terminated surface with the peripheral chains perpendicular to it.

  11. A 3D tomographic EBSD analysis of a CVD diamond thin film

    International Nuclear Information System (INIS)

    Liu Tao; Raabe, Dierk; Zaefferer, Stefan

    2008-01-01

    We have studied the nucleation and growth processes in a chemical vapor deposition (CVD) diamond film using a tomographic electron backscattering diffraction method (3D EBSD). The approach is based on the combination of a focused ion beam (FIB) unit for serial sectioning in conjunction with high-resolution EBSD. Individual diamond grains were investigated in 3-dimensions particularly with regard to the role of twinning.

  12. Pure and Sn-doped ZnO films produced by pulsed laser deposition

    DEFF Research Database (Denmark)

    Holmelund, E.; Schou, Jørgen; Tougaard, S.

    2002-01-01

    A new technique, metronome doping, has been used for doping of films during pulsed laser deposition (PLD). This technique makes it possible to dope continuously during film growth with different concentrations of a dopant in one deposition sequence. Films of pure and doped ZnO have been produced...

  13. Simultaneous detection of iodine and iodide on boron doped diamond electrodes.

    Science.gov (United States)

    Fierro, Stéphane; Comninellis, Christos; Einaga, Yasuaki

    2013-01-15

    Individual and simultaneous electrochemical detection of iodide and iodine has been performed via cyclic voltammetry on boron doped diamond (BDD) electrodes in a 1M NaClO(4) (pH 8) solution, representative of typical environmental water conditions. It is feasible to compute accurate calibration curve for both compounds using cyclic voltammetry measurements by determining the peak current intensities as a function of the concentration. A lower detection limit of about 20 μM was obtained for iodide and 10 μM for iodine. Based on the comparison between the peak current intensities reported during the oxidation of KI, it is probable that iodide (I(-)) is first oxidized in a single step to yield iodine (I(2)). The latter is further oxidized to obtain IO(3)(-). This technique, however, did not allow for a reasonably accurate detection of iodate (IO(3)(-)) on a BDD electrode. Copyright © 2012 Elsevier B.V. All rights reserved.

  14. Thermoluminescent behavior of diamond thin films exposed to ultraviolet radiation

    International Nuclear Information System (INIS)

    Barboza F, M.; Gastelum, S.; Melendrez, R.; Chernov, V.; Bernal, R.; Cruz V, C.; Brown, F.

    2002-01-01

    In this work the thermoluminescent properties of diamond thin films are discussed which are grown up through the chemical vapor method exposed to ultraviolet radiation of 200-280 nm. The films with thickness 3, 6, 9, 12, 180 and 500 microns were grown up using a precursor gas formed of H 2 -CH 4 -CO excited through microwave energy or hot filament.The structure and morphology of the films were examined through scanning electron microscopy, indicating the formation of different diamond polycrystal structures which depend on the type of heating of the precursor gas used as well as the film dimensions. In general, the brilliance curve depends on the sample and the wavelength of the irradiation ultraviolet light, however it presents clearly thermoluminescence bands in 148, 160, 272, 304, 320 and 324 C degrees. The maximum of the thermoluminescence efficiency is obtained for the case of sample exposure with light of 214 nm. The sample of 500 microns is what exhibits greater thermoluminescent efficiency of those studied samples. The thermoluminescent behavior in function of radiation dose presents regions of linearity and supra linearity for higher and small doses respectively. The disappearance of the thermoluminescent signal depends on the characteristics of the film and it can reach until a 30 % of loss before to reach the stability. (Author)

  15. Nitrogen doping for adhesion improvement of DLC film deposited on Si substrate by Filtered Cathodic Vacuum Arc (FCVA) technique

    Energy Technology Data Exchange (ETDEWEB)

    Bootkul, D., E-mail: mo_duangkhae@hotmail.com [Department of General Science, Faculty of Science, Srinakharinwirot University, Bangkok 10110 (Thailand); Supsermpol, B.; Saenphinit, N. [Western Digital Company, Ayutthaya 13160 (Thailand); Aramwit, C. [Plasma and Beam Physics Research Facility, Department of Physics and Materials Science, Faculty of Science, Chiang Mai University, Chiang Mai 50202 (Thailand); Intarasiri, S., E-mail: saweat@gmail.com [Science and Technology Research Institute, Chiang Mai University, Chiang Mai 50202 (Thailand)

    2014-08-15

    Diamond-like carbon (DLC) films have been used in many applications due to their attractive combination of properties including chemical inertness, corrosion protection, biocompatibility, high hardness, and low wear rates. However, they still have some limitations such as high internal stresses and low toughness which lead to poor adhesion of films. Synthesis of nitrogen-doped DLC (N-DLC) offers the possibility of overcoming these limitations. In this study, DLC films, namely tetrahedral amorphous carbon (ta-C) and nitrogen doped tetrahedral amorphous carbon (ta-C:N) were deposited on single crystalline Si wafer substrates using the Filtered Cathodic Vacuum Arc (FCVA) technique. Film characterizations were carried out by Raman spectroscopy, atomic force microscopy (AFM), scanning electron microscopy (SEM), triboindenter tester and nano-scratch tester. Measurement results showed that intentionally doping with nitrogen reduced the carbon sp{sup 3} content and increased the surface roughness in comparison with that of pure ta-C films. The hardness measurement confirmed the Raman and AFM analyses that adding nitrogen in ta-C films decreased the hardness, especially with high nitrogen content. However, the nano-scratch test revealed the increasing of the critical load with nitrogen. This work, then, extended its scope to investigate the properties of double-layer ta-C films which were composed of ta-C:N interlayer of various thickness around 10–30 nm and ta-C top-layer with thickness of around 80 nm. Microstructure characterization demonstrated that a ta-C:N interlayer gradually decreased the sp{sup 3} fraction in the films and increased film roughness whenever the ta-C:N interlayer thickness increased. In this structure, the tribological property in terms of adhesion to the Si substrate was significantly improved by about 20–90%, but the mechanical property in terms of hardness was gradually degraded by about 2–10%, compared to pure ta-C film, when the ta

  16. Hybrid laser technology and doped biomaterials

    Science.gov (United States)

    Jelínek, Miroslav; Zemek, Josef; Remsa, Jan; Mikšovský, Jan; Kocourek, Tomáš; Písařík, Petr; Trávníčková, Martina; Filová, Elena; Bačáková, Lucie

    2017-09-01

    Hybrid laser-based technologies for deposition of new types of doped thin films are presented. The focus is on arrangements combining pulsed laser deposition (PLD) with magnetron sputtering (MS), and on the setup with two simultaneously running PLD systems (dual PLD). Advantages and disadvantages of both arrangements are discussed. Layers of different dopants concentration were prepared. Experience with deposition of chromium and titanium doped diamond-like carbon (DLC) films for potential coating of bone implants is presented. Properties of the layers prepared by both technologies are compared and discussed. The suitability of the layers for colonization with human bone marrow mesenchymal stem cells and human osteoblast-like cells, were also evaluated under in vitro conditions.

  17. Optical and mechanical properties of diamond like carbon films ...

    Indian Academy of Sciences (India)

    Diamond like carbon (DLC) films were deposited on Si (111) substrates by microwave electron cyclotron resonance (ECR) plasma chemical vapour deposition (CVD) process using plasma of argon and methane gases. During deposition, a d.c. self-bias was applied to the substrates by application of 13.56 MHz rf power.

  18. Electrochemical Behavior of TiO2 Nanoparticle Doped WO3 Thin Films

    Directory of Open Access Journals (Sweden)

    Suvarna R. Bathe

    2014-01-01

    Full Text Available Nanoparticle TiO2 doped WO3 thin films by pulsed spray pyrolysis technique have been studied on fluorine tin doped (FTO and glass substrate. XRD shows amorphous nature for undoped and anatase phase of TiO2 having (101 plane for nanoparticle TiO2 doped WO3 thin film. SEM shows microfibrous reticulated porous network for WO3 with 600 nm fiber diameter and nanocrystalline having size 40 nm for TiO2 nanoparticle doped WO3 thin film. TiO2 nanoparticle doped WO3 thin film shows ~95% reversibility due to may be attributed to nanocrystalline nature of the film, which helpful for charge insertion and deinsertion process. The diffusion coefficient for TiO2 nanoparticle doped WO3 film is less than undoped WO3.

  19. n-Type phosphorus-doped nanocrystalline diamond: electrochemical and in situ Raman spectroelectrochemical study

    Czech Academy of Sciences Publication Activity Database

    Vlčková Živcová, Zuzana; Frank, Otakar; Drijkoningen, S.; Haenen, K.; Mortet, Vincent; Kavan, Ladislav

    2016-01-01

    Roč. 6, č. 56 (2016), s. 51387-51393 ISSN 2046-2069 R&D Projects: GA ČR GA13-31783S Grant - others:AV ČR(CZ) G.0456.1 Institutional support: RVO:61388955 ; RVO:68378271 Keywords : Amorphous films * Cyclic voltammetry * Diamond films Subject RIV: CG - Electrochemistry; BM - Solid Matter Physics ; Magnetism (FZU-D) Impact factor: 3.108, year: 2016

  20. Fabrication and characterization of polyvinyl alcohol/metal (Ca, Mg, Ti) doped zirconium phosphate nanocomposite films for scaffold-guided tissue engineering application.

    Science.gov (United States)

    Kalita, Himani; Pal, Pallabi; Dhara, Santanu; Pathak, Amita

    2017-02-01

    Nanocomposite films of polyvinyl alcohol (PVA) and zirconium phosphate (ZrP)/doped ZrP (doped with Ca, Mg, Ti) nanoparticles have been developed by solvent casting method to assess their potential as matrix material in scaffold-guided tissue engineering application. The prepared ZrP and doped ZrP nanoparticles as well as the nanocomposite films were characterized by various spectroscopic and microscopic techniques. Nanoindentation studies revealed improved nanomechanical properties in the PVA/doped ZrP nanocomposite films (highest for PVA/Ti doped ZrP: hardness=262.4MPa; elastic modulus=5800MPa) as compared to the PVA/ZrP and neat PVA films. In-vitro cell culture experiments carried out to access the cellular viability, attachment, proliferation, and migration on the substrates, using mouse fibroblast (3T3) cell lines, inferred enhanced bioactivity in the PVA/doped ZrP nanocomposite films (highest for PVA/Ca doped ZrP) in contrast to PVA/ZrP and neat PVA films. Controlled biodegradability as well as swelling behavior, superior bioactivity and improved mechanical properties of the PVA/doped ZrP nanocomposite films make them promising matrix materials for scaffold-guided tissue engineering application. Copyright © 2016 Elsevier B.V. All rights reserved.

  1. A 3D tomographic EBSD analysis of a CVD diamond thin film

    Directory of Open Access Journals (Sweden)

    Tao Liu, Dierk Raabe and Stefan Zaefferer

    2008-01-01

    Full Text Available We have studied the nucleation and growth processes in a chemical vapor deposition (CVD diamond film using a tomographic electron backscattering diffraction method (3D EBSD. The approach is based on the combination of a focused ion beam (FIB unit for serial sectioning in conjunction with high-resolution EBSD. Individual diamond grains were investigated in 3-dimensions particularly with regard to the role of twinning.

  2. Surface plasmon effect in electrodeposited diamond-like carbon films for photovoltaic application

    Science.gov (United States)

    Ghosh, B.; Ray, Sekhar C.; Espinoza-González, Rodrigo; Villarroel, Roberto; Hevia, Samuel A.; Alvarez-Vega, Pedro

    2018-04-01

    Diamond-like carbon (DLC) films and nanocrystalline silver particles containing diamond-like carbon (DLC:Ag) films were electrodeposited on n-type silicon substrate (n-Si) to prepare n-Si/DLC and n-Si/DLC:Ag heterostructures for photovoltaic (PV) applications. Surface plasmon resonance (SPR) effect in this cell structure and its overall performance have been studied in terms of morphology, optical absorption, current-voltage characteristics, capacitance-voltage characteristics, band diagram and external quantum efficiency measurements. Localized surface plasmon resonance effect of silver nanoparticles (Ag NPs) in n-Si/DLC:Ag PV structure exhibited an enhancement of ∼28% in short circuit current density (JSC), which improved the overall efficiency of the heterostructures.

  3. Morphology and thermal stability of Ti-doped copper nitride films

    International Nuclear Information System (INIS)

    Fan Xiaoyan; Wu Zhiguo; Li Huajun; Geng Baisong; Li Chun; Yan Pengxun

    2007-01-01

    A weakly Ti-doped copper nitride (Cu 3 N) film was prepared by cylindrical magnetron sputtering. The XPS results indicate that Ti atoms do not substitute for the Cu atoms but probably locate at the grain boundaries. The columnar grains size is about half of that of the undoped Cu 3 N film and the surface is smoother. For weakly Ti-doped Cu 3 N films, a dense layer appears on top of the columnar crystals. The RMS of the Cu film formed by annealing of the weakly Ti-doped Cu 3 N film is more than twice larger than that of the film before annealing. Compared with the undoped Cu 3 N film, it possesses fine thermal stability both in vacuum and in atmosphere

  4. Growth, microstructure, and field-emission properties of synthesized diamond film on adamantane-coated silicon substrate by microwave plasma chemical vapor deposition

    International Nuclear Information System (INIS)

    Tiwari, Rajanish N.; Chang Li

    2010-01-01

    Diamond nucleation on unscratched Si surface is great importance for its growth, and detailed understanding of this process is therefore desired for many applications. The pretreatment of the substrate surface may influence the initial growth period. In this study, diamond films have been synthesized on adamantane-coated crystalline silicon {100} substrate by microwave plasma chemical vapor deposition from a gaseous mixture of methane and hydrogen gases without the application of a bias voltage to the substrates. Prior to adamantane coating, the Si substrates were not pretreated such as abraded/scratched. The substrate temperature was ∼530 deg. C during diamond deposition. The deposited films are characterized by scanning electron microscopy, Raman spectrometry, x-ray diffraction, and x-ray photoelectron spectroscopy. These measurements provide definitive evidence for high-crystalline quality diamond film, which is synthesized on a SiC rather than clean Si substrate. Characterization through atomic force microscope allows establishing fine quality criteria of the film according to the grain size of nanodiamond along with SiC. The diamond films exhibit a low-threshold (55 V/μm) and high current-density (1.6 mA/cm 2 ) field-emission (FE) display. The possible mechanism of formation of diamond films and their FE properties have been demonstrated.

  5. Conductive Langmuir-Blodgett films. Doping with iodine or self-doping?

    International Nuclear Information System (INIS)

    Bourgoin, Jean-Philippe

    1991-01-01

    In this research thesis dealing with molecular architecture, the author reports the testing of two strategies aiming at reducing the importance of defects in conductive Langmuir-Blodgett films, and at enabling the production of conductive mono-molecular layer. According to the first strategy, conductive films are obtained after doping based on the use of iodine vapours of an insulating precursor film of molecules derived from BEDT-TTF. The so-produced films display a high conductivity and can be used as sensitive elements in gas sensors, but remain macroscopically insulating, probably because molecular reorganisation, as shown by a study based on different techniques (IR and UV linear dichroism, Raman spectroscopy, X ray diffraction), generates too many defects. The second strategy, self-doping, is based on a mixing of two derivatives of the same electro-active nucleus (the TCNQ, tetracyanoquinodimethane), an amphiphilic one and a semi-amphiphilic one. This strategy opens new perspectives in molecular engineering as it is a general way to produce conductive LB films from TCNQ [fr

  6. Electrical transport characterization of Al and Sn doped Mg 2 Si thin films

    KAUST Repository

    Zhang, Bo

    2017-05-22

    Thin-film Mg2Si was deposited using radio frequency (RF) magnetron sputtering. Al and Sn were incorporated as n-type dopants using co-sputtering to tune the thin-film electrical properties. X-ray diffraction (XRD) analysis confirmed that the deposited films are polycrystalline Mg2Si. The Sn and Al doping concentrations were measured using Rutherford backscattering spectroscopy (RBS) and energy dispersive X-ray spectroscopy (EDS). The charge carrier concentration and the charge carrier type of the Mg2Si films were measured using a Hall bar structure. Hall measurements show that as the doping concentration increases, the carrier concentration of the Al-doped films increases, whereas the carrier concentration of the Sn-doped films decreases. Combined with the resistivity measurements, the mobility of the Al-doped Mg2Si films is found to decrease with increasing doping concentration, whereas the mobility of the Sn-doped Mg2Si films is found to increase.

  7. Evaluation of the adhesion strength of diamond films brazed on K-10 type hard metal

    Directory of Open Access Journals (Sweden)

    Santos Sérgio Ivan dos

    2004-01-01

    Full Text Available The coating of cutting tools with diamond films considerably increases the tool performance due to the combination of the unique tribological properties of diamond with the bulk properties of the substrate (toughness. The tool performance, however, is strongly related to the adhesion strength between the film and the substrate. In this work our main goal was to propose and to test a procedure, based on a tensile strength test, to evaluate the adhesion strength of a diamond wafer brazed on a hard metal substrate, taking into account the effect of the brazing temperature and time. The temperature range studied was from 800 to 980 °C and the brazing time ranged from 3 to 40 min. The obtained results could be used to optimize the costs and time required to the production of high performance cutting tools with brazed diamond wafers.

