  1. Paleodosimetrical properties of sodium alkali feldspars and problems of luminescence dating of sediments

    International Nuclear Information System (INIS)

    Huett, Galina; Jaek, Ivar

    1996-01-01

    Emission spectra of natural alkali feldspars extracted from sediments are studied using a CCD-camera based high sensitivity spectrometer. Applying a semiconductor laser (860± 1 nm), two dominant emission bands, blue (410 nm) and orange (570 nm), are revealed in infrared optically stimulated luminescence (IROSL) spectra for the most of the sediments from Scandinavian sections. Luminescence and dosimetric al properties of the hole traps, the induced orange emission band typical of sodium alkali feldspars are studied. As a result, high light bleach ability but low stability of the dosimetric al information lit sodium alkali feldspars are established. Problems of luminescence dating of sediments based on the mixture of potassium-sodium alkali feldspars are discussed. (author)

  2. Optically stimulated luminescence characteristics of natural and doped quartz and alkali feldspars

    Energy Technology Data Exchange (ETDEWEB)

    Huett, G.; Jaek, I.; Brodski, L. [Institute of Geology at Tallinn Technical University, Tallinn (Estonia); Vasilchenko, V. [Institute of Experimental Physics and Technology of Tartu University, Tartu (Estonia)

    1999-05-01

    Natural alkali feldspars and quartz were doped by Tl and Cu by thermodiffusion and electrodiffusion technology. As a result of doping, intensive UV emission bands were created. The OSL stimulation spectra of irradiated natural and doped quartz and alkali feldspars were measured in the span of 400-1300 nm using UV emission of Tl at 280 nm and of Cu at 380 nm. One-trap centre conception was confirmed for high-temperature palaeodosimetrical TL peaks and OSL stimulation spectrum bands: for alkali feldspars at 880 and 420 nm and visible region of the spectrum for quartz. A thermooptical mechanism of the optical depopulation of the corresponding trap is confirmed in alkali feldspars, but there is no evidence for processes of this kind in quartz. An analogy between the physical background of OSL properties of both minerals is discussed.

  3. Optically stimulated luminescence characteristics of natural and doped quartz and alkali feldspars

    International Nuclear Information System (INIS)

    Huett, G.; Jaek, I.; Brodski, L.; Vasilchenko, V.

    1999-01-01

    Natural alkali feldspars and quartz were doped by Tl and Cu by thermodiffusion and electrodiffusion technology. As a result of doping, intensive UV emission bands were created. The OSL stimulation spectra of irradiated natural and doped quartz and alkali feldspars were measured in the span of 400-1300 nm using UV emission of Tl at 280 nm and of Cu at 380 nm. One-trap centre conception was confirmed for high-temperature palaeodosimetrical TL peaks and OSL stimulation spectrum bands: for alkali feldspars at 880 and 420 nm and visible region of the spectrum for quartz. A thermooptical mechanism of the optical depopulation of the corresponding trap is confirmed in alkali feldspars, but there is no evidence for processes of this kind in quartz. An analogy between the physical background of OSL properties of both minerals is discussed

  4. Metasomatic alkali-feldspar syenites (episyenites) of the Proterozoic Suomenniemi rapakivi granite complex, southeastern Finland

    Science.gov (United States)

    Suikkanen, E.; Rämö, O. T.

    2017-12-01

    Peralkaline to marginally metaluminous alkali-feldspar syenites and quartz alkali-feldspar syenites are hosted by subalkaline, ferroan rapakivi granites in the 1644 Ma Suomenniemi complex of southeastern Finland. These alkali syenites form NW-oriented dikes and small (fingerprints are, within error, identical to those of the subalkaline granites of the complex. We propose that the Suomenniemi alkali-feldspar syenites are episyenites, formed as the result of pervasive local metasomatism of the subalkaline granites caused by high-temperature oxidizing peralkaline fluids. The process led to major geochemical changes, e.g., addition of Na, Al and Fe3 +, depletion of Si and Fe2 +, and partial to complete recrystallization of the granites along fluid pathways.

  5. Alkali feldspar syenites with shoshonitic affinities from Chhotaudepur area: Implication for mantle metasomatism in the Deccan large igneous province

    Directory of Open Access Journals (Sweden)

    K.R. Hari

    2014-03-01

    Full Text Available Two petrologically distinct alkali feldspar syenite bodies (AFS-1 and AFS-2 from Chhotaudepur area, Deccan Large Igneous Province are reported in the present work. AFS-1 is characterized by hypidiomorphic texture and consists of feldspar (Or55Ab43 to Or25Ab71, ferro-pargasite/ferro-pargasite hornblende, hastingsite, pyroxene (Wo47, En5, Fs46, magnetite and biotite. AFS-2 exhibits panidiomorphic texture with euhedral pyroxene (Wo47-50, En22-39, Fs12–31 set in a groundmass matrix of alkali feldspar (Or99Ab0.77 to Or1.33Ab98, titanite and magnetite. In comparison to AFS-1, higher elemental concentrations of Ba, Sr and ∑REE are observed in AFS-2. The average peralkaline index of the alkali feldspar syenites is ∼1 indicating their alkaline nature. Variation discrimination diagrams involving major and trace elements and their ratios demonstrate that these alkali feldspar syenites have a shoshonite affinity but emplaced in a within-plate and rifting environment. No evidence of crustal contamination is perceptible in the multi-element primitive mantle normalized diagram as well as in terms of trace elemental ratios. The enrichment of incompatible elements in the alkali feldspar syenites suggests the involvement of mantle metasomatism in their genesis.

  6. K-Ar dating: incomplete extraction of radiogenic argon from alkali feldspar - a comment

    International Nuclear Information System (INIS)

    Baksi, A.K.

    1984-01-01

    In a recent paper, McDowell (1983) discussed the difficulties involved in obtaining accurate K-Ar ages on alkali feldspar samples. These difficulties primarily stem from the fact that the feldspars melt at high temperatures and lack structural volatiles which could flush out all of the 40 Ar* from the viscous melt at temperatures below 1600 0 C. Evidently, if feldspar samples could be satisfactorily melted at lower temperatures by the use of a suitable flux, complete release of 40 Ar* should occur. McDowell (1983) also commented on the lack of a suitable feldspar standard sample for argon dating work. This comment will briefly address these two problems. (Auth.)

  7. To the problem of paleodosimetrical information stability in alkali feldspars

    International Nuclear Information System (INIS)

    Huett, Galina; Jaek, Ivar

    1997-01-01

    The stability of holes of the centres of recombination in alkali feldspars, extracted from sediments, is studied. For the emission centres with 410 and 570 nm the energy of activation of thermal quenching is obtained (> 2 eV). Problems of fading and difference between thermoluminescence (TL) and optically stimulated luminescence (OSL), as well as bleach abilities, are discussed. Values of thermal activation energy (> 2 eV) obtained for two different emission bands (410 and 570 nm) in alkali feldspars prove the upper limit of dating (c 10 5 years). The absence of a permanent channel of fading is supported by experimental data. Differences in bleach ability, as well as in residuals of TL and OSL response dating signals, are explained within the frame of the proposed model of identity of defects responsible for those signals. It is supposed that better bleach ability of the OSL signal is connected with optical selection of more transparent grains (or more easily bleach able centres). The applicability of the orange band of emission (570 nm) for dating is recommended for future study

  8. Potassium self-diffusion in a K-rich single-crystal alkali feldspar

    CERN Document Server

    Hergemöller, Fabian; Deicher, Manfred; Wolf, Herbert; Brenner, Florian; Hutter, Herbert; Abart, Rainer; Stolwijk, Nicolaas A.

    The paper reports potassium diffusion measurements performed on gem-quality single-crystal alkali feldspar in the temperature range from 1169 to 1021 K. Natural sanidine from Volkesfeld, Germany was implanted with {}^{43}K at the ISOLDE/CERN radioactive ion-beam facility normal to the (001) crystallographic plane. Diffusion coefficients are well described by the Arrhenius equation with an activation energy of 2.4 eV and a pre-exponential factor of 5×10^{-6}m^{2}/s, which is more than three orders of magnitude lower than the {}^{22}Na diffusivity in the same feldspar and the same crystallographic direction. State-of-the-art considerations including ionic conductivity data on the same crystal and Monte Carlo simulations of diffusion in random binary alloy structures point to a correlated motion of K and Na through the interstitialcy mechanism.

  9. Structure-dependent interactions between alkali feldspars and organic compounds: implications for reactions in geologic carbon sequestration.

    Science.gov (United States)

    Yang, Yi; Min, Yujia; Jun, Young-Shin

    2013-01-02

    Organic compounds in deep saline aquifers may change supercritical CO(2) (scCO(2))-induced geochemical processes by attacking specific components in a mineral's crystal structure. Here we investigate effects of acetate and oxalate on alkali feldspar-brine interactions in a simulated geologic carbon sequestration (GCS) environment at 100 atm of CO(2) and 90 °C. We show that both organics enhance the net extent of feldspar's dissolution, with oxalate showing a more prominent effect than acetate. Further, we demonstrate that the increased reactivity of Al-O-Si linkages due to the presence of oxalate results in the promotion of both Al and Si release from feldspars. As a consequence, the degree of Al-Si order may affect the effect of oxalate on feldspar dissolution: a promotion of ~500% in terms of cumulative Si concentration was observed after 75 h of dissolution for sanidine (a highly disordered feldspar) owing to oxalate, while the corresponding increase for albite (a highly ordered feldspar) was ~90%. These results provide new insights into the dependence of feldspar dissolution kinetics on the crystallographic properties of the mineral under GCS conditions.

  10. Wadi Ladid Al-JI,Dan Alkali Feldspar Granites and Associated Pegmatites, North Eastern Eser, Egypt:Geology,Mineralogy and Radioactivity

    International Nuclear Information System (INIS)

    Abu Steet, A.A.; Ayoub, R.R.; Bakhit, A.F.

    2013-01-01

    This article deals with the geology, structure, mineralogy and radioactivity of the alkali feldspar granites at wadi Ladid al-Ji,dan, north Eastern Desert of Egypt. Geologically, the area consists mainly of alkali feldspar granites. These granites are medium to coarse grained, pink to red in colour and form numbers of moderate to relatively high elevated outcrops. These rocks are altered in some parts due to secondary processes especially along the fault zones and contacts. The area displays primary and secondary structures. Primary structures comprise layering, volcanic flows, vesicular tops of lavas and volcanic bombs. The secondary structures are represented by exfoliation, joints and faults. The granites are dissected by several sets of joints predominating in the N-S direction, dipping 84°-88° mainly to west; E-W direction, dipping 70°-75° mainly to south and NW-SE direction, dipping 80°-82° to SW direction. The majority of joints are tension ones. These tension joints are commonly filled with quartz, feldspars, epidote, iron oxides, manganese oxides and aplite. The studied area is dissected by major regional faults. Along the fault zones; the granites are marked by fault breccia and alteration features, especially silicification, hematitization, kaolinitization and chloritization. The area is cutting by faults trending mainly in N-S, NE-SW and NNW-SSE directions. The average uranium and thorium contents of the alkali feldspar granites are 12 and 23 ppm and reaches up to 36 and 37 ppm in the normal pegmatites. In the anomalous pegmatites the maximum values recorded are 91 and 72 ppm. Generally, the averages of uranium and thorium contents in the studied pegmatites are higher than that of the world and Egyptian uraniferous pegmatites. The high uranium content in alkali feldspar granites is related to the presence of some accessory minerals such as zircon, fluorite and apatite but the high uranium content in the pegmatites is related to the presence of

  11. Possible reasons for anomalous fading in alkali feldspars used for luminescence dating of Quaternary deposits

    Directory of Open Access Journals (Sweden)

    Jaek, Ivar

    2007-09-01

    Full Text Available According to many publications, alkali feldspars are characterized by specific athermal (anomalous fading of their thermoluminescence and optically-stimulated luminescence. This phenomenon is manifested as spontaneous decline in luminescence intensity over relatively long (months and years time after laboratory irradiation, possibly due to tunnelling of electrons from lattice defects and impurities acting as dosimetric traps. It can hamper reliable luminescent dating of Quaternary deposits on the basis of feldspar extractions due to possible unpredictable underestimation of the ages. In this paper we present some experimental results related to the manifestation of the phenomenon. It is found that, in general case, the assumed long-term anomalous fading cannot be connected to electron tunnelling from the deep dosimetric traps. At the same time, some decrease in the dosimetric luminescence signal observable in just irradiated feldspar samples can really be caused by tunnelling. However, the probability of this process quickly goes down, already within some days after irradiation. Interpretation of some other short- and long-term anomalous fading-like effects requires involvement of radiation- and thermo-induced ionic processes.

  12. Photoionization of radiation-induced traps in quartz and alkali feldspars.

    Science.gov (United States)

    Hütt, G; Jaek, I; Vasilchenko, V

    2001-01-01

    For the optimization of luminescence dating and dosimetry techniques on the basis of the optically stimulated luminescence, the stimulation spectra of quartz and alkali feldspars were measured in the spectral region of 250-1100 nm using optically stimulated afterglow. Optically stimulated luminescence in all studied spectral regions is induced by the same kind of deep traps, that produce thermoluminescence in the regions of palaeodosimetric peaks for both minerals. The mechanism for photoionization of deep traps was proposed as being due to delocalization of the excited state of the corresponding lattice defects. The excited state overlaps the zone states; i.e. is situated in the conduction band. Because of the high quantum yield of deep electron trap ionization in the UV spectral region, the present aim was to study the possibility of using UV-stimulation for palaeodose reconstruction.

  13. Photoionization of radiation-induced traps in quartz and alkali feldspars

    International Nuclear Information System (INIS)

    Huett, G.; Jaek, I.; Vasilchenko, V.

    2001-01-01

    For the optimization of luminescence dating and dosimetry techniques on the basis of the optically stimulated luminescence, the stimulation spectra of quartz and alkali feldspars were measured in the spectral region of 250-1100 nm using optically stimulated afterglow. Optically stimulated luminescence in all studied spectral regions is induced by the same kind of deep traps, that produce thermoluminescence in the regions of palaeodosimetric peaks for both minerals. The mechanism for photoionization of deep traps was proposed as being due to delocalization of the excited state of the corresponding lattice defects. The excited state overlaps the zone states; i.e. is situated in the conduction band. Because of the high quantum yield of deep electron trap ionization in the UV spectral region, the present aim was to study the possibility of using UV-stimulation for palaeodose reconstruction

  14. Photoionization of radiation-induced traps in quartz and alkali feldspars

    Energy Technology Data Exchange (ETDEWEB)

    Huett, G. E-mail: hutt@pdos.gi.ee; Jaek, I.; Vasilchenko, V

    2001-01-15

    For the optimization of luminescence dating and dosimetry techniques on the basis of the optically stimulated luminescence, the stimulation spectra of quartz and alkali feldspars were measured in the spectral region of 250-1100 nm using optically stimulated afterglow. Optically stimulated luminescence in all studied spectral regions is induced by the same kind of deep traps, that produce thermoluminescence in the regions of palaeodosimetric peaks for both minerals. The mechanism for photoionization of deep traps was proposed as being due to delocalization of the excited state of the corresponding lattice defects. The excited state overlaps the zone states; i.e. is situated in the conduction band. Because of the high quantum yield of deep electron trap ionization in the UV spectral region, the present aim was to study the possibility of using UV-stimulation for palaeodose reconstruction.

  15. Can cathodoluminescence of feldspar be used as provenance indicator?

    Science.gov (United States)

    Scholonek, Christiane; Augustsson, Carita

    2016-05-01

    We have studied feldspar from crystalline rocks for its textural and spectral cathodoluminescence (CL) characteristics with the aim to reveal their provenance potential. We analyzed ca. 60 rock samples of plutonic, volcanic, metamorphic, and pegmatitic origin from different continents and of 16 Ma to 2 Ga age for their feldspar CL textures and ca. 1200 feldspar crystals from these rocks for their CL color spectra. Among the analyzed rocks, igneous feldspar is most commonly zoned, whereby oscillatory zoning can be confirmed to be typical for volcanic plagioclase. The volcanic plagioclase also less commonly contains twin lamellae that are visible in CL light than crystals from other rock types. Alkali feldspar, particularly from igneous and pegmatitic rocks, was noted to be most affected by alteration features, visible as dark spots, lines and irregular areas. The size of all textural features of up to ca. 150 μm, in combination with possible alteration in both the source area and the sedimentary system, makes the CL textures of feldspar possible to use for qualitative provenance research only. We observed alkali feldspar mostly to luminesce in a bluish color and sometimes in red, and plagioclase in green to yellow. The corresponding CL spectra are dominated by three apparent intensity peaks at 440-520 nm (mainly blue), 540-620 nm (mainly green) and 680-740 nm (red to infrared). A dominance of the peak in the green wavelength interval over the blue one for plagioclase makes CL particularly useful for the differentiation of plagioclase from alkali feldspar. An apparent peak position in red to infrared at < 710 nm for plagioclase mainly is present in mafic rocks. Present-day coastal sand from Peru containing feldspar with the red to infrared peak position mainly exceeding 725 nm for northern Peruvian sand and a larger variety for sand from southern Peru illustrates a discriminative effect of different source areas. We conclude that the provenance application

  16. Exchange of Na+ and K+ between water vapor and feldspar phases at high temperature and low vapor pressure

    Science.gov (United States)

    Fournier, R.O.

    1976-01-01

    In order to determine whether gas (steam) containing a small amount of dissolved alkali chloride is effective in promoting base exchange of Na+ and K+ among alkali feldspars and coexisting brine or brine plus solid salt, experiments were carried out at 400-700??C and steam densities ranging down to less than 0.05. For bulk compositions rich in potassium, the low pressure results are close to previous high-pressure results in composition of the fluid and coexisting solid phase. However, when the bulk composition is more sodic, alkali feldspars are relatively richer in potassium at low pressure than at high pressure. This behaviour corresponds to enrichment of potassium in the gas phase relative to coexisting brine and precipitation of solid NaCl when the brine plus gas composition becomes moderately sodic. The gas phase is very effective in promoting base exchange between coexisting alkali feldspars at high temperature and low water pressure. This suggests that those igneous rocks which contain coexisting alkali feldspars out of chemical equilibrium either remained very dry during the high-temperature part of their cooling history or that the pore fluid was a gas containing very little potassium relative to sodium. ?? 1976.

  17. Plagioclase-mantled K-feldspar in the Carboniferous porphyritic microgranite of Altenberg-Frauenstein, Eastern Erzgebirge/Krusné Hory

    Directory of Open Access Journals (Sweden)

    Axel Müller

    2002-01-01

    Full Text Available The Upper Carboniferous porphyritic microgranite of Altenberg-Frauenstein, formerly known as Granitporphyr (Dalmer 1896 and here abbreviated as GP, forms a 36 km long and up to 18 km wide complex of ring dykes related to the Teplice-Altenberg caldera in the German–Czech border region of the Eastern Erzgebirge/Krusné Hory. The microgranites are characterized by the occurrence of plagioclase-mantled K-feldspar phenocrysts. The microgranite varieties representtwo main stages of intrusion evolved from acid (GP I to intermediaterocks (GP II within the intrusion. The most acid rock (GP Icum occurs as enclaves in GP I and GP II and is interpreted as a cumulate of K-feldspar and quartz phenocrysts. The porphyritic microgranites show field, textural and geochemical evidence suggesting that some of them have formed as a result of interaction between felsic and mafic magmas. Mixing features are abundant in the porphyriticquartz-feldspar-hornblende microgranite (GP II interpreted as a hybrid rock. They are less discrete in the early phase (GP I and not obvious in the acid enclaves (GP Icum. This trend seems to reflect a continuous deflation of the magma chamber from the top to the bottom. According to the definition of rapakivi granites after Haapala and Rämö (1992, the porphyritic microgranite of Altenberg-Frauenstein may be considered as rapakivi granite although ovoid alkali feldspar megacrysts typical of classical rapakivi granites are not recorded.However, due to its Carboniferous age and being the only known granitewith rapakivi texture in the German–Czech part of the Variscan belt, the microgranite of Altenberg-Frauenstein is exceptional.

  18. Bleaching of the thermoluminescence of feldspars by sunlight

    International Nuclear Information System (INIS)

    Robertson, G.B.; Prescott, J.R.; Hutton, J.T.

    1991-01-01

    Feldspars are an important component of materials used for thermoluminescence (TL) and photoluminescence (PL) dating of sediments; and successful dating implies a knowledge of the degree of re-setting by exposure to sunlight of the stored luminescence energy. We have studied the bleaching by full sunlight of the TL of six alkali feldspars of representative composition and of one oligoclase. The high potassium and high sodium feldspars are the brightest, and are also the least easily bleached, whereas those of intermediate (K-Na) composition bleach quickly. On a time scale of upwards of 16 h, all samples would have bleached enough for them to be useful for TL dating. A search was made for individual glow curve peaks that bleach particularly quickly (and are thus similar to the well-known 325 o C peak used in the TL dating of quartz). In the samples studied, there was only one glow curve peak that was selectively susceptible to bleaching: the 280 o C peak in oligoclase. (author)

  19. The History of a Plutonic-Volcanic System Determined from Compositional and Mineral Inclusion Mapping of Alkali Feldspar Megacrysts

    Science.gov (United States)

    Belfanti, S. A. D.; Gualda, G. A. R.

    2017-12-01

    Alkali-feldspar megacrysts (2-20 cm long) occur in many granitic rocks, providing extensive records of crystallization within magma bodies. We will use megacrysts from Yosemite National Park's Tuolumne Intrusive Suite to determine if and how megacrysts record recharge and eruption. Preliminary work has focused on 4 crystals. Based on BSE patterns, crystals can be divided into 3 zones: (1) the core, which represents the crystal's first growth and sometimes displays some resorption; (2) the interior, including a series of sub-zones that correspond to different growth periods; and (3) the rim, or outermost growth stage. Common BSE patterns include decreasing brightness from the inner portion of a growth period outward, increasing brightness towards either side of a boundary, and periods of constant brightness, for a full or partial period. Most mineral inclusions appear as single crystals ( 10-25%) or as groups of 2-4 crystals ( 60-75%). Large clusters of 10 or more individuals are less common ( 5-15%), and clusters of >20 crystals are rare ( 1-3%). Most crystals (85-95%) occur on growth boundaries or within the core. Magnetite is common in the more central parts of the interior zone, appearing only occasionally in the core and towards the rim. Accessories, amphibole, and biotite are more evenly distributed within the megacryst. Biotite and titanite grains large enough to display habit appear to be within 20 degrees of parallel with zone boundaries. Most other inclusions are small or not elongated enough to display clear alignment. The total volume of inclusions (excluding quartz and plagioclase, which have X-ray attenuation very similar to that of alkali feldspar) does not exceed 1% of megacryst volume. Plagioclase seems to be at least equal in volume to all other inclusions combined, but as noted above, its exact volume is currently indiscernible. Magnetite makes up about 1/6 of inclusion volume, zircon 1/3, and all others the remaining half. We will complement our

  20. Oxygen mobility in alkali feldspars; Etude de la mobilite de l'oxygene dans les feldspaths alcalins

    Energy Technology Data Exchange (ETDEWEB)

    Merigoux, H [Commissariat a l' Energie Atomique, Saclay (France). Centre d' Etudes Nucleaires

    1968-03-15

    The oxygen mobility is shown from oxygen atoms exchange between potassic and sodic feldspars and 18 oxygen enriched water. Exchanges are carried out in autoclaves between 400 and 800 deg. C under a water pressure between 300 and 800 bars. The oxygen is extracted from silicate by a ClF{sub 3} attack. Two distinct mechanisms may be found. The first one is auto-diffusion; for adularia we have: D = 9.10{sup -7} exp(-32000/RT) (cm{sup 2}.s{sup -1}), for albite: D 4.5.10{sup -5} exp(-37000/RT) (cm{sup 2}.s{sup -1}). The second one, more rapid, is associated with alkali atoms exchanges. These results are applied to the order-disorder problem in feldspars and to the oxygen geochemistry. (author) [French] La mobilite de l'oxygene est mise en evidence a partir d'echanges d'atomes d'oxygene entre des feldspaths potassiques et sodiques en presence d'une eau enrichie en oxygene 18. Les echanges sont effectues en autoclave entre 400 et 800 deg. C sous des pressions de vapeur d'eau comprises entre 300 et 800 bars. L'oxygene est extrait du silicate par attaque au ClF{sub 3}. Deux mecanismes, bien distincts, peuvent se rencontrer. Le premier correspond a l'autodiffusion de l'oxygene; dans le domaine etudie on trouve pour l'adulaire: D = 9,10{sup -7} exp(-32000/RT) (cm{sup 2}.s{sup -1}), et pour l'albite: D 4,5.10{sup -5} exp(-37000/RT) (cm{sup 2}.s{sup -1}). Le second, beaucoup plus rapide, est associe a l'echange des atomes alcalins avec la solution. Ces resultats sont appliques au probleme du passage ordre-desordre dans les feldspaths et a la geochimie de l'oxygene. (auteur)

  1. Rare earth element geochemistry of feldspars: examples from Fe-oxide Cu-Au systems in the Olympic Cu-Au Province, South Australia

    Science.gov (United States)

    Kontonikas-Charos, Alkis; Ciobanu, Cristiana L.; Cook, Nigel J.; Ehrig, Kathy; Krneta, Sasha; Kamenetsky, Vadim S.

    2018-04-01

    Rare earth element (REE) fractionation trends in feldspars are reported from Olympic Dam (including Wirrda Well and Phillip's Ridge) and Cape Donington (Port Lincoln), for comparison with two other igneous-hydrothermal terranes within the eastern Gawler Craton: Moonta-Wallaroo and Hillside. The case studies were selected as they represent 1590 Ma Hiltaba Suite and/or 1845 - 1810 Ma Donington Suite granites, and, aside from Cape Donington, are associated with Mesoproterozoic iron-oxide copper gold (IOCG)-type mineralization. Both plagioclase and alkali feldspar were analyzed within selected samples with the purpose of constraining and linking changes in REE concentrations and fractionation trends in feldspars to local and whole-rock textures and geochemistry. Two unique, reproducible fractionation trends were obtained for igneous plagioclase and alkali feldspars, distinguished from one another by light rare earth element enrichment, Eu-anomalies and degrees of fractionation (e.g. La/Lu slopes). Results for hydrothermal albite and K-feldspar indicate that REE concentrations and fractionation trends are generally inherited from igneous predecessors, however in some instances, significant amounts of REE appear to have been lost to the fluid. These results may have critical implications for the formation of world-class IOCG systems, in which widespread alkali metasomatism plays a key role by altering the physical and chemical properties of the host rocks during early stages of IOCG formation, as well as trapping trace elements (including REE).

  2. Alkali-ions diffusion, mullite formation, and crystals dissolution during sintering of porcelain bodies: Microstructural approach

    DEFF Research Database (Denmark)

    Leonelli, C.; Kamseu, E.; Boccaccini, Dino

    2009-01-01

    The effect of alkali-silicate glassy matrix as replacement for feldspar in soft and hard porcelain compositions was studied. SEM and X-ray diffraction analysis were used to evidence phase evolution. For each composition, the influence of soaking time was evaluated. The difference in chemical...... to hard porcelain. Replacing the feldspar by alkali-silicate glassy matrices with similar chemical composition, the amount of secondary mullite and mechanical properties increased in both soft and hard compositions....

  3. Zoning and exsolution in cumulate alkali feldspars from the eruption (12.9 Ka) of Laacher see volcano (Western Germany) as an indicator of time-scales and dynamics of carbonate-silicate unmixing

    Science.gov (United States)

    Sourav Rout, Smruti; Wörner, Gerhard

    2017-04-01

    Time-scales extracted from the detailed analysis of chemically zoned minerals provide insights into crystal ages, magma storage and compositional evolution, including mixing and unmixing events. This allows having a better understanding of pre-eruptive history of large and potentially dangerous magma chambers. We present a comprehensive study of chemical diffusion across zoning and exsolution patterns of alkali feldspars in carbonatite-bearing cognate syenites from the 6.3 km3 (D.R.E) phonolitic Laacher See Tephra (LST) eruption 12.9 ka ago. The Laacher See volcano is located in the Quaternary East Eifel volcanic field of the Paleozoic Rhenish Massif in Western Germany and has produced a compositionally variable sequence in a single eruption from a magma chamber that was zoned from mafic phonolite at the base to highly evolved, actively degassing phonolite magma at the top. Diffusion chronometry is applied to major and trace element compositions obtained on alkali feldspars from carbonate-bearing syenitic cumulates. Methods used were laser ablation inductively coupled plasma mass spectrometry (LA ICP-MS) in combination with energy-dispersive and wavelength-dispersive electron microprobe analyses (EDS & WDS-EMPA). The grey scale values extracted from multiple accumulations of back-scattered electron images represent the K/Na ratio owing to the extremely low concentrations of Ba and Sr (transition and phase separation). A distinctive uphill diffusive analysis is used specifically for the phase separation in the case of exsolution features (comprising of albite- and orthoclase-rich phases) in sanidines. The error values are aggregates of propagated error through calculations and the uncertainty in temperature values. Trace element compositional data of distinct feldspar compositions that are assumed to have grown before and after silicate-carbonate unmixing are used to estimate partition coefficients between carbonate and silicate melt. The resulting values correlate

  4. Oxygen mobility in alkali feldspars; Etude de la mobilite de l'oxygene dans les feldspaths alcalins

    Energy Technology Data Exchange (ETDEWEB)

    Merigoux, H. [Commissariat a l' Energie Atomique, Saclay (France). Centre d' Etudes Nucleaires

    1968-03-15

    The oxygen mobility is shown from oxygen atoms exchange between potassic and sodic feldspars and 18 oxygen enriched water. Exchanges are carried out in autoclaves between 400 and 800 deg. C under a water pressure between 300 and 800 bars. The oxygen is extracted from silicate by a ClF{sub 3} attack. Two distinct mechanisms may be found. The first one is auto-diffusion; for adularia we have: D = 9.10{sup -7} exp(-32000/RT) (cm{sup 2}.s{sup -1}), for albite: D 4.5.10{sup -5} exp(-37000/RT) (cm{sup 2}.s{sup -1}). The second one, more rapid, is associated with alkali atoms exchanges. These results are applied to the order-disorder problem in feldspars and to the oxygen geochemistry. (author) [French] La mobilite de l'oxygene est mise en evidence a partir d'echanges d'atomes d'oxygene entre des feldspaths potassiques et sodiques en presence d'une eau enrichie en oxygene 18. Les echanges sont effectues en autoclave entre 400 et 800 deg. C sous des pressions de vapeur d'eau comprises entre 300 et 800 bars. L'oxygene est extrait du silicate par attaque au ClF{sub 3}. Deux mecanismes, bien distincts, peuvent se rencontrer. Le premier correspond a l'autodiffusion de l'oxygene; dans le domaine etudie on trouve pour l'adulaire: D = 9,10{sup -7} exp(-32000/RT) (cm{sup 2}.s{sup -1}), et pour l'albite: D 4,5.10{sup -5} exp(-37000/RT) (cm{sup 2}.s{sup -1}). Le second, beaucoup plus rapide, est associe a l'echange des atomes alcalins avec la solution. Ces resultats sont appliques au probleme du passage ordre-desordre dans les feldspaths et a la geochimie de l'oxygene. (auteur)

  5. Principles of Thermal Expansion in Feldspars

    Science.gov (United States)

    Hovis, Guy; Medford, Aaron; Conlon, Maricate; Tether, Allison; Romanoski, Anthony

    2010-05-01

    Following the recent thermal expansion work of Hovis et al. (1) on AlSi3 feldspars, we have investigated the thermal expansion of plagioclase, Ba-K, and Ca-K feldspar crystalline solutions. X-ray powder diffraction data were collected between room temperature and 925 °C on six natural plagioclase specimens ranging in composition from anorthite to oligoclase, the K-exchanged equivalents of these plagioclase specimens, and five synthetic Ba-K feldspars with compositions ranging from 25 to 99 mol % BaAl2Si2O8. The resulting thermal expansion coefficients (α) for volume have been combined with earlier results for end-member Na- and K-feldspars (2,3). Unlike AlSi3 feldspars, Al2Si2 feldspars, including anorthite and celsian from the present study plus Sr- and Pb-feldspar from other workers (4,5), show essentially constant and very limited thermal expansion, regardless of divalent cation size. In the context of structures where the Lowenstein rule (6) requires Al and Si to alternate among tetrahedra, the proximity of bridging Al-O-Si oxygen ions to divalent neighbors (ranging from 0 to 2) produces short Ca-O (or Ba-O) bonds (7,8) that apparently are the result of local charge-balance requirements (9). Gibbs et al. (10) suggest that short bonds such as these have a partially covalent character. This in turn stiffens the structure. Thus, for feldspar series with coupled substitution the change away from a purely divalent M-site occupant gives the substituting (less strongly bonded) monovalent cations increasingly greater influence on thermal expansion. Overall, then, thermal expansion in the feldspar system is well represented on a plot of α against room-temperature volume, where one sees a quadrilateral bounded by data for (A) AlSi3 feldspars whose expansion behavior is controlled largely by the size of the monovalent alkali-site occupant, (B) Al2Si2 feldspars whose expansion is uniformly limited by partially-covalent bonds between divalent M-site occupants and

  6. Feldspar dissolution rates in the Topopah Spring Tuff, Yucca Mountain, Nevada

    Science.gov (United States)

    Bryan, C.R.; Helean, K.B.; Marshall, B.D.; Brady, P.V.

    2009-01-01

    Two different field-based methods are used here to calculate feldspar dissolution rates in the Topopah Spring Tuff, the host rock for the proposed nuclear waste repository at Yucca Mountain, Nevada. The center of the tuff is a high silica rhyolite, consisting largely of alkali feldspar (???60 wt%) and quartz polymorphs (???35 wt%) that formed by devitrification of rhyolitic glass as the tuff cooled. First, the abundance of secondary aluminosilicates is used to estimate the cumulative amount of feldspar dissolution over the history of the tuff, and an ambient dissolution rate is calculated by using the estimated thermal history. Second, the feldspar dissolution rate is calculated by using measured Sr isotope compositions for the pore water and rock. Pore waters display systematic changes in Sr isotopic composition with depth that are caused by feldspar dissolution. The range in dissolution rates determined from secondary mineral abundances varies from 10-16 to 10-17 mol s-1 kg tuff-1 with the largest uncertainty being the effect of the early thermal history of the tuff. Dissolution rates based on pore water Sr isotopic data were calculated by treating percolation flux parametrically, and vary from 10-15 to 10-16 mol s-1 kg tuff-1 for percolation fluxes of 15 mm a-1 and 1 mm a-1, respectively. Reconciling the rates from the two methods requires that percolation fluxes at the sampled locations be a few mm a-1 or less. The calculated feldspar dissolution rates are low relative to other measured field-based feldspar dissolution rates, possibly due to the age (12.8 Ma) of the unsaturated system at Yucca Mountain; because oxidizing and organic-poor conditions limit biological activity; and/or because elevated silica concentrations in the pore waters (???50 mg L-1) may inhibit feldspar dissolution. ?? 2009 Elsevier Ltd. All rights reserved.

  7. Alkali control of high-grade metamorphism and granitization

    Directory of Open Access Journals (Sweden)

    Oleg G. Safonov

    2014-09-01

    Full Text Available We review petrologic observations of reaction textures from high-grade rocks that suggest the passage of fluids with variable alkali activities. Development of these reaction textures is accompanied by regular compositional variations in plagioclase, pyroxenes, biotite, amphibole and garnet. The textures are interpreted in terms of exchange and net-transfer reactions controlled by the K and Na activities in the fluids. On the regional scale, these reactions operate in granitized, charnockitized, syenitized etc. shear zones within high-grade complexes. Thermodynamic calculations in simple chemical systems show that changes in mineral assemblages, including the transition from the hydrous to the anhydrous ones, may occur at constant pressure and temperature due only to variations in the H2O and the alkali activities. A simple procedure for estimating the activity of the two major alkali oxides, K2O and Na2O, is implemented in the TWQ software. Examples of calculations are presented for well-documented dehydration zones from South Africa, southern India, and Sri Lanka. The calculations have revealed two end-member regimes of alkalis during specific metamorphic processes: rock buffered, which is characteristic for the precursor rocks containing two feldspars, and fluid-buffered for the precursor rocks without K-feldspar. The observed reaction textures and the results of thermodynamic modeling are compared with the results of available experimental studies on the interaction of the alkali chloride and carbonate-bearing fluids with metamorphic rocks at mid-crustal conditions. The experiments show the complex effect of alkali activities in the fluid phase on the mineral assemblages. Both thermodynamic calculations and experiments closely reproduce paragenetic relations theoretically predicted by D.S. Korzhinskii in the 1940s.

  8. Porcelain tiles using nepheline as alternative source of alkalis

    International Nuclear Information System (INIS)

    Cruz, C.M. da; Oliveira, D.C. de; Faustino, L.M.; Maestrelli, S.C.; Roveri, C.D.

    2016-01-01

    Porcelain tiles present good aesthetical properties, low water absorption and high mechanical and chemical attack resistance. The feldspar, one of its raw materials, is responsible form diminishing porosity and enhance mechanical resistance. It is normally imported, making the production more expensive. In this paper, it was studied the substitution of feldspar by nepheline under the rheological point of view, determining the optimum amount of deffloculant and the maximum concentration of solids of the suspensions. The results showed similar rheological behaviour, with a small reduction on the maximum concentration of solids as the proportion of nepheline increases. The pieces made with nepheline are darker than the ones made of feldspar; however, the magnetic separation results in lighter pieces. The formulations with nepheline as alkalis source presented a high increase of the density after heating. (author)

  9. Atmospheric weathering and silica-coated feldspar: analogy with zeolite molecular sieves, granite weathering, soil formation, ornamental slabs, and ceramics.

    Science.gov (United States)

    Smith, J V

    1998-03-31

    Feldspar surfaces respond to chemical, biological, and mechanical weathering. The simplest termination is hydroxyl (OH), which interacts with any adsorption layer. Acid leaching of alkalis and aluminum generated a silica-rich, nanometers-thick skin on certain feldspars. Natural K, Na-feldspars develop fragile surfaces as etch pits expand into micrometer honeycombs, possibly colonized by lichens. Most crystals have various irregular coats. Based on surface-catalytic processes in molecular sieve zeolites, I proposed that some natural feldspars lose weakly bonded Al-OH (aluminol) to yield surfaces terminated by strongly bonded Si-OH (silanol). This might explain why some old feldspar-bearing rocks weather slower than predicted from brief laboratory dissolution. Lack of an Al-OH infrared frequency from a feldspar surface is consistent with such a silanol-dominated surface. Raman spectra of altered patches on acid-leached albite correspond with amorphous silica rather than hydroxylated silica-feldspar, but natural feldspar may respond differently. The crystal structure of H-exchanged feldspar provides atomic positions for computer modeling of complex ideas for silica-terminated feldspar surfaces. Natural weathering also depends on swings of temperature and hydration, plus transport of particles, molecules, and ionic complexes by rain and wind. Soil formation might be enhanced by crushing granitic outcrops to generate new Al-rich surfaces favorable for chemical and biological weathering. Ornamental slabs used by architects and monumental masons might last longer by minimizing mechanical abrasion during sawing and polishing and by silicifying the surface. Silica-terminated feldspar might be a promising ceramic surface.

  10. Natural radioactivity and Rare Earth elements in feldspar samples, Central Eastern desert, Egypt

    International Nuclear Information System (INIS)

    Walley El-Dine, Nadia; El-Shershaby, Amal; Afifi, Sofia; Sroor, Amany; Samir, Eman

    2011-01-01

    The pegmatite bodies of the Eastern Desert of Egypt are widely distributed especially along the Marsa-Alam-Idfu road. The Abu Dob area covers about 150 km 2 of the Arabian Nubian shield at the central part of the Eastern Desert of Egypt. Most of the pegmatite is zoned; the zonation starts with milky quartz at the core followed by alkali feldspar at the margins. The feldspars vary in color from rose to milky and in composition from K-feldspar to Na-feldspar, sometimes interactions of both types are encountered. Thirteen feldspar samples were collected from different locations in the Abu Dob area for measuring the natural radioactivity of 238 U, 232 Th and 40 K using an HPGe detector. The variation in concentration of radionuclides for the area under investigation can be classified into regions of high, medium and low natural radioactivity. The average concentration in BqKg -1 has been observed to be from 9.5 to 183675.7 BqKg -1 for 238 U, between 6.1 and 94,314.2 BqKg -1 for 232 Th and from 0 to 7894.6 BqKg -1 for 40 K. Radium equivalent activities (Ra eq ), dose rate (D R ) and external hazard (H ex ) have also been determined. In the present work, the concentration of rare earth elements are measured for two feldspar samples using two techniques, Environmental Scanning Electron microscope XIL 30 ESEM, Philips, and Inductively Coupled Plasma Mass Spectroscopy (ICP-MS). The existence of rare earth elements in this area are very high and can be used in different important industries.

  11. Natural radioactivity and Rare Earth elements in feldspar samples, Central Eastern desert, Egypt

    Energy Technology Data Exchange (ETDEWEB)

    Walley El-Dine, Nadia, E-mail: nadia_walley5@hotmail.co [Department of physics, Faculty of girls for Art, Science and Education, Ain Shams University, Heliopolis, Cairo (Egypt); El-Shershaby, Amal [Department of physics, Faculty of girls for Art, Science and Education, Ain Shams University, Heliopolis, Cairo (Egypt); Afifi, Sofia [Nuclear Materials Authority (Egypt); Sroor, Amany; Samir, Eman [Department of physics, Faculty of girls for Art, Science and Education, Ain Shams University, Heliopolis, Cairo (Egypt)

    2011-05-15

    The pegmatite bodies of the Eastern Desert of Egypt are widely distributed especially along the Marsa-Alam-Idfu road. The Abu Dob area covers about 150 km{sup 2} of the Arabian Nubian shield at the central part of the Eastern Desert of Egypt. Most of the pegmatite is zoned; the zonation starts with milky quartz at the core followed by alkali feldspar at the margins. The feldspars vary in color from rose to milky and in composition from K-feldspar to Na-feldspar, sometimes interactions of both types are encountered. Thirteen feldspar samples were collected from different locations in the Abu Dob area for measuring the natural radioactivity of {sup 238}U, {sup 232}Th and {sup 40}K using an HPGe detector. The variation in concentration of radionuclides for the area under investigation can be classified into regions of high, medium and low natural radioactivity. The average concentration in BqKg{sup -1} has been observed to be from 9.5 to 183675.7 BqKg{sup -1} for {sup 238}U, between 6.1 and 94,314.2 BqKg{sup -1} for {sup 232}Th and from 0 to 7894.6 BqKg{sup -1} for {sup 40}K. Radium equivalent activities (Ra{sub eq}), dose rate (D{sub R}) and external hazard (H{sub ex}) have also been determined. In the present work, the concentration of rare earth elements are measured for two feldspar samples using two techniques, Environmental Scanning Electron microscope XIL 30 ESEM, Philips, and Inductively Coupled Plasma Mass Spectroscopy (ICP-MS). The existence of rare earth elements in this area are very high and can be used in different important industries.

  12. OSL-thermochronometry of feldspar from the KTB borehole, Germany

    DEFF Research Database (Denmark)

    Guralnik, Benny; Jain, Mayank; Herman, Frédéric

    2015-01-01

    a new thermochronometer based on the infrared stimulated luminescence (IRSL) from feldspar, and validate the extrapolation of its response to artificial radiation and heat in the laboratory to natural environmental conditions. Specifically, we present a new detailed Na-feldspar IRSL thermochronology...... the current geothermal gradient, or (ii) inverted into a geothermal palaeogradient of 29±2 °C km−1, integrating natural thermal conditions over the last ∼65 ka. The demonstrated ability to invert a depth–luminescence dataset into a meaningful geothermal palaeogradient opens new venues for reconstructing...

  13. Understanding optically stimulated charge movement in quartz and feldspar using time-resolved measurements

    DEFF Research Database (Denmark)

    Ankjærgaard, Christina

    . Although, results are only presented for some quartz and feldspar samples, they were found to be very similar within the each group during the course of this work.Thermoluminescence (TL) and optically stimulated luminescence (OSL) from quartz and feldspar are widely used in accident dosimetry...... stimulation energy. The thesis first delves into three main methodological developments, namely (i) research and development of the equipment for TR-OSL measurements, (ii) finding the best method for multiple-exponential analysis of a TR-OSL curve, and (iii) optimisation of the pulsing configuration...... of the equipment for TR-OSL measurements, (ii) finding the best method for multiple-exponential analysis of a TR-OSL curve, and (iii) optimisation of the pulsing configuration for the best separation of quartz OSL from a mixed quarts-feldspar sample. It then proceeds to study the different charge transport...

  14. Complex Diffusion Mechanisms for Li in Feldspar: Re-thinking Li-in-Plag Geospeedometry

    Science.gov (United States)

    Holycross, M.; Watson, E. B.

    2017-12-01

    how Li-in-plagioclase geospeedometry is used to time igneous processes. Giletti, B.J., and T.M. Shanahan (1997) Alkali diffusion in plagioclase feldspar, Chem. Geol., 139, 3-20

  15. Bleaching of the thermoluminescence of feldspars by selected wavelengths present in sunlight

    International Nuclear Information System (INIS)

    Robertson, G.B.; Prescott, J.R.; Hutton, J.T.

    1993-01-01

    Feldspars occur in many sediments, and dating them by thermoluminescence (TL) requires a knowledge of how efficiently sunlight bleaches these minerals. The relative bleaching efficiencies of various wavelengths have been investigated for four alkali feldspars and an oligoclase, using the natural TL of the samples and the artificial TL induced by laboratory irradiation, bleached by wavelengths in the range 322-550 nm. Ultraviolet wavelengths are more efficient than the longer wavelengths at bleaching all the glow-curve peaks and are responsible for most of the phototransfer from high-temperature peaks to low-temperature peaks. Some feldspars show an initial increase in TL intensity with bleaching. Two sanidines of similar bulk composition but different TL glow curves show different dependences on bleaching wavelength. In a sodic sanidine with a dominant 240 o C peak the energy required to bleach to 50% was a thousand times greater at 550 nm than at 322 nm. In contrast, another sanidine with a complex glow curve between 150 and 450 o C showed a much slower change in the 330 o C peak with wavelength - a factor of 10 between 322 and 550 nm - with a region between 400 and 500 nm which was almost independent of wavelength. This behaviour is explained by competing mechanisms of phototransfer and bleaching which depend on wavelength in different ways. (author)

  16. Research on mouse model of grade II corneal alkali burn

    Directory of Open Access Journals (Sweden)

    Jun-Qiang Bai

    2016-04-01

    Full Text Available AIM: To choose appropriate concentration of sodium hydroxide (NaOH solution to establish a stable and consistent corneal alkali burn mouse model in grade II. METHODS: The mice (n=60 were randomly divided into four groups and 15 mice each group. Corneal alkali burns were induced by placing circle filter paper soaked with NaOH solutions on the right central cornea for 30s. The concentrations of NaOH solutions of groups A, B, C, and D were 0.1 mol/L, 0.15 mol/L , 0.2 mol/L, and 1.0 mol/L respectively. Then these corneas were irrigated with 20 mL physiological saline (0.9% NaCl. On day 7 postburn, slit lamp microscope was used to observe corneal opacity, corneal epithelial sodium fluorescein staining positive rate, incidence of corneal ulcer and corneal neovascularization, meanwhile pictures of the anterior eyes were taken. Cirrus spectral domain optical coherence tomography was used to scan cornea to observe corneal epithelial defect and corneal ulcer. RESULTS: Corneal opacity scores ( were not significantly different between the group A and group B (P=0.097. Incidence of corneal ulcer in group B was significantly higher than that in group A (P=0.035. Incidence of corneal ulcer and perforation rate in group B was lower than that in group C. Group C and D had corneal neovascularization, and incidence of corneal neovascularization in group D was significantly higher than that in group C (P=0.000. CONCLUSION: Using 0.15 mol/L NaOH can establish grade II mouse model of corneal alkali burns.

  17. Feldspar, Infrared Stimulated Luminescence

    DEFF Research Database (Denmark)

    Jain, Mayank

    2014-01-01

    This entry primarily concerns the characteristics and the origins of infrared-stimulated luminescence in feldspars.......This entry primarily concerns the characteristics and the origins of infrared-stimulated luminescence in feldspars....

  18. Structures of the K- and Na-components of two-phase feldspar from Primorskii Krai

    International Nuclear Information System (INIS)

    Organova, N.I.; Marsii, I.M.; Zakharov, N.D.; Nasedkin, V.V.; Borisovskii, S.B.; Rozhdestvenskaya, I.V.; Ivanova, T.I.

    1999-01-01

    The structures of two components of the decomposed solid solution of an alkali feldspar are refined. These structures exhibit at least two specific features: (1) the complete phase separation into pure K and pure Na phases and (2) an anomalous distribution of Al atoms over four crystallographically independent positions of silicon-aluminum tetrahedra in the Na-component (different from its usual distribution). To explain the results obtained, the ideas of synergetics are invoked (the geological history of the specimen includes a powerful explosion, which threw out the material from the volcano to the Earth's surface)

  19. Alkali/Surfactant/Polymer Flooding in the Daqing Oilfield Class II Reservoirs Using Associating Polymer

    Directory of Open Access Journals (Sweden)

    Ru-Sen Feng

    2013-01-01

    Full Text Available Hydrophobically modified associating polyacrylamide (HAPAM has good compatibility with the Daqing heavy alkylbenzene sulfonate surfactant. The HAPAM alkali/surfactant/polymer (ASP system can generate ultralow interfacial tension in a wide range of alkali/surfactant concentrations and maintain stable viscosity and interfacial tension for 120 days. The HAPAM ASP system has good injectivity for the Daqing class II reservoirs (100–300 × 10−3 μm2 and can improve oil recovery by more than 25% on top of water flooding. In the presence of both the alkali and the surfactant, the surfactant interacts with the associating groups of the polymer to form more micelles, which can significantly enhance the viscosity of the ASP system. Compared with using HPAM (Mw = 2.5 MDa, using HAPAM can reduce the polymer use by more than 40%.

  20. The Thermal Expansion Of Feldspars

    Science.gov (United States)

    Hovis, G. L.; Medford, A.; Conlon, M.

    2009-12-01

    Hovis and others (1) investigated the thermal expansion of natural and synthetic AlSi3 feldspars and demonstrated that the coefficient of thermal expansion (α) decreases significantly, and linearly, with increasing room-temperature volume (VRT). In all such feldspars, therefore, chemical expansion limits thermal expansion. The scope of this work now has been broadened to include plagioclase and Ba-K feldspar crystalline solutions. X-ray powder diffraction data have been collected between room temperature and 925 °C on six plagioclase specimens ranging in composition from anorthite to oligoclase. When combined with thermal expansion data for albite (2,3,4) a steep linear trend of α as a function of VRT emerges, reflecting how small changes in composition dramatically affect expansion behavior. The thermal expansion data for five synthetic Ba-K feldspars ranging in composition from 20 to 100 mole percent celsian, combined with data for pure K-feldspar (3,4), show α-VRT relationships similar in nature to the plagioclase series, but with a slope and intercept different from the latter. Taken as a group all Al2Si2 feldspars, including anorthite and celsian from the present study along with Sr- (5) and Pb-feldspar (6) from other workers, show very limited thermal expansion that, unlike AlSi3 feldspars, has little dependence on the divalent-ion (or M-) site occupant. This apparently is due to the necessitated alternation of Al and Si in the tetrahedral sites of these minerals (7), which in turn locks the tetrahedral framework and makes the M-site occupant nearly irrelevant to expansion behavior. Indeed, in feldspar series with coupled chemical substitution it is the change away from a 1:1 Al:Si ratio that gives feldspars greater freedom to expand. Overall, the relationships among α, chemical composition, and room-temperature volume provide useful predictive tools for estimating feldspar thermal expansion and give insight into the controls of expansion behavior in

  1. Assessment of the Alteration of Granitic Rocks and its Influence on Alkalis Release

    Science.gov (United States)

    Ferraz, Ana Rita; Fernandes, Isabel; Soares, Dora; Santos Silva, António; Quinta-Ferreira, Mário

    2017-12-01

    Several concrete structures had shown signs of degradation some years after construction due to internal expansive reactions. Among these reactions there are the alkali-aggregate reactions (AAR) that occur between the aggregates and the concrete interstitial fluids which can be divided in two types: the alkali-silica reaction (ASR) and alkali-carbonate reaction (ACR). The more common is the ASR which occurs when certain types of reactive silica are present in the aggregates. In consequence, an expansive alkali-silica gel is formed leading to the concrete cracking and degradation. Granites are rocks composed essentially of quartz, micas and feldspars, the latter being the minerals which contain more alkalis in their structure and thus, able to release them in conditions of high alkalinity. Although these aggregates are of slow reaction, some structures where they were applied show evidence of deterioration due to ASR some years or decades after the construction. In the present work, the possible contribution of granitic aggregates to the interstitial fluids of concrete by alkalis release was studied by performing chemical attack with NaOH and KOH solutions. Due to the heterogeneity of the quarries in what concerns the degree of alteration and/or fracturing, rock samples with different alteration were analysed. The alteration degree was characterized both under optical microscope and image analysis and compared with the results obtained from the chemical tests. It was concluded that natural alteration reduces dramatically the releasable alkalis available in the rocks.

  2. Alteration of alkali reactive aggregates autoclaved in different alkali solutions and application to alkali-aggregate reaction in concrete (II) expansion and microstructure of concrete microbar

    International Nuclear Information System (INIS)

    Lu Duyou; Mei Laibao; Xu Zhongzi; Tang Mingshu; Mo Xiangyin; Fournier, Benoit

    2006-01-01

    The effect of the type of alkalis on the expansion behavior of concrete microbars containing typical aggregate with alkali-silica reactivity and alkali-carbonate reactivity was studied. The results verified that: (1) at the same molar concentration, sodium has the strongest contribution to expansion due to both ASR and ACR, followed by potassium and lithium; (2) sufficient LiOH can completely suppress expansion due to ASR whereas it can induce expansion due to ACR. It is possible to use the duplex effect of LiOH on ASR and ACR to clarify the ACR contribution when ASR and ACR may coexist. It has been shown that a small amount of dolomite in the fine-grained siliceous Spratt limestone, which has always been used as a reference aggregate for high alkali-silica reactivity, might dedolomitize in alkaline environment and contribute to the expansion. That is to say, Spratt limestone may exhibit both alkali-silica and alkali-carbonate reactivity, although alkali-silica reactivity is predominant. Microstructural study suggested that the mechanism in which lithium controls ASR expansion is mainly due to the favorable formation of lithium-containing less-expansive product around aggregate particles and the protection of the reactive aggregate from further attack by alkalis by the lithium-containing product layer

  3. Alkali trace elements in Gale crater, Mars, with ChemCam: Calibration update and geological implications

    Science.gov (United States)

    Payré, V.; Fabre, C.; Cousin, A.; Sautter, V.; Wiens, R. C.; Forni, O.; Gasnault, O.; Mangold, N.; Meslin, P.-Y.; Lasue, J.; Ollila, A.; Rapin, W.; Maurice, S.; Nachon, M.; Le Deit, L.; Lanza, N.; Clegg, S.

    2017-03-01

    The Chemistry Camera (ChemCam) instrument onboard Curiosity can detect minor and trace elements such as lithium, strontium, rubidium, and barium. Their abundances can provide some insights about Mars' magmatic history and sedimentary processes. We focus on developing new quantitative models for these elements by using a new laboratory database (more than 400 samples) that displays diverse compositions that are more relevant for Gale crater than the previous ChemCam database. These models are based on univariate calibration curves. For each element, the best model is selected depending on the results obtained by using the ChemCam calibration targets onboard Curiosity. New quantifications of Li, Sr, Rb, and Ba in Gale samples have been obtained for the first 1000 Martian days. Comparing these data in alkaline and magnesian rocks with the felsic and mafic clasts from the Martian meteorite NWA7533—from approximately the same geologic period—we observe a similar behavior: Sr, Rb, and Ba are more concentrated in soluble- and incompatible-element-rich mineral phases (Si, Al, and alkali-rich). Correlations between these trace elements and potassium in materials analyzed by ChemCam reveal a strong affinity with K-bearing phases such as feldspars, K-phyllosilicates, and potentially micas in igneous and sedimentary rocks. However, lithium is found in comparable abundances in alkali-rich and magnesium-rich Gale rocks. This very soluble element can be associated with both alkali and Mg-Fe phases such as pyroxene and feldspar. These observations of Li, Sr, Rb, and Ba mineralogical associations highlight their substitution with potassium and their incompatibility in magmatic melts.

  4. ALKALI RESISTANT CATALYST

    DEFF Research Database (Denmark)

    2008-01-01

    The present invention concerns the selective removal of nitrogen oxides (NOx) from gasses. In particular, the invention concerns a process, a catalyst and the use of a catalyst for the selective removal of nitrogen oxides in the presence of ammonia from gases containing a significant amount...... of alkali metal and/or alkali-earth compounds which process comprises using a catalyst combined of (i) a formed porous superacidic support, said superacidic support having an Hammett acidity stronger than Ho=-12, and (ii) a metal oxide catalytic component deposited on said superacidic support selected from...

  5. Differential rates of feldspar weathering in granitic regoliths

    Science.gov (United States)

    White, A.F.; Bullen, T.D.; Schulz, M.S.; Blum, A.E.; Huntington, T.G.; Peters, N.E.

    2001-01-01

    Differential rates of plagioclase and K-feldspar weathering commonly observed in bedrock and soil environments are examined in terms of chemical kinetic and solubility controls and hydrologic permeability. For the Panola regolith, in the Georgia Piedmont Province of southeastern United States, petrographic observations, coupled with elemental balances and 87Sr/86Sr ratios, indicate that plagioclase is being converted to kaolinite at depths > 6 m in the granitic bedrock. K-feldspar remains pristine in the bedrock but subsequently weathers to kaolinite at the overlying saprolite. In contrast, both plagioclase and K-feldspar remain stable in granitic bedrocks elsewhere in Piedmont Province, such as Davis Run, Virginia, where feldspars weather concurrently in an overlying thick saprolite sequence. Kinetic rate constants, mineral surface areas, and secondary hydraulic conductivities are fitted to feldspar losses with depth in the Panola and Davis Run regoliths using a time-depth computer spreadsheet model. The primary hydraulic conductivities, describing the rates of meteoric water penetration into the pristine granites, are assumed to be equal to the propagation rates of weathering fronts, which, based on cosmogenic isotope dating, are 7 m/106 yr for the Panola regolith and 4 m/106 yr for the Davis Run regolith. Best fits in the calculations indicate that the kinetic rate constants for plagioclase in both regoliths are factors of two to three times faster than K-feldspar, which is in agreement with experimental findings. However, the range for plagioclase and K-feldspar rates (kr = 1.5 x 10-17 to 2.8 x 10-16 mol m-2 s-1) is three to four orders of magnitude lower than for that for experimental feldspar dissolution rates and are among the slowest yet recorded for natural feldspar weathering. Such slow rates are attributed to the relatively old geomorphic ages of the Panola and Davis Run regoliths, implying that mineral surface reactivity decreases significantly with

  6. The chemistry of the liquid alkali metals

    International Nuclear Information System (INIS)

    Addison, C.C.

    1984-01-01

    A study of liquid alkali metals. It encourages comparison with molecular solvents in chapter covering the nature and reactivity of dissolved species, solvation, solubility and electrical conductivity of solutions. It demonstrates lab techniques unique to liquid alkali metals. It discusses large-scale applications from storage batteries to sodium-cooled reactors and future fusion reactors, and associated technological problems. Contents: Some Basic Physical and Chemical Properties; Manipulation of the Liquids; The Chemistry of Purification Methods; Species Formed by Dissolved Elements; Solubilities and Analytical Methods; Alkali Metal Mixtures; Solvation in Liquid Metal; Reactions Between Liquid Alkali Metals and Water; Reactions of Nitrogen with Lithium and the Group II Metals in Liquid Sodium; The Formation, Dissociation and Stability of Heteronuclear Polyatomic Anions; Reactions of the Liquid Alkali Metals and Their Alloys with Simple Alipatic Hydrocarbons; Reactions of the Liquid Alkali Metals with Some Halogen Compounds; Hydrogen, Oxygen and Carbon Meters; Surface Chemistry and Wetting; Corrosion of Transition Metals by the Liquid Alkali Metals; Modern Applications of the Liquid Alkali Metals

  7. Alkali trace elements in Gale crater, Mars, with ChemCam: Calibration update and geological implications

    International Nuclear Information System (INIS)

    Payre, Valerie; Fabre, Cecile; Cousin, Agnes; Sautter, Violaine; Wiens, Roger Craig

    2017-01-01

    The Chemistry Camera (ChemCam) instrument onboard Curiosity can detect minor and trace elements such as lithium, strontium, rubidium, and barium. Their abundances can provide some insights about Mars' magmatic history and sedimentary processes. We focus on developing new quantitative models for these elements by using a new laboratory database (more than 400 samples) that displays diverse compositions that are more relevant for Gale crater than the previous ChemCam database. These models are based on univariate calibration curves. For each element, the best model is selected depending on the results obtained by using the ChemCam calibration targets onboard Curiosity. New quantifications of Li, Sr, Rb, and Ba in Gale samples have been obtained for the first 1000 Martian days. Comparing these data in alkaline and magnesian rocks with the felsic and mafic clasts from the Martian meteorite NWA7533—from approximately the same geologic period—we observe a similar behavior: Sr, Rb, and Ba are more concentrated in soluble- and incompatible-element-rich mineral phases (Si, Al, and alkali-rich). Correlations between these trace elements and potassium in materials analyzed by ChemCam reveal a strong affinity with K-bearing phases such as feldspars, K-phyllosilicates, and potentially micas in igneous and sedimentary rocks. However, lithium is found in comparable abundances in alkali-rich and magnesium-rich Gale rocks. This very soluble element can be associated with both alkali and Mg-Fe phases such as pyroxene and feldspar. Here, these observations of Li, Sr, Rb, and Ba mineralogical associations highlight their substitution with potassium and their incompatibility in magmatic melts.

  8. Decalcification resistance of alkali-activated slag

    Energy Technology Data Exchange (ETDEWEB)

    Komljenovic, Miroslav M., E-mail: miroslav.komljenovic@imsi.rs [Institute for Multidisciplinary Research, University of Belgrade, Kneza Viseslava 1, 11030 Belgrade (Serbia); Bascarevic, Zvezdana, E-mail: zvezdana@imsi.bg.ac.rs [Institute for Multidisciplinary Research, University of Belgrade, Kneza Viseslava 1, 11030 Belgrade (Serbia); Marjanovic, Natasa, E-mail: natasa@imsi.bg.ac.rs [Institute for Multidisciplinary Research, University of Belgrade, Kneza Viseslava 1, 11030 Belgrade (Serbia); Nikolic, Violeta, E-mail: violeta@imsi.bg.ac.rs [Institute for Multidisciplinary Research, University of Belgrade, Kneza Viseslava 1, 11030 Belgrade (Serbia)

    2012-09-30

    Highlights: Black-Right-Pointing-Pointer The effects of decalcification on properties of alkali-activated slag were studied. Black-Right-Pointing-Pointer Decalcification was performed by concentrated NH{sub 4}NO{sub 3} solution (accelerated test). Black-Right-Pointing-Pointer Portland-slag cement (CEM II/A-S 42.5 N) was used as a benchmark material. Black-Right-Pointing-Pointer Decalcification led to strength decrease and noticeable structural changes. Black-Right-Pointing-Pointer Alkali-activated slag showed significantly higher resistance to decalcification. - Abstract: This paper analyses the effects of decalcification in concentrated 6 M NH{sub 4}NO{sub 3} solution on mechanical and microstructural properties of alkali-activated slag (AAS). Portland-slag cement (CEM II/A-S 42.5 N) was used as a benchmark material. Decalcification process led to a decrease in strength, both in AAS and in CEM II, and this effect was more pronounced in CEM II. The decrease in strength was explicitly related to the decrease in Ca/Si atomic ratio of C-S-H gel. A very low ratio of Ca/Si {approx}0.3 in AAS was the consequence of coexistence of C-S-H(I) gel and silica gel. During decalcification of AAS almost complete leaching of sodium and tetrahedral aluminum from C-S-H(I) gel also took place. AAS showed significantly higher resistance to decalcification in relation to the benchmark CEM II due to the absence of portlandite, high level of polymerization of silicate chains, low level of aluminum for silicon substitution in the structure of C-S-H(I), and the formation of protective layer of polymerized silica gel during decalcification process. In stabilization/solidification processes alkali-activated slag represents a more promising solution than Portland-slag cement due to significantly higher resistance to decalcification.

  9. Lead-isotope inhomogeneity in Precambrian igneous K-feldspars

    International Nuclear Information System (INIS)

    Ludwig, K.R.; Silver, L.T.

    1977-01-01

    Stepwise PB-removal experiments, using both vacuum volatilization and HF-leaching techniques, on acid-washed K-feldspar concentrates from Precambrian igneous rocks show that all contain some unsupported radiogenic Pb. Two types of radiogenic Pb were recognised. One has a 'normal' isotopic composition, with relative abundances of 206 Pb, 207 Pb and 208 Pb consistent with the age and U-Th contents of the rocks. The other type of unsupported radiogenic lead in the feldspars is apparently pure 206 Pb, derived from long-term migration and accumulation of radioactive daughter(s) of 238 U. This 'pure' 206 Pb lead occupies different sites from the 'normal' radiogenic lead, and tends to show a release maximum during vacuum volatilization at about 1150 0 C. The usefulness of stepwise vacuum volatilization may be limited by the tendency of a small amount of radiogenic lead to concentrate in the least volatile fraction. Stepwise partial HF attacks appear to give at least as good separation of radiogenic from original feldspar lead, and are recommended as a routine procedure for isotopic analyses of Precambrian feldspars. The fact that most of the five K-feldspars examined contained unsupported radiogenic lead implies that caution must be used in applying total-sample lead analyses of Precambrian feldspars to problems of lead-isotope evolution in crustal rocks. (author)

  10. Understanding optically stimulated charge movement in quartz and feldspar using time-resolved measurements

    International Nuclear Information System (INIS)

    Ankjaergaard, C.

    2010-02-01

    Thermoluminescence (TL) and optically stimulated luminescence (OSL) from quartz and feldspar are widely used in accident dosimetry and luminescence dating. In order to improve already existing methods or to develop new methods towards extending the current limits of the technique, it is important to understand the charge movement within these materials. Earlier studies have primarily focussed on examination of the trap behaviour; however, this only tells half of the story as OSL is a combination of charge stimulation and recombination. By using time-resolved OSL (TR-OSL), one can directly examine the recombination route(s), and thus obtain insight into the other half of the process involved in luminescence emission. This thesis studies the TR-OSL and optically stimulated phosphorescence signals from quartz and feldspars spanning several orders of magnitude in time (few ns to the seconds time scale) in order to identify various charge transport mechanisms in the different time regimes. The techniques employed are time-resolved OSL, continuous-wave OSL, TL, optically stimulated exo-electron (OSE) emission and time-resolved OSE. These different techniques are used in combination with variable thermal or optical stimulation energy. The thesis first delves into three main methodological developments, namely (i) research and development of the equipment for TR-OSL measurements, (ii) finding the best method for multiple-exponential analysis of a TR-OSL curve, and (iii) optimisation of the pulsing configuration for the best separation of quartz OSL from a mixed quarts-feldspar sample. It then proceeds to study the different charge transport mechanisms subsequent to an optical stimulation pulse in quartz and feldspars. The results obtained for quartz conclude that the main lifetime component in quartz represents an excited state lifetime of the recombination centre, and the more slowly decaying components on the millisecond to seconds time scale arise from charge recycling

  11. Understanding optically stimulated charge movement in quartz and feldspar using time-resolved measurements

    Energy Technology Data Exchange (ETDEWEB)

    Ankjaergaard, C.

    2010-02-15

    Thermoluminescence (TL) and optically stimulated luminescence (OSL) from quartz and feldspar are widely used in accident dosimetry and luminescence dating. In order to improve already existing methods or to develop new methods towards extending the current limits of the technique, it is important to understand the charge movement within these materials. Earlier studies have primarily focussed on examination of the trap behaviour; however, this only tells half of the story as OSL is a combination of charge stimulation and recombination. By using time-resolved OSL (TR-OSL), one can directly examine the recombination route(s), and thus obtain insight into the other half of the process involved in luminescence emission. This thesis studies the TR-OSL and optically stimulated phosphorescence signals from quartz and feldspars spanning several orders of magnitude in time (few ns to the seconds time scale) in order to identify various charge transport mechanisms in the different time regimes. The techniques employed are time-resolved OSL, continuous-wave OSL, TL, optically stimulated exo-electron (OSE) emission and time-resolved OSE. These different techniques are used in combination with variable thermal or optical stimulation energy. The thesis first delves into three main methodological developments, namely (i) research and development of the equipment for TR-OSL measurements, (ii) finding the best method for multiple-exponential analysis of a TR-OSL curve, and (iii) optimisation of the pulsing configuration for the best separation of quartz OSL from a mixed quarts-feldspar sample. It then proceeds to study the different charge transport mechanisms subsequent to an optical stimulation pulse in quartz and feldspars. The results obtained for quartz conclude that the main lifetime component in quartz represents an excited state lifetime of the recombination centre, and the more slowly decaying components on the millisecond to seconds time scale arise from charge recycling

  12. Mylonitic volcanics near Puging, Upper Siang district, Arunachal ...

    Indian Academy of Sciences (India)

    the minor presence of tiny plagioclase indicate that the alkali feldspars might have replaced the plagio- clase grains. However, in the mylonitic volcanics, the alkali feldspars, pyroxenes, actinolites and chlo- ritoids appear as porphyroclasts in a matrix dom- inated by feldspar, pyroxene in a calcareous and cherty matrix.