  8. Electrochemical impedance spectroscopy of polycrystalline boron doped diamond layers with hydrogen and oxygen terminated surface

    Czech Academy of Sciences Publication Activity Database

    Vlčková Živcová, Zuzana; Petrák, Václav; Frank, Otakar; Kavan, Ladislav

    2015-01-01

    Roč. 55, MAY 2015 (2015), s. 70-76 ISSN 0925-9635 R&D Projects: GA ČR GA13-31783S Institutional support: RVO:61388955 ; RVO:68378271 Keywords : Boron doped diamond * Electrochemical impedance spectroscopy * Aqueous electrolyte solution Subject RIV: CG - Electrochemistry Impact factor: 2.125, year: 2015

  9. Optical properties of diamond like carbon nanocomposite thin films

    Science.gov (United States)

    Alam, Md Shahbaz; Mukherjee, Nillohit; Ahmed, Sk. Faruque

    2018-05-01

    The optical properties of silicon incorporated diamond like carbon (Si-DLC) nanocomposite thin films have been reported. The Si-DLC nanocomposite thin film deposited on glass and silicon substrate by radio frequency plasma enhanced chemical vapor deposition (RF-PECVD) process. Fourier transformed infrared spectroscopic analysis revealed the presence of different bonding within the deposited films and deconvolution of FTIR spectra gives the chemical composition i.e., sp3/sp2 ratio in the films. Optical band gap calculated from transmittance spectra increased from 0.98 to 2.21 eV with a variation of silicon concentration from 0 to 15.4 at. %. Due to change in electronic structure by Si incorporation, the Si-DLC film showed a broad photoluminescence (PL) peak centered at 467 nm, i.e., in the visible range and its intensity was found to increase monotonically with at. % of Si.

  10. Electrochemical degradation of some herbicides in aqueous solution on boron doped diamond anodes

    International Nuclear Information System (INIS)

    Zaouak, Amira; Dachraoui, Mohamed; Matoussi, Fatma

    2009-01-01

    Bifenox(a) and acifluorfen(b), respectively (Methyl 5-(2,4-dichlorophenoxy)-2-nitrobenzoate and 5-(2-Chloro-4-trifluoro methylphenoxy)-2-nitrobenzoic acid, are two highly toxic herbicides of the diphenyl ether class. They are widely used in agriculture. Their electrochemical oxidation behaviour is studied by cyclic voltammetry in various media with different electrodes. When galvanostatic electrolysis is realized on Boron Doped Diamond electrode (BDD) we observe that the studied contaminants undergo an almost complete degradation due to hydroxy radical action as commonly suggested. The rate of the mineralization is followed by spectrophotometric analysis and COD measurements. The optimization of this advanced oxidation process is studied as a function of the current density. It shows that the best results are obtained with low current densities. The obtained COD abatement values are superior to 90 pour cent.

  11. Effects of the shape anisotropy and biasing field on the magnetization reversal process of the diamond-shaped NiFe nano films

    Science.gov (United States)

    Xu, Sichen; Yin, Jianfeng; Tang, Rujun; Zhang, Wenxu; Peng, Bin; Zhang, Wanli

    2017-11-01

    The effects of the planar shape anisotropy and biasing field on the magnetization reversal process (MRP) of the diamond-shaped NiFe nano films have been investigated by micromagnetic simulations. Results show that when the length to width ratio (LWR) of the diamond-shaped film is small, the MRP of the diamond-shaped films are sensitive to LWR. But when LWR is larger than 2, a stable domain switching mode is observed which nucleates from the center of the diamond and then expands to the edges. At a fixed LWR, the magnitude of the switching fields decrease with the increase of the biasing field, but the domain switching mode is not affected by the biasing field. Further analysis shows that demagnetization energy dominates over the MRP of the diamond-shaped films. The above LWR dependence of MRP can be well explained by a variation of the shape anisotropic factor with LWR.

  12. Synthesis of diamond films by pulsed liquid injection chemical vapor deposition using a mixture of acetone and water as precursor

    International Nuclear Information System (INIS)

    Apatiga, L.M.; Morales, J.

    2009-01-01

    A chemical vapor deposition reactor based on the flash evaporation of an organic liquid precursor was used to grow diamond films on Si substrates. An effective pulsed liquid injection mechanism consisting of an injector, normally used for fuel injection in internal combustion engines, injects micro-doses of the precursor to the evaporation zone at 280 o C and is instantly evaporated. The resulting vapor mixture is transported by a carrier gas to the high-temperature reaction chamber where the diamond nucleates and grows on the substrate surface at temperatures ranging from 750 to 850 o C. The injection frequency, opening time, number of pulses and other injector parameters are controlled by a computer-driven system. The diamond film morphology and structure were characterized by scanning electron microscopy and Raman spectroscopy. The as-deposited diamond films show a ball-shaped morphology with a grain size that varies from 100 to 400 nm, as well as the characteristic diamond Raman band at 1332 cm -1 . The effects of the experimental parameters and operation principle on the diamond films quality are analyzed and discussed in terms of crystallinity, composition, structure, and morphology.

  13. The bonding of protective films of amorphic diamond to titanium

    Science.gov (United States)

    Collins, C. B.; Davanloo, F.; Lee, T. J.; Jander, D. R.; You, J. H.; Park, H.; Pivin, J. C.

    1992-04-01

    Films of amorphic diamond can be deposited from laser plasma ions without the use of catalysts such as hydrogen or fluorine. Prepared without columnar patterns of growth, the layers of this material have been reported to have ``bulk'' values of mechanical properties that have suggested their usage as protective coatings for metals. Described here is a study of the bonding and properties realized in one such example, the deposition of amorphic diamond on titanium. Measurements with Rutherford backscattering spectrometry and transmission electron microscopy showed that the diamond coatings deposited from laser plasmas were chemically bonded to Ti substrates in 100-200-Å-thick interfacial layers containing some crystalline precipitates of TiC. Resistance to wear was estimated with a modified sand blaster and in all cases the coating was worn away without any rupture or deterioration of the bonding layer. Such wear was greatly reduced and lifetimes of the coated samples were increased by a factor of better than 300 with only 2.7 μm of amorphic diamond.

  14. Enhanced thermoelectric properties of bismuth telluride-organic hybrid films via graphene doping

    International Nuclear Information System (INIS)

    Rahman, Airul Azha Abd; Umar, Akrajas Ali; Salleh, Muhamad Mat; Chen, Xiaomei; Oyama, Munetaka

    2016-01-01

    The thermoelectric properties of graphene-doped bismuth telluride-PEDOT:PSS-glycerol (hybrid) films were investigated. Prior to the study, p-type and n-type hybrid films were prepared by doping the PEDOT:PSS-glycerol with the p- and n-type bismuth telluride. Graphene-doped hybrid films were prepared by adding graphene particles of concentration ranging from 0.02 to 0.1 wt% into the hybrid films. Films of graphene-doped hybrid system were then prepared on a glass substrate using a spin-coating technique. It was found that the electrical conductivity of the hybrid films increases with the increasing of the graphene-dopant concentration and optimum at 0.08 wt% for both p- and n-type films, namely 400 and 195 S/cm, respectively. Further increasing in the concentration caused a decreasing in the electrical conductivity. Analysis of the thermoelectric properties of the films obtained that the p-type film exhibited significant improvement in its thermoelectric properties, where the thermoelectric properties increased with the increasing of the doping concentration. Meanwhile, for the case of n-type film, graphene doping showed a negative effect to the thermoelectrical properties, where the thermoelectric properties decreased with the increasing of doping concentration. Seebeck coefficient (and power factor) for optimum p-type and n-type hybrid thin films, i.e., doped with 0.08 wt% of graphene, is 20 μV/K (and 160 μW m -1 K -2 ) and 10 μV/K (and 19.5 μW m -1 K -2 ), respectively. The obtained electrical conductivity and thermoelectric properties of graphene-doped hybrid film are interestingly several orders higher than the pristine hybrid films. A thermocouple device fabricated utilizing the p- and n-type graphene-doped hybrid films can generate an electric voltage as high as 2.2 mV under a temperature difference between the hot-side and the cold-side terminal as only low as 55 K. This is equivalent to the output power as high as 24.2 nW (for output load as high as 50

  15. SiV color centers in Si-doped isotopically enriched {sup 12}C and {sup 13}C CVD diamonds

    Energy Technology Data Exchange (ETDEWEB)

    Sedov, Vadim; Bolshakov, Andrey [General Physics Institute, RAS, Moscow (Russian Federation); National Research Nuclear University MEPhI, Moscow (Russian Federation); Boldyrev, Kirill [Institute of Spectroscopy, RAS, Troitsk, Moscow (Russian Federation); Krivobok, Vladimir; Nikolaev, Sergei [Lebedev Physical Institute, RAS, Moscow (Russian Federation); Khomich, Alex [Institute of Radio Engineering and Electronics, RAS, Fryazino (Russian Federation); Khomich, Andrew [General Physics Institute, RAS, Moscow (Russian Federation); Institute of Radio Engineering and Electronics, RAS, Fryazino (Russian Federation); Krasilnikov, Anatoly [Institution ' ' ProjectCenter ITER' ' , Moscow (Russian Federation); Ralchenko, Victor [General Physics Institute, RAS, Moscow (Russian Federation); National Research Nuclear University MEPhI, Moscow (Russian Federation); Harbin Institute of Technology, Harbin (China)

    2017-11-15

    The effect of isotopic modification of diamond lattice on photoluminescence (PL) and optical absorption spectra of ensembles of SiV{sup -} centers was studied. Thin epitaxial diamond layers were grown by a microwave plasma CH{sub 4}/H{sub 2} mixtures using methane enriched to 99.96% for either {sup 12}C or {sup 13}C isotopes, while the Si doping was performed by adding a small percentage of silane SiH{sub 4} into the plasma. Temperature dependent SiV{sup -} ZPL spectra in absorption were measured at 3-80 K to monitor the evolution of the ZPL fine structure. It is found that the SiV{sup -} ZPL at 736.9 nm observed in PL for {sup 12}C diamond at T = 5 K, exhibits a blue shift of 1.78 meV, to 736.1 nm in {sup 13}C diamond matrix. Narrow ZPL with the width (FWHM) of 0.09 meV (21 GHz) was measured in absorption spectra at T = 3-30 K in the Si-doped {sup 13}C diamond. Besides the charged SiV{sup -} center, the absorption of the neutral SiV{sup 0} defect at 946 nm wavelength has also been detected. From changes observed in SiV{sup -} phonon band structure in PL with isotopic modification, the band at 64 meV was confirmed to be a local vibration mode (LVM) involving a Si atom. (copyright 2017 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim)

  16. Low-temperature (200 C or below) fabrication of diamond films for electronic application

    International Nuclear Information System (INIS)

    Hiraki, A.

    2003-01-01

    Fabrication of Diamond (including Diamond Like Carbon: DLC) films as electronic materials, for example: to be used as electron-emitter, requires several following conditions. They are: 1 ) Low temperature fabrication (or deposition on several substrates and sometimes ones with low melting point, like glasses) below 400 C, 2) Wide area film deposition onto wide substrates of several square inches, like Si wafer and glass substrate, 3) Reproducible deposition of well defined film quality, 4) others. In these respects, we have initiated, in the author's laboratories at Osaka University and Kochi University of Technology, a quite new approach to satisfy the above requirements by using microwave plasma CVD under a magnetic field to be called as m agneto-active plasma CVD . The films fabricated by the magnets-active plasma CVD and also recently by cathodic arc methods combined with cur special nano-seeding method, have been utilized for electron emitter to exhibit very high efficiency. (Author)

  17. Polycrystalline boron-doped diamond electrodes for electrocatalytic and electrosynthetic applications.

    Science.gov (United States)

    Ivandini, Tribidasari A; Einaga, Yasuaki

    2017-01-24

    Boron-doped diamond (BDD) electrodes are recognized as being superior to other electrode materials due to their outstanding chemical and dimensional stability, their exceptionally low background current, the extremely wide potential window for water electrolysis that they have, and their excellent biocompatibility. However, whereas these properties have been utilized in the rapid development of electroanalytical applications, very few studies have been done in relation to their applications in electrocatalysis or electrosynthesis. In this report, following on from reports of the electrosynthesis of various products through anodic and cathodic reactions using BDD electrodes, the potential use of these electrodes in electrosynthesis is discussed.

  18. Lunar Production and Application of Solar Cells, and Synthesis of Diamond Film

    Science.gov (United States)

    Fang, P. H.

    1991-01-01

    Two projects which are carried out under the Summer Faculty Fellowship Program-1991 are discussed. A conceptual design of a solar cell manufacturing plant on a lunar base is discussed. This is a large program that requires a continuous and expanded effort, the present status of which is reflected here. An experiment on the synthesis of diamond film is discussed. Encouraging, but not yet conclusive evidence has been obtained on a new method to synthesize diamond film. The procedures and observations are presented. A third project is an analysis of the solar cell performance over five years on the moon based on Apollo missions. A paper has been completed and will be submitted to the journal Solar Cells for publication.

  19. Diamond semiconducting devices

    International Nuclear Information System (INIS)

    Polowczyk, M.; Klugmann, E.

    1999-01-01

    Many efforts to apply the semiconducting diamond for construction of electronic elements: resistors, thermistors, photoresistors, piezoresistors, hallotrons, pn diodes, Schottky diodes, IMPATT diodes, npn transistor, MESFETs and MISFETs are reviewed. Considering the possibilities of acceptor and donor doping, electrical resistivity and thermal conductivity of diamond as well as high electric-field breakdown points, that diamond devices could be used at about 30-times higher frequency and more then 8200 times power than silicon devices. Except that, due to high heat resistant of diamond, it is concluded that diamond devices can be used in environment at high temperature, range of 600 o C. (author)

  20. Optimizing biosensing properties on undecylenic Acid-functionalized diamond.

    Science.gov (United States)

    Zhong, Yu Lin; Chong, Kwok Feng; May, Paul W; Chen, Zhi-Kuan; Loh, Kian Ping

    2007-05-08

    The optimization of biosensing efficiency on a diamond platform depends on the successful coupling of biomolecules on the surface, and also on effective signal transduction in the biorecognition events. In terms of biofunctionalization of diamond surfaces, surface electrochemical studies of diamond modified with undecylenic acid (UA), with and without headgroup protection, were performed. The direct photochemical coupling method employing UA was found to impart a higher density of carboxylic acid groups on the diamond surface compared to that using trifluoroethyl undecenoate (TFEU) as the protecting group during the coupling process. Non-faradic impedimetric DNA sensing revealed that lightly doped diamond gives better signal transduction sensitivity compared to highly doped diamond.

  1. Effect of doping concentration on the structural, morphological, optical and electrical properties of Mn-doped CdO thin films

    Directory of Open Access Journals (Sweden)

    Manjula N.

    2015-12-01

    Full Text Available Thin films of manganese-doped cadmium oxide (CdO:Mn with different Mn-doping levels (0, 1, 2, 3 and 4 at.% were deposited on glass substrates by employing an inexpensive, simplified spray technique using a perfume atomizer at 375 °C. The influence of Mn incorporation on the structural, morphological, optical and electrical properties of CdO films has been studied. All the films exhibit cubic crystal structure with a (1 1 1 preferential orientation. Mn-doping causes a slight shift of the (1 1 1 diffraction peak towards higher angle. The crystallite size of the films is found to decrease from 34.63 nm to 17.68 nm with an increase in Mn doping concentration. The CdO:Mn film coated with 1 at.% Mn exhibit a high transparency of nearly 90 % which decreases for higher doping concentration. The optical band gap decreases with an increase in Mn doping concentration. All the films have electrical resistivity of the order of 10−4 Ω·cm.

  2. Surface modification on 304 SS by plasma-immersed ion implantation to improve the adherence of a CVD diamond film

    Energy Technology Data Exchange (ETDEWEB)

    Nono, M.C.A.; Corat, E.J. (Instituto Nacional de Pesquisas Espaciais, Sao Jose dos Campos, SP (Brazil)); Ueda, M.; Stellati, C.; Barroso, J.J.; Conrad, J.R.; Shamim, M.; Fetherston, P.; Sridharan, K.

    1999-02-01

    The weak adherence of chemical vapor deposited (CVD) diamond films on steel substrates is an important factor that limits the technological applications of these materials. We are interested in enhancing the film-to-substrate adherence by using substrate surfaces with a previous modification by plasma-immersed ion implantation (PIII). In this work we present and discuss the preliminary results on phase formation, microstructure and adherence evaluations. CVD diamond films were deposited on 304 SS, the surface of which was modified by implanted carbon ions. The samples were first submitted to implantation with 30 keV carbon ions at different doses. Later, these surfaces were examined by Auger spectroscopy (SAM), scanning electron microscopy (SEM) and X-ray diffraction. We observed a metastable carbide phase formed from carbon and iron, which is considered to be a good polycrystalline material for the nucleation of CVD diamond crystals. The CVD diamond nucleation and film growth were observed by SEM and Raman spectroscopy. These results are discussed with the emphasis on the carbon diffusion barrier on the substrate surfaces. The preliminary results of diamond growth were encouraging. (orig.) 7 refs.