  13. Kiglapait Feldspar States 5 to Review

    Science.gov (United States)

    Morse, S. A.

    2017-12-01

    The 1305 Ga Kiglapait Intrusion of coastal Labrador records the crystallization of troctolite through olivine gabbro to magnetite- and apatite-bearing rocks to monoclinic sanidine- mesoperthite-ferrosyenite below an inverted stratigraphy of a thin Upper Border Zone. The crystallization history was about 1 Ma. ¶The evolutionary history of Kiglapait feldspars in an 8.4 km thick magma chamber runs from plagioclase An70 at 5 kbar and 1250°C, cooling through to ferrosyenite with mesoperthite and two feldspars at 3 kbar and 1,000°C. The residual magma encountered the binodal solvus and finished crystallizing as an azeotrope with plagioclase (Or 21, An 15) and sanidine (Or 52, An 8) in liquid (Xor = 1/3; An 11). Cooling in the subsolidus brought the feldspars to compositions An15-Or 3, An0-Or 80-85 at 800-730°C. Metastable mesoperthite on the coherent solvus in various stages of late equilibration persists in the local assemblages. Arrested to complete feldspar symplectites suggest the local presence of a vapor phase. ¶Splits of the final Or-rich feldspar were found by mass spectrometry to have a dominant quantity of Rb and 87Sr/86Sr along with % amounts of Ba; in contrast, the plag fraction has very low Rb and 87Sr/86Sr. The estimated timing of the isotopic segregation was plausibly continuous with major-element fractionation or perhaps at the moment(s) of exsolution. ¶The cooling record of the solidified intrusion at 3 kbar is shown by 40Ar/39Ar data to have been rapid, reaching an ambient temperature near 240°C within the first 20 Ma, compared to the ambient country-rock temperature before intrusion of 350°C. The difference suggests a late uplift of the region after the Kiglapait magmatism. ¶Contributions from Y. Yu, T. Krogh, M. Hamilton, D. Lindsley, D. DePaolo, M. Jercinovic and S.R. Hart are especially acknowledged.

  14. [Energy related studies utilizing K-feldspar thermochronology

    International Nuclear Information System (INIS)

    1992-01-01

    In our second year of current funding cycle, we have investigated the Ar diffusion properties and microstructures of K-feldspars and the application of domain theory to natural K-feldspars. We completed a combined TEM and argon diffusion study of the effect of laboratory heat treatment on the microstructure and kinetic properties of K-feldspar. We conclude in companion papers that, with one minor exception, no observable change in the diffusion behavior occurs during laboratory extraction procedures until significant fusion occurs at about 1100 degrees C. The effect that is observed involves a correlation between the homogenization of cryptoperthite lamelle and the apparent increase in retentivity of about 5% of the argon in the K-feldspar under study. We can explain this effect of both as an artifact of the experiment or the loss of a diffusion boundary. Experiments are being considered to resolve this question. Refinements have been made to our experimental protocol that appears that greatly enhance the retrieval of multi-activation energies from K-feldspars. We have applied the multi-domain model to a variety of natural environments (Valles Caldera, Red River fault, Appalachian basin) with some surprising results. Detailed 40 Ar/ 39 Ar coverage of the Red River shear zone, thought to be responsible for the accommodation of a significant fraction of the Indo-Asian convergence, strongly suggests that our technique can precisely date both the termination of ductile strike-slip motion and the initiation of normal faulting. Work has continued on improving our numerical codes for calculating thermal histories and the development of computer based graphing tools has significantly increased our productivity

  15. Thermo-optical properties of optically stimulated luminescence in feldspars

    DEFF Research Database (Denmark)

    Poolton, N.R.J.; Bøtter-Jensen, L.; Johnsen, O.

    1995-01-01

    Optically stimulated luminescence processes in feldspars are subject to competing thermal enhancement and quenching processes: this article describes the thermal enhancement effects for orthoclase, albite and plagioclase feldspars. It is demonstrated that certain lattice vibrational modes can be ...

  16. Application of Cathodoluminescence to The Study of Feldspars: Imaging and Spectrometry

    Science.gov (United States)

    Fonseca, Rute; Couto, Helena

    2017-12-01

    Cathodoluminescence (CL) studies were carried out on polished thin sections of different feldspar samples (from migmatites, granites, aplite-pegmatites and granitic aggregates) using a hot cathode CL equipment HC3-LM coupled to an optical microscope and to a spectrometer (SpectraPro 2300i and a CCD Pixis 400B detector and the software Winspec32) from the Faculty of Sciences of University of Porto. The system was operated at 14kV and a filament current of 0.18 mA. The samples were coated with a thin gold film using a Cressington 108 Auto device. Luminescence images were acquired during the CL analysis with an adapted digital video-camera (KAPPA PS 40C-285 (DX) with dual stage Peltier cooling) and an acquisition time between 351ms and 3,52s. The CL study, including imaging and spectrometry, proved to be an important tool to complement the feldspar petrography as it contributes to the identification of features not observed under optical microscope. The application of the Cathodoluminescence to feldspar allows distinguishing between potassic feldspar and plagioclase, differentiating generations of feldspar and displaying internal zoning and growth areas, among other. The spectrometry complements the CL imaging. It allows obtaining a qualitative level of emission intensity, which permits the interpretation of the nature of this luminescence in each feldspar. Bands shown in the spectra are related to the existing activator elements. In the present study, it was found an association of each feldspar to different spectra and respective colour. The plagioclases exhibit yellow or green luminescence. The activator element is Mn2+, showing a broad emission band between 550 - 570 nm specially detected on this type of feldspars, due to the replacement of K+ for Mn2+. The potassium feldspars have more or less intense blue colour associated with various activators elements: the activator element is Cu2+ showing a broad emission band between 420±5 nm. This emission band can be

  17. [Study on the fine structure of K-feldspar of Qichun granite].

    Science.gov (United States)

    Du, Deng-Wen; Hong, Han-Lie; Fan, Kan; Wang, Chao-Wen; Yin, Ke

    2013-03-01

    Fine structure of K-feldspar from the Qichun granite was investigated using X-ray diffraction (XRD), Fourier infrared absorption spectroscopy (FTIR), and inductively coupled plasma mass spectrometry methods to understand the evolution of the granitic magmatism and its correlation to molybdenite mineralization. The XRD results showed that K-feldspar of the potassic alteration veins has higher ordering index and triclinicity and is namely microcline with triclinic symmetry. K-feldspar of the early cretaceous granite has relatively lower ordering index and has widening [131] peak and is locally triclinic ordering. K-feldspar of the late cretaceous granite has lowest ordering index and sharp [131] peak and is honiogeneously monoclinic. The FTIR results showed that the IR spectra of the Qichun K-feldspar are similar to that of orthoclase reported by Farmer (1974). The 640 cm-1 absorption band increases while the 540 cm-' absorption band decreases with increase in K-feldspar ordering index, also, the 1,010 cm-1 absorption band separates into 1,010 and 1,046 cm-1 absorption bands, with a change in the band shape from widening to sharp outline. The ICP-MS results suggested that K-feldspar of the early cretaceous granite has relatively higher metal elements and rare earth elements, and the granite exhibits better mineralization background, K-feldspar of the potassic alteration veins has markedly lower Sr and Ba, indicating that the alteration fluid originated from the granitic magmatism, and hence, potassic alteration is a good indicator for molybdenite exploration.

  18. Muonium centers in the alkali halides

    International Nuclear Information System (INIS)

    Baumeler, H.; Kiefl, R.F.; Keller, H.; Kuendig, W.; Odermatt, W.; Patterson, B.D.; Schneider, J.W.; Savic, I.M.

    1986-01-01

    Muonium centers (Mu) in single crystals and powdered alkali halides have been studied using the high-timing-resolution transverse field μSR technique. Mu has been observed and its hyperfine parameter (HF) determined in every alkali halide. For the rocksalt alkali halides, the HF parameter A μ shows a systematic dependence on the host lattice constant. A comparison of the Mu HF parameter with hydrogen ESR data suggests that the Mu center is the muonic analogue of the interstitial hydrogen H i 0 -center. The rate of Mu diffusion can be deduced from the motional narrowing of the nuclear hyperfine interaction. KBr shows two different Mu states, a low-temperature Mu I -state and a high-temperature Mu II -state. (orig.)

  19. Geology and mineralization of the Jabalat alkali-feldspar granite, northern Asir region, Kingdom of Saudi Arabia

    Science.gov (United States)

    Al Tayyar, Jaffar; Jackson, Norman J.; Al-Yazidi, Saeed

    The Jabalat post-tectonic granite pluton is composed of albite- and oligoclase-bearing, low-calcium, F-, Sn- and Rb-rich subsolvus granites. These granites display evidence of late-magmatic, granitophile- and metallic-element specialization, resulting ultimately in the development of post-magmatic, metalliferous hydrothermal systems characterized by a Mo sbnd Sn sbnd Cu sbnd Pb sbnd Zn sbnd Bi sbnd Ag sbnd F signature. Two main types of mineralization are present within the pluton and its environs: (1) weakly mineralized felsic and aplitic dikes and veins enhanced in Mo, Bi, Ag, Pb and Cu; and (2) pyrite—molybdenite—chalcopyrite-bearing quartz and quartz—feldspar veins rich in Mo, Sn, Bi, Cu, Zn and Ag. A satellite stock, 3 km north of the main intrusion, is composed of fine-grained, miarolitic, muscovite—albite—microcline (microperthite) granite. The flanks of this intrusion and adjacent dioritic rocks are greisenized and highly enriched in Sn, Bi and Ag. Quartz veins which transect the satellite stock contain molybdenite and stannite.

  20. Measurement of the dose in quartz in the presence of feldspar contamination

    DEFF Research Database (Denmark)

    Wallinga, J.; Murray, A.S.; Bøtter-Jensen, L.

    2002-01-01

    To allow the determination of the dose in quartz in the presence of feldspar contamination. the quartz-to-feldspar optically stimulated luminescence (OSL) ratio needs to be maximised. Experiments were carried Out to find the optimum procedure to bleach the feldspar by exposure to infrared light...

  1. Water Content of Lunar Alkali Fedlspar

    Science.gov (United States)

    Mills, R. D.; Simon, J. I.; Wang, J.; Alexander, C. M. O'D.; Hauri, E. H.

    2016-01-01

    Detection of indigenous hydrogen in a diversity of lunar materials, including volcanic glass, melt inclusions, apatite, and plagioclase suggests water may have played a role in the chemical differentiation of the Moon. Spectroscopic data from the Moon indicate a positive correlation between water and Th. Modeling of lunar magma ocean crystallization predicts a similar chemical differentiation with the highest levels of water in the K- and Th-rich melt residuum of the magma ocean (i.e. urKREEP). Until now, the only sample-based estimates of water content of KREEP-rich magmas come from measurements of OH, F, and Cl in lunar apatites, which suggest a water concentration of alkali feldspar, a common mineral in K-enriched rocks, can have approx. 20 ppm of water, which implies magmatic water contents of approx. 1 wt % in the high-silica magmas. This estimate is 2 to 3 orders of magnitude higher than that estimated from apatite in similar rocks. However, the Cl and F contents of apatite in chemically similar rocks suggest that these melts also had high Cl/F ratios, which leads to spuriously low water estimates from the apatite. We can only estimate the minimum water content of urKREEP (+ bulk Moon) from our alkali feldspar data because of the unknown amount of degassing that led to the formation of the granites. Assuming a reasonable 10 to 100 times enrichment of water from urKREEP into the granites produces an estimate of 100-1000 ppm of water for the urKREEP reservoir. Using the modeling of and the 100-1000 ppm of water in urKREEP suggests a minimum bulk silicate Moon water content between 2 and 20 ppm. However, hydrogen loss was likely very significant in the evolution of the lunar mantle. Conclusions: Lunar granites crystallized between 4.3-3.8 Ga from relatively wet melts that degassed upon crystallization. The formation of these granites likely removed significant amounts of water from some mantle source regions, e.g. later mare basalts predicting derivation from a

  2. Developing Effective Separation of Feldspar and Quartz While Recycling Tailwater by HF Pretreatment

    Directory of Open Access Journals (Sweden)

    Weiqing Wang

    2018-04-01

    Full Text Available The effect of hydrofluoric acid (HF pretreatment on flotation of feldspar and quartz using dodecylamine (DDA as collector was investigated by micro-flotation, zeta potential, pyrene fluorescence spectroscopy, attenuated total reflection flourier transformed infrared spectroscopy (ATR-FTIR, scanning electron microscope (SEM, X-ray photoelectron spectroscopy (XPS and bench scale flotation. The micro-flotation tests revealed that there was little difference in the flotation of feldspar and quartz at pH 2, using H2SO4 as pH regulator. After HF pretreatment, the floatability of feldspar significantly increased while the floatability of quartz showed no change. HF pretreatment resulted in leaching of SiO2 and enrichment of Na, K and Al on the feldspar surface. Consequently, the negative surface charge of feldspar increased at pH 2, which allowed for the flotation separation of the feasible minerals. This took place via an increased electrostatic adsorption between DDA and Na, K, Al on the feldspar surface, which effectively increased its hydrophobicity and as a result, improved the floatability of feldspar. An alternative process which exhibited effective separation of quartz and feldspar while recycling the tailwater from the flotation was proposed.

  3. Formation of halloysite from feldspar: Low temperature, artificial weathering versus natural weathering

    Science.gov (United States)

    Parham, Walter E.

    1969-01-01

    Weathering products formed on surfaces of both potassium and plagioclase feldspar (An70), which were continuously leached in a Soxhlet extraction apparatus for 140 days with 7.21 of distilled water per day at a temperature of approximately 78°C, are morphologically identical to natural products developed on potassium feldspars weathered under conditions of good drainage in the humid tropics. The new products, which first appear as tiny bumps on the feldspar surface, start to develop mainly at exposed edges but also at apparently random sites on flat cleavage surfaces. As weathering continues, the bumps grow outward from the feldspar surface to form tapered projections, which then develop into wide-based thin films or sheets. The thin sheets of many projections merge laterally to form one continuous flame-shaped sheet. The sheets formed on potassium feldspars may then roll to form tubes that are inclined at a high angle to the feldspar surface. Etch pits of triangular outline on the artificially weathered potassium feldspars serve as sites for development of continuous, non-rolled, hollow tubes. It is inferred from its morphology that this weathering product is halloysite or its primitive form. The product of naturally weathered potassium feldspars is halloysite . 4H2O.The flame-shaped films or sheets formed on artificially weathered plagioclase feldspar do not develop into hollow tubes, but instead give rise to a platy mineral that is most probably boehmite. These plates form within the flame-shaped films, and with continued weathering are released as the film deteriorates. There is no indication from this experiment that platy pseudohexagonal kaolinite forms from any of these minerals under the initial stage of weathering.

  4. Origin of felsic granulite microstructure by heterogeneous decomposition of alkali feldspar and extreme weakening of orogenic lower crust during the Variscan orogeny

    Czech Academy of Sciences Publication Activity Database

    Franěk, J.; Schulmann, K.; Lexa, O.; Ulrich, Stanislav; Štípská, P.; Haloda, J.; Týcová, P.

    2011-01-01

    Roč. 29, č. 1 (2011), s. 103-130 ISSN 0263-4929 R&D Projects: GA ČR GA205/09/0539 Grant - others:GA ČR(CZ) GA205/05/2187 Institutional research plan: CEZ:AV0Z30120515 Keywords : felsic granulites * Moldanubian domain * quantitative microstructural analysis * quartz and feldspar rheology * Variscan belt Subject RIV: DB - Geology ; Mineralogy Impact factor: 2.990, year: 2011

  5. Assessment of bleaching of K-feldspar grains

    International Nuclear Information System (INIS)

    Zhang Jiafu; Li Shenghua; Tso, M-Y.W.

    2001-01-01

    Based on the difference in the bleaching rate between IRSL and TL signals, a new method of assessing the bleaching of sedimentary feldspar is proposed. All measurements for De and the bleaching factor (normalized ratio of IRSL to TL) are carried out on the same grain. K-feldspar grains from two sediments, a marine and an alluvium, from Hong Kong were tested. Their bleaching factors indicate that bleaching of the marine sediment was not uniform, whereas the latter was relatively homogeneous. Furthermore, the relatively well-bleached grains in each sample were identified

  6. Electrons in feldspar II: A consideration of the influence of conduction band-tail states on luminescence processes

    DEFF Research Database (Denmark)

    Poolton, H.R.J.; Ozanyan, K.B.; Wallinga, J.

    2002-01-01

    consider what influence the band tails have on the luminescence properties of feldspar, where electrons travel through the sample prior to recombination. The work highlights the dominant role that 0.04-0.05-eV phonons play in both the luminescence excitation and emission processes of these materials...

  7. Alkali elemental and potassium isotopic compositions of Semarkona chondrules

    Science.gov (United States)

    Alexander, C.M. O'D.; Grossman, J.N.

    2005-01-01

    We report measurements of K isotope ratios in 28 Semarkona chondrules with a wide range of petrologic types and bulk compositions as well as the compositions of CPX-mesostasis pairs in 17 type I Semarkona chondrules, including two chondrules with radial alkali zonation and 19 type II chondrules. Despite the wide range in K/Al ratios, no systematic variations in K isotopic compositions were found. Semarkona chondrules do not record a simple history of Rayleigh-type loss of K. Experimentally determined evaporation rates suggest that considerable alkali evaporation would have occurred during chondrule formation. Nevertheless, based on Na CPX-mesostasis distribution coefficients, the alkali contents of the cores of most chondrules in Semarkona were probably established at the time of final crystallization. However, Na CPX-mesostasis distribution coefficients also show that alkali zonation in type I Semarkona chondrules was produced by entry of alkalis after solidification, probably during parent body alteration. This alkali metasomatism may have gone to completion in some chondrules. Our preferred explanation for the lack of systematic isotopic enrichments, even in alkali depleted type I chondrule cores, is that they exchanged with the ambient gas as they cooled. ?? The Meteoritical Society, 2005.

  8. Ultrapotassic rocks geology from Salgueiro region, Pernambuco state, Brazil

    International Nuclear Information System (INIS)

    Silva Filho, A.F. da; Guimaraes, I.P.

    1990-01-01

    The Cachoeirinha-Salgueiro belt has Proterozoic age and is located in the Borborema Province, NE Brazil. The ultrapotassic rocks from Salgueiro region intrudes the Cachoeirinha-Salgueiro belt rocks. The ultrapotassics from Salgueiro region constitutes of three units; Serra do Livramento pluton, and two dyke swarms called respectively beige alkali feldspar granites and green alkali feldspar syenite/quartz-syenite. The Serra do Livramento pluton shows E-W direction, boudin shape, width between 0,15 and 2,10 km, and it is intruded into metamorphic rocks and into the Terra Nova complex. Detailed geological mapping at the Serra das Duas Irmas allowed us to establish the dyke swarm chronology. The mapping reveals seven intrusion episodes, into the Terra Nova pluton, of green alkali feldspar syenite/quartz-syenite and five episodes of bege alkali feldspar granite. They alternate between them in space and time, and there are evidence that they were intruded under the tectonic control of the Pernambuco lineament. A systematic whole-rock Rb-Sr geochronology was done in the green alkali feldspar syenite/quartz-syenite, and an age of 514,8 ± 20,3 Ma was obtained. The initial ratio is 0,710615 + 0,000441. The age obtained shows small error and an initial ratio compatible with a strong crustal contamination. (author)

  9. Influence of mesostasis in volcanic rocks on the alkali-aggregate reaction

    KAUST Repository

    Tiecher, Francieli

    2012-11-01

    Mesostasis material present in the interstices of volcanic rocks is the main cause of the alkali-aggregate reaction (AAR) in concretes made with these rock aggregates. Mesostasis often is referred to as volcanic glass, because it has amorphous features when analyzed by optical microscopy. However, this study demonstrates that mesostasis in the interstitials of volcanic rocks most often consists of micro to cryptocrystalline mineral phases of quartz, feldspars, and clays. Mesostasis has been identified as having different characteristics, and, thus, this new characterization calls for a re-evaluation of their influence on the reactivity of the volcanic rocks. The main purpose of this study is to correlate the characteristics of mesostasis with the AAR in mortar bars containing basalts and rhyolites. © 2012 Elsevier Ltd. All rights reserved.

  10. Influence of mesostasis in volcanic rocks on the alkali-aggregate reaction

    KAUST Repository

    Tiecher, Francieli; Dal Molin, Denise Carpena Coitinho; Gomes, Má rcia Elisa Boscato; Hasparyk, Nicole Pagan; Monteiro, Paulo José Meleragno

    2012-01-01

    Mesostasis material present in the interstices of volcanic rocks is the main cause of the alkali-aggregate reaction (AAR) in concretes made with these rock aggregates. Mesostasis often is referred to as volcanic glass, because it has amorphous features when analyzed by optical microscopy. However, this study demonstrates that mesostasis in the interstitials of volcanic rocks most often consists of micro to cryptocrystalline mineral phases of quartz, feldspars, and clays. Mesostasis has been identified as having different characteristics, and, thus, this new characterization calls for a re-evaluation of their influence on the reactivity of the volcanic rocks. The main purpose of this study is to correlate the characteristics of mesostasis with the AAR in mortar bars containing basalts and rhyolites. © 2012 Elsevier Ltd. All rights reserved.

  11. Calcium silicate hydrate: Crystallisation and alkali sorption

    International Nuclear Information System (INIS)

    Hong, S.

    2000-01-01

    Homogeneous single C-S-H gels has been prepared for the investigation of alkali binding potential and crystallisation. A distribution coefficient, R d , was introduced to express the partition of alkali between solid and aqueous phases at 25 deg. C. R d is independent of alkali hydroxide concentration and depends only on Ca:Si ratio over wide ranges of alkali concentration. The trend of numerical values of R d indicates that alkali bonding into the solid improves as its Ca:Si ratio decreases. Reversibility is demonstrated, indicating a possibility of constant R d value of the material. Al has been introduced to form C-A-S-H gels and their alkali sorption properties also determined. Al substituted into C-S-H markedly increases R d , indicating enhancement of alkali binding. However, the dependence of R d on alkali concentration is non-ideal with composition. A two-site model for bonding is presented. Crystallisation both under saturated steam and 1 bar vapour pressure has been investigated. It has been shown that heat treatment by saturated steam causes crystallisation of gels. The principal minerals obtained were (i) C-S-H gel and Ca(OH) 2 at -55 deg. C, (ii) 1.1 nm tobermorite, jennite and afwillite at 85 -130 deg. C, and (iii) xonotlite, foshagite and hillebrandite at 150-180 deg. C. Properties of crystalline C-S-H were also reported for reversible phase transformation, pH conditioning ability, seeding effect and solubility. At 1 bar pressure, crystallisation is slower than in saturated steam due to lower water activity. Tobermorite-like nanodomains develop during reaction at low Ca/Si ratios. In some Ca-rich compositions, Ca(OH) 2 is exsolved and occurs as nano-sized crystallites. (author)

  12. Use of rice straw ash as substitute of feldspar in triaxial porcelain

    International Nuclear Information System (INIS)

    Alvaro Guzman, A.; Silverio Delvasto, A.; Enrique Sanchez, V.; Vicente Amigo, B.

    2013-01-01

    The substitution of raw materials for processing high energy consumption materials by agricultural and agro-industrial wastes causes a positive impacts on the environment preservation. One of these residues is rice straw, which according to FAO estimation, its annual production is about 600 million tons. In this research was studied the use of rice straw ash as substitute of the use of feldspar in the white ware production. Clay-feldspar-quartz porcelains are referred to as triaxial white ware. Specimens of semidry triaxial mixtures, where feldspar was substituted for different percentages of CTA, were prepared by uniaxial pressing, followed by drying and sintering. Physical and mechanical properties of sintered bodies were evaluated. The porosity and the compressive strength of the fired pieces do increase with additions of up to 75% of CTA in substitution of feldspar. Their mineralogical phases were determined by DRX and SEM; grains of quartz, and needles of primary and secondary mullite were identified in a vitreous phase. It was concluded that feldspar can be substituted positively by CTA in white ware pastes. (Author) 22 refs.

  13. Bio-beneficiation of kaolin and feldspar and its effect on fired

    Indian Academy of Sciences (India)

    Presence of iron compounds as impurities in kaolin and feldspar, impart reddish colour to ceramic products manufactured using these minerals. The quality of kaolin and feldspar was enriched mainly through iron removal by biological methods. Bacteria isolated from kaolin of Indian origin were used for bioleaching.

  14. Electrolytic method to make alkali alcoholates using ion conducting alkali electrolyte/separator

    Science.gov (United States)

    Joshi, Ashok V [Salt Lake City, UT; Balagopal, Shekar [Sandy, UT; Pendelton, Justin [Salt Lake City, UT

    2011-12-13

    Alkali alcoholates, also called alkali alkoxides, are produced from alkali metal salt solutions and alcohol using a three-compartment electrolytic cell. The electrolytic cell includes an anolyte compartment configured with an anode, a buffer compartment, and a catholyte compartment configured with a cathode. An alkali ion conducting solid electrolyte configured to selectively transport alkali ions is positioned between the anolyte compartment and the buffer compartment. An alkali ion permeable separator is positioned between the buffer compartment and the catholyte compartment. The catholyte solution may include an alkali alcoholate and alcohol. The anolyte solution may include at least one alkali salt. The buffer compartment solution may include a soluble alkali salt and an alkali alcoholate in alcohol.

  15. Cement Type Influence on Alkali-Silica Reaction in Concrete with Crushed Gravel Aggregate

    Science.gov (United States)

    Rutkauskas, A.; Nagrockienė, D.; Skripkiūnas, G.

    2017-10-01

    Alkali-silica reaction is one of the chemical reactions which have a significant influence for durability of concrete. During alkali and silica reaction, silicon located in aggregates of the concrete, reacts with high alkali content. This way in the micropores of concrete is forming hygroscopic gel, which at wet environment, expanding and slowly but strongly destroying concrete structures. The goal of this paper- to determine the influence of cement type on alkali-silica reaction of mortars with crushed gravel. In the study crushed gravel with fraction 4/16 mm was used and four types of cements tested: CEM I 42.5 R; CEM I 42.5 SR; CEM II/A-S 42.5; CEM II/A-V 52.5. This study showed that crushed gravel is low contaminated on reactive particles containing of amorphous silica dioxide. The expansion after 14 days exceed 0.054 %, by RILEM AAR-2 research methodology (testing specimen dimension 40×40×160 mm). Continuing the investigation to 56 days for all specimens occurred alkaline corrosion features: microcracking and the surface plaque of gel. The results showed that the best resistance to alkaline corrosion after 14 days was obtained with cement CEM I 42.5 SR containing ash additive, and after 56 days with cement CEM II/A-V 52.5 containing low alkali content. The highest expansion after 14 and 56 days was obtained with cement CEM I 42.5 R without active mineral additives.

  16. New insights into the oleate flotation response of feldspar particles of different sizes: Anisotropic adsorption model.

    Science.gov (United States)

    Xu, Longhua; Tian, Jia; Wu, Houqin; Deng, Wei; Yang, Yaohui; Sun, Wei; Gao, Zhiyong; Hu, Yuehua

    2017-11-01

    The anisotropic adsorption of sodium oleate (NaOL) on feldspar surfaces was investigated to elucidate the different flotation properties of feldspar particles of four different size ranges. Microflotation experiments showed that the feldspar flotation recovery of particles with sizes spanning different ranges decreased in the order 0-19>19-38>45-75>38-45μm. Zeta potential and FTIR measurements showed that NaOL was chemically adsorbed on the Al sites of the feldspar surface. The anisotropic surface energies and broken bond densities estimated by density functional theory calculations showed that, although feldspar mostly exposed (010) and (001) surfaces, only the (001) surfaces contained the Al sites needed for NaOL adsorption. The interaction energies calculated by molecular dynamics simulations confirmed the more favorable NaOL adsorption on (001) than (010) surfaces, which may represent the main cause for the anisotropic NaOL adsorption on feldspar particles of different sizes. SEM measurements showed that the main exposed surfaces on coarse and fine feldspar particles were the side (010) and basal (001) ones, respectively. A higher fraction of Al-rich (001) surfaces is exposed on fine feldspar particles, resulting in better floatability compared with coarse particles. XPS and adsorption measurements confirmed that the Al content on the feldspar surface varied with the particle size, explaining the different NaOL flotation of feldspar particles of different sizes. Therefore, the present results suggest that coarsely ground ore should be used for the separation of feldspar gangue minerals. Further improvements in the flotation separation of feldspar from associated valuable minerals can be achieved through selective comminution or grinding processes favoring the exposure of (010) surfaces. Copyright © 2017 Elsevier Inc. All rights reserved.

  17. Laboratory fading rates of various luminescence signals from feldspar-rich sediment extracts

    DEFF Research Database (Denmark)

    Thomsen, Kristina Jørkov; Murray, A.S.; Jain, Mayank

    2008-01-01

    Feldspar as a retrospective dosimeter is receiving more and more attention because of its useful luminescence properties; in particular the dose response curve extends to significantly higher doses than quartz. However, feldspars have one major disadvantage; both the thermoluminescence (TL...

  18. Isochron measurements of naturally irradiated K-feldspar grains

    International Nuclear Information System (INIS)

    Li Bo; Li Shenghua; Wintle, Ann G.; Zhao Hui

    2007-01-01

    The equivalent doses of K-feldspar grains in a range of grain sizes from 90 to 250μm diameter were measured using a single-aliquot regenerative-dose protocol for the infrared stimulated luminescence (IRSL) signals for two samples of desert sand. The equivalent doses for each sample were compared with that for the 125-150μm grains of quartz from the same samples. The results suggested that the K-feldspar equivalent doses were underestimated because of anomalous fading. Measurements of the decay of the IRSL signals following laboratory irradiation for these two samples, and an additional one from a previously published isochron study, showed anomalous fading during the period of laboratory storage. The decay rate was about 3% per decade for all samples and was independent of the grain size used. Using plots of equivalent doses for K-feldspars as a function of their calculated internal dose rate, and the quartz equivalent dose as a function of grain size, it was concluded that the IRSL signal derived from the internal dose rate had not faded over the 13,000 years that had elapsed since the grains were deposited

  19. Quantitative analysis of time-resolved infrared stimulated luminescence in feldspars

    DEFF Research Database (Denmark)

    Pagonis, Vasilis; Ankjærgaard, Christina; Jain, Mayank

    2016-01-01

    Time-resolved infrared-stimulated luminescence (TR-IRSL) from feldspar samples is of importance in the field of luminescence dating, since it provides information on the luminescence mechanism in these materials. In this paper we present new analytical equations which can be used to analyze TR-IR....... The equations are applied to experimental TR-IRSL data of natural feldspars, and good agreement is found between experimental and modeling results....

  20. Optical excitation processes in the near band-edge region of KAlSi3O8 and NaAlSi3O8 feldspar

    DEFF Research Database (Denmark)

    Poolton, N.R.J.; Mauz, B.; Lang, A.

    2006-01-01

    -stimulated phosphorescence and energy-dependent photo-transferred optically stimulated luminescence. The photo-transferred OSL confirms the bandgap energy of alkali feldspars to be 7.7eV at 10K, and highlights the role played by a dominant optically active defect 4.4 eV below the conduction band, associated with blue......)) yielding a characteristically narrow feature at 4.61 eV: significantly, excitation to this level allows photo-transferred OSL to take place, a process that is not obviously identifiable with the other transitions of the set. The conclusion of the work is that synchrotron-based luminescence methods can...

  1. Research on isotope geology. Assessment of heat production potential of granitic rocks and development of geothermal exploration techniques using radioactive/stable isotopes and fission track 2

    Energy Technology Data Exchange (ETDEWEB)

    Shin, Seong Cheon; Chi, Se Jung [Korea Inst. of Geology Mining and Materials, Taejon (Korea, Republic of)

    1995-12-01

    Radioelements and heat production rates of granitic rocks and stable isotopes of groundwaters were analyzed to investigate the geothermal potential of Wolchulsan granite complex in the southern Yeongam area. Wolchulsan granite complex is composed mainly by Cretaceous pink alkali-feldspar granite and partly Jurassic biotite granite. The main target for the geothermal exploration is the alkali-feldspar granite that is known in general to be favorable geothermal reservoir(e.g., Shap granite in UK). To develop exploration techniques for geothermal anomalies, all geochemical data were compared to those from the Jeonju granite complex. Heat production rates(HPR) of the alkali-feldspar granite is 1.8 - 10.6 {mu}Wm{sup -3}. High radio-thermal anomalies were revealed from the central western and northern parts of the granite body. These are relatively higher than the Caledonian hot dry granites in the UK. The integrated assessment of Wolchulsan granite complex suggests potential of the Cretaceous alkali-feldspar granite as a geothermal targets. Groundwater geochemistry of the Yeongam area reflects simple evaporation process and higher oxidation environment. Stable isotope data of groundwaters are plotted on or close to the Meteoric Water Line(MWL). These isotopic data indicate a significant meteoric water dominance and do not show oxygen isotope fractionation between groundwater and wall rocks. In despite of high HPR values of the Yeongam alkali-feldspar granite, groundwater samples do not show the same geochemical properties as a thermal water in the Jeonju area. This reason can be well explained by the comparison with geological settings of the Jeonju area. The Yeongam alkali-feldspar granite does not possess any adjacent heat source rocks despite its high radio-thermal HPR. While the Jeonju granite batholith has later heat source intrusive and suitable deep fracture system for water circulation with sedimentary cap rocks. (Abstract Truncated)

  2. CHARACTERIZATION OF MERCURY EMISSIONS AT A CHLOR-ALKALI PLANT, VOLUME II. APPENDICES F-J

    Science.gov (United States)

    The report gives results of a characterization of mercury (Hg) emissions at a chlor-alkali plant. Up to 160 short tons (146 Mg) of Hg is consumed by the chlor-alkali industry each year. Very little quantitative information is currently available however, on the actual Hg losses f...

  3. Plasma assisted measurements of alkali metal concentrations in pressurized combustion processes

    International Nuclear Information System (INIS)

    Hernberg, R.; Haeyrinen, V.

    1995-01-01

    The plasma assisted method for continuous measurement of alkali metal concentrations in product gas flows of pressurized energy processes will be tested and applied at the 1.6 MW PFBC/G facility at Delft University of Technology in the Netherlands. Measurements will be performed during 1995 and 1996 at different stages of the research programme. The results are expected to give information about the influence of different process conditions on the generation of alkali metal vapours, the comparison of different methods for alkali measurement and the specific performance of our system. The project belongs to the Joule II extension program under contract JOU2-CT93-0431. (author)

  4. Single-grain dating of young sediments using the pIRIR signal from feldspar

    DEFF Research Database (Denmark)

    Reimann, Tony; Thomsen, Kristina Jørkov; Jain, Mayank

    2012-01-01

    In this article we test for the first time the potential of single-grains of K-rich feldspar to date well-bleached and poorly bleached sediments using a post-IR IRSL (pIRIR) protocol. We measure natural dose distributions using K-rich feldspars from four coastal samples applying the pIRIR protocol.......5%.The analysis of the well-bleached samples shows that only the brightest 30% of the grains give pIRIR single-grain ages in agreement with the age control; this effect may arise from the suggested correlation between blue emission and potassium content of individual grains. Comparison of single......-grain quartz and feldspar dose distributions from the poorly bleached samples shows that quartz is relatively better bleached; nevertheless, selection of a reliable ‘minimum’ feldspar dose was achieved using two different statistical models....

  5. Beryllium(II), manganese(II) and uranyl(VI)-salicylamide complexes

    Energy Technology Data Exchange (ETDEWEB)

    Maurya, P L; Agarwala, B V; Dey, A K [Allahabad Univ. (India)

    1977-01-01

    The preparation, composition, general properties and i.r. absorption spectra of the solid chelates formed by salicylamide with beryllium(II), manganese(II) and uranyl(VI) are described. The complexes have been synthesized by refluxing a mixture of ethanolic solutions of the reactants (metal:ligand :: 1:2) for several hours in the presence of alkali. Attempts to isolate the complexes by the interaction of ethanolic solutions of the metal salts and the ligand in the absence of alkali did not succeed.

  6. Iron removal on feldspar by using Averrhoa bilimbii as bioleaching agent

    Science.gov (United States)

    Amin, Muhammad; Aji, Bramantyo B.; Supriyatna, Yayat Iman; Bahfie, Fathan

    2017-01-01

    Investigation of Averrhoa bilimbii as bioleaching agent was carried out. Parameters of leaching duration, acid concentration, and temperature were performed in iron removal process. Feldspar with sized 149 µm was diluted in 30 ml acid solution in order to reduce its iron content. The experimental results showed a good technical feasibility of the process which iron oxide content of feldspar was decreased from 2.24% to 0.29%. The lowest iron concentration remained was obtained after 5 hours of leaching treatment at 60 °C, and concentrated (100 vol%) Averrhoa bilimbii extract as bioleaching agent. SEM characterizations were carried out on the feldspar before and after the leaching treatment. The result shows that there were no significant effect of leaching process on the ore morphology.

  7. Salinity-Dependent Adhesion Response Properties of Aluminosilicate (K-Feldspar) Surfaces

    DEFF Research Database (Denmark)

    Lorenz, Bärbel; Ceccato, Marcel; Andersson, Martin Peter

    2017-01-01

    is composed predominantly of quartz with some clay, but feldspar grains are often also present. While the wettability of quartz and clay surfaces has been thoroughly investigated, little is known about the adhesion properties of feldspar. We explored the interaction of model oil compounds, molecules...... in well sorted sandstone. Adhesion forces, measured with the chemical force mapping (CFM) mode of atomic force microscopy (AFM), showed a low salinity effect on the fresh feldspar surfaces. Adhesion force, measured with -COO(H)-functionalized tips, was 60% lower in artificial low salinity seawater (LS......, ∼1500 ppm total dissolved solids) than in the high salinity solution, artificial seawater (HS, ASW, ∼35 600 ppm). Adhesion with the -CH3 tips was as much as 30% lower in LS than in HS. Density functional theory calculations indicated that the low salinity response resulted from expansion of the electric...

  8. Luminescence characterization of a sodium rich feldspar

    International Nuclear Information System (INIS)

    Correcher, V.; Sanchez M, L.; Garcia G, J.; Rivera, T.

    2006-01-01

    This paper reports on the radioluminescence (RL) and thermoluminescence (TL) properties of a sodium rich feldspar ((Na,K)[AlSi 3 O 8 ]) with a mean molecular composition of orthoclase (Or) and albite (Ab) of Or 1 Ab 99 . Despite the complexity of the luminescence signals of the sample, it is possible to determine six different emission bands at about 300, 380, 420, 460, 550 and 680 nm. The 300 nm emission can be associated to structural defects related to the recombination process in which the Na + ion diffusion-limited is involved. The UV-blue emission band at (i) 380 nm is characteristic of mineral phases containing SiO 4 tetrahedral and could be related to intrinsic defects in the lattice, (ii) the 420 nm band could be associated to the presence of Cu (II) ions placed next to the hole traps or the recombination on a centre formed from a hole-oxygen atom adjacent to two Al atoms (Al-O-Al) and (iii) the 460 nm waveband could be due to the presence of Ti 4+ . The green and red emissions are respectively associated to the presence of Mn 2+ and Fe 3+ ions. The ratio between the relative intensities, peaked at 290 (the more intense waveband) and 550 nm is about 10:1 in both TL and RL; this fact indicates that the efficiency of recombination centres does no changes regardless on the type of the process. (Author)

  9. Feldspar basalts in lunar soil and the nature of the lunar continents

    Science.gov (United States)

    Reid, A. M.; Ridley, W. I.; Harmon, R. S.; Warner, J.; Brett, R.; Jakes, P.; Brown, R. W.

    1974-01-01

    It is found that 25% on the Apollo-14 glasses have the same composition as the glasses in two samples taken from the Luna-16 column. The compositions are equivalent to feldspar basalt and anorthosite gabbro, and are similar to the feldspar basalts identified from Surveyor-7 analysis for lunar continents.

  10. Stoneware tile manufacturing using rice straw ash as feldspar replacement

    International Nuclear Information System (INIS)

    Alvaro Guzman, A.; John Torres, L.; Martha Cedeno, V.; Silvio Delvasto, A.; Vicente Amigo, B.; Enrique Sanchez, V.

    2013-01-01

    In this research are presented the results of using rice straw ash (RSA) in low proportions as substitute of feldspar for manufacturing stoneware tiles. Specimens of semidry triaxial mixtures, where feldspar was substituted for different percentages (25 % and 50 %) of RSA, were prepared by uniaxial pressing, followed by drying and sintering. Physical and mechanical properties of sintered bodies were evaluated. Porcelain stoneware tile specimens C0 and CF25 reached bending strength and water absorption values were in accordance with standard ISO 13006 (Annex G, BIa) ( ≥ 35 MPa and ≤ 0.5 %, respectively). However, in porcelain stoneware tile specimens CF50 due to bloating phenomenon was not possible obtain commercial tiles in accordance with standard ISO 13006. By using Scanning Electron Microscopy (SEM) needles of primary and secondary mullite were identified in a vitreous phase; and by using X-Ray Diffraction (XRD) mullite and quartz phases were identified. It was concluded that feldspar can be substituted positively by RSA in stoneware tile pastes. (Author)

  11. Probing luminescence centers in Na rich feldspar

    DEFF Research Database (Denmark)

    Prasad, Amit Kumar; Lapp, Torben; Kook, Myung Ho

    2016-01-01

    our understanding of the luminescence mechanisms and recombination sites, in a sample of Na rich plagioclase feldspar (oligoclase). Both the UV and violet–blue emissions show resonant excitations arising from a distribution of energy levels. We propose, contrary to the general understanding...

  12. Determining the K-content of single-grains of feldspar for luminescence dating

    International Nuclear Information System (INIS)

    Smedley, R.K.; Duller, G.A.T.; Pearce, N.J.G.; Roberts, H.M.

    2012-01-01

    Feldspars form a solid-solution series whereby the K-content may range from 0 to 14%. LA-ICP-MS measurements for density-separated single-grains of feldspar yielded realistic concentrations of K within the range of those naturally occurring, and also highlighted the difficulty in isolating the pure end members during density-separation. No direct relationship was found between the thermal stability of the infrared-stimulated luminescence (IRSL) signal and measured K-content of individual grains. However, the brightest IRSL and post-IR IRSL signals originated from grains with ∼12% K-content. All grains giving a measurable signal had K-content between 6 and 13%, therefore it is suggested that an internal K-content of 10 ± 2% can be assumed for routine single-grain dating of density-separated K-feldspars. - Highlights: ► Measure range of K for single-grains of density separated feldspar using LA-ICP-MS. ► Single-grain thermal stability and brightness do not directly relate to K-content. ► Brightest 3 grains measured ∼12% K and provided the majority of the IRSL signals.

  13. Hydrothermal alteration of plagioclase and growth of secondary feldspar in the Hengill Volcanic Centre, SW Iceland

    Science.gov (United States)

    Larsson, D.; Grönvold, K.; Oskarsson, N.; Gunnlaugsson, E.

    2002-05-01

    Dissolution of igneous feldspar and the formation and occurrence of secondary feldspar in tholeiitic basalts from the Hengill volcanic centre, in SW Iceland was studied by microprobe analysis of cuttings from two ca. 2000 m deep geothermal wells. Well NG-7 in Nesjavellir represents a geothermal system in a rift zone where the intensity of young, insignificantly altered intrusions increases with depth. Well KhG-1 in Kolviðarhóll represents the margin of a rift zone where the intensity of intrusives is lower and the intensity of alteration higher. This marginal well represents altered basaltic crust in an early retrograde state. The secondary plagioclase in both wells is mainly oligoclase, occurring in association with K-feldspar and chlorite±actinolite. The texture of this assemblage depends on the lithology and intensity of alteration. In Nesjavellir (NG-7) the composition of secondary albite-oligoclase is correlated with the host-rock composition. This connection is not apparent in more intensely altered samples from Kolviðarhóll (KhG-1). The influence of temperature on composition of secondary Na-feldspar is unclear in both wells although Ca is expected to increase with temperature. Any temperature dependence may be suppressed by the influence of rock composition in Nesjavellir and by retrograde conditions at Kolviðarhóll. The absence of clear compositional gradients between igneous plagioclase and secondary feldspar and between Na-feldspar and K-feldspar suggests that secondary feldspars formed by dissolution precipitation reactions.

  14. Kinetics of infrared stimulated luminescence from feldspars

    DEFF Research Database (Denmark)

    Jain, Mayank; Sohbati, Reza; Guralnik, Benny

    2015-01-01

    thermal and optical, of the infrared stimulated luminescence signal from feldspar. Based on the application of this model, it is concluded that different infra-red stimulated luminescence emissions (UV, blue, yellow and far-red) follow the same kinetics, and, therefore, involve participation of the same...

  15. OSL, TL and IRSL emission spectra of sedimentary quartz and feldspar samples

    International Nuclear Information System (INIS)

    Lomax, Johanna; Mittelstraß, Dirk; Kreutzer, Sebastian; Fuchs, Markus

    2015-01-01

    This contribution presents a variety of different luminescence emission spectra from sedimentary feldspar and quartz samples under various stimulation modes. These are green stimulated quartz (OSL-) spectra, quartz TL spectra, feldspar IRSL and post-IR IRSL spectra. A focus was set at recording OSL and IRSL spectra at elevated stimulation temperatures such as routinely applied in luminescence dating. This was to test whether optical stimulation at elevated temperatures results in a shift of emission peaks. For OSL emissions of quartz, this has so far not been tested. In case of feldspar emissions, post-IR IRSL conditions, hence IRSL emissions at a low temperature, directly followed by high temperature post-IRSL emissions, are explicitly investigated. All spectra were recorded using a new system incorporated into a Lexsyg luminescence reader. Thus, this study, besides presenting new spectral data, also serves as a feasibility study for this new device. It is shown that (a) the new device is capable of automatically measuring different sorts of spectra, also at elevated temperatures, (b) known thermally and optically stimulated peak emissions of quartz and feldspar are confirmed, (c) obtained IRSL and OSL spectra indicate that there is no significant relation between peak emission and stimulation temperature. - Highlights: • We have measured OSL, IRSL and TL emission spectra of sedimentary quartz and feldspar samples. • Spectral analyses were performed at elevated stimulation temperatures. • Emission spectra show very little variation with stimulation temperatures.

  16. Further investigations into pulsed optically stimulated luminescence from feldspars using blue and green light

    DEFF Research Database (Denmark)

    Ankjærgaard, Christina; Jain, Mayank; Kalchgruber, R.

    2009-01-01

    The purpose of this paper is to investigate characteristics of luminescence signals resulting from pulsed optical stimulation of feldspars and thereby to understand the underlying processes giving rise to the signal. Fourteen different feldspar specimens were investigated using time-resolved opti......The purpose of this paper is to investigate characteristics of luminescence signals resulting from pulsed optical stimulation of feldspars and thereby to understand the underlying processes giving rise to the signal. Fourteen different feldspar specimens were investigated using time...... suggests that the TR-OSL signal decay is governed by the recombination process and not by the excited state lifetime. Furthermore data from the TR-OSL signal dependence on stimulation time and preheat temperature suggest that the recombination process may not be a sum of exponentials, although the model...... cannot be rejected definitively....

  17. Alkali silica reaction (ASR) in cement free alkali activated sustainable concrete.

    Science.gov (United States)

    2016-12-19

    This report summarizes the findings of an experimental evaluation into alkali silica : reaction (ASR) in cement free alkali-activated slag and fly ash binder concrete. The : susceptibility of alkali-activated fly ash and slag concrete binders to dele...

  18. Process to separate alkali metal salts from alkali metal reacted hydrocarbons

    Energy Technology Data Exchange (ETDEWEB)

    Gordon, John Howard; Alvare, Javier; Larsen, Dennis; Killpack, Jeff

    2017-06-27

    A process to facilitate gravimetric separation of alkali metal salts, such as alkali metal sulfides and polysulfides, from alkali metal reacted hydrocarbons. The disclosed process is part of a method of upgrading a hydrocarbon feedstock by removing heteroatoms and/or one or more heavy metals from the hydrocarbon feedstock composition. This method reacts the oil feedstock with an alkali metal and an upgradant hydrocarbon. The alkali metal reacts with a portion of the heteroatoms and/or one or more heavy metals to form an inorganic phase containing alkali metal salts and reduced heavy metals, and an upgraded hydrocarbon feedstock. The inorganic phase may be gravimetrically separated from the upgraded hydrocarbon feedstock after mixing at a temperature between about 350.degree. C. to 400.degree. C. for a time period between about 15 minutes and 2 hours.

  19. Angrites: A Volatile-rich Variety of Asteroidal Basalt (Except for Alkalis and Gallium!)

    Science.gov (United States)

    Warren, P. H.; Kallemeyn, G. W.

    1995-09-01

    Angrites are commonly viewed as extremely volatile-depleted, and a related notion is that they formed by differentiation of a very CAI-rich material [e.g., 1]. Partial melting experiments reportedly reproduce the bulk compositions (although not fassaite-rich mineralogy) of angrites with Allende as starting material [2], but highly CAI-rich parent materials are difficult to reconcile with isotopic and REE data [3,4]. Mittlefehldt and Lindstrom [5] inferred from the low Na/Al ratios of angrites that outgassing, and thus primordial magmatism, was more intense on their parent body than on the eucrite parent asteroid. Of seven elements that (a) have been adequately determined in angrites, and (b) are far more volatile (solar-nebula 50% condensation T [6] = 690-430 K) than the alkalis (1000-910 K), four are enriched, and none is significantly depleted, in average angrite compared to average eucrite or low-Ti mare basalt (Figure). Gallium, which is of intermediate volatility (830 K), is depleted to roughly the same extent as Na and K. Results for A881371 [3] are incomplete (Zn, 6 micrograms/g, is near INAA detection limit), but even based only on AdoR and the two LEW angrites, this pattern seems firmly established. Apparent gas cavities in A881371 [7] also suggest that volatiles are far from uniformly depleted. The only elements known to be depleted, as volatiles, by clearly significant factors in angrites versus eucrites or lunar basalts, are alkalis plus gallium. Besides being moderately volatile, a noteworthy characteristic shared among Ga and alkalis (and not shared with elements such as Br, Se, and Zn) is that these elements probably tend to partition into crustal feldspar during gross differentiation of small (low-pressure) bodies. If gallium + alkalis were depleted by a single process starting from "normal" chondritic material, that process would seem to require selective exposure of a feldspar-enriched region (i.e., crust) to extremely high temperature. Igneous

  20. Application of pulsed OSL to the separation of the luminescence components from a mixed quartz/feldspar sample

    International Nuclear Information System (INIS)

    Denby, P.M.; Botter-Jensen, L.; Murray, A.S.; Thomsen, K.J.; Moska, P.

    2006-01-01

    It is known that the pulsed optically stimulated luminescence (OSL) characteristics of quartz and feldspars are very different. These differences can be used to preferentially discriminate against the feldspar signal in mixed quartz-bar feldspar mineral assemblages, or in separated quartz contaminated with a feldspar signal. We have developed instrumentation for the study of high-speed pulse stimulated OSL. Our system uses the standard blue/IR LED stimulation unit of a Riso reader (allowing stimulation pulses down to 1-2μs duration) and can thus be applied to the routine analysis of samples. Using this stimulation source, and high-speed photon timing, the OSL yield can be monitored throughout the pulsing cycle and subsequent OSL decay. It is found that the total photon yield per unit stimulation power in pulsed mode is, for quartz, twice and, for feldspar, nearly four times, that in continuous wave mode. Observation of this OSL signal, between stimulation pulses, is seen to be characteristic of the mineral being examined, and has been used to preferentially discriminate against feldspar contamination in a mixed quartz/feldspar sample. Simple implementation of this technique by gating the counting period, so that counts are only accumulated during a windowed period, reduces the feldspar signal to 1.6% of its original value relative to that of the quartz

  1. Plasma assisted measurements of alkali metal concentrations in pressurized combustion processes

    Energy Technology Data Exchange (ETDEWEB)

    Hernberg, R.; Haeyrinen, V. [Tampere Univ. of Technology (Finland). Dept. of Physics

    1996-12-01

    The plasma assisted method for continuous measurement of alkali concentrations in product gas flows of pressurized energy processes will be tested and applied at the 1.6 MW PFBC/G facility at Delft University of Technology in the Netherlands. During the reporting period the alkali measuring device has been tested under pressurized conditions at VTT Energy, DMT, Foster-Wheeler Energia and ABB Carbon. Measurements in Delft will be performed during 1996 after installation of the hot gas filter. The original plan for measurements in Delft has been postponed due to schedule delays in Delft. The results are expected to give information about the influence of different process conditions on the generation of alkali vapours, the comparison of different methods for alkali measurement and the specific performance of our system. This will be the first test of the plasma assisted measurement method in a gasification process. The project belongs to the Joule II extension program under contract JOU2-CT93-0431. (author)

  2. IRSL dating of K-feldspars: Modelling natural dose response curves to deal with anomalous fading and trap competition

    International Nuclear Information System (INIS)

    Kars, Romee H.; Wallinga, Jakob

    2009-01-01

    We recently proposed a model that reconstructs the natural dose response curve for K-rich feldspars, using laboratory fading measurements and dose response as input parameters. The model is based on the relationship between recombination centre density and trap lifetime. In this study we test the working of the model by comparing modelled feldspar ages with known quartz OSL ages of the same samples and with anomalous fading-corrected feldspar ages. The modelled feldspar ages are in good agreement with quartz OSL ages and corrected feldspar ages, opening possibilities for future use of the model on samples without independent age constraints. Furthermore, we investigate the effects of trap competition on the build-up of IRSL signal using two new variations of the model. Results show that incorporating trap competition into the model reduces the agreement between feldspar IRSL ages and quartz OSL ages.

  3. Optimising the separation of quartz and feldspar optically stimulated luminescence using pulsed excitation

    International Nuclear Information System (INIS)

    Ankjaergaard, C.; Jain, M.; Thomsen, K.J.; Murray, A.S.

    2010-01-01

    In luminescence dating, the two most commonly used natural minerals, quartz and feldspar, are exposed to different dose rates in the natural environment, and so record different doses. The luminescence signals also have different stabilities. For accurate dosimetry, the signals from these two minerals must be separated, either by physical separation of the mineral grains, or by instrumental separation of the luminescence signals. The luminescence signals from quartz and feldspar have different luminescence lifetimes under pulsed optical stimulation. This difference in lifetime can be used to discriminate between the two signals from a mixed quartz-feldspar sample. The purpose of this study is to identify optimum measurement conditions for the best separation of quartz OSL from that of feldspar in a mixed sample using pulsed stimulation and time-resolved OSL. We integrate the signal from 5 μs after the LEDs are switched off until just before the LEDs are switched on again, with the pulse on-time equal to the pulse off-time of 50 μs. By using only the initial interval of the pulsed OSL decay curve (equivalent to 0.2 s of CW-OSL using blue light at 50 mW cm -2 ) we find that the quartz to feldspar pulsed OSL intensity ratio is at a maximum. By using these parameters with an additional infrared (IR) stimulation at 175 o C before measurement (to further reduce the feldspar signal intensity), we obtain a factor of 25 enhancement in signal separation compared to that from a conventional prior-IR CW measurement. This ratio can be further improved if the counting window in the pulse off-time is restricted to detect between 20 and 50 μs instead of the entire off-period.

  4. Effect of ageing of K-feldspar on its ice nucleating efficiency in immersion, deposition and contact freezing modes

    Science.gov (United States)

    Peckhaus, Andreas; Bachmann, Felix; Hoffmann, Nadine; Koch, Michael; Kiselev, Alexei; Leisner, Thomas

    2015-04-01

    Recently K-feldspar was identified as one of the most active atmospheric ice nucleating particles (INP) of mineral origin [1]. Seeking the explanation to this phenomena we have conducted extensive experimental investigation of the ice nucleating efficiency of K-feldspar in three heterogeneous freezing modes. The immersion freezing of K-feldspar was investigated with the cold stage using arrays of nanoliter-size droplets containing aqueous suspension of polydisperse feldspar particles. For contact freezing, the charged droplets of supercooled water were suspended in the laminar flow of the DMA-selected feldspar-containing particles, allowing for determination of freezing probability on a single particle-droplet contact [2]. The nucleation and growth of ice via vapor deposition on the crystalline surfaces of macroscopic feldspar particles have been investigated in the Environmental Scanning Electron Microscope (ESEM) under humidified nitrogen atmosphere. The ice nucleation experiments were supplemented with measurements of effective surface area of feldspar particles and ion chromatography (IC) analysis of the leached framework cations (K+, Na+, Ca2+, Mg2+). In this contribution we focus on the role of surface chemistry influencing the IN efficiency of K-feldspar, in particular the connection between the degree of surface hydroxylation and its ability to induce local structural ordering in the interfacial layer in water molecules (as suggested by recent modeling efforts). We mimic the natural process of feldspar ageing by suspending it in water or weak aqueous solution of carbonic acid for different time periods, from minutes to months, and present its freezing efficiency as a function of time. Our immersion freezing experiments show that ageing have a nonlinear effect on the freezing behavior of feldspar within the investigated temperature range (-40°C to -10°C). On the other hand, deposition nucleation of ice observed in the ESEM reveals clear different pattern

  5. Climatic aridity over India 11,000 years ago: Evidence from feldspar distribution in shelf sediments

    Digital Repository Service at National Institute of Oceanography (India)

    Hashimi, N.H.; Nair, R.R.

    Feldspars and quartz contents of sand and silt fractions of forty three samples from the western continental shelf of India were determined by the X-ray diffraction method. The results indicate that the feldspar content in the relict (9000...

  6. Use of rice straw ash as substitute of feldspar in triaxial porcelain

    OpenAIRE

    Guzmán, Álvaro; Delvasto, Silvio; Sánchez, Enrique; Amigó Borrás, Vicente

    2013-01-01

    [EN] The substitution of raw materials for processing high energy consumption materials by agricultural and agro-industrial wastes causes a positive impacts on the environment preservation. One of these residues is rice straw, which according to FAO estimation, its annual production is about 600 million tons. In this research was studied the use of rice straw ash (RSA) as substitute of the use of feldspar in the whiteware production. Clay-feldspar-quartz porcelains are referred to...

  7. Evaluation of The Use of Bentonite, Kaolin and Feldspar For Immobilizing The Uranium Radionuclide Slugdewaste

    International Nuclear Information System (INIS)

    Prayitno

    2006-01-01

    The experimental investigation on the mixture of bentonite, kaolin, feldspar, sludge waste and with the ratio of bentonite, kaolin, feldspar for evaluating its effectiveness has been done. Experimentally, this investigation is the preliminary study of the use of bentonite, kaolin, feldspar as a material for the immobilization of sludge waste containing material element especially uranium. This investigation was conducted by mixing waste (2,5; 5; 7.5; 10; 12.5 and 15 %) of total weight sludge waste and bentonite, kaolin, feldspar with of 800, 900 and 1000 o C temperature. The obtained the process condition in which the uranium fraction immobilized could be kept in the limit of safety standard for the sludge waste. Therefore, it could be concluded that the addition of hay ash as an additive in the formation of block monolith tend to minimize the leached sludge waste in the leaching media. (author)

  8. Alkali metal and alkali earth metal gadolinium halide scintillators

    Science.gov (United States)

    Bourret-Courchesne, Edith; Derenzo, Stephen E.; Parms, Shameka; Porter-Chapman, Yetta D.; Wiggins, Latoria K.

    2016-08-02

    The present invention provides for a composition comprising an inorganic scintillator comprising a gadolinium halide, optionally cerium-doped, having the formula A.sub.nGdX.sub.m:Ce; wherein A is nothing, an alkali metal, such as Li or Na, or an alkali earth metal, such as Ba; X is F, Br, Cl, or I; n is an integer from 1 to 2; m is an integer from 4 to 7; and the molar percent of cerium is 0% to 100%. The gadolinium halides or alkali earth metal gadolinium halides are scintillators and produce a bright luminescence upon irradiation by a suitable radiation.

  9. Full analysis of feldspar texture and crystal structure by combining X-ray and electron techniques

    DEFF Research Database (Denmark)

    Balic Zunic, Tonci; Piazolo, Sandra; Katerinopoulou, Anna

    2013-01-01

    identification plus crystal structure refinement of all components in a feldspar intergrowth. This procedure was applied to perthitic intergrowths in feldspars from two different pegmatites in the Larvik plutonic complex in the southern part of the Oslo region, Norway. It revealed that the two starting high...

  10. Milk-alkali syndrome

    Science.gov (United States)

    Calcium-alkali syndrome; Cope syndrome; Burnett syndrome; Hypercalcemia; Calcium metabolism disorder ... Milk-alkali syndrome is almost always caused by taking too many calcium supplements, usually in the form of calcium carbonate. Calcium ...

  11. Liquid alkali metals and alkali-based alloys as electron-ion plasmas

    International Nuclear Information System (INIS)

    Tosi, M.P.

    1981-06-01

    The article reviews the theory of thermodynamic and structural properties of liquid alkali metals and alkali-based alloys, within the framework of linear screening theory for the electron-ion interactions. (author)

  12. Time-resolved infrared stimulated luminescence signals in feldspars: Analysis based on exponential and stretched exponential functions

    International Nuclear Information System (INIS)

    Pagonis, V.; Morthekai, P.; Singhvi, A.K.; Thomas, J.; Balaram, V.; Kitis, G.; Chen, R.

    2012-01-01

    Time-resolved infrared-stimulated luminescence (TR-IRSL) signals from feldspar samples have been the subject of several recent experimental studies. These signals are of importance in the field of luminescence dating, since they exhibit smaller fading effects than the commonly employed continuous-wave infrared signals (CW-IRSL). This paper presents a semi-empirical analysis of TR-IRSL data from feldspar samples, by using a linear combination of exponential and stretched exponential (SE) functions. The best possible estimates of the five parameters in this semi-empirical approach are obtained using five popular commercially available software packages, and by employing a variety of global optimization techniques. The results from all types of software and from the different fitting algorithms were found to be in close agreement with each other, indicating that a global optimum solution has likely been reached during the fitting process. Four complete sets of TR-IRSL data on well-characterized natural feldspars were fitted by using such a linear combination of exponential and SE functions. The dependence of the extracted fitting parameters on the stimulation temperature is discussed within the context of a recently proposed model of luminescence processes in feldspar. Three of the four feldspar samples studied in this paper are K-rich, and these exhibited different behavior at higher stimulation temperatures, than the fourth sample which was a Na-rich feldspar. The new method of analysis proposed in this paper can help isolate mathematically the more thermally stable components, and hence could lead to better dating applications in these materials. - Highlights: ► TR-IRSL from four feldspars were analyzed using exponential and stretched exponential functions. ► A variety of global optimization techniques give good agreement. ► Na-rich sample behavior is different from the three K-rich samples. ► Experimental data are fitted for stimulation temperatures

  13. Radioluminescence dating: the IR emission of feldspar

    International Nuclear Information System (INIS)

    Schilles, Thomas.; Habermann, Jan

    2000-01-01

    A new luminescence reader for radioluminescence (RL) measurements is presented. The system allows detection of RL emissions in the near infrared region (IR). Basic bleaching properties of the IR-RL emission of feldspars are investigated. Sunlight-bleaching experiments as a test for sensitivity changes are presented. IR-bleaching experiments were carried out to obtain information about the underlying physical processes of the IR-RL emission

  14. Methods of recovering alkali metals

    Science.gov (United States)

    Krumhansl, James L; Rigali, Mark J

    2014-03-04

    Approaches for alkali metal extraction, sequestration and recovery are described. For example, a method of recovering alkali metals includes providing a CST or CST-like (e.g., small pore zeolite) material. The alkali metal species is scavenged from the liquid mixture by the CST or CST-like material. The alkali metal species is extracted from the CST or CST-like material.

  15. Alkali-vapor laser-excimer pumped alkali laser

    International Nuclear Information System (INIS)

    Yue Desheng; Li Wenyu; Wang Hongyan; Yang Zining; Xu Xiaojun

    2012-01-01

    Based on the research internal and overseas, the principle of the excimer pumped alkali laser (XPAL) is explained, and the advantages and disadvantages of the XPAL are analyzed. Taking into consideration the difficulties that the diode pumped alkali laser (DPAL) meets on its development, the ability to solve or avoid these difficulties of XPAL is also analyzed. By summing up the achievements of the XPAL, the possible further prospect is proposed. The XPAL is of possibility to improve the performance of the DPAL. (authors)

  16. Deliberate and Accidental Gas-Phase Alkali Doping of Chalcogenide Semiconductors: Cu(In,Ga)Se2.

    Science.gov (United States)

    Colombara, Diego; Berner, Ulrich; Ciccioli, Andrea; Malaquias, João C; Bertram, Tobias; Crossay, Alexandre; Schöneich, Michael; Meadows, Helene J; Regesch, David; Delsante, Simona; Gigli, Guido; Valle, Nathalie; Guillot, Jérome; El Adib, Brahime; Grysan, Patrick; Dale, Phillip J

    2017-02-24

    Alkali metal doping is essential to achieve highly efficient energy conversion in Cu(In,Ga)Se 2 (CIGSe) solar cells. Doping is normally achieved through solid state reactions, but recent observations of gas-phase alkali transport in the kesterite sulfide (Cu 2 ZnSnS 4 ) system (re)open the way to a novel gas-phase doping strategy. However, the current understanding of gas-phase alkali transport is very limited. This work (i) shows that CIGSe device efficiency can be improved from 2% to 8% by gas-phase sodium incorporation alone, (ii) identifies the most likely routes for gas-phase alkali transport based on mass spectrometric studies, (iii) provides thermochemical computations to rationalize the observations and (iv) critically discusses the subject literature with the aim to better understand the chemical basis of the phenomenon. These results suggest that accidental alkali metal doping occurs all the time, that a controlled vapor pressure of alkali metal could be applied during growth to dope the semiconductor, and that it may have to be accounted for during the currently used solid state doping routes. It is concluded that alkali gas-phase transport occurs through a plurality of routes and cannot be attributed to one single source.

  17. Alkali metal ion battery with bimetallic electrode

    Science.gov (United States)

    Boysen, Dane A; Bradwell, David J; Jiang, Kai; Kim, Hojong; Ortiz, Luis A; Sadoway, Donald R; Tomaszowska, Alina A; Wei, Weifeng; Wang, Kangli

    2015-04-07

    Electrochemical cells having molten electrodes having an alkali metal provide receipt and delivery of power by transporting atoms of the alkali metal between electrode environments of disparate chemical potentials through an electrochemical pathway comprising a salt of the alkali metal. The chemical potential of the alkali metal is decreased when combined with one or more non-alkali metals, thus producing a voltage between an electrode comprising the molten the alkali metal and the electrode comprising the combined alkali/non-alkali metals.

  18. Potential energy surfaces for alkali plus noble gas pairs: a systematic comparison

    Science.gov (United States)

    Blank, L. Aaron; Kedziora, Gary S.; Weeks, David E.

    2010-02-01

    Optically Pumped Alkali Lasers (OPAL) involve interactions of alkali atoms with a buffer gas typically consisting of a noble gas together with C2H4. Line broadening mechanisms are of particular interest because they can be used to match a broad optical pumping source with relatively narrow alkali absorption spectra. To better understand the line broadening processes at work in OPAL systems we focus on the noble gas collisional partners. A matrix of potential energy surfaces (PES) has been generated at the multi-configurational self consistent field (MCSCF) level for M + Ng, where M=Li, Na, K, Rb, Cs and Ng=He, Ne, Ar. The PES include the X2Σ ground state surface and the A2II, B2Σ excited state surfaces. In addition to the MCSCF surfaces, PES for Li+He have been calculated at the multi-reference singles and doubles configuration interaction (MRSDCI) level with spin-orbit splitting effects included. These surfaces provide a way to check the qualitative applicability of the MCSCF calculations. They also exhibit the avoided crossing between the B2Σ and A2II1/2 surfaces that is partially responsible for collision induced relaxation from the 2P3/2 to the 2P1/2 atomic levels.

  19. Mathematical characterization of continuous wave infrared stimulated luminescence signals (CW-IRSL) from feldspars

    International Nuclear Information System (INIS)

    Pagonis, V.; Phan, Huy; Goodnow, Rebecca; Rosenfeld, Sara; Morthekai, P.