  3. Fabrication of Nickel/nanodiamond/boron-doped diamond electrode for non-enzymatic glucose biosensor

    International Nuclear Information System (INIS)

    Dai, Wei; Li, Mingji; Gao, Sumei; Li, Hongji; Li, Cuiping; Xu, Sheng; Wu, Xiaoguo; Yang, Baohe

    2016-01-01

    Highlights: • Nanodiamonds (NDs) were electrophoretically deposited on the BDD film. • The NDs significantly extended the potential window. • Ni/NDs/BDD electrode was prepared by electrodeposition. • The electrode shows good catalytic activity for glucose oxidation. - Abstract: A stable and sensitive non-enzymatic glucose sensor was prepared by modifying a boron-doped diamond (BDD) electrode with nickel (Ni) nanosheets and nanodiamonds (NDs). The NDs were electrophoretically deposited on the BDD surface, and acted as nucleation sites for the subsequent electrodeposition of Ni. The morphology and composition of the modified BDD electrodes were characterized by field-emission scanning electron microscopy and energy-dispersive X-ray spectroscopy, respectively. The Ni nanosheet-ND modified BDD electrode exhibited good current response towards the non-enzymatic oxidation of glucose in alkaline media. The NDs significantly extended the potential window. The response to glucose was linear over the 0.2–1055.4-μM range. The limit of detection was 0.05 μM, at a signal-to-noise ratio of 3. The Ni nanosheet-ND/BDD electrode exhibited good selectivity, reproducibility and stability. Its electrochemical performance, low cost and simple preparation make it a promising non-enzymatic glucose sensor.

  4. VO{sub x} effectively doping CVD-graphene for transparent conductive films

    Energy Technology Data Exchange (ETDEWEB)

    Ji, Qinghua; Shi, Liangjing [State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Dingxi Road, Shanghai 200050 (China); Zhang, Qinghong [State Key Laboratory of Modification of Chemical Fibers and Polymer Materials, College of Material Science and Engineering, Donghua University, 2999 North Renmin Road, Shanghai 201620 (China); Wang, Weiqi; Zheng, Huifeng [State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Dingxi Road, Shanghai 200050 (China); Zhang, Yuzhi [The Key Laboratory of Inorganic Coating Materials, Shanghai Institute of Ceramics, Chinese Academy of Sciences,1295 Dingxi Road, Shanghai 200050 (China); Liu, Yangqiao, E-mail: yqliu@mail.sic.ac.cn [State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Dingxi Road, Shanghai 200050 (China); Sun, Jing, E-mail: jingsun@mail.sic.ac.cn [State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Dingxi Road, Shanghai 200050 (China)

    2016-11-30

    Highlights: • Doping process operated easily. • Sheet resistance decreased efficiently after doping. • Sheet resistance of doped graphene is stable after exposed in the air. • Mechanism of doping process is studied. - Abstract: Chemical vapor deposition(CVD)-synthesized graphene is potentially an alternative for tin-doped indium oxide (ITO) transparent conductive films (TCFs), however its sheet resistance is still too high to meet many demands. Vanadium oxide has been widely applied as smart window materials, however, no study has been reported to use it as dopant to improve the conductivity of graphene TCFs. In this study, we firstly reported that VO{sub x} doping can effectively lower the sheet resistance of CVD-graphene films while keeping its good optical properties, whose transmittance is as high as 86–90%. The optimized VO{sub x}-doped graphene exhibits a sheet resistance as low as 176 Ω/□, which decreases by 56% compared to the undoped graphene films. The doping process is convenient, stable, economical and easy to operate. What is more, VO{sub x} can effectively increase the work function(WF) of the film, making it more appropriate for use in solar cells. The evolution of the VO{sub x} species annealed at different temperatures below 400 °C has been detailed studied for the first time, based on which the doping mechanism is proposed. The prepared VO{sub x} doped graphene is expected to be a promising candidate for transparent conductive film purposes.

  5. Fabrication of boron-doped nanocrystalline diamond nanoflowers based on 3D Cu(OH){sub 2} dendritic architectures

    Energy Technology Data Exchange (ETDEWEB)

    Sim, Huijun; Hong, Sukin; Lee, Seungkoo; Lim, Daesoon; Jin, Juneon; Hwang, Sungwoo [Korea University, Seoul (Korea, Republic of)

    2012-03-15

    Hot-filament chemical vapor deposition (HFCVD) was used to prepare boron-doped nanocrystalline diamond (BDND) nanoflowers on a Cu substrate with a Cu(OH){sub 2} dendritic architecture that had been formed by using electrostatic self-assembly (ESA) method with nanodiamond particles. The formation of diamond nanoflowers is controlled by the reaction time between the Cu(OH){sub 2} nanoflowers and the polymeric linker for the electrostatic attachment of nanodiamonds and by the deposition time for CVD diamond growth with a high nucleation density. Through analysis by field emission scanning electron microscopy (FESEM) and Raman spectroscopy, the optimal conditions for the synthesis of BDND nanoflowers are determined, and a possible explanation is provided.

  6. A comparative investigation on structure and multiferroic properties of bismuth ferrite thin films by multielement co-doping

    Energy Technology Data Exchange (ETDEWEB)

    Dong, Guohua; Tan, Guoqiang, E-mail: tan3114@163.com; Luo, Yangyang; Liu, Wenlong; Xia, Ao; Ren, Huijun

    2014-12-15

    Highlights: • Multielement (Tb, Cr and Mn) co-doped BiFeO{sub 3} films were fabricated by CSD method. • Multielement co-doping induces a structural transition. • It is found effective to stabilize the valence of Fe ions at +3 by the strategy. • The co-doping at A/B-sites gives rise to the superior multiferroic properties. - Abstract: (Tb, Cr and Mn) multielement co-doped BiFeO{sub 3} (BTFCMO) thin films were prepared by the chemical solution deposition method on fluorine doped tin oxide (FTO) substrates. X-ray diffraction, Rietveld refinement and Raman analyses revealed that a phase transition from rhombohedral to triclinic structure occurs in the multielement co-doped BiFeO{sub 3} films. It is found that the doping is conducive to stabilizing the valence of Fe ions and reducing leakage current. In addition, the highly enhanced ferroelectric properties with a huge remanent polarization (2P{sub r}) of 239.6 μC/cm{sup 2} and a low coercive field (2E{sub c}) of 615.6 kV/cm are ascribed to the well film texture, the structure transition and the reduced leakage current by the co-doping. Moreover, the structure transition is the dominant factor resulting in the significant enhancement observed in magnetization (M{sub s} ∼ 10.5 emu/cm{sup 3}), owing to the collapse of the space-modulated spin structure. In this contribution, these results demonstrate that the multielement co-doping is in favor of the enhanced multiferroic properties of the BFO films for possible multifunctional applications.

  7. Temperature dependent simulation of diamond depleted Schottky PIN diodes

    International Nuclear Information System (INIS)

    Hathwar, Raghuraj; Dutta, Maitreya; Chowdhury, Srabanti; Goodnick, Stephen M.; Koeck, Franz A. M.; Nemanich, Robert J.

    2016-01-01

    Diamond is considered as an ideal material for high field and high power devices due to its high breakdown field, high lightly doped carrier mobility, and high thermal conductivity. The modeling and simulation of diamond devices are therefore important to predict the performances of diamond based devices. In this context, we use Silvaco ® Atlas, a drift-diffusion based commercial software, to model diamond based power devices. The models used in Atlas were modified to account for both variable range and nearest neighbor hopping transport in the impurity bands associated with high activation energies for boron doped and phosphorus doped diamond. The models were fit to experimentally reported resistivity data over a wide range of doping concentrations and temperatures. We compare to recent data on depleted diamond Schottky PIN diodes demonstrating low turn-on voltages and high reverse breakdown voltages, which could be useful for high power rectifying applications due to the low turn-on voltage enabling high forward current densities. Three dimensional simulations of the depleted Schottky PIN diamond devices were performed and the results are verified with experimental data at different operating temperatures

  8. Temperature dependent simulation of diamond depleted Schottky PIN diodes

    Science.gov (United States)

    Hathwar, Raghuraj; Dutta, Maitreya; Koeck, Franz A. M.; Nemanich, Robert J.; Chowdhury, Srabanti; Goodnick, Stephen M.

    2016-06-01

    Diamond is considered as an ideal material for high field and high power devices due to its high breakdown field, high lightly doped carrier mobility, and high thermal conductivity. The modeling and simulation of diamond devices are therefore important to predict the performances of diamond based devices. In this context, we use Silvaco® Atlas, a drift-diffusion based commercial software, to model diamond based power devices. The models used in Atlas were modified to account for both variable range and nearest neighbor hopping transport in the impurity bands associated with high activation energies for boron doped and phosphorus doped diamond. The models were fit to experimentally reported resistivity data over a wide range of doping concentrations and temperatures. We compare to recent data on depleted diamond Schottky PIN diodes demonstrating low turn-on voltages and high reverse breakdown voltages, which could be useful for high power rectifying applications due to the low turn-on voltage enabling high forward current densities. Three dimensional simulations of the depleted Schottky PIN diamond devices were performed and the results are verified with experimental data at different operating temperatures

  9. Temperature dependent simulation of diamond depleted Schottky PIN diodes

    Energy Technology Data Exchange (ETDEWEB)

    Hathwar, Raghuraj; Dutta, Maitreya; Chowdhury, Srabanti; Goodnick, Stephen M. [Department of Electrical Engineering, Arizona State University, Tempe, Arizona 85287-8806 (United States); Koeck, Franz A. M.; Nemanich, Robert J. [Department of Physics, Arizona State University, Tempe, Arizona 85287-8806 (United States)

    2016-06-14

    Diamond is considered as an ideal material for high field and high power devices due to its high breakdown field, high lightly doped carrier mobility, and high thermal conductivity. The modeling and simulation of diamond devices are therefore important to predict the performances of diamond based devices. In this context, we use Silvaco{sup ®} Atlas, a drift-diffusion based commercial software, to model diamond based power devices. The models used in Atlas were modified to account for both variable range and nearest neighbor hopping transport in the impurity bands associated with high activation energies for boron doped and phosphorus doped diamond. The models were fit to experimentally reported resistivity data over a wide range of doping concentrations and temperatures. We compare to recent data on depleted diamond Schottky PIN diodes demonstrating low turn-on voltages and high reverse breakdown voltages, which could be useful for high power rectifying applications due to the low turn-on voltage enabling high forward current densities. Three dimensional simulations of the depleted Schottky PIN diamond devices were performed and the results are verified with experimental data at different operating temperatures.

  10. Thermoluminescence characterisation of chemical vapour deposited diamond films

    CERN Document Server

    Mazzocchi, S; Bucciolini, M; Cuttone, G; Pini, S; Sabini, M G; Sciortino, S

    2002-01-01

    The thermoluminescence (TL) characteristics of a set of six chemical vapour deposited diamond films have been studied with regard to their use as off-line dosimeters in radiotherapy. The structural characterisation has been performed by means of Raman spectroscopy. Their TL responses have been tested with radiotherapy beams ( sup 6 sup 0 Co photons, photons and electrons from a linear accelerator (Linac), 26 MeV protons from a TANDEM accelerator) in the dose range 0.1-7 Gy. The dosimetric characterisation has yielded a very good reproducibility, a very low dependence of the TL response on the type of particle and independence of the radiation energy. The TL signal is not influenced by the dose rate and exhibits a very low thermal fading. Moreover, the sensitivity of the diamond samples compares favourably with that of standard TLD100 dosimeters.

  11. Roughness transitions of diamond(100) induced by hydrogen-plasma treatment

    Science.gov (United States)

    Koslowski, B.; Strobel, S.; Wenig, M. J.; Ziemann, P.

    To investigate the influence of hydrogen-plasma treatment on diamond(100) surfaces, heavily boron (B)-doped HPHT diamond crystals were mechanically and chemo-mechanically polished, and exposed to a microwave-assisted hydrogen plasma on a time scale of several minutes. The resulting surface morphology was analyzed on macroscopic scales by stylus profilometry (PFM) and on microscopic scales by STM and AFM. The polished samples have a roughness of typically 100 pmrms (PFM), with no obvious anisotropic structures at the surface. After exposure of the B-doped diamond(100) to the H-plasma, the roughness increases dramatically, and pronounced anisotropic structures appear, these being closely aligned with the crystallographic axis' and planes. An exposure for 3 minutes to the plasma leads to an increase of the roughness to 2-4 nmrms (STM), and a `brick-wall' pattern appears, formed by weak cusps running along . Very frequently, the cusps are replaced by `negative' pyramids that are bordered by {11X} facets. After an exposure of an additional 5 minutes, the surface roughness of the B-doped samples increases further to 20-40 nmrms (STM), and frequently exhibits a regular pattern with structures at a characteristic length scale of about 100 nm. Those structures are aligned approximately with and they are faceted with faces of approximately {XX1}. These results will be discussed in terms of strain relaxation, similar to the surface roughening observed on SiGe/Si and anisotropic etching.

  12. Atomic layer deposition of Al-doped ZnO thin films

    Energy Technology Data Exchange (ETDEWEB)

    Tynell, Tommi; Yamauchi, Hisao; Karppinen, Maarit; Okazaki, Ryuji; Terasaki, Ichiro [Department of Chemistry, Aalto University, FI-00076 Aalto (Finland); Department of Physics, Nagoya University, Nagoya 464-8602 (Japan)

    2013-01-15

    Atomic layer deposition has been used to fabricate thin films of aluminum-doped ZnO by depositing interspersed layers of ZnO and Al{sub 2}O{sub 3} on borosilicate glass substrates. The growth characteristics of the films have been investigated through x-ray diffraction, x-ray reflection, and x-ray fluorescence measurements, and the efficacy of the Al doping has been evaluated through optical reflectivity and Seebeck coefficient measurements. The Al doping is found to affect the carrier density of ZnO up to a nominal Al dopant content of 5 at. %. At nominal Al doping levels of 10 at. % and higher, the structure of the films is found to be strongly affected by the Al{sub 2}O{sub 3} phase and no further carrier doping of ZnO is observed.

  13. Boron-doped Diamond Electrodes: Electrochemical, Atomic Force Microscopy and Raman Study towards Corrosion-modifications at Nanoscale

    Czech Academy of Sciences Publication Activity Database

    Kavan, Ladislav; Vlčková Živcová, Zuzana; Petrák, Václav; Frank, Otakar; Janda, Pavel; Tarábková, Hana; Nesladek, M.; Mortet, Vincent

    2015-01-01

    Roč. 179, OCT 2015 (2015), s. 626-636 ISSN 0013-4686 R&D Projects: GA ČR GA13-31783S Institutional support: RVO:61388955 ; RVO:68378271 Keywords : Raman spectroelectrochemistry * atomic force microscopy * boron doped diamond Subject RIV: CG - Electrochemistry Impact factor: 4.803, year: 2015

  14. Fabrication and characterization of n-type zinc oxide/p-type boron doped diamond heterojunction

    Czech Academy of Sciences Publication Activity Database

    Marton, M.; Mikolášek, M.; Bruncko, J.; Novotný, I.; Ižák, Tibor; Vojs, M.; Kozak, Halyna; Varga, Marián; Artemenko, Anna; Kromka, Alexander

    2015-01-01

    Roč. 66, č. 5 (2015), s. 277-281 ISSN 1335-3632 R&D Projects: GA ČR(CZ) GBP108/12/G108; GA MŠk(CZ) 7AMB14SK024 Institutional support: RVO:68378271 Keywords : boron doped diamond * zinc oxide * Raman spectroscopy * bipolar heterostructure * wide-bandgap Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 0.407, year: 2015

  15. Bragg superlattice for obtaining individual photoluminescence of diamond color centers in dense 3D ensembles

    Science.gov (United States)

    Kukushkin, V. A.

    2017-10-01

    A way to significantly increase the spatial resolution of the color center photoluminescence collection in chemically vapor-deposited (CVD) diamond at a fixed exciting beam focal volume is suggested. It is based on the creation of a narrow waveguide for the color center photoluminescence with a small number of allowed vertical indices of guided modes. The waveguide is formed between the top surface of a CVD diamond film and an underlaid mirror—a Bragg superlattice made of interchanging high- and low boron-doped layers of CVD diamond. The guided color center photoluminescence is extracted through the top surface of a CVD diamond film with the frustrated total internal reflection method. According to the results of simulation made for a case when color centers are nitrogen-vacancy (NV) centers, the suggested way allows to increase the maximal value of the NV center concentration still compatible with selective collection of their photoluminescence by several times at a fixed exciting beam focal volume. This increase is provided without the deterioration of the NV center photoluminescence collection efficiency.

  16. Improvement of physical properties of ZnO thin films by tellurium doping

    Energy Technology Data Exchange (ETDEWEB)

    Sönmezoğlu, Savaş, E-mail: svssonmezoglu@kmu.edu.tr; Akman, Erdi

    2014-11-01

    Highlights: • We report the synthesis of tellurium-doped zinc oxide (Te–ZnO) thin films using sol–gel method. • Highly c-axis oriented Te-doped ZnO thin films were grown on FTO glasses as substrate. • 1.5% Te-doping ratio could improve the physical properties of ZnO thin films. - Abstract: This investigation addressed the structural, optical and morphological properties of tellurium incorporated zinc oxide (Te–ZnO) thin films. The obtained results indicated that Te-doped ZnO thin films exhibit an enhancement of band gap energy and crystallinity compared with non-doped films. The optical transmission spectra revealed a shift in the absorption edge toward lower wavelengths. X-ray diffraction measurement demonstrated that the film was crystallized in the hexagonal (wurtzite) phase and presented a preferential orientation along the c-axis. The XRD obtained patterns indicate that the crystallite size of the thin films, ranging from 23.9 to 49.1 nm, changed with the Te doping level. The scanning electron microscopy and atomic force microscopy results demonstrated that the grain size and surface roughness of the thin films increased as the Te concentration increased. Most significantly, we demonstrate that it is possible to control the structural, optical and morphological properties of ZnO thin films with the isoelectronic Te-incorporation level.