    2014-01-01

    Continuous-wave infrared stimulated luminescence signals (CW-IRSL) from feldspars have been the subject of many experimental studies, due to their importance in luminescence dating and dosimetry. Accurate mathematical characterization of the shape of these CW-IRSL signals in feldspars is of practical and theoretical importance, especially in connection with “anomalous fading” of luminescence signals in dating studies. These signals are known to decay in a non-exponential manner and their exact mathematical shape as a function of stimulation time is an open research question. At long stimulation times the IRSL decay has been shown experimentally to follow a power law of decay, and previous researchers have attempted to fit the overall shape of these signals empirically using the well known Becquerel function (or compressed hyperbola decay law). This paper investigates the possibility of fitting CW-IRSL curves using either the Becquerel decay law, or a recently developed analytical equation based on localized electronic recombination of donor–acceptor pairs in luminescent materials. It is shown that both mathematical approaches can give excellent fits to experimental CW-IRSL curves, and the precision of the fitting process is studied by analyzing a series of curves measured using a single aliquot of a feldspar sample. Both fitting equations are solutions of differential equations involving numerically similar time dependent recombination probabilities k(t). It is concluded that both fitting equations provide approximately equivalent mathematical descriptions of the CW-IRSL curves in feldspars, and can be used as mathematical representations of the shape of CW-IRSL signals. - Highlights: • Feldspar CW-IRSL curves fitted using Becquerel decay law and new analytical equation. • Both mathematical approaches give excellent fits to experimental CW-IRSL curves. • Series of experimental CW-IRSL curves analyzed using both fitting expressions. • The time

  20. On the effect of optical and isothermal treatments on luminescence signals from feldspars

    International Nuclear Information System (INIS)

    Pagonis, Vasilis; Polymeris, George; Kitis, George

    2015-01-01

    During luminescence dosimetry and luminescence dating applications it is often necessary to precondition the geological samples by applying a thermal or optical treatment before measuring the luminescence signal. In luminescence applications using apatites or feldspars, measurement of continuous-wave infrared or optically stimulated signals (CW-IRSL and CW-OSL) are customarily preceded by either an isothermal heating of the samples at a fixed temperature for a short time interval, or alternatively by optically bleaching the samples using light from LEDs with the appropriate wavelength. This paper presents new analytical equations which can be used to describe these commonly employed double experimental procedures. The equations are based on a recently published model which assumes that tunneling processes are taking place in random distributions of donor–acceptor pairs. The concentration of charge carriers during the CW-IRSL or CW-OSL experiment is expressed in terms of the parameters of the preceding thermal or optical bleaching procedure, and depends also on the distribution of distances between electron and hole pairs. The analytical equations in this paper are compared with experimental data from a feldspar sample which undergoes an isothermal procedure followed by measurement of the CW-IRSL signal. Additional comparisons with experiment are provided using a feldspar sample which undergoes an infrared bleaching process, followed by measurement of the CW-OSL signal. These results and conditions under which the equations can be used are discussed within the framework of the model. - Highlights: • CW-IRSL and CW-OSL measurements are preceded by heating or optical bleaching. • New analytical equations are derived to describe these double experimental procedures. • Equations are compared with data from a feldspar sample following isothermal procedure. • Equations are compared with data from a feldspar sample following optical bleaching.

  1. What classic greywacke (litharenite) can reveal about feldspar diagenesis: An example from Permian Rotliegend sandstone in Hessen, Germany

    Science.gov (United States)

    Molenaar, Nicolaas; Felder, Marita; Bär, Kristian; Götz, Annette E.

    2015-08-01

    Rotliegend siliciclastic sediments in southern Hessen (Germany) are a good example of dissolution of detrital feldspars, which is a common feature in many sandstones. Dissolution occurred after mechanical compaction of the lithic-rich sandstone, which experienced framework collapse with pores and pore connections filled and obstructed by deformed ductile lithic grains (pseudomatrix) thereby reducing pore space to microporosity., The advanced degree of compaction and reduced porosity caused low permeability and low hydraulic conductivity of the rock mass. This is further reduced by the presence of wackes and shales that occur intercalated with the sandstones. Feldspar dissolution thus took place in low permeable sediments when large-scale flow of meteoric or acidic fluids is ruled out as a cause of feldspar dissolution. Mineral precipitation (illite, kaolinite, and albite) took place within pseudomatrix and detrital matrix as well as in secondary pores created by feldspar dissolution. Feldspar was the source for the authigenesis. The system was thus closed during burial after framework collapse, and diagenetic reactants in the form of detrital components were already present within the system. The original mass was preserved, but redistributed and diagenetic minerals were the local sinks for the dissolved reactants, precipitating within the system. This also suggests that burial diagenesis in general might be more mass conservative than usually assumed. Rotliegend sandstones thus form a case where, despite of the lack of external exchange of mass by fluid flow, major diagenetic processes did take place and significantly modified the original mineralogy and texture. Feldspar diagenesis can take place from other processes than mere large-scale flushing of open systems as often supposed. It implies that the volumes of rock affected by feldspar diagenesis may be much larger than anticipated based upon the common hold believe that feldspar diagenesis is linked to

  2. Mechanical behavior of alumina and alumina-feldspar based ceramics in an acetic acid (4%) environment

    International Nuclear Information System (INIS)

    Stumpf, Aisha S.G.; Bergmann, Carlos P.; Vicenzi, Juliane; Fetter, Rebecca; Mundstock, Karina S.

    2009-01-01

    This study investigates the mechanical properties of alumina-feldspar based ceramics when exposed to an aggressive environment (acetic acid 4%). Alumina ceramics containing different concentrations of feldspar (0%, 1%, 5%, 10%, or 40%) were sintered at either 1300, 1600, or 1700 o C. Flaws (of width 0%, 30%, or 50%) were introduced into the specimens using a saw. Half of these ceramic bodies were exposed to acetic acid. Their flexural strength, K IC , and porosity were measured and the fractured samples were evaluated using scanning electronic- and optical microscopy. It was found that in the ceramic bodies sintered at 1600 o C, feldspar content up to 10% improved flexural strength and K IC, and reduced porosities. Generally, it was found that acetic acid had a weakening effect on the flexural strength of samples sintered at 1700 o C but a beneficial effect on K IC of ceramics sintered at 1600 o C. It was concluded that alumina-based ceramics with feldspar content up to 10% and sintered at higher temperatures would perform better in an aggressive environment similar to oral cavity.

  3. Feldspar 40Ar/39Ar dating of ICDP PALEOVAN cores

    Science.gov (United States)

    Engelhardt, Jonathan Franz; Sudo, Masafumi; Stockhecke, Mona; Oberhänsli, Roland

    2017-11-01

    Volcaniclastic fall deposits in ICDP drilling cores from Lake Van, Turkey, contain sodium-rich sanidine and calcium-rich anorthoclase, which both comprise a variety of textural zoning and inclusions. An age model records the lake's history and is based on climate-stratigraphic correlations, tephrostratigraphy, paleomagnetics, and earlier 40Ar/39Ar analyses (Stockhecke et al., 2014b). Results from total fusion and stepwise heating 40Ar/39Ar analyses presented in this study allow for the comparison of radiometric constraints from texturally diversified feldspar and the multi-proxy lacustrine age model and vice versa. This study has investigated several grain-size fractions of feldspar from 13 volcaniclastic units. The feldspars show textural features that are visible in cathodoluminescence (CL) or back-scattered electron (BSE) images and can be subdivided into three dominant zoning-types: (1) compositional zoning, (2) round pseudo-oscillatory zoning and (3) resorbed and patchy zoning (Ginibre et al., 2004). Round pseudo-oscillatory zoning records a sensitive alternation of Fe and Ca that also reflects resorption processes. This is only visible in CL images. Compositional zoning reflects anticorrelated anorthite and orthoclase contents and is visible in BSE. Eleven inverse isochron ages from total fusion and three from stepwise heating analyses fit the age model. Four experiments resulted in older inverse isochron ages that do not concur with the model within 2σ uncertainties and that deviate from 1 ka to 17 ka minimum. C- and R-type zoning are interpreted as representing growth in magma chamber cupolas, as wall mushes, or in narrow conduits. Persistent compositions of PO-type crystals and abundant surfaces recording dissolution features correspond to formation within a magma chamber. C-type zoning and R-type zoning have revealed an irregular incorporation of melt and fluid inclusions. These two types of zoning in feldspar are interpreted as preferentially

  4. Time-resolved luminescence from feldspars: New insight into fading

    DEFF Research Database (Denmark)

    Tsukamoto, S.; Denby, P.M.; Murray, A.S.

    2006-01-01

    Time-resolved infrared optically stimulated luminescence (IR-OSL) signals of K- and Na-feldspar samples extracted from sediments were measured in UV, blue and red detection windows, using a fast photon counter and pulsed IR stimulation (lambda = 875 nm). We observe that the relative contribution ...

  5. Alkali resistant optical coatings for alkali lasers and methods of production thereof

    Science.gov (United States)

    Soules, Thomas F; Beach, Raymond J; Mitchell, Scott C

    2014-11-18

    In one embodiment, a multilayer dielectric coating for use in an alkali laser includes two or more alternating layers of high and low refractive index materials, wherein an innermost layer includes a thicker, >500 nm, and dense, >97% of theoretical, layer of at least one of: alumina, zirconia, and hafnia for protecting subsequent layers of the two or more alternating layers of high and low index dielectric materials from alkali attack. In another embodiment, a method for forming an alkali resistant coating includes forming a first oxide material above a substrate and forming a second oxide material above the first oxide material to form a multilayer dielectric coating, wherein the second oxide material is on a side of the multilayer dielectric coating for contacting an alkali.

  6. Alkali metal and alkali metal hydroxide intercalates of the layered transition metal disulfides

    International Nuclear Information System (INIS)

    Kanzaki, Y.; Konuma, M.; Matsumoto, O.

    1981-01-01

    The intercalation reaction of some layered transition metal disulfides with alkali metals, alkali metal hydroxides, and tetraalkylammonium hydroxides were investigated. The alkali metal intercalates were prepared in the respective metal-hexamethylphosphoric triamide solutions in vaccuo, and the hydroxide intercalates in aqueous hydroxide solutions. According to the intercalation reaction, the c-lattice parameter was increased, and the increase indicated the expansion of the interlayer distance. In the case of alkali metal intercalates, the expansion of the interlayer distance increased continuously, corresponding to the atomic radius of the alkali metal. On the other hand, the hydroxide intercalates showed discrete expansion corresponding to the effective ionic radius of the intercalated cation. All intercalates of TaS 2 amd NbS 2 were superconductors. The expansion of the interlayer distance tended to increase the superconducting transition temperature in the intercalates of TaS 2 and vice versa in those of NbS 2 . (orig.)

  7. Strontium and argon isotopes in naturally weathered biotites, muscovites and feldspars

    International Nuclear Information System (INIS)

    Clauer, N.

    1981-01-01

    A Rb-Sr and K-Ar isotopical study on progressively weathered biotites, muscovites and feldspars from plutonic and eruptive rocks shows that their continental weathering is a complex phenomenon controlled by environmental conditions. During weathering of biotites, the K-Ar couple often mimics the Rb-Sr couple. The radiogenic Sr and Ar isotopes are systematically leached out, but the behaviour of the elemental Rb, K, Sr and Ar depends upon the environment. In contrast, the Sr and Ar balances of muscovites are maintained, even during very intensive weathering. In mixtures of feldspars, the common Sr seems to be leached out preferentially to the radiogenic isotope, while the K-Ar balance is maintained. (Auth.)

  8. ALKALI FUSION OF ROSETTA ZIRCON

    International Nuclear Information System (INIS)

    DAHER, A.

    2008-01-01

    The decomposition of Rosetta zircon by fusion with different types of alkalis has been investigated. These alkalis include sodium hydroxide, potassium hydroxide and eutectic mixture of both. The influences of the reaction temperature, zircon to alkalis ratio, fusion time and the stirring of the reactant on the fusion reaction have been evaluated. The obtained results favour the decomposition of zircon with the eutectic alkalis mixture by a decomposition efficiency of 96% obtained at 500 0 C after one hour

  9. A comparative study of semi-empirical interionic potentials for alkali halides - II

    International Nuclear Information System (INIS)

    Khwaja, F.A.; Naqvi, S.H.

    1985-08-01

    A comprehensive study of some semi-empirical interionic potentials is carried out through the calculation of the cohesive energy, relative stability and pressure induced solid-solid phase transformations in alkali halides. The theoretical values of these properties of the alkali halides are obtained using a new set of van der Waals coefficients and zero-point energy in the expression for interionic potential. From the comparison of the present calculations with some previous sophisticated ab-initio quantum-mechanical calculations and other semi-empirical approaches, it is concluded that the present calculations in the simplest central pairwise interaction description with the new values of the van der Waals coefficients and zero-point energy are in better agreement with the experimental data than the previous calculations. It is also concluded that in some cases the better choice of the interionic potential alone in the simplest semi-empirical picture of interaction gives an agreement of the theoretical predictions with the experimental data much superior to the ab-initio quantum mechanical approaches. (author)

  10. Electron detachment energies in high-symmetry alkali halide solvated-electron anions

    Science.gov (United States)

    Anusiewicz, Iwona; Berdys, Joanna; Simons, Jack; Skurski, Piotr

    2003-07-01

    We decompose the vertical electron detachment energies (VDEs) in solvated-electron clusters of alkali halides in terms of (i) an electrostatic contribution that correlates with the dipole moment (μ) of the individual alkali halide molecule and (ii) a relaxation component that is related to the polarizability (α) of the alkali halide molecule. Detailed numerical ab initio results for twelve species (MX)n- (M=Li,Na; X=F,Cl,Br; n=2,3) are used to construct an interpolation model that relates the clusters' VDEs to their μ and α values as well as a cluster size parameter r that we show is closely related to the alkali cation's ionic radius. The interpolation formula is then tested by applying it to predict the VDEs of four systems [i.e., (KF)2-, (KF)3-, (KCl)2-, and (KCl)3-] that were not used in determining the parameters of the model. The average difference between the model's predicted VDEs and the ab initio calculated electron binding energies is less than 4% (for the twelve species studied). It is concluded that one can easily estimate the VDE of a given high-symmetry solvated electron system by employing the model put forth here if the α, μ and cation ionic radii are known. Alternatively, if VDEs are measured for an alkali halide cluster and the α and μ values are known, one can estimate the r parameter, which, in turn, determines the "size" of the cluster anion.

  11. Alkali metal for ultraviolet band-pass filter

    Science.gov (United States)

    Mardesich, Nick (Inventor); Fraschetti, George A. (Inventor); Mccann, Timothy A. (Inventor); Mayall, Sherwood D. (Inventor); Dunn, Donald E. (Inventor); Trauger, John T. (Inventor)

    1993-01-01

    An alkali metal filter having a layer of metallic bismuth deposited onto the alkali metal is provided. The metallic bismuth acts to stabilize the surface of the alkali metal to prevent substantial surface migration from occurring on the alkali metal, which may degrade optical characteristics of the filter. To this end, a layer of metallic bismuth is deposited by vapor deposition over the alkali metal to a depth of approximately 5 to 10 A. A complete alkali metal filter is described along with a method for fabricating the alkali metal filter.

  12. Sorption of Eu(III) at feldspar/water interface. Effects of pH, organic matter, counter ions, and temperature

    Energy Technology Data Exchange (ETDEWEB)

    Li, Ping; Liang, Jianjun; Fan, Qiaohui [Chinese Academy of Sciences, Lanzhou (China). Key Lab. of Petroleum Resources Research; Wu, Hanyu [Chinese Academy of Sciences, Lanzhou (China). Key Lab. of Petroleum Resources Research; Lanzhou Univ. (China). Radiochemistry Lab.; Yin, Zhuoxin; Pan, Duoqiang; Wu, Wangsuo [Lanzhou Univ. (China). Radiochemistry Lab.; Xu, Di [Chinese Academy of Sciences, Nanjing (China). State Key Lab. of Lake Science and Environment

    2017-07-01

    The sorption of Eu(III) on potassium feldspar (K-feldspar) was studied under various physicochemical conditions such as pH, temperature, counter ions and organic matter. The results showed that the sorption of Eu(III) on K-feldspar significantly increased with the increase of pH, and high Eu(III) concentration can inhibit such immobility to some extent. The presence of humic acid (HA) can increase the sorption of Eu(III) on K-feldspar in low pH range; while inhibit to a large extent under alkaline conditions. It is very interesting that at pH ∝6.5, high ionic strength can promote the sorption of Eu(III) on K-feldspar in the presence of HA. In contrast, Eu(III) sorption was restricted obviously by NaCl in the absence of HA. The sorption procedure was involved with ion exchange and/or outer-sphere complexation as well as inner-sphere complexation. The presence of F{sup -} and PO{sub 4}{sup 3-} dramatically enhanced Eu(III) sorption on K-feldspar, whereas both SO{sub 4}{sup 2-} and CO{sub 3}{sup 2-} had negative effects on Eu(III) sorption. X-ray photoelectron spectroscopy analysis indicated that Eu(III) tended to form hydrolysates at high initial concentration (3 x 10{sup -4} mol/L) and high temperature (338 K).

  13. A comparative study of the luminescence characteristics of polymineral fine grains and coarse-grained K-, and Na-rich feldspars

    DEFF Research Database (Denmark)

    Tsukamoto, Sumiko; Jain, Mayank; Murray, Andrew S.

    2012-01-01

    for K-feldspar samples, when a preheat temperature of 250 °C for 60 s is used. After preheating to a higher temperature (320 °C for 60 s) all samples show a TL reduction around 410 °C in the blue detection window. Pulse annealing experiments for IRSL and pIRIR signals for preheats between 320 °C and 500...... °C indicate that the signal stabilities are similar among the different feldspar types, when a higher preheat temperature (>320 °C) is used. Thermal activation energies for IRSL and pIRIR signals are largest in K-feldspar and smallest in polymineral fine grains, in both blue and UV detection windows...... for both fast time-resolved (TR) and continuous wave (CW) signals. These results suggest that IRSL and pIRIR signals in polymineral fine grains originate mainly from Na-feldspar grains; these signals are less thermally stable than those from K-feldspar, but a more stable signal (presumably from K...

  14. Peculiar Feldspar And Quartz Inclusions Within Zircons From Anorthosites, North Eastern Desert, Egypt

    Science.gov (United States)

    Eliwa, H. A.; Dawoud, M. I.; Khalaf, I. M.; Negendank, J. F.; Itaya, T.

    2004-12-01

    Zircons from three anorthosite outcrops along Wadi Dib area, north Eastern Desert of Egypt contain abundant and conspicuous inclusions of quartz, feldspar, amphibole and apatite. These anorthosites, as (50-100m thick) layers, represent the top of mafic-ultramafic intrusions exhibiting rhythmic layering visible by reputation of melanocratic and leucocratic layers. Field and microscopic studies exhibit that these anorthosites were affected by the action of residual magmatic solutions associated with the late stage crystallization of the younger granites, which modified their mineralogical composition. They are composed totally of plagioclase with subordinate amount of clinoenstatite, augite, amphibole, biotite, K-feldspar, and quartz. Accessories are magnetite, ilmenite, apatite and zircon. The abundance and the mode of occurrence of K-feldspar, quartz, and biotite with apatite and zircon among the megacrysts suggest their formation is ascribed to the interaction with the residual solutions. The microprobe data exhibit difference between feldspar and amphiboles contained herein zircons and those as anorthosite mineral constituents. The genetic relationship between zircons and their inclusions suggests later growth of zircons than inclusions and most probably at the final stage of rock modification. Zircons are magmatic and found in the interstitial feldspar and quartz among plagioclase megacrysts in aggregates or as individual grains. The microscopic and SEM images investigation exhibit that most zircons are subhedral to euhedral equant and prismatic crystals. Most zircons have same range of crystal morphologies and internal growth structures with predominance of prism /{100/} and pyramid /{101/} and occasionally prism /{110/} and pyramid /{111/}. No evidences for poly-faceted grains, inherited cores or later overgrowths were detected. CL images distinguished zircons with visible core-rim structures and others with regular and continuous growth zones contained herein

  15. Alkali metal hydride formation

    International Nuclear Information System (INIS)

    1976-01-01

    The present invention relates to a method of producing alkali metal hydrides by absorbing hydrogen gas under pressure into a mixture of lower alkyl mono amines and alkali metal alkyl amides selected from sodium and potassium amides formed from said amines. The present invention also includes purification of a mixture of the amines and amides which contain impurities, such as is used as a catalytic exchange liquid in the enrichment of deuterium, involving the formation of the alkali metal hydride

  16. Process for the disposal of alkali metals

    International Nuclear Information System (INIS)

    Lewis, L.C.

    1979-01-01

    The invention describes a method of disposing of alkali metals by forming a solid waste for storage. The method comprises preparing an aqueous disposal solution of at least 55 weight percent alkali metal hydroxide, heating the alkali metal to melting temperature to form a feed solution, and spraying the molten feed solution into the disposal solution. The alkali metal reacts with the water in the disposal solution in a controlled reaction which produces alkali metal hydroxide, hydrogen and heat and thereby forms a solution of alkali metal hydroxides. Water is added to the solution in amounts sufficient to maintain the concentration of alkali metal hydroxides in the solution at 70 to 90 weight percent, and to maintain the temperature of the solution at about the boiling point. Removing and cooling the alkali metal hydroxide solution thereby forms a solid waste for storage. The method is particularly applicable to radioactive alkali metal reactor coolant. (auth)

  17. On-line alkali monitoring - Part 1

    International Nuclear Information System (INIS)

    Andersson, Christer; Ljung, P.; Woxlin, H.

    1997-02-01

    As a consequence of the increased knowledge of the environmental impact of combustion based heat and power generation, the use of renewable biofuels will be increased. An obstacle associated to biofuel combustion compared to other fuels is the large release of alkali. Alkali compounds in flue gases are known to cause severe operational problems. Three of the major problems are; fouling of superheating tubes (causing reduced heat transfer and possibly corrosion), agglomeration of the bed material in fluidized beds, and poisoning of SCR catalysts. Yet another alkali related problem arises when, in order to increase the electric efficiency of combustion power plants, combined-cycle technology is used. Alkali vapour present in the fuel gas for the gas turbine is condensed to particles which increase corrosion and erosion of the turbine blades. The research on ash related operational problems has to be extended in order to ensure future use of biofuels in heat and power generation. In all successful research, adequate tools are necessary. To investigate ash related problems the key issue is to be able to perform continuous alkali measurements. This pilot study has investigated the need of continuous alkali measurements, which alkali species are harmful in the different applications and also available instrumentation capable of measuring the specific alkali species. The report gives a short summary presenting alkali related operational problems. In addition a schematic overview is given, showing the alkali species that possibly can exist in various parts of the power plant. 48 refs, 13 figs, 4 tabs

  18. Correlation of basic TL, OSL and IRSL properties of ten K-feldspar samples of various origins

    Energy Technology Data Exchange (ETDEWEB)

    Sfampa, I.K. [Aristotle University of Thessaloniki, Nuclear Physics Laboratory, 54124 Thessaloniki (Greece); Polymeris, G.S. [Institute of Nuclear Sciences, Ankara University, 06100 Besevler, Ankara (Turkey); Pagonis, V. [McDaniel College, Physics Department, Westminster, MD 21157 (United States); Theodosoglou, E. [Department of Mineralogy-Petrology-Economic Geology, School of Geology, Aristotle University of Thessaloniki, 54124 Thessaloniki (Greece); Tsirliganis, N.C. [Laboratory of Radiation Applications and Archaeological Dating, Department of Archaeometry and Physicochemical Measurements, ‘Athena’ R.& I.C., Kimmeria University Campus, GR67100 Xanthi (Greece); Kitis, G., E-mail: gkitis@auth.gr [Aristotle University of Thessaloniki, Nuclear Physics Laboratory, 54124 Thessaloniki (Greece)

    2015-09-15

    Highlights: • OSL and IRSL bleaching behavior of ten K-feldspar samples is presented. • OSL and IRSL decay curves were component resolved using tunneling model. • The growth of integrated OSL and IRSL signals versus time was described by new expression based on tunneling model. • Correlation between TL, OSL and IRSL signals and of all properties with K-feldspar structure was discussed. - Abstract: Feldspars stand among the most widely used minerals in dosimetric methods of dating using thermoluminescence (TL), optically stimulated luminescence (OSL) and infrared stimulated luminescence (IRSL). Having very good dosimetric properties, they can in principle contribute to the dating of every site of archaeological and geological interest. The present work studies basic properties of ten naturally occurring K-feldspar samples belonging to three feldspar species, namely sanidine, orthoclase and microcline. The basic properties studied are (a) the influence of blue light and infrared stimulation on the thermoluminescence glow-curves, (b) the growth of OSL, IRSL, residual TL and TL-loss as a function of OSL and IRSL bleaching time and (c) the correlation between the OSL and IRSL signals and the energy levels responsible for the TL glow-curve. All experimental data were fitted using analytical expressions derived from a recently developed tunneling recombination model. The results show that the analytical expressions provide excellent fits to all experimental results, thus verifying the tunneling recombination mechanism in these materials and providing valuable information about the concentrations of luminescence centers.

  19. Quantitative analysis of time-resolved infrared stimulated luminescence in feldspars

    Energy Technology Data Exchange (ETDEWEB)

    Pagonis, Vasilis, E-mail: vpagonis@mcdaniel.edu [McDaniel College, Physics Department, Westminster, MD 21157 (United States); Ankjærgaard, Christina [Soil Geography and Landscape Group & Netherlands Centre for Luminescence dating, Wageningen University, PO Box 47, 6700 AA Wageningen (Netherlands); Jain, Mayank [Center for Nuclear Technologies, Technical University of Denmark, DTU Risø Campus, Roskilde (Denmark); Chithambo, Makaiko L. [Department of Physics and Electronics, Rhodes University, PO BOX 94, Grahamstown 6140 (South Africa)

    2016-09-15

    Time-resolved infrared-stimulated luminescence (TR-IRSL) from feldspar samples is of importance in the field of luminescence dating, since it provides information on the luminescence mechanism in these materials. In this paper we present new analytical equations which can be used to analyze TR-IRSL signals, both during and after short infrared stimulation pulses. The equations are developed using a recently proposed kinetic model, which describes localized electronic recombination via tunneling between trapped electrons and recombination centers in luminescent materials. Recombination is assumed to take place from the excited state of the trapped electron to the nearest-neighbor center within a random distribution of luminescence recombination centers. Different possibilities are examined within the model, depending on the relative importance of electron de-excitation and recombination. The equations are applied to experimental TR-IRSL data of natural feldspars, and good agreement is found between experimental and modeling results.

  20. Effect of alkali lignins with different molecular weights from alkali pretreated rice straw hydrolyzate on enzymatic hydrolysis.

    Science.gov (United States)

    Li, Yun; Qi, Benkun; Luo, Jianquan; Wan, Yinhua

    2016-01-01

    This study investigated the effect of alkali lignins with different molecular weights on enzymatic hydrolysis of lignocellulose. Different alkali lignins fractions, which were obtained from cascade ultrafiltration, were added into the dilute acid pretreated (DAP) and alkali pretreated (AP) rice straws respectively during enzymatic hydrolysis. The results showed that the addition of alkali lignins enhanced the hydrolysis and the enhancement for hydrolysis increased with increasing molecular weights of alkali lignins, with maximum enhancement being 28.69% for DAP and 20.05% for AP, respectively. The enhancement was partly attributed to the improved cellulase activity, and filter paper activity increased by 18.03% when adding lignin with highest molecular weight. It was found that the enhancement of enzymatic hydrolysis was correlated with the adsorption affinity of cellulase on alkali lignins, and the difference in surface charge and hydrophobicity of alkali lignins were responsible for the difference in affinity between cellulase and lignins. Copyright © 2015 Elsevier Ltd. All rights reserved.

  1. Determination of potassium in feldspars by beta counting using a GM multicounter system

    Energy Technology Data Exchange (ETDEWEB)

    Boetter-Jensen, L; Mejdahl, V

    1985-01-01

    A gas flow multicounter system developed at Risoe National laboratory for low-level beta counting applications was adopted for measuring potassium in feldspars extracted from archaeological and geological materials, in connection with TL dating work. A guard counter reduces the background by using an anticoincidence technique. Calibration was accomplished by measuring KCl and a feldspar standard. A potassium content of 1% yields a net beta count rate (background subtracted) of about 40 c.p.h.; the background is around 15 c.p.h. The precision in repeated measurements is better than 2% and the estimated accuracy is about 3%.

  2. Identifying well-bleached quartz using the different bleaching rates of quartz and feldspar luminescence signals

    DEFF Research Database (Denmark)

    Murray, A.S.; Thomsen, Kristina Jørkov; Masuda, N.

    2012-01-01

    When dating older sedimentary deposits using quartz, there are no unambiguous methods for identifying the presence of incomplete bleaching. Current statistical analysis of dose distributions depends entirely on the assumption that incomplete bleaching and mixing are the main causes of any excess...... dispersion in the distribution; the only existing way to test this assumption is using independent age control. Here we suggest a new approach to this question, based on the differential bleaching rates of quartz and feldspar luminescence signals. We first present data that confirm the differences...... in relative bleaching rates of quartz optically stimulated luminescence (OSL) and feldspar luminescence stimulated at 50 °C by infrared light (IR50) and feldspar luminescence stimulated at 290 °C by infrared light after a stimulation at 50 °C (pIRIR290), and use recently deposited samples to determine...

  3. Deformation of quartz and feldspar at mid-crustal depths in an extensional normal fault (Viveiro Fault, NW Spain)

    Science.gov (United States)

    López-Sánchez, M. A.; Llana-Fúnez, S.; Marcos, A.; Martínez, F. J.

    2012-04-01

    Metamorphic reactions, deformation mechanism and chemical changes during mylonitization and ultramylonitization of granite affected by a crustal-scale shear zone are investigated using microstructural observations and quantitative analysis. The Vivero Fault (VF) is a large extensional shear zone (>140Km) in NW of Iberia that follows the main Variscan trend dipping 60° toward the West. The movement accumulated during its tectonic history affects the major lithostratigraphic sequence of Palaeozoic and Neoproterozoic rocks and the metamorphic facies developed during Variscan orogenesis. Staurolite, and locally, andalucite plus biotite grew in the hangingwall during the development of VF, overprinted the previous regional Variscan greenschist facies metamorphism. Andalusite growth took place during the intrusion of syntectonic granitic bodies, such as the deformed granite studied here. The Penedo Gordo granite is coarse-grained two-mica biotite-rich granite intruding the VF and its hangingwall. This granite developed a localized deformation consisting of a set of narrow zones (mm to metric scales) heterogeneously distributed subsequently to its intrusion. Based on pseudosections for representative hangingwall pelites hosting the granite and the inferred metamorphic evolution, the shear zone that outcrops at present-day erosion surface was previously active at 14,7-17 km depth (390-450 MPa). Temperature estimates during deformation reach at least the range 500-600° C, implying a local gradient of 35±6°C/km. Microstructures in the mylonites are characterized by bulging (BLG) to subgrain rotation (SGR) recristallization in quartz with the increasing of deformation. Albitisation, flame-perthite and tartan twining are common in K-feldspar at the early stage of deformation. The inferred dominant deformation mechanisms are: i) intracrystalline plasticity in quartz, ii) cataclasis with syntectonic crystallisation of very fine albite-oligoclase and micas in K-feldspar, and

  4. On-chip fabrication of alkali-metal vapor cells utilizing an alkali-metal source tablet

    International Nuclear Information System (INIS)

    Tsujimoto, K; Hirai, Y; Sugano, K; Tsuchiya, T; Tabata, O; Ban, K; Mizutani, N

    2013-01-01

    We describe a novel on-chip microfabrication technique for the alkali-metal vapor cell of an optically pumped atomic magnetometer (OPAM), utilizing an alkali-metal source tablet (AMST). The newly proposed AMST is a millimeter-sized piece of porous alumina whose considerable surface area holds deposited alkali-metal chloride (KCl) and barium azide (BaN 6 ), source materials that effectively produce alkali-metal vapor at less than 400 °C. Our experiments indicated that the most effective pore size of the AMST is between 60 and 170 µm. The thickness of an insulating glass spacer holding the AMST was designed to confine generated alkali metal to the interior of the vapor cell during its production, and an integrated silicon heater was designed to seal the device using a glass frit, melted at an optimum temperature range of 460–490 °C that was determined by finite element method thermal simulation. The proposed design and AMST were used to successfully fabricate a K cell that was then operated as an OPAM with a measured sensitivity of 50 pT. These results demonstrate that the proposed concept for on-chip microfabrication of alkali-metal vapor cells may lead to effective replacement of conventional glassworking approaches. (paper)

  5. Porous alkali activated materials with slow alkali release dynamic. Role of composition

    International Nuclear Information System (INIS)

    Bumanis, G.; Bajare, D.

    2018-01-01

    Alkali activated materials (AAM) based on calcined metakaolin or illite clay together with waste by-products, such as waste glass or aluminium scrap recycling waste, were tested as value-added materials for pH stabilization in biogas technology where decrease of pH should be avoided. Porous materials with ability to slowly leach alkalis in the water media thus providing continuous control of the pH level were obtained. XRD, FTIR, SEM and titration methods were used to characterize AAM and their leaching properties. It is clear that composition of the material has an important effect on the diffusion of alkali from structure. Namely, higher Si/Al and Na/Al molar ratios may increase pore solution transfer to the leachate. The leaching rate of alkalis from the structure of AAM is high for the first few days, decreasing over time. It was possible to calculate the buffer capacity from the mixture design of AAM. [es

  6. Ligand design for alkali-metal-templated self-assembly of unique high-nuclearity CuII aggregates with diverse coordination cage units: crystal structures and properties.

    Science.gov (United States)

    Du, Miao; Bu, Xian-He; Guo, Ya-Mei; Ribas, Joan

    2004-03-19

    The construction of two unique, high-nuclearity Cu(II) supramolecular aggregates with tetrahedral or octahedral cage units, [(mu(3)-Cl)[Li subset Cu(4)(mu-L(1))(3)](3)](ClO(4))(8)(H(2)O)(4.5) (1) and [[Na(2) subset Cu(12)(mu-L(2))(8)(mu-Cl)(4)](ClO(4))(8)(H(2)O)(10)(H(3)O(+))(2)](infinity) (2) by alkali-metal-templated (Li(+) or Na(+)) self-assembly, was achieved by the use of two newly designed carboxylic-functionalized diazamesocyclic ligands, N,N'-bis(3-propionyloxy)-1,4-diazacycloheptane (H(2)L(1)) or 1,5-diazacyclooctane-N,N'-diacetate acid (H(2)L(2)). Complex 1 crystallizes in the trigonal R3c space group (a = b = 20.866(3), c = 126.26(4) A and Z = 12), and 2 in the triclinic P1 space group (a = 13.632(4), b = 14.754(4), c = 19.517(6) A, alpha = 99.836(6), beta = 95.793(5), gamma = 116.124(5) degrees and Z = 1). By subtle variation of the ligand structures and the alkali-metal templates, different polymeric motifs were obtained: a dodecanuclear architecture 1 consisting of three Cu(4) tetrahedral cage units with a Li(+) template, and a supramolecular chain 2 consisting of two crystallographically nonequivalent octahedral Cu(6) polyhedra with a Na(+) template. The effects of ligand functionality and alkali metal template ions on the self-assembly processes of both coordination supramolecular aggregates, and their magnetic behaviors are discussed in detail.

  7. Purification of alkali metal nitrates

    Science.gov (United States)

    Fiorucci, Louis C.; Gregory, Kevin M.

    1985-05-14

    A process is disclosed for removing heavy metal contaminants from impure alkali metal nitrates containing them. The process comprises mixing the impure nitrates with sufficient water to form a concentrated aqueous solution of the impure nitrates, adjusting the pH of the resulting solution to within the range of between about 2 and about 7, adding sufficient reducing agent to react with heavy metal contaminants within said solution, adjusting the pH of the solution containing reducing agent to effect precipitation of heavy metal impurities and separating the solid impurities from the resulting purified aqueous solution of alkali metal nitrates. The resulting purified solution of alkali metal nitrates may be heated to evaporate water therefrom to produce purified molten alkali metal nitrate suitable for use as a heat transfer medium. If desired, the purified molten form may be granulated and cooled to form discrete solid particles of alkali metal nitrates.

  8. Beneficiation of feldspar ore for application in the ceramic industry: Influence of composition on the physical characteristics

    Directory of Open Access Journals (Sweden)

    M.E. Gaied

    2015-03-01

    Experimental studies indicate that an acceptable concentrate for industrial application can be obtained from these rocks. The feldspar yield was used to evaluate the process efficiency. Besides, the cone shrinkage, water absorption, degree of vitrification, mechanical properties (flexural strength and dielectric behaviour were used to monitor the quality of the recovered feldspars.

  9. Thermal quenching of luminescence processes in feldspars

    DEFF Research Database (Denmark)

    Poolton, N.R.J.; Bøtter-Jensen, L.; Duller, G.A.T.

    1995-01-01

    , which display very different behaviour. The first involves the internal transitions of common transition metal ions. The second is typical of centres not displaying excited states within the band gap that are likely to arise from direct recombination between the conduction band and the ground state......The technique of optically stimulated luminescence has important uses in the dose evaluation of irradiated feldspars. The luminescence process involves the eviction of electrons from donor traps, charge transfer through the conduction band, and recombination at acceptor sites; each...

  10. Quantitative analysis of time-resolved infrared stimulated luminescence in feldspars

    DEFF Research Database (Denmark)

    Pagonis, Vasilis; Ankjærgaard, Christina; Jain, Mayank

    2016-01-01

    Time-resolved infrared-stimulated luminescence (TR-IRSL) from feldspar samples is of importance in the field of luminescence dating, since it provides information on the luminescence mechanism in these materials. In this paper we present new analytical equations which can be used to analyze TR-IR...

  11. Detrital K-feldspar thermochronology of the Nanaimo Group: Characterization of Basement and Extraregional Basin Contributions

    Science.gov (United States)

    Isava, V.; Grove, M.; Mahoney, J. B.; Kimbrough, D. L.

    2016-12-01

    The Late Cretaceous-Early Paleogene Nanaimo Group covers the contact between Triassic basement Wrangellia terrane and the Jurassic-Cretaceous Coast Plutonic Complex (CPC) in southern British Columbia. Prior detrital zircon U-Pb and Hf studies indicate a change in sediment source for the Nanaimo basin, from the primitive CPC in Santonian-Early Campanian time to an isotopically evolved continental extraregional source during the late Campanian/Maastrictian. Two notably different areas have been proposed as potential source regions: (1) the Idaho/Boulder batholith and Belt Supergroup, and (2) the Mojave/Salinia segment of structurally disrupted late Cretaceous southern California margin. Single crystal 40Ar/39Ar laser fusion of ca. 100-200 grains apiece from seven detrital K-feldspar samples from Santonian-Maastrichtian strata of the northern Nanaimo Group constrain the history of the sediments' source regions. The two oldest samples, from the K-feldspar poor Comox and Extension Fms., display a monotonic increasing distribution of cooling ages 80-125 Ma that reflects shallow erosion of the CPC. In contrast, Late Campanian strata of the Cedar District and De Courcy Fms. exhibit a more pronounced cluster of cooling ages 80-95 Ma as well as a greater proportion of Jurassic ages that represent progressively deeper erosion of the CPC. Evidence for an extraregional sediment source appears abruptly in the Geoffrey Fm. by 72 Ma, matching the time of local-to-extraregional shift indicated in detrital zircon U-Pb studies. Over 90% of the detrital K-feldspars from these arkosic sandstones yield cooling ages of 70-80 Ma, with sparse older ages associated with the CPC. Samples from the successively younger Spray and Gabriola Fms. also yield >90% K-feldspar ages younger than 80 Ma and exhibit age maxima of 68 Ma and 65 Ma, respectively. These results are distinct from detrital zircon U-Pb and K-feldspar 40Ar/39Ar ages of the southern Sierra Nevada, Mojave/Salina, and northern

  12. Electrons in feldspar I: On the wavefunction of electrons trapped at simple lattice defects

    DEFF Research Database (Denmark)

    Poolton, H.R.J.; Wallinga, J.; Murray, A.S.

    2002-01-01

    The purpose of this article is to make an initial consideration of the physical properties of electrons trapped at classic hydrogenic lattice defects in feldspar. We are particularly interested to determine the radial extent of the electron wavefunctions in the ground and excited states. It is sh......The purpose of this article is to make an initial consideration of the physical properties of electrons trapped at classic hydrogenic lattice defects in feldspar. We are particularly interested to determine the radial extent of the electron wavefunctions in the ground and excited states...

  13. Alkali metal hafnium oxide scintillators

    Science.gov (United States)

    Bourret-Courchesne, Edith; Derenzo, Stephen E.; Taylor, Scott Edward

    2018-05-08

    The present invention provides for a composition comprising an inorganic scintillator comprising an alkali metal hafnate, optionally cerium-doped, having the formula A2HfO3:Ce; wherein A is an alkali metal having a valence of 1, such as Li or Na; and the molar percent of cerium is 0% to 100%. The alkali metal hafnate are scintillators and produce a bright luminescence upon irradiation by a suitable radiation.

  14. Surface studies of feldspar dissolution using surface replication combined with electron microscopic and spectroscopic techniques

    Energy Technology Data Exchange (ETDEWEB)

    Fung, P C [Petro-Canada, Calgary, Alberta; Sanipelli, G G

    1982-04-01

    The replica of a microcline cleavage surface was examined before and at various stages of interaction with water and acid solutions at 70/sup 0/C, as part of basic geochemical research for the Canadian Nuclear Fuel Waste Management Program to investigate the feasibility of disposal of these wastes in repositories mined in crystalline rocks. The objective of the report presented was to investigate the mechanism for Al and Si removal during incongruent dissolution of feldspars and its effect on dissolution rate. It was found that phase transformation, like dissolution occured preferentially along crystal defects on the surfaces of the feldspars. Secondary minerals always occured as discrete particles occupying only a very small fraction of the total parent surface, and hence, their presence would not affect the bulk composition or, in this regard, the overall dissolution rate of the feldspars by the formation of diffusion barriers.

  15. Luminescence at the end of the tunnelling - Investigating charge transfer mechanisms and luminescence dating methods for feldspar minerals

    NARCIS (Netherlands)

    Kars, R.H.

    2014-01-01

    This thesis comprises analyses of mineral physics with an application in geology and archeology. The thesis contributes to the development of feldspar luminescence dating methods in order to extend the applicable age range of feldspar luminescence dating in the Quaternary (last 2.6 Ma). The research

  16. Chemical effects of alkali atoms on critical temperature in superconducting alkali-doped fullerides

    Science.gov (United States)

    Hetfleisch, F.; Gunnarsson, O.; Srama, R.; Han, J. E.; Stepper, M.; Roeser, H.-P.; Bohr, A.; Lopez, J. S.; Mashmool, M.; Roth, S.

    2018-03-01

    Alkali metal doped fullerides (A3C60) are superconductors with critical temperatures, Tc, extending up to 38 K. Tc is known to depend strongly on the lattice parameter a, which can be adjusted by physical or chemical pressure. In the latter case an alkali atom is replaced by a different sized one, which changes a. We have collected an extensive data base of experimental data for Tc from very early up to recent measurements. We disentangle alkali atom chemical effects on Tc, beyond the well-known consequences of changing a. It is found that Tc, for a fixed a, is typically increased as smaller alkali atoms are replaced by larger ones, except for very large a. Possible reasons for these results are discussed. Although smaller in size than the lattice parameter contribution, the chemical effect is not negligible and should be considered in future physical model developments.

  17. Ultraviolet optical absorption of alkali cyanides and alkali halide cyanides

    International Nuclear Information System (INIS)

    Souza Camargo Junior, S.A. de.

    1982-09-01

    The ultraviolet absorption spectra of alkali cyanide and mixed alkali halide cyanide crystals were measured at temperatures ranging from 300K down to 4.2K. A set of small absorption peaks was observed at energies near 6 eV and assigned to parity forbidden X 1 Σ + →a' 3 Σ + transitions of the CN - molecular ions. It was observed that the peak position depends on the alkali atom while the absorption cross section strongly depends on the halogen and on the CN - concentration of the mixed crystals. These effects are explained in terms of an interaction between the triplet molecular excitons and charge transfer excitons. The experimental data were fit with a coupling energy of a few meV. The coupling mechanism is discussed and it is found to be due to the overlap between the wave functions of the two excitations. (Author) [pt

  18. Ultrafast electron dynamics at alkali/ice structures adsorbed on a metal surface

    International Nuclear Information System (INIS)

    Meyer, Michael

    2011-01-01

    mediated by tunneling through a potential barrier which is determined by the thickness of the ice layer. In the second system electron solvation at small alkali/water clusters directly prepared at the metal substrate is investigated. In these experiments the average number of water molecules in such a cluster can be controlled so that the population and stabilization dynamics of excess electrons can be investigated as a function of D 2 O coverage. Two main effects are observed: (i) the alkalis are solvated by a reorientation of the surrounding solvent molecules in the cluster; and (ii) above a critical number of water molecules per alkali excess electrons can localize at the clusters where they are energetically stabilized. This critical ratio depends on the type of alkali and is inversely proportional to the alkali-induced dipole moment. Finally, it is demonstrated that trapped electrons in crystalline ice adsorbed on Ru(001) can very efficiently mediate chemical reactions via dissociative electron attachment. When electronegative molecules like CFCl 3 are coadsorbed with crystalline ice a DEA process between trapped electrons and CFCl 3 molecules occurs, resulting in the formation of .CFCl 2 radicals and Cl - anions. These results suggest that photoexcited trapped electrons can play an important role in heterogeneous chemical processes on ice surfaces and could thus be relevant in the polar stratosphere chemistry.

  19. Pyrolysis characteristic of kenaf studied with separated tissues, alkali pulp, and alkali li

    Directory of Open Access Journals (Sweden)

    Yasuo Kojima

    2015-12-01

    Full Text Available To estimate the potential of kenaf as a new biomass source, analytical pyrolysis was performed using various kenaf tissues, i.e., alkali lignin and alkali pulp. The distribution of the pyrolysis products from the whole kenaf was similar to that obtained from hardwood, with syringol, 4-vinylsyringol, guaiacol, and 4-vinylguaiacol as the major products. The phenols content in the pyrolysate from the kenaf core was higher than that from the kenaf cuticle, reflecting the higher lignin content of the kenaf core. The ratios of the syringyl and guaiacyl compounds in the pyrolysates from the core and cuticle samples were 2.79 and 6.83, respectively. Levoglucosan was the major pyrolysis product obtained from the kenaf alkali pulp, although glycol aldehyde and acetol were also produced in high yields, as previously observed for other cellulosic materials. Moreover, the pathways for the formation of the major pyrolysis products from alkali lignin and alkali pulp were also described, and new pyrolysis pathways for carbohydrates have been proposed herein. The end groups of carbohydrates bearing hemiacetal groups were subjected to ring opening and then they underwent further reactions, including further thermal degradation or ring reclosing. Variation of the ring-closing position resulted in the production of different compounds, such as furans, furanones, and cyclopentenones.

  20. Magmatic evolution and controls on rare metal-enrichment of the Strange Lake A-type peralkaline granitic pluton, Québec-Labrador

    Science.gov (United States)

    Siegel, Karin; Vasyukova, Olga V.; Williams-Jones, Anthony E.

    2018-05-01

    Although it is well known that A-type granites are enriched in the rare earth elements (REE) and other high field strength elements (HFSE), the magmatic processes that concentrate these elements are still poorly understood. The 1.24 Ga Strange Lake pluton in northern Québec-Labrador provides an extraordinary example of hyper-enrichment in the REE, Zr, and Nb in a peralkaline A-type granite. The pluton consists of two hypersolvus granite units (southern and northern) and a transsolvus granite, all of which contain perthitic alkali feldspar as the earliest major mineral; the transsolvus granite also contains separate albite and microcline crystals. Arfvedsonite, a sodic amphibole, occurs exclusively as phenocrysts in the transsolvus granite, whereas in the hypersolvus granite it is present as a late, interstitial phase. The primary HFSE minerals are zircon, monazite-(Ce), gagarinite-(Ce) and the pyrochlore group minerals. Magma evolution was monitored by the alumina content in the bulk rock, which decreases from the southern to the northern hypersolvus granite and is lowest in the transsolvus granite. Alkalinity indices and bulk Si, Fe, Rb, REE, Zr, Nb concentrations show the opposite trend. Alkali feldspar compositions mirror the trend shown by the bulk rock, i.e., decreasing Al contents are accompanied by increasing Si, Fe3+, REE, Zr and Nb contents. The major driving forces for the evolution of the hypersolvus magma prior to emplacement were the early separation of a fluoride melt from the silicate melt and the crystallization of alkali feldspar and HFSE-rich phases (zircon, monazite-(Ce), pyrochlore group). An alkali feldspar-rich crystal-mush containing LREE-fluoride melt droplets was emplaced as the least evolved southern hypersolvus granite. Massive fractionation of alkali feldspar led to a sharp increase in ƒH2O and F- activity in the magma chamber that triggered the crystallization of arfvedsonite and was followed by emplacement of the northern hypersolvus

  1. Structure peculiarities of mixed alkali silicate glasses

    International Nuclear Information System (INIS)

    Bershtein, V.A.; Gorbachev, V.V.; Egorov, V.

    1980-01-01

    The thermal porperties and structure of alkali and mixed alkali (Li, Na, K) silicate glasses by means of differential scanning calorimetry (DSC), the positron annihilation method, X-ray fluorescence and infrared (300-30 cm -1 ) spectroscopy were studied. Introduction of different alkali cations in glass results in nonadditive change in their electron structure (bond covalence degree growth) and the thermal behaviour. The different manifestations of mixed alkali effect can be explained by the lessening of long distance Coulomb interactions and strengthening the short-range forces in the mixed alkali glasses. (orig.)

  2. Density of mixed alkali borate glasses: A structural analysis

    International Nuclear Information System (INIS)

    Doweidar, H.; El-Damrawi, G.M.; Moustafa, Y.M.; Ramadan, R.M.

    2005-01-01

    Density of mixed alkali borate glasses has been correlated with the glass structure. It is assumed that in such glasses each alkali oxide associates with a proportional quantity of B 2 O 3 . The number of BO 3 and BO 4 units related to each type of alkali oxide depends on the total concentration of alkali oxide. It is concluded that in mixed alkali borate glasses the volumes of structural units related to an alkali ion are the same as in the corresponding binary alkali borate glass. This reveals that each type of alkali oxide forms its own borate matrix and behaves as if not affected with the presence of the other alkali oxide. Similar conclusions are valid for borate glasses with three types of alkali oxide

  3. Microfluidic Leaching of Soil Minerals: Release of K+ from K Feldspar

    Science.gov (United States)

    Ciceri, Davide; Allanore, Antoine

    2015-01-01

    The rate of K+ leaching from soil minerals such as K-feldspar is believed to be too slow to provide agronomic benefit. Currently, theories and methods available to interpret kinetics of mineral processes in soil fail to consider its microfluidic nature. In this study, we measure the leaching rate of K+ ions from a K-feldspar-bearing rock (syenite) in a microfluidic environment, and demonstrate that at the spatial and temporal scales experienced by crop roots, K+ is available at a faster rate than that measured with conventional apparatuses. We present a device to investigate kinetics of mineral leaching at an unprecedented simultaneous resolution of space (~101-102 μm), time (~101-102 min) and fluid volume (~100-101 mL). Results obtained from such a device challenge the notion that silicate minerals cannot be used as alternative fertilizers for tropical soils. PMID:26485160

  4. Thermoluminescence of annealed and shock-loaded feldspar

    International Nuclear Information System (INIS)

    Hartmetz, C.P.

    1988-01-01

    Samples of oligoclase and bytownite were shock-loaded to a variety of pressures, and annealed for a variety of temperatures and times. The effect of Mrad doses of gamma-rays on oligoclase TL were also studied. After these treatments, thermoluminescence (TL) and X-ray diffraction (XRD) measurements were made to: (1) determine the effects of shock on terrestrial feldspar and compare with variations in the TL emission of ordinary chondrites (OCs); (2) determine if disordering in feldspar was responsible for any related changes in TL properties of OCs; (3) determine if the combined effect of shock plus annealing causes the changes in TL properties; (4) see if radiation damage from cosmic ray exposure plays a role in the TL variations; (5) examine the implications of this work to the thermal and shock histories of OCs. The lightly shock-loaded and annealed oligoclase samples have a dominant peak temperature of 120-140 C, identical to type 3.3-3.5 OCs. The heavily shocked samples dominant peak is at 230C, similar to type > 3.5 OCs . While the heavily annealed/disordered oligoclase samples have a peak at 280C, this peak is rarely observed in OCs. Radiation damage from Mrad doses of gamma-rays produced no change in peak temperature, but facilitated the shift to higher peak temperatures. The TL sensitivity of the shocked samples decreased by a factor of 25. Samples annealed at low temperatures (438-533C) showed a factor of 2 decrease in TL, but at the highest temperatures, the TL was a factor of 8 higher

  5. Cementation of nitrate solutions by alkali-activated slag-metakaolin cement

    International Nuclear Information System (INIS)

    Rakhimova, N.R.; Rakhimov, R.Z.; Naumkina, N.I.; Gubaidullina, A.M.; Yakovlev, G.I.; Shaybadullina, A.V.

    2015-01-01

    This paper considered the feasibility of solidification of liquid salt wastes by NaNO 3 solutions of concentration 100-700 g/l by alkali-activated slag (AASC) and alkali-activated slag-meta-kaolin cements (AASMC). The AASC (activated by 5% Na 2 O) and AASMC (activated by 5% Na 2 O and introduced with 5% of MK) mixed with NaNO 3 solutions were more effective in comparison with Portland cement. The compressive strength of hardened AASC and AASMC pastes was 1.6-12. and 7- 21 MPa in 3-day age and 13.4-31 and 20-37 MPa in 28-day age, respectively, depending on concentration of NaNO 3 solution. The incorporation of 3-5% meta-kaolin in AASC: (i) increased the compressive strength of hardened AASMC pastes up to 50% depending on the type of meta-kaolin, (ii) shortened setting times of fresh AASMC pastes

  6. (e, 2e) triple differential cross sections of alkali and alkali earth atoms: Na, K and Mg, Ca

    International Nuclear Information System (INIS)

    Hitawala, U; Purohit, G; Sud, K K

    2008-01-01

    Recently low-energy measurements have been reported for alkali targets Na and K and alkali earth targets Mg and Ca in coplanar symmetric geometry. We report the results of our calculation of triple differential cross section (TDCS) for electron impact single ionization (i.e. (e, 2e) processes) of alkali atoms Na, K and alkali earth atoms Mg, Ca in coplanar symmetric geometry. We have performed the present calculations using the distorted-wave Born approximation (DWBA) formalism at intermediate incident electron energies used in the recently performed experiments. Ionization takes place from the valence shell for all the targets investigated and the outgoing electrons share the excess energy equally. We have also considered the effect of target polarization in our DWBA calculations which may be an important quantity at incident electron energies used in the present investigation. We find that the DWBA formalism is able to reproduce most of the trend of experimental data and may provide a future direction for further investigation of ionization process on alkali and alkali earth metals. It is also observed that the second-order effects are more important to understand the collision dynamics of (e, 2e) processes on alkali earth targets

  7. Construction of thermionic alkali-ion sources

    International Nuclear Information System (INIS)

    Ul Haq, F.

    1986-01-01

    A simple technique is described by which singly charged alkali ions of K, Na, Li, Rb and Cs are produced by heating ultra-pure chemical salts of different alkali metals on tungsten filaments without employing a temperature measuring device. The character of alkali-ion currents at different heating powers and the remarkably constant ion emission current for prolonged periods are discussed. (author)

  8. On the shape of continuous wave infrared stimulated luminescence signals from feldspars: A case study

    DEFF Research Database (Denmark)

    Pagonis, V.; Jain, Mayank; Thomsen, Kristina Jørkov

    2014-01-01

    The continuous-wave IRSL (CW-IRSL) signals from feldspars are known to decay in a non-exponential manner, and their exact mathematical description is of great importance in dosimetric and dating studies. This paper investigates the possibility of fitting experimental CW-IRSL curves from a variety...... to guide future modeling work on luminescence processes in feldspars. Small statistical differences were found between K-rich and Na-rich fractions of the same sample. However, the experimental data shows that the parameters depend on the irradiation dose, but do not depend on the time elapsed after...

  9. Local structure of alkalis in mixed-alkali borate glass to elucidate the origin of mixed-alkali effect

    Directory of Open Access Journals (Sweden)

    Yomei Tokuda

    2015-12-01

    Full Text Available We report the structural analysis of Na+ and Cs+ in sodium cesium borate crystals and glasses using 23Na and 133Cs magic-angle spinning nuclear magnetic resonance (MAS NMR spectroscopy. The composition dependence of NMR spectra of the borate was similar to that of the silicate: (1 the peak position of cesium borate crystals shifted to upfield for structures with larger Cs+ coordination numbers, (2 the MAS NMR spectra of xNa2O-yCs2O-3B2O3 (x = 0, 0.25, 0.5, 0.75, 1.0, x + y = 1 glass showed that the average coordination number (CN of both the alkali cations decreases with increasing Cs+/(Na+ + Cs+ ratio. However, the degree of decrement in borates is much smaller than that in silicates. We have considered that the small difference in CN is due to 4-coordinated B, because it is electrically compensated by the alkali metal ions resulting in the restriction of having various coordinations of O to alkali metal.

  10. Biochemical evolution. I. Polymerization on internal, organophilic silica surfaces of dealuminated zeolites and feldspars

    Science.gov (United States)

    Smith, Joseph V.

    1998-01-01

    Catalysis at mineral surfaces might generate replicating biopolymers from simple chemicals supplied by meteorites, volcanic gases, and photochemical gas reactions. Many ideas are implausible in detail because the proposed mineral surfaces strongly prefer water and other ionic species to organic ones. The molecular sieve silicalite (Union Carbide; = Al-free Mobil ZSM-5 zeolite) has a three-dimensional, 10-ring channel system whose electrically neutral Si-O surface strongly adsorbs organic species over water. Three -O-Si tetrahedral bonds lie in the surface, and the fourth Si-O points inwards. In contrast, the outward Si-OH of simple quartz and feldspar crystals generates their ionic organophobicity. The ZSM-5-type zeolite mutinaite occurs in Antarctica with boggsite and tschernichite (Al-analog of Mobil Beta). Archean mutinaite might have become de-aluminated toward silicalite during hot/cold/wet/dry cycles. Catalytic activity of silicalite increases linearly with Al-OH substitution for Si, and Al atoms tend to avoid each other. Adjacent organophilic and catalytic Al-OH regions in nanometer channels might have scavenged organic species for catalytic assembly into specific polymers protected from prompt photochemical destruction. Polymer migration along weathered silicic surfaces of micrometer-wide channels of feldspars might have led to assembly of replicating catalytic biomolecules and perhaps primitive cellular organisms. Silica-rich volcanic glasses should have been abundant on the early Earth, ready for crystallization into zeolites and feldspars, as in present continental basins. Abundant chert from weakly metamorphosed Archaean rocks might retain microscopic clues to the proposed mineral adsorbent/catalysts. Other framework silicas are possible, including ones with laevo/dextro one-dimensional channels. Organic molecules, transition-metal ions, and P occur inside modern feldspars. PMID:9520372

  11. Coprecipitation of alkali metal ions with calcium carbonate

    International Nuclear Information System (INIS)

    Okumura, Minoru; Kitano, Yasushi

    1986-01-01

    The coprecipitation of alkali metal ions Li + , Na + , K + and Rb + with calcium carbonate has been studied experimentally and the following results have been obtained: (1) Alkali metal ions are more easily coprecipitated with aragonite than with calcite. (2) The relationship between the amounts of alkali metal ions coprecipitated with aragonite and their ionic radii shows a parabolic curve with a peak located at Na + which has approximately the same ionic radius as Ca 2+ . (3) However, the amounts of alkali metal ions coprecipitated with calcite decrease with increasing ionic radius of alkali metals. (4) Our results support the hypothesis that (a) alkali metals are in interstitial positions in the crystal structure of calcite and do not substitute for Ca 2+ in the lattice, but (b) in aragonite, alkali metals substitute for Ca 2+ in the crystal structure. (5) Magnesium ions in the parent solution increase the amounts of alkali metal ions (Li + , Na + , K + and Rb + ) coprecipitated with calcite but decrease those with aragonite. (6) Sodium-bearing aragonite decreases the incorporation of other alkali metal ions (Li + , K + and Rb + ) into the aragonite. (author)

  12. Petrography, Gamma Radiation Measurements and Dose Rate, Northeastern Um Ara Area, South Eastern Desert, Egypt

    International Nuclear Information System (INIS)

    Moghazy, N.M.

    2016-01-01

    The northern part of Um Ara alkali feldspar micro granite has subjected to extensive post-magmatic metasomatic reworking resulting in development of amazonitized and albitized zones, reflecting K- and Na metasomatism leading to gross enrichment in U and Th towards the more evolved phases (e.g., albitized zones). Spectrometric survey data indicate that eU in Dokhan volcanics has the range of 2 to 42 ppm with an average value of 10 ppm and in monzogranites. It varies from 3 to 13 ppm with an average of 7 ppm while in alkali feldspar microgranites eU contents vary from 3 to 282 ppm with an average value of 30 ppm. The (eTh) contents in Dokhan volcanics ranges from 5-51 ppm with an average 18 ppm, in monzogranites their content was in the range of 11 to 47 ppm with an average value of 27 ppm where it ranges from 14 to 83 ppm with an average 46 ppm in alkali feldspar granite. The enhanced uranium content in altered zones was attributed to disseminated and fracture filling uranophane, autonite, in addition to other U and Th bearing minerals (such as columbite, zircon, monazite, xenotime and fluorite). Gamma-radiation dose rate and annual effective dose equivalents in mSv/y, Radium equivalent activity, external (H e x) and internal hazard index (H i n) and gamma activity index (Iγ) for all investigated samples were calculated to assess the potential radiation hazard for people living in dwellings made of the studied granites. Alkali feldspar granite activities would suggest that caution must be taken when using granites as building materials because they have radioactivity above the proposed acceptable level.

  13. Studies on the alkali-silica reaction rim in a simplified calcium-alkali-silicate system

    NARCIS (Netherlands)

    Zheng, Kunpeng; Adriaensens, Peter; De Schutter, Geert; Ye, G.; Taerwe, Luc

    2016-01-01

    This work is intended to provide a better understanding about the properties and roles of the reaction rim in an alkali-silica reaction. A simplified calcium-alkali-silicate system was created to simulate the multiple interactions among reactive silica, alkaline solution and portlandite near the

  14. Rapakivi texture in porphyritic dikes within the Karavanke Granitic Massif (Slovenia

    Directory of Open Access Journals (Sweden)

    Giuliano Bellieni

    2002-01-01

    Full Text Available The northern Karavanke Granitic Massif straddles the Slovenian–Austrian border. The investigated area lies in northern Slovenia, and extends from the western Slovenian–Austrian border to the east for about 30 km, with a maximum width of 2 km. The massif exhibits a bimodal magmatic association comprising mainly syenogranite and syenite with contemporaneous gabbroic rocks. Rocks of intermediate composition are less abundant and show field, textural and chemical features suggesting that they have formed as a result of the interaction (mixing and mingling between felsic and mafic magmas. Plagioclasemantled alkali feldspars occur in dikes of porphyritic syenite, which cut larger bodies of gabbroic rocks. Field, mineralogical, petrographic and geochemical evidences suggest that the porphyritic syenite is a hybrid rock, formed by the interaction of mafic and felsic magmas. The formation of plagioclase-mantled alkali feldspar can be explained by the introduction of alkali feldspar from felsic, syenogranitic magma into more mafic magma, causing local undercooling in the portion of mafic magma surrounding the crystals. This resulted in the growth of cellular plagioclase, with quartz infilling, in a thermally and compositionally equilibrating system.

  15. Computer augumented modelling studies of Pb(II, Cd(II, Hg(II, Co(II, Ni(II, Cu(II and Zn(II complexes of L-glutamic acid in 1,2-propanediol–water mixtures

    Directory of Open Access Journals (Sweden)

    MAHESWARA RAO VEGI

    2008-12-01

    Full Text Available Chemical speciation of Pb(II, Cd(II, Hg(II, Co(II, Ni(II, Cu(II and Zn(II complexes of L-glutamic acid was studied at 303 K in 0–60 vol. % 1,2-propanediol–water mixtures, whereby the ionic strength was maintained at 0.16 mol dm-3. The active forms of the ligand are LH3+, LH2 and LH–. The predominant detected species were ML, ML2, MLH, ML2H and ML2H2. The trend of the variation in the stability constants with changing dielectric constant of the medium is explained based on the cation stabilizing nature of the co-solvents, specific solvent–water interactions, charge dispersion and specific interactions of the co-solvent with the solute. The effect of systematic errors in the concentrations of the substances on the stability constants is in the order alkali > > acid > ligand > metal. The bioavailability and transportation of metals are explained based on distribution diagrams and stability constants.

  16. Method of handling radioactive alkali metal waste

    Science.gov (United States)

    Wolson, R.D.; McPheeters, C.C.

    Radioactive alkali metal is mixed with particulate silica in a rotary drum reactor in which the alkali metal is converted to the monoxide during rotation of the reactor to produce particulate silica coated with the alkali metal monoxide suitable as a feed material to make a glass for storing radioactive material. Silica particles, the majority of which pass through a 95 mesh screen or preferably through a 200 mesh screen, are employed in this process, and the preferred weight ratio of silica to alkali metal is 7 to 1 in order to produce a feed material for the final glass product having a silica to alkali metal monoxide ratio of about 5 to 1.

  17. Method of handling radioactive alkali metal waste

    International Nuclear Information System (INIS)

    Mcpheeters, C.C.; Wolson, R.D.

    1980-01-01

    Radioactive alkali metal is mixed with particulate silica in a rotary drum reactor in which the alkali metal is converted to the monoxide during rotation of the reactor to produce particulate silica coated with the alkali metal monoxide suitable as a feed material to make a glass for storing radioactive material. Silica particles, the majority of which pass through a 95 mesh screen or preferably through a 200 mesh screen, are employed in this process, and the preferred weight ratio of silica to alkali metal is 7 to 1 in order to produce a feed material for the final glass product having a silica to alkali metal monoxide ratio of about 5 to 1

  18. Luminescence characteristics of quartz and feldspar from tectonically uplifted terraces in Kashmir Basin, Jammu and Kashmir, India

    International Nuclear Information System (INIS)

    Jaiswal, Manoj K.; Bhat, M.I.; Bali, B.S.; Ahmad, Shabir; Chen, Y.G.

    2009-01-01

    The Kashmir Valley or the Jhelum basin is an intermontane-basin in NW Himalaya bounded by the Pir Panjal Range in the south and southwest and the Great Himalayan Range in the north and northeast. The valley is marked by active major thrust boundaries in its south and southwestern parts. Remote sensing studies and morphometric analysis suggest neo-tectonic activities and the formation of tectonic terraces due to uplift on the major thrust boundaries in NW Himalayas. The quartz from freshly eroded mountain belts is usually found to show very poor luminescence sensitivity and thus not suitable for optical dating. Similar problems occurred with the quartz from the Srinagar Basin. Due to this, feldspar was selected as a natural dose meter for dating tectonically uplifted terraces in an active and dynamic belt of the NW Himalayas. We report here for the first time the luminescence characteristics of quartz and feldspar minerals from the study area. However, feldspar also shows poor luminescence sensitivity, although enough to perform optical dating. Athermal fading was observed in all the feldspar samples, which was corrected using 'g' values; a large scatter was found in the g values, probably due to intermixing of feldspar grains from varying source rock types and also due to poor luminescence sensitivity. An average g value correction to the mean paleodose was found to agree if compared with the thermo-luminescence date of loess deposit dated earlier. The ages show that the terrace formation started taking place at ∼100 ka in the southwestern part of the Jhelum basin and continued with pulses at 50 ka and 11 ka towards the northwestern part.

  19. Testing feldspar luminescence dating of young archaeological heated materials using potshards from Pella (Tell Tabqat Fahl) in the Jordan valley

    DEFF Research Database (Denmark)

    Khasswneh, Sahar Al; Murray, Andrew Sean; Bourke, Stephen

    2017-01-01

    Recent developments in the use of more stable feldspar signals in the luminescence dating of sediments offer the possibility of obtaining accurate feldspar luminescence ages for ceramic artefacts; this is especially interesting in locations which do not provide suitable quartz extracts. Here we e...

  20. Alkali Influence on Synthesis of Solid Electrolyte Based on Alkali Nitrate-Alumina

    International Nuclear Information System (INIS)

    Yustinus Purwamargapratala; Purnama, S.; Purwanto, P.

    2008-01-01

    Research of solid electrolyte based on alumina with addition of alkali materials of barium nitrate, calcium nitrate, sodium nitrate and lithium nitrate has been done. Aluminium hydroxide and alkali nitrate were mixed in mole ratio of 1 : 1 in water media and pyrolyzed at 300 o C for 1 hour Pyrolysis result were then mixed with alumina in mole ratio of 1 : 1, compacted and heated at 600 o C for 3 hours. To characterize the sample, XRD (X-Ray Diffractometers) and LCR meter (impedance, capacitance, and resistance) were used for analysis the phase and conductivity properties. The result showed formation of alkali-aluminate in which Li-base have the highest room temperature conductivity of 3.1290 x 10 -5 S.cm -1 , while Ba-base have the lowest conductivity of 5.7266 x 10 -8 S.cm -1 . (author)

  1. Thermodynamic properties of alkali borosilicate gasses and metaborates

    International Nuclear Information System (INIS)

    Asano, Mitsuru

    1992-01-01

    Borosilicate glasses are the proposed solidifying material for storing high level radioactive wastes in deep underground strata. Those have low melting point, and can contain relatively large amount of high level radioactive wastes. When borosilicate glasses are used for this purpose, they must be sufficiently stable and highly reliable in the vitrification process, engineered storage and the disposal in deep underground strata. The main vaporizing components from borosilicate glasses are alkali elements and boron. In this report, as for the vaporizing behavior of alkali borosilicate glasses, the research on thermodynamic standpoint carried out by the authors is explained, and the thermodynamic properties of alkali metaborates of monomer and dimer which are the main evaporation gases are reported. The evaporation and the activity of alkali borosilicate glasses, the thermodynamic properties of alkali borosilicate glasses, gaseous alkali metaborates and alkali metaborate system solid solution and so on are described. (K.I.)