  17. Phosphorylated nano-diamond/ Polyimide Nanocomposites

    International Nuclear Information System (INIS)

    Beyler-Çiǧil, Asli; Çakmakçi, Emrah; Kahraman, Memet Vezir

    2014-01-01

    In this study, a novel route to synthesize polyimide (PI)/phosphorylated nanodiamond films with improved thermal and mechanical properties was developed. Surface phosphorylation of nano-diamond was performed in dichloromethane. Phosphorylation dramatically enhanced the thermal stability of nano-diamond. Poly(amic acid) (PAA), which is the precursor of PI, was successfully synthesized with 3,3',4,4'-Benzophenonetetracarboxylic dianhydride (BTDA) and 4,4'-oxydianiline (4,4'-ODA) in the solution of N,N- dimethylformamide (DMF). Pure BTDA-ODA polyimide films and phosphorylated nanodiamond containing BTDA-ODA PI films were prepared. The PAA displayed good compatibility with phosphorylated nano-diamond. The morphology of the polyimide (PI)/phosphorylated nano-diamond was characterized by scanning electron microscopy (SEM). Chemical structure of polyimide and polyimide (PI)/phosphorylated nano-diamond was characterized by FTIR. SEM and FTIR results showed that the phosphorylated nano-diamond was successfully prepared. Thermal properties of the polyimide (PI)/phosphorylated nanodiamond was characterized by thermogravimetric analysis (TGA). TGA results showed that the thermal stability of (PI)/phosphorylated nano-diamond film was increased

  18. Stable iodide doping induced by photonic curing for carbon nanotube transparent conductive films

    Science.gov (United States)

    Wachi, Atsushi; Nishikawa, Hiroyuki; Zhou, Ying; Azumi, Reiko

    2018-06-01

    Doping has become crucial for achieving stable and high-performance conductive transparent carbon nanotube (CNT) films. In this study, we systematically investigate the doping effects of a few materials including alkali metal iodides, nonmetal iodide, and metals. We demonstrate that photonic curing can enhance the doping effects, and correspondingly improve the conductivity of CNT films, and that such iodides have better doping effects than metals. In particular, doping with a nonmetal compound (NH4I) shows the largest potential to improve the conductivity of CNT films. Typically, doping with metal iodides reduces the sheet resistance (R S) of CNT films with 70–80% optical transmittances at λ = 550 nm from 600–2400 to 250–440 Ω/square, whereas doping with NH4I reduces R S to 57 and 84 Ω/square at 74 and 84% optical transmittances, respectively. Interestingly, such a doped CNT film exhibits only a slight increase in sheet resistance under an extreme environment of high temperature (85 °C) and high relative humidity (85%) for 350 h. The results suggest that photonic-curing-induced iodide doping is a promising approach to producing high-performance conductive transparent CNT films.

  19. Flux pinning in MOD YBCO films by chemical doping

    International Nuclear Information System (INIS)

    Zhou, Y X; Ghalsasi, S; Rusakova, I; Salama, K

    2007-01-01

    A novel nanomaterial synthesis technique has been developed to introduce 0D (particles), 1D (columnar defects) and 3D (domains) nanoscale pinning centres in MOD Y 1 Ba 2 Cu 3 O 7 (YBCO) coated conductors. We have succeeded in introducing nanoscale Y enriched particles, nanoscale 90 0 rotated Y 1/3 Sm 2/3 Ba 2 Cu 3 O 7 domains and nanoscale Zr enriched columnar defects into YBCO layers by different chemical doping. The pinning force density in Y 2 O 3 -doped YBCO film is found to be larger than that of pure YBCO film at all fields. Also it was found that YBCO films with Sm substituting for Y have yielded improved critical current density characteristics over a wide range of magnetic fields. Maximum pinning force densities exceeding 7 and 8 GN m -3 are obtained in 5% BZO-doped and Sm substituted YBCO films, respectively. Additionally, TEM studies revealed nanoscale Zr enriched columnar defects distributing in the matrix of the c-oriented YBCO film throughout the whole cross section. This indicates that chemical doping is a promising fabrication technique to create specific pinning landscapes in YBCO coated conductors

  20. Synthesis and characterization of Fe doped cadmium selenide thin films by spray pyrolysis

    Energy Technology Data Exchange (ETDEWEB)

    Yadav, Abhijit A., E-mail: aay_physics@yahoo.co.in [Thin Film Physics Laboratory, Department of Physics, Electronics and Photonics, Rajarshi Shahu Mahavidyalaya, Latur 413 512, Maharashtra (India)

    2012-12-05

    Highlights: Black-Right-Pointing-Pointer Simple and inexpensive method to dope trivalent Fe in CdSe thin films. Black-Right-Pointing-Pointer Fe doped CdSe thin films are highly photosensitive. Black-Right-Pointing-Pointer AFM analysis shows uniform deposition of film over the entire substrate surface. Black-Right-Pointing-Pointer The band gap energy decreases from 1.74 to 1.65 eV with Fe doping. Black-Right-Pointing-Pointer Film resistivity decreases to 6.76 Multiplication-Sign 10{sup 4} {Omega}-cm with Fe doping in CdSe thin films. - Abstract: Undoped and Fe doped CdSe thin films have been deposited onto the amorphous and fluorine doped tin oxide coated glass substrates by spray pyrolysis. The Fe doping concentration has been optimized by photoelectrochemical (PEC) characterization technique. The structural, surface morphological, compositional, optical and electrical properties of undoped and Fe doped CdSe thin films have been studied. X-ray diffraction study reveals that the as deposited CdSe films possess hexagonal crystal structure with preferential orientation along (1 0 0) plane. AFM analysis shows uniform deposition of the film over the entire substrate surface with minimum surface roughness of 7.90 nm. Direct allowed type of transition with band gap decreasing from 1.74 to 1.65 eV with Fe doping has been observed. The activation energy of the films has been found to be in the range of 0.14-0.19 eV at low temperature and 0.27-0.44 eV at high temperature. Semi-conducting behavior has been observed from resistivity measurements. The thermoelectric power measurements reveal that the films are of n type.

  1. Nitrogen-doped diamond electrode shows high performance for electrochemical reduction of nitrobenzene

    International Nuclear Information System (INIS)

    Zhang, Qing; Liu, Yanming; Chen, Shuo; Quan, Xie; Yu, Hongtao

    2014-01-01

    Highlights: • A metal-free nitrogen-doped diamond electrode was synthesized. • The electrode exhibits high electrocatalytic activity for nitrobenzene reduction. • The electrode exhibits high selectivity for reduction of nitrobenzene to aniline. • High energy efficiency was obtained compared with graphite electrode. -- Abstract: Effective electrode materials are critical to electrochemical reduction, which is a promising method to pre-treat anti-oxidative and bio-refractory wastewater. Herein, nitrogen-doped diamond (NDD) electrodes that possess superior electrocatalytic properties for reduction were fabricated by microwave-plasma-enhanced chemical vapor deposition technology. Nitrobenzene (NB) was chosen as the probe compound to investigate the material's electro-reduction activity. The effects of potential, electrolyte concentration and pH on NB reduction and aniline (AN) formation efficiencies were studied. NDD exhibited high electrocatalytic activity and selectivity for reduction of NB to AN. The NB removal efficiency and AN formation efficiency were 96.5% and 88.4% under optimal conditions, respectively; these values were 1.13 and 3.38 times higher than those of graphite electrodes. Coulombic efficiencies for NB removal and AN formation were 27.7% and 26.1%, respectively; these values were 4.70 and 16.6 times higher than those of graphite electrodes under identical conditions. LC–MS analysis revealed that the dominant reduction pathway on the NDD electrode was NB to phenylhydroxylamine (PHA) to AN

  2. The irradiation studies on diamond-like carbon films

    CERN Document Server

    LiuGuIang; Xie Er Qin

    2002-01-01

    Diamond-like carbon (DLC) films have been deposited on glass substrates using radio-frequency (r.f.) plasma deposition method. gamma-ray, ultraviolet (UV) ray and neutron beam were used to irradiate the DLC films. Raman spectroscopy and infrared (IR) spectroscopy were used to characterize the changing characteristics of SP sup 3 C-H bond and hydrogen content in the films due to the irradiations. It showed that, the damage degrees of the gamma-ray, UV ray and neutron beam on the SP sup 3 C-H bonds are different. Among them, the damage of gamma-ray on the SP sup 3 C-H bond is the weakest. When the irradiation dose of gamma-ray reaches 10x10 sup 4 Gy, the SP sup 3 C-H bond reduces about 50% in number. The square resistance of the films is reduced due to the irradiation of UV ray and this is caused by severe oxidation of the films. Compared with that of the as-deposited one, the IR transmittance of the films irradiated by both gamma-ray and neutron beam is increased to some extent. By using the results on optical...

  3. Nanocrystalline diamond film as cathode for gas discharge sensors

    Energy Technology Data Exchange (ETDEWEB)

    Jou, Shyankay, E-mail: sjou@mail.ntust.edu.t [Graduate Institute of Materials Science and Technology, National Taiwan University of Science and Technology, Taipei 106, Taiwan (China); Huang, Bohr-Ran [Graduate Institute of Electro-Optical Engineering and Department of Electronic Engineering, National Taiwan University of Science and Technology, Taipei 106, Taiwan (China); Wu, Meng-Chang [Department of Electronic Engineering, National Yunlin University of Science and Technology, Touliu 640, Taiwan (China)

    2010-05-31

    Nanocrystalline diamond (NCD) film was deposited on a silicon substrate utilizing microwave plasma-enhanced chemical vapor deposition in a mixed flow of methane, hydrogen and argon. The deposited film had a cauliflower-like morphology, and was composed of NCD, carbon clusters and mixed sp{sup 2}- and sp{sup 3}-bonded carbon. Electron field emission (EFE) in vacuum and electrical discharges in Ar, N{sub 2} and O{sub 2} using the NCD film as the cathode were characterized. The turn-on field for EFE and the geometric enhancement factor for the NCD film were 8.5 V/{mu}m and 668, respectively. The breakdown voltages for Ar, N{sub 2} and O{sub 2} increased with pressures from 1.33 x 10{sup 4} Pa to 1.01 x 10{sup 5} Pa, following the right side of the normal Paschen curve.

  4. Methods for enhancing P-type doping in III-V semiconductor films

    Science.gov (United States)

    Liu, Feng; Stringfellow, Gerald; Zhu, Junyi

    2017-08-01

    Methods of doping a semiconductor film are provided. The methods comprise epitaxially growing the III-V semiconductor film in the presence of a dopant, a surfactant capable of acting as an electron reservoir, and hydrogen, under conditions that promote the formation of a III-V semiconductor film doped with the p-type dopant. In some embodiments of the methods, the epitaxial growth of the doped III-V semiconductor film is initiated at a first hydrogen partial pressure which is increased to a second hydrogen partial pressure during the epitaxial growth process.

  5. Influence of Ag doping on structural, optical, and photoluminescence properties of nanostructured AZO films by sol–gel technique

    International Nuclear Information System (INIS)

    Khan, Firoz; Baek, Seong-Ho; Kim, Jae Hyun

    2014-01-01

    Graphical abstract: The optical band gap of the Ag–AZO film first decreased to a value of ∼3.31 eV for a 1% Ag/Zn atomic ratio from a value of ∼3.69 for undoped AZO film. For higher values (beyond a 1% Ag/Zn atomic ratio) of Ag doping, the values of Eg started to increase and finally attained a value of ∼3.66 eV for an Ag/Zn 3% atomic ratio. The photoluminescence (PL) studies showed that the relative PL intensity of the Ag–AZO films in blue (IB) and green (IG) regions increased with Ag doping. The PL positions of these peaks were blue shifted with increased Ag content up to an Ag/Zn atomic ratio of 3%. The increase in IB and IG is due to the charge difference between Ag + and Zn 2+ , whereas shifting of the PL positions is due to the size of Ag + and Zn 2+ ions. -- Highlights: • The optical band gap of the Ag–AZO film is tuned with Ag doping. • The PL intensity of the Ag–AZO film in visible region is increased with Ag doping. • The PL positions of these peaks were blue shifted with increased Ag content. • The increase in I B and I G is due to the charge difference between Ag + and Zn 2+ . • The shifting of the PL positions is due to the size of Ag + and Zn 2+ ions. -- Abstract: The effects of Ag doping on the structural, electrical, optical, and photoluminescence properties of sol-gel derived Al rich zinc oxide (Ag–AZO) films are studied. The Al/Zn atomic ratio was constant (∼20%) in all the films, whereas the Ag/Zn atomic ratio varied from 0% to 3%. All the films were highly transparent in the 400–1200 nm wavelength range. The XRD results and surface morphologies of the films confirmed that the grain size increased with Ag doping. The optical band gap (E g ) of the Ag–AZO film first decreased to a value of ∼3.31 eV for a 1% Ag/Zn atomic ratio from a value of ∼3.69 for undoped AZO film. For higher values (beyond a 1% Ag/Zn atomic ratio) of Ag doping, the values of E g started to increase and finally attained a value of ∼3.66 e

  6. Photocatalytic properties of P25-doped TiO2 composite film synthesized via sol-gel method on cement substrate.

    Science.gov (United States)

    Guo, Xiang; Rao, Lei; Wang, Peifang; Wang, Chao; Ao, Yanhui; Jiang, Tao; Wang, Wanzhong

    2018-04-01

    TiO 2 films have received increasing attention for the removal of organic pollutants via photocatalysis. To develop a simple and effective method for improving the photodegradation efficiency of pollutants in surface water, we herein examined the preparation of a P25-TiO 2 composite film on a cement substrate via a sol-gel method. In this case, Rhodamine B (RhB) was employed as the target organic pollutant. The self-generated TiO 2 film and the P25-TiO 2 composite film were characterized by X-ray diffraction (XRD), N 2 adsorption/desorption measurements, scanning electron microscopy (SEM), transmission electron microscopy (TEM), and diffuse reflectance spectroscopy (DRS). The photodegradation efficiencies of the two films were studied by RhB removal in water under UV (ultraviolet) irradiation. Over 4day exposure, the P25-TiO 2 composite film exhibited higher photocatalytic performance than the self-generated TiO 2 film. The photodegradation rate indicated that the efficiency of the P25-TiO 2 composite film was enhanced by the addition of the rutile phase Degussa P25 powder. As such, cooperation between the anatase TiO 2 and rutile P25 nanoparticles was beneficial for separation of the photo-induced electrons and holes. In addition, the influence of P25 doping on the P25-TiO 2 composite films was evaluated. We found that up to a certain saturation point, increased doping enhanced the photodegradation ability of the composite film. Thus, we herein demonstrated that the doping of P25 powders is a simple but effective strategy to prepare a P25-TiO 2 composite film on a cement substrate, and the resulting film exhibits excellent removal efficiency in the degradation of organic pollutants. Copyright © 2017. Published by Elsevier B.V.

  7. Micro-Raman Analysis of Irradiated Diamond Films

    Science.gov (United States)

    Newton, Robert L.

    2003-01-01

    Owing to its unique and robust physical properties, diamond is a much sought after material for use in advanced technologies, even in Microelectromechanical Systems (MEMS). The volume and weight savings promised by MEMS-based devices are of particular interest to spaceflight applications. However, much basic materials science research remains to be completed in this field. Results of micro-Raman analysis of proton (10(exp 15) - 10(exp 17) H(+)/sq cm doses) irradiated chemical vapor deposited (CVD) films are presented and indicate that their microstructure is retained even after high radiation exposure.

  8. Nitrogen and hydrogen related infrared absorption in CVD diamond films

    Energy Technology Data Exchange (ETDEWEB)

    Titus, E. [Department of Mechanical Engineering, University of Aveiro, 3810-193 (Portugal)]. E-mail: elby@mec.ua.pt; Ali, N. [Department of Mechanical Engineering, University of Aveiro, 3810-193 (Portugal); Cabral, G. [Department of Mechanical Engineering, University of Aveiro, 3810-193 (Portugal); Madaleno, J.C. [Department of Mechanical Engineering, University of Aveiro, 3810-193 (Portugal); Neto, V.F. [Department of Mechanical Engineering, University of Aveiro, 3810-193 (Portugal); Gracio, J. [Department of Mechanical Engineering, University of Aveiro, 3810-193 (Portugal); Ramesh Babu, P [Materials Ireland, Polymer research Centre, School of Physics, Dublin (Ireland); Sikder, A.K. [Department of Physics, Indian Institute of Technology (IIT), Bombay (India); Okpalugo, T.I. [Northern Ireland Bio-Engineering Centre, NIBEC, University of Ulster (United Kingdom); Misra, D.S. [Department of Physics, Indian Institute of Technology (IIT), Bombay (India)

    2006-09-25

    In this paper, we investigate on the presence of hydrogen and nitrogen related infrared absorptions in chemical vapour deposited (CVD) diamond films. Investigations were carried out in cross sections of diamond windows, deposited using hot filament CVD (HFCVD). The results of Scanning Electron Microscopy (SEM), Fourier Transform Infrared (FTIR) and Raman spectroscopy carried out in a cross section of self-standing diamond sheets are presented. The FTIR spectra showed several features that have not been reported before. In order to confirm the frequency of nitrogen related vibrations, ab-initio calculations were carried out using GAMESS program. The investigations showed the presence of several C-N related peaks in one-phonon (1000-1333 cm{sup -1}). The deconvolution of the spectra in the three-phonon region (2700-3150 cm{sup -1}) also showed a number of vibration modes corresponding to sp {sup m}CH {sub n} phase of carbon. Elastic recoil detection analysis (ERDA) was employed to compare the H content measured using FTIR technique. Using these measurements we point out that the oscillator strength of the different IR modes varies depending upon the structure and H content of CVD diamond sheets.

  9. Coating dental implant abutment screws with diamondlike carbon doped with diamond nanoparticles: the effect on maintaining torque after mechanical cycling.