  2. Physical and optical studies in mixed alkali borate glasses with three types of alkali ions

    International Nuclear Information System (INIS)

    Samee, M.A.; Awasthi, A.M.; Shripathi, T.; Bale, Shashidhar; Srinivasu, Ch.; Rahman, Syed

    2011-01-01

    Research highlights: → We report, for the first time, the mixed alkali effect in the (40-x)Li 2 O-xNa 2 O-10K 2 O-50B 2 O 3 glasses through optical properties, density and modulated DSC studies. → Optical band gap (E opt ) and Urbach energy (ΔE) have been evaluated. → The values of E opt and ΔE show non-linear behavior with compositional parameter showing the mixed alkali effect. → The glass stability S is observed to be less which may be important for the present glasses as promising material for non-optical applications. - Abstract: So far only a handful of publications have been concerned with the study of the mixed alkali effect in borate glasses containing three types of alkali ions. In the present work, the mixed alkali effect (MAE) has been investigated in the glass system (40-x)Li 2 O-xNa 2 O-10K 2 O-50B 2 O 3 . (0 ≤ x ≤ 40 mol%) through density and modulated DSC studies. The density and glass transition temperature of the present glasses varies non-linearly exhibiting mixed alkali effect. The glass stability is observed to be less which may be important for the present glasses as promising material for non-optical applications. We report, for the first time, the mixed alkali effect in the present glasses through optical properties. From the absorption edge studies, the values of indirect optical band gap (E opt ), direct optical band gap and Urbach energy (ΔE) have been evaluated. The values of E opt and ΔE show non-linear behavior with compositional parameter showing the mixed alkali effect. The average electronic polarizability of oxide ions α O 2- , optical basicity Λ, and Yamashita-Kurosawa's interaction parameter A have been examined to check the correlations among them and bonding character. Based on good correlation among electronic polarizability of oxide ions, optical basicity and interaction parameter, the present Li 2 O-Na 2 O-K 2 O-B 2 O 3 glasses are classified as normal ionic (basic) oxides.

  3. Some evidence of uranium in volcanic feldspar rocks in the state of Sonora

    Energy Technology Data Exchange (ETDEWEB)

    Marquina M, O. E. [Uranio Mexicano, Mexico City

    1983-05-15

    Description is given of four projects of exploration and survey for uranium associated with tertiary volcanic feldspar rocks importantly dispersed in the State of Sonora and being carried out by Uranium Mexicano.

  4. Experimental early crystallization of K-feldspar in granitic systems. Implications on the origin of magmatic fabrics in granitic rocks

    Energy Technology Data Exchange (ETDEWEB)

    Díaz-Alvarado, J.

    2017-07-01

    One of the most outstanding characteristics of some granodioritic to granitic rocks is the presence of K-feldspar megacrysts. For instance, granodiorites and monzogranites of the Spanish Central System batholith present variable amounts of large (up to 10cm in length) euhedral K-feldspar crystals. The porphyritic textures, the euhedral shape, the alignment of plagioclase and biotite inclusions and the magmatic fabrics point to a magmatic origin for these megacrysts. This work presents a phase equilibria study in a high-K2O granodioritic system. A series of experiments were conducted with a granodioritic composition (GEMbiot) to study the crystallization sequence at the emplacement conditions in the Gredos massif, i.e. 4 H2O wt.% and 0.4GPa. Experimental results show that orthopiroxene is the liquidus phase at 1010ºC, which reacts with the H2O-rich melt to stabilize biotite between 980 and 940ºC. Plagioclase crystallizes at around 910ºC, and K-feldspar crystallizes in the matrix between 750 and 700ºC when the crystal fraction is around 0.5. However, at 850 ºC, a pelite-doped experiment shows euhedral K-feldspar (≈5vol%) in both the reactive xenolith domain together with cordierite and the granodioritic domain, where the K2O wt.% rise from 4.5 in the normal experiment to 5.9 in the doped experiment. These results suggest that the bulk-assimilation process promotes the bulk and heterogeneous K2O enrichment in a huge granodioritic magma volume, which triggers an early crystallization of K-feldspar megacrysts. Because of this early crystallization of the megacrysts, the magmatic foliations defined by K-feldspar megacrysts are formed during and after the emplacement processes and are highly influenced by tectonic kinematics.

  5. Relation between the electroforming voltage in alkali halide-polymer diodes and the bandgap of the alkali halide

    International Nuclear Information System (INIS)

    Bory, Benjamin F.; Wang, Jingxin; Janssen, René A. J.; Meskers, Stefan C. J.; Gomes, Henrique L.; De Leeuw, Dago M.

    2014-01-01

    Electroforming of indium-tin-oxide/alkali halide/poly(spirofluorene)/Ba/Al diodes has been investigated by bias dependent reflectivity measurements. The threshold voltages for electrocoloration and electroforming are independent of layer thickness and correlate with the bandgap of the alkali halide. We argue that the origin is voltage induced defect formation. Frenkel defect pairs are formed by electron–hole recombination in the alkali halide. This self-accelerating process mitigates injection barriers. The dynamic junction formation is compared to that of a light emitting electrochemical cell. A critical defect density for electroforming is 10 25 /m 3 . The electroformed alkali halide layer can be considered as a highly doped semiconductor with metallic transport characteristics

  6. 40 CFR 721.4740 - Alkali metal nitrites.

    Science.gov (United States)

    2010-07-01

    ... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Alkali metal nitrites. 721.4740... Substances § 721.4740 Alkali metal nitrites. (a) Chemical substances and significant new use subject to reporting. (1) The category of chemical substances which are nitrites of the alkali metals (Group IA in the...

  7. Method for the safe disposal of alkali metal

    International Nuclear Information System (INIS)

    Johnson, T.R.

    1977-01-01

    Alkali metals such as those employed in liquid metal coolant systems can be safely reacted to form hydroxides by first dissolving the alkali metal in relatively inert metals such as lead or bismuth. The alloy thus formed is contacted with a molten salt including the alkali metal hydroxide and possibly the alkali metal carbonate in the presence of oxygen. This oxidizes the alkali metal to an oxide which is soluble within the molten salt. The salt is separated and contacted with steam or steam--CO 2 mixture to convert the alkali metal oxide to the hydroxide. These reactions can be conducted with minimal hydrogen evolution and with the heat of reaction distributed between the several reaction steps. 5 claims, 1 figure

  8. Elastic modulus of the alkali-silica reaction rim in a simplified calcium-alkali-silicate system determined by nano-indentation

    NARCIS (Netherlands)

    Zheng, Kunpeng; Lukovic, M.; De Schutter, Geert; Ye, G.; Taerwe, Luc

    2016-01-01

    This work aims at providing a better understanding of the mechanical properties of the reaction rim in the alkali-silica reaction. The elastic modulus of the calcium alkali silicate constituting the reaction rim, which is formed at the interface between alkali silicate and Ca(OH)2 in a

  9. Radiation-induced growth and isothermal decay of infrared-stimulated luminescence from feldspar

    DEFF Research Database (Denmark)

    Guralnik, Benny; Li, Bo; Jain, Mayank

    2015-01-01

    the growth and decay of laboratory-regenerated luminescence signals. Here we review a selection of common models describing the response of infrared stimulated luminescence (IRSL) of feldspar to constant radiation and temperature as administered in the laboratory. We use this opportunity to introduce...

  10. Alkali binding in hydrated Portland cement paste

    NARCIS (Netherlands)

    Chen, Wei; Brouwers, Jos

    2010-01-01

    The alkali-binding capacity of C–S–H in hydrated Portland cement pastes is addressed in this study. The amount of bound alkalis in C–S–H is computed based on the alkali partition theories firstly proposed by Taylor (1987) and later further developed by Brouwers and Van Eijk (2003). Experimental data

  11. Alkali-aggregate reactivity (AAR) facts book.

    Science.gov (United States)

    2013-03-01

    This document provides detailed information on alkali-aggregate reactivity (AAR). It primarily discusses alkali-silica reaction (ASR), covering the chemistry, symptoms, test methods, prevention, specifications, diagnosis and prognosis, and mitigation...

  12. Beneficiation of feldspar ore for application in the ceramic industry: Influence of composition on the physical characteristics

    OpenAIRE

    Gaied, M.E.; Gallala, W.

    2015-01-01

    In this study, physical and physicochemical experiments were carried out to improve the quality of feldspar ore in Sidi Aïch massive, located in the Gafsa region of south-western Tunisia. After determination of the mineralogical and the chemical composition, flotation methods were applied. In this study, non-hydrofluoric acid flotation methods used in feldspar-quartz separation were compared with each other and with the conventional HF/amine method. The results showed that conventional HF/ami...

  13. Alkali depletion and ion-beam mixing in glasses

    International Nuclear Information System (INIS)

    Arnold, G.W.

    1983-01-01

    Ion-implantation-induced alkali depletion in simple alkali-silicate glasses (12M 2 O.88SiO 2 ) has been studied for implantations at room temperature and near 77K. Results are consistent with a mechanism for alkali removal, by heavy ion bombardment, based on radiation-enhanced migration and preferential removal of alkali from the outermost layers. Similar results were obtained for mixed-alkali glasses ((12-x)Cs 2 .O.xM 2 O.88SiO 2 ) where, in addition, a mixed-alkali effect may also be operative. Some preliminary experiments with ion implantation through thin Al films on SiO 2 glass and on a phosphate glass show that inter-diffusion takes place and suggest that this ion-mixing technique may be a useful method for altering the physical properties of glass surfaces

  14. Ionic interactions in alkali-aluminium tetrafluoride clusters

    International Nuclear Information System (INIS)

    Akdeniz, Z.; Cicek, Z.; Karaman, A.; Pastore, G.; Tosi, M.P.

    1999-08-01

    Complex anion structures ((AlF 4 ) - , (AlF 5 ) 2- and (AlF 6 ) 3- ) coexist in liquid mixtures of aluminium trifluoride and alkali fluorides in composition-dependent relative concentrations and are known to interact with the alkali counterions. We present a comparative study of the static and vibrational structures of MAlF 4 molecules (with M = any alkali), with the aim of developing and testing a refined model of the ionic interactions for applications to the Al-M fluoride mixtures. We find that, whereas an edge-bridged coordination is strongly favoured for Li in LiAIF 4 , edge-bridging and face-bridging of the alkali ion become energetically equivalent as one moves from Na to the heavier alkalis. This result is sensitive to the inclusion of alkali polarizability and may be interpreted as implying (for M = K, Rb or Cs) almost free relative rotations of the M + and (AlF 4 ) - partners at temperatures of relevance to experiment. The consistency of such a viewpoint with electron diffraction data on vapours and with Raman spectra on melts is discussed. (author)

  15. (abstract) Experimental and Modeling Studies of the Exchange Current at the Alkali Beta'-Alumina/Porous Electrode/Alkali Metal Vapor Three Phase Boundary

    Science.gov (United States)

    Williams, R. M.; Jeffries-Nakamura, B.; Ryan, M. A.; Underwood, M. L.; O'Connor, D.; Kikkert, S.

    1993-01-01

    The microscopic mechanism of the alkali ion-electron recombination reaction at the three phase boundary zone formed by a porous metal electrode in the alkali vapor on the surface of an alkali beta'-alumina solid electrolyte (BASE) ceramic has been studied by comparison of the expected rates for the three simplest reaction mechanisms with known temperature dependent rate data; and the physical parameters of typical porous metal electrode/BASE/alkali metal vapor reaction zones. The three simplest reactions are tunneling of electrons from the alkali coated electrode to a surface bound alkali metal ion; emission of an electron from the electrode with subsequent capture by a surface bound alkali metal ion; and thermal emission of an alkali cation from the BASE and its capture on the porous metal electrode surface where it may recombine with an electron. Only the first reaction adequately accounts for both the high observed rate and its temperature dependence. New results include crude modeling of simple, one step, three phase, solid/solid/gas electrochemical reaction.

  16. Controlled in-situ dissolution of an alkali metal

    Science.gov (United States)

    Jones, Jeffrey Donald; Dooley, Kirk John; Tolman, David Donald

    2012-09-11

    A method for the controllable dissolution of one or more alkali metals from a vessel containing a one or more alkali metals and/or one or more partially passivated alkali metals. The vessel preferably comprising a sodium, NaK or other alkali metal-cooled nuclear reactor that has been used. The alkali metal, preferably sodium, potassium or a combination thereof, in the vessel is exposed to a treatment liquid, preferably an acidic liquid, more preferably citric acid. Preferably, the treatment liquid is maintained in continuous motion relative to any surface of unreacted alkali metal with which the treatment liquid is in contact. The treatment liquid is preferably pumped into the vessel containing the one or more alkali metals and the resulting fluid is extracted and optionally further processed. Preferably, the resulting off-gases are processed by an off-gas treatment system and the resulting liquids are processed by a liquid disposal system. In one preferred embodiment, an inert gas is pumped into the vessel along with the treatment liquid.

  17. Extreme alkali bicarbonate- and carbonate-rich fluid inclusions in granite pegmatite from the Precambrian Rønne granite, Bornholm Island, Denmark

    Science.gov (United States)

    Thomas, Rainer; Davidson, Paul; Schmidt, Christian

    2011-02-01

    Our study of fluid and melt inclusions in quartz and feldspar from granite pegmatite from the Precambrian Rønne granite, Bornholm Island, Denmark revealed extremely alkali bicarbonate- and carbonate-rich inclusions. The solid phases (daughter crystals) are mainly nahcolite [NaHCO3], zabuyelite [Li2CO3], and in rare cases potash [K2CO3] in addition to the volatile phases CO2 and aqueous carbonate/bicarbonate solution. Rare melt inclusions contain nahcolite, dawsonite [NaAl(CO3)(OH)2], and muscovite. In addition to fluid and melt inclusions, there are primary CO2-rich vapor inclusions, which mostly contain small nahcolite crystals. The identification of potash as a naturally occurring mineral would appear to be the first recorded instance. From the appearance of high concentrations of these carbonates and bicarbonates, we suggest that the mineral-forming media were water- and alkali carbonate-rich silicate melts or highly concentrated fluids. The coexistence of silicate melt inclusions with carbonate-rich fluid and nahcolite-rich vapor inclusions indicates a melt-melt-vapor equilibrium during the crystallization of the pegmatite. These results are supported by the results of hydrothermal diamond anvil cell experiments in the pseudoternary system H2O-NaHCO3-SiO2. Additionally, we show that boundary layer effects were insignificant in the Bornholm pegmatites and are not required for the origin of primary textures in compositionally simple pegmatites at least.

  18. Dynamics of the deep red Fe3+ photoluminescence emission in feldspar

    DEFF Research Database (Denmark)

    Prasad, Amit Kumar; Jain, Mayank

    2018-01-01

    be exploited for site discrimination within a complex feldspar sample. The radiative relaxation in Fe3+ (4T1 → 6A1) is shown to be a dynamic process depending on whether the ion is excited using resonant or non-resonant transition. We suggest that during resonant excitation, the excited state of Fe3+ undergoes...

  19. Effect of alkali ion on relaxation properties of binary alkali-borate glasses

    International Nuclear Information System (INIS)

    Lomovskoj, V.A.; Bartenev, G.M.

    1992-01-01

    Method of relaxation spectrometry were used to analyze the data on internal friction spectra of lithium, sodium, potassium and rubidium alkali-borate glasses in wide range of temperatures and frequencies. The nature of two relaxation processes was clarified: β m -process, related with mobility of alkaline metal cations, and α-process (vitrification), conditioned by system transformation from viscous-flow to vitreous state. It is shown that atomic-molecular mechanism of vitrification process changes when passing from vitreous B 2 O 3 to alkali-borate glasses

  20. Charge transfer in gold--alkali-metal systems

    International Nuclear Information System (INIS)

    Watson, R.E.; Weinert, M.

    1994-01-01

    Based on conventional electronegativity arguments, gold--alkali-metal compounds are expected to be among the most ''ionic'' of metallic compounds. The concepts of ionicity and charge transfer are difficult to quantify. However, the changes in bonding in the 50/50 Au--alkali-metal systems between the elemental metals and the compounds are so severe that observations can readily be made concerning their character. The results, as obtained from self-consistent electronic-structure calculations, lead to the apparently odd observation that the electron density at the alkali-metal sites in the compound increases significantly and this involves high l componennts in the charge density. This increase, however, can be attributed to Au-like orbitals spatially overlapping the alkali-metal sites. In a chemical sense, it is reasonable to consider the alkali-metal transferring charge to these Au orbitals. While normally the difference in heats of formation between muffin-tin and full-potential calculations for transition-metal--transition-metal and transition-metal--main-group (e.g., Al) compounds having high site symmetry are small, for the gold--alkali-metal systems, the changes in bonding in the compounds cause differences of ∼0.5 eV/atom between the two classes of potential. Any serious estimate of the electronic structure in these systems must account for these aspherical bonding charges. The origin of the semiconducting behavior of the heavy-alkali-metal Au compounds is shown to arise from a combination of the Au-Au separations and the ionic character of the compounds; the light-alkali-metal Au compounds, with their smaller Au-Au separations, do not have a semiconducting gap. Core-level shifts and isomer shifts are also briefly discussed

  1. Application of pulsed OSL to the separation of the luminescence components from a mixed quartz/feldspar sample

    DEFF Research Database (Denmark)

    Denby, Phil M.; Bøtter-Jensen, L.; Murray, A.S.

    2006-01-01

    with a feldspar signal. We have developed instrumentation for the study of high-speed pulse stimulated OSL. Our system uses the standard blue/IR LED stimulation unit of a Riso reader (allowing stimulation pulses down to 1-2 mu s duration) and can thus be applied to the routine analysis of samples. Using...... that counts are only accumulated during a windowed period, reduces the feldspar signal to 1.6% of its original value relative to that of the quartz. (c) 2006 Elsevier Ltd. All rights reserved....

  2. Formation of lysinoalanine in egg white under alkali treatment.

    Science.gov (United States)

    Zhao, Yan; Luo, Xuying; Li, Jianke; Xu, Mingsheng; Tu, Yonggang

    2016-03-01

    To investigate the formation mechanism of lysinoalanine (LAL) in eggs during the alkali treatment process, NaOH was used for the direct alkali treatment of egg white, ovalbumin, and amino acids; in addition, the amount of LAL formed during the alkali treatment process was measured. The results showed that the alkali treatment resulted in the formation of LAL in the egg white. The LAL content increased with increasing pH and temperature, with the LAL content first increasing and then leveling off with increasing time. The amount of LAL formed in the ovalbumin under the alkali treatment condition accounted for approximately 50.51% to 58.68% of the amount of LAL formed in the egg white. Thus, the LAL formed in the ovalbumin was the main source for the LAL in the egg white during the alkali treatment process. Under the alkali treatment condition, free L-serine, L-cysteine, and L-cystine reacted with L-lysine to form LAL; therefore, they are the precursor amino acids of LAL formed in eggs during the alkali treatment process. © 2016 Poultry Science Association Inc.

  3. Method of making alkali metal hydrides

    Science.gov (United States)

    Pecharsky, Vitalij K.; Gupta, Shalabh; Pruski, Marek; Hlova, Ihor; Castle, Andra

    2017-05-30

    A method is provided for making alkali metal hydrides by mechanochemically reacting alkali metal and hydrogen gas under mild temperature (e.g room temperature) and hydrogen pressure conditions without the need for catalyst, solvent, and intentional heating or cooling.

  4. Red-IR stimulated luminescence in K-feldspar: Single or multiple trap origin?

    DEFF Research Database (Denmark)

    Andersen, Martin Thalbitzer; Jain, Mayank; Tidemand-Lichtenberg, Peter

    2012-01-01

    We investigate on the origins of the infra-red stimulated luminescence (IRSL) signals in 3 potassium feldspars based on IR-red spectroscopy (700–1050 nm) using a fiber-coupled tunable Ti:Sapphire laser, in combination with different thermal and optical (pre)treatments of the samples. We also...

  5. Petrological studies of plutonic rocks of Ecuador

    International Nuclear Information System (INIS)

    Aly, S.

    1980-01-01

    The feldspars of many tonalitic plutonic rocks in the coastal regions and West Andean regions are zoned. This leads to the conclusion that they are relatively flat intrusions and to some extent transition rocks in the subvulcanite direction. This is in accordance with the genetic and chronological relationship between plutonites and the surrounding vulcanites of the Basic Igreous Complex (BIC). The composition of representative minerals, e.g. alkali feldspar, plagioclase feldspar, biotite, chlorite, and amphibole has been determined as well as the age of plutonite samples by the K/Ar dating method. (DG) [de

  6. Relaxation of quadrupole orientation in an optically pumped alkali vapour

    Energy Technology Data Exchange (ETDEWEB)

    Bernabeu, E; Tornos, J

    1985-04-01

    The relaxation of quadrupole orientation (alignment) in an optically pumped alkali vapour is theoretically studied by taking into account the relaxation processes by alkali-buffer gas, alkali-alkali with spin exchange and alkali-cell wall (diffusion process) collisions. The relaxation transients of the quadrupole orientation are obtained by introducing a first-order weak-pumping approximation (intermediate pumping) less restrictive than the usually considered (zeroth order) one.

  7. Determination of Potassium in Feldspars by Beta Counting Using a GM Multicounter System

    DEFF Research Database (Denmark)

    Bøtter-Jensen, Lars; Mejdahl, V.

    1985-01-01

    A gas flow multicounter system developed at Riso National Laboratory for low-level beta counting applications was adopted for measuring potassium in feldspars extracted from archaeological and geological materials, in connection with TL dating work. A guard counter reduces the background by using...

  8. Na-rich feldspar as a luminescence dosimeter in infrared stimulated luminescence (IRSL) dating

    DEFF Research Database (Denmark)

    Sohbati, Reza; Murray, Andrew; Jain, Mayank

    2013-01-01

    on geological origin and erosion history, but the dosimetry of K-rich feldspar grains extracted from rocks is complicated because the internal dose rate is very dependent on the original feldspar grain size. The in situ grain size information is lost during the crushing process used to separate the grains...... settings for which independent age control is available. The blue and yellow luminescence emissions are measured for IR stimulation at 50 °C (IR50), and post-IR IR stimulation at 290 °C (pIRIR290). Thermal stability experiments imply that the corresponding signals in both emissions have comparable thermal...... stabilities and that all signals have similar recombination kinetics and are thermally stable over geological timescales. The IR50 doses measured using blue and yellow emissions are similar to or lower than quartz doses while pIRIR290 blue doses are higher than those from yellow emission and quartz doses...

  9. Milk Alkali and Hydrochlorothiazide: A Case Report

    Directory of Open Access Journals (Sweden)

    Babar Parvez

    2011-01-01

    Full Text Available Hypercalcemia is a relatively common clinical problem in both outpatient and inpatient settings. Primary pathophysiology is the entry of calcium that exceeds its excretion into urine or deposition in bone into circulation. Among a wide array of causes of hypercalcemia, hyperparathyroidism and malignancy are the most common, accounting for greater than 90 percent of cases. Concordantly, there has been a resurgence of milk-alkali syndrome associated with the ingestion of large amounts of calcium and absorbable alkali, making it the third leading cause of hypercalcemia (Beall and Scofield, 1995 and Picolos et al., 2005. This paper centers on a case of over-the-counter calcium and alkali ingestion for acid reflux leading to milk alkali with concordant use of thiazide diuretic for hypertension.

  10. Vibrations of alkali metal overlayers on metal surfaces

    International Nuclear Information System (INIS)

    Rusina, G G; Eremeev, S V; Borisova, S D; Echenique, P M; Chulkov, E V; Benedek, G

    2008-01-01

    We review the current progress in the understanding of vibrations of alkalis adsorbed on metal surfaces. The analysis of alkali vibrations was made on the basis of available theoretical and experimental results. We also include in this discussion our recent calculations of vibrations in K/Pt(111) and Li(Na)/Cu(001) systems. The dependence of alkali adlayer localized modes on atomic mass, adsorption position and coverage as well as the dependence of vertical vibration frequency on the substrate orientation is discussed. The square root of atomic mass dependence of the vertical vibration energy has been confirmed by using computational data for alkalis on the Al(111) and Cu(001) substrates. We have confirmed that in a wide range of submonolayer coverages the stretch mode energy remains nearly constant while the energy of in-plane polarized modes increases with the increase of alkali coverage. It was shown that the spectrum of both stretch and in-plane vibrations can be very sensitive to the adsorption position of alkali atoms and substrate orientation

  11. OSL and IRSL characteristics of quartz and feldspar from southern California, USA

    International Nuclear Information System (INIS)

    Lawson, Michael J.; Roder, Belinda J.; Stang, Dallon M.; Rhodes, Edward J.

    2012-01-01

    Southern California comprises of a wide range of diverse landscapes and environments, from high mountains with glacial and periglacial sediments to deserts with large sand dunes, extensive alluvial fans and ephemeral playas. Highly active tectonic processes has exposed ancient (c. 2 Ga) plutonic and metamorphic basement from deep within the crust, while similar Palaeozoic, Mesozoic and Cenozoic rocks are also common. A rich array of volcanic lithologies extending into the late Quaternary complement many thick sedimentary sequences that formed in equally diverse ancient environments typical of an accreting active continental margin. In some locations, notably in the Coachella Valley close to Palm Springs and the Salton Sea, low OSL sensitivity and poor characteristics restrict the application of the quartz SAR protocol to date late Pleistocene and Holocene fluvial sediments. In other locations such as the Malibu coastline, high sensitivity of the quartz OSL signal is observed, despite local source rocks being dominated by volcanic lithologies. Problems of poor quartz characteristics, along with uncertainty in predicting quartz OSL behavior for future dating campaigns poses a significant problem for projects, in particular for neotectonic contexts. While K-feldspar has been used extensively to date eolian and fluvial sediments in southern California, little information regarding signal stability is available. We explore the characteristics of both quartz and feldspar sub-samples from eolian, fluvial, lacustrine environments, in order to help develop mineral selection criteria for optical dating applications and clarify these issues. The importance of radiation quenching in quartz grains recently eroded from bedrock and the role of fires in enhancing OSL sensitivity are considered. The relative bleachability of quartz and feldspar fractions, along with thermal stability considerations is discussed. A simple test for quartz OSL signal contamination based on thermal

  12. Alkali aggregate reactivity in concrete structures in western Canada

    International Nuclear Information System (INIS)

    Morgan, D.R.; Empey, D.

    1989-01-01

    In several regions of Canada, particularly parts of Ontario, Quebec and the Maritime Provinces, research, testing and evaluation of aged concrete structures in the field has shown that alkali aggregate reactivity can give rise to pronounced concrete deterioration, particularly in hydraulic structures subjected to saturation or alternate wetting and drying such as locks, dams, canals, etc. Concrete deterioration is mainly caused by alkali-silica reactions and alkali-carbonate reactions, but a third type of deterioration involves slow/late expanding alkali-silicate/silica reactivity. The alkalies NaOH and KOH in the concrete pore solutions are mainly responsible for attack on expansive rocks and minerals in concrete. Methods for evaluating alkali-aggregate reaction potential in aggregates, and field and laboratory methods for detecting deterioration are discussed. Examples of alkali-aggregate reactions in structures is western Canada are detailed, including a water reservoir at Canadian Forces Base Chilliwack in British Columbia, the Oldman River diversion and flume, the Lundbreck Falls Bridge, and the St Mary's Reservoir spillway, all in southern Alberta. Mitigative measures include avoidance of use of suspect aggregates, but if this cannot be avoided it is recommended to keep the total alkalies in the concrete as low as possible and minimize opportunities for saturation of concrete by moisture. 16 refs., 19 figs., 1 tab

  13. Further investigations into pulsed optically stimulated luminescence from feldspars using blue and green light

    International Nuclear Information System (INIS)

    Ankjaergaard, C.; Jain, M.; Kalchgruber, R.; Lapp, T.; Klein, D.; McKeever, S.W.S.; Murray, A.S.; Morthekai, P.

    2009-01-01

    The purpose of this paper is to investigate characteristics of luminescence signals resulting from pulsed optical stimulation of feldspars and thereby to understand the underlying processes giving rise to the signal. Fourteen different feldspar specimens were investigated using time-resolved optically stimulated luminescence (TR-OSL), and these signals can be mathematically described as a sum of 4 exponential components (a, b, c, d). The slowest component, d, increases with the duration of the light pulse as expected from the exponential model. The stimulation temperature dependence experiment suggests that the TR-OSL signal decay is governed by the recombination process and not by the excited state lifetime. Furthermore data from the TR-OSL signal dependence on stimulation time and preheat temperature suggest that the recombination process may not be a sum of exponentials, although the model cannot be rejected definitively.

  14. 40 CFR 721.5278 - Substituted naphthalenesulfonic acid, alkali salt.

    Science.gov (United States)

    2010-07-01

    ..., alkali salt. 721.5278 Section 721.5278 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... Specific Chemical Substances § 721.5278 Substituted naphthalenesulfonic acid, alkali salt. (a) Chemical... as a substituted naphthalenesulfonic acid, alkali salt (PMN P-95-85) is subject to reporting under...

  15. 40 CFR 721.8900 - Substituted halogenated pyridinol, alkali salt.

    Science.gov (United States)

    2010-07-01

    ..., alkali salt. 721.8900 Section 721.8900 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... Specific Chemical Substances § 721.8900 Substituted halogenated pyridinol, alkali salt. (a) Chemical... as substituted halogenated pyridinols, alkali salts (PMNs P-88-1271 and P-88-1272) are subject to...

  16. Alkali-activated blast furnace slag-zeolite cements and concretes

    International Nuclear Information System (INIS)

    Rakhimov, R.; Rakhimova, N.

    2012-01-01

    The aim of this work has been the study of alkali-activated slag-zeolite cements and concretes based on them. Various compositions have been tested and some characteristics such as the compressive strength have been measured versus zeolite additions. A table lists the specific surface area and particle size distributions of different cements. The conclusions of the study are the following. First, alkali-activated slag cements and concretes based on them are effective for immobilization of radioactive wastes and the production of building structures, designed for high radiation load. Secondly, zeolite-containing mineral additions are able to increase the immobilization capacity and radiation resistance of alkali-activated blast furnace slag cements and concretes. Thirdly, the efficiency of different zeolite-containing additions - 10% to increase alkali-activated blast furnace slag-zeolite cement strength was established. It is with alkaline components of water-glass, sodium carbonate, sodium sulphate. Fourth, the effective way of introducing zeolite additions in alkali-activated blast furnace slag-zeolite cement is inter-grinding of the slag and addition. Increase in strength of alkali-activated blast furnace slag-zeolite cement stone is 40% higher than that of the stone of a mixture of separately milled components. Fifth, Alkali-activated blast furnace slag-zeolite cements with zeolite-containing additions with a compressive strength of 10.1 to 140 MPa; alkali-activated blast furnace slag-zeolite cements mortars with compressive strength from 35.2 to 97.7 MPa; alkali-activated blast furnace slag-zeolite cements concretes with compressive strength up to 84.5 MPa and frost resistant up to 800 cycles were obtained

  17. FTIR measurements of OH in deformed quartz and feldspars of the South Tibetan Detachment, Greater Himalaya

    Science.gov (United States)

    Jezek, L.; Law, R. D.; Jessup, M. J.; Searle, M. P.; Kronenberg, A. K.

    2017-12-01

    OH absorption bands due to water in deformed quartz and feldspar grains of mylonites from the low-angle Lhotse Detachment (of the South Tibetan Detachment System, Rongbuk Valley north of Mount Everest) have been measured by Fourier Transform Infrared (FTIR) Spectroscopy. Previous microstructural studies have shown that these rocks deformed by dislocation creep at high temperature conditions in the middle crust (lower - middle amphibolite facies), and oxygen isotope studies suggest significant influx of meteoric water. OH absorption bands at 3400 cm-1 of quartz mylonites from the footwall of the Lhotse Detachment Fault are large, with the character of the molecular water band due to fluid inclusions in milky quartz. Mean water contents depend on structural position relative to the core of the Lhotse Detachment, from 1000 ppm (OH/106 Si) at 420 m below the fault to 11,350 (+/-1095) ppm near its center. The gradient in OH content shown by quartz grains implies influx of meteoric water along the Lhotse Detachment from the Tibetan Plateau ground surface to middle crustal depths, and significant fluid penetration into the extruding Himalayan slab by intergranular, permeable fluid flow processes. Feldspars of individual samples have comparable water contents to those of quartz and some are wetter. Large water contents of quartz and feldspar may have contributed to continued deformation and strain localization on the South Tibetan Detachment System. Dislocation creep in quartz is facilitated by water in laboratory experiments, and the water contents of the Lhotse fault rocks are similar to (and even larger than) water contents of quartz experimentally deformed during water weakening. Water contents of feldspars are comparable to those of plagioclase aggregates deformed experimentally by dislocation and diffusion creep under wet conditions.

  18. Characterization of the extent of Mercury Contamination in the Androscoggin River from a former Chlor-alkali Facility, Berlin, New Hampshire

    Science.gov (United States)

    Chalmers, A.; Marvin-Dipasquale, M. C.; Rosiu, C.; Luce, D.; Coles, J.; Zimmerman, M.; Smith, T.

    2010-12-01

    From the late 1800s to the 1960s a chlor-alkali plant was used to produce chlorine gas for the papermaking industry in Berlin, New Hampshire. During operation of the chlor-alkali facility, elemental mercury (Hg) was released to the environment, contaminating soils and the underlying fractured rock. Investigations have revealed that elemental Hg continues to seep through bedrock fractures into the adjacent Androscoggin River. This study evaluates the extent and transformation of Hg contamination in the Androscoggin River by comparing a reference site 17 kilometers above the former chlor-alkali facility to 5 sites ranging from 1 to 16 km downstream from the facility. Total and methyl Hg (THg and MeHg, respectively), among other analytes, were characterized in surface water, pore water, sediment and biological tissue samples at each site. Bed sediment was also assessed for bio-available (tin-reducible) inorganic Hg (II) and microbial MeHg production potential rates. Acid extractable ferrous iron, crystalline and amorphous (poorly crystalline) ferric iron, total reduced sulfur, particle size, and organic content in bed sediment was analyzed to help explain spatial differences in MeHg production rates and bio-available Hg (II) among sites. The information provided by this study will help evaluate the extent of Hg contamination in the Androscoggin River, will improve our understanding of the controls on MeHg production in the Androscoggin River system, and will be used by the U.S. Environmental Protection Agency to support remediation of the chlor-alkali facility site.

  19. Alkali-Resistant Mechanism of a Hollandite DeNOx Catalyst.

    Science.gov (United States)

    Hu, Pingping; Huang, Zhiwei; Gu, Xiao; Xu, Fei; Gao, Jiayi; Wang, Yue; Chen, Yaxin; Tang, Xingfu

    2015-06-02

    A thorough understanding of the deactivation mechanism by alkalis is of great importance for rationally designing improved alkali-resistant deNOx catalysts, but a traditional ion-exchange mechanism cannot often accurately describe the nature of the deactivation, thus hampering the development of superior catalysts. Here, we establish a new exchange-coordination mechanism on the basis of the exhaustive study on the strong alkali resistance of a hollandite manganese oxide (HMO) catalyst. A combination of isothermal adsorption measurements of ammonia with X-ray absorption near-edge structure spectra and X-ray photoelectron spectra reveals that alkali metal ions first react with protons from Brønsted acid sites of HMO via the ion exchange. Synchrotron X-ray diffraction patterns and extended X-ray absorption fine structure spectra coupled with theoretical calculations demonstrate that the exchanged alkali metal ions are subsequently stabilized at size-suitable cavities in the HMO pores via a coordination model with an energy savings. This exchange-coordination mechanism not only gives a wholly convincing explanation for the intrinsic nature of the deactivation of the reported catalysts by alkalis but also provides a strategy for rationally designing improved alkali-resistant deNOx catalysts in general.

  20. Comparison of the properties of various optically stimulated luminescence signals from potassium feldspar

    International Nuclear Information System (INIS)

    Fu Xiao; Zhang Jiafu; Zhou Liping

    2012-01-01

    Various optically stimulated luminescence signals from K-feldspar have been used to determine the equivalent doses of sediment samples. Understanding the properties of these optical signals is critical to evaluate their applicability and limitations to optical dating. In this paper, some properties of IRSL, post-IR OSL and post-IR IRSL signals (detected in the UV region using U-340 filters) from a museum sample of K-feldspar were investigated by analyzing the relationships between optical and TL signals, and the effect of optical bleaching and heating on optical signals. The trap parameters of the different optical signals were calculated using the pulse annealing method. The results show that this sample exhibits two regenerated TL peaks at ∼140 and ∼330 °C. Corresponding to the low temperature TL peak, the OSL and post-IR OSL signals appear to be more associated with lower temperature TL than the IRSL signal measured at 50 °C. Corresponding to the high temperature TL peak, the post-IR IRSL signals mainly originate from the more thermally stable traps associated with the high temperature TL, compared with the IRSL and post-IR OSL signals. However, the post-IR IRSL 225°C signal is shown to be hard to be bleached by blue light and simulated sunlight, compared with the IRSL 50°C and low temperature post-IR IRSL signals. The implication for optical dating is that the elevated temperature post-IR IRSL signals can be preferentially applied over other signals from K-feldspar, but it is desirable that the effectiveness of the pre-depositional zeroing of these signals is assessed.

  1. [Enhancement of anaerobic digestion of excess sludge by acid-alkali pretreatment].

    Science.gov (United States)

    Yuan, Guang-Huan; Zhou, Xing-Qiu; Wu, Jian-Dong

    2012-06-01

    In order to enhance the efficiency of anaerobic digestion of excess sludge, acid-alkali pretreatment method was studied. Three different pretreatment methods (alkali alone,acid-alkali, alkali-acid) were compared to investigate their impacts on hydrolysis and acidification of activated sludge. In addition, their influences on methane-producing in subsequent anaerobic digestion process were also studied. The results showed that the soluble chemical oxygen demand (SCOD) of alkaline treatment alone was about 16% higher than the combining of acid and alkali treatment, SCOD concentration increased to 5406.1 mg x L(-1) after 8 d pretreatment. After treated by acid (pH 4.0, 4 d) and alkali (pH 10.0, 4 d), the acetic acid production and its content in short-chain fatty acids (SCFAs) were higher than other pretreatment methods. And the acetic acid production (as COD/VSS) could reach 74.4 mg x g(-1), accounting for 60.5% of SCFAs. After acid-alkali pretreatment, the C: N ratio of the sludge mixed liquor was about 25, and the C: P ratio was between 35-40, which was more favorable than C: N and C: P ratio of alkali alone and alkali-acid to subsequent anaerobic digestion. The control experiments showed that, after acid-alkali pretreatment, anaerobic digestion cumulative methane yield (CH4/VSS(in)) reached to 136.1 mL x g(-1) at 15 d, which was about 2.5-, 1.6-, and 1.7-fold of the blank (unpretreated), alkali alone pretreatment and alkali-acid pretreatment, respectively. After acid-alkali pretreatment for 8 d and anaerobic digestion for 15 d, the removal efficiency of VSS was about 60.9%, and the sludge reduction effect was better than other pretreatments. It is obvious that the acid-alkali pretreatment method was more favorable to anaerobic digestion and sludge reduction.

  2. 40 CFR 721.1878 - Alkali metal alkyl borohydride (generic).

    Science.gov (United States)

    2010-07-01

    ... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Alkali metal alkyl borohydride... Specific Chemical Substances § 721.1878 Alkali metal alkyl borohydride (generic). (a) Chemical substance... alkali metal alkyl borohydride (PMN P-00-1089) is subject to reporting under this section for the...

  3. Concrete alkali-silica reaction and nuclear radiation damage

    International Nuclear Information System (INIS)

    Ichikawa, Tsuneki

    2008-01-01

    The deterioration of concrete by alkali-silica reaction of aggregates (ASR) and the effect of nuclear radiations on the ASR have been reviewed based on our studies on the mechanism of ASR and the effect of nuclear radiations on the resistivity of minerals to alkaline solution. It has been found that the ASR is initiated by the attack of alkaline solution in concrete to silicious aggregates to convert them into hydrated alkali silicate. The consumption of alkali hydroxide by the aggregates induces the dissolution of Ca 2+ ions into the solution. The alkali silicate surrounding the aggregates then reacts with Ca 2+ ions to convert to insoluble tight and rigid reaction rims. The reaction rim allows the penetration of alkaline solution but prevents the leakage of viscous alkali silicate, so that alkali silicate generated afterward is accumulated in the aggregate to give an expansive pressure enough for cracking the aggregate and the surrounding concrete. The effect of nuclear radiation on the reactivity of quartz and plagioclase, a part of major minerals composing volcanic rocks as popular aggregates, to alkaline solution has been examined for clarifying whether nuclear radiations accelerates the ASR. It has been found that the irradiation of these minerals converts them into alkali-reactive amorphous ones. The radiation dose for plagioclase is as low as 10 8 Gy, which suggests that the ASR of concrete surrounding nuclear reactors is possible to be accelerated by nuclear radiation. (author)

  4. The utilization of alkali-treated melon husk by broilers.

    Science.gov (United States)

    Abiola, S S; Amalime, A C; Akadiri, K C

    2002-09-01

    The effects of alkali treatment on chemical constituents of melon husk (MH) and performance characteristics of broilers fed alkali-treated MH (ATMH) diets were investigated. The chemical analysis showed that alkali treatment increased the ash content of MH (from 15.70% to 16.86%) and reduced the crude fibre content (from 29.00% to 14.00%). Result of feed intake was superior on 30% alkali diet with a value of 100.14 g/bird/day. Body weight gain decreased with increase in the level of ATMH in the diet. Highest dressing percentage of 66.33% and best meat/bone ratio of 2.57 were obtained on 10% and 20% alkali diets, respectively. Dietary treatments had significant effect (P poultry carcases and chicken meat with favourable shelf life.

  5. Chemical Zoning of Feldspars in Lunar Granitoids: Implications for the Origins of Lunar Silicic Magmas

    Science.gov (United States)

    Mills, R. D; Simon, J. I.; Alexander, C.M. O'D.; Wang, J.; Christoffersen, R.; Rahman, Z..

    2014-01-01

    Fine-scale chemical and textural measurements of alkali and plagioclase feldspars in the Apollo granitoids (ex. Fig. 1) can be used to address their petrologic origin(s). Recent findings suggest that these granitoids may hold clues of global importance, rather than of only local significance for small-scale fractionation. Observations of morphological features that resemble silicic domes on the unsampled portion of the Moon suggest that local, sizable net-works of high-silica melt (>65 wt % SiO2) were present during crust-formation. Remote sensing data from these regions suggest high concentrations of Si and heat-producing elements (K, U, and Th). To help under-stand the role of high-silica melts in the chemical differentiation of the Moon, three questions must be answered: (1) when were these magmas generated?, (2) what was the source material?, and (3) were these magmas produced from internal differentiation. or impact melting and crystallization? Here we focus on #3. It is difficult to produce high-silica melts solely by fractional crystallization. Partial melting of preexisting crust may therefore also have been important and pos-sibly the primary mechanism that produced the silicic magmas on the Moon. Experimental studies demonstrate that partial melting of gabbroic rock under mildly hydrated conditions can produce high-silica compositions and it has been suggested by that partial melting by basaltic underplating is the mechanism by which high-silica melts were produced on the Moon. TEM and SIMS analyses, coordinated with isotopic dating and tracer studies, can help test whether the minerals in the Apollo granitoids formed in a plutonic setting or were the result of impact-induced partial melting. We analyzed granitoid clasts from 3 Apollo samples: polymict breccia 12013,141, crystalline-matrix breccia 14303,353, and breccia 15405,78

  6. [Raman spectra of endospores of Bacillus subtilis by alkali stress].

    Science.gov (United States)

    Dong, Rong; Lu, Ming-qian; Li, Feng; Shi, Gui-yu; Huang, Shu-shi

    2013-09-01

    To research the lethal mechanism of spores stressed by alkali, laser tweezers Raman spectroscopy (LTRS) combined with principal components analysis (PCA) was used to study the physiological process of single spore with alkali stress. The results showed that both spores and germinated spores had tolerance with alkali in a certain range, but the ability of spores was obviously lower than that of spores due to the release of their Ca2+ -DPA which plays a key role in spores resistance as well as spores resistance to many stresses; A small amount of Ca2+ -DPA of spores was observed to release after alkali stress, however, the behavior of release was different with the normal Ca2+ -DPA release behavior induced by L-alanine; The data before and after alkali stress of the spores and g. spores with PCA reflected that alkali mainly injured the membrane of spores, and alkali could be easily enter into the inner structure of spores to damage the structure of protein backbone and injure the nucleic acid of spores. We show that the alkali could result in the small amount of Ca2+ -DPA released by destroying the member channel of spores.

  7. A coupled channel study on a binding mechanism of positronic alkali atoms

    International Nuclear Information System (INIS)

    Kubota, Yoshihiro; Kino, Yasushi

    2008-01-01

    In order to investigate the binding mechanism of weakly bound states of positronic alkali atoms, we calculate the energies and wavefunctions using the Gaussian expansion method (GEM) where a positronium (Ps)-alkali ion channel and a positron-alkali atom channel are explicitly introduced. The energies of the bound states are updated using a model potential that reproduces well the observed energy levels of alkali atoms. The binding mechanism of the positronic alkali atom is analyzed by the wavefunctions obtained. The structure of the positronic alkali atom has been regarded as a Ps cluster orbiting the alkali ion, which is described by the Ps-alkali ion channel. We point out that the fraction having the positron-alkali atom configuration is small but plays an indispensable role for the weakly bound system

  8. IRMPD Action Spectroscopy of Alkali Metal Cation-Cytosine Complexes: Effects of Alkali Metal Cation Size on Gas Phase Conformation

    NARCIS (Netherlands)

    Yang, B.; Wu, R.R.; Polfer, N.C.; Berden, G.; Oomens, J.; Rodgers, M.T.

    2013-01-01

    The gas-phase structures of alkali metal cation-cytosine complexes generated by electrospray ionization are probed via infrared multiple photon dissociation (IRMPD) action spectroscopy and theoretical calculations. IRMPD action spectra of five alkali metal cation-cytosine complexes exhibit both

  9. Alkali absorption and citrate excretion in calcium nephrolithiasis

    Science.gov (United States)

    Sakhaee, K.; Williams, R. H.; Oh, M. S.; Padalino, P.; Adams-Huet, B.; Whitson, P.; Pak, C. Y.

    1993-01-01

    The role of net gastrointestinal (GI) alkali absorption in the development of hypocitraturia was investigated. The net GI absorption of alkali was estimated from the difference between simple urinary cations (Ca, Mg, Na, and K) and anions (Cl and P). In 131 normal subjects, the 24 h urinary citrate was positively correlated with the net GI absorption of alkali (r = 0.49, p origin of hypocitraturia. However, the normal dependence was maintained in CDS and in idiopathic hypocitraturia, suggesting that reduced citrate excretion was largely dietary in origin as a result of low net alkali absorption (from a probable relative deficiency of vegetables and fruits or a relative excess of animal proteins).

  10. The 4843 Alkali Metal Storage Facility Closure Plan

    International Nuclear Information System (INIS)

    1991-06-01

    The 4843 AMSF has been used primarily to provide a centralized building to receive and store dangerous and mixed alkali metal waste, including sodium and lithium, which has been generated at the Fast Flux Test Facility and at various other Hanford Site operations that used alkali metals. Most of the dangerous and mixed alkali metal waste received consists of retired equipment from liquid sodium processes. The unit continues to store material. In general, only solid alkali metal waste that is water reactive is stored at the 4843 AMSF. The 4843 AMSF will be closed in a manner consistent with Ecology guidelines and regulations (WAC 173-303-610). The general closure procedure is detailed as follows

  11. On-line alkali monitoring - Part 1; Kontinuerlig alkalimaetning - Etapp 1

    Energy Technology Data Exchange (ETDEWEB)

    Andersson, Christer; Ljung, P; Woxlin, H

    1997-02-01

    As a consequence of the increased knowledge of the environmental impact of combustion based heat and power generation, the use of renewable biofuels will be increased. An obstacle associated to biofuel combustion compared to other fuels is the large release of alkali. Alkali compounds in flue gases are known to cause severe operational problems. Three of the major problems are; fouling of superheating tubes (causing reduced heat transfer and possibly corrosion), agglomeration of the bed material in fluidized beds, and poisoning of SCR catalysts. Yet another alkali related problem arises when, in order to increase the electric efficiency of combustion power plants, combined-cycle technology is used. Alkali vapour present in the fuel gas for the gas turbine is condensed to particles which increase corrosion and erosion of the turbine blades. The research on ash related operational problems has to be extended in order to ensure future use of biofuels in heat and power generation. In all successful research, adequate tools are necessary. To investigate ash related problems the key issue is to be able to perform continuous alkali measurements. This pilot study has investigated the need of continuous alkali measurements, which alkali species are harmful in the different applications and also available instrumentation capable of measuring the specific alkali species. The report gives a short summary presenting alkali related operational problems. In addition a schematic overview is given, showing the alkali species that possibly can exist in various parts of the power plant. 48 refs, 13 figs, 4 tabs

  12. Salts of alkali metal anions and process of preparing same

    Science.gov (United States)

    Dye, James L.; Ceraso, Joseph M.; Tehan, Frederick J.; Lok, Mei Tak

    1978-01-01

    Compounds of alkali metal anion salts of alkali metal cations in bicyclic polyoxadiamines are disclosed. The salts are prepared by contacting an excess of alkali metal with an alkali metal dissolving solution consisting of a bicyclic polyoxadiamine in a suitable solvent, and recovered by precipitation. The salts have a gold-color crystalline appearance and are stable in a vacuum at -10.degree. C. and below.

  13. Mineralogical, micromorphological and geochemical transformations in the initial steps of the weathering process of charnockite from the Caparaó Range, southeastern Brazil

    Science.gov (United States)

    Soares, Caroline Cibele Vieira; Varajão, Angélica Fortes Drummond Chicarino; Varajão, César Augusto Chicarino; Boulangé, Bruno

    2014-12-01

    X-ray diffraction (XRD), X-ray Fluorescence (XRF), optical microscopy, Scanning Electron Microscopy coupled with Energy Dispersive Spectrometry (SEM-EDS) and Electron Probe micro-analyser (EPMA) and Wavelength-Dispersive Spectroscopy (WDS) were conducted on charnockite from the Caparaó Suite and its alteration cortex to determine the mineralogical, micromorphological and geochemical transformations resulting from the weathering process. The hydrolysis of the charnockite occurred in different stages, in accordance with the order of stability of the minerals with respect to weathering: andesine/orthopyroxene, pargasite and alkali feldspar. The rock modifications had begun with the formation of a layer of incipient alteration due to the percolation of weathering solutions first in the pressure relief fractures and then in cleavage and mineral edges. The iron exuded from ferromagnesian minerals precipitated in the intermineral and intramineral discontinuities. The layer of incipient alteration evolves into an inner cortex where the plagioclase changes into gibbsite by direct alitisation, the ferromagnesian minerals initiate the formation of goethitic boxworks with kaolinitic cores, and the alkali feldspar initiates indirect transformation into gibbsite, forming an intermediate phase of illite and kaolinite. In the outer cortex, mostly traces of alkali feldspar remain, and they are surrounded by goethite and gibbsite as alteromorphics, characterising the formation of the isalteritic horizon that occurs along the slope and explains the bauxitization process at the Caparaó Range, SE Brazil.

  14. Two-phase alkali-metal experiments in reduced gravity

    International Nuclear Information System (INIS)

    Antoniak, Z.I.

    1986-06-01

    Future space missions envision the use of large nuclear reactors utilizing either a single or a two-phase alkali-metal working fluid. The design and analysis of such reactors require state-of-the-art computer codes that can properly treat alkali-metal flow and heat transfer in a reduced-gravity environment. A literature search of relevant experiments in reduced gravity is reported on here, and reveals a paucity of data for such correlations. The few ongoing experiments in reduced gravity are noted. General plans are put forth for the reduced-gravity experiments which will have to be performed, at NASA facilities, with benign fluids. A similar situation exists regarding two-phase alkali-metal flow and heat transfer, even in normal gravity. Existing data are conflicting and indequate for the task of modeling a space reactor using a two-phase alkali-metal coolant. The major features of past experiments are described here. Data from the reduced-gravity experiments with innocuous fluids are to be combined with normal gravity data from the two-phase alkali-metal experiments. Analyses undertaken here give every expectation that the correlations developed from this data base will provide a valid representation of alkali-metal heat transfer and pressure drop in reduced gravity

  15. High alkali-resistant basalt fiber for reinforcing concrete

    International Nuclear Information System (INIS)

    Lipatov, Ya.V.; Gutnikov, S.I.; Manylov, M.S.; Zhukovskaya, E.S.; Lazoryak, B.I.

    2015-01-01

    Highlights: • Doping of basalt fiber with ZrSiO 4 increased its alkali resistance. • Alkali treatment results in formation of protective surface layer on fibers. • Morphology and chemical composition of surface layer were investigated. • Mechanical properties of fibers were analyzed by a Weibull distribution. • Zirconia doped basalt fibers demonstrate high performance in concrete. - Abstract: Basalt glasses and fibers with zirconia content in the range from 0 to 7 wt% were obtained using ZrSiO 4 as a zirconium source. Weight loss and tensile strength loss of fibers after refluxing in alkali solution were determined. Basalt fiber with 5.7 wt% ZrO 2 had the best alkali resistance properties. Alkali treatment results in formation of protective surface layer on fibers. Morphology and chemical composition of surface layer were investigated. It was shown that alkali resistance of zirconia doped basalt fibers is caused by insoluble compounds of Zr 4+ , Fe 3+ and Mg 2+ in corrosion layer. Mechanical properties of initial and leached fibers were evaluated by a Weibull distribution. The properties of basalt fibers with ZrSiO 4 were compared with AR-glass fibers. The performance of concrete with obtained fibers was investigated

  16. Removal of Copper (II Ions in Aqueous Solutions by Sorption onto Alkali Activated Fly Ash

    Directory of Open Access Journals (Sweden)

    Darmayanti Lita

    2018-01-01

    Full Text Available Fly ash is a particulate material produced from coal combustion power plants with major components are silica, alumina, iron oxide, calcium oxide, magnesium oxide, and carbon which are ideal for metal adsorbents. The potential use of fly ash in the wastewater treatment process is obvious because it can be obtained cheaply in large quatities and it can be used as an adsorbent. However, fly ash still shows lower adsorption capacity unless it is activated. In this study, fly ash activated by NaOH 14 M and KOH 14 M solutions. The batch experiments were carried out to study the sorption of copper ions from aqueous on alkali activated fly ash. The influence of initial concentration and contact time were examined at constant pH and dose of adsorbent. The sorption capacity of copper ions increased with the initial concentration and contact time. The sorption capacities followed the order Na1>Ka1>FA. The adsorption isotherm model exhibited that the Langmuir model is very suitable with copper ions adsorption onto fly ash and alkali activated fly ash. Kinetic study shows that adsorption of copper ions onto FA, Na1, and Ka1 follows the pseudo second-order kinetics.

  17. Upgrading platform using alkali metals

    Science.gov (United States)

    Gordon, John Howard

    2014-09-09

    A process for removing sulfur, nitrogen or metals from an oil feedstock (such as heavy oil, bitumen, shale oil, etc.) The method involves reacting the oil feedstock with an alkali metal and a radical capping substance. The alkali metal reacts with the metal, sulfur or nitrogen content to form one or more inorganic products and the radical capping substance reacts with the carbon and hydrogen content to form a hydrocarbon phase. The inorganic products may then be separated out from the hydrocarbon phase.

  18. Validating post IR-IRSL dating on K-feldspars through comparison with quartz OSL ages

    NARCIS (Netherlands)

    Kars, R.H.; Busschers, F.S.; Wallinga, J.

    2012-01-01

    Recent developments have opened up the possibilities of using potassium feldspar for dating Pleistocene sediments; a stable (less-fading) part of the infrared stimulated luminescence (IRSL) signal can be selected by largely depleting the unstable part of the IR signal, using a combination of thermal

  19. Dependence of (anomalous) fading of infra-red stimulated luminescence on trap occupancy in feldspars

    DEFF Research Database (Denmark)

    Morthekai, P.; Jain, Mayank; Gach, Grzegorz

    2013-01-01

    Dose dependency of anomalous fading of infra-red stimulated luminescence (IRSL) from feldspars has been investigated using radiations of different ionisation qualities. The rate of fading of the IRSL signal after proton irradiation (9.4–30%/decade) is on an average almost twice compared...

  20. Alkali-slag cements for the immobilization of radioactive wastes

    International Nuclear Information System (INIS)

    Shi, C.; Day, R.L.

    1996-01-01

    Alkali-slag cements consist of glassy slag and an alkaline activator and can show both higher early and later strengths than Type III Portland cement, if a proper alkaline activator is used. An examination of microstructure of hardened alkali-slag cement pastes with the help of XRD and SEM with EDAX shows that the main hydration product is C-S-H (B) with low C/S ratio and no crystalline substances exist such as Ca(OH) 2 , Al (OH) 3 and sulphoaluminates. Mercury intrusion tests indicate that hardened alkali-slag cement pastes have a lower porosity than ordinary Portland cement, and contain mainly gel pores. The fine pore structure of hardened alkali-slag cement pastes will restrict the ingress of deleterious substances and the leaching of harmful species such as radionuclides. The leachability of Cs + from hardened alkali-slag cement pastes is only half of that from hardened Portland cement. From all these aspects, it is concluded that alkali-slag cements are a better solidification matrix than Portland cement for radioactive wastes

  1. Saccharification of gamma-ray and alkali pretreated lignocellulosics

    International Nuclear Information System (INIS)

    Begum, A.; Choudhury, N.

    1988-01-01

    Enzymic saccharification of gamma ray and alkali pretreated sawdust, rice straw, and sugar cane bagasse showed higher release of reducing sugar from pretreated substrates. By gamma ray treatment alone (500 kGy) reducing sugar release of 2.8, 9.2, and 10 g/l was obtained from 7.5% (w/v) sawdust, rice straw, and bagasse and the same substrates showed reducing sugar release of 4.2, 30, and 20 g/l respectively when treated with alkali (0.1 g/g). Combination of gamma ray with alkali treatment further increased the reducing sugar release to 10.2, 33, and 36 g/l from sawdust, rice straw, and bagasse respectively. The effects of gamma ray and alkali treatment on saccharification varied with the nature of the substrate

  2. The alkali halide disk technique in infra-red spectrometry : Anomalous behaviour of some samples dispersed in alkali halide disks

    NARCIS (Netherlands)

    Tolk, A.

    1961-01-01

    Some difficulties encountered in the application of the alkali halide disk technique in infra-red spectrometry are discussed. Complications due to interaction of the sample with the alkali halide have been studied experimentally. It was found that the anomalous behaviour of benzoic acid, succinic

  3. Complexes in polyvalent metal - Alkali halide melts

    International Nuclear Information System (INIS)

    Akdeniz, Z.; Tosi, M.P.

    1991-03-01

    Experimental evidence is available in the literature on the local coordination of divalent and trivalent metal ions by halogens in some 140 liquid mixtures of their halides with alkali halides. After brief reference to classification criteria for main types of local coordination, we focus on statistical mechanical models that we are developing for Al-alkali halide mixtures. Specifically, we discuss theoretically the equilibrium between (AlF 6 ) 3- and (AlF 4 ) - complexes in mixtures of AlF 3 and NaF as a function of composition in the NaF-rich region, the effect of the alkali counterion on this equilibrium, the possible role of (AlF 5 ) 2- as an intermediate species in molten cryolite, and the origin of the different complexing behaviours of Al-alkali fluorides and chlorides. We also present a theoretical scenario for processes of structure breaking and electron localization in molten cryolite under addition of sodium metal. (author). 26 refs, 2 tabs

  4. Long term mechanical properties of alkali activated slag

    Science.gov (United States)

    Zhu, J.; Zheng, W. Z.; Xu, Z. Z.; Leng, Y. F.; Qin, C. Z.

    2018-01-01

    This article reports a study on the microstructural and long-term mechanical properties of the alkali activated slag up to 180 days, and cement paste is studied as the comparison. The mechanical properties including compressive strength, flexural strength, axis tensile strength and splitting tensile strength are analyzed. The results showed that the alkali activated slag had higher compressive and tensile strength, Slag is activated by potassium silicate (K2SiO3) and sodium hydroxide (NaOH) solutions for attaining silicate modulus of 1 using 12 potassium silicate and 5.35% sodium hydroxide. The volume dosage of water is 35% and 42%. The results indicate that alkali activated slag is a kind of rapid hardening and early strength cementitious material with excellent long-term mechanical properties. Single row of holes block compressive strength, single-hole block compressive strength and standard solid brick compressive strength basically meet engineering requirements. The microstructures of alkali activated slag are studied by X-ray diffraction (XRD). The hydration products of alkali-activated slag are assured as hydrated calcium silicate and hydrated calcium aluminate.

  5. Ternary alkali-metal and transition metal or metalloid acetylides as alkali-metal intercalation electrodes for batteries

    Science.gov (United States)

    Nemeth, Karoly; Srajer, George; Harkay, Katherine C; Terdik, Joseph Z

    2015-02-10

    Novel intercalation electrode materials including ternary acetylides of chemical formula: A.sub.nMC.sub.2 where A is alkali or alkaline-earth element; M is transition metal or metalloid element; C.sub.2 is reference to the acetylide ion; n is an integer that is 0, 1, 2, 3 or 4 when A is alkali element and 0, 1, or 2 when A is alkaline-earth element. The alkali elements are Lithium (Li), Sodium (Na), Potassium (K), Rubidium (Rb), Cesium (Cs) and Francium (Fr). The alkaline-earth elements are Berilium (Be), Magnesium (Mg), Calcium (Ca), Strontium (Sr), Barium (Ba), and Radium (Ra). M is a transition metal that is any element in groups 3 through 12 inclusive on the Periodic Table of Elements (elements 21 (Sc) to element 30 (Zn)). In another exemplary embodiment, M is a metalloid element.

  6. Alkali metals and group IIA metals

    International Nuclear Information System (INIS)

    Fenton, D.E.

    1987-01-01

    This chapter on the coordination complexes of the alkali metals of group IIA starts with a historical perspective of their chemistry, from simple monodentate ligands, metal-β-diketonates to the macrocyclic polyethers which act as ligands to the alkali and akaline earth metals. Other macrocyclic ligands include quarterenes, calixarenes, porphyrins, phthalocyanines and chlorophylls. A section on the naturally occurring ionophores and carboxylic ionophores is included. (UK)

  7. Mechanical filter for alkali atoms

    CERN Document Server

    Toporkov, D K

    2000-01-01

    A device for separating gases of different mass is discussed. Such a device could be used in a laser-driven spin exchange source of polarized hydrogen atoms to reduce the contamination of alkali atoms. A Monte Carlo simulation has shown that the suggested apparatus based on a commercial turbo pump could reduce by a factor of 10-15 the concentration of the alkali-metal atoms in the hydrogen flow from a laser driven polarized source. This would greatly enhance the effective polarization in hydrogen targets.

  8. The influence of alkali promoters on coadsorbed molecules

    International Nuclear Information System (INIS)

    Umbach, E.

    1986-01-01

    A model has been suggested recently based on the results of an extensive study of the coadsorbate system CO + K on Ru(001). It is introduced and discussed in this article based on previous results and on results obtained very recently for a similar coadsorbate system, CO + K/Ni(111). This model is in competition with a variety of differing or similar ideas and interpretations which are mostly based on similar experimental results. Some of these other models postulate a lying-down, or strongly tilted, molecule in the presence of alkali atoms, at least at low coverages. The CO molecule is usually considered to be attached to the substrate and to be closely coadsorbed to the alkali neighbor(s) but sometimes even a vertical or horizontal adsorption on top of the alkali layer has been suggested. The interaction between alkali and CO has been described as indirect via the substrate or direct by forming a ''π''-bond between adjacent alkalis and CO molecules or even by forming an ionic K/sub x/-CO/sub y/ complex. Some authors prefer a model in which the main (or exclusive) interaction comes from a charge transfer from the donating alkali into the 2π orbital of the coadsorbed CO, thus, enhancing the C- metal and reducing the C-O bond strength

  9. Alkali-heat treatment of a low modulus biomedical Ti-27Nb alloy

    International Nuclear Information System (INIS)

    Zhou, Y; Wang, Y B; Zhang, E W; Cheng, Y; Xiong, X L; Zheng, Y F; Wei, S C

    2009-01-01

    This study focuses on the surface modification of a near β-type Ti-27 wt.% Nb alloy by alkali-heat treatment. The influence of alkali concentration, alkali-treated time and alkali-treated temperature on the microstructure and constitutional phases of the modified surface is investigated by SEM, XRD and ICP. Immersion experiments in a simulated body fluid (SBF) were carried out to examine the Ca-P phase forming ability of the modified surfaces. The SEM observation and XRD analysis revealed that a sodium titanate layer is formed after alkali-heat treatment. The morphology and Ca-P phase forming of the layer are greatly affected by the surface roughness of the samples, the alkali concentration, the alkali-treated time and alkali-treated temperature. The results of SBF immersion, which are obtained by ICP analysis, indicate that the activated sodium titanate layer prepared by alkali-heat treatment is beneficial to further improving the biocompatibility of the Ti-27 wt.% Nb alloy.

  10. Luminescence from potassium feldspars stimulated by infrared and green light

    DEFF Research Database (Denmark)

    Duller, G.A.T.; Bøtter-Jensen, L.

    1993-01-01

    A series of experiments are reported which investigate stimulated luminescence from potassium feldspar. The aim is to provide a basic phenomenological description of the response of the material to stimulation by heat, infrared radiation (875 DELTA 80 nm) and a green light wavelength band from 5 15...... to 560 nm. Two conclusions are drawn: firstly it is suggested that the majority of the trapped charge responsible for the infrared stimulated luminescence signal does not give rise to a thermoluminescence signal, and secondly that a large traction of the two optically stimulated luminescence signals...

  11. Process for the disposal of alkali metals

    International Nuclear Information System (INIS)

    Lewis, L.C.

    1977-01-01

    Large quantities of alkali metals may be safely reacted for ultimate disposal by contact with a hot concentrated caustic solution. The alkali metals react with water in the caustic solution in a controlled reaction while steam dilutes the hydrogen formed by the reaction to a safe level. 6 claims

  12. Developing a numerical simulation for fading in feldspar

    International Nuclear Information System (INIS)

    Larsen, A.; Greilich, S.; Jain, M.; Murray, A.S.

    2009-01-01

    Most models describing anomalous fading in feldspars are based on analytical solutions. As an alternative approach we present an entirely numerical model based on statistical sampling that simulates stepwise the charge creation/trapping and recombination in a given phosphor. We assume the number density of electrons and holes at any time to be equal, although the model is not bound to that assumption. The model is flexible enough to be used on any combination of geological and laboratory timescales and for any defined configuration of defects. Using this approach we observed reorganization of nearest-neighbor distances with time. The best agreement with experimental data is achieved if we assume the crystal to consist of small subvolumes (nanocrystals) only within which charge carriers are allowed to recombine.

  13. Thermodynamic modelling of alkali-activated slag cements

    International Nuclear Information System (INIS)

    Myers, Rupert J.; Lothenbach, Barbara; Bernal, Susan A.; Provis, John L.

    2015-01-01

    Highlights: • A thermodynamic modelling analysis of alkali-activated slag cements is presented. • Thermodynamic database describes zeolites, alkali carbonates, C–(N–)A–S–H gel. • Updated thermodynamic model for Mg–Al layered double hydroxides. • Description of phase assemblages in Na 2 SiO 3 - and Na 2 CO 3 -activated slag cements. • Phase diagrams for NaOH-activated and Na 2 SiO 3 -activated slag cements are simulated. - Abstract: This paper presents a thermodynamic modelling analysis of alkali-activated slag-based cements, which are high performance and potentially low-CO 2 binders relative to Portland cement. The thermodynamic database used here contains a calcium (alkali) aluminosilicate hydrate ideal solid solution model (CNASH-ss), alkali carbonate and zeolite phases, and an ideal solid solution model for a hydrotalcite-like Mg–Al layered double hydroxide phase. Simulated phase diagrams for NaOH- and Na 2 SiO 3 -activated slag-based cements demonstrate the high stability of zeolites and other solid phases in these materials. Thermodynamic modelling provides a good description of the chemical compositions and types of phases formed in Na 2 SiO 3 -activated slag cements over the most relevant bulk chemical composition range for these cements, and the simulated volumetric properties of the cement paste are consistent with previously measured and estimated values. Experimentally determined and simulated solid phase assemblages for Na 2 CO 3 -activated slag cements were also found to be in good agreement. These results can be used to design the chemistry of alkali-activated slag-based cements, to further promote the uptake of this technology and valorisation of metallurgical slags

  14. Mineralization dynamics of metakaolin-based alkali-activated cements

    International Nuclear Information System (INIS)

    Gevaudan, Juan Pablo; Campbell, Kate M.; Kane, Tyler J.; Shoemaker, Richard K.; Srubar, Wil V.

    2017-01-01

    This paper investigates the early-age dynamics of mineral formation in metakaolin-based alkali-activated cements. The effects of silica availability and alkali content on mineral formation were investigated via X-ray diffraction and solid-state 29 Si magic-angle spinning nuclear magnetic resonance spectroscopy at 2, 7, 14, and 28 days. Silica availability was controlled by using either liquid- (immediate) or solid-based (gradual) sodium silicate supplements. Mineral (zeolitic) and amorphous microstructural characteristics were correlated with observed changes in bulk physical properties, namely shrinkage, density, and porosity. Results demonstrate that, while alkali content controls the mineralization in immediately available silica systems, alkali content controls the silica availability in gradually available silica systems. Immediate silica availability generally leads to a more favorable mineral formation as demonstrated by correlated improvements in bulk physical properties.