    Science.gov (United States)

    Lepesqueur, Laura Soares; de Figueiredo, Viviane Maria Gonçalves; Ferreira, Leandro Lameirão; Sobrinho, Argemiro Soares da Silva; Massi, Marcos; Bottino, Marco Antônio; Nogueira Junior, Lafayette

    2015-01-01

    To determine the effect of maintaining torque after mechanical cycling of abutment screws that are coated with diamondlike carbon and coated with diamondlike carbon doped with diamond nanoparticles, with external and internal hex connections. Sixty implants were divided into six groups according to the type of connection (external or internal hex) and the type of abutment screw (uncoated, coated with diamondlike carbon, and coated with diamondlike carbon doped with diamond nanoparticles). The implants were inserted into polyurethane resin and crowns of nickel chrome were cemented on the implants. The crowns had a hole for access to the screw. The initial torque and the torque after mechanical cycling were measured. The torque values maintained (in percentages) were evaluated. Statistical analysis was performed using one-way analysis of variance and the Tukey test, with a significance level of 5%. The largest torque value was maintained in uncoated screws with external hex connections, a finding that was statistically significant (P = .0001). No statistically significant differences were seen between the groups with and without coating in maintaining torque for screws with internal hex connections (P = .5476). After mechanical cycling, the diamondlike carbon with and without diamond doping on the abutment screws showed no improvement in maintaining torque in external and internal hex connections.

  10. On the changing electrochemical behaviour of boron-doped diamond surfaces with time after cathodic pre-treatments

    International Nuclear Information System (INIS)

    Salazar-Banda, Giancarlo R.; Andrade, Leonardo S.; Nascente, Pedro A.P.; Pizani, Paulo S.; Rocha-Filho, Romeu C.; Avaca, Luis A.

    2006-01-01

    The electrochemical response of the Fe(CN) 6 4-/3- redox couple on boron-doped diamond (BDD) electrodes immediately after a cathodic pre-treatment and as a function of time exposed to atmospheric conditions is reported here. After this pre-treatment the electrode exhibits a changing electrochemical behaviour, i.e., a loss of the reversibility for the Fe(CN) 6 4-/3- redox couple as a function of time. Raman spectra showed that neither important bulk structural differences nor significant changes in the sp 2 /sp 3 content are introduced into the BDD film by the cathodic pre-treatment indicating that H-terminated sites play an important role in the electrochemical response of the electrodes. Thus, the changing behaviour reflected by a progressive decrease of the electron transfer rate with time must be associated to a loss of superficial hydrogen due to oxidation by oxygen from the air, as confirmed by X-ray photoelectron spectroscopy (XPS) analysis. Moreover, it was also found that this changing electrochemical behaviour is inversely proportional to the doping level, suggesting that the boron content has a stabilizing effect on the H-terminated surface. These results point out the necessity of doing the cathodic pre-treatment just before the electrochemical experiments are carried out in order to ensure reliable and reproducible results

  11. Influence of Ag thickness of aluminum-doped ZnO/Ag/aluminum-doped ZnO thin films

    Energy Technology Data Exchange (ETDEWEB)

    Wu, Hung-Wei, E-mail: hwwu@mail.ksu.edu.tw [Department of Computer and Communication, Kun Shan University, No. 949, Dawan Rd., Yongkang Dist., Tainan City 710, Taiwan (China); Yang, Ru-Yuan [Graduate Institute of Materials Engineering, National Pingtung University of Science and Technology, 1, Shuefu Rd., Neipu, Pingtung City 912, Taiwan (China); Hsiung, Chin-Min; Chu, Chien-Hsun [Department of Mechanical Engineering, National Pingtung University of Science and Technology, 1, Shuefu Rd., Neipu, Pingtung City 912, Taiwan (China)

    2012-10-01

    Highly conducting aluminum-doped ZnO (30 nm)/Ag (5-15 nm)/aluminum-doped ZnO (30 nm) multilayer thin films were deposited on glass substrate by rf magnetron sputtering (for top/bottom aluminum-doped ZnO films) and e-beam evaporation (for Ag film). The transmittance is more than 70% for wavelengths above 400 nm with the Ag layer thickness of 10 nm. The resistivity is 3.71 Multiplication-Sign 10{sup -4} {Omega}-cm, which can be decreased to 3.8 Multiplication-Sign 10{sup -5} {Omega}-cm with the increase of the Ag layer thickness to 15 nm. The Haacke figure of merit has been calculated for the films with the best value being 8 Multiplication-Sign 10{sup -3} {Omega}{sup -1}. It was shown that the multilayer thin films have potential for applications in optoelectronics. - Highlights: Black-Right-Pointing-Pointer High-quality Al-doped ZnO (AZO)/Ag/AZO Transparent Conducting Oxide films. Black-Right-Pointing-Pointer AZO films (30 nm) made by RF sputtering; E-beam evaporation for Ag film (5-15 nm). Black-Right-Pointing-Pointer Influence of Ag thickness on optical and electrical properties were analyzed. Black-Right-Pointing-Pointer High quality multilayer film with optimal intermediate Ag layer thickness of 10 nm. Black-Right-Pointing-Pointer 3.71 Multiplication-Sign 10{sup -4} {Omega}-cm resistivity, 91.89% transmittance at 470 nm obtained and reproducible.

  12. Synthesis, characterization and electrochemical behavior of Sb-doped ZnO microsphere film

    Energy Technology Data Exchange (ETDEWEB)

    Li, Qian [Department of Materials Science and Engineering, State Key Laboratory of Silicon Materials, Cyrus Tang Center for Sensor Materials and Applications, Zhejiang University, Hangzhou, 310027 (China); Cheng, Kui, E-mail: chengkui@zju.edu.cn [Department of Materials Science and Engineering, State Key Laboratory of Silicon Materials, Cyrus Tang Center for Sensor Materials and Applications, Zhejiang University, Hangzhou, 310027 (China); Weng, Wenjian, E-mail: wengwj@zju.edu.cn [Department of Materials Science and Engineering, State Key Laboratory of Silicon Materials, Cyrus Tang Center for Sensor Materials and Applications, Zhejiang University, Hangzhou, 310027 (China); The Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Dingxi Road, Shanghai, 200050 (China); Du, Piyi; Han, Gaorong [Department of Materials Science and Engineering, State Key Laboratory of Silicon Materials, Cyrus Tang Center for Sensor Materials and Applications, Zhejiang University, Hangzhou, 310027 (China)

    2013-10-01

    Sb-doped ZnO microsphere film was fabricated by a carboxylate ion assisted hydrothermal route coupled with a post-calcination process. The structure, chemical composition and optical band gap of the Sb-doped ZnO microsphere film were characterized by X-ray diffraction, X-ray photoelectron spectroscopy, inductively couple plasma optical emission spectroscopy and UV–visible spectrophotometry, and compared with the un-doped ZnO microsphere film. The results suggest that the formation of zinc–antimony tartrate complex species during hydrothermal growth is the key to realize Sb-doped ZnO microstructures, and the present hydrothermal method with post-calcination is an effective way to dope Sb into ZnO. Furthermore, the Sb-doped ZnO microsphere film based electrochemical biosensor exhibits a good sensing performance for the detection of hydrogen peroxide, with a sensitivity of 271 μA mM{sup −1} cm{sup −2} which is more than three times higher than that of the un-doped ZnO biosensor. - Highlights: • Sb-doped ZnO microsphere (SZM) films were grown by hydrothermal deposition. • Carboxylate ions were used to form complex during hydrothermal growth. • The formation of Zn–Sb tartrate complex is the key to realize SZM. • The biosensors based on SZM film are feasible and sensitive to detect H{sub 2}O{sub 2}. • The Sb doping could improve the electrochemical property of ZnO.

  13. Chromium-doped DLC for implants prepared by laser-magnetron deposition.

    Science.gov (United States)

    Jelinek, Miroslav; Kocourek, Tomáš; Zemek, Josef; Mikšovský, Jan; Kubinová, Šárka; Remsa, Jan; Kopeček, Jaromir; Jurek, Karel

    2015-01-01

    Diamond-like carbon (DLC) thin films are frequently used for coating of implants. The problem of DLC layers lies in bad layer adhesion to metal implants. Chromium is used as a dopant for improvement of adhesion of DLC films. DLC and Cr-DLC layers were deposited on silicon, Ti6Al4V and CoCrMo substrates by a hybrid technology using combination of pulsed laser deposition (PLD) and magnetron sputtering. The topology of layers was studied using SEM, AFM and mechanical profilometer. Carbon and chromium content and concentration of trivalent and toxic hexavalent chromium bonds were determined by XPS and WDS. It follows from the scratch tests that Cr doping improved adhesion of DLC layers. Ethylene glycol, diiodomethane and deionized water were used to measure the contact angles. The surface free energy (SFE) was calculated. The antibacterial properties were studied using Pseudomonas aeruginosa and Staphylococcus aureus bacteria. The influence of SFE, hydrophobicity and surface roughness on antibacterial ability of doped layers is discussed. Copyright © 2014 Elsevier B.V. All rights reserved.

  14. Dry And Ringer Solution Lubricated Tribology Of Thin Osseoconductive Metal Oxides And Diamond-Like Carbon Films

    Directory of Open Access Journals (Sweden)

    Waldhauser W.

    2015-09-01

    Full Text Available Achieving fast and strong adhesion to jawbone is essential for dental implants. Thin deposited films may improve osseointegration, but they are prone to cohesive and adhesive fracture due to high stresses while screwing the implant into the bone, leading to bared, less osteoconductive substrate surfaces and nano- and micro-particles in the bone. Aim of this work is the investigation of the cohesion and adhesion failure stresses of osteoconductive tantalum, titanium, silicon, zirconium and aluminium oxide and diamond-like carbon films. The tribological behaviour under dry and lubricated conditions (Ringer solution reveals best results for diamond-like carbon, while cohesion and adhesion of zirconium oxide films is highest.

  15. Magnetic and electromagnetic properties of Pr doped strontium ferrite/polyaniline composite film

    Energy Technology Data Exchange (ETDEWEB)

    Huang, Ying; Li, Yuqing; Wang, Yan, E-mail: wangyan287580632@126.com

    2014-11-15

    This paper reported three acid (including hydrochloric acid HCl, p-toluenesulfonic acid PTS and D-camphor-10-acid CSA) doped SrPr{sub 0.2}Fe{sub 11.8}O{sub 19}/PANI composite film and the HCl–PANI film prepared by a sol–gel method and in-situ oxidative polymerization. The characteristics of the film phase structure, surface morphology, conductivity and magnetic and electromagnetic properties were studied by using XRD, XPS, FESEM, four-probe tester, VSM and Vector Network Analyzer. The resistivity of organic acid doped composite films is higher than that of the HCl doped one. The saturation and remanent magnetization of PTS and HCl doped composite films are greater than the CSA-doped one; however, the coercivity of the three acid doped composite films is basically 5546 Oe. The saturation magnetization, remanent magnetization and coercivity of SrPr{sub 0.2}Fe{sub 11.8}O{sub 19} film are greater than those of the SrPr{sub 0.2}Fe{sub 11.8}O{sub 19}–PANI composite film. In the frequency range of 8–12 GHz, the dielectric loss of HCl–PANI film is the maximum, and the dielectric loss of SrPr{sub 0.2}Fe{sub 11.8}O{sub 19} film is the minimum; the magnetic loss of the four films is in descending order as SrPr{sub 0.2}Fe{sub 11.8}O{sub 19} film, PrSrM/(HCl–PANI) composite film, PrSrM/(CSA–PANI) and HCl–PANI film. - Highlights: • Synthesizing three acid doped SrPr{sub 0.2}Fe{sub 11.8}O{sub 19}/PANI composite films. • By sol–gel method and in-situ oxidative polymerization. • With excellent magnetic and electromagnetic properties. • The particular coating structure of PANI and Sr-ferrite. • Great interest for magnetic material and microwave absorbers.

  16. Effect of sputtered titanium interlayers on the properties of nanocrystalline diamond films

    Energy Technology Data Exchange (ETDEWEB)

    Li, Cuiping, E-mail: licp226@126.com, E-mail: limingji@163.com; Li, Mingji, E-mail: licp226@126.com, E-mail: limingji@163.com; Wu, Xiaoguo; Yang, Baohe [Tianjin Key Laboratory of Film Electronic and Communicate Devices, School of Electronics Information Engineering, Tianjin University of Technology, Tianjin 300384 (China); Dai, Wei; Xu, Sheng [Tianjin Key Laboratory of Film Electronic and Communicate Devices, School of Electronics Information Engineering, Tianjin University of Technology, Tianjin 300384 (China); College of Precision Instrument and Optoelectronics Engineering, Tianjin University, Tianjin 300072 (China); Li, Hongji [Tianjin Key Laboratory of Organic Solar Cells and Photochemical Conversion, School of Chemistry and Chemical Engineering, Tianjin University of Technology, Tianjin 300384 (China)

    2016-04-07

    Ti interlayers with different thicknesses were sputtered on Si substrates and then ultrasonically seeded in a diamond powder suspension. Nanocrystalline diamond (NCD) films were deposited using a dc arc plasma jet chemical vapor deposition system on the seeded Ti/Si substrates. Atomic force microscopy and scanning electron microscopy tests showed that the roughness of the prepared Ti interlayer increased with increasing thickness. The effects of Ti interlayers with various thicknesses on the properties of NCD films were investigated. The results show nucleation, growth, and microstructure of the NCD films are strongly influenced by the Ti interlayers. The addition of a Ti interlayer between the Si substrate and the NCD films can significantly enhance the nucleation rate and reduce the surface roughness of the NCD. The NCD film on a 120 nm Ti interlayer possesses the fastest nucleation rate and the smoothest surface. Raman spectra of the NCD films show trans-polyacetylene relevant peaks reduce with increasing Ti interlayer thickness, which can owe to the improvement of crystalline at grain boundaries. Furthermore, nanoindentation measurement results show that the NCD film on a 120 nm Ti interlayer displays a higher hardness and elastic modulus. High resolution transmission electron microscopy images of a cross-section show that C atoms diffuse into the Ti layer and Si substrate and form TiC and SiC hard phases, which can explain the enhancement of mechanical properties of NCD.

  17. Characterization of diamond thin films deposited by a CO{sub 2} laser-assisted combustion-flame method

    Energy Technology Data Exchange (ETDEWEB)

    McKindra, Travis, E-mail: mckindra@mst.edu [Department of Materials Science and Engineering, Missouri University of Science and Technology, Rolla, MO 65409 (United States); O' Keefe, Matthew J. [Department of Materials Science and Engineering, Missouri University of Science and Technology, Rolla, MO 65409 (United States); Xie Zhiqiang; Lu Yongfeng [Department of Electrical Engineering, University of Nebraska-Lincoln, Lincoln, NE 68588 (United States)

    2010-06-15

    Diamond thin films were deposited by a CO{sub 2} laser-assisted O{sub 2}/C{sub 2}H{sub 2}/C{sub 2}H{sub 4} combustion-flame process. The effect of the deposition parameters, in particular the laser wavelength and power, on the film surface morphology, microstructure and phases present was the primary focus of the work. The laser power was set at 100, 400 and 800 W while the wavelength was varied and set at 10.591 {mu}m in the untuned condition and set at 10.532 {mu}m to resonantly match the CH{sub 2}-wagging vibrational mode of the C{sub 2}H{sub 4} molecule when in the tuned condition. When the laser was coupled to the combustion flame during deposition the diamond film growth was enhanced as the lateral grain size increased from 1 {mu}m to greater than 5 {mu}m. The greatest increase in grain size occurred when the wavelength was in the tuned condition. Scanning transmission electron microscopy images from focused-ion beam cross-sectioned samples revealed a sub-layer of smaller grains less than 1 {mu}m in size near the substrate surface at the lower laser powers and untuned wavelength. X-ray diffraction results showed a more intense Diamond (111) peak as the laser power increased from 100 to 800 W for the films deposited with the tuned laser wavelength. Micro-Raman spectra showed a diamond peak nearly twice as intense from the films with the tuned laser wavelength.

  18. Effect of hydrogen doping on the properties of Al and F co-doped ZnO films for thin film silicon solar cell applications

    Energy Technology Data Exchange (ETDEWEB)

    Wang, Fang-Hsing, E-mail: fansen@dragon.nchu.edu.tw; Yang, Tung-Hsin

    2016-04-30

    Aluminum and fluorine co-doped zinc oxide (AFZO) thin films were prepared in Ar + H{sub 2} atmospheres by rf magnetron sputtering at room temperature. The structural, electrical, and optical properties of the prepared films were investigated using X-ray diffraction, scanning electron microscopy, atomic force microscopy, Hall-effect measurement, X-ray photoelectron spectroscopy, and ultraviolet–visible spectrometry, and their dependence on deposition atmosphere (i.e. H{sub 2} / (H{sub 2} + Ar) ratio) was studied. The resulting films showed a (0 0 2) diffraction peak, indicating a typical wurtzite structure, and the optimal film crystallinity was obtained with the H{sub 2} / (H{sub 2} + Ar) ratio of 3%. The electrical resistivity of AFZO films decreased to 9.16 × 10{sup −4} Ω-cm, which was lower than ZnO:Al and ZnO:F films due to double doping effect of Al and F. The resistivity further decreased to below 5 × 10{sup −4} Ω-cm for the AFZO film with the H{sub 2} / (H{sub 2} + Ar) ratio of 3%–5%. All the films regardless of hydrogen content displayed high transmittances (> 92%) in the visible wavelength range. Applying the developed AFZO films as front transparent electrodes, amorphous Si thin film solar cells were fabricated and the open-circuit voltage, fill factor, and efficiency of the cell with the hydrogenated AFZO film were improved in contrast to those without the hydrogenated film. - Highlights: • H{sub 2} doping improves optoelectronic properties of Al, F co-doped ZnO (AFZO) films. • Resistivity of AFZO films decreases to 4.4 × 10{sup −4} Ω-cm with the 3% H{sub 2}/(Ar + H{sub 2}) ratio. • AFZO films show high average visible transmittances of above 92%. • Efficiency of a-Si thin film solar cells is improved by AFZO:H as front electrode.

  19. Diamond surface functionalization with biomimicry - Amine surface tether and thiol moiety for electrochemical sensors

    Science.gov (United States)

    Sund, James B.; Causey, Corey P.; Wolter, Scott D.; Parker, Charles B.; Stoner, Brian R.; Toone, Eric J.; Glass, Jeffrey T.

    2014-05-01

    The surface of conducting diamond was functionalized with a terminal thiol group that is capable of binding and detecting nitrogen-oxygen species. The functionalization process employed multiple steps starting with doped diamond films grown by plasma enhanced chemical vapor deposition followed by hydrogen termination and photochemical attachment of a chemically protected amine alkene. The surface tether was deprotected to reveal the amine functionality, which enabled the tether to be extended with surface chemistry to add a terminal thiol moiety for electrochemical sensing applications. Each step of the process was validated using X-ray photoelectron spectroscopy analysis.

  20. Ultra-high wear resistance of ultra-nanocrystalline diamond film: Correlation with microstructure and morphology

    Science.gov (United States)

    Rani, R.; Kumar, N.; Lin, I.-Nan

    2016-05-01

    Nanostructured diamond films are having numerous unique properties including superior tribological behavior which is promising for enhancing energy efficiency and life time of the sliding devices. High wear resistance is the principal criterion for the smooth functioning of any sliding device. Such properties are achievable by tailoring the grain size and grain boundary volume fraction in nanodiamond film. Ultra-nanocrystalline diamond (UNCD) film was attainable using optimized gas plasma condition in a microwave plasma enhanced chemical vapor deposition (MPECVD) system. Crystalline phase of ultra-nanodiamond grains with matrix phase of amorphous carbon and short range ordered graphite are encapsulated in nanowire shaped morphology. Film showed ultra-high wear resistance and frictional stability in micro-tribological contact conditions. The negligible wear of film at the beginning of the tribological contact was later transformed into the wearless regime for prolonged sliding cycles. Both surface roughness and high contact stress were the main reasons of wear at the beginning of sliding cycles. However, the interface gets smoothened due to continuous sliding, finally leaded to the wearless regime.

  1. Physical properties of P and B doped microcrystalline SI:H deposited by PECVD

    International Nuclear Information System (INIS)

    Rubino, A.; Addonizio, M.L.; Conte, G.; Nobile, G.; Terzini, E.

    1993-01-01

    Boron and phosphorus doped high conductivity microcrystalline thin films were deposited in a PECVD reactor. This paper reports conductivities as high as 3 and 41 S/cm for B and P doped materials respectively on films deposited at 210 degrees C. The conductivity, as well as, the microcrystalline fraction increase for the n layer with decreasing RF power, while, for the p material, an increase of power is needed to improve the film characteristics. The conductivity prefactor, as well as, the conductivity itself as a function of the activation energy show a slope inversion for both n and p materials at an activation energy of about 40 meV and 80 meV respectively. Different possible transport mechanisms are examined in order to explain the experimental data

  2. H-terminated polycrystalline boron doped diamond electrode for geochemical sensing into underground components of nuclear repositories

    International Nuclear Information System (INIS)

    Boussadi, A.; Betelu, S.; Ignatiadis, I.; Silva, F.

    2012-01-01

    was 1.5 microns. On the Raman spectrum of a single crystal diamond intrinsic film (undoped), the diamond peak is usually observed at 1332 cm -1 . The intense peak at 1327 cm -1 corresponding to diamond is shifted due to the 'Fano' effect. Its intensity shows that the investigated sample was highly doped. The lack of peak around 1350 cm -1 and 1570 cm -1 , which corresponds respectively to D and G graphite peak of impurity phases of non-diamond carbon (sp2), attests to the crystalline quality of the deposit. The slight width at half maximum of the characteristic peak of diamond compared to that of natural diamond reflects the degree of organization and structural perfection of this phase indicating that the coating was of high quality. Electrodes made in this way have been used for 8 month without any surface treatments or conditioning. The electrochemical behavior of Hydrogen-terminated BDD was studied by cyclic voltammetry. Electrodes showed a wide potential range of about 2 V/SCE. They also showed and a rapid reversible charge transfer in the presence of redox probes such FeCN 6 3 -/4- and Ru(NH) 6 3+/2+ . Performances, reliability and robustness for pH or redox monitoring were examined by potentiometric measurements at 25 C under anaerobic conditions (oxygen-free atmosphere, 100 % nitrogen) in a glove box. Investigation has been limited in pH, ranging from 5.5 to 13.5, close to those encountered in the environment of the nuclear repositories. The feasibility of measuring pH with BDD electrodes was first tested in NH 4 Cl/NH 3 -NaCl buffer solutions, leading to electrode calibration over the widest range of pH, from around neutral to basic pH. Experiments were also conducted in NaHCO 3 /Na 2 CO 3 buffer samples, similar to conditions prevailing in the COx formation. For redox measurements, [Fe 3+ ]/[Fe 2+ ] ratios were analysed at different pH and/or ionic strengths. The same measurements were also done using a 10-mm disk platinum electrode with a surface of 78

  3. Enhanced ultraviolet photo-response in Dy doped ZnO thin film

    Science.gov (United States)

    Kumar, Pawan; Singh, Ranveer; Pandey, Praveen C.

    2018-02-01

    In the present work, a Dy doped ZnO thin film deposited by the spin coating method has been studied for its potential application in a ZnO based UV detector. The investigations on the structural property and surface morphology of the thin film ensure that the prepared samples are crystalline and exhibit a hexagonal crystal structure of ZnO. A small change in crystallite size has been observed due to Dy doping in ZnO. AFM analysis ascertains the grain growth and smooth surface of the thin films. The Dy doped ZnO thin film exhibits a significant enhancement in UV region absorption as compared to the pure ZnO thin film, which suggests that Dy doped ZnO can be used as a UV detector. Under UV irradiation of wavelength 325 nm, the photocurrent value of Dy doped ZnO is 105.54 μA at 4.5 V, which is 31 times greater than that of the un-doped ZnO thin film (3.39 μA). The calculated value of responsivity is found to increase significantly due to the incorporation of Dy in the ZnO lattice. The observed higher value of photocurrent and responsivity could be attributed to the substitution of Dy in the ZnO lattice, which enhances the conductivity, electron mobility, and defects in ZnO and benefits the UV sensing property.

  4. Modification of rubber surface with hydrogenated diamond-like carbon thin films

    NARCIS (Netherlands)

    Pei, Y. T.; Bui, X. L.; De Hosson, J. Th. M.; Laudon, M; Romanowicz, B

    2009-01-01

    Thin films of hydrogenated diamond-like carbon (DLC) have been deposited on hydrogenated nitrile butadiene rubber (HNBR) for reduction of friction and enhancement of wear resistance of dynamic rubber seals, by sputtering graphite targets in C(2)H(2)/Ar plasma. The wax removal and pre-deposition

  5. Study of hard diamond-like carbon films deposited in an inductively coupled plasma source

    International Nuclear Information System (INIS)

    Yu Shiji; Ma Tengcai

    2003-01-01

    Chemical vapor deposition of the hard diamond-like carbon (DLC) films was achieved using an inductively coupled plasma source (ICPS). The microscopy, microhardness, deposition rate and structure characteristic of the DLC films were analyzed. It is shown that the ICPS is suitable for the hard DLC film deposition at relatively low substrate negative bias voltage, and the substrate negative bias voltage greatly affects chemical vapor deposition of the DLC film and its quality

  6. Influence of coil current modulation on polycrystalline diamond film deposition by irradiation of Ar/CH4/H2 inductively coupled thermal plasmas

    Science.gov (United States)

    Betsuin, Toshiki; Tanaka, Yasunori; Arai, T.; Uesugi, Y.; Ishijima, T.

    2018-03-01

    This paper describes the application of an Ar/CH4/H2 inductively coupled thermal plasma with and without coil current modulation to synthesise diamond films. Induction thermal plasma with coil current modulation is referred to as modulated induction thermal plasma (M-ITP), while that without modulation is referred to as non-modulated ITP (NM-ITP). First, spectroscopic observations of NM-ITP and M-ITP with different modulation waveforms were made to estimate the composition in flux from the thermal plasma by measuring the time evolution in the spectral intensity from the species. Secondly, we studied polycrystalline diamond film deposition tests on a Si substrate, and we studied monocrystalline diamond film growth tests using the irradiation of NM-ITP and M-ITP. From these tests, diamond nucleation effects by M-ITP were found. Finally, following the irradiation results, we attempted to use a time-series irradiation of M-ITP and NM-ITP for polycrystalline diamond film deposition on a Si substrate. The results indicated that numerous larger diamond particles were deposited with a high population density on the Si substrate by time-series irradiation.

  7. Enhanced field emission from Si doped nanocrystalline AlN thin films

    International Nuclear Information System (INIS)

    Thapa, R.; Saha, B.; Chattopadhyay, K.K.

    2009-01-01

    Si doped and undoped nanocrystalline aluminum nitride thin films were deposited on various substrates by direct current sputtering technique. X-ray diffraction analysis confirmed the formation of phase pure hexagonal aluminum nitride with a single peak corresponding to (1 0 0) reflection of AlN with lattice constants, a = 0.3114 nm and c = 0.4986 nm. Energy dispersive analysis of X-rays confirmed the presence of Si in the doped AlN films. Atomic force microscopic studies showed that the average particle size of the film prepared at substrate temperature 200 deg. C was 9.5 nm, but when 5 at.% Si was incorporated the average particle size increased to ∼21 nm. Field emission study indicated that, with increasing Si doping concentration, the emission characteristics have been improved. The turn-on field (E to ) was 15.0 (±0.7) V/μm, 8.0 (±0.4) V/μm and 7.8 (±0.5) V/μm for undoped, 3 at.% and 5 at.% Si doped AlN films respectively and the maximum current density of 0.27 μA/cm 2 has been observed for 5 at.% Si doped nanocrystalline AlN film. It was also found that the dielectric properties were highly dependent on Si doping.

  8. Diamond-like carbon films deposited by a hybrid ECRCVD system

    International Nuclear Information System (INIS)

    Guo, C.T.; Dittrich, K.-H.

    2007-01-01

    A novel hybrid technique for diamond-like carbon (DLC) film deposition has been developed. This technique combines the electron cyclotron resonance chemical vapor deposition (ECRCVD) of C 2 H 2 and metallic magnetron sputtering. Here we described how DLC film is used for a variety of applications such as stamper, PCB micro-tools, and threading form-tools by taking advantage of hybrid ECRCVD system. The structure of the DLC films is delineated by a function of bias voltages by Raman spectroscopy. This function includes parameters such as dependence of G peak positions and the intensity ratio (I D /I G ). Atomic force microscope (AFM) examines the root-mean-square (R.M.S.) roughness and the surface morphology. Excellent adhesion and lower friction coefficients of a DLC film were also assessed

  9. Optical and electrochromic properties of sol-gel deposited Ti- doped vanadium oxide films

    International Nuclear Information System (INIS)

    Oezer, N.; Sabuncu, S.

    1997-01-01

    Because of the yellowish color, vanadium oxide films in the as deposited state is not as favorable as transparent coatings for most elector chromic devices. an interesting possibility to alter the yellowish colours is the doping with other non-absorbing metal oxides. Ti doped vanadium oxide films with various amounts of titanium were synthesized and investigated as transparent counter electrodes for electrochromic transmissive device application. Electrochromic titanium doped vanadium pentoxide (V sub 2 O 5) coatings were prepared by the sol-gel dip coating technique. The coating solutions were synthesized from vanadium tri(isopropoxide) precursors. X-ray diffraction (XRD) studies showed that the sol-gel deposited doped films heat treated at temperatures below 350 degree centigrade, were amorphous, whereas hose heat treated at higher temperatures were slight y crystalline. The optical and electrochemical properties of the Ti doped vanadium oxide films has been investigated in 0.1 m LiClO sub 4 propylene carbonate solution color changes by dropping were noted for all investigated films exhibits good electrochemical cycling (CV) measurements also showed that Ti doped V sub 2 O sub 5 films exhibits good electrochemical cycling reversibility, 'in situ' optical measurement revealed that those films exhibits good electrochemical cycling the spectra range 300 < lambda < 800 nm and change color between yellow and light green. The change in visible transmittance was 25 % for 5% Ti doped film. (author)

  10. Enhanced physicochemical properties of polydimethylsiloxane based microfluidic devices and thin films by incorporating synthetic micro-diamond.

    Science.gov (United States)

    Waheed, Sidra; Cabot, Joan M; Macdonald, Niall P; Kalsoom, Umme; Farajikhah, Syamak; Innis, Peter C; Nesterenko, Pavel N; Lewis, Trevor W; Breadmore, Michael C; Paull, Brett

    2017-11-08

    Synthetic micro-diamond-polydimethylsiloxane (PDMS) composite microfluidic chips and thin films were produced using indirect 3D printing and spin coating fabrication techniques. Microfluidic chips containing up to 60 wt% micro-diamond were successfully cast and bonded. Physicochemical properties, including the dispersion pattern, hydrophobicity, chemical structure, elasticity and thermal characteristics of both chip and films were investigated. Scanning electron microscopy indicated that the micro-diamond particles were embedded and interconnected within the bulk material of the cast microfluidic chip, whereas in the case of thin films their increased presence at the polymer surface resulted in a reduced hydrophobicity of the composite. The elastic modulus increased from 1.28 for a PDMS control, to 4.42 MPa for the 60 wt% composite, along with a three-fold increase in thermal conductivity, from 0.15 to 0.45 W m -1 K -1 . Within the fluidic chips, micro-diamond incorporation enhanced heat dissipation by efficient transfer of heat from within the channels to the surrounding substrate. At a flow rate of 1000 μL/min, the gradient achieved for the 60 wt% composite chip equalled a 9.8 °C drop across a 3 cm long channel, more than twice that observed with the PDMS control chip.

  11. Diamond network: template-free fabrication and properties.

    Science.gov (United States)

    Zhuang, Hao; Yang, Nianjun; Fu, Haiyuan; Zhang, Lei; Wang, Chun; Huang, Nan; Jiang, Xin

    2015-03-11

    A porous diamond network with three-dimensionally interconnected pores is of technical importance but difficult to be produced. In this contribution, we demonstrate a simple, controllable, and "template-free" approach to fabricate diamond networks. It combines the deposition of diamond/β-SiC nanocomposite film with a wet-chemical selective etching of the β-SiC phase. The porosity of these networks was tuned from 15 to 68%, determined by the ratio of the β-SiC phase in the composite films. The electrochemical working potential and the reactivity of redox probes on the diamond networks are similar to those of a flat nanocrystalline diamond film, while their surface areas are hundreds of times larger than that of a flat diamond film (e.g., 490-fold enhancement for a 3 μm thick diamond network). The marriage of the unprecedented physical/chemical features of diamond with inherent advantages of the porous structure makes the diamond network a potential candidate for various applications such as water treatment, energy conversion (batteries or fuel cells), and storage (capacitors), as well as electrochemical and biochemical sensing.

  12. Tantalum-doped hydroxyapatite thin films: Synthesis and characterization

    International Nuclear Information System (INIS)

    Ligot, S.; Godfroid, T.; Music, D.; Bousser, E.; Schneider, J.M.; Snyders, R.

    2012-01-01

    To achieve a good bioactivity, magnetron-sputtered (MS) hydroxyapatite (HA) coatings have to be stoichiometric and crystalline. It has also been suggested that doping HA with metallic elements improves its bioactivity but frequently reduces its Young’s modulus. Therefore, efforts are still necessary to identify adequate growth conditions, good doping elements and finally to grow doped HA films. In a first attempt, HA films have been synthesized by MS. Our conditions enabled us to grow at ∼10 nm min −1 stoichiometric and crystallized HA coatings that presented a strong texture. The latter is discussed in view of the competitive growth of the material under the strong electron and ion bombardments used here. Based on ab initio calculations identifying Ta as a promising doping element, we then investigated the growth of Ta-doped hydroxyapatite (HA:Ta) by magnetron co-sputtering. The HA:Ta films were in situ crystallized. Our data reveals that for Ta contents <4.5 at.%, Ta could substitute Ca in the HA cell. For higher doping contents, a deviation from the stoichiometric compound is observed and CaO appears. By nanoindentation, we have measured an elastic modulus of 120 ± 9 GPa for a Ta content of 3 at.%. This value is very close to the value of 110 GPa calculated by ab initio calculations, supporting the substitution scenario. The elasticity drop may be understood by screening of the ionic interaction between constituents in HA upon Ta incorporation.

  13. Structural, morphological and optical properties of spray deposited Mn-doped CeO2 thin films

    International Nuclear Information System (INIS)

    Pavan Kumar, CH.S.S.; Pandeeswari, R.; Jeyaprakash, B.G.