  15. Alkali and heavy metal emissions of the PCFB-process; Alkalipaeaestoet PCFB-prosessissa

    Energy Technology Data Exchange (ETDEWEB)

    Kuivalainen, R.; Eriksson, T.; Lehtonen, P. [Foster Wheeler Energia Oy, Karhula (Finland)

    1996-12-01

    Pressurized Circulating Fluidized Bed (PCFB) combustion technology has been developed in Karhula R and D Center since 1986. As a part of the development, 10 MW PCFB Test Facility was built in 1989. The Test Facility has been used for performance testing with different coal types through the years 1990-1995 in order to gain data for design and commercialization of the high-efficiency low-emission PCFB combustion technology. The project Y44 `Alkali and heavy metal emissions of the PCFB-process` was part of national LIEKKI 2 research program. The main object of the project was to measure vapor phase Na and K concentrations in the PCFB flue gas after hot gas filter and investigate the effects of process conditions and sorbents on alkali release. The measurements were performed using plasma assisted method by TUT Laboratory of Plasma Technology and wet absorption method of VTT Energy. The measured Na concentrations were below 30 ppb(w) in all measured data points. The results of K were below 10 ppb(w). The accuracies of the both methods are about + 50 % at this concentration range. The scatter of the data covers the effects of different process variables on the alkali emission. The measured emissions are at the same order of magnitude as the guideline emission limits estimated by gas turbine manufacturers. The measurements and development of the analyses methods are planned to be continued during PCFB test runs in spring 1996 for example within Joule II research program. (author)

  16. Use of rice straw ash as substitute of feldspar in triaxial porcelain; Cenizas del tamo de arroz como substituto del feldespato en la fabricacion de ceramica blanca

    Energy Technology Data Exchange (ETDEWEB)

    Alvaro Guzman, A.; Silverio Delvasto, A.; Enrique Sanchez, V.; Vicente Amigo, B.

    2013-02-01

    The substitution of raw materials for processing high energy consumption materials by agricultural and agro-industrial wastes causes a positive impacts on the environment preservation. One of these residues is rice straw, which according to FAO estimation, its annual production is about 600 million tons. In this research was studied the use of rice straw ash as substitute of the use of feldspar in the white ware production. Clay-feldspar-quartz porcelains are referred to as triaxial white ware. Specimens of semidry triaxial mixtures, where feldspar was substituted for different percentages of CTA, were prepared by uniaxial pressing, followed by drying and sintering. Physical and mechanical properties of sintered bodies were evaluated. The porosity and the compressive strength of the fired pieces do increase with additions of up to 75% of CTA in substitution of feldspar. Their mineralogical phases were determined by DRX and SEM; grains of quartz, and needles of primary and secondary mullite were identified in a vitreous phase. It was concluded that feldspar can be substituted positively by CTA in white ware pastes. (Author) 22 refs.

  17. The solvent extraction of alkali metal ions with β-diketones

    International Nuclear Information System (INIS)

    Munakata, Megumu; Niina, Syozo; Shimoji, Noboru

    1974-01-01

    This work was undertaken to investigate effects of solvent and chelating-agent on the solvent extraction of alkali metal ions by seven β-diketones, acetylacetone (Acac), benzoylacetone (BzA), dipivaloylmethane (DPM), dibenzoylmethane (DBM), thenoyltrifluoloacetone (TTA), benzoyltrifluoroacetone (BFA) and hexafluoroacetylacetone (HFA), and to separate lithium from alkali metals. The extraction of alkali metals increase with increasing donor power of the solvent: i.e., benzene Na>K>Rb>Cs, which is also the order in which the adduct formation of these β-diketone chelates with donor solvents increase. The adduct formations between β-diketone chelates of alkali metals and donor solvents markedly enhance the solubilities of the chelates in solvents and, consequently, the extractabilities of alkali metals with β-diketones. Lithium was extracted with TTA in ether at such a low base concentration that sodium, potassium, rubidium and cesium were hardly extracted, and this enabled to separate lithium from other metals by the use of rubidium hydroxide (0.02 M). An attempt has been made to isolate alkali metal β-diketone chelates and some chelates have been obtained as crystals. The infrared absorption bands arising from C=O and C.=C of TTA shift to lower frequencies in the alkali metal chelates with TTA, and consequently, β-diketones is suggested to coordinate to alkali metal as a bidentate ligand. (JPN)

  18. Bleaching of the post-IR IRSL signal from individual grains of K-feldspar: Implications for single-grain dating

    International Nuclear Information System (INIS)

    Smedley, R.K.; Duller, G.A.T.; Roberts, H.M.

    2015-01-01

    Post-IR IRSL (pIRIR) signals from K-feldspar grains measured at elevated temperatures are increasingly being used for dating sediments. Unfortunately the pIRIR signal from K-feldspars bleaches more slowly than other signals (e.g. OSL from quartz) upon exposure to daylight, leading to concerns about residual signals remaining at deposition. However, earlier studies have not assessed whether the pIRIR signal bleaches at the same rate in all feldspar grains. In this study laboratory bleaching experiments have been conducted and for the first time the results show that the rate at which the pIRIR signal from individual K-feldspar grains bleach varies. To determine whether grain-to-grain variability in bleaching rate has a dominant control on equivalent dose (D e ) distributions determined using single grains, analysis was undertaken on three samples with independent age control from different depositional environments (two aeolian and one glaciofluvial). The D e value determined from each grain was compared with the rate at which the pIRIR 225 signal from the grain bleaches. The bleaching rate of each grain was assessed by giving a 52 Gy dose and measuring the residual D e after bleaching for an hour in a solar simulator. There is no clear relationship between the rate at which the pIRIR 225 signal of an individual grain bleaches and the magnitude of its D e . It is concluded that variability in the bleaching rate of the pIRIR 225 signal from one grain to another does not appear to be a dominant control on single grain D e distributions. - Highlights: • The bleaching rate of the pIRIR signal from single K-feldspar grains was assessed. • The pIRIR 225 signal bleaches more rapidly than the pIRIR 290 signal. • pIRIR 225 and pIRIR 290 signals reach the same level after 4–20 h of bleaching. • The bleaching rate of the pIRIR signal varies from one grain to another. • Variable pIRIR bleaching rates do not control single-grain D e distributions

  19. Luminescence and ESR properties of Brazilian feldspars

    International Nuclear Information System (INIS)

    Bitencourt, J.F.S.; Silva, D.M.; Silva, P.H.; Kinoshita, A.; Munita, C.S.; Tatumi, S.H.

    2006-01-01

    The IRSL and TL responses of three different feldspar crystals have been analysed. TL measurements were taken in the ultraviolet UV (290-370nm) and the visible VIS (340-610nm) regions of the spectrum. For the UV region and for a natural sample, peaks were observed at 283, 287 and 310 deg. C for grey, white and pink crystals, respectively. For samples irradiated after prior preheating, it was noted that TL peaks occurred at about 200 deg. C for all the samples; irradiation with high doses above 500Gy induced the formation of one additional peak at 170 deg. C. The VIS region results were similar to those for the UV. ESR experiments have been developed to verify the influence of radiation and heat treatments on the centres and preliminary results showed great variation in the intensities of [TiO 4 ] - , Al-O - -Al and Fe 3+ centres

  20. 40 CFR 721.4663 - Fluorinated carboxylic acid alkali metal salts.

    Science.gov (United States)

    2010-07-01

    ... Specific Chemical Substances § 721.4663 Fluorinated carboxylic acid alkali metal salts. (a) Chemical... fluorinated carboxylic acid alkali metal salts (PMNs P-95-979/980/981) are subject to reporting under this... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Fluorinated carboxylic acid alkali...

  1. Testing the application of quartz and feldspar luminescence dating to MIS 5 Japanese marine deposits

    DEFF Research Database (Denmark)

    Thiel, Christine; Tsukamoto, Sumiko; Tokuyasu, Kayoko

    2015-01-01

    The applicability of both quartz and feldspar luminescence dating was tested on twenty-five samples from a marine succession now forming a coastal cliff at Oga Peninsula, Honshu Island, Japan. The quartz optically stimulated luminescence (OSL) signal shows thermal instability and linear modulated...

  2. Structure and electrical resistivity of alkali-alkali and lithium-based liquid binary alloys

    International Nuclear Information System (INIS)

    Mishra, A.K.; Mukherjee, K.K.

    1990-01-01

    Harmonic model potential, developed and used for simple metals is applied here to evaluate hardsphere diameters, which ensure minimum interionic pair potential for alkali-alkali (Na-K, Na-Rb, Na-Cs, K-Rb, K-Cs) and lithium-based (Li-Na, Li-Mg, Li-In, Li-Tl) liquid binary alloys as a function of composition for use in the determination of their partial structure factors. These structure factors are then used to calculate electrical resistivities of alloys considered. The computed values of electrical resistivity as a function of composition agree both, in magnitude and gradient reasonably well with experimental values in all cases except in Cs systems, where the disagreement is appreciable. (author)

  3. Adsorption of lead and cadmium ions in aqueous solutions onto modified lignin from alkali glycerol delignication

    International Nuclear Information System (INIS)

    Demirbas, Ayhan

    2004-01-01

    Adsorptions of toxic metal ions (Pb(II) and Cd(II)) onto modified lignin from beech and poplar woods by alkali glycerol delignification are presented in this paper. The material exhibits good adsorption capacity and the adsorption data follow the Langmuir model. The maximum adsorption capacities are 8.2-9.0 and 6.7-7.5 mg/g of the modified lignin for Pb(II) and Cd(II), respectively. The maximum adsorption percentage is 95.8 for Pb(II) for 4 h at 330 K and is 95.0 for Cd(II) for 10 h at 290 K. The adsorption of both the metal ions increased with increasing temperature indicating endothermic nature of the adsorption process. The maximum adsorption percentages of Pb(II) and Cd(II) ions decrease with time till 48 and 42 h and then again increase slightly with time. The adsorption of both heavy metal ions increases with pH. The adsorption of Pb(II) ions reached a maximum at a 5.0 value of pH

  4. Mineralization dynamics of metakaolin-based alkali-activated cements

    Science.gov (United States)

    Gevaudan, Juan Pablo; Campbell, Kate M.; Kane, Tyler; Shoemaker, Richard K.; Srubar, Wil V.

    2017-01-01

    This paper investigates the early-age dynamics of mineral formation in metakaolin-based alkali-activated cements. The effects of silica availability and alkali content on mineral formation were investigated via X-ray diffraction and solid-state 29Si magic-angle spinning nuclear magnetic resonance spectroscopy at 2, 7, 14, and 28 days. Silica availability was controlled by using either liquid- (immediate) or solid-based (gradual) sodium silicate supplements. Mineral (zeolitic) and amorphous microstructural characteristics were correlated with observed changes in bulk physical properties, namely shrinkage, density, and porosity. Results demonstrate that, while alkali content controls the mineralization in immediately available silica systems, alkali content controls the silica availability in gradually available silica systems. Immediate silica availability generally leads to a more favorable mineral formation as demonstrated by correlated improvements in bulk physical properties.

  5. In situ alkali-silica reaction observed by x-ray microscopy

    International Nuclear Information System (INIS)

    Kurtis, K.E.; Monteiro, P.J.M.; Brown, J.T.; Meyer-Ilse, W.

    1997-01-01

    In concrete, alkali metal ions and hydroxyl ions contributed by the cement and reactive silicates present in aggregate can participate in a destructive alkali-silica reaction (ASR). This reaction of the alkalis with the silicates produces a gel that tends to imbibe water found in the concrete pores, leading to swelling of the gel and eventual cracking of the affected concrete member. Over 104 cases of alkali-aggregate reaction in dams and spillways have been reported around the world. At present, no method exists to arrest the expansive chemical reaction which generates significant distress in the affected structures. Most existing techniques available for the examination of concrete microstructure, including ASR products, demand that samples be dried and exposed to high pressure during the observation period. These sample preparation requirements present a major disadvantage for the study of alkali-silica reaction. Given the nature of the reaction and the affect of water on its products, it is likely that the removal of water will affect the morphology, creating artifacts in the sample. The purpose of this research is to observe and characterize the alkali-silica reaction, including each of the specific reactions identified previously, in situ without introducing sample artifacts. For observation of unconditioned samples, x-ray microscopy offers an opportunity for such an examination of the alkali-silica reaction. Currently, this investigation is focusing on the effect of calcium ions on the alkali-silica reaction

  6. In situ alkali-silica reaction observed by x-ray microscopy

    Energy Technology Data Exchange (ETDEWEB)

    Kurtis, K.E.; Monteiro, P.J.M. [Univ. of California, Berkeley, CA (United States); Brown, J.T.; Meyer-Ilse, W. [Ernest Orlando Lawrence Berkeley National Lab., CA (United States)

    1997-04-01

    In concrete, alkali metal ions and hydroxyl ions contributed by the cement and reactive silicates present in aggregate can participate in a destructive alkali-silica reaction (ASR). This reaction of the alkalis with the silicates produces a gel that tends to imbibe water found in the concrete pores, leading to swelling of the gel and eventual cracking of the affected concrete member. Over 104 cases of alkali-aggregate reaction in dams and spillways have been reported around the world. At present, no method exists to arrest the expansive chemical reaction which generates significant distress in the affected structures. Most existing techniques available for the examination of concrete microstructure, including ASR products, demand that samples be dried and exposed to high pressure during the observation period. These sample preparation requirements present a major disadvantage for the study of alkali-silica reaction. Given the nature of the reaction and the affect of water on its products, it is likely that the removal of water will affect the morphology, creating artifacts in the sample. The purpose of this research is to observe and characterize the alkali-silica reaction, including each of the specific reactions identified previously, in situ without introducing sample artifacts. For observation of unconditioned samples, x-ray microscopy offers an opportunity for such an examination of the alkali-silica reaction. Currently, this investigation is focusing on the effect of calcium ions on the alkali-silica reaction.

  7. Alkali adsorption on Ni(1 1 1) and their coadsorption with CO and O

    International Nuclear Information System (INIS)

    Politano, A.; Formoso, V.; Chiarello, G.

    2008-01-01

    The adsorption of alkalis (Na, K) on Ni(1 1 1) and their coadsorption with CO and O were studied by high-resolution electron energy loss spectroscopy. Loss measurements of clean alkali adlayers provided the expected behaviour of the alkali-substrate vibration energy as a function of the alkali coverage. This result was achieved by eliminating any trace of CO contamination from the alkali adlayer. As a matter of fact, a significant softening of the alkali-Ni vibration energy was revealed in the alkali + CO coadsorbed phase. Moreover, alkali coadsorption with oxygen caused a weakening of the O-Ni bond and a strengthening of the alkali-Ni bond

  8. Alkali (Li, K and Na) and alkali-earth (Be, Ca and Mg) adatoms on SiC single layer

    Science.gov (United States)

    Baierle, Rogério J.; Rupp, Caroline J.; Anversa, Jonas

    2018-03-01

    First-principles calculations within the density functional theory (DFT) have been addressed to study the energetic stability, and electronic properties of alkali and alkali-earth atoms adsorbed on a silicon carbide (SiC) single layer. We observe that all atoms are most stable (higher binding energy) on the top of a Si atom, which moves out of the plane (in the opposite direction to the adsorbed atom). Alkali atoms adsorbed give raise to two spin unpaired electronic levels inside the band gap leading the SiC single layer to exhibit n-type semiconductor properties. For alkaline atoms adsorbed there is a deep occupied spin paired electronic level inside the band gap. These finding suggest that the adsorption of alkaline and alkali-earth atoms on SiC layer is a powerful feature to functionalize two dimensional SiC structures, which can be used to produce new electronic, magnetic and optical devices as well for hydrogen and oxygen evolution reaction (HER and OER, respectively). Furthermore, we observe that the adsorption of H2 is ruled by dispersive forces (van der Waals interactions) while the O2 molecule is strongly adsorbed on the functionalized system.

  9. Tibetan tectonics from 40Ar/39Ar analysis of a single K-feldspar sample

    International Nuclear Information System (INIS)

    Richter, F.M.; Lovera, O.M.; Harrison, T.M.; Copeland, P.

    1991-01-01

    40 Ar/ 39 Ar data on an alkali feldspar sample from the Quxu pluton, Gangdese batholith, southern Tibet, allow a detailed assessment of unroofing and uplift history between 35 and 18 Ma. The 39 Ar Arrhenius plot for this sample shows departures from a linear relationship between the effective diffusion parameter, log(D/r 2 ), and reciprocal temperature, which we interpret to be the result of a distribution of distinct diffusion-domain sizes. We use an alternative way of plotting the Arrhenius data that exhibits domain size versus cumulative % 39 Ar released during step heating. The 40 Ar/ 39 Ar age spectrum of the sample has features, such as local age plateaus, that are most easily explained in terms of the distinctive closure age of particular domains. The fact that the same distribution of diffusion-domain sizes explains both the Arrhenius data and the age spectrum is an indication that the diffusion properties operating in the laboratory are those of the sample while it was in its natural environment. Modelling of the age spectrum with a distribution of domain sizes results in the recovery of a continuous cooling-history segment rather than a single time-temperature datum. We demonstrate the robustness of the cooling-curve determination by showing the large misfits to the age spectrum that arise from relatively small changes in the cooling history. The best-fit cooling curve for the Quxu sample shows a decreasing rate of cooling in the time interval 35-18 Ma, followed by a very rapid cooling beginning at about 18 Ma. We have used a thermal model for the conductive cooling of an unroofing pluton to estimate the rate of unroofing required to explain the Quxu cooling curve, and find that in the 35-20 Ma time interval, the primary control of the thermal evolution is the conductive loss of magmatic heat with little or no unroofing (unroofing rates of approximately 0.05 mm/yr) followed by a brief period (<5 Ma) of very rapid unroofing with rates of order 2 mm

  10. [Identification and function test of an alkali-tolerant denitrifying bacterium].

    Science.gov (United States)

    Wang, Ru; Zheng, Ping; Li, Wei; Chen, Hui; Chen, Tingting; Ghulam, Abbas

    2013-04-04

    We obtained an alkali-tolerant denitrifying bacterium, and determined its denitrifying activity and alkali-tolerance. An alkali-tolerant denitrifying bacterial strain was obtained by isolation and purification. We identified the bacterial strain by morphological observation, physiological test and 16S rRNA analysis. We determined the denitrifying activity and alkali-tolerance by effects of initial nitrate concentration and initial pH on denitrification. An alkali-tolerant denitrifier strain R9 was isolated from the lab-scale high-rate denitrifying reactor, and it was identified as Diaphorobater nitroreducens. The strain R9 grew heterotrophically with methanol as the electron donor and nitrate as the electron acceptor. The nitrate conversion was 93.25% when strain R9 was cultivated for 288 h with initial nitrate concentration 50 mg/L and initial pH 9.0. The denitrification activity could be inhibited at high nitrate concentration with a half inhibition constant of 202.73 mg N/L. Strain R9 showed a good alkali tolerance with the nitrate removal rate at pH 11.0 remained 86% of that at pH 9.0. Strain R9 was identified as Diaphorobater nitroreducens, and it was an alkali-tolerant denitrifying bacterium with optimum pH value of 9.0.

  11. Maternal exposure to alkali, alkali earth, transition and other metals: Concentrations and predictors of exposure

    International Nuclear Information System (INIS)

    Hinwood, A.L.; Stasinska, A.; Callan, A.C.; Heyworth, J.; Ramalingam, M.; Boyce, M.; McCafferty, P.; Odland, J.Ø.

    2015-01-01

    Most studies of metals exposure focus on the heavy metals. There are many other metals (the transition, alkali and alkaline earth metals in particular) in common use in electronics, defense industries, emitted via combustion and which are naturally present in the environment, that have received limited attention in terms of human exposure. We analysed samples of whole blood (172), urine (173) and drinking water (172) for antimony, beryllium, bismuth, cesium, gallium, rubidium, silver, strontium, thallium, thorium and vanadium using ICPMS. In general most metals concentrations were low and below the analytical limit of detection with some high concentrations observed. Few factors examined in regression models were shown to influence biological metals concentrations and explained little of the variation. Further study is required to establish the source of metals exposures at the high end of the ranges of concentrations measured and the potential for any adverse health impacts in children. - This study has demonstrated exposure to alkali, alkali earth and transition metals in pregnant women with factors such as breastfeeding, fish oil use and diet affecting exposures

  12. Limits to depletion of blue-green light stimulated luminescence in feldspars: Implications for quartz dating

    DEFF Research Database (Denmark)

    Jain, M.; Singhvi, A.K.

    2001-01-01

    stimulation curve of otherwise pure quartz. In this study, the functional relationship between the infra-red stimulated luminescence (IRSL) and BGSL of feldspars, (1) at different preheats, and (2) with IR bleaching at different stimulation temperatures and durations, is examined. The results suggest two trap...

  13. Stability of IRSL signals from sedimentary K-feldspar samples

    DEFF Research Database (Denmark)

    Thomsen, Kristina Jørkov; Murray, A.S.; Jain, Mayank

    2011-01-01

    for potassium-rich sedimentary feldspars. We show that the natural post-IR IRSL (pIRIR) signal from a 3.6 Ma old sample is in apparent saturation on a laboratory generated dose response curve, i.e. it does not show detectable fading in nature although a low fading rate is observed on laboratory time scales. We...... be explained in terms of either a single- or multiple-trap model. We present evidence that may suggest that at least part of pIRIR signal is derived from a high temperature trap (∼550°C thermoluminescence (TL) peak), although again the data can also be explained in terms of a single-trap model. Finally, we...

  14. Morphological evolution of dissolving feldspar particles with anisotropic surface kinetics and implications for dissolution rate normalization and grain size dependence: A kinetic modeling study

    Science.gov (United States)

    Zhang, Li; Lüttge, Andreas

    2009-11-01

    With previous two-dimensional (2D) simulations based on surface-specific feldspar dissolution succeeding in relating the macroscopic feldspar kinetics to the molecular-scale surface reactions of Si and Al atoms ( Zhang and Lüttge, 2008, 2009), we extended our modeling effort to three-dimensional (3D) feldspar particle dissolution simulations. Bearing on the same theoretical basis, the 3D feldspar particle dissolution simulations have verified the anisotropic surface kinetics observed in the 2D surface-specific simulations. The combined effect of saturation state, pH, and temperature on the surface kinetics anisotropy has been subsequently evaluated, found offering diverse options for morphological evolution of dissolving feldspar nanoparticles with varying grain sizes and starting shapes. Among the three primary faces on the simulated feldspar surface, the (1 0 0) face has the biggest dissolution rate across an extensively wide saturation state range and thus acquires a higher percentage of the surface area upon dissolution. The slowest dissolution occurs to either (0 0 1) or (0 1 0) faces depending on the bond energies of Si-(O)-Si ( ΦSi-O-Si/ kT) and Al-(O)-Si ( ΦAl-O-Si/ kT). When the ratio of ΦSi-O-Si/ kT to ΦAl-O-Si/ kT changes from 6:3 to 7:5, the dissolution rates of three primary faces change from the trend of (1 0 0) > (0 1 0) > (0 0 1) to the trend of (1 0 0) > (0 0 1) > (0 1 0). The rate difference between faces becomes more distinct and accordingly edge rounding becomes more significant. Feldspar nanoparticles also experience an increasing degree of edge rounding from far-from-equilibrium to close-to-equilibrium. Furthermore, we assessed the connection between the continuous morphological modification and the variation in the bulk dissolution rate during the dissolution of a single feldspar particle. Different normalization treatments equivalent to the commonly used mass, cube assumption, sphere assumption, geometric surface area, and reactive

  15. Alkali content of fly ash : measuring and testing strategies for compliance.

    Science.gov (United States)

    2015-04-01

    Sodium and potassium are the common alkalis present in fly ash. Excessive amounts of fly ash alkalis can cause efflorescence : problems in concrete products and raise concern about the effectiveness of the fly ash to mitigate alkali-silica reaction (...

  16. Absorption lineshape of FA centers in alkali halides

    International Nuclear Information System (INIS)

    Baldacchini, G.; Giovenale, E.; De Matteis, F.; Scacco, A.; Somma, F.; Grassano, U.M.

    1988-01-01

    The line shape of the absorption bands of F A centers in alkali halides have been studied for the first time. The new method used for this investigation is based on the determination of the overlap between the F A1 and F A2 bands from luminescence measurements. The experimental results have been compared with calculated values deduced from the theoretical F A bands of different shapes. For both F A (I) centers in KCl:Na + and F A (II) centers in KCl:Li + and RbCl:Li + the absorption lineshape at low temperature is much closer to a sum of two Lorentzian curves than that of two Gaussian or Poissonian bands. This results shows an unexpected difference with the F centers, whose absorption lineshape is known to be Poissonian at the same temperatures

  17. Interaction of alkali metal nitrates with calcium carbonate and kyanite

    International Nuclear Information System (INIS)

    Protsyuk, A.P.; Malakhov, A.I.; Karabanov, V.P.; Lebedeva, L.P.

    1978-01-01

    Thermographic, thermodynamic and X-ray phase studies have been made into the interaction of alkali metal nitrates with calcium carbonate and kyanite. Examined among other things was the effect of water vapor and carbon dioxide on the interaction between alkali metal nitrates and kyanite. The chemical mechanism of the occurring processes has been established. The interaction with calcium carbonates results in the formation of alkali metal carbonates and calcium oxide with liberation of nitrogen oxide and oxygen. The products of the interaction with kyanite are shown to be identical with the compounds forming when alkali metal carbonates are used

  18. Electronic and atomic structures of liquid tellurium containing alkali elements

    International Nuclear Information System (INIS)

    Kawakita, Yukinobu; Yao, Makoto; Endo, Hirohisa.

    1997-01-01

    The measurements of electrical conductivity σ, density, EXAFS and neutron scattering were carried out for liquid K-Te and Rb-Te mixtures. The conductivity σ decreases rapidly with alkali concentration and a metal-semiconductor transition occurs at about 10 at.% alkali. It is found that the compositional variation of σ is nearly independent of the alkali species. The Te-Te bond length deduced from EXAFS and neutron scattering measurements is 2.8 A and changes little with alkali concentrations. The average distances from K and Rb atom to Te atoms are 3.6 A and 3.8 A, respectively. Two kinds of relaxation processes are observed in quasielastic neutron scattering for K 20 Te 80 . Upon the addition of alkali the interaction between the neighbouring Te chains, which is responsible for the metallic conduction, weaken considerably. (author)

  19. Survival probability in small angle scattering of low energy alkali ions from alkali covered metal surfaces

    International Nuclear Information System (INIS)

    Neskovic, N.; Ciric, D.; Perovic, B.

    1982-01-01

    The survival probability in small angle scattering of low energy alkali ions from alkali covered metal surfaces is considered. The model is based on the momentum approximation. The projectiles are K + ions and the target is the (001)Ni+K surface. The incident energy is 100 eV and the incident angle 5 0 . The interaction potential of the projectile and the target consists of the Born-Mayer, the dipole and the image charge potentials. The transition probability function corresponds to the resonant electron transition to the 4s projectile energy level. (orig.)

  20. Reaction of alkali nitrates with PuO2

    International Nuclear Information System (INIS)

    Yamashita, T.; Ohuchi, K.; Takahashi, K.; Fujino, T.

    1990-01-01

    Improvement of solubility of plutonium dioxide (PuO 2 ) in acid solution is important to establish the nuclear fuel reprocessing technique for uranium-plutonium mixed oxide fuels. If insoluble PuO 2 can be converted into any soluble plutonium compounds, problems arising from the fuel dissolution process will be reduced to a great extent. Alkali metal plutonates and alkaline-earth plutonates are known to have enhanced solubility in mineral acids. However, the reaction conditions to form such plutonates and characterization thereof are not well elucidated. Then the reactivity and reaction conditions to form lithium and sodium plutonates from their nitrates and PuO 2 were studied at temperatures between 500 and 900 degree C and alkali metal to plutonium atom ratios between 0.5 and 6 by means of thermogravimetry as well as X-ray diffraction technique. The reaction behavior of alkali plutonates will be discussed in comparison with corresponding alkali uranates

  1. Transcriptome alteration in a rice introgression line with enhanced alkali tolerance.

    Science.gov (United States)

    Zhang, Yunhong; Lin, Xiuyun; Ou, Xiufang; Hu, Lanjuan; Wang, Jinming; Yang, Chunwu; Wang, Shucai; Liu, Bao

    2013-07-01

    Alkali stress inhibits plant growth and development and thus limits crop productivity. To investigate the possible genetic basis of alkali tolerance in rice, we generated an introgressed rice line (K83) with significantly enhanced tolerance to alkali stress compared to its recipient parental cultivar (Jijing88). By using microarray analysis, we examined the global gene expression profiles of K83 and Jijing88, and found that more than 1200 genes were constitutively and differentially expressed in K83 in comparison to Jijing88 with 572 genes up- and 654 down-regulated. Upon alkali treatment, a total of 347 genes were found up- and 156 down-regulated in K83 compared to 591 and 187, respectively, in Jijing88. Among the up-regulated genes in both K83 and Jijing88, only 34 were constitutively up-regulated in K83, suggesting that both the constitutive differentially expressed genes in K83 and those induced by alkali treatment are most likely responsible for enhanced alkali tolerance. A gene ontology analysis based on all annotated, differentially expressed genes revealed that genes with expression alterations were enriched in pathways involved in metabolic processes, catalytic activity, and transport and transcription factor activities, suggesting that these pathways are associated with alkali stress tolerance in rice. Our results illuminated the novel genetic aspects of alkali tolerance in rice and established a repertory of potential target genes for biotechnological manipulations that can be used to generate alkali-tolerant rice cultivars. Copyright © 2013 Elsevier Masson SAS. All rights reserved.

  2. The alkali-aggregate reaction - concrete microstructure evolution

    International Nuclear Information System (INIS)

    Regourd, M.; Hornain, H.; Poitevin, P.

    1981-01-01

    The alkali-aggregate reaction has been studied by scanning electron microscopy and energy dispersive X-ray analysis, electron probe microanalysis, and X-ray diffraction in concretes containing glass aggregates or hornfels and greywacke aggregates. The surface reaction of the natural aggregates in alkaline solutions has been analysed by X-ray photo-electron spectrometry. The study of concretes with glass aggregates stored at 20 degrees Celcius and 100 percent relative humidity has revealed, irrespective of alkali content and type of cement, the formation of a gel containing SiO 2 , Na 2 O, CaO, MgO and Al 2 O 3 . Under heat and pressure (210 degrees Celcius at MPa for 48 hours), the gel crystallizes and yields silicates not very different from tobermorite found in autoclaved normal concretes but cotaining Na and K in solid solutions. The alkali reaction in two natural aggregate concretes, is also shown by the formation of gels and silicate crystals. The progressive structuring of the gels in silicate crystals is promoted by an increase in temperature. Ettringite and Ca(OH) 2 reinforce the alkali-aggregate reaction which may be looked upon as a hydration reaction, partially of the pozzolanic type

  3. Fluorescent sensing and determination of mercury (II) ions in water ...

    African Journals Online (AJOL)

    In this study we report on a fluorescent sensing probe based on a naphthyl azo dye modified dibenzo-18-crown-6-ether (DB18C6) for the detection and determination of mercury (II) ions in water. The probe showed high sensitivity and selectivity towards the mercury (II) ion among various alkali, alkaline earth, and transition ...

  4. Modeling of the shape of infrared stimulated luminescence signals in feldspars

    DEFF Research Database (Denmark)

    Pagonis, Vasilis; Jain, Mayank; Murray, Andrew S.

    2012-01-01

    This paper presents a new empirical model describing infrared (IR) stimulation phenomena in feldspars. In the model electrons from the ground state of an electron trap are raised by infrared optical stimulation to the excited state, and subsequently recombine with a nearest-neighbor hole via...... corresponds to a fast rate of recombination processes taking place along the infrared stimulated luminescence (IRSL) curves. The subsequent decay of the simulated IRSL signal is characterized by a much slower recombination rate, which can be described by a power-law type of equation.Several simulations...

  5. Comparative study of diode-pumped alkali vapor laser and exciplex-pumped alkali laser systems and selection principal of parameters

    Science.gov (United States)

    Huang, Wei; Tan, Rongqing; Li, Zhiyong; Han, Gaoce; Li, Hui

    2017-03-01

    A theoretical model based on common pump structure is proposed to analyze the output characteristics of a diode-pumped alkali vapor laser (DPAL) and XPAL (exciplex-pumped alkali laser). Cs-DPAL and Cs-Ar XPAL systems are used as examples. The model predicts that an optical-to-optical efficiency approaching 80% can be achieved for continuous-wave four- and five-level XPAL systems with broadband pumping, which is several times the pumped linewidth for DPAL. Operation parameters including pumped intensity, temperature, cell's length, mixed gas concentration, pumped linewidth, and output coupler are analyzed for DPAL and XPAL systems based on the kinetic model. In addition, the predictions of selection principal of temperature and cell's length are also presented. The concept of the equivalent "alkali areal density" is proposed. The result shows that the output characteristics with the same alkali areal density but different temperatures turn out to be equal for either the DPAL or the XPAL system. It is the areal density that reflects the potential of DPAL or XPAL systems directly. A more detailed analysis of similar influences of cavity parameters with the same areal density is also presented.

  6. 40 CFR 721.10098 - Disubstituted benzoic acid, alkali metal salt (generic).

    Science.gov (United States)

    2010-07-01

    ... New Uses for Specific Chemical Substances § 721.10098 Disubstituted benzoic acid, alkali metal salt... identified generically as disubstituted benzoic acid, alkali metal salt (PMN P-03-643) is subject to... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Disubstituted benzoic acid, alkali...

  7. Alkali solution extraction of rice residue protein isolates: Influence of alkali concentration on protein functional, structural properties and lysinoalanine formation.

    Science.gov (United States)

    Hou, Furong; Ding, Wenhui; Qu, Wenjuan; Oladejo, Ayobami Olayemi; Xiong, Feng; Zhang, Weiwei; He, Ronghai; Ma, Haile

    2017-03-01

    This study evaluated the nutrient property and safety of the rice residue protein isolates (RRPI) product (extracted by different alkali concentrations) by exploring the protein functional, structural properties and lysinoalanine (LAL) formation. The results showed that with the rising of alkali concentration from 0.03M to 0.15M, the solubility, emulsifying and foaming properties of RRPI increased at first and then descended. When the alkali concentration was greater than 0.03M, the RRPI surface hydrophobicity decreased and the content of thiol and disulfide bond, Lys and Cys significantly reduced. By the analysis of HPLC, the content of LAL rose up from 276.08 to 15,198.07mg/kg and decreased to 1340.98mg/kg crude protein when the alkali concentration increased from 0.03 to 0.09M and until to 0.15M. These results indicated that RRPI alkaline extraction concentration above 0.03M may cause severe nutrient or safety problems of protein. Copyright © 2016 Elsevier Ltd. All rights reserved.

  8. Alkali-Activated Natural Pozzolan/Slag Binder for Sustainable Concrete

    Science.gov (United States)

    Najimi, Meysam

    This study aimed to fully replace Portland cement (PC) with environmentally friendly binders capable of improving longevity of concrete. The new binders consisted of different proportions of natural Pozzolan and slag which were alkaline-activated with various combinations of sodium hydroxide and sodium silicate. A step-by-step research program was designed to (1) develop alkali-activated natural Pozzolan/slag pastes with adequate fresh and strength properties, (2) produce alkali-activated natural Pozzolan/slag mortars to assess the effects of dominant variables on their plastic and hardened properties, and (3) finally produce and assess fresh, mechanical, dimensional, transport and durability properties of alkali-activated natural Pozzolan/slag concretes. The major variables included in this study were binder combination (natural Pozzolan/slag combinations of 70/30, 50/50 and 30/70), activator combination (sodium silicate/sodium hydroxide combinations of 20/80, 25/75 and 30/70), and sodium hydroxide concentration (1, 1.75 and 2.5M). The experimental program assessed performance of alkali-activated natural Pozzolan/slag mixtures including fresh properties (flow and setting times), unit weights (fresh, demolded and oven-dry), mechanical properties (compressive and tensile strengths, and modulus of elasticity), transport properties (absorption, rapid chloride penetration, and rapid chloride migration), durability (frost resistance, chloride induced corrosion, and resistance to sulfuric acid attack), and dimensional stability (drying shrinkage). This study also compared the performance of alkali-activated natural Pozzolan/slag concretes with that of an equivalent reference Portland cement concrete having a similar flow and strength characteristics. The results of this study revealed that it was doable to find optimum binder proportions, activator combinations and sodium hydroxide concentrations to achieve adequate plastic and hardened properties. Nearly for all studied

  9. Determination of the common and rare alkalies in mineral analysis

    Science.gov (United States)

    Wells, R.C.; Stevens, R.E.

    1934-01-01

    Methods are described which afford a determination of each member of the alkali group and are successful in dealing with the quantities of the rare alkalies found in rocks and minerals. The procedures are relatively rapid and based chiefly on the use of chloroplatinic acid, absolute alcohol and ether, and ammonium sulfate. The percentages of all the alkalies found in a number of minerals are given.

  10. 40 CFR 721.5452 - Alkali metal salt of halogenated organoborate (generic).

    Science.gov (United States)

    2010-07-01

    ... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Alkali metal salt of halogenated... Specific Chemical Substances § 721.5452 Alkali metal salt of halogenated organoborate (generic). (a... generically as alkali metal salt of halogenated organoborate (PMN P-00-0638) is subject to reporting under...

  11. Physiological Evaluation of Alkali-Salt Tolerance of Thirty Switchgrass (Panicum virgatum Lines.

    Directory of Open Access Journals (Sweden)

    Guofu Hu

    Full Text Available Soil salt-alkalization is a major limiting factor for crop production in many regions. Switchgrass (Panicum virgatum L. is a warm-season C4 perennial rhizomatous bunchgrass and a target lignocellulosic biofuel species. The objective of this study was to evaluate relative alkali-salt tolerance among 30 switchgrass lines. Tillers of each switchgrass line were transplanted into pots filled with fine sand. Two months after transplanting, plants at E5 developmental stage were grown in either half strength Hoagland's nutrient solution with 0 mM Na+ (control or half strength Hoagland's nutrient solution with 150 mM Na+ and pH of 9.5 (alkali-salt stress treatment for 20 d. Alkali-salt stress damaged cell membranes [higher electrolyte leakage (EL], reduced leaf relative water content (RWC, net photosynthetic rate (Pn, stomatal conductance (gs, and transpiration rate (Tr. An alkali-salt stress tolerance trait index (ASTTI for each parameter was calculated based on the ratio of the value under alkali-salt stress and the value under non-stress conditions for each parameter of each line. Relative alkali-salt tolerance was determined based on principal components analysis and cluster analysis of the physiological parameters and their ASTTI values. Significant differences in alkali-salt stress tolerance were found among the 30 lines. Lowland lines TEM-SEC, Alamo, TEM-SLC and Kanlow were classified as alkali-salt tolerant. In contrast, three lowland lines (AM-314/MS-155, BN-13645-64 and two upland lines (Caddo and Blackwell-1 were classified as alkali-salt sensitive. The results suggest wide variations exist in alkali-salt stress tolerance among the 30 switchgrass lines. The approach of using a combination of principal components and cluster analysis of the physiological parameters and related ASTTI is feasible for evaluating alkali-salt tolerance in switchgrass.

  12. Physiological Evaluation of Alkali-Salt Tolerance of Thirty Switchgrass (Panicum virgatum) Lines.

    Science.gov (United States)

    Hu, Guofu; Liu, Yiming; Zhang, Xunzhong; Yao, Fengjiao; Huang, Yan; Ervin, Erik H; Zhao, Bingyu

    2015-01-01

    Soil salt-alkalization is a major limiting factor for crop production in many regions. Switchgrass (Panicum virgatum L.) is a warm-season C4 perennial rhizomatous bunchgrass and a target lignocellulosic biofuel species. The objective of this study was to evaluate relative alkali-salt tolerance among 30 switchgrass lines. Tillers of each switchgrass line were transplanted into pots filled with fine sand. Two months after transplanting, plants at E5 developmental stage were grown in either half strength Hoagland's nutrient solution with 0 mM Na+ (control) or half strength Hoagland's nutrient solution with 150 mM Na+ and pH of 9.5 (alkali-salt stress treatment) for 20 d. Alkali-salt stress damaged cell membranes [higher electrolyte leakage (EL)], reduced leaf relative water content (RWC), net photosynthetic rate (Pn), stomatal conductance (gs), and transpiration rate (Tr). An alkali-salt stress tolerance trait index (ASTTI) for each parameter was calculated based on the ratio of the value under alkali-salt stress and the value under non-stress conditions for each parameter of each line. Relative alkali-salt tolerance was determined based on principal components analysis and cluster analysis of the physiological parameters and their ASTTI values. Significant differences in alkali-salt stress tolerance were found among the 30 lines. Lowland lines TEM-SEC, Alamo, TEM-SLC and Kanlow were classified as alkali-salt tolerant. In contrast, three lowland lines (AM-314/MS-155, BN-13645-64) and two upland lines (Caddo and Blackwell-1) were classified as alkali-salt sensitive. The results suggest wide variations exist in alkali-salt stress tolerance among the 30 switchgrass lines. The approach of using a combination of principal components and cluster analysis of the physiological parameters and related ASTTI is feasible for evaluating alkali-salt tolerance in switchgrass.

  13. 40 CFR 721.5985 - Fatty alkyl phosphate, alkali metal salt (generic).

    Science.gov (United States)

    2010-07-01

    ... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Fatty alkyl phosphate, alkali metal... Specific Chemical Substances § 721.5985 Fatty alkyl phosphate, alkali metal salt (generic). (a) Chemical... as a fatty alkyl phosphate, alkali metal salt (PMN P-99-0385) is subject to reporting under this...

  14. Lead (II) removal from natural soils by enhanced electrokinetic remediation.

    Science.gov (United States)

    Altin, Ahmet; Degirmenci, Mustafa

    2005-01-20

    Electrokinetic remediation is a very effective method to remove metal from fine-grained soils having low adsorption and buffering capacity. However, remediation of soil having high alkali and adsorption capacity via the electrokinetic method is a very difficult process. Therefore, enhancement techniques are required for use in these soil types. In this study, the effect of the presence of minerals having high alkali and cation exchange capacity in natural soil polluted with lead (II) was investigated by means of the efficiency of electrokinetic remediation method. Natural soil samples containing clinoptilolite, gypsum and calcite minerals were used in experimental studies. Moreover, a sample containing kaolinite minerals was studied to compare with the results obtained from other samples. Best results for soils bearing alkali and high sorption capacity minerals were obtained upon addition of 3 mol AcH and application of 20 V constant potential after a remediation period of 220 h. In these test conditions, lead (II) removal efficiencies for these samples varied between 60% and 70% up to 0.55 normalized distance. Under the same conditions, removal efficiencies in kaolinite sample varied between 50% and 95% up to 0.9 normalized distance.

  15. 40 CFR 721.4660 - Alcohol, alkali metal salt.

    Science.gov (United States)

    2010-07-01

    ... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Alcohol, alkali metal salt. 721.4660 Section 721.4660 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY (CONTINUED) TOXIC SUBSTANCES CONTROL ACT SIGNIFICANT NEW USES OF CHEMICAL SUBSTANCES Significant New Uses for Specific Chemical Substances § 721.4660 Alcohol, alkali metal sal...

  16. Utilization of Mineral Wools as Alkali-Activated Material Precursor

    Directory of Open Access Journals (Sweden)

    Juho Yliniemi

    2016-04-01

    Full Text Available Mineral wools are the most common insulation materials in buildings worldwide. However, mineral wool waste is often considered unrecyclable because of its fibrous nature and low density. In this paper, rock wool (RW and glass wool (GW were studied as alkali-activated material precursors without any additional co-binders. Both mineral wools were pulverized by a vibratory disc mill in order to remove the fibrous nature of the material. The pulverized mineral wools were then alkali-activated with a sodium aluminate solution. Compressive strengths of up to 30.0 MPa and 48.7 MPa were measured for RW and GW, respectively, with high flexural strengths measured for both (20.1 MPa for RW and 13.2 MPa for GW. The resulting alkali-activated matrix was a composite-type in which partly-dissolved fibers were dispersed. In addition to the amorphous material, sodium aluminate silicate hydroxide hydrate and magnesium aluminum hydroxide carbonate phases were identified in the alkali-activated RW samples. The only crystalline phase in the GW samples was sodium aluminum silicate. The results of this study show that mineral wool is a very promising raw material for alkali activation.

  17. Infrared stimulated luminescence dating of an Eemian (MIS 5e) site in Denmark using K-feldspar

    DEFF Research Database (Denmark)

    Buylaert, Jan-Pieter; Huot, Sebastian; Murray, Andrew S.

    2011-01-01

    Infrared stimulated luminescence (IRSL) dating of K-feldspars may be an alternative to quartz optically stimulated luminescence (OSL) dating when the quartz OSL signal is too close to saturation or when the quartz luminescence characteristics are unsuitable. In this paper, Eemian (MIS 5e) coastal...

  18. Thorium valency in molten alkali halides in equilibrium with metallic thorium

    International Nuclear Information System (INIS)

    Smirnov, M.V.; Kudyakov, V.Ya.

    1983-01-01

    Metallic thorium is shown to corrode in molten alkali halides even in the absence of external oxidizing agents, alkali cations acting as oxidizing agents. Its corrosion rate grows in the series of alkali chlorides from LiCl to CsCl at constant temperature. Substituting halide anions for one another exerts a smaller influence, the rate rising slightly in going from chlorides to bromides and iodides, having the same alkali cations. Thorium valency is determined coulometrically, the metal being dissolved anodically in molten alkali halides and their mixtures. In fluoride melts it is equal to 4 but in chloride, bromide and iodide ones, as a rule, it has non-integral values between 4 and 2 which diminish as the temperature is raised, as the thorium concentration is lowered, as the radii of alkali cations decrease and those of halide anions increase. The emf of cells Th/N ThHlsub(n) + (1-N) MHl/MHl/C, Hlsub(2(g)) where Hl is Cl, Br or I, M is Li, Na, K, Cs or Na + K, and N < 0.05, is measured as a function of concentration at several temperatures. Expressions are obtained for its concentration dependence. The emf grows in the series of alkali chlorides from LiCl to CsCl, other conditions being equal. (author)

  19. Autoclave-hardening slag-alkali binder with high water content

    International Nuclear Information System (INIS)

    Korenevskij, V.V.; Kozyrin, N.A.; Melikhova, N.I.; Narkevich, N.K.; Ryabov, G.G.

    1987-01-01

    The results of investigations into properties of slag-alkali binder, that may be used for concretes of reactor radiation and thermal shieldings, are presented. These concretes have increased chemical stability and mechanical strength, high content of chemically bound water (approximately 14%), that is not lost under heating up to 550 deg C. Dumping and granulated slags of blast-furnace process, sodium-bicarbonate-alkali fusion cake formed at burning of adipic acid residues, technical sodium hydroxide and sodium liquid glass are used as raw material for slag-alkali binder

  20. ALKALI-ACTIVATION KINETICS OF PHOSPHORUS SLAG CEMENT USING COMPRESSIVE STRENGTH DATA

    Directory of Open Access Journals (Sweden)

    Hojjatollah Maghsoodloorad

    2015-09-01

    Full Text Available In this research, through compressive strength data, the order and kinetics of alkali-activation of phosphorus slag activated with two compound activators of NaOH + Na2CO3 and Na2CO3 + Ca(OH2, has been evaluated. The kinetics and order of alkali activation is a key factor to forecasting the mechanical behavior of alkali activated cement at different curing time and temperatures without carrying out experimental tests. The apparent activation energy was obtained as 35.6 kJ.mol-1 and 60.7 kJ.mol-1 for the two activators, respectively. Investigations proved that the alkali-activation kinetics of phosphorus slag resembles chemical reactions of second order. Moreover, the order of alkali-activation of phosphorus slag does not depend on the type of activator.

  1. Effects of Alkali and Counter Ions in Sn-Beta Catalyzed Carbohydrate Conversion

    DEFF Research Database (Denmark)

    Elliot, Samuel G.; Tolborg, Søren; Madsen, Robert

    2018-01-01

    Alkali ions have been shown to strongly influence the catalytic behavior of stannosilicates in the conversion of carbohydrates. An effect of having alkali ions present is a pronounced increase in selectivity towards methyl lactate. Mechanistic details of this effect have remained obscure and are ......Alkali ions have been shown to strongly influence the catalytic behavior of stannosilicates in the conversion of carbohydrates. An effect of having alkali ions present is a pronounced increase in selectivity towards methyl lactate. Mechanistic details of this effect have remained obscure...... and are herein addressed experimentally through kinetic experiments and isotope tracking. Alkali ions have a differential effect in competing reaction pathways: they promote the rate of carbon-carbon bond breakage of carbohydrate substrates, but decrease the rates of competing dehydration pathways. Further...... addition of alkali inhibits activity of Sn-Beta in all major reaction pathways. The alkali effects on product distributions and on rates of product formation are similar, thus pointing to a kinetic reaction control and to irreversible reaction steps in the main pathways. Additionally, an effect...

  2. IR-RF dating of sand-sized K-feldspar extracts: A test of accuracy

    DEFF Research Database (Denmark)

    Buylaert, Jan-Pieter; Jain, Mayank; Murray, A.S.

    2012-01-01

    In this paper we use a recently developed radioluminescence (RL) attachment to the Risø TL/OSL reader to test the InfraRed-RadioFluorescence (IR-RF) dating method applied to K-feldspar rich extracts from our known-age archive samples. We present experiments to characterise the instrument performa......In this paper we use a recently developed radioluminescence (RL) attachment to the Risø TL/OSL reader to test the InfraRed-RadioFluorescence (IR-RF) dating method applied to K-feldspar rich extracts from our known-age archive samples. We present experiments to characterise the instrument...... performance and to test the reproducibility of IR-RF measurements. These experiments illustrate the high sensitivity and dose rate of our RL system, the negligible influence of the turntable movement on IR-RF signals and the effectiveness of the built in 395 nm LED at bleaching IR-RF signals. We measure IR......-RF ages on a set of samples with independent age control using a robust analytical method, which is able to detect any possible sensitivity change. Our IR-RF ages do not agree well with the independent age control; the ages of the younger samples (20–45 ka) are significantly over-estimated while the ages...

  3. [Diversity of uncultured actinomycetes in saline-alkali soil from Jiuquan area of Hexi Corridor].

    Science.gov (United States)

    Li, Hai-yun; Niu, Shi-quan; Kong, Wei-bao; Yan, Wei-ru; Geng, Hui; Han, Cai-hong; Da, Wen-yan; Zhang, Ai-mei; Zhu, Xue-tai

    2015-09-01

    In order to more accurately understand community structure and diversity of actinomycetes in saline-alkali soil from Jiuquan area of Hexi Corridor, the community structure and diversity from three kinds of soil samples (primary, secondary saline alkali soil and farmland soil) were analyzed using uncultured methods. The results showed that the 16S rDNA clone library of actinomycetales from the primary saline-alkali soil belonged to 19 OTUs, Micrococcineae, Propionibacterineae, Corynebacterineae, Frankineae, Pseudonocardineae and unknown groups of Actinomycetales; the 16S r DNA clone library of actinomycetales from the secondary saline-alkali soil belonged to 14 OTUs, Micrococcineae, Propionibacterineae, Corynebacterineae, Frankineae, Pseudonocardineae and unknown groups of Actinomycetales; the 16S rDNA clone library of farmland soil belonged to 7 OTUs, Micrococcineae, Propionibacterineae, Corynebacterineae, Frankineae, Pseudonocardineae and unknown groups of Actinomycetales; Micrococcineae was the common population in the three soils, and also was the dominant population in primary saline alkali soil and farmland soil. The diversity index and rarefaction curves analysis showed that actinomycetes species richness was in order of primary saline-alkali soil > secondary saline-alkali soil > farmland soil. The dilution curves of primary saline-alkali soil and secondary saline-alkali soil were not leveled off, which indicated the actinomycetes diversity in saline-alkali soil was more enriched than the actual. The rich and diverse actinomycetes resources in saline-alkali soil from Jiuquan area of Hexi Corridor provide important data on the actinomycetes ecology distribution research, exploitation and utilization in saline-alkali soil.

  4. Development of cataclastic foliation in deformation bands in feldspar-rich conglomerates of the Rio do Peixe Basin, NE Brazil

    Science.gov (United States)

    Nicchio, Matheus A.; Nogueira, Francisco C. C.; Balsamo, Fabrizio; Souza, Jorge A. B.; Carvalho, Bruno R. B. M.; Bezerra, Francisco H. R.

    2018-02-01

    In this work we describe the deformation mechanisms and processes that occurred during the evolution of cataclastic deformation bands developed in the feldspar-rich conglomerates of the Rio do Peixe Basin, NE Brazil. We studied bands with different deformation intensities, ranging from single cm-thick tabular bands to more evolved clustering zones. The chemical identification of cataclastic material within deformation bands was performed using compositional mapping in SEM images, EDX and XRD analyses. Deformation processes were identified by microstructural analysis and by the quantification of comminution intensity, performed using digital image processing. The deformation bands are internally non homogeneous and developed during five evolutionary stages: (1) moderate grain size reduction, grain rotation and grain border comminution; (2) intense grain size reduction with preferential feldspar fragmentation; (3) formation of subparallel C-type slip zones; (4) formation of S-type structures, generating S-C-like fabric; and (5) formation of C‧-type slip zones, generating well-developed foliation that resembles S-C-C‧-type structures in a ductile environment. Such deformation fabric is mostly imparted by the preferential alignment of intensely comminuted feldspar fragments along thin slip zones developed within deformation bands. These processes were purely mechanical (i.e., grain crushing and reorientation). No clays or fluids were involved in such processes.

  5. Magnetic properties of free alkali and transition metal clusters

    International Nuclear Information System (INIS)

    Heer, W. de; Milani, P.; Chatelain, A.

    1991-01-01

    The Stern-Gerlach deflections of small alkali clusters (N<6) and iron clusters (10< N<500) show that the paramagnetic alkali clusters always have a nondeflecting component, while the iron clusters always deflect in the high field direction. Both of these effects appear to be related to spin relaxation however in the case of alkali clusters it is shown that they are in fact caused by avoided level crossing in the Zeeman diagram. For alkali clusters the relatively weak couplings cause reduced magnetic moments where levels cross. For iron clusters however the total spin is strongly coupled to the molecular framework. Consequently this coupling is responsible for avoided level crossing which ultimately cause the total energy of the cluster to decrease with increasing magnetic field so that the iron clusters will deflect in one direction when introduced in an inhomogeneous magnetic field. Experiment and theory are discussed for both cases. (orig.)

  6. Post-IR IRSL290 dating of K-rich feldspar sand grains in a wind-dominated system on Sardinia

    DEFF Research Database (Denmark)

    Andreucci, S.; Sechi, D.; Buylaert, Jan-Pieter

    2017-01-01

    The reliability of a post-IR elevated temperature IRSL (290 °C; pIRIR290) is tested on wind-blown, sand-sized (180–250 μm) K-rich feldspar grains. The pIRIR290 ages were compared with quartz SAR-OSL data, other independent age controls and historical information. Three study areas along the coast....... The pIRIR290 ages indicate an offset up to ∼1000 years. We can conclude that the pIRIR290 method on sand-sized K-feldspar grains shows great promise for samples at or beyond the quartz OSL age limit but should not be applied to Late Holocene or modern deposits....

  7. Mechanisms of Retinal Damage after Ocular Alkali Burns.

    Science.gov (United States)

    Paschalis, Eleftherios I; Zhou, Chengxin; Lei, Fengyang; Scott, Nathan; Kapoulea, Vassiliki; Robert, Marie-Claude; Vavvas, Demetrios; Dana, Reza; Chodosh, James; Dohlman, Claes H

    2017-06-01

    Alkali burns to the eye constitute a leading cause of worldwide blindness. In recent case series, corneal transplantation revealed unexpected damage to the retina and optic nerve in chemically burned eyes. We investigated the physical, biochemical, and immunological components of retinal injury after alkali burn and explored a novel neuroprotective regimen suitable for prompt administration in emergency departments. Thus, in vivo pH, oxygen, and oxidation reduction measurements were performed in the anterior and posterior segment of mouse and rabbit eyes using implantable microsensors. Tissue inflammation was assessed by immunohistochemistry and flow cytometry. The experiments confirmed that the retinal damage is not mediated by direct effect of the alkali, which is effectively buffered by the anterior segment. Rather, pH, oxygen, and oxidation reduction changes were restricted to the cornea and the anterior chamber, where they caused profound uveal inflammation and release of proinflammatory cytokines. The latter rapidly diffuse to the posterior segment, triggering retinal damage. Tumor necrosis factor-α was identified as a key proinflammatory mediator of retinal ganglion cell death. Blockade, by either monoclonal antibody or tumor necrosis factor receptor gene knockout, reduced inflammation and retinal ganglion cell loss. Intraocular pressure elevation was not observed in experimental alkali burns. These findings illuminate the mechanism by which alkali burns cause retinal damage and may have importance in designing therapies for retinal protection. Copyright © 2017 American Society for Investigative Pathology. Published by Elsevier Inc. All rights reserved.

  8. The Shahewan rapakivi-textured granite – quartz monzonite pluton, Qinling orogen, central China: mineral composition and petrogenetic significance

    Directory of Open Access Journals (Sweden)

    Xiaoxia Wang

    2002-01-01

    Full Text Available The Mesozoic Shahewan pluton consists of four texturally different types of biotite-hornblende quartz monzonite. In the porphyritic types alkali feldspar occurs as euhedral or ovoidal megacrysts that are often mantled by one or more plagioclase shells, and as smaller grains in the groundmass. Quartz, plagioclase (An20–28, biotite, and hornblende occur as inclusions in the alkali feldspar megacrystsand, more abundantly, in the groundmass. Euhedral quartz crystals in the groundmass are not as common and well developed as in typical rapakivi granite. Compared to typical rapakivi granites, the mafic minerals (biotite and hornblende are rich in Mg and poor in Fe, and the whole rock is low in Si, K, F, Ga, Zr, LREE, Fe/Mg, and K/Na. The rocks of the Shahewan pluton are thus regarded as rapakivi-textured quartz monzonites and granites but not true rapakivi granites.

  9. Spectroscopic and Kinetic Measurements of Alkali Atom-Rare Gas Excimers

    Science.gov (United States)

    2009-11-04

    vapors – Exciplex molecules absorb over much greater bandwidth • Control of inherent high optical gain to minimize ASE and optimize laser oscillation... Exciplex assisted diode Pumped Alkali Laser (XPAL) • Education of a future generation of laser scientists VG09-227-2 Physical Sciences Inc. Novel Approach...This new laser exploits the optical properties of weakly-bound alkali/rare-gas exciplexes for pumping the 2P1/2, 3/2 alkali atomic excited states 4

  10. Conduction bands and invariant energy gaps in alkali bromides

    NARCIS (Netherlands)

    Boer, P.K. de; Groot, R.A. de

    1998-01-01

    Electronic structure calculations of the alkali bromides LiBr, NaBr, KBr, RbBr and CsBr are reported. It is shown that the conduction band has primarily bromine character. The size of the band gaps of bromides and alkali halides in general is reinterpreted.

  11. Dating Last Interglacial Coastal Systems Using New Feldspar Luminescence Technologies

    Science.gov (United States)

    Lamothe, M.

    2017-12-01

    The recent explosion in new luminescence dating technologies offers new opportunities to explore Quaternary marine coastal facies and landforms. However, tectonic and climatic processes controlling the development of Pleistocene coastal lithosomes are commonly obscured by their poorly constrained geological age. Luminescence dating of feldspar probes one order of magnitude deeper into geological time than radiocarbon and more than 5 times the current age range of quartz optically-stimulated luminescence, routinely used in luminescence dating. However, feldspar luminescence stimulated by infrared photons (eg IRSL) is hampered by anomalous fading. Successful correction methods developed by us over the last 15 years did produce sound chronologies but the fading-corrected ages carried large uncertainties. New approaches initiated by other laboratories, mainly in Europe, have isolated high temperature post-IRSL luminescence as this signal seems to be only slightly affected by fading. However, the gain in stability seems to be lessened due to bleachibility issues, generating age overestimations. We developed a novel protocol known as post-isothermal IRSL dating (Pit-IR) that focuses on a dual system of luminescence signals, probing low (50C) and medium (225C) temperature IRSL signals following isothermal treatments of various intensities. These protocols have been tested on Last interglacial coastal sediments in strikingly different GIA contexts along the Atlantic coastal areas of SE USA as well as from Morocco, Brazil and LIG sites in the Mediterranean basin. A systematic analysis of these results would suggest that a) falling-stages sequences are more commonly preserved as the OSL/IRSL ages are preferentially dating from the end of the MIS5e high stand and b) MIS5a marine sediments may be detectable away from areas generally thought to be affected by peripheral bulge collapse.

  12. Alkali cyanides; destructive distillation

    Energy Technology Data Exchange (ETDEWEB)

    Clancy, J C

    1925-12-02

    The destructive distillation of carbonaceous substances can be accomplished by heating them in a bath of molten alkali and cyanide. Liquid hydrocarbons are produced. The separation of the cyanide from the coke or carbonaceous residues by filtration leaves a substantial quantity of cyanide absorbed by the carbon. A feasible method for removal has been developed by mixing the mixture of cyanide and coke with sodium carbonate or other alkali in the molten state, then treating this substance with nitrogen with or without ammonia to convert most of the carbon to cyanide. The carbonaceous material may be mixed with a liquid hydrocarbon such as petroleum, shale oil, or heavy tar oil, heated, and introduced below the surface of the liquid cyanide which partially decomposes and hydrogenates the coal to increase the yield of hydrocarbons. Dry ammonia may be bubbled through the reaction mixture to effect agitation and to form more cyanide.

  13. Binding of chloride and alkalis in Portland cement systems

    International Nuclear Information System (INIS)

    Nielsen, Erik P.; Herfort, Duncan; Geiker, Mette R.

    2005-01-01

    A thermodynamic model for describing the binding of chloride and alkalis in hydrated Portland cement pastes has been developed. The model is based on the phase rule, which for cement pastes in aggressive marine environment predicts multivariant conditions, even at constant temperature and pressure. The effect of the chloride and alkalis has been quantified by experiments on cement pastes prepared from white Portland cements containing 4% and 12% C 3 A, and a grey Portland cement containing 7% C 3 A. One weight percent calcite was added to all cements. The pastes prepared at w/s ratio of 0.70 were stored in solutions of different Cl (CaCl 2 ) and Na (NaOH) concentrations. When equilibrium was reached, the mineralogy of the pastes was investigated by EDS analysis on the SEM. A well-defined distribution of chloride was found between the pore solution, the C-S-H phase, and an AFm solid solution phase consisting of Friedel's salt and monocarbonate. Partition coefficients varied as a function of iron and alkali contents. The lower content of alkalis in WPC results in higher chloride contents in the C-S-H phase. High alkali contents result in higher chloride concentrations in the pore solution

  14. 40 CFR 721.2565 - Alkylated sulfonated diphenyl oxide, alkali and amine salts.

    Science.gov (United States)

    2010-07-01

    ..., alkali and amine salts. 721.2565 Section 721.2565 Protection of Environment ENVIRONMENTAL PROTECTION... New Uses for Specific Chemical Substances § 721.2565 Alkylated sulfonated diphenyl oxide, alkali and... substances identified as alkylated sulfonated diphenyl oxide, alkali salt (PMN P-93-352) and alkylated...

  15. The release of iron-bearing minerals and dissolution of feldspars by heterotrophic bacteria of Bacillus species

    Czech Academy of Sciences Publication Activity Database

    Štyriaková, I.; Štyriak, I.; Galko, I.; Hradil, David; Bezdička, Petr

    2003-01-01

    Roč. 47, č. 1 (2003), s. 20-26 ISSN 0862-5468 Grant - others:AV SR(SK) 2/2107/22; GA SR(SK) 73/2000 Institutional research plan: CEZ:AV0Z4032918 Keywords : bioleaching * feldspars * Bacillus Subject RIV: CA - Inorganic Chemistry Impact factor: 0.449, year: 2003

  16. Thermochemical properties of the alkali hydroxides: A review

    International Nuclear Information System (INIS)

    Konings, R.J.M.; Cordfunke, E.H.P.

    1989-01-01

    The formation of volatile alkali hydroxides as a result of high-temperature steam corrosion plays an important role in nuclear technology. For the modeling of the volatilization processes, reliable thermodynamic data are required. In the present paper recent physico-chemical experiments by the authors will be discussed and the thermochemical properties of the alkali hydroxide series will be evaluated. (orig.)

  17. Possible applications of alkali-activated systems in construction

    OpenAIRE

    Boháčová, J.; Staněk, S.; Vavro, M. (Martin)

    2013-01-01

    This paper deals with the possibilities of using alkali-activated systems in construction. This article summarizes the advantages and disadvantages of geopolymer in comparison to Portland cement, summarizes research and practical applications of alkali-activated materials in our country and abroad, and provides an overview of directions where these alternative inorganic binders can be in the future very well applied.

  18. Accumulated phenocrysts and origin of feldspar porphyry in the Chanho area, western Yunnan, China

    Science.gov (United States)

    Xu, Xing-Wang; Jiang, Neng; Yang, Kai; Zhang, Bao-Lin; Liang, Guang-He; Mao, Qian; Li, Jin-Xiang; Du, Shi-Jun; Ma, Yu-Guang; Zhang, Yong; Qin, Ke-Zhang

    2009-12-01

    The No. 1 feldspar porphyry in the Chanho area, western Yunnan, China is characterized by the development of deformed glomeroporphyritic aggregates (GA) that contain diagnostic gravity settling textures. These textures include interlocking curved grain boundaries caused by compaction, bent twins, and arch-like structures. The GAs are accumulated phenocrysts (AP) and antecrysts. The unstable textural configurations such as extensive penetrative microfractures that are restricted within the AP and fractured cores of zircon grains, all suggest that the GAs are transported fragments of fractured cumulates that formed in a pre-emplacement magma chamber rather than form in situ at the current intrusion site. Compositions of minerals and melt as represented by different mineral aggregates formed at various stages of the magmatic process and their relations to the composition of porphyry bodies in the Chanho area indicate that the porphyritic melt for the No. 1 feldspar porphyry experienced two stages of melt mixing. Pulses of potassic melt flowed into a pre-emplacement magma chamber and mixed with crystallizing dioritic magma containing phenocrysts resulted in the first hybrid alkaline granitic melt. The mixing caused denser phenocrysts to settle and aggregate to form cumulates. Secondly, new dioritic melt was injected into the magma chamber and was mixed with the previously formed hybrid alkaline granitic melt to produce syenitic melt. Geochron data, including U-Pb age of zircon and 39Ar/ 40Ar age of hornblende and oligoclase phenocrysts, indicate that hornblende and oligoclase phenocrysts, as well as the core of zircon grains, were antecrysts that formed in a number of crystallization events between 36.3 and 32.78 Ma. Gravity settling of phenocrysts took place at about 33.1 to 32.78 Ma and melts with deformed GAs were transported upwards and emplaced into the current site at 32 Ma. Results of this research indicate that the No. 1 feldspar porphyry was a shallow

  19. Continuing studies of alkali-aggregate reactions in concrete

    International Nuclear Information System (INIS)

    Gilliot, J.E.; Beddoes, R.J.

    1981-01-01

    Studies are continuing into the nature of the different forms of the alkali-aggregate reaction. No general agreement exists as to the detailed nature of the expansive mechanisms. Alkali is known to react internally with opaline silica because of its microporous nature whereas reaction at the external surface is thought to be relatively more important in the case of quartz. A combination of Fourier shape and surface texture analysis, microscopy and osmotic studies is being used to obtain information on the relative importance of these two forms of alkaline attack on silica. Analytical methods are much more rapid than dimensional change tests and it is hoped that a better understanding of the expansion mechanism will lead to more certain recognition of potentially alkali expansive aggregates

  20. Investigations of the post-IR IRSL protocol applied to single K-feldspar grains from fluvial sediment samples

    International Nuclear Information System (INIS)

    Nian, Xiaomei; Bailey, Richard M.; Zhou, Liping

    2012-01-01

    The post-IR IRSL protocol with single K-feldspar grains was applied to three samples taken from a fluvial sedimentary sequence at the archaeological site of the Dali Man, Shaanxi Province, China. K-feldspar coarse grains were extracted for measurement. Approximately 30–40% of the grains were sufficiently bright to measure, and after application of rejection criteria based on signal strength, recuperation, recycling ratio and saturation dose, ∼10–15% of the grains were used for D e calculation. The relationship of signal decay rate and form of D e (t) with the recovery dose were investigated. The dose recovery ratios of the samples after initial bleaching with the four different light sources were within uncertainties of unity. No anomalous fading was observed. The over-dispersion of the recovered dose and D e values were similar, suggesting neither incomplete resetting of the post-IR IRSL signals nor spatially heterogeneous dose rates significantly affected the natural dose estimates. The values of D e obtained with the single K-feldspar grain post-IR IRSL protocol were in the range ∼400–490 Gy. Combining all of the measured single-grain signals for each of the individual samples (into a ‘synthetic single aliquot’) increased the D e estimates to the range ∼700–900 Gy, suggesting that the grains screened-out by the rejection criteria may have the potential to cause palaeodose over-estimation, although this finding requires a more extensive investigation. Thermally transferred signals were found in the single K-feldspar grains post-IR IRSL protocol, and the proportion of thermally transferred signal to test-dose OSL signal (stimulation at 290 °C) from the natural dose was higher than from regenerative doses, and the proportion was grain- and dose-dependent. As such, TT-post-IR IRSL signals at 290 °C have the potential to cause dose underestimation, although this may be reduced by using larger test-dose irradiations. Our study demonstrates

  1. The effects of potassium and rubidium hydroxide on the alkali-silica reaction

    International Nuclear Information System (INIS)

    Shomglin, K.; Turanli, L.; Wenk, H.-R.; Monteiro, P.J.M.; Sposito, G.