    2014-01-01

    Highlights: • Spray deposited undoped and Mn-doped CeO 2 thin films were polycrystalline. • Complete changeover of surface morphology upon 4 wt% Mn doping. • 4 wt% Mn-doped CeO 2 thin film exhibited a hydrophobic nature. • Optical band-gap decreases beyond 2 wt% Mn doping. - Abstract: Cerium oxide and manganese (Mn) doped cerium oxide thin films on glass substrates were prepared by home built spray pyrolysis system. The effect of Mn doping on the structural, morphological and optical properties of CeO 2 films were studied. It was found that both the undoped and doped CeO 2 films were polycrystalline in nature but the preferential orientation and grain size changed upon doping. Atomic force micrograph showed a complete changeover of surface morphology from spherical to flake upon doping. A water contact angle result displayed the hydrophobic nature of the doped CeO 2 film. Optical properties indicated an increase in band-gap and a decrease in transmittance upon doping owing to Moss–Burstein effect and inverse Moss–Burstein effects. Other optical properties such as refractive index, extinction coefficient and dielectric constant as a function of doping were analysed and reported

  14. Diamond films on stainless steel substrates with an interlayer applied by laser cladding

    Energy Technology Data Exchange (ETDEWEB)

    Contin, Andre; Alves, Kenya Aparecida; Damm, Djoille Denner; Trava-Airoldi, Vladimir Jesus; Corat, Evaldo Jose, E-mail: andrecontin@yahoo.com.br [Instituto Nacional de Pesquisas Espaciais (LAS/INPE), Sao Jose dos Campos, SP (Brazil). Laboratorio Associado de Sensores e Materiais; Campos, Raonei Alves [Universidade Federal do Sul e Sudeste do Para (UNIFESSPA), Maraba, PA (Brazil); Vasconcelos, Getulio de [Instituto de Estudos Avancados (DedALO/IEAv), Sao Jose dos Campos, SP (Brazil). Laboratorio de Desenvolvimento de Aplicacoes de Lasers e Optica

    2017-03-15

    The objective of this work is the Hot Filament Chemical Vapor Deposition (HFCVD) of diamond films on stainless steel substrates using a new technique for intermediate barrier forming, made by laser cladding process. In this technique, a powder layer is irradiated by a laser beam to melt the powder layer and the substrate surface layer to create the interlayer. The control of the laser beam parameters allows creating homogeneous coating layers, in rather large area in few seconds. In this work, the silicon carbide powder (SiC) was used to create an intermediate layer. Before the diamond growth, the samples were subjected to the seeding process with diamond powder. The diamond deposition was performed using Hot-Filament CVD reactor and the characterizations were Scanning Electron Microscopy, X-ray diffraction, Raman Scattering Spectroscopy and Scratch Test. (author)

  15. Improvement in the degradation resistance of silicon nanostructures by the deposition of diamond-like carbon films

    Energy Technology Data Exchange (ETDEWEB)

    Klyui, N. I., E-mail: klyui@isp.kiev.ua; Semenenko, M. A.; Khatsevich, I. M.; Makarov, A. V.; Kabaldin, A. N. [National Academy of Sciences of Ukraine, Lashkarev Institute of Semiconductor Physics (Ukraine); Fomovskii, F. V. [Kremenchug National University (Ukraine); Han, Wei [Jilin University, College of Physics (China)

    2015-08-15

    It is established that the deposition of a diamond-like film onto a structure with silicon nanoclusters in a silicon dioxide matrix yields an increase in the long-wavelength photoluminescence intensity of silicon nanoclusters due to the passivation of active-recombination centers with hydrogen and a shift of the photoluminescence peak to the region of higher photosensitivity of silicon-based solar cells. It is also shown that, due to the deposited diamond-like film, the resistance of such a structure to degradation upon exposure to γ radiation is improved, which is also defined by the effect of the passivation of radiation-induced activerecombination centers by hydrogen that is released from the films during treatment.

  16. Diamond: a material for acoustic devices

    OpenAIRE

    MORTET, Vincent; WILLIAMS, Oliver; HAENEN, Ken

    2008-01-01

    Diamond has been foreseen to replace silicon for high power, high frequency electronic applications or for devices that operates in harsh environments. However, diamond electronic devices are still in the laboratory stage due to the lack of large substrates and the complexity of diamond doping. On another hand, surface acoustic wave filters based on diamond are commercially available. Diamond is especially suited for acoustic applications because of its exceptional mechanical properties. The ...

  17. A short literature survey on iron and cobalt ion doped TiO2 thin films and photocatalytic activity of these films against fungi

    International Nuclear Information System (INIS)

    Tatlıdil, İlknur; Bacaksız, Emin; Buruk, Celal Kurtuluş; Breen, Chris; Sökmen, Münevver

    2012-01-01

    Highlights: ► Co or Fe doped TiO 2 thin films were prepared by sol–gel method. ► We obtained lower E g values for Fe-doped and Co-TiO 2 thin films. ► Doping greatly affected the size and shape of the TiO 2 nanoparticles. ► Photocatalytic killing effect of the doped TiO 2 thin films on C. albicans and A. niger was significantly higher than undoped TiO 2 thin film for short exposure periods. - Abstract: In this study, a short recent literature survey which concentrated on the usage of Fe 3+ or Co 2+ ion doped TiO 2 thin films and suspensions were summarized. Additionally, a sol–gel method was used for preparation of the 2% Co or Fe doped TiO 2 thin films. The surface of the prepared materials was characterised using scanning-electron microscopy (SEM) combined with energy dispersive X-ray (EDX) analysis and band gap of the films were calculated from the transmission measurements that were taken over the range of 190 and 1100 nm. The E g value was 3.40 eV for the pure TiO 2 , 3.00 eV for the Fe-doped TiO 2 film and 3.25 eV for Co-TiO 2 thin film. Iron or cobalt doping at lower concentration produce more uniformed particles and doping greatly affected the size and shape of the TiO 2 nanoparticles. Photocatalytic killing effect of the 2% Co doped TiO 2 thin film on Candida albicans was significantly higher than Fe doped TiO 2 thin film for short and long exposure periods. Doped thin films were more effective on Aspergillus niger for short exposure periods.

  18. Microcrystalline diamond cylindrical resonators with quality-factor up to 0.5 million

    Energy Technology Data Exchange (ETDEWEB)

    Saito, Daisuke; Yang, Chen; Lin, Liwei [Department of Mechanical Engineering, University of California, Berkeley, California 94720 (United States); Heidari, Amir [Department of Mechanical and Aerospace Engineering, University of California, Davis, California 95616 (United States); Najar, Hadi [Department of Electrical and Computer Engineering, University of California, Davis, California 95616 (United States); Horsley, David A. [Department of Mechanical and Aerospace Engineering, University of California, Davis, California 95616 (United States); Department of Electrical and Computer Engineering, University of California, Davis, California 95616 (United States)

    2016-02-01

    We demonstrate high quality-factor 1.5 mm diameter batch-fabricated microcrystalline diamond cylindrical resonators (CR) with quality-factors limited by thermoelastic damping (TED) and surface loss. Resonators were fabricated 2.6 and 5.3 μm thick in-situ boron-doped microcrystalline diamond films deposited using hot filament chemical vapor deposition. The quality-factor (Q) of as-fabricated CR's was found to increase with the resonator diameter and diamond thickness. Annealing the CRs at 700 °C in a nitrogen atmosphere led to a three-fold increase in Q, a result we attribute to thinning of the diamond layer via reaction with residual O{sub 2} in the annealing furnace. Post-anneal Q exceeding 0.5 million (528 000) was measured at the 19 kHz elliptical wineglass modes, producing a ring-down time of 8.9 s. A model for Q versus diamond thickness and resonance frequency is developed including the effects of TED and surface loss. Measured quality factors are shown to agree with the predictions of this model.

  19. Thermally stimulated currents in polycrystalline diamond films and their application to ultraviolet dosimetry

    International Nuclear Information System (INIS)

    Trajkov, E.; Prawer, S.

    1999-01-01

    Quantifying individual exposure to solar ultraviolet radiation (UVR) is imperative to understanding the epidemiology of UVR related skin cancer. The development of personal UVR dosimeters is hence essential for obtaining data regarding individual UVR exposure, which can then be used to establish appropriate protective measures for occupational and recreational exposure. Because diamond is a tissue equivalent material and has a wide band-gap, CVD polycrystalline diamond has been proposed for use in solar-blind UV dosimetry. It has been reported that the photoconductivity in polycrystalline diamond films is enhanced after UV illumination Photo-generated carriers can be trapped at some deep levels after illumination. Because these levels are deep the thermal release of carriers is a slow process at room temperature. Therefore the new carrier distribution reached after illumination can result in a metastable state because the temperature is too low to restore the initial equilibrium. The sample can be bought back to initial equilibrium by heating. If the current is recorded during heating of the samples one can observe current peaks corresponding to the thermal release of trapped carriers, the so-called thermally stimulated currents (TSC). From first-order kinetics, we find that the TSC intensity is proportional to the initial density of trapped carriers, n to . Since n to varies with the radiation dose, the measurement of TSC can find an application in radiation dosimetry since the measurement of TSC gives a direct measure of that dose. Nitrogen can be used to introduce deep traps in diamond. This investigation will involve examining the affect of the nitrogen concentration on the irradiation response of the films. Furthermore, we will analyse the fading rate of the TSC signal. If diamond films are to have a practical application in UVR dosimetry, then ideally we require a linear relationship between the dose response and the TSC, and we also require a low fading rate

  20. Microarray of neuroblastoma cells on the selectively functionalized nanocrystalline diamond thin film surface

    International Nuclear Information System (INIS)

    Park, Young-Sang; Son, Hyeong-Guk; Kim, Dae-Hoon; Oh, Hong-Gi; Lee, Da-Som; Kim, Min-Hye; Lim, Ki-Moo; Song, Kwang-Soup

    2016-01-01

    Graphical abstract: - Highlights: • The nanocrystalline diamond (NCD) surface is functionalized with F or O. • The cell adhesion and growth are evaluated on the functionalized NCD surface. • The cell adhesion and growth depend on the wettability of the surface. • Cell patterning was achieved by using of hydrophilic and hydrophobic surfaces. • Neuroblastoma cells were arrayed on the micro-patterned NCD surface. - Abstract: Nanocrystalline diamond (NCD) film surfaces were modified with fluorine or oxygen by plasma treatment in an O_2 or C_3F_8 gas environment in order to induce wettability. The oxygenated-NCD (O-NCD) film surface was hydrophilic and the fluorinated-NCD (F-NCD) surface was hydrophobic. The efficiency of early cell adhesion, which is dependent on the wettability of the cell culture plate and necessary for the growth and proliferation of cells, was 89.62 ± 3.92% on the O-NCD film and 7.78 ± 0.77% on the F-NCD film surface after 3 h of cell culture. The wettability of the NCD film surface was artificially modified using a metal mask and plasma treatment to fabricate a micro-pattern. Four types of micro-patterns were fabricated (line, circle, mesh, and word) on the NCD film surface. We precisely arrayed the neuroblastoma cells on the micro-patterned NCD film surfaces by controlling the surface wettability and cell seeding density. The neuroblastoma cells adhered and proliferated along the O-NCD film surface.

  1. Microarray of neuroblastoma cells on the selectively functionalized nanocrystalline diamond thin film surface

    Energy Technology Data Exchange (ETDEWEB)

    Park, Young-Sang; Son, Hyeong-Guk; Kim, Dae-Hoon; Oh, Hong-Gi; Lee, Da-Som; Kim, Min-Hye; Lim, Ki-Moo; Song, Kwang-Soup, E-mail: kssong10@kumoh.ac.kr

    2016-01-15

    Graphical abstract: - Highlights: • The nanocrystalline diamond (NCD) surface is functionalized with F or O. • The cell adhesion and growth are evaluated on the functionalized NCD surface. • The cell adhesion and growth depend on the wettability of the surface. • Cell patterning was achieved by using of hydrophilic and hydrophobic surfaces. • Neuroblastoma cells were arrayed on the micro-patterned NCD surface. - Abstract: Nanocrystalline diamond (NCD) film surfaces were modified with fluorine or oxygen by plasma treatment in an O{sub 2} or C{sub 3}F{sub 8} gas environment in order to induce wettability. The oxygenated-NCD (O-NCD) film surface was hydrophilic and the fluorinated-NCD (F-NCD) surface was hydrophobic. The efficiency of early cell adhesion, which is dependent on the wettability of the cell culture plate and necessary for the growth and proliferation of cells, was 89.62 ± 3.92% on the O-NCD film and 7.78 ± 0.77% on the F-NCD film surface after 3 h of cell culture. The wettability of the NCD film surface was artificially modified using a metal mask and plasma treatment to fabricate a micro-pattern. Four types of micro-patterns were fabricated (line, circle, mesh, and word) on the NCD film surface. We precisely arrayed the neuroblastoma cells on the micro-patterned NCD film surfaces by controlling the surface wettability and cell seeding density. The neuroblastoma cells adhered and proliferated along the O-NCD film surface.

  2. Nitrogen-doped graphene films from simple photochemical doping for n-type field-effect transistors

    Energy Technology Data Exchange (ETDEWEB)

    Li, Xinyu [College of Science, Guilin University of Technology, Guilin 541004 (China); Department of Physics and Nanjing National Laboratory of Microstructures, Nanjing University, Nanjing 210093 (China); Tang, Tao; Li, Ming, E-mail: liming928@163.com, E-mail: lixinyu5260@163.com [College of Science, Guilin University of Technology, Guilin 541004 (China); He, Xiancong, E-mail: liming928@163.com, E-mail: lixinyu5260@163.com [School of Materials Science and Engineering, Nanjing Institute of Technology, Nanjing 211167 (China)

    2015-01-05

    Highly nitrogen-doped GO (NGO) and n-type graphene field effect transistor (FET) have been achieved by simple irradiation of graphene oxide (GO) thin films in NH{sub 3} atmosphere. The electrical properties of the NGO film were performed on electric field effect measurements, and it displays an n-type FET behavior with a charge neutral point (Dirac point) located at around −8 V. It is suggested that the amino-like nitrogen (N-A) mainly contributes to the n-type behavior. Furthermore, compared to the GO film irradiated in Ar atmosphere, the NGO film is much more capable to improve the electrical conductivity. It may attribute to nitrogen doping and oxygen reduction, both of which can effectively enhance the electrical conductivity.

  3. Electronic Power System Application of Diamond-Like Carbon Films

    Science.gov (United States)

    Wu, Richard L. C.; Kosai, H.; Fries-Carr, S.; Weimer, J.; Freeman, M.; Schwarze, G. E.

    2003-01-01

    A prototype manufacturing technology for producing high volume efficiency and high energy density diamond-like carbon (DLC) capacitors has been developed. Unique dual ion-beam deposition and web-handling systems have been designed and constructed to deposit high quality DLC films simultaneously on both sides of capacitor grade aluminum foil and aluminum-coated polymer films. An optimized process, using inductively coupled RF ion sources, has been used to synthesize electrically robust DLC films. DLC films are amorphous and highly flexible, making them suitable for the production of wound capacitors. DLC capacitors are reliable and stable over a wide range of AC frequencies from 20 Hz to 1 MHz, and over a temperature range from .500 C to 3000 C. The compact DLC capacitors offer at least a 50% decrease in weight and volume and a greater than 50% increase in temperature handling capability over equal value capacitors built with existing technologies. The DLC capacitors will be suitable for high temperature, high voltage, pulsed power and filter applications.

  4. Vertically aligned nanowires from boron-doped diamond.

    Science.gov (United States)

    Yang, Nianjun; Uetsuka, Hiroshi; Osawa, Eiji; Nebel, Christoph E

    2008-11-01

    Vertically aligned diamond nanowires with controlled geometrical properties like length and distance between wires were fabricated by use of nanodiamond particles as a hard mask and by use of reactive ion etching. The surface structure, electronic properties, and electrochemical functionalization of diamond nanowires were characterized by atomic force microscopy (AFM) and scanning tunneling microscopy (STM) as well as electrochemical techniques. AFM and STM experiments show that diamond nanowire etched for 10 s have wire-typed structures with 3-10 nm in length and with typically 11 nm spacing in between. The electrode active area of diamond nanowires is enhanced by a factor of 2. The functionalization of nanowire tips with nitrophenyl molecules is characterized by STM on clean and on nitrophenyl molecule-modified diamond nanowires. Tip-modified diamond nanowires are promising with respect to biosensor applications where controlled biomolecule bonding is required to improve chemical stability and sensing significantly.

  5. Structural and X-Ray Photoelectron Spectroscopy Study of Al-Doped Zinc-Oxide Thin Films

    Directory of Open Access Journals (Sweden)

    Bong Ju Lee

    2015-01-01

    Full Text Available Al-doped zinc-oxide (AZO thin films were prepared by RF magnetron sputtering at different oxygen partial pressures and substrate temperatures. The charge-carrier concentrations in the films decreased from 1.69 × 1021 to 6.16 × 1017 cm−3 with increased gas flow rate from 7 to 21 sccm. The X-ray diffraction (XRD patterns show that the (002/(103 peak-intensity ratio decreased as the gas flow rate increased, which was related to the increase of AZO thin film disorder. X-ray photoelectron spectra (XPS of the O1s were decomposed into metal oxide component (peak A and the adsorbed molecular oxygen on thin films (peak B. The area ratio of XPS peaks (A/B was clearly related to the stoichiometry of AZO films; that is, the higher value of A/B showed the higher stoichiometric properties.

  6. Properties of antimony doped ZnO thin films deposited by spray pyrolysis technique

    Energy Technology Data Exchange (ETDEWEB)

    Sadananda Kumar, N., E-mail: sadanthara@gmail.com; Bangera, Kasturi V.; Shivakumar, G. K. [National Institute of Technology Karnataka, Surathkal, Thin Films Laboratory, Department of Physics (India)

    2015-07-15

    Antimony (Sb) doped zinc oxide (ZnO) thin films were deposited on the glass substrate at 450°C using spray pyrolysis technique. Effect of Sb doping on surface morphology structural, optical and electrical properties were studied. X-ray diffraction (XRD) analysis showed that both the undoped and doped ZnO thin films are polycrystalline in nature with (101) preferred orientation. SEM analysis showed a change in surface morphology of Sb doped ZnO thin films. Doping results in a marked increase in conductivity without affecting the transmittance of the films. ZnO films prepared with 3 at % Sb shows the lowest resistivity of 0.185 Ohm cm with a Hall mobility of 54.05 cm{sup 2} V{sup –1} s{sup –1}, and a hole concentration of 6.25 × 10{sup 17} cm{sup –3}.

  7. Screening metal nanoparticles using boron-doped diamond microelectrodes

    Energy Technology Data Exchange (ETDEWEB)

    Ivandini, Tribidasari A., E-mail: ivandini.tri@sci.ui.ac.id; Rangkuti, Prasmita K. [Department of Chemistry, FMIPA, Universitas Indonesia, Kampus UI Depok (Indonesia); Einaga, Yasuaki [Department of Chemistry, Faculty of Science and Technology, Keio University (Japan); JST ACCEL, 3-14-1 Hiyoshi, Yokohama 223-8522 (Japan)

    2016-04-19

    Boron-doped diamond (BDD) microelectrodes were used to observe the correlation between electrocatalytic currents caused by individual Pt nanoparticle (Pt-np) collisions at the electrode. The BDD microelectrodes, ∼20 µm diameter and ∼2 µm particle size, were fabricated at the surface of tungsten wires. Pt-np with a size of 1 to 5 nm with agglomerations up to 20 nm was used for observation. The electrolytic currents were observed via catalytic reaction of 15 mM hydrazine in 50 mM phosphate buffer solution at Pt-np at 0.4 V when it collides with the surface of the microelectrodes. The low current noise and wider potential window in the measurements using BDD microelectrode produced a better results, which represents a better correlation to the TEM result of the Pt-np, compared to when gold microelectrodes was used.

  8. Screening metal nanoparticles using boron-doped diamond microelectrodes

    International Nuclear Information System (INIS)

    Ivandini, Tribidasari A.; Rangkuti, Prasmita K.; Einaga, Yasuaki

    2016-01-01

    Boron-doped diamond (BDD) microelectrodes were used to observe the correlation between electrocatalytic currents caused by individual Pt nanoparticle (Pt-np) collisions at the electrode. The BDD microelectrodes, ∼20 µm diameter and ∼2 µm particle size, were fabricated at the surface of tungsten wires. Pt-np with a size of 1 to 5 nm with agglomerations up to 20 nm was used for observation. The electrolytic currents were observed via catalytic reaction of 15 mM hydrazine in 50 mM phosphate buffer solution at Pt-np at 0.4 V when it collides with the surface of the microelectrodes. The low current noise and wider potential window in the measurements using BDD microelectrode produced a better results, which represents a better correlation to the TEM result of the Pt-np, compared to when gold microelectrodes was used.

  9. Thermal characterization of polycrystalline diamond thin film heat spreaders grown on GaN HEMTs

    Science.gov (United States)

    Zhou, Yan; Ramaneti, Rajesh; Anaya, Julian; Korneychuk, Svetlana; Derluyn, Joff; Sun, Huarui; Pomeroy, James; Verbeeck, Johan; Haenen, Ken; Kuball, Martin

    2017-07-01

    Polycrystalline diamond (PCD) was grown onto high-k dielectric passivated AlGaN/GaN-on-Si high electron mobility transistor (HEMT) structures, with film thicknesses ranging from 155 to 1000 nm. Transient thermoreflectance results were combined with device thermal simulations to investigate the heat spreading benefit of the diamond layer. The observed thermal conductivity (κDia) of PCD films is one-to-two orders of magnitude lower than that of bulk PCD and exhibits a strong layer thickness dependence, which is attributed to the grain size evolution. The films exhibit a weak temperature dependence of κDia in the measured 25-225 °C range. Device simulation using the experimental κDia and thermal boundary resistance values predicts at best a 15% reduction in peak temperature when the source-drain opening of a passivated AlGaN/GaN-on-Si HEMT is overgrown with PCD.

  10. Silicon and aluminum doping effects on the microstructure and properties of polymeric amorphous carbon films

    Energy Technology Data Exchange (ETDEWEB)

    Liu, Xiaoqiang, E-mail: lxq_suse@sina.com [Material Corrosion and Protection Key Laboratory of Sichuan province, Sichuan University of Science and Engineering, Zigong 643000 (China); Hao, Junying, E-mail: jyhao@licp.cas.cn [State Key Laboratory of Solid Lubrication, Lanzhou Institute of Chemical Physics, Chinese Academy of Sciences, Lanzhou 730000 (China); Xie, Yuntao [Material Corrosion and Protection Key Laboratory of Sichuan province, Sichuan University of Science and Engineering, Zigong 643000 (China)

    2016-08-30

    Highlights: • Evolution of nanostructure and properties of the polymeric amorphous carbon films were firstly studied. • Si doping enhanced polymerization of the hydrocarbon chains and Al doping resulted in increase in the ordered carbon clusters of polymeric amorphous carbon films. • Soft polymeric amorphous carbon films exhibited an unconventional frictional behaviors with a superior wear resistance. • The mechanical and vacuum tribological properties of the polymeric amorphous carbon films were significantly improved by Si and Al co-doping. - Abstract: Polymeric amorphous carbon films were prepared by radio frequency (R.F. 13.56 MHz) magnetron sputtering deposition. The microstructure evolution of the deposited polymeric films induced by silicon (Si) and aluminum(Al) doping were scrutinized through infrared spectroscopy, multi-wavelength Raman spectroscopy, scanning electron microscopy (SEM) and high resolution transmission electron microscopy (HRTEM). The comparative results show that Si doping can enhance polymerization and Al doping results in an increase in the ordered carbon clusters. Si and Al co-doping into polymeric films leads to the formation of an unusual dual nanostructure consisting of cross-linked polymer-like hydrocarbon chains and fullerene-like carbon clusters. The super-high elasticity and super-low friction coefficients (<0.002) under a high vacuum were obtained through Si and Al co-doping into the films. Unconventionally, the co-doped polymeric films exhibited a superior wear resistance even though they were very soft. The relationship between the microstructure and properties of the polymeric amorphous carbon films with different elements doping are also discussed in detail.

  11. Chromium-doped diamond-like carbon films deposited by dual-pulsed laser deposition

    Czech Academy of Sciences Publication Activity Database

    Písařík, Petr; Jelínek, Miroslav; Kocourek, Tomáš; Zezulová, M.; Remsa, Jan; Jurek, Karel

    2014-01-01

    Roč. 117, č. 1 (2014), s. 83-88 ISSN 0947-8396 R&D Projects: GA MŠk LD12069 Institutional support: RVO:68378271 Keywords : diamond like carbon * chromium * contact angle * surface free energy * dual laser deposition * zeta potential Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 1.704, year: 2014

  12. Effect of La doping on crystalline orientation, microstructure and dielectric properties of PZT thin films

    Energy Technology Data Exchange (ETDEWEB)

    Xu, Wencai; Li, Qi; Wang, Xing [Dalian Univ. of Technology, Dalian (China). School of Mechanical Engineering; Yin, Zhifu [Jilin Univ., Changchun (China). Faculty of the School of Mechanical Science and Engineering; Zou, Helin [Dalian Univ. of Technology, Dalian (China). Key Lab. for Micro/Nano Systems and Technology

    2017-11-01

    Lanthanum (La)-modified lead zirconate titanate (PLZT) thin films with doping concentration from 0 to 5 at.-% have been fabricated by sol-gel methods to investigate the effects of La doping on crystalline orientation, microstructure and dielectric properties of the modified films. The characterization of PLZT thin films were performed by X-ray diffractometry (XRD), scanning electron microscopy (SEM) and precision impedance analysis. XRD analysis showed that PLZT films with La doping concentration below 4 at.-% exhibited (100) preferred orientation. SEM results indicated that PLZT films presented dense and columnar microstructures when La doping concentration was less than 3 at.-%, while the others showed columnar microstructures only at the bottom of the cross section. The maximum dielectric constant (1502.59 at 100 Hz) was obtained in a 2 at.-% La-doped film, which increased by 53.9 % compared with undoped film. Without introducing a seed layer, (100) oriented PLZT thin films were prepared by using conventional heat treatment process and adjusting La doping concentration.

  13. Comparison of the surface properties of DLC and ultrananocrystalline diamond films with respect to their bio-applications

    Czech Academy of Sciences Publication Activity Database

    Jelínek, Miroslav; Voss, A.; Kocourek, Tomáš; Mozafari, M.; Vymětalová, V.; Zezulová, Markéta; Písařík, Petr; Kotzianová, A.; Popov, C.; Mikšovský, Jan

    2014-01-01

    Roč. 210, č. 10 (2014), 2106-2110 ISSN 1862-6300 R&D Projects: GA MŠk LD12069 Institutional support: RVO:68378271 Keywords : antibacterial tests * diamond-like carbon * surface properties * ultrananocrystalline diamond films Subject RIV: BM - Solid Matter Physics ; Magnetism Impact factor: 1.616, year: 2014

  14. Electrochemical applications of CVD diamond

    International Nuclear Information System (INIS)

    Pastor-Moreno, Gustavo

    2002-01-01

    Diamond technology has claimed an important role in industry since non-expensive methods of synthesis such as chemical vapour deposition allow to elaborate cheap polycrystalline diamond. This fact has increased the interest in the scientific community due to the outstanding properties of diamond. Since Pleskov published in 1987 the first paper in electrochemistry, many researchers around the world have studied different aspects of diamond electrochemistry such as reactivity, electrical structure, etc. As part of this worldwide interest these studies reveal new information about diamond electrodes. These studies report investigation of diamond electrodes characterized using structural techniques like scanning electrode microscopy and Raman spectroscopy. A new electrochemical theory based on surface states is presented that explains the metal and the semiconductor behaviour in terms of the doping level of the diamond electrode. In an effort to characterise the properties of diamond electrodes the band edges for hydrogen and oxygen terminated surface are located in organic solvent, hence avoiding possible interference that are present in aqueous solution. The determination of the band edges is performed by Mott-Schottky studies. These allow the calculation of the flat band potential and therefore the band edges. Additional cyclic voltammetric studies are presented for both types of surface termination. Mott-Schottky data and cyclic voltammograms are compared and explained in terms of the band edge localisation. Non-degenerately p-type semiconductor behaviour is presented for hydrogen terminated boron doped diamond. Graphitic surface states on oxidised surface boron doped diamond are responsible for the electrochemistry of redox couples that posses similar energy. Using the simple redox couple 1,4-benzoquinone effect of surface termination on the chemical behaviour of diamond is presented. Hydrogen sublayers in diamond electrodes seem to play an important role for the

  15. Silicon solar cell performance deposited by diamond like carbon thin film ;Atomic oxygen effects;

    Science.gov (United States)

    Aghaei, Abbas Ail; Eshaghi, Akbar; Karami, Esmaeil

    2017-09-01

    In this research, a diamond-like carbon thin film was deposited on p-type polycrystalline silicon solar cell via plasma-enhanced chemical vapor deposition method by using methane and hydrogen gases. The effect of atomic oxygen on the functioning of silicon coated DLC thin film and silicon was investigated. Raman spectroscopy, field emission scanning electron microscopy, atomic force microscopy and attenuated total reflection-Fourier transform infrared spectroscopy were used to characterize the structure and morphology of the DLC thin film. Photocurrent-voltage characteristics of the silicon solar cell were carried out using a solar simulator. The results showed that atomic oxygen exposure induced the including oxidation, structural changes, cross-linking reactions and bond breaking of the DLC film; thus reducing the optical properties. The photocurrent-voltage characteristics showed that although the properties of the fabricated thin film were decreased after being exposed to destructive rays, when compared with solar cell without any coating, it could protect it in atomic oxygen condition enhancing solar cell efficiency up to 12%. Thus, it can be said that diamond-like carbon thin layer protect the solar cell against atomic oxygen exposure.

  16. Oxygen plasma etching of silver-incorporated diamond-like carbon films

    International Nuclear Information System (INIS)

    Marciano, F.R.; Bonetti, L.F.; Pessoa, R.S.; Massi, M.; Santos, L.V.; Trava-Airoldi, V.J.

    2009-01-01

    Diamond-like carbon (DLC) film as a solid lubricant coating represents an important area of investigation related to space devices. The environment for such devices involves high vacuum and high concentration of atomic oxygen. The purpose of this paper is to study the behavior of silver-incorporated DLC thin films against oxygen plasma etching. Silver nanoparticles were produced through an electrochemical process and incorporated into DLC bulk during the deposition process using plasma enhanced chemical vapor deposition technique. The presence of silver does not affect significantly DLC quality and reduces by more than 50% the oxygen plasma etching. Our results demonstrated that silver nanoparticles protect DLC films against etching process, which may increase their lifetime in low earth orbit environment.

  17. Oxygen plasma etching of silver-incorporated diamond-like carbon films

    Energy Technology Data Exchange (ETDEWEB)

    Marciano, F.R., E-mail: fernanda@las.inpe.b [Instituto Nacional de Pesquisas Espaciais (INPE), Laboratorio Associado de Sensores e Materiais (LAS), Av. dos Astronautas 1758, Sao Jose dos Campos, 12227-010, SP (Brazil); Instituto Tecnologico de Aeronautica (ITA), Centro Tecnico Aeroespacial (CTA), Pca. Marechal Eduardo Gomes, 50-Sao Jose dos Campos, 12228-900, SP (Brazil); Bonetti, L.F. [Clorovale Diamantes Industria e Comercio Ltda, Estr. do Torrao de Ouro, 500-Sao Jose dos Campos, 12229-390, SP (Brazil); Pessoa, R.S.; Massi, M. [Instituto Tecnologico de Aeronautica (ITA), Centro Tecnico Aeroespacial (CTA), Pca. Marechal Eduardo Gomes, 50-Sao Jose dos Campos, 12228-900, SP (Brazil); Santos, L.V.; Trava-Airoldi, V.J. [Instituto Nacional de Pesquisas Espaciais (INPE), Laboratorio Associado de Sensores e Materiais (LAS), Av. dos Astronautas 1758, Sao Jose dos Campos, 12227-010, SP (Brazil)

    2009-08-03

    Diamond-like carbon (DLC) film as a solid lubricant coating represents an important area of investigation related to space devices. The environment for such devices involves high vacuum and high concentration of atomic oxygen. The purpose of this paper is to study the behavior of silver-incorporated DLC thin films against oxygen plasma etching. Silver nanoparticles were produced through an electrochemical process and incorporated into DLC bulk during the deposition process using plasma enhanced chemical vapor deposition technique. The presence of silver does not affect significantly DLC quality and reduces by more than 50% the oxygen plasma etching. Our results demonstrated that silver nanoparticles protect DLC films against etching process, which may increase their lifetime in low earth orbit environment.

  18. Flexible diamond-like carbon thin film coated rubbers: fundamentals and applications

    NARCIS (Netherlands)

    Pei, Y.T.

    2015-01-01

    Dynamic rubber seals are major sources of friction of lubrication systems and bearings, which may take up to 75% of the total friction. The solution we present is to coat rubbers with diamond-like carbon (DLC) thin film, by which the coefficient of friction is reduced to less than one tenth. Coating

  19. Structural and optical properties of Na-doped ZnO films

    Science.gov (United States)

    Akcan, D.; Gungor, A.; Arda, L.

    2018-06-01

    Zn1-xNaxO (x = 0.0-0.05) solutions have been synthesized by the sol-gel technique using Zinc acetate dihydrate and Sodium acetate which were dissolved into solvent and chelating agent. Na-doped ZnO nanoparticles were obtained from solutions to find phase and crystal structure. Na-doped ZnO films have been deposited onto glass substrate by using sol-gel dip coating system. The effects of dopant concentration on the structure, morphology, and optical properties of Na-doped ZnO thin films deposited on glass substrate are investigated. Characterization of Zn1-xNaxO nanoparticles and thin films are examined using differential thermal analysis (DTA)/thermogravimetric analysis (TGA), Scanning electron microscope (SEM) and X-Ray diffractometer (XRD). Optical properties of Zn1-xNaxO thin films were obtained by using PG Instruments UV-Vis-NIR spectrophotometer in 190-1100 nm range. The structure, morphology, and optical properties of thin films are presented.

  20. Local Electrical Response in Alkaline-Doped Electrodeposited CuInSe2/Cu Films

    Directory of Open Access Journals (Sweden)

    Javier A. Barón-Miranda

    2016-12-01

    Full Text Available The local electrical response in alkaline-doped CuInSe2 films prepared by single-step electrodeposition onto Cu substrates was studied by current-sensing atomic force microscopy. The CuInSe2 (CIS films were prepared from single baths containing the dopant ions (Li, Na, K or Cs and were studied by X-ray diffraction, scanning electron microscopy, energy dispersive X-ray spectroscopy and photocurrent response. Increased crystallinity and surface texturing as the ion size increased were observed, as well as an enhanced photocurrent response in Cs-doped CIS. Li- and Na-doped films had larger conductivity than the undoped film while the K- and Cs-doped samples displayed shorter currents and the current images indicated strong charge accumulation in the K- and Cs-doped films, forming surface capacitors. Corrected current-sensing AFM IV curves were adjusted with the Shockley equation.