    2003-01-01

    Expansion of mortar specimens prepared with an aggregate of mylonite from the Santa Rosa mylonite zone in southern California was studied to investigate the effect of different alkali ions on the alkali-silica reaction in concrete. The expansion tests indicate that mortar has a greater expansion when subjected to a sodium hydroxide bath than in a sodium-potassium-rubidium hydroxide bath. Electron probe microanalysis (EPMA) of mortar bars at early ages show that rubidium ions, used as tracer, were present throughout the sample by the third day of exposure. The analysis also shows a high concentration of rubidium in silica gel from mortar bars exposed to bath solutions containing rubidium. The results suggest that expansion of mortar bars using ASTM C 1260 does not depend on the diffusion of alkali ions. The results indicate that the expansion of alkali-silica gel depends on the type of alkali ions present. Alkali-silica gel containing rubidium shows a lower concentration of calcium, suggesting competition for the same sites

  2. Properties of Hooked Steel Fibers Reinforced Alkali Activated Material Concrete

    OpenAIRE

    Faris M. A.; Abdullah Mohd Mustafa Al Bakri; Ismail Khairul Nizar; Muniandy Ratnasamy; Mahmad Nor Aiman; Putra Jaya Ramadhansyah; Waried Wazien A. Z.

    2016-01-01

    In this study, alkali activated material was produced by using Class F fly ash from Manjung power station, Lumut, Perak, Malaysia. Fly ash then was activated by alkaline activator which is consisting of sodium silicate (Na2SiO3) and sodium hydroxide (NaOH). Hooked end steel fibers were added into the alkali activated material system with percentage vary from 0 % – 5 %. Chemical compositions of fly ash were first analyzed by using x-ray fluorescence (XRF). All hardened alkali activated materia...

  3. Behaviour of gaseous alkali compounds in coal gasification; Kaasumaisten alkaliyhdisteiden kaeyttaeytyminen kivihiilien kaasutuksessa

    Energy Technology Data Exchange (ETDEWEB)

    Nykaenen, J [Imatran Voima Oy, Vantaa (Finland)

    1997-10-01

    In this project the behaviour of alkali compounds emitting from CO{sub 2}/O{sub 2}- and airblown gasification are studied. This research project is closely connected to an EU-project coordinated by the Delft University of Technology (DUT). In that project alkali emissions from a 1.6 MW pilot plant will be measured. The results from those measurements will be compared with the calculations performed in this LIEKKI 2 project. The equilibrium calculations show that the major gaseous alkali compounds emitting from combustion and gasification are chlorides and hydroxides. This applies both to air- and CO{sub 2}/O{sub 2}-blown processes. In all the cases studied the concentration of gaseous alkali compounds is determined mainly by the amount of chlorides. The key parameters, with respect to alkali behaviour, are the temperature of the process and chlorine content of the coal. By cooling the gases down to 600 deg C prior to a ceramic filter the alkali concentration can be kept about at 100 ppbv. In combustion, the addition of calcium carbonate increases the amount of gaseous alkali compounds by decreasing the amount of alkali sulphates. In the case of gasification the importance of limestone is negligible. The difference between air- and CO{sub 2}/O{sub 2}-blown processes, in terms of gaseous alkali emissions, is small. This is because CO{sub 2} concentration of the gas does not have a strong impact on alkali chlorides. Furthermore, the effect of CO{sub 2}/O{sub 2}-ratio of the recirculation process is negligible. (orig.)

  4. An automated procedure for themoluminescence dating of pottery and burnt stones

    International Nuclear Information System (INIS)

    Mejdahl, V.

    1982-01-01

    An automated procedure for dating of quartz and feldspar inclusions in pottery has been developed and tested in a comprehensive programme comprising material from a number of well-dated Danish sites. The results indicate that TL dating of pottery can now be carried out on a routine basis with an accuracy of about 5%. Experiments on dating of large grains of alkali feldspars extracted from burnt stones are described. The results are encouraging and show that the method may enable a reduction of some of the uncertainties associated with the conventional inclusion technique. (author)

  5. Defluidization in fluidized bed gasifiers using high-alkali content fuels

    DEFF Research Database (Denmark)

    Narayan, Vikas; Jensen, Peter Arendt; Henriksen, Ulrik Birk

    2016-01-01

    samples,agglomeration could be attributed to viscous silicate melts formed from reaction of inorganic alkalineand alkali earth species with silica from the bed particles. A mathematical model that addresses the defluidization behavior of alkali-rich samples was developed based on the experiments performed...... and calcium, which may form viscous melts that adhere on the surface of the colliding bed particles and bind them to form agglomerates. In this paper, studies were made to understand the behavior of inorganic elements (mainly K, Si and Ca) on agglomeration and de-fluidization of alkali rich bed...... in the bench-scale fluidized bed reactor as well as on results from literature. The model was then used topredict the de-fluidization behavior of alkali-rich bed material in a large-scale LTCFB gasifier....

  6. Spectra of alkali atoms

    International Nuclear Information System (INIS)

    Santoso, Budi; Arumbinang, Haryono.

    1981-01-01

    Emission spectra of alkali atoms has been determined by using spectrometer at the ultraviolet to infra red waves range. The spectra emission can be obtained by absorption spectrophotometric analysis. Comparative evaluations between experimental data and data handbook obtained by spark method were also presented. (author tr.)

  7. Control of alkali species in gasification systems: Final report

    Energy Technology Data Exchange (ETDEWEB)

    Turn, S.; Kinoshita, C.; Ishimura, D. Zhou, J.; Hiraki, T.; Masutani, S.

    2000-07-13

    Gas-phase alkali metal compounds contribute to fouling, slagging, corrosion, and agglomeration problems in energy conversion facilities. One mitigation strategy applicable at high temperature is to pass the gas stream through a fixed bed sorbent or getter material, which preferentially absorbs alkali via physical adsorption or chemisorption. This report presents results of an experimental investigation of high-temperature alkali removal from a hot filtered gasifier product gas stream using a packed bed of sorbent material. Two getter materials, activated bauxite and emathlite, were tested at two levels of space time by using two interchangeable reactors of different internal diameters. The effect of getter particle size was also investigated.

  8. Sputtering/redeposition analysis of alkali-based tungsten composites for limiter/divertor applications

    International Nuclear Information System (INIS)

    DeWald, A.B.; Krauss, A.R.; Gruen, D.M.; Valentine, M.G.

    1986-07-01

    Composites of porous tungsten infiltrated with alkali metal-bearing alloys have been projected as a means of reducing plasma impurities and sputter erosion in magnetic fusion devices. Self-sustaining alkali metal overlayers have been observed to inhibit erosion of the underlying structural substrate by 2X to 10X. The alkali metal itself, insofar as it sputters as a secondary ion, is trapped at the surface by sheath potential and tangential magnetic fields. Self-regeneration of the alkali metal coating is obtained by thermal and radiation-induced segregation from the bulk

  9. Alkali based slagging: a case study from Leigh Creek

    Energy Technology Data Exchange (ETDEWEB)

    R.A. Creelman; J. Bamberry; L.A. Juniper; C. Ward [University of Western Sydney, Penrith South, NSW (Australia)

    2003-07-01

    A systematic study was undertaken at NRG Port Augusta Power station in South Australia to determine the cause of ash deposition (slagging) in the boilers. Conventional wisdom suggests that iron in the ash is generally a major player in furnace ash deposition; however, mineralogical and chemical analyses of the deposits showed that the binding phase was plagioclase feldspar, dominated by the sodic feldspar albite. The study resulted in recognition that the cause of the formation of ash deposits in the North Flinders furnaces was the result of the ingestion of sodium and calcium into the melt that bound the deposits. This finding was a breakthrough in understanding the deposition process within these furnaces, and emphasises that not all slagging is iron related and that systematic studies of deposits, coal and ash make fundamental contributions to understanding the ash deposition mechanisms. 9 refs., 5 figs., 2 tabs.

  10. Citrate, malate and alkali content in commonly consumed diet sodas: implications for nephrolithiasis treatment.

    Science.gov (United States)

    Eisner, Brian H; Asplin, John R; Goldfarb, David S; Ahmad, Ardalanejaz; Stoller, Marshall L

    2010-06-01

    Citrate is a known inhibitor of calcium stone formation. Dietary citrate and alkali intake may have an effect on citraturia. Increasing alkali intake also increases urine pH, which can help prevent uric acid stones. We determined citrate, malate and total alkali concentrations in commonly consumed diet sodas to help direct dietary recommendations in patients with hypocitraturic calcium or uric acid nephrolithiasis. Citrate and malate were measured in a lemonade beverage commonly used to treat hypocitraturic calcium nephrolithiasis and in 15 diet sodas. Anions were measured by ion chromatography. The pH of each beverage was measured to allow calculation of the unprotonated anion concentration using the known pK of citric and malic acid. Total alkali equivalents were calculated for each beverage. Statistical analysis was done using Pearson's correlation coefficient. Several sodas contained an amount of citrate equal to or greater than that of alkali and total alkali as a lemonade beverage commonly used to treat hypocitraturic calcium nephrolithiasis (6.30 mEq/l citrate as alkali and 6.30 as total alkali). These sodas were Diet Sunkist Orange, Diet 7Up, Sprite Zero, Diet Canada Dry Ginger Ale, Sierra Mist Free, Diet Orange Crush, Fresca and Diet Mountain Dew. Colas, including Caffeine Free Diet Coke, Coke Zero, Caffeine Free Diet Pepsi and Diet Coke with Lime, had the lowest total alkali (less than 1.0 mEq/l). There was no significant correlation between beverage pH and total alkali content. Several commonly consumed diet sodas contain moderate amounts of citrate as alkali and total alkali. This information is helpful for dietary recommendations in patients with calcium nephrolithiasis, specifically those with hypocitraturia. It may also be useful in patients with low urine pH and uric acid stones. Beverage malate content is also important since malate ingestion increases the total alkali delivered, which in turn augments citraturia and increases urine pH. Copyright

  11. Degradation of cellulosic materials under the alkaline conditions of a cementitious repository for low- and intermediate level radioactive waste. Pt. III. Effect of degradation products on the sorption of radionuclides on feldspar

    International Nuclear Information System (INIS)

    Loon, L.R. van; Glaus, M.A.; Laube, A.; Stallone, S.

    1999-01-01

    The effect of degradation products of different cellulosic materials on the sorption behaviour of Th(IV), Eu(III) and Ni(II) on feldspar at pH 13.3 was studied. For all three metals, a decrease in sorption could be observed with increasing concentration of organics in solution. For Th(IV), α-ISA is the effective ligand present in the solutions of degraded cellulose, independent on the type of cellulose studied. For Eu(III), α-ISA is the effective ligand in the case of pure cellulose degradation. In the case of other cellulosic materials, unknown ligands cause the sorption reduction. For Ni(II), also unknown ligands cause sorption reduction, independent on the type of cellulose studied. These unknown ligands are not formed during alkaline degradation of cellulose, but are present as impurities in certain cellulosic materials. (orig.)

  12. Mineral shock signatures in rocks from Dhala (Mohar) impact structure, Shivpuri district, Madhya Pradesh, India

    Science.gov (United States)

    Roy, Madhuparna; Pandey, Pradeep; Kumar, Shailendra; Parihar, P. S.

    2017-12-01

    A concrete study combining optical microscopy, Raman spectroscopy and X-ray diffractometry, was carried out on subsurface samples of basement granite and melt breccia from Mohar (Dhala) impact structure, Shivpuri district, Madhya Pradesh, India. Optical microscopy reveals aberrations in the optical properties of quartz and feldspar in the form of planar deformation feature-like structures, lowered birefringence and mosaics in quartz, toasting, planar fractures and ladder texture in alkali feldspar and near-isotropism in bytownite. It also brings to light incidence of parisite, a radioactive rare mineral in shocked granite. Raman spectral pattern, peak positions, peak widths and multiplicity of peak groups of all minerals, suggest subtle structural/crystallographic deviations. XRD data further reveals minute deviations of unit cell parameters of quartz, alkali feldspar and plagioclase, with respect to standard α-quartz, high- and low albite and microcline. Reduced cell volumes in these minerals indicate compression due to pressure. The c0/a0 values indicate an inter-tetrahedral angle roughly between 120o and 144o, further pointing to a possible pressure maxima of around 12 GPa. The observed unit cell aberration of minerals may indicate an intermediate stage between crystalline and amorphous stages, thereby, signifying possible overprinting of decompression signatures over shock compression effects, from a shock recovery process.

  13. Language and Style in Zaynab Alkali's The Stillborn | Azuike ...

    African Journals Online (AJOL)

    This paper examines the language and style of Zaynab Alkali's The Stillborn. Alkali's style in The Stillborn lies in her effective deployment of linguo-literary resources to tell the story. The study scrutinizes the nexus of figures of speech and linguistic artifacts, which link the events and characters that populate her novel and ...

  14. Stoneware tile manufacturing using rice straw ash as feldspar replacement; Fabricacion de gres porcelanico empleando ceniza de tamo de arroz en sustitucion del feldespato

    Energy Technology Data Exchange (ETDEWEB)

    Alvaro Guzman, A.; John Torres, L.; Martha Cedeno, V.; Silvio Delvasto, A.; Vicente Amigo, B.; Enrique Sanchez, V.

    2013-07-01

    In this research are presented the results of using rice straw ash (RSA) in low proportions as substitute of feldspar for manufacturing stoneware tiles. Specimens of semidry triaxial mixtures, where feldspar was substituted for different percentages (25 % and 50 %) of RSA, were prepared by uniaxial pressing, followed by drying and sintering. Physical and mechanical properties of sintered bodies were evaluated. Porcelain stoneware tile specimens C0 and CF25 reached bending strength and water absorption values were in accordance with standard ISO 13006 (Annex G, BIa) ( {>=} 35 MPa and {<=} 0.5 %, respectively). However, in porcelain stoneware tile specimens CF50 due to bloating phenomenon was not possible obtain commercial tiles in accordance with standard ISO 13006. By using Scanning Electron Microscopy (SEM) needles of primary and secondary mullite were identified in a vitreous phase; and by using X-Ray Diffraction (XRD) mullite and quartz phases were identified. It was concluded that feldspar can be substituted positively by RSA in stoneware tile pastes. (Author)

  15. A procedure for preparing alkali metal hydrides

    International Nuclear Information System (INIS)

    Lemieux, R.U.; Sanford, C.E.; Prescott, J.F.

    1976-01-01

    A plain low cost, procedure for the continuous, low temperature preparation of sodium or potassium hydrides using cheap reagents is presented. Said invention is especially concerned with a process of purifying of a catalytic exchange liquid used for deuterium enrichment, in which an alkali metal hydride is produced as intermediate product. The procedure for producing the sodium and potassium hydrides consists in causing high pressure hydrogen to be absorbed by a mixture of at least a lower monoalkylamine and an alkylamide of an alkali metal from at least one of said amines [fr

  16. Comparative study of ice nucleating efficiency of K-feldspar in immersion and deposition freezing modes

    Science.gov (United States)

    Hiron, T.; Hoffmann, N.; Peckhaus, A.; Kiselev, A. A.; Leisner, T.; Flossmann, A. I.

    2016-12-01

    One of the main challenges in understanding the evolution of Earth's climate resides in the understanding the role of ice nucleation on the development of tropospheric clouds as well as its initiation. K-feldspar is known to be a very active ice nucleating particle and this study focuses on the characterization of its activity in two heterogeneous nucleation modes, immersion and deposition freezing.We use a newly built humidity-controlled cold stage allowing the simultaneous observation of up to 2000 identical 0.6-nanoliter droplets containing suspension of mineral dust particles. The droplets are first cooled down to observe immersion freezing, the obtained ice crystals are then evaporated and finally, the residual particles are exposed to the water vapor supersaturated with respect to ice.The ice nucleation abilities for the individual residual particles are then compared for the different freezing modes and correlation between immersion ice nuclei and deposition ice nuclei is investigated.Based on the electron microscopy analysis of the residual particles, we discuss the possible relationship between the ice nucleation properties of feldspar and its microstructure. Finally, we discuss the atmospheric implications of our experimental results, using DESCAM, a 1.5D bin-resolved microphysics model.

  17. Density functional study of ferromagnetism in alkali metal thin films

    Indian Academy of Sciences (India)

    thickness uniform jellium model (UJM), and it is argued that within LSDA or GGA, alkali metal thin films cannot be claimed to have an FM ground state. Relevance of these results to the experiments on transition metal-doped alkali metal thin films ...

  18. Neuropsychiatric manifestations of alkali metal deficiency and excess

    Energy Technology Data Exchange (ETDEWEB)

    Yung, C.Y.

    1984-01-01

    The alkali metals from the Group IA of the periodic table (lithium, sodium, potassium, rubidium, cesium and francium) are reviewed. The neuropsychiatric aspects of alkali metal deficiencies and excesses (intoxications) are described. Emphasis was placed on lithium due to its clinical uses. The signs and symptoms of these conditions are characterized by features of an organic brain syndrome with delirium and encephalopathy prevailing. There are no clinically distinctive features that could be reliably used for diagnoses. Sodium and potassium are two essential alkali metals in man. Lithium is used as therapeutic agent in bipolar affective disorders. Rubidium has been investigated for its antidepressant effect in a group of psychiatric disorders. Cesium is under laboratory investigation for its role in carcinogenesis and in depressive illness. Very little is known of francium due to its great instability for experimental study.

  19. Structural Investigation of Alkali Activated Clay Minerals for Application in Water Treatment Systems

    Science.gov (United States)

    Bumanis, G.; Bajare, D.; Dembovska, L.

    2015-11-01

    Alkali activation technology can be applied for a wide range of alumo-silicates to produce innovative materials with various areas of application. Most researches focuse on the application of alumo-silicate materials in building industry as cement binder replacement to produce mortar and concrete [1]. However, alkali activation technology offers high potential also in biotechnologies [2]. In the processes where certain pH level, especially alkaline environment, must be ensured, alkali activated materials can be applied. One of such fields is water treatment systems where high level pH (up to pH 10.5) ensures efficient removal of water pollutants such as manganese [3]. Previous investigations had shown that alkali activation technology can be applied to calcined clay powder and aluminium scrap recycling waste as a foam forming agent to create porous alkali activated materials. This investigation focuses on the structural investigation of calcined kaolin and illite clay alkali activation processes. Chemical and mineralogical composition of both clays were determined and structural investigation of alkali activated materials was made by using XRD, DTA, FTIR analysis; the microstructure of hardened specimens was observed by SEM. Physical properties of the obtained material were determined. Investigation indicates the essential role of chemical composition of the clay used in the alkali activation process, and potential use of the obtained material in water treatment systems.

  20. Structural, elastic, electronic and optical properties of bi-alkali ...

    Indian Academy of Sciences (India)

    The structural parameters, elastic constants, electronic and optical properties of the bi-alkali ... and efficient method for the calculation of the ground-state ... Figure 2. Optimization curve (E–V) of the bi-alkali antimonides: (a) Na2KSb, (b) Na2RbSb, (c) Na2CsSb, .... ical shape of the charge distributions in the contour plots.

  1. Gamma-spectrometric surveys in differentiated granites. II: the Joaquim Murtinho Granite in the Cunhaporanga Granitic Complex, Parana, SE Brazil; Levantamentos gamaespectrometricos em granitos diferenciados. II: O exemplo do Granito Joaquim Murtinho, Complexo Granitico Cunhaporanga, Parana

    Energy Technology Data Exchange (ETDEWEB)

    Ferreira, Francisco Jose Fonseca [Universidade Federal do Parana (UFPR), Curitiba, PR (Brazil). Dept. de Geologia. Lab. de Pesquisas em Geofisica Aplicada; Fruchting, Allan [Votorantim Metais, Sao Paulo, SP (Brazil)], e-mail: allan.fruchting@vmetais.com.br; Guimaraes, Gilson Burigo [Universidade Estadual de Ponta Grossa (UEPG), PR (Brazil). Dept. de Geociencias], e-mail: gburigo@ig.com.br; Alves, Luizemara Soares [PETROBRAS S.A., Rio de Janeiro, RJ (Brazil)], e-mail: luizemara@petrobras.com.br; Martin, Victor Miguel Oliveira; Ulbrich, Horstpeter Herberto Gustavo Jose [Universidade de Sao Paulo (USP), SP (Brazil). Inst. de Geociencias. Dept. de Mineralogia e Geotectonica], e-mail: vicmartin6@ig.com.br, e-mail: hulbrich@usp.br

    2009-07-01

    Detailed mapping at the NW corner of the large Neo proterozoic Cunhaporanga Granitic Complex (CGC), Parana state, SE Brazil, redefined the Joaquim Murtinho Granite (JMG), a late intrusion in CGC with an exposed area of about 10 km{sup 2}, made up mainly by evolved 'alaskites' (alkali-feldspar leuco granites). This unit is in tectonic contact with the Neoproterozoic-Eocambrian volcano-sedimentary Castro Group, to the W, and is intrusive into other less evolved granitic units of the CGC to the E. Petrographically, JMG shows mainly mesoperthite and quartz, with subordinate amounts of altered micas and some accessory phases, mainly zircon. The equi to inequigranular granites are usually deformed with cataclastic textures, are often brecciated, and may have miarolitic structures. Formation of late albite, sericite, carbonate and hematite was caused by deuteric and hydrothermal alteration. A gamma-ray spectrometric survey at 231 stations which measured total counts (TC), Ueq K%, eU ppm and eTh ppm was used to construct several direct and derived maps. Compared to neighboring units the JMG has significant anomalies, especially in the TC, %K, eTh and eU maps, although the differences are less obvious in some derived maps. These evolved granites are enriched in these three elements. Geochemical behavior of K, Th and U is used to analyse the results observed in maps. Enhanced weathering under a subtropical climate with moderate to high average temperatures and heavy rainfall affects mainly feldspars and biotite, and may also destabilize most U and Th-bearing accessory phases. Th is most likely retained in restite minerals in soils, being relatively immobile, while part of U may migrate as uranyl ion in oxidizing media. K is especially affected by feldspar alteration to K-free clays (mainly kaolinite), and may be completely leached. Gamma-ray spectrometric methods are valid tools to study facies in granitic rocks, especially in those that are enriched in K, Th and U

  2. Photoemission spectroscopy study of a multi-alkali photocathode

    CERN Document Server

    Ettema, A R H

    2000-01-01

    In this paper a photoemission study of the highest core levels of the elements and the electron escape barrier (work function) in a multi-alkali photocathode are presented. The core levels indicate that the alkali atoms are in an oxidized state and therefore the compound Na sub 2 KSb can be regarded as an ionic semiconductor. The measured escape barrier of the Cs sub 2 O surface layer is determined as 2.3 eV.

  3. Study of sensitivity change of OSL signals from quartz and feldspars as a function of preheat temperature

    DEFF Research Database (Denmark)

    Jungner, H.; Bøtter-Jensen, L.

    1994-01-01

    and as a result, the equivalent dose (ED) would be underestimated. A study of sensitivity changes in feldspars and quartz was carried out with emphasis on the effect of preheat and annealing on the OSL signal. Measurement results obtained are presented, and possible elimination of errors in dating caused...

  4. Effects of alkali and steaming on mechanical properties of snake fruit (Salacca) fiber

    Science.gov (United States)

    Darmanto, Seno; Rochardjo, Heru S. B.; Jamasri, Widyorini, Ragil

    2017-01-01

    The aim of this research is to investigate the effect of alkali treatment and steaming on mechanical properties of Snake Fruit frond fiber. The presence of surface impurities and a lot of hydroxyl groups makes natural fiber less compatible for composite materials reinforcement. Efforts to remove the impurities can be done by physical, chemical and mechanical treatments. This paper reports the treatment of Snake Fruit frond single fiber by subjecting it to alkali treatments with 2%- 8% NaOH for 2 - 6 hours at room temperature. The treatment is then followed by steaming at a pressure of 2 bars in 1 hour. Results show that the treatment of alkali and the alkali-steaming combination can increase cellulose percentage. The tensile tests show that this type of treatment in combination resulted in the higher tensile strength compared to untreated fiber. There is a significant increase in tensile strength with increasing alkali percentage. However, the further increase in the percentage of alkali solution will result in decreasing tensile strength. The highest value of tensile strength after treatment was 275 MPa with 6 hours treatment at alkali percentage of 2 %.

  5. Structure of xanthan gum and cell ultrastructure at different times of alkali stress.

    Science.gov (United States)

    Luvielmo, Márcia de Mello; Borges, Caroline Dellinghausen; Toyama, Daniela de Oliveira; Vendruscolo, Claire Tondo; Scamparini, Adilma Regina Pippa

    2016-01-01

    The effect of alkali stress on the yield, viscosity, gum structure, and cell ultrastructure of xanthan gum was evaluated at the end of fermentation process of xanthan production by Xanthomonas campestris pv. manihotis 280-95. Although greater xanthan production was observed after a 24h-alkali stress process, a lower viscosity was observed when compared to the alkali stress-free gum, regardless of the alkali stress time. However, this outcome is not conclusive as further studies on gum purification are required to remove excess sodium, verify the efficiency loss and the consequent increase in the polymer viscosity. Alkali stress altered the structure of xanthan gum from a polygon-like shape to a star-like form. At the end of the fermentation, early structural changes in the bacterium were observed. After alkali stress, marked structural differences were observed in the cells. A more vacuolated cytoplasm and discontinuities in the membrane cells evidenced the cell lysis. Xanthan was observed in the form of concentric circles instead of agglomerates as observed prior to the alkali stress. Copyright © 2015 Sociedade Brasileira de Microbiologia. Published by Elsevier Editora Ltda. All rights reserved.

  6. The influence of polycarboxylate-type super-plasticizers on alkali-free liquid concrete accelerators performance

    Science.gov (United States)

    Guo, Wenkang; Yin, Haibo; Wang, Shuyin; He, Zhifeng

    2017-04-01

    Through studying on the setting times, cement mortar compressive strength and cement mortar compressive strength ratio, the influence of alkali-free liquid accelerators polycarboxylate-type super-plasticizers on the performance of alkali-free liquid accelerators in cement-based material was investigated. The results showed that the compatibility of super-plasticizers and alkali-free liquid accelerators was excellent. However, the dosage of super-plasticizers had a certain impact on the performance of alkali-free liquid accelerators as follows: 1) the setting times of alkali-free liquid accelerators was in the inverse proportional relationship to the dosage of super-plasticizers; 2)the influence of super-plasticizers dosage on the cement mortar compressive strength of alkali-free liquid accelerators was related to the types of accelerators, where exist an optimum super-plasticizers dosage for cement mortar compressive strength at 28d; 3)the later cement mortar compressive strength with alkali-free liquid accelerators were decreasing with the increment of the super-plasticizers dosage. In the practical application of alkali-free liquid accelerators and super-plasticizer, the dosage of super-plasticizer must be determined by dosage optimization test results.

  7. Petrological and geochemical studies of alkaline rocks from continental Brazil. 8. The syenitic intrusion of Morro Redondo, RJ

    International Nuclear Information System (INIS)

    Brotzu, P.; Melluso, L.; Beccaluva, L.

    1989-01-01

    The alkaline complex of Morro Redondo is mainly composed of syenites, alkali syenites and nepheline syenites. The age of the intrusion, utilizing eleven newly available K/Ar data, is about 73 Ma. Petrography, mineral chemistry and geochemistry strongly support cogeneticity among the various lithotypes, linked by fractional crystallisation of the observed phases and crystal accumulation, preferentially of alkali feldspar. Initial Sr isotopic ratios indicate a mantle parental magma, probably generated in the subcontinental lithosphere, like other Brazilian alkaline complexes (e.g. Fortaleza, Juquia, Piratini, Tunas). (author) [pt

  8. [Using a modified remote sensing imagery for interpreting changes in cultivated saline-alkali land].

    Science.gov (United States)

    Gao, Hui; Liu, Hui-tao; Liu, Hong-juan; Liu, Jin-tong

    2015-04-01

    This paper developed a new interpretation symbol system for grading and classifying saline-alkali land, using Huanghua, a cosatal city in Hebei Province as a case. The system was developed by inverting remote sensing images from 1992 to 2011 based on site investigation, plant cover characteristics and features of remote sensing images. Combining this interpretation symbol system with supervising classification method, the information on arable land was obtained for the coastal saline-alkali ecosystem of Huanghua City, and the saline-alkali land area, changes in intensity of salinity-alkalinity and spatial distribution from 1992 to 2011 were analyzed. The results showed that salinization of arable land in Huanghua City alleviated from 1992 to 2011. The severely and moderately saline-alkali land area decreased in 2011 compared with 1992, while the non/slightly saline land area increased. The moderately saline-alkali land in southeast transformed to non/slightly saline-alkaline, while the severely saline-alkali land in west of the city far from the coastal zone became moderately saline-alkaline. The center of gravity (CG) of severely and non/slightly saline-alkali land moved closer the coastline, while that of the moderately saline-alkali land moved from southwest coastal line to northwest. Factors influencing changes in arable land within the saline-alkali ecosystem of Huanghua City were climate, hydrology and human activities.

  9. Influence of alkali metal cations/type of activator on the structure of alkali-activated fly ash - ATR-FTIR studies

    Science.gov (United States)

    Król, M.; Rożek, P.; Chlebda, D.; Mozgawa, W.

    2018-06-01

    Coal fly ash as a secondary aluminosiliceous raw material that is commonly used in the so-called geopolymerization process has been activated with different alkali hydroxides solutions: LiOH, NaOH and KOH. Changes in the aluminosilicate structure of the material during alkali-activation have been analyzed in detail on the basis of ATR/FT-IR spectra. These changes mainly affect both the integral intensity and FWHM of bands in the range of 1200-950 cm-1, however dehydration and carbonation process can be also analyzed based on obtaining results.

  10. Alkali content of fly ash : measuring and testing strategies for compliance : [tech transfer summary].

    Science.gov (United States)

    2015-04-01

    This study investigated the test methods used to determine the : alkali content of fly ash. It also evaluated if high-alkali fly ash : exacerbates alkali-silica reaction in laboratory tests and field : concrete.

  11. Influence of alkali metal hydroxides on corrosion of Zr-base alloys

    International Nuclear Information System (INIS)

    Jeong, Yong Hwan

    1996-01-01

    The influence of group-1 alkali hydroxides on different Zr-based alloys have been carried out in static autoclaves at 350 deg C in pressurized water, conditioned in low(0.32 mmol), medium(4.3 mmol) and high(31.5 mmol) equimolar concentration of Li-, Na-, K-, Rb- and Cs-hydroxide. Two types of alloys have been investigated: Zr-Sn-(TRM, Transition metal) and Zr-Sn-Nb-(TRM, Transition metal). From the experiments the cation could be identified as the responsible species for corrosion of Zr alloy in alkalized water. The radius of the cation governs the accelerated corrosion in the pre-transition region of Zr alloy. Incorporation of alkali cation into the zirconium oxide lattice is probably the mechanism which allows the corrosion enhancement for Li and Na and the significant lower effect for the other bases. Nb containing alloys showed lower corrosion resistance than Zr-Sn-TRM alloys in all alkali solutions. Both types of alloys were corroded significantly more in LiOH and NaOH than in the other alkali environments. Lowest corrosive aggressiveness has been found for CsOH followed by KOH. Concluding from the corrosion behavior in the different alkali environments and taking into account the tendency to accelerate the corrosion of Zr alloys, CsOH and KOH are possible alternate alkali for PWR (Pressurized Water Reactor) application. (author)

  12. Solubility of 1:1 Alkali Nitrates and Chlorides in Near-Critical and Supercritical Water : 1 Alkali Nitrates and Chlorides in Near-Critical and Supercritical Water

    NARCIS (Netherlands)

    Leusbrock, Ingo; Metz, Sybrand J.; Rexwinkel, Glenn; Versteeg, Geert F.

    2009-01-01

    To increase the available data oil systems containing supercritical water and inorganic compounds, all experimental setup was designed to investigate the solubilities of inorganic compounds Ill supercritical water, In this work, three alkali chloride salts (LiCl, NaCl, KCl) and three alkali nitrate

  13. On the polymorphic and morphological changes of cellulose nanocrystals (CNC-I) upon mercerization and conversion to CNC-II.

    Science.gov (United States)

    Jin, Ersuo; Guo, Jiaqi; Yang, Fang; Zhu, Yangyang; Song, Junlong; Jin, Yongcan; Rojas, Orlando J

    2016-06-05

    Polymorphic and morphological transformations of cellulosic materials are strongly associated to their properties and applications, especially in the case of emerging nanocelluloses. Related changes that take place upon treatment of cellulose nanocrystals (CNC) in alkaline conditions are studied here by XRD, TEM, AFM, and other techniques. The results indicate polymorphic transformation of CNC proceeds gradually in a certain range of alkali concentrations, i.e. from about 8% to 12.5% NaOH. In such transition alkali concentration, cellulose I and II allomorphs coexists. Such value and range of the transition concentration is strongly interdependent with the crystallite size of CNCs. In addition, it is distinctively lower than that for macroscopic fibers (12-15% NaOH). Transmission electron microscopy and particle sizing reveals that after mercerization CNCs tend to associate. Furthermore, TEMPO-oxidized mercerized CNC reveals the morphology of individual nanocrystal of the cellulose II type, which is composed of some interconnected granular structures. Overall, this work reveals how the polymorphism and morphology of individual CNC change in alkali conditions and sheds light onto the polymorphic transition from cellulose I to II. Copyright © 2016 Elsevier Ltd. All rights reserved.

  14. Journal of Earth System Science | Indian Academy of Sciences

    Indian Academy of Sciences (India)

    A concrete study combining optical microscopy, Raman spectroscopy and X-ray diffractometry, was carried out on subsurface samples of basement granite and melt ... XRD data further reveals minute deviations of unit cell parameters of quartz, alkali feldspar and plagioclase, with respect to standard α-quartz, high- and low ...

  15. Alkali Release from Typical Danish Aggregates to Potential ASR Reactive Concrete

    DEFF Research Database (Denmark)

    Thomsen, Hans Christian Brolin; Grelk, Bent; Barbosa, Ricardo Antonio

    Alkali-silica reaction (ASR) in concrete is a well-known deterioration mechanism affecting the long term durability of Danish concrete structures. Deleterious ASR cracking can be significantly reduced or prevented by limiting the total alkali content of concrete under a certain threshold limit......, which in Denmark is recommended to 3 kg/m3 Na2Oeq.. However, this threshold limit does not account for the possible internal contribution of alkali to the concrete pore solution by release from aggregates or external contributions from varies sources. This study indicates that certain Danish aggregates...... are capable of releasing more than 0.46 kg/m3 Na2Oeq. at 13 weeks of exposure in laboratory test which may increase the risk for deleterious cracking due to an increase in alkali content in the concrete....

  16. An alkali ion source based on graphite intercalation compounds for ion mobility spectrometry

    International Nuclear Information System (INIS)

    Tabrizchi, Mahmoud; Hosseini, Zahra S

    2008-01-01

    A variety of alkali cation emitters were developed as the ion source for ion mobility spectrometry. The cation emitters were constructed based on alkali ion graphite intercalation compounds (GICs). The compounds were prepared by fusing alkali salts with ground graphite. In order to produce alkali ions, the compounds were loaded on a filament and heated to red. Reactant ions of the form alk + ions were observed for the alkali salts NaCl, KCl.LiCl, CsCl and SrCl. In addition to Na + ions, K + ions were observed at the beginning of thermionic emission from Na-GIC. This is due to the low ionization potential of potassium that exists in trace amounts in sodium salts. In addition to the potassium ion, Na + was observed in the case of LiCl salt. The Na + and K + peaks originating from impurities totally disappeared after about 40 min. However, the thermionic emission of the main ion of the corresponding salt lasted for several days. No negative ions were observed upon reversing the drift field. Selected organic compounds (methyl isobutyl ketone, dimethyl sulfoxide, acetone and tetrahydrofuran) were also ionized via alkali cation attachment reaction. Distinct ion mobility patterns were observed for different substances using one type of alkali reactant ion. However, the ion mobility pattern for a given substance changed when a different alkali reactant ion was used. Ammonia and amines were not ionized when this source was used

  17. The Effects of Biochar on Germination and Growth of Wheat in Different Saline-alkali Soil

    Institute of Scientific and Technical Information of China (English)

    Guijun; WANG; Zhenwen; XU

    2013-01-01

    Saline alkali soil can cause physiological drought on crops,so only some salinity tolerant crops can grow in saline alkali soil.Biochar can increase the utilize efficiency of nutrient and the water retention of the soil,and affect the growth of the plant.In this research,four different proportion of biochar was added in five different levels of saline-alkali soil for pot culture experiment.The pH of the soil increases as the proportion of biochar increase in same saline-alkali level soil,while the EC decrease as the proportion of biochar increase.The germination rate of wheat seeds varies as the different of soil’s saline-alkali level.Notable among these results is the germination of wheat seeds in the serious saline-alkali soil without biochar added is 0,while in 45%biochar added in serious saline-alkali soil,the germination rate get to as high as 48.9%.Also,biochar improve the growth of wheat seedling,while for mild saline alkali soil and normal soil.Biochar had no obvious effect on the growth of wheat seedling.

  18. Alkali-Resistant Quasi-Solid-State Electrolyte for Stretchable Supercapacitors.

    Science.gov (United States)

    Tang, Qianqiu; Wang, Wenqiang; Wang, Gengchao

    2016-10-05

    Research on stretchable energy-storage devices has been motivated by elastic electronics, and considerable research efforts have been devoted to the development of stretchable electrodes. However, stretchable electrolytes, another critical component in stretchable devices, have earned quite little attention, especially the alkali-resistant ones. Here, we reported a novel stretchable alkali-resistant electrolyte made of a polyolefin elastomer porous membrane supported potassium hydroxide-potassium polyacrylate (POE@KOH-PAAK). The as-prepared electrolyte shows a negligible plastic deformation even after 1000 stretching cycles at a strain of 150% as well as a high conductivity of 0.14 S cm -1 . It also exhibits excellent alkali resistance, which shows no obvious degradation of the mechanical performance after immersion in 2 M KOH for up to 2 weeks. To demonstrate its good properties, a high-performance stretchable supercapacitor is assembled using a carbon-nanotube-film-supported NiCo 2 O 4 (CNT@NiCo 2 O 4 ) as the cathode and Fe 2 O 3 (CNT@Fe 2 O 3 ) as the anode, proving great application promise of the stretchable alkali-resistant electrolyte in stretchable energy-storage devices.

  19. Mechanical Behaviour of Soil Improved by Alkali Activated Binders

    Directory of Open Access Journals (Sweden)

    Enza Vitale

    2017-11-01

    Full Text Available The use of alkali activated binders to improve engineering properties of clayey soils is a novel solution, and an alternative to the widely diffused improvement based on the use of traditional binders such as lime and cement. In the paper the alkaline activation of two fly ashes, by-products of coal combustion thermoelectric power plants, has been presented. These alkali activated binders have been mixed with a clayey soil for evaluating the improvement of its mechanical behaviour. One-dimensional compression tests on raw and treated samples have been performed with reference to the effects induced by type of binder, binder contents and curing time. The experimental evidences at volume scale of the treated samples have been directly linked to the chemo-physical evolution of the binders, investigated over curing time by means of X Ray Diffraction. Test results showed a high reactivity of the alkali activated binders promoting the formation of new mineralogical phases responsible for the mechanical improvement of treated soil. The efficiency of alkali activated binders soil treatment has been highlighted by comparison with mechanical performance induced by Portland cement.

  20. Alkali-explosion pretreatment of straw and bagasse for enzymic hydrolysis.

    Science.gov (United States)

    Puri, V P; Pearce, G R

    1986-04-01

    Sugarcane bagasse and wheat straw were subjected to alkali treatment at 200 degrees C for 5 min and at 3.45 MPa gas pressure (steam and nitrogen), followed by an explosive discharge through a defibrating nozzle, in an attempt to improve the rate and extent of digestibility. The treatment resulted in the solubilization of 40-45% of the components and in the production of a pulp that gave saccharification yields of 80 and 65% in 8 h for bagasse and wheat straw, respectively. By comparison, alkali steaming at 200 degrees C (1.72 MPa) for 5 min gave saccharification yields of only 58 and 52% in 48 h. The increase in temperature from 140 to 200 degrees C resulted in a gradual increase in in vitro organic matter digestibility (IVOMD) for both the substrates. Also, the extent of alkalinity during pretreatment appears to effect the reactivity of the final product towards enzymes. Pretreatment times ranging from 5 to 60 caused a progressive decline in the IVOMD of bagasse and wheat straw by the alkali explosion method and this was accompanied by a progressive decrease in pH values after explosion. In the alkali-steaming method, pretreatment time had no apparent effect with either substrate. An analysis of the alkali-exploded products showed that substantial amounts of hemicellulose and a small proportion of the lignin were solubilized. The percentage crystallinity of the cellulose did not alter in either substrate but there was a substantial reduction in the degree of polymerization. The superiority of the alkali-explosion pretreatment is attributed to the efficacy of fiber separation and disintegration; this increases the surface area and reduces the degree of polymerization.

  1. Using Modified Remote Sensing Imagery to Interpret Changes in Cultivated Land under Saline-Alkali Conditions

    Directory of Open Access Journals (Sweden)

    Hui Gao

    2016-07-01

    Full Text Available Managing the rapidly changing saline-alkali land under cultivation in the coastal areas of China is important not only for mitigating the negative impacts of such land on the environment, but also for ensuring long-term sustainability of agriculture. In this light, setting up rapid monitoring systems to assist decision-making in developing sustainable management plans is therefore an absolute necessity. In this study, we developed a new interpretation system where symbols are used to grade and classify saline-alkali lands in space and time, based on the characteristics of plant cover and features of remote sensing images. The system was used in combination with the maximum likelihood supervised classification to analyze the changes in cultivated lands under saline-alkali conditions in Huanghua City. The analysis revealed changes in the area and spatial distribution of cultivated under saline-alkali conditions in the region. The total area of saline-alkali land was 139,588.8 ha in 1992 and 134,477.5 ha in 2011. Compared with 1992, severely and moderately saline-alkali land areas decreased in 2011. However, non/slightly saline land areas increased over that in 1992. The results showed that the salinization rate of arable lands in Huanghua City decreased from 1992 to 2011. The moderately saline-alkali land southeast of the city transformed into non/slightly saline-alkaline. Then, severely saline-alkali land far from the coastal zone west of the city became moderately saline-alkaline. Spatial changes in cultivated saline-alkali lands in Huanghua City were such that the centers of gravity (CG of severely and non/slightly saline-alkali land moved closer the coastline, while that of the moderately saline-alkali land moved from southwest coastal line to northwest. Factors influencing changes in cultivated lands in the saline-alkali ecosystem included climate, hydrology and human activity. Thus, studies are required to further explore these factors in

  2. Alkali roasting of bomar ilmenite: rare earths recovery and physico-chemical changes

    Directory of Open Access Journals (Sweden)

    Sanchez-Segado Sergio

    2014-11-01

    (FeTiO3 is presented as a process route for integrated beneficiation of the mineral for rutile-rich phase and rare earth oxides; the latter is released as a consequence of physical changes in the ilmenite matrix, during the water leaching after roasting. The oxidative alkali roasting transforms ilmenite mineral into water-insoluble alkali titanate and water-soluble ferrite. After roasting the insoluble alkali titanate is separated from rare-earth oxide mixture in colloidal form and water-soluble ferrite. Further leaching of alkali titanate is carried out with oxalic (0.3M and ascorbic (0.01M acid solution which removes the remaining Fe2+ ions into the leachate and allows precipitation of high-purity synthetic rutile containing more than 95% TiO2. Iron is removed as iron oxalate. The physico-chemical changes occurred during the roasting and leaching processes are reported by comparing the role of alkali on the roasting process and product morphologies formed.

  3. Influence of alkali metal hydroxides on corrosion of Zr-based alloys

    International Nuclear Information System (INIS)

    Jeong, Y.H.; Ruhmann, H.; Garzarolli, F.

    1997-01-01

    In this study the influence of group-1 alkali hydroxides on different zirconium based alloys has been evaluated. The experiments have been carried out in small stainless steel autoclaves at 350 deg. C in pressurized 17 MPa water, with in low (0.32 mmol), medium (4.3 mmol) and high (31.5 mmol) equimolar concentrations of Li-, Na-, K-, Rb- and Cs-Hydroxides. Two types of alloys have been investigated: Zr-Sn-(Transition metal) and Zr-Sn-Nb-(Transition metal). The corrosion behaviour was evaluated from weight gain measurements. From the experiments the cation could be identified as the responsible species for zirconium alloy corrosion in alkalized water. The radius of the cation governs the corrosion behaviour in the pre accelerated region of zircaloy corrosion. Incorporating of alkali cations into the zirconium oxide lattice is probably the mechanism which allows the corrosion enhancement for Li and Na and the significantly lower effect for the other bases. Nb containing alloys show lower corrosion resistance than alloys from the Zr-Sn-TRM system in all alkali solutions. Both types of alloys corrode significantly more in LiOH and NaOH than in the other alkali environments. Lowest corrosive aggressiveness has been found for CsOH followed by KOH. Concluding from the corrosion behaviour in the different alkali environments and taking into account the tendency to promote accelerate corrosion, CsOH and KOH are possible alternate alkalis for PWR application. (author). 17 refs, 15 figs, 5 tabs

  4. Influence of alkali metal hydroxides on corrosion of Zr-based alloys

    Energy Technology Data Exchange (ETDEWEB)

    Jeong, Y H [Korea Atomic Energy Research Inst., Dae Jun (Korea, Republic of); Ruhmann, H; Garzarolli, F [Siemens-KWU, Power Generation Group, Erlangen (Germany)

    1997-02-01

    In this study the influence of group-1 alkali hydroxides on different zirconium based alloys has been evaluated. The experiments have been carried out in small stainless steel autoclaves at 350 deg. C in pressurized 17 MPa water, with in low (0.32 mmol), medium (4.3 mmol) and high (31.5 mmol) equimolar concentrations of Li-, Na-, K-, Rb- and Cs-Hydroxides. Two types of alloys have been investigated: Zr-Sn-(Transition metal) and Zr-Sn-Nb-(Transition metal). The corrosion behaviour was evaluated from weight gain measurements. From the experiments the cation could be identified as the responsible species for zirconium alloy corrosion in alkalized water. The radius of the cation governs the corrosion behaviour in the pre accelerated region of zircaloy corrosion. Incorporating of alkali cations into the zirconium oxide lattice is probably the mechanism which allows the corrosion enhancement for Li and Na and the significantly lower effect for the other bases. Nb containing alloys show lower corrosion resistance than alloys from the Zr-Sn-TRM system in all alkali solutions. Both types of alloys corrode significantly more in LiOH and NaOH than in the other alkali environments. Lowest corrosive aggressiveness has been found for CsOH followed by KOH. Concluding from the corrosion behaviour in the different alkali environments and taking into account the tendency to promote accelerate corrosion, CsOH and KOH are possible alternate alkalis for PWR application. (author). 17 refs, 15 figs, 5 tabs.

  5. Mechanism of the alkali degradation of (6-4) photoproduct-containing DNA.

    Science.gov (United States)

    Arichi, Norihito; Inase, Aki; Eto, Sachise; Mizukoshi, Toshimi; Yamamoto, Junpei; Iwai, Shigenori

    2012-03-21

    The (6-4) photoproduct is one of the major damaged bases produced by ultraviolet light in DNA. This lesion is known to be alkali-labile, and strand breaks occur at its sites when UV-irradiated DNA is treated with hot alkali. We have analyzed the product obtained by the alkali treatment of a dinucleoside monophosphate containing the (6-4) photoproduct, by HPLC, NMR spectroscopy, and mass spectrometry. We previously found that the N3-C4 bond of the 5' component was hydrolyzed by a mild alkali treatment, and the present study revealed that the following reaction was the hydrolysis of the glycosidic bond at the 3' component. The sugar moiety of this component was lost, even when a 3'-flanking nucleotide was not present. Glycosidic bond hydrolysis was also observed for a dimer and a trimer containing 5-methyl-2-pyrimidinone, which was used as an analog of the 3' component of the (6-4) photoproduct, and its mechanism was elucidated. Finally, the alkali treatment of a tetramer, d(GT(6-4)TC), yielded 2'-deoxycytidine 5'-monophosphate, while 2'-deoxyguanosine 3'-monophosphate was not detected. This result demonstrated the hydrolysis of the glycosidic bond at the 3' component of the (6-4) photoproduct and the subsequent strand break by β-elimination. It was also shown that the glycosidic bond at the 3' component of the Dewar valence isomer was more alkali-labile than that of the (6-4) photoproduct.

  6. Molybdenum/alkali metal/ethylene glycol complexes useful as epoxidation catalysts

    International Nuclear Information System (INIS)

    Marquis, E.T.; Sanderson, J.R.; Keating, K.P.

    1987-01-01

    This patent describes a clear, storage stable solution of a molybdenum/alkali metal/ethylene glycol complex in ethylene glycol made by the process comprising: reacting at an elevated temperature between about 25 0 and 150 0 C a solid ammonium molybdate or a hydrate thereof and a solid alkali metal molybdate or a hydrate thereof with ethylene glycol, such that the ratio of moles of ethylene glycol to total gram atoms of molybdenum in the molybdates ranges from about 7:10 to 10:1, and the ratio of gram atoms of molybdenum in the ammonium molybdate or hydrate thereof to gram atoms of molybdenum in the alkali metal molybdate is from about 1:1 to about 20:1 to thereby provide a reaction product composed of a solution of an alkali metal-containing complex of molybdenum, alkali metal and ethylene glycol and by-products, including water, in the ethylene glycol and subsequently stripping the solution at a reduced pressure to remove from about 5 to about 25% of the reaction product, as distillate, to thereby provide a storage stable solution of the complex in the ethylene glycol having a molybdenum content of about 6 wt. % to about 20 wt. %, a water concentration of about 0.1 wt. % to about 6 wt. % and an acid number of more than about 60

  7. Behaviour of gaseous alkali compounds from coal gasification

    International Nuclear Information System (INIS)

    Nykaenen, J.

    1996-01-01

    In this project the behaviour of alkali compounds has been studied with a chemical equilibrium model. The goal is to evaluate the possibilities to remove the sodium and potassium compounds together with the fly ash particles by using a ceramic honeycomb filter. The studied processes include both CO 2 /O 2 - and air-blown gasification and combustion. The results show that the difference between the processes with flue gas recirculation and air-blown processes is small. This is due to that the equilibrium concentration of the dominant gaseous alkali compound, chloride, is more or less the same in both processes. This research project is closely connected to the EU-project coordinated by the Delft University of Technology (DUT). In that project alkali concentration of the fuel gas from a 1.6 MW pilot plant will be measured. During the next phase of this research the results from DUT will be compared with the results of this presentation. (author)

  8. Alkali and heavy metal emissions of the PCFB-process; Alkali- ja raskasmetallipaeaestoet PCFB-prosessista

    Energy Technology Data Exchange (ETDEWEB)

    Kuivalainen, R; Eriksson, T; Lehtonen, P [Foster Wheeler Energia Oy, Karhula (Finland)

    1997-10-01

    Pressurized Circulating Fluidized Bed (PCFB) combustion technology has been developed in Karhula R and D Center since 1986. As part of the development, 10 MW PCFB test facility was built in 1989. The test facility has been used for performance testing with different coal types through the years 1990-1995 in order to gain data for design and commercialization of the high-efficiency low-emission PCFB combustion technology. The main object of the project was to measure vapor phase Na and K concentrations in the PCFB flue gas after hot gas filter and investigate the effects of process conditions and sorbents on alkali release. The measurements were performed using plasma assisted method of TUT Laboratory of Plasma Technology and wet absorption method of VTT Energy. The measurements were carried out during three test campaigns at PCFB Test Facility in Karhula. In autumn 1995 both VTT and TUT methods were used. The measurements of the following test period in spring 1996 were performed by VTT, and during the last test segment in autumn 1996 TUT method was in use. During the last test period, the TUT instrument was used as semi-continuous (3 values/minute) alkali analyzer for part of the time. The measured Na concentrations were below 30 ppb(w) in all measured data points. The results of K were below 10 ppb(w). The accuracies of the both methods are about +50 % at this concentration range. The scatter of the data covers the effects of different process variables on the alkali emission. The measured emissions are at the same order of magnitude as the guideline emission limits estimated by gas turbine manufacturers

  9. Influence of curing conditions on durability of alkali-resistant glass ...

    Indian Academy of Sciences (India)

    Glass fibres in concrete material often increase the flexural strength. However, these fibres when in contact with cement are altered by alkali reactions due to the presence of portlandite. This study presents the results of investigation to show the effect of curing conditions on the durability of alkali-resistant glass fibres in ...

  10. Filling material for a buried cavity in a collapse area using light-weighted foam and active feldspar

    Science.gov (United States)

    Cho, Jin Woo; Lee, Ju-hyoung; Kim, Sung-Wook; Choi, Eun-Kyeong

    2017-04-01

    Concrete which is generally used as filling material for a buried cavity has very high strength but significantly high self-load is considered its disadvantage. If it is used as filling material, the second collapse due to additional load, causing irreversible damage. If light-weighted foam and active feldspar are used to solve this problem, the second collapse can be prevented by reducing of self-load of filling material. In this study, the specimen was produced by mixing light-weighted foam, active feldspar and cement, and changes in the density, unconfined compressive strength and hydraulic conductivity were analyzed. Using the light-weighted foam could enable the adjustment of density of specimen between 0.5 g/cm3 and 1.7 g/cm3, and if the mixing ratio of the light-weighted foam increases, the specimen has more pores and smaller range of cross-sectional area. It is confirmed that it has direct correlation with the density, and if the specimen has more pores, the density of the specimen is lowered. The density of the specimen influences the unconfined compressive strength and the hydraulic conductivity, and it was also confirmed that the unconfined compressive strength could be adjusted between 0.6 MPa and 8 MPa and the hydraulic conductivity could be adjusted between 10-9cm/sec and 10-3cm/sec. These results indicated that we can adjust unconfined compressive strength and hydraulic conductivity of filling materials by changing the mixing amount of lightweight-weighted foam according to the requirements of the field condition. Keywords: filling material, buried cavity, light-weighted foam, feldspar Acknowledgement This research was supported by a Grant from a Strategic Research Project (Horizontal Drilling and Stabilization Technologies for Urban Search and Rescue (US&R) Operation) funded by the Korea Institute of Civil Engineering and Building Technology.

  11. Alkali replacement raises urinary citrate excretion in patients with topiramate-induced hypocitraturia.

    Science.gov (United States)

    Jhagroo, R Allan; Wertheim, Margaret L; Penniston, Kristina L

    2016-01-01

    The aims of this study were to assess (1) the magnitude and temporality of decreased urinary citrate excretion in patients just starting topiramate and (2) the effect of alkali replacement on topiramate-induced hypocitraturia. Study 1 was a prospective, non-intervention study in which patients starting topiramate for headache remediation provided pre- and post-topiramate 24 h urine collections for measurement of urine citrate. Study 2 was a clinical comparative effectiveness study in which patients reporting to our stone clinic for kidney stones and who were treated with topiramate were prescribed alkali therapy. Pre- and post-alkali 24 h urinary citrate excretion was compared. Data for 12 and 22 patients (studies 1 and 2 respectively) were evaluated. After starting topiramate, urinary citrate excretion dropped significantly by 30 days (P = 0.016) and 62% of patients had hypocitraturia (citrate alkali, urine citrate increased in stone-forming patients on topiramate (198 ± 120 to 408 ± 274 mg day(-1) ; P = 0.042 for difference). 85% of patients were hypocitraturic on topiramate alone vs. 40% after adding alkali. The increase in urinary citrate was greater in patients provided ≥ 90 mEq potassium citrate. Our study is the first to provide clinical evidence that alkali therapy can raise urinary citrate excretion in patients who form kidney stones while being treated with topiramate. Clinicians should consider alkali therapy for reducing the kidney stone risk of patients benefitting from topiramate treatment for migraine headaches or other conditions. © 2015 The British Pharmacological Society.

  12. 40 CFR 721.10097 - Disubstituted benzenesulfonic acid, alkali metal salt (generic).

    Science.gov (United States)

    2010-07-01

    ... chemical substance identified generically as disubstituted benzenesulfonic acid, alkali metal salt (PMN P... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Disubstituted benzenesulfonic acid, alkali metal salt (generic). 721.10097 Section 721.10097 Protection of Environment ENVIRONMENTAL...

  13. Anion exchange membrane based on alkali doped poly(2,5-benzimidazole) for fuel cell

    CSIR Research Space (South Africa)

    Luo, H

    2012-02-01

    Full Text Available The properties of alkali doped poly(2,5-benzimidazole) membrane with different alkali doping level for fuel cell application is reported in this work. The alkali doping level played an important role for the ion conductivity of the membrane. The ion...

  14. Increase in Ice Nucleation Efficiency of Feldspars, Kaolinite and Mica in Dilute NH3 and NH4+-containing Solutions

    Science.gov (United States)

    Kumar, A.; Marcolli, C.; Luo, B.; Krieger, U. K.; Peter, T.

    2017-12-01

    Semivolatile species present in the atmosphere are prone to adhere to mineral dust particle surfaces during long range transport, and could potentially change the particle surface properties and its ice nucleation (IN) efficiency. Immersion freezing experiments were performed with microcline (K-feldspar), known to be highly IN active, suspended in aqueous solutions of ammonia, (NH4)2SO4, NH4HSO4, NH4NO3, NH4Cl, Na2SO4, H2SO4, K2SO4 and KCl to investigate the effect of solutes on the IN efficiency. Freezing of emulsified droplets investigated with a differential scanning calorimeter (DSC) showed that the heterogeneous ice nucleation temperatures deviate from the water activity-based IN theory, describing heterogeneous ice nucleation temperatures as a function of solution water activity by a constant offset with respect to the ice melting point curve (Zobrist et al. 2008). IN temperatures enhanced up to 4.5 K were observed for very dilute NH3 and NH4+-containing solutions while a decrease was observed as the concentration was further increased. For all solutes with cations other than NH4+, the IN efficiency decreased. An increase of the IN efficiency in very dilute NH3 and NH4+-containing solutions followed by a decrease with increasing concentration was also observed for sanidine (K-feldspar) and andesine (Na/Ca-feldspar). This is an important indication towards specific chemical interactions between solutes and the feldspar surface which is not captured by the water activity-based IN theory. A similar trend is present but less pronounced in case of kaolinite and mica, while quartz is barely affected. We hypothesize that the hydrogen bonding of NH3 molecules with surface -OH groups could be the reason for the enhanced freezing temperatures in dilute ammonia and ammonium containing solutions as they could form an ice-like overlayer providing hydrogen bonding groups for ice to nucleate on top of it. This implies to possibilities of enhanced IN efficiency, especially

  15. Powder X-ray diffraction study af alkali alanates

    DEFF Research Database (Denmark)

    Cao, Thao; Mosegaard Arnbjerg, Lene; Jensen, Torben René

    Powder X-ray diffraction study of alkali alanates Thao Cao, Lene Arnbjerg, Torben R. Jensen. Center for Materials Crystallography (CMC), Center for Energy Materials (CEM), iNANO and Department of Chemistry, Aarhus University, DK-8000, Denmark. Abstract: To meet the energy demand in the future...... for mobile applications, new materials with high gravimetric and volumetric storage capacity of hydrogen have to be developed. Alkali alanates are promising for hydrogen storage materials. Sodium alanate stores hydrogen reversibly at moderate conditions when catalysed with, e.g. titanium, whereas potassium...

  16. Origin of K-feldspar megacrystals from Monte das Gameleiras granite, Rio Grande do Norte/Paraiba, Brazil

    International Nuclear Information System (INIS)

    Galindo, A.C.

    1988-01-01

    The Monte das Gameleiras granitic batholith is located at the boundary between Rio Grande do Norte and Paraiba States in northeastern Brazil. Two main types of granitic rocks have been identified in this batholith. Dioritic inclusions occur in both of them. The predominating type is an extremely porphyritic syenogranite, which is intruded by a fine-grained monzogranite. K-feldspar megacrysts are found in both porphyritic granite and dioritic inclusions. The megacrysts long axes average around 4 cm, reaching up to 9 or 10 cm. The megacrysts are euhedral, zoned, and, sometimes, they show rapakivi texture. Flow textures and tuillage are common, but irregularly distributed. The K-feldspar megacrysts contain inclusions of plagioclase, biotite, quartz, hornblende, sphene, and apatite. These inclusions are concentrically arranged and parallel to the megacrysts zones. The included minerals are generally smaller than the same minerals in the groundmass. Microprobe analyses and X-ray difraction studies show that the megacrysts of both facies are similar in composition, containing around 90% of orthoclase. Taking into account the textural and compositional aspects, it is concluded that the megacrysts of porphyritic granite and dioritic inclusions are phenocrysts and not porphyroblasts. (author) [pt

  17. Enzymatic regulation of organic acid metabolism in an alkali-tolerant ...

    African Journals Online (AJOL)

    Chloris virgata, an alkali-tolerant halophyte, was chosen as the test material for our research. The seedlings of C. virgata were treated with varying salt and alkali stress. First, the composition and content of organic acids in shoots were analyzed and the results indicated that there was not only a significant increase in total ...

  18. An exsolution silica-pump model for the origin of myrmekite

    Science.gov (United States)

    Castle, R.O.; Lindsley, D.H.

    1993-01-01

    Myrmekite, as defined here, is the microscopic intergrowth between vermicular quartz and modestly anorthitic plagioclase (calcic albite-oligoclase), intimately associated with potassium feldspar in plutonic rocks of granitic composition. Hypotheses previously invoked in explanation of myrmekite include: (1) direct crystallization; (2) replacement; (3) exsolution. The occurrence of myrmekite in paragneisses and its absence in rocks devold of discrete grains of potassium feldspar challenge those hypotheses based on direct crystallization or replacement. However, several lines of evidence indicate that myrmekite may in fact originate in response to kinetic effects associated with the exsolution of calcic alkali feldspar into discrete potassium feldspar and plagioclase phases. Exsolution of potassium feldspar system projected from [AlSi2O8] involves the exchange CaAlK-1Si-1, in which the AlSi-1 tetrahedral couple is resistant to intracrystalline diffusion. By contrast, diffusion of octahedral K proceeds relatively easily where it remains uncoupled to the tetrahedral exchange. We suggest here that where the ternary feldspar system is open to excess silica, the exchange reaction that produces potassium feldspar in the ternary plane is aided by the net-transfer reaction K+Si=Orthoclase, leaving behind indigenous Si that reports as modal quartz in the evolving plagioclase as the CaAl component is concomitantly incorporated in this same phase. Thus silica is "pumped" into the reaction volume from a "silica reservoir", a process that enhances redistribution of both Si and Al through the exsolving ternary feldspar. ?? 1993 Springer-Verlag.

  19. Assesment of Alkali Resistance of Basalt Used as Concrete Aggregates

    Directory of Open Access Journals (Sweden)

    al-Swaidani Aref M.

    2015-11-01

    Full Text Available The objective of this paper is to report a part of an ongoing research on the influence of using crushed basalt as aggregates on one of durability-related properties of concrete (i.e. alkali-silica reaction which is the most common form of Alkali-Aggregate Reaction. Alkali resistance has been assessed through several methods specified in the American Standards. Results of petrographic examination, chemical test (ASTM C289 and accelerated mortar bar test (ASTM C1260 have particularly been reported. In addition, the weight change and compressive strength of 28 days cured concrete containing basaltic aggregates were also reported after 90 days of exposure to 10% NaOH solution. Dolomite aggregate were used in the latter test for comparison. The experimental results revealed that basaltic rocks quarried from As-Swaida’a region were suitable for production of aggregates for concrete. According to the test results, the studied basalt aggregates can be classified as innocuous with regard to alkali-silica reaction. Further, the 10% sodium hydroxide attack did not affect the compressive strength of concrete.

  20. Charge-charge liquid structure factor and the freezing of alkali halides

    International Nuclear Information System (INIS)

    March, N.H.; Tosi, M.P.

    1980-10-01

    The peak height of the charge-charge liquid structure factor Ssub(QQ) in molten alkali halides is proposed as a criterion for freezing. Available data on molten alkali chlorides, when extrapolated to the freezing point suggests Ssub(QQ)sup(max) approximately 5. (author)

  1. Investigation on lithium migration for treating alkali-silica reaction affected concrete

    NARCIS (Netherlands)

    Silva De Souza, L.M.; Polder, R.B.; Copuroglu, O.

    2014-01-01

    Alkali-silica reaction (ASR) is one of the major deterioration mechanisms that affect numerous concrete structures worldwide. During the reaction, hydroxyl and alkali (sodium and potassium ) ions react with certain siliceous compounds in the aggregate, forming a hygroscopic gel. The gel absorbs

  2. Gradient heating protocol for a diode-pumped alkali laser

    Science.gov (United States)

    Cai, He; Wang, You; Han, Juhong; Yu, Hang; Rong, Kepeng; Wang, Shunyan; An, Guofei; Wang, Hongyuan; Zhang, Wei; Wu, Peng; Yu, Qiang

    2018-06-01

    A diode-pumped alkali laser (DPAL) has gained rapid development in the recent years. Until now, the structure with single heater has been widely utilized to adjust the temperature of an alkali vapor cell in most of the literatures about DPALs. However, for an end-pumped DPAL using single heater, most pump energy is absorbed by the gain media near the entrance cell window because of the large absorption cross section of atomic alkali. As a result, the temperature in the pumping area around the entrance window will go up rapidly, especially in a case of high pumping density. The temperature rise would bring about some negative influences such as thermal effects and variations in population density. In addition, light scattering and window contamination aroused by the chemical reaction between the alkali vapor and the buffer gas will also affect the output performance of a DPAL system. To find a solution to these problems, we propose a gradient heating approach in which several heaters are tandem-set along the optical axis to anneal an alkali vapor cell. The temperature at the entrance window is adjusted to be lower than that of the other side. By using this novel scheme, one can not only achieve a homogeneous absorption of the pump energy along the cell axis, but also decrease the possibility of the window damage in a DPAL configuration. The theoretical simulation of the laser output features has been carried out for a configuration of multiple heaters. Additionally, the DPAL output performance under different gradient temperatures is also discussed in this paper. The conclusions might be helpful for development of a high-powered and high-beam-quality DPAL.

  3. Alkali and heavy metals emissions of the PCFB-process

    International Nuclear Information System (INIS)

    Kuivalainen, R.; Eriksson, T.; Koskinen, J.; Lehtonen, P.

    1995-01-01

    Pressurized Circulating Fluidized Bed (PCFB) combustion technology has been developed by A. Ahlstrom Corporation since 1986. As a part of the development, a 10 MV PCFB Test Facility was constructed at Hans Ahlstrom Laboratory in Karhula, Finland in 1989. The Test Facility has been used for performance testing with different coal types through the years 1990-1994 for obtaining data for design and commercialization of the high-efficiency low-emission PCFB combustion technology. The project Y44 'Alkali and heavy metal emissions of the PCFB-process' is part of national LIEKKI 2 research program and it continues the work started under alkali measurement project Y33 in 1994. The objective of the project is to measure vapor phase alkali and heavy metal concentrations in the PCFB flue gas after high-temperature high-pressure particulate filter and to investigate the effects of process conditions and sorbents on alkali release. The measured Na concentrations were between 0,03 and 0,21 ppm(w). The results of K were between 0,01 and 0,08 ppm(w). The accuracy of the results is about +-50 percent at this concentration range. The scatter of the data covers the effects of different process variables on the alkali emission. The measured emissions at 800-850 deg C are at the same order of magnitude as the guideline emission limits given by gas turbine manufacturers for flue gas at 1000-1200 deg C. The measurements and development of the analyses methods are planned to be continued during PCFB test runs in autumn 1995 in cooperation with laboratories of VTT Energy and Tampere University of Technology. (author)

  4. The direct observation of alkali vapor species in biomass combustion and gasification

    Energy Technology Data Exchange (ETDEWEB)

    French, R J; Dayton, D C; Milne, T A

    1994-01-01

    This report summarizes new data from screening various feedstocks for alkali vapor release under combustion conditions. The successful development of a laboratory flow reactor and molecular beam, mass spectrometer interface is detailed. Its application to several herbaceous and woody feedstocks, as well as a fast-pyrolysis oil, under 800 and 1,100{degrees}C batch combustion, is documented. Chlorine seems to play a large role in the facile mobilization of potassium. Included in the report is a discussion of relevant literature on the alkali problem in combustors and turbines. Highlighted are the phenomena identified in studies on coal and methods that have been applied to alkali speciation. The nature of binding of alkali in coal versus biomass is discussed, together with the implications for the ease of release. Herbaceous species and many agricultural residues appear to pose significant problems in release of alkali species to the vapor at typical combustor temperatures. These problems could be especially acute in direct combustion fired turbines, but may be ameliorated in integrated gasification combined cycles.

  5. Metal analyses of ash derived alkalis from banana and plantain ...

    African Journals Online (AJOL)

    The objective of this work was to determine the metal content of plantain and banana peels ash derived alkali and the possibility of using it as alternate and cheap source of alkali in soap industry. This was done by ashing the peels and dissolving it in de-ionised water to achieve the corresponding hydroxides with pH above ...

  6. Measurement of alkali-vapor emission from pressurized fluidized-bed combustion of Illinois coals

    Energy Technology Data Exchange (ETDEWEB)

    Lee, S.H.D.; Teats, F.G.; Swift, W.M. (Argonne National Lab., IL (United States)); Banerjee, D.D. (Illinois Clean Coal Inst., Carterville, IL (United States))

    1993-01-01

    Two Illinois Herrin No. 6 coals and one Illinois Springfield No. 5 coal were separately combusted in a laboratory-scale (15-cm dia) pressurized fluidized-bed combustor (PFBC) combined with an alkali sorber. These coals were combusted in a fluidized bed of Tymochtee dolomite at temperatures ranging from 910 to 950[degree]C and a system pressure of 9.2 atm absolute. Alkali-vapor emission (Na and K) in the PFBC flue gas was determined by the analytical activated-bauxite sorber bed technique developed at Argonne National Laboratory. The test results showed that sodium is the major alkali-vapor species present in the PFBC flue gas, and that the level of sodium-vapor emission increases linearly with both Na and Cl contents in the coals. This suggests that the sodium-vapor emission results from direct vaporization of NaCl present in the coals. The measured alkali-vapor concentration (Na + K), 67 to 190 ppbW, is more than 2.5 times greater than the allowable alkali limit of 24 ppb for an industrial gas turbine. Combusting these coals in a PFBC for power generation may require developing a method to control alkali vapors.

  7. Measurement of alkali-vapor emission from pressurized fluidized-bed combustion of Illinois coals

    Energy Technology Data Exchange (ETDEWEB)

    Lee, S.H.D.; Teats, F.G.; Swift, W.M. [Argonne National Lab., IL (United States); Banerjee, D.D. [Illinois Clean Coal Inst., Carterville, IL (United States)

    1993-04-01

    Two Illinois Herrin No. 6 coals and one Illinois Springfield No. 5 coal were separately combusted in a laboratory-scale (15-cm dia) pressurized fluidized-bed combustor (PFBC) combined with an alkali sorber. These coals were combusted in a fluidized bed of Tymochtee dolomite at temperatures ranging from 910 to 950{degree}C and a system pressure of 9.2 atm absolute. Alkali-vapor emission (Na and K) in the PFBC flue gas was determined by the analytical activated-bauxite sorber bed technique developed at Argonne National Laboratory. The test results showed that sodium is the major alkali-vapor species present in the PFBC flue gas, and that the level of sodium-vapor emission increases linearly with both Na and Cl contents in the coals. This suggests that the sodium-vapor emission results from direct vaporization of NaCl present in the coals. The measured alkali-vapor concentration (Na + K), 67 to 190 ppbW, is more than 2.5 times greater than the allowable alkali limit of 24 ppb for an industrial gas turbine. Combusting these coals in a PFBC for power generation may require developing a method to control alkali vapors.

  8. Structural, K-Ar and 40Ar-39Ar age studies of adularia K-feldspars from the Lizard Complex, England

    International Nuclear Information System (INIS)

    Halliday, A.N.; Mitchell, J.G.

    1976-01-01

    Conventional K-Ar analyses of fifteen adularia feldspars from the Lizard Complex yield ages between 181+-2 Ma and 220+-3 Ma (with one exception from Holseer Cove yielding an age of 156+-3 Ma). The feldspars are dominantly monoclinic but most contain a minor but constant proportion of triclinic material with variable triclinicity. An inverse correlation exists between triclinicity and K-Ar age interpreted as representing argon loss related to the structural state. Extrapolation of the data to zero triclinicity indicates a true age of 210-220 Ma. 40 Ar- 39 Ar stepwise degassing analyses yield plateau ages related to the K-Ar ages and not the crystallization age. The results can be explained in terms of postcrystallization Al-Si ordering resulting in argon loss from lattice sites which under normal diffusion conditions requires a range of activation energies. The Holseer Cove sample is monoclinic and an 40 Ar- 39 Ar stepheating analysis suggests a later crystallization at 160-170 Ma. Neither primary crystallization nor spontaneous ordering through time explain the origin of the triclinic adularia. It is suggested that ordering has been induced by the passage of low-temperature alkaline solutions at a subsequent point in geological time. Argon loss by ordering could explain the low ages found using both K-Ar and 40 Ar- 39 Ar stepheating methods when applied to feldspars in general. The 210-220 Ma, and 160-170 Ma hydrothermal events affected much of southwest England and are probably related to major geotectonic movements in western Europe. (Auth.)

  9. Effect of alkali and heat treatments for bioactivity of TiO{sub 2} nanotubes

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Seo young, E-mail: mast6269@nate.com [Dept. of Dental Biomaterials and Institute of Bio degradable material, Institute of Oral Bioscience and BK21 plus project, School of Dentistry, Chonbuk National University, Jeonju, 561-756 (Korea, Republic of); Kim, Yu kyoung, E-mail: yk0830@naver.com [Dept. of Dental Biomaterials and Institute of Bio degradable material, Institute of Oral Bioscience and BK21 plus project, School of Dentistry, Chonbuk National University, Jeonju, 561-756 (Korea, Republic of); Park, Il song, E-mail: ilsong@jbnu.ac.kr [Division of Advanced Materials Engineering, Research Center for Advanced Materials Development and Institute of Biodegradable Materials, Chonbuk National University, Jeonju 561-756 (Korea, Republic of); Jin, Guang chun, E-mail: jingc88@126.com [Oral Medical College, Beihua University, Jilin City 132013 (China); Bae, Tae sung, E-mail: bts@jbnu.ac.kr [Dept. of Dental Biomaterials and Institute of Bio degradable material, Institute of Oral Bioscience and BK21 plus project, School of Dentistry, Chonbuk National University, Jeonju, 561-756 (Korea, Republic of); Lee, Min ho, E-mail: mh@jbnu.ac.kr [Dept. of Dental Biomaterials and Institute of Bio degradable material, Institute of Oral Bioscience and BK21 plus project, School of Dentistry, Chonbuk National University, Jeonju, 561-756 (Korea, Republic of)

    2014-12-01

    Highlights: • TiO{sub 2} nanotubes formed via anodization were treated by alkali and heat. • The surface roughness was increased after alkali treatment (p < 0.05). • After alkali and heat treatment, the wettability was better than before treatment. • Alkali treated TiO{sub 2} nanotubes were shown higher HAp formation in SBF. • Heat treatment affected on the attachment of cells for alkali treated nanotubes. - Abstract: In this study, for improving the bioactivity of titanium used as an implant material, alkali and heat treatments were carried out after formation of the nanotubes via anodization. Nanotubes with uniform length, diameter, and thickness were formed by anodization. The alkali and heat-treated TiO{sub 2} nanotubes were covered with the complex network structure, and the Na compound was generated on the surface of the specimens. In addition, after 5 and 10 days of immersion in the SBF, the crystallized OCP and HAp phase was significantly increased on the surface of the alkali-treated TiO{sub 2} nanotubes (PNA) and alkali and heat-treated TiO{sub 2} nanotubes (PNAH) groups. Cell proliferation was decreased due to the formation of amorphous sodium titanate (Na{sub 2}TiO{sub 3}) layer on the surface of the PNA group. However, anatase and crystalline sodium titanate were formed on the surface of the PNAH group after heat treatment at 550 °C, and cell proliferation was improved. Thus, PNA group had higher HAp forming ability in the simulated body fluid. Additional heat treatment affected on enhancement of the bioactivity and the attachment of osteoblasts for PNA group.

  10. Mechanisms and kinetics of electrodeposition of alkali metals on solid and liquid mercury electrodes

    Energy Technology Data Exchange (ETDEWEB)

    Lu, Wenzhe.

    1993-01-01

    Electroreduction of alkali metal ions at mercury is an important area in electrochemistry related to the battery industry. In this work, four major topics were considered: alkali metal/mercury interactions; electrosorption of alkali metal ions on solid mercury; electroreduction of alkali metal/crown ether complexes; and ammonium amalgam formation. The formation of alkali metal-mercury intermetallic compounds was studied on liquid and frozen thin layer mercury electrodes. The stoichiometry of the compounds produced under these conditions was determined using cyclic voltammetry. As expected, formation of a new phase was preceded by nucleation phenomena, which were particularly easy to monitor at solid Hg electrodes. The nucleation kinetics were studied using the chronoamperometric method. At very low temperatures, when the mobility of mercury atoms was restricted, the electrosorption of alkali metal ions on solid mercury electrodes was noted. Subsequent study allowed determination of the electrosorption parameters. The free energy of electrosorption is discussed in terms of interactions between alkali metals and mercury. The effect of crown ethers on the kinetics of alkali metal ion reduction was studied at both standard size and ultramicro-mercury electrodes in nonaqueous solutions using ultrafast cyclic voltammetry and ac voltammetry. The usefulness of ultrafast cyclic voltammetry with ultramicroelectrodes in measurements of the kinetics of amalgam formation was verified in a brief study of cadmium ion reduction. The mechanism of the complex reduction at mercury was analyzed based on the free energy changes before and after the activation state. In addition, the stoichiometry and formation constants of the crown ether/alkali metal complexes were determined using cyclic voltammetry. The mechanism of electroreduction of ammonium ions at mercury electrodes in non-aqueous media was analyzed.

  11. Characterisation and properties of alkali activated pozzolanic materials

    Science.gov (United States)

    Bordeian, Georgeta Simona

    Many of the waste materials produced from modem heavy industries are pozzalans, which develop cementitious properties when finely divided in the presence of free lime. This property allows a potential industrial use for this waste as a cement replacement material in concrete. An example of such a waste material is blast furnace slag from the smelting of iron and steel. The US produces 26 million tons of blast furnace slag annually. Most of the slag is slowly cooled in air and it makes a poor pozzolan. Only 1.6 million tons of the slag is available in the granulated form, which is suitable as a cementitious and pozzolanic admixture. Most European countries are well endowed with coal-fired power stations and this produces fly and bottom ash, flue gas desulphurisation (FGD) gypsum. However, less than 25% of the total ash from power stations has found an industrial use mainly in cement and concrete industry. This creates a massive waste-disposal problem. Disposal of unused fly ash in open tips and ponds, for example, creates pollution problems since the drainage of effluents from the ash in the deposit ponds threaten water supplies by polluting the ground water with traces of toxic chemicals.Recent research has concentrated on the alkali activation of waste pozzolanic materials, especially ground blast furnace slag. This thesis has investigated the alkali activation of low calcium fly ashes. These form very poor pozzolans and the alkali activation of the fly ash offers the opportunity for the large scale use of fly ash. Water glass was selected as a suitable activator for the fly ash. A comprehensive series of tests have been carried out to gain information on the effect of different parameters, such as proportion and composition of the constituent materials, curing conditions and casting methods, in developing high performance construction materials. Laboratory investigations were carried out to determine the following characteristics of alkali activated materials

  12. Hydrothermal alteration and mass exchange in the hornblende latite porphyry, Rico, Colorado

    Science.gov (United States)

    Larson, P.B.; Cunningham, C.G.; Naeser, C.W.

    1994-01-01

    The Rico paleothermal anomaly, southwestern Colorado, records the effects of a large hydrothermal system that was active at 4 Ma. This hydrothermal system produced the deep Silver Creek stockwork Mo deposit, which formed above the anomaly's heat source, and shallower base and precious-metal vein and replacement deposits. A 65 Ma hornblende latite porphyry is present as widespread sills throughout the area and provided a homogenous material that recorded the effects of the hydrothermal system up to 8 km from the center. Hydrothermal alteration in the latite can be divided into a proximal facies which consists of two assemblages, quartz-illite-calcite and chlorite-epidote, and a distal facies which consists of a distinct propylitic assemblage. Temperatures were gradational vertically and laterally in the anomaly, and decreased away from the centra heat source. A convective hydrothermal plume, 3 km wide and at least 2 km high, was present above the stock-work molybdenum deposit and consisted of upwelling, high-temperature fluids that produced the proximal alteration facies. Distal facies alteration was produced by shallower cooler fluids. The most important shallow base and precious-metal vein deposits in the Rico district are at or close to the boundary of the thermal plume. Latite within the plume had a large loss of Na2O, large addition of CaO, and variable SiO2 exchante. Distal propylitized latite samples lost small amounts of Na2O and CaO and exchanged minor variable amounts of SiO2. The edge of the plume is marked by steep Na2O exchange gradients. Na2O exchange throughout the paleothermal anomaly was controlled by the reaction of the albite components in primary plagioclase and alkali feldspars. Initial feldspar alteration in the distal facies was dominated by reaction of the plagioclase, and the initial molar ratio of reactants (alkali feldspar albite component to plagioclase albite component) was 0.35. This ratio of the moles of plagioclase to alkali feldspar

  13. Long-range interactions among three alkali-metal atoms

    International Nuclear Information System (INIS)

    Marinescu, M.; Starace, A.F.

    1996-01-01

    The long-range asymptotic form of the interaction potential surface for three neutral alkali-metal atoms in their ground states may be expressed as an expansion in inverse powers of inter-nuclear distances. The first leading powers are proportional to the dispersion coefficients for pairwise atomic interactions. They are followed by a term responsible for a three body dipole interaction. The authors results consist in evaluation of the three body dipole interaction coefficient between three alkali-metal atoms. The generalization to long-range n atom interaction terms will be discussed qualitatively

  14. Exciton emissions in alkali cyanides

    International Nuclear Information System (INIS)

    Weid, J.P. von der.

    1979-10-01

    The emissions of Alkali Cyanides X irradiated at low temperature were measured. In addition to the molecular (Frenkel Type) exciton emissions, another emitting centre was found and tentatively assigned to a charge transfer self trapped exciton. The nature of the molecular exciton emitting state is discussed. (Author) [pt

  15. The Impact of the Source of Alkali on Sludge Batch 3 Melt Rate

    International Nuclear Information System (INIS)

    Smith, M

    2005-01-01

    Previous Savannah River National Laboratory (SRNL) melt rate tests in support of the Defense Waste Processing Facility (DWPF) have indicated that improvements in melt rate can be achieved through an increase in the total alkali of the melter feed. Higher alkali can be attained by the use of an ''underwashed'' sludge, a high alkali frit, or a combination of the two. Although the general trend between melt rate and total alkali (in particular Na 2 O content) has been demonstrated, the question of ''does the source of alkali (SOA) matter?'' still exists. Therefore the purpose of this set of tests was to determine if the source of alkali (frit versus sludge) can impact melt rate. The general test concept was to transition from a Na 2 O-rich frit to a Na 2 O-deficient frit while compensating the Na 2 O content in the sludge to maintain the same overall Na 2 O content in the melter feed. Specifically, the strategy was to vary the amount of alkali in frits and in the sludge batch 3 (SB3) sludge simulant (midpoint or baseline feed was SB3/Frit 418 at 35% waste loading) so that the resultant feeds had the same final glass composition when vitrified. A set of SOA feeds using frits ranging from 0 to 16 weight % Na 2 O (in 4% increments) was first tested in the Melt Rate Furnace (MRF) to determine if indeed there was an impact. The dry-fed MRF tests indicated that if the alkali is too depleted from either the sludge (16% Na 2 O feed) or the frit (the 0% Na 2 O feed), then melt rate was negatively impacted when compared to the baseline SB3/Frit 418 feed currently being processed at DWPF. The MRF melt rates for the 4 and 12% SOA feeds were similar to the baseline SB3/Frit 418 (8% SOA) feed. Due to this finding, a smaller subset of SOA feeds that could be processed in the DWPF (4 and 12% SOA feeds) was then tested in the Slurry-fed Melt Rate Furnace (SMRF). The results from a previous SMRF test with SB3/Frit 418 (Smith et al. 2004) were used as the SMRF melt rate of the baseline

  16. Adsorption of Pb(II) ions from aqueous solution using lignin from ...

    African Journals Online (AJOL)

    The adsorption of lead(II) ions from aqueous solution onto alkali lignin extracted from Hagenia abyssinica was investigated by electrochemical methods. The effect of solution pH, lignin dosage and contact time were investigated at room temperature in a batch system. Adsorption equilibrium was approached within 80 min.

  17. Self-trapped holes in alkali silver halide crystals

    International Nuclear Information System (INIS)

    Awano, T.; Ikezawa, M.; Matsuyama, T.

    1995-01-01

    γ-Ray irradiation at 77 K induces defects in M 2 AgX 3 (M=Rb, K and NH 4 ; X=Br and I) crystals. The irradiation induces self-trapped holes of the form of I 0 in the case of alkali silver iodides, and (halogen) 2 - and (halogen) 0 in the case of ammonium silver halides. The (halogen) 0 is weakly coupled with the nearest alkali metal ion or ammonium ion. It is able to be denoted as RbI + , KI + , NH 4 I + or NH 4 Br + . The directions of hole distribution of (halogen) 2 - and (halogen) 0 were different in each case of the alkali silver iodides, ammonium silver halides and mixed crystal of them. The (halogen) 0 decayed at 160 K in annealing process. The (halogen) 2 - was converted into another form of (halogen) 2 - at 250 K and this decayed at 310 K. A formation of metallic layers was observed on the crystal surface parallel with the c-plane of (NH 4 ) 2 AgI 3 irradiated at room temperature. (author)

  18. Luminescence dating of the PASADO core 5022-1D from Laguna Potrok Aike (Argentina) using IRSL signals from feldspar

    DEFF Research Database (Denmark)

    Buylaert, Jan-Pieter; Murray, A.S.; Gebhardt, A.C.

    2013-01-01

    We have measured and tested a luminescence chronology for the PASADO core 5022-1D from the maar lake of Laguna Potrok Aike. Because of unsuitable quartz OSL characteristics, sand-sized K-feldspar extracts were chosen as a dosimeter and the dose was measured using a post-IR IRSL (pIRIR290......) measurement protocol. Using this approach we were able to access a stable signal and thus avoid the ubiquitous problem of feldspar signal instability. Extensive laboratory tests show that the chosen pIRIR290 protocol is applicable to these samples. We also developed a new criterion based on known relative...... or stratigraphy; the resulting age–depth profile is self-consistent, increases smoothly with depth and is in agreement with independent age control based on volcanic ash layers (Reclús, Mt Burney and Hudson tephras) at the top and middle of the core. Our new luminescence chronology suggests that the 5022-1D core...

  19. The dependence of orange-red IRSL decay curves of potassium feldspars on sample temperature

    International Nuclear Information System (INIS)

    Fattahi, Morteza

    2004-01-01

    This paper presents the effects of stimulation temperature on the infrared stimulated orange-red (600-650 nm) luminescence emission (orange-red infrared simulated luminescence (IRSL)) in potassium feldspar. Investigations explore the relationship between initial (0-2 s), integral (0-100 s), net initial (0-2 s less background over 2 s), net integral (0-100 s less background over 100 s) and last 2 s of the orange-red IRSL signals obtained for 100 s versus stimulation temperature (20-460 degree sign C) on both unpreheated and preheated samples. In the potassium feldspar sample examined, competition effects, including thermal enhancement, depletion and possibly quenching affect the orange-red IRSL signals measured. Observed effects (e.g., thermal enhancement, thermal activation energy and the decay rate) over the temperature range 20-120 degree sign C may be explained by tunnelling luminescence processes, IR transitions to the conduction band following excitations from ground state of electron trap by acquiring thermal energy from the lattice and or the random-walk band-tail model. Preheating prior to orange-red IRSL and Thermoluminescence (TL) measurements provides evidence that there are both shallow and deep traps responsible for low- and high-temperature orange-red IRSL and TL peaks. The effects of both preheating and IR bleaching on the orange-red thermally stimulated luminescence (red emission during thermoluminescence, RTL) provide evidence that bleached RTL traps have no significant contribution in the production of orange-red IRSL signals

  20. Compression-Driven Enhancement of Electronic Correlations in Simple Alkali Metals

    Science.gov (United States)

    Fabbris, Gilberto; Lim, Jinhyuk; Veiga, Larissa; Haskel, Daniel; Schilling, James

    2015-03-01

    Alkali metals are the best realization of the nearly free electron model. This scenario appears to change dramatically as the alkalis are subjected to extreme pressure, leading to unexpected properties such as the departure from metallic behavior in Li and Na, and the occurrence of remarkable low-symmetry crystal structures in all alkalis. Although the mechanism behind these phase transitions is currently under debate, these are believed to be electronically driven. In this study the high-pressure electronic and structural ground state of Rb and Cs was investigated through low temperature XANES and XRD measurements combined with ab initio calculations. The results indicate that the pressure-induced localization of the conduction band triggers a Peierls-like mechanism, inducing the low symmetry phases. This localization process is evident by the pressure-driven increase in the number of d electrons, which takes place through strong spd hybridization. These experimental results indicate that compression turns the heavy alkali metals into strongly correlated electron systems. Work at Argonne was supported by DOE No. DE-AC02-06CH11357. Research at Washington University was supported by NSF DMR-1104742 and CDAC/DOE/NNSA DE-FC52-08NA28554.

  1. Long-range interactions between excited helium and alkali-metal atoms

    KAUST Repository

    Zhang, J.-Y.

    2012-12-03

    The dispersion coefficients for the long-range interaction of the first four excited states of He, i.e., He(2 1,3S) and He(2 1,3P), with the low-lying states of the alkali-metal atoms Li, Na, K, and Rb are calculated by summing over the reduced matrix elements of the multipole transition operators. For the interaction between He and Li the uncertainty of the calculations is 0.1–0.5%. For interactions with other alkali-metal atoms the uncertainty is 1–3% in the coefficient C5, 1–5% in the coefficient C6, and 1–10% in the coefficients C8 and C10. The dispersion coefficients Cn for the interaction of He(2 1,3S) and He(2 1,3P) with the ground-state alkali-metal atoms and for the interaction of He(2 1,3S) with the alkali-metal atoms in their first 2P states are presented in this Brief Report. The coefficients for other pairs of atomic states are listed in the Supplemental Material.

  2. Structural and Magnetic Diversity in Alkali-Metal Manganate Chemistry: Evaluating Donor and Alkali-Metal Effects in Co-complexation Processes.

    Science.gov (United States)

    Uzelac, Marina; Borilovic, Ivana; Amores, Marco; Cadenbach, Thomas; Kennedy, Alan R; Aromí, Guillem; Hevia, Eva

    2016-03-24

    By exploring co-complexation reactions between the manganese alkyl Mn(CH2SiMe3)2 and the heavier alkali-metal alkyls M(CH2SiMe3) (M=Na, K) in a benzene/hexane solvent mixture and in some cases adding Lewis donors (bidentate TMEDA, 1,4-dioxane, and 1,4-diazabicyclo[2,2,2] octane (DABCO)) has produced a new family of alkali-metal tris(alkyl) manganates. The influences that the alkali metal and the donor solvent impose on the structures and magnetic properties of these ates have been assessed by a combination of X-ray, SQUID magnetization measurements, and EPR spectroscopy. These studies uncover a diverse structural chemistry ranging from discrete monomers [(TMEDA)2 MMn(CH2SiMe3)3] (M=Na, 3; M=K, 4) to dimers [{KMn(CH2SiMe3)3 ⋅C6 H6}2] (2) and [{NaMn(CH2SiMe3)3}2 (dioxane)7] (5); and to more complex supramolecular networks [{NaMn(CH2SiMe3)3}∞] (1) and [{Na2Mn2 (CH2SiMe3)6 (DABCO)2}∞] (7)). Interestingly, the identity of the alkali metal exerts a significant effect in the reactions of 1 and 2 with 1,4-dioxane, as 1 produces coordination adduct 5, while 2 forms heteroleptic [{(dioxane)6K2Mn2 (CH2SiMe3)4(O(CH2)2OCH=CH2)2}∞] (6) containing two alkoxide-vinyl anions resulting from α-metalation and ring opening of dioxane. Compounds 6 and 7, containing two spin carriers, exhibit antiferromagnetic coupling of their S=5/2 moments with varying intensity depending on the nature of the exchange pathways. © 2016 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

  3. Yellow stimulated luminescence from potassium feldspar: Observations on its suitability for dating

    International Nuclear Information System (INIS)

    Lauer, T.; Krbetschek, M.; Mauz, B.; Frechen, M.

    2012-01-01

    Yellow stimulated luminescence (Y-OSL) is the light detected from potassium-rich feldspars at 410 nm under stimulation by a yellow light source emitting 590 nm. The investigation of this study aimed at understanding basic luminescence physics of Y-OSL in order to assess the suitability of the technique for dating. The Y-OSL signal properties tested were signal intensity, thermal assistance, thermal stability, sensitivity to daylight and the suitability of a single aliquot regenerative (SAR) protocol to be employed for equivalent dose (D e ) estimation. D e measurements were conducted on samples of Holocene, last glacial and Tertiary age. The tests were undertaken on sedimentary feldspar separates extracted from aeolian, fluvial and coastal deposits. Results from experiments show that the signal intensity increases by measuring Y-OSL at elevated temperature suggesting thermal assistance characteristics similar to infrared stimulated luminescence (IRSL). The yellow stimulated signal remains unaffected by preheat temperatures up to ∼200 °C suggesting higher thermal stability than the IRSL signal. The Y-OSL signal is less light sensitive than the IRSL signal and D e residuals obtained from modern samples are up to 7 Gy indicating suitability of the technique for ‘older’ and well-bleached sediments. The dose recovery tests successfully recovered the given dose if the specific light sensitivity of Y-OSL is taken into account. For every sample Y-OSL D e values obtained by a single aliquot regenerative dose protocol (SAR) are higher than those obtained by an IRSL SAR approach. From these results we infer high thermal stability and a minimal anomalous fading of the Y-OSL signal. We conclude that Y-OSL has a high potential to date Quaternary sediments that were sufficiently bleached in nature.

  4. Alkali production in the mouth and its relationship with certain patient's characteristics

    Directory of Open Access Journals (Sweden)

    Valeria Veiga GORDAN

    2014-12-01

    Full Text Available Objectives To assess the relationships among alkali production, diet, oral health behaviors, and oral hygiene. Methods Data from 52 subjects including demographics, diet, and oral hygiene scores were analyzed against the level of arginine and urea enzymes in plaque and saliva samples. An oral habit survey was completed that included: use of tobacco (TB, alcohol (AH, sugary drinks (SD, and diet. Alkali production through arginine deiminase (ADS and urease activities were measured in smooth-surface supragingival dental plaque and un stimulated saliva samples from all subjects. ADS and urease activities were measured by quantification of the ammonia generated from the incubation of plaque or saliva samples. Spearman correlations were used to compute all associations. Results Participants in the lowest SES (Socio-economic status group had the habit of consuming sugary drinks the most and had the highest rate of tobacco use. Males consumed significantly more alcohol than females. No significant relationship was found between age or gender and alkali production. Higher rates of sugary drink consumption and tobacco use were significantly related to lower alkali production. Conclusion The study showed a relationship between alkali production and oral hygiene, diet, and certain oral health behaviors. Poor oral hygiene was significantly associated with age, lower SES, tobacco use, and alcohol, and sugary drinks consumption. Clinical relevance Certain oral health behaviors have an impact on oral hygiene and on alkali production; it is important to address these factors with patients as a strategy for caries control.

  5. Alkali production in the mouth and its relationship with certain patient's characteristics.

    Science.gov (United States)

    Gordan, Valeria Veiga; McEdward, Deborah Landry; Ottenga, Marc Edward; Garvan, Cynthia Wilson; Harris, Pearl Ann

    2014-01-01

    To assess the relationships among alkali production, diet, oral health behaviors, and oral hygiene. Data from 52 subjects including demographics, diet, and oral hygiene scores were analyzed against the level of arginine and urea enzymes in plaque and saliva samples. An oral habit survey was completed that included: use of tobacco (TB), alcohol (AH), sugary drinks (SD), and diet. Alkali production through arginine deiminase (ADS) and urease activities were measured in smooth-surface supragingival dental plaque and un stimulated saliva samples from all subjects. ADS and urease activities were measured by quantification of the ammonia generated from the incubation of plaque or saliva samples. Spearman correlations were used to compute all associations. Participants in the lowest SES (Socio-economic status) group had the habit of consuming sugary drinks the most and had the highest rate of tobacco use. Males consumed significantly more alcohol than females. No significant relationship was found between age or gender and alkali production. Higher rates of sugary drink consumption and tobacco use were significantly related to lower alkali production. The study showed a relationship between alkali production and oral hygiene, diet, and certain oral health behaviors. Poor oral hygiene was significantly associated with age, lower SES, tobacco use, and alcohol, and sugary drinks consumption. Clinical relevance Certain oral health behaviors have an impact on oral hygiene and on alkali production; it is important to address these factors with patients as a strategy for caries control.

  6. Alkali-treated titanium selectively regulating biological behaviors of bacteria, cancer cells and mesenchymal stem cells.

    Science.gov (United States)

    Li, Jinhua; Wang, Guifang; Wang, Donghui; Wu, Qianju; Jiang, Xinquan; Liu, Xuanyong

    2014-12-15

    Many attentions have been paid to the beneficial effect of alkali-treated titanium to bioactivity and osteogenic activity, but few to the other biological effect. In this work, hierarchical micro/nanopore films were prepared on titanium surface by acid etching and alkali treatment and their biological effects on bacteria, cancer cells and mesenchymal stem cells were investigated. Gram-positive Staphylococcus aureus, Gram-negative Escherichia coli, and human cholangiocarcinoma cell line RBE were used to investigate whether alkali-treated titanium can influence behaviors of bacteria and cancer cells. Responses of bone marrow mesenchymal stem cells (BMMSCs) to alkali-treated titanium were also subsequently investigated. The alkali-treated titanium can potently reduce bacterial adhesion, inhibit RBE and BMMSCs proliferation, while can better promote BMMSCs osteogenesis and angiogenesis than acid-etched titanium. The bacteriostatic ability of the alkali-treated titanium is proposed to result from the joint effect of micro/nanotopography and local pH increase at bacterium/material interface due to the hydrolysis of alkali (earth) metal titanate salts. The inhibitory action of cell proliferation is thought to be the effect of local pH increase at cell/material interface which causes the alkalosis of cells. This alkalosis model reported in this work will help to understand the biologic behaviors of various cells on alkali-treated titanium surface and design the intended biomedical applications. Copyright © 2014 Elsevier Inc. All rights reserved.

  7. Is Electronegativity a Useful Descriptor for the 'Pseudo-Alkali-Metal' NH4?

    International Nuclear Information System (INIS)

    Whiteside, Alexander; Xantheas, Sotiris S.; Gutowski, Maciej S.

    2011-01-01

    Molecular ions in the form of 'pseudo-atoms' are common structural motifs in chemistry, with properties that are transferrable between different compounds. We have determined the electronegativity of the 'pseudo-alkali metal' ammonium (NH4) and evaluated its reliability as a descriptor in comparison to the electronegativities of the alkali metals. The computed properties of its binary complexes with astatine and of selected borohydrides confirm the similarity of NH4 to the alkali metal atoms, although the electronegativity of NH4 is relatively large in comparison to its cationic radius. We paid particular attention to the molecular properties of ammonium (angular anisotropy, geometric relaxation, and reactivity), which can cause deviations from the behaviour expected of a conceptual 'true alkali metal' with this electronegativity. These deviations allow for the discrimination of effects associated with the polyatomic nature of NH4.

  8. Method and composition for testing for the presence of an alkali metal

    International Nuclear Information System (INIS)

    Guon, J.

    1981-01-01

    A method and composition for detecting the presence of an alkali metal on the surface of a body such as a metal plate, tank, pipe or the like is provided. The method comprises contacting the surface with a thin film of a liquid composition comprising a light-colored pigment, an acid-base indicator, and a nonionic wetting agent dispersed in a liquid carrier comprising a minor amount of water and a major amount of an organic solvent selected from the group consisting of the lower aliphatic alcohols, ketones and ethers. Any alkali metal present on the surface in elemental form or as an alkali metal hydroxide or alkali metal carbonate will react with the acid-base indicator to produce a contrasting color change in the thin film, which is readily discernible by visual observation or automatic techniques

  9. The alkali and alkaline earth metal doped ZnO nanotubes: DFT studies

    International Nuclear Information System (INIS)

    Peyghan, Ali Ahmadi; Noei, Maziar

    2014-01-01

    Doping of several alkali and alkaline earth metals into sidewall of an armchair ZnO nanotube has been investigated by employing the density functional theory in terms of energetic, geometric, and electronic properties. It has been found that doping processes of the alkali and alkaline metals are endothermic and exothermic, respectively. Based on the results, contrary to the alkaline metal doping, the electronic properties of the tube are much more sensitive to alkali metal doping so that it is transformed from intrinsic semiconductor with HOMO–LUMO energy gap of 3.77 eV to an extrinsic semiconductor with the energy gap of ∼1.11–1.95 eV. The doping of alkali and alkaline metals increases and decreases the work function of the tube, respectively, which may influence the electron emission from the tube surface

  10. Graphite-based detectors of alkali metals for nuclear power plants

    International Nuclear Information System (INIS)

    Kalandarishvili, A.G.; Kuchukhidze, V.A.; Sordiya, T.D.; Shartava, Sh.Sh.; Stepennov, B.S.

    1993-01-01

    The coolants most commonly used in today's fast reactors are alkali metals or their alloys. A major problem in nuclear plant design is leakproofing of the liquid-metal cooling system, and many leak detection methods and safety specifications have been developed as a result. Whatever the safety standards adopted for nuclear plants in different countries, they all rely on the basic fact that control of the contamination and radiation hazards involved requires reliable monitoring equipment. Results are presented of trials with some leak detectors for the alkali-metal circuits of nuclear reactors. The principal component affecting the detector performance is the sensing element. In the detectors graphite was employed, whose laminar structure enables it to absorb efficiently alkali-metal vapors at high temperatures (320--500 K). This produces a continuous series of alkali-metal-graphite solid solutions with distinct electrical, thermal, and other physical properties. The principle of operation of the detectors resides in the characteristic reactions of the metal-graphite system. One detector type uses the change of electrical conductivity of the graphite-film sensor when it is exposed to alkali-metal vapor. In order to minimize the effect of temperature on the resistance the authors prepared composite layers of graphite intercalated with a donor impurity (cesium or barium), and a graphite-nickel material. The addition of a small percentage of cesium, barium, or nickel produces a material whose temperature coefficient of resistance is nearly zero. Used as a sensing element, such a material can eliminate the need for thermostatic control of the detector

  11. Mass Spectrometric Analyses of Phosphatidylcholines in Alkali-Exposed Corneal Tissue

    Science.gov (United States)

    Crane, Ashley M.; Hua, Hong-Uyen; Coggin, Andrew D.; Gugiu, Bogdan G.; Lam, Byron L.; Bhattacharya, Sanjoy K.

    2012-01-01

    Purpose. The aims were to determine whether exposure to sodium hydroxide results in predictable changes in phosphatidylcholine (PC) in corneal tissue and if PC profile changes correlate to exposure duration. PCs are major components of the cell membrane lipid bilayer and are often involved in biological processes such as signaling. Methods. Enucleated porcine (n = 140) and cadaver human eyes (n = 20) were exposed to water (control) and 11 M NaOH. The corneas were excised and lipids were extracted using the Bligh and Dyer method with suitable modifications. Class-specific lipid identification was carried out using a ratiometric lipid standard on a TSQ Quantum Access Max mass spectrometer. Protein amounts were determined using Bradford assays. Results. Control and alkali-treated corneas showed reproducible PC spectra for both porcine and human corneas. Over 200 PCs were identified for human and porcine control and each experimental time point. Several PC species (m/z values) consequent upon alkali exposure could not be ascribed to a recorded PC species. Control and treated groups showed 41 and 29 common species among them for porcine and human corneas, respectively. The unique PC species peaked at 12 minutes and at 30 minutes for human and porcine corneas followed by a decline consistent with an interplay of alkali penetration and hydrolyses at various time points. Conclusions. Alkali exposure dramatically changes the PC profile of cornea. Our data are consistent with penetration and hydrolysis as stochastic contributors to changes in PCs due to exposure to alkali for a finite duration and amount. PMID:22956606

  12. Magnetoelectric Jones spectroscopy of alkali atoms

    International Nuclear Information System (INIS)

    Chernushkin, V V; Mironova, P V; Ovsiannikov, V D

    2008-01-01

    The Jones effect in a medium of free atoms exposed to static electric and magnetic fields is a useful tool for determining details of an atomic structure. For atoms in their nS ground states irradiated by a monochromatic wave in resonance with a single-photon transition to an n' D state, the bilinear Jones effect is not shaded by the quadratic Kerr and Cotton-Mouton effects, nor by the linear in magnetic field Faraday effect. The position and shape of the amplitude resonance may provide information on spectroscopic properties of atomic levels. We generalize equations for the Jones-effect amplitude to the case of a doublet structure of energy levels and calculate corresponding parameters for alkali atoms. General equations are derived for the amplitude dependence on the relative orientation of the static electric and magnetic fields and on the angle between the static field and the major axis of the wave polarization vector. These equations demonstrate explicitly that the three bilinear-in-static-fields optical birefringence effects-(i) the Jones birefringence (in parallel fields), (ii) the linear birefringence and (iii) the directional birefringence (the last two in perpendicular fields)-correspond to particular cases of the bilinear-in-static-fields correction to the amplitude of Rayleigh forward scattering

  13. Electron core ionization in compressed alkali metal cesium

    Science.gov (United States)

    Degtyareva, V. F.

    2018-01-01

    Elements of groups I and II in the periodic table have valence electrons of s-type and are usually considered as simple metals. Crystal structures of these elements at ambient pressure are close-packed and high-symmetry of bcc and fcc-types, defined by electrostatic (Madelung) energy. Diverse structures were found under high pressure with decrease of the coordination number, packing fraction and symmetry. Formation of complex structures can be understood within the model of Fermi sphere-Brillouin zone interactions and supported by Hume-Rothery arguments. With the volume decrease there is a gain of band structure energy accompanied by a formation of many-faced Brillouin zone polyhedra. Under compression to less than a half of the initial volume the interatomic distances become close to or smaller than the ionic radius which should lead to the electron core ionization. At strong compression it is necessary to assume that for alkali metals the valence electron band overlaps with the upper core electrons, which increases the valence electron count under compression.

  14. A hybrid composite dike suite from the northern Arabian Nubian Shield, southwest Jordan: Implications for magma mixing and partial melting of granite by mafic magma

    Science.gov (United States)

    Jarrar, Ghaleb H.; Yaseen, Najel; Theye, Thomas

    2013-03-01

    The Arabian Nubian Shield is an exemplary juvenile continental crust of Neoproterozoic age (1000-542 Ma). The post-collisional rift-related stage (~ 610 to 542 Ma) of its formation is characterized among others by the intrusion of several generations of simple and composite dikes. This study documents a suite of hybrid composite dikes and a natural example of partial melting of granite by a mafic magma from the northernmost extremity of Arabian Nubian Shield in southwest Jordan. The petrogenesis of this suite is discussed on the basis of field, petrographic, geochemical, and Rb/Sr isotopic data. These dikes give spectacular examples of the interaction between basaltic magma and the granitic basement. This interaction ranges from brecciation, partial melting of the host alkali feldspar granite to complete assimilation of the granitic material. Field structures range from intrusive breccia (angular partially melted granitic fragments in a mafic groundmass) to the formation of hybrid composite dikes that are up to 14 m in thickness. The rims of these dikes are trachyandesite (latite) with alkali feldspar ovoids (up to 1 cm in diameter); while the central cores are trachydacite to dacite and again with alkali feldspar ovoids and xenoliths from the dike rims. The granitic xenoliths in the intrusive breccia have been subjected to at least 33% partial melting. A seven-point Rb/Sr isochron from one of these composite dikes yields an age of 561 ± 33 Ma and an initial 87Sr/86Sr ratio of 0.70326 ± 0.0003 (2σ) and MSWD of 0.62. Geochemical modeling using major, trace, rare earth elements and isotopes suggests the generation of the hybrid composite dike suite through the assimilation of 30% to 60% granitic crustal material by a basaltic magma, while the latter was undergoing fractional crystallization at different levels in the continental crust.

  15. Petrological and geochemical studies of alkaline rocks from continental Brazil. The tunas massif, state of Parana

    International Nuclear Information System (INIS)

    Gomes, C.B.; Barbieri, M.

    1987-01-01

    The Tunas massif, outcropping 80 km from the city of Curitiba, Parana State, southern Brazil, covers about 22 km 2 . It intruded into Precambrian metaigneous and metasedimentary units about 80 Ma ago (K/Ar and Rb/Sr data); five subcircular volcanic structures are recognized. Syenites and alkali syenites (plus some pulaskites) are the main rock-types, with subordinate alkali gabbros, syenogabbros, essexites and syenodiorites; small late syenitic dikes are also found. Magmatic breccias containing clasts of all rock-types are widespread. Main minerals are feldspars (both alkali feldspars and plagioclases, varying from bytownite to more sodic members), Ca-pyroxenes (Ti-salites grading towards ferrosalites and aegirine-augites), amphiboles (mainly pargasites, although kaersutites and katophorites are also present), Fe-biotites (sometimes enriched in Ti), olivines (hortonolites to ferrohortonolites), quartz and feldspathoids (both fresh and altered nephelines and sodalites); main accessories are Ti-magnetites (with exsolved ilmenite) and apatite. In the AFM diagram, whole rock chemistry depicts a typical alkaline trend. Binary variation diagrams (D.I. vs. several elements) show positive correlation for Si, Na and K, and negative slopes for Mg and Ca. The variation in the amounts of Ni, Cr and V with differentiation can be explained by withdrawal of olivine, Ca-pyroxenes and magnetite, and that of Sr and Ba by the fractionation of feldspars. The rocks are also relatively enriched in REE, a trend which is more pronounced for the light REE. Mass balance calculations show that the overall differentiation trend of the Tunas rocks can be explained by crystal fractionation, although several complexities arise and point to more complex genetic patterns. Isotopic Rb/Sr ratios are consistent with a mantle origin for the parental magma; dike rocks, however, with 87 Sr 86 Sr i = 0.70777 - 0.70806, were probably contaminated by crustal material. (author) [pt

  16. Long-range interactions between excited helium and alkali-metal atoms

    KAUST Repository

    Zhang, J.-Y.; Schwingenschlö gl, Udo; Shi, T.-Y.; Tang, L.-Y.; Yan, Z.-C.

    2012-01-01

    –5% in the coefficient C6, and 1–10% in the coefficients C8 and C10. The dispersion coefficients Cn for the interaction of He(2 1,3S) and He(2 1,3P) with the ground-state alkali-metal atoms and for the interaction of He(2 1,3S) with the alkali-metal atoms in their first

  17. Influence of diopside: feldspar ratio in ceramic reactions assessed by quantitative phase analysis (X-ray diffraction - Rietveld method)

    International Nuclear Information System (INIS)

    Kuzmickas, L.; Andrade, F.R.D.; Szabo, G.A.J.; Motta, J.F.M.; Cabral Junior, M.

    2013-01-01

    White ceramics were produced with raw mixtures prepared with varying proportions of diopside-rich rock (0 to 20 wt.%) and potassic feldspar (40 to 20 wt.%), and fixed proportions of kaolinite (40 wt.%) and quartz (20 wt.%), fired in a temperature range from 1170 to 1210 deg C. The phases identified in the experimental ceramics were quartz, anorthite, mullite and glass, and their relative mass proportions were determined by X-ray diffraction (Rietveld method). The addition of diopside as a partial substitute for potassic feldspar causes the formation of a calcium silicate, analogous of the natural anorthite (CaSi 2 Al 2 O 8 ) in the ceramics, with proportional reduction in its glass and mullite contents. Water absorption and porosity of the ceramic bodies clearly decrease with increasing firing temperature, while the effect of the raw mixture composition on the physical and mechanical properties of the ceramics is less evident. Diopside-rich rock has low iron content (1.5 wt.% Fe 2 O 3 ) and, therefore, promotes white burning. (author)

  18. Influence of diopside: feldspar ratio in ceramic reactions assessed by quantitative phase analysis (X-ray diffraction - Rietveld method)

    Energy Technology Data Exchange (ETDEWEB)

    Kuzmickas, L.; Andrade, F.R.D.; Szabo, G.A.J. [Universidade de Sao Paulo (IGc/USP), SP (Brazil). Inst. de Geociencias. Dept. de Mineralogia e Geotecnia; Motta, J.F.M.; Cabral Junior, M., E-mail: lukuzmickas@gmail.com, E-mail: dias@usp.br, E-mail: gajszabo@usp.b, E-mail: motta.jf@gmail.com, E-mail: marsis@ipt.br [Instituto de Pesquisas Tecnologicas (IPT), Sao Paulo, SP (Brazil). Secao de Recursos Minerais e Tecnologia Ceramica

    2013-04-15

    White ceramics were produced with raw mixtures prepared with varying proportions of diopside-rich rock (0 to 20 wt.%) and potassic feldspar (40 to 20 wt.%), and fixed proportions of kaolinite (40 wt.%) and quartz (20 wt.%), fired in a temperature range from 1170 to 1210 deg C. The phases identified in the experimental ceramics were quartz, anorthite, mullite and glass, and their relative mass proportions were determined by X-ray diffraction (Rietveld method). The addition of diopside as a partial substitute for potassic feldspar causes the formation of a calcium silicate, analogous of the natural anorthite (CaSi{sub 2}Al{sub 2}O{sub 8}) in the ceramics, with proportional reduction in its glass and mullite contents. Water absorption and porosity of the ceramic bodies clearly decrease with increasing firing temperature, while the effect of the raw mixture composition on the physical and mechanical properties of the ceramics is less evident. Diopside-rich rock has low iron content (1.5 wt.% Fe{sub 2}O{sub 3}) and, therefore, promotes white burning. (author)

  19. Sequence specificity of alkali-labile DNA damage photosensitized by suprofen.

    Science.gov (United States)

    Starrs, S M; Davies, R J

    2000-09-01

    On irradiation at UVB wavelengths, in aerated neutral aqueous solution, the anti-inflammatory drug suprofen (SP) photosensitizes the production of alkali-labile cleavage sites in DNA much more efficiently than direct strand breaks. It is active at submillimolar concentrations despite having no significant binding affinity for DNA. Gel sequencing studies utilizing 32P-end-labeled oligonucleotides have revealed that piperidine-sensitive lesions are formed predominantly at the positions of guanine (G) bases, with the extent of modification being UV dose- and SP concentration-dependent. Quite distinct patterns of G-specific damage are observed in single-stranded and duplex DNA molecules. The uniform attack at all G residues in single-stranded DNA, which is enhanced in D2O, is compatible with a Type-II mechanism. SP is a known generator of singlet oxygen whose participation in the reaction is supported by the effects of quenchers and scavengers. In duplex DNA, piperidine-induced cleavage occurs with high selectivity at the 5'-G of GG and (less prominently) GA doublets. This behavior is characteristic of a Type-I process involving electron transfer from DNA to photoexcited SP molecules. The ability of SP to sensitize the formation of Type-I and Type-II photo-oxidation products from 2'-deoxyguanosine attests to the feasibility of competing mechanisms in DNA.

  20. Energy conservation in the primary aluminum and chlor-alkali industries

    Energy Technology Data Exchange (ETDEWEB)

    1980-10-01

    The primary aluminum and chlor-alkali industries together use nearly 13% of the electrical energy consumed by US industry. As part of its mission to promote energy conservation in basic US industries, the DOE surveys the present technological status of the major electrochemical industries and evaluates promising technological innovations that may lead to reduced energy requirements. This study provides technical and economic analyses in support of a government program of research and development in advanced electrolytic technology. This program is intended to supplement the development efforts directed toward energy savings by private industry. Sections II and III of this report cover aluminum and chlorine production processes only, since these two industries represent over 90% of the electrical energy requirements of all electrolytic industries in the United States. Section IV examines barriers to accelerated research and development by the electrolytic industries, and makes suggestions for government actions to overcome these barriers.

  1. Alkali and chlorine in biomass - a problem in connection with power generation. Alkali och klor i biomassa - ett problem vid elgenerering

    Energy Technology Data Exchange (ETDEWEB)

    Gaerdenaes, S

    1991-06-04

    The literature survey gives a summary of the macronutrients and the variations in different biomass. Especially alkali is discussed. The work gives an account of difficult biomass fuels which will rather be used in hot water boilers than in gas turbines of power generation. The amount of alkali and chlorine increases from hardwood < softwood < salix < straw from Phalaris arundineral (harvested during summer). The range of variation was 10-25 between the assortments. The fraction division is the most important factor for the variation. Alkaline content also depend on age, soil fertility and storage methods. Seasonal aspects and local depositions are less important. However, great care should be taken with fuel from coastal areas because of chlorine depositions. Gasification of biomass to produce gas for combined cycle operation poses special problems. The alkali content of logging residues have to be cleaned up to approximately 99 % in the example. When the process gas is originated from straw or salix the separation have to be even more efficient. The method used for the separation could be based on wet or dry technic hotgas cleanup has not yet been tested in large scale but seems to be a promising method to attain high degree of separation and power efficiency. Difficulties of power generation make straw fuels less interesting. The content of alkali and chlorine can be considerably decreased by changing the way of fertilization and cultivation period. If everything turns out well, this would give a complementary for gasification or steam generation. To the greates part this fuels will however be used in pure heat production. (author).

  2. Alkali-labile sites and post-irradiation effects in single-stranded DNA induced by H radicals

    International Nuclear Information System (INIS)

    Lafleur, M.V.M.; Heuvel, N. van; Woldhuis, J.; Loman, H.

    1978-01-01

    Single-stranded phiX174 DNA in aqueous solutions has been irradiated in the absence of oxygen, under conditions in which H radicals react with the DNA. It was shown that H radical reactions result in breaks, which contribute approximately 10 per cent inactivation. Further, two types of alkali-labile sites were formed. One was lethal and gave rise to single-strand breaks by alkali and was most probably identical with post-irradiation heat damage and contributed about 33 per cent to the inactivation mentioned above. The other consisted of non-lethal damage, partly dihydropyrimidine derivatives, and was converted to lethal damage by alkali. This followed from experiments in which the DNA was treated with osmium-tetroxide, which oxidized thymine to 5,6-dihydroxydihydrothymine. Treatment with alkali of this DNA gave the same temperature dependence as found for the non-lethal alkali-labile sites in irradiated DNA. A similar temperature dependence was found for dihydrothymine and irradiated pyrimidines with alkali. (author)

  3. Alkali promotion of N-2 dissociation over Ru(0001)

    DEFF Research Database (Denmark)

    Mortensen, Jens Jørgen; Hammer, Bjørk; Nørskov, Jens Kehlet

    1998-01-01

    Using self-consistent density functional calculations, we show that adsorbed Na and Cs lower the barrier for dissociation of N2 on Ru(0001). Since N2 dissociation is a crucial step in the ammonia synthesis reaction, we explain in this way the experimental observation that alkali metals promote th...... the ammonia synthesis reaction over Ru catalysts. We also show that the origin of this effect is predominantly a direct electrostatic attraction between the adsorbed alkali atoms and the dissociating molecule....

  4. High effective silica fume alkali activator

    Indian Academy of Sciences (India)

    Unknown

    Abstract. Growing demands on the engineering properties of cement based materials and the urgency to decrease unsuitable ecologic impact of Portland cement manufacturing represent significant motivation for the development of new cement corresponding to these aspects. One category represents prospective alkali.

  5. luminescence in coloured alkali halide crystals

    Indian Academy of Sciences (India)

    have studied the effect of annealing in chlorine gas on the ML of X-rayed KCl crystals. ..... high temperature because of the thermal bleaching of the coloration in alkali halide ..... [31] J Hawkins, Ph.D. Thesis (University of Reading, 1976).

  6. Negative ion formation in collisions involving excited alkali atoms

    International Nuclear Information System (INIS)

    Cheret, M.

    1988-01-01

    Ion-pair production is considered as the prototype of the crossing problem between potential energy curves. In general an alkali atom is one of the reactants the other being an halogen, hydrogen atom or molecule. Experimental results are generally analyzed in the framework of the Landau-Zener-Stuekelberg theory, ionization potential and electron affinity, being the most important parameters. In order to vary these parameters over a wide range two experimental works have been devoted to systems of excited alkali atoms colliding with ground state alkali atoms. In the first study Rb atoms are excited to various ns or nd states from Rb(5d) to Rb(9s) in a cell. The second study is devoted to the Na(3p)-Na(3s) system, in this study also the possibility of creating excited negative ions (Na - (3s3p)) has been investigated. These results are presented and analyzed. Finally further developments of the subject are suggested. 17 refs.; 8 figs.; 1 table

  7. Theoretical study on the thermal and optical features of a diode side-pumped alkali laser

    Science.gov (United States)

    Han, Juhong; Liu, Xiaoxu; Wang, Hongyuan; Cai, He; An, Guofei; Zhang, Wei; Wang, You

    2018-03-01

    As one of the most hopeful candidates to achieve high power performances, a diode-pumped alkali laser (DPAL) has attracted a lot of attention in the last decade. Comparing with a diode end-pumped alkali laser (DEPAL), a diode side-pumped alkali laser (DSPAL) has great potentiality to realize an even-higher output of alkali lasers. However, there are few related researching studies concern DSPAL. In this paper, we introduce a theoretical model to investigate the physical features of a double-directions side-pumped alkali laser. The distributions of the population density, temperature, and absorption power at the cross section of a vapor cell are systematically studied. The analyses should be valuable for design of a steady high-powered DPAL.

  8. Comparative metabolic responses and adaptive strategies of wheat (Triticum aestivum) to salt and alkali stress.

    Science.gov (United States)

    Guo, Rui; Yang, Zongze; Li, Feng; Yan, Changrong; Zhong, Xiuli; Liu, Qi; Xia, Xu; Li, Haoru; Zhao, Long

    2015-07-07

    It is well known that salinization (high-pH) has been considered as a major environmental threat to agricultural systems. The aim of this study was to investigate the differences between salt stress and alkali stress in metabolic profiles and nutrient accumulation of wheat; these parameters were also evaluated to determine the physiological adaptive mechanisms by which wheat tolerates alkali stress. The harmful effect of alkali stress on the growth and photosynthesis of wheat were stronger than those of salt stress. High-pH of alkali stress induced the most of phosphate and metal ions to precipitate; as a result, the availability of nutrients significantly declined. Under alkali stress, Ca sharply increased in roots, however, it decreased under salt stress. In addition, we detected the 75 metabolites that were different among the treatments according to GC-MS analysis, including organic acids, amino acids, sugars/polyols and others. The metabolic data showed salt stress and alkali stress caused different metabolic shifts; alkali stress has a stronger injurious effect on the distribution and accumulation of metabolites than salt stress. These outcomes correspond to specific detrimental effects of a highly pH environment. Ca had a significant positive correlation with alkali tolerates, and increasing Ca concentration can immediately trigger SOS Na exclusion system and reduce the Na injury. Salt stress caused metabolic shifts toward gluconeogenesis with increased sugars to avoid osmotic stress; energy in roots and active synthesis in leaves were needed by wheat to develop salt tolerance. Alkali stress (at high pH) significantly inhibited photosynthetic rate; thus, sugar production was reduced, N metabolism was limited, amino acid production was reduced, and glycolysis was inhibited.

  9. Hydrothermal calcification of alkali treated titanium in CaHPO_4 solution

    International Nuclear Information System (INIS)

    Fu, T.; Fan, J.T.; Shen, Y.G.; Sun, J.M.

    2017-01-01

    The alkali treated titanium was hydrothermally treated in water and 10 mM CaHPO_4 solution (nominal concentration) at 80–180 °C to crystallize the titanate hydrogel layer and calcify the alkali treated titanium. Surface structure and elemental composition of the samples were analyzed by scanning electron microscopy, energy dispersive x-ray analysis, x-ray photoelectron spectroscopy, x-ray diffraction and Raman spectroscopy. Porous titanate hydrogel layer is formed on titanium after the alkali treatment. For the hydrothermal treatment in water, the hydrogel layer is crystallized as anatase TiO_2 with nanoporous or nanofibrous structure at 100 and 120 °C, and the layer is converted to anatase nanoparticles at 150 and 180 °C. For the hydrothermal treatment in the CaHPO_4 solution, hydroxyapatite nanocrystallites are deposited at the samples surface at 80–120 °C, but only anatase nanoparticles are formed at 150 and 180 °C. The growth of hydroxyapatite nanocrystallites is influenced by pH and temperature variations of the solution. The present alkali-hydrothermal treatment can avoid higher temperatures involved in the traditional alkali-heat treatments, which is applicable for bioactive surface modification of the thermally sensitive titanium alloys. The results also show that Raman spectroscopy is a useful technique to analyze the microstructure of TiO_2 and apatite films. - Highlights: • The alkali treated titanium is hydrothermally calcified in a CaHPO_4 solution. • HA nanocrystallites are formed at 80–120 °C, but TiO_2 nanoparticles at 150–180 °C. • The growth mechanism of HA nanocrystallites is discussed. • This low-temperature method is fit for some special titanium alloys.

  10. Electrochemical lithium migration to mitigate alkali-silica reaction in existing concrete structures

    NARCIS (Netherlands)

    Silva De Souza, L.M.

    2016-01-01

    Alkali-silica reaction (ASR) is a deterioration process that affects the durability of concrete structures worldwide. During the reaction, hydroxyl and alkali ions present in the pore solution react with reactive silica from the aggregate, forming a hygroscopic ASR gel. Alternatively, the silica

  11. Structural and functional properties of alkali-treated high-amylose rice starch.

    Science.gov (United States)

    Cai, Jinwen; Yang, Yang; Man, Jianmin; Huang, Jun; Wang, Zhifeng; Zhang, Changquan; Gu, Minghong; Liu, Qiaoquan; Wei, Cunxu

    2014-02-15

    Native starches were isolated from mature grains of high-amylose transgenic rice TRS and its wild-type rice TQ and treated with 0.1% and 0.4% NaOH for 7 and 14 days at 35 °C. Alkali-treated starches were characterised for structural and functional properties using various physical methods. The 0.1% NaOH treatment had no significant effect on structural and functional properties of starches except that it markedly increased the hydrolysis of starch by amylolytic enzymes. The 0.4% NaOH treatment resulted in some changes in structural and functional properties of starches. The alkali treatment affected granule morphology and decreased the electron density between crystalline and amorphous lamellae of starch. The effect of alkali on the crystalline structure including long- and short-range ordered structure was not pronounced. Compared with control starch, alkali-treated TRS starches had lower amylose content, higher onset and peak gelatinisation temperatures, and faster hydrolysis of starch by HCl and amylolytic enzymes. Copyright © 2013 Elsevier Ltd. All rights reserved.

  12. Synergistic capture mechanisms for alkali and sulfur species from combustion. Final report

    Energy Technology Data Exchange (ETDEWEB)

    Peterson, T.W.; Shadman, F.; Wendt, J.O.L.; Mwabe, P.O.

    1994-02-01

    Experimental work was carried out on a 17 kW, 600 cm long, gas laboratory combustor, to investigate the post flame reactive capture of alkali species by kaolinite. Emphasis was on alkali/sorbent interactions occurring in flue gas at temperatures above the alkali dewpoint and on the formation of water insoluble reaction products. Time-temperature studies were carried out by injecting kaolinite at different axial points along the combustor. The effect of chlorine and sulfur on alkali capture was investigated by doping the flame with SO{sub 2} and Cl{sub 2} gases to simulate coal flame environments. Particle time and temperature history was kept as close as possible to that which would ordinarily be found in a practical boiler. Experiments designed to extract apparent initial reaction rates were carried using a narrow range, 1-2 {mu}m modal size sorbent, while, a coarse, multi size sorbent was used to investigate the governing transport mechanisms. The capture reaction has been proposed to be between alkali hydroxide and activated kaolinite, and remains so in the presence of sulfur and chlorine. The presence of sulfur reduces sodium capture by under 10% at 1300{degree}C. Larger reductions at lower temperatures are attributed to the elevated dewpoint of sodium ({approximately}850{degree}C) with subsequent reduction in sorbent residence time in the alkali gas phase domain. Chlorine reduces sodium capture by 30% across the temperature range covered by the present experiments. This result has been linked to thermodynamic equilibria between sodium hydroxide, sodium chloride and water.

  13. Therapeutic effects of zerumbone in an alkali-burned corneal wound healing model.

    Science.gov (United States)

    Kim, Jong Won; Jeong, Hyuneui; Yang, Myeon-Sik; Lim, Chae Woong; Kim, Bumseok

    2017-07-01

    Cornea is an avascular transparent tissue. Ocular trauma caused by a corneal alkali burn induces corneal neovascularization (CNV), inflammation, and fibrosis, leading to vision loss. The purpose of this study was to examine the effects of Zerumbone (ZER) on corneal wound healing caused by alkali burns in mice. CNV was induced by alkali-burn injury in BALB/C female mice. Topical ZER (three times per day, 3μl each time, at concentrations of 5, 15, and 30μM) was applied to treat alkali-burned mouse corneas for 14 consecutive days. Histopathologically, ZER treatment suppressed alkali burn-induced CNV and decreased corneal epithelial defects induced by alkali burns. Corneal tissue treated with ZER showed reduced mRNA levels of pro-angiogenic genes, including vascular endothelial growth factor, matrix metalloproteinase-2 and 9, and pro-fibrotic factors such as alpha smooth muscle actin and transforming growth factor-1 and 2. Immunohistochemical analysis demonstrated that the infiltration of F4/80 and/or CCR2 positive cells was significantly decreased in ZER-treated corneas. ZER markedly inhibited the mRNA and protein levels of monocyte chemoattractant protein-1 (MCP-1) in human corneal fibroblasts and murine peritoneal macrophages. Immunoblot analysis revealed that ZER decreased the activation of signal transducer and activator of transcription 3 (STAT3), with consequent reduction of MCP-1 production by these cells. In conclusion, topical administration of ZER accelerated corneal wound healing by inhibition of STAT3 and MCP-1 production. Copyright © 2017. Published by Elsevier B.V.

  14. Pembuatan Sabun Cair Menggunakan Alkali Dari Kulit Coklat (Theobroma cacao L.) dengan Minyak Kelapa

    OpenAIRE

    Paduana, Aulia Bismar

    2017-01-01

    120405037 Penelitian ini bertujuan untuk mengetahui potensi kulit coklat sebagai alkali pada proses pembuatan sabun natural dan mengetahui sifat-sifat sabun natural yang dihasilkan dari minyak kelapa sebagai sumber asam lemak. Bahan ? bahan yang digunakan, antara lain minyak kelapa, alkali dari kulit coklat dan aquadest. Variabel ? variabel yang diamati, antara lain temperatur reaksi pembuatan sabun, waktu pengadukan dan waktu reaski penyabunan. Penelitian diawali dengan pembuatan alkali d...

  15. Device for removing alkali metal residues from heat exchanger

    International Nuclear Information System (INIS)

    Matal, O.

    1987-01-01

    The main parts of the facility consists of a condensing vessel and a vacuum pump unit interconnected via a vacuum pipe. The heat exchanger is heated to a temperature at which the alkali metal residues evaporate. Metal vapors are collected in the condensing vessel where they condense. The removal of the alkali metal residues from the heat exchanger pipes allows thorough inspection of the pipe inside during scheduled nuclear power plant shutdowns. The facility can be used especially with reverse steam generators. (E.S.). 1 fig

  16. Tuning the electronic structure of graphene through alkali metal and halogen atom intercalation

    Science.gov (United States)

    Ahmad, Sohail; Miró, Pere; Audiffred, Martha; Heine, Thomas

    2018-04-01

    The deposition, intercalation and co-intercalation of heavy alkali metals and light halogens atoms in graphene mono- and bilayers have been studied using first principles density-functional calculations. Both the deposition and the intercalation of alkali metals gives rise to n-type doping due to the formation of M+-C- pairs. The co-intercalation of a 1:1 ratio of alkali metals and halogens derives into the formation of ionic pairs among the intercalated species, unaltering the electronic structure of the layered material.

  17. Alkali emissions of the PCFB-process

    International Nuclear Information System (INIS)

    Kuivalainen, R.; Eriksson, T.; Koskinen, J.; Lehtonen, P.

    1995-01-01

    Pressurized Circulating Fluidized Bed (PCFB) combustion technology has been developed by A. Ahlstrom Corporation since 1986. As a part of the development, a 10 MW PCFB Test Facility was constructed at Hans Ahlstrom Laboratory in Karhula, Finland in 1989. The Test Facility has been used for performance testing with different coal types through the years 1990-1994 in order to gain data for design and commercialization of the high-efficiency low- emission PCFB combustion technology. The project Y33 'Alkali emissions of the PCFB-process' was part of national LIEKKI 2 research program. The object of the project was to measure vapor phase Na and K concentrations in the PCFB flue gas after hot gas filter and investigate the effects of process conditions and sorbents on alkali release. The measured Na concentrations were between 0,03 and 0,21 ppm(w). The results of K were between 0,01 and 0,08 ppm(w). The accuracy of the results is about +-50 percent at this concentration range. The scatter of the data covers the effects of different process variables on the alkali emission . The measured emissions at 800-850 deg C are at the same order of magnitude as the guideline emission limits given by gas turbine manufacturers for flue gas at 1000-1200 deg C. The measurements and development of the analyses methods are planned to be continued during PcFB test runs in autumn 1995 in cooperation with laboratories of VTT Energy and Tampere University of Technology. (author)

  18. Conductivity in alkali doped CoO-B2O3 glasses

    International Nuclear Information System (INIS)

    Nagaraja, N; Sankarappa, T; Santoshkumar; Sadashivaiah, P J; Yenkayya

    2009-01-01

    Two series of cobalt-borate glasses doped with Li 2 O and K 2 O in single and mixed proportions have been synthesized by melt quenching method and investigated for ac conductivity in the frequency range of 50Hz to 5MHz and temperature range of 310K to 610K. From the measured total conductivity, the pure ac component and its frequency exponent, s were determined. In the single alkali doped glasses, for all the frequencies, the conductivity increased with increase of Li 2 O up to 0.4 mole fractions and decreased for further increase of Li 2 O. The temperature dependence of conductivity has been analyzed using Mott's small polaron hopping model and activation energy for ac conduction has been determined. Based on conductivity and activation behaviors, in single alkali glasses, a change over of conduction mechanism predominantly from ionic to electronic has been predicted. In mixed alkali doped glasses, the conductivity passed through minimum and activation energy passed through maximum for second alkali (K 2 O) content of 0.2 mole fractions. This result revealed the mixed alkali effect to be occurring at 0.2 mole fractions of K 2 O. The frequency exponent, s, was compared with theoretical models such as Quantum Mechanical Tunneling and Correlated Barrier Hopping models and found them to be inadequate to explain the experimental observations. Time-temperature superposition principle has been verified in both the sets of glasses.

  19. Promotion Effect of Alkali Metal Hydroxides on Polymer-Stabilized Pd Nanoparticles for Selective Hydrogenation of C–C Triple Bonds in Alkynols

    OpenAIRE

    Nikoshvili, Linda Zh.; Bykov, Alexey V.; Khudyakova, Tatiana E.; Lagrange, Thomas; Héroguel, Florent; Luterbacher, Jeremy S.; Matveeva, Valentina G.; Sulman, Esther M.; Dyson, Paul J.; Kiwi-Minsker, Lioubov

    2017-01-01

    Postimpregnation of Pd nanoparticles (NPs) stabilized within hyper-cross-linked polystyrene with sodium or potassium hydroxides of optimal concentration was found to significantly increase the catalytic activity for the partial hydrogenation of the C–C triple bond in 2-methyl-3-butyn-2-ol at ambient hydrogen pressure. The alkali metal hydroxide accelerates the transformation of the residual Pd(II) salt into Pd(0) NPs and diminishes the reaction induction period. In addition, the selectivity t...

  20. Alkali Metal Coolants. Proceedings of the Symposium on Alkali Metal Coolants - Corrosion Studies and System Operating Experience

    Energy Technology Data Exchange (ETDEWEB)

    NONE

    1967-06-15

    Proceedings of a Symposium organized by the IAEA and held in Vienna, 28 November - 2 December 1966. The meeting was attended by 107 participants from 16 countries and two international organizations. Contents: Review papers (2 papers); Corrosion of steels and metal alloys (6 papers); Mass transfer in alkali metal systems, behaviour of carbon (5 papers); Effects of sodium environment on mechanical properties of materials (3 papers); Effect of water leakage into sodium systems (2 papers); Design-and operation of testing apparatus (6 papers); Control, measurements and removal of impurities (13 papers); Corrosion by other alkali metals: NaK, K, Li, Cs (6 papers); Behaviour of fission products (3 papers). Each paper is in its original language (32 English, 6 French and 8 Russian) and is preceded by an abstract in English and one in the original language if this is not English. Discussions are in English. (author)

  1. Alkali Metal Coolants. Proceedings of the Symposium on Alkali Metal Coolants - Corrosion Studies and System Operating Experience

    International Nuclear Information System (INIS)

    1967-01-01

    Proceedings of a Symposium organized by the IAEA and held in Vienna, 28 November - 2 December 1966. The meeting was attended by 107 participants from 16 countries and two international organizations. Contents: Review papers (2 papers); Corrosion of steels and metal alloys (6 papers); Mass transfer in alkali metal systems, behaviour of carbon (5 papers); Effects of sodium environment on mechanical properties of materials (3 papers); Effect of water leakage into sodium systems (2 papers); Design-and operation of testing apparatus (6 papers); Control, measurements and removal of impurities (13 papers); Corrosion by other alkali metals: NaK, K, Li, Cs (6 papers); Behaviour of fission products (3 papers). Each paper is in its original language (32 English, 6 French and 8 Russian) and is preceded by an abstract in English and one in the original language if this is not English. Discussions are in English. (author)

  2. Recent materials compatibility studies in refractory metal-alkali metal systems for space power applications.

    Science.gov (United States)

    Harrison, R. W.; Hoffman, E. E.; Davies, R. L.

    1972-01-01

    Advanced Rankine and other proposed space power systems utilize refractory metals in contact with both single-phase and two-phase alkali metals at elevated temperatures. A number of recent compatibility experiments are described which emphasize the excellent compatibility of refractory metals with the alkali metals, lithium, sodium, and potassium, under a variety of environmental conditions. The alkali metal compatibilities of tantalum-, columbium-, molybdenum-, and tungsten-base alloys are discussed.

  3. Assessment of concrete bridge decks with alkali silica reactions

    DEFF Research Database (Denmark)

    Eriksen, Kirsten; Jansson, Jacob; Geiker, Mette Rica

    2008-01-01

    Based on investigations of concrete from an approximately 40 years old bridge a procedure to support the management of maintenance and repair of alkali silica damaged bridges is proposed. Combined petrography and accelerated expansion testing were undertaken on cores from the Bridge at Skovdiget......, Bagsværd, Denmark to provide information on the damage condition as well as the residual reactivity of the concrete. The Danish Road Directory’s guidelines for inspection and assessment of alkali silica damaged bridges will be briefly presented, and proposed modifications will be describe...

  4. Exploration of the catalytic use of alkali metal bases

    OpenAIRE

    Bao, Wei

    2017-01-01

    This PhD thesis project was concerned with the use of alkali metal amide Brønsted bases and alkali metal alkoxide Lewis bases in (asymmetric) catalysis. The first chapter deals with formal allylic C(sp3)–H bond activation of aromatic and functionalized alkenes for subsequent C–C and C–H bond formations. The second chapter is focused on C(sp3)–Si bond activation of fluorinated pro-nucleophiles in view of C–C bond formations. In the first chapter, a screening of various metal amides...

  5. Structural Diversity in Alkali Metal and Alkali Metal Magnesiate Chemistry of the Bulky 2,6-Diisopropyl-N-(trimethylsilyl)anilino Ligand.

    Science.gov (United States)

    Fuentes, M Ángeles; Zabala, Andoni; Kennedy, Alan R; Mulvey, Robert E

    2016-10-10

    Bulky amido ligands are precious in s-block chemistry, since they can implant complementary strong basic and weak nucleophilic properties within compounds. Recent work has shown the pivotal importance of the base structure with enhancement of basicity and extraordinary regioselectivities possible for cyclic alkali metal magnesiates containing mixed n-butyl/amido ligand sets. This work advances alkali metal and alkali metal magnesiate chemistry of the bulky arylsilyl amido ligand [N(SiMe 3 )(Dipp)] - (Dipp=2,6-iPr 2 -C 6 H 3 ). Infinite chain structures of the parent sodium and potassium amides are disclosed, adding to the few known crystallographically characterised unsolvated s-block metal amides. Solvation by N,N,N',N'',N''-pentamethyldiethylenetriamine (PMDETA) or N,N,N',N'-tetramethylethylenediamine (TMEDA) gives molecular variants of the lithium and sodium amides; whereas for potassium, PMDETA gives a molecular structure, TMEDA affords a novel, hemi-solvated infinite chain. Crystal structures of the first magnesiate examples of this amide in [MMg{N(SiMe 3 )(Dipp)} 2 (μ-nBu)] ∞ (M=Na or K) are also revealed, though these breakdown to their homometallic components in donor solvents as revealed through NMR and DOSY studies. © 2016 The Authors. Published by Wiley-VCH Verlag GmbH & Co. KGaA.

  6. Micelle formation during extraction of alkali elements from strongly alkaline mediums

    International Nuclear Information System (INIS)

    Apanasenko, V.V.; Reznik, A.M.; Bukin, V.I.; Brodskaya, A.V.

    1988-01-01

    Extraction of potassium, rubidium and cesium by phenol reagents in hydrocarbon solvents from strongly alkakine solutions was considered. Tendency of prepared alkali metal phenolates to form micelles in aqueous and organic phases was revealed. Phenolates tendency to form micelles is dictated mainly by the size and position of hydrocarbon substituent in molecule. It is shown that when micelles form in organic phase, alkali elements can be extracted both according to cation-exchange mechanism and according to micellar one. It is noted that alkai element extraction from strongly alkaline media requires the correct choice of extractant: alkali metal phenolate shouldn't form micelles in aqueous solution. n-Alkyl- and arylphenoldisulfides and polysulfides are most preferable for solvent extraction among considered phenol derivatives

  7. Highly reproducible alkali metal doping system for organic crystals through enhanced diffusion of alkali metal by secondary thermal activation.

    Science.gov (United States)

    Lee, Jinho; Park, Chibeom; Song, Intek; Koo, Jin Young; Yoon, Taekyung; Kim, Jun Sung; Choi, Hee Cheul

    2018-05-16

    In this paper, we report an efficient alkali metal doping system for organic single crystals. Our system employs an enhanced diffusion method for the introduction of alkali metal into organic single crystals by controlling the sample temperature to induce secondary thermal activation. Using this system, we achieved intercalation of potassium into picene single crystals with closed packed crystal structures. Using optical microscopy and Raman spectroscopy, we confirmed that the resulting samples were uniformly doped and became K 2 picene single crystal, while only parts of the crystal are doped and transformed into K 2 picene without secondary thermal activation. Moreover, using a customized electrical measurement system, the insulator-to-semiconductor transition of picene single crystals upon doping was confirmed by in situ electrical conductivity and ex situ temperature-dependent resistivity measurements. X-ray diffraction studies showed that potassium atoms were intercalated between molecular layers of picene, and doped samples did not show any KH- nor KOH-related peaks, indicating that picene molecules are retained without structural decomposition. During recent decades, tremendous efforts have been exerted to develop high-performance organic semiconductors and superconductors, whereas as little attention has been devoted to doped organic crystals. Our method will enable efficient alkali metal doping of organic crystals and will be a resource for future systematic studies on the electrical property changes of these organic crystals upon doping.

  8. Alkali-bonded ceramics with hierarchical tailored porosity

    Czech Academy of Sciences Publication Activity Database

    Landi, E.; Medri, V.; Papa, E.; Dědeček, Jiří; Klein, Petr; Benito, P.; Vaccari, A.

    2013-01-01

    Roč. 73, SI (2013), s. 56-64 ISSN 0169-1317 Institutional support: RVO:61388955 Keywords : alkali-bonded ceramics * metalcaolin * geopolymerization parameters Subject RIV: CF - Physical ; Theoretical Chemistry Impact factor: 2.703, year: 2013

  9. DFT study of the interaction between DOTA chelator and competitive alkali metal ions.

    Science.gov (United States)

    Frimpong, E; Skelton, A A; Honarparvar, B

    2017-09-01

    1, 4, 7, 10-tetraazacyclododecane-1, 4, 7, 10-tetracetic acid (DOTA) is an important chelator for radiolabeling of pharmaceuticals. The ability of alkali metals found in the body to complex with DOTA and compete with radio metal ions can alter the radiolabeling process. Non-covalent interactions between DOTA complexed with alkali metals Li + , Na + , K + and Rb + , are investigated with density functional theory using B3LYP and ωB97XD functionals. Conformational possibilities of DOTA were explored with a varying number of carboxylic pendant arms of DOTA in close proximity to the ions. It is found that the case in which four arms of DOTA are interacting with ions is more stable than other conformations. The objective of this study is to explore the electronic structure properties upon complexation of alkali metals Li + Na + , K + and Rb + with a DOTA chelator. Interaction energies, relaxation energies, entropies, Gibbs free energies and enthalpies show that the stability of DOTA, complexed with alkali metals decreases down the group of the periodic table. Implicit water solvation affects the complexation of DOTA-ions leading to decreases in the stability of the complexes. NBO analysis through the natural population charges and the second order perturbation theory, revealed a charge transfer between DOTA and alkali metals. Conceptual DFT-based properties such as HOMO/LUMO energies, ΔE HOMO-LUMO and chemical hardness and softness indicated a decrease in the chemical stability of DOTA-alkali metal complexes down the alkali metal series. This study serves as a guide to researchers in the field of organometallic chelators, particularly, radiopharmaceuticals in finding the efficient optimal match between chelators and various metal ions. Copyright © 2017 Elsevier Inc. All rights reserved.

  10. Oster pluton (Central Karelia) - the ancient massif of two-feldspar granites of Baltic Shield

    International Nuclear Information System (INIS)

    Kovalenko, A.V.; Rizvanova, N.G.

    2000-01-01

    Geochronological study of two-feldspar granites forming the Oster pluton in the Central Karelia was performed using the methods of U-Pb- and Sm-Nd-dating. U-Pb isotope data for zircons from granite of the Oster pluton correspond to the age of 2876±21 mln. years, whereas Sm-Nd isotope data obtained for three samples of the garnet correspond to the age varying from 3.0 to 3.5 bln. years. The ancient age of granites of the Oster pluton is explained by the presence of a sufficiently powerful crust in the region by that moment [ru

  11. Alkali production in the mouth and its relationship with certain patient’s characteristics

    Science.gov (United States)

    GORDAN, Valeria Veiga; McEDWARD, Deborah Landry; OTTENGA, Marc Edward; GARVAN, Cynthia Wilson; HARRIS, Pearl Ann

    2014-01-01

    Objectives To assess the relationships among alkali production, diet, oral health behaviors, and oral hygiene. Methods Data from 52 subjects including demographics, diet, and oral hygiene scores were analyzed against the level of arginine and urea enzymes in plaque and saliva samples. An oral habit survey was completed that included: use of tobacco (TB), alcohol (AH), sugary drinks (SD), and diet. Alkali production through arginine deiminase (ADS) and urease activities were measured in smooth-surface supragingival dental plaque and un stimulated saliva samples from all subjects. ADS and urease activities were measured by quantification of the ammonia generated from the incubation of plaque or saliva samples. Spearman correlations were used to compute all associations. Results Participants in the lowest SES (Socio-economic status) group had the habit of consuming sugary drinks the most and had the highest rate of tobacco use. Males consumed significantly more alcohol than females. No significant relationship was found between age or gender and alkali production. Higher rates of sugary drink consumption and tobacco use were significantly related to lower alkali production. Conclusion The study showed a relationship between alkali production and oral hygiene, diet, and certain oral health behaviors. Poor oral hygiene was significantly associated with age, lower SES, tobacco use, and alcohol, and sugary drinks consumption. Clinical relevance Certain oral health behaviors have an impact on oral hygiene and on alkali production; it is important to address these factors with patients as a strategy for caries control. PMID:25591024

  12. Behaviour of zirconium oxidation and is oxide films in alkali halide solutions as studied by electrochemical techniques

    International Nuclear Information System (INIS)

    Saleh, H.E.M.

    1996-01-01

    Study of the properties of Zr electrode and the oxide films that cover the metal surface is of extreme importance due to their wide applications in chemical and nuclear industry. In this thesis the electrochemical behaviour of Zr electrode in alkali halide solutions and with various surface conditions was studied, Also the galvanostatic oxidation of the metal in addition to the open circuit and impedance measurements were employed. Chapter I is a literature survey of the electrochemistry of Zr metal with particular emphasis on the stability and growth process of Zr in different media. Chapter II contains the experimental part, including details of the electrochemical techniques used in the measurements. The electrode impedance was always balanced as a series capacitance Cs and resistance Rs.Chapter III includes the experimental results and discussion. It is divide into sections, A and B. Section A includes the results of some experimental parameters which affect the reactivity of the oxide growth process on the zirconium surface, such as surface pre - treatment, electrolyte composition, the effect of different alkali halide anions, as well as the triiodide ion. 9 tabs.,26 figs.,67 refs

  13. A light water excess heat reaction suggests that cold fusion may be alkali-hydrogen fusion

    International Nuclear Information System (INIS)

    Bush, R.T.

    1992-01-01

    This paper reports that Mills and Kneizys presented data in support of a light water excess heat reaction obtained with an electrolytic cell highly reminiscent of the Fleischmann-Pons cold fusion cell. The claim of Mills and Kneizys that their excess heat reaction can be explained on the basis of a novel chemistry, which supposedly also explains cold fusion, is rejected in favor of their reaction being, instead, a light water cold fusion reaction. It is the first known light water cold fusion reaction to exhibit excess heat, it may serve as a prototype to expand our understanding of cold fusion. From this new reactions are deduced, including those common to past cold fusion studies. This broader pattern of nuclear reactions is typically seen to involve a fusion of the nuclides of the alkali atoms with the simplest of the alkali-type nuclides, namely, protons, deuterons, and tritons. Thus, the term alkali-hydrogen fusion seems appropriate for this new type of reaction with three subclasses: alkali-hydrogen fusion, alkali-deuterium fusion, and alkali-tritium fusion. A new three-dimensional transmission resonance model (TRM) is sketched. Finally, preliminary experimental evidence in support of the hypothesis of a light water nuclear reaction and alkali-hydrogen fusion is reported. Evidence is presented that appears to strongly implicate the transmission resonance phenomenon of the new TRM

  14. Effects of alkali on protein polymerization and textural characteristics of textured wheat protein.

    Science.gov (United States)

    Li, Ting; Guo, Xiao-Na; Zhu, Ke-Xue; Zhou, Hui-Ming

    2018-01-15

    The impact of alkali addition on the degree of gluten polymerization and textural characteristics of textured wheat protein was investigated. Results showed that the extrusion process increased the average molecular weight of gluten as evidenced by SDS-PAGE and SDS extractable protein. The addition of alkali not only promoted the degree of gluten polymerization, but also induced dehydroalanine-derived cross-linking. Alkali addition decreased the content of cystine and increased the contents of dehydroalanine and lanthionine. The obvious decrease of free SH showed that dehydroalanine-derived cross-linking was quantitatively less crucial than disulfide cross-linking. Furthermore, the protein cross-linking induced by alkali improved the texture properties of gluten extrudates. SEM analysis showed extrusion under alkaline condition conferred a more fibrous microstructure as a consequence of a compact gluten network. Copyright © 2017 Elsevier Ltd. All rights reserved.

  15. Pengaruh Perlakukan Alkali terhadap Sifat Fisik, dan Mekanik Serat Kulit Buah Pinang

    Directory of Open Access Journals (Sweden)

    Cokorda Putri Kusuma Kencanawati

    2018-04-01

    Full Text Available Makalah ini menganalisis pengaruh perlakukan alkali dan tanpa perlakukan alkali terhadap karakateristik fisik, morfologi dan sifat mekanik serat kulit buah pinang (areca Catechu L.. Selama ini pemanfaatan limbah pertanian belum dilakukan secara maksimal, sehingga dapat menimbulkan pencemaran terhadap lingkungan. Serat kulit buah pinang (Areca Husk Fiber/AHF selama ini hanya dipergunakan sebagai bahan bakar biomassa dan media tanam sedangkan untuk pemanfaatan lain belum ada sama sekali. AHF diberi perlakukan NaOH 2,5%, 5%, 7,5% dan 10% dengan waktu perendaman 2 jam pada temperatur kamar, untuk mengetahui karakteristik fisik AHF maka dilakukan pengukuran panjang dan diameter serat, pengujian densitas, pengujian kadar air dan moisture sedangkan untuk mengetahui karakteristik mekanik dilakukan pengujian tarik serat tunggal sesuai dengan ASTM D 3379. Dari penelitian ini diketahui bahwa diameter AHF mengalami pengurangan diameter akibat perlakukan alkali, hal ini terkait dengan hilangnya kandungan lignin, pektin dan wax. Densitas AHF menurun dengan meningkatan prosentase NaOH bila dibandingkan dengan AHF tanpa perlakukan NaOH. Kekuatan tarik bervariasi dengan adanya perlakuan alkali.  Kekuatan tarik AHF tertinggi pada serat yang mengalami perlakukan NaOH 5% yaitu sebesar 165 Mpa dan kekuatan tarik terendah pada AHF dengan perlakuan Alkali 10% yaitu sebesar 137 MPa . This paper analyzes the effect of alkali and non-alkali treatments on the physical characteristics, morphology and mechanical properties of betel nut huks fiber (areca Catechu L.. the used of agricultural waste has not been done optimally, causing environmental pollution. Areca Husk Fiber (AHF only used as biomass fuel and planting medium, while for the other uses it has not existed. AHF was given 2.5%, 5%, 7.5% and 10% NaOH treatment with 2 hours immersion at room temperature, to known the physical characteristics of AHF then measured the length and diameter of fiber, density test, water

  16. Temperature dependent mobility measurements of alkali earth ions in superfluid helium

    Science.gov (United States)

    Putlitz, Gisbert Zu; Baumann, I.; Foerste, M.; Jungmann, K.; Riediger, O.; Tabbert, B.; Wiebe, J.; Zühlke, C.

    1998-05-01

    Mobility measurements of impurity ions in superfluid helium are reported. Alkali earth ions were produced with a laser sputtering technique and were drawn inside the liquid by an electric field. The experiments were carried out in the temperature region from 1.27 up to 1.66 K. The temperature dependence of the mobility of Be^+-ions (measured here for the first time) differs from that of the other alkali earth ions Mg^+, Ca^+, Sr^+ and Ba^+, but behaves similar to that of He^+ (M. Foerste, H. Günther, O. Riediger, J. Wiebe, G. zu Putlitz, Z. Phys. B) 104, 317 (1997). Theories of Atkins (A. Atkins, Phys. Rev.) 116, 1339 (1959) and Cole (M.W. Cole, R.A. Bachmann Phys. Rev. B) 15, 1388 (1977) predict a different defect structure for He^+ and the alkali earth ions: the helium ion is assumed to form a snowball like structure whereas for the alkali earth ions a bubble structure is assumed. If the temperature dependence is a characteristic feature for the different structures, then it seems likely that the Be^+ ion builds a snowball like structure.

  17. Multi-quantum excitation in optically pumped alkali atom: rare gas mixtures

    Science.gov (United States)

    Galbally-Kinney, K. L.; Rawlins, W. T.; Davis, S. J.

    2014-03-01

    Diode-pumped alkali laser (DPAL) technology offers a means of achieving high-energy gas laser output through optical pumping of the D-lines of Cs, Rb, and K. The exciplex effect, based on weak attractive forces between alkali atoms and polarizable rare gas atoms (Ar, Kr, Xe), provides an alternative approach via broadband excitation of exciplex precursors (XPAL). In XPAL configurations, we have observed multi-quantum excitation within the alkali manifolds which result in infrared emission lines between 1 and 4 μm. The observed excited states include the 42FJ states of both Cs and Rb, which are well above the two-photon energy of the excitation laser in each case. We have observed fluorescence from multi-quantum states for excitation wavelengths throughout the exciplex absorption bands of Cs-Ar, Cs-Kr, and Cs-Xe. The intensity scaling is roughly first-order or less in both pump power and alkali concentration, suggesting a collisional energy pooling excitation mechanism. Collisional up-pumping appears to present a parasitic loss term for optically pumped atomic systems at high intensities, however there may also be excitation of other lasing transitions at infrared wavelengths.

  18. Properties of Hooked Steel Fibers Reinforced Alkali Activated Material Concrete

    Directory of Open Access Journals (Sweden)

    Faris M. A.

    2016-01-01

    Full Text Available In this study, alkali activated material was produced by using Class F fly ash from Manjung power station, Lumut, Perak, Malaysia. Fly ash then was activated by alkaline activator which is consisting of sodium silicate (Na2SiO3 and sodium hydroxide (NaOH. Hooked end steel fibers were added into the alkali activated material system with percentage vary from 0 % – 5 %. Chemical compositions of fly ash were first analyzed by using x-ray fluorescence (XRF. All hardened alkali activated material samples were tested for density, workability, and compression after 28 days. Results show a slight increase of density with the addition of steel fibers. However, the workability was reduced with the addition of steel fibers content. Meanwhile, the addition of steel fibers shows the improvement of compressive strength which is about 19 % obtained at 3 % of steel fibers addition.

  19. Corrosion resistance of metals and alloys in molten alkalies

    International Nuclear Information System (INIS)

    Zarubitskij, O.G.; Dmitruk, B.F.; Minets, L.A.

    1979-01-01

    Literature data on the corrosion of non-ferrous and noble metals, iron and steels in the molten alkalis and mixtures of their base are presented. It is shown that zirconium, niobium and tantalum are characterized by high corrosion stability in the molten NaOH. Additions of NaOH and KOH to the alkali chloride melts result in a 1000 time decrease of zirconium corrosion rate at 850 deg. The data testify to the characteristic passivating properties of OH - ions; Mo and W do not possess an ability to selfpassivation in hydroxide melts. Corrosion resistance of carbon and chromium-nickel steels in hydroxide melts depends considerably on the temperature, electrolyte composition and atmosphere over them. At the temperatures up to 600 deg C chromium-nickel steel is corrosion resistant in the molten alkali only in the inert atmosphere. Corrosion rate of chromium-nickel alloy is the lower the less chromium and the more nickel it contains. For the small installations the 4Kh18N25S2 and Kh23N28M3D3T steels can be recommended

  20. Optical dating using feldspar from Quaternary alluvial and colluvial sediments from SE Brazilian Plateau, Brazil

    International Nuclear Information System (INIS)

    Tatumi, Sonia H.; Peixoto, Maria Naise O.; Moura, Josilda R.S.; Mello, Claudio L.; Carmo, Isabela O.; Kowata, Emilia A.; Yee, Marcio; Brito, Silvio Luiz M.; Gozzi, Giuiliano; Kassab, Luciana R.P.

    2003-01-01

    Opticallly stimulated luminescence (OSL) dating has been applied to a wide variety of materials such as loess, sand dunes, colluvium, alluvium, volcanic products, etc., helping geologic geomorphologic studies. OSL dating results using feldspar crystals extracted from alluvial and colluvial deposits of SE Brazilian Plateau will be presented in this work. The methodology used is based on the regeneration method, with multiple aliquot protocol. A total of 23 sample ages were obtained spanning 6.5-97.2 kyr. Results of radioactive contents and comparison with radiocarbon ages will be discussed

  1. Effect of Rice Straw Extract and Alkali Lignin on the Corrosion Inhibition of Carbon Steel

    International Nuclear Information System (INIS)

    Rabiahtul Zulkafli; Norinsan Kamil Othman; Irman Abdul Rahman; Azman Jalar

    2014-01-01

    A paddy residue based corrosion inhibitor was prepared by treating finely powdered rice straw with aqueous ethanol under acid catalyst (0.01 M H 2 SO 4 ). Commercial alkali lignin was obtained from Sigma-Aldrich. Prior to the corrosion test, the extraction yield and alkali lignin was characterized via FTIR to determine the functional group. The effect of paddy residue extract and commercial alkali lignin on the corrosion inhibition of carbon steel in 1 M HCl was investigated through the weight loss method, potentiodynamic polarization technique and scanning electron microscopy (SEM). The corrosion inhibition efficiency of the extract and alkali lignin at different immersion times (3 h, 24 h and 42 h) was evaluated. The results show that the paddy waste extract exhibited lesser weight loss of carbon steel in the acidic medium in comparison to the commercial alkali lignin, suggesting that the paddy residue extract is more effective than the commercial alkali lignin in terms of its corrosion inhibition properties. The results obtained proves that the extract from paddy residue could serve as an effective inhibitor for carbon steel in acidic mediums. (author)

  2. Plasma assisted measurements of alkali metal concentrations in pressurised combustion processes

    Energy Technology Data Exchange (ETDEWEB)

    Hernberg, R; Haeyrinen, V [Tampere Univ. of Technology (Finland)

    1997-10-01

    In this project the continuous alkali measurement method plasma excited alkali resonance line spectroscopy (PEARLS) was developed, tested and demonstrated in pressurised combustion facilities. The PEARLS method has been developed at Tampere University of Technology (TUT). During 1994-1996 the PEARLS method was developed from the laboratory level to an industrial prototype. The alkali measuring instrument has been tested and used for regular measurements in four different pressurised combustion installations ranging up to industrial pilot scale. The installations are: (1) a pressurised entrained flow reactor (PEFR) at VTT Energy in Jyvaeskylae, Finland (2) a pressurised fluidised bed combustion facility, called FRED, at DMT in Essen, Germany. (3) a 10 MW pressurised circulating fluidised bed combustion pilot plant at Foster Wheeler Energia Oy in Karhula, Finland (4) PFBC Research Facility at ABB Carbon in Finspaang, Sweden

  3. Heidelberg polarized alkali source

    International Nuclear Information System (INIS)

    Kraemer, D.; Steffens, E.; Jaensch, H.; Philipps Universitaet, Marburg, Germany)

    1984-01-01

    A new atomic beam type polarized alkali ion source has been installed at Heidelberg. In order to improve the beam polarization considerably optical pumping is applied in combination with an adiabatic medium field transition which results in beams in single hyperfine sublevels. The m state population is determined by laser-induced fluorescence spectroscopy. Highly polarized beams (P/sub s/ > 0.9, s = z, zz) with intensities of 30 to 130 μA can be extracted for Li + and Na + , respectively

  4. Spin-rotation interaction of alkali-metal endash He-atom pairs

    International Nuclear Information System (INIS)

    Walker, T.G.; Thywissen, J.H.; Happer, W.

    1997-01-01

    A treatment of the spin-rotation coupling between alkali-metal atoms and He atoms is presented. Rotational distortions are accounted for in the wave function using a Coriolis interaction in the rotating frame. The expectation value of the spin-orbit interaction gives values of the spin-rotation coupling that explain previous experimental results. For spin-exchange optical pumping, the results suggest that lighter alkali-metal atoms would be preferred spin-exchange partners, other factors being equal. copyright 1997 The American Physical Society

  5. Direct observation of the release of alkali vapor species in biofuel combustion and gasification

    Energy Technology Data Exchange (ETDEWEB)

    French, R.J.; Milne, T.A. [National Renewable Energy Lab., Golden, CO (United States)

    1993-12-31

    The largest present use of biomass for energy is in combustion for steam and electrical power. Biofuels have an acknowledged advantage over coal as a solid fuel because of their low sulfur and ash content. However, some forms of biomass have substantial quantities of alkali metals and chlorine. In addition, evidence indicates that the alkali in biomass is largely atomically dispersed, resulting in its facile mobilization into the gas-phase. Gaseous alkali compounds aggravate problems of slagging, fouling, and corrosion on heat transfer surfaces in present-day boilers. These problems can be particularly severe when mixed and variable agricultural residues are burned. Furthermore, the next generation of biomass-to-power systems will likely involve combined cycle gas turbines, where alkali tolerances are especially restrictive. In this paper, we report on laboratory studies in which biofuels are combusted under simulated turbine or boiler-firing conditions. Gaseous alkali, sulfur, nitrogen, and halogen-containing species are measured by direct extraction from the hot gases through molecular-beam mass spectrometry (MBMS). The experimental apparatus will be described and its capability illustrated with results of time-resolved evolution of species like K, KCl, KOH, SO{sub 2} and NO{sub x} from small samples of biomass in combustion environments. The nature and release of such species will be explicated by referring to thermodynamic equilibrium predictions and the form of alkali in solid, gaseous, and liquid biofuels.

  6. Hydrothermal calcification of alkali treated titanium in CaHPO{sub 4} solution

    Energy Technology Data Exchange (ETDEWEB)

    Fu, T., E-mail: taofu@xjtu.edu.cn [Key Laboratory of Biomedical Information Engineering of Ministry of Education, School of Life Science and Technology, Xi’an Jiaotong University, Shaanxi, 710049 (China); Fan, J.T., E-mail: jitang_fan@hotmail.com [State Key Laboratory of Explosion Science and Technology, Beijing Institute of Technology, Beijing, 100081 (China); Shen, Y.G. [Department of Mechanical and Biomedical Engineering, City University of Hong Kong, Kowloon, Hong Kong (China); Sun, J.M. [Key Laboratory of Biomedical Information Engineering of Ministry of Education, School of Life Science and Technology, Xi’an Jiaotong University, Shaanxi, 710049 (China)

    2017-03-01

    The alkali treated titanium was hydrothermally treated in water and 10 mM CaHPO{sub 4} solution (nominal concentration) at 80–180 °C to crystallize the titanate hydrogel layer and calcify the alkali treated titanium. Surface structure and elemental composition of the samples were analyzed by scanning electron microscopy, energy dispersive x-ray analysis, x-ray photoelectron spectroscopy, x-ray diffraction and Raman spectroscopy. Porous titanate hydrogel layer is formed on titanium after the alkali treatment. For the hydrothermal treatment in water, the hydrogel layer is crystallized as anatase TiO{sub 2} with nanoporous or nanofibrous structure at 100 and 120 °C, and the layer is converted to anatase nanoparticles at 150 and 180 °C. For the hydrothermal treatment in the CaHPO{sub 4} solution, hydroxyapatite nanocrystallites are deposited at the samples surface at 80–120 °C, but only anatase nanoparticles are formed at 150 and 180 °C. The growth of hydroxyapatite nanocrystallites is influenced by pH and temperature variations of the solution. The present alkali-hydrothermal treatment can avoid higher temperatures involved in the traditional alkali-heat treatments, which is applicable for bioactive surface modification of the thermally sensitive titanium alloys. The results also show that Raman spectroscopy is a useful technique to analyze the microstructure of TiO{sub 2} and apatite films. - Highlights: • The alkali treated titanium is hydrothermally calcified in a CaHPO{sub 4} solution. • HA nanocrystallites are formed at 80–120 °C, but TiO{sub 2} nanoparticles at 150–180 °C. • The growth mechanism of HA nanocrystallites is discussed. • This low-temperature method is fit for some special titanium alloys.

  7. Alternative alkali resistant deNO{sub x} technologies

    Energy Technology Data Exchange (ETDEWEB)

    Buus Kristensen, S.; Due-Hansen, J.; Putluru, S.S.R.; Kunov-Kruse, A.; Fehrmann, R.; Degn Jensen, A.

    2011-04-15

    The aim of the project is to identify, make and test possible alkali resistant deNO{sub x} catalysts for use in biomass, waste or fossil fuelled power plants, where the flue gas typically has a high level of potassium compounds, which rapidly de-activate the traditional V{sub 2}O{sub 5}/TiO{sub 2} catalyst. Furthermore, new technologies are investigated based on a protective coating of the catalyst elements and selective reversible absorption of NO{sub x} with ionic liquids. Several promising alternative deNO{sub x} catalyst types have been made during the project: 1) V, Fe, CU based nano-TiO{sub 2} and nano-TiO{sub 2}-SO{sub 4}{sup 2-} catalysts; 2) V/ZrO{sub 2}-SO{sub 2}- and V/ZrO{sub 2}-CeO{sub 2} catalysts; V, Fe, Cu based Zeolite catalysts; 4) V, Fe, Cu based Heteropoly acid catalysts. Several of these are promising alternatives to the state-of the art industrial reference catalyst. All catalysts prepared in the present project exhibit higher to much higher alkali resistance compared to the commercial reference. Furthermore, two catalysts, i.e. 20 wt% V{sub 2}O-3-TiO{sub 2} nano-catalyst and the 4 wt% CuO-Mordenite zeolite based catalyst have also a higher initial SCR activity compared to the commercial one before alkali poisoning. Thus, those two catalysts might be attractive for SCR deNO{sub x} purposes even under ''normal'' fuel conditions in power plants and elsewhere making them strong candidates for further development. These efforts regarding all the promising catalysts will be pursued after this project has expired through a one year Proof of Concept project granted by the Danish Agency for Science, Technology and Innovation. Also the severe rate of deactivation due to alkali poisons can be avoided by coating the vanadium catalyst with Mg. Overall, the protective coating of SCR catalysts developed in the project seems promising and a patent application has been filed for this technology. Finally, a completely different approach to

  8. Interactions of Various types between Rock and Alkali-Activated Blast Furnace Slag

    Directory of Open Access Journals (Sweden)

    Mec Pavel

    2017-03-01

    Full Text Available Alkali-activated binders (AAB are very intensively studied materials nowadays. Because of possible usage as secondary raw materials, they can be environmentally efficient. Intensive research is focused especially on binder matrix, composition and its structure. For industrial usage, it is necessary to work with some aggregate for the preparation of mortars and concretes. Due to different structures of alkali-activated binders, the interaction with the aggregate will be different in comparison to an ordinary Portland cement binder. This paper deals with the study of interactions between several types of rocks used as aggregate and alkali-activated blast furnace slag. The research was focused especially on mechanical properties of prepared mortars.

  9. Understanding the ice nucleation characteristics of feldspars suspended in solution

    Science.gov (United States)

    Kumar, Anand; Marcolli, Claudia; Kaufmann, Lukas; Krieger, Ulrich; Peter, Thomas

    2017-04-01

    Chemical) and 5 wt% lanolin (Fluka Chemical) is emulsified with a rotor-stator homogenizer for 40 s at a rotation frequency of 7000 rpm. 4 - 10 mg of this mixture is pipetted in an aluminum pan (closed hermetically), placed in the DSC and subjected to three freezing cycles. The first and the third freezing cycles are executed at a cooling rate of 10 K/min to control the stability of the sample. The second freezing cycle is executed at a 1 K/min cooling rate and is used for evaluation. Freezing temperatures are obtained by evaluating the onset of the freezing signal in the DSC curve and plotted against water activity. Results Based on Koop et al. (2000), a general decreasing trend in ice nucleation efficiency of the mineral samples with increasing solute concentrations is expected. Interestingly, feldspars (microcline, sanidine, plagioclase) in very dilute solutions of ammonia and ammonium salts (water activity close to one) show an increase in ice nucleation efficiency of 4 to 6 K compared to that in pure water. Similar trends but less pronounced are observed for kaolinite while quartz shows barely any effect. Therefore, there seem to be specific interactions between the feldspar surface and ammonia and/or ammonium ions which result in an increase in freezing temperatures at low solute concentrations. The surface ion exchange seems to be secondary for this effect since it is also present in ammonia solution. We hypothesize that ammonia adsorbs on the aluminol/silanol groups present on feldspar (viz. aluminosilicate surface) surfaces (Nash and Marshall, 1957; Belchinskaya et al., 2013). Hence allowing one of the N-H bonds to stick outwards from the surface, facing towards the bulk water and providing a favorable template for ice to grow. The current study gives an insight into the ice nucleation behavior of aluminosilicate minerals when present in conjunction with chemical species, eg. ammonium/sulfates, which is of high atmospheric relevance. References Koop et al., (2000

  10. Modifier constraint in alkali borophosphate glasses using topological constraint theory

    Energy Technology Data Exchange (ETDEWEB)

    Li, Xiang [Key Laboratory for Ultrafine Materials of Ministry of Education, School of Materials Science and Engineering, East China University of Science and Technology, Shanghai 200237 (China); Zeng, Huidan, E-mail: hdzeng@ecust.edu.cn [Key Laboratory for Ultrafine Materials of Ministry of Education, School of Materials Science and Engineering, East China University of Science and Technology, Shanghai 200237 (China); Jiang, Qi [Key Laboratory for Ultrafine Materials of Ministry of Education, School of Materials Science and Engineering, East China University of Science and Technology, Shanghai 200237 (China); Zhao, Donghui [Unifrax Corporation, Niagara Falls, NY 14305 (United States); Chen, Guorong [Key Laboratory for Ultrafine Materials of Ministry of Education, School of Materials Science and Engineering, East China University of Science and Technology, Shanghai 200237 (China); Wang, Zhaofeng; Sun, Luyi [Department of Chemical & Biomolecular Engineering and Polymer Program, Institute of Materials Science, University of Connecticut, Storrs, CT 06269 (United States); Chen, Jianding [Key Laboratory for Ultrafine Materials of Ministry of Education, School of Materials Science and Engineering, East China University of Science and Technology, Shanghai 200237 (China)

    2016-12-01

    In recent years, composition-dependent properties of glasses have been successfully predicted using the topological constraint theory. The constraints of the glass network are derived from two main parts: network formers and network modifiers. The constraints of the network formers can be calculated on the basis of the topological structure of the glass. However, the latter cannot be accurately calculated in this way, because of the existing of ionic bonds. In this paper, the constraints of the modifier ions in phosphate glasses were thoroughly investigated using the topological constraint theory. The results show that the constraints of the modifier ions are gradually increased with the addition of alkali oxides. Furthermore, an improved topological constraint theory for borophosphate glasses is proposed by taking the composition-dependent constraints of the network modifiers into consideration. The proposed theory is subsequently evaluated by analyzing the composition dependence of the glass transition temperature in alkali borophosphate glasses. This method is supposed to be extended to other similar glass systems containing alkali ions.

  11. Comparison of ion balance and nitrogen metabolism in old and young leaves of alkali-stressed rice plants.

    Science.gov (United States)

    Wang, Huan; Wu, Zhihai; Han, Jiayu; Zheng, Wei; Yang, Chunwu

    2012-01-01

    Alkali stress is an important agricultural contaminant and has complex effects on plant metabolism. The aim of this study was to investigate whether the alkali stress has different effects on the growth, ion balance, and nitrogen metabolism in old and young leaves of rice plants, and to compare functions of both organs in alkali tolerance. The results showed that alkali stress only produced a small effect on the growth of young leaves, whereas strongly damaged old leaves. Rice protected young leaves from ion harm via the large accumulation of Na(+) and Cl(-) in old leaves. The up-regulation of OsHKT1;1, OsAKT1, OsHAK1, OsHAK7, OsHAK10 and OsHAK16 may contribute to the larger accumulation of Na(+) in old leaves under alkali stress. Alkali stress mightily reduced the NO(3)(-) contents in both organs. As old leaf cells have larger vacuole, under alkali stress these scarce NO(3)(-) was principally stored in old leaves. Accordingly, the expression of OsNRT1;1 and OsNRT1;2 in old leaves was up-regulated by alkali stress, revealing that the two genes might contribute to the accumulation of NO(3)(-) in old leaves. NO(3)(-) deficiency in young leaves under alkali stress might induce the reduction in OsNR1 expression and the subsequent lacking of NH(4)(+), which might be main reason for the larger down-regulation of OsFd-GOGAT and OsGS2 in young leaves. Our results strongly indicated that, during adaptation of rice to alkali stress, young and old leaves have distinct mechanisms of ion balance and nitrogen metabolism regulation. We propose that the comparative studies of young and old tissues may be important for abiotic stress tolerance research.

  12. Structure and thermodynamic properties of molten alkali chlorides

    International Nuclear Information System (INIS)

    Ballone, P.; Pastore, G.; Tosi, M.P.; Trieste Univ.

    1984-03-01

    Self-consistent calculations of partial pair distribution functions and thermodynamic properties are presented for molten alkali chlorides in a non-polarizable-ion model. The theory starts from the hypernetted chain approximation and analyzes the role of bridge diagrams both for a two-component ionic plasma on a neutralizing background and for a binary ionic liquid of cations and anions. A simple account of excluded-volume effects suffices for a good description of the pair distribution functions in the two-component plasma, in analogy with earlier work on one-component fluids. The interplay of Coulomb attractions and repulsions in the molten salt requires, on the other hand, the inclusion of (i) excluded-volume effects for the various ion pairs as in a mixture of hard spheres with non-additive radii and (ii) medium-range Coulomb effects reflected mainly in the like-ion correlations. All these effects are included approximately in an empirical evaluation of the bridge functions, with numerical results which compare very well with computer simulation data. A detailed discussion of the results against experimental structural data is then given in the case of molten sodium chloride. (author)

  13. The African novel and the city: a reading of Zaynab Alkali's The ...

    African Journals Online (AJOL)

    This paper has explored the African novel in the light of the influence of city life to it. Zaynab Alkali's The Initiates was examined with a close look at how the city has influenced characters and happenings in the novel. The paper revealed that the city as presented by Alkali in The Initiates is corrupt and morally bankrupt.

  14. Fabrication and characterization of low temperature co-fired cordierite glass–ceramics from potassium feldspar

    International Nuclear Information System (INIS)

    Wu, Jianfang; Li, Zhen; Huang, Yanqiu; Li, Fei; Yang, Qiuran

    2014-01-01

    Highlights: • Low cost cordierite glass–ceramics were fabricated from potassium feldspar. • The glass–ceramics could be highly densified below 950 °C. • The glass–ceramics exhibit extraordinary properties. • The glass–ceramics can be used as LTCC substrates. • The excess SiO 2 improved the microstructure and properties of the glass–ceramics. -- Abstract: Cordierite glass–ceramics for low temperature co-fired ceramic (LTCC) substrates were fabricated successfully using potassium feldspar as the main raw material. The sintering and crystallization behaviors of the glass–ceramics were investigated by the differential scanning calorimetry (DSC), X-ray diffraction (XRD), and field emission scanning electron microscope (FESEM). The results indicated that the glass–ceramics could be highly densified at 850 °C and the cordierite was the main crystalline phase precipitated from the glasses in the temperature range between 900 and 925 °C. The study also evaluated the physical properties including dielectric properties, thermal expansion and flexural strength of the glass–ceramics. The glass–ceramics showed low dielectric constants in the range of 6–8 and low dielectric losses in the range of 0.0025–0.01. The coefficients of thermal expansion (CTEs) are between 4.32 and 5.48 × 10 −6 K −1 and flexural strength of the glass–ceramics are 90–130 MPa. All of those qualify the glass–ceramics for further research to be used as potential LTCC substrates in the multilayer electronic substrate field. Additionally, the excess SiO 2 acted as a great role in improving the sinterability of the glasses, and the microstructure and dielectric properties of the relevant glass–ceramics

  15. Microbial reverse-electrodialysis chemical-production cell for acid and alkali production

    KAUST Repository

    Zhu, Xiuping

    2013-06-01

    A new type of bioelectrochemical system, called a microbial reverse-electrodialysis chemical-production cell (MRCC), was developed to produce acid and alkali using energy derived from organic matter (acetate) and salinity gradients (NaCl solutions representative of seawater and river water). A bipolar membrane (BPM) was placed next to the anode to prevent Cl- contamination and acidification of the anolyte, and to produce protons for HCl recovery. A 5-cell paired reverse-electrodialysis (RED) stack provided the electrical energy required to overcome the BPM over-potential (0.3-0.6 V), making the overall process spontaneous. The MRCC reactor produced electricity (908 mW/m2) as well as concentrated acidic and alkaline solutions, and therefore did not require an external power supply. After a fed-batch cycle, the pHs of the chemical product solutions were 1.65 ± 0.04 and 11.98 ± 0.10, due to the production of 1.35 ± 0.13 mmol of acid, and 0.59 ± 0.14 mmol of alkali. The acid- and alkali-production efficiencies based on generated current were 58 ± 3% and 25 ± 3%. These results demonstrated proof-of-concept acid and alkali production using only renewable energy sources. © 2013 Elsevier B.V.

  16. Neutron scattering investigation of layer-bending modes in alkali-metal--graphite intercalation compounds

    International Nuclear Information System (INIS)

    Zabel, H.; Kamitakahara, W.A.; Nicklow, R.M.

    1982-01-01

    Phonon dispersion curves for low-frequency transverse modes propagating in the basal plane have been measured in the alkali-metal--graphite intercalation compounds KC 8 , CsC 8 , KC 24 , and RbC 24 by means of neutron spectroscopy. The acoustic branches show an almost quadratic dispersion relation at small q, characteristic of strongly layered materials. The optical branches of stage-1 compounds can be classified as either graphitelike branches showing dispersion, or as almost dispersionless alkali-metal-like modes. Macroscopic shear constants C 44 and layer-bending moduli have been obtained for the intercalation compounds by analyzing the data in terms of a simple semicontinuum model. In stage-2 compounds, a dramatic softening of the shear constant by about a factor of 8 compared with pure graphite has been observed. Low-temperature results on KC 24 indicate the opening of a frequency gap near the alkali-metal Brillouin-zone boundary, possibly due to the formation of the alkali-metal superstructure

  17. Removal of oxides from alkali metal melts by reductive titration to electrical resistance-change end points

    Science.gov (United States)

    Tsang, Floris Y.

    1980-01-01

    Alkali metal oxides dissolved in alkali metal melts are reduced with soluble metals which are converted to insoluble oxides. The end points of the reduction is detected as an increase in electrical resistance across an alkali metal ion-conductive membrane interposed between the oxide-containing melt and a material capable of accepting the alkali metal ions from the membrane when a difference in electrical potential, of the appropriate polarity, is established across it. The resistance increase results from blocking of the membrane face by ions of the excess reductant metal, to which the membrane is essentially non-conductive.

  18. Laser-Induced Photofragmentation Fluorescence Imaging of Alkali Compounds in Flames.

    Science.gov (United States)

    Leffler, Tomas; Brackmann, Christian; Aldén, Marcus; Li, Zhongshan

    2017-06-01

    Laser-induced photofragmentation fluorescence has been investigated for the imaging of alkali compounds in premixed laminar methane-air flames. An ArF excimer laser, providing pulses of wavelength 193 nm, was used to photodissociate KCl, KOH, and NaCl molecules in the post-flame region and fluorescence from the excited atomic alkali fragment was detected. Fluorescence emission spectra showed distinct lines of the alkali atoms allowing for efficient background filtering. Temperature data from Rayleigh scattering measurements together with simulations of potassium chemistry presented in literature allowed for conclusions on the relative contributions of potassium species KOH and KCl to the detected signal. Experimental approaches for separate measurements of these components are discussed. Signal power dependence and calculated fractions of dissociated molecules indicate the saturation of the photolysis process, independent on absorption cross-section, under the experimental conditions. Quantitative KCl concentrations up to 30 parts per million (ppm) were evaluated from the fluorescence data and showed good agreement with results from ultraviolet absorption measurements. Detection limits for KCl photofragmentation fluorescence imaging of 0.5 and 1.0 ppm were determined for averaged and single-shot data, respectively. Moreover, simultaneous imaging of KCl and NaCl was demonstrated using a stereoscope with filters. The results indicate that the photofragmentation method can be employed for detailed studies of alkali chemistry in laboratory flames for validation of chemical kinetic mechanisms crucial for efficient biomass fuel utilization.

  19. 50 years of superbases made from organolithium compounds and heavier alkali metal alkoxides

    Czech Academy of Sciences Publication Activity Database

    Lochmann, Lubomír; Janata, Miroslav

    2014-01-01

    Roč. 12, č. 5 (2014), s. 537-548 ISSN 1895-1066 R&D Projects: GA ČR GAP106/12/0844 Institutional support: RVO:61389013 Keywords : superbases * heavier alkali metal compounds * lithium -heavier alkali metal interchange Subject RIV: CD - Macromolecular Chemistry Impact factor: 1.329, year: 2013

  20. Effect of alkali treatment on surface morphology of titanium

    Energy Technology Data Exchange (ETDEWEB)

    Tan, K. J., E-mail: gd130056@siswa.uthm.edu.my; Wahab, M. A. A., E-mail: cd110006@siswa.uthm.edu.my; Mahmod, S., E-mail: cd110201@siswa.uthm.edu.my; Idris, M. I., E-mail: izwana@uthm.edu.my; Abdullah, H. Z., E-mail: hasan@uthm.edu.my [Faculty of Mechanical and Manufacturing Engineering, Universiti Tun Hussein Onn Malaysia, 86400 Parit Raja, Batu Pahat, Johor (Malaysia)

    2015-07-22

    Alkali and heat treatments were first introduced by Kim et al. to prepare a bioactive surface on titanium. This method has been proven very effective and widely used in other studies to promote titanium osteointegration. This study aims to investigate further the effect of alkali treatment on surface morphology of high purity titanium. High purity titanium foils were immersed in NaOH aqueous solutions of 0.5 M, 5 M and 15 M at 60°C and 80 °C for 1, 3 and 7 days. The surface morphology was examined using Field Emission Scanning Electron Microscope (FESEM). The obtained phases were analysed using Fourier Transform Infrared Spectroscopy (FTIR) in the spectra range of 4000-600 cm{sup −1} at 4 cm{sup −1} resolution and 50 scans. At the same soaking temperature and soaking time, a thicker porous network was observed with increasing concentration of NaOH. At the same soaking temperature, a much porous structure was observed with increasing soaking time. At constant alkali concentration, more homogenously distributed porous surface structure was observed with increasing soaking temperature.

  1. Effects of Alkali Concentration and Conching Temperature on Flavour, Hardness and Colour of Chocolate

    Directory of Open Access Journals (Sweden)

    Misnawi Jati

    2006-05-01

    Full Text Available Alkalization is an addition of alkali into cocoa mass to improve product quality in terms of flavour and colour appearance. Sodium bicarbonate and potassium bicarbonate are usual to be added into cocoa cotyledon prior to roasting. A study has been carried out to evaluate the effects of alkalization proceeded upon conching on chocolate sensory properties, hardness and colour. Re sponse Surface Methodology design at alkali concentrations of 1—15 g kg -1 and conching temperature of 40—80 oC have been used in the study. Parameters evaluated were sensory properties, particle size, hardness and colour. Results of the study showed that alkali concentration significantly influenced aroma, overall preference, particle size and hardness; meanwhile, conching temperature showed significant influence on aroma, taste, appearance, overall preference and texture of chocolate. Alkali concentration and conching temperature showed interactively influence on aroma and overall preference. A good quality of chocolate could be found at the alkali concentration of 8—15 g kg -1 and conching temperature of 74—80 oC. Key words: cocoa bean, chocolate, flavour, conching, alkalization, colour, particle size, texture.

  2. Electrical properties of alkali-activated slag composite with combined graphite/CNT filler

    Science.gov (United States)

    Rovnaník, P.; Míková, M.; Kusák, I.

    2017-10-01

    Alkali-activated industrial by-products such as blast furnace slag are known to possess properties which are comparable to or even better than those observed for ordinary Portland cement. The combination of alkali-activated slag matrix with conductive filler introduces new functionalities which are commonly known for self-sensing or self-heating concrete. The present paper discusses the effect of the mixture of two different conductive fillers, graphite powder and carbon nanotubes (CNTs), on the electrical properties of alkali-activated slag mortars. Prepared samples were also tested for their mechanical properties and microstructure was investigated by means of mercury intrusion porosimetry and scanning electron microscopy. The percolation threshold for the resistance was reached for the mixture containing 0.1% CNTs and 8% graphite powder.

  3. Cationic polyelectrolyte induced separation of some inorganic contaminants and their mixture (zirconium silicate, kaolin, K-feldspar, zinc oxide) as well as of the paraffin oil from water.

    Science.gov (United States)

    Ghimici, Luminita

    2016-03-15

    The flocculation efficiency of a cationic polyelectrolyte with quaternary ammonium salt groups in the backbone, namely PCA5 was evaluated on zirconium silicate (kreutzonit), kaolin, K- feldspar and zinc oxide (ZnO) suspensions prepared either with each pollutant or with their mixture. The effect of several parameters such as settling time, polymer dose and the pollutant type on the separation efficacy was evaluated and followed by optical density and zeta potential measurements. Except for ZnO, the interactions between PCA5 and suspended particles led to low residual turbidity values (around 4% for kreutzonit, 5% for kaolin and 8% for K-feldspar) as well as to the reduction of flocs settling time (from 1200 min to 30 min and 120 min in case of kaolinit and K-feldspar, respectively), that meant a high efficiency in their separation. The negative value of the zeta potential and flocs size measurements, at the optimum polymer dose, point to contribution from charge patch mechanism for the particles flocculation. A good efficiency of PCA5 in separation of paraffin oil (a minimum residual turbidity of 9.8%) has been also found. Copyright © 2015 Elsevier Ltd. All rights reserved.

  4. Metal induced gap states at alkali halide/metal interface

    International Nuclear Information System (INIS)

    Kiguchi, Manabu; Yoshikawa, Genki; Ikeda, Susumu; Saiki, Koichiro

    2004-01-01

    The electronic state of a KCl/Cu(0 0 1) interface was investigated using the Cl K-edge near-edge X-ray absorption fine structure (NEXAFS). A pre-peak observed on the bulk edge onset of thin KCl films has a similar feature to the peak at a LiCl/Cu(0 0 1) interface, which originates from the metal induced gap state (MIGS). The present result indicates that the MIGS is formed universally at alkali halide/metal interfaces. The decay length of MIGS to an insulator differs from each other, mainly due to the difference in the band gap energy of alkali halide

  5. The behaviour of gaseous alkali compounds in coal gasification

    International Nuclear Information System (INIS)

    Nykaenen, J.

    1995-01-01

    In this project the behaviour of alkali compounds emitting from CO 2 /O 2 -and air gasification will be studied by using an equilibrium model developed at the Aabo Akademi. This research project is closely connected to the EU-project coordinated by the Delft University of Technology (DUT). In that project alkali emissions from a 1.6 MW pilot plant are measured. The results from those measurements will be compared with the calculations performed in this LIEKKI 2 -project. Furthermore, in the project carried out at DUT the behaviour of a honeycomb-structured filter under CO 2 /O 2 -gasification environment is going to be studied. (author)

  6. Thermochemistry of uranium(VI), arsenic, and alkali metal triple oxides

    International Nuclear Information System (INIS)

    Karyakin, N.V.; Chernorukov, G.N.

    1994-01-01

    The standard enthalpies of reactions of stoichiometric mixtures of potassium dyhydrogen orthoarsenate, uranium(VI) oxide, alkali metal nitrates, and of mixtures of triple oxides with the general formula M I AsUO 6 (M I =Li, Na, K, Rb, and Cs) and potassium nitrate with aqueous solution of hydrofluoric acid were determined an an adiabatic calorimeter at 298.15 K. The standard enthalpies of formation of uranium(VI), arsenic, and alkali metal triple oxides at 298.15 K were calculated form the data obtained. 8 refs., 1 tab

  7. Positronium-alkali atom scattering at medium energies

    International Nuclear Information System (INIS)

    Chakraborty, Ajoy; Basu, Arindam; Sarkar, Nirmal K; Sinha, Prabal K

    2004-01-01

    We investigate the scattering of orthopositronium (o-Ps) atom off different atomic alkali targets (Na to Cs) at low and medium energies (up to 120 eV). Projectile-elastic and target-elastic close-coupling models have been employed to investigate the systems in addition to the static-exchange model. Elastic, excitation and total cross sections have been reported for all four systems. The magnitude of the alkali excitation cross section increases with increasing atomic number of the target atom while the position of the peak value shifts towards lower incident energies. The magnitudes of the Ps excitation and ionization cross sections increase steadily with atomic number with no change in the peak position. The reported results show regular behaviour with increasing atomic number of the target atom. Scattering parameters for the Ps-Rb and Ps-Cs systems are being reported for the first time

  8. Re ‘Luminescence dating of K-feldspar from sediments: a protocol without anomalous fading correction’ by Bo Li and Sheng-Hua Li

    DEFF Research Database (Denmark)

    Thomsen, Kristina Jørkov; Murray, Andrew; Jain, Mayank

    2012-01-01

    Have recently proposed a new measurement procedure (MET-pIRIR) for luminescence dating using feldspar; they argue that this procedure reduces anomalous fading to negligible levels, and that it is a significant improvement over existing protocols (pIRIR290). Here we compare the measured equivalent...

  9. Effects of alkali stress on growth, free amino acids and carbohydrates metabolism in Kentucky bluegrass (Poa pratensis).

    Science.gov (United States)

    Zhang, Pingping; Fu, Jinmin; Hu, Longxing

    2012-10-01

    Soil alkalization is one of the most prominent adverse environmental factors limiting plant growth, while alkali stress affects amino acids and carbohydrates metabolism. The objective of this study was conducted to investigate the effects of alkali stress on growth, amino acids and carbohydrates metabolism in Kentucky bluegrass (Poa pratensis). Seventy-day-old plants were subjected to four pH levels: 6.0 (control), 8.0 (low), 9.4 (moderate) and 10.3 (severe) for 7 days. Moderate to severe alkali stress (pH >9.4) caused a significant decline in turf quality and growth rate in Kentucky bluegrass. Soluble protein was unchanged in shoots, but decreased in roots as pH increased. The levels of amino acids was kept at the same level as control level at 4 days after treatment (DAT) in shoots, but greater at 7 DAT, when plants were subjected to severe (pH 10.3) alkali stress. The alkali stressed plants had a greater level of starch, water soluble carbohydrate and sucrose content, but lower level of fructose and glucose. Fructan and total non-structural carbohydrate (TNC) increased at 4 DAT and decreased at 7 DAT for alkali stressed plants. These results suggested that the decrease in fructose and glucose contributed to the growth reduction under alkali stress, while the increase in amino acids, sucrose and storage form of carbohydrate (fructan, starch) could be an adaptative mechanism in Kentucky bluegrass under alkali stress.

  10. Microbialproperty improvement of saline-alkali soil for vegetable cultivation in Shanghai coastal area and its evaluation

    Directory of Open Access Journals (Sweden)

    KOU Yiming

    2015-10-01

    Full Text Available In order to improve the fertility of saline-alkali soil in Shanghai coastal area,and make it suitable for vegetable cultiration,in the study,the saline-alkali soil was mixed with organic fertilizer,and then sprayed with composite microbes,which have the ability of the synergistically degrading organic substrate.The results showed that the saline-alkali soil added with 5∶1 organic fertilizer can rapidly increase the utilization ability soil organic matter.The soil microbial populations and microbial diversity index were significantly improved when applied with the 0.5% composite microbial liquid which containeds 1∶3∶3∶1 of Bacillus licheniformis,Pseudomonas sp., Flavobacterium sp.and Sphingomonas sp..At the same time,the enzymology indicators of soil urease,phosphatase,cellulase and catalase increased significantly.The vegetable cultivation experiments showed that:the biomass of Brassica chinensis nearly doubled in the original saline-alkali soil,while the yield of organic fertilizer increased 30.2% after 50 days.The research result on of the biological improvement for saline-alkali soil will have good application value in vegetable planting in coastal saline-alkali soil.

  11. Selective release of phosphorus and nitrogen from waste activated sludge with combined thermal and alkali treatment.

    Science.gov (United States)

    Kim, Minwook; Han, Dong-Woo; Kim, Dong-Jin

    2015-08-01

    Selective release characteristics of phosphorus and nitrogen from waste activated sludge (WAS) were investigated during combined thermal and alkali treatment. Alkali (0.001-1.0N NaOH) treatment and combined thermal-alkali treatment were applied to WAS for releasing total P(T-P) and total nitrogen(T-N). Combined thermal-alkali treatment released 94%, 76%, and 49% of T-P, T-N, and COD, respectively. Release rate was positively associated with NaOH concentration, while temperature gave insignificant effect. The ratio of T-N and COD to T-P that released with alkali treatment ranged 0.74-0.80 and 0.39-0.50, respectively, while combined thermal-alkali treatment gave 0.60-0.90 and 0.20-0.60, respectively. Selective release of T-P and T-N was negatively associated with NaOH. High NaOH concentration created cavities on the surface of WAS, and these cavities accelerated the release rate, but reduced selectivity. Selective release of P and N from sludge has a beneficial effect on nutrient recovery with crystallization processes and it can also enhance methane production. Copyright © 2015 Elsevier Ltd. All rights reserved.

  12. Secondary cell with orthorhombic alkali metal/manganese oxide phase active cathode material

    Science.gov (United States)

    Doeff, Marca M.; Peng, Marcus Y.; Ma, Yanping; Visco, Steven J.; DeJonghe, Lutgard C.

    1996-01-01

    An alkali metal manganese oxide secondary cell is disclosed which can provide a high rate of discharge, good cycling capabilities, good stability of the cathode material, high specific energy (energy per unit of weight) and high energy density (energy per unit volume). The active material in the anode is an alkali metal and the active material in the cathode comprises an orthorhombic alkali metal manganese oxide which undergoes intercalation and deintercalation without a change in phase, resulting in a substantially linear change in voltage with change in the state of charge of the cell. The active material in the cathode is an orthorhombic structure having the formula M.sub.x Z.sub.y Mn.sub.(1-y) O.sub.2, where M is an alkali metal; Z is a metal capable of substituting for manganese in the orthorhombic structure such as iron, cobalt or titanium; x ranges from about 0.2 in the fully charged state to about 0.75 in the fully discharged state, and y ranges from 0 to 60 atomic %. Preferably, the cell is constructed with a solid electrolyte, but a liquid or gelatinous electrolyte may also be used in the cell.

  13. Energy loss spectroscopy study of Si(111)--alkali metal interfaces at low temperatures

    International Nuclear Information System (INIS)

    Avci, R.

    1986-01-01

    Studies are made at approx.150 K under ultrahigh vacuum conditions on a wide range of alkali metal coverages on Si(111)-7 x 7. Negative second-derivative backscattered electron energy loss spectroscopy is used with 100 eV primary electrons. The interaction of the alkali metals with the silicon substrate goes through two stages as a function of alkali coverage: In the initial coverages, for less than approx.0.3 monolayer of alkali atoms, the basic reaction is that of charge transfer from the alkali atoms to the Si surface with a loss peak at approx.3.3 eV associated with the charge transfer states. The second stage of reaction: starting after the depletion of all the Si surface states: falls in a coverage range between approx.0.3 and approx.1 monolayer, in which the formation of a metallic layer with a coverage-dependent loss feature at about 2 eV is observed. At still higher coverages, multiple surface and bulk plasmon excitations and their combinations are dominant. In the overall scattering processes most of the parallel momentum (approx.3 A -1 ) is transferred to the sample during the elastic backscattering from the surface, and all the losses are essentially attributed to the forward inelastic scattering before and/or after the elastic process takes place near the metal/Si interface

  14. Freezing of liquid alkali metals as screened ionic plasmas

    International Nuclear Information System (INIS)

    Badirkhan, Z.; Rovere, M.; Tosi, M.P.

    1990-08-01

    The relationship between Wigner crystallization of the classical ionic plasma and the liquid-solid transition of alkali metals is examined within the density wave theory of freezing. Freezing of the classical plasma on a rigid neutralizing background into the bcc structure is first re-evaluated, in view of recent progress in the determination of its thermodynamic functions by simulation and of the known difficulties of the theory relating to the order parameter at the (200) star of reciprocal lattice vectors. Freezing into the fcc structure is also considered in this context and found to be unfavoured. On allowing for long-wavelength deformability of the background, the ensuing appearance of a volume change on freezing into the bcc structure is accompanied by reduced stability of the fluid phase and by an increase in the entropy of melting. Freezing of alkali metals into the bcc structure is next evaluated, taking their ionic pair structure as that of an ionic plasma reference fluid screened by conduction electrons and asking that the correct ionic coupling strength at liquid-solid coexistence should be approximately reproduced. The ensuring values of the volume and entropy changes across the phase transition, as estimated from the theory by two alternative routes, are in reasonable agreement with experiment. The order parameters of the phase transition, excepting the (200) one, conform rather closely to a Gaussian behaviour and yield a Lindemann ratio in reasonable agreement with the empirical value for melting of bcc crystals. It is suggested that ionic ordering at the (200) star in the metal may be (i) assisted by medium range ordering in the conduction electrons, as indicated by differences in X-ray and neutron diffraction intensities from the liquid, and/or (ii) quite small in the hot bcc solid. Such a possible premelting behaviour of bcc metals should be worth testing experimentally by diffraction. (author). 48 refs, 1 fig., 1 tab

  15. Terahertz radiation in alkali vapor plasmas

    International Nuclear Information System (INIS)

    Sun, Xuan; Zhang, X.-C.

    2014-01-01

    By taking advantage of low ionization potentials of alkali atoms, we demonstrate terahertz wave generation from cesium and rubidium vapor plasmas with an amplitude nearly one order of magnitude larger than that from nitrogen gas at low pressure (0.02–0.5 Torr). The observed phenomena are explained by the numerical modeling based upon electron tunneling ionization

  16. The influence of alkali treatment on banana fibre’s mechanical properties

    Directory of Open Access Journals (Sweden)

    Julio César Mejía Osorio

    2012-01-01

    Full Text Available This work analyses the effect of alkali treatment on the mechanical properties of banana fibre (Musa Paradisiaca. Fibres were extracted from the pseudostem by a defibring machine; they were mercerised and modified by 5% NaOH (w/v alkali treatment. Morphological characterisation showed that treated fibres’ surface was rougher than that of untreated fibres. Mechanical characterisation indicated that Young’s modulus, ultimate tensile strength and strain became decreased by increasing both treated and untreated fibres’ diameter.

  17. Heterogeneous studies in pulping of wood: Modelling mass transfer of alkali

    OpenAIRE

    Simão, João P. F.; Egas, Ana P. V.; Carvalho, M. Graça; Baptista, Cristina M. S. G.; Castro, José Almiro A. M.

    2008-01-01

    In this paper a heterogeneous lumped parameter model is proposed to describe the mass transfer of effective alkali during the kraft pulping of wood. This model, based on the spatial mean of the concentration profile of effective alkali along the chip thickness, enables the estimation of the effective diffusion coefficient that characterizes the internal resistance to mass transfer and the contribution of the external resistance to mass transfer which has often been neglected. http://www.sc...

  18. Alkali Metal Variation and Twisting of the FeNNFe Core in Bridging Diiron Dinitrogen Complexes.

    Science.gov (United States)

    McWilliams, Sean F; Rodgers, Kenton R; Lukat-Rodgers, Gudrun; Mercado, Brandon Q; Grubel, Katarzyna; Holland, Patrick L

    2016-03-21

    Alkali metal cations can interact with Fe-N2 complexes, potentially enhancing back-bonding or influencing the geometry of the iron atom. These influences are relevant to large-scale N2 reduction by iron, such as in the FeMoco of nitrogenase and the alkali-promoted Haber-Bosch process. However, to our knowledge there have been no systematic studies of a large range of alkali metals regarding their influence on transition metal-dinitrogen complexes. In this work, we varied the alkali metal in [alkali cation]2[LFeNNFeL] complexes (L = bulky β-diketiminate ligand) through the size range from Na(+) to K(+), Rb(+), and Cs(+). The FeNNFe cores have similar Fe-N and N-N distances and N-N stretching frequencies despite the drastic change in alkali metal cation size. The two diketiminates twist relative to one another, with larger dihedral angles accommodating the larger cations. In order to explain why the twisting has so little influence on the core, we performed density functional theory calculations on a simplified LFeNNFeL model, which show that the two metals surprisingly do not compete for back-bonding to the same π* orbital of N2, even when the ligand planes are parallel. This diiron system can tolerate distortion of the ligand planes through compensating orbital energy changes, and thus, a range of ligand orientations can give very similar energies.

  19. New insight into atmospheric alteration of alkali-lime silicate glasses

    International Nuclear Information System (INIS)

    Alloteau, Fanny; Lehuédé, Patrice; Majérus, Odile; Biron, Isabelle; Dervanian, Anaïs; Charpentier, Thibault; Caurant, Daniel

    2017-01-01

    Highlights: •Glass silicate network hydrolysis is by far the predominant reaction at 80 °C. •Atmospheric conditions yield different altered layer structure than in immersion. •The altered layer bears about 10 wt% of water mainly as H-bonded SiOH groups. •Alkali ions stay embedded into the altered layer closed to SiOH and H 2 O species. -- Abstract: A mixed alkali lime silicate glass altered in atmospheric conditions (80 °C/85%RH, Relative Humidity) for various lengths of time was characterized at all scales. The altered glass forms a hydrated solid phase bearing about 10 wt% of H 2 O in the form of Si-OH groups and molecular water. No alkali depletion was observed after ageing tests. Structural results from 1 H, 23 Na and 29 Si MAS NMR point out the close proximity of Si-OH, H 2 O and Na + species. This study gives new insight into the mechanisms of the atmospheric alteration, essential to conservation strategies in industry and cultural heritage.

  20. Theoretical investigation on the alkali-metal doped BN fullerene as a material for hydrogen storage

    International Nuclear Information System (INIS)

    Venkataramanan, Natarajan Sathiyamoorthy; Belosludov, Rodion Vladimirovich; Note, Ryunosuke; Sahara, Ryoji; Mizuseki, Hiroshi; Kawazoe, Yoshiyuki

    2010-01-01

    Graphical abstract: First-principles calculations have been used to investigate hydrogen adsorption on alkali atom doped B 36 N 36 clusters. Adsorption of alkali atoms involves a charge transfer process, creating positively-charged alkali atoms and this polarizes the H 2 molecules and increases their binding energy. The maximum hydrogen storage capacity of Li doped BN fullerene is 8.9 wt.% in which 60 hydrogen atoms were chemisorbed and 12 H 2 were adsorbed in molecular form. - Abstract: First-principles calculations have been used to investigate hydrogen adsorption on alkali atom doped B 36 N 36 clusters. The alkali atom adsorption takes place near the six tetragonal bridge sites available on the cage, thereby avoiding the notorious clustering problem. Adsorption of alkali atoms involves a charge transfer process, creating positively charged alkali atoms and this polarizes the H 2 molecules thereby, increasing their binding energy. Li atom has been found to adsorb up to three hydrogen molecules with an average binding energy of 0.189 eV. The fully doped Li 6 B 36 N 36 cluster has been found to hold up to 18 hydrogen molecules with the average binding energy of 0.146 eV. This corresponds to a gravimetric density of hydrogen storage of 3.7 wt.%. Chemisorption on the Li 6 B 36 N 36 has been found to be an exothermic reaction, in which 60 hydrogen atoms chemisorbed with an average chemisorption energy of -2.13 eV. Thus, the maximum hydrogen storage capacity of Li doped BN fullerene is 8.9 wt.% in which 60 hydrogen atoms were chemisorbed and 12 hydrogen molecules were adsorbed in molecular form